Thu Aug 25 16:38:42 2022

Number of Points = 9925

Depth (nm)	Load (N)	Time (s)
1.437823	95.852193	0.000000
1.570537	103.750389	0.005005
1.585967	116.814454	0.010010
1.323066	103.909444	0.015014
1.430305	102.241172	0.020019
1.092327	103.009172	0.025024
1.283214	98.853711	0.030029
1.201144	88.672876	0.035034
0.614853	79.406288	0.040038
0.383554	71.542588	0.045043
0.097996	73.482465	0.050048
-0.095741	60.883028	0.055053
0.114860	55.066668	0.060058
-0.435257	50.283832	0.065062
-0.515231	39.558526	0.070067
-1.138184	36.887855	0.075072
-1.267351	18.112132	0.080077
-1.501820	24.533394	0.085082
-1.668722	14.919553	0.090086
-1.909841	11.249419	0.095091
-2.277741	5.134572	0.100096
-2.974330	0.820791	0.105101
-2.951786	-1.419498	0.110106
-3.583901	6.310587	0.115110
-3.580230	-3.032575	0.120115
-4.127895	-0.466341	0.125120
-4.528728	3.070311	0.130125
-4.481661	-6.371398	0.135130
-5.164526	-2.066054	0.140134
-5.070015	-10.259178	0.145139
-5.456383	-4.962575	0.150144
-5.402678	-12.013511	0.155149
-5.499843	-15.174682	0.160154
-5.889608	-4.369425	0.165158
-6.348243	-7.752373	0.170163
-6.844264	2.696212	0.175168
-6.749819	-5.579162	0.180173
-6.904025	-7.102055	0.185178
-7.849836	3.385367	0.190182
-7.905999	2.125522	0.195187
-8.079806	-10.834491	0.200192
-8.379333	0.829830	0.205197
-8.467881	-1.965696	0.210202
-8.441299	-2.197624	0.215206
-8.547936	-7.227100	0.220211
-8.398092	-1.413395	0.225216
-9.067344	-1.561608	0.230221
-9.431568	1.735189	0.235226
-9.794798	7.553357	0.240230
-9.219311	0.243490	0.245235
-10.490604	0.800216	0.250240
-11.256905	-6.084276	0.255245
-11.131665	-1.067149	0.260250
-11.231829	11.217678	0.265254
-11.175884	3.546286	0.270259
-11.657567	1.865893	0.275264
-11.572188	1.415943	0.280269
-11.744570	0.205947	0.285274
-12.623345	-1.023084	0.290278
-12.894156	-7.937753	0.295283
-13.082299	-1.229528	0.300288
-13.108794	-1.953016	0.305293
-13.105020	-8.926527	0.310298
-13.148357	7.509750	0.315302
-13.721124	-5.327644	0.320307
-14.145088	2.236947	0.325312
-14.188986	2.629834	0.330317
-14.216653	1.245301	0.335322
-14.730945	-3.435563	0.340326
-14.933457	0.256678	0.345331
-15.924279	4.926653	0.350336
-16.060148	-1.711767	0.355341
-15.728298	2.713000	0.360346
-16.068845	1.810928	0.365350
-16.182086	0.341727	0.370355
-16.014403	5.655927	0.375360
-16.663919	1.492962	0.380365
-16.953346	-3.583805	0.385370
-17.339054	4.946071	0.390374
-17.593708	9.073592	0.395379
-18.030410	-6.575566	0.400384
-18.833977	1.909048	0.405389
-18.259368	2.524564	0.410394
-18.781790	4.681882	0.415398
-19.040975	-0.361659	0.420403
-18.763182	3.590685	0.425408
-18.947750	-0.486941	0.430413
-19.166812	0.910996	0.435418
-19.609060	6.659286	0.440422
-19.752876	4.119193	0.445427
-20.153118	6.323806	0.450432
-20.753477	6.440048	0.455437
-21.271557	14.088994	0.460442
-21.819336	12.906178	0.465446
-21.120777	1.846940	0.470451
-21.610847	-2.964270	0.475456
-21.556661	1.459710	0.480461
-21.264155	-2.562952	0.485466
-22.067749	0.423036	0.490470
-22.225741	6.712085	0.495475
-22.621471	0.974926	0.500480
-22.910600	1.542279	0.505485
-23.311353	3.924143	0.510490
-24.211335	7.450420	0.515494
-24.084150	4.054776	0.520499
-24.311762	8.402688	0.525504
-24.312386	8.080109	0.530509
-24.064378	1.637806	0.535514
-24.857512	12.265827	0.540518
-25.401000	3.378557	0.545523
-25.822190	4.159592	0.550528
-26.002475	1.185450	0.555533
-25.740780	5.988207	0.560538
-25.674069	8.315809	0.565542
-25.751674	2.962242	0.570547
-26.423124	2.823866	0.575552
-27.076781	3.581213	0.580557
-26.661310	9.372283	0.585562
-27.309423	6.553701	0.590566
-27.469562	5.987195	0.595571
-28.023623	-4.910572	0.600576
-28.468353	0.477435	0.605581
-28.493536	1.639349	0.610586
-28.498292	12.368470	0.615590
-28.243187	8.244098	0.620595
-28.963664	12.628106	0.625600
-29.261602	8.732758	0.630605
-29.607116	7.942196	0.635610
-30.024667	8.972599	0.640614
-29.890887	12.764011	0.645619
-30.342441	1.771084	0.650624
-31.006107	-1.029241	0.655629
-31.612488	10.983722	0.660634
-31.515877	9.294978	0.665638
-31.187408	6.696704	0.670643
-31.629706	4.874099	0.675648
-31.897500	7.212984	0.680653
-31.495394	6.887415	0.685658
-31.906084	13.298318	0.690662
-32.314321	9.872671	0.695667
-32.875817	11.295790	0.700672
-32.790822	6.233122	0.705677
-32.977051	0.355570	0.710682
-34.096444	2.736140	0.715686
-34.089624	2.757246	0.720691
-34.657479	5.538618	0.725696
-34.553458	6.835313	0.730701
-34.649066	6.597220	0.735706
-34.792083	8.274309	0.740710
-34.517261	-1.614377	0.745715
-35.210884	0.601403	0.750720
-35.848409	0.906968	0.755725
-35.700837	7.787221	0.760730
-35.911469	-0.772548	0.765734
-36.079861	-4.770449	0.770739
-37.193334	0.181337	0.775744
-37.627451	0.477177	0.780749
-37.428211	-1.148553	0.785754
-37.626313	6.216135	0.790758
-37.487310	1.910638	0.795763
-37.750428	1.562749	0.800768
-37.882006	5.041395	0.805773
-37.657309	-0.084290	0.810778
-38.416283	8.845760	0.815782
-39.125751	2.873022	0.820787
-39.221768	13.540512	0.825792
-39.051328	4.718550	0.830797
-39.646182	-4.556137	0.835802
-40.313210	6.726004	0.840806
-40.285774	4.348906	0.845811
-40.453574	8.399542	0.850816
-40.621783	4.901486	0.855821
-40.420479	5.148384	0.860826
-40.825005	13.646411	0.865830
-41.696330	6.148785	0.870835
-41.801056	8.920866	0.875840
-41.950581	6.245627	0.880845
-41.809860	2.575779	0.885850
-42.209279	15.881936	0.890854
-42.806513	12.460593	0.895859
-43.030288	12.394443	0.900864
-43.461345	9.171691	0.905869
-43.435014	7.930559	0.910874
-43.616558	11.154441	0.915878
-43.580150	-2.300422	0.920883
-43.552658	11.944920	0.925888
-44.368288	14.300042	0.930893
-44.407543	7.994498	0.935898
-45.015231	11.978018	0.940902
-45.066399	0.106105	0.945907
-45.638751	5.722920	0.950912
-46.434127	12.643354	0.955917
-46.080191	2.612556	0.960922
-46.559391	14.804911	0.965926
-46.418088	8.676720	0.970931
-46.782451	8.958468	0.975936
-46.888710	21.668199	0.980941
-46.636235	6.664026	0.985946
-46.852079	13.487327	0.990950
-47.206996	10.755684	0.995955
-47.692810	14.084191	1.000960
-48.176876	11.774583	1.005965
-48.472603	8.021259	1.010970
-49.524189	16.348589	1.015974
-49.336419	5.673105	1.020979
-49.254452	1.287960	1.025984
-49.356230	9.327257	1.030989
-49.436438	3.619756	1.035994
-49.880103	17.489671	1.040998
-49.584657	4.927527	1.046003
-50.186179	11.627760	1.051008
-50.716112	12.245500	1.056013
-50.674192	6.857386	1.061018
-50.743388	14.739719	1.066022
-51.551018	8.665302	1.071027
-51.536319	9.232505	1.076032
-52.432809	15.906191	1.081037
-52.397284	5.071065	1.086042
-52.519726	9.389842	1.091046
-52.457749	16.020916	1.096051
-52.658388	17.975955	1.101056
-53.386274	24.272047	1.106061
-53.622444	12.764475	1.111066
-54.052359	16.315179	1.116070
-53.994744	9.140237	1.121075
-53.831425	10.029005	1.126080
-54.157756	13.009818	1.131085
-54.338021	9.618055	1.136090
-55.371711	9.678810	1.141094
-55.507301	8.330171	1.146099
-55.447665	6.982580	1.151104
-55.439985	20.731156	1.156109
-55.300312	12.913765	1.161114
-55.978353	16.509675	1.166118
-56.466495	10.378870	1.171123
-57.007633	15.848427	1.176128
-57.210119	10.353075	1.181133
-56.884245	14.357996	1.186138
-57.278952	15.941645	1.191142
-57.465141	8.529657	1.196147
-58.045154	15.169574	1.201152
-58.701825	7.793340	1.206157
-58.531242	5.944308	1.211162
-58.774273	16.751893	1.216166
-58.376893	16.971232	1.221171
-59.099840	16.651102	1.226176
-59.595006	9.996212	1.231181
-59.712684	10.802458	1.236186
-60.227524	12.392275	1.241190
-59.994251	11.947625	1.246195
-59.904881	4.761382	1.251200
-60.956564	7.827376	1.256205
-61.123185	7.195447	1.261210
-61.356056	9.490896	1.266214
-61.632117	1.843056	1.271219
-61.417598	7.795323	1.276224
-61.591969	11.508466	1.281229
-61.669877	7.433110	1.286234
-62.810459	11.762723	1.291238
-62.720642	9.901036	1.296243
-62.991477	1.888543	1.301248
-63.262749	11.482499	1.306253
-63.251073	12.303278	1.311258
-64.162525	5.030244	1.316262
-64.054091	15.058253	1.321267
-64.545219	13.224318	1.326272
-64.871986	10.678092	1.331277
-64.389141	11.561085	1.336282
-64.863017	18.772834	1.341286
-64.535067	8.733449	1.346291
-65.354019	9.972283	1.351296
-66.042298	6.223522	1.356301
-65.812283	0.052960	1.361306
-65.986541	8.483265	1.366310
-66.221899	2.676688	1.371315
-66.662522	-0.832465	1.376320
-66.985398	6.434713	1.381325
-66.836993	3.665335	1.386330
-67.710823	13.638446	1.391334
-67.832309	10.917684	1.396339
-67.651906	10.648998	1.401344
-68.271306	14.175608	1.406349
-68.760255	3.286623	1.411354
-68.987844	10.693896	1.416358
-69.366451	4.368760	1.421363
-69.660579	-0.587043	1.426368
-69.958576	-0.378969	1.431373
-69.378510	-1.754322	1.436378
-69.622483	0.024007	1.441382
-69.274845	-1.783164	1.446387
-69.954244	0.547449	1.451392
-70.384377	6.537451	1.456397
-71.140571	-1.851407	1.461402
-71.493070	7.185795	1.466406
-71.561524	2.444567	1.471411
-71.651089	-2.976725	1.476416
-71.720038	3.352153	1.481421
-71.714040	-11.929757	1.486426
-72.947067	1.507007	1.491430
-73.055736	-7.967242	1.496435
-73.410877	-4.792091	1.501440
-73.628656	0.168048	1.506445
-73.062996	1.626525	1.511450
-73.732768	5.110406	1.516454
-73.750194	3.638848	1.521459
-73.385097	1.863742	1.526464
-74.422033	15.696900	1.531469
-74.564888	-6.272048	1.536474
-75.001609	-0.173448	1.541478
-75.510703	6.309819	1.546483
-76.075615	4.088813	1.551488
-76.028198	7.646979	1.556493
-75.699880	-6.169995	1.561498
-76.215645	7.651097	1.566502
-76.682722	10.976668	1.571507
-76.547811	7.076774	1.576512
-76.500349	2.178178	1.581517
-76.865262	6.247045	1.586522
-77.797316	9.632818	1.591526
-77.984028	0.303673	1.596531
-77.758364	10.528446	1.601536
-78.319321	7.920839	1.606541
-78.235646	-1.191244	1.611546
-79.024353	6.813317	1.616550
-79.446560	1.064494	1.621555
-79.394142	7.703388	1.626560
-79.990133	3.740850	1.631565
-79.169757	-2.322897	1.636570
-79.749402	6.281658	1.641574
-79.643290	-3.517313	1.646579
-80.372741	-3.111919	1.651584
-80.843497	3.514037	1.656589
-81.239537	-2.004766	1.661594
-80.874487	5.724096	1.666598
-81.453616	4.726533	1.671603
-81.896856	3.087578	1.676608
-82.435771	-0.251148	1.681613
-82.484469	-5.457378	1.686618
-82.709614	2.243738	1.691622
-82.490774	3.797688	1.696627
-82.524753	-1.246334	1.701632
-83.180257	4.440458	1.706637
-83.331190	5.289880	1.711642
-83.861413	5.167345	1.716646
-84.002704	9.685229	1.721651
-83.799621	2.424223	1.726656
-84.939166	7.512979	1.731661
-84.992302	0.674937	1.736666
-85.587084	1.622381	1.741670
-85.203801	2.040080	1.746675
-85.019069	-5.844474	1.751680
-85.550923	3.094279	1.756685
-85.384201	-1.588884	1.761690
-86.446006	-1.596486	1.766694
-86.768516	-0.786619	1.771699
-86.762293	-10.085878	1.776704
-87.194078	5.072980	1.781709
-87.163367	-2.793768	1.786714
-87.344731	-0.063464	1.791718
-88.151088	-7.305500	1.796723
-88.341161	4.265737	1.801728
-88.716399	3.290010	1.806733
-88.581258	-0.442238	1.811738
-89.197099	4.893489	1.816742
-88.903883	6.755325	1.821747
-88.846575	-1.324400	1.826752
-88.728962	2.115197	1.831757
-89.568604	-8.472053	1.836762
-90.015752	2.247282	1.841766
-90.406449	0.451398	1.846771
-90.183499	-4.515823	1.851776
-90.665526	-4.256766	1.856781
-91.374874	-13.731800	1.861786
-91.574362	0.371922	1.866790
-91.748319	0.737731	1.871795
-91.401109	3.138438	1.876800
-91.942142	-2.990398	1.881805
-91.775882	-8.692220	1.886810
-92.209291	1.585198	1.891814
-92.605827	2.466777	1.896819
-92.821739	-0.982672	1.901824
-93.262855	0.690507	1.906829
-93.694481	1.188441	1.911834
-94.087475	3.572255	1.916838
-94.222650	10.885952	1.921843
-94.094327	7.914076	1.926848
-94.527539	11.158410	1.931853
-94.313500	-3.665719	1.936858
-95.092867	-3.056348	1.941862
-95.902600	5.312176	1.946867
-95.791545	2.124706	1.951872
-96.222580	10.889476	1.956877
-96.168809	2.158567	1.961882
-95.937216	7.345689	1.966886
-95.894578	2.862303	1.971891
-96.228866	7.312351	1.976896
-96.992667	1.686658	1.981901
-97.379932	0.560955	1.986906
-97.386225	12.862703	1.991910
-97.835677	17.716779	1.996915
-98.133446	6.221385	2.006912
-97.797179	7.252144	2.016909
-97.594155	0.305038	2.026906
-96.489712	2.469885	2.036902
-96.633799	8.305469	2.046899
-95.852841	-1.443850	2.056896
-95.144558	2.297291	2.066893
-95.048812	2.450239	2.076890
-94.551719	-0.738395	2.086886
-93.968038	3.304207	2.096883
-93.135959	3.012323	2.106880
-92.499353	-4.718649	2.116877
-92.563656	-5.972476	2.126874
-91.671366	6.052189	2.136870
-91.096647	-0.744083	2.146867
-91.002322	-0.537059	2.156864
-90.265082	-2.914346	2.166861
-89.816436	3.404902	2.176858
-89.447295	4.436846	2.186854
-88.618585	7.056717	2.196851
-88.074364	0.493307	2.206848
-88.174759	2.264066	2.216845
-87.267122	6.617038	2.226842
-87.185780	-1.356382	2.236838
-86.102062	7.369102	2.246835
-85.449083	5.381988	2.256832
-85.087138	4.713941	2.266829
-84.987484	1.356332	2.276826
-84.052556	1.628045	2.286822
-83.796812	-0.334839	2.296819
-83.274219	0.302426	2.306816
-82.580603	0.824194	2.316813
-82.214806	-5.388139	2.326810
-81.994590	2.281547	2.336806
-81.294964	-1.046527	2.346803
-80.967349	-3.701753	2.356800
-79.705335	-2.049438	2.366797
-79.740232	3.813385	2.376794
-79.582182	-1.637799	2.386790
-78.803941	7.284439	2.396787
-78.011576	2.785579	2.406784
-77.920704	1.748190	2.416781
-77.017553	-6.309649	2.426778
-76.933102	1.631568	2.436774
-76.294576	-0.384958	2.446771
-75.340247	6.060964	2.456768
-75.152443	10.054725	2.466765
-75.002010	4.379818	2.476762
-74.424156	1.935639	2.486758
-73.804171	-1.858296	2.496755
-73.196672	-3.442305	2.506752
-72.366606	-1.034889	2.516749
-72.367511	7.293508	2.526746
-72.002292	4.207901	2.536742
-71.524573	9.385350	2.546739
-70.624792	-0.034127	2.556736
-70.069462	0.281227	2.566733
-69.635735	-2.989343	2.576730
-69.586668	4.200311	2.586726
-68.464365	5.545067	2.596723
-68.208200	11.587201	2.606720
-68.118955	2.000119	2.616717
-66.922276	7.758666	2.626714
-66.633827	2.936452	2.636710
-66.545211	5.561417	2.646707
-65.673565	10.141781	2.656704
-65.378218	7.421918	2.666701
-64.558345	3.004279	2.676698
-64.117370	10.180045	2.686694
-64.096188	6.983619	2.696691
-62.832516	2.531287	2.706688
-62.608853	4.856324	2.716685
-62.588212	2.312554	2.726682
-61.320219	5.132862	2.736678
-61.392069	1.551868	2.746675
-60.797019	4.106984	2.756672
-59.755327	2.451774	2.766669
-59.515190	-0.883497	2.776666
-59.543523	7.094402	2.786662
-59.121599	2.346309	2.796659
-58.194409	2.017350	2.806656
-57.208337	-0.712538	2.816653
-56.761095	2.553155	2.826650
-56.570121	3.679542	2.836646
-56.755300	8.080207	2.846643
-55.828508	6.423994	2.856640
-55.367516	2.604286	2.866637
-54.301736	1.806950	2.876634
-53.899357	6.096544	2.886630
-53.754243	-1.582760	2.896627
-53.386382	-1.076471	2.906624
-52.618923	-1.310709	2.916621
-52.268453	-1.460602	2.926618
-51.593022	1.496904	2.936614
-50.739086	5.972338	2.946611
-50.741486	5.906246	2.956608
-50.521911	3.331305	2.966605
-49.630187	-11.478534	2.976602
-49.320852	4.701793	2.986598
-48.261164	3.696336	2.996595
-47.974467	4.151986	3.006592
-47.849515	2.434512	3.016589
-47.498401	-6.721594	3.026586
-46.831129	-1.374273	3.036582
-46.256033	2.080463	3.046579
-45.334144	3.668868	3.056576
-44.604672	-0.655408	3.066573
-44.757097	-1.635668	3.076570
-44.726755	1.340553	3.086566
-43.808701	0.734260	3.096563
-43.200321	1.225037	3.106560
-42.241081	0.108607	3.116557
-41.920558	-4.772484	3.126554
-42.100232	-5.824501	3.136550
-41.143000	-6.351402	3.146547
-41.062482	-3.402050	3.156544
-39.891556	-3.376387	3.166541
-39.341353	-7.453994	3.176538
-39.264059	-7.722642	3.186534
-38.824320	-7.842172	3.196531
-37.909931	-4.285375	3.206528
-37.671390	-9.102935	3.216525
-37.470827	-12.292619	3.226522
-36.458465	-7.458705	3.236518
-36.235539	-0.160075	3.246515
-35.628028	-6.692218	3.256512
-35.004846	-8.468750	3.266509
-34.734184	-2.115275	3.276506
-33.684676	-5.374623	3.286502
-33.196947	-3.056115	3.296499
-33.557518	-4.751367	3.306496
-32.945505	-5.445922	3.316493
-32.037573	-1.596674	3.326490
-31.705019	2.149493	3.336486
-30.557830	-2.442974	3.346483
-30.322242	5.537924	3.356480
-30.378038	5.274290	3.366477
-29.808202	1.085900	3.376474
-29.343714	0.493655	3.386470
-28.849904	7.645307	3.396467
-27.698183	3.261205	3.406464
-27.313911	3.055332	3.416461
-26.965340	0.776962	3.426458
-26.998167	5.061888	3.436454
-25.910895	3.269660	3.446451
-25.664675	-1.406553	3.456448
-25.730338	-5.786807	3.466445
-24.719388	-3.160638	3.476442
-23.628796	-3.831978	3.486438
-23.195619	-5.581906	3.496435
-23.169801	-6.010383	3.506432
-23.086576	-6.742462	3.516429
-22.171522	-0.071800	3.526426
-21.569130	-2.076325	3.536422
-21.131338	2.635377	3.546419
-20.498133	0.885785	3.556416
-20.069732	-3.974196	3.566413
-19.694978	2.426329	3.576410
-18.884903	-2.851418	3.586406
-18.741756	-1.603495	3.596403
-18.368194	-6.565756	3.606400
-17.842568	-1.329287	3.616397
-16.808460	1.686065	3.626394
-15.897065	4.131430	3.636390
-15.917473	8.065951	3.646387
-15.672582	-0.158014	3.656384
-15.505339	-0.475602	3.666381
-14.424059	-1.326047	3.676378
-14.208347	1.757347	3.686374
-13.828154	8.904628	3.696371
-12.863260	0.634373	3.706368
-12.672833	10.032031	3.716365
-12.093357	-0.012005	3.726362
-11.584679	5.208116	3.736358
-11.283858	2.015391	3.746355
-9.993965	10.049680	3.756352
-9.628229	2.510035	3.766349
-9.734236	4.465408	3.776346
-9.400900	6.079510	3.786342
-8.719910	7.455407	3.796339
-8.278795	4.722209	3.806336
-7.485373	2.763780	3.816333
-6.754215	1.150897	3.826330
-6.517236	4.905705	3.836326
-6.201031	4.479247	3.846323
-5.477946	12.146180	3.856320
-4.908905	11.626253	3.866317
-4.855941	11.269550	3.876314
-4.003914	15.463356	3.886310
-3.684056	19.556810	3.896307
-2.953940	30.583713	3.906304
-2.986026	32.733416	3.916301
-2.710666	38.376579	3.926298
-2.224188	53.021316	3.936294
-1.535350	71.198172	3.946291
-1.083218	88.791239	3.956288
-0.760434	101.225172	3.966285
0.000000	117.211806	3.971290
0.319843	121.670123	3.976294
0.169071	127.217757	3.981299
0.270061	127.961272	3.986304
0.023276	128.322674	3.991309
0.410906	147.209935	3.996314
0.775130	154.967475	4.001318
0.403735	149.609273	4.006323
0.642702	146.291002	4.011328
0.623277	159.319429	4.016333
0.921159	148.474742	4.021338
0.886898	148.470647	4.026342
0.499984	138.097099	4.031347
1.353031	146.338037	4.036352
1.328472	149.464580	4.041357
0.861086	141.875125	4.046362
1.036110	146.270717	4.051366
0.946607	151.599948	4.056371
1.004288	146.899027	4.061376
0.521656	154.998065	4.066381
0.969779	147.537250	4.071386
1.467658	146.791708	4.076390
0.867094	143.108261	4.081395
0.336089	132.070749	4.086400
0.530695	143.654578	4.091405
0.842069	147.241021	4.096410
0.648374	151.722860	4.101414
0.790612	142.503445	4.106419
1.140846	146.912714	4.111424
0.971208	155.212652	4.116429
1.072351	152.216535	4.121434
1.400066	151.019921	4.126438
0.978527	155.388763	4.131443
1.338379	144.638774	4.136448
1.071986	153.956794	4.141453
1.304686	157.378393	4.146458
1.271368	155.061414	4.151462
1.000454	154.534406	4.156467
1.209918	146.917993	4.161472
0.937478	155.882616	4.166477
1.520964	142.294464	4.171482
1.232790	139.378332	4.176486
1.038007	154.190137	4.181491
1.178098	143.686556	4.186496
0.895779	148.802384	4.191501
1.182187	155.755857	4.196506
1.243903	148.994672	4.201510
1.026184	154.742631	4.206515
1.227236	139.698942	4.211520
1.263767	147.900134	4.216525
1.337749	149.869107	4.221530
1.640031	150.612723	4.226534
1.226538	146.827197	4.231539
1.401181	141.684003	4.236544
1.674834	153.116245	4.241549
1.720008	144.674513	4.246554
1.438745	148.752451	4.251558
1.647633	146.365885	4.256563
1.495061	131.690826	4.261568
0.954936	140.393659	4.266573
1.469953	147.004422	4.271578
1.503605	142.291448	4.276582
0.750812	140.700976	4.281587
1.373206	143.719825	4.286592
1.400903	160.575391	4.291597
1.346807	158.394546	4.296602
1.284117	154.304114	4.301606
1.208909	154.432987	4.306611
1.612345	158.235965	4.311616
1.457763	160.028777	4.316621
1.524732	150.916065	4.321626
1.408936	154.107525	4.326630
1.449023	148.972757	4.331635
1.374016	143.764273	4.336640
1.249020	149.905833	4.341645
1.551407	151.298010	4.346650
1.640565	150.812663	4.351654
0.979510	155.877102	4.356659
1.549444	163.599251	4.361664
1.777539	167.220893	4.366669
1.783568	175.907774	4.371674
2.125767	174.288104	4.376678
1.624781	162.435936	4.381683
1.626328	151.761066	4.386688
1.548357	155.699584	4.391693
1.561748	161.038006	4.396698
2.321439	167.369992	4.401702
1.512670	158.837421	4.406707
1.779829	148.924540	4.411712
1.439138	154.043189	4.416717
1.472979	161.400074	4.421722
1.794122	174.637746	4.426726
1.731309	184.955284	4.431731
1.884715	177.651366	4.436736
1.634949	190.624156	4.441741
1.798155	180.028345	4.446746
1.865920	176.404694	4.451750
1.888819	180.539388	4.456755
1.657441	170.040209	4.461760
1.761477	176.924187	4.466765
1.995244	174.138245	4.471770
2.078250	177.159353	4.476774
1.737742	182.983509	4.481779
2.239341	175.874976	4.486784
2.072931	186.730775	4.491789
2.319641	183.594784	4.496794
2.234305	182.734973	4.501798
2.001759	180.363783	4.506803
2.333211	173.414791	4.511808
1.989686	175.186587	4.516813
1.695519	158.717670	4.521818
2.197149	174.078445	4.526822
2.297383	181.700187	4.531827
1.890696	168.162753	4.536832
1.604902	167.353334	4.541837
1.804954	176.845059	4.546842
1.850514	172.136539	4.551846
1.735068	181.067086	4.556851
2.122287	172.884964	4.561856
1.690676	176.363196	4.566861
1.800853	169.461530	4.571866
1.738723	174.552357	4.576870
2.257536	193.317872	4.581875
2.551987	186.548681	4.586880
2.486044	194.756459	4.591885
2.052122	183.969463	4.596890
1.972998	177.768180	4.601894
1.988489	179.335027	4.606899
2.104105	186.236177	4.611904
2.025161	204.136729	4.616909
2.229836	211.036590	4.621914
2.186233	203.750874	4.626918
2.462057	209.984679	4.631923
2.290304	203.842194	4.636928
2.441695	207.007619	4.641933
2.251513	211.542708	4.646938
2.608345	208.553977	4.651942
2.490618	202.516924	4.656947
2.830843	196.477724	4.661952
2.529290	184.692372	4.666957
1.948425	192.249989	4.671962
2.192617	193.936030	4.676966
2.420487	202.515398	4.681971
2.329091	202.830308	4.686976
2.590052	208.746897	4.691981
2.091272	208.575134	4.696986
2.568759	204.412710	4.701990
1.987306	204.560790	4.706995
2.385918	207.070538	4.712000
2.115294	210.039490	4.717005
2.195343	203.952466	4.722010
2.428923	199.394817	4.727014
2.431294	213.255113	4.732019
2.244066	202.008667	4.737024
2.269628	216.697413	4.742029
2.316176	221.173266	4.747034
2.814398	224.040738	4.752038
2.439747	238.061368	4.757043
2.962021	231.452620	4.762048
2.732219	238.186445	4.767053
2.665191	228.392322	4.772058
2.811564	233.652982	4.777062
2.610517	234.165410	4.782067
2.809190	240.838428	4.787072
2.867539	236.520201	4.792077
2.889734	226.610858	4.797082
2.869795	216.417051	4.802086
2.488206	212.553744	4.807091
2.615274	216.937885	4.812096
2.564262	228.547597	4.817101
2.753501	230.267563	4.822106
2.511822	228.565362	4.827110
2.532402	235.405490	4.832115
2.784254	237.438354	4.837120
2.716984	241.220188	4.842125
2.702176	231.708952	4.847130
2.931234	230.831517	4.852134
2.696185	237.544017	4.857139
2.825258	235.128815	4.862144
2.607513	243.929886	4.867149
2.539956	234.120024	4.872154
2.736320	237.256262	4.877158
2.418896	235.967732	4.882163
2.811750	253.857687	4.887168
2.883194	256.826836	4.892173
3.466510	259.257031	4.897178
3.505087	253.923148	4.902182
2.862560	245.095564	4.907187
3.334841	242.977770	4.912192
2.875890	239.325899	4.917197
2.729074	236.529974	4.922202
2.822126	230.833216	4.927206
2.875833	247.387390	4.932211
3.325844	249.680279	4.937216
3.379868	254.442876	4.942221
3.107553	246.841794	4.947226
2.959090	232.960125	4.952230
2.890173	236.814983	4.957235
3.096898	245.625480	4.962240
3.026661	257.269861	4.967245
3.031687	264.745201	4.972250
3.520927	256.395193	4.977254
3.364174	258.235812	4.982259
3.097425	256.455277	4.987264
2.820992	252.584977	4.992269
3.352792	263.407357	4.997274
3.087791	255.128068	5.002278
3.156957	260.078123	5.007283
3.003723	249.731173	5.012288
3.039146	257.787053	5.017293
3.349264	257.884026	5.022298
3.595786	263.284030	5.027302
3.361612	262.020420	5.032307
3.639396	263.910017	5.037312
3.439706	262.349933	5.042317
3.189616	260.516166	5.047322
3.390760	259.886717	5.052326
3.358997	264.542533	5.057331
3.448625	255.179440	5.062336
3.555618	261.945927	5.067341
3.529065	262.405705	5.072346
3.647467	261.805039	5.077350
3.135888	248.812336	5.082355
3.157589	254.484848	5.087360
3.145035	258.277095	5.092365
2.892638	258.054073	5.097370
3.521445	258.344727	5.102374
3.062350	266.139565	5.107379
3.462409	268.120737	5.112384
3.379672	265.279965	5.117389
3.537925	262.660868	5.122394
3.451648	269.261482	5.127398
3.187743	261.149702	5.132403
3.549378	266.800595	5.137408
3.733435	279.531467	5.142413
3.268659	264.993802	5.147418
3.729168	269.898362	5.152422
3.777952	287.930848	5.157427
3.719101	267.147474	5.162432
3.425128	265.735042	5.167437
3.548067	275.590086	5.172442
3.739772	282.251557	5.177446
3.590121	284.692191	5.182451
3.632178	284.846985	5.187456
3.709329	279.620949	5.192461
4.137402	290.386829	5.197466
3.982172	276.088562	5.202470
3.476031	273.893107	5.207475
3.461507	264.457741	5.212480
3.803775	271.503750	5.217485
3.998030	283.151000	5.222490
3.504378	273.360421	5.227494
3.612553	287.204196	5.232499
3.974365	288.425719	5.237504
3.730929	291.738445	5.242509
3.585089	291.922679	5.247514
3.927060	290.764952	5.252518
4.013755	293.276127	5.257523
4.181106	279.974540	5.262528
4.028656	280.074386	5.267533
3.753231	287.919551	5.272538
4.091258	282.418516	5.277542
3.842148	292.784289	5.282547
4.123561	287.203536	5.287552
3.938407	298.846967	5.292557
3.598609	289.082894	5.297562
4.045885	286.548225	5.302566
3.235779	295.268123	5.307571
3.342483	296.390409	5.312576
3.340237	297.377902	5.317581
3.427127	292.204121	5.322586
3.971477	313.768909	5.327590
3.699131	317.601873	5.332595
3.935828	316.900411	5.337600
3.973225	316.717406	5.342605
4.045037	319.594756	5.347610
4.243001	321.034947	5.352614
4.182906	319.263156	5.357619
3.998673	316.403476	5.362624
4.081334	317.969302	5.367629
4.236621	316.777548	5.372634
4.422143	322.930626	5.377638
4.429547	326.080667	5.382643
4.322412	318.814350	5.387648
4.084759	315.921911	5.392653
4.206807	320.262570	5.397658
4.634197	314.798145	5.402662
4.248816	325.593422	5.407667
4.275861	325.728421	5.412672
4.469002	315.355635	5.417677
4.297991	315.021782	5.422682
4.487627	317.453555	5.427686
4.103453	324.977245	5.432691
4.316985	314.594938	5.437696
4.255974	316.800221	5.442701
4.384797	319.608526	5.447706
4.540081	325.291769	5.452710
4.104488	330.928386	5.457715
3.900823	319.934383	5.462720
4.161920	315.929227	5.467725
4.221363	319.080604	5.472730
4.117411	317.894666	5.477734
3.783004	327.821396	5.482739
4.057836	322.096128	5.487744
4.257058	342.050852	5.492749
4.029527	341.235459	5.497754
4.424973	343.647644	5.502758
4.310609	347.835522	5.507763
4.508243	338.347892	5.512768
4.428914	340.492772	5.517773
4.484413	347.454025	5.522778
4.626933	337.462490	5.527782
4.553926	349.281376	5.532787
4.713281	346.608309	5.537792
4.363460	343.366435	5.542797
4.367265	345.773543	5.547802
5.073503	343.793092	5.552806
4.545894	349.118256	5.557811
4.704815	346.454749	5.562816
5.274598	347.203917	5.567821
4.510494	342.454530	5.572826
4.847295	349.922216	5.577830
4.356785	352.084064	5.582835
4.540279	342.120909	5.587840
4.758970	346.528692	5.592845
4.753940	342.356414	5.597850
4.714951	346.871012	5.602854
4.630692	340.635674	5.607859
4.775654	343.786312	5.612864
4.711662	341.439313	5.617869
4.543232	340.877258	5.622874
4.735578	341.967145	5.627878
4.587754	345.261737	5.632883
4.902175	342.551719	5.637888
4.581969	346.177047	5.642893
4.390454	348.652724	5.647898
4.644244	353.681448	5.652902
4.975930	368.376140	5.657907
5.136114	361.254588	5.662912
4.967154	365.615543	5.667917
4.730191	356.838256	5.672922
4.960518	365.015511	5.677926
4.768593	370.240628	5.682931
5.096660	370.284169	5.687936
5.138013	365.623716	5.692941
4.758577	355.299490	5.697946
5.282914	360.029555	5.702950
5.358836	368.851116	5.707955
5.074875	348.697718	5.712960
4.798979	353.619605	5.717965
4.428470	350.121537	5.722970
5.221155	359.374968	5.727974
5.178087	363.893372	5.732979
5.014407	371.214851	5.737984
5.343128	361.152999	5.742989
5.124561	367.299802	5.747994
4.958345	344.498814	5.752998
4.909624	360.537618	5.758003
5.064937	365.948780	5.763008
5.173948	369.538500	5.768013
4.887155	372.649221	5.773018
5.282825	373.757875	5.778022
4.715233	382.006371	5.783027
4.693544	378.747881	5.788032
5.197575	370.866915	5.793037
4.737056	365.620690	5.798042
5.111038	365.897488	5.803046
5.222425	368.170681	5.808051
4.948433	368.210475	5.813056
5.234284	371.781980	5.818061
5.104325	377.759876	5.823066
5.303523	377.162366	5.828070
5.299495	398.025382	5.833075
5.578442	385.791428	5.838080
5.272589	377.875997	5.843085
5.149647	390.205784	5.848090
5.633714	384.700820	5.853094
5.400041	393.159601	5.858099
5.078206	382.658651	5.863104
5.243720	394.921098	5.868109
5.161118	404.900169	5.873114
5.725476	402.767931	5.878118
5.424616	403.536454	5.883123
5.373976	411.181933	5.888128
5.540788	401.749721	5.893133
5.513798	398.147199	5.898138
5.761195	404.376035	5.903142
5.548917	406.313956	5.908147
5.321980	407.096208	5.913152
5.607776	407.560836	5.918157
5.468640	402.919160	5.923162
5.525123	398.686610	5.928166
5.421983	407.463477	5.933171
5.820539	403.234278	5.938176
5.484785	408.121264	5.943181
5.238149	406.239483	5.948186
5.749040	401.166921	5.953190
5.451709	406.895797	5.958195
5.767563	406.903285	5.963200
5.834279	409.243595	5.968205
5.776643	404.484743	5.973210
6.029292	406.004960	5.978214
5.438550	412.048736	5.983219
5.773632	395.705640	5.988224
5.727458	402.356969	5.993229
5.409747	399.701692	5.998234
5.867161	400.506436	6.003238
5.787203	403.050065	6.008243
5.948461	398.288557	6.013248
5.418103	389.149088	6.018253
5.565501	378.416428	6.023258
5.471905	389.137551	6.028262
5.631456	405.172237	6.033267
5.688308	409.858500	6.038272
5.536563	406.183771	6.043277
5.557623	398.761291	6.048282
5.558030	401.311311	6.053286
5.376383	405.936863	6.058291
5.566131	393.982642	6.063296
5.739462	400.055398	6.068301
5.920015	400.482730	6.073306
5.856682	398.534264	6.078310
5.721664	407.116803	6.083315
5.847557	393.897559	6.088320
6.139345	398.043958	6.093325
5.372493	388.052505	6.098330
5.702502	382.498911	6.103334
5.579002	380.063151	6.108339
5.518294	380.588396	6.113344
5.509598	391.903676	6.118349
5.622420	399.460261	6.123354
5.872189	399.873584	6.128358
5.706330	396.745250	6.133363
5.667490	394.093738	6.138368
5.999309	384.920426	6.143373
5.632903	385.658089	6.148378
5.669389	376.353880	6.153382
5.744395	371.985553	6.158387
5.535357	365.725464	6.163392
5.788953	367.283495	6.168397
5.608561	372.190423	6.173402
5.792774	370.446789	6.178406
5.694546	374.337907	6.183411
5.781379	375.286137	6.188416
5.812059	378.666664	6.193421
6.027485	369.008547	6.198426
5.848022	372.270134	6.203430
5.493599	371.145583	6.208435
5.708749	373.842292	6.213440
5.864243	369.663840	6.218445
5.665098	372.589981	6.223450
5.702449	365.202928	6.228454
5.527655	376.724560	6.233459
5.393227	372.968030	6.238464
5.267380	373.294668	6.243469
5.379942	373.216947	6.248474
5.747455	370.555555	6.253478
5.792522	376.708512	6.258483
5.796867	379.321189	6.263488
5.974317	365.138409	6.268493
5.725570	379.712077	6.273498
5.685801	371.622077	6.278502
5.726462	383.154250	6.283507
5.670632	374.566878	6.288512
5.586571	377.807191	6.293517
5.449949	377.793824	6.298522
5.547766	370.080911	6.303526
5.268033	384.605652	6.308531
5.685855	376.393332	6.313536
5.779940	377.001895	6.318541
5.327243	381.647762	6.323546
5.270587	376.645148	6.328550
5.589819	384.919216	6.333555
5.546357	388.292379	6.338560
5.956739	390.455451	6.343565
5.746158	388.352881	6.348570
5.581101	373.964324	6.353574
5.491855	390.790973	6.358579
5.412251	383.400090	6.363584
6.033269	386.624846	6.368589
5.507455	391.788387	6.373594
5.535832	388.186683	6.378598
5.609089	391.823140	6.383603
5.716921	405.069095	6.388608
6.267073	404.527331	6.393613
5.629127	382.869584	6.398618
5.865258	375.793075	6.403622
5.693444	386.077187	6.408627
5.408524	371.489108	6.413632
6.082787	376.597494	6.418637
5.608612	378.487860	6.423642
5.586072	371.135498	6.428646
5.367272	378.604826	6.433651
5.622219	371.452603	6.438656
5.959255	367.081187	6.443661
5.966146	379.409607	6.448666
5.895720	370.830852	6.453670
5.638078	376.581974	6.458675
5.702420	368.219392	6.463680
5.896442	364.455695	6.468685
5.630413	374.105975	6.473690
6.054240	371.910335	6.478694
5.762575	371.886457	6.483699
5.654928	373.153067	6.488704
5.841920	371.646285	6.493709
5.446982	369.790909	6.498714
5.621120	380.042959	6.503718
5.761878	384.950193	6.508723
5.728609	372.015338	6.513728
6.190889	369.313787	6.518733
5.630300	367.199620	6.523738
5.521977	360.806690	6.528742
5.699427	372.589514	6.533747
5.608608	373.034053	6.538752
5.647435	374.714323	6.543757
5.503097	375.110299	6.548762
5.700404	379.584717	6.553766
5.634317	370.052968	6.558771
5.651416	373.340707	6.563776
5.805147	382.131099	6.568781
5.464338	370.519458	6.573786
5.732122	368.379906	6.578790
5.495568	377.664893	6.583795
5.606578	374.467871	6.588800
5.734522	371.739609	6.593805
5.477704	377.133088	6.598810
5.715892	359.074587	6.603814
5.955103	375.023997	6.608819
5.685601	372.304222	6.613824
5.708589	371.111045	6.618829
5.745361	383.766990	6.623834
5.780969	375.788567	6.628838
5.571842	367.775726	6.633843
5.467813	367.171942	6.638848
5.906733	373.848498	6.643853
5.369029	361.375511	6.648858
5.645958	366.698013	6.653862
5.375283	377.269699	6.658867
5.711909	372.214958	6.663872
5.786005	368.381462	6.668877
5.378277	382.018235	6.673882
5.914908	381.905708	6.678886
5.409739	373.249532	6.683891
5.551521	379.112083	6.688896
5.330161	377.539565	6.693901
5.694811	377.384380	6.698906
5.842742	372.881237	6.703910
5.408460	371.383210	6.708915
5.475984	372.321809	6.713920
5.699952	374.764030	6.718925
5.367485	372.864062	6.723930
5.483561	367.688850	6.728934
5.453913	376.270685	6.733939
5.125611	376.341135	6.738944
5.569441	363.110065	6.743949
5.379433	378.234527	6.748954
5.712059	393.198018	6.753958
5.817375	394.307872	6.758963
5.445515	383.637584	6.763968
5.855979	387.350924	6.768973
5.540095	390.697166	6.773978
5.860785	385.325370	6.778982
5.820286	380.627116	6.783987
5.563454	379.395522	6.788992
5.645901	372.593038	6.793997
5.725048	378.183821	6.799002
5.821189	371.891733	6.804006
5.548244	369.406621	6.809011
5.740411	376.650201	6.814016
5.688422	373.257250	6.819021
5.692607	375.120122	6.824026
5.808094	376.702957	6.829030
5.608061	370.460439	6.834035
5.632233	371.405831	6.839040
5.768980	372.960024	6.844045
5.492287	375.395265	6.849050
5.958750	376.344127	6.854054
5.750327	374.649356	6.859059
5.769635	378.025337	6.864064
5.480094	375.254916	6.869069
5.489846	374.351722	6.874074
5.659333	377.166321	6.879078
5.694770	383.478981	6.884083
5.528395	378.806778	6.889088
5.640112	370.120389	6.894093
5.524989	378.399233	6.899098
5.587280	375.640126	6.904102
5.521781	366.864443	6.909107
5.295935	372.332164	6.914112
5.716339	381.058626	6.919117
5.493525	390.977399	6.924122
5.906273	393.342586	6.929126
5.604427	393.722111	6.934131
5.542743	385.255878	6.939136
5.996551	386.406044	6.944141
5.376697	382.646473	6.949146
6.102361	383.238339	6.954150
5.643292	375.517762	6.959155
5.572886	377.629610	6.964160
5.673512	374.813876	6.969165
5.618987	381.643681	6.974170
5.714699	368.698110	6.979174
5.791972	375.032687	6.984179
5.770607	378.421369	6.989184
5.921920	375.309784	6.994189
5.023159	384.065762	6.999194
5.736140	374.184148	7.004198
5.720578	370.902552	7.009203
5.213786	369.140633	7.014208
5.845186	377.995390	7.019213
5.481102	381.172008	7.024218
6.117283	387.548736	7.029222
5.573731	383.979695	7.034227
5.463722	374.948383	7.039232
5.527302	369.398572	7.044237
5.599195	385.848782	7.049242
5.630814	395.936505	7.054246
5.771564	398.069056	7.059251
5.487298	392.687637	7.064256
5.857616	390.639588	7.069261
5.467504	391.577123	7.074266
5.952309	393.611472	7.079270
5.478952	381.419462	7.084275
5.797497	387.633981	7.089280
5.705747	381.570650	7.094285
5.460694	383.605456	7.099290
5.752295	379.541721	7.104294
5.656728	382.185872	7.109299
5.578582	374.453070	7.114304
5.974199	379.105230	7.119309
5.451989	374.700757	7.124314
5.625119	375.167218	7.129318
5.753718	378.209691	7.134323
5.613647	374.580598	7.139328
5.591026	373.828013	7.144333
5.609325	383.300868	7.149338
5.756791	382.730447	7.154342
5.896571	375.216607	7.159347
6.049346	382.055062	7.164352
5.704119	366.188754	7.169357
5.541072	370.096355	7.174362
5.830943	375.717397	7.179366
5.540842	373.636780	7.184371
5.622660	371.096083	7.189376
5.867698	367.666086	7.194381
5.779477	372.786369	7.199386
5.820754	366.132710	7.204390
5.780185	374.880774	7.209395
5.905181	372.254216	7.214400
5.847459	371.744419	7.219405
5.830445	373.082252	7.224410
5.918959	365.949781	7.229414
5.635311	381.867221	7.234419
5.693011	371.765567	7.239424
5.901384	378.788304	7.244429
5.873513	380.165805	7.249434
5.936003	373.790401	7.254438
5.644270	362.098308	7.259443
5.119530	358.678188	7.264448
5.656773	356.910881	7.269453
5.491989	364.938065	7.274458
5.417069	373.716822	7.279462
5.695472	380.168587	7.284467
5.630813	380.226204	7.289472
5.474832	362.276917	7.294477
5.327699	370.196932	7.299482
5.519977	368.847514	7.304486
5.193348	371.581652	7.309491
5.384668	376.012714	7.314496
5.704052	377.329478	7.319501
5.556218	383.860684	7.324506
5.569079	391.116544	7.329510
5.573408	384.750249	7.334515
5.396130	375.058743	7.339520
5.642386	373.485727	7.344525
5.168560	381.330380	7.349530
5.914642	396.668867	7.354534
5.801008	391.668848	7.359539
5.254028	400.322259	7.364544
6.043050	404.675498	7.369549
5.641040	400.223711	7.374554
5.788836	384.188388	7.379558
5.568387	390.879674	7.384563
5.507602	383.403583	7.389568
5.604280	395.996364	7.394573
5.707302	388.602176	7.399578
5.983816	393.469159	7.404582
5.832942	387.623903	7.409587
5.734110	384.137047	7.414592
5.711589	376.531573	7.419597
5.372502	381.219753	7.424602
5.243137	379.139262	7.429606
5.720968	389.112774	7.434611
5.561982	395.414771	7.439616
5.909335	395.088285	7.444621
5.762655	393.301579	7.449626
5.580699	389.103226	7.454630
5.564436	383.790553	7.459635
5.827350	386.239328	7.464640
6.015770	377.800352	7.469645
5.495272	382.634017	7.474650
5.450420	376.772154	7.479654
5.545482	374.352771	7.484659
5.558308	376.100392	7.489664
5.855290	379.730267	7.494669
5.356894	378.558669	7.499674
5.669880	388.165694	7.504678
5.853465	394.546897	7.509683
5.983731	399.835440	7.514688
5.963028	385.161657	7.519693
5.417926	381.475798	7.524698
5.759134	369.618089	7.529702
5.539373	372.357629	7.534707
5.303327	373.331137	7.539712
5.387548	364.054258	7.544717
5.757607	384.839662	7.549722
5.719496	386.525660	7.554726
5.620470	383.427987	7.559731
5.861324	395.447670	7.564736
5.758490	385.801444	7.569741
5.528495	377.032546	7.574746
5.683992	380.788997	7.579750
5.820776	379.264771	7.584755
5.347110	378.206360	7.589760
5.638865	380.916378	7.594765
5.686901	389.928984	7.599770
5.938018	391.939836	7.604774
6.022703	383.235528	7.609779
5.614491	377.883025	7.614784
5.643918	370.677550	7.619789
5.653340	382.451905	7.624794
5.456876	375.939899	7.629798
5.643874	378.498647	7.634803
5.542542	378.938506	7.639808
5.437602	371.788885	7.644813
5.576567	382.210967	7.649818
5.569905	385.809324	7.654822
5.885056	400.098497	7.659827
5.287288	393.801227	7.664832
5.793222	401.001982	7.669837
5.701798	400.298143	7.674842
5.715266	409.774932	7.679846
5.736513	399.400557	7.684851
5.483117	387.003231	7.689856
5.891233	387.043722	7.694861
5.566178	394.140551	7.699866
5.698755	381.717557	7.704870
5.763924	381.786470	7.709875
5.584516	373.351343	7.714880
5.773108	371.221035	7.719885
5.569856	379.140355	7.724890
5.579903	377.003218	7.729894
5.744735	383.978994	7.734899
5.364011	381.593028	7.739904
5.702872	385.589676	7.744909
5.805450	397.969557	7.749914
5.964626	398.659673	7.754918
5.670907	380.852175	7.759923
5.944124	379.651430	7.764928
5.587329	377.046574	7.769933
5.729161	381.308216	7.774938
5.742777	375.895949	7.779942
5.586717	373.341901	7.784947
5.495917	380.402022	7.789952
5.904060	373.950314	7.794957
5.491766	378.479116	7.799962
5.828565	372.649207	7.804966
5.857943	377.346094	7.809971
5.715195	382.503397	7.814976
5.753951	377.672500	7.819981
5.784964	384.678734	7.824986
5.671306	376.935676	7.829990
5.694653	390.261298	7.834995
5.510801	380.627768	7.840000
5.489834	377.210973	7.845005
5.246735	387.999813	7.850010
5.790320	376.983610	7.855014
5.849621	381.922589	7.860019
5.549544	374.686480	7.865024
5.352749	375.701295	7.870029
5.544230	378.737080	7.875034
5.271878	380.646446	7.880038
5.545393	382.065312	7.885043
5.622696	401.216607	7.890048
5.830138	391.860294	7.895053
5.822718	396.543969	7.900058
5.589018	381.235992	7.905062
5.073341	390.808334	7.910067
5.145964	395.068168	7.915072
5.596230	399.009398	7.920077
5.689974	412.747961	7.925082
5.401848	411.654150	7.930086
5.847236	404.320211	7.935091
5.380822	407.642584	7.940096
5.888183	407.268880	7.945101
5.693395	412.639996	7.950106
