Thu Aug 25 16:41:44 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
0.690247	104.583791	0.000000
0.466193	99.946014	0.005005
0.152265	101.017144	0.010010
0.557623	95.534095	0.015014
0.426604	96.677807	0.020019
0.245319	92.340218	0.025024
0.191498	91.668475	0.030029
0.025544	78.346489	0.035034
-0.084891	78.237279	0.040038
-0.467751	55.796461	0.045043
-0.781825	66.605740	0.050048
-0.727901	47.443781	0.055053
-1.112125	49.193481	0.060058
-1.487810	28.074034	0.065062
-1.676727	23.769296	0.070067
-2.329871	20.005534	0.075072
-2.568346	4.303152	0.080077
-2.993697	10.846083	0.085082
-3.070723	-6.077494	0.090086
-3.966674	-4.905686	0.095091
-4.124822	-4.219640	0.100096
-4.043367	-2.479634	0.105101
-4.483185	-3.692012	0.110106
-4.073140	-5.907587	0.115110
-4.537347	-11.991516	0.120115
-4.858564	-6.626011	0.125120
-5.243946	-10.055231	0.130125
-6.057370	-8.254108	0.135130
-6.668308	-7.987502	0.140134
-6.373929	-20.081229	0.145139
-6.510972	-3.446754	0.150144
-6.955888	-10.761250	0.155149
-7.062261	-2.676925	0.160154
-7.215166	-6.892385	0.165158
-7.122828	-2.455386	0.170163
-7.712177	-1.584718	0.175168
-8.010698	-1.686604	0.180173
-8.286842	-6.629405	0.185178
-8.594338	-1.870329	0.190182
-8.857682	-4.730210	0.195187
-8.968203	9.078037	0.200192
-8.942419	-2.948307	0.205197
-9.213794	-1.760463	0.210202
-9.794383	-8.525352	0.215206
-10.010448	-7.229115	0.220211
-10.140677	-3.146388	0.225216
-10.153238	-14.230239	0.230221
-10.781274	-8.497120	0.235226
-11.174288	-9.941459	0.240230
-11.159265	-12.892409	0.245235
-11.340174	-3.366382	0.250240
-11.342852	-0.958293	0.255245
-11.804189	2.704913	0.260250
-12.570496	-5.340680	0.265254
-12.955888	-8.504141	0.270259
-13.045692	-6.085565	0.275264
-12.841686	-5.041809	0.280269
-13.009235	-6.568931	0.285274
-13.032916	-5.714128	0.290278
-13.333129	-5.635413	0.295283
-14.443647	-6.331412	0.300288
-14.305690	-9.453486	0.305293
-14.614211	-9.278557	0.310298
-14.644817	-7.663363	0.315302
-14.687616	-7.409845	0.320307
-15.480761	-5.532804	0.325312
-15.501490	-6.288823	0.330317
-15.997492	-3.230795	0.335322
-16.171586	-5.823083	0.340326
-16.119850	-5.381895	0.345331
-15.987000	4.711911	0.350336
-16.648644	-10.920988	0.355341
-17.258982	-2.991820	0.360346
-17.472322	-6.055688	0.365350
-17.002387	-13.950125	0.370355
-17.260795	-4.127215	0.375360
-17.920725	-10.949274	0.380365
-18.430389	-7.591711	0.385370
-18.552437	-8.913989	0.390374
-18.510617	-8.597799	0.395379
-18.802943	-2.173793	0.400384
-19.297204	-9.660891	0.405389
-20.031559	-2.158382	0.410394
-20.354204	-9.337010	0.415398
-20.482589	-4.849610	0.420403
-20.570949	-0.805081	0.425408
-20.163923	-7.351388	0.430413
-20.437850	-6.394099	0.435418
-20.402239	-5.460000	0.440422
-20.967123	-18.248002	0.445427
-21.519814	-12.074271	0.450432
-21.464043	-15.199286	0.455437
-21.383495	-15.306781	0.460442
-22.334491	-4.296508	0.465446
-22.991352	-10.356578	0.470451
-23.264251	-13.806584	0.475456
-23.231882	-6.177437	0.480461
-23.795100	-10.692439	0.485466
-23.456427	-4.139510	0.490470
-23.162575	-12.870067	0.495475
-23.613980	-9.489996	0.500480
-23.720021	-12.994620	0.505485
-23.783857	-6.498848	0.510490
-24.753501	-3.872811	0.515494
-25.115414	-13.177667	0.520499
-25.482542	-5.612475	0.525504
-25.623826	-4.074853	0.530509
-25.682371	-6.226498	0.535514
-25.669345	-13.982905	0.540518
-26.114532	-4.358522	0.545523
-26.970065	-5.923380	0.550528
-27.156390	0.300519	0.555533
-27.182551	-2.463645	0.560538
-27.497369	0.692546	0.565542
-27.520195	0.269051	0.570547
-27.578732	-6.833900	0.575552
-27.466464	-10.306291	0.580557
-28.227260	-13.157828	0.585562
-28.703273	-6.455104	0.590566
-28.845735	-7.062335	0.595571
-29.015608	-8.633385	0.600576
-28.968275	-3.467996	0.605581
-29.760517	1.870073	0.610586
-30.448175	-7.557752	0.615590
-30.613863	-10.417113	0.620595
-29.940016	-2.648029	0.625600
-29.864643	-11.508871	0.630605
-30.375237	2.570863	0.635610
-31.010848	0.196422	0.640614
-31.615808	-8.333195	0.645619
-31.786125	2.361771	0.650624
-32.262226	-2.758508	0.655629
-32.335532	-4.135880	0.660634
-32.180517	-6.640528	0.665638
-32.140887	-0.018596	0.670643
-32.238569	7.232298	0.675648
-32.696491	-3.775448	0.680653
-33.281746	-3.642579	0.685658
-33.684363	-4.670958	0.690662
-33.543560	-2.139817	0.695667
-34.076336	-3.970383	0.700672
-34.711504	-4.203018	0.705677
-35.034490	-4.212484	0.710682
-35.112733	-1.077543	0.715686
-35.299320	-6.328605	0.720691
-35.194870	-1.469560	0.725696
-34.955345	-8.432549	0.730701
-35.116318	-7.622673	0.735706
-35.671103	-9.196688	0.740710
-36.159284	-14.596646	0.745715
-36.670412	-9.501944	0.750720
-36.553859	-2.461793	0.755725
-37.457407	5.415244	0.760730
-38.054116	-7.130493	0.765734
-37.998745	-6.031811	0.770739
-38.132865	2.439679	0.775744
-37.925254	-0.348459	0.780749
-38.098445	-3.206645	0.785754
-38.146682	-2.151840	0.790758
-38.295451	-9.655105	0.795763
-39.113395	-4.759102	0.800768
-39.138623	-4.236252	0.805773
-39.177018	-12.997008	0.810778
-39.560350	1.711357	0.815782
-40.299986	-4.101624	0.820787
-40.787657	0.872346	0.825792
-40.868338	-2.269255	0.830797
-40.807394	-4.379511	0.835802
-41.191486	2.413217	0.840806
-41.022402	-10.005733	0.845811
-41.427614	5.130008	0.850816
-41.404479	-1.390951	0.855821
-41.995345	0.147512	0.860826
-42.287004	4.448524	0.865830
-42.208773	-1.982991	0.870835
-42.605981	-4.995901	0.875840
-43.098481	-3.226077	0.880845
-43.784950	3.943063	0.885850
-43.692218	2.406797	0.890854
-43.688160	-0.931581	0.895859
-43.885414	-3.498093	0.900864
-43.719020	-4.318234	0.905869
-44.679591	-5.480651	0.910874
-45.270842	-4.869113	0.915878
-45.512821	0.275169	0.920883
-45.439315	-5.076758	0.925888
-45.700115	-3.912717	0.930893
-45.467326	-10.944252	0.935898
-45.824344	-8.505954	0.940902
-46.261510	-17.191570	0.945907
-46.918699	-12.779503	0.950912
-47.060428	-7.100436	0.955917
-46.945231	-8.943943	0.960922
-47.132935	-2.713502	0.965926
-46.958260	-8.517881	0.970931
-47.968039	0.375552	0.975936
-47.929697	-1.588793	0.980941
-48.055341	-9.627194	0.985946
-48.375402	-2.784389	0.990950
-49.353797	-9.445811	0.995955
-49.604770	-6.255333	1.000960
-49.460457	-6.046951	1.005965
-49.821257	-2.896211	1.010970
-49.468134	-11.389281	1.015974
-49.584829	-7.716803	1.020979
-49.797986	-3.137026	1.025984
-50.541561	-5.500875	1.030989
-51.050189	-8.977220	1.035994
-51.163141	-0.774806	1.040998
-50.868257	-7.790762	1.046003
-51.264936	-6.032788	1.051008
-52.124398	-1.234682	1.056013
-52.677966	-2.356467	1.061018
-52.998357	-4.062121	1.066022
-52.565374	-8.594007	1.071027
-53.068514	-2.225555	1.076032
-52.643848	-8.145035	1.081037
-53.083099	-1.688516	1.086042
-53.204453	-6.073434	1.091046
-53.686757	-4.257749	1.096051
-54.155804	-3.424912	1.101056
-53.959237	-1.965537	1.106061
-54.534981	-0.344020	1.111066
-55.290664	-4.199273	1.116070
-55.662589	-5.377993	1.121075
-55.702897	-3.653711	1.126080
-55.676393	-10.694052	1.131085
-55.568768	-11.992205	1.136090
-56.063070	-6.336987	1.141094
-55.846864	-9.189746	1.146099
-56.496668	-7.252904	1.151104
-56.887866	-10.428107	1.156109
-56.899650	-12.330812	1.161114
-57.333459	-9.016772	1.166118
-57.100063	-17.934007	1.171123
-58.016449	-6.074940	1.176128
-58.507710	-10.778384	1.181133
-58.296138	-8.444997	1.186138
-58.532015	-0.669414	1.191142
-58.303408	-12.667415	1.196147
-58.804463	-11.943458	1.201152
-59.736548	-17.580742	1.206157
-59.960418	-10.433472	1.211162
-60.349627	-7.059981	1.216166
-60.096028	-16.486585	1.221171
-60.606509	-15.134724	1.226176
-60.421713	-11.170964	1.231181
-60.470771	-5.889234	1.236186
-60.925768	-10.383223	1.241190
-61.277179	-19.101256	1.246195
-61.454051	-9.620160	1.251200
-61.634898	-11.926647	1.256205
-62.126405	-7.540540	1.261210
-63.026095	-7.143264	1.266214
-63.041396	-14.240329	1.271219
-63.255112	-4.221944	1.276224
-63.146572	-11.221355	1.281229
-63.220365	-16.322406	1.286234
-63.522982	-11.064222	1.291238
-63.435546	-12.969819	1.296243
-63.754175	-2.719858	1.301248
-63.901601	-18.015695	1.306253
-64.598785	-10.079249	1.311258
-65.019847	-8.627504	1.316262
-64.756624	-11.569887	1.321267
-65.615044	-14.099237	1.326272
-66.160392	-10.346939	1.331277
-66.113777	-3.979207	1.336282
-66.264006	-8.732924	1.341286
-66.369169	-12.658465	1.346291
-66.371594	-12.256248	1.351296
-66.122887	-10.627873	1.356301
-66.680115	-7.351442	1.361306
-67.828988	-9.243657	1.366310
-67.683136	-7.421994	1.371315
-67.703484	-2.923049	1.376320
-68.024068	-10.200071	1.381325
-68.370291	-4.384557	1.386330
-69.161110	0.358502	1.391334
-69.245701	-11.457545	1.396339
-69.357927	-11.980927	1.401344
-69.603343	-20.282130	1.406349
-69.716713	-15.085238	1.411354
-69.577197	-4.454647	1.416358
-69.555062	-21.422210	1.421363
-70.284138	-15.733372	1.426368
-70.406302	-15.258609	1.431373
-71.127198	-17.556405	1.436378
-71.479861	-9.145593	1.441382
-70.528399	-12.012318	1.446387
-71.279378	-12.707697	1.451392
-71.867254	-18.253381	1.456397
-72.347355	-14.103181	1.461402
-72.346605	-19.620873	1.466406
-72.379370	-19.675813	1.471411
-73.715266	-4.410072	1.476416
-73.737049	-13.556244	1.481421
-73.215968	-8.819433	1.486426
-73.656815	-2.081089	1.491430
-73.433112	-8.168397	1.496435
-73.773296	-10.978267	1.501440
-73.878601	-18.045408	1.506445
-74.517069	-14.847998	1.511450
-75.108718	-14.331308	1.516454
-75.148530	-22.386314	1.521459
-75.452927	-8.813467	1.526464
-75.541491	-9.245644	1.531469
-76.216809	-6.988425	1.536474
-76.665240	-7.380032	1.541478
-76.563879	-6.041783	1.546483
-76.917758	-11.696900	1.551488
-76.786574	-5.222197	1.556493
-76.758774	-9.709577	1.561498
-77.150417	-7.408223	1.566502
-77.826288	-16.904322	1.571507
-78.143615	-12.858721	1.576512
-78.236139	-16.308512	1.581517
-78.229304	-7.397206	1.586522
-78.609938	-8.229709	1.591526
-78.372782	-9.915156	1.596531
-79.407076	-4.865027	1.601536
-80.058057	-9.856656	1.606541
-80.014146	-10.100781	1.611546
-80.273556	-4.972753	1.616550
-80.233357	-7.231618	1.621555
-80.213091	-10.594679	1.626560
-79.981564	-7.033713	1.631565
-80.488679	-11.665067	1.636570
-80.581250	-17.807219	1.641574
-81.014967	-9.851944	1.646579
-81.502192	-5.352611	1.651584
-81.833670	-9.027554	1.656589
-82.218285	-4.889150	1.661594
-82.739630	-1.213377	1.666598
-83.040489	-4.560923	1.671603
-82.797494	-4.848898	1.676608
-82.853951	-7.067308	1.681613
-83.305091	-4.370651	1.686618
-84.147619	-6.127366	1.691622
-84.026316	-6.285541	1.696627
-84.278001	-1.367531	1.701632
-84.542120	-11.478647	1.706637
-84.291642	-14.941055	1.711642
-84.351401	-1.330605	1.716646
-85.304275	-6.758987	1.721651
-85.842119	-3.745021	1.726656
-85.730211	-6.992728	1.731661
-86.112818	-3.208980	1.736666
-86.330269	4.462476	1.741670
-85.908365	-1.867863	1.746675
-86.882895	4.283387	1.751680
-87.210751	1.104587	1.756685
-87.760469	-2.368481	1.761690
-87.843412	8.489964	1.766694
-87.618938	-2.817690	1.771699
-87.563520	-1.839239	1.776704
-87.893119	4.473549	1.781709
-87.565665	-6.657250	1.786714
-88.410942	1.194838	1.791718
-88.248923	-10.258050	1.796723
-89.519275	-5.528438	1.801728
-90.111494	-9.570651	1.806733
-90.275023	-12.354416	1.811738
-90.279770	-11.167221	1.816742
-89.870538	-12.762571	1.821747
-90.239855	-11.303114	1.826752
-90.336738	-9.240936	1.831757
-90.335422	-4.735895	1.836762
-91.376198	0.106443	1.841766
-91.582685	-12.209360	1.846771
-92.043621	-6.825127	1.851776
-92.130803	-7.431527	1.856781
-92.371650	-13.442877	1.861786
-92.206414	-0.234679	1.866790
-91.942556	-5.809421	1.871795
-92.770092	-2.512779	1.876800
-93.019682	-1.976920	1.881805
-92.761316	-2.147081	1.886810
-93.923445	-1.455578	1.891814
-94.241832	-6.818862	1.896819
-94.485319	-4.970994	1.901824
-94.654196	-6.918687	1.906829
-94.635653	-12.844131	1.911834
-94.651675	-10.772477	1.916838
-95.102489	-9.958313	1.921843
-95.894100	2.808193	1.926848
-96.135190	-3.997229	1.931853
-96.094090	-13.640473	1.936858
-96.301915	-9.757563	1.941862
-96.074360	-3.437168	1.946867
-96.531300	2.557050	1.951872
-96.425675	-4.438742	1.956877
-97.064282	-5.534543	1.961882
-97.552104	2.600058	1.966886
-97.389973	-8.232749	1.971891
-97.671783	-3.088556	1.976896
-98.243454	-4.849746	1.981901
-98.811076	-11.274967	1.986906
-99.765571	-14.605511	1.991910
-99.518431	-18.722295	1.996915
-98.863123	-8.202842	2.006912
-98.901066	-8.659322	2.016909
-98.047790	-11.374722	2.026906
-98.049452	-8.368124	2.036902
-97.790965	-6.571215	2.046899
-96.854612	-8.989187	2.056896
-96.450001	-11.007056	2.066893
-96.169666	-12.742523	2.076890
-95.352739	-8.454512	2.086886
-95.272935	-9.021310	2.096883
-94.466630	-2.384278	2.106880
-94.099023	-10.063581	2.116877
-92.925241	-9.224223	2.126874
-92.546335	-8.139935	2.136870
-92.498951	-12.376324	2.146867
-92.650862	-3.320987	2.156864
-91.467926	-6.382651	2.166861
-90.997426	-3.133254	2.176858
-90.305155	-4.211005	2.186854
-89.884984	-1.885062	2.196851
-89.888231	-3.224465	2.206848
-88.854839	-7.634363	2.216845
-88.443442	-2.573214	2.226842
-87.938885	-9.646748	2.236838
-87.362102	-12.116083	2.246835
-87.133886	-9.886775	2.256832
-85.932331	-9.742352	2.266829
-85.585212	-9.273976	2.276826
-85.496834	-13.665676	2.286822
-85.332197	-9.060044	2.296819
-84.416275	-7.866665	2.306816
-84.012305	-11.129387	2.316813
-83.596393	-13.573514	2.326810
-82.877887	-12.944752	2.336806
-82.643302	-14.422792	2.346803
-81.439223	-14.760273	2.356800
-80.940565	-15.798182	2.366797
-81.091128	-10.316359	2.376794
-80.650622	-11.246954	2.386790
-79.881664	-13.128675	2.396787
-79.656366	-11.918948	2.406784
-79.026944	-13.512708	2.416781
-78.173161	-22.867935	2.426778
-78.165006	-15.009777	2.436774
-77.174638	-13.793217	2.446771
-77.087699	-9.498527	2.456768
-76.555137	-14.960858	2.466765
-75.679606	-10.656686	2.476762
-75.438904	-6.737717	2.486758
-75.079018	-16.303830	2.496755
-74.317212	-13.502392	2.506752
-74.162038	-12.075768	2.516749
-73.290204	-12.383363	2.526746
-72.949892	-9.211769	2.536742
-72.634141	-12.333954	2.546739
-71.619953	-18.318413	2.556736
-71.611520	-10.156185	2.566733
-70.709143	-11.814890	2.576730
-70.166614	-6.245262	2.586726
-69.970477	-7.479691	2.596723
-69.778883	-9.936187	2.606720
-68.639335	-7.567738	2.616717
-68.524951	-7.034384	2.626714
-67.721029	-13.879223	2.636710
-67.226451	-7.975797	2.646707
-67.382873	-4.542634	2.656704
-66.456480	-10.804778	2.666701
-65.827989	-9.807114	2.676698
-65.071434	-8.031226	2.686694
-64.603392	-8.757058	2.696691
-64.233587	-7.189834	2.706688
-64.121987	-11.607349	2.716685
-63.302940	-14.082964	2.726682
-62.760070	-17.316763	2.736678
-62.694963	-8.225740	2.746675
-62.095525	-15.041706	2.756672
-61.369781	-15.627351	2.766669
-60.647967	-13.716138	2.776666
-59.701215	-12.730328	2.786662
-59.825385	-7.867197	2.796659
-59.556834	-13.424377	2.806656
-59.102132	-13.866183	2.816653
-58.209058	-4.322011	2.826650
-58.006593	-12.171843	2.836646
-57.242207	-15.472030	2.846643
-56.847561	-11.358603	2.856640
-56.676727	-8.572269	2.866637
-55.681022	-5.351311	2.876634
-55.238752	-10.555573	2.886630
-55.171717	-7.676947	2.896627
-54.526401	-5.240559	2.906624
-53.821796	-5.810221	2.916621
-53.188631	-3.552494	2.926618
-52.624893	-11.731367	2.936614
-52.441868	-15.060838	2.946611
-51.863411	-11.860033	2.956608
-51.041385	-4.724944	2.966605
-50.860994	-12.020116	2.976602
-50.485320	-8.603803	2.986598
-49.496348	-7.320496	2.996595
-49.502127	-7.249823	3.006592
-49.184341	-13.505302	3.016589
-48.174655	-15.614810	3.026586
-47.988223	-13.290254	3.036582
-47.505186	-13.635129	3.046579
-46.710960	-11.656065	3.056576
-46.583783	-10.475312	3.066573
-45.543052	-14.496712	3.076570
-44.689696	-11.963040	3.086566
-44.844628	-11.976702	3.096563
-44.808850	-6.726815	3.106560
-43.623090	-11.204932	3.116557
-43.725159	-5.451937	3.126554
-42.593761	-6.240526	3.136550
-42.212698	-7.770028	3.146547
-42.054292	-12.112513	3.156544
-41.194741	-11.626224	3.166541
-40.967519	-6.013524	3.176538
-40.280647	-5.389305	3.186534
-39.388962	-2.345282	3.196531
-39.190029	-2.664648	3.206528
-39.016762	-3.638900	3.216525
-38.589177	-3.458731	3.226522
-38.036443	-6.089022	3.236518
-37.050225	-9.268744	3.246515
-36.538239	-6.659408	3.256512
-36.504640	1.448199	3.266509
-36.210451	-1.613588	3.276506
-35.131924	-1.627280	3.286502
-34.816790	-5.756737	3.296499
-33.830443	-6.367375	3.306496
-33.232388	1.360351	3.316493
-33.876942	-0.366415	3.326490
-33.157528	-1.185486	3.336486
-32.162323	-3.384591	3.346483
-31.881633	-1.347235	3.356480
-31.143094	-1.732143	3.366477
-30.467231	-4.587635	3.376474
-30.420876	-8.025574	3.386470
-29.995496	-6.619112	3.396467
-29.100334	-7.643118	3.406464
-28.679453	-3.033281	3.416461
-28.524354	-2.243376	3.426458
-27.712250	-5.142390	3.436454
-27.167262	-4.679672	3.446451
-26.856112	-3.606939	3.456448
-26.298586	-5.442858	3.466445
-26.200193	-1.666314	3.476442
-25.127494	-1.945188	3.486438
-24.947033	-2.458064	3.496435
-23.997147	-1.593118	3.506432
-23.311165	-4.656104	3.516429
-23.292723	-7.481448	3.526426
-23.148102	-1.624552	3.536422
-22.424444	-3.334445	3.546419
-22.115308	-2.730234	3.556416
-21.136957	-4.837998	3.566413
-20.529549	-3.707146	3.576410
-20.450672	-0.424892	3.586406
-19.468391	-1.997909	3.596403
-18.927565	-1.974866	3.606400
-19.068904	0.005071	3.616397
-18.403421	0.160638	3.626394
-17.265730	0.400608	3.636390
-16.940898	-4.804262	3.646387
-17.129981	0.702609	3.656384
-16.622508	-1.952269	3.666381
-15.879396	2.169922	3.676378
-14.793182	-8.267112	3.686374
-14.564722	-6.785445	3.696371
-14.425986	2.690030	3.706368
-14.085451	-1.896407	3.716365
-12.928578	-4.304574	3.726362
-12.902908	-2.677091	3.736358
-12.240466	-4.991950	3.746355
-11.576760	-4.459133	3.756352
-11.515801	-12.603578	3.766349
-10.606068	-13.591851	3.776346
-9.812374	-14.115279	3.786342
-9.875456	-8.159316	3.796339
-9.490235	-5.416074	3.806336
-8.605353	-9.324354	3.816333
-8.520322	-7.167642	3.826330
-7.506771	-5.413007	3.836326
-6.853396	-6.532175	3.846323
-7.037137	-9.363854	3.856320
-6.542055	-5.019068	3.866317
-5.734673	-2.158236	3.876314
-5.409726	-3.257624	3.886310
-4.872437	4.346579	3.896307
-4.528598	15.532230	3.906304
-3.994127	15.670311	3.916301
-3.610271	28.690208	3.926298
-2.953225	31.213468	3.936294
-2.230380	44.816997	3.946291
-2.192423	50.022211	3.956288
-1.775984	71.153026	3.966285
-1.145023	82.670705	3.976282
-0.876504	96.247256	3.986278
-0.223462	108.946265	3.996275
0.000000	129.827143	4.001280
0.324815	130.057867	4.006285
0.529461	138.216912	4.011290
0.562276	145.393633	4.016294
1.153302	147.556857	4.021299
1.161460	157.265321	4.026304
1.222115	154.471711	4.031309
0.854725	159.028238	4.036314
0.672487	154.880612	4.041318
1.114350	150.853503	4.046323
1.029710	166.752252	4.051328
1.180519	151.254506	4.056333
1.477504	163.799943	4.061338
1.340810	161.913625	4.066342
1.336915	161.607385	4.071347
0.958596	167.848770	4.076352
1.228628	159.833716	4.081357
0.999824	156.111007	4.086362
1.405134	155.446418	4.091366
1.401497	164.280361	4.096371
1.158462	167.773352	4.101376
1.429400	152.367515	4.106381
1.365746	150.115409	4.111386
1.211779	149.298000	4.116390
1.094453	149.879578	4.121395
1.147028	157.451846	4.126400
1.425341	164.637566	4.131405
1.338939	153.587326	4.136410
1.135260	156.267379	4.141414
1.206035	157.268744	4.146419
1.196711	164.815912	4.151424
1.301475	160.718230	4.156429