5.606573	409.812496	7.955110
5.929584	404.949709	7.960115
5.802117	414.739657	7.965120
5.895200	402.974588	7.970125
5.459232	405.828058	7.975142
5.469092	402.093264	7.980160
5.385449	400.209779	7.985178
5.772453	402.506532	7.990195
5.624121	398.572465	7.995213
5.547932	411.961745	8.000230
5.869145	409.702404	8.005248
5.249660	406.239784	8.010266
5.583701	411.501794	8.015283
5.702907	407.838228	8.020301
5.933802	398.918584	8.025318
5.393802	402.591332	8.030336
5.638111	410.508781	8.035354
5.637608	412.089930	8.040371
6.099580	404.014539	8.045389
6.171218	413.505372	8.050406
5.934309	414.410357	8.055424
5.923616	411.325715	8.060442
5.830432	402.838695	8.065459
5.746807	416.115535	8.070477
5.757817	404.090347	8.075494
6.034549	414.161265	8.080512
5.968884	403.079044	8.085530
5.790877	405.407519	8.090547
5.841074	397.418739	8.095565
5.509937	407.831046	8.100582
5.409461	407.935179	8.105600
5.793365	403.586363	8.110618
5.265127	409.636721	8.115635
5.543613	405.496923	8.120653
5.801104	421.298587	8.125670
5.783504	412.335820	8.130688
6.131824	415.585367	8.135706
5.721503	422.756488	8.140723
5.985663	406.813187	8.145741
5.777273	411.257635	8.150758
5.499842	412.938978	8.155776
5.391019	412.182893	8.160794
5.601686	407.327893	8.165811
5.609608	403.618649	8.170829
5.689136	414.667198	8.175846
5.711671	428.823654	8.180864
6.229023	432.640006	8.185882
5.890209	437.429941	8.190899
6.180805	429.192043	8.195917
5.856946	414.988181	8.200934
5.644755	416.760287	8.205952
5.730267	418.839195	8.210970
5.701237	439.586685	8.215987
5.984672	430.901787	8.221005
5.836861	432.559667	8.226022
5.913313	439.272677	8.231040
6.258320	434.377687	8.236058
6.091718	434.874029	8.241075
6.174965	424.144000	8.246093
5.835431	421.382276	8.251110
5.890336	411.896915	8.256128
6.415257	404.430191	8.261146
5.848866	413.146843	8.266163
5.762839	412.178905	8.271181
6.068445	407.955964	8.276198
5.459563	410.897899	8.281216
5.778036	416.900801	8.286234
6.104886	427.557160	8.291251
6.553648	426.423379	8.296269
6.196018	426.675099	8.301286
6.090391	411.821671	8.306304
6.013433	404.487121	8.311322
5.870681	403.947788	8.316339
6.133859	407.093910	8.321357
6.151573	409.057209	8.326374
5.955015	405.465208	8.331392
6.069684	401.458376	8.336410
6.019475	410.621164	8.341427
6.041160	406.568939	8.346445
5.926260	400.414282	8.351462
5.916257	410.293442	8.356480
5.916320	400.466388	8.361498
6.014771	410.700936	8.366515
5.976760	410.880488	8.371533
5.946346	417.057973	8.376550
6.134597	428.139988	8.381568
6.186927	428.299073	8.386586
6.096095	437.796440	8.391603
6.317581	422.008133	8.396621
5.918540	407.475234	8.401638
5.871388	410.095629	8.406656
5.864886	423.032191	8.411674
5.995626	436.543701	8.416691
5.917040	429.682761	8.421709
6.288417	435.409139	8.426726
6.301931	443.204976	8.431744
6.640966	435.271908	8.436762
6.336566	442.511647	8.441779
6.172116	411.304734	8.446797
5.893465	411.783918	8.451814
6.013466	416.378885	8.456832
6.365814	422.275496	8.461850
6.398521	429.143677	8.466867
6.091391	422.365886	8.471885
6.458914	419.745842	8.476902
6.088204	418.544800	8.481920
6.100274	403.540395	8.486938
6.174557	418.231528	8.491955
6.172233	420.671333	8.496973
6.272381	414.025390	8.501990
6.176782	421.926675	8.507008
6.357691	413.229448	8.512026
5.907415	420.895973	8.517043
5.850663	428.803798	8.522061
6.215731	431.305961	8.527078
5.897931	446.083795	8.532096
6.008757	430.925040	8.537114
6.179005	440.555070	8.542131
6.185556	434.662236	8.547149
6.433483	435.775277	8.552166
6.023973	435.542825	8.557184
6.201299	423.523122	8.562202
6.387347	439.654729	8.567219
6.550903	432.273015	8.572237
6.020486	438.393151	8.577255
6.276263	442.001183	8.582272
6.518895	436.579439	8.587290
6.239422	442.126931	8.592307
6.448346	435.410288	8.597325
6.334856	438.208338	8.602343
5.807961	442.210397	8.607360
6.269935	437.341260	8.612378
6.133535	436.299163	8.617395
5.748883	444.359356	8.622413
6.121879	447.702871	8.627431
5.965001	449.942836	8.632448
6.247761	465.939394	8.637466
6.285207	466.542622	8.642483
6.181182	464.110062	8.647501
6.581212	458.124011	8.652519
6.130237	458.409292	8.657536
6.520391	464.041220	8.662554
6.183629	464.725169	8.667571
6.215271	460.239030	8.672589
6.413221	456.203357	8.677607
6.210703	455.540845	8.682624
6.158004	457.054437	8.687642
6.200049	462.157087	8.692659
6.358730	462.170122	8.697677
6.382422	458.385813	8.702695
6.558443	461.820153	8.707712
6.675482	459.283530	8.712730
6.582276	454.261537	8.717747
6.569600	461.780621	8.722765
6.727652	456.630897	8.727783
6.265846	469.373745	8.732800
6.312851	467.766426	8.737818
6.396714	459.658735	8.742835
6.353370	459.801253	8.747853
6.556192	455.868958	8.752871
6.155246	463.338425	8.757888
6.298011	456.439638	8.762906
6.522439	481.218420	8.767923
6.581487	487.848969	8.772941
6.813507	480.320810	8.777959
6.589903	478.374040	8.782976
6.645433	461.216845	8.787994
6.747592	468.102561	8.793011
6.147954	467.536983	8.798029
6.302288	457.193425	8.803047
6.597083	475.236207	8.808064
6.536150	485.726143	8.813082
6.518777	482.730898	8.818099
6.597889	489.689661	8.823117
6.688580	485.263691	8.828135
6.742279	491.674174	8.833152
6.605055	473.228049	8.838170
6.568675	470.788046	8.843187
6.358788	470.306567	8.848205
7.005109	477.122806	8.853223
6.638408	476.249333	8.858240
6.588455	478.049673	8.863258
6.765141	466.456073	8.868275
6.533144	463.529172	8.873293
6.848614	459.702301	8.878311
6.519238	463.379929	8.883328
6.609934	459.585121	8.888346
6.713905	460.708096	8.893363
6.142017	467.573192	8.898381
6.781692	476.549027	8.903399
6.865601	490.396117	8.908416
7.021593	486.155574	8.913434
7.002456	469.350894	8.918451
6.782425	466.251706	8.923469
7.070101	465.569192	8.928487
7.080717	465.460260	8.933504
6.786583	465.010916	8.938522
6.960122	464.633462	8.943539
6.752953	460.642329	8.948557
7.134916	463.605749	8.953575
6.890333	461.021645	8.958592
6.905315	463.739609	8.963610
6.999709	461.326454	8.968627
6.826045	466.740611	8.973645
6.987285	467.630553	8.978663
6.796254	462.829010	8.983680
6.505072	452.836123	8.988698
6.813117	457.221757	8.993715
6.578543	463.516453	8.998733
6.785286	464.374019	9.003751
6.581079	471.153106	9.008768
6.735850	467.427151	9.013786
6.608205	457.651633	9.018803
6.501048	468.117244	9.023821
6.861514	452.856240	9.028839
6.543983	468.590252	9.033856
6.817689	466.950570	9.038874
6.789821	465.680028	9.043891
6.579378	461.171859	9.048909
6.763548	457.728477	9.053927
6.446847	464.739780	9.058944
6.449703	465.168547	9.063962
6.827284	481.819288	9.068979
7.025452	489.336906	9.073997
7.064984	478.916649	9.079015
6.927849	483.624504	9.084032
6.870111	481.730640	9.089050
7.324939	474.249624	9.094067
6.899475	479.592786	9.099085
6.951175	454.897028	9.104103
6.794996	466.440128	9.109120
6.799222	476.329718	9.114138
6.808414	475.217471	9.119155
7.218147	487.501887	9.124173
7.038081	475.323553	9.129191
6.828368	465.289492	9.134208
6.623172	466.126395	9.139226
7.057683	477.444409	9.144243
6.960209	486.526279	9.149261
6.710127	478.884310	9.154279
7.042973	477.765533	9.159296
6.968813	487.736838	9.164314
6.799691	487.280529	9.169331
6.981309	483.373641	9.174349
7.056380	483.431334	9.179367
6.858463	488.760936	9.184384
6.920055	498.010393	9.189402
7.618581	487.540527	9.194419
7.387874	487.169606	9.199437
7.173435	485.729481	9.204455
6.743389	477.547669	9.209472
7.023407	484.045765	9.214490
7.493998	484.426493	9.219507
7.278235	478.142446	9.224525
6.928650	474.501825	9.229543
6.824915	475.982390	9.234560
7.076804	482.443868	9.239578
7.331295	491.622073	9.244595
7.059235	483.412348	9.249613
7.317247	481.267041	9.254631
6.914959	483.283532	9.259648
7.085606	480.984658	9.264666
7.242699	484.605004	9.269683
7.212524	490.517391	9.274701
7.440373	479.985577	9.279719
7.096822	468.344100	9.284736
6.880477	470.501867	9.289754
7.123708	474.373801	9.294771
7.171816	480.835649	9.299789
7.187031	485.229302	9.304807
7.380974	479.793083	9.309824
6.980919	479.054224	9.314842
7.227692	470.062629	9.319859
6.717822	490.954944	9.324877
7.080160	480.083324	9.329895
7.150982	490.565242	9.334912
6.759745	495.953539	9.339930
7.111056	482.521145	9.344947
7.100530	494.729403	9.349965
6.852361	484.972754	9.354983
7.181104	484.997014	9.360000
6.574223	497.415475	9.365018
6.999885	498.390220	9.370035
7.247732	518.930319	9.375053
7.752935	516.228729	9.380071
7.688721	496.250050	9.385088
7.372636	494.106330	9.390106
7.292670	486.365121	9.395123
7.482527	491.668680	9.400141
7.382468	488.153061	9.405159
7.373151	485.099749	9.410176
7.211875	496.776210	9.415194
7.065326	490.771646	9.420211
7.159974	493.843204	9.425229
7.047687	487.170559	9.430247
7.200023	508.009631	9.435264
7.205961	513.190536	9.440282
7.381319	505.109514	9.445299
7.506167	518.420038	9.450317
7.054026	515.682255	9.455335
7.686407	512.067650	9.460352
7.233399	518.339785	9.465370
7.364654	515.412764	9.470387
7.698551	516.689065	9.475405
7.755751	515.455684	9.480423
7.432863	504.656697	9.485440
7.506120	497.424804	9.490458
7.420144	492.499496	9.495475
7.318746	500.865625	9.500493
7.632525	500.636610	9.505511
7.670220	501.170372	9.510528
7.048761	496.076501	9.515546
7.176314	502.693166	9.520563
7.545217	508.662951	9.525581
7.493853	509.646166	9.530599
7.636067	512.628224	9.535616
7.581102	519.314518	9.540634
7.541289	509.184385	9.545651
7.603774	505.517063	9.550669
7.139282	504.362267	9.555687
7.788215	511.310652	9.560704
7.257896	513.804796	9.565722
7.521802	514.214753	9.570739
7.524116	514.656229	9.575757
7.394840	515.418124	9.580775
7.602831	520.415895	9.585792
7.577093	523.020328	9.590810
7.430242	512.910120	9.595827
7.347232	508.473490	9.600845
7.537083	512.719868	9.605863
7.405894	516.237067	9.610880
7.513313	513.247510	9.615898
7.682867	513.990985	9.620915
7.618602	505.458359	9.625933
7.490995	507.592760	9.630951
7.638890	512.483181	9.635968
7.461368	520.902271	9.640986
7.690559	513.469215	9.646003
7.389429	512.238330	9.651021
7.354903	515.080824	9.656039
7.529003	516.151789	9.661056
7.139556	514.745394	9.666074
7.570878	528.377134	9.671091
7.543258	531.963315	9.676109
7.601380	534.665064	9.681127
7.629574	543.926089	9.686144
7.311083	540.599318	9.691162
7.458985	538.625891	9.696179
7.798346	535.824050	9.701197
7.816375	537.159311	9.706215
7.990842	543.061742	9.711232
7.656018	548.428592	9.716250
8.011427	538.788782	9.721267
7.925222	548.449585	9.726285
7.946042	548.910253	9.731303
8.111598	535.604754	9.736320
7.882520	539.680092	9.741338
7.841198	521.865829	9.746355
7.797358	515.078307	9.751373
7.688350	515.975881	9.756391
7.818070	512.907091	9.761408
7.463241	520.180008	9.766426
7.407568	529.996963	9.771443
7.808861	542.680369	9.776461
7.444155	538.884314	9.781479
7.904865	536.767203	9.786496
7.730517	542.478135	9.791514
7.881853	541.984238	9.796531
7.990827	550.440505	9.801549
7.632984	546.832721	9.806567
7.852346	535.724693	9.811584
7.523970	542.321291	9.816602
7.902510	544.215446	9.821619
8.113607	547.710580	9.826637
8.070766	544.921285	9.831655
8.421835	541.394932	9.836672
7.939555	551.411283	9.841690
8.199241	543.566338	9.846707
8.112743	536.687663	9.851725
8.134105	542.058663	9.856743
7.788648	540.219340	9.861760
7.591015	541.342239	9.866778
8.139250	539.700562	9.871795
8.254047	539.720473	9.876813
8.163740	545.383525	9.881831
8.190704	534.842129	9.886848
8.370305	539.039626	9.891866
8.222771	519.806119	9.896883
8.185417	516.315383	9.901901
8.106991	517.268125	9.906919
7.933023	508.089971	9.911936
8.081568	512.109291	9.916954
7.585571	508.463201	9.921971
7.974409	517.588812	9.926989
7.885826	513.594865	9.932007
8.096058	510.687029	9.937024
7.875330	523.748747	9.942042
8.058457	533.095944	9.947059
8.144390	538.829209	9.952077
8.159968	539.928169	9.957095
8.131772	529.682596	9.962112
8.143374	538.090997	9.967130
7.976786	531.063927	9.972147
8.173456	532.803541	9.977165
7.938902	543.121899	9.982183
8.112233	539.096377	9.987200
8.157553	540.219079	9.992218
8.199587	543.204215	9.997235
8.117509	536.690919	10.002253
7.865881	544.553589	10.007271
8.097243	531.493402	10.012288
8.089297	543.464605	10.017306
8.051927	539.364798	10.022323
8.232474	527.972524	10.027341
7.741381	539.987867	10.032359
8.249339	541.628216	10.037376
7.974591	546.925692	10.042394
7.871307	547.718229	10.047411
8.113492	529.708059	10.052429
8.130103	538.159857	10.057447
8.171287	538.563686	10.062464
7.934549	544.688336	10.067482
8.301521	539.537412	10.072499
8.150534	546.260852	10.077517
8.199317	550.090685	10.082535
8.566692	556.764469	10.087552
8.443832	550.472152	10.092570
8.449583	541.685542	10.097587
7.939595	540.332745	10.102605
8.098455	547.695601	10.107623
8.507684	552.431478	10.112640
8.628769	558.285474	10.117658
8.020377	548.029811	10.122675
8.653960	549.937655	10.127693
8.499128	547.440461	10.132711
8.440592	540.932942	10.137728
8.179175	542.258338	10.142746
8.308768	553.144494	10.147763
8.373327	533.770445	10.152781
8.500817	536.874734	10.157799
8.418113	538.033274	10.162816
8.447625	535.238956	10.167834
8.181963	536.492433	10.172851
8.473132	542.528058	10.177869
8.406359	542.863595	10.182887
8.517111	539.201327	10.187904
8.408884	543.671140	10.192922
8.561963	545.045201	10.197939
8.621388	536.366949	10.202957
8.160588	536.814716	10.207975
8.395072	548.978310	10.212992
8.658659	559.660440	10.218010
8.375015	558.133322	10.223027
8.556368	562.466250	10.228045
8.386803	567.172897	10.233063
8.991215	556.357975	10.238080
8.696394	554.491783	10.243098
8.336515	553.027103	10.248115
8.610007	542.828927	10.253133
8.397414	547.968343	10.258151
8.511432	541.200259	10.263168
8.748877	542.090888	10.268186
8.423710	537.771088	10.273203
8.759149	539.391130	10.278221
8.291130	545.286931	10.283239
8.588582	550.314875	10.288256
8.762471	555.021354	10.293274
8.435879	565.540338	10.298291
8.539277	555.823240	10.303309
8.110804	563.325463	10.308327
8.211789	568.280054	10.313344
8.522089	563.024394	10.318362
8.448749	570.073347	10.323379
8.834517	569.716287	10.328397
8.836105	573.963775	10.333415
8.744738	569.758813	10.338432
8.849872	570.483982	10.343450
8.462858	566.776622	10.348467
8.618487	557.912873	10.353485
8.460632	559.105280	10.358503
8.348118	558.236157	10.363520
8.874518	559.599064	10.368538
8.327551	564.131313	10.373555
8.438846	565.805412	10.378573
8.430433	579.780645	10.383591
8.452739	587.972798	10.388608
8.957849	591.245149	10.393626
8.934275	594.442545	10.398643
8.785642	585.541248	10.403661
8.826895	587.305218	10.408679
8.990765	594.711489	10.413696
9.250207	587.999498	10.418714
8.737139	578.031839	10.423731
8.923833	568.257502	10.428749
8.629571	572.125310	10.433767
8.605433	566.177281	10.438784
8.855044	578.483692	10.443802
8.875265	587.850131	10.448819
9.097256	584.971998	10.453837
8.970805	580.510599	10.458855
9.348254	569.822749	10.463872
8.856291	561.953555	10.468890
8.504214	568.001611	10.473907
8.795877	554.427031	10.478925
8.490589	564.933209	10.483943
8.914614	574.113295	10.488960
9.400714	582.229623	10.493978
8.909897	581.700639	10.498995
8.917542	568.697567	10.504013
8.839246	583.087695	10.509031
8.965137	585.753587	10.514048
9.363574	582.320789	10.519066
8.984452	579.953407	10.524083
8.958590	559.899220	10.529101
8.804574	575.891728	10.534119
9.094686	579.333462	10.539136
8.939086	573.661648	10.544154
9.061184	588.834579	10.549171
9.194410	590.101301	10.554189
9.015899	586.796770	10.559207
8.855958	568.616037	10.564224
9.091415	579.690750	10.569242
9.105598	590.216315	10.574259
9.103808	590.090392	10.579277
9.221401	594.152450	10.584295
9.098566	582.242786	10.589312
9.164379	573.632943	10.594330
8.882760	573.191102	10.599347
9.101178	581.955284	10.604365
9.065896	587.805388	10.609383
9.166597	598.894914	10.614400
8.902776	594.751681	10.619418
8.880904	597.330273	10.624435
9.213851	581.032056	10.629453
9.329678	588.840328	10.634471
9.246805	593.975211	10.639488
9.303855	592.830211	10.644506
9.358670	603.005435	10.649523
9.466763	597.813005	10.654541
9.440943	586.453028	10.659559
9.091021	577.270848	10.664576
8.958393	571.892081	10.669594
9.245088	584.094856	10.674611
9.070723	587.053946	10.679629
9.253079	587.028558	10.684647
8.971672	588.518036	10.689664
8.871758	583.639068	10.694682
8.727685	594.299884	10.699699
9.225653	591.735116	10.704717
8.967795	597.500176	10.709735
9.218689	589.902741	10.714752
9.297723	585.459638	10.719770
8.983941	598.611730	10.724787
9.206610	591.596230	10.729805
9.596158	601.021573	10.734823
9.297866	597.748431	10.739840
9.287649	594.354413	10.744858
9.145048	590.296329	10.749875
9.390821	606.428197	10.754893
9.266178	603.058418	10.759911
9.008028	608.122938	10.764928
9.652704	611.824705	10.769946
9.519377	616.617206	10.774963
9.379183	624.228921	10.779981
9.499543	612.268510	10.784999
9.520480	616.563469	10.790016
9.679655	604.035248	10.795034
9.371979	616.533144	10.800051
9.565227	604.999975	10.805069
9.530103	600.259174	10.810087
9.224327	608.101954	10.815104
9.559593	601.081431	10.820122
9.526973	618.090061	10.825139
9.935426	614.750362	10.830157
9.538705	580.578373	10.835175
9.111856	590.178962	10.840192
9.558082	599.055782	10.845210
9.420155	612.622143	10.850227
9.569838	616.294170	10.855245
9.677411	614.282873	10.860263
9.801092	619.227610	10.865280
9.632309	606.741304	10.870298
9.289638	607.886932	10.875315
9.207127	616.152326	10.880333
9.653713	618.102100	10.885351
9.524325	612.877447	10.890368
9.582271	617.217100	10.895386
9.771745	615.158257	10.900403
9.364799	624.339179	10.905421
9.552824	616.830479	10.910439
9.602573	627.931162	10.915456
9.985451	619.874378	10.920474
10.020274	622.084329	10.925491
9.649307	624.594545	10.930509
9.905526	623.901176	10.935527
9.971238	625.339425	10.940544
9.874275	616.057631	10.945562
9.534018	607.880624	10.950579
9.621896	618.287362	10.955597
9.480373	614.642515	10.960615
9.360294	621.837666	10.965632
9.560827	613.070996	10.970650
9.513262	625.935243	10.975667
9.269532	628.703236	10.980685
9.902918	624.375238	10.985703
9.381667	624.135044	10.990720
9.402074	617.716115	10.995738
9.290238	625.336011	11.000755
9.564391	642.290286	11.005773
9.708326	642.902081	11.010791
10.002546	652.900967	11.015808
9.988090	637.007426	11.020826
10.216291	642.475437	11.025843
9.871429	648.430871	11.030861
10.128191	640.229735	11.035879
10.063235	648.918428	11.040896
10.095986	632.367398	11.045914
9.859707	630.719244	11.050931
9.826862	636.834070	11.055949
9.707180	631.248128	11.060967
10.053392	640.225845	11.065984
9.933082	645.312960	11.071002
9.939978	645.154117	11.076019
9.978027	638.344251	11.081037
10.056476	633.358428	11.086055
9.601429	639.204890	11.091072
9.826951	640.397194	11.096090
9.787753	648.728400	11.101107
9.984464	648.464077	11.106125
10.097344	637.337956	11.111143
10.061011	649.357859	11.116160
10.479948	651.166801	11.121178
10.550588	647.031112	11.126195
10.133806	633.498045	11.131213
10.166589	629.513459	11.136231
10.197277	617.731196	11.141248
10.171717	621.048829	11.146266
9.777691	622.584357	11.151283
9.622146	618.941705	11.156301
10.144968	627.465710	11.161319
10.029089	641.031795	11.166336
10.243201	644.924107	11.171354
10.348113	642.026440	11.176371
10.303349	656.139973	11.181389
10.391850	638.115904	11.186407
10.120157	628.520652	11.191424
10.061854	629.467091	11.196442
10.106754	628.649041	11.201459
9.965027	638.896105	11.206477
10.234398	650.003418	11.211495
9.814404	652.956822	11.216512
10.229819	652.604583	11.221530
10.478588	648.617710	11.226547
10.115500	648.639913	11.231565
10.525416	642.163102	11.236583
10.397210	648.914568	11.241600
10.270231	645.936468	11.246618
10.478376	649.346877	11.251635
10.134725	651.379445	11.256653
10.697681	639.362293	11.261671
10.475323	640.908794	11.266688
10.026105	621.608837	11.271706
10.541151	628.991659	11.276723
10.128483	630.990857	11.281741
10.229593	632.701272	11.286759
10.055091	641.069453	11.291776
10.723456	637.215655	11.296794
10.389117	632.184055	11.301811
10.302949	644.549435	11.306829
10.380642	636.155451	11.311847
10.513790	649.994949	11.316864
10.407748	649.879048	11.321882
10.558363	650.189994	11.326899
10.368704	650.557411	11.331917
10.533907	642.241232	11.336935
10.563741	649.933615	11.341952
10.204370	645.518162	11.346970
10.483062	646.973536	11.351987
10.227504	651.561134	11.357005
10.405428	648.841375	11.362023
10.216047	646.084492	11.367040
10.099412	652.597461	11.372058
10.428840	642.059104	11.377075
10.119643	652.458647	11.382093
10.415487	641.657308	11.387111
10.531146	652.586734	11.392128
10.623983	651.578134	11.397146
10.432972	645.230190	11.402163
10.256722	648.533568	11.407181
10.732955	647.704740	11.412199
10.244108	659.498903	11.417216
10.415807	669.015220	11.422234
10.846892	673.075516	11.427251
10.550762	686.237529	11.432269
10.715328	676.627547	11.437287
10.797627	683.424940	11.442304
10.384553	680.882982	11.447322
10.575004	674.087093	11.452339
10.517288	684.134827	11.457357
10.771695	669.944301	11.462375
10.721341	667.623225	11.467392
10.585142	673.662738	11.472410
11.075695	673.737385	11.477427
10.808908	680.015113	11.482445
10.930122	676.411138	11.487463
10.665704	679.236029	11.492480
10.637784	672.288162	11.497498
10.814924	667.927497	11.502515
10.895169	683.327973	11.507533
11.060283	676.261497	11.512551
10.536934	680.423999	11.517568
10.625198	677.216509	11.522586
10.708450	667.764440	11.527603
10.743525	678.889545	11.532621
11.029586	668.818716	11.537639
10.772791	672.024265	11.542656
10.415243	674.879526	11.547674
10.778374	676.564670	11.552691
11.071891	680.479263	11.557709
10.957025	673.822731	11.562727
10.825968	680.069725	11.567744
10.744467	669.829267	11.572762
10.878114	666.617824	11.577779
10.577600	677.202215	11.582797
10.812645	674.763837	11.587815
10.916319	672.418628	11.592832
10.639539	674.279774	11.597850
10.355382	685.117228	11.602867
10.803694	697.320005	11.607885
10.510895	692.048349	11.612903
10.702061	703.944280	11.617920
10.628058	702.898702	11.622938
10.978708	701.076529	11.627955
10.802818	710.293876	11.632973
11.030589	696.716576	11.637991
11.180871	713.750288	11.643008
11.033432	717.011295	11.648026
11.073535	713.798721	11.653043
11.312561	714.102127	11.658061
11.262992	703.575778	11.663079
11.101932	706.677970	11.668096
11.006008	696.600704	11.673114
11.296076	690.505573	11.678131
10.974557	702.213586	11.683149
11.214754	701.459608	11.688167
11.073421	698.717279	11.693184
10.886034	709.094615	11.698202
11.380018	714.722977	11.703219
11.139153	730.164338	11.708237
11.392756	727.644150	11.713255
11.414929	730.537755	11.718272
11.286955	720.127823	11.723290
11.588681	705.914075	11.728307
11.241284	709.013905	11.733325
11.328817	702.988373	11.738343
11.339221	691.531134	11.743360
10.943946	696.200595	11.748378
11.475109	698.111880	11.753395
11.476922	701.696639	11.758413
11.322804	702.475057	11.763431
11.249208	702.540265	11.768448
11.174902	705.739318	11.773466
11.337343	695.672065	11.778483
11.294711	698.026705	11.783501
11.373196	698.964338	11.788519
11.634990	703.609747	11.793536
11.211485	707.157005	11.798554
11.295232	696.928510	11.803571
11.505362	704.078269	11.808589
11.375515	697.629203	11.813607
11.548383	699.886962	11.818624
11.559337	709.807186	11.823642
11.200815	704.545823	11.828659
11.399135	711.340827	11.833677
11.647926	717.159088	11.838695
11.794790	709.991315	11.843712
11.604566	707.417593	11.848730
11.648034	703.469186	11.853747
11.480862	706.168390	11.858765
11.399207	699.661280	11.863783
11.406433	694.560366	11.868800
11.627613	698.874463	11.873818
11.572113	696.355373	11.878835
11.647707	702.648892	11.883853
11.239494	698.301039	11.888871
11.204026	703.882964	11.893888
11.492033	717.963341	11.898906
11.754795	723.454364	11.903923
11.666160	734.333798	11.908941
11.383336	733.939479	11.913959
11.597263	725.360005	11.918976
11.369820	728.513627	11.923994
11.906022	726.555081	11.929011
11.645980	731.114999	11.934029
11.636458	728.471935	11.939047
11.672504	721.173198	11.944064
11.411067	733.231582	11.949082
11.590670	724.802654	11.954099
11.782879	724.984007	11.959117
11.775717	730.678272	11.964135
11.871859	720.492003	11.969152
11.820901	728.367494	11.974170
11.977825	722.056526	11.979187
11.468773	733.367906	11.984205
11.579858	729.686612	11.989223
11.820143	726.830837	11.994240
11.736544	733.202959	11.999258
11.853053	725.736977	12.004275
11.810251	731.856551	12.009293
11.867473	733.150971	12.014311
11.897381	729.353007	12.019328
11.890943	734.453864	12.024346
12.295669	727.876848	12.029363
12.010839	732.134535	12.034381
11.751676	735.577154	12.039399
12.115334	726.153704	12.044416
11.924171	726.742265	12.049434
11.577401	729.655806	12.054451
12.025781	727.385969	12.059469
11.669753	728.480048	12.064487
12.026006	737.718175	12.069504
11.927939	746.481532	12.074522
12.348513	747.166752	12.079539
12.312386	732.658776	12.084557
12.102286	732.376140	12.089575
12.153430	729.774064	12.094592
11.990851	720.287900	12.099610
11.983270	715.687921	12.104627
12.369619	718.464504	12.109645
11.946232	730.333664	12.114663
11.956281	723.654386	12.119680
11.554832	715.411177	12.124698
11.901772	732.786483	12.129715
12.020841	743.317795	12.134733
12.246656	749.925468	12.139751
12.484151	746.016079	12.144768
12.399030	751.148204	12.149786
12.882098	748.648865	12.154803
12.198050	735.769827	12.159821
12.001506	737.274423	12.164839
12.128561	722.415838	12.169856
12.197474	726.659124	12.174874
12.453615	719.063969	12.179891
12.124249	723.344411	12.184909
11.852667	727.009882	12.189927
12.349071	731.441812	12.194944
12.387734	746.523807	12.199962
12.386893	743.857289	12.204979
12.572640	739.410051	12.209997
12.628767	736.901868	12.215015
12.577380	725.514250	12.220032
12.502678	728.217904	12.225050
12.356371	723.434529	12.230067
12.231403	723.065971	12.235085
11.932466	722.143998	12.240103
12.057358	716.535489	12.245120
12.222124	736.284120	12.250138
12.253771	738.210558	12.255155
12.354653	750.868598	12.260173
12.538372	755.614616	12.265191
12.251820	751.329739	12.270208
12.569870	753.277577	12.275226
12.642191	760.123899	12.280243
12.810562	750.399672	12.285261
12.438587	761.336139	12.290279
12.446459	748.093058	12.295296
12.563384	759.704011	12.300314
12.421594	744.174312	12.305331
12.709803	748.222297	12.310349
12.155359	747.349823	12.315367
12.496057	742.960358	12.320384
12.348919	748.402003	12.325402
12.470109	746.344376	12.330419
12.732623	752.763261	12.335437
12.583864	752.240638	12.340455
12.479730	741.028533	12.345472
12.097518	745.897934	12.350490
12.067662	745.391395	12.355507
12.529178	751.100596	12.360525
12.242135	776.909833	12.365543
12.665198	774.116933	12.370560
12.776385	773.013932	12.375578
12.786833	759.114026	12.380595
12.758658	767.446716	12.385613
12.642864	770.563917	12.390631
13.159428	771.928383	12.395648
13.011873	771.566518	12.400666
12.882876	776.257396	12.405683
12.899683	757.988816	12.410701
13.084034	781.808611	12.415719
12.703873	761.165919	12.420736
13.076942	751.759916	12.425754
12.663674	750.025871	12.430771
12.622615	745.380636	12.435789
12.933573	769.221603	12.440807
12.834483	763.761783	12.445824
12.792246	769.606724	12.450842
12.752610	771.964060	12.455859
13.448472	757.445518	12.460877
12.739958	757.745907	12.465895
12.829430	748.056134	12.470912
12.691788	755.910504	12.475930
13.148739	772.252433	12.480947
13.253492	769.462069	12.485965
12.944248	775.023795	12.490983
12.982526	767.756248	12.496000
12.738986	769.706870	12.501018
12.472215	772.951870	12.506035
13.089782	755.545384	12.511053
12.986363	772.227579	12.516071
12.822141	767.096702	12.521088
13.162781	764.752222	12.526106
12.663253	769.854607	12.531123
13.004984	762.971865	12.536141
12.946630	765.947521	12.541159
13.386712	762.511321	12.546176
13.299385	760.925024	12.551194
12.801412	759.276834	12.556211
13.121888	761.940667	12.561229
13.119479	767.119797	12.566247
13.013170	758.972338	12.571264
13.182725	765.718221	12.576282
13.014704	764.545358	12.581299
13.134151	766.404393	12.586317
13.180222	783.580733	12.591335
13.456713	786.021085	12.596352
13.491541	795.928148	12.601370
13.294447	777.765647	12.606387
13.220860	767.751113	12.611405
13.394596	768.061595	12.616423
13.203820	769.372783	12.621440
13.230973	776.863669	12.626458
13.104345	784.309223	12.631475
13.473827	786.144863	12.636493
13.131870	795.697547	12.641511
13.329427	789.679993	12.646528
13.489085	797.598255	12.651546
13.486541	789.131564	12.656563
13.542525	781.772873	12.661581
13.040612	784.792782	12.666599
13.430976	785.321789	12.671616
13.726269	791.688216	12.676634
13.588307	791.618341	12.681651
13.196579	789.827268	12.686669
13.247697	800.334546	12.691687
13.400621	785.329843	12.696704
13.431944	790.260695	12.701722
13.333185	789.916431	12.706739
13.524087	785.651413	12.711757
13.447212	795.269861	12.716775
13.325447	799.410496	12.721792
13.541035	791.581820	12.726810
13.137340	797.884195	12.731827
13.650084	799.826780	12.736845
13.672842	806.261160	12.741863
13.992588	813.384320	12.746880
13.868167	786.446649	12.751898
13.253780	800.349740	12.756915
13.483767	794.762610	12.761933
13.853554	805.409312	12.766951
13.963989	805.811764	12.771968
13.728710	797.659248	12.776986
13.702544	796.621949	12.782003
13.796474	793.429329	12.787021
13.637494	800.289817	12.792039
13.508915	791.729261	12.797056
13.845060	791.528297	12.802074
13.726084	811.069001	12.807091
14.327154	802.902208	12.812109
13.939694	806.058825	12.817127
13.524948	797.000299	12.822144
13.830159	787.813195	12.827162
13.524711	791.988918	12.832179
14.111894	797.896198	12.837197
13.927382	806.584765	12.842215
14.079216	802.751903	12.847232
13.921859	787.527566	12.852250
13.802912	792.453561	12.857267
14.209903	791.414667	12.862285
14.199851	790.043480	12.867303
13.865617	792.708912	12.872320
14.055086	785.745875	12.877338
14.009901	784.856725	12.882355
14.121751	782.431324	12.887373
14.105423	783.980271	12.892391
13.679562	784.094361	12.897408
13.881059	784.968544	12.902426
13.988452	796.593638	12.907443
14.254145	803.078316	12.912461
14.256684	796.864096	12.917479
14.071707	794.494668	12.922496
14.200618	780.850741	12.927514
13.852437	781.012622	12.932531
13.869271	794.371834	12.937549
13.906709	802.271378	12.942567
14.074850	808.421044	12.947584
14.095501	818.213575	12.952602
14.117958	807.694814	12.957619
14.228304	811.915850	12.962637
14.500997	817.247554	12.967655
14.304818	818.657424	12.972672
14.222172	819.910648	12.977690
14.244752	819.850333	12.982707
14.776934	810.536136	12.987725
14.473832	816.866939	12.992743
14.002196	812.415384	12.997760
14.412344	811.912487	13.002778
14.242486	813.769518	13.007795
14.469813	811.149293	13.012813
14.271311	812.711007	13.017831
14.133976	812.028800	13.022848
14.357690	808.929453	13.027866
14.371029	809.154612	13.032883
14.268165	811.884782	13.037901
14.413535	808.349580	13.042919
14.028170	812.023428	13.047936
14.438938	803.002816	13.052954
14.207672	815.507814	13.057971
14.109964	810.707334	13.062989
14.160526	818.046244	13.068007
14.471281	825.385416	13.073024
14.843570	832.957949	13.078042
14.497455	835.196054	13.083059
14.622756	826.630417	13.088077
14.580988	825.115872	13.093095
14.105807	814.053377	13.098112
14.817375	819.079630	13.103130
14.352740	833.375854	13.108147
14.580161	832.279885	13.113165
14.514864	840.148204	13.118183
14.543686	837.022583	13.123200
14.887551	838.723386	13.128218
14.606543	843.037305	13.133235
14.453220	837.298778	13.138253
14.907302	843.331070	13.143271
14.805156	848.904553	13.148288
14.955085	837.965010	13.153306
14.925357	847.263670	13.158323
14.920637	840.580350	13.163341
15.052248	836.308830	13.168359
14.793633	833.723714	13.173376
14.932038	813.936998	13.178394
14.707881	815.647900	13.183411
14.846949	822.575308	13.188429
14.686250	818.744073	13.193447
14.668462	834.131636	13.198464
15.261046	832.025387	13.203482
15.019407	841.726481	13.208499
15.053434	829.476490	13.213517
14.629511	819.715637	13.218535
14.648105	830.196470	13.223552
14.633906	824.918993	13.228570
14.736382	835.462427	13.233587
15.013551	832.054895	13.238605
14.862124	837.721304	13.243623
14.971544	842.725143	13.248640
14.763089	826.088648	13.253658
15.092450	840.528720	13.258675
15.085105	834.388620	13.263693
14.995063	827.740764	13.268711
14.910374	834.577002	13.273728
14.725506	830.061576	13.278746
14.898457	833.872015	13.283763
15.145871	830.254549	13.288781
15.171521	828.549557	13.293799
14.922843	828.781055	13.298816
15.206005	833.940708	13.303834
15.452113	837.001218	13.308851
14.973854	838.512091	13.313869
15.476510	841.374613	13.318887
15.264421	843.137277	13.323904
15.174467	830.319723	13.328922
15.126673	835.076789	13.333939
15.223442	848.470855	13.338957
15.566440	849.553248	13.343975
15.025276	848.864883	13.348992
15.122371	854.328254	13.354010
15.444244	853.135433	13.359027
15.592747	858.748544	13.364045
15.248334	848.587047	13.369063
15.319123	851.864380	13.374080
15.542842	857.531977	13.379098
15.668166	854.274467	13.384115
15.308104	851.222397	13.389133
15.524489	845.015680	13.394151
15.600212	859.186235	13.399168
15.612410	847.782265	13.404186
15.401837	839.019935	13.409203
15.158930	848.686517	13.414221
15.523840	852.397456	13.419239
15.417948	851.120177	13.424256
15.298414	845.016585	13.429274
15.623681	856.301464	13.434291
15.652426	859.967243	13.439309
15.745969	844.921300	13.444327
15.541443	855.531783	13.449344
15.702964	849.879622	13.454362
15.493468	852.020582	13.459379
15.471941	849.625538	13.464397
15.627465	848.048520	13.469415
15.723126	857.879814	13.474432
15.866854	856.131072	13.479450
15.970464	851.778728	13.484467
15.909075	855.253498	13.489485
15.886194	853.426718	13.494503
15.592209	853.936718	13.499520
15.675377	847.867639	13.504538
15.413151	853.573504	13.509555
15.910748	849.430834	13.514573
15.901557	849.549068	13.519591
15.613826	849.966569	13.524608
16.111937	849.077499	13.529626
15.594137	846.611886	13.534643
15.571000	842.298338	13.539661
16.056908	846.978098	13.544679
15.445751	860.401040	13.549696
15.782895	855.210518	13.554714
15.975252	853.391041	13.559731
15.553817	851.708759	13.564749
15.918702	855.044156	13.569767
15.794434	862.688191	13.574784
15.701325	857.252652	13.579802
15.739344	855.640396	13.584819
15.952683	872.222560	13.589837
16.302446	877.330765	13.594855
15.900559	887.498811	13.599872
15.910595	875.280950	13.604890
16.387648	877.762476	13.609907
16.197254	879.802615	13.614925
16.486737	869.327188	13.619943
16.016813	858.872921	13.624960
16.192912	852.962852	13.629978
16.113086	854.354494	13.634995
16.002388	856.479975	13.640013
16.510668	860.730194	13.645031
16.040387	868.542056	13.650048
16.284408	872.139394	13.655066
15.909967	876.436402	13.660083
16.388665	873.060404	13.665101
16.369738	869.746596	13.670119
16.123815	872.814775	13.675136
16.130657	881.325071	13.680154
16.443780	875.159992	13.685171
16.063653	873.916211	13.690189
16.321778	871.998063	13.695207
15.769464	876.477578	13.700224
16.130074	880.656262	13.705242
16.498498	876.057290	13.710259
16.728329	882.563396	13.715277
16.462158	875.179402	13.720295
16.255063	881.078612	13.725312
16.477339	881.072216	13.730330
16.201477	881.939145	13.735347
16.304176	884.331000	13.740365
16.290698	877.825767	13.745383
16.083413	882.607835	13.750400
16.214174	900.159188	13.755418
16.528640	904.793240	13.760435
16.541761	898.820327	13.765453
16.898305	900.642228	13.770471
16.759359	907.247149	13.775488
16.884397	907.773550	13.780506
16.554352	901.409428	13.785523
16.570784	908.081524	13.790541
16.867124	903.799958	13.795559
16.655249	902.775970	13.800576
16.669045	900.804581	13.805594
16.786009	888.153384	13.810611
16.628606	900.631089	13.815629
16.957577	900.658470	13.820647
16.701344	898.871403	13.825664
16.548673	908.094682	13.830682
16.958542	897.029167	13.835699
16.668833	904.181581	13.840717
17.166866	896.390658	13.845735
16.489265	899.056255	13.850752
17.070815	907.470206	13.855770
17.475100	893.448527	13.860787
16.975564	891.478672	13.865805
16.848355	887.238224	13.870823
16.639036	882.171185	13.875840
16.544391	883.659827	13.880858
17.077254	895.259348	13.885875
16.785386	898.808109	13.890893
16.817276	898.538049	13.895911
16.797460	898.500156	13.900928
16.754537	896.941604	13.905946
16.688354	900.158354	13.910963
16.862580	912.767147	13.915981
17.383380	905.253525	13.920999
17.214902	902.632184	13.926016
16.596583	905.970159	13.931034
17.023562	898.360784	13.936051
17.004612	905.795830	13.941069
17.091349	901.793262	13.946087
17.151191	901.919616	13.951104
16.946432	907.641741	13.956122
17.279304	909.502066	13.961139
17.018608	928.200396	13.966157
17.114482	929.899037	13.971175
17.062953	935.704462	13.976192
16.986837	931.386570	13.981210
17.259309	923.466871	13.986227
17.119694	934.190309	13.991245
17.070458	926.204248	13.996263
17.051812	923.613078	14.001280
17.142688	927.174461	14.006298
17.050541	926.661897	14.011315
17.319568	932.054172	14.016333
17.105442	939.598708	14.021351
17.543138	949.518476	14.026368
17.388751	951.253174	14.031386
17.242369	953.033956	14.036403
17.287754	959.382792	14.041421
17.589860	950.634757	14.046439
17.558120	951.113139	14.051456
17.528252	957.691520	14.056474
18.072048	949.571506	14.061491
17.713971	945.537634	14.066509
17.541938	948.098778	14.071527
17.655417	949.696830	14.076544
17.798489	953.546692	14.081562
18.102934	935.627347	14.086579
17.467537	935.010548	14.091597
17.817814	921.972471	14.096615
17.741429	918.405720	14.101632
17.712611	925.883346	14.106650
18.118526	914.808972	14.111667
17.756616	914.802587	14.116685
17.744361	916.982080	14.121703
18.049196	923.542722	14.126720
17.710135	920.007659	14.131738
17.816304	922.739809	14.136755
17.649178	923.835860	14.141773
17.788445	920.096461	14.146791
17.903543	914.817634	14.151808
17.374034	925.911430	14.156826
17.860975	913.549393	14.161843
17.461133	927.327446	14.166861
17.479686	938.960240	14.171879
17.354411	945.193797	14.176896
17.632375	951.550372	14.181914
17.863167	941.794170	14.186931
17.979742	947.690027	14.191949
17.912006	947.590213	14.196967
18.387414	946.950853	14.201984
17.826647	955.909887	14.207002
17.908180	945.192438	14.212019
17.907319	943.422160	14.217037
18.130701	947.202632	14.222055
17.794796	947.416239	14.227072
18.042091	953.032835	14.232090
18.533569	956.219026	14.237107
18.015263	962.028166	14.242125
17.898803	958.123695	14.247143
18.518791	961.810471	14.252160
18.299185	956.123316	14.257178
17.948088	948.402296	14.262195
18.212490	964.973390	14.267213
18.411195	968.016103	14.272231
18.575906	964.979624	14.277248
18.385654	966.303368	14.282266
18.553542	951.132076	14.287283
18.340592	946.475850	14.292301
18.362802	944.373748	14.297319
18.595914	939.398321	14.302336
18.153045	945.678483	14.307354
18.460566	931.242738	14.312371
18.401826	936.484393	14.317389
17.737624	946.166542	14.322407
18.349144	951.804968	14.327424
18.361454	954.731713	14.332442
18.795850	964.835047	14.337459
18.604005	961.422079	14.342477
18.508307	961.373984	14.347495
18.630012	957.438510	14.352512
18.416640	962.830636	14.357530
18.751813	962.020740	14.362547
18.798718	971.323237	14.367565
18.769728	964.801467	14.372583
18.910164	966.859210	14.377600
18.472269	962.336057	14.382618
18.878181	960.476797	14.387635
18.572947	958.429152	14.392653
18.498169	966.418936	14.397671
18.778006	963.039364	14.402688
18.556348	967.877356	14.407706
18.927372	959.800187	14.412723
19.026856	959.847745	14.417741
18.700613	963.641751	14.422759
18.690862	962.311530	14.427776
18.714381	963.371401	14.432794
18.812574	966.000664	14.437811
18.937677	969.824941	14.442829
18.823110	969.839764	14.447847
19.163266	967.842480	14.452864
18.564179	967.595539	14.457882
18.796574	958.059988	14.462899
19.210609	963.076095	14.467917
19.132224	962.867493	14.472935
19.188308	962.375886	14.477952
19.064142	971.525302	14.482970
19.040249	961.016870	14.487987
19.103372	961.003852	14.493005
19.010964	961.012047	14.498023
19.452310	958.929481	14.503040
18.959274	966.855406	14.508058
18.870823	956.593781	14.513075
19.066956	955.149250	14.518093
19.222111	947.251079	14.523111
19.262198	949.425531	14.528128
19.151306	953.435106	14.533146
19.077388	950.284536	14.538163
18.992263	953.494796	14.543181
18.897099	954.519613	14.548199
19.269212	957.538310	14.553216
18.952046	957.089405	14.558234
18.867843	962.950452	14.563251
19.397235	972.300432	14.568269
19.347996	974.807625	14.573287
19.995763	973.895102	14.578304
19.651536	970.196733	14.583322
19.465055	961.405321	14.588339
19.642392	948.103982	14.593357
18.921180	955.560715	14.598375
19.465123	957.429000	14.603392
19.586547	974.391742	14.608410
19.749688	966.792119	14.613427
19.561097	949.805250	14.618445
19.178033	952.926488	14.623463
19.368021	970.194070	14.628480
19.593234	972.027088	14.633498
19.500621	974.585259	14.638515
19.979715	972.146475	14.643533
20.036836	979.001575	14.648551
19.859823	972.039081	14.653568
19.682697	957.382598	14.658586
19.538295	957.982775	14.663603
19.884380	964.038342	14.668621
19.637706	963.032426	14.673639
19.806552	967.998587	14.678656
19.645815	982.215755	14.683674
19.957252	979.004803	14.688691
19.882687	969.441599	14.693709
19.542756	973.206192	14.698727
19.937295	970.764877	14.703744
19.253417	973.977433	14.708762
19.435602	969.817881	14.713779
19.568473	970.522941	14.718797
19.640696	970.719941	14.723815
20.032059	967.780496	14.728832
19.408975	977.418349	14.733850
19.953132	984.856720	14.738867
20.292388	991.727582	14.743885
20.151541	992.279865	14.748903
20.387944	978.158189	14.753920
20.211009	973.180726	14.758938
19.819896	972.702380	14.763955
20.317203	965.949823	14.768973
19.978430	965.898787	14.773991
20.273094	965.622268	14.779008
20.313576	968.506731	14.784026
19.898811	965.453745	14.789043
20.141574	979.497236	14.794061
20.161442	999.846386	14.799079
20.748133	987.083652	14.804096
20.622162	984.001194	14.809114
20.103113	964.954807	14.814131
20.010203	968.106328	14.819149
20.051053	976.248416	14.824167
20.536547	993.980972	14.829184
20.457102	993.535846	14.834202
20.148007	983.791625	14.839219
20.726239	980.453662	14.844237
20.326477	984.211853	14.849255
20.596956	994.416627	14.854272
20.433936	992.220461	14.859290
20.587883	985.240822	14.864307
20.322966	977.477883	14.869325
20.065088	982.611895	14.874343
20.464166	985.007821	14.879360
20.600741	994.147954	14.884378
20.682940	999.440131	14.889395
20.719558	992.071764	14.894413
20.294617	992.457115	14.899431
20.482311	999.329636	14.904448
20.668899	993.430501	14.909466
20.666682	996.511010	14.914483
20.857700	993.527211	14.919501
20.761745	998.058331	14.924519
20.738469	993.378687	14.929536
20.218067	998.661135	14.934554
20.576286	1006.138115	14.939571
20.991768	991.997838	14.944589
20.573651	1002.282103	14.949607
20.704088	999.080571	14.954624
20.538205	996.402004	14.959642
20.519023	999.592472	14.964659
20.788254	1014.004236	14.969677
20.874470	1017.257091	14.974695
20.991358	1026.169946	14.979712
21.111120	1032.974226	14.984730
21.257040	1031.345048	14.989747
21.717005	1019.864499	14.994765
21.103599	1005.427815	14.999783
20.998184	992.486332	15.004800
21.055763	992.859200	15.009818
20.840643	998.529327	15.014835
21.306595	990.058565	15.019853
20.752624	1004.460443	15.024871
20.966010	1011.969586	15.029888
21.229062	1016.479176	15.034906
21.135705	1026.516907	15.039923
21.365210	1010.351276	15.044941
21.167804	1013.989403	15.049959
21.329450	1014.304939	15.054976
21.349271	1023.403419	15.059994
21.390055	1025.041271	15.065011
21.414822	1020.180519	15.070029
21.530161	1018.919059	15.075047
21.291881	1004.975880	15.080064
21.409146	1014.204257	15.085082
21.417344	1020.861907	15.090099
21.225423	1005.393485	15.095117
21.006648	1010.240505	15.100135
21.359274	1014.351043	15.105152
21.485053	1007.836567	15.110170
21.294722	1013.805779	15.115187
21.299497	1015.963680	15.120205
21.314190	1028.253560	15.125223
21.554431	1024.652958	15.130240
21.412970	1020.225359	15.135258
20.899365	1022.398207	15.140275
21.615242	1031.700065	15.145293
21.505228	1036.946628	15.150311
22.076481	1037.728176	15.155328
21.979837	1038.712202	15.160346
21.690786	1023.555636	15.165363
21.704098	1027.476338	15.170381
21.400599	1022.591277	15.175399
21.593690	1037.510463	15.180416
21.759561	1038.582750	15.185434
21.731427	1037.198598	15.190451
22.107912	1035.978274	15.195469
21.792059	1044.027954	15.200487
22.196813	1034.222354	15.205504
22.174594	1038.776647	15.210522
21.922469	1045.456157	15.215539
22.047698	1041.113004	15.220557
22.120793	1036.784331	15.225575
21.807236	1016.052011	15.230592
21.722104	1027.407611	15.235610
21.486595	1030.827644	15.240627
22.063085	1032.264794	15.245645
21.676616	1029.983710	15.250663
21.964629	1038.519457	15.255680
22.053867	1036.798171	15.260698
21.798386	1037.560925	15.265715
22.116800	1042.879222	15.270733
21.760414	1037.159822	15.275751
22.112400	1053.256517	15.280768
22.452846	1058.397793	15.285786
22.137470	1066.990222	15.290803
21.916954	1056.048625	15.295821
22.104875	1066.537781	15.300839
22.333313	1067.922168	15.305856
22.347601	1073.101927	15.310874
22.426234	1074.825374	15.315891
22.291276	1068.948191	15.320909
22.348668	1065.628700	15.325927
22.587066	1069.141750	15.330944
22.418245	1077.045329	15.335962
21.950953	1076.496862	15.340979
22.770404	1062.334262	15.345997
22.846234	1065.809666	15.351015
22.396071	1063.753157	15.356032
22.631343	1062.173094	15.361050
22.454556	1074.878025	15.366067
22.642107	1057.636454	15.371085
23.016636	1065.256075	15.376103
22.474581	1059.029258	15.381120
22.960903	1062.058482	15.386138
22.653148	1064.397903	15.391155
22.632768	1062.277213	15.396173
22.687727	1065.320373	15.401191
22.450890	1064.543290	15.406208
22.647366	1066.273520	15.411226
22.554302	1073.155343	15.416243
22.494630	1064.845799	15.421261
22.712951	1072.120658	15.426279
22.527178	1059.340044	15.431296
22.612725	1062.861262	15.436314
22.786376	1086.051962	15.441331
22.966888	1085.244202	15.446349
23.175852	1092.823502	15.451367
23.037424	1091.961569	15.456384
23.325444	1087.854837	15.461402
22.813442	1094.732878	15.466419
22.922310	1087.148019	15.471437
23.267623	1087.696719	15.476455
23.145470	1083.610071	15.481472
23.237729	1088.907010	15.486490
23.140342	1093.731877	15.491507
23.165938	1089.139227	15.496525
23.030361	1092.635135	15.501543
23.061085	1087.849173	15.506560
23.001783	1088.858910	15.511578
22.840360	1093.097346	15.516595
22.902516	1093.737750	15.521613
23.425889	1084.106047	15.526631
23.512173	1079.945715	15.531648
23.450870	1086.885686	15.536666
23.252421	1095.172621	15.541683
23.352344	1088.352889	15.546701
23.581748	1083.955532	15.551719
23.456685	1086.758652	15.556736
23.416164	1087.670770	15.561754
23.424336	1095.234192	15.566771
23.320975	1093.382126	15.571789
23.261077	1093.230589	15.576807
23.326288	1089.900401	15.581824
23.467221	1084.548046	15.586842
23.061853	1095.868656	15.591859
23.869264	1108.577201	15.596877
23.727241	1112.762108	15.601895
24.009460	1112.983014	15.606912
23.990808	1101.839342	15.611930
23.754499	1100.001794	15.616947
23.651351	1090.016958	15.621965
23.489801	1092.368191	15.626983
23.452454	1089.284452	15.632000
23.798411	1104.173431	15.637018
24.262993	1113.442120	15.642035
24.192134	1104.597807	15.647053
24.088516	1090.841750	15.652071
23.851266	1092.813513	15.657088
23.809775	1087.530767	15.662106
23.395214	1090.262477	15.667123
23.786905	1101.881096	15.672141
24.303659	1095.002365	15.677159
23.938685	1109.876501	15.682176
24.602324	1101.655589	15.687194
24.297897	1091.124760	15.692211
24.274799	1081.809059	15.697229
24.358814	1073.625324	15.702247
23.931166	1071.915591	15.707264
24.284861	1076.467801	15.712282
24.114462	1077.463385	15.717299
23.998420	1078.280035	15.722317
23.953983	1077.176153	15.727335
23.967751	1094.528271	15.732352
24.449375	1089.621167	15.737370
24.036930	1100.747223	15.742387
24.491599	1099.445215	15.747405
24.507602	1102.693307	15.752423
24.386501	1107.206304	15.757440
24.400700	1100.362127	15.762458
24.395181	1102.982413	15.767475
24.410316	1099.189840	15.772493
24.787352	1086.390456	15.777511
24.312318	1101.742590	15.782528
24.397330	1097.986409	15.787546
24.513546	1099.255833	15.792563
24.300552	1099.383910	15.797581
24.542291	1097.932222	15.802599
24.406803	1100.607585	15.807616
24.525073	1094.128969	15.812634
24.507355	1105.092193	15.817651
24.476514	1100.344276	15.822669
24.695713	1088.743612	15.827687
24.558258	1097.705821	15.832704
24.633540	1090.930976	15.837722
24.762448	1101.284228	15.842739
24.918038	1096.377711	15.847757
24.899408	1097.819745	15.852775
24.698037	1101.673112	15.857792
24.590412	1098.284793	15.862810
24.678885	1092.744990	15.867827
24.689811	1109.359090	15.872845
24.967941	1115.191820	15.877863
25.197250	1121.047980	15.882880
24.969935	1121.771609	15.887898
25.100708	1120.473010	15.892915
25.187918	1123.883523	15.897933
25.057509	1103.125562	15.902951
24.836022	1099.685653	15.907968
25.181833	1104.166520	15.912986
24.875700	1113.959919	15.918003
24.899815	1123.247130	15.923021
24.892674	1118.410286	15.928039
24.871425	1117.596266	15.933056
25.158357	1123.594882	15.938074
24.992113	1120.130534	15.943091
25.029287	1121.926756	15.948109
25.092638	1118.035104	15.953127
24.628553	1121.121728	15.958144
25.132404	1132.991045	15.963162
25.518975	1146.077989	15.968179
25.493555	1144.403060	15.973197
25.741286	1136.108437	15.978215
25.587929	1140.266723	15.983232
25.367238	1142.084413	15.988250
25.417505	1144.667561	15.993267
25.532657	1142.071176	15.998285
25.884489	1134.514503	16.003303
25.971252	1139.673458	16.008320
26.034658	1129.252238	16.013338
25.696498	1115.110020	16.018355
25.394382	1121.147276	16.023373
25.592555	1106.002667	16.028391
25.652924	1120.279979	16.033408
25.878487	1127.635780	16.038426
25.880143	1127.253685	16.043443
25.756845	1134.231790	16.048461
25.980756	1128.408816	16.053479
25.717901	1136.200918	16.058496
25.788600	1128.319055	16.063514
26.085878	1129.253991	16.068531
25.956340	1138.435893	16.073549
25.773917	1127.084328	16.078567
25.909093	1131.323641	16.083584
26.036147	1136.394229	16.088602
25.958903	1131.969165	16.093619
25.725275	1130.333171	16.098637
26.190863	1127.107508	16.103655
26.147558	1125.451162	16.108672
26.340153	1123.603217	16.113690
26.204121	1128.434149	16.118707
25.824730	1126.107760	16.123725
25.878646	1120.964695	16.128743
25.826221	1125.987659	16.133760
25.970587	1129.831044	16.138778
26.392487	1130.064780	16.143795
26.068956	1124.554805	16.148813
26.134328	1127.113492	16.153831
25.919009	1129.959163	16.158848
25.997176	1138.824491	16.163866
26.151402	1143.070289	16.168883
26.084937	1150.269877	16.173901
26.365583	1151.289473	16.178919
25.989123	1159.585394	16.183936
26.142109	1155.607104	16.188954
26.465389	1161.912473	16.193971
26.352071	1157.063851	16.198989
26.519216	1155.810044	16.204007
26.454243	1170.728748	16.209024
26.663206	1172.753687	16.214042
26.849051	1165.996205	16.219059
26.780612	1172.220936	16.224077
27.151009	1168.211736	16.229095
27.171772	1159.586578	16.234112
26.892446	1152.150878	16.239130
26.839516	1148.978049	16.244147
26.686030	1144.186219	16.249165
26.891122	1151.384286	16.254183
27.005590	1146.948116	16.259200
26.767354	1141.465798	16.264218
26.894212	1143.932801	16.269235
26.666667	1141.472163	16.274253
27.105101	1138.399079	16.279271
26.859977	1142.196192	16.284288
26.966059	1144.256183	16.289306
26.790338	1139.407875	16.294323
26.499520	1160.736877	16.299341
26.871938	1152.899252	16.304359
26.743042	1160.582011	16.309376
26.861093	1167.604368	16.314394
27.548539	1167.234747	16.319411
27.363937	1172.010181	16.324429
27.285840	1171.432291	16.329447
27.422893	1167.210335	16.334464
27.196081	1164.355091	16.339482
27.320093	1163.736067	16.344499
27.202425	1168.229605	16.349517
27.338321	1160.328046	16.354535
27.050518	1165.564631	16.359552
27.177683	1175.766716	16.364570
27.783965	1167.106622	16.369587
27.229185	1176.026955	16.374605
26.806930	1169.513077	16.379623
27.239959	1183.672089	16.384640
27.356190	1196.047165	16.389658
27.522516	1189.153872	16.394675
27.299591	1203.355712	16.399693
27.568211	1198.030657	16.404711
27.575649	1193.791132	16.409728
27.489961	1196.193610	16.414746
28.041696	1193.229002	16.419763
27.597711	1198.275465	16.424781
27.979974	1195.583571	16.429799
27.871151	1196.515864	16.434816
27.902223	1195.958739	16.439834
28.113748	1191.150733	16.444851
28.116955	1189.591239	16.449869
27.909838	1193.798988	16.454887
27.850919	1197.680550	16.459904
27.975185	1194.842880	16.464922
28.111477	1180.796692	16.469939
27.860283	1184.957694	16.474957
27.777711	1187.549037	16.479975
27.814345	1184.646201	16.484992
27.823720	1185.736705	16.490010
28.369300	1186.522283	16.495027
28.180274	1198.433930	16.500045
28.401399	1201.826633	16.505063
28.295293	1178.912444	16.510080
28.137574	1184.939721	16.515098
28.417344	1187.717298	16.520115
27.979763	1183.591683	16.525133
28.570277	1200.051939	16.530151
28.440750	1197.004716	16.535168
27.965626	1186.617344	16.540186
28.162634	1198.424325	16.545203
28.147145	1213.922312	16.550221
28.466864	1216.438005	16.555239
28.686196	1201.368898	16.560256
28.331072	1208.086698	16.565274
28.606579	1200.336822	16.570291
28.311296	1211.110062	16.575309
28.475109	1206.461011	16.580327
28.649465	1200.636310	16.585344
28.448007	1214.074221	16.590362
28.559671	1204.115627	16.595379
28.482608	1207.034325	16.600397
28.597308	1205.132302	16.605415
28.974318	1204.817632	16.610432
28.528461	1216.599112	16.615450
28.903990	1204.046041	16.620467
28.457246	1214.177117	16.625485
28.960723	1225.528985	16.630503
29.105840	1234.939313	16.635520
28.849686	1238.312124	16.640538
29.066672	1232.644842	16.645555
28.983624	1222.700965	16.650573
29.219311	1235.934697	16.655591
28.894423	1225.637376	16.660608
28.862334	1223.382796	16.665626
28.852194	1224.971839	16.670643
29.365980	1225.554110	16.675661
29.430837	1218.654613	16.680679
29.412897	1224.710498	16.685696
29.333080	1227.998873	16.690714
29.166127	1222.306539	16.695731
29.240785	1227.489508	16.700749
29.397079	1222.251475	16.705767
29.141029	1227.129640	16.710784
29.266901	1224.935520	16.715802
29.333340	1215.514200	16.720819
29.313524	1228.532329	16.725837
29.566121	1221.647598	16.730855
29.705011	1215.468675	16.735872
29.148063	1224.645001	16.740890
29.428659	1223.202995	16.745907
29.257727	1219.903470	16.750925
29.739117	1220.415075	16.755943
29.814266	1215.410671	16.760960
29.600226	1225.110804	16.765978
29.566047	1222.326357	16.770995
29.361267	1228.064367	16.776013
29.317316	1227.913486	16.781031
29.650720	1231.749366	16.786048
29.921252	1237.592794	16.791066
30.082642	1240.575126	16.796083
29.994632	1238.411360	16.801101
30.202622	1248.171618	16.806119
29.767914	1227.802029	16.811136
30.009300	1231.137912	16.816154
30.137154	1239.752500	16.821171
29.848275	1234.287556	16.826189
29.890297	1237.307526	16.831207
30.228046	1238.876778	16.836224
30.023475	1242.269912	16.841242
29.871449	1236.695160	16.846259
30.203745	1241.891417	16.851277
30.027086	1243.194115	16.856295
30.288333	1236.781411	16.861312
30.801454	1224.143650	16.866330
30.917493	1218.924549	16.871347
30.836778	1212.019459	16.876365
30.662495	1195.939016	16.881383
30.856527	1199.361211	16.886400
30.837744	1201.750051	16.891418
30.659831	1190.574471	16.896435
30.830256	1190.686657	16.901453
30.480940	1193.916261	16.906471
30.736856	1190.672944	16.911488
30.770396	1190.105965	16.916506
30.737531	1173.561558	16.921523
30.751689	1173.221686	16.926541
30.561503	1173.317787	16.931559
30.424675	1171.385747	16.936576
30.504081	1173.923306	16.941594
30.838992	1190.805467	16.946611
30.710446	1196.070759	16.951629
30.418567	1195.747277	16.956647
30.840130	1198.389027	16.961664
30.986756	1203.497595	16.966682
30.699184	1198.414323	16.971699
31.166876	1190.148329	16.976717
30.668424	1193.647461	16.981735
30.802861	1187.598638	16.986752
30.738436	1191.572583	16.991770
30.704139	1192.663618	16.996787
31.000959	1200.951902	17.001805
30.983785	1199.480810	17.006823
31.332884	1195.910457	17.011840
31.173557	1200.438934	17.016858
30.933945	1199.409806	17.021875
30.942162	1197.253060	17.026893
30.743694	1208.345656	17.031911
31.642499	1214.519844	17.036928
31.077230	1219.777826	17.041946
31.161076	1225.637877	17.046963
31.772199	1226.801365	17.051981
31.311533	1224.945306	17.056999
31.437197	1214.820404	17.062016
31.333196	1225.585775	17.067034
31.093496	1224.733391	17.072051
31.146865	1229.036039	17.077069
31.330503	1223.276151	17.082087
31.310026	1217.491439	17.087104
31.005975	1223.958238	17.092122
31.288899	1238.844582	17.097139
31.483132	1246.792342	17.102157
31.235407	1256.851232	17.107175
31.289144	1250.568870	17.112192
31.308370	1259.576041	17.117210
31.524878	1255.512035	17.122227
31.882007	1262.645300	17.127245
31.629252	1281.049253	17.132263
31.912110	1280.872415	17.137280
31.695851	1273.811806	17.142298
31.670971	1274.263874	17.147315
32.143405	1270.648934	17.152333
31.998157	1276.349228	17.157351
32.240738	1271.520555	17.162368
31.806892	1277.676337	17.167386
32.210913	1270.663717	17.172403
32.190397	1272.024008	17.177421
31.999356	1266.976086	17.182439
32.316792	1267.219880	17.187456
32.364852	1272.293416	17.192474
32.168001	1266.877162	17.197491
32.194218	1264.471425	17.202509
32.265121	1274.382569	17.207527
32.442484	1256.984606	17.212544
32.090830	1272.162915	17.217562
32.513934	1273.441075	17.222579
32.398269	1270.925019	17.227597
32.388610	1268.767908	17.232615
32.395539	1265.973858	17.237632
32.523446	1271.915386	17.242650
32.250470	1272.103357	17.247667
32.700762	1281.090339	17.252685
32.393170	1296.132372	17.257703
33.071197	1292.374758	17.262720
32.902624	1293.556268	17.267738
32.725230	1290.970982	17.272755
32.854925	1284.559937	17.277773
32.757195	1291.988551	17.282791
32.650014	1279.997070	17.287808
32.478770	1290.801419	17.292826
32.693428	1294.722192	17.297843
33.068379	1287.622599	17.302861
32.847359	1293.293743	17.307879
33.242630	1282.375451	17.312896
33.084327	1285.710849	17.317914
33.173873	1291.090327	17.322931
32.751313	1298.219529	17.327949
32.724960	1292.842828	17.332967
33.161361	1289.580683	17.337984
33.168896	1290.927112	17.343002
33.061729	1291.751848	17.348019
33.321760	1279.857474	17.353037
33.312323	1290.743772	17.358055
33.312057	1280.502859	17.363072
32.951566	1291.087541	17.368090
33.005804	1299.862021	17.373107
33.410098	1306.224178	17.378125
33.483741	1307.872687	17.383143
33.478778	1304.458776	17.388160
33.452386	1309.218927	17.393178
33.330680	1317.071046	17.398195
33.951263	1315.386409	17.403213
34.097347	1319.873376	17.408231
34.320792	1309.647891	17.413248
33.869868	1324.475709	17.418266
33.951103	1314.367181	17.423283
34.195237	1302.797187	17.428301
33.486771	1296.214491	17.433319
33.563389	1304.758239	17.438336
33.801177	1307.807511	17.443354
34.254059	1307.982745	17.448371
34.060945	1310.503060	17.453389
33.861708	1313.279964	17.458407
33.935086	1301.973420	17.463424
34.024663	1306.863729	17.468442
33.943169	1313.289378	17.473459
34.017363	1304.630530	17.478477
33.671806	1317.456754	17.483495
33.712129	1315.739949	17.488512
33.850588	1312.997871	17.493530
33.827374	1317.397749	17.498547
34.660739	1309.330039	17.503565
34.046566	1316.467178	17.508583
33.926169	1317.205623	17.513600
34.334742	1321.862912	17.518618
34.269029	1340.398574	17.523635
34.362961	1330.158654	17.528653
34.329695	1337.321555	17.533671
34.444766	1336.183197	17.538688
34.724557	1332.084011	17.543706
34.464809	1335.353258	17.548723
35.003614	1325.962015	17.553741
34.734718	1340.890721	17.558759
34.358789	1336.745942	17.563776
34.667004	1331.461983	17.568794
34.500097	1326.738480	17.573811
34.743530	1330.061438	17.578829
34.697579	1341.398475	17.583847
34.495254	1334.509235	17.588864
34.724893	1334.164002	17.593882
34.842739	1329.616800	17.598899
34.742151	1327.770587	17.603917
34.560187	1337.105977	17.608935
34.751841	1350.217299	17.613952
35.030637	1355.175809	17.618970
35.102868	1363.717117	17.623987
35.051194	1355.245231	17.629005
34.918921	1358.753297	17.634023
35.045423	1354.662343	17.639040
35.347242	1350.398749	17.644058
35.035025	1354.771331	17.649075
35.279089	1348.269758	17.654093
35.323796	1358.551142	17.659111
35.477089	1353.117872	17.664128
35.490169	1353.223153	17.669146
35.250423	1355.021758	17.674163
35.564535	1353.789095	17.679181
35.492942	1357.322368	17.684199
35.922637	1351.429209	17.689216
35.992780	1346.163611	17.694234
35.368577	1348.303330	17.699251
35.506904	1343.472037	17.704269
35.562629	1352.486160	17.709287
35.409499	1359.598420	17.714304
35.573550	1359.837844	17.719322
35.612969	1373.632627	17.724339
35.820008	1369.677381	17.729357
35.909082	1371.935731	17.734375
35.745943	1370.594797	17.739392
36.006856	1370.001656	17.744410
36.062320	1384.889045	17.749427
36.217281	1378.262560	17.754445
35.910077	1372.178724	17.759463
35.999887	1371.038010	17.764480
36.374416	1361.798725	17.769498
36.245835	1367.127191	17.774515
36.383247	1364.767138	17.779533
36.231265	1360.164370	17.784551
36.168080	1364.223369	17.789568
36.725963	1359.932277	17.794586
36.421115	1361.337122	17.799603
36.369230	1359.281295	17.804621
36.306519	1361.320418	17.809639
36.044179	1371.053444	17.814656
35.990117	1363.932672	17.819674
36.203582	1370.675060	17.824691
36.719533	1366.324261	17.829709
36.815431	1359.861678	17.834727
36.451608	1363.181952	17.839744
36.771940	1345.016701	17.844762
36.139136	1361.356337	17.849779
36.564696	1353.674407	17.854797
36.644937	1368.248619	17.859815
36.667048	1381.332877	17.864832
36.988331	1386.316298	17.869850
36.932622	1387.839908	17.874867
36.898958	1386.163092	17.879885
36.647755	1381.755753	17.884903
36.974290	1384.797445	17.889920
37.004537	1382.681408	17.894938
37.005910	1387.790695	17.899955
37.379092	1389.812022	17.904973
36.845056	1386.089652	17.909991
36.760706	1387.734520	17.915008
37.156485	1389.304162	17.920026
37.271297	1382.478829	17.925043
37.503013	1376.058079	17.930061
37.258527	1381.979091	17.935079
37.043006	1388.630902	17.940096
37.490954	1379.421132	17.945114
36.754751	1382.045483	17.950131
37.109207	1384.050807	17.955149
37.242344	1383.607079	17.960167
37.238877	1397.537993	17.965184
37.559366	1404.967403	17.970202
37.664427	1412.077102	17.975219
37.579967	1413.084487	17.980237
37.477439	1409.550137	17.985255
37.911842	1408.166073	17.990272
37.816521	1407.130105	17.995290
37.566540	1402.631047	18.000307
37.771094	1403.864561	18.005325
37.691169	1406.506017	18.010343
37.568089	1402.542523	18.015360
37.728342	1408.882990	18.020378
37.745898	1408.813993	18.025395
38.080161	1406.893328	18.030413
37.891066	1408.646131	18.035431
37.807551	1403.694938	18.040448
38.181725	1417.651910	18.045466
38.029607	1438.151588	18.050483
38.473173	1433.001034	18.055501
38.449422	1427.769059	18.060519
37.885467	1422.864731	18.065536
38.019083	1423.604409	18.070554
38.306837	1428.425830	18.075571
38.196505	1432.577442	18.080589
38.227905	1432.225396	18.085607
38.442294	1437.339194	18.090624
38.941246	1436.598297	18.095642
38.979158	1441.203234	18.100659
38.524519	1429.398642	18.105677
38.733528	1432.856407	18.110695
38.512882	1430.060116	18.115712
38.903595	1431.706298	18.120730
38.367190	1427.362568	18.125747
38.862957	1434.489960	18.130765
38.831030	1427.413033	18.135783
38.770523	1435.747945	18.140800
38.854220	1421.148049	18.145818
38.670649	1431.976506	18.150835
38.777782	1430.662652	18.155853
39.239023	1419.923298	18.160871
38.994533	1445.543786	18.165888
38.950769	1427.242985	18.170906
38.839120	1427.393056	18.175923
39.075064	1429.647339	18.180941
39.079476	1446.445817	18.185959
39.079382	1450.848418	18.190976
39.130301	1453.418885	18.195994
39.325176	1453.031757	18.201011
39.579963	1449.072169	18.206029
39.447350	1450.257522	18.211047
39.135659	1455.491622	18.216064
38.996390	1453.717731	18.221082
39.108356	1456.439587	18.226099
39.249302	1454.296729	18.231117
39.362249	1455.699242	18.236135
39.682436	1453.035972	18.241152
39.592776	1448.811599	18.246170
39.597930	1448.712985	18.251187
39.330566	1451.784621	18.256205
39.744768	1456.554678	18.261223
39.876099	1470.218365	18.266240
40.161282	1460.702679	18.271258
39.870679	1464.652159	18.276275
40.009206	1466.063288	18.281293
39.939868	1455.877280	18.286311
39.839426	1459.730690	18.291328
40.095498	1458.983663	18.296346
40.317396	1461.072884	18.301363
40.133813	1466.141741	18.306381
40.323621	1463.473649	18.311399
39.834135	1468.691426	18.316416
40.087175	1463.087853	18.321434
40.193412	1463.781327	18.326451
40.189357	1469.683633	18.331469
40.528547	1462.627446	18.336487
40.180224	1461.053574	18.341504
40.276475	1465.876606	18.346522
40.407335	1460.784507	18.351539
40.336002	1462.938607	18.356557
40.361086	1460.659259	18.361575
40.307566	1463.798383	18.366592
40.060682	1461.448032	18.371610
40.366766	1476.286763	18.376627
40.297610	1488.003088	18.381645
40.508044	1490.327650	18.386663
40.815408	1496.613540	18.391680
40.874044	1488.247390	18.396698
40.674492	1486.501877	18.401715
40.610629	1494.269268	18.406733
40.870300	1490.608722	18.411751
40.995321	1508.114233	18.416768
41.176760	1509.982570	18.421786
41.464323	1508.343780	18.426803
41.021306	1497.903855	18.431821
41.233439	1502.610906	18.436839
41.471377	1503.880224	18.441856
41.410697	1492.222159	18.446874
41.408162	1489.303319	18.451891
40.994857	1480.670272	18.456909
41.705368	1491.005213	18.461927
41.629518	1491.701970	18.466944
41.634354	1479.607593	18.471962
41.558404	1477.078973	18.476979
41.509234	1480.293161	18.481997
41.517339	1475.362309	18.487015
41.438674	1483.188822	18.492032
41.521921	1493.682007	18.497050
41.849043	1499.848031	18.502067
41.698107	1501.279268	18.507085
41.641027	1498.476275	18.512103
41.671701	1509.211247	18.517120
41.816051	1503.902416	18.522138
41.970296	1498.074459	18.527155
41.629219	1504.910095	18.532173
41.878919	1493.575804	18.537191
41.773342	1495.063052	18.542208
41.540507	1497.583304	18.547226
42.117234	1495.028164	18.552243
41.842909	1505.163948	18.557261
42.070154	1511.336158	18.562279
42.489669	1521.120232	18.567296
42.617806	1518.480730	18.572314
42.578446	1507.428417	18.577331
41.890191	1498.898403	18.582349
42.333093	1506.867282	18.587367
42.726075	1508.917080	18.592384
42.550953	1512.902128	18.597402
42.924645	1514.781371	18.602419
42.499065	1494.296431	18.607437
42.138989	1490.527847	18.612455
42.287078	1512.426005	18.617472
42.433708	1515.833596	18.622490
42.831594	1509.787571	18.627507
42.680879	1519.553684	18.632525
42.628194	1514.812236	18.637543
42.891303	1529.970186	18.642560
42.825178	1524.703793	18.647578
43.325482	1514.217052	18.652595
43.014304	1524.194511	18.657613
43.040419	1512.147274	18.662631
43.047126	1513.222436	18.667648
42.918713	1517.137047	18.672666
43.137323	1516.815631	18.677683
42.895265	1521.720087	18.682701
42.910587	1515.629853	18.687719
43.526464	1530.483211	18.692736
42.763856	1541.124730	18.697754
43.136472	1538.304902	18.702771
43.061428	1547.024016	18.707789
43.184443	1550.346946	18.712807
43.205262	1552.316196	18.717824
43.329233	1551.157494	18.722842
43.551691	1544.640299	18.727859
43.226352	1555.749832	18.732877
43.519758	1561.271030	18.737895
43.574911	1571.219522	18.742912
43.512562	1579.381210	18.747930
43.780473	1577.874889	18.752947
43.513830	1574.142144	18.757965
43.902011	1570.382548	18.762983
43.739451	1577.931896	18.768000
43.529678	1574.572115	18.773018
43.691053	1586.384936	18.778035
43.719989	1596.526908	18.783053
44.106130	1593.424071	18.788071
43.993065	1598.967938	18.793088
44.420353	1599.424913	18.798106
44.528395	1592.871975	18.803123
44.366436	1597.719718	18.808141
44.549789	1592.982295	18.813159
44.432672	1596.566932	18.818176
44.493259	1593.934847	18.823194
44.825064	1587.106999	18.828211
44.800397	1596.979644	18.833229
44.684910	1586.169596	18.838247
44.552674	1589.377883	18.843264
44.693950	1587.866153	18.848282
44.909525	1588.267931	18.853299
44.907363	1594.880078	18.858317
44.777825	1587.764729	18.863335
44.587603	1587.478963	18.868352
44.545261	1594.378287	18.873370
44.814454	1588.810017	18.878387
44.797293	1592.663030	18.883405
44.774993	1586.240976	18.888423
44.917846	1591.852047	18.893440
44.703727	1589.474454	18.898458
44.664338	1584.686720	18.903475
45.207517	1604.285500	18.908493
45.462746	1601.171612	18.913511
45.483409	1590.608489	18.918528
45.335587	1585.806184	18.923546
45.487985	1580.035296	18.928563
45.477874	1585.417853	18.933581
45.433219	1581.956457	18.938599
45.184224	1579.748440	18.943616
45.287233	1596.537923	18.948634
45.367680	1594.221481	18.953651
45.613657	1606.185171	18.958669
45.575487	1610.735796	18.963687
45.555929	1605.679847	18.968704
45.264887	1616.484225	18.973722
45.496973	1605.275707	18.978739
45.721121	1612.082789	18.983757
45.645799	1608.294813	18.988775
45.939034	1603.461272	18.993792
46.023928	1618.372648	18.998810
46.046359	1614.976478	19.003827
46.116259	1621.981310	19.008845
46.103591	1620.487386	19.013863
46.228643	1611.176602	19.018880
46.413921	1621.647564	19.023898
46.464567	1622.198266	19.028915
46.536883	1616.878596	19.033933
46.725544	1598.960950	19.038951
46.845261	1598.607687	19.043968
46.484427	1595.912234	19.048986
46.604808	1585.024204	19.054003
46.238535	1591.494571	19.059021
46.381595	1589.414485	19.064039
46.748825	1584.108582	19.069056
46.596763	1593.136447	19.074074
46.506058	1584.787339	19.079091
46.710230	1611.423425	19.084109
46.891524	1607.813007	19.089127
46.779556	1614.798992	19.094144
46.437142	1616.370697	19.099162
47.175941	1608.065193	19.104179
46.709253	1616.252376	19.109197
46.566401	1620.134557	19.114215
47.178030	1615.459422	19.119232
47.073848	1621.860332	19.124250
47.485263	1611.043459	19.129267
46.910677	1610.862097	19.134285
47.089691	1613.522977	19.139303
47.278887	1617.444655	19.144320
47.301902	1639.002783	19.149338
47.486742	1628.085692	19.154355
47.475034	1637.517647	19.159373
47.373119	1641.740576	19.164391
47.392368	1644.281317	19.169408
47.250521	1645.083099	19.174426
47.664386	1639.855084	19.179443
47.857559	1647.171991	19.184461
47.761987	1641.705039	19.189479
47.861232	1646.328823	19.194496
47.741115	1649.058667	19.199514
47.777285	1641.308228	19.204531
47.311811	1637.429887	19.209549
47.630133	1642.161365	19.214567
47.582578	1644.497965	19.219584
47.708972	1654.984484	19.224602
47.964883	1657.791122	19.229619
48.021443	1668.354867	19.234637
47.850742	1666.058828	19.239655
48.149923	1660.043998	19.244672
47.885237	1669.512450	19.249690
48.118458	1673.809118	19.254707
48.288654	1685.974095	19.259725
48.436445	1679.146639	19.264743
48.300235	1672.953852	19.269760
48.547360	1683.484592	19.274778
48.787624	1672.628223	19.279795
48.736904	1678.724113	19.284813
49.131198	1673.893655	19.289831
49.157954	1664.847567	19.294848
48.840372	1679.263442	19.299866
49.124990	1673.904180	19.304883
48.922417	1658.058141	19.309901
48.712439	1658.094224	19.314919
49.078744	1668.562099	19.319936
48.827883	1677.141555	19.324954
49.011460	1673.035274	19.329971
49.127873	1674.797045	19.334989
49.141246	1676.887403	19.340007
49.170234	1673.868914	19.345024
48.932069	1673.969377	19.350042
49.276672	1680.738677	19.355059
49.410340	1676.466636	19.360077
49.178509	1685.522825	19.365095
49.286392	1678.225066	19.370112
49.158008	1680.145118	19.375130
49.205786	1684.934776	19.380147
49.546954	1700.074328	19.385165
49.475008	1697.668133	19.390183
49.562069	1696.900237	19.395200
49.548845	1703.368981	19.400218
49.711714	1705.783080	19.405235
49.926092	1706.446996	19.410253
49.869210	1695.536177	19.415271
49.762659	1700.892850	19.420288
49.769346	1696.656479	19.425306
49.742386	1693.558384	19.430323
50.188422	1721.415984	19.435341
49.833060	1723.608304	19.440359
50.252899	1717.577706	19.445376
50.271129	1727.939195	19.450394
50.317443	1729.661458	19.455411
50.498462	1725.965847	19.460429
50.760645	1724.372043	19.465447
50.876952	1725.704619	19.470464
50.699143	1721.774876	19.475482
50.708962	1724.550650	19.480499
51.196608	1721.649652	19.485517
50.604228	1712.716324	19.490535
50.694802	1706.421718	19.495552
50.821494	1724.454232	19.500570
50.804396	1723.469109	19.505587
50.535797	1718.490019	19.510605
50.468728	1716.177737	19.515623
50.944070	1714.544225	19.520640
50.811282	1717.563261	19.525658
50.861429	1719.114498	19.530675
51.148000	1720.130044	19.535693
50.915928	1718.531623	19.540711
51.392077	1712.504829	19.545728
51.293685	1714.600078	19.550746
50.882740	1712.338518	19.555763
51.396480	1730.259900	19.560781
51.435021	1745.601550	19.565799
51.766405	1739.853065	19.570816
51.366575	1745.760663	19.575834
51.363666	1734.383742	19.580851
51.766123	1737.003320	19.585869
51.586570	1741.699214	19.590887
51.676505	1738.825809	19.595904
51.546727	1733.679788	19.600922
51.453612	1746.204817	19.605939
51.701225	1732.645717	19.610957
51.481748	1749.318602	19.615975
51.515902	1737.894843	19.620992
51.821409	1755.852032	19.626010
51.910680	1762.014386	19.631027
52.066443	1767.080656	19.636045
52.112996	1775.392639	19.641063
51.919371	1768.195735	19.646080
52.088617	1777.984446	19.651098
52.343507	1766.358817	19.656115
52.550835	1767.427810	19.661133
52.440292	1771.342833	19.666151
52.467851	1766.686581	19.671168
52.639818	1768.035687	19.676186
52.572916	1759.392415	19.681203
52.682607	1760.685002	19.686221
52.423028	1761.855552	19.691239
52.477177	1767.821426	19.696256
52.348901	1767.380774	19.701274
52.613719	1789.639704	19.706291
52.700031	1779.668983	19.711309
52.496646	1785.138690	19.716327
52.820444	1781.717363	19.721344
52.896861	1787.253692	19.726362
52.722433	1801.394755	19.731379
52.890353	1801.418970	19.736397
53.197697	1810.567483	19.741415
53.533056	1799.658265	19.746432
53.185721	1803.338977	19.751450
52.939123	1808.521952	19.756467
52.972784	1799.582019	19.761485
53.213944	1807.712038	19.766503
53.196454	1808.794165	19.771520
53.504087	1826.145136	19.776538
53.565301	1835.966584	19.781555
54.075937	1829.707114	19.786573
53.651123	1820.914748	19.791591
53.791851	1822.653787	19.796608
53.847439	1818.677987	19.801626
53.984533	1827.471304	19.806643
54.209086	1817.216953	19.811661
54.037714	1820.747014	19.816679
54.385826	1807.030091	19.821696
54.120810	1822.495112	19.826714
53.972537	1812.800983	19.831731
54.328375	1807.181198	19.836749
54.104776	1810.896177	19.841767
54.444028	1813.399429	19.846784
54.529140	1814.607502	19.851802
54.133780	1810.708669	19.856819
54.670460	1815.311301	19.861837
54.290378	1816.181977	19.866855
54.596809	1822.452348	19.871872
54.700058	1828.066543	19.876890
54.661771	1839.270141	19.881907
54.960889	1837.042492	19.886925
54.936232	1844.324176	19.891943
55.003103	1837.266324	19.896960
55.065839	1836.552730	19.901978
54.837010	1830.813087	19.906995
54.954641	1828.219371	19.912013
54.782514	1840.109860	19.917031
54.965942	1839.096470	19.922048
54.824814	1834.381417	19.927066
54.810905	1833.869193	19.932083
55.303593	1826.899275	19.937101
55.077402	1834.938416	19.942119
55.099396	1849.762004	19.947136
55.647010	1863.976194	19.952154
55.177485	1858.955957	19.957171
55.723336	1862.351562	19.962189
55.622738	1869.067601	19.967207
55.573120	1866.534800	19.972224
55.769748	1858.822248	19.977242
55.656526	1863.381540	19.982259
55.625941	1854.470581	19.987277
55.419049	1859.025612	19.992295
55.428299	1862.296992	19.997312
56.199279	1873.844067	20.002330
56.064647	1886.536656	20.007347
56.371910	1877.443356	20.012365
56.204743	1882.837985	20.017383
56.233197	1874.037696	20.022400
56.358793	1882.491990	20.027418
56.261520	1891.767059	20.032435
56.445522	1875.904445	20.037453
56.211875	1880.441581	20.042471
56.187123	1874.209170	20.047488
56.692507	1877.396508	20.052506
56.427204	1885.508076	20.057523
56.719006	1879.503798	20.062541
56.243592	1894.818795	20.067559
56.538038	1903.868383	20.072576
57.020651	1905.708511	20.077594
56.806786	1909.860675	20.082611
56.977954	1901.041168	20.087629
57.108764	1899.925558	20.092647
57.105038	1904.527670	20.097664
57.376744	1905.529776	20.102682
57.059928	1903.187166	20.107699
56.967850	1908.065073	20.112717
57.048280	1905.578167	20.117735
57.227503	1916.192272	20.122752
57.297626	1928.966428	20.127770
57.293234	1940.038537	20.132787
57.796736	1927.726863	20.137805
57.871537	1926.863041	20.142823
57.376590	1925.356284	20.147840
57.621223	1924.409045	20.152858
57.616013	1928.553769	20.157875
57.728693	1928.798095	20.162893
57.881217	1929.219228	20.167911
57.890045	1926.055521	20.172928
57.951190	1918.247397	20.177946
57.650298	1928.160346	20.182963
58.124132	1939.643558	20.187981
58.104434	1953.706846	20.192999
58.112023	1953.876111	20.198016
58.599901	1958.685258	20.203034
58.346686	1948.824448	20.208051
58.289183	1950.925942	20.213069
58.415905	1956.489159	20.218087
58.031142	1955.359641	20.223104
58.766019	1934.004363	20.228122
58.757275	1934.081506	20.233139
59.027921	1923.292814	20.238157
59.186785	1919.171414	20.243175
59.024684	1924.278062	20.248192
59.417759	1924.068171	20.253210
59.325995	1921.036999	20.258227
59.289206	1918.536896	20.263245
59.373156	1920.575197	20.268263
59.567306	1920.822538	20.273280
59.301334	1926.194788	20.278298
59.140793	1925.825464	20.283315
59.521019	1919.412813	20.288333
59.671458	1919.509201	20.293351
59.375623	1900.890777	20.298368
59.324763	1902.123315	20.303386
59.243447	1915.666013	20.308403
59.464827	1913.482095	20.313421
59.126066	1911.985584	20.318439
59.375398	1912.350521	20.323456
59.734911	1919.742472	20.328474
59.720093	1908.629257	20.333491
59.623195	1921.218122	20.338509
59.527291	1933.532263	20.343527
59.557589	1937.314794	20.348544
59.768970	1936.502162	20.353562
59.703922	1942.559358	20.358579
59.777893	1935.222624	20.363597
59.806086	1945.143988	20.368615
60.029382	1963.325721	20.373632
60.443271	1965.384922	20.378650
59.947054	1971.329787	20.383667
59.910510	1967.696618	20.388685
60.142386	1965.933959	20.393703
60.396656	1986.616764	20.398720
60.914489	1986.980664	20.403738
60.511121	1999.286214	20.408755
60.483840	2009.030097	20.413773
60.396222	2000.702404	20.418791
60.430076	2004.654818	20.423808
60.882348	2001.251194	20.428826
60.980038	2006.427625	20.433843
61.215199	2020.365821	20.438861
61.226507	2013.313449	20.443879
61.456412	2022.562573	20.448896
61.543903	2025.869066	20.453914
61.496526	2023.563127	20.458931
61.410503	2013.543531	20.463949
61.339284	2016.095342	20.468967
61.304693	2025.045053	20.473984
61.661918	2018.819023	20.479002
61.683251	2010.559468	20.484019
61.893381	2021.459150	20.489037
61.579957	2017.241297	20.494055
61.695851	2022.626335	20.499072
61.595633	2014.660400	20.504090
61.784988	2018.721009	20.509107
61.694585	2016.819475	20.514125
61.706759	2017.025896	20.519143
62.055494	2035.920254	20.524160
62.066492	2031.200252	20.529178
62.134288	2039.426972	20.534195
62.017935	2037.393791	20.539213
62.788729	2031.806761	20.544231
62.066184	2034.971903	20.549248
62.408709	2037.165380	20.554266
62.448113	2038.156549	20.559283
62.477143	2029.917872	20.564301
62.366584	2048.413951	20.569319
62.246599	2063.493508	20.574336
62.675605	2060.380720	20.579354
62.872197	2066.456931	20.584371
62.784551	2068.032943	20.589389
62.569151	2055.972684	20.594407
62.853180	2059.538748	20.599424
62.787209	2066.795434	20.604442
63.488445	2083.851439	20.609459
63.608541	2087.900822	20.614477
63.563315	2069.085156	20.619495
63.399599	2065.424551	20.624512
63.602374	2056.779912	20.629530
63.482896	2068.917944	20.634547
63.463666	2064.701327	20.639565
63.625816	2074.999439	20.644583
63.271958	2090.835245	20.649600
63.841557	2088.319014	20.654618
63.738502	2090.307732	20.659635
63.786522	2076.634464	20.664653
63.654068	2078.324804	20.669671
63.855455	2087.231262	20.674688
63.883209	2082.186702	20.679706
63.886578	2080.734412	20.684723
63.803200	2081.482867	20.689741
64.071682	2089.381497	20.694759
64.227340	2101.315485	20.699776
64.681269	2100.395411	20.704794
64.652023	2104.433479	20.709811
64.687462	2107.145333	20.714829
64.902604	2097.750748	20.719847
64.667395	2092.756853	20.724864
64.725133	2096.907534	20.729882
64.662454	2093.297371	20.734899
64.278989	2091.902531	20.739917
65.121431	2087.140617	20.744935
64.926625	2091.270900	20.749952
64.820059	2100.493879	20.754970
64.815099	2101.353136	20.759987
64.769435	2096.689334	20.765005
65.075343	2105.964467	20.770023
65.062002	2124.656849	20.775040
65.652576	2120.669754	20.780058
65.575958	2118.387321	20.785075
65.336296	2121.442105	20.790093
65.989135	2113.689527	20.795111
65.870709	2114.086839	20.800128
65.654411	2113.877738	20.805146
65.691666	2113.600507	20.810163
65.556260	2113.697496	20.815181
65.692843	2112.394759	20.820199
65.220679	2112.389862	20.825216
65.868690	2124.357188	20.830234
65.837112	2139.053697	20.835251
65.925259	2138.699059	20.840269
66.002826	2142.802459	20.845287
66.116491	2146.868644	20.850304
66.284746	2133.612034	20.855322
66.066020	2141.899473	20.860339
66.333518	2148.561101	20.865357
66.331110	2152.238339	20.870375
66.425424	2158.393727	20.875392
66.561440	2162.510067	20.880410
66.256988	2157.675338	20.885427
66.334697	2161.068602	20.890445
67.042981	2162.769251	20.895463
66.934488	2161.283982	20.900480
67.457559	2170.907010	20.905498
67.266527	2148.642414	20.910515
66.962841	2155.336725	20.915533
67.344704	2160.023670	20.920551
67.371850	2175.039240	20.925568
67.339076	2177.354657	20.930586
67.510416	2173.133405	20.935603
67.820055	2188.445584	20.940621
67.721582	2167.990680	20.945639
67.754960	2159.621862	20.950656
67.375688	2148.543507	20.955674
67.457213	2162.291272	20.960691
67.238492	2172.065237	20.965709
67.647108	2168.213947	20.970727
67.788014	2179.039356	20.975744
67.673939	2175.654999	20.980762
67.717594	2171.999755	20.985779
67.947972	2179.888615	20.990797
68.041217	2189.468533	20.995815
68.097196	2204.631103	21.000832
68.274498	2200.263731	21.005850
68.331900	2196.735728	21.010867
68.124449	2202.168325	21.015885
68.305660	2204.970973	21.020903
68.370063	2196.221704	21.025920
68.318625	2206.742720	21.030938
68.896349	2213.914396	21.035955
68.650397	2224.402777	21.040973
68.789577	2222.193827	21.045991
68.725073	2226.085955	21.051008
68.613897	2229.537231	21.056026
68.746832	2219.047674	21.061043
68.790858	2229.638962	21.066061
69.071075	2244.274082	21.071079
69.225155	2249.309192	21.076096
69.107872	2252.338511	21.081114
69.166321	2249.501519	21.086131
69.118449	2251.819311	21.091149