1.755511	159.172797	4.161434
1.168825	166.038460	4.166438
1.227643	164.127836	4.171443
1.585742	161.961510	4.176448
1.400610	160.810457	4.181453
1.080464	164.230106	4.186458
1.128212	174.802423	4.191462
1.508424	167.251001	4.196467
1.081122	168.880909	4.201472
1.363214	166.574628	4.206477
1.653759	164.963061	4.211482
1.368705	178.026816	4.216486
1.291632	171.496182	4.221491
1.135783	166.717985	4.226496
1.579570	187.814346	4.231501
1.704661	198.001230	4.236506
1.971822	195.728923	4.241510
2.014398	177.160235	4.246515
1.516225	172.027542	4.251520
1.753417	169.604908	4.256525
1.541622	171.780026	4.261530
1.416675	173.223353	4.266534
1.914594	170.611169	4.271539
1.251359	170.053889	4.276544
1.723982	163.525717	4.281549
1.258573	173.340028	4.286554
1.598209	181.702573	4.291558
1.528745	183.342855	4.296563
1.682267	192.892520	4.301568
1.801931	195.689598	4.306573
1.814950	192.887626	4.311578
2.029079	193.243262	4.316582
1.988783	188.266617	4.321587
1.630115	197.266938	4.326592
1.857816	192.153387	4.331597
2.002070	197.275175	4.336602
1.722626	196.328725	4.341606
2.259736	192.163295	4.346611
1.748684	189.823093	4.351616
1.343404	179.597932	4.356621
1.164168	189.617354	4.361626
1.706072	196.676364	4.366630
2.000821	202.537052	4.371635
1.684156	201.137682	4.376640
1.890065	191.538100	4.381645
1.554940	183.709603	4.386650
1.570256	196.055582	4.391654
1.977179	196.460106	4.396659
1.825324	202.147156	4.401664
2.070412	201.102701	4.406669
2.112373	199.859116	4.411674
1.985258	200.489686	4.416678
2.321256	197.890212	4.421683
1.930066	190.383714	4.426688
1.870445	193.585376	4.431693
1.867436	201.163207	4.436698
2.069765	214.603050	4.441702
2.123056	210.228679	4.446707
1.899009	216.518677	4.451712
2.472615	217.906341	4.456717
2.446524	209.842747	4.461722
1.969059	204.921939	4.466726
2.141975	205.511827	4.471731
1.844940	212.708618	4.476736
2.459850	210.676058	4.481741
2.486702	212.181027	4.486746
2.254386	205.608264	4.491750
2.115280	191.377138	4.496755
2.168988	193.893480	4.501760
2.464985	206.701698	4.506765
2.466267	202.692988	4.511770
1.947491	198.417743	4.516774
2.112737	199.755492	4.521779
2.187420	215.689434	4.526784
1.927643	211.031915	4.531789
1.971785	222.810237	4.536794
2.347852	219.688781	4.541798
2.265377	211.298657	4.546803
2.767383	218.113986	4.551808
2.920869	216.577673	4.556813
2.353034	220.501222	4.561818
2.048150	222.361895	4.566822
2.273915	212.968002	4.571827
2.064340	220.141601	4.576832
2.451174	217.806248	4.581837
2.308501	223.156502	4.586842
2.312563	215.518459	4.591846
2.296536	208.573279	4.596851
1.967056	219.283823	4.601856
2.017930	220.601527	4.606861
2.461488	232.719079	4.611866
2.482759	238.733362	4.616870
2.846297	241.359357	4.621875
2.470599	240.206518	4.626880
2.400617	232.152955	4.631885
2.640623	241.274635	4.636890
2.755512	250.191293	4.641894
2.661103	229.400867	4.646899
2.291768	230.331986	4.651904
2.983315	238.981112	4.656909
2.743752	223.509665	4.661914
2.426018	230.899535	4.666918
2.791992	234.660957	4.671923
2.481062	239.600971	4.676928
2.755438	234.274447	4.681933
2.523016	231.346407	4.686938
2.755604	243.930464	4.691942
2.725336	244.865407	4.696947
2.863045	252.133305	4.701952
3.088878	242.818482	4.706957
2.821705	227.199495	4.711962
2.717547	230.199329	4.716966
2.940073	215.266105	4.721971
2.550124	221.585262	4.726976
2.427575	227.460721	4.731981
3.079700	230.832451	4.736986
2.845830	238.525566	4.741990
2.802831	230.799976	4.746995
3.066638	238.459407	4.752000
2.932996	227.033701	4.757005
2.804041	227.265920	4.762010
2.934611	231.431227	4.767014
2.808449	232.514074	4.772019
2.742573	241.142668	4.777024
2.845603	237.937436	4.782029
3.125141	242.677366	4.787034
3.407726	241.753588	4.792038
3.015611	235.876580	4.797043
2.666582	235.896503	4.802048
3.078369	238.163753	4.807053
3.054003	240.815724	4.812058
2.826480	236.241730	4.817062
2.802132	240.573684	4.822067
2.898080	250.461437	4.827072
3.096722	245.526434	4.832077
3.065899	249.286753	4.837082
2.910522	255.793801	4.842086
3.220059	246.244393	4.847091
2.937458	254.185600	4.852096
3.116488	252.205511	4.857101
3.402496	258.383969	4.862106
2.847167	252.529365	4.867110
3.427634	245.136363	4.872115
3.270893	247.717324	4.877120
2.952600	242.059707	4.882125
3.340520	241.631962	4.887130
3.324158	242.438173	4.892134
3.307107	243.978498	4.897139
3.162169	254.929073	4.902144
2.930689	246.467364	4.907149
3.368881	243.355153	4.912154
2.712937	242.584752	4.917158
3.065872	248.819161	4.922163
3.128109	248.012165	4.927168
3.112333	249.792741	4.932173
3.561520	245.935310	4.937178
3.040012	248.620881	4.942182
3.147539	242.431464	4.947187
2.796973	253.249737	4.952192
3.111046	265.529972	4.957197
3.302878	271.640931	4.962202
3.094009	280.190706	4.967206
3.622534	270.239971	4.972211
3.368046	277.534527	4.977216
3.689690	276.392651	4.982221
3.144940	269.979550	4.987226
3.296383	287.337905	4.992230
3.466791	280.069250	4.997235
3.177799	278.472543	5.002240
3.445121	272.020792	5.007245
3.515467	273.667651	5.012250
3.078338	280.133430	5.017254
3.245837	274.178220	5.022259
3.115294	280.159354	5.027264
3.657703	294.590034	5.032269
3.915103	290.386148	5.037274
3.583580	285.217819	5.042278
3.541900	286.872740	5.047283
3.613996	277.078939	5.052288
3.714375	282.612596	5.057293
3.627167	281.541106	5.062298
3.589552	292.876694	5.067302
3.920216	291.078492	5.072307
3.569078	287.156619	5.077312
3.578471	283.880627	5.082317
3.957572	291.221453	5.087322
3.820591	288.189862	5.092326
3.895382	277.297791	5.097331
3.546863	281.443260	5.102336
3.919931	275.098328	5.107341
3.687733	278.801618	5.112346
3.740591	275.079046	5.117350
3.887321	272.676900	5.122355
3.666902	280.934250	5.127360
3.630180	271.815576	5.132365
3.831476	273.375478	5.137370
3.847458	289.755291	5.142374
3.858010	290.598417	5.147379
3.625986	288.802955	5.152384
3.720837	289.939764	5.157389
4.171411	295.329968	5.162394
3.658297	300.323825	5.167398
3.806434	289.097544	5.172403
3.967816	301.601049	5.177408
4.080322	298.331045	5.182413
3.687578	301.651361	5.187418
3.880233	300.751161	5.192422
4.040091	297.201649	5.197427
3.738820	299.773625	5.202432
4.071223	292.353030	5.207437
4.470571	296.327539	5.212442
3.825561	301.579349	5.217446
3.768037	300.800607	5.222451
3.885468	301.415011	5.227456
3.915795	296.829076	5.232461
4.105144	296.103405	5.237466
3.892532	303.340790	5.242470
4.064337	296.499026	5.247475
3.782974	304.319836	5.252480
3.937126	296.303894	5.257485
3.938112	290.096351	5.262490
3.883388	296.593970	5.267494
4.066432	306.116923	5.272499
4.059164	312.341351	5.277504
4.187913	319.506274	5.282509
4.524949	323.851230	5.287514
4.210296	329.364506	5.292518
4.447424	310.553220	5.297523
3.766034	313.238540	5.302528
4.310821	315.621007	5.307533
4.304591	321.699739	5.312538
4.302028	324.522316	5.317542
4.384221	320.073785	5.322547
3.978470	318.289720	5.327552
4.410948	325.321634	5.332557
4.512839	315.383934	5.337562
4.361804	322.646481	5.342566
4.452502	314.064656	5.347571
4.552867	316.190881	5.352576
4.289585	315.748105	5.357581
4.372899	300.687921	5.362586
4.025610	321.041500	5.367590
4.392931	318.895857	5.372595
4.450236	320.443521	5.377600
4.247852	328.255131	5.382605
4.338690	330.550534	5.387610
3.986847	344.346229	5.392614
4.232303	321.756008	5.397619
3.966184	335.785043	5.402624
4.365610	324.367504	5.407629
4.486212	318.641096	5.412634
3.989321	331.532505	5.417638
4.739817	336.894713	5.422643
4.582236	348.236477	5.427648
4.648604	344.533921	5.432653
4.460438	332.063134	5.437658
4.495112	346.253862	5.442662
4.641181	352.685239	5.447667
4.413846	356.748461	5.452672
5.000578	359.795095	5.457677
4.955213	347.574013	5.462682
4.538468	335.585139	5.467686
4.493046	330.558635	5.472691
4.688941	344.426702	5.477696
4.702603	349.565832	5.482701
5.041833	339.008787	5.487706
4.552486	343.461080	5.492710
4.650664	327.857528	5.497715
4.646335	345.373227	5.502720
4.694991	350.484727	5.507725
4.797609	354.758849	5.512730
4.836630	364.117733	5.517734
4.957530	347.064730	5.522739
4.460490	344.155985	5.527744
4.760441	355.071717	5.532749
4.764449	347.971479	5.537754
4.795315	356.259096	5.542758
4.899251	350.171447	5.547763
4.990921	355.526153	5.552768
4.780338	356.125512	5.557773
4.824946	348.088745	5.562778
4.638587	364.408579	5.567782
4.852898	351.314718	5.572787
5.077599	355.427339	5.577792
4.895940	347.324781	5.582797
5.212481	342.659187	5.587802
5.036567	357.832071	5.592806
5.158899	349.934989	5.597811
4.846508	350.278210	5.602816
4.900369	350.772859	5.607821
5.129998	354.043127	5.612826
4.472810	357.895281	5.617830
4.866607	353.015095	5.622835
4.918882	356.468180	5.627840
4.649233	360.389332	5.632845
4.881881	357.407386	5.637850
4.913724	362.451920	5.642854
4.842333	356.999196	5.647859
5.150551	355.245634	5.652864
5.238386	368.700368	5.657869
5.306224	355.619962	5.662874
4.762859	367.028512	5.667878
4.762750	371.597151	5.672883
5.105167	377.200485	5.677888
5.362665	379.457126	5.682893
5.529037	375.542736	5.687898
5.451636	387.906539	5.692902
5.542406	372.098460	5.697907
5.193208	368.796377	5.702912
4.692192	359.459332	5.707917
5.277088	370.903083	5.712922
5.358604	378.325374	5.717926
5.833830	381.202817	5.722931
5.203814	365.899994	5.727936
5.338149	362.537970	5.732941
5.194141	357.890748	5.737946
4.850433	365.930166	5.742950
5.082622	363.865803	5.747955
5.000866	389.230506	5.752960
5.511042	385.300212	5.757965
5.292208	371.929344	5.762970
5.394417	380.455737	5.767974
5.689351	377.372277	5.772979
5.705134	380.201480	5.777984
5.544060	382.001670	5.782989
5.769436	377.040296	5.787994
5.644511	381.441827	5.792998
5.336882	380.629500	5.798003
5.545000	384.001224	5.803008
5.505648	387.221891	5.808013
5.791269	383.665313	5.813018
5.430508	388.037356	5.818022
5.557113	377.602191	5.823027
5.546800	382.406556	5.828032
5.422921	383.640919	5.833037
5.524260	375.452878	5.838042
5.561356	380.721226	5.843046
5.544202	372.165763	5.848051
5.422659	380.103938	5.853056
5.371287	378.394059	5.858061
5.361390	376.785253	5.863066
5.647533	383.128253	5.868070
5.657496	383.218482	5.873075
5.245068	381.691728	5.878080
5.561095	382.562928	5.883085
5.516016	378.567770	5.888090
5.430403	388.898510	5.893094
5.848197	379.164387	5.898099
5.587096	377.575957	5.903104
5.681257	379.234913	5.908109
5.844083	380.054185	5.913114
5.404695	386.950638	5.918118
5.682005	390.358979	5.923123
5.885025	408.221913	5.928128
5.886632	408.069835	5.933133
5.600816	394.532269	5.938138
5.641857	402.856279	5.943142
5.917236	396.178588	5.948147
5.710433	401.235213	5.953152
5.714002	406.173455	5.958157
5.672421	402.263167	5.963162
5.065387	403.876963	5.968166
5.607911	398.343856	5.973171
5.164865	402.899643	5.978176
6.004664	425.386444	5.983181
6.143126	428.364117	5.988186
6.096463	423.458008	5.993190
6.092353	426.584573	5.998195
6.136304	425.441903	6.003200
5.898819	424.476211	6.008205
5.861478	418.094290	6.013210
5.897325	434.660954	6.018214
6.265920	435.125276	6.023219
6.120704	427.529515	6.028224
5.578147	424.441221	6.033229
5.887939	424.047861	6.038234
5.804179	437.754167	6.043238
5.575794	429.320360	6.048243
5.545019	427.404763	6.053248
5.550235	438.490117	6.058253
5.997612	433.759706	6.063258
5.406108	439.291083	6.068262
5.722436	426.253951	6.073267
6.279726	435.186809	6.078272
6.202771	439.574511	6.083277
6.560173	436.674248	6.088282
6.478749	435.835968	6.093286
6.266368	436.166685	6.098291
6.498330	427.477248	6.103296
6.240639	440.097132	6.108301
6.368600	430.386245	6.113306
6.281223	418.060963	6.118310
6.129057	411.488221	6.123315
6.209151	405.015136	6.128320
6.146050	403.155228	6.133325
6.462361	400.242426	6.138330
6.054948	404.134551	6.143334
5.869920	405.770813	6.148339
5.896858	397.879165	6.153344
6.035270	411.686686	6.158349
5.982682	400.175401	6.163354
5.746670	410.213334	6.168358
5.873148	397.028795	6.173363
5.770205	401.243384	6.178368
5.546018	401.582277	6.183373
5.821809	400.732323	6.188378
5.644284	408.609677	6.193382
6.246268	416.570550	6.198387
6.331606	411.843085	6.203392
5.767181	408.710762	6.208397
5.801061	404.959498	6.213402
5.840907	412.454773	6.218406
6.046117	417.351932	6.223411
6.106847	427.074454	6.228416
5.632476	429.252777	6.233421
6.111342	421.632005	6.238426
6.264962	437.430388	6.243430
6.343859	429.489454	6.248435
6.102465	419.172037	6.253440
5.901472	417.972830	6.258445
5.798110	413.154704	6.263450
5.689825	418.183243	6.268454
6.141238	421.475723	6.273459
6.432649	421.578804	6.278464
5.869528	416.481526	6.283469
6.216990	406.631853	6.288474
5.586281	406.233988	6.293478
5.670083	405.221121	6.298483
5.887756	420.816458	6.303488
5.932304	415.687246	6.308493
6.126771	429.625207	6.313498
6.264309	431.875340	6.318502
6.141286	411.440373	6.323507
6.082419	407.336634	6.328512
6.160281	410.048544	6.333517
6.112357	408.094506	6.338522
5.689046	409.445391	6.343526
5.903097	409.538445	6.348531
5.767329	404.291952	6.353536
5.580016	411.572874	6.358541
6.034562	416.323396	6.363546
6.136271	429.285606	6.368550
5.797051	431.562981	6.373555
6.071375	434.721854	6.378560
6.303121	430.756079	6.383565
6.064089	428.806672	6.388570
5.886537	414.204893	6.393574
5.706561	405.738203	6.398579
5.939066	411.627695	6.403584
5.974731	422.550076	6.408589
6.168071	427.151696	6.413594
5.864040	437.168663	6.418598
5.842769	432.983095	6.423603
5.753168	434.550623	6.428608
5.884898	439.190374	6.433613
5.912062	435.136427	6.438618
5.661316	435.799031	6.443622
5.842996	425.950012	6.448627
5.894464	431.662227	6.453632
6.061720	437.141159	6.458637
6.212562	430.596867	6.463642
6.228361	431.461324	6.468646
6.182498	432.038042	6.473651
6.048527	433.283481	6.478656
6.012206	438.383010	6.483661
5.980981	431.788147	6.488666
6.271135	432.258431	6.493670
6.039823	422.379207	6.498675
6.301541	424.353611	6.503680
5.824856	433.306099	6.508685
6.089447	425.456299	6.513690
6.272412	435.786115	6.518694
6.015371	413.413720	6.523699
5.843389	410.634373	6.528704
5.469184	415.498926	6.533709
5.823155	424.178888	6.538714
5.809056	434.406698	6.543718
5.967818	431.980498	6.548723
5.881347	432.652166	6.553728
5.715697	424.075651	6.558733
5.892125	432.457559	6.563738
5.736668	439.549997	6.568742
5.903214	435.932969	6.573747
5.988607	428.089098	6.578752
5.929441	445.613487	6.583757
6.204149	435.987176	6.588762
5.929558	437.985498	6.593766
5.680122	434.525399	6.598771
6.232647	437.751418	6.603776
5.872307	436.773336	6.608781
6.103722	428.748393	6.613786
6.306293	440.210962	6.618790
5.810311	440.114699	6.623795
6.018331	441.967800	6.628800
5.919670	438.692891	6.633805
6.349612	440.074609	6.638810
6.119914	440.917419	6.643814
6.189523	432.022456	6.648819
5.977305	438.680849	6.653824
5.900691	445.605908	6.658829
6.280874	446.071578	6.663834
6.258834	441.708953	6.668838
6.248696	439.508539	6.673843
6.231647	430.529076	6.678848
6.456367	423.448011	6.683853
6.167764	420.848291	6.688858
6.129832	412.859229	6.693862
6.030345	410.805699	6.698867
6.152000	409.198425	6.703872
5.894431	419.429572	6.708877
5.756704	414.882593	6.713882
5.916138	424.845920	6.718886
6.298109	409.931844	6.723891
5.976462	426.209655	6.728896
6.099027	414.841765	6.733901
6.072101	411.451214	6.738906
5.894502	410.463484	6.743910
5.720503	405.495072	6.748915
6.310214	403.880903	6.753920
5.717182	410.535675	6.758925
5.884327	405.292343	6.763930
5.744479	417.862109	6.768934
5.921316	399.243679	6.773939
6.068322	405.735041	6.778944
5.863000	411.693134	6.783949
5.752713	418.364023	6.788954
5.712974	413.130956	6.793958
5.856557	425.181742	6.798963
6.581198	434.841375	6.803968
5.859799	426.108318	6.808973
5.910325	407.522326	6.813978
5.527042	415.090226	6.818982
6.101274	424.045734	6.823987
6.439729	423.198616	6.828992
6.435688	428.549357	6.833997
6.187842	419.976231	6.839002
6.147616	414.860302	6.844006
5.974550	412.530390	6.849011
5.787385	412.433200	6.854016
5.781229	415.145620	6.859021
5.840375	403.999651	6.864026
5.553277	414.273388	6.869030
5.748337	418.438125	6.874035
5.835192	425.483101	6.879040
5.859996	430.013050	6.884045
6.035679	432.159127	6.889050
5.765939	444.198753	6.894054
5.673197	439.815567	6.899059
5.713127	437.914202	6.904064
5.836318	446.753725	6.909069
6.023976	427.095827	6.914074
5.943905	436.429114	6.919078
6.020584	433.136224	6.924083
5.778602	437.087860	6.929088
5.865503	438.460050	6.934093
5.960735	434.974422	6.939098
5.787991	435.007854	6.944102
5.630958	442.676361	6.949107
6.064625	440.684830	6.954112
5.766902	437.871394	6.959117
5.670109	434.722746	6.964122
6.066887	448.996031	6.969126
6.185449	449.711506	6.974131
6.194639	444.480255	6.979136
6.145186	441.077409	6.984141
6.157023	437.848464	6.989146
5.881110	447.639561	6.994150
5.959815	442.871997	6.999155
5.763345	442.712988	7.004160
5.591448	449.422016	7.009165
6.037963	453.496742	7.014170
6.341997	467.411238	7.019174
6.171671	454.450336	7.024179
6.021211	444.251538	7.029184
6.025556	451.714425	7.034189
6.063662	452.819005	7.039194
6.164887	445.501009	7.044198
6.131651	453.659506	7.049203
6.106535	445.576669	7.054208
5.950631	449.913467	7.059213
6.045136	440.369173	7.064218
5.849346	448.723984	7.069222
5.842148	441.502075	7.074227
5.828611	437.302639	7.079232
6.012909	445.180267	7.084237
6.486673	440.683009	7.089242
6.075156	442.481316	7.094246
6.229950	446.060728	7.099251
6.316900	446.047143	7.104256
5.785281	445.118043	7.109261
6.347478	439.088281	7.114266
6.192183	443.064302	7.119270
6.123890	440.645202	7.124275
6.303261	446.144386	7.129280
5.674691	444.901436	7.134285
6.393164	447.579421	7.139290
6.089974	443.466497	7.144294
5.749470	438.441904	7.149299
5.946197	435.196645	7.154304
5.856515	435.422713	7.159309
6.048980	432.118010	7.164314
6.296592	441.273404	7.169318
6.271428	428.565031	7.174323
6.149486	421.848341	7.179328
5.844019	416.495551	7.184333
5.961453	408.092995	7.189338
5.861876	412.012822	7.194342
5.612203	419.543970	7.199347
6.119488	430.411444	7.204352
5.814081	438.887833	7.209357
5.932275	444.845869	7.214362
5.850559	442.232713	7.219366
6.089128	443.935490	7.224371
6.072563	447.291808	7.229376
6.152612	448.848575	7.234381
6.187898	439.712206	7.239386
6.141657	443.190235	7.244390
5.817183	424.776879	7.249395
5.928003	427.670295	7.254400
5.506150	431.042653	7.259405
5.855790	445.380270	7.264410
5.870051	445.887454	7.269414
6.177805	449.357477	7.274419
6.260496	448.205572	7.279424
5.948582	459.394412	7.284429
6.138123	450.347767	7.289434
6.321764	449.025016	7.294438
6.236786	444.349538	7.299443
6.067993	422.959918	7.304448
5.911570	418.463326	7.309453
6.043301	429.753484	7.314458
5.857812	414.286054	7.319462
5.878127	414.058276	7.324467
6.182775	410.005151	7.329472
6.132691	424.174419	7.334477
6.123435	416.348547	7.339482
5.960712	420.373185	7.344486
6.119376	429.732340	7.349491
5.821480	419.967957	7.354496
5.982501	418.816436	7.359501
5.827357	410.260428	7.364506
5.813396	423.003469	7.369510
6.216741	417.919283	7.374515
6.036224	418.903086	7.379520
5.951871	419.846513	7.384525
6.176340	417.558721	7.389530
5.961475	416.848920	7.394534
5.939736	410.597439	7.399539
6.157280	415.935604	7.404544
5.796141	418.915621	7.409549
5.975551	411.031716	7.414554
5.868912	410.406202	7.419558
5.695657	419.187751	7.424563
6.008111	412.611816	7.429568
5.865452	423.723493	7.434573
6.253778	421.207541	7.439578
5.907548	417.332328	7.444582