69.411235	2248.383819	21.096167
69.537922	2255.102266	21.101184
69.529617	2269.075644	21.106202
69.775124	2265.982103	21.111219
69.655919	2275.639538	21.116237
70.065828	2273.924703	21.121255
69.836496	2275.365127	21.126272
70.017399	2271.508462	21.131290
70.038323	2273.701858	21.136307
70.061252	2282.377573	21.141325
70.208967	2276.806031	21.146343
70.089419	2273.015376	21.151360
70.223836	2284.832882	21.156378
70.485809	2290.135148	21.161395
70.026500	2292.444816	21.166413
70.329419	2299.151449	21.171431
70.535497	2297.405425	21.176448
70.768211	2290.138358	21.181466
70.422372	2292.906819	21.186483
70.783094	2310.556085	21.191501
71.057290	2310.257509	21.196519
71.137611	2305.217275	21.201536
71.103282	2311.926252	21.206554
71.836718	2313.035940	21.211571
71.989988	2312.200835	21.216589
71.958192	2305.063575	21.221607
71.671652	2289.870822	21.226624
71.752456	2281.510298	21.231642
71.863448	2273.583746	21.236659
71.750917	2274.601889	21.241677
71.706948	2278.749611	21.246695
71.679059	2274.076667	21.251712
72.054120	2276.328199	21.256730
72.227798	2272.576817	21.261747
71.832953	2279.780964	21.266765
72.041367	2281.503132	21.271783
71.806889	2276.957237	21.276800
71.899630	2295.898290	21.281818
71.771982	2301.883357	21.286835
71.804133	2299.183033	21.291853
71.796221	2308.087677	21.296871
72.111455	2300.018650	21.301888
71.847056	2319.126146	21.306906
72.207123	2326.313032	21.311923
72.387956	2329.024232	21.316941
72.362790	2328.112931	21.321959
72.311954	2333.360068	21.326976
72.577536	2349.865985	21.331994
72.931695	2357.309455	21.337011
72.821350	2356.951193	21.342029
72.996286	2354.326331	21.347047
73.087017	2354.378422	21.352064
72.977528	2344.599026	21.357082
72.709201	2347.579436	21.362099
73.203057	2362.989147	21.367117
73.758768	2367.323829	21.372135
74.369125	2370.075048	21.377152
73.922389	2358.997664	21.382170
74.368518	2351.024883	21.387187
73.976632	2340.096723	21.392205
74.181209	2345.430091	21.397223
74.496695	2330.225041	21.402240
73.999249	2341.339929	21.407258
74.251093	2337.790903	21.412275
74.171800	2340.208311	21.417293
74.033009	2334.858382	21.422311
74.119161	2333.576156	21.427328
73.828501	2338.393764	21.432346
74.185829	2349.567259	21.437363
74.348752	2355.554160	21.442381
74.540241	2356.228000	21.447399
74.512555	2365.495567	21.452416
74.468169	2364.050736	21.457434
74.532876	2364.116373	21.462451
74.737369	2372.829964	21.467469
74.860354	2376.683281	21.472487
74.911724	2385.865881	21.477504
74.969168	2391.250720	21.482522
75.140947	2380.597177	21.487539
75.164065	2387.612795	21.492557
75.167351	2394.035015	21.497575
75.237111	2388.065357	21.502592
75.033453	2396.388424	21.507610
75.474973	2404.705097	21.512627
75.430021	2409.746186	21.517645
75.344626	2409.377703	21.522663
75.628771	2411.037520	21.527680
75.447953	2412.650252	21.532698
76.010259	2419.653997	21.537715
76.006603	2424.114205	21.542733
76.038624	2442.017091	21.547751
76.072384	2424.107111	21.552768
75.939882	2427.160938	21.557786
76.230251	2427.295372	21.562803
76.111578	2429.671621	21.567821
76.270239	2426.840993	21.572839
76.410533	2423.271554	21.577856
76.533121	2430.489377	21.582874
76.717783	2437.968904	21.587891
76.708313	2455.770996	21.592909
76.730651	2448.072875	21.597927
76.858251	2441.412412	21.602944
76.575379	2449.703729	21.607962
76.714469	2442.975187	21.612979
76.695271	2449.183177	21.617997
77.025856	2477.236785	21.623015
77.226521	2467.916867	21.628032
77.248110	2477.132585	21.633050
77.613424	2467.209298	21.638067
77.487144	2462.955705	21.643085
77.340717	2468.590282	21.648103
77.754633	2468.528616	21.653120
77.668252	2474.627207	21.658138
77.703595	2467.684513	21.663155
77.607663	2469.545910	21.668173
77.451001	2484.729407	21.673191
77.911537	2495.924696	21.678208
77.478525	2500.638405	21.683226
77.920283	2496.927035	21.688243
78.043452	2496.345973	21.693261
78.146726	2509.004883	21.698279
78.673678	2514.139456	21.703296
78.420323	2520.134821	21.708314
78.533841	2513.590159	21.713331
78.575142	2511.434383	21.718349
78.184772	2511.375639	21.723367
78.675040	2517.500676	21.728384
78.605821	2523.107392	21.733402
78.892309	2529.939776	21.738419
78.947907	2543.944386	21.743437
78.905021	2540.996979	21.748455
79.132087	2545.689342	21.753472
79.063496	2544.257756	21.758490
79.047672	2534.081689	21.763507
79.239396	2543.075104	21.768525
79.510457	2558.280022	21.773543
79.561789	2562.614871	21.778560
79.683044	2562.652713	21.783578
79.886469	2555.525843	21.788595
79.725055	2557.511130	21.793613
79.837858	2567.173401	21.798631
80.030839	2556.522745	21.803648
79.671941	2563.749778	21.808666
80.364129	2571.616956	21.813683
80.480751	2583.276483	21.818701
80.608592	2591.986409	21.823719
80.775999	2594.368356	21.828736
80.735671	2590.587315	21.833754
80.496203	2586.364051	21.838771
80.833433	2586.579517	21.843789
80.316085	2594.424745	21.848807
80.727018	2578.715327	21.853824
80.602085	2584.182452	21.858842
80.539398	2582.506915	21.863859
80.776699	2580.007964	21.868877
80.756292	2610.048337	21.873895
81.124273	2611.505669	21.878912
80.917053	2616.019911	21.883930
80.905456	2616.662457	21.888947
80.924549	2617.167636	21.893965
80.877762	2637.866798	21.898983
81.257857	2633.940974	21.904000
81.478028	2632.940721	21.909018
81.787435	2644.907793	21.914035
82.041039	2649.207817	21.919053
82.060873	2654.226199	21.924071
82.141405	2648.346296	21.929088
82.142855	2659.724081	21.934106
82.086007	2654.935640	21.939123
82.357508	2655.562239	21.944141
82.177393	2661.325244	21.949159
82.553779	2650.475365	21.954176
82.333785	2652.482465	21.959194
82.652513	2650.523076	21.964211
82.766935	2654.807034	21.969229
82.433455	2656.156494	21.974247
82.444984	2663.439153	21.979264
82.973204	2671.843364	21.984282
82.994811	2669.463411	21.989299
82.948234	2671.111945	21.994317
82.958780	2669.652170	21.999335
83.316744	2668.453582	22.004352
83.076186	2673.042497	22.009370
83.363183	2672.659850	22.014387
83.487398	2676.203734	22.019405
84.014320	2685.068956	22.024423
83.875861	2674.757370	22.029440
83.926005	2678.044585	22.034458
83.867388	2671.867701	22.039475
84.134136	2676.866342	22.044493
84.271606	2687.736784	22.049511
84.267860	2699.014410	22.054528
84.180341	2695.606857	22.059546
84.656977	2695.835202	22.064563
84.570710	2694.418998	22.069581
84.408191	2702.675794	22.074599
84.531204	2688.709413	22.079616
84.661057	2696.825714	22.084634
84.822062	2688.465061	22.089651
84.734155	2693.541365	22.094669
84.713222	2696.151673	22.099687
84.935163	2690.764058	22.104704
84.544955	2689.925711	22.109722
84.318943	2696.469181	22.114739
84.793938	2706.832264	22.119757
84.729139	2721.370332	22.124775
85.248624	2723.700292	22.129792
85.130385	2732.051161	22.134810
85.447867	2739.443725	22.139827
85.346381	2741.912008	22.144845
85.448060	2748.129568	22.149863
85.546886	2745.494480	22.154880
85.353483	2753.629891	22.159898
85.454579	2765.298280	22.164915
85.953427	2769.932340	22.169933
85.817384	2776.629021	22.174951
86.202806	2773.418788	22.179968
86.033984	2775.219044	22.184986
86.136133	2786.281294	22.190003
86.123511	2797.323658	22.195021
86.211913	2803.757938	22.200039
86.775597	2798.859614	22.205056
86.512571	2791.199743	22.210074
86.750667	2785.626509	22.215091
86.921651	2796.498077	22.220109
86.861257	2816.356873	22.225127
87.193469	2810.999288	22.230144
86.961813	2809.552199	22.235162
86.808378	2810.557843	22.240179
87.562057	2797.212182	22.245197
87.706435	2803.479883	22.250215
87.722467	2800.472704	22.255232
87.394959	2800.568230	22.260250
87.397319	2813.341007	22.265267
87.665557	2820.722383	22.270285
88.138695	2822.182195	22.275303
88.170430	2824.815832	22.280320
88.686725	2826.906435	22.285338
88.559024	2815.201199	22.290355
88.455175	2819.822388	22.295373
88.629326	2819.438482	22.300391
88.739157	2812.783822	22.305408
89.104016	2802.740488	22.310426
88.380955	2796.033267	22.315443
88.800279	2778.564362	22.320461
88.639982	2787.508898	22.325479
88.667712	2800.722714	22.330496
88.873873	2805.702478	22.335514
88.733311	2805.585656	22.340531
88.791947	2805.383970	22.345549
88.944245	2808.232274	22.350567
88.897915	2809.599881	22.355584
89.136364	2812.321065	22.360602
89.456051	2830.734759	22.365619
89.692895	2832.812333	22.370637
89.514644	2842.971689	22.375655
89.207528	2828.403475	22.380672
89.537363	2826.950475	22.385690
89.612545	2829.419496	22.390707
89.732375	2839.601586	22.395725
89.821616	2864.490068	22.400743
90.101906	2865.121610	22.405760
90.036334	2863.427562	22.410778
89.862276	2861.346516	22.415795
90.287342	2863.451416	22.420813
90.157083	2874.420728	22.425831
90.158703	2885.246293	22.430848
90.347463	2888.625452	22.435866
90.326958	2894.448743	22.440883
90.785124	2903.378501	22.445901
90.818582	2913.488947	22.450919
90.797387	2910.841077	22.455936
90.630257	2915.244957	22.460954
90.796266	2918.514063	22.465971
90.898038	2924.340299	22.470989
91.173284	2931.635405	22.476007
91.259606	2940.522441	22.481024
91.595956	2941.463981	22.486042
91.735359	2939.914559	22.491059
92.136988	2938.361929	22.496077
91.598766	2947.419409	22.501095
91.990946	2966.907624	22.506112
92.137182	2961.970504	22.511130
91.991561	2961.901816	22.516147
92.084183	2959.902070	22.521165
92.241755	2957.560745	22.526183
92.123986	2963.891667	22.531200
92.385174	2977.892810	22.536218
92.629360	2983.068664	22.541235
92.642639	2982.997175	22.546253
92.510218	2989.507150	22.551271
92.844576	2989.940852	22.556288
92.769403	2986.673339	22.561306
93.048404	2984.966325	22.566323
93.386660	2990.455691	22.571341
93.381334	2999.754799	22.576359
93.630269	3003.143490	22.581376
93.633379	3007.350284	22.586394
93.393429	3005.128045	22.591411
93.591480	2999.570489	22.596429
93.766339	3005.060209	22.601447
93.663045	2999.786581	22.606464
93.754218	3008.609766	22.611482
93.589253	3003.752953	22.616499
93.888825	3013.373578	22.621517
94.968029	3006.693223	22.626535
95.158365	3008.216296	22.631552
95.746057	2987.905455	22.636570
95.119845	2987.681658	22.641587
95.218320	2978.475330	22.646605
95.310837	2977.545559	22.651623
95.023377	2978.468054	22.656640
95.327522	2964.599330	22.661658
95.075237	2948.709439	22.666675
95.393728	2937.628587	22.671693
95.577380	2944.167931	22.676711
95.238573	2943.491954	22.681728
95.307133	2944.005173	22.686746
95.144798	2945.236310	22.691763
95.587751	2958.918590	22.696781
95.678252	2970.159527	22.701799
95.414390	2979.780034	22.706816
95.340016	2976.196775	22.711834
95.324401	2980.804181	22.716851
95.407681	2978.004215	22.721869
95.796699	2989.267831	22.726887
95.250474	2999.750050	22.731904
95.861706	3009.025159	22.736922
96.160145	3022.203037	22.741939
96.241418	3028.556453	22.746957
96.236315	3031.628296	22.751975
96.009093	3039.065293	22.756992
96.235210	3038.199805	22.762010
96.269224	3050.197669	22.767027
96.700967	3052.254203	22.772045
97.216495	3061.064585	22.777063
96.865989	3075.429920	22.782080
97.014262	3084.200008	22.787098
97.220557	3084.862089	22.792115
97.690316	3088.629668	22.797133
97.670405	3084.482356	22.802151
97.487469	3083.437922	22.807168
97.509360	3078.779064	22.812186
97.385434	3091.420323	22.817203
97.653423	3100.613537	22.822221
97.749623	3108.811047	22.827239
97.724600	3110.389963	22.832256
97.865143	3111.491596	22.837274
97.814652	3127.388092	22.842291
98.030985	3134.528386	22.847309
97.951876	3126.495525	22.852327
98.262334	3140.482763	22.857344
98.799724	3147.339198	22.862362
98.507947	3155.815296	22.867379
98.495219	3153.791002	22.872397
98.816116	3154.826507	22.877415
98.845007	3174.715895	22.882432
99.374815	3170.611845	22.887450
99.362097	3183.131589	22.892467
99.299068	3187.052099	22.897485
99.415779	3177.356749	22.902503
99.570656	3187.056949	22.907520
99.931543	3167.437943	22.912538
99.906034	3174.701361	22.917555
100.053315	3192.741592	22.922573
100.274404	3188.663811	22.927591
100.492027	3189.803873	22.932608
100.530285	3184.321795	22.937626
100.515122	3194.664111	22.942643
100.502387	3194.795541	22.947661
100.804567	3185.727631	22.952679
100.472943	3191.227322	22.957696
100.565742	3187.810362	22.962714
100.372168	3196.258467	22.967731
100.556258	3192.293795	22.972749
100.590027	3203.284952	22.977767
100.765076	3208.623204	22.982784
101.134944	3209.594227	22.987802
100.670978	3219.574463	22.992819
100.969173	3218.905988	22.997837
101.449800	3232.437385	23.002855
100.984623	3244.194803	23.007872
101.803951	3232.227299	23.012890
101.617874	3229.961873	23.017907
101.389423	3235.132942	23.022925
102.246543	3241.386974	23.027943
102.081177	3254.451468	23.032960
102.478825	3262.617601	23.037978
102.577420	3265.171389	23.042995
102.508425	3258.535114	23.048013
102.753531	3270.462177	23.053031
102.544159	3259.747894	23.058048
102.591844	3251.259546	23.063066
102.580641	3258.605976	23.068083
102.551174	3261.148265	23.073101
102.774994	3262.322080	23.078119
103.075870	3276.001610	23.083136
103.307682	3286.248471	23.088154
103.252651	3286.591687	23.093171
103.210719	3286.437314	23.098189
103.333346	3285.259777	23.103207
103.321179	3288.967182	23.108224
103.399358	3298.515332	23.113242
103.441033	3310.827797	23.118259
103.526475	3303.068923	23.123277
103.577313	3321.468427	23.128295
103.855479	3329.814280	23.133312
104.071885	3334.682116	23.138330
103.949523	3337.977541	23.143347
104.070819	3337.535623	23.148365
104.429100	3350.559177	23.153383
104.257469	3360.945040	23.158400
104.808637	3350.771212	23.163418
105.275744	3343.817349	23.168435
105.302517	3344.387627	23.173453
105.296070	3344.578043	23.178471
105.253158	3342.526894	23.183488
105.583547	3333.596525	23.188506
105.527581	3334.523801	23.193523
105.523311	3344.495210	23.198541
105.700718	3350.694801	23.203559
105.743166	3362.104481	23.208576
105.933777	3361.812674	23.213594
106.181036	3360.877578	23.218611
106.081870	3367.249914	23.223629
106.357366	3357.169773	23.228647
106.058190	3373.140166	23.233664
106.554833	3365.159029	23.238682
106.375144	3364.672733	23.243699
106.551471	3382.670728	23.248717
106.472768	3385.810975	23.253735
106.434319	3386.612414	23.258752
106.738050	3393.095233	23.263770
106.502257	3389.379366	23.268787
106.545440	3405.103616	23.273805
106.684208	3413.837478	23.278823
106.879806	3423.278922	23.283840
106.983746	3433.350210	23.288858
107.477779	3447.943344	23.293875
107.313993	3437.063997	23.298893
107.752258	3438.119007	23.303911
107.629288	3447.338931	23.308928
107.963345	3458.920771	23.313946
108.159955	3469.766637	23.318963
107.963395	3465.324970	23.323981
108.417377	3469.858929	23.328999
108.318470	3479.138225	23.334016
108.584816	3479.440563	23.339034
108.531451	3473.451961	23.344051
108.393337	3468.196276	23.349069
108.792684	3478.773662	23.354087
108.746293	3489.461921	23.359104
108.956062	3492.623274	23.364122
109.340840	3487.149941	23.369139
108.800976	3492.543469	23.374157
109.234751	3486.951989	23.379175
109.273286	3499.337670	23.384192
109.653338	3501.604360	23.389210
109.580388	3502.445928	23.394227
109.432208	3513.251150	23.399245
109.753296	3513.298719	23.404263
109.670645	3519.191917	23.409280
109.661014	3533.030761	23.414298
109.559208	3539.968552	23.419315
109.793303	3543.738430	23.424333
110.539422	3541.623612	23.429351
110.102155	3562.195630	23.434368
110.266430	3567.895498	23.439386
110.300386	3558.812611	23.444403
110.649320	3575.132997	23.449421
110.791920	3587.562404	23.454439
110.993490	3588.493533	23.459456
111.417558	3590.974282	23.464474
111.544651	3593.511027	23.469491
111.491367	3588.428241	23.474509
111.658774	3590.008614	23.479527
111.582931	3590.636009	23.484544
111.787157	3606.388860	23.489562
112.111992	3604.090687	23.494579
112.221993	3608.258780	23.499597
112.291649	3607.020082	23.504615
112.233618	3603.721364	23.509632
112.187824	3602.933171	23.514650
112.436081	3601.944248	23.519667
112.369901	3609.375186	23.524685
112.795567	3619.159447	23.529703
112.687760	3623.961372	23.534720
113.087065	3624.574297	23.539738
113.141579	3622.779298	23.544755
113.178719	3635.386234	23.549773
113.093917	3636.368544	23.554791
112.787004	3632.881557	23.559808
112.963813	3650.355790	23.564826
113.317748	3660.539543	23.569843
113.531073	3653.814703	23.574861
113.754869	3669.624514	23.579879
113.788194	3678.725378	23.584896
113.932488	3687.341723	23.589914
113.741353	3675.251323	23.594931
113.897095	3691.598925	23.599949
114.310226	3700.974870	23.604967
114.279944	3703.643603	23.609984
114.345167	3708.487881	23.615002
114.643222	3703.002820	23.620019
114.753319	3715.333247	23.625037
115.242723	3715.449139	23.630055
115.102034	3731.183540	23.635072
115.202718	3717.579688	23.640090
115.650976	3711.963776	23.645107
115.224628	3723.311407	23.650125
115.552647	3712.515818	23.655143
115.680423	3713.692085	23.660160
115.881761	3718.739142	23.665178
115.900140	3733.530126	23.670195
115.509500	3735.785023	23.675213
115.785461	3738.295309	23.680231
116.055383	3746.888844	23.685248
116.151674	3735.002726	23.690266
116.071592	3738.323162	23.695283
116.402352	3750.104557	23.700301
116.876348	3758.984917	23.705319
116.902380	3755.256362	23.710336
116.634253	3757.072271	23.715354
116.669715	3754.617409	23.720371
116.868826	3758.765263	23.725389
116.953004	3773.890014	23.730407
117.523811	3781.912470	23.735424
117.204559	3775.675038	23.740442
117.451076	3783.748301	23.745459
117.033284	3788.898688	23.750477
117.500586	3801.103771	23.755495
117.464137	3810.752217	23.760512
117.568709	3814.646604	23.765530
118.122804	3826.752885	23.770547
118.245905	3841.994693	23.775565
118.412178	3836.432391	23.780583
118.337324	3835.718180	23.785600
118.380075	3846.743041	23.790618
118.904746	3843.596029	23.795635
118.781253	3847.421994	23.800653
118.748072	3850.318461	23.805671
118.998967	3850.711605	23.810688
118.927094	3850.675548	23.815706
119.150680	3867.347256	23.820723
119.222740	3882.294083	23.825741
119.320620	3869.375491	23.830759
119.589785	3883.562315	23.835776
119.700191	3902.136147	23.840794
120.036302	3897.872899	23.845811
119.768453	3908.548754	23.850829
119.852206	3905.893766	23.855847
120.159148	3915.633662	23.860864
120.078286	3926.292857	23.865882
120.360861	3928.224515	23.870899
120.692430	3941.830301	23.875917
120.545444	3947.875755	23.880935
121.115044	3950.835621	23.885952
120.868746	3956.315860	23.890970
121.123132	3950.373577	23.895987
121.276526	3956.008988	23.901005
121.187714	3974.213243	23.906023
121.877986	3977.431971	23.911040
121.638437	3980.120904	23.916058
122.003272	3982.885595	23.921075
122.196384	3972.483443	23.926093
121.896991	3978.988367	23.931111
122.071311	3978.755919	23.936128
121.969769	3986.009480	23.941146
122.193725	3987.811446	23.946163
122.437255	3997.160458	23.951181
122.599355	3998.022039	23.956199
122.889219	4004.873395	23.961216
122.914692	4005.907889	23.966234
122.993038	4016.425408	23.971251
123.087924	4018.708434	23.976269
123.288900	4012.714526	23.981287
123.243134	4021.717480	23.986304
123.026957	4020.495126	23.991322
123.398928	4035.338277	23.996339
123.422801	4042.142940	24.001357
123.348029	4042.760714	24.006375
123.962117	4056.357045	24.011392
123.763922	4069.717658	24.016410
124.212820	4072.500757	24.021427
124.473580	4083.804092	24.026445
124.145707	4074.010625	24.031463
124.246934	4077.962409	24.036480
124.041955	4088.612737	24.041498
124.576663	4094.551440	24.046515
124.790060	4097.346187	24.051533
125.117813	4090.325494	24.056551
125.721356	4096.537491	24.061568
125.756450	4098.034477	24.066586
125.483917	4097.070305	24.071603
125.477533	4105.060232	24.076621
125.872415	4112.428611	24.081639
125.900974	4107.077187	24.086656
125.701350	4126.075434	24.091674
125.872153	4114.035356	24.096691
126.046191	4125.724761	24.101709
126.182600	4140.920546	24.106727
125.966456	4138.770190	24.111744
126.302654	4145.065122	24.116762
126.146911	4144.199438	24.121779
126.380736	4170.825196	24.126797
126.485360	4168.627738	24.131815
127.434989	4160.796237	24.136832
127.536251	4171.108244	24.141850
128.039540	4171.364005	24.146867
128.389713	4168.777714	24.151885
128.221473	4164.842778	24.156903
128.237199	4153.672893	24.161920
128.083293	4149.770435	24.166938
128.091905	4139.333965	24.171955
128.492988	4156.587321	24.176973
128.532080	4168.938652	24.181991
128.674234	4179.073810	24.187008
128.296153	4179.079412	24.192026
128.618400	4180.727116	24.197043
128.787394	4171.237681	24.202061
128.662802	4166.112246	24.207079
128.740227	4176.333297	24.212096
128.890457	4190.450615	24.217114
129.024627	4196.205901	24.222131
129.142681	4204.422579	24.227149
129.075490	4218.362501	24.232167
129.313339	4215.314022	24.237184
129.582183	4224.387732	24.242202
130.231247	4212.623025	24.247219
130.470965	4219.119328	24.252237
130.585098	4220.613410	24.257255
131.021694	4221.043756	24.262272
131.078046	4225.864311	24.267290
131.296327	4217.190962	24.272307
131.294869	4217.468986	24.277325
131.512234	4210.415038	24.282343
131.347497	4191.328646	24.287360
131.325856	4196.417084	24.292378
131.493623	4205.879080	24.297395
131.461800	4207.342368	24.302413
131.592854	4215.048828	24.307431
131.859675	4218.965230	24.312448
131.631517	4223.265355	24.317466
131.512970	4214.183938	24.322483
131.539725	4227.648308	24.327501
131.509468	4240.543990	24.332519
131.815505	4238.851565	24.337536
131.875348	4258.753078	24.342554
131.680113	4275.601253	24.347571
132.374716	4288.225585	24.352589
132.227802	4299.463510	24.357607
132.375729	4305.769055	24.362624
132.448747	4316.240236	24.367642
132.565887	4325.647097	24.372659
132.544947	4335.542751	24.377677
132.567721	4359.970235	24.382695
133.055953	4359.306670	24.387712
133.175998	4378.753821	24.392730
133.512721	4388.950151	24.397747
133.917801	4394.593616	24.402765
133.298169	4403.023806	24.407783
133.729754	4410.487563	24.412800
134.097053	4419.296585	24.417818
133.707650	4425.645320	24.422835
134.187887	4438.622145	24.427853
134.176299	4451.448767	24.432871
134.693073	4458.826599	24.437888
134.669619	4484.890237	24.442906
134.787814	4472.482542	24.447923
135.249577	4487.498230	24.452941
135.627772	4497.438762	24.457959
135.768521	4498.827690	24.462976
135.680826	4501.079408	24.467994
135.789752	4491.359325	24.473011
136.007943	4497.657085	24.478029
136.266587	4519.437414	24.483047
136.377380	4522.478726	24.488064
136.736338	4508.565518	24.493082
136.581577	4510.215384	24.498099
136.968788	4513.696333	24.503117
137.020071	4515.806333	24.508135
136.993878	4506.221044	24.513152
137.421913	4514.376673	24.518170
137.237036	4522.921882	24.523187
137.385006	4520.581863	24.528205
137.500210	4523.584606	24.533223
138.320901	4513.266902	24.538240
138.185055	4513.285056	24.543258
137.862538	4515.223194	24.548275
138.389328	4521.867178	24.553293
138.585932	4524.648840	24.558311
138.550216	4531.109495	24.563328
138.785712	4543.073626	24.568346
138.851817	4536.958633	24.573363
138.956398	4537.860818	24.578381
138.861756	4543.077579	24.583399
139.147416	4539.538613	24.588416
138.979313	4542.165930	24.593434
139.165636	4557.799311	24.598451
139.417680	4560.657519	24.603469
139.731509	4561.400662	24.608487
139.897403	4564.556453	24.613504
139.595418	4568.479975	24.618522
139.689200	4582.410739	24.623539
139.983480	4582.197369	24.628557
139.738652	4597.756288	24.633575
140.172868	4598.060757	24.638592
140.149293	4606.372406	24.643610
140.215889	4613.842926	24.648627
140.699999	4633.031295	24.653645
140.275370	4644.044637	24.658663
140.632029	4653.594065	24.663680
140.887772	4666.410521	24.668698
141.067039	4664.456988	24.673715
141.548338	4677.275993	24.678733
141.777525	4696.936811	24.683751
141.879760	4692.037682	24.688768
142.119226	4693.070255	24.693786
142.033373	4699.128476	24.698803
142.307728	4693.574232	24.703821
142.132477	4696.354204	24.708839
142.205494	4709.193005	24.713856
142.539695	4720.182205	24.718874
142.862276	4718.424014	24.723891
142.958800	4717.023205	24.728909
142.664608	4742.621427	24.733927
143.149994	4739.347846	24.738944
142.950220	4743.833038	24.743962
143.257119	4750.521025	24.748979
143.339437	4756.111003	24.753997
143.781801	4768.197544	24.759015
143.789038	4769.721045	24.764032
143.816563	4776.080339	24.769050
144.078455	4793.529719	24.774067
144.407197	4793.380392	24.779085
144.099380	4802.955086	24.784103
144.671734	4811.470181	24.789120
144.629859	4812.467924	24.794138
144.518787	4821.623549	24.799155
145.281049	4816.835627	24.804173
145.016934	4826.614975	24.809191
144.978537	4841.434695	24.814208
145.235047	4849.087048	24.819226
144.978547	4853.060322	24.824243
145.583291	4870.276139	24.829261
145.803952	4874.010523	24.834279
146.077218	4887.354691	24.839296
146.445674	4897.322221	24.844314
146.445918	4901.694045	24.849331
146.764664	4904.191479	24.854349
146.743795	4907.947927	24.859367
146.521804	4908.876040	24.864384
146.727400	4925.179065	24.869402
146.922063	4913.437751	24.874419
147.688428	4918.456598	24.879437
147.820284	4932.293281	24.884455
148.688035	4917.271011	24.889472
148.721483	4899.576436	24.894490
148.889695	4897.255293	24.899507
149.159962	4881.259741	24.904525
149.320737	4886.745929	24.909543
149.342123	4884.605618	24.914560
149.206663	4884.693156	24.919578
149.039522	4882.165715	24.924595
149.799427	4867.561265	24.929613
149.144314	4873.162643	24.934631
149.365038	4870.782772	24.939648
149.456362	4872.719243	24.944666
149.481461	4878.791707	24.949683
149.534727	4876.084535	24.954701
149.389161	4878.174912	24.959719
149.388650	4887.483704	24.964736
149.780185	4905.503157	24.969754
149.915438	4907.407497	24.974771
149.776027	4915.396526	24.979789
149.602741	4935.868762	24.984807
150.192211	4955.170386	24.989824
149.956429	4960.109505	24.994842
150.086647	4973.157333	24.999859
150.430313	4982.595334	25.004877
150.366184	5002.820113	25.009895
150.745797	5017.053654	25.014912
150.965523	5024.386715	25.019930
151.023699	5048.705410	25.024947
151.519864	5041.910496	25.029965
151.505178	5063.074572	25.034983
151.731636	5074.295514	25.040000
152.108017	5068.649415	25.045018
151.712588	5078.837730	25.050035
152.333641	5091.111140	25.055053
152.107556	5104.498976	25.060071
152.561473	5104.872971	25.065088
152.963571	5122.344894	25.070106
152.927344	5125.538761	25.075123
153.063195	5126.467643	25.080141
153.225543	5138.238447	25.085159
153.410922	5147.862318	25.090176
153.913953	5156.053837	25.095194
153.629816	5160.438709	25.100211
154.020646	5152.893202	25.105229
154.159121	5167.641285	25.110247
154.261154	5180.295945	25.115264
154.325053	5180.317529	25.120282
154.478163	5196.215504	25.125299
154.831246	5200.115449	25.130317
154.941099	5197.560353	25.135335
155.010752	5210.068589	25.140352
155.265985	5217.516118	25.145370
155.527750	5232.680551	25.150387
155.483325	5230.632582	25.155405
155.164033	5242.128525	25.160423
155.298471	5244.386570	25.165440
156.035984	5257.693002	25.170458
155.271787	5263.987104	25.175475
155.665363	5283.303983	25.180493
155.975435	5309.395464	25.185511
156.064360	5313.134794	25.190528
156.668746	5318.927253	25.195546
156.918681	5338.475032	25.200563
156.792790	5339.122953	25.205581
157.116859	5350.931691	25.210599
157.278779	5359.280911	25.215616
157.876932	5365.551014	25.220634
157.573426	5372.243318	25.225651
157.987660	5366.963681	25.230669
158.006126	5375.379576	25.235687
158.303425	5397.675746	25.240704
158.628914	5389.512206	25.245722
158.385771	5394.370522	25.250739
158.479568	5407.436993	25.255757
158.973869	5412.334458	25.260775
159.213426	5412.369559	25.265792
159.557048	5421.286948	25.270810
159.279505	5440.103058	25.275827
159.486900	5446.194501	25.280845
159.140301	5447.167415	25.285863
159.241605	5454.216164	25.290880
159.637999	5464.915130	25.295898
160.058190	5469.581157	25.300915
160.339342	5488.401332	25.305933
160.234223	5497.199660	25.310951
160.416136	5495.346639	25.315968
161.102266	5500.488704	25.320986
160.969375	5513.631803	25.326003
161.355152	5510.866132	25.331021
161.510267	5518.266335	25.336039
161.406003	5525.138977	25.341056
161.602633	5536.914138	25.346074
161.998949	5541.994292	25.351091
162.230736	5532.942561	25.356109
162.197374	5539.400047	25.361127
162.468719	5544.206210	25.366144
162.596565	5544.877520	25.371162
162.663436	5557.171777	25.376179
163.073564	5563.338825	25.381197
162.884692	5553.904738	25.386215
162.947876	5558.361559	25.391232
163.215458	5562.555922	25.396250
163.055041	5585.116586	25.401267
162.978368	5584.794018	25.406285
163.343829	5590.106300	25.411303
163.265109	5599.231993	25.416320
163.606203	5602.294227	25.421338
163.616568	5620.699242	25.426355
163.972279	5641.872251	25.431373
163.972961	5652.652262	25.436391
164.041754	5673.100024	25.441408
164.210213	5672.881102	25.446426
164.920837	5696.975334	25.451443
164.936428	5702.572900	25.456461
165.337653	5705.133287	25.461479
165.218397	5720.133692	25.466496
165.518991	5721.080989	25.471514
165.443080	5740.225682	25.476531
165.677872	5750.022062	25.481549
165.655887	5755.578181	25.486567
165.884349	5773.750309	25.491584
166.044061	5787.387561	25.496602
166.224760	5790.973716	25.501619
166.820168	5798.074615	25.506637
167.257387	5807.492075	25.511655
167.100771	5802.734215	25.516672
167.566718	5807.184820	25.521690
168.017024	5816.139353	25.526707
167.702706	5823.644790	25.531725
168.391581	5826.134877	25.536743
167.971063	5824.950724	25.541760
168.791612	5817.747998	25.546778
168.469918	5831.646948	25.551795
168.565835	5844.552407	25.556813
169.082241	5840.427773	25.561831
169.037543	5847.704735	25.566848
169.368978	5841.181559	25.571866
169.197403	5851.556202	25.576883
169.468556	5860.838713	25.581901
169.558286	5873.265341	25.586919
169.409603	5873.847403	25.591936
170.144528	5885.582652	25.596954
169.730231	5899.369891	25.601971
169.847731	5894.392287	25.606989
170.417514	5908.205298	25.612007
170.608533	5929.720115	25.617024
170.940521	5911.813640	25.622042
171.481811	5909.778007	25.627059
171.518828	5913.017358	25.632077
171.603238	5926.445539	25.637095
171.516388	5939.827956	25.642112
171.593685	5934.916617	25.647130
171.409086	5944.128517	25.652147
171.211959	5953.329757	25.657165
172.110999	5957.134865	25.662183
172.106456	5976.009771	25.667200
172.416099	5985.873471	25.672218
172.662302	5997.502266	25.677236
172.625735	5998.584474	25.682253
172.749856	6009.717853	25.687271
172.902356	6021.724369	25.692288
173.066088	6024.549295	25.697306
173.408019	6042.467158	25.702324
173.301735	6049.510777	25.707341
173.773155	6053.114574	25.712359
173.593223	6068.841354	25.717376
174.197394	6070.675513	25.722394
174.282574	6072.496274	25.727412
174.491861	6082.764030	25.732429
174.721376	6087.497971	25.737447
174.848754	6102.832549	25.742464
174.950561	6100.966763	25.747482
174.731709	6107.977532	25.752500
174.731846	6115.563252	25.757517
175.608112	6112.458640	25.762535
175.588499	6142.833031	25.767552
175.571060	6149.149339	25.772570
175.825945	6159.706731	25.777588
176.268095	6168.729009	25.782605
175.932126	6182.447367	25.787623
175.982661	6188.216387	25.792640
176.264874	6200.890878	25.797658
176.543111	6211.450955	25.802676
176.465632	6232.225308	25.807693
177.063287	6234.682392	25.812711
176.922477	6255.712923	25.817728
177.004563	6262.869169	25.822746
177.703797	6276.415949	25.827764
177.889001	6289.222501	25.832781
177.742380	6288.667805	25.837799
178.429435	6306.010988	25.842816
178.502397	6311.274601	25.847834
178.719145	6316.272617	25.852852
178.757825	6326.684038	25.857869
179.496752	6325.775947	25.862887
179.255756	6340.000416	25.867904
179.428454	6345.898717	25.872922
179.572464	6358.828573	25.877940
179.661333	6368.487148	25.882957
180.012855	6367.248302	25.887975
179.935497	6386.921084	25.892992
180.206280	6393.116559	25.898010
180.648424	6395.317071	25.903028
180.710640	6420.363024	25.908045
180.982319	6415.127521	25.913063
180.937990	6427.446096	25.918080
181.011289	6431.181789	25.923098
181.786632	6434.371859	25.928116
181.656947	6442.145363	25.933133
182.022644	6434.417018	25.938151
181.816007	6452.547496	25.943168
182.004372	6462.042163	25.948186
182.434938	6467.480247	25.953204
182.233593	6487.668184	25.958221
182.365778	6491.041099	25.963239
182.429946	6505.328377	25.968256
182.659143	6516.073096	25.973274
183.338816	6523.363117	25.978292
183.314052	6547.112781	25.983309
183.332222	6549.269243	25.988327
183.366954	6556.868667	25.993344
183.501620	6574.993149	25.998362
183.634516	6584.231394	26.003380
183.928566	6608.606756	26.008397
184.447344	6613.317616	26.013415
184.813690	6627.655513	26.018432
184.997172	6634.922293	26.023450
185.096602	6634.392177	26.028468
185.456468	6653.122298	26.033485
185.530188	6648.735369	26.038503
185.885568	6655.441718	26.043520
186.049412	6655.709667	26.048538
185.915704	6666.381895	26.053556
186.302969	6678.951868	26.058573
186.370445	6686.839805	26.063591
186.472661	6688.023429	26.068608
186.316619	6697.941527	26.073626
187.060742	6711.980385	26.078644
187.053883	6701.847934	26.083661
187.408440	6729.916987	26.088679
187.361367	6737.008417	26.093696
187.547550	6729.879466	26.098714
187.844824	6734.966002	26.103732
188.367451	6762.850932	26.108749
188.629177	6761.689265	26.113767
188.474374	6766.767710	26.118784
188.568132	6762.159790	26.123802
188.832716	6785.921256	26.128820
188.838074	6791.419737	26.133837
189.231709	6784.406640	26.138855
189.158997	6805.278757	26.143872
189.300142	6808.097872	26.148890
189.423156	6830.252621	26.153908
189.402991	6840.089527	26.158925
189.675277	6856.162845	26.163943
189.797960	6868.266137	26.168960
190.029231	6883.667172	26.173978
190.639534	6894.336623	26.178996
190.431793	6902.659224	26.184013
190.780783	6913.808434	26.189031
191.042186	6931.079990	26.194048
191.170480	6936.249878	26.199066
191.713437	6942.778573	26.204084
191.810731	6953.597879	26.209101
192.267340	6948.989892	26.214119
192.704511	6969.978047	26.219136
192.444158	6966.318957	26.224154
192.852839	6963.723116	26.229172
193.211972	6973.235492	26.234189
193.290330	6987.861870	26.239207
193.687794	6997.633434	26.244224
193.651738	6988.045234	26.249242
194.190997	6986.985294	26.254260
194.218434	6994.608140	26.259277
194.480486	7009.092108	26.264295
194.386985	7017.759909	26.269312
194.447374	7020.759025	26.274330
194.567272	7015.727076	26.279348
194.764568	7032.453151	26.284365
194.972181	7030.472832	26.289383
194.732374	7045.067018	26.294400
194.872328	7054.774777	26.299418
195.371493	7064.274734	26.304436
195.513739	7086.755099	26.309453
195.587393	7094.291823	26.314471
195.692457	7107.360899	26.319488
195.791182	7116.393250	26.324506
196.533032	7128.838530	26.329524
196.491994	7140.352046	26.334541
197.129641	7153.798635	26.339559
197.129815	7175.452147	26.344576
197.192344	7180.600838	26.349594
197.779312	7179.277700	26.354612
197.788785	7197.974876	26.359629
197.845261	7200.873612	26.364647
198.199483	7204.799069	26.369664
198.139725	7215.185375	26.374682
198.723065	7224.122917	26.379700
198.646145	7231.765367	26.384717
198.463831	7246.426473	26.389735
199.108298	7252.030171	26.394752
199.363396	7262.439789	26.399770
199.439943	7271.264174	26.404788
199.254376	7279.144651	26.409805
199.645822	7282.338190	26.414823
200.112847	7296.146252	26.419840
199.983117	7305.700659	26.424858
200.320185	7316.943535	26.429876
200.640615	7337.038032	26.434893
200.411229	7336.347890	26.439911
200.762037	7349.040843	26.444928
200.873194	7373.711060	26.449946
201.199447	7378.947927	26.454964
201.259282	7394.843481	26.459981
201.357857	7406.325821	26.464999
201.720737	7422.732711	26.470016
201.814103	7427.706162	26.475034
202.153724	7442.636084	26.480052
202.130786	7451.589792	26.485069
202.463251	7479.117290	26.490087
203.035801	7472.164300	26.495104
203.274657	7485.926168	26.500122
203.943375	7486.345498	26.505140
204.066029	7487.383907	26.510157
203.923794	7493.016215	26.515175
204.175509	7506.132054	26.520192
204.480811	7509.998943	26.525210
204.716042	7508.516211	26.530228
204.596808	7528.998652	26.535245
205.138493	7546.290018	26.540263
205.109697	7544.245655	26.545280
205.068026	7555.737431	26.550298
205.256224	7567.111120	26.555316
205.310757	7586.543530	26.560333
205.450744	7597.700642	26.565351
206.052489	7619.370929	26.570368
206.198265	7637.166387	26.575386
206.279515	7632.519167	26.580404
206.714383	7653.678943	26.585421
206.578633	7660.693066	26.590439
207.013884	7681.515011	26.595456
207.130207	7698.004971	26.600474
207.440776	7715.560008	26.605492
207.723887	7728.248043	26.610509
208.047509	7737.700081	26.615527
208.230235	7743.309970	26.620544
208.230796	7750.476410	26.625562
208.338718	7761.913308	26.630580
208.816615	7777.592160	26.635597
209.027516	7798.638807	26.640615
209.118709	7803.034959	26.645632
208.767976	7818.954155	26.650650
209.160063	7827.546264	26.655668
209.352038	7853.445186	26.660685
209.537960	7867.237730	26.665703
210.114210	7874.355074	26.670720
210.532502	7886.469553	26.675738
211.167692	7885.422952	26.680756
211.335830	7896.430610	26.685773
211.917736	7893.318158	26.690791
212.126783	7888.294105	26.695808
211.879192	7890.129295	26.700826
212.314989	7901.953749	26.705844
212.642253	7918.492944	26.710861
212.853471	7929.484401	26.715879
212.948235	7915.174334	26.720896
212.965076	7920.636625	26.725914
213.349765	7925.400404	26.730932
213.005951	7947.822210	26.735949
213.318143	7934.721956	26.740967
213.374232	7945.475688	26.745984
213.587970	7963.857502	26.751002
213.561263	7969.203503	26.756020
213.677577	7983.149108	26.761037
214.008833	8002.851156	26.766055
214.577560	8009.827662	26.771072
214.840692	8026.067605	26.776090
214.856094	8030.766137	26.781108
214.995508	8045.014407	26.786125
215.189008	8061.019036	26.791143
215.813432	8062.465066	26.796160
215.697894	8071.471466	26.801178
215.807209	8086.346434	26.806196
216.075143	8089.341624	26.811213
216.260241	8110.152729	26.816231
216.547683	8117.848963	26.821248
216.954030	8135.667223	26.826266
217.116763	8145.280431	26.831284
217.292478	8149.073043	26.836301
217.279011	8163.294841	26.841319
217.666995	8161.270361	26.846336
217.414845	8183.138224	26.851354
217.775658	8194.311617	26.856372
217.963167	8222.304929	26.861389
218.138023	8232.317239	26.866407
218.466313	8250.896078	26.871424
218.810098	8273.201088	26.876442
219.088566	8282.995137	26.881460
219.758552	8283.988892	26.886477
220.408243	8293.431178	26.891495
221.157640	8282.832101	26.896512
221.476388	8286.217163	26.901530
221.643083	8284.056851	26.906548
221.909666	8284.842287	26.911565
221.806531	8280.179591	26.916583
222.022226	8278.595674	26.921600
222.433051	8282.124169	26.926618
222.315537	8276.001970	26.931636
222.282678	8279.079043	26.936653
222.289867	8277.489904	26.941671
222.651777	8277.275379	26.946688
222.121344	8286.744680	26.951706
222.333858	8301.594182	26.956724
222.693165	8312.370083	26.961741
223.053674	8331.243885	26.966759
223.287245	8331.197851	26.971776
223.202855	8350.545484	26.976794
223.489423	8362.583041	26.981812
223.441832	8376.693534	26.986829
223.539675	8396.520969	26.991847
224.062835	8416.468069	26.996864
224.234142	8450.090329	27.001882
224.282431	8458.449290	27.006900
225.412203	8454.742617	27.011917
225.353039	8461.138868	27.016935
225.352169	8466.881925	27.021952
225.806006	8488.121774	27.026970
225.581391	8502.045407	27.031988
226.100466	8523.530807	27.037005
226.159700	8538.502385	27.042023
226.550774	8544.477684	27.047040
226.274931	8567.634685	27.052058
226.677572	8575.120476	27.057076
226.898828	8601.426293	27.062093
227.158296	8624.815226	27.067111
227.762269	8634.880503	27.072128
227.529777	8650.624028	27.077146
227.957209	8663.394285	27.082164
228.219474	8676.048351	27.087181
228.408158	8689.496941	27.092199
228.595101	8703.214176	27.097216
228.651093	8719.742913	27.102234
228.708834	8732.987885	27.107252
229.309638	8747.044442	27.112269
229.252356	8769.605471	27.117287
229.710710	8781.187007	27.122304
229.683696	8799.357946	27.127322
229.850147	8818.272117	27.132340
230.106520	8822.999402	27.137357
230.397406	8852.780251	27.142375
230.371513	8865.710067	27.147392
230.432955	8885.483739	27.152410
231.002263	8911.325030	27.157428
231.576835	8926.642418	27.162445
232.610349	8927.591892	27.167463
233.027285	8929.872441	27.172480
233.327110	8936.642004	27.177498
233.472092	8931.637178	27.182516
233.950851	8933.718608	27.187533
233.963296	8932.333811	27.192551
234.326786	8949.360785	27.197568
234.400351	8955.821659	27.202586
234.532056	8960.871606	27.207604
234.532812	8955.005337	27.212621
234.537382	8966.156074	27.217639
234.594499	8983.439453	27.222656
234.700808	8993.418712	27.227674
234.802953	9010.442482	27.232692
235.763380	9012.726304	27.237709
235.528036	9043.155047	27.242727
235.801893	9048.075402	27.247744
236.231460	9057.470476	27.252762
236.559793	9068.096964	27.257780
237.166702	9075.137356	27.262797
237.023516	9089.695912	27.267815
237.117805	9101.644096	27.272832
237.232764	9115.972796	27.277850
237.745098	9127.858665	27.282868
237.870232	9132.767610	27.287885
237.775030	9155.941246	27.292903
237.951006	9172.966228	27.297920
237.889710	9187.047910	27.302938
238.512769	9212.161338	27.307956
238.682679	9213.887049	27.312973
239.049536	9239.413210	27.317991
239.190578	9254.729325	27.323008
239.139300	9265.276473	27.328026
239.487668	9290.707724	27.333044
239.903430	9302.867733	27.338061
239.927149	9334.872913	27.343079
240.681267	9341.985065	27.348096
240.881882	9355.814305	27.353114
241.022228	9372.737702	27.358132
241.550093	9387.017714	27.363149
241.490139	9397.342126	27.368167
241.521658	9414.389958	27.373184
241.895846	9420.766012	27.378202
242.167550	9442.013385	27.383220
242.391992	9459.627773	27.388237
242.521457	9467.882909	27.393255
243.074299	9478.294494	27.398272
243.449687	9500.494996	27.403290
243.481385	9513.113134	27.408308
243.716763	9519.788814	27.413325
243.685894	9542.239291	27.418343
243.787378	9563.166159	27.423360
244.356176	9576.176962	27.428378
244.405625	9598.302346	27.433396
244.605208	9612.703420	27.438413
244.629302	9630.886108	27.443431
244.798847	9643.211207	27.448448
245.131591	9660.691996	27.453466
245.369320	9679.602192	27.458484
245.587865	9692.086987	27.463501
245.832609	9706.184266	27.468519
245.949261	9733.641573	27.473536
246.548906	9754.841087	27.478554
246.500533	9771.576550	27.483572
247.078592	9785.801646	27.488589
247.263244	9811.638143	27.493607
247.752692	9819.413950	27.498624
248.146147	9847.506903	27.503642
248.028381	9852.144664	27.508660
248.571747	9874.682400	27.513677
248.821065	9893.783599	27.518695
249.082803	9907.979406	27.523712
249.355145	9914.684169	27.528730
249.643876	9934.047616	27.533748
249.827172	9948.243112	27.538765
249.985269	9967.399723	27.543783
250.376164	9978.544222	27.548800
250.697004	9989.633397	27.553818
250.664424	10013.360309	27.558836
251.137157	10020.077922	27.563853
251.496658	10052.865294	27.568871
251.322385	10061.206164	27.573888
251.984367	10078.004281	27.578906
252.122611	10082.646199	27.583924
252.635036	10094.216929	27.588941
252.845032	10119.317355	27.593959
252.739008	10120.183346	27.598976
253.101708	10143.580119	27.603994
253.149921	10160.250280	27.609012
253.838835	10170.350453	27.614029
253.648791	10188.153601	27.619047
254.141231	10203.052338	27.624064
254.598201	10220.523666	27.629082
254.526885	10235.561263	27.634100
255.140926	10249.670566	27.639117
255.470927	10263.028692	27.644135
255.611466	10284.948013	27.649152
255.896370	10280.050366	27.654170
256.047484	10306.110667	27.659188
256.370854	10312.586556	27.664205
256.675001	10335.433868	27.669223
256.976219	10346.564218	27.674240
257.211574	10356.962883	27.679258
257.235519	10378.663768	27.684276
257.577221	10381.486745	27.689293
257.954006	10395.806988	27.694311
257.563282	10410.301152	27.699328
258.548633	10425.552272	27.704346
258.513718	10452.447083	27.709364
258.781778	10455.310026	27.714381
259.112616	10483.941050	27.719399
259.333258	10495.264090	27.724416
260.159921	10510.476989	27.729434
260.068924	10522.647717	27.734452
260.549143	10532.016660	27.739469
260.702580	10553.438545	27.744487
260.732967	10551.109875	27.749504
260.925908	10564.470742	27.754522
261.100137	10581.819352	27.759540
261.552436	10594.947003	27.764557
261.645324	10605.008165	27.769575
261.801490	10620.117791	27.774592
262.166794	10627.837605	27.779610
262.159107	10644.643256	27.784628
262.662154	10660.450070	27.789645
262.643145	10676.537604	27.794663
262.712409	10695.481534	27.799680
263.002348	10701.324971	27.804698
263.001699	10733.633173	27.809716
263.508136	10747.166089	27.814733
263.757159	10771.828692	27.819751
264.064113	10794.016193	27.824768
264.278431	10800.424082	27.829786
264.198033	10835.334155	27.834804
264.961746	10855.599840	27.839821
265.193701	10870.460978	27.844839
265.552445	10899.246145	27.849856
266.319268	10905.586463	27.854874
266.542073	10921.175319	27.859892
267.126499	10931.361742	27.864909
267.323141	10939.048112	27.869927
266.947050	10945.886401	27.874944
268.043560	10971.051181	27.879962
267.983985	10974.173931	27.884980
268.293566	10993.263656	27.889997
268.540943	11004.083916	27.895015
268.775846	11023.131692	27.900032
269.029596	11017.992441	27.905050
269.508711	11038.186076	27.910068
269.710445	11047.696790	27.915085
269.830251	11055.587859	27.920103
270.055183	11072.291143	27.925120
270.518369	11079.121153	27.930138
270.765485	11107.403121	27.935156
270.612879	11110.957272	27.940173
271.161171	11129.776079	27.945191
271.272242	11136.490757	27.950208
271.659359	11150.993103	27.955226
271.771346	11181.168822	27.960244
272.125799	11190.482015	27.965261
272.590672	11202.521899	27.970279
272.588648	11230.723090	27.975296
272.991768	11248.592205	27.980314
272.814912	11265.920663	27.985332
272.981560	11272.945606	27.990349
273.662252	11301.775687	27.995367
273.441237	11316.534466	28.000384
273.843541	11338.398226	28.005402
274.585043	11358.150081	28.010420
275.285660	11357.860370	28.015437
275.916266	11372.842602	28.020455
276.053671	11388.198926	28.025472
276.607663	11384.073519	28.030490
276.450099	11396.463646	28.035508
277.052076	11407.834863	28.040525
277.445741	11421.913266	28.045543
276.993451	11427.203776	28.050560
277.795368	11432.897772	28.055578
277.733672	11449.043177	28.060596
277.918941	11455.490575	28.065613
278.178955	11463.997703	28.070631
278.429131	11469.029772	28.075648
278.439304	11484.841866	28.080666
278.647132	11495.046542	28.085684
278.631259	11514.077262	28.090701
279.162113	11529.233130	28.095719
279.468261	11549.653347	28.100736
279.679193	11569.513802	28.105754
279.804091	11589.097246	28.110772
280.356621	11600.779466	28.115789
280.416596	11615.377627	28.120807
280.557300	11637.004837	28.125824
280.825670	11654.102863	28.130842
280.868462	11671.128879	28.135860
280.990118	11697.413611	28.140877
281.621001	11718.525205	28.145895
281.405610	11745.598551	28.150912
281.868783	11760.654687	28.155930
282.374325	11788.297229	28.160948
282.786228	11816.724968	28.165965
282.808677	11841.639195	28.170983
282.821348	11864.676129	28.176000
283.608542	11896.866070	28.181018
283.831995	11915.272363	28.186036
284.037320	11940.998036	28.191053
284.561474	11956.079512	28.196071
284.345825	11982.161701	28.201088
284.886691	12000.047847	28.206106
285.731239	12024.514599	28.211124
285.692300	12040.587474	28.216141
286.191938	12056.692833	28.221159
286.472775	12088.100350	28.226176
287.006609	12098.626904	28.231194
287.275829	12112.327438	28.236212
287.558348	12127.298488	28.241229
287.881797	12140.797924	28.246247
288.071558	12165.076915	28.251264
288.476276	12181.317246	28.256282
288.608526	12201.860146	28.261300
288.758573	12215.532057	28.266317
289.187577	12232.295980	28.271335
289.011989	12253.705031	28.276352
289.827809	12274.996696	28.281370
289.924576	12291.692721	28.286388
290.037955	12319.965882	28.291405
290.386357	12334.803622	28.296423
290.511564	12362.787633	28.301440
290.742665	12384.780479	28.306458
291.251973	12399.580432	28.311476
291.520202	12428.135808	28.316493
292.117839	12434.777888	28.321511
292.222625	12463.090504	28.326528
292.597650	12479.354691	28.331546
292.691405	12500.791301	28.336564
292.792197	12521.228951	28.341581
293.053123	12541.673117	28.346599
293.438484	12575.212415	28.351616
293.678032	12597.469446	28.356634
294.547191	12616.953159	28.361652
294.888741	12630.933264	28.366669
295.440029	12638.327935	28.371687
295.884693	12655.099256	28.376704
296.183192	12668.362979	28.381722
296.539513	12676.817676	28.386740
296.406560	12702.123695	28.391757
297.311838	12693.130365	28.396775
297.019426	12717.286651	28.401792
297.332743	12733.933354	28.406810
297.739114	12754.626546	28.411828
298.160164	12772.544827	28.416845
298.261068	12780.117475	28.421863
298.205385	12800.519939	28.426880
298.560739	12824.634890	28.431898
299.034443	12831.148104	28.436916
298.758639	12856.814603	28.441933
299.470992	12878.034738	28.446951
299.788992	12896.471388	28.451968
300.008893	12912.589721	28.456986
300.243393	12917.517265	28.462004
300.429045	12942.966330	28.467021
300.740494	12953.496620	28.472039
300.789201	12980.356675	28.477056
301.444880	12999.387905	28.482074
301.736795	13023.907789	28.487092
301.745907	13045.920389	28.492109
302.185712	13064.508651	28.497127
302.369429	13088.685563	28.502144
302.537455	13107.155386	28.507162
302.539980	13135.267127	28.512180
302.929039	13156.948753	28.517197
303.331282	13179.060980	28.522215
303.564360	13212.138935	28.527232
303.801739	13239.617185	28.532250
304.461522	13263.324998	28.537268
304.563539	13293.976193	28.542285
305.104680	13324.934451	28.547303
305.082774	13355.172512	28.552320
305.330458	13374.694361	28.557338
306.002576	13398.397253	28.562356
306.396268	13420.258461	28.567373
306.594754	13447.493622	28.572391
306.993479	13472.584745	28.577408
307.621724	13482.854119	28.582426
309.251231	13467.715174	28.587444
309.552348	13484.361291	28.592461
309.916910	13491.605543	28.597479
310.212322	13510.873730	28.602496
310.221458	13494.033777	28.607514
310.833878	13494.809485	28.612532
310.725946	13500.071886	28.617549
311.780056	13511.708306	28.622567
311.254229	13520.052083	28.627584
311.771498	13526.542925	28.632602
312.307538	13534.300353	28.637620
311.986285	13560.568630	28.642637
311.882359	13562.103949	28.647655
311.992808	13582.332801	28.652672
312.337199	13599.698588	28.657690
312.294388	13626.722321	28.662708
312.848430	13650.791410	28.667725
312.643599	13660.108171	28.672743
313.005518	13702.451449	28.677760
313.315643	13727.035710	28.682778
313.895295	13756.062226	28.687796
313.773234	13790.008441	28.692813
314.129574	13819.073192	28.697831
314.524775	13848.027684	28.702848
314.756808	13879.152116	28.707866
314.847163	13906.553304	28.712884
315.449352	13940.686353	28.717901
315.830724	13959.142533	28.722919
316.027772	13998.493160	28.727936
316.422422	14026.200560	28.732954
317.187522	14045.828375	28.737972
317.121371	14077.937800	28.742989
317.625485	14103.910153	28.748007
318.097011	14129.025479	28.753024
318.042840	14162.472212	28.758042
318.408762	14180.751014	28.763060
318.650826	14211.763884	28.768077
319.091500	14234.695595	28.773095
319.297738	14270.252418	28.778112
319.608427	14296.732213	28.783130
320.035394	14330.359682	28.788148
319.924104	14352.405286	28.793165
320.553558	14377.278288	28.798183
321.245598	14400.053970	28.803200
321.433025	14431.644226	28.808218
321.822454	14448.160502	28.813236
321.794810	14477.223244	28.818253
322.093755	14495.253869	28.823271
322.536647	14522.986017	28.828288
322.828025	14558.296334	28.833306
323.436886	14571.844383	28.838324
323.930619	14605.319760	28.843341
324.202851	14620.607054	28.848359
324.748380	14643.333340	28.853376
324.591589	14665.894904	28.858394
325.227647	14686.813197	28.863412
325.582837	14715.004670	28.868429
325.952932	14732.686446	28.873447
326.216597	14758.466807	28.878464
326.159165	14788.141066	28.883482
326.412511	14812.476647	28.888500
326.980775	14834.558478	28.893517
327.090794	14858.237547	28.898535
327.667619	14884.856489	28.903552
327.923187	14908.825488	28.908570
329.227799	14914.302849	28.913588
329.936808	14928.716617	28.918605
330.670213	14944.948890	28.923623
331.277806	14941.572314	28.928640
331.293185	14958.346595	28.933658
331.861619	14948.811232	28.938676
331.637449	14948.953756	28.943693
331.895449	14964.853100	28.948711
332.104063	14966.525910	28.953728
331.999175	14988.833380	28.958746
332.227148	15007.753605	28.963764
332.319774	15026.129719	28.968781
332.512836	15042.614105	28.973799
332.606167	15061.296495	28.978816
333.095991	15096.848334	28.983834
333.581718	15121.084742	28.988852
333.866622	15146.865458	28.993869
334.264880	15176.437356	28.998887
334.622946	15203.631079	29.003904
334.706839	15230.040313	29.008922
334.856228	15259.471299	29.013940
335.240528	15286.089377	29.018957
335.298624	15311.132056	29.023975
335.636884	15328.623554	29.028992
335.587288	15367.924045	29.034010
336.224582	15404.239777	29.039028
336.189466	15438.810122	29.044045
336.725159	15467.126030	29.049063
337.065425	15503.340036	29.054080
337.337672	15550.799035	29.059098
338.122737	15582.130181	29.064116
338.312342	15612.616618	29.069133
338.894746	15641.655050	29.074151
339.447864	15668.588319	29.079168
339.587450	15698.334192	29.084186
340.227263	15723.207327	29.089204
340.640104	15753.876949	29.094221
341.140119	15775.951610	29.099239
341.908607	15794.579489	29.104256
341.779138	15820.151239	29.109274
341.904174	15828.397217	29.114292
342.414943	15868.425821	29.119309
342.748480	15892.816539	29.124327
343.136964	15916.674385	29.129344
342.849152	15937.287114	29.134362
343.378078	15961.593620	29.139380
343.812447	15990.605235	29.144397
343.901377	16017.456942	29.149415
344.476618	16037.056542	29.154432
344.454756	16069.989875	29.159450
345.128536	16087.003120	29.164468
345.436618	16123.716055	29.169485
345.256410	16152.552556	29.174503
346.129733	16174.048053	29.179520
345.988292	16218.411885	29.184538
346.579659	16243.940769	29.189556
346.795397	16272.999691	29.194573
347.043276	16307.037702	29.199591
347.531392	16345.226295	29.204608
347.796627	16370.717996	29.209626
348.497960	16397.837532	29.214644
348.753905	16432.259838	29.219661
348.913607	16460.389745	29.224679
349.393000	16484.297224	29.229696
349.557784	16522.634730	29.234714
350.058488	16556.245081	29.239732
350.716254	16597.177622	29.244749
350.637875	16627.991913	29.249767
351.014049	16647.768612	29.254784
351.289894	16683.142126	29.259802
351.912900	16719.408889	29.264820
352.672176	16759.122467	29.269837
352.795318	16782.536532	29.274855
353.099536	16797.409940	29.279872
354.426309	16806.946302	29.284890
355.839862	16812.561932	29.289908
356.130997	16817.371068	29.294925
356.438914	16820.784650	29.299943
356.375044	16841.448545	29.304960
356.992067	16852.185811	29.309978
357.145286	16858.340002	29.314996
357.097600	16874.727852	29.320013
357.471978	16892.546769	29.325031
357.810162	16910.055513	29.330048
357.693783	16937.307057	29.335066
358.083912	16950.644689	29.340084
358.368139	16979.785547	29.345101
358.293084	16999.014204	29.350119
358.646498	17015.661521	29.355136
358.750836	17055.032938	29.360154
358.985177	17102.457477	29.365172
359.679816	17125.463419	29.370189
359.861066	17155.764091	29.375207
360.154587	17187.765515	29.380224
360.457828	17221.774357	29.385242
360.948571	17249.847243	29.390260
361.325934	17283.156001	29.395277
361.492045	17323.150014	29.400295
361.938957	17351.608950	29.405312
362.228723	17390.269734	29.410330
362.907461	17415.508525	29.415348
363.231801	17455.793894	29.420365
363.305801	17474.355306	29.425383
364.003601	17508.871410	29.430400
364.335574	17547.405866	29.435418
364.790126	17575.396450	29.440436
365.238381	17605.472798	29.445453
365.432234	17635.671167	29.450471
365.931332	17655.423327	29.455488
366.044705	17693.676446	29.460506
366.661826	17715.646544	29.465524
367.327293	17755.234724	29.470541
367.402503	17777.384538	29.475559
367.830848	17801.614360	29.480576
368.252830	17825.706225	29.485594
368.612150	17847.521014	29.490612
369.348177	17871.462665	29.495629
368.950905	17909.113909	29.500647
369.825452	17913.152805	29.505664
369.904100	17944.083576	29.510682
370.539333	17960.738104	29.515700
370.591981	17978.260955	29.520717
370.499020	18020.425987	29.525735
371.265640	18046.890070	29.530752
371.249410	18090.647887	29.535770
371.563016	18117.473634	29.540788
372.476425	18145.683774	29.545805
372.472321	18187.923696	29.550823
372.492160	18213.374136	29.555840
372.924435	18256.790417	29.560858
373.377066	18295.098977	29.565876
373.777924	18331.653107	29.570893
374.147253	18369.930640	29.575911
374.537961	18393.333169	29.580928
374.899070	18445.049763	29.585946
375.427906	18476.795336	29.590964
376.042802	18507.996795	29.595981
376.586686	18559.192283	29.600999
376.734924	18583.492228	29.606016
376.839485	18612.145629	29.611034
377.484993	18652.048332	29.616052
377.940324	18695.916857	29.621069
378.557267	18726.044331	29.626087
379.008230	18747.125552	29.631104
379.068055	18777.751025	29.636122
379.899841	18812.715977	29.641140
380.420633	18834.626620	29.646157
380.425381	18866.454921	29.651175
381.407158	18889.702285	29.656192
381.528154	18908.226115	29.661210
382.551403	18930.468819	29.666228
382.807245	18948.251334	29.671245
383.030337	18983.280349	29.676263
383.623972	19001.932405	29.681280
383.740394	19023.603344	29.686298
383.898437	19043.959993	29.691316
384.749437	19059.842480	29.696333
384.675801	19092.087770	29.701351
385.578871	19113.433418	29.706368
385.504115	19145.344124	29.711386
385.630483	19166.855717	29.716404
385.954816	19189.865256	29.721421
386.362858	19226.906419	29.726439
387.078877	19257.328773	29.731456
387.341654	19293.426174	29.736474
387.778868	19316.740396	29.741492
387.841267	19351.018134	29.746509
387.841492	19384.174757	29.751527
388.417246	19404.731706	29.756544
388.611419	19438.843644	29.761562
388.793146	19472.110980	29.766580
389.600637	19508.780527	29.771597
389.604206	19548.330721	29.776615
390.334888	19588.916982	29.781632
390.521893	19627.288722	29.786650
390.456942	19671.973828	29.791668
390.990065	19705.312879	29.796685
391.816512	19749.991217	29.801703
391.838202	19783.113561	29.806720
392.570561	19819.719642	29.811738
392.998472	19859.734717	29.816756
393.355027	19879.454601	29.821773
393.902879	19923.033392	29.826791
394.138506	19946.531576	29.831808
394.574268	19983.721465	29.836826
394.651753	20006.707449	29.841844
395.537733	20036.592624	29.846861
395.809061	20081.996807	29.851879
396.014927	20110.326943	29.856896
396.674947	20147.292469	29.861914
396.755807	20188.196578	29.866932
397.292906	20211.692086	29.871949
397.503581	20252.070536	29.876967
397.847332	20278.970350	29.881984
398.729614	20316.280475	29.887002
399.098006	20353.102521	29.892020
399.637554	20391.445807	29.897037
399.404557	20422.808411	29.902055
400.528475	20447.033662	29.907072
400.911486	20481.863395	29.912090
400.933810	20513.078739	29.917108
401.307507	20544.662423	29.922125
402.016225	20583.794651	29.927143
401.885891	20620.891186	29.932160
402.821572	20644.748111	29.937178
403.056294	20681.876036	29.942196
403.514219	20718.754245	29.947213
403.643162	20759.595145	29.952231
404.386655	20792.258616	29.957248
404.673242	20829.694617	29.962266
404.867589	20869.072261	29.967284
405.317013	20906.015337	29.972301
406.231091	20943.511228	29.977319
406.580417	20974.309612	29.982336
406.671201	21008.459425	29.987354
406.825631	21043.161674	29.992372
407.872230	21063.596067	29.997389
408.453098	21106.224536	30.002407
408.772268	21133.420021	30.007424
409.469270	21159.362159	30.012442
410.029297	21188.769391	30.017460
410.038230	21203.439676	30.022477
410.568350	21247.188462	30.027495
410.997476	21273.273807	30.032512
411.672895	21299.282696	30.037530
411.663827	21339.874715	30.042548
412.221971	21359.115890	30.047565
412.835533	21381.217048	30.052583
413.020498	21410.417978	30.057600
413.313975	21447.184299	30.062618
413.725868	21485.012627	30.067636
414.319571	21507.369783	30.072653
414.385620	21541.448569	30.077671
414.571429	21566.175990	30.082688
415.156886	21607.604278	30.087706
415.471489	21643.956943	30.092724
415.712382	21677.572587	30.097741
416.380436	21719.417843	30.102759
416.543742	21741.747899	30.107776
416.999456	21791.695572	30.112794
417.199636	21836.381966	30.117812
417.565755	21871.817080	30.122829
418.071344	21908.468891	30.127847
418.486897	21950.581663	30.132864
419.199195	21984.831694	30.137882
419.602241	22018.498343	30.142900
420.073987	22042.834038	30.147917
420.854222	22084.946844	30.152935
420.853061	22111.227069	30.157952
421.467720	22145.562179	30.162970
421.744257	22172.904787	30.167988
421.905169	22212.688431	30.173005
422.140791	22244.207998	30.178023
422.515785	22288.514172	30.183040
423.012866	22324.403500	30.188058
423.072611	22367.236373	30.193076
423.522647	22407.550142	30.198093
424.087091	22450.518986	30.203111
424.580746	22479.755286	30.208128
425.625112	22518.579700	30.213146
425.716841	22561.161542	30.218164
426.538737	22589.076475	30.223181
427.131313	22629.001867	30.228199
427.148663	22658.161379	30.233216
427.776412	22686.309068	30.238234
428.202495	22732.074242	30.243252
428.961864	22754.849192	30.248269
429.166343	22792.466062	30.253287
429.019600	22829.739915	30.258304
429.950463	22859.211608	30.263322
430.030943	22909.707437	30.268340
430.591292	22931.300499	30.273357
430.801366	22982.401804	30.278375
431.258559	23017.237020	30.283392
431.930904	23059.836410	30.288410
431.807123	23107.818123	30.293428
432.305483	23141.414874	30.298445
432.891943	23189.317132	30.303463
433.175045	23228.022046	30.308480
433.946791	23274.138751	30.313498
434.517598	23316.242738	30.318516
434.831032	23355.214874	30.323533
435.009199	23398.916108	30.328551
435.325994	23447.474191	30.333568
436.121439	23483.110341	30.338586
436.796419	23532.490906	30.343604
437.080589	23567.569041	30.348621
437.461342	23604.066593	30.353639
437.860388	23654.824055	30.358656
438.679904	23692.112471	30.363674
438.700011	23732.711122	30.368692
439.251316	23764.720794	30.373709
439.512197	23809.484261	30.378727
440.136588	23847.220609	30.383744
440.469341	23895.631935	30.388762
441.021156	23935.427302	30.393780
442.216719	23952.662695	30.398797
443.219542	23979.514859	30.403815
443.742227	24005.500668	30.408832
444.563238	24017.537016	30.413850
444.860102	24047.204566	30.418868
445.391786	24058.205630	30.423885
445.996183	24076.968242	30.428903
446.381964	24097.010048	30.433920
447.309367	24099.247254	30.438938
447.618371	24119.231594	30.443956
447.907390	24135.421079	30.448973
448.339768	24145.521422	30.453991
448.155908	24172.900971	30.459008
448.521722	24189.116388	30.464026
448.713843	24215.451264	30.469044
449.312839	24247.182501	30.474061
449.331767	24258.175517	30.479079
449.400235	24302.679528	30.484096
449.997886	24329.380763	30.489114
450.327844	24371.404628	30.494132
450.468119	24399.308795	30.499149
451.214607	24435.150220	30.504167
451.038385	24477.714920	30.509184
451.790952	24502.262422	30.514202
451.704169	24553.894528	30.519220
452.448083	24592.321358	30.524237
452.608238	24647.409776	30.529255
453.005803	24683.818189	30.534272
453.436846	24718.496157	30.539290
453.819708	24762.857148	30.544308
453.872135	24811.984481	30.549325
454.480524	24863.584333	30.554343
454.723448	24919.633766	30.559360
455.410397	24972.460258	30.564378
455.624355	25031.516416	30.569396
456.073297	25081.473385	30.574413
456.752423	25134.080335	30.579431
456.777256	25199.347361	30.584448
457.254732	25242.449588	30.589466
457.699818	25310.855302	30.594484
458.832318	25366.886722	30.599501
459.412374	25412.532790	30.604519
459.827092	25477.316217	30.609536
460.343835	25527.725025	30.614554
460.725604	25572.157489	30.619572
461.013367	25628.663225	30.624589
461.472025	25678.525352	30.629607
461.996786	25730.930519	30.634624
462.399516	25781.509498	30.639642
462.752300	25833.714349	30.644660
463.564037	25892.357075	30.649677
463.920013	25948.909902	30.654695
464.109405	26004.338727	30.659712
464.947930	26041.603255	30.664730
465.494701	26103.650374	30.669748
465.988227	26158.899265	30.674765
467.136576	26199.212410	30.679783
467.333440	26250.861308	30.684800
468.022133	26293.856854	30.689818
468.758992	26328.072562	30.694836
469.276448	26377.105581	30.699853
469.893186	26414.683624	30.704871
470.004195	26458.237696	30.709888
470.754414	26504.371515	30.714906
471.056436	26537.113551	30.719924
471.890633	26583.954904	30.724941
471.919086	26613.238497	30.729959
472.347275	26661.009495	30.734976
472.690049	26702.802358	30.739994
473.043336	26748.461680	30.745012
473.555409	26795.840638	30.750029
474.089401	26833.287051	30.755047
474.071488	26886.209987	30.760064
475.148089	26929.354697	30.765082
475.353653	26958.901784	30.770100
476.169362	27007.567275	30.775117
476.639951	27049.094336	30.780135
477.084026	27087.004048	30.785152
478.100019	27135.094920	30.790170
478.287500	27165.195015	30.795188
478.813094	27208.306534	30.800205
479.028722	27252.496926	30.805223
479.485505	27302.338060	30.810240
479.957023	27336.445339	30.815258
480.718046	27382.939730	30.820276
480.548073	27421.540368	30.825293
481.044095	27453.425508	30.830311
481.208957	27509.026614	30.835328
481.961510	27552.729047	30.840346
482.769830	27598.205235	30.845364
483.170803	27640.376463	30.850381
483.792532	27677.077501	30.855399
483.856100	27733.990805	30.860416
484.364064	27759.174720	30.865434
484.797760	27799.426008	30.870452
485.275449	27853.835024	30.875469
485.581471	27898.796417	30.880487
486.579251	27945.640570	30.885504
487.055887	27975.127712	30.890522
487.649301	28016.125533	30.895540
488.106894	28048.510637	30.900557
488.839532	28086.604557	30.905575
488.954605	28138.795673	30.910592
489.230618	28175.545436	30.915610
490.004196	28224.473264	30.920628
490.364972	28272.391335	30.925645
490.885869	28314.665266	30.930663
490.941920	28373.313419	30.935680
491.459527	28414.873822	30.940698
491.956461	28476.752679	30.945716
492.287777	28526.515319	30.950733
493.237379	28573.646577	30.955751
493.788421	28621.744253	30.960768
494.245663	28670.741657	30.965786
494.560964	28714.344397	30.970804
495.226668	28767.468536	30.975821
495.584747	28822.088487	30.980839
495.900376	28872.764639	30.985856
496.418934	28918.889642	30.990874
496.794231	28975.561619	30.995892
496.998418	29034.523469	31.000909
498.382451	29086.707875	31.005927
499.142442	29113.529055	31.010944
500.259515	29155.850408	31.015962
500.485271	29191.857661	31.020980
500.955549	29235.418271	31.025997
501.412603	29277.533518	31.031015
501.967935	29331.264263	31.036032
502.256967	29364.335242	31.041050
502.540452	29405.068330	31.046068
503.028060	29467.204477	31.051085
503.575903	29509.742139	31.056103
503.945921	29557.257207	31.061120
504.181747	29600.602465	31.066138
504.943685	29654.478686	31.071156
505.011740	29699.860568	31.076173
505.807830	29749.825186	31.081191
506.210086	29809.706416	31.086208
506.510794	29868.371080	31.091226
506.625696	29923.506136	31.096244
507.023920	29982.010459	31.101261
507.811753	30043.785256	31.106279
508.089284	30106.316545	31.111296
508.396076	30171.277158	31.116314
509.276908	30232.924170	31.121332
509.762985	30293.008599	31.126349
510.076796	30350.376694	31.131367
510.360176	30408.944462	31.136384
511.127479	30472.316753	31.141402
511.995944	30529.535258	31.146420
511.989452	30607.694942	31.151437
512.938676	30658.788285	31.156455
513.981328	30721.776853	31.161472
514.322183	30762.844994	31.166490
515.288637	30814.271063	31.171508
515.407229	30858.604514	31.176525
516.321192	30902.560624	31.181543
516.733795	30967.121544	31.186560
517.123066	31012.670926	31.191578
517.624304	31057.071302	31.196596
517.923992	31107.945083	31.201613
518.768670	31149.270125	31.206631
518.739290	31210.108038	31.211648
519.326867	31250.108070	31.216666
519.881028	31301.998190	31.221684
520.100496	31365.225110	31.226701
520.675475	31414.545636	31.231719
521.022397	31477.417883	31.236736
521.300401	31532.607529	31.241754
522.035363	31586.493005	31.246772
522.359677	31656.810069	31.251789
522.968753	31722.518416	31.256807
523.628527	31785.993742	31.261824
523.710491	31848.219526	31.266842
525.402179	31892.049600	31.271860
525.639105	31948.277245	31.276877
526.408769	32007.057837	31.281895
526.817383	32059.895639	31.286912
527.508517	32113.049677	31.291930
528.232495	32155.040460	31.296948
528.560413	32216.457542	31.301965
529.217018	32266.563867	31.306983
529.691646	32322.609885	31.312000
530.016428	32384.293474	31.317018
530.946692	32431.423918	31.322036
531.298303	32487.533899	31.327053
531.745468	32537.129980	31.332071
532.086580	32585.478372	31.337088
532.622323	32652.389682	31.342106
533.384384	32695.526210	31.347124
533.856039	32768.700500	31.352141
534.480216	32807.717856	31.357159
534.881425	32880.555852	31.362176
534.956652	32933.087710	31.367194
535.766183	32986.908221	31.372212
536.318652	33057.737970	31.377229
536.490556	33121.262149	31.382247
536.860472	33184.572162	31.387264
537.338397	33244.799144	31.392282
538.103423	33316.386759	31.397300
538.692912	33384.025370	31.402317
539.248853	33445.353436	31.407335
540.171740	33509.905513	31.412352
540.319122	33568.389642	31.417370
541.399912	33630.540145	31.422388
541.606873	33691.790816	31.427405
542.379755	33742.552634	31.432423
542.953162	33793.870580	31.437440
543.831494	33850.546595	31.442458
544.920509	33893.280321	31.447476
545.902936	33931.971793	31.452493
546.804342	33972.149166	31.457511
547.848017	34006.854333	31.462528
548.211707	34036.298240	31.467546
548.955827	34059.202018	31.472564
549.167936	34102.876471	31.477581
549.748986	34130.364416	31.482599
550.024937	34162.705321	31.487616
550.543853	34206.704968	31.492634
551.305807	34247.625482	31.497652
551.555845	34278.990624	31.502669
551.814185	34320.369510	31.507687
551.966261	34361.328860	31.512704
552.111031	34412.178021	31.517722
552.809878	34448.809422	31.522740
553.129374	34505.694855	31.527757
553.070431	34555.678449	31.532775
554.024768	34609.847148	31.537792
553.912225	34669.570024	31.542810
554.476519	34719.867371	31.547828
554.794492	34782.381007	31.552845
555.633882	34847.070388	31.557863
556.063051	34905.729058	31.562880
556.586546	34967.224698	31.567898
557.241030	35025.639759	31.572916
557.763130	35091.220513	31.577933
557.986389	35159.415351	31.582951
558.823675	35227.482626	31.587968
558.946851	35297.059320	31.592986
559.624644	35367.693826	31.598004
560.327137	35434.442417	31.603021
560.741588	35503.240707	31.608039
561.614343	35570.380374	31.613056
562.314083	35643.939898	31.618074
562.821993	35704.441079	31.623092
563.202210	35771.304432	31.628109
564.171153	35847.459201	31.633127
565.117004	35907.550925	31.638144
565.385972	35975.374480	31.643162
566.478784	36026.224454	31.648180
566.228930	36101.654167	31.653197
566.867370	36168.181135	31.658215
567.641586	36226.789407	31.663232
567.944351	36298.301424	31.668250
568.371476	36366.689508	31.673268
568.634243	36444.348114	31.678285
569.276477	36511.033636	31.683303
571.631369	36547.883540	31.688320
572.880451	36600.569450	31.693338
573.570327	36634.689364	31.698356
574.410117	36687.585027	31.703373
574.898433	36721.218136	31.708391
575.753274	36756.475899	31.713408
575.925754	36807.339087	31.718426
576.586774	36842.513527	31.723444
576.681521	36884.390947	31.728461
577.514608	36933.544840	31.733479
577.866296	36972.511379	31.738496
578.054585	37026.970620	31.743514
578.522186	37071.135993	31.748532
579.060497	37124.598474	31.753549
579.075394	37179.325548	31.758567
579.993254	37228.568015	31.763584
580.361682	37289.455967	31.768602
580.834077	37344.655629	31.773620
581.481669	37416.167961	31.778637
582.241136	37475.629317	31.783655
582.489410	37535.082368	31.788672
582.602162	37593.772686	31.793690
583.442872	37661.657477	31.798708
583.973343	37725.676757	31.803725
584.440945	37794.777623	31.808743
585.303379	37857.448960	31.813760
585.715137	37930.890708	31.818778
586.565410	37985.691356	31.823796
587.280465	38054.577238	31.828813
587.705940	38116.913047	31.833831
588.175181	38175.884275	31.838848
588.692181	38246.262572	31.843866
589.588395	38310.548820	31.848884
590.315776	38376.278232	31.853901
590.270652	38435.539412	31.858919
591.079980	38494.546781	31.863936
591.297873	38554.241381	31.868954
591.941259	38612.769154	31.873972
592.479716	38684.916202	31.878989
592.740128	38755.336341	31.884007
593.467899	38808.286386	31.889024
594.317190	38881.871532	31.894042
594.712513	38945.283199	31.899060
595.774003	39015.319440	31.904077
595.885700	39090.310905	31.909095
596.287659	39157.206680	31.914112
597.185879	39226.573532	31.919130
597.501533	39295.171770	31.924148
597.940958	39370.024336	31.929165
598.611428	39449.154020	31.934183
599.290401	39516.437557	31.939200
599.660502	39599.396660	31.944218
600.161178	39675.865994	31.949236
600.385467	39746.838884	31.954253
600.922388	39841.864656	31.959271
602.018973	39910.064262	31.964288
602.433492	40007.696544	31.969306
603.208020	40090.891420	31.974324
603.818875	40163.892145	31.979341
604.558659	40251.311396	31.984359
605.609216	40329.157828	31.989376
605.847256	40407.859092	31.994394
606.532335	40482.310191	31.999412
607.386282	40569.036123	32.004429
607.607190	40651.516636	32.009447
608.627427	40712.735858	32.014464
609.813835	40783.042828	32.019482
610.411621	40843.575963	32.024500
611.023801	40920.848057	32.029517
611.183205	41000.942518	32.034535
611.944359	41071.449831	32.039552
612.484313	41166.063462	32.044570
613.077225	41231.209071	32.049588
613.393140	41310.508545	32.054605
613.822457	41396.210089	32.059623
614.491896	41471.508181	32.064640
614.812580	41563.609011	32.069658
615.303417	41649.105839	32.074676
615.937391	41731.785034	32.079693
616.349167	41820.368748	32.084711
617.363627	41908.700311	32.089728
617.904164	41999.174675	32.094746
618.518292	42085.058677	32.099764
619.894893	42161.646177	32.104781
620.267078	42239.668880	32.109799
621.083251	42313.169568	32.114816
622.163324	42397.027406	32.119834
622.634398	42470.981139	32.124852
622.967602	42550.959141	32.129869
623.935999	42624.974652	32.134887
624.793196	42693.340585	32.139904
625.469735	42770.843119	32.144922
626.499860	42839.112844	32.149940
626.897012	42895.578061	32.154957
627.654577	42981.126826	32.159975
628.233368	43036.387481	32.164992
628.976380	43097.795913	32.170010
629.813041	43171.201368	32.175028
630.177499	43235.085685	32.180045
630.872843	43298.640056	32.185063
631.749616	43352.830148	32.190080
632.198217	43417.663249	32.195098
632.318522	43488.809973	32.200116
633.029501	43544.734322	32.205133
633.538096	43619.729683	32.210151
634.117794	43677.939389	32.215168
634.448456	43749.300689	32.220186
635.103581	43822.458412	32.225204
635.355890	43883.876287	32.230221
636.079158	43965.499825	32.235239
636.618651	44027.252644	32.240256
637.025559	44114.505300	32.245274
637.424582	44199.488685	32.250292
638.586470	44263.801386	32.255309
639.260767	44347.179827	32.260327
640.148530	44418.127093	32.265344
641.041796	44481.084546	32.270362
641.718698	44559.700231	32.275380
642.390184	44619.517367	32.280397
643.010619	44688.230144	32.285415
643.971162	44766.998231	32.290432
644.037243	44836.222096	32.295450
644.634937	44901.459979	32.300468
645.529239	44977.424256	32.305485
646.248895	45058.192058	32.310503
646.979242	45132.620086	32.315520
647.538280	45206.891742	32.320538
648.529920	45270.335746	32.325556
649.232839	45348.950126	32.330573
649.370224	45424.623281	32.335591
650.400171	45494.805246	32.340608
650.695232	45569.992410	32.345626
651.322847	45651.036119	32.350644
651.948340	45724.299589	32.355661
652.444219	45802.498840	32.360679
653.007054	45881.668399	32.365696
653.501274	45969.635757	32.370714
653.885710	46062.820622	32.375732
654.677160	46143.543123	32.380749
654.980492	46239.145306	32.385767
655.773272	46322.373355	32.390784
656.366410	46406.683107	32.395802
656.836408	46496.288442	32.400820
657.570650	46597.378991	32.405837
658.523424	46693.128106	32.410855
659.360834	46777.337723	32.415872
660.230538	46863.978193	32.420890
660.882419	46942.093695	32.425908
662.143892	47025.326845	32.430925
662.502649	47108.480252	32.435943
663.231614	47187.520819	32.440960
663.937276	47280.097347	32.445978
664.504889	47347.206960	32.450996
665.994960	47409.756499	32.456013
667.126312	47476.645357	32.461031
667.576522	47541.015622	32.466048
668.583810	47608.177353	32.471066
669.054811	47685.102738	32.476084
669.959606	47737.312521	32.481101
670.549897	47808.506844	32.486119
671.643727	47857.701198	32.491136
672.359519	47919.342180	32.496154
672.785938	47980.199870	32.501172
673.092555	48041.373832	32.506189
673.658597	48109.966355	32.511207
674.112955	48179.392704	32.516224
674.400425	48238.912627	32.521242
674.948524	48310.747786	32.526260
675.560342	48390.044961	32.531277
676.334949	48471.562885	32.536295
677.070469	48537.175596	32.541312
677.477105	48618.289821	32.546330
677.698127	48686.558504	32.551348
678.452072	48763.449539	32.556365
678.847492	48840.795565	32.561383
679.353553	48924.558875	32.566400
679.924612	49000.340522	32.571418
680.563536	49093.770000	32.576436
681.130436	49186.040667	32.581453
681.637730	49281.528774	32.586471
682.333514	49379.398315	32.591488
683.122594	49463.391326	32.596506
683.517333	49557.158294	32.601524
684.255300	49642.425357	32.606541
684.785962	49738.025584	32.611559
685.331557	49836.844335	32.616576
686.048864	49938.958333	32.621594
686.717986	50033.044910	32.626612
687.995355	50130.383667	32.631629
688.628617	50235.625085	32.636647
689.104038	50330.888426	32.641664
690.042072	50425.086341	32.646682
690.935954	50525.106281	32.651700
691.526801	50613.804024	32.656717
692.029847	50710.975435	32.661735
692.803794	50801.688937	32.666752
693.338121	50904.190181	32.671770
693.916589	50999.187039	32.676788
694.819922	51106.123816	32.681805
695.550062	51201.553322	32.686823
696.412950	51301.745979	32.691840
697.310046	51395.403761	32.696858
698.008276	51488.074336	32.701876
698.746049	51584.162276	32.706893
699.571710	51684.077672	32.711911
700.396110	51776.210776	32.716928
701.702024	51854.031745	32.721946
702.688782	51930.833587	32.726964
704.030282	51995.949935	32.731981
704.786265	52072.421381	32.736999
705.499751	52154.835093	32.742016
706.099985	52232.590663	32.747034
706.561488	52298.636628	32.752052
707.305949	52375.401946	32.757069
707.986023	52458.056085	32.762087
708.631265	52527.022658	32.767104
709.453801	52612.654401	32.772122
709.698551	52686.834992	32.777140
710.478812	52771.088141	32.782157
711.267559	52847.829089	32.787175
711.784076	52928.485586	32.792192
712.783024	53016.248987	32.797210
712.831616	53105.053781	32.802228
713.618122	53187.586250	32.807245
714.106970	53278.904562	32.812263
714.909772	53355.499425	32.817280
715.709287	53455.432805	32.822298
715.821888	53557.163772	32.827316
716.501361	53649.251002	32.832333
717.223301	53750.944334	32.837351
717.623564	53850.150898	32.842368
718.346043	53951.205867	32.847386
719.193060	54057.576428	32.852404
719.785819	54154.672151	32.857421
720.568257	54248.409915	32.862439
721.125983	54368.312660	32.867456
721.975580	54472.558384	32.872474
722.332442	54581.241947	32.877492
723.400871	54670.677632	32.882509
724.141080	54772.416793	32.887527
725.076566	54859.184447	32.892544
726.096930	54951.103123	32.897562
726.620506	55043.511300	32.902580
727.251270	55133.403303	32.907597
727.789757	55219.633238	32.912615
728.320181	55323.280846	32.917632
729.139773	55433.458989	32.922650
729.589335	55534.253341	32.927668
730.143872	55633.088798	32.932685
730.928401	55739.926014	32.937703
731.577661	55850.012511	32.942720
732.560250	55941.491591	32.947738
733.016849	56066.044998	32.952756
733.878832	56167.549542	32.957773
734.601686	56273.145708	32.962791
735.657619	56390.297212	32.967808
736.821378	56492.072315	32.972826
737.220178	56590.860171	32.977844
737.295671	56693.787524	32.982861
738.206233	56813.780216	32.987879
738.927301	56920.404796	32.992896
739.950282	57027.444585	32.997914
740.997212	57133.443144	33.002932
741.926399	57235.992299	33.007949
742.931855	57340.726130	33.012967
743.654241	57449.909789	33.017984
744.665407	57547.112011	33.023002
745.200439	57654.541126	33.028020
745.975988	57748.958262	33.033037
746.777167	57847.992062	33.038055
747.215008	57956.849150	33.043072
748.033589	58061.919178	33.048090
749.054355	58158.451457	33.053108
749.896118	58264.879529	33.058125
750.890740	58359.568548	33.063143
751.690542	58463.978682	33.068160
752.138639	58557.507176	33.073178
752.442575	58665.584584	33.078196
753.155895	58775.357946	33.083213
754.032462	58883.992255	33.088231
754.496755	58995.425948	33.093248
755.379510	59104.161543	33.098266
756.397537	59209.262269	33.103284
756.933895	59311.533602	33.108301
757.993192	59420.072061	33.113319
758.820656	59539.711501	33.118336
759.636831	59640.674469	33.123354
760.214530	59745.814811	33.128372
760.829021	59849.152206	33.133389
761.643271	59953.553800	33.138407
762.499896	60066.481729	33.143424
763.685587	60185.770732	33.148442
764.262784	60289.793114	33.153460
764.739456	60389.419772	33.158477
765.434305	60497.982104	33.163495
766.254115	60611.937419	33.168512
767.018770	60719.730210	33.173530
767.958823	60833.053716	33.178548
768.838853	60931.897792	33.183565
770.098032	61031.094342	33.188583
770.735354	61141.706788	33.193600
771.615408	61230.215098	33.198618
772.247837	61336.012000	33.203636
773.160383	61431.333455	33.208653
774.016132	61528.930362	33.213671
774.942458	61624.218753	33.218688
776.064399	61719.869350	33.223706
776.654809	61807.861699	33.228724
777.323823	61896.405442	33.233741
778.292795	61978.648235	33.238759
778.622291	62069.233463	33.243776
779.879941	62145.829308	33.248794
780.417308	62234.622765	33.253812
781.036600	62324.201334	33.258829
781.591261	62411.941880	33.263847
782.108972	62508.677676	33.268864
783.268815	62602.977372	33.273882
783.623399	62701.436014	33.278900
784.658796	62798.338758	33.283917
785.600475	62881.943536	33.288935
786.258495	62991.250579	33.293952
787.291714	63075.772258	33.298970
788.105234	63170.698084	33.303988
788.643670	63269.870855	33.309005
789.560034	63368.896210	33.314023
789.991094	63470.903714	33.319040
791.201605	63570.143361	33.324058
791.374450	63667.583379	33.329076
791.988544	63773.653078	33.334093
793.060194	63887.558670	33.339111