5.684660	421.511930	7.449587
6.258432	424.949760	7.454592
6.343181	426.119799	7.459597
6.100157	422.282199	7.464602
5.843944	420.572773	7.469606
5.838253	412.698886	7.474611
6.019058	413.613422	7.479616
5.821697	420.816826	7.484621
5.788119	416.566749	7.489626
6.235900	418.110191	7.494630
6.079270	419.178840	7.499635
6.219626	411.715517	7.504640
6.131126	421.167179	7.509645
6.190041	416.491311	7.514650
6.125916	414.318341	7.519654
5.901523	413.780881	7.524659
6.209013	411.340873	7.529664
6.010594	420.015631	7.534669
6.012414	413.643395	7.539674
5.953723	416.269131	7.544678
5.970074	417.747288	7.549683
6.009477	415.827024	7.554688
5.723501	417.203850	7.559693
6.039978	425.975111	7.564698
6.301570	412.750407	7.569702
5.878324	417.619481	7.574707
6.193160	421.518673	7.579712
5.637414	426.996985	7.584717
6.008954	413.413358	7.589722
6.076733	412.899724	7.594726
5.909189	427.425930	7.599731
6.248593	414.594006	7.604736
6.011152	418.905605	7.609741
6.293167	418.484959	7.614746
5.942114	420.394016	7.619750
6.052697	413.675698	7.624755
6.337229	409.938946	7.629760
5.930912	423.442672	7.634765
5.662809	413.107295	7.639770
5.980427	415.519042	7.644774
6.291592	415.815185	7.649779
5.868578	416.144101	7.654784
5.890666	421.813458	7.659789
6.151258	413.806097	7.664794
5.902965	421.795788	7.669798
5.904242	421.874723	7.674803
6.094293	415.457174	7.679808
5.890609	423.933437	7.684813
6.278829	416.263592	7.689818
6.234080	414.397644	7.694822
5.992597	421.857906	7.699827
5.715098	410.571685	7.704832
6.153946	419.251001	7.709837
6.061681	416.702779	7.714842
5.947269	414.670570	7.719846
6.280367	422.176851	7.724851
6.403782	415.117990	7.729856
6.002008	415.671375	7.734861
6.048977	400.980644	7.739866
6.026219	404.920071	7.744870
5.871175	399.382362	7.749875
6.071684	402.309179	7.754880
5.702068	402.715153	7.759885
5.776464	413.216995	7.764890
6.158239	413.502075	7.769894
5.982726	408.771188	7.774899
6.169325	416.983811	7.779904
6.032369	415.186095	7.784909
5.833579	408.079641	7.789914
6.256194	414.888503	7.794918
6.094564	404.280177	7.799923
6.081983	395.163986	7.804928
5.767485	402.078843	7.809933
5.844633	389.477858	7.814938
5.697274	396.470932	7.819942
5.827777	413.218904	7.824947
5.972136	406.549083	7.829952
6.184476	413.283319	7.834957
6.226697	408.088033	7.839962
6.033943	408.652962	7.844966
6.064842	410.220591	7.849971
6.119108	400.034035	7.854976
5.800462	405.373948	7.859981
5.772170	400.423837	7.864986
6.135966	406.836939	7.869990
6.136998	412.341908	7.874995
6.139110	393.152894	7.880000
6.047813	399.615151	7.885005
5.936831	396.516192	7.890010
5.781041	394.832164	7.895014
5.622901	403.854953	7.900019
6.201928	407.728567	7.905024
5.822982	414.561775	7.910029
6.369681	409.480441	7.915034
5.956602	409.038986	7.920038
6.023355	416.371854	7.925043
5.982110	403.634381	7.930048
6.132226	406.910789	7.935053
5.987358	395.828430	7.940058
6.089569	393.623074	7.945062
5.737357	385.831966	7.950067
6.178604	381.342982	7.955072
5.593166	404.356794	7.960077
5.694413	404.078369	7.965082
5.959814	413.278419	7.970086
6.038125	418.739643	7.975091
6.250447	415.852624	7.980096
5.989462	415.102592	7.985101
6.234125	415.991303	7.990106
6.085521	413.455072	7.995110
5.919830	396.162180	8.000115
6.080725	388.686456	8.005133
5.607647	390.483669	8.010150
6.155538	408.284787	8.015168
6.299470	414.810509	8.020186
6.239935	407.217611	8.025203
5.899955	392.621817	8.030221
5.886129	400.854278	8.035238
5.741104	397.064864	8.040256
6.292816	399.518857	8.045274
5.878861	407.009291	8.050291
6.169580	406.152745	8.055309
5.853783	409.121355	8.060326
6.242674	402.433334	8.065344
6.161058	407.536424	8.070362
6.022265	394.922490	8.075379
6.217246	393.746433	8.080397
5.764102	395.919215	8.085414
6.134764	393.794146	8.090432
6.091646	399.604407	8.095450
6.016084	409.938823	8.100467
6.429229	397.339393	8.105485
6.021501	399.009604	8.110502
5.731036	397.764441	8.115520
6.273924	398.389468	8.120538
5.776259	406.760855	8.125555
5.949260	406.307758	8.130573
5.917333	410.071327	8.135590
5.828027	411.076271	8.140608
6.095645	415.752264	8.145626
5.970928	409.018482	8.150643
5.924638	412.610735	8.155661
5.735677	422.202383	8.160678
6.236970	412.899542	8.165696
6.231300	411.884309	8.170714
6.046432	412.004830	8.175731
5.933927	408.888811	8.180749
6.231313	411.824462	8.185766
6.337300	414.824816	8.190784
6.345481	411.364842	8.195802
6.118380	414.609887	8.200819
6.103042	408.313400	8.205837
5.958444	416.512710	8.210854
5.979182	414.268897	8.215872
6.381519	410.870241	8.220890
5.995368	417.977631	8.225907
6.294864	410.486267	8.230925
6.088507	416.978512	8.235942
6.031425	418.180377	8.240960
6.335651	434.621691	8.245978
6.130224	446.532275	8.250995
6.274973	439.222935	8.256013
6.066816	436.472189	8.261030
6.320836	437.521171	8.266048
6.292998	445.093134	8.271066
6.488144	446.801432	8.276083
6.453264	448.337490	8.281101
6.386382	432.963575	8.286118
6.235996	431.974171	8.291136
5.830176	432.397553	8.296154
5.876660	438.812320	8.301171
6.337336	441.176442	8.306189
6.401551	447.020393	8.311206
6.405039	445.883803	8.316224
6.392973	437.967877	8.321242
6.569582	443.140971	8.326259
6.108569	439.644053	8.331277
6.322595	438.480788	8.336294
6.437697	441.445005	8.341312
6.656248	444.721215	8.346330
6.425565	443.353074	8.351347
6.048514	434.828466	8.356365
6.243838	442.387553	8.361382
6.362867	441.778810	8.366400
6.314746	437.260999	8.371418
6.018096	442.176886	8.376435
6.127915	435.371634	8.381453
6.120673	442.637414	8.386470
6.430887	434.901365	8.391488
6.567398	454.341720	8.396506
6.336984	450.082839	8.401523
6.445391	441.608397	8.406541
6.736873	446.078689	8.411558
6.149385	446.366434	8.416576
6.273051	442.048922	8.421594
6.410931	447.619401	8.426611
6.486728	440.361890	8.431629
6.469251	441.554395	8.436646
6.446219	444.010084	8.441664
6.355145	444.911167	8.446682
6.321191	445.023822	8.451699
6.474684	443.128432	8.456717
6.923732	449.701033	8.461734
6.597587	445.750641	8.466752
6.752206	441.175816	8.471770
6.373652	444.646567	8.476787
6.635574	449.585391	8.481805
6.292380	450.406056	8.486822
6.407257	450.182970	8.491840
6.497430	445.637176	8.496858
6.266637	451.126567	8.501875
6.719756	444.204407	8.506893
6.380102	449.076542	8.511910
6.664447	454.122306	8.516928
6.778305	448.872217	8.521946
6.566636	449.505018	8.526963
6.962715	446.426071	8.531981
6.422802	449.385621	8.536998
6.080312	449.442477	8.542016
6.372153	449.339985	8.547034
6.358722	448.221825	8.552051
6.403855	431.650098	8.557069
6.526039	437.576482	8.562087
6.288731	438.115471	8.567104
6.502659	446.567886	8.572122
6.667792	444.298290	8.577139
6.700523	443.327531	8.582157
6.740767	441.244760	8.587175
6.589355	435.244136	8.592192
6.775545	444.587671	8.597210
6.549944	439.479133	8.602227
6.685104	435.506958	8.607245
6.841586	439.837455	8.612263
6.763722	451.778548	8.617280
6.968537	438.858283	8.622298
6.583935	443.077901	8.627315
6.777482	435.568414	8.632333
6.610826	438.863952	8.637351
6.405762	447.265252	8.642368
6.517793	445.026067	8.647386
6.601123	449.244952	8.652403
6.442620	436.447886	8.657421
6.349046	437.639691	8.662439
6.371069	441.817689	8.667456
6.656997	456.538833	8.672474
7.073986	458.303891	8.677491
6.782775	460.473400	8.682509
6.454360	449.290306	8.687527
6.531294	467.370399	8.692544
6.612503	470.049599	8.697562
6.653322	469.386838	8.702579
6.707052	470.940572	8.707597
6.710445	475.345557	8.712615
6.661944	475.012369	8.717632
6.863726	471.367416	8.722650
6.957158	477.645454	8.727667
6.877159	471.592604	8.732685
6.723265	474.195033	8.737703
6.584449	476.394314	8.742720
6.942207	477.603769	8.747738
6.749456	476.576819	8.752755
6.671077	474.992309	8.757773
6.845097	469.720165	8.762791
6.827480	469.694561	8.767808
6.852262	471.136067	8.772826
6.727460	477.842771	8.777843
7.105498	470.174976	8.782861
7.242060	469.607666	8.787879
6.926092	468.846174	8.792896
6.692542	453.305853	8.797914
6.659343	464.965404	8.802931
6.868700	470.145998	8.807949
7.249454	464.109321	8.812967
6.544674	465.655667	8.817984
6.672059	463.319400	8.823002
7.140124	466.963616	8.828019
6.970306	474.655667	8.833037
6.962320	471.851462	8.838055
6.964068	472.267790	8.843072
7.096777	469.772899	8.848090
6.679015	453.191629	8.853107
6.937487	463.533699	8.858125
7.060748	464.950307	8.863143
6.717738	466.686122	8.868160
7.098008	470.394587	8.873178
6.871376	463.064531	8.878195
6.547563	478.424024	8.883213
6.826870	458.868076	8.888231
6.804231	476.591398	8.893248
6.716744	471.817815	8.898266
6.745226	474.849257	8.903283
6.675424	481.156028	8.908301
6.995051	471.076895	8.913319
6.581637	482.404713	8.918336
6.540855	466.632206	8.923354
7.285437	474.651199	8.928371
6.848080	475.638097	8.933389
6.900173	472.761363	8.938407
6.797302	473.497039	8.943424
7.168542	494.835157	8.948442
7.126982	497.315847	8.953459
6.774112	486.448984	8.958477
7.329549	493.875931	8.963495
7.062397	501.441232	8.968512
7.250355	485.418276	8.973530
6.972468	485.771122	8.978547
6.907317	483.843714	8.983565
7.092661	485.250596	8.988583
7.114129	503.595036	8.993600
7.267049	491.503370	8.998618
6.801044	484.927174	9.003635
7.003437	504.035370	9.008653
7.434660	501.736698	9.013671
6.957138	503.853353	9.018688
7.133993	495.264019	9.023706
7.172268	495.835570	9.028723
6.743113	504.609678	9.033741
6.835795	501.896992	9.038759
7.290462	510.075034	9.043776
7.415693	506.697687	9.048794
7.364619	499.093958	9.053811
7.256031	506.337773	9.058829
7.142562	501.082261	9.063847
6.966897	507.197346	9.068864
7.034901	503.750071	9.073882
7.667889	502.492756	9.078899
6.966455	506.762031	9.083917
7.042232	504.465402	9.088935
7.155056	512.416140	9.093952
7.090250	514.509156	9.098970
7.209064	504.057527	9.103987
7.418323	508.793180	9.109005
7.540756	501.806046	9.114023
7.340013	499.423357	9.119040
7.304163	506.109823	9.124058
7.401538	480.526393	9.129075
6.616652	481.952749	9.134093
6.931420	489.941263	9.139111
6.741032	502.597450	9.144128
7.139786	501.446262	9.149146
7.315544	500.617192	9.154163
7.047253	503.398493	9.159181
7.213817	498.910145	9.164199
7.410145	501.893203	9.169216
7.291318	497.720968	9.174234
7.324539	506.902311	9.179251
7.514866	511.186498	9.184269
7.430306	494.777044	9.189287
7.162301	507.473798	9.194304
7.121547	507.912565	9.199322
7.065421	503.992436	9.204339
7.075856	519.570991	9.209357
7.076932	509.346088	9.214375
7.612223	517.464164	9.219392
7.375954	513.354508	9.224410
7.624821	513.151452	9.229427
7.086939	504.983368	9.234445
7.261700	509.572949	9.239463
7.193987	526.899441	9.244480
7.344216	531.533897	9.249498
7.600667	532.434182	9.254515
7.696693	532.879921	9.259533
7.551072	525.997892	9.264551
7.245225	517.197002	9.269568
7.432596	518.187004	9.274586
7.726515	517.572947	9.279603
7.496527	512.244171	9.284621
7.662842	509.324288	9.289639
7.422411	510.542264	9.294656
7.781679	510.233548	9.299674
7.341782	509.235852	9.304691
7.106314	509.944968	9.309709
7.644048	499.478197	9.314727
7.178075	498.402536	9.319744
7.195878	509.949984	9.324762
7.480362	526.063117	9.329779
7.549397	527.406175	9.334797
7.830616	520.296325	9.339815
7.644538	520.476997	9.344832
7.742973	521.458843	9.349850
7.376855	512.468583	9.354867
7.335488	515.419458	9.359885
7.445548	521.404573	9.364903
7.823288	533.813978	9.369920
7.570159	522.751585	9.374938
7.443142	521.900525	9.379955
7.625534	529.852994	9.384973
7.864450	523.866922	9.389991
7.588910	515.029726	9.395008
7.328660	516.282366	9.400026
7.474223	516.335336	9.405043
7.715452	533.979502	9.410061
7.722442	527.979275	9.415079
7.713298	521.924774	9.420096
7.679121	521.198023	9.425114
7.558771	501.449028	9.430131
7.710490	502.248956	9.435149
7.613739	500.159241	9.440167
7.385888	498.478229	9.445184
7.447783	522.664036	9.450202
7.585062	523.658731	9.455219
7.597375	531.842975	9.460237
7.223487	526.192759	9.465255
7.824173	528.960988	9.470272
7.161860	527.553172	9.475290
7.832924	524.850847	9.480307
7.467826	527.521088	9.485325
7.547037	522.639323	9.490343
7.538010	530.905805	9.495360
7.540336	529.311802	9.500378
7.728126	521.329811	9.505395
7.725939	532.400725	9.510413
7.913387	528.527633	9.515431
7.921959	521.933871	9.520448
7.505184	527.348284	9.525466
7.871195	529.395891	9.530483
7.923526	534.178230	9.535501
7.786920	525.533854	9.540519
7.829990	522.721642	9.545536
7.717247	528.858433	9.550554
8.234932	523.387260	9.555571
8.011614	528.692467	9.560589
7.854017	527.994521	9.565607
7.691126	529.538019	9.570624
7.447123	539.823162	9.575642
7.779222	537.555796	9.580659
7.456512	535.507792	9.585677
7.393911	527.410396	9.590695
7.869974	552.310833	9.595712
7.699695	556.642063	9.600730
7.720291	548.260224	9.605747
7.568066	563.577125	9.610765
8.284914	567.135045	9.615783
8.362016	559.407066	9.620800
8.342646	562.458644	9.625818
8.520190	540.507519	9.630835
7.965367	533.250946	9.635853
7.890250	535.629602	9.640871
7.795424	529.263476	9.645888
7.496906	535.129576	9.650906
8.085779	524.493832	9.655923
7.963126	535.678296	9.660941
7.845697	534.917252	9.665959
7.825396	526.346171	9.670976
7.805306	542.396587	9.675994
8.031093	551.538314	9.681011
7.830700	557.231257	9.686029
7.956426	550.079486	9.691047
8.353407	559.115499	9.696064
7.924607	561.820973	9.701082
7.917259	563.949173	9.706099
7.897985	568.092645	9.711117
7.728576	565.118057	9.716135
8.009016	566.203933	9.721152
8.009137	572.442976	9.726170
8.253821	563.057188	9.731187
8.292672	562.047593	9.736205
7.943415	571.778046	9.741223
8.062592	559.530675	9.746240
8.023816	567.145429	9.751258
7.975288	567.721115	9.756275
7.796397	560.806417	9.761293
7.769356	554.155106	9.766311
8.272613	559.131887	9.771328
7.911386	559.194835	9.776346
7.935829	562.384715	9.781363
7.942997	566.732326	9.786381
8.296643	565.468282	9.791399
8.241057	555.542565	9.796416
7.933066	562.798711	9.801434
7.896197	570.454192	9.806451
7.888735	561.890550	9.811469
7.981691	561.200682	9.816487
8.103290	570.437638	9.821504
7.780310	579.845242	9.826522
7.967232	589.655797	9.831539
8.458216	595.846341	9.836557
8.467462	598.606263	9.841575
8.501713	593.311800	9.846592
8.254029	584.842590	9.851610
8.100338	569.056127	9.856627
8.357821	566.393349	9.861645
7.978860	570.457478	9.866663
8.113675	570.174462	9.871680
8.341708	580.818015	9.876698
8.436960	589.879228	9.881715
8.353942	580.658384	9.886733
8.275765	578.026106	9.891751
8.294500	567.160931	9.896768
8.075269	573.923492	9.901786
8.353652	586.187554	9.906803
8.367961	583.745913	9.911821
8.307174	584.863163	9.916839
8.190669	586.964288	9.921856
7.912470	593.717161	9.926874
8.483021	585.264915	9.931891
8.711274	596.325009	9.936909
8.374967	586.790397	9.941927
8.810663	584.756103	9.946944
8.351050	579.302338	9.951962
8.314867	571.670998	9.956979
8.074168	571.494155	9.961997
8.241480	582.421777	9.967015
8.647316	579.956660	9.972032
8.652013	587.533053	9.977050
8.409077	581.341593	9.982067
8.403752	581.348777	9.987085
8.112628	582.912372	9.992103
8.462451	581.588965	9.997120
8.703475	594.079793	10.002138
8.592898	591.171723	10.007155
8.462459	577.685348	10.012173
8.385211	580.900632	10.017191
8.566347	575.740950	10.022208
8.523886	574.456917	10.027226
8.579568	569.111766	10.032243
8.328093	566.298360	10.037261
8.220151	578.029655	10.042279
8.642748	576.720093	10.047296
8.396625	591.243845	10.052314
8.805210	585.420518	10.057331
8.836066	587.987704	10.062349
8.349847	582.231993	10.067367
8.431812	575.266950	10.072384
8.539743	583.799154	10.077402
8.453508	592.787819	10.082419
8.796977	593.898535	10.087437
8.580980	594.834977	10.092455
8.771429	582.822576	10.097472
8.535561	582.401979	10.102490
8.059666	574.410343	10.107507
8.551198	588.282028	10.112525
8.513838	594.776260	10.117543
8.628411	596.232110	10.122560
8.610325	584.514313	10.127578
8.756332	584.538812	10.132595
8.866195	595.844673	10.137613
8.872844	597.803427	10.142631
8.506225	600.300348	10.147648
8.360145	605.252648	10.152666
8.256339	604.003471	10.157683
8.377871	592.610933	10.162701
8.140108	600.048595	10.167719
8.590956	596.178400	10.172736
8.708391	595.550967	10.177754
8.406739	595.907538	10.182771
8.657627	595.091938	10.187789
8.515078	588.487115	10.192807
8.687510	608.868752	10.197824
8.825453	622.451881	10.202842
8.817732	623.396717	10.207859
8.995349	609.006827	10.212877
8.547321	607.783180	10.217895
8.870879	614.037833	10.222912
8.907662	612.457358	10.227930
8.502878	604.161077	10.232947
8.892180	605.652777	10.237965
8.865861	621.530670	10.242983
8.879539	613.929370	10.248000
8.728718	617.872557	10.253018
8.741931	624.901676	10.258035
8.551996	619.951601	10.263053
8.831763	624.953950	10.268071
9.134983	618.370791	10.273088
8.993022	628.782008	10.278106
9.098122	624.782942	10.283123
9.055802	619.790804	10.288141
8.733590	616.101689	10.293159
8.661657	617.463686	10.298176
8.752745	613.444727	10.303194
9.005688	620.934901	10.308211
9.120936	626.180779	10.313229
9.058279	629.538952	10.318247
8.991107	616.241452	10.323264
8.673624	617.222198	10.328282
8.857351	623.148468	10.333299
9.474320	615.837652	10.338317
9.128426	618.195628	10.343335
8.907102	606.667451	10.348352
8.929498	602.179575	10.353370
8.680475	613.298680	10.358387
9.298103	618.582607	10.363405
8.873727	620.571027	10.368423
9.017078	620.340321	10.373440
8.671437	618.983866	10.378458
8.910672	628.846207	10.383475
8.731621	625.674304	10.388493
8.799302	629.725270	10.393511
8.793135	625.636340	10.398528
9.226205	627.357871	10.403546
9.189098	625.426053	10.408563
9.223818	631.609203	10.413581
8.977695	633.074232	10.418599
9.088572	623.513717	10.423616
9.328956	625.511591	10.428634
9.023608	617.206035	10.433651
8.973703	617.750380	10.438669
8.864923	625.164688	10.443687
8.937524	628.580564	10.448704
8.713947	621.985269	10.453722
8.984426	632.079402	10.458739
9.223912	626.241531	10.463757
8.703083	630.835987	10.468775
8.962708	643.156676	10.473792
9.154796	650.343972	10.478810
8.837989	652.968796	10.483827
9.439420	652.543240	10.488845
9.076656	650.539367	10.493863
9.065446	653.753785	10.498880
8.960948	660.094457	10.503898
9.036190	661.225113	10.508915
9.578787	650.034810	10.513933
9.161719	652.817354	10.518951
8.983914	656.572273	10.523968
9.088801	642.938524	10.528986
8.604065	649.840544	10.534003
9.392087	651.910407	10.539021
8.987970	657.048319	10.544039
9.051871	668.446635	10.549056
9.512157	677.599022	10.554074
9.178162	680.990252	10.559091
9.573716	671.479782	10.564109
9.757059	671.539457	10.569127
9.229333	667.235588	10.574144
8.994425	656.974992	10.579162
8.962759	675.413140	10.584179
9.178617	675.303617	10.589197
9.293655	681.824496	10.594215
8.991617	684.235570	10.599232
9.554016	680.748669	10.604250
9.331440	685.422641	10.609267
9.434949	685.889303	10.614285
9.317683	691.436719	10.619303
8.956301	688.167140	10.624320
9.446922	684.814561	10.629338
9.206841	683.185941	10.634355
9.596048	683.156556	10.639373
9.256364	689.149077	10.644391
9.464274	685.670380	10.649408
9.908530	685.357813	10.654426
9.514808	685.331177	10.659443
9.654329	685.912117	10.664461
9.132026	685.104048	10.669479
9.709168	678.247574	10.674496
9.434462	680.793221	10.679514
9.399353	682.143141	10.684531
9.436451	671.369700	10.689549
9.340856	681.524374	10.694567
9.438258	685.428684	10.699584
9.862321	686.327962	10.704602
9.245779	689.050247	10.709619
9.690262	688.923838	10.714637
9.550652	698.915003	10.719655
9.534204	704.901066	10.724672
9.664557	693.207279	10.729690
9.560906	703.205436	10.734707
9.665166	704.953246	10.739725
9.669248	702.200763	10.744743
9.564670	702.920936	10.749760
9.585968	701.055699	10.754778
9.297687	711.486735	10.759795
9.899838	703.846843	10.764813
9.623588	713.546998	10.769831
9.742729	713.146514	10.774848
9.884592	714.181528	10.779866
9.884000	708.362311	10.784883
9.671820	708.726956	10.789901
9.787166	714.632412	10.794919
9.756803	703.708574	10.799936
9.685099	695.407400	10.804954
9.825279	707.942510	10.809971
10.028114	703.912334	10.814989
9.538177	705.156792	10.820007
9.997690	697.021696	10.825024
9.622199	690.715266	10.830042
9.813711	691.777214	10.835059
9.943910	696.875601	10.840077
10.019853	691.038087	10.845095
9.419721	684.485988	10.850112
9.939522	698.552147	10.855130
9.667771	704.606614	10.860147
9.949235	704.291151	10.865165
9.966879	708.665558	10.870183
9.819172	710.875728	10.875200
10.139421	701.276055	10.880218
9.887631	692.239388	10.885235
9.622187	679.042334	10.890253
9.757573	692.389231	10.895271
9.894141	702.517009	10.900288
9.809355	704.966630	10.905306
9.726241	708.782463	10.910323
9.815442	711.965379	10.915341
9.738396	709.424424	10.920359
10.065342	710.405192	10.925376
10.257061	703.347163	10.930394
10.030343	719.944512	10.935411
10.094255	710.555412	10.940429
10.174087	711.069965	10.945447
10.194255	715.746938	10.950464
9.960395	713.448304	10.955482
10.100427	707.013759	10.960499
9.842432	712.955619	10.965517
9.871911	712.282003	10.970535
9.779124	715.323019	10.975552
10.066490	709.625943	10.980570
10.177557	709.318243	10.985587
10.262610	716.516024	10.990605
10.054267	715.627203	10.995623
10.223257	705.865033	11.000640
10.100758	716.096526	11.005658
10.202581	709.876251	11.010675
10.011192	705.690090	11.015693
9.871142	710.994927	11.020711
10.021397	711.943419	11.025728
9.962743	710.507277	11.030746
9.929329	704.828905	11.035763
9.945995	717.579035	11.040781
10.087551	700.606941	11.045799
10.245375	712.318774	11.050816
10.339246	704.020056	11.055834
10.396675	708.239905	11.060851
10.429663	694.983458	11.065869
10.264363	700.910791	11.070887
10.147794	709.345685	11.075904
10.455955	694.168406	11.080922
9.896837	700.842257	11.085939
10.532489	700.909959	11.090957
10.424742	700.904788	11.095975
10.359547	702.060607	11.100992
10.283332	704.922298	11.106010
10.421421	706.440744	11.111027
10.299642	710.524570	11.116045
10.380677	696.216014	11.121063
10.364619	707.200846	11.126080
10.586465	710.315642	11.131098
10.309051	706.288127	11.136115
10.190212	703.848396	11.141133
10.210156	702.551420	11.146151
10.120839	706.144161	11.151168
9.862665	706.020547	11.156186
9.848884	708.383304	11.161203
10.080348	707.245692	11.166221
10.096596	707.776519	11.171239
10.107838	729.234439	11.176256
10.521915	730.416153	11.181274
10.374380	727.999849	11.186291
10.501129	726.512567	11.191309
10.714331	728.079207	11.196327
10.572031	736.171004	11.201344
10.566029	737.102953	11.206362
10.405429	733.631492	11.211379
10.172087	735.646797	11.216397
10.411796	738.784046	11.221415
10.348509	739.762841	11.226432
10.637005	738.871914	11.231450
10.507114	736.702155	11.236467
10.362328	739.918582	11.241485
10.664426	733.872048	11.246503
10.458408	743.532814	11.251520
10.653022	731.112558	11.256538
10.539271	734.551341	11.261555
10.074981	734.592567	11.266573
10.225108	729.803776	11.271591
10.085350	743.301119	11.276608
10.594412	737.963778	11.281626
10.352079	742.975379	11.286643
10.490569	758.035456	11.291661
10.933021	761.765799	11.296679
10.439584	774.286621	11.301696
11.103270	763.244535	11.306714
10.721807	757.317718	11.311731
10.698384	747.926503	11.316749
10.688675	733.796238	11.321767
10.361949	746.833724	11.326784
10.900705	746.115027	11.331802
10.871846	757.013531	11.336819
10.484238	749.036386	11.341837
10.820997	747.304757	11.346855
10.990398	762.407332	11.351872
10.921777	753.076845	11.356890
10.811803	739.757556	11.361907
10.615507	740.889736	11.366925
10.905957	734.592561	11.371943
10.596921	738.579499	11.376960
11.050910	741.711577	11.381978
10.942192	738.295102	11.386995
10.525286	738.180579	11.392013
10.791669	741.058026	11.397031
10.897633	759.092840	11.402048
11.060218	762.567228	11.407066
10.915867	750.572458	11.412083
10.841436	735.735958	11.417101
10.843646	728.808598	11.422119
10.593533	740.817898	11.427136
10.978109	749.199538	11.432154
11.257413	755.991355	11.437171
10.876402	753.226617	11.442189
10.868986	749.923657	11.447207
10.965501	752.821410	11.452224
10.985413	759.723298	11.457242
11.184905	748.466771	11.462259
10.547151	752.076022	11.467277
11.342103	750.360965	11.472295
10.928174	750.498442	11.477312
10.823506	740.908519	11.482330
11.070113	747.162653	11.487347
11.055106	762.038499	11.492365
11.418039	756.553632	11.497383
11.052299	744.653514	11.502400
10.766521	743.009957	11.507418
10.909719	750.795094	11.512435
11.071278	756.964726	11.517453
11.295855	749.055766	11.522471
11.368613	758.581341	11.527488
10.987057	744.275798	11.532506
11.366052	751.620044	11.537523
10.853127	746.177736	11.542541
11.107548	746.434560	11.547559
10.739888	756.357346	11.552576
10.636116	760.602465	11.557594
11.267374	753.623873	11.562611
11.083224	749.941501	11.567629
11.044999	754.955840	11.572647
11.199641	759.119444	11.577664
11.155834	757.314896	11.582682
11.178989	752.378734	11.587699
11.192421	762.607890	11.592717
10.959745	757.295240	11.597735
11.407839	759.374196	11.602752
10.995245	756.841626	11.607770
11.311296	757.997674	11.612787
11.284839	751.248368	11.617805
11.442783	751.804334	11.622823
11.523211	762.474278	11.627840
11.351180	756.173816	11.632858
11.232210	755.065861	11.637875
11.061172	752.347121	11.642893
11.176157	754.481423	11.647911
11.349688	760.254700	11.652928
10.887434	759.856945	11.657946
11.387975	756.367098	11.662963
11.502247	783.902863	11.667981
11.552968	775.424677	11.672999
11.394929	768.541345	11.678016
11.198607	784.922551	11.683034
11.706826	780.421628	11.688051
11.233264	789.152337	11.693069
11.494923	782.427306	11.698087
11.791997	790.500779	11.703104
11.625801	781.520085	11.708122
11.347489	763.231458	11.713139
11.012503	772.666291	11.718157
11.175323	773.745362	11.723175
11.229115	786.524439	11.728192
11.203885	783.741822	11.733210
11.841257	782.092478	11.738227
11.502814	787.093903	11.743245
11.661429	782.884444	11.748263
11.666567	790.435606	11.753280
11.303680	783.959909	11.758298
11.469803	781.857376	11.763315
11.623850	793.847568	11.768333
11.758723	788.745568	11.773351
11.791730	789.150694	11.778368
11.684767	790.357244	11.783386
11.918521	782.718234	11.788403
11.719591	786.760516	11.793421
11.625142	787.343404	11.798439
11.767985	795.412642	11.803456
11.637062	796.373635	11.808474
11.796776	785.044421	11.813491
11.533979	789.882514	11.818509
11.426874	787.734426	11.823527
11.606785	797.230609	11.828544
11.445442	792.673642	11.833562
11.692067	787.333224	11.838579
11.436222	790.469229	11.843597
11.773155	790.321801	11.848615
11.557074	783.927245	11.853632
11.528015	793.512974	11.858650
11.918959	787.878540	11.863667
11.690569	795.185425	11.868685
11.990635	803.053305	11.873703
12.046950	796.445650	11.878720
11.554823	795.639159	11.883738
11.971262	796.170403	11.888755
11.980109	796.945393	11.893773
11.910022	783.480965	11.898791
11.577851	796.702379	11.903808
11.964497	806.727916	11.908826
12.299690	805.138539	11.913843
11.588424	803.779396	11.918861
12.148891	807.380802	11.923879
11.824710	811.256519	11.928896
11.674009	805.965725	11.933914
11.832739	814.370158	11.938931
11.864881	818.433047	11.943949
11.876187	812.791815	11.948967
11.564580	818.492798	11.953984
11.487520	821.543992	11.959002
12.046173	812.717958	11.964019
11.557523	827.863732	11.969037
11.875909	816.430741	11.974055
11.961214	818.844260	11.979072
11.952688	822.683146	11.984090
12.130848	829.904254	11.989107
12.197540	842.356297	11.994125
11.764475	832.170829	11.999143
12.074639	840.179157	12.004160
12.000915	841.481490	12.009178
12.153125	846.014730	12.014195
12.335676	847.235883	12.019213
12.328649	842.512712	12.024231
12.635636	842.748678	12.029248
12.072396	826.615894	12.034266
12.293760	821.279424	12.039283
11.935355	822.105644	12.044301
11.680888	824.626049	12.049319
12.536734	835.136673	12.054336
12.176602	838.345832	12.059354
12.423159	836.997561	12.064371
12.273201	844.134384	12.069389
12.402875	844.290833	12.074407
12.603254	842.823563	12.079424
11.836037	840.551674	12.084442
12.235635	836.235015	12.089459
12.291991	849.666997	12.094477
12.105251	844.956203	12.099495
12.086247	839.354426	12.104512
12.083119	848.024080	12.109530
12.034150	847.981297	12.114547
11.836156	854.005322	12.119565
12.283794	852.720220	12.124583
12.487239	838.698489	12.129600
12.254484	845.314947	12.134618
12.308439	846.849743	12.139635
12.268164	848.257290	12.144653
12.375873	846.962332	12.149671
12.763235	858.770843	12.154688
12.555233	849.061351	12.159706
12.626837	843.555831	12.164723
12.679532	848.896783	12.169741
12.411877	840.973387	12.174759
12.517207	844.863866	12.179776
12.402748	847.791534	12.184794
12.585059	839.216960	12.189811
12.500851	849.713933	12.194829
12.589007	842.359646	12.199847
12.786932	846.440749	12.204864
12.414528	838.445402	12.209882
12.547854	843.073120	12.214899
12.528979	847.273399	12.219917
12.665639	852.938872	12.224935
12.949165	845.512947	12.229952
12.437012	854.142436	12.234970
12.734662	850.577062	12.239987
12.836674	848.904294	12.245005
12.330928	844.934614	12.250023
12.408212	850.546273	12.255040
12.456214	848.790447	12.260058
13.015462	866.609180	12.265075
12.956212	866.577475	12.270093
12.563281	868.381111	12.275111
12.995931	868.603700	12.280128
12.582380	860.270802	12.285146
12.709861	855.182564	12.290163
12.868442	862.387819	12.295181
12.533228	870.345798	12.300199
12.832664	864.706743	12.305216
12.515736	868.631829	12.310234
12.843239	867.438134	12.315251
12.641361	862.818071	12.320269
12.678824	866.728657	12.325287
13.128727	861.558341	12.330304
12.849523	870.309132	12.335322
12.960506	859.470352	12.340339
12.827457	869.820352	12.345357
13.032381	858.193669	12.350375
12.753512	865.416971	12.355392
12.657358	873.261755	12.360410
13.197275	862.955380	12.365427
13.156557	863.962204	12.370445
12.685428	871.887830	12.375463
13.357800	861.254584	12.380480
13.174873	867.326747	12.385498
13.137447	864.104209	12.390515
13.154824	864.303499	12.395533
13.068069	870.474206	12.400551
13.179767	867.411341	12.405568
12.919478	867.871891	12.410586
12.831163	875.021159	12.415603
13.141750	869.771681	12.420621
12.846643	868.584017	12.425639
13.246747	865.400225	12.430656
13.331213	874.415935	12.435674
13.016106	861.210749	12.440691
13.235847	865.118021	12.445709
13.193161	866.207206	12.450727
13.122409	866.489733	12.455744
13.219449	867.481285	12.460762
12.952668	870.009938	12.465779
13.313982	874.191681	12.470797
12.911127	859.665316	12.475815
13.018633	857.493062	12.480832
12.733485	872.351364	12.485850
12.613652	862.691167	12.490867
13.161234	872.590538	12.495885
12.938258	878.911981	12.500903
13.360883	886.984762	12.505920
13.491650	894.592026	12.510938
13.702230	886.637861	12.515955
13.569564	873.959511	12.520973
12.976135	868.962131	12.525991
13.229265	855.538527	12.531008
13.162893	870.394108	12.536026
13.359654	881.086921	12.541043
13.636179	881.668493	12.546061
13.235134	893.275502	12.551079
13.581300	889.652025	12.556096
13.520840	893.751531	12.561114
13.489778	885.295576	12.566131
13.519361	874.567372	12.571149
13.230919	885.522406	12.576167
13.490427	885.674292	12.581184
13.645309	888.291517	12.586202
13.522290	881.150186	12.591219
13.675512	883.448929	12.596237
13.430658	890.285053	12.601255
13.777237	884.124200	12.606272
13.661168	873.999496	12.611290
13.522127	870.859151	12.616307
13.579682	863.055207	12.621325
13.527623	863.839742	12.626343
13.979399	866.915384	12.631360
13.717266	868.493395	12.636378
13.405856	869.085033	12.641395
13.621430	859.492208	12.646413
13.339852	874.700253	12.651431
13.322318	879.645112	12.656448
13.673050	888.082614	12.661466
13.169100	886.081900	12.666483
13.824754	881.488422	12.671501
13.694153	888.013149	12.676519
13.666435	885.069957	12.681536
13.607318	887.338853	12.686554
13.684420	885.824622	12.691571
13.574193	891.844376	12.696589
13.440273	888.308743	12.701607
13.438357	890.060583	12.706624
13.401719	883.764111	12.711642
13.572135	910.114137	12.716659
13.994689	913.408964	12.721677
13.683423	922.060660	12.726695
14.314708	919.541239	12.731712
14.248389	911.813488	12.736730
13.763970	897.934200	12.741747
14.037799	882.503361	12.746765
13.863271	888.044030	12.751783
14.130420	890.040897	12.756800
14.041685	887.968815	12.761818
13.573334	889.478151	12.766835
13.683381	882.224561	12.771853
13.705148	896.548793	12.776871
14.144197	903.672250	12.781888
14.155936	911.509614	12.786906
14.065288	912.192898	12.791923
14.467359	902.510868	12.796941
14.248704	896.334429	12.801959
13.983022	887.243035	12.806976
13.947139	885.216322	12.811994
14.061060	887.981979	12.817011
13.968774	883.379454	12.822029
13.370969	894.196769	12.827047
14.494803	903.485153	12.832064
14.218359	907.353411	12.837082
14.161446	918.486787	12.842099
14.280771	919.222381	12.847117
14.099354	929.336992	12.852135
14.318070	925.234850	12.857152
14.196260	921.454311	12.862170
14.489965	915.721462	12.867187
14.309772	906.474649	12.872205
14.093343	902.484873	12.877223
14.018662	890.071986	12.882240
14.181565	908.757605	12.887258
14.049152	917.406523	12.892275
14.221049	908.259181	12.897293
14.109017	924.737763	12.902311
14.226572	922.377730	12.907328
13.998402	919.178756	12.912346
14.082268	914.624364	12.917363
14.338637	917.418201	12.922381
14.153754	922.259902	12.927399
14.155426	918.977578	12.932416
13.796901	917.253882	12.937434
14.187962	929.588890	12.942451
14.716938	942.243132	12.947469
14.306908	941.632058	12.952487
14.441087	943.485659	12.957504
14.181222	936.460423	12.962522
14.557418	946.418247	12.967539
14.663688	946.291180	12.972557
14.380954	948.610899	12.977575
14.619105	950.807980	12.982592
14.721740	943.179979	12.987610
14.349703	945.788251	12.992627
14.864114	943.902533	12.997645
14.573930	940.785857	13.002663
14.631210	948.303669	13.007680
14.935065	952.671163	13.012698
14.778236	945.288945	13.017715
14.859476	919.871520	13.022733
14.436355	916.542142	13.027751
14.517418	913.099055	13.032768
14.553877	912.168713	13.037786
14.823400	928.470749	13.042803
14.978327	922.223145	13.047821
14.843558	919.741697	13.052839
14.716030	906.633322	13.057856
14.545058	903.775689	13.062874
14.590323	911.989659	13.067891
14.456500	926.240461	13.072909
14.485297	931.001347	13.077927
14.801017	952.951482	13.082944
14.915784	935.617282	13.087962
14.907228	942.514234	13.092979
15.037592	946.646971	13.097997
15.317151	935.601848	13.103015
14.992891	934.058978	13.108032
15.011223	921.644120	13.113050
14.688872	914.786476	13.118067
14.747798	915.802937	13.123085
14.709974	929.644218	13.128103
15.144095	942.348036	13.133120
15.076790	936.804291	13.138138
14.958607	930.905594	13.143155
15.256115	927.204524	13.148173
15.015762	932.099101	13.153191
14.918620	919.225801	13.158208
14.926139	909.813873	13.163226
15.174025	918.229633	13.168243
15.058672	907.312676	13.173261
14.966758	916.094105	13.178279
14.642604	912.414700	13.183296
15.316079	924.636027	13.188314
15.593845	927.237161	13.193331
14.875484	919.280203	13.198349
14.829241	928.553110	13.203367
15.056524	933.008336	13.208384
15.148790	930.065273	13.213402
15.049661	937.434015	13.218419
15.415246	935.650513	13.223437
15.539930	938.086282	13.228455
15.161715	934.210211	13.233472
15.246484	930.633993	13.238490
15.084912	939.372698	13.243507
15.204092	933.335823	13.248525
15.081506	946.732796	13.253543
15.311385	939.359420	13.258560
15.602241	934.832554	13.263578
15.422867	939.357809	13.268595
15.279701	936.331709	13.273613
15.526973	946.619009	13.278631
15.013149	944.020220	13.283648
15.505687	947.139983	13.288666
15.620920	938.935641	13.293683
15.461043	946.209761	13.298701
15.454007	937.652184	13.303719
15.024433	941.232011	13.308736
15.101318	943.577437	13.313754
14.975401	944.799590	13.318771
15.263474	940.699201	13.323789
15.304712	941.342887	13.328807
14.995522	947.763070	13.333824
15.225592	937.438927	13.338842
15.394469	946.962166	13.343859
15.328742	964.591734	13.348877
15.429748	963.007477	13.353895
15.382259	976.698827	13.358912
15.464810	961.076978	13.363930
15.131440	966.194425	13.368947
15.504532	968.449262	13.373965
15.081120	969.339324	13.378983
15.492089	975.902308	13.384000
15.590458	968.031962	13.389018
15.250119	982.163684	13.394035
15.719511	987.691859	13.399053
15.887678	993.497611	13.404071
16.025881	995.653551	13.409088
16.227887	982.591321	13.414106
15.725275	974.262856	13.419123
15.969027	968.471544	13.424141
16.040915	967.324204	13.429159
15.561021	968.576573	13.434176
16.035477	962.051668	13.439194
15.912760	967.789376	13.444211
15.754013	963.812639	13.449229
15.771131	964.529535	13.454247
15.706270	966.726756	13.459264
15.556963	952.220551	13.464282
16.030609	956.091217	13.469299
15.428123	951.426600	13.474317
15.679155	988.872780	13.479335
15.255844	985.278325	13.484352
15.770022	989.429833	13.489370
15.681442	990.687166	13.494387
15.685680	993.189152	13.499405
16.052367	985.993142	13.504423
15.940332	991.987966	13.509440
16.040302	982.627788	13.514458
15.794548	985.478217	13.519475
15.969222	981.695394	13.524493
15.882008	988.355374	13.529511
16.086808	997.746777	13.534528
16.218386	1005.445481	13.539546
16.205580	1011.424764	13.544563
16.075504	1005.549997	13.549581
16.327972	1002.449275	13.554599
16.311278	999.933537	13.559616
16.390847	985.994217	13.564634
15.982263	982.911864	13.569651
16.344578	993.452571	13.574669
16.434602	980.865489	13.579687
16.396883	982.723936	13.584704
16.106429	988.276488	13.589722
16.328306	998.406847	13.594739
16.059487	991.300939	13.599757
16.129973	986.751781	13.604775
16.331788	1005.109505	13.609792
16.310821	1014.993892	13.614810
16.649656	1018.121971	13.619827
16.391468	1004.522742	13.624845
16.180200	996.842913	13.629863
15.936077	1006.920054	13.634880
16.386584	1001.626525	13.639898
16.549868	1013.561768	13.644915
16.524435	1012.041500	13.649933
16.799871	1024.871228	13.654951
16.754523	1016.941326	13.659968
16.727569	1009.472459	13.664986
16.373638	994.483872	13.670003
16.250922	1004.286364	13.675021
16.978302	999.687930	13.680039
16.549846	1001.456118	13.685056
16.867731	996.177058	13.690074
16.717644	991.791850	13.695091
16.629906	987.295886	13.700109
16.253076	980.001773	13.705127
16.573165	995.576409	13.710144
16.644751	1002.312501	13.715162
16.564564	1002.621755	13.720179
16.728740	1013.629030	13.725197
16.602432	1004.499959	13.730215
16.454402	1008.628992	13.735232
16.728551	1004.126817	13.740250
16.592259	1008.541195	13.745267
16.722583	1008.262032	13.750285
16.822287	1006.498090	13.755303
16.531757	1008.563413	13.760320
16.916421	1013.580995	13.765338
17.051763	1013.326292	13.770355
16.700808	1008.868408	13.775373
16.791167	1006.316961	13.780391
16.815093	1011.185930	13.785408
17.075625	1014.007533	13.790426
16.850608	1007.279773	13.795443
16.663676	1013.431510	13.800461
16.654727	1004.631198	13.805479