793.432941	64004.328108	33.344128
794.064257	64106.059937	33.349146
794.798518	64228.452530	33.354164
795.582919	64344.715929	33.359181
796.104762	64464.224407	33.364199
796.878787	64584.485327	33.369216
797.794552	64711.017588	33.374234
798.391179	64839.601047	33.379252
798.915903	64958.953143	33.384269
799.919049	65082.700600	33.389287
800.592332	65225.645488	33.394304
801.466514	65346.825021	33.399322
802.346093	65476.994507	33.404340
803.167359	65612.453991	33.409357
804.565573	65726.816915	33.414375
805.054034	65856.397478	33.419392
806.308824	65979.058923	33.424410
807.677418	66101.120660	33.429428
808.395912	66216.041747	33.434445
809.470146	66302.619179	33.439463
810.333310	66419.696514	33.444480
810.941540	66540.638475	33.449498
811.860354	66653.909328	33.454516
812.585538	66767.090706	33.459533
813.415147	66864.034965	33.464551
814.157947	66981.551601	33.469568
815.348410	67099.714142	33.474586
815.710136	67215.411056	33.479604
815.988375	67322.244662	33.484621
817.241055	67450.137076	33.489639
817.762177	67568.640860	33.494656
818.911652	67686.711218	33.499674
819.341287	67803.324571	33.504692
820.356782	67930.123138	33.509709
821.171307	68043.118866	33.514727
822.198991	68167.915854	33.519744
822.371580	68280.987817	33.524762
823.731918	68408.196961	33.529780
824.193004	68528.576128	33.534797
824.948633	68657.071584	33.539815
825.450324	68799.436438	33.544832
826.444134	68908.190791	33.549850
827.563024	69040.677408	33.554868
828.155171	69167.250731	33.559885
829.062068	69278.306116	33.564903
829.449448	69403.810874	33.569920
830.411562	69523.546314	33.574938
831.591395	69626.638948	33.579956
832.429537	69752.701689	33.584973
833.506883	69864.727042	33.589991
834.742017	69976.791492	33.595008
835.872799	70070.977765	33.600026
836.636251	70175.328237	33.605044
837.834063	70286.399359	33.610061
838.792917	70395.545343	33.615079
839.132535	70503.104336	33.620096
839.867950	70596.480544	33.625114
840.912688	70719.203756	33.630132
841.802043	70822.903854	33.635149
842.812938	70939.376935	33.640167
843.140855	71051.005457	33.645184
843.961526	71169.117800	33.650202
844.686079	71276.518364	33.655220
845.011024	71400.978606	33.660237
846.419229	71515.352931	33.665255
847.092455	71628.677634	33.670272
848.027346	71751.017573	33.675290
848.974639	71861.893946	33.680308
849.582764	71988.478401	33.685325
850.341736	72111.366838	33.690343
851.065605	72235.236593	33.695360
851.868057	72365.782080	33.700378
852.756890	72484.826893	33.705396
853.841116	72618.166618	33.710413
854.550888	72735.429388	33.715431
855.011761	72873.605019	33.720448
855.954913	73004.878904	33.725466
856.633506	73132.483721	33.730484
857.209091	73268.300225	33.735501
858.331012	73409.300986	33.740519
859.116779	73548.341202	33.745536
859.980119	73677.591636	33.750554
861.178872	73820.634472	33.755572
861.846067	73958.175425	33.760589
862.972793	74095.214468	33.765607
863.906196	74241.771714	33.770624
864.526392	74376.573534	33.775642
865.599853	74500.196398	33.780660
866.068811	74646.347242	33.785677
867.083830	74784.091294	33.790695
867.983963	74924.982752	33.795712
869.102138	75060.710703	33.800730
870.153083	75192.865108	33.805748
870.908986	75335.402666	33.810765
871.517173	75465.461668	33.815783
872.465516	75615.342824	33.820800
873.153804	75756.373124	33.825818
874.235278	75895.037140	33.830836
874.976776	76038.467362	33.835853
875.911003	76177.054536	33.840871
876.943913	76311.814046	33.845888
877.773194	76473.233340	33.850906
878.689910	76609.025920	33.855924
879.073883	76748.031517	33.860941
880.270530	76883.933646	33.865959
881.115853	77027.492160	33.870976
881.991511	77177.912680	33.875994
883.096409	77305.533795	33.881012
883.927391	77452.428457	33.886029
885.001686	77589.670722	33.891047
885.945807	77732.660064	33.896064
886.692586	77869.929676	33.901082
888.454498	77989.343435	33.906100
889.972874	78087.918445	33.911117
891.568693	78194.209388	33.916135
892.719934	78290.334272	33.921152
893.704944	78390.767461	33.926170
894.274566	78487.148792	33.931188
894.922721	78593.348958	33.936205
895.648300	78687.502240	33.941223
896.488885	78795.953401	33.946240
896.805937	78910.175206	33.951258
897.406826	79019.741613	33.956276
898.128297	79149.661008	33.961293
898.992556	79268.422721	33.966311
899.930467	79391.721550	33.971328
900.414668	79510.163738	33.976346
902.425272	79617.636764	33.981364
903.316274	79741.451249	33.986381
904.857175	79848.124547	33.991399
905.298685	79971.110926	33.996416
906.010075	80068.349720	34.001434
907.327173	80178.771408	34.006452
907.831381	80300.685202	34.011469
908.777904	80420.617192	34.016487
909.383792	80538.335202	34.021504
910.122422	80665.864449	34.026522
911.633083	80778.931462	34.031540
912.349751	80888.461740	34.036557
913.246736	81009.873680	34.041575
914.161319	81138.682497	34.046592
914.655433	81264.478987	34.051610
915.680475	81391.763965	34.056628
916.119005	81524.640080	34.061645
917.109471	81657.430399	34.066663
917.930754	81801.676175	34.071680
918.171172	81935.041359	34.076698
919.352375	82071.376716	34.081716
920.042161	82222.689817	34.086733
921.025096	82371.018324	34.091751
921.639493	82515.249444	34.096768
922.431485	82669.082984	34.101786
923.417412	82817.045908	34.106804
923.744515	82977.948001	34.111821
924.871794	83130.578517	34.116839
926.009070	83292.914014	34.121856
926.326858	83454.821233	34.126874
927.297053	83617.944980	34.131892
928.355057	83778.825832	34.136909
929.205975	83946.937114	34.141927
930.117874	84113.544649	34.146944
931.063095	84281.060252	34.151962
932.497186	84447.385221	34.156980
933.052263	84615.267963	34.161997
934.510842	84754.157620	34.167015
936.144773	84901.155514	34.172032
937.238601	85060.618725	34.177050
938.889548	85201.165715	34.182068
939.836252	85346.017945	34.187085
940.810968	85496.378675	34.192103
941.461306	85630.393793	34.197120
942.171067	85779.796411	34.202138
943.271742	85923.917796	34.207156
943.964427	86071.778622	34.212173
945.034245	86212.674936	34.217191
945.949699	86356.421958	34.222208
946.626007	86510.813658	34.227226
947.536402	86652.649444	34.232244
948.568306	86802.729168	34.237261
949.240169	86958.720623	34.242279
950.285536	87107.709984	34.247296
950.837196	87252.861632	34.252314
951.964281	87399.343214	34.257332
952.885724	87548.823094	34.262349
953.599882	87688.236136	34.267367
954.641602	87838.978586	34.272384
955.248719	87999.307062	34.277402
955.934373	88147.990494	34.282420
957.091699	88308.057076	34.287437
958.104691	88459.073313	34.292455
958.813595	88611.189787	34.297472
959.359067	88779.959668	34.302490
960.478920	88943.165785	34.307508
961.616977	89116.876022	34.312525
961.982171	89285.233429	34.317543
963.828479	89447.276681	34.322560
964.326999	89634.688556	34.327578
965.015772	89794.418265	34.332596
966.023299	89965.061538	34.337613
966.986573	90144.622271	34.342631
968.032394	90317.872321	34.347648
968.867813	90498.012824	34.352666
970.282274	90666.340431	34.357684
971.333180	90843.230100	34.362701
971.903617	91017.661234	34.367719
973.172581	91188.739442	34.372736
974.092692	91364.778130	34.377754
975.036495	91554.971230	34.382772
975.925332	91741.511254	34.387789
977.252770	91916.614837	34.392807
978.352412	92083.035078	34.397824
979.277731	92267.646098	34.402842
980.438004	92453.539605	34.407860
981.563632	92627.411406	34.412877
982.484355	92809.199964	34.417895
983.849271	92967.965970	34.422912
984.757139	93141.063592	34.427930
985.855459	93306.349951	34.432948
987.305858	93472.355250	34.437965
987.966526	93632.540478	34.442983
989.364476	93805.793256	34.448000
990.368286	93975.546978	34.453018
991.251973	94137.258957	34.458036
992.398173	94299.386991	34.463053
993.148267	94460.208945	34.468071
994.927224	94621.605823	34.473088
995.446631	94788.955445	34.478106
997.079200	94941.504019	34.483124
998.517019	95091.536020	34.488141
1000.431263	95214.849766	34.493159
1002.441131	95343.193987	34.498176
1003.337896	95483.602944	34.503194
1004.346122	95601.647492	34.508212
1005.516789	95719.312125	34.513229
1006.359017	95851.339806	34.518247
1007.182000	95975.816138	34.523264
1008.037610	96097.448412	34.528282
1008.479262	96235.333393	34.533300
1009.322448	96364.181367	34.538317
1009.906797	96498.571882	34.543335
1011.105910	96643.337340	34.548352
1011.719198	96793.886869	34.553370
1012.458813	96934.948050	34.558388
1013.016791	97085.520302	34.563405
1013.644019	97249.088557	34.568423
1014.312719	97406.756539	34.573440
1015.166702	97573.460114	34.578458
1016.186130	97738.097703	34.583476
1016.782352	97903.017909	34.588493
1018.118285	98071.207878	34.593511
1019.054617	98229.053532	34.598528
1019.775015	98391.396077	34.603546
1020.759559	98554.839023	34.608564
1021.934869	98712.928542	34.613581
1022.939487	98889.617648	34.618599
1023.587034	99038.448309	34.623616
1024.609197	99220.093288	34.628634
1025.839436	99388.889870	34.633652
1026.512934	99562.021449	34.638669
1027.650114	99731.886622	34.643687
1028.997803	99899.539183	34.648704
1029.944881	100075.178869	34.653722
1031.133139	100247.523569	34.658740
1032.625693	100408.715797	34.663757
1033.741397	100572.541429	34.668775
1035.159425	100727.014962	34.673792
1036.111638	100891.159385	34.678810
1036.991897	101056.748515	34.683828
1038.174427	101227.730066	34.688845
1039.136077	101388.528486	34.693863
1040.280082	101556.094676	34.698880
1041.417467	101723.142948	34.703898
1042.506413	101896.259909	34.708916
1043.184278	102058.209053	34.713933
1044.088949	102233.156970	34.718951
1044.987386	102403.365008	34.723968
1046.055504	102579.011844	34.728986
1047.164436	102754.399646	34.734004
1047.954956	102931.270928	34.739021
1048.866197	103122.400613	34.744039
1050.247962	103302.287615	34.749056
1050.882053	103489.430907	34.754074
1052.141889	103676.451920	34.759092
1052.618952	103857.827537	34.764109
1053.699169	104048.974108	34.769127
1054.898684	104243.463094	34.774144
1055.739802	104438.021997	34.779162
1057.085922	104629.472583	34.784180
1058.358799	104821.924723	34.789197
1059.666527	105013.142588	34.794215
1060.661640	105198.945564	34.799232
1062.699784	105365.046871	34.804250
1064.596744	105529.865084	34.809268
1066.002250	105687.913949	34.814285
1067.224727	105862.044908	34.819303
1068.163610	106024.783865	34.824320
1069.094777	106184.456250	34.829338
1069.883836	106346.370638	34.834356
1071.012043	106511.491482	34.839373
1071.567834	106687.924689	34.844391
1072.853780	106849.712944	34.849408
1073.689824	107035.652276	34.854426
1074.399981	107212.482460	34.859444
1075.137622	107386.874605	34.864461
1076.319186	107569.770144	34.869479
1077.092690	107753.821067	34.874496
1078.303908	107933.404261	34.879514
1079.344232	108113.814024	34.884532
1080.431985	108306.149897	34.889549
1081.300037	108494.881831	34.894567
1082.561296	108677.770737	34.899584
1083.551434	108862.161359	34.904602
1084.449745	109047.239426	34.909620
1085.632520	109239.464120	34.914637
1086.444869	109436.756926	34.919655
1087.575982	109617.375826	34.924672
1088.617664	109803.792331	34.929690
1089.858705	109992.347125	34.934708
1090.578637	110176.457238	34.939725
1091.711055	110366.578172	34.944743
1093.333642	110543.409189	34.949760
1094.612113	110722.615701	34.954778
1095.686187	110889.972369	34.959796
1096.887599	111064.018538	34.964813
1097.799552	111255.535697	34.969831
1098.508158	111427.923385	34.974848
1099.210350	111610.128737	34.979866
1101.395203	111786.801813	34.984884
1102.588176	111957.569016	34.989901
1103.760337	112149.735055	34.994919
1105.331305	112324.097281	34.999936
1106.304645	112496.702303	35.004954
1106.974434	112674.885168	35.009972
1108.417008	112864.526949	35.014989
1109.005470	113046.059844	35.020007
1109.768052	113222.112905	35.025024
1110.827088	113408.532806	35.030042
1111.621953	113607.018172	35.035060
1112.516451	113812.502565	35.040077
1113.675223	114014.788726	35.045095
1114.533340	114215.119182	35.050112
1115.521977	114424.409817	35.055130
1116.699322	114637.388222	35.060148
1117.783656	114848.226298	35.065165
1118.834991	115055.316534	35.070183
1120.004884	115267.310461	35.075200
1121.281221	115480.024571	35.080218
1122.442316	115698.452776	35.085236
1123.987624	115893.459216	35.090253
1124.755399	116110.505507	35.095271
1126.121067	116316.018866	35.100288
1127.705428	116516.527127	35.105306
1128.652457	116740.715280	35.110324
1129.702542	116937.948255	35.115341
1130.929485	117142.359010	35.120359
1132.370646	117352.876361	35.125376
1133.764879	117565.114575	35.130394
1134.781090	117760.822397	35.135412
1136.342745	117956.509261	35.140429
1137.394414	118161.003705	35.145447
1138.711928	118367.842274	35.150464
1139.618484	118562.848395	35.155482
1140.751138	118766.052293	35.160500
1142.021546	118954.318771	35.165517
1143.143786	119161.585431	35.170535
1144.382855	119370.788350	35.175552
1145.650487	119569.827515	35.180570
1146.349538	119779.383575	35.185588
1147.526361	119965.830374	35.190605
1148.620186	120184.345721	35.195623
1149.735722	120378.402341	35.200640
1151.090343	120581.847457	35.205658
1152.294871	120786.167035	35.210676
1153.399851	120989.754847	35.215693
1154.859025	121187.440394	35.220711
1155.825696	121392.028714	35.225728
1157.141506	121602.982222	35.230746
1157.853261	121806.610470	35.235764
1159.663757	121999.906708	35.240781
1160.887630	122192.788311	35.245799
1161.966918	122395.753160	35.250816
1163.373721	122592.794322	35.255834
1164.213986	122794.872583	35.260852
1165.720271	122986.813156	35.265869
1166.887835	123180.837417	35.270887
1167.778517	123370.415160	35.275904
1168.724455	123552.868330	35.280922
1169.465339	123744.424933	35.285940
1170.241237	123939.617874	35.290957
1171.161152	124137.960752	35.295975
1172.351949	124342.021736	35.300992
1173.359015	124553.026533	35.306010
1174.446014	124767.001208	35.311028
1175.204275	124973.822598	35.316045
1176.307791	125192.262544	35.321063
1177.627540	125413.739954	35.326080
1178.998801	125619.225380	35.331098
1179.524588	125852.095167	35.336116
1180.922313	126057.667459	35.341133
1182.042396	126296.891599	35.346151
1182.919660	126528.543012	35.351168
1184.008037	126763.144110	35.356186
1185.192747	127002.387599	35.361204
1186.510983	127230.472291	35.366221
1187.670234	127468.973917	35.371239
1188.952469	127700.606544	35.376256
1190.273368	127946.253887	35.381274
1191.738531	128182.973541	35.386292
1192.658818	128420.008204	35.391309
1193.781651	128660.349316	35.396327
1194.929131	128909.137884	35.401344
1196.634634	129134.393732	35.406362
1197.861653	129380.520897	35.411380
1198.983451	129624.293338	35.416397
1200.290001	129861.745057	35.421415
1201.426469	130095.595966	35.426432
1202.966364	130339.852624	35.431450
1204.411199	130587.284892	35.436468
1205.507410	130817.263477	35.441485
1206.652829	131054.823154	35.446503
1207.800756	131304.183876	35.451520
1209.591627	131522.231956	35.456538
1210.542804	131768.339855	35.461556
1211.516723	132000.856177	35.466573
1213.046905	132246.190951	35.471591
1213.942273	132488.923793	35.476608
1215.028854	132726.654060	35.481626
1216.182023	132975.122600	35.486644
1218.387458	133198.329230	35.491661
1219.829275	133418.877654	35.496679
1221.120686	133667.962891	35.501696
1222.592496	133889.321053	35.506714
1223.831894	134122.263802	35.511732
1225.556918	134337.899821	35.516749
1226.869791	134552.332474	35.521767
1228.186656	134781.637400	35.526784
1229.536962	134993.198511	35.531802
1230.552153	135214.050983	35.536820
1231.849639	135425.292461	35.541837
1232.760485	135658.383419	35.546855
1233.546377	135879.414611	35.551872
1234.357445	136099.224723	35.556890
1235.842146	136342.850613	35.561908
1237.100831	136571.450369	35.566925
1237.899271	136800.605526	35.571943
1239.238659	137041.910245	35.576960
1240.467398	137271.850609	35.581978
1242.144619	137501.975711	35.586996
1243.818164	137716.214488	35.592013
1245.241881	137938.044021	35.597031
1246.334180	138164.736094	35.602048
1248.595148	138360.345425	35.607066
1249.886354	138571.056623	35.612084
1251.392914	138778.118285	35.617101
1252.248767	138957.224098	35.622119
1253.725580	139152.718362	35.627136
1254.828261	139336.774348	35.632154
1256.028469	139535.651112	35.637172
1257.032962	139736.843666	35.642189
1257.921108	139933.727746	35.647207
1259.052059	140141.882111	35.652224
1260.039746	140344.399697	35.657242
1260.809148	140560.315812	35.662260
1262.002420	140776.598036	35.667277
1262.785928	140988.021264	35.672295
1263.681446	141226.675591	35.677312
1265.217437	141455.699797	35.682330
1265.893667	141710.622780	35.687348
1267.081531	141940.376394	35.692365
1268.214579	142198.758581	35.697383
1269.118157	142453.243720	35.702400
1270.493045	142701.171067	35.707418
1271.481706	142955.747012	35.712436
1272.438793	143212.715225	35.717453
1273.793761	143479.851949	35.722471
1275.020328	143748.672819	35.727488
1276.350709	144013.734808	35.732506
1277.555812	144293.197674	35.737524
1278.358719	144566.823306	35.742541
1279.660179	144838.925491	35.747559
1280.956488	145121.780116	35.752576
1282.444462	145392.840709	35.757594
1283.880446	145672.655802	35.762612
1285.192124	145956.731100	35.767629
1286.829659	146233.458866	35.772647
1287.721897	146515.140589	35.777664
1289.420020	146795.301521	35.782682
1290.682381	147083.274629	35.787700
1291.971852	147357.130899	35.792717
1293.651785	147635.395304	35.797735
1294.764589	147918.243190	35.802752
1296.044364	148203.363857	35.807770
1297.507517	148482.517086	35.812788
1298.707126	148769.823831	35.817805
1300.171649	149051.454957	35.822823
1300.973693	149345.135458	35.827840
1302.765525	149627.365722	35.832858
1304.083667	149897.943082	35.837876
1306.015475	150173.998085	35.842893
1307.841841	150447.176915	35.847911
1309.546597	150717.482056	35.852928
1311.057642	150980.824755	35.857946
1312.894222	151250.921492	35.862964
1314.364238	151504.994156	35.867981
1315.229043	151761.231789	35.872999
1316.390372	152021.029201	35.878016
1318.048157	152274.657107	35.883034
1318.800758	152540.664700	35.888052
1320.119277	152799.095579	35.893069
1321.375196	153062.043793	35.898087
1322.402913	153330.500066	35.903104
1323.432336	153597.281728	35.908122
1325.074154	153855.387555	35.913140
1326.433252	154132.338882	35.918157
1327.721975	154403.920204	35.923175
1329.014341	154662.630220	35.928192
1330.566276	154936.787877	35.933210
1331.588325	155197.726028	35.938228
1332.847453	155475.549969	35.943245
1334.258624	155743.322750	35.948263
1335.642465	156012.319713	35.953280
1337.009536	156267.889594	35.958298
1338.422842	156517.232940	35.963316
1339.007680	156778.373494	35.968333
1340.418968	157036.097871	35.973351
1341.938668	157301.639121	35.978368
1343.361559	157565.952598	35.983386
1344.395463	157835.241079	35.988404
1346.090636	158103.437037	35.993421
1347.278793	158365.619901	35.998439
1348.104985	158630.018726	36.003456
1349.611056	158900.532917	36.008474
1350.922232	159181.450830	36.013492
1351.904597	159449.573834	36.018509
1353.613084	159732.247487	36.023527
1354.748471	160025.485860	36.028544
1355.977317	160301.699027	36.033562
1357.059504	160595.303867	36.038580
1358.258237	160887.368358	36.043597
1360.063975	161171.417090	36.048615
1361.816753	161460.096620	36.053632
1362.852272	161741.907051	36.058650
1364.618531	162035.157541	36.063668
1365.514457	162322.388091	36.068685
1367.478359	162618.390690	36.073703
1368.558068	162908.477043	36.078720
1369.919962	163201.656439	36.083738
1371.365774	163491.738851	36.088756
1372.819811	163790.835530	36.093773
1374.285285	164094.680157	36.098791
1375.640052	164394.442597	36.103808
1377.005428	164704.488755	36.108826
1378.431303	165000.065668	36.113844
1379.596011	165298.389098	36.118861
1380.848511	165610.450416	36.123879
1382.086145	165913.450133	36.128896
1383.513674	166217.018203	36.133914
1384.637253	166519.619449	36.138932
1386.115595	166850.112004	36.143949
1387.859945	167145.394357	36.148967
1389.243179	167453.126601	36.153984
1390.498299	167759.661336	36.159002
1391.954551	168071.041546	36.164020
1393.611381	168368.983673	36.169037
1395.867547	168663.278048	36.174055
1397.388301	168963.046920	36.179072
1398.972854	169252.116030	36.184090
1400.599479	169539.008477	36.189108
1402.203744	169834.857123	36.194125
1403.622561	170120.387670	36.199143
1405.057178	170404.101123	36.204160
1406.240241	170696.273419	36.209178
1407.558805	170981.403949	36.214196
1409.255782	171275.682027	36.219213
1410.848288	171570.193462	36.224231
1411.894806	171863.826481	36.229248
1413.302760	172158.737308	36.234266
1414.902835	172444.654613	36.239284
1416.151914	172722.247398	36.244301
1417.751717	173007.468448	36.249319
1419.190222	173299.598019	36.254336
1420.661528	173589.983932	36.259354
1422.020926	173879.067843	36.264372
1423.464394	174160.051030	36.269389
1425.047758	174439.032417	36.274407
1426.523932	174731.859754	36.279424
1427.615732	175015.351707	36.284442
1428.856005	175307.722823	36.289460
1430.366111	175598.313096	36.294477
1431.499471	175873.788952	36.299495
1432.510195	176163.786376	36.304512
1433.844431	176446.877070	36.309530
1434.722930	176731.767036	36.314548
1435.862918	177027.258320	36.319565
1437.410961	177321.467713	36.324583
1438.870768	177629.126965	36.329600
1439.874078	177938.357204	36.334618
1441.378689	178256.957853	36.339636
1442.516701	178556.492875	36.344653
1443.916889	178866.146847	36.349671
1445.196077	179185.319509	36.354688
1446.247925	179507.982974	36.359706
1447.690477	179833.481788	36.364724
1448.953791	180161.168646	36.369741
1450.323425	180500.548461	36.374759
1451.750279	180848.454297	36.379776
1452.580160	181183.755861	36.384794
1454.422010	181526.087921	36.389812
1455.854071	181880.905115	36.394829
1457.211536	182229.207950	36.399847
1458.919574	182575.679303	36.404864
1460.074468	182922.797256	36.409882
1462.209360	183279.287550	36.414900
1463.565505	183623.862055	36.419917
1464.764901	183982.126853	36.424935
1466.700919	184326.206675	36.429952
1468.406923	184685.994850	36.434970
1469.890901	185035.583241	36.439988
1471.365968	185390.939837	36.445005
1473.040979	185746.367969	36.450023
1474.570615	186101.794679	36.455040
1476.069340	186453.061935	36.460058
1477.623974	186844.833810	36.465076
1479.359796	187226.317335	36.470093
1480.768612	187574.554420	36.475111
1482.315461	187930.213149	36.480128
1483.940892	188284.489144	36.485146
1485.627817	188627.555288	36.490164
1487.105592	188984.244220	36.495181
1488.507719	189332.614899	36.500199
1490.444562	189684.636776	36.505216
1491.712723	190027.010705	36.510234
1494.457181	190354.727211	36.515252
1495.804617	190696.963701	36.520269
1497.517210	191020.855709	36.525287
1498.954288	191359.473217	36.530304
1500.494283	191700.260019	36.535322
1502.317445	192020.581329	36.540340
1503.639675	192354.241054	36.545357
1505.256869	192686.128257	36.550375
1506.791691	193023.134803	36.555392
1507.817813	193365.683064	36.560410
1509.096436	193697.752913	36.565428
1510.273674	194045.334127	36.570445
1511.314137	194381.684974	36.575463
1512.981202	194734.804995	36.580480
1514.309203	195095.497789	36.585498
1515.817412	195434.114989	36.590516
1516.792139	195789.810050	36.595533
1518.902715	196148.859053	36.600551
1520.285855	196496.896964	36.605568
1521.656818	196853.777382	36.610586
1523.632242	197209.649623	36.615604
1525.231564	197563.854283	36.620621
1526.873349	197917.316497	36.625639
1528.290557	198271.576751	36.630656
1529.792106	198614.266778	36.635674
1531.539758	198945.107153	36.640692
1532.654992	199284.963313	36.645709
1533.910503	199624.798252	36.650727
1535.422675	199968.785093	36.655744
1536.503074	200313.627710	36.660762
1537.986209	200666.104890	36.665780
1539.240396	201022.911633	36.670797
1540.767859	201373.960840	36.675815
1542.124116	201744.190949	36.680832
1543.358135	202108.598422	36.685850
1545.249863	202466.197457	36.690868
1546.326292	202842.417845	36.695885
1548.136841	203203.612801	36.700903
1550.140818	203572.475185	36.705920
1551.632089	203940.859676	36.710938
1553.395544	204294.062254	36.715956
1555.476516	204662.279621	36.720973
1557.185337	205028.574497	36.725991
1558.978820	205388.734698	36.731008
1560.869305	205748.727931	36.736026
1562.860875	206093.921449	36.741044
1564.447318	206437.934186	36.746061
1566.320318	206789.421916	36.751079
1568.394601	207144.130296	36.756096
1569.313074	207498.588273	36.761114
1570.883006	207844.231560	36.766132
1572.755667	208198.261835	36.771149
1574.250908	208551.335574	36.776167
1575.838446	208892.938509	36.781184
1577.322247	209249.520685	36.786202
1578.559700	209592.474926	36.791220
1580.537081	209950.479621	36.796237
1581.845139	210312.857318	36.801255
1583.932848	210667.848098	36.806272
1585.045997	211031.578220	36.811290
1586.654951	211385.806513	36.816308
1587.703766	211756.508166	36.821325
1589.250243	212122.635959	36.826343
1591.263147	212479.774530	36.831360
1592.920765	212847.740233	36.836378
1594.498692	213213.661126	36.841396
1596.201395	213583.475050	36.846413
1597.584253	213948.461914	36.851431
1599.234224	214315.007776	36.856448
1601.042157	214680.817973	36.861466
1602.557033	215047.792147	36.866484
1603.951879	215421.288812	36.871501
1605.906015	215783.622222	36.876519
1607.295454	216152.877944	36.881536
1609.112016	216525.776086	36.886554
1610.482471	216893.765184	36.891572
1611.807434	217273.752315	36.896589
1613.348122	217643.696827	36.901607
1615.131005	218026.229442	36.906624
1616.357275	218415.860914	36.911642
1618.124697	218787.930027	36.916660
1619.583044	219170.691995	36.921677
1621.289805	219548.436123	36.926695
1623.439171	219927.000323	36.931712
1624.835877	220319.578496	36.936730
1626.585718	220701.508113	36.941748
1627.938890	221079.308305	36.946765
1629.429835	221475.632034	36.951783
1630.919143	221862.302625	36.956800
1632.118554	222270.485140	36.961818
1633.578203	222666.001228	36.966836
1635.121909	223058.811430	36.971853
1636.881864	223451.384639	36.976871
1638.513468	223826.499997	36.981888
1640.349033	224207.401019	36.986906
1641.962443	224583.129008	36.991924
1644.095224	224956.946647	36.996941
1645.934684	225325.424533	37.001959
1647.951900	225692.960053	37.006976
1649.239043	226072.321096	37.011994
1650.859346	226438.750102	37.017012
1652.296804	226817.223815	37.022029
1653.652078	227201.172210	37.027047
1655.574676	227571.135725	37.032064
1656.685341	227964.140694	37.037082
1658.773055	228343.807950	37.042100
1660.386361	228732.618587	37.047117
1661.982191	229122.295568	37.052135
1663.726240	229517.004611	37.057152
1665.461187	229901.019825	37.062170
1667.954022	230263.576898	37.067188
1670.013809	230642.790390	37.072205
1671.932663	231023.194332	37.077223
1673.903444	231399.982580	37.082240
1675.123346	231780.774929	37.087258
1676.699052	232153.966396	37.092276
1678.344859	232534.259755	37.097293
1679.824490	232923.876692	37.102311
1681.273720	233311.694426	37.107328
1682.184372	233715.930834	37.112346
1684.050794	234112.065928	37.117364
1685.573189	234513.005036	37.122381
1687.338344	234917.817974	37.127399
1688.819429	235327.577907	37.132416
1690.379172	235750.230221	37.137434
1692.000750	236161.542342	37.142452
1693.619206	236579.992937	37.147469
1695.365733	236998.041949	37.152487
1696.937519	237423.078400	37.157504
1698.442237	237845.355817	37.162522
1700.342004	238273.210453	37.167540
1701.968333	238701.132700	37.172557
1703.187578	239130.312015	37.177575
1705.410151	239557.580854	37.182592
1706.467426	239999.739990	37.187610
1708.515056	240431.836124	37.192628
1710.553373	240875.694763	37.197645
1711.735154	241320.321773	37.202663
1713.849099	241748.645668	37.207680
1715.374271	242199.873032	37.212698
1717.194362	242643.178424	37.217716
1718.765843	243089.544854	37.222733
1719.927853	243539.708740	37.227751
1721.832281	243990.695451	37.232768
1723.550131	244449.407519	37.237786
1725.531874	244904.393883	37.242804
1727.669874	245351.911770	37.247821
1729.052250	245819.843736	37.252839
1731.204236	246273.606463	37.257856
1732.603226	246732.998344	37.262874
1734.331164	247184.285017	37.267892
1736.428333	247632.032670	37.272909
1738.239894	248093.287228	37.277927
1739.978870	248536.871883	37.282944
1741.796505	248985.193346	37.287962
1743.464101	249437.245852	37.292980
1745.192372	249890.252938	37.297997
1747.000523	250346.853389	37.303015
1749.120678	250801.650994	37.308032
1750.331634	251251.585391	37.313050
1751.655481	251701.297620	37.318068
1753.697289	252131.870209	37.323085
1755.253995	252582.559487	37.328103
1757.394523	253015.400263	37.333120
1758.838252	253459.220698	37.338138
1760.333507	253905.013030	37.343156
1762.148634	254339.780484	37.348173
1763.958412	254796.519621	37.353191
1765.659941	255231.276669	37.358208
1767.133124	255690.656437	37.363226
1768.819748	256145.784646	37.368244
1770.666356	256595.120218	37.373261
1772.651330	257060.739998	37.378279
1774.485396	257499.380596	37.383296
1776.342106	257972.713577	37.388314
1777.825793	258444.121885	37.393332
1779.804900	258893.555571	37.398349
1781.400159	259368.321132	37.403367
1783.273340	259820.536591	37.408384
1786.043888	260282.693806	37.413402
1787.539702	260745.150265	37.418420
1789.837692	261199.656116	37.423437
1791.723864	261666.264177	37.428455
1793.372062	262115.762629	37.433472
1794.902194	262584.048155	37.438490
1796.646600	263049.935981	37.443508
1798.385229	263519.200841	37.448525
1800.255420	263982.093194	37.453543
1802.271434	264455.044226	37.458560
1803.501862	264929.081209	37.463578
1805.368556	265395.625315	37.468596
1807.897245	265865.492553	37.473613
1809.442946	266343.969227	37.478631
1811.266509	266807.440273	37.483648
1812.930201	267294.631044	37.488666
1814.777099	267766.399230	37.493684
1816.799943	268260.615103	37.498701
1818.196338	268733.591933	37.503719
1820.688787	269204.134443	37.508736
1822.739291	269668.673613	37.513754
1824.902998	270132.913345	37.518772
1827.022382	270609.348540	37.523789
1828.758149	271090.158827	37.528807
1830.536530	271553.638808	37.533824
1832.122340	272022.352931	37.538842
1834.123147	272507.025205	37.543860
1835.828831	272981.582137	37.548877
1837.261146	273458.693503	37.553895
1839.290021	273929.283463	37.558912
1840.907211	274414.944583	37.563930
1842.228545	274906.185579	37.568948
1844.727058	275384.744472	37.573965
1846.412582	275883.846251	37.578983
1847.908987	276365.679882	37.584000
1849.669268	276852.802438	37.589018
1851.155393	277353.094449	37.594036
1853.031022	277845.195762	37.599053
1854.251723	278358.068233	37.604071
1856.148089	278864.965278	37.609088
1857.802875	279372.176097	37.614106
1859.636622	279898.909508	37.619124
1861.620506	280405.553954	37.624141
1863.180486	280926.101244	37.629159
1864.818643	281453.743003	37.634176
1866.899596	281976.055068	37.639194
1868.912240	282502.741784	37.644212
1870.697032	283024.305338	37.649229
1872.572760	283564.642022	37.654247
1874.833743	284073.832818	37.659264
1877.088017	284567.099421	37.664282
1879.341753	285065.390380	37.669300
1881.329393	285548.991522	37.674317
1882.973339	286051.154196	37.679335
1884.715396	286537.859176	37.684352
1886.522819	287025.743807	37.689370
1888.327995	287523.782004	37.694388
1890.448489	288021.208458	37.699405
1892.173516	288526.132739	37.704423
1894.170550	289018.924177	37.709440
1895.681310	289523.087016	37.714458
1897.654346	290038.878795	37.719476
1900.213034	290525.400635	37.724493
1902.113694	291029.515806	37.729511
1903.873912	291538.244525	37.734528
1906.023343	292042.617193	37.739546
1907.748194	292549.946593	37.744564
1910.078245	293053.825600	37.749581
1911.930692	293557.292717	37.754599
1913.656926	294055.494350	37.759616
1915.475543	294570.916582	37.764634
1917.352217	295078.810093	37.769652
1919.513653	295597.571780	37.774669
1921.104216	296114.285519	37.779687
1922.852140	296633.737320	37.784704
1925.325406	297161.677447	37.789722
1926.737852	297700.441512	37.794740
1928.506328	298212.208540	37.799757
1930.365888	298754.192912	37.804775
1932.397288	299289.874505	37.809792
1934.060807	299825.709999	37.814810
1935.845937	300374.823771	37.819828
1937.715975	300919.806128	37.824845
1939.364490	301475.378227	37.829863
1941.493101	302017.110354	37.834880
1943.539117	302574.005032	37.839898
1945.116952	303127.895472	37.844916
1947.479247	303691.151293	37.849933
1949.630165	304237.781728	37.854951
1951.970705	304775.466773	37.859968
1954.060456	305335.980396	37.864986
1955.803416	305896.339040	37.870004
1957.748723	306440.465083	37.875021
1959.652697	306998.527143	37.880039
1961.576052	307559.397446	37.885056
1963.228308	308125.278836	37.890074
1965.366861	308695.748003	37.895092
1967.373653	309253.819255	37.900109
1969.488244	309824.304336	37.905127
1971.273763	310391.585317	37.910144
1973.565833	310962.790562	37.915162
1975.281847	311535.068938	37.920180
1977.252023	312107.782850	37.925197
1978.999880	312677.885007	37.930215
1980.735428	313256.636708	37.935232
1982.466926	313844.391605	37.940250
1984.781707	314424.992272	37.945268
1986.711088	314994.301432	37.950285
1988.634662	315587.815672	37.955303
1990.687617	316174.830375	37.960320
1993.013751	316746.364792	37.965338
1995.096301	317332.268408	37.970356
1997.358041	317898.164222	37.975373
1999.837690	318482.569302	37.980391
2001.711881	319044.932789	37.985408
2003.722642	319622.772616	37.990426
2005.321993	320186.306230	37.995444
2007.828147	320747.356003	38.000461
2010.026127	321294.008010	38.005479
2012.367698	321843.853143	38.010496
2014.440597	322377.721677	38.015514
2016.373358	322924.520929	38.020532
2018.231189	323448.589544	38.025549
2020.583323	323990.513467	38.030567
2022.608596	324523.778322	38.035584
2024.543181	325059.765361	38.040602
2026.435814	325610.036802	38.045620
2027.950349	326151.530336	38.050637
2030.129044	326701.361604	38.055655
2032.065514	327261.016732	38.060672
2034.114851	327802.252107	38.065690
2035.929360	328367.923785	38.070708
2037.805067	328926.347151	38.075725
2039.920042	329485.739958	38.080743
2041.594723	330062.039284	38.085760
2043.772460	330624.095147	38.090778
2045.282204	331202.762690	38.095796
2047.854131	331778.414036	38.100813
2049.787528	332370.164084	38.105831
2051.567210	332954.775194	38.110848
2053.806303	333532.862013	38.115866
2055.322842	334129.292034	38.120884
2057.549856	334724.282317	38.125901
2059.714047	335334.188361	38.130919
2061.618197	335927.586408	38.135936
2063.502677	336525.746694	38.140954
2065.569252	337139.316098	38.145972
2067.892731	337747.660561	38.150989
2069.673936	338363.384558	38.156007
2071.843474	338980.660556	38.161024
2073.964077	339594.585595	38.166042
2075.913224	340226.001970	38.171060
2077.891888	340851.670538	38.176077
2079.922455	341474.428595	38.181095
2081.925345	342108.009323	38.186112
2084.263610	342742.210810	38.191130
2086.209856	343374.052754	38.196148
2088.156437	344005.705540	38.201165
2090.352524	344649.581771	38.206183
2092.070815	345290.781792	38.211200
2094.276106	345926.745663	38.216218
2096.519559	346584.271490	38.221236
2098.598996	347237.448546	38.226253
2100.884841	347893.420539	38.231271
2103.120991	348556.208317	38.236288
2104.839929	349191.197131	38.241306
2107.056041	349853.480153	38.246324
2108.991089	350512.598950	38.251341
2111.033223	351175.769736	38.256359
2113.132336	351834.126045	38.261376
2115.457274	352492.839198	38.266394
2117.661198	353165.932973	38.271412
2119.598356	353830.611802	38.276429
2121.982474	354487.170117	38.281447
2123.629640	355156.150905	38.286464
2125.869913	355826.038654	38.291482
2128.429849	356493.073429	38.296500
2130.628127	357157.032380	38.301517
2133.014557	357826.600514	38.306535
2134.872691	358497.301333	38.311552
2137.267962	359157.105004	38.316570
2139.320749	359831.725654	38.321588
2141.389331	360488.661784	38.326605
2143.825911	361156.095532	38.331623
2145.762688	361828.230907	38.336640
2147.934575	362476.160072	38.341658
2150.451850	363127.011734	38.346676
2152.379914	363762.176995	38.351693
2154.210205	364396.355395	38.356711
2156.853375	365035.486859	38.361728
2159.255410	365672.006350	38.366746
2161.252210	366309.335501	38.371764
2163.308311	366948.491215	38.376781
2165.316545	367583.839014	38.381799
2167.253575	368230.004199	38.386816
2169.743458	368868.668950	38.391834
2171.529292	369521.138000	38.396852
2173.614819	370165.791397	38.401869
2175.762674	370832.211023	38.406887
2177.971936	371484.998870	38.411904
2180.069931	372136.927327	38.416922
2182.071323	372809.758006	38.421940
2183.501826	373472.476594	38.426957
2185.981420	374159.058039	38.431975
2188.043685	374835.883055	38.436992
2190.132233	375524.289972	38.442010
2192.209312	376220.965088	38.447028
2194.389281	376899.873312	38.452045
2196.870412	377606.227601	38.457063
2199.002005	378304.055911	38.462080
2201.575346	379002.835307	38.467098
2203.780891	379690.609933	38.472116
2206.311924	380388.396656	38.477133
2208.360360	381086.468220	38.482151
2211.067883	381785.709687	38.487168
2213.259574	382489.318601	38.492186
2215.887444	383185.166187	38.497204
2217.841209	383877.909336	38.502221
2220.174391	384581.995976	38.507239
2222.283722	385293.771448	38.512256
2224.416210	385995.672415	38.517274
2226.898354	386694.840255	38.522292
2228.985939	387410.433847	38.527309
2230.895717	388113.500640	38.532327
2233.083148	388823.568654	38.537344
2235.604493	389535.564384	38.542362
2237.936441	390251.291146	38.547380
2240.271327	390979.402709	38.552397
2242.183856	391691.102090	38.557415
2244.009955	392411.958990	38.562432
2246.709991	393143.796938	38.567450
2249.207640	393863.746053	38.572468
2250.914772	394587.898269	38.577485
2253.735564	395315.853987	38.582503
2256.072974	396044.571855	38.587520
2258.471273	396768.549700	38.592538
2260.947303	397493.100684	38.597556
2262.884924	398211.436469	38.602573
2265.630925	398935.141387	38.607591
2267.543176	399664.471716	38.612608
2270.421968	400388.768709	38.617626
2272.644755	401106.312540	38.622644
2274.740304	401840.961442	38.627661
2276.960254	402554.765689	38.632679
2279.375490	403274.944650	38.637696
2281.565205	403999.083605	38.642714
2283.875989	404723.787768	38.647732
2285.651874	405459.381990	38.652749
2287.755157	406193.635814	38.657767
2289.802833	406927.368222	38.662784
2292.370745	407662.361316	38.667802
2294.999988	408403.898368	38.672820
2296.554977	409147.349497	38.677837
2299.336258	409865.741154	38.682855
2301.376326	410588.120966	38.687872
2303.185630	411298.876706	38.692890
2305.482166	412024.963213	38.697908
2307.674790	412745.729782	38.702925
2310.344253	413465.385939	38.707943
2312.353037	414194.277366	38.712960
2314.550070	414920.281831	38.717978
2316.668102	415650.067613	38.722996
2318.671466	416402.961555	38.728013
2321.146322	417156.817110	38.733031
2323.616150	417896.535533	38.738048
2325.707093	418637.399808	38.743066
2328.040629	419393.270730	38.748084
2330.305252	420150.945569	38.753101
2333.027095	420895.727105	38.758119
2335.237093	421657.906602	38.763136
2337.437033	422412.525132	38.768154
2339.688746	423178.080178	38.773172
2341.923363	423953.620492	38.778189
2344.408133	424710.890443	38.783207
2346.522167	425493.671446	38.788224
2349.066256	426277.214270	38.793242
2351.728111	427056.764887	38.798260
2354.224831	427845.915917	38.803277
2356.381011	428624.422863	38.808295
2358.862197	429406.639581	38.813312
2360.959131	430202.330797	38.818330
2363.730854	430981.002541	38.823348
2366.194041	431774.298369	38.828365
2368.576303	432564.794954	38.833383
2371.280831	433355.866036	38.838400
2373.697439	434149.779912	38.843418
2375.930666	434944.650000	38.848436
2378.135499	435743.483725	38.853453
2380.908144	436535.626476	38.858471
2383.549412	437328.767473	38.863488
2385.666704	438124.281541	38.868506
2388.127570	438923.750355	38.873524
2390.650478	439731.006413	38.878541
2393.382967	440523.241372	38.883559
2395.627862	441330.876264	38.888576
2398.663983	442118.651669	38.893594
2401.023910	442904.478952	38.898612
2402.718510	443709.924549	38.903629
2405.932964	444495.954612	38.908647
2408.319419	445301.777981	38.913664
2410.586774	446100.463479	38.918682
2413.334387	446890.857624	38.923700
2415.236735	447699.933444	38.928717
2418.004017	448493.638171	38.933735
2420.120391	449291.903861	38.938752
2422.753174	450098.940074	38.943770
2425.307391	450904.487995	38.948788
2427.591631	451701.105376	38.953805
2430.448781	452501.080997	38.958823
2432.790163	453311.046456	38.963840
2434.999672	454109.031308	38.968858
2437.607623	454910.703575	38.973876
2439.780326	455709.580558	38.978893
2442.356225	456512.193999	38.983911
2444.565447	457317.957049	38.988928
2446.797053	458125.849364	38.993946
2449.961170	458927.501964	38.998964
2452.313673	459732.272083	39.003981
2454.719386	460534.775778	39.008999
2457.684957	461331.351300	39.014016
2460.237685	462132.293531	39.019034
2462.624763	462915.917620	39.024052
2464.582358	463707.645118	39.029069
2466.705829	464474.739910	39.034087
2469.451227	465248.008495	39.039104
2471.259263	466021.539333	39.044122
2473.938125	466794.444135	39.049140
2476.155516	467593.413063	39.054157
2478.606117	468377.982314	39.059175
2481.474158	469151.857309	39.064192
2483.831162	469946.807009	39.069210
2486.892588	470736.615282	39.074228
2488.962957	471512.470609	39.079245
2491.003789	472308.414060	39.084263
2493.546557	473108.626975	39.089280
2495.985672	473903.673526	39.094298
2498.533316	474718.579689	39.099316
2500.779079	475533.491805	39.104333
2502.957651	476348.373031	39.109351
2505.471115	477166.789993	39.114368
2507.623176	478006.191670	39.119386
2510.419945	478827.301782	39.124404
2512.627469	479666.102816	39.129421
2515.784374	480492.463247	39.134439
2518.663100	481319.126119	39.139456
2521.790377	482161.581190	39.144474
2524.157236	482990.050027	39.149492
2526.293295	483825.515128	39.154509
2528.942747	484657.277390	39.159527
2531.275447	485489.195581	39.164544
2533.492407	486356.556075	39.169562
2536.623534	487204.882684	39.174580
2539.690637	488043.399184	39.179597
2542.580947	488876.356082	39.184615
2544.992093	489720.121687	39.189632
2547.861620	490569.661690	39.194650
2550.342002	491411.357733	39.199668
2553.003536	492257.913899	39.204685
2554.915085	493106.654689	39.209703
2557.728047	493950.774903	39.214720
2559.885704	494806.430505	39.219738
2563.007366	495671.200993	39.224756
2564.636562	496529.458064	39.229773
2567.600896	497385.341894	39.234791
2570.239166	498246.009411	39.239808
2572.501077	499113.078340	39.244826
2575.447955	499985.928357	39.249844
2577.577325	500864.793222	39.254861
2580.357758	501733.084672	39.259879
2583.225424	502615.351634	39.264896
2585.598934	503488.734505	39.269914
2588.165772	504361.782442	39.274932
2591.410568	505229.588997	39.279949
2593.890271	506107.827314	39.284967
2596.431629	506980.014669	39.289984
2599.068588	507858.120163	39.295002
2602.000384	508735.169184	39.300020
2603.990730	509628.910640	39.305037
2606.713840	510506.837566	39.310055
2609.417812	511393.614819	39.315072
2611.626511	512271.863380	39.320090
2614.281893	513144.002147	39.325108
2617.026320	514030.856355	39.330125
2619.650491	514923.052757	39.335143
2622.732102	515805.918582	39.340160
2624.982046	516698.410281	39.345178
2627.706782	517579.860180	39.350196
2630.150339	518471.602498	39.355213
2632.702854	519366.888518	39.360231
2635.493012	520236.695109	39.365248
2638.035403	521115.933416	39.370266
2640.388481	521967.552760	39.375284
2642.810840	522836.093119	39.380301
2645.504408	523704.936728	39.385319
2648.279589	524566.927611	39.390336
2650.170687	525426.790176	39.395354
2653.063057	526292.469342	39.400372
2656.176529	527179.709665	39.405389
2658.499916	528047.824382	39.410407
2661.296029	528923.091326	39.415424
2663.610048	529821.379398	39.420442
2666.197981	530704.194333	39.425460
2668.485155	531601.610669	39.430477
2670.858379	532509.346473	39.435495
2673.689999	533407.808073	39.440512
2676.312172	534332.750768	39.445530
2678.671689	535240.346837	39.450548
2681.131173	536171.257563	39.455565
2683.763445	537106.641606	39.460583
2686.748986	538044.210736	39.465600
2688.862483	538990.831354	39.470618
2691.404540	539938.418334	39.475636
2694.109851	540893.938109	39.480653
2697.053529	541854.817692	39.485671
2699.470222	542808.480667	39.490688
2702.276908	543788.199984	39.495706
2705.517405	544764.563644	39.500724
2707.911362	545733.558572	39.505741
2710.859234	546708.259848	39.510759
2713.779807	547674.261451	39.515776
2716.401566	548646.503030	39.520794
2719.298539	549624.291305	39.525812
2722.006407	550614.717558	39.530829
2724.470850	551599.585904	39.535847
2727.866848	552596.762851	39.540864
2730.224270	553585.647953	39.545882
2733.447603	554573.113532	39.550900
2736.604215	555554.293068	39.555917
2739.275836	556540.480166	39.560935
2741.892720	557514.616737	39.565952
2744.749249	558510.785643	39.570970
2747.861806	559494.504480	39.575988
2750.528290	560486.127690	39.581005
2753.072860	561474.079512	39.586023
2756.222460	562471.772586	39.591040
2758.780356	563468.872230	39.596058
2762.132876	564449.284117	39.601076
2764.927801	565434.708957	39.606093
2766.854517	566432.955901	39.611111
2770.063856	567420.300633	39.616128
2772.575718	568430.852140	39.621146
2775.530670	569425.875704	39.626164
2778.186446	570425.064873	39.631181
2781.166934	571429.171680	39.636199
2783.885815	572428.325912	39.641216
2786.606575	573429.894420	39.646234
2789.951026	574420.617729	39.651252
2793.174342	575406.969782	39.656269
2795.387814	576417.209692	39.661287
2798.437459	577397.460283	39.666304
2801.084259	578398.848794	39.671322
2803.972374	579387.804613	39.676340
2806.918856	580387.867112	39.681357
2809.647343	581400.826643	39.686375
2813.103588	582394.826882	39.691392
2815.585921	583390.189898	39.696410
2818.057672	584382.464586	39.701428
2820.702363	585366.123489	39.706445
2823.108906	586334.284418	39.711463
2826.099225	587302.118118	39.716480
2828.784040	588272.712309	39.721498
2831.477014	589251.414360	39.726516
2834.372512	590211.906432	39.731533
2836.791465	591186.078366	39.736551
2839.839717	592157.615416	39.741568
2842.906935	593135.655835	39.746586
2846.092028	594110.990699	39.751604
2848.802749	595086.060687	39.756621
2851.483976	596071.534049	39.761639
2854.763733	597046.484654	39.766656
2857.290898	598029.102970	39.771674
2859.786573	599024.366727	39.776692
2863.147929	600011.163100	39.781709
2866.193197	601000.062481	39.786727
2869.500139	601987.279880	39.791744
2871.828979	602982.791963	39.796762
2874.707461	603986.556834	39.801780
2877.695036	604979.129168	39.806797
2880.482975	605995.537810	39.811815
2883.310576	606997.920077	39.816832
2886.066191	608022.664799	39.821850
2889.277792	609033.567978	39.826868
2891.745744	610057.455285	39.831885
2894.230662	611089.216412	39.836903
2897.632242	612119.532479	39.841920
2900.777220	613151.977630	39.846938
2903.279403	614184.268039	39.851956
2906.424410	615216.003025	39.856973
2909.038907	616269.896388	39.861991
2911.657603	617314.606973	39.867008
2914.422246	618374.434997	39.872026
2917.292871	619430.196862	39.877044
2920.200176	620503.129812	39.882061
2923.275618	621575.521425	39.887079
2926.323533	622640.477941	39.892096
2929.377510	623717.770241	39.897114
2931.664945	624791.776906	39.902132
2935.068969	625878.737073	39.907149
2937.981508	626960.972283	39.912167
2940.874088	628038.011743	39.917184
2944.072517	629129.568946	39.922202
2946.437134	630220.087786	39.927220
2949.606974	631309.909226	39.932237
2952.362346	632418.283413	39.937255
2955.091004	633512.352271	39.942272
2958.711643	634628.843291	39.947290
2961.425742	635738.330683	39.952308
2964.860750	636841.954812	39.957325
2967.840375	637955.468278	39.962343
2970.603002	639052.572970	39.967360
2973.889965	640171.743627	39.972378
2976.920865	641272.624086	39.977396
2979.953279	642372.330635	39.982413
2982.423969	643489.243025	39.987431
2985.635983	644600.487941	39.992448
2988.519030	645720.049154	39.997466
2991.396990	646838.581036	40.002484
2994.893753	647957.377075	40.007501
2997.541115	649081.534490	40.012519
3000.698657	650184.016895	40.017536
3004.065856	651311.810615	40.022554
3006.606008	652423.653904	40.027572
3009.898110	653540.953252	40.032589
3012.831285	654663.780593	40.037607
3015.914846	655773.886045	40.042624
3019.205552	656874.342245	40.047642
3022.123666	657953.679956	40.052660
3025.608555	659021.832599	40.057677
3028.339558	660091.959773	40.062695
3031.646604	661161.967354	40.067712
3034.199507	662229.186006	40.072730
3037.489685	663289.663445	40.077748
3040.565651	664354.113350	40.082765
3043.264434	665438.724082	40.087783
3046.159881	666515.534881	40.092800
3049.010126	667601.936471	40.097818
3051.929474	668692.058187	40.102836
3055.234888	669774.102915	40.107853
3058.484636	670866.675537	40.112871
3061.239493	671971.128594	40.117888
3064.446123	673076.211896	40.122906
3067.279655	674179.279782	40.127924
3070.210568	675297.395947	40.132941
3073.000567	676422.469734	40.137959
3075.894701	677548.220716	40.142976
3078.707343	678680.420234	40.147994
3081.750823	679827.926823	40.153012
3084.529604	680974.972759	40.158029
3087.638775	682127.947751	40.163047
3090.528576	683286.390534	40.168064
3093.436401	684463.718442	40.173082
3096.429012	685650.859966	40.178100
3099.866166	686820.204480	40.183117
3102.706524	688007.479154	40.188135
3105.736411	689196.136579	40.193152
3108.974563	690382.662486	40.198170
3112.080698	691594.001722	40.203188
3115.297963	692785.127971	40.208205
3118.531078	693993.424418	40.213223
3121.409634	695203.327100	40.218240
3124.751102	696414.509349	40.223258
3127.925060	697630.081724	40.228276
3131.341860	698856.249871	40.233293
3134.526479	700078.614069	40.238311
3137.544090	701302.596374	40.243328
3140.662013	702538.471143	40.248346
3143.809618	703764.723178	40.253364
3146.861474	704990.209702	40.258381
3150.237570	706227.200576	40.263399
3153.932093	707461.235503	40.268416
3156.719497	708690.188466	40.273434
3160.182846	709908.043366	40.278452
3164.062035	711135.359332	40.283469
3167.564764	712360.076970	40.288487
3170.531890	713593.116429	40.293504
3174.178042	714822.059641	40.298522
3177.233231	716042.030493	40.303540
3181.074070	717262.376517	40.308557
3183.870688	718483.432262	40.313575
3187.101025	719690.434711	40.318592
3190.484284	720914.756957	40.323610
3193.576449	722131.050525	40.328628
3196.688256	723343.011931	40.333645
3199.619959	724571.349100	40.338663
3203.053582	725783.413369	40.343680
3206.457577	726988.694314	40.348698
3208.974798	728220.835881	40.353716
3212.581954	729434.551265	40.358733
3215.471702	730658.561404	40.363751
3218.870470	731883.521711	40.368768
3222.057426	733112.494036	40.373786
3225.173508	734336.162023	40.378804
3228.066544	735550.569955	40.383821
3231.642960	736776.958896	40.388839
3234.039760	737968.587952	40.393856
3237.326048	739147.553668	40.398874
3240.539631	740351.001487	40.403892
3243.893486	741544.898187	40.408909
3246.971802	742744.781504	40.413927
3249.586667	743943.214338	40.418944
3253.451140	745135.314540	40.423962
3255.974243	746357.221659	40.428980
3259.654101	747562.596341	40.433997
3262.726227	748778.070461	40.439015
3265.752861	749992.316293	40.444032
3269.438907	751221.458961	40.449050
3272.328129	752461.647434	40.454068
3275.498101	753686.621832	40.459085
3278.452757	754932.058177	40.464103
3282.045963	756181.930762	40.469120
3285.075938	757425.937065	40.474138
3288.244028	758692.633594	40.479156
3291.624457	759956.423730	40.484173
3294.715242	761230.758354	40.489191
3297.655140	762508.165779	40.494208
3301.293658	763794.582112	40.499226
3304.063754	765095.582438	40.504244
3307.315067	766385.643085	40.509261
3310.446811	767692.804928	40.514279
3313.899688	769003.436390	40.519296
3316.938595	770315.301673	40.524314
3320.273359	771648.095451	40.529332
3323.279139	772969.826132	40.534349
3327.235837	774308.507279	40.539367
3330.709485	775647.147292	40.544384
3334.411443	776978.939299	40.549402
3337.512396	778313.885558	40.554420
3341.093033	779661.193436	40.559437
3344.793275	780991.656480	40.564455
3347.715759	782354.546316	40.569472
3351.551299	783692.703895	40.574490
3354.965430	785038.126756	40.579508
3358.229495	786384.911350	40.584525
3361.658032	787742.764751	40.589543
3365.034883	789097.810938	40.594560
3367.862645	790454.810410	40.599578
3371.391024	791819.075583	40.604596
3374.694052	793187.089559	40.609613
3378.019816	794545.504617	40.614631
3380.846160	795937.191308	40.619648
3384.477868	797307.164340	40.624666
3388.019362	798694.737695	40.629684
3391.480730	800077.107216	40.634701
3394.813627	801457.690977	40.639719
3398.017384	802849.145196	40.644736
3401.601079	804227.000715	40.649754
3405.123360	805620.624899	40.654772
3408.987060	807008.004790	40.659789
3412.540742	808394.935519	40.664807
3415.892086	809790.929808	40.669824
3418.967184	811165.949693	40.674842
3422.605993	812563.521343	40.679860
3426.158560	813943.691281	40.684877
3429.934884	815328.962970	40.689895
3432.956773	816725.507594	40.694912
3436.307010	818113.238378	40.699930
3439.659076	819496.580588	40.704948
3443.180987	820896.089622	40.709965
3446.679554	822283.153446	40.714983
3450.055298	823684.963459	40.720000
3453.371208	825081.030157	40.725018
3456.468655	826463.563146	40.730023
3459.786822	827800.737682	40.735028
3463.052080	829103.123693	40.740032
3465.915057	830349.128112	40.745037
3469.129725	831530.894956	40.750042
3471.723830	832661.823532	40.755047
3474.780773	833723.903026	40.760052
3477.664451	834734.844138	40.765056
3480.078541	835684.913005	40.770061
3482.623530	836569.967422	40.775066
3484.880995	837415.530494	40.780071
3487.512879	838182.018121	40.785076
3489.564441	838900.078387	40.790080
3491.654175	839572.445671	40.795085
3493.241118	840189.033644	40.800090
3495.107286	840747.312291	40.805095
3497.160141	841253.132160	40.810100
3498.787081	841725.126962	40.815104
3500.231307	842144.646574	40.820109
3501.612466	842520.702033	40.825114
3503.007945	842862.016690	40.830119
3504.049019	843161.091044	40.835124
3505.610015	843423.224561	40.840128
3506.716060	843665.832599	40.845133
3507.733356	843856.866227	40.850138
3508.257553	844029.453456	40.855143
3509.098944	844164.855449	40.860148
3510.101128	844288.208023	40.865152
3510.810736	844383.781048	40.870157
3511.601836	844452.777657	40.875162
3512.318589	844502.590701	40.880167
3512.815181	844512.691946	40.885172
3513.526740	844517.815570	40.890176
3513.756501	844505.468138	40.895181
3514.359156	844478.327247	40.900186
3514.558079	844431.473083	40.905191
3514.984832	844367.908647	40.910196
3515.374515	844301.537923	40.915200
3515.574477	844225.501517	40.920205
3516.199790	844121.573712	40.925210
3516.189458	844013.186815	40.930215
3516.350614	843899.341843	40.935220
3517.106056	843769.501421	40.940224
3517.023651	843633.002217	40.945229
3517.309631	843484.613380	40.950234
3517.034247	843333.593665	40.955239
3517.458922	843175.382334	40.960244
3517.361143	843009.297228	40.965248
3517.334970	842837.281160	40.970253
3517.430301	842663.592569	40.975258
3517.378676	842491.764359	40.980263
3517.318678	842298.209503	40.985268
3517.877527	842113.861726	40.990272
3517.585855	841928.089419	40.995277
3517.489563	841720.555655	41.000282
3517.905585	841530.683771	41.005287
3517.719087	841326.932926	41.010292
3517.530169	841128.898264	41.015296
3517.517060	840916.764473	41.020301
3517.906555	840709.119330	41.025306
3517.559933	840488.097989	41.030311
3517.518422	840283.803583	41.035316
3517.675017	840062.784747	41.040320
3517.454048	839852.779716	41.045325
3517.562464	839639.805135	41.050330
3517.298459	839428.433534	41.055335
3517.129961	839202.679314	41.060340
3517.188348	838988.330822	41.065344
3516.733143	838780.750326	41.070349
3516.754608	838551.933628	41.075354
3516.594496	838348.755727	41.080359
3516.333233	838129.283036	41.085364
3516.524656	837915.554457	41.090368
3516.189655	837696.659661	41.095373
3516.295535	837483.511293	41.100378
3516.058055	837283.803223	41.105383
3515.824406	837063.316396	41.110388
3515.965038	836861.982103	41.115392
3515.810201	836654.377683	41.120397
3515.807913	836449.460254	41.125402
3515.515211	836238.659538	41.130407
3515.586919	836034.395861	41.135412
3515.356215	835827.259993	41.140416
3515.158257	835615.840030	41.145421
3515.261456	835411.550187	41.150426
3515.126178	835211.174390	41.155431
3514.755385	835009.663555	41.160436
3514.665002	834806.063019	41.165440
3514.124722	834610.391243	41.170445
3514.312129	834411.686150	41.175450
3513.735960	834232.709899	41.180455
3514.037780	834036.887794	41.185460
3514.061045	833840.325934	41.190464
3513.785207	833657.886574	41.195469
3513.763689	833470.448737	41.200474
3513.321130	833280.448522	41.205479
3513.281060	833095.138631	41.210484
3513.259406	832915.842240	41.215488
3513.168042	832735.191545	41.220493
3513.246759	832547.515044	41.225498
3512.892196	832370.391460	41.230503
3512.411183	832194.350998	41.235508
3512.720322	832017.113288	41.240512
3512.278617	831853.394100	41.245517
3512.389653	831676.274499	41.250522
3511.926529	831516.046915	41.255527
3511.925400	831358.657521	41.260532
3512.153714	831183.934037	41.265536
3511.992470	831026.755347	41.270541
3511.725327	830852.294050	41.275546
3511.415242	830690.271704	41.280551
3511.419808	830526.738302	41.285556
3511.296758	830367.495967	41.290560
3511.171473	830226.712790	41.295565
3511.334851	830067.320615	41.300570
3511.149383	829907.881602	41.305575
3510.840720	829752.636441	41.310580
3510.766550	829597.059096	41.315584
3510.695733	829453.139557	41.320589
3510.693610	829302.111120	41.325594
3510.900863	829156.391686	41.330599
3510.354706	829008.356702	41.335604
3510.523148	828865.066168	41.340608
3510.024358	828726.347646	41.345613
3509.777457	828572.617795	41.350618
3509.653944	828430.917861	41.355623
3509.576677	828299.025044	41.360628
3510.119035	828160.714082	41.365632
3509.569000	828037.929713	41.370637
3509.811876	827891.785557	41.375642
3509.561045	827756.408515	41.380647
3509.000043	827617.091121	41.385652
3508.963297	827492.465628	41.390656
3508.634012	827374.105344	41.395661
3508.718326	827251.303157	41.400666
3508.646215	827138.828585	41.405671
3508.456061	827021.995277	41.410676
3508.463525	826905.128837	41.415680
3508.596854	826794.463104	41.420685
3508.556718	826667.001638	41.425690
3508.524448	826551.787558	41.430695
3508.115552	826436.144006	41.435700
3508.681041	826317.137158	41.440704
3507.929961	826206.501779	41.445709
3508.102161	826089.788449	41.450714
3507.831083	825982.671842	41.455719
3507.811695	825862.677917	41.460724
3507.941631	825755.300151	41.465728
3507.893039	825658.742776	41.470733
3507.485020	825557.961148	41.475738
3507.563705	825457.782522	41.480743
3507.433461	825350.535569	41.485748
3507.180462	825243.111419	41.490752
3507.127261	825142.656490	41.495757
3507.554354	825034.636094	41.500762
3507.290371	824942.185846	41.505767
3506.852974	824835.464169	41.510772
3507.129475	824732.227698	41.515776
3506.786553	824644.648354	41.520781
3506.697550	824554.596464	41.525786
3506.430556	824467.294505	41.530791
3506.614803	824378.072695	41.535796
3506.652490	824289.942447	41.540800
3506.451120	824214.785150	41.545805
3506.462102	824109.245228	41.550810
3506.526071	824021.885189	41.555815
3506.206473	823934.875687	41.560820
3506.500896	823845.628910	41.565824
3506.050956	823773.617870	41.570829
3506.124843	823677.788327	41.575834
3506.191386	823597.523130	41.580839
3505.772259	823505.853697	41.585844
3506.010613	823436.065834	41.590848
3505.120470	823363.145969	41.595853
3505.591806	823287.288452	41.600858
3505.496679	823215.604533	41.605863
3505.457319	823144.300205	41.610868
3505.513556	823079.401079	41.615872
3505.202999	822995.295463	41.620877
3505.006292	822933.547576	41.625882
3504.765194	822861.785057	41.630887
3505.007144	822794.421619	41.635892
3505.184385	822732.321379	41.640896
3504.926280	822668.342688	41.645901
3504.993405	822596.528891	41.650906
3505.099772	822537.162022	41.655911
3504.830446	822473.766837	41.660916
3505.143222	822408.139446	41.665920
3504.914457	822346.682571	41.670925
3505.054736	822281.567292	41.675930
3505.085174	822227.171603	41.680935
3504.694953	822149.391424	41.685940
3504.568306	822080.423658	41.690944
3504.612010	822021.353520	41.695949
3504.957816	821959.608354	41.700954
3505.058985	821903.641869	41.705959
3504.856986	821846.359971	41.710964
3504.633477	821777.890493	41.715968
3504.681114	821722.319961	41.720973
3505.247573	821644.189234	41.725978
3504.750085	821582.474806	41.730983
3504.506993	821523.444729	41.735988
3504.757445	821462.682615	41.740992
3504.603924	821409.865475	41.745997
3504.542279	821337.667878	41.751002
3504.500290	821286.486599	41.756007
3504.454426	821222.946288	41.761012
3504.237664	821165.465734	41.766016
3503.771448	821122.524088	41.771021
3504.287703	821072.226950	41.776026
3504.096292	821022.623946	41.781031
3503.877004	820966.699053	41.786036
3504.245295	820915.937170	41.791040
3503.868957	820861.982309	41.796045
3504.167110	820804.612546	41.801050
3503.987890	820758.606477	41.806055
3503.813963	820713.377835	41.811060
3503.966381	820662.452966	41.816064
3503.805616	820620.627982	41.821069
3503.904844	820568.542739	41.826074
3503.862937	820537.307251	41.831079
3503.569810	820486.547908	41.836084
3503.450638	820434.106358	41.841088
3503.482916	820394.390907	41.846093
3503.374663	820354.210516	41.851098
3503.568762	820301.232215	41.856103
3503.630476	820262.971287	41.861108
3503.690886	820217.702383	41.866112
3503.383228	820175.897350	41.871117
3503.330009	820139.308288	41.876122
3502.885362	820102.196191	41.881127
3503.180783	820059.030745	41.886132
3503.259454	820017.456253	41.891136
3502.881395	819991.429346	41.896141
3503.069705	819948.279871	41.901146
3503.066363	819923.848829	41.906151
3503.351482	819884.674603	41.911156
3503.335523	819847.007270	41.916160
3502.839971	819807.662577	41.921165
3503.187856	819763.610819	41.926170
3503.229346	819743.941704	41.931175
3503.035799	819699.487427	41.936180
3503.000554	819663.671467	41.941184
3503.118858	819629.388767	41.946189
3502.982623	819593.588188	41.951194
3502.971626	819549.493666	41.956199
3502.837230	819521.382483	41.961204
3503.135803	819485.026589	41.966208
3502.925928	819447.873861	41.971213
3502.928657	819425.289451	41.976218
3502.883995	819383.827328	41.981223
3503.140583	819362.371153	41.986228
3502.840998	819315.789082	41.991232
3502.806905	819294.280765	41.996237
3502.975052	819257.359842	42.001242
3502.909732	819228.360400	42.006247
3502.936043	819184.841539	42.011252
3502.939256	819163.911030	42.016256
3502.755609	819131.133011	42.021261
3502.810579	819088.874542	42.026266
3502.605071	819057.851859	42.031271
3502.494565	819039.664529	42.036276
3502.553016	819013.175860	42.041280
3502.657318	818991.158099	42.046285
3502.522396	818956.229796	42.051290
3502.503910	818922.743388	42.056295
3502.706773	818901.196665	42.061300
3503.162737	818863.060164	42.066304
3502.635940	818837.246353	42.071309
3502.504232	818795.015062	42.076314
3503.045861	818778.769479	42.081319
3502.511208	818741.565926	42.086324
3502.790356	818701.216887	42.091328
3502.709193	818681.174146	42.096333
3502.514075	818655.599798	42.101338
3502.620869	818621.605396	42.106343
3502.698109	818604.750448	42.111348
3502.511551	818569.925398	42.116352
3502.280669	818556.428672	42.121357
3502.595220	818524.835230	42.126362
3502.606940	818500.006781	42.131367
3502.363104	818472.200021	42.136372
3502.595759	818437.406055	42.141376
3502.758985	818415.571761	42.146381
3502.465842	818389.330112	42.151386
3502.476832	818365.961660	42.156391
3502.259141	818328.706079	42.161396
3502.728991	818296.892477	42.166400
3502.217548	818270.100270	42.171405
3502.389522	818244.758933	42.176410
3502.199552	818222.005536	42.181415
3502.208843	818197.663076	42.186420
3502.821208	818171.960507	42.191424
3502.130854	818150.648174	42.196429
3502.353388	818131.724564	42.201434
3502.428695	818106.495139	42.206439
3502.105770	818086.488268	42.211444
3502.266970	818052.092778	42.216448
3502.039782	818037.328578	42.221453
3501.998072	818010.072350	42.226458
3502.318683	817989.964569	42.231463
3501.612298	817970.990944	42.236468
3502.007814	817948.826595	42.241472
3501.895047	817955.270551	42.246477
3501.703864	817932.321543	42.251482
3501.967346	817915.435612	42.256487
3501.866221	817893.348701	42.261492
3502.256769	817883.745499	42.266496
3501.491086	817853.972787	42.271501
3501.848798	817842.719370	42.276506
3501.807561	817826.757161	42.281511
3501.672765	817812.562203	42.286516
3502.271756	817799.615694	42.291520
3501.815543	817776.025944	42.296525
3501.824011	817749.831810	42.301530
3501.998978	817741.235803	42.306535
3501.515803	817719.986969	42.311540
3501.784493	817693.557176	42.316544
3501.741727	817697.264033	42.321549
3501.722695	817677.110964	42.326554
3501.888295	817661.018624	42.331559
3501.877855	817645.537998	42.336564
3501.611673	817621.333716	42.341568
3501.837388	817623.148553	42.346573
3501.863919	817603.669737	42.351578
3502.080321	817595.261798	42.356583
3501.577143	817565.933535	42.361588
3501.950790	817552.534870	42.366592
3501.694554	817539.039891	42.371597
3501.910294	817514.467733	42.376602
3502.042910	817498.769630	42.381607
3501.316749	817487.003376	42.386612
3501.663231	817482.469969	42.391616
3501.549376	817464.862797	42.396621
3501.645937	817459.199931	42.401626
3501.733028	817452.370028	42.406631
3501.632918	817436.123890	42.411636
3501.516483	817422.801557	42.416640
3501.146680	817406.500124	42.421645
3501.299085	817375.705205	42.426650
3501.531153	817385.796178	42.431655
3501.567776	817376.734408	42.436660
3501.619423	817355.984986	42.441664
3501.424671	817353.288886	42.446669
3501.778891	817336.776713	42.451674
3501.599403	817325.411583	42.456679
3501.452758	817308.685497	42.461684
3501.674541	817308.748234	42.466688
3501.593430	817287.727201	42.471693
3501.595806	817278.962779	42.476698
3501.597117	817267.958796	42.481703
3501.532706	817255.504382	42.486708
3501.782677	817243.779832	42.491712
3501.704232	817227.919281	42.496717
3501.906268	817208.022271	42.501722
3501.390726	817201.675817	42.506727
3501.287313	817185.916441	42.511732
3501.590766	817173.891259	42.516736
3501.381833	817168.957547	42.521741
3501.675575	817153.622908	42.526746
3501.751155	817145.333757	42.531751
3501.280451	817136.740468	42.536756
3501.834820	817107.244719	42.541760
3501.516823	817111.481856	42.546765
3501.465385	817096.687943	42.551770
3501.327289	817080.349431	42.556775
3501.457023	817078.284160	42.561780
3501.272818	817071.106721	42.566784
3501.337621	817057.268363	42.571789
3501.356085	817040.807892	42.576794
3501.420433	817041.869068	42.581799
3501.553318	817044.867178	42.586804
3501.444809	817025.310277	42.591808
3501.335319	817013.836252	42.596813
3501.412594	817009.149821	42.601818
3501.396286	816987.046430	42.606823
3501.436937	816980.418035	42.611828
3501.349537	816978.970975	42.616832
3501.506338	816968.234306	42.621837
3501.071343	816955.545070	42.626842
3501.252274	816955.127280	42.631847
3501.620954	816951.661241	42.636852
3501.619990	816933.840151	42.641856
3501.503120	816919.640349	42.646861
3501.392548	816919.073356	42.651866
3501.547415	816900.838273	42.656871
3501.314455	816881.884684	42.661876
3501.749380	816888.438896	42.666880
3501.444870	816867.451366	42.671885
3501.254265	816850.341376	42.676890
3501.311087	816848.092657	42.681895
3501.178789	816857.754520	42.686900
3501.540158	816834.812467	42.691904
3501.160443	816821.724772	42.696909
3501.388497	816817.988486	42.701914
3501.339725	816807.478448	42.706919
3501.377037	816791.793461	42.711924
3501.427171	816776.690749	42.716928
3501.179168	816784.325695	42.721933
3501.225408	816776.138026	42.726938
3501.501270	816764.213755	42.731943
3501.329606	816750.314293	42.736948
3501.671774	816738.671769	42.741952
3501.619884	816736.147842	42.746957
3501.358308	816721.093723	42.751962
3501.565863	816716.386706	42.756967
3501.478432	816701.013153	42.761972
3501.881908	816684.783719	42.766976
3501.803791	816678.757898	42.771981
3501.602119	816655.805814	42.776986
3501.934002	816634.133683	42.781991
3501.312760	816627.608381	42.786996
3501.414192	816611.328583	42.792001
3501.005703	816612.950693	42.797005
3501.344402	816616.111616	42.802010
3501.590995	816587.538026	42.807015
3501.377785	816584.162749	42.812020
3501.415575	816574.515292	42.817025
3501.366365	816565.757930	42.822029
3501.412616	816548.804865	42.827034
3501.636786	816542.342097	42.832039
3501.506831	816542.946782	42.837044
3501.768737	816504.728777	42.842049
3501.505962	816515.677647	42.847053
3501.274317	816494.969640	42.852058
3501.418105	816480.533308	42.857063
3501.338959	816481.811793	42.862068
3501.380435	816476.156646	42.867073
3501.132607	816460.710181	42.872077
3501.336382	816449.575711	42.877082
3501.264251	816435.075635	42.882087
3501.322560	816447.337919	42.887092
3501.269370	816436.048810	42.892097
3501.700573	816427.313546	42.897101
3501.646266	816415.635007	42.902106
3501.310996	816404.584721	42.907111
3501.393386	816388.794280	42.912116
3501.759837	816381.043001	42.917121
3501.378561	816373.700775	42.922125
3501.111833	816361.957948	42.927130
3501.476488	816352.551231	42.932135
3501.233588	816357.848461	42.937140
3501.252500	816334.373744	42.942145
3501.070860	816335.181314	42.947149
3501.300716	816326.964352	42.952154
3501.247513	816325.317006	42.957159
3501.368210	816324.713804	42.962164
3501.128460	816298.357575	42.967169
3501.377833	816298.318621	42.972173
3501.539008	816286.703550	42.977178
3501.465256	816286.812501	42.982183
3501.479973	816276.096853	42.987188
3501.605757	816248.709329	42.992193
3501.268582	816245.840219	42.997197
3501.069295	816219.866912	43.002202
3501.495971	816218.436707	43.007207
3501.548853	816220.571165	43.012212
3501.146171	816201.836824	43.017217
3501.637655	816194.065768	43.022221
3501.382480	816188.067150	43.027226
3501.265741	816185.845323	43.032231
3501.271909	816175.617817	43.037236
3501.341690	816143.953163	43.042241
3501.506628	816152.790481	43.047245
3501.584642	816140.506363	43.052250
3501.755200	816122.363949	43.057255
3501.275838	816124.094657	43.062260
3501.427598	816105.955134	43.067265
3501.072551	816100.361631	43.072269
3501.134197	816086.716405	43.077274
3501.334998	816084.152712	43.082279
3500.933549	816088.306185	43.087284
3501.321187	816074.025588	43.092289
3501.291797	816064.095651	43.097293
3501.219123	816056.802206	43.102298
3501.443622	816059.299484	43.107303
3501.120877	816054.674868	43.112308
3501.233106	816029.041660	43.117313
3501.441328	816034.366041	43.122317
3501.344660	816025.225744	43.127322
3501.177525	816004.019027	43.132327
3501.248111	815988.229418	43.137332
3501.189611	815988.433388	43.142337
3501.479935	815987.803640	43.147341
3501.483528	815977.478813	43.152346
3501.649810	815960.894983	43.157351
3501.338668	815961.041048	43.162356
3501.236856	815948.200267	43.167361
3501.309098	815929.975263	43.172365
3501.494592	815930.920292	43.177370
3501.409812	815932.102371	43.182375
3500.897730	815919.715263	43.187380
3501.071485	815908.292322	43.192385
3501.180763	815910.418071	43.197389
3501.132373	815906.140057	43.202394
3501.226656	815897.164522	43.207399
3501.246693	815904.661239	43.212404
3500.946450	815891.753960	43.217409
3501.003577	815879.277792	43.222413
3501.070664	815865.241630	43.227418
3501.156378	815870.780104	43.232423
3501.070480	815872.449372	43.237428
3501.422787	815870.251511	43.242433
3501.370141	815851.753599	43.247437
3500.914104	815847.928873	43.252442
3501.151523	815850.813819	43.257447
3501.212318	815856.356202	43.262452
3501.353870	815843.769365	43.267457
3501.245472	815815.247732	43.272461
3501.044499	815816.253192	43.277466
3501.027281	815822.197406	43.282471
3501.051856	815814.498870	43.287476
3501.236043	815812.814278	43.292481
3501.332118	815807.247391	43.297485
3500.933036	815784.809963	43.302490
3501.223512	815778.628250	43.307495
3501.271527	815787.873972	43.312500
3501.311350	815783.776888	43.317505
3501.242476	815768.008523	43.322509
3501.028894	815753.139362	43.327514
3501.470725	815751.998894	43.332519
3501.257845	815757.584145	43.337524
3501.397365	815738.568845	43.342529
3501.175520	815727.986638	43.347533
3501.085890	815723.130527	43.352538
3501.517133	815720.433259	43.357543
3501.036036	815713.398064	43.362548
3501.367087	815696.008548	43.367553
3501.463651	815688.590813	43.372557
3501.098146	815694.297383	43.377562
3501.632534	815677.655259	43.382567
3501.399914	815660.645970	43.387572
3501.292521	815644.104080	43.392577
3501.574817	815652.534146	43.397581
3501.594596	815635.193120	43.402586
3501.753982	815617.538009	43.407591
3501.135508	815613.348909	43.412596
3501.181037	815592.594572	43.417601
3501.150917	815584.125060	43.422605
3501.272976	815581.670877	43.427610
3500.968878	815581.718442	43.432615
3501.213441	815582.556887	43.437620
3501.074170	815575.565505	43.442625
3501.312244	815560.527876	43.447629
3501.120952	815550.914646	43.452634
3501.623750	815546.745035	43.457639
3501.224208	815540.963169	43.462644
3501.203767	815523.628120	43.467649
3500.991684	815514.505116	43.472653
3501.470812	815520.079809	43.477658
3501.597483	815519.767817	43.482663
3501.213445	815508.333934	43.487668
3501.440935	815489.985971	43.492673
3501.755744	815486.722367	43.497677
3501.263784	815465.564594	43.502682
3501.387600	815456.973440	43.507687
3501.126782	815457.890904	43.512692
3501.492112	815452.379019	43.517697
3501.362724	815429.118892	43.522701
3501.226836	815434.594987	43.527706
3501.352016	815423.276161	43.532711
3500.965376	815432.785171	43.537716
3501.094214	815410.653500	43.542721
3501.055105	815404.425532	43.547725
3500.889117	815397.535534	43.552730
3501.231119	815400.209527	43.557735
3501.280467	815393.675496	43.562740
3501.361287	815389.766562	43.567745
3501.361293	815375.252743	43.572749
3501.360744	815374.960632	43.577754
3501.488779	815371.920982	43.582759
3500.882560	815358.963019	43.587764
3501.034374	815336.340449	43.592769
3500.911361	815340.548296	43.597773
3500.827695	815343.873309	43.602778
3500.815012	815337.251506	43.607783
3500.980929	815338.881552	43.612788
3501.170412	815335.345233	43.617793
3501.107203	815333.601778	43.622797
3500.881265	815332.955261	43.627802
3501.209261	815312.058427	43.632807
3501.061199	815304.288839	43.637812
3501.171270	815294.335876	43.642817
3501.081183	815304.383181	43.647821
3500.984930	815311.898789	43.652826
3501.277355	815301.819922	43.657831
3501.171515	815286.543166	43.662836
3501.318008	815284.182457	43.667841
3501.010998	815282.184869	43.672845
3500.992377	815283.941187	43.677850
3501.303628	815288.665643	43.682855
3500.818904	815270.525780	43.687860
3500.927974	815246.838057	43.692865
3500.901913	815253.855710	43.697869
3501.141278	815254.597603	43.702874
3501.299922	815246.292946	43.707879
3501.144739	815259.759865	43.712884
3501.184334	815244.752503	43.717889
3501.253620	815221.947600	43.722893
3500.966624	815220.141685	43.727898
3501.107912	815222.944542	43.732903
3501.238569	815220.781106	43.737908
3501.240895	815213.864594	43.742913
3501.382646	815198.256686	43.747917
3501.226716	815189.611483	43.752922
3501.101572	815188.462137	43.757927
3500.728489	815195.339280	43.762932
3500.985194	815196.370703	43.767937
3501.004920	815182.632645	43.772941
3501.224156	815161.557487	43.777946
3501.338639	815158.519852	43.782951
3501.064213	815163.920428	43.787956
3500.939762	815154.393550	43.792961
3501.373575	815154.423176	43.797965
3501.406116	815147.404455	43.802970
3501.297998	815128.815660	43.807975
3501.101977	815132.158348	43.812980
3501.520367	815114.948391	43.817985
3501.097574	815098.844009	43.822989
3500.986760	815097.887232	43.827994
3501.393821	815088.471992	43.832999
3501.143247	815093.381836	43.838004
3501.098064	815088.810520	43.843009
3501.173758	815068.926445	43.848013
3501.066166	815056.279556	43.853018
3501.102723	815060.462646	43.858023
3501.293265	815064.426836	43.863028
3501.101970	815057.443005	43.868033
3501.514513	815053.676832	43.873037
3501.167395	815040.969942	43.878042
3501.089873	815027.636400	43.883047
3500.748940	815039.281966	43.888052
3500.934536	815036.525397	43.893057
3500.783204	815039.666320	43.898061
3500.963941	815038.761372	43.903066
3501.024574	815020.145874	43.908071
3500.929304	815019.576310	43.913076
3501.152370	815003.955206	43.918081
3501.300157	815013.868379	43.923085
3501.009654	815019.076764	43.928090
3501.222847	815011.834823	43.933095
3501.257434	815000.724223	43.938100
3501.300133	814990.001993	43.943105
3501.098404	814975.908440	43.948109
3501.163777	814972.293904	43.953114
3501.071648	814982.926533	43.958119
3500.910584	814964.442939	43.963124
3501.129177	814951.647434	43.968129
3500.796424	814948.679611	43.973133
3500.781679	814957.546714	43.978138
3500.643282	814951.431229	43.983143
3500.665261	814959.415853	43.988148
3501.267391	814957.665701	43.993153
3500.909125	814962.884726	43.998157
3500.891185	814963.277218	44.003162
3501.016552	814957.704997	44.008167
3500.887147	814947.594087	44.013172
3500.625128	814939.549613	44.018177
3500.965877	814934.235948	44.023181
3500.937685	814936.773181	44.028186
3500.997709	814937.737979	44.033191
3501.048071	814935.294752	44.038196
3501.133264	814930.508109	44.043201
3501.189578	814944.137477	44.048205
3501.103026	814927.005937	44.053210
3501.226483	814898.151623	44.058215
3501.009561	814910.947032	44.063220
3501.178643	814907.121415	44.068225
3500.992326	814918.158541	44.073229
3501.213383	814915.298960	44.078234
3500.891726	814898.009261	44.083239
3500.862758	814899.475056	44.088244
3500.875581	814889.926315	44.093249
3501.087754	814882.976633	44.098253
3500.711182	814883.717441	44.103258
3501.097302	814877.714723	44.108263
3500.814076	814889.351546	44.113268
3501.067133	814894.182816	44.118273
3501.168945	814885.886566	44.123277
3500.696891	814873.880777	44.128282
3501.076374	814854.922695	44.133287
3500.890453	814860.796779	44.138292
3500.727810	814859.458401	44.143297
3500.969889	814864.388827	44.148301
3500.894538	814861.575557	44.153306
3500.665450	814855.863821	44.158311
3500.558594	814873.220679	44.163316
3500.911289	814870.243084	44.168321
3500.557166	814866.304397	44.173325
3500.563744	814876.239863	44.178330
3500.883554	814873.462242	44.183335
3500.571282	814883.739788	44.188340
3501.063738	814874.895376	44.193345
3500.729427	814875.045080	44.198349
3500.942854	814874.329831	44.203354
3501.099681	814846.054558	44.208359
3500.685013	814855.666239	44.213364
3500.944638	814852.605768	44.218369
3501.083987	814852.291763	44.223373
3500.533948	814856.371854	44.228378
3500.668736	814852.064482	44.233383
3500.659719	814863.463655	44.238388
3501.064335	814865.933260	44.243393
3501.093136	814858.525134	44.248397
3500.871074	814864.989363	44.253402
3501.164020	814863.482351	44.258407
3500.831911	814852.233976	44.263412
3501.034816	814838.466526	44.268417
3501.174212	814838.931848	44.273421
3500.883389	814829.917566	44.278426
3500.922473	814833.418494	44.283431
3500.836122	814846.485875	44.288436
3501.291961	814831.315036	44.293441
3500.810047	814818.921015	44.298445
3500.588543	814808.532025	44.303450
3501.092399	814810.109384	44.308455
3500.922272	814811.499849	44.313460
3500.958102	814814.514210	44.318465
3501.063849	814805.340483	44.323469
3500.996841	814811.196025	44.328474
3500.757791	814807.921233	44.333479
3500.856672	814810.730906	44.338484
3500.594157	814810.674553	44.343489
3500.982008	814816.946072	44.348493
3500.717997	814809.388826	44.353498
3500.885294	814796.893276	44.358503
3500.701034	814795.947933	44.363508
3500.755447	814779.281039	44.368513
3500.747400	814792.238875	44.373517
3501.053801	814790.924577	44.378522
3500.766857	814787.267592	44.383527
3500.724101	814783.962103	44.388532
3500.865235	814792.317984	44.393537
3501.353985	814793.508039	44.398541
3501.121678	814796.856577	44.403546
3501.297336	814779.878480	44.408551
3501.323021	814777.828720	44.413556
3501.457144	814763.487350	44.418561
3501.545243	814765.129713	44.423565
3501.005581	814746.704657	44.428570
3501.349937	814733.304538	44.433575
3500.989017	814726.346851	44.438580
3501.148808	814731.485083	44.443585
3501.054132	814722.732239	44.448589
3500.880659	814720.323918	44.453594
3500.873605	814683.208421	44.458599
3500.886500	814690.999969	44.463604
3501.204473	814682.279982	44.468609
3500.921994	814681.057716	44.473613
3500.758210	814696.865253	44.478618
3501.183723	814691.635553	44.483623
3500.787083	814696.665958	44.488628
3501.269326	814696.882859	44.493633
3501.194097	814676.339194	44.498637
3500.979281	814677.054738	44.503642
3500.877911	814661.580915	44.508647
3500.820567	814669.091212	44.513652
3500.653698	814668.337969	44.518657
3500.979527	814668.384483	44.523661
3501.075051	814675.286359	44.528666
3501.184400	814660.656369	44.533671
3500.811047	814652.336667	44.538676
3500.892950	814638.392854	44.543681
3500.747688	814643.384005	44.548685
3500.592610	814651.396701	44.553690
3500.798417	814645.811628	44.558695
3500.718302	814645.531920	44.563700
3500.783647	814662.083086	44.568705
3501.134507	814652.286301	44.573709
3500.842983	814657.787403	44.578714
3500.941486	814653.485567	44.583719
3501.123456	814672.843644	44.588724
3501.000488	814645.487977	44.593729
3501.094584	814631.639663	44.598733
3501.056531	814633.788880	44.603738
3501.109710	814631.832194	44.608743
3500.883525	814634.303081	44.613748
3501.084120	814639.142751	44.618753
3501.230318	814639.119925	44.623757
3501.088500	814612.741261	44.628762
3500.994502	814606.131395	44.633767
3500.984423	814612.660166	44.638772
3500.884059	814607.415182	44.643777
3501.128474	814609.422832	44.648781
3501.156141	814613.899872	44.653786
3500.887078	814605.953488	44.658791
3500.874940	814592.121692	44.663796
3501.011974	814579.825281	44.668801
3500.756454	814578.891043	44.673805
3500.950487	814587.238931	44.678810
3501.420743	814579.079520	44.683815
3501.020939	814588.689285	44.688820
3501.281942	814573.256018	44.693825
3501.306387	814555.326740	44.698829
3501.020017	814557.514801	44.703834
3501.371544	814556.875351	44.708839
3501.221580	814554.658133	44.713844
3500.883646	814541.071995	44.718849
3501.276193	814524.838674	44.723853
3501.145469	814519.988049	44.728858
3500.898843	814516.129757	44.733863
3500.776701	814522.091609	44.738868