16.793140	1010.649905	13.810496
16.729893	1005.979682	13.815514
16.954202	1008.251524	13.820531
16.592752	1003.804753	13.825549
17.214373	1018.707300	13.830567
17.130039	1021.532443	13.835584
16.873884	1015.639556	13.840602
17.181083	1011.826495	13.845619
16.808478	1009.568497	13.850637
17.007502	1020.879592	13.855655
17.347132	1033.765543	13.860672
17.395212	1034.638540	13.865690
17.167288	1020.236119	13.870707
17.044319	1005.498521	13.875725
17.046252	1011.538612	13.880743
17.124208	1020.306101	13.885760
17.181429	1024.090545	13.890778
17.156046	1035.742932	13.895795
17.127760	1039.285150	13.900813
17.285882	1027.293296	13.905831
17.359525	1041.047769	13.910848
17.261944	1037.613712	13.915866
17.597380	1039.836588	13.920883
17.578882	1036.860368	13.925901
17.428190	1029.830613	13.930919
17.713604	1023.991729	13.935936
17.306029	1012.678669	13.940954
17.319313	1004.581791	13.945971
17.191823	1013.656027	13.950989
17.258321	1015.154158	13.956007
17.278945	1031.337492	13.961024
17.058958	1034.669898	13.966042
17.319353	1034.341952	13.971059
17.485869	1029.967090	13.976077
17.670575	1034.167075	13.981095
17.213178	1038.155233	13.986112
17.372875	1035.858012	13.991130
17.623880	1026.909659	13.996147
17.390986	1038.288439	14.001165
17.476391	1035.368525	14.006183
17.496746	1039.458558	14.011200
17.339348	1026.146486	14.016218
17.448878	1024.854386	14.021235
17.330917	1037.133519	14.026253
17.783842	1050.131122	14.031271
17.899721	1057.977480	14.036288
17.683821	1056.774237	14.041306
17.940912	1063.269842	14.046323
17.541200	1052.072293	14.051341
17.451315	1042.877534	14.056359
17.592351	1059.707919	14.061376
17.813548	1060.711588	14.066394
17.909691	1058.152915	14.071411
17.920154	1063.402715	14.076429
17.950042	1048.426532	14.081447
17.795076	1065.571551	14.086464
17.843534	1059.053395	14.091482
17.929160	1056.546864	14.096499
17.985366	1063.433716	14.101517
17.984522	1058.545412	14.106535
17.952462	1061.501231	14.111552
17.709242	1061.204853	14.116570
18.137140	1053.614207	14.121587
17.863196	1059.965790	14.126605
18.019240	1045.067675	14.131623
17.695207	1058.259603	14.136640
17.955833	1058.329263	14.141658
18.117459	1055.813980	14.146675
17.646241	1060.255601	14.151693
17.957597	1058.834043	14.156711
18.024662	1053.206091	14.161728
17.997148	1061.412597	14.166746
17.944245	1055.320589	14.171763
18.056018	1050.613464	14.176781
17.788311	1050.270428	14.181799
18.009942	1069.032222	14.186816
18.120546	1071.801583	14.191834
18.377786	1073.932571	14.196851
18.097267	1079.518309	14.201869
18.063540	1072.321884	14.206887
18.394130	1076.533737	14.211904
17.746967	1081.144944	14.216922
18.266688	1076.364427	14.221939
18.276283	1083.993913	14.226957
18.371693	1075.407595	14.231975
18.153440	1082.974947	14.236992
18.346014	1082.357816	14.242010
18.196439	1080.156385	14.247027
18.560419	1073.888597	14.252045
18.426527	1072.003455	14.257063
18.322591	1069.504532	14.262080
18.287971	1076.509764	14.267098
18.472144	1064.008861	14.272115
18.434483	1081.163918	14.277133
18.727946	1084.062426	14.282151
18.543217	1077.886920	14.287168
18.345119	1080.253358	14.292186
18.838055	1075.742133	14.297203
18.766013	1086.732813	14.302221
18.968335	1083.532633	14.307239
18.827807	1066.875796	14.312256
18.606297	1074.749777	14.317274
18.828384	1062.631109	14.322291
18.330120	1062.718683	14.327309
18.731044	1069.261185	14.332327
18.694682	1066.691713	14.337344
18.645815	1064.730131	14.342362
18.761468	1071.317330	14.347379
18.620066	1080.384312	14.352397
18.882565	1091.265773	14.357415
19.031773	1084.902240	14.362432
18.681650	1090.760827	14.367450
19.196762	1084.071713	14.372467
18.902951	1073.425619	14.377485
18.864726	1072.869898	14.382503
18.750796	1067.879386	14.387520
18.853299	1078.931079	14.392538
19.172886	1076.892831	14.397555
19.075874	1082.809590	14.402573
18.794046	1074.525383	14.407591
18.984323	1079.788041	14.412608
18.861376	1097.328873	14.417626
19.304028	1092.775027	14.422643
19.052984	1095.493755	14.427661
19.116378	1092.712984	14.432679
19.060421	1098.506547	14.437696
19.066152	1099.307286	14.442714
19.162020	1091.090129	14.447731
19.080433	1097.837632	14.452749
19.194752	1092.107587	14.457767
19.436113	1092.606311	14.462784
19.127047	1087.207698	14.467802
19.188569	1090.098365	14.472819
19.130418	1095.355769	14.477837
19.111529	1085.884769	14.482855
19.564661	1083.276471	14.487872
19.082973	1093.880046	14.492890
19.292034	1089.618429	14.497907
19.271485	1098.451884	14.502925
18.959937	1101.656633	14.507943
19.373004	1093.976772	14.512960
19.272992	1095.617767	14.517978
19.223345	1094.142313	14.522995
19.145543	1103.596985	14.528013
19.156659	1100.477255	14.533031
19.558669	1093.720649	14.538048
19.187058	1089.676247	14.543066
19.292992	1087.658850	14.548083
19.299840	1093.076488	14.553101
19.444508	1098.576678	14.558119
19.821850	1105.621520	14.563136
19.361953	1111.816058	14.568154
19.745035	1108.663294	14.573171
19.941482	1112.719442	14.578189
19.596548	1098.991717	14.583207
19.748690	1087.190114	14.588224
19.748980	1092.450985	14.593242
19.576682	1090.524519	14.598259
19.368794	1088.919220	14.603277
19.381241	1101.761806	14.608295
19.623574	1110.806550	14.613312
19.668678	1115.063142	14.618330
20.020382	1103.810946	14.623347
20.015419	1120.433883	14.628365
19.748928	1110.373640	14.633383
20.005075	1106.133044	14.638400
19.718652	1118.170376	14.643418
19.746636	1117.279222	14.648435
19.794714	1121.153485	14.653453
19.724747	1119.217295	14.658471
19.921893	1114.812367	14.663488
19.791345	1118.866100	14.668506
19.760134	1114.130866	14.673523
19.926193	1115.383026	14.678541
19.765806	1113.823932	14.683559
19.687438	1111.349400	14.688576
19.720340	1110.684700	14.693594
19.631800	1102.865671	14.698611
19.907510	1125.005329	14.703629
20.407143	1133.653155	14.708647
20.205344	1137.636002	14.713664
20.316918	1136.327794	14.718682
20.091386	1137.470891	14.723699
20.292117	1138.739711	14.728717
20.170490	1125.380934	14.733735
20.242622	1124.820544	14.738752
20.164740	1138.071796	14.743770
20.441918	1133.300863	14.748787
20.280221	1123.227349	14.753805
20.469404	1126.400986	14.758823
20.417719	1117.228606	14.763840
20.153178	1109.475021	14.768858
20.196579	1113.927545	14.773875
20.125055	1123.668431	14.778893
20.287919	1132.381644	14.783911
20.168139	1126.675643	14.788928
20.226576	1138.731542	14.793946
20.349057	1131.665258	14.798963
20.393995	1129.834143	14.803981
20.549183	1135.916539	14.808999
20.598792	1135.874089	14.814016
20.699889	1135.826729	14.819034
20.612483	1131.305429	14.824051
20.824478	1133.380395	14.829069
20.476004	1140.217069	14.834087
20.602796	1135.444450	14.839104
20.455141	1138.819193	14.844122
20.788686	1134.560152	14.849139
20.856021	1129.891527	14.854157
20.258275	1131.130813	14.859175
20.785735	1129.296683	14.864192
20.582554	1141.822777	14.869210
20.615065	1129.522322	14.874227
20.797067	1134.641121	14.879245
20.665505	1133.872797	14.884263
20.873925	1130.040473	14.889280
20.406919	1132.464829	14.894298
20.566240	1131.139673	14.899315
21.138793	1129.888632	14.904333
20.522774	1140.696324	14.909351
20.592837	1138.065984	14.914368
20.563395	1138.995315	14.919386
20.830926	1154.161745	14.924403
20.806556	1146.875458	14.929421
20.603158	1156.624400	14.934439
20.900167	1157.149122	14.939456
20.978782	1166.314224	14.944474
21.157984	1162.262401	14.949491
21.427381	1158.284813	14.954509
20.984519	1167.862991	14.959527
21.513968	1155.203781	14.964544
21.431783	1155.226164	14.969562
21.183353	1156.350759	14.974579
21.142280	1161.917941	14.979597
21.024350	1167.923215	14.984615
21.019474	1155.685406	14.989632
21.026494	1161.828896	14.994650
21.338603	1165.977392	14.999667
21.351038	1161.718161	15.004685
20.931422	1162.055353	15.009703
21.408357	1151.881762	15.014720
21.470486	1158.269089	15.019738
21.218658	1159.766613	15.024755
21.210500	1160.515879	15.029773
21.421144	1161.442310	15.034791
21.333729	1154.367876	15.039808
21.381317	1157.298608	15.044826
21.327331	1158.506350	15.049843
21.464060	1157.197355	15.054861
21.072188	1157.918376	15.059879
21.486301	1156.505959	15.064896
21.136966	1161.209383	15.069914
21.437147	1172.088145	15.074931
21.182997	1181.655698	15.079949
21.369578	1184.466823	15.084967
21.476904	1183.093004	15.089984
21.717334	1188.455137	15.095002
21.098735	1189.006549	15.100019
21.431299	1186.925229	15.105037
21.307801	1194.433599	15.110055
21.304436	1187.737317	15.115072
21.726103	1196.905491	15.120090
21.624618	1210.908447	15.125107
22.044235	1207.267086	15.130125
22.067965	1211.886824	15.135143
21.921715	1195.322285	15.140160
21.989989	1193.272906	15.145178
21.933895	1184.142210	15.150195
22.074815	1179.159076	15.155213
21.983001	1177.245238	15.160231
22.093223	1176.716749	15.165248
21.943453	1177.680714	15.170266
21.752200	1177.268891	15.175283
22.088201	1175.379544	15.180301
21.946232	1177.869749	15.185319
21.990598	1176.540509	15.190336
21.718272	1181.354953	15.195354
21.721968	1200.996816	15.200371
21.885395	1198.954619	15.205389
21.755980	1206.091522	15.210407
21.841051	1206.841963	15.215424
22.104996	1199.854477	15.220442
22.077667	1203.409202	15.225459
22.279175	1208.051579	15.230477
22.438635	1211.375060	15.235495
22.742898	1203.175695	15.240512
22.725340	1203.030157	15.245530
22.630867	1197.869296	15.250547
22.568555	1195.177635	15.255565
22.447360	1197.648807	15.260583
22.453678	1185.715348	15.265600
22.204125	1179.663576	15.270618
22.302651	1185.830609	15.275635
22.592975	1189.666931	15.280653
22.517176	1190.401550	15.285671
22.177484	1187.160038	15.290688
22.604627	1185.168045	15.295706
22.413046	1202.533534	15.300723
22.693972	1196.909900	15.305741
22.322236	1200.597483	15.310759
22.698235	1192.784529	15.315776
22.570418	1207.858307	15.320794
22.661812	1206.452267	15.325811
22.861987	1197.278255	15.330829
22.851731	1199.012498	15.335847
22.579781	1183.165122	15.340864
22.636250	1180.962954	15.345882
22.642709	1196.577437	15.350899
22.958568	1198.367884	15.355917
22.633750	1200.700541	15.360935
22.651488	1197.182112	15.365952
22.603049	1203.993892	15.370970
22.587720	1195.749926	15.375987
22.664347	1196.476443	15.381005
22.853836	1201.395266	15.386023
22.588613	1189.005714	15.391040
22.871232	1193.909944	15.396058
22.677533	1202.240386	15.401075
23.117223	1183.933509	15.406093
22.655642	1194.764375	15.411111
22.884211	1193.024407	15.416128
23.041188	1196.818506	15.421146
22.736167	1204.513117	15.426163
23.106839	1204.786449	15.431181
23.150914	1213.458352	15.436199
23.120638	1215.842696	15.441216
23.223498	1212.055297	15.446234
22.979410	1216.265701	15.451251
23.005523	1207.128425	15.456269
23.455328	1217.403083	15.461287
23.479629	1214.672601	15.466304
23.198719	1210.749665	15.471322
23.270986	1216.983940	15.476339
23.264085	1212.222781	15.481357
23.346791	1210.423612	15.486375
23.217485	1211.775706	15.491392
23.619689	1211.712727	15.496410
23.142764	1216.622355	15.501427
23.307891	1215.678150	15.506445
23.495901	1216.920565	15.511463
23.311456	1219.799296	15.516480
23.351820	1218.981939	15.521498
23.713685	1209.470152	15.526515
23.427707	1201.126574	15.531533
23.906816	1212.305541	15.536551
23.359081	1213.477034	15.541568
23.573126	1208.034295	15.546586
23.420294	1213.836762	15.551603
23.694784	1208.242536	15.556621
23.774958	1207.441033	15.561639
23.590046	1206.545360	15.566656
23.885840	1209.935846	15.571674
23.764948	1210.087374	15.576691
23.693531	1204.197039	15.581709
23.652632	1214.125687	15.586727
23.450278	1208.722941	15.591744
23.767671	1205.523646	15.596762
23.723648	1216.989715	15.601779
23.981660	1209.886386	15.606797
23.780599	1211.315997	15.611815
23.782235	1208.532261	15.616832
23.917980	1208.122853	15.621850
24.029151	1218.327488	15.626867
23.883574	1214.544299	15.631885
23.744510	1216.358687	15.636903
23.686723	1218.318136	15.641920
23.838705	1215.621300	15.646938
23.875645	1207.949828	15.651955
23.875046	1220.554694	15.656973
23.924066	1241.385593	15.661991
24.205967	1246.018540	15.667008
24.309533	1233.542772	15.672026
24.212270	1238.241437	15.677043
24.294419	1239.699263	15.682061
24.210396	1227.767306	15.687079
23.999226	1239.994909	15.692096
24.752368	1237.664644	15.697114
24.246106	1228.670731	15.702131
24.248119	1233.054027	15.707149
24.148132	1235.708081	15.712167
24.132150	1234.978450	15.717184
24.507884	1236.267196	15.722202
24.198016	1238.663790	15.727219
24.216948	1236.609513	15.732237
24.060535	1230.521040	15.737255
24.219071	1235.267991	15.742272
24.237037	1234.075432	15.747290
24.146175	1248.237705	15.752307
24.493555	1252.926669	15.757325
24.145530	1262.919243	15.762343
24.406263	1262.149411	15.767360
24.376867	1257.634770	15.772378
24.584718	1263.939341	15.777395
24.762415	1258.193000	15.782413
24.822856	1251.688676	15.787431
24.335513	1263.085374	15.792448
24.521465	1251.533995	15.797466
24.412828	1257.146509	15.802483
24.627960	1252.527282	15.807501
24.589283	1272.141147	15.812519
24.483336	1275.796569	15.817536
24.969856	1280.937130	15.822554
25.206260	1285.583528	15.827571
25.175723	1279.712010	15.832589
25.260114	1276.258864	15.837607
24.980672	1277.101135	15.842624
24.982329	1267.210237	15.847642
24.737404	1270.521346	15.852659
25.142357	1287.872351	15.857677
24.962441	1291.110160	15.862695
25.143136	1300.562305	15.867712
25.194310	1286.261113	15.872730
25.425180	1287.632524	15.877747
25.088587	1276.469126	15.882765
24.989814	1270.488378	15.887783
25.004077	1287.834322	15.892800
25.362087	1285.610143	15.897818
25.121618	1284.505411	15.902835
25.361526	1286.853744	15.907853
25.536711	1281.423383	15.912871
25.157698	1286.595410	15.917888
25.346201	1281.289200	15.922906
25.284849	1284.596797	15.927923
25.530165	1281.481368	15.932941
25.400143	1278.270107	15.937959
25.317332	1281.038246	15.942976
25.307284	1275.289756	15.947994
25.261122	1279.046270	15.953011
25.339492	1283.995150	15.958029
25.490189	1281.513108	15.963047
25.241727	1285.904102	15.968064
25.503808	1285.437027	15.973082
25.336667	1285.816717	15.978099
25.361529	1279.182252	15.983117
25.641763	1281.372781	15.988135
25.793093	1301.389270	15.993152
25.628928	1290.463947	15.998170
25.681121	1294.034634	16.003187
25.824685	1302.394334	16.008205
26.152239	1304.997191	16.013223
25.486532	1303.189036	16.018240
25.490881	1303.327254	16.023258
25.526260	1309.056080	16.028275
25.604862	1305.834219	16.033293
25.956263	1298.848771	16.038311
25.608180	1308.308027	16.043328
25.684164	1295.552504	16.048346
25.707991	1307.686526	16.053363
25.966670	1307.816455	16.058381
25.989394	1306.743071	16.063399
25.809270	1323.668208	16.068416
26.080467	1320.384608	16.073434
25.639266	1330.903081	16.078451
25.979932	1334.255001	16.083469
26.027973	1332.855743	16.088487
25.893744	1337.844260	16.093504
26.196978	1332.570553	16.098522
26.116368	1340.567747	16.103539
26.146208	1343.245658	16.108557
26.395672	1330.551296	16.113575
26.624082	1331.708491	16.118592
26.519257	1326.268338	16.123610
26.430423	1335.942620	16.128627
26.378232	1335.272309	16.133645
26.574122	1322.901939	16.138663
26.525387	1336.511705	16.143680
26.316264	1339.075571	16.148698
26.737321	1329.576538	16.153715
26.485468	1328.543018	16.158733
26.715286	1329.024622	16.163751
26.033215	1336.390185	16.168768
26.520173	1332.741404	16.173786
26.546625	1329.565581	16.178803
26.523021	1340.867577	16.183821
26.796215	1326.099204	16.188839
26.371555	1337.571337	16.193856
26.714777	1345.019268	16.198874
26.705548	1358.827997	16.203891
26.824683	1357.603799	16.208909
26.958938	1358.251862	16.213927
27.012007	1361.355345	16.218944
26.874737	1351.441984	16.223962
27.051041	1346.775166	16.228979
26.756439	1335.115982	16.233997
27.016958	1335.851563	16.239015
26.770814	1343.735833	16.244032
26.879308	1350.949132	16.249050
27.201712	1358.719081	16.254067
27.389169	1364.285236	16.259085
27.176520	1337.505714	16.264103
26.820577	1333.780707	16.269120
26.943451	1340.278507	16.274138
26.755416	1351.615741	16.279155
26.858253	1360.938100	16.284173
27.298519	1362.264085	16.289191
27.180103	1356.601979	16.294208
26.953433	1372.208958	16.299226
27.066175	1364.932660	16.304243
26.936113	1360.083455	16.309261
27.294216	1361.750531	16.314279
27.130139	1367.987175	16.319296
27.081452	1360.736171	16.324314
27.061115	1362.077515	16.329331
27.060228	1382.108476	16.334349
27.459360	1377.930624	16.339367
27.395854	1379.335540	16.344384
27.499833	1381.878760	16.349402
27.474029	1384.309765	16.354419
27.497283	1382.390500	16.359437
27.570967	1373.163630	16.364455
27.809252	1377.692988	16.369472
27.664411	1382.064614	16.374490
27.627385	1379.965437	16.379507
27.748454	1386.005924	16.384525
27.899878	1377.366503	16.389543
27.662598	1382.292279	16.394560
27.590263	1382.944308	16.399578
27.863183	1383.927268	16.404595
27.638659	1389.245541	16.409613
28.073354	1388.016082	16.414631
27.843627	1374.623561	16.419648
27.746026	1375.500464	16.424666
27.831899	1372.937044	16.429683
27.764820	1382.560604	16.434701
27.935392	1380.794990	16.439719
28.353660	1396.364061	16.444736
28.229851	1384.788543	16.449754
28.122566	1372.705493	16.454771
28.325291	1373.642644	16.459789
28.115082	1382.013627	16.464807
28.004856	1377.098191	16.469824
28.107445	1377.069532	16.474842
28.265596	1374.671520	16.479859
28.354113	1372.173960	16.484877
28.192268	1373.729990	16.489895
28.181497	1387.838797	16.494912
28.333636	1395.537604	16.499930
28.671592	1394.686237	16.504947
28.462118	1391.525275	16.509965
28.512335	1387.487299	16.514983
28.347232	1378.648151	16.520000
28.327600	1395.279953	16.525018
28.710073	1399.376452	16.530035
28.435942	1405.428370	16.535053
28.302434	1401.905194	16.540071
28.248060	1402.172539	16.545088
28.204869	1403.195561	16.550106
28.548303	1403.589935	16.555123
28.238426	1404.922996	16.560141
28.505225	1397.168090	16.565159
28.452643	1392.783286	16.570176
28.182226	1399.115500	16.575194
28.443812	1406.282744	16.580211
28.800696	1418.099558	16.585229
29.066818	1419.194044	16.590247
29.266077	1433.058530	16.595264
29.025063	1417.190320	16.600282
29.058132	1397.782388	16.605299
28.750357	1405.398617	16.610317
28.805437	1396.774281	16.615335
28.991535	1406.560167	16.620352
28.664248	1423.656785	16.625370
29.220625	1416.484535	16.630387
29.124242	1426.485112	16.635405
29.345576	1424.244460	16.640423
29.164848	1419.037087	16.645440
29.171664	1424.732554	16.650458
29.230548	1416.205447	16.655475
28.909784	1423.252492	16.660493
28.756781	1424.037087	16.665511
28.827493	1426.323581	16.670528
29.021031	1426.795093	16.675546
29.333608	1415.690851	16.680563
28.997793	1424.794779	16.685581
29.112720	1427.923298	16.690599
29.351425	1437.183381	16.695616
29.461358	1450.512741	16.700634
29.326772	1443.578134	16.705651
29.175592	1463.194054	16.710669
29.416636	1447.225041	16.715687
29.645948	1452.364924	16.720704
29.554899	1449.554644	16.725722
29.832888	1444.900272	16.730739
29.510316	1455.561184	16.735757
29.706156	1450.575682	16.740775
29.588671	1457.606670	16.745792
29.442168	1459.520083	16.750810
29.540546	1450.361892	16.755827
29.535294	1446.367309	16.760845
29.685267	1442.985911	16.765863
29.890569	1445.409118	16.770880
29.789020	1449.041795	16.775898
30.053866	1450.979123	16.780915
30.102858	1451.533246	16.785933
30.331589	1449.272496	16.790951
30.500692	1448.523325	16.795968
29.918474	1439.626417	16.800986
29.860442	1439.073787	16.806003
30.110215	1442.256923	16.811021
29.864275	1440.733296	16.816039
30.129761	1439.249466	16.821056
29.744698	1441.519006	16.826074
30.270661	1450.008219	16.831091
30.443403	1456.324670	16.836109
30.577296	1466.478548	16.841127
30.551827	1446.830414	16.846144
30.383833	1447.835120	16.851162
30.368323	1433.102425	16.856179
30.260283	1447.788279	16.861197
30.149265	1434.607498	16.866215
30.379827	1443.884641	16.871232
30.143032	1467.531516	16.876250
30.209436	1468.799315	16.881267
30.278915	1468.842118	16.886285
30.214360	1463.780640	16.891303
30.603077	1469.097534	16.896320
30.566836	1467.995508	16.901338
30.667799	1460.945089	16.906355
30.356394	1473.889178	16.911373
30.536221	1476.953885	16.916391
30.654202	1460.701169	16.921408
30.421499	1469.527020	16.926426
30.501497	1473.579404	16.931443
30.645300	1489.175779	16.936461
30.784034	1493.503001	16.941479
31.158468	1487.353359	16.946496
30.876929	1496.868564	16.951514
31.172765	1496.986361	16.956531
31.093077	1494.789708	16.961549
30.869319	1495.569612	16.966567
31.528702	1492.843731	16.971584
31.049951	1492.161347	16.976602
31.130351	1476.570946	16.981619
31.123377	1472.595563	16.986637
31.227115	1475.839458	16.991655
31.539557	1469.507021	16.996672
31.636986	1453.468981	17.001690
31.589457	1447.110897	17.006707
31.573694	1445.727939	17.011725
31.933211	1446.937188	17.016743
32.037049	1454.905533	17.021760
31.778979	1453.661530	17.026778
31.614311	1435.382812	17.031795
31.621139	1426.923820	17.036813
31.409835	1417.782607	17.041831
31.623620	1410.522018	17.046848
31.520706	1419.235986	17.051866
31.656091	1411.851975	17.056883
31.411690	1417.309076	17.061901
31.412103	1414.402417	17.066919
31.641724	1421.284328	17.071936
31.367272	1438.887103	17.076954
31.263682	1441.033642	17.081971
32.024247	1437.187331	17.086989
31.921735	1448.738456	17.092007
32.174795	1442.781423	17.097024
31.897885	1445.390641	17.102042
32.253611	1435.772394	17.107059
31.803445	1430.152776	17.112077
31.892034	1423.233705	17.117095
32.229081	1424.853591	17.122112
31.947411	1429.704280	17.127130
31.880701	1425.741423	17.132147
32.257710	1433.499693	17.137165
31.910134	1434.431545	17.142183
32.050856	1437.139437	17.147200
32.100573	1440.953550	17.152218
31.968415	1436.439184	17.157235
32.001416	1438.362342	17.162253
31.822351	1436.888200	17.167271
32.297964	1425.130372	17.172288
32.043706	1435.742698	17.177306
31.905970	1437.029855	17.182323
32.065393	1440.656357	17.187341
32.375656	1443.823705	17.192359
32.511766	1448.905602	17.197376
32.351446	1453.614202	17.202394
32.669818	1467.109742	17.207411
32.669629	1448.707405	17.212429
32.312898	1449.536545	17.217447
32.547226	1452.359168	17.222464
32.439364	1459.836796	17.227482
32.711905	1460.949214	17.232499
32.782950	1453.578422	17.237517
32.630252	1461.454414	17.242535
32.872281	1456.796205	17.247552
32.740254	1465.505289	17.252570
32.923998	1466.306557	17.257587
33.234467	1467.349914	17.262605
32.524185	1457.232768	17.267623
32.802201	1458.741980	17.272640
32.829051	1464.831972	17.277658
32.304369	1458.810588	17.282675
32.842927	1468.670680	17.287693
32.452237	1461.416412	17.292711
32.529585	1463.919633	17.297728
32.918126	1474.093580	17.302746
33.249298	1487.681809	17.307763
33.345150	1484.435121	17.312781
32.927925	1485.289520	17.317799
33.359007	1476.322198	17.322816
32.814712	1492.395634	17.327834
33.412519	1486.738041	17.332851
33.379147	1485.247380	17.337869
32.837220	1493.588333	17.342887
33.201203	1488.226164	17.347904
32.915048	1504.183422	17.352922
33.127227	1489.219336	17.357939
33.154577	1487.031161	17.362957
32.947954	1497.853822	17.367975
33.561681	1508.311260	17.372992
33.150652	1513.043376	17.378010
33.368215	1521.994376	17.383027
33.399103	1514.014436	17.388045
33.156474	1525.129948	17.393063
33.419380	1516.826462	17.398080
33.345740	1530.575983	17.403098
33.513635	1538.670036	17.408115
33.523417	1541.644626	17.413133
33.964215	1549.856881	17.418151
34.075243	1541.734978	17.423168
34.363355	1538.685387	17.428186
34.385840	1537.662522	17.433203
34.192505	1539.248748	17.438221
34.129505	1530.860610	17.443239
34.002083	1513.658476	17.448256
33.917295	1518.446782	17.453274
33.653444	1533.254954	17.458291
34.048967	1536.961255	17.463309
34.351404	1537.374680	17.468327
34.215619	1541.823825	17.473344
34.284549	1541.895119	17.478362
34.387530	1533.383139	17.483379
34.348783	1518.878088	17.488397
34.296438	1529.430430	17.493415
34.055758	1527.438887	17.498432
34.357800	1531.424935	17.503450
34.397631	1532.106735	17.508467
34.870417	1522.375422	17.513485
34.312660	1521.048973	17.518503
34.491575	1517.167539	17.523520
34.752281	1525.471118	17.528538
34.696404	1526.385675	17.533555
34.505865	1523.448953	17.538573
34.805819	1516.840731	17.543591
34.875461	1517.631474	17.548608
34.684159	1517.503687	17.553626
34.606195	1519.990222	17.558643
34.835579	1516.220807	17.563661
35.004794	1526.388120	17.568679
34.682927	1518.709614	17.573696
34.579288	1515.169111	17.578714
34.655228	1523.489015	17.583731
34.807282	1511.242155	17.588749
34.889638	1523.641723	17.593767
35.107521	1536.881646	17.598784
35.246184	1537.074565	17.603802
34.862385	1543.860118	17.608819
35.108237	1545.049311	17.613837
34.812569	1539.777856	17.618855
34.892492	1543.770305	17.623872
34.968776	1539.412613	17.628890
34.674127	1543.665731	17.633907
35.028662	1539.864079	17.638925
34.990306	1543.202836	17.643943
35.220920	1554.102200	17.648960
35.482796	1562.636000	17.653978
35.326581	1565.551391	17.658995
35.271865	1564.360730	17.664013
35.383972	1570.352188	17.669031
35.632660	1573.791153	17.674048
35.386538	1573.047070	17.679066
35.347111	1577.885092	17.684083
35.455133	1567.428222	17.689101
35.595758	1573.973822	17.694119
35.406208	1572.267770	17.699136
35.703489	1572.508425	17.704154
35.643598	1578.025033	17.709171
35.772509	1587.232966	17.714189
35.811257	1599.285948	17.719207
35.939258	1606.246972	17.724224
35.883340	1596.967706	17.729242
35.638403	1599.205842	17.734259
36.031379	1594.956318	17.739277
36.187771	1603.367801	17.744295
36.089524	1599.747537	17.749312
36.037767	1590.066812	17.754330
36.192062	1598.175647	17.759347
36.305564	1595.813006	17.764365
36.172752	1602.874855	17.769383
36.117359	1592.333115	17.774400
36.154900	1590.742968	17.779418
36.163170	1601.023908	17.784435
36.489885	1598.918211	17.789453
36.160000	1598.493381	17.794471
35.825296	1599.571555	17.799488
36.446705	1606.029214	17.804506
37.073063	1616.939200	17.809523
37.229830	1593.986436	17.814541
36.876112	1579.780007	17.819559
36.863624	1581.909133	17.824576
37.300483	1568.898047	17.829594
37.057988	1571.599726	17.834611
37.490453	1573.801157	17.839629
37.105390	1560.839954	17.844647
36.809265	1556.262881	17.849664
36.916033	1548.100615	17.854682
37.297283	1545.898012	17.859699
37.013251	1531.907932	17.864717
36.781242	1540.828389	17.869735
36.986679	1548.348489	17.874752
37.038163	1537.285079	17.879770
36.933580	1539.270832	17.884787
36.775381	1535.448523	17.889805
36.839568	1556.570919	17.894823
37.112810	1562.928470	17.899840
37.372197	1567.883783	17.904858
37.133309	1567.223778	17.909875
37.646432	1565.467597	17.914893
37.283474	1566.957317	17.919911
37.413792	1570.140257	17.924928
37.374553	1561.757850	17.929946
37.284314	1568.238628	17.934963
37.475836	1564.197409	17.939981
37.513688	1563.913790	17.944999
37.366393	1557.978419	17.950016
37.608385	1559.187154	17.955034
37.540484	1562.098175	17.960051
37.292199	1569.313811	17.965069
37.307396	1569.595506	17.970087
37.920142	1571.550928	17.975104
37.204703	1568.929981	17.980122
37.405864	1574.727597	17.985139
37.421548	1573.604805	17.990157
37.445924	1587.856594	17.995175
37.395459	1592.077778	18.000192
37.735285	1593.296434	18.005210
37.504659	1595.595447	18.010227
37.904040	1600.380504	18.015245
37.881272	1593.737605	18.020263
37.817254	1597.661095	18.025280
37.998013	1607.438460	18.030298
37.967978	1628.174892	18.035315
37.908483	1615.345688	18.040333
38.109054	1620.824657	18.045351
38.079465	1622.899660	18.050368
38.439011	1624.718023	18.055386
38.312674	1632.100781	18.060403
38.333656	1627.663365	18.065421
38.205099	1619.790416	18.070439
38.168892	1621.399369	18.075456
38.371216	1614.594956	18.080474
38.219791	1623.341872	18.085491
38.230457	1630.330757	18.090509
38.393372	1646.252498	18.095527
38.297838	1654.331069	18.100544
38.707238	1646.146591	18.105562
38.528766	1646.042040	18.110579
38.594916	1648.468141	18.115597
38.722547	1645.680376	18.120615
38.676643	1649.771462	18.125632
38.902639	1638.870007	18.130650
39.044088	1640.776195	18.135667
38.984099	1650.771195	18.140685
38.717245	1649.304478	18.145703
38.809612	1644.256235	18.150720
39.265991	1648.947163	18.155738
38.775977	1653.410807	18.160755
39.056154	1656.396703	18.165773
39.301212	1666.893062	18.170791
39.252485	1674.058537	18.175808
39.604471	1662.954280	18.180826
39.464292	1661.410907	18.185843
39.619334	1646.622910	18.190861
39.559543	1649.583170	18.195879
39.541553	1638.950330	18.200896
39.645149	1632.423327	18.205914
39.522194	1646.316371	18.210931
39.362031	1631.644048	18.215949
39.712865	1626.271274	18.220967
39.570334	1642.490192	18.225984
39.716916	1632.418585	18.231002
39.320750	1634.803504	18.236019
39.603585	1644.249297	18.241037
39.701110	1660.998698	18.246055
39.558747	1672.385787	18.251072
40.200742	1663.603090	18.256090
39.975009	1659.750309	18.261107
39.608968	1661.616083	18.266125
39.903281	1669.087593	18.271143
39.839840	1662.649870	18.276160
40.171433	1661.932039	18.281178
40.015201	1662.947539	18.286195
39.713657	1670.913219	18.291213
39.619558	1658.351354	18.296231
39.907316	1667.158876	18.301248
40.090207	1661.114930	18.306266
39.802575	1664.164542	18.311283
40.026476	1675.655204	18.316301
40.154998	1676.654493	18.321319
40.037380	1688.864587	18.326336
40.286256	1683.375219	18.331354
40.069551	1693.151784	18.336371
39.976808	1689.009900	18.341389
40.021137	1693.970539	18.346407
40.323962	1716.321290	18.351424
40.455209	1711.443672	18.356442
40.349448	1714.281750	18.361459
40.534701	1716.360975	18.366477
40.933589	1708.228611	18.371495
40.876615	1722.682613	18.376512
40.836190	1712.173173	18.381530
40.976611	1713.997474	18.386547
40.701858	1708.413403	18.391565
41.029162	1709.425734	18.396583
40.941204	1715.196106	18.401600
41.193561	1713.666971	18.406618
41.062050	1716.837308	18.411635
41.065419	1710.373319	18.416653
40.990653	1710.312484	18.421671
41.025755	1711.676728	18.426688
41.156300	1714.626114	18.431706
41.060271	1711.702957	18.436723
41.103145	1707.798612	18.441741
41.173474	1719.423823	18.446759
41.305952	1737.348166	18.451776
41.561015	1735.117971	18.456794
41.709803	1729.843099	18.461811
41.537403	1735.146995	18.466829
41.643100	1725.918084	18.471847
41.280333	1731.507442	18.476864
41.735568	1729.293226	18.481882
41.688992	1726.804159	18.486899
41.503136	1726.691296	18.491917
42.013599	1722.997728	18.496935
41.705299	1725.842292	18.501952
41.892061	1722.123697	18.506970
41.807274	1725.832704	18.511987
41.792730	1729.287693	18.517005
41.744876	1725.287099	18.522023
42.137028	1718.427657	18.527040
41.914162	1712.475671	18.532058
41.991436	1718.131788	18.537075
41.822126	1720.680003	18.542093
42.055953	1718.532037	18.547111
41.728009	1728.335519	18.552128
42.206398	1731.842673	18.557146
42.324125	1736.236367	18.562163
42.390346	1745.801365	18.567181
42.671367	1743.254656	18.572199
42.328325	1752.852220	18.577216
42.432322	1741.458544	18.582234
42.585271	1744.776834	18.587251
42.601112	1743.770779	18.592269
42.791989	1742.529003	18.597287
42.527005	1753.370429	18.602304
42.473888	1733.773651	18.607322
42.512513	1736.869995	18.612339
42.378499	1742.688620	18.617357
42.596474	1740.132855	18.622375
42.430219	1742.349212	18.627392
42.454309	1738.548796	18.632410
42.890884	1750.536394	18.637427
42.723343	1739.696537	18.642445
42.521337	1749.401398	18.647463
42.777298	1776.209544	18.652480
42.979138	1777.661286	18.657498
42.971870	1778.770225	18.662515
42.727967	1772.070382	18.667533
43.104950	1776.069992	18.672551
42.790622	1776.835694	18.677568
42.957405	1774.325817	18.682586
43.060885	1783.449466	18.687603
42.892926	1796.996204	18.692621
43.209344	1794.096781	18.697639
42.908759	1812.123766	18.702656
43.136906	1804.210628	18.707674
43.474275	1796.662260	18.712691
43.452593	1809.684282	18.717709
43.510493	1801.207643	18.722727
43.686586	1812.835279	18.727744
43.719729	1818.760293	18.732762
44.034667	1825.032504	18.737779
44.153476	1825.338998	18.742797
43.784650	1797.431308	18.747815
43.825356	1803.645485	18.752832
43.915640	1816.255466	18.757850
44.237035	1811.755157	18.762867
44.132713	1815.565080	18.767885
44.079341	1812.322776	18.772903
43.941101	1816.100141	18.777920
43.794780	1819.768312	18.782938
44.296619	1822.416528	18.787955
44.543333	1823.832839	18.792973
44.508698	1814.587998	18.797991
44.242873	1816.400214	18.803008
44.309060	1811.261345	18.808026
44.708367	1821.575826	18.813043
44.389136	1822.080348	18.818061
44.755091	1814.316039	18.823079
44.262768	1818.874767	18.828096
44.125271	1817.312024	18.833114
43.938049	1813.929734	18.838131
44.209281	1817.264221	18.843149
44.334912	1812.062386	18.848167
44.501081	1837.972602	18.853184
44.259551	1848.576865	18.858202
44.588561	1846.615957	18.863219
44.603050	1853.882061	18.868237
44.787152	1849.920841	18.873255
44.776521	1849.404956	18.878272
44.659854	1854.567602	18.883290
44.583886	1864.401111	18.888307
44.861305	1864.783748	18.893325
45.192532	1867.386114	18.898343
45.204060	1873.507049	18.903360
45.044248	1868.615027	18.908378
45.497270	1869.131109	18.913395
45.207485	1871.975951	18.918413
45.197229	1870.708871	18.923431
45.512223	1872.376439	18.928448
45.174922	1874.120958	18.933466
45.497454	1862.853924	18.938483
45.497104	1866.183630	18.943501
45.386825	1864.351512	18.948519
45.428263	1875.952947	18.953536
45.486577	1880.352828	18.958554
45.878196	1878.214838	18.963571
45.671961	1884.808585	18.968589
45.944084	1888.935111	18.973607
45.747512	1887.978108	18.978624
45.806010	1893.507825	18.983642
46.044773	1882.569506	18.988659
45.494564	1894.771772	18.993677
45.879941	1885.420060	18.998695
45.869434	1891.935803	19.003712
45.899118	1891.075904	19.008730
46.285636	1892.075812	19.013747
45.680700	1890.624172	19.018765
45.947598	1894.066658	19.023783
46.026527	1904.125247	19.028800
46.126679	1905.135306	19.033818
46.283588	1913.815118	19.038835
46.033947	1913.014762	19.043853
46.152667	1912.431269	19.048871
46.093446	1912.535267	19.053888
46.262350	1925.057262	19.058906
46.520835	1939.332616	19.063923
46.242708	1940.695457	19.068941
46.511726	1932.406602	19.073959
46.931576	1936.115488	19.078976
46.511350	1937.131335	19.083994
46.864400	1932.490327	19.089011
47.067238	1934.525794	19.094029
46.907116	1928.109434	19.099047
46.722772	1936.094741	19.104064
46.926597	1940.222512	19.109082
47.051523	1945.640843	19.114099
47.122759	1958.238129	19.119117
47.304431	1964.281941	19.124135
47.621384	1958.399942	19.129152
47.359211	1961.679163	19.134170
47.533103	1953.307365	19.139187
47.473914	1945.852626	19.144205
47.330170	1930.445283	19.149223
47.559202	1939.186396	19.154240
47.485051	1958.014401	19.159258
48.002241	1959.312601	19.164275
47.473950	1943.940248	19.169293
47.635418	1946.499789	19.174311
47.642255	1953.438903	19.179328
47.449380	1968.851742	19.184346
47.822904	1955.594661	19.189363
48.087855	1966.791877	19.194381
47.842298	1948.828290	19.199399
48.160272	1956.106851	19.204416
48.168081	1956.178254	19.209434
48.175770	1959.058560	19.214451
48.215370	1955.710139	19.219469
48.298229	1955.769784	19.224487
48.373489	1957.964108	19.229504
48.380104	1962.993852	19.234522
47.991468	1954.779621	19.239539
47.965146	1956.955145	19.244557
48.128284	1961.527986	19.249575
48.222776	1969.580082	19.254592
48.051336	1971.024047	19.259610
48.332119	1968.543623	19.264627
48.335418	1969.284816	19.269645
48.035683	1968.467058	19.274663
48.415605	1980.526807	19.279680
48.331540	1977.434461	19.284698
48.433010	1972.813923	19.289715
48.648341	1989.261129	19.294733
48.742068	1981.286916	19.299751
48.897348	1982.736502	19.304768
48.971146	1981.004930	19.309786
48.877105	1976.238283	19.314803
48.660729	1982.555922	19.319821
48.726659	1978.575317	19.324839
48.766493	1998.524841	19.329856
48.564151	2007.604995	19.334874
48.905588	2013.563827	19.339891
48.871089	2007.686379	19.344909
49.180727	2010.014415	19.349927
49.440386	2007.821340	19.354944
49.357687	2012.486364	19.359962
49.624266	2015.506012	19.364979
49.415696	2025.906383	19.369997
49.593328	2032.326422	19.375015
49.525755	2028.578179	19.380032
49.600184	2038.003180	19.385050
49.410203	2028.138731	19.390067
49.540184	2038.224113	19.395085
49.243590	2022.985817	19.400103
49.686573	2027.114010	19.405120
49.635216	2038.250367	19.410138
49.694002	2030.789734	19.415155
49.878858	2044.385530	19.420173
49.614448	2053.204009	19.425191
50.181777	2061.286214	19.430208
50.105559	2060.269316	19.435226
50.606539	2058.458182	19.440243
50.341258	2059.594939	19.445261
50.488105	2054.361305	19.450279
50.476905	2058.623787	19.455296
50.766134	2053.386782	19.460314
51.025986	2053.166212	19.465331
50.843548	2050.695230	19.470349
50.751051	2034.702209	19.475367
50.660080	2028.290759	19.480384
50.585149	2027.481962	19.485402
50.660819	2018.582680	19.490419
50.457122	2028.227991	19.495437
50.449633	2034.058447	19.500455
50.692358	2042.396646	19.505472
50.599226	2044.588959	19.510490
50.809631	2040.276410	19.515507
51.078913	2044.747429	19.520525
50.706041	2039.251216	19.525543
50.854365	2047.335942	19.530560
50.711563	2057.015912	19.535578
50.919000	2056.071347	19.540595
51.294167	2066.519150	19.545613
51.398814	2075.674327	19.550631
51.265388	2072.810623	19.555648
51.431946	2072.904496	19.560666
51.253884	2068.532874	19.565683
51.301177	2065.858625	19.570701
51.090233	2071.796716	19.575719
51.212102	2074.769613	19.580736
51.367826	2087.325348	19.585754
51.422521	2089.330390	19.590771
51.457194	2097.978945	19.595789
51.591351	2098.002149	19.600807
51.768868	2091.595953	19.605824
51.724573	2098.669377	19.610842
51.851303	2096.203603	19.615859
51.466863	2101.850123	19.620877
51.973932	2105.640062	19.625895
51.925489	2119.083103	19.630912
52.052830	2119.464011	19.635930
52.271711	2139.953734	19.640947
52.282226	2133.971354	19.645965
52.481753	2117.588492	19.650983
52.468628	2114.137840	19.656000
52.102390	2123.628771	19.661018
52.799115	2117.661971	19.666035
52.542199	2121.546363	19.671053
52.227182	2123.874445	19.676071
52.387061	2122.770055	19.681088
52.713747	2117.135810	19.686106
52.683498	2117.958011	19.691123
53.060720	2125.801764	19.696141
52.754970	2119.442870	19.701159
52.754521	2106.484133	19.706176
52.854371	2116.883575	19.711194
52.671187	2121.040462	19.716211
52.998145	2123.854992	19.721229
52.807832	2131.992812	19.726247
53.202213	2138.704006	19.731264
52.886909	2144.816276	19.736282
53.050624	2149.957169	19.741299
53.286699	2146.552681	19.746317
53.192594	2146.621117	19.751335
53.147570	2142.092921	19.756352
53.109302	2144.178812	19.761370
52.907541	2148.660536	19.766387
53.411583	2157.226113	19.771405
53.567760	2162.885788	19.776423
53.642678	2169.195726	19.781440