3501.285231	814516.069412	44.743873
3501.435804	814514.292309	44.748877
3500.997472	814495.168716	44.753882
3501.078010	814484.829393	44.758887
3500.861926	814488.954937	44.763892
3501.047245	814476.261086	44.768897
3501.102990	814479.662186	44.773901
3501.111841	814496.417466	44.778906
3501.337066	814465.986496	44.783911
3500.966971	814455.522724	44.788916
3500.904505	814443.549500	44.793921
3501.026689	814455.708290	44.798925
3501.138884	814455.495934	44.803930
3501.345086	814446.500824	44.808935
3501.428304	814430.802730	44.813940
3501.457061	814419.984279	44.818945
3501.309182	814420.591963	44.823949
3501.410299	814422.427228	44.828954
3501.412949	814393.881744	44.833959
3501.273325	814396.339192	44.838964
3501.099861	814386.916227	44.843969
3501.247968	814376.955860	44.848973
3500.884970	814362.788708	44.853978
3501.057399	814361.884963	44.858983
3500.856337	814357.824601	44.863988
3500.878423	814358.600571	44.868993
3500.939421	814357.616821	44.873997
3500.794836	814364.751423	44.879002
3500.828012	814355.588382	44.884007
3501.108990	814366.650855	44.889012
3501.043288	814342.792181	44.894017
3501.293400	814334.277169	44.899021
3500.841246	814334.055604	44.904026
3501.000117	814337.538085	44.909031
3501.250705	814335.940147	44.914036
3500.840285	814330.938248	44.919041
3501.016881	814337.438125	44.924045
3500.849589	814326.163035	44.929050
3500.985530	814297.693700	44.934055
3501.137925	814311.504278	44.939060
3501.127037	814306.537329	44.944065
3501.023943	814308.501975	44.949069
3500.871882	814312.227926	44.954074
3501.250287	814300.672636	44.959079
3501.239839	814293.075126	44.964084
3500.807054	814268.104446	44.969089
3501.336381	814258.084297	44.974093
3501.173753	814279.445979	44.979098
3501.214797	814271.158414	44.984103
3500.965712	814254.732418	44.989108
3501.016522	814244.397346	44.994113
3501.214021	814240.566883	44.999117
3501.130016	814242.820843	45.004122
3501.144622	814243.695423	45.009127
3501.251689	814229.259635	45.014132
3500.927748	814213.040083	45.019137
3501.170573	814205.987435	45.024141
3500.830769	814209.255662	45.029146
3500.881805	814210.709111	45.034151
3501.148755	814214.856753	45.039156
3501.078456	814211.555266	45.044161
3501.076391	814185.445233	45.049165
3501.106792	814180.958865	45.054170
3501.135192	814182.221005	45.059175
3501.029709	814189.836829	45.064180
3501.146340	814179.004225	45.069185
3501.140994	814170.821206	45.074189
3500.955058	814153.995365	45.079194
3501.060954	814142.774667	45.084199
3500.872801	814146.993496	45.089204
3501.074461	814154.074211	45.094209
3501.281041	814152.190824	45.099213
3500.982198	814146.976479	45.104218
3500.810228	814145.931686	45.109223
3501.052305	814118.516649	45.114228
3500.889611	814119.029250	45.119233
3501.173235	814114.308394	45.124237
3500.622178	814116.927694	45.129242
3500.831898	814126.248027	45.134247
3501.058790	814118.710632	45.139252
3501.174238	814119.861750	45.144257
3501.072308	814122.995408	45.149261
3501.156303	814107.491238	45.154266
3501.215035	814094.426689	45.159271
3501.465771	814091.659525	45.164276
3501.152735	814092.975057	45.169281
3501.251007	814080.391441	45.174285
3500.799499	814070.134604	45.179290
3501.031066	814054.996951	45.184295
3500.977907	814056.759011	45.189300
3500.782029	814062.440539	45.194305
3500.933967	814056.181362	45.199309
3500.903438	814062.519046	45.204314
3501.257924	814064.704525	45.209319
3500.999489	814064.355236	45.214324
3501.092587	814035.891409	45.219329
3501.005008	814024.311026	45.224333
3500.657134	814032.354650	45.229338
3500.788769	814024.734603	45.234343
3501.082138	814032.872845	45.239348
3500.922544	814039.425586	45.244353
3501.262500	814045.315656	45.249357
3501.092107	814028.876765	45.254362
3500.967141	814006.390085	45.259367
3500.982917	814004.049331	45.264372
3500.988956	814016.811711	45.269377
3501.259473	814006.831621	45.274381
3500.896255	814010.590758	45.279386
3501.183283	814003.433544	45.284391
3500.943388	813980.867308	45.289396
3500.868736	813965.290155	45.294401
3501.159488	813969.044519	45.299405
3500.757949	813969.886759	45.304410
3501.315237	813971.261126	45.309415
3501.024354	813971.111765	45.314420
3501.159038	813971.383030	45.319425
3500.866858	813961.588260	45.324429
3500.975183	813949.879684	45.329434
3500.682555	813947.099966	45.334439
3500.688947	813951.288515	45.339444
3500.716179	813954.012344	45.344449
3501.219798	813950.815865	45.349453
3500.978951	813948.515206	45.354458
3501.061951	813948.989413	45.359463
3501.189692	813947.410581	45.364468
3501.029102	813937.595203	45.369473
3501.169404	813917.015353	45.374477
3501.198822	813919.738855	45.379482
3500.949001	813908.281049	45.384487
3501.107359	813930.275763	45.389492
3500.996461	813920.744884	45.394497
3501.001051	813894.437734	45.399501
3500.886738	813895.235084	45.404506
3500.897032	813888.120998	45.409511
3501.034333	813892.776279	45.414516
3500.756823	813882.491934	45.419521
3501.111022	813880.877685	45.424525
3500.771695	813890.186767	45.429530
3501.082282	813883.123164	45.434535
3500.976615	813884.114027	45.439540
3500.848812	813875.170311	45.444545
3500.985353	813868.231331	45.449549
3500.754023	813867.877793	45.454554
3500.627630	813858.738968	45.459559
3500.323482	813861.514639	45.464564
3500.639253	813862.439626	45.469569
3500.909186	813852.751679	45.474573
3500.512251	813860.998055	45.479578
3501.035343	813861.695769	45.484583
3500.865254	813870.004104	45.489588
3500.924408	813867.461655	45.494593
3501.036745	813869.587625	45.499597
3501.088744	813876.984347	45.504602
3500.946998	813869.699143	45.509607
3501.344456	813849.760896	45.514612
3500.811925	813839.808642	45.519617
3501.104634	813834.404130	45.524621
3500.817162	813826.557060	45.529626
3500.957573	813830.237577	45.534631
3501.093759	813833.626454	45.539636
3501.047974	813842.499989	45.544641
3500.834446	813826.651904	45.549645
3500.515596	813817.737970	45.554650
3500.805738	813806.975033	45.559655
3500.856467	813818.659068	45.564660
3500.801472	813814.478085	45.569665
3500.950748	813802.178235	45.574669
3500.978591	813818.542629	45.579674
3501.130435	813810.724298	45.584679
3501.202589	813820.651189	45.589684
3501.124416	813820.858303	45.594689
3500.993186	813797.787257	45.599693
3500.624942	813784.496508	45.604698
3500.838365	813785.534939	45.609703
3501.172204	813788.795510	45.614708
3500.967432	813797.401663	45.619713
3500.940425	813787.078001	45.624717
3500.700589	813790.623115	45.629722
3500.850184	813792.548421	45.634727
3500.776375	813798.016240	45.639732
3500.534398	813804.094939	45.644737
3500.775707	813803.570081	45.649741
3500.751793	813803.671280	45.654746
3500.827129	813796.741789	45.659751
3501.035473	813784.335238	45.664756
3500.826950	813767.219587	45.669761
3500.998406	813767.387679	45.674765
3500.525747	813772.333268	45.679770
3500.905651	813764.771530	45.684775
3500.985199	813767.779563	45.689780
3500.810613	813762.350603	45.694785
3501.054584	813767.866206	45.699789
3500.942150	813778.893786	45.704794
3501.046445	813766.503465	45.709799
3500.967436	813773.628488	45.714804
3500.795573	813766.250437	45.719809
3501.005616	813754.817898	45.724813
3500.870041	813745.680344	45.729818
3500.671015	813744.542277	45.734823
3501.025091	813728.312913	45.739828
3500.468571	813681.533949	45.744833
3500.717217	813581.526154	45.749837
3500.654321	813437.523354	45.754842
3500.326024	813222.816256	45.759847
3500.495367	812986.780899	45.764852
3500.095781	812672.475870	45.769857
3499.745555	812328.520876	45.774861
3499.272189	811933.593889	45.779866
3499.113930	811487.226937	45.784871
3498.546294	810988.840032	45.789876
3498.328765	810457.311696	45.794881
3497.783887	809861.833985	45.799885
3496.906128	809232.713458	45.804890
3496.415673	808546.765468	45.809895
3495.471685	807820.194836	45.814900
3494.753075	807046.785489	45.819905
3494.408287	806227.765425	45.824909
3493.355737	805358.164241	45.829914
3492.609363	804444.486947	45.834919
3491.445097	803487.999185	45.839924
3490.567033	802488.913577	45.844929
3489.853495	801440.542414	45.849933
3488.604967	800352.784094	45.854938
3487.629636	799209.965299	45.859943
3486.656569	798034.662512	45.864948
3485.073103	796812.593510	45.869953
3484.265192	795532.572007	45.874957
3483.142220	794237.541627	45.879962
3481.597528	792862.848089	45.884967
3480.563490	791463.440438	45.889972
3478.935363	790018.793032	45.894977
3477.682798	788539.876526	45.899981
3476.065994	787019.348912	45.904986
3474.685443	785454.691173	45.909991
3473.064544	783840.172687	45.914996
3471.521171	782186.038417	45.920001
3469.727177	780504.357753	45.925005
3467.934105	778787.676308	45.930010
3466.332295	777024.181075	45.935015
3464.784385	775227.237269	45.940020
3462.968718	773398.586216	45.945025
3460.902125	771516.823788	45.950029
3458.748405	769612.732582	45.955034
3457.207289	767672.204988	45.960039
3455.046320	765690.988812	45.965044
3453.201317	763691.485736	45.970049
3451.276913	761645.461759	45.975053
3449.161745	759568.515357	45.980058
3446.947046	757457.365092	45.985063
3444.674010	755316.154328	45.990068
3442.868945	753147.136503	45.995073
3440.825635	750947.793684	46.000077
3438.210011	748715.103708	46.005082
3436.073860	746437.704638	46.010087
3433.980659	744136.546038	46.015092
3431.621758	741818.944834	46.020097
3429.211056	739450.378063	46.025101
3426.479615	737078.487031	46.030106
3424.453139	734654.762886	46.035111
3421.641795	732212.227842	46.040116
3419.053283	729746.222485	46.045121
3416.741830	727254.006631	46.050125
3414.154466	724733.523652	46.055130
3411.352044	722190.665069	46.060135
3409.048407	719614.141297	46.065140
3406.192443	717023.107630	46.070145
3403.290810	714394.249475	46.075149
3400.449303	711759.748825	46.080154
3398.200672	709091.187109	46.085159
3395.630858	706411.582241	46.090164
3392.630861	703687.346024	46.095169
3390.078139	700933.647285	46.100173
3387.219341	698178.062901	46.105178
3384.123659	695393.193492	46.110183
3381.524637	692586.631144	46.115188
3378.341703	689756.447471	46.120193
3375.429566	686907.251733	46.125197
3372.178197	684042.202307	46.130202
3369.546354	681150.769450	46.135207
3366.496760	678239.796721	46.140212
3363.373229	675315.275588	46.145217
3360.141991	672379.241559	46.150221
3357.256045	669418.402506	46.155226
3354.076907	666438.805412	46.160231
3351.564009	663444.067935	46.165236
3347.939897	660421.080743	46.170241
3345.073068	657390.378918	46.175245
3341.554188	654349.495651	46.180250
3338.686961	651271.039679	46.185255
3335.594990	648186.347609	46.190260
3332.547970	645094.034421	46.195265
3329.318753	641971.559013	46.200269
3326.010669	638848.947677	46.205274
3322.870096	635696.296396	46.210279
3319.063728	632522.744768	46.215284
3315.945257	629360.359295	46.220289
3312.965663	626166.661759	46.225293
3309.682723	622969.466306	46.230298
3306.374881	619753.299082	46.235303
3302.418809	616525.794412	46.240308
3299.108831	613289.897791	46.245313
3295.935569	610045.340588	46.250317
3292.649258	606792.213402	46.255322
3289.119451	603515.527528	46.260327
3285.723222	600229.476366	46.265332
3282.068164	596935.724713	46.270337
3278.817476	593634.923027	46.275341
3274.933398	590325.634104	46.280346
3271.593595	586998.354961	46.285351
3268.425034	583682.363094	46.290356
3264.868674	580343.417747	46.295361
3261.503269	576992.051790	46.300365
3257.823320	573621.419594	46.305370
3254.348361	570248.698377	46.310375
3250.705784	566871.896912	46.315380
3246.797811	563489.330156	46.320385
3243.414014	560099.976140	46.325389
3240.238616	556712.129765	46.330394
3236.461004	553296.526862	46.335399
3232.529391	549885.462129	46.340404
3228.735848	546476.943318	46.345409
3225.364113	543055.043179	46.350413
3221.869247	539646.615585	46.355418
3218.013637	536198.922610	46.360423
3214.334604	532764.871916	46.365428
3210.520814	529330.937626	46.370433
3207.313846	525881.752540	46.375437
3203.192294	522450.403870	46.380442
3199.583063	518998.190206	46.385447
3196.313696	515539.248226	46.390452
3192.207420	512068.574506	46.395457
3188.836279	508603.375827	46.400461
3184.678440	505135.178128	46.405466
3181.009176	501658.593584	46.410471
3177.811519	498186.550569	46.415476
3173.481827	494710.429264	46.420481
3169.938080	491227.867632	46.425485
3166.259963	487748.208454	46.430490
3162.691399	484251.219647	46.435495
3159.203990	480764.898168	46.440500
3155.265918	477277.266399	46.445505
3151.577486	473778.266495	46.450509
3147.526374	470281.750867	46.455514
3143.538364	466781.445240	46.460519
3139.880009	463286.775790	46.465524
3136.025739	459786.455805	46.470529
3132.491026	456294.480205	46.475533
3128.495152	452797.928813	46.480538
3124.744764	449296.496941	46.485543
3120.849867	445792.177894	46.490548
3116.803825	442300.884117	46.495553
3113.004161	438808.996899	46.500557
3109.703903	435316.234009	46.505562
3105.882927	431819.522512	46.510567
3101.867285	428314.765801	46.515572
3098.104703	424827.397124	46.520577
3094.278163	421315.609783	46.525581
3090.537396	417826.129926	46.530586
3086.747854	414330.701985	46.535591
3083.003423	410836.876885	46.540596
3078.916600	407354.112023	46.545601
3075.407329	403855.235823	46.550605
3070.974388	400378.241689	46.555610
3067.324250	396892.227992	46.560615
3063.593883	393412.615561	46.565620
3059.456653	389931.853620	46.570625
3055.848347	386451.024566	46.575629
3051.661820	382975.288841	46.580634
3047.666017	379498.494878	46.585639
3044.217912	376044.140942	46.590644
3039.917665	372584.904739	46.595649
3036.342375	369115.213200	46.600653
3032.282351	365668.622059	46.605658
3028.546115	362203.197900	46.610663
3024.742311	358763.351972	46.615668
3020.888913	355318.372245	46.620673
3017.050270	351862.461601	46.625677
3013.256533	348431.186913	46.630682
3008.849573	344990.803853	46.635687
3005.360336	341560.277527	46.640692
3001.049888	338139.257137	46.645697
2997.491574	334712.326627	46.650701
2993.414885	331309.781334	46.655706
2989.444690	327887.128411	46.660711
2985.303757	324473.364619	46.665716
2980.777065	321078.559167	46.670721
2977.186132	317683.361595	46.675725
2973.315631	314297.742154	46.680730
2969.696018	310930.790222	46.685735
2965.842858	307552.846462	46.690740
2961.630540	304182.541349	46.695745
2957.893674	300824.361977	46.700749
2953.815264	297464.754186	46.705754
2949.503494	294114.782698	46.710759
2945.874539	290782.053661	46.715764
2941.696446	287454.552353	46.720769
2937.952147	284129.156306	46.725773
2933.681586	280812.084337	46.730778
2929.931745	277507.027359	46.735783
2925.900728	274197.520290	46.740788
2921.672243	270913.043974	46.745793
2917.853536	267619.368545	46.750797
2913.940892	264346.602921	46.755802
2909.645069	261076.620947	46.760807
2905.486041	257826.004696	46.765812
2901.023781	254572.498993	46.770817
2897.273507	251337.574691	46.775821
2893.171051	248122.757506	46.780826
2889.037260	244902.971674	46.785831
2884.910129	241698.899344	46.790836
2880.836241	238514.031135	46.795841
2876.822354	235335.716603	46.800845
2872.545600	232167.045073	46.805850
2868.428805	229012.262656	46.810855
2864.267649	225872.478858	46.815860
2859.990155	222748.858694	46.820865
2856.201856	219620.583145	46.825869
2851.917615	216515.396549	46.830874
2847.555902	213427.026067	46.835879
2843.383143	210343.262961	46.840884
2839.585134	207293.831918	46.845889
2835.620133	204226.054250	46.850893
2831.387869	201185.539932	46.855898
2827.160666	198149.128033	46.860903
2823.132579	195138.721280	46.865908
2819.022711	192132.850139	46.870913
2814.863245	189143.764597	46.875917
2810.169406	186166.121835	46.880922
2806.077199	183210.240728	46.885927
2802.298509	180260.383804	46.890932
2797.833263	177323.486071	46.895937
2793.882008	174405.959110	46.900941
2789.296124	171507.286450	46.905946
2785.676105	168625.834144	46.910951
2781.618619	165665.708494	46.915956
2777.309457	162788.001045	46.920961
2773.440978	159941.241575	46.925965
2769.007886	157096.150513	46.930970
2765.050666	154280.340278	46.935975
2760.715714	151468.417098	46.940980
2756.266198	148671.861233	46.945985
2752.776901	145900.801940	46.950989
2748.464666	143133.048562	46.955994
2744.519323	140387.046706	46.960999
2740.468896	137639.169368	46.966004
2736.007025	134918.348551	46.971009
2732.256526	132211.509617	46.976013
2728.184742	129505.409201	46.981018
2723.953872	126825.427527	46.986023
2719.606819	124139.722829	46.991028
2715.627276	121495.281280	46.996033
2711.671645	118846.766143	47.001037
2707.362492	116227.023908	47.006042
2703.346305	113611.411662	47.011047
2699.375992	110998.255173	47.016052
2695.025564	108426.222617	47.021057
2691.120926	105846.631443	47.026061
2686.987225	103285.295625	47.031066
2682.929030	100738.468819	47.036071
2678.807336	98210.177000	47.041076
2674.518261	95695.111266	47.046081
2670.770899	93188.383540	47.051085
2666.815354	90696.453495	47.056090
2662.592105	88220.982382	47.061095
2658.735188	85755.798106	47.066100
2654.443835	83310.960967	47.071105
2650.247811	80874.014754	47.076109
2646.300218	78450.919282	47.081114
2642.185264	76038.437563	47.086119
2638.160788	73645.254057	47.091124
2633.820938	71265.703919	47.096129
2629.871190	68896.603988	47.101133
2625.208371	66550.543348	47.106138
2621.148545	64221.264363	47.111143
2617.644145	61904.698557	47.116148
2613.844040	59608.530278	47.121153
2609.369577	57312.860106	47.126157
2605.227678	55031.333224	47.131162
2600.969183	52774.607157	47.136167
2596.924358	50527.211361	47.141172
2592.606275	48299.770389	47.146177
2588.440531	46086.081724	47.151181
2583.848836	43889.177083	47.156186
2579.661490	41706.178715	47.161191
2575.677681	39541.415347	47.166196
2571.588034	37405.158611	47.171201
2567.358717	35280.773923	47.176205
2562.881140	33168.169433	47.181210
2558.427836	31075.090665	47.186215
2554.710590	29010.282254	47.191220
2550.218570	26962.992928	47.196225
2546.081975	24922.125968	47.201229
2541.875057	22906.564183	47.206234
2537.249870	20913.493192	47.211239
2532.897758	18933.343353	47.216244
2528.326252	16995.108307	47.221249
2523.850305	15070.246284	47.226253
2519.091324	13176.446328	47.231258
2514.106858	11307.268597	47.236263
2508.320341	9494.993777	47.241268
2501.484384	7746.232431	47.246273
2488.318162	6204.737264	47.251277
2474.128706	4811.508034	47.256282
2461.272655	3519.448302	47.261287
2449.017705	2372.400582	47.266292
2437.466134	1388.806299	47.271297
2425.105454	565.585071	47.276301
2404.763350	145.143257	47.281306
2373.852723	232.299704	47.286311
2359.367035	229.060763	47.291316
2356.227044	231.703458	47.296321
2360.188364	231.669082	47.301325
2366.755300	232.176241	47.306330
2371.589686	238.703214	47.311335
2374.662603	219.410096	47.316340
2374.995341	229.004728	47.321345
2373.827604	226.368425	47.326349
2371.081443	220.698115	47.331354
2367.545524	229.891857	47.336359
2364.608709	211.475647	47.341364
2361.651327	221.249619	47.346369
2358.621105	219.622892	47.351373
2355.571443	219.625438	47.356378
2352.894716	228.365216	47.361383
2350.076566	213.524610	47.366388
2346.374596	221.231999	47.371393
2343.814780	215.168700	47.376397
2341.002258	209.277822	47.381402
2337.721189	213.309384	47.386407
2334.364961	209.746754	47.391412
2331.023020	215.047062	47.396417
2328.159768	216.317641	47.401421
2324.949689	215.057596	47.406426
2321.385374	207.885907	47.411431
2318.176215	204.986835	47.416436
2315.073396	213.476886	47.421441
2312.112656	207.008070	47.426445
2308.669308	210.071571	47.431450
2305.314644	214.699971	47.436455
2301.964807	206.305120	47.441460
2298.481067	209.748280	47.446465
2295.096611	209.173611	47.451469
2291.756804	204.472597	47.456474
2288.370430	207.074756	47.461479
2285.288802	195.736687	47.466484
2281.241682	208.519146	47.471489
2278.141158	211.741000	47.476493
2275.323564	206.417270	47.481498
2271.494614	211.993109	47.486503
2268.333676	206.134617	47.491508
2264.866999	213.852670	47.496513
2261.427618	205.278848	47.501517
2257.833899	212.146714	47.506522
2254.908391	210.117642	47.511527
2251.773503	205.150456	47.516532
2248.076831	208.225132	47.521537
2244.303925	209.856357	47.526541
2240.869167	204.407724	47.531546
2237.284731	214.653156	47.536551
2234.049705	207.411000	47.541556
2230.594671	206.394959	47.546561
2226.880381	195.102109	47.551565
2223.424703	205.583668	47.556570
2220.234149	207.433848	47.561575
2217.111734	206.729617	47.566580
2213.597209	210.699656	47.571585
2210.468882	212.033883	47.576589
2206.946234	203.400342	47.581594
2202.852690	206.543453	47.586599
2199.673852	200.754228	47.591604
2196.348407	198.484016	47.596609
2192.883720	201.930551	47.601613
2189.225799	200.234398	47.606618
2185.399959	200.908944	47.611623
2182.908465	189.124233	47.616628
2178.847705	196.150611	47.621633
2175.378973	190.033419	47.626637
2172.471487	193.240914	47.631642
2168.867737	199.275108	47.636647
2165.269712	197.019080	47.641652
2161.273738	197.887938	47.646657
2158.311777	202.426457	47.651661
2154.852709	193.691241	47.656666
2151.155058	199.882506	47.661671
2148.001100	194.440597	47.666676
2144.147819	195.948383	47.671681
2140.624448	196.142170	47.676685
2137.440049	191.606730	47.681690
2134.080507	193.100545	47.686695
2130.594961	181.291049	47.691700
2127.071456	201.277992	47.696705
2123.159463	194.765083	47.701709
2120.151242	191.394860	47.706714
2116.403857	195.037514	47.711719
2112.935007	194.643792	47.716724
2109.679804	189.436045	47.721729
2106.367153	197.319864	47.726733
2102.852694	192.203305	47.731738
2099.123143	198.507147	47.736743
2095.608511	196.143180	47.741748
2091.839414	194.201856	47.746753
2088.651376	187.986991	47.751757
2085.199970	193.927765	47.756762
2081.931303	195.246020	47.761767
2078.565765	188.793167	47.766772
2074.929450	192.437438	47.771777
2071.564718	192.827895	47.776781
2067.439903	183.462872	47.781786
2064.116895	181.717526	47.786791
2060.770010	183.171415	47.791796
2057.045673	186.149233	47.796801
2053.939393	179.595713	47.801805
2050.730510	184.122267	47.806810
2047.190082	188.118550	47.811815
2043.893491	188.789429	47.816820
2040.066717	190.014683	47.821825
2036.562068	181.761232	47.826829
2033.037955	183.075176	47.831834
2029.308933	185.984131	47.836839
2026.315554	180.276688	47.841844
2022.269993	185.804229	47.846849
2018.825699	178.360782	47.851853
2015.620974	182.127368	47.856858
2012.210529	180.452669	47.861863
2008.581805	183.307970	47.866868
2005.056275	187.944197	47.871873
2000.874980	182.286596	47.876877
1998.289930	188.980873	47.881882
1994.378882	186.156934	47.886887
1991.090672	182.963446	47.891892
1987.496578	187.920465	47.896897
1984.387758	189.340290	47.901901
1980.850636	182.857375	47.906906
1976.862094	190.046527	47.911911
1973.769613	196.367781	47.916916
1970.155327	188.988914	47.921921
1966.631037	195.883956	47.926925
1963.404477	182.917161	47.931930
1959.502813	189.039159	47.936935
1956.462189	182.282402	47.941940
1952.426627	180.860571	47.946945
1949.036687	188.731206	47.951949
1945.611033	176.276485	47.956954
1942.683368	174.083325	47.961959
1938.848191	176.679878	47.966964
1935.239352	178.225418	47.971969
1931.760802	180.585829	47.976973
1928.045178	176.703084	47.981978
1924.617926	178.520778	47.986983
1921.299560	182.336811	47.991988
1917.390411	184.609579	47.996993
1914.292839	180.744023	48.001997
1910.988782	176.195749	48.007002
1907.785586	179.712180	48.012007
1904.251138	167.397898	48.017012
1900.403167	164.475542	48.022017
1896.796847	183.083365	48.027021
1893.233016	179.648294	48.032026
1889.369668	185.356179	48.037031
1886.437958	175.908948	48.042036
1882.893192	182.775574	48.047041
1879.564900	182.192249	48.052045
1876.051733	178.935924	48.057050
1872.298754	179.377708	48.062055
1868.937349	175.613568	48.067060
1865.084562	182.740378	48.072065
1861.967928	176.511260	48.077069
1858.668021	166.593299	48.082074
1854.719039	177.639357	48.087079
1851.700550	177.260670	48.092084
1847.449446	178.659965	48.097089
1844.256412	174.597394	48.102093
1840.933048	182.261477	48.107098
1837.260303	185.886210	48.112103
1833.864016	175.910568	48.117108
1830.081481	175.461621	48.122113
1826.936777	171.404149	48.127117
1823.542070	172.457457	48.132122
1819.894519	168.738115	48.137127
1815.889056	164.277496	48.142132
1812.955845	172.427872	48.147137
1809.426096	170.338466	48.152141
1806.065492	166.102811	48.157146
1802.776419	163.108849	48.162151
1799.379128	166.209579	48.167156
1795.850299	171.393726	48.172161
1791.744402	174.728742	48.177165
1788.094715	172.914385	48.182170
1784.172567	177.954439	48.187175
1781.643711	167.586802	48.192180
1778.047978	174.249452	48.197185
1774.277743	171.979387	48.202189
1771.095937	170.186730	48.207194
1767.819885	176.441839	48.212199
1763.705632	166.407743	48.217204
1760.176860	167.042276	48.222209
1756.850939	175.965990	48.227213
1753.494816	169.204899	48.232218
1749.808096	180.007458	48.237223
1746.486792	177.426693	48.242228
1743.154064	171.826241	48.247233
1739.403277	174.330559	48.252237
1735.910051	170.049243	48.257242
1732.340363	172.930194	48.262247
1728.319596	176.429087	48.267252
1725.249828	173.138228	48.272257
1722.015759	179.092542	48.277261
1718.609562	167.976353	48.282266
1714.813163	171.683752	48.287271
1711.277277	159.613403	48.292276
1707.789778	169.916540	48.297281
1704.315037	169.966815	48.302285
1701.355316	167.149139	48.307290
1697.677269	177.577019	48.312295
1694.246443	166.736787	48.317300
1690.354704	172.873131	48.322305
1686.879653	168.060627	48.327309
1683.249699	171.093398	48.332314
1679.674712	169.479368	48.337319
1676.395148	155.739540	48.342324
1672.827906	170.892685	48.347329
1669.138683	175.674854	48.352333
1665.804996	171.412889	48.357338
1662.463697	175.558460	48.362343
1659.408416	167.718908	48.367348
1655.632389	167.866974	48.372353
1651.653004	164.228108	48.377357
1648.319954	163.142553	48.382362
1644.712973	167.427788	48.387367
1641.331534	162.091272	48.392372
1638.188498	162.064344	48.397377
1634.849950	170.240230	48.402381
1631.433266	158.698607	48.407386
1627.512289	163.767002	48.412391
1623.851120	154.702973	48.417396
1620.063063	165.483452	48.422401
1616.507755	169.494846	48.427405
1613.614569	164.142036	48.432410
1609.924890	160.236377	48.437415
1606.376814	166.565738	48.442420
1602.910104	166.023152	48.447425
1599.463891	167.862898	48.452429
1595.714026	160.239655	48.457434
1592.312855	166.103091	48.462439
1588.851541	166.480343	48.467444
1585.836875	158.286443	48.472449
1582.291556	159.053343	48.477453
1578.630494	164.767628	48.482458
1574.455247	164.753576	48.487463
1571.617974	162.929207	48.492468
1567.512162	159.708809	48.497473
1564.247643	158.754930	48.502477
1561.260604	162.193328	48.507482
1557.137985	167.907093	48.512487
1553.721989	162.288110	48.517492
1550.517756	157.534516	48.522497
1546.645301	166.331842	48.527501
1543.381860	157.819381	48.532506
1539.903137	165.226269	48.537511
1536.573040	151.845602	48.542516
1532.782963	164.198849	48.547521
1528.865134	162.774581	48.552525
1526.365970	155.401713	48.557530
1522.425147	160.422628	48.562535
1518.897828	151.989448	48.567540
1515.185074	160.388451	48.572545
1511.508701	161.454306	48.577549
1508.794527	151.239167	48.582554
1504.889776	164.774665	48.587559
1501.543527	150.225921	48.592564
1497.944453	157.158096	48.597569
1494.190864	154.145199	48.602573
1490.933899	157.239876	48.607578
1487.022335	156.532837	48.612583
1483.910699	148.066248	48.617588
1480.290049	153.793218	48.622593
1477.122781	153.893523	48.627597
1473.777302	153.398448	48.632602
1469.872914	157.141814	48.637607
1466.440647	151.905075	48.642612
1462.847385	154.910027	48.647617
1459.418529	163.403819	48.652621
1455.853602	144.564362	48.657626
1452.020788	154.108499	48.662631
1448.655337	153.730457	48.667636
1445.400400	155.056244	48.672641
1441.683177	157.719929	48.677645
1438.809090	153.601253	48.682650
1434.970065	156.742762	48.687655
1430.845934	154.047326	48.692660
1427.676744	160.361725	48.697665
1423.941616	153.220322	48.702669
1421.067816	150.746802	48.707674
1417.520492	154.209662	48.712679
1414.140947	154.178696	48.717684
1410.501751	152.315382	48.722689
1406.728486	153.345820	48.727693
1403.162197	156.330751	48.732698
1399.672228	162.818761	48.737703
1396.501309	148.907028	48.742708
1392.814771	153.318692	48.747713
1389.130985	148.035932	48.752717
1385.772521	149.118510	48.757722
1382.226546	155.412803	48.762727
1378.960833	149.691272	48.767732
1375.269036	151.847950	48.772737
1371.789739	161.697455	48.777741
1368.407348	152.858828	48.782746
1364.649043	156.180721	48.787751
1361.633745	149.268361	48.792756
1358.149638	150.614230	48.797761
1354.099734	159.800067	48.802765
1350.720056	151.299555	48.807770
1347.182293	155.330432	48.812775
1343.907465	143.883801	48.817780
1340.125304	159.947035	48.822785
1336.715043	153.877977	48.827789
1333.607048	151.279790	48.832794
1329.743364	152.764184	48.837799
1326.525626	150.388827	48.842804
1322.962001	143.894521	48.847809
1318.907222	142.175396	48.852813
1315.685574	147.526736	48.857818
1312.128273	149.061253	48.862823
1308.965572	147.319546	48.867828
1305.388406	154.691285	48.872833
1301.710277	155.463254	48.877837
1297.841196	146.469888	48.882842
1294.175678	142.158771	48.887847
1291.279714	153.059119	48.892852
1288.119848	153.629737	48.897857
1284.345055	153.537299	48.902861
1281.166737	151.054544	48.907866
1277.205880	154.044335	48.912871
1273.557087	150.708231	48.917876
1270.158660	145.630793	48.922881
1266.453340	154.962035	48.927885
1263.212467	148.569091	48.932890
1259.873361	143.529829	48.937895
1256.390604	155.107354	48.942900
1252.604097	148.508759	48.947905
1249.188409	144.958999	48.952909
1246.056701	144.917766	48.957914
1242.166477	148.776057	48.962919
1238.438712	145.271993	48.967924
1235.026525	151.599171	48.972929
1231.621520	147.993959	48.977933
1228.389478	145.332969	48.982938
1224.506703	145.754180	48.987943
1221.027303	150.516296	48.992948
1217.756993	150.885922	48.997953
1214.171364	149.412942	49.002957
1210.650901	142.949892	49.007962
1207.161023	149.706866	49.012967
1203.633098	137.252696	49.017972
1200.479894	142.299116	49.022977
1196.758941	139.202138	49.027981
1193.123498	143.536263	49.032986
1189.500005	147.843209	49.037991
1186.334895	148.209031	49.042996
1182.660802	147.316237	49.048001
1179.064107	150.635041	49.053005
1175.716372	143.135703	49.058010
1171.930894	145.655141	49.063015
1168.487104	147.890127	49.068020
1165.317096	143.156630	49.073025
1161.600271	146.029164	49.078029
1158.272969	135.359645	49.083034
1154.288900	140.722821	49.088039
1151.179116	135.986232	49.093044
1147.285827	146.109415	49.098049
1144.103678	145.595210	49.103053
1140.739881	141.578613	49.108058
1137.285944	147.456764	49.113063
1133.679172	137.988969	49.118068
1130.294102	140.173645	49.123073
1126.197634	140.508125	49.128077
1122.987263	137.964006	49.133082
1119.408762	146.259844	49.138087
1116.376498	139.030689	49.143092
1112.474744	144.099413	49.148097
1109.024139	147.718079	49.153101
1105.931485	142.029673	49.158106
1102.230120	147.639682	49.163111
1098.758028	138.906971	49.168116
1095.145361	138.703801	49.173121
1091.659987	145.555018	49.178125
1087.961362	141.021375	49.183130
1084.401877	143.581394	49.188135
1081.282791	147.056413	49.193140
1077.687365	153.981816	49.198145
1073.788759	147.755201	49.203149
1070.695515	141.725208	49.208154
1067.141948	144.698767	49.213159
1063.360625	149.391143	49.218164
1059.762469	135.223753	49.223169
1056.177579	142.112707	49.228173
1053.445153	138.538307	49.233178
1049.663790	143.816000	49.238183
1046.096573	140.305863	49.243188
1042.760117	142.644311	49.248193
1039.075465	145.587783	49.253197
1035.871514	132.507156	49.258202
1031.987249	134.573865	49.263207
1028.319061	135.176697	49.268212
1025.140728	145.399953	49.273217
1021.562142	149.092471	49.278221
1018.054799	126.466642	49.283226
1014.457227	139.909869	49.288231
1011.042922	144.117682	49.293236
1007.578606	143.211095	49.298241
1003.614063	142.996613	49.303245
1000.541087	137.811379	49.308250
997.216074	143.340348	49.313255
993.695110	141.034735	49.318260
990.152385	135.787011	49.323265
986.898059	138.735891	49.328269
983.091275	140.388683	49.333274
979.173668	139.553081	49.338279
975.852206	142.559934	49.343284
972.391351	134.202017	49.348289
968.804976	144.112682	49.353293
965.651595	126.987134	49.358298
961.988401	133.360018	49.363303
958.199122	141.473766	49.368308
954.952910	133.094904	49.373313
951.512913	132.466111	49.378317
947.917010	122.493661	49.383322
944.409931	140.696941	49.388327
940.664473	132.111514	49.393332
937.269059	136.373339	49.398337
933.935270	133.060822	49.403341
930.793259	133.087746	49.408346
927.283666	138.797500	49.413351
923.432433	137.584525	49.418356
920.204960	134.233219	49.423361
915.984692	134.489096	49.428365
912.484084	133.521787	49.433370
909.422303	140.177014	49.438375
906.116462	132.759820	49.443380
902.748141	140.038863	49.448385
898.914469	142.572276	49.453389
895.467886	135.888983	49.458394
892.151084	134.465785	49.463399
888.421685	141.823519	49.468404
885.478227	131.992544	49.473409
881.161234	139.186018	49.478413
877.965204	131.631417	49.483418
874.281616	137.982213	49.488423
870.620138	136.891411	49.493428
867.228071	128.611360	49.498433
863.491086	140.418617	49.503437
860.322984	143.085111	49.508442
857.027559	144.455395	49.513447
853.409550	135.498866	49.518452
849.993941	134.363245	49.523457
846.200664	135.688101	49.528461
842.586744	134.887262	49.533466
839.395276	143.132070	49.538471
835.947481	142.191322	49.543476
832.691975	141.236285	49.548481
828.827999	143.676392	49.553485
825.434666	136.314060	49.558490
821.708065	141.823708	49.563495
818.375970	131.170913	49.568500
814.671365	133.459516	49.573505
811.083632	134.416835	49.578509
808.063279	131.956972	49.583514
804.662025	133.378647	49.588519
801.074098	134.649218	49.593524
797.239075	134.256351	49.598529
793.330271	137.649473	49.603533
790.147714	129.194274	49.608538
786.820900	137.893732	49.613543
783.490152	133.024198	49.618548
780.390197	131.598723	49.623553
776.218197	141.974480	49.628557
772.600677	130.195790	49.633562
768.911061	139.084947	49.638567
765.619026	140.536990	49.643572
762.892499	133.421450	49.648577
758.923872	138.880434	49.653581
755.724455	126.890745	49.658586
751.659158	136.411387	49.663591
747.903720	128.650208	49.668596
744.766770	131.656715	49.673601
740.992523	132.045308	49.678605
737.680451	127.527217	49.683610
734.117104	130.701744	49.688615
730.797257	129.035469	49.693620
727.302935	127.940696	49.698625
723.524475	136.119266	49.703629
720.442044	126.044364	49.708634
716.788112	131.808426	49.713639
713.326355	128.525527	49.718644
709.977848	129.303049	49.723649
706.147706	134.246809	49.728653
703.020702	123.400598	49.733658
699.451009	131.448402	49.738663
695.331384	138.623697	49.743668
692.306348	136.509463	49.748673
688.669207	134.263295	49.753677
685.273259	123.506667	49.758682
681.363823	133.369927	49.763687
678.184216	126.005831	49.768692
674.502557	117.701617	49.773697
670.871637	127.774364	49.778701
668.226955	118.016919	49.783706
664.381602	126.550836	49.788711
661.020271	123.603414	49.793716
657.261895	130.276049	49.798721
653.779346	124.987410	49.803725
650.411684	126.875287	49.808730
646.649209	128.793359	49.813735
643.083723	124.403581	49.818740
639.379289	126.771318	49.823745
636.047111	124.053463	49.828749
632.648301	119.511034	49.833754
629.251887	117.182900	49.838759
625.541100	122.437031	49.843764
621.932981	119.676975	49.848769
618.552533	123.237356	49.853773
615.247538	121.091065	49.858778
611.900936	129.081810	49.863783
608.204155	129.350755	49.868788
604.674732	125.236924	49.873793
601.155913	125.867149	49.878797
597.801498	121.972690	49.883802
594.139082	134.533988	49.888807
590.490233	128.271656	49.893812
587.441707	127.230506	49.898817
583.379716	133.504622	49.903821
580.241620	118.547252	49.908826
576.332186	119.156405	49.913831
572.959375	121.035624	49.918836
569.672408	120.496905	49.923841
566.295385	129.302363	49.928845
562.923390	123.430126	49.933850
558.922358	130.156619	49.938855
555.334942	132.297251	49.943860
552.327790	118.872816	49.948865
548.516552	124.310390	49.953869
545.054313	125.656287	49.958874
541.056157	123.473053	49.963879
538.007676	114.813467	49.968884
534.833109	113.978742	49.973889
530.905843	112.869597	49.978893
527.905663	120.236621	49.983898
524.277579	136.405630	49.988903
520.288458	120.857065	49.993908
517.018013	116.550849	49.998913
513.448748	131.229984	50.003917
510.253538	121.258261	50.008922
506.600573	124.576621	50.013927
503.214162	132.776119	50.018932
499.183264	120.306168	50.023937
495.855810	123.143271	50.028941
492.674722	128.950412	50.033946
488.913659	128.391065	50.038951
485.285091	124.571229	50.043956
482.539435	119.467809	50.048961
478.431710	129.409651	50.053965
475.247892	116.278684	50.058970
471.835534	120.650883	50.063975
468.200900	127.006804	50.068980
464.592046	121.513401	50.073985
460.649298	131.337660	50.078989
457.437884	122.346114	50.083994
453.712365	118.063745	50.088999
450.320869	122.315624	50.094004
446.936959	116.888238	50.099009
443.447006	121.275765	50.104013
440.310152	122.447346	50.109018
436.890505	129.044856	50.114023
432.956462	131.591010	50.119028
429.705037	119.429284	50.124033
425.559806	132.369980	50.129037
422.453008	122.811561	50.134042
418.999242	129.446059	50.139047
415.666495	124.048636	50.144052
412.267587	127.219669	50.149057
408.156719	126.136172	50.154061
404.677754	123.242080	50.159066
401.367279	129.689621	50.164071
397.947618	131.421215	50.169076
394.650751	120.769430	50.174081
390.879090	119.101291	50.179085
387.796880	117.359960	50.184090
383.792660	120.296782	50.189095
379.956779	127.291707	50.194100
376.631587	118.204124	50.199105
373.400862	120.459797	50.204109
370.086476	113.844621	50.209114
366.516802	120.206219	50.214119
362.735063	123.424581	50.219124
359.563693	115.347476	50.224129
355.829419	114.625800	50.229133
352.504975	112.808530	50.234138
348.957075	124.194004	50.239143
345.349253	118.399933	50.244148
342.051476	114.977606	50.249153
338.460410	118.055375	50.254157
334.837632	113.108388	50.259162
331.416434	116.558190	50.264167
327.903202	118.905589	50.269172
324.414872	113.058010	50.274177
320.592233	122.736947	50.279181
317.260077	115.175437	50.284186
314.058740	116.477386	50.289191
310.408808	126.755708	50.294196
307.132489	118.767831	50.299201
303.314031	127.629862	50.304205
299.501436	112.879533	50.309210
296.063271	108.504767	50.314215
292.312805	113.338121	50.319220
289.348834	109.436413	50.324225
285.927235	117.413690	50.329229
282.639976	111.487175	50.334234
278.996421	118.338110	50.339239
275.657144	114.175654	50.344244
272.156197	113.493394	50.349249
268.323831	122.300665	50.354253
264.959751	117.177140	50.359258
261.206524	124.203453	50.364263
257.355737	118.494941	50.369268
254.268300	106.449989	50.374273
250.597686	113.460197	50.379277
247.825393	113.783785	50.384282
243.776632	118.657561	50.389287
239.878423	112.004184	50.394292
236.844578	108.698745	50.399297
233.548681	121.044534	50.404301
229.869545	109.993967	50.409306
226.498241	116.767468	50.414311
222.931687	115.203315	50.419316
219.807722	108.979160	50.424321
215.653951	115.780330	50.429325
212.218832	112.968038	50.434330
208.982093	110.077213	50.439335
204.820104	110.786203	50.444340
201.729978	109.422673	50.449345
197.874400	115.196359	50.454349
194.712229	112.932944	50.459354
190.972077	107.871533	50.464359
187.601007	108.421824	50.469364
183.857547	114.114674	50.474369
180.471649	122.871015	50.479373
177.086509	117.342697	50.484378
173.665171	115.379323	50.489383
170.031556	116.907235	50.494388
166.926648	112.483479	50.499393
163.485360	113.620590	50.504397
159.801407	115.475936	50.509402
156.195461	119.951341	50.514407
152.754497	119.098378	50.519412
149.159688	112.081136	50.524417
145.700765	115.824820	50.529421
142.118784	110.469728	50.534426
138.810387	118.562197	50.539431
135.513938	116.614074	50.544436
131.864846	110.570303	50.549441
127.957109	119.474854	50.554445
124.820586	113.477333	50.559450
121.323225	113.360892	50.564455
117.452630	128.277169	50.569460
114.383442	115.277113	50.574465
110.602498	123.367696	50.579469
107.046859	114.708654	50.584474
103.894197	112.674741	50.589479
100.224050	124.585650	50.594484
96.659979	115.348959	50.599489
92.860241	116.624516	50.604493
89.202296	119.573652	50.609498
85.944077	114.971464	50.614503
82.283228	111.106248	50.619508
79.198093	106.201698	50.624513
75.657311	113.840205	50.629517
72.203178	106.522548	50.634522
68.622811	109.864502	50.639527
65.144216	113.937168	50.644532
61.943809	103.564670	50.649537
57.846256	114.090371	50.654541
54.286854	105.865389	50.659546
51.129182	113.624216	50.664551
47.589667	120.389330	50.669556
44.057077	113.862269	50.674561
40.673260	113.199717	50.679565
37.443386	112.339039	50.684570
34.018625	102.147241	50.689575
30.105463	106.923927	50.694580
26.385805	101.081093	50.699585
22.691916	107.582494	50.704589
19.520728	107.769334	50.709594
15.978422	110.532700	50.714599
12.576741	107.085659	50.719604
9.589043	109.739984	50.724609
5.899981	109.372049	50.729613
2.124126	109.979506	50.734618