53.589144	2167.982747	19.786458
53.896840	2169.288537	19.791475
54.136854	2164.002402	19.796493
53.936707	2169.964082	19.801511
54.134006	2158.255696	19.806528
54.632161	2155.264620	19.811546
54.171820	2156.400383	19.816563
54.469498	2151.193587	19.821581
54.219059	2154.111210	19.826599
54.534618	2142.046605	19.831616
54.602896	2156.497113	19.836634
54.330356	2139.383392	19.841651
54.725152	2132.425541	19.846669
54.520044	2122.187837	19.851687
54.454417	2111.546400	19.856704
54.515257	2114.752947	19.861722
54.613450	2114.766006	19.866739
54.807466	2125.469464	19.871757
54.851321	2139.093736	19.876775
54.748412	2134.928091	19.881792
54.851659	2133.397035	19.886810
54.682837	2141.370533	19.891827
55.065570	2140.556303	19.896845
54.721881	2144.122907	19.901863
54.697699	2143.943681	19.906880
55.172238	2141.297164	19.911898
54.907389	2141.556468	19.916915
55.126525	2145.912281	19.921933
54.740903	2147.058429	19.926951
55.047341	2141.247452	19.931968
54.807302	2154.837313	19.936986
54.971955	2161.745469	19.942003
55.563909	2164.717321	19.947021
55.299698	2175.691435	19.952039
55.336906	2170.493882	19.957056
55.468031	2174.658346	19.962074
55.201773	2180.519924	19.967091
55.105149	2183.268273	19.972109
55.327568	2191.335143	19.977127
55.567792	2187.775349	19.982144
55.688109	2201.779043	19.987162
55.471501	2211.114021	19.992179
55.928541	2203.215344	19.997197
55.912847	2199.121235	20.002215
55.499221	2198.889406	20.007232
55.589064	2208.110091	20.012250
55.697771	2216.216881	20.017267
56.107520	2223.250777	20.022285
56.052676	2230.010296	20.027303
56.150186	2229.250218	20.032320
56.438807	2232.528406	20.037338
56.748651	2229.759344	20.042355
57.149845	2210.015121	20.047373
56.789680	2215.481132	20.052391
56.961960	2203.713514	20.057408
57.153845	2203.907571	20.062426
57.079565	2208.643917	20.067443
57.038804	2203.509068	20.072461
56.725075	2198.536919	20.077479
57.120650	2200.308669	20.082496
57.021475	2202.804933	20.087514
56.741908	2206.588741	20.092531
57.063942	2196.997461	20.097549
57.089302	2209.930345	20.102567
57.113668	2201.723883	20.107584
57.356022	2194.550029	20.112602
57.308224	2200.920234	20.117619
57.717059	2199.940952	20.122637
57.805380	2199.147598	20.127655
57.463172	2192.033771	20.132672
57.495312	2192.476939	20.137690
57.518680	2189.907415	20.142707
57.691085	2188.810528	20.147725
57.990531	2203.843449	20.152743
58.007994	2202.594095	20.157760
57.767865	2189.164719	20.162778
57.691374	2195.750876	20.167795
58.288876	2201.562346	20.172813
58.196505	2206.292057	20.177831
58.362772	2206.338635	20.182848
58.336373	2202.028432	20.187866
57.910989	2196.183760	20.192883
58.219156	2198.057575	20.197901
58.131342	2201.811339	20.202919
58.271104	2205.835589	20.207936
58.469542	2210.270408	20.212954
58.174390	2216.101808	20.217971
58.709258	2215.929675	20.222989
58.524879	2213.471599	20.228007
58.598683	2211.093004	20.233024
58.330204	2215.178062	20.238042
58.017636	2215.801481	20.243059
58.502401	2225.051827	20.248077
58.787823	2231.521328	20.253095
58.255685	2227.422912	20.258112
58.598148	2247.637752	20.263130
58.700728	2253.012337	20.268147
59.262315	2250.579406	20.273165
59.047814	2270.894159	20.278183
59.318627	2265.688383	20.283200
59.552949	2260.665068	20.288218
59.178791	2263.703088	20.293235
59.373742	2272.759002	20.298253
59.711045	2269.253416	20.303271
59.240553	2258.123007	20.308288
59.156218	2266.051761	20.313306
58.899543	2272.006551	20.318323
59.541410	2259.325801	20.323341
59.269118	2263.326252	20.328359
59.688610	2273.158104	20.333376
59.764949	2283.697039	20.338394
59.371361	2301.183610	20.343411
59.597212	2284.411427	20.348429
59.634949	2296.143113	20.353447
59.725475	2292.654094	20.358464
59.909991	2311.019025	20.363482
60.104736	2316.634833	20.368499
60.439653	2308.909893	20.373517
60.264456	2320.201540	20.378535
59.945733	2319.424613	20.383552
60.097264	2309.976763	20.388570
60.057029	2313.852497	20.393587
60.332766	2324.281312	20.398605
60.359321	2329.042920	20.403623
60.841674	2340.345178	20.408640
60.451346	2339.317511	20.413658
61.042086	2341.753044	20.418675
61.038454	2343.082376	20.423693
60.645984	2342.698892	20.428711
60.908345	2341.767800	20.433728
60.792468	2335.268616	20.438746
61.121836	2338.644591	20.443763
61.474037	2332.327716	20.448781
61.146123	2340.294667	20.453799
60.975221	2341.924788	20.458816
61.285266	2350.331485	20.463834
61.261497	2354.463449	20.468851
61.653301	2355.872852	20.473869
61.599236	2356.146475	20.478887
61.488920	2360.149975	20.483904
61.730030	2356.331207	20.488922
61.881905	2368.038745	20.493939
61.601895	2356.420794	20.498957
61.850431	2358.518585	20.503975
61.791371	2362.359405	20.508992
62.156035	2355.743894	20.514010
61.966430	2359.876593	20.519027
62.171766	2354.163447	20.524045
62.049651	2355.855360	20.529063
61.763092	2355.196481	20.534080
62.281200	2355.803378	20.539098
62.153190	2379.993041	20.544115
62.691563	2370.478239	20.549133
62.853009	2383.598230	20.554151
62.485996	2383.040326	20.559168
62.942028	2380.402987	20.564186
62.765372	2385.186980	20.569203
62.760942	2376.120173	20.574221
62.828760	2377.154262	20.579239
62.834352	2372.239343	20.584256
63.183749	2372.178327	20.589274
62.840957	2374.564446	20.594291
62.664594	2372.127185	20.599309
63.043323	2382.347375	20.604327
62.764945	2381.810302	20.609344
63.116794	2377.273520	20.614362
62.944756	2384.597468	20.619379
63.300569	2380.056908	20.624397
63.099340	2390.948695	20.629415
63.004681	2403.676437	20.634432
63.544752	2402.547181	20.639450
63.081550	2407.009964	20.644467
63.317348	2406.537513	20.649485
63.755198	2403.653686	20.654503
63.310798	2421.041025	20.659520
63.758877	2408.406313	20.664538
63.544776	2425.555583	20.669555
63.996357	2424.973576	20.674573
64.090038	2427.382845	20.679591
64.002282	2430.158247	20.684608
64.262803	2417.928494	20.689626
63.937909	2424.342192	20.694643
63.991389	2423.431198	20.699661
63.963103	2428.674845	20.704679
64.173508	2435.310823	20.709696
64.467233	2423.265232	20.714714
64.252203	2449.122434	20.719731
64.517698	2447.073574	20.724749
64.878070	2449.478936	20.729767
64.816580	2457.107519	20.734784
65.138822	2452.266056	20.739802
64.859605	2451.258848	20.744819
65.046875	2448.707794	20.749837
65.248685	2449.840827	20.754855
65.119798	2452.439621	20.759872
65.421185	2451.196264	20.764890
65.402236	2455.750418	20.769907
64.824932	2443.879155	20.774925
64.822908	2443.062072	20.779943
65.014186	2447.270829	20.784960
65.063321	2443.273816	20.789978
65.174339	2452.122042	20.794995
65.039635	2461.217075	20.800013
65.440714	2466.361901	20.805031
65.264072	2472.184284	20.810048
65.689083	2469.933686	20.815066
65.384708	2474.488378	20.820083
65.530404	2492.992134	20.825101
65.977509	2493.663815	20.830119
65.732690	2500.083931	20.835136
65.875911	2502.769502	20.840154
65.910957	2502.754581	20.845171
65.925701	2507.372904	20.850189
66.116395	2495.621148	20.855207
66.181190	2506.771158	20.860224
66.626002	2507.960807	20.865242
66.450261	2516.904491	20.870259
66.433076	2519.858219	20.875277
66.643252	2518.392437	20.880295
66.320341	2526.614333	20.885312
66.680202	2513.131741	20.890330
66.379260	2514.671786	20.895347
66.286842	2518.420025	20.900365
66.740830	2523.313554	20.905383
66.840233	2540.833582	20.910400
67.239998	2527.414163	20.915418
67.151511	2542.142034	20.920435
67.239654	2534.645031	20.925453
67.225037	2533.533238	20.930471
67.346710	2540.773358	20.935488
67.460873	2538.410490	20.940506
67.117750	2536.946179	20.945523
67.318092	2529.882928	20.950541
67.256833	2528.055686	20.955559
67.409221	2545.595823	20.960576
67.589369	2553.442236	20.965594
67.425176	2562.412538	20.970611
67.657626	2560.940107	20.975629
68.001703	2562.328599	20.980647
67.571053	2570.400119	20.985664
67.876539	2556.468371	20.990682
67.971187	2559.303587	20.995699
67.705544	2573.749937	21.000717
68.239084	2575.216056	21.005735
68.035740	2576.838656	21.010752
68.111841	2576.296536	21.015770
68.279891	2580.717271	21.020787
68.118164	2579.830518	21.025805
68.245361	2577.307795	21.030823
68.190121	2589.350919	21.035840
68.521590	2600.112028	21.040858
68.547280	2605.322020	21.045875
68.515079	2616.894440	21.050893
68.866273	2605.338398	21.055911
68.726519	2599.903329	21.060928
68.967310	2615.797949	21.065946
69.523612	2628.919378	21.070963
69.516299	2623.905415	21.075981
69.598530	2621.598038	21.080999
69.176799	2608.610258	21.086016
69.222179	2605.702674	21.091034
69.534161	2615.829301	21.096051
69.644865	2617.601540	21.101069
69.368891	2625.939217	21.106087
69.213572	2624.868400	21.111104
69.597120	2623.122954	21.116122
69.811542	2622.164641	21.121139
69.466591	2620.495459	21.126157
69.938560	2627.772260	21.131175
70.005460	2644.136012	21.136192
69.967184	2640.020092	21.141210
70.387808	2635.431441	21.146227
70.302165	2640.185461	21.151245
70.497989	2638.952319	21.156263
70.207978	2635.750098	21.161280
70.631799	2632.903151	21.166298
70.620523	2632.175881	21.171315
70.726416	2634.791572	21.176333
70.924474	2626.093747	21.181351
70.765396	2630.183850	21.186368
70.724514	2626.784791	21.191386
70.998506	2625.744553	21.196403
70.908276	2620.828798	21.201421
71.094126	2620.061176	21.206439
71.006482	2626.889106	21.211456
71.222755	2627.798954	21.216474
71.515229	2628.554835	21.221491
71.362232	2629.475195	21.226509
71.687433	2617.238329	21.231527
71.165119	2621.685176	21.236544
71.523668	2633.758184	21.241562
71.650555	2646.634445	21.246579
71.493064	2640.697155	21.251597
71.543294	2641.793983	21.256615
71.611288	2643.550822	21.261632
71.758188	2640.384302	21.266650
72.067655	2643.772922	21.271667
72.084575	2651.960568	21.276685
72.176745	2642.625998	21.281703
71.664028	2646.291774	21.286720
72.065658	2657.426978	21.291738
72.214310	2663.820223	21.296755
72.268226	2668.037929	21.301773
72.279275	2656.920199	21.306791
72.219853	2666.830458	21.311808
72.384077	2666.918389	21.316826
72.224599	2669.878654	21.321843
72.354238	2668.472821	21.326861
72.515072	2679.409052	21.331879
72.814402	2692.794879	21.336896
72.791101	2699.843156	21.341914
73.125955	2692.073877	21.346931
72.887706	2698.827589	21.351949
73.098080	2695.909920	21.356967
73.026714	2699.516026	21.361984
73.332001	2694.566690	21.367002
73.155615	2702.645774	21.372019
73.038207	2716.324154	21.377037
73.194663	2713.320245	21.382055
73.293998	2711.925469	21.387072
73.219462	2731.294051	21.392090
73.496424	2724.963579	21.397107
73.421160	2729.084760	21.402125
73.755478	2739.520420	21.407143
73.710244	2749.106570	21.412160
73.330102	2749.712187	21.417178
73.727702	2755.637220	21.422195
73.853151	2757.047357	21.427213
73.940091	2748.108075	21.432231
74.309901	2761.653344	21.437248
74.505365	2772.069748	21.442266
74.494136	2782.808910	21.447283
74.404154	2784.031868	21.452301
74.842470	2772.985997	21.457319
74.545084	2772.313017	21.462336
74.256775	2765.051645	21.467354
74.709440	2764.706173	21.472371
74.556652	2776.123998	21.477389
74.671338	2785.142247	21.482407
74.673733	2791.760449	21.487424
74.999806	2788.925637	21.492442
75.525496	2788.575037	21.497459
75.255670	2798.947575	21.502477
75.353346	2793.806649	21.507495
75.422393	2795.171970	21.512512
75.313453	2782.277087	21.517530
75.712732	2794.489007	21.522547
75.718289	2812.128157	21.527565
75.750470	2816.563925	21.532583
76.025724	2819.011079	21.537600
76.116423	2813.262094	21.542618
76.188295	2808.551293	21.547635
75.498859	2820.021662	21.552653
75.935161	2809.796696	21.557671
75.998848	2810.320154	21.562688
76.242554	2812.907966	21.567706
76.139938	2808.347595	21.572723
76.375866	2813.000779	21.577741
76.236313	2818.931086	21.582759
76.704908	2830.418869	21.587776
76.999693	2827.854074	21.592794
77.018936	2827.544946	21.597811
76.792706	2833.378370	21.602829
77.016004	2839.523268	21.607847
77.192271	2839.517783	21.612864
77.039803	2837.228212	21.617882
77.142005	2828.176033	21.622899
76.665842	2829.371125	21.627917
77.281242	2836.549791	21.632935
77.218831	2825.241469	21.637952
77.257318	2829.912967	21.642970
77.282134	2821.882900	21.647987
77.303668	2829.195637	21.653005
77.649293	2844.654259	21.658023
77.470389	2857.120930	21.663040
77.363342	2857.996228	21.668058
77.603940	2854.167968	21.673075
77.382725	2862.389863	21.678093
77.538832	2859.449109	21.683111
77.533274	2869.767659	21.688128
77.796287	2877.216174	21.693146
77.771952	2884.403559	21.698163
77.629291	2893.976645	21.703181
77.993490	2897.129491	21.708199
78.294899	2907.444156	21.713216
78.235995	2921.883642	21.718234
78.103734	2909.159602	21.723251
78.583138	2915.955612	21.728269
78.601554	2933.144682	21.733287
78.664042	2923.221249	21.738304
78.576350	2940.417482	21.743322
78.721479	2938.662017	21.748339
78.730052	2935.924270	21.753357
79.029351	2930.331939	21.758375
78.572999	2942.220362	21.763392
79.036110	2955.265101	21.768410
79.622471	2956.293732	21.773427
79.206530	2956.523060	21.778445
79.311026	2959.372578	21.783463
79.318427	2969.042129	21.788480
79.467057	2981.915223	21.793498
79.688164	2982.385616	21.798515
79.656228	2986.572660	21.803533
79.695858	2991.313457	21.808551
80.033812	2985.077495	21.813568
79.966399	2983.557324	21.818586
80.149494	2984.889011	21.823603
80.568631	3006.232090	21.828621
80.415758	3008.601160	21.833639
80.735102	3014.746851	21.838656
80.924957	3017.766066	21.843674
80.974710	3002.690454	21.848691
80.497803	2996.146595	21.853709
80.993291	2992.843337	21.858727
81.204349	2998.639865	21.863744
80.824002	3006.905695	21.868762
81.228664	3009.231601	21.873779
81.156115	3003.419758	21.878797
80.916261	3003.299563	21.883815
81.354678	2999.146750	21.888832
81.157041	3003.675382	21.893850
81.117578	2998.076137	21.898867
81.280402	3007.831826	21.903885
81.384493	3003.570424	21.908903
81.636564	3012.141171	21.913920
81.502199	3012.398979	21.918938
81.812372	3021.686561	21.923955
81.627313	3019.045419	21.928973
81.475627	3025.034506	21.933991
81.718693	3024.848119	21.939008
81.835202	3044.789946	21.944026
82.059643	3047.377655	21.949043
82.174196	3054.316098	21.954061
82.359272	3052.118803	21.959079
82.577394	3042.505482	21.964096
82.334624	3051.210588	21.969114
82.619307	3044.241235	21.974131
82.237945	3053.031181	21.979149
82.311275	3066.181256	21.984167
82.769401	3068.871231	21.989184
82.644034	3073.401183	21.994202
82.806404	3076.573057	21.999219
82.490863	3074.069131	22.004237
82.793417	3093.887176	22.009255
83.176058	3094.865670	22.014272
83.088778	3111.020440	22.019290
83.278883	3104.334163	22.024307
83.413965	3101.907976	22.029325
82.909544	3103.697730	22.034343
83.538558	3115.166875	22.039360
83.220211	3132.405741	22.044378
83.530664	3127.648009	22.049395
83.745917	3134.267706	22.054413
83.549764	3131.969161	22.059431
83.792922	3135.885889	22.064448
83.654019	3154.851540	22.069466
83.738124	3160.585948	22.074483
84.176610	3166.801400	22.079501
84.037194	3166.236216	22.084519
84.492538	3171.928246	22.089536
84.635265	3180.339454	22.094554
84.518894	3174.584922	22.099571
84.785358	3176.648439	22.104589
84.854748	3172.196746	22.109607
85.371266	3167.971689	22.114624
85.143768	3169.683345	22.119642
85.427867	3162.177474	22.124659
85.801418	3161.216297	22.129677
85.454379	3168.590073	22.134695
85.318966	3162.586027	22.139712
85.424561	3172.240302	22.144730
85.659844	3162.359102	22.149747
85.956829	3163.344708	22.154765
85.523448	3166.733031	22.159783
85.771565	3157.310637	22.164800
85.878329	3166.125161	22.169818
86.002896	3168.031002	22.174835
86.378073	3171.314740	22.179853
86.286592	3184.304504	22.184871
86.117714	3184.842316	22.189888
86.500513	3184.233190	22.194906
86.342269	3181.275352	22.199923
86.317708	3183.772686	22.204941
86.231532	3184.010320	22.209959
86.580806	3175.714636	22.214976
86.374148	3181.999607	22.219994
86.636013	3192.409007	22.225011
86.976829	3199.532996	22.230029
86.538151	3209.869098	22.235047
87.121336	3206.160685	22.240064
86.889263	3206.525335	22.245082
87.238610	3201.297519	22.250099
87.305355	3204.064615	22.255117
86.892441	3225.617221	22.260135
87.433076	3219.639801	22.265152
87.648119	3231.397973	22.270170
87.590880	3238.221371	22.275187
87.998243	3239.028718	22.280205
87.729968	3234.273253	22.285223
87.860078	3229.591094	22.290240
87.515971	3240.729871	22.295258
87.965468	3237.575808	22.300275
88.414613	3255.041735	22.305293
88.395199	3256.667141	22.310311
88.479870	3254.422427	22.315328
88.454107	3252.898864	22.320346
88.488957	3253.284820	22.325363
88.750518	3247.177519	22.330381
88.047865	3252.441840	22.335399
88.632238	3257.715992	22.340416
88.626385	3272.478855	22.345434
88.657793	3280.178450	22.350451
88.952871	3278.348960	22.355469
89.127973	3283.264299	22.360487
88.920843	3280.206790	22.365504
89.022279	3277.410254	22.370522
89.342559	3282.141877	22.375539
89.231483	3288.705444	22.380557
89.152323	3307.030638	22.385575
89.354200	3296.513874	22.390592
89.362930	3305.883550	22.395610
89.140649	3311.284098	22.400627
90.010940	3320.793396	22.405645
89.933448	3332.783688	22.410663
89.927522	3327.993409	22.415680
90.026961	3318.483755	22.420698
89.676937	3322.818557	22.425715
90.345171	3332.129109	22.430733
90.206019	3346.445787	22.435751
90.414897	3339.062099	22.440768
90.493552	3346.921603	22.445786
90.619044	3354.477081	22.450803
90.487499	3355.078487	22.455821
90.648161	3377.096917	22.460839
90.905972	3370.999631	22.465856
91.333696	3374.786494	22.470874
90.995776	3368.615260	22.475891
91.133818	3366.917678	22.480909
91.065562	3371.785949	22.485927
91.780926	3383.216487	22.490944
91.744182	3391.447596	22.495962
91.598837	3391.378873	22.500979
91.926722	3396.327120	22.505997
92.068494	3409.230000	22.511015
92.204625	3392.511878	22.516032
92.125219	3402.119510	22.521050
92.370697	3399.063665	22.526067
92.339586	3390.246720	22.531085
92.547345	3386.818030	22.536103
92.655081	3385.986864	22.541120
92.543260	3388.254863	22.546138
91.834007	3392.557586	22.551155
92.613828	3390.506949	22.556173
92.750082	3408.877405	22.561191
92.713891	3419.642951	22.566208
92.905462	3417.539284	22.571226
92.330463	3407.103138	22.576243
92.800824	3412.568795	22.581261
92.992677	3424.248663	22.586279
93.250399	3435.896124	22.591296
93.273183	3446.068530	22.596314
93.013304	3445.919905	22.601331
93.234176	3437.896723	22.606349
93.053546	3457.857153	22.611367
93.316233	3462.143338	22.616384
93.285740	3464.297602	22.621402
93.471707	3480.255232	22.626419
94.018299	3487.242937	22.631437
93.698641	3500.644278	22.636455
94.099409	3493.467187	22.641472
94.420893	3491.952327	22.646490
94.214693	3496.447703	22.651507
94.651092	3508.382850	22.656525
94.351156	3514.250134	22.661543
94.673040	3511.507401	22.666560
94.884532	3510.255965	22.671578
95.051526	3511.694372	22.676595
95.346515	3520.984592	22.681613
95.162113	3513.362598	22.686631
95.064849	3513.283185	22.691648
95.242518	3508.577721	22.696666
95.189446	3506.417683	22.701683
95.660338	3502.269138	22.706701
95.509595	3521.770446	22.711719
95.734642	3523.392295	22.716736
95.583131	3528.153711	22.721754
95.485852	3537.527491	22.726771
95.806372	3522.311178	22.731789
95.662448	3532.029989	22.736807
95.236681	3538.349412	22.741824
95.363035	3551.040179	22.746842
95.268748	3561.710752	22.751859
95.881993	3570.105239	22.756877
96.325465	3587.177837	22.761895
96.656115	3587.040850	22.766912
96.983583	3581.061991	22.771930
96.478582	3591.437107	22.776947
96.836450	3580.766329	22.781965
96.480501	3597.569641	22.786983
97.001393	3612.070345	22.792000
97.009103	3609.774518	22.797018
96.789693	3616.269955	22.802035
97.209451	3613.956916	22.807053
97.514280	3631.199625	22.812071
98.470843	3623.291512	22.817088
98.413849	3609.485186	22.822106
98.172258	3595.448972	22.827123
98.486625	3586.767185	22.832141
98.348751	3587.379058	22.837159
98.529666	3590.964754	22.842176
98.503154	3585.798872	22.847194
98.642438	3592.335950	22.852211
98.616899	3579.440055	22.857229
98.451300	3580.892700	22.862247
98.642901	3583.880174	22.867264
98.757964	3583.391892	22.872282
98.732572	3589.048901	22.877299
99.064296	3579.490093	22.882317
99.144321	3596.824803	22.887335
99.107765	3609.174999	22.892352
99.610424	3604.690039	22.897370
99.029907	3613.599834	22.902387
99.375487	3603.956777	22.907405
99.602725	3607.629910	22.912423
99.403463	3608.090428	22.917440
99.629164	3606.912512	22.922458
99.628340	3606.480261	22.927475
99.921381	3616.253755	22.932493
99.487428	3619.866349	22.937511
99.650059	3625.970520	22.942528
99.811421	3633.113327	22.947546
99.765162	3634.458901	22.952563
100.090675	3637.753664	22.957581
100.403531	3646.877019	22.962599
100.685335	3653.426511	22.967616
100.537357	3651.543300	22.972634
100.631589	3659.097491	22.977651
100.760755	3651.180117	22.982669
100.437789	3650.618424	22.987687
100.667462	3662.488214	22.992704
100.949339	3676.603467	22.997722
100.910769	3666.853276	23.002739
101.373491	3669.220676	23.007757
101.419114	3665.198692	23.012775
101.378427	3681.741215	23.017792
101.440597	3695.594206	23.022810
101.748354	3700.570942	23.027827
101.958155	3691.365750	23.032845
101.910009	3696.912730	23.037863
101.863854	3695.692178	23.042880
102.341198	3684.882679	23.047898
102.019213	3693.490031	23.052915
101.741469	3693.284232	23.057933
102.371145	3712.975956	23.062951
102.068218	3719.017374	23.067968
102.523926	3720.426347	23.072986
102.592393	3719.118396	23.078003
102.414181	3718.161571	23.083021
102.458602	3725.111261	23.088039
102.654680	3738.854928	23.093056
102.772090	3731.965178	23.098074
102.627435	3747.633956	23.103091
102.860805	3752.758084	23.108109
102.989160	3774.734714	23.113127
103.123806	3770.209524	23.118144
103.287411	3793.648365	23.123162
103.677576	3792.296320	23.128179
103.717569	3799.963228	23.133197
104.240292	3797.135329	23.138215
103.804771	3802.793533	23.143232
104.115510	3793.032736	23.148250
104.064142	3809.946344	23.153267
104.305237	3811.190097	23.158285
104.271223	3815.456568	23.163303
104.151956	3822.536100	23.168320
104.455881	3812.268184	23.173338
104.702901	3833.143659	23.178355
104.785274	3840.005380	23.183373
105.099365	3839.605852	23.188391
104.923771	3840.476153	23.193408
105.087417	3835.993749	23.198426
104.892924	3848.106873	23.203443
104.869903	3845.806361	23.208461
105.317179	3863.449929	23.213479
105.315934	3867.070532	23.218496
105.439477	3864.194689	23.223514
105.572661	3882.086336	23.228531
105.904927	3886.459570	23.233549
105.867668	3891.218963	23.238567
106.060785	3888.404813	23.243584
106.544721	3892.274516	23.248602
106.366351	3892.056301	23.253619
106.494086	3908.638928	23.258637
106.786533	3922.405513	23.263655
106.376042	3925.537876	23.268672
106.846407	3927.424342	23.273690
107.085457	3918.842576	23.278707
107.512592	3920.237104	23.283725
107.312500	3924.482273	23.288743
107.444668	3916.138201	23.293760
107.474775	3919.807561	23.298778
107.019103	3916.066069	23.303795
107.178092	3930.109237	23.308813
107.515706	3943.067039	23.313831
107.868191	3931.424729	23.318848
107.880062	3943.079472	23.323866
108.025705	3938.199001	23.328883
107.984003	3934.922922	23.333901
108.103540	3943.704261	23.338919
108.301356	3958.483121	23.343936
108.418984	3964.442950	23.348954
108.362427	3964.963186	23.353971
108.809817	3962.263851	23.358989
108.816212	3962.812101	23.364007
108.367752	3964.129177	23.369024
108.943037	3958.575359	23.374042
109.032385	3978.049012	23.379059
108.976125	3980.330473	23.384077
109.011650	3985.583512	23.389095
108.752719	4000.203547	23.394112
109.236004	3985.898800	23.399130
109.464293	4001.843947	23.404147
109.223727	4009.286603	23.409165
109.375085	4011.611295	23.414183
109.607059	4019.115649	23.419200
109.790906	4021.356342	23.424218
109.712226	4031.639665	23.429235
109.777333	4027.204215	23.434253
109.745438	4036.012480	23.439271
109.690306	4053.169948	23.444288
110.431498	4055.275980	23.449306
110.270040	4059.347838	23.454323
110.474245	4061.995680	23.459341
110.720187	4080.545331	23.464359
110.502122	4092.457143	23.469376
110.681647	4091.778832	23.474394
110.814946	4098.739991	23.479411
110.912865	4105.141697	23.484429
111.393127	4111.028977	23.489447
111.341378	4119.063913	23.494464
111.760453	4112.183572	23.499482
111.897234	4120.962295	23.504499
111.808023	4130.676011	23.509517
112.260497	4136.457179	23.514535
112.340772	4139.168639	23.519552
112.321747	4134.228690	23.524570
112.437087	4133.418394	23.529587
112.396370	4135.025121	23.534605
112.909297	4120.137998	23.539623
112.559862	4128.566782	23.544640
112.665803	4129.206760	23.549658
113.157522	4146.455401	23.554675
113.026641	4146.554855	23.559693
113.512663	4150.569483	23.564711
113.458791	4157.926136	23.569728
113.374094	4162.677249	23.574746
113.429442	4154.203063	23.579763
113.490654	4161.844705	23.584781
113.922225	4153.968114	23.589799
113.474922	4161.515820	23.594816
113.421958	4178.619407	23.599834
113.751952	4180.925604	23.604851
113.706946	4180.613893	23.609869
113.937878	4191.925145	23.614887
114.153980	4208.481576	23.619904
114.417390	4219.948735	23.624922
114.290605	4222.777872	23.629939
114.134913	4228.161945	23.634957
114.532945	4235.106933	23.639975
114.682469	4242.179237	23.644992
114.598794	4245.528750	23.650010
114.777443	4251.535929	23.655027
115.404357	4249.209296	23.660045
115.742561	4240.883298	23.665063
115.685455	4249.136925	23.670080
115.684028	4254.834578	23.675098
115.956516	4249.006154	23.680115
115.911333	4249.262631	23.685133
116.104025	4237.253761	23.690151
116.189423	4255.850839	23.695168
116.361892	4270.794904	23.700186
116.457843	4275.353610	23.705203
116.306177	4277.823661	23.710221
116.609241	4263.534305	23.715239
116.718919	4268.911536	23.720256
116.835017	4283.081643	23.725274
116.675069	4269.988520	23.730291
116.383205	4269.065253	23.735309
116.412530	4274.944325	23.740327
116.743619	4297.129717	23.745344
116.355152	4295.151545	23.750362
117.231250	4310.641949	23.755379
117.295886	4317.219393	23.760397
117.593735	4315.291517	23.765415
117.498308	4320.937631	23.770432
117.540167	4340.513806	23.775450
117.957434	4350.340834	23.780467
117.856120	4351.912883	23.785485
117.934515	4349.179765	23.790503
117.965690	4368.063222	23.795520
118.256277	4372.092736	23.800538
118.702074	4377.338428	23.805555
118.055469	4387.231144	23.810573
118.187452	4385.910038	23.815591
118.247669	4406.468228	23.820608
118.694425	4418.790602	23.825626
118.968074	4422.642862	23.830643
119.129065	4424.350585	23.835661
119.257332	4417.184261	23.840679
119.663548	4444.408428	23.845696
119.731329	4445.341636	23.850714
120.016548	4444.690944	23.855731
119.553875	4452.964012	23.860749
120.054036	4447.368158	23.865767
120.124276	4453.663846	23.870784
120.393069	4471.515890	23.875802
120.503709	4471.334457	23.880819
120.457900	4474.981102	23.885837
120.712371	4475.001246	23.890855
120.559006	4483.860323	23.895872
120.578874	4485.735360	23.900890
121.168720	4495.898426	23.905907
121.036440	4508.636696	23.910925
121.604945	4508.579233	23.915943
121.016428	4509.583700	23.920960
121.234531	4512.945956	23.925978
121.584625	4513.844407	23.930995
121.498442	4527.986422	23.936013
121.577127	4525.319519	23.941031
121.720027	4537.509658	23.946048
121.999197	4550.890553	23.951066
122.242827	4559.744288	23.956083
121.993864	4567.245304	23.961101
122.192824	4562.630929	23.966119
122.464713	4571.726449	23.971136
122.560295	4580.243546	23.976154
122.701744	4585.701119	23.981171
122.768190	4590.589647	23.986189
123.065305	4585.647394	23.991207
123.139519	4601.131104	23.996224
123.018198	4615.938403	24.001242
123.360496	4603.950046	24.006259
123.428381	4599.965403	24.011277
123.294053	4611.656105	24.016295
123.738497	4630.124714	24.021312
123.399850	4637.500923	24.026330
123.920694	4640.465400	24.031347
123.861128	4652.990362	24.036365
124.028486	4653.967954	24.041383
124.325475	4663.416274	24.046400
124.625262	4669.414083	24.051418
124.301497	4666.513498	24.056435
124.672473	4680.063183	24.061453
124.902059	4686.810622	24.066471
124.922120	4695.156527	24.071488
124.503744	4702.201191	24.076506
125.057017	4691.076177	24.081523
125.047681	4703.596462	24.086541
125.371717	4708.646683	24.091559
125.303464	4722.268369	24.096576
125.633496	4722.396624	24.101594
125.715641	4738.084383	24.106611
125.599834	4742.717417	24.111629
125.840131	4745.823717	24.116647
126.021380	4744.510650	24.121664
126.401946	4760.520989	24.126682
126.777997	4761.143925	24.131699
126.015078	4768.002696	24.136717
126.538499	4765.398657	24.141735
126.774826	4774.733435	24.146752
126.873877	4796.665389	24.151770
127.256427	4791.362476	24.156787
127.005909	4792.534961	24.161805
126.963134	4789.685030	24.166823
127.141605	4808.921495	24.171840
127.645916	4823.766678	24.176858
127.957423	4814.901676	24.181875
128.140524	4822.098365	24.186893
127.891001	4823.848344	24.191911
127.908402	4837.084225	24.196928
127.998051	4831.770370	24.201946
128.419211	4831.717053	24.206963
127.871053	4851.559824	24.211981
128.359209	4848.812940	24.216999
128.654600	4855.474376	24.222016
128.540321	4866.900107	24.227034
129.038417	4879.404145	24.232051
128.968101	4885.797760	24.237069
129.121294	4885.338193	24.242087
129.314651	4901.797809	24.247104
128.740041	4911.139755	24.252122
129.516311	4907.492296	24.257139
129.664384	4929.056881	24.262157
129.808254	4944.675173	24.267175
130.134242	4942.840678	24.272192
129.897935	4944.500215	24.277210
130.327927	4952.920903	24.282227
130.763435	4967.234053	24.287245
130.866663	4967.536733	24.292263
130.818224	4969.798153	24.297280
130.815513	4966.070703	24.302298
131.024811	4958.790461	24.307315
131.115298	4973.650094	24.312333
131.573532	4986.425604	24.317351
131.811625	4983.029744	24.322368
131.633473	4990.040040	24.327386
132.245781	4990.045160	24.332403
132.070495	5001.818286	24.337421
132.111676	4991.486706	24.342439
131.872287	4986.025492	24.347456
131.818446	5001.018239	24.352474
132.100576	5004.869295	24.357491
132.327593	5020.629299	24.362509
132.469757	5018.457432	24.367527
132.628213	5026.115767	24.372544
132.387946	5043.186379	24.377562
132.905735	5033.888067	24.382579
132.737196	5043.946138	24.387597
132.786209	5056.719520	24.392615
133.315925	5057.627738	24.397632
133.005193	5071.900052	24.402650
133.257505	5077.340405	24.407667
133.349039	5086.682244	24.412685
133.423113	5102.242161	24.417703
133.611047	5098.282794	24.422720
133.744676	5114.682515	24.427738
134.376295	5124.062867	24.432755
134.177499	5128.014548	24.437773
134.323994	5128.967025	24.442791
134.662035	5139.239348	24.447808
134.600094	5149.012466	24.452826
134.919794	5147.346236	24.457843
135.033499	5154.329810	24.462861
135.029559	5158.200464	24.467879
135.614180	5162.837508	24.472896
135.463464	5168.088501	24.477914
135.532598	5174.681333	24.482931
135.717014	5169.835494	24.487949
135.696397	5180.069332	24.492967
136.219363	5189.353103	24.497984
136.186671	5198.247283	24.503002
136.108153	5203.903647	24.508019
136.349743	5206.163852	24.513037
136.335097	5216.665087	24.518055
136.728824	5216.890693	24.523072
136.518555	5225.793768	24.528090
136.680635	5220.853560	24.533107
137.074411	5241.975975	24.538125
137.252730	5240.972681	24.543143
137.337607	5243.926645	24.548160
137.361953	5247.129996	24.553178
137.378919	5271.736414	24.558195
137.513287	5273.811401	24.563213
137.666544	5280.309020	24.568231
137.976636	5289.727204	24.573248
138.123736	5299.114110	24.578266
138.200249	5294.805987	24.583283
138.255703	5305.839232	24.588301
138.591579	5322.813528	24.593319
138.878304	5316.635306	24.598336
138.718117	5333.542124	24.603354
138.819368	5328.595634	24.608371
139.171854	5340.412560	24.613389
139.346666	5345.356916	24.618407
139.883510	5337.185543	24.623424
139.665796	5337.194437	24.628442
139.944380	5334.878052	24.633459
140.012026	5348.090648	24.638477
139.902925	5363.284905	24.643495
140.816110	5358.798339	24.648512
140.769491	5364.913782	24.653530
140.786352	5359.955252	24.658547
140.861587	5359.703598	24.663565
140.774395	5359.568935	24.668583
141.238960	5362.940087	24.673600
140.825609	5368.005004	24.678618
141.455095	5370.558003	24.683635
141.607098	5381.497251	24.688653
141.205566	5393.766945	24.693671
141.809752	5388.015618	24.698688
141.601061	5392.035195	24.703706
141.742211	5398.118075	24.708723
141.996048	5409.316014	24.713741
141.969788	5415.627154	24.718759
141.853434	5420.263601	24.723776
141.933130	5432.082287	24.728794
142.482443	5440.759138	24.733811
142.584583	5434.682398	24.738829
142.690562	5440.205762	24.743847
142.977112	5447.885243	24.748864
142.905569	5457.363304	24.753882
143.115774	5463.290181	24.758899
143.123875	5468.140736	24.763917
143.222588	5478.343419	24.768935
143.507976	5480.423180	24.773952
143.675570	5503.023928	24.778970
143.796945	5496.821043	24.783987
144.017725	5512.232060	24.789005
144.057989	5520.660407	24.794023
144.484874	5529.148141	24.799040
144.331560	5531.227191	24.804058
144.121022	5540.865964	24.809075
144.492704	5546.227779	24.814093
144.471474	5562.184977	24.819111
144.603913	5561.488738	24.824128
144.934889	5568.148017	24.829146
144.933152	5589.247568	24.834163
145.025941	5601.875580	24.839181
145.499966	5612.909724	24.844199
145.419490	5620.331110	24.849216
145.371330	5633.382125	24.854234
145.652278	5638.994934	24.859251
146.056091	5660.858084	24.864269
146.204268	5662.962520	24.869287
146.265274	5670.393328	24.874304
146.248464	5683.938224	24.879322
146.510049	5689.718231	24.884339
146.900611	5699.101924	24.889357
146.830320	5718.927588	24.894375
146.913765	5725.180609	24.899392
147.342448	5735.868381	24.904410
147.222981	5738.156808	24.909427
147.534503	5740.033632	24.914445
147.308616	5761.512579	24.919463
147.831741	5762.829084	24.924480
147.895126	5772.788087	24.929498
147.523714	5784.343061	24.934515
148.520795	5795.933029	24.939533
148.038270	5808.215688	24.944551
148.735064	5816.509748	24.949568
148.532029	5822.271042	24.954586
148.891097	5834.241937	24.959603
149.031281	5853.621241	24.964621
148.853215	5868.567870	24.969639
149.412679	5867.050261	24.974656
149.475245	5877.148345	24.979674
149.427366	5881.281731	24.984691
149.774699	5885.877219	24.989709
149.743469	5907.909837	24.994727
150.088521	5911.713348	24.999744
150.372145	5925.697493	25.004762
150.483034	5935.333468	25.009779
151.050987	5938.912660	25.014797
151.144437	5949.365814	25.019815
151.058798	5940.332046	25.024832
151.020139	5952.160140	25.029850
150.883837	5962.406226	25.034867
151.281840	5963.780230	25.039885
151.413452	5981.671029	25.044903
151.763482	5986.449212	25.049920
151.629080	5992.038813	25.054938
151.776914	6001.905791	25.059955
152.031939	6011.396111	25.064973
151.989706	6021.160293	25.069991
152.532307	6021.040600	25.075008
152.892275	6032.509560	25.080026
152.697767	6046.057308	25.085043
153.190759	6041.049255	25.090061
152.928598	6052.157963	25.095079
152.777874	6050.972575	25.100096
153.359960	6068.928627	25.105114
153.496608	6074.179053	25.110131
153.665740	6073.587533	25.115149
153.494199	6080.616150	25.120167
153.933170	6090.895296	25.125184
154.350585	6088.803296	25.130202
154.075763	6097.811608	25.135219
154.610486	6106.175388	25.140237
154.281365	6117.098905	25.145255
154.527710	6125.747787	25.150272
154.812789	6132.550205	25.155290
154.536546	6158.750570	25.160307
154.685698	6154.847561	25.165325
154.917472	6164.149040	25.170343
154.966038	6177.185287	25.175360
155.377273	6185.745229	25.180378
155.683088	6213.631753	25.185395
156.100916	6206.652968	25.190413
156.124940	6213.720447	25.195431
156.018258	6229.413814	25.200448
156.398219	6230.474987	25.205466
156.400538	6241.321399	25.210483
157.089830	6244.973190	25.215501
157.025696	6262.547683	25.220519
156.786136	6263.791148	25.225536
156.913858	6273.831891	25.230554
156.423280	6280.111895	25.235571
157.254676	6289.830900	25.240589
157.455117	6307.818566	25.245607
157.674304	6317.665066	25.250624
157.913456	6338.352080	25.255642
158.010347	6346.216337	25.260659
158.356428	6349.063266	25.265677
158.366566	6362.051999	25.270695
158.521137	6368.524545	25.275712
158.253126	6373.967882	25.280730
158.468992	6401.811961	25.285747
159.027994	6406.630124	25.290765
159.305773	6424.618415	25.295783
159.374193	6435.653466	25.300800
159.843589	6438.023351	25.305818
159.856392	6434.971889	25.310835
160.316608	6446.491697	25.315853
160.035438	6457.467883	25.320871
160.490715	6462.157096	25.325888
160.852635	6459.900124	25.330906
160.465448	6468.894652	25.335923
160.753151	6479.677554	25.340941
160.822385	6483.303419	25.345959
160.672896	6496.345667	25.350976
161.090539	6510.751220	25.355994
160.885389	6520.503308	25.361011
161.627827	6527.366809	25.366029
161.651918	6537.944811	25.371047
161.751956	6539.517069	25.376064
161.914719	6547.393190	25.381082
161.920156	6566.999554	25.386099
162.104411	6569.382559	25.391117
162.196213	6575.861855	25.396135
162.367166	6589.851532	25.401152
162.730879	6595.798924	25.406170
162.673491	6620.229389	25.411187
163.281165	6619.417620	25.416205
163.893037	6614.715946	25.421223
163.861163	6610.610750	25.426240
164.199768	6611.722621	25.431258
164.291478	6601.461139	25.436275
164.470012	6592.796055	25.441293
164.634002	6602.720806	25.446311
164.750199	6597.474889	25.451328
164.775691	6603.535251	25.456346
165.012722	6625.056331	25.461363
165.309418	6623.437773	25.466381
165.044357	6632.387993	25.471399
165.223267	6625.329677	25.476416
165.365025	6623.590176	25.481434
165.121617	6631.867750	25.486451
165.917803	6641.169441	25.491469
165.938214	6650.109672	25.496487
165.830704	6659.739204	25.501504
166.228112	6666.435832	25.506522
166.244836	6678.464070	25.511539
166.052210	6682.437214	25.516557
166.189823	6691.346477	25.521575
166.601779	6702.798242	25.526592
166.625803	6713.082766	25.531610
166.302173	6733.763688	25.536627
166.636219	6738.001590	25.541645
166.620628	6757.459921	25.546663
166.970501	6781.889936	25.551680
167.114432	6796.161809	25.556698
167.452780	6815.792049	25.561715
167.586253	6825.914272	25.566733
167.793992	6841.325293	25.571751
168.297077	6860.554101	25.576768
168.624196	6858.302534	25.581786
168.492441	6885.567269	25.586803
168.880581	6884.458408	25.591821
168.988514	6895.102403	25.596839
169.273243	6903.505715	25.601856
170.037938	6900.626817	25.606874
169.742712	6910.765738	25.611891
170.257245	6901.110269	25.616909
170.376071	6905.394555	25.621927
170.377164	6919.335328	25.626944
171.186868	6920.285022	25.631962
171.187548	6919.628317	25.636979
171.097695	6921.359790	25.641997
171.195576	6919.330386	25.647015
171.324584	6920.819216	25.652032
171.423142	6915.080338	25.657050
171.299196	6926.082682	25.662067
171.813430	6935.671778	25.667085
171.937559	6940.921257	25.672103
172.015755	6953.625095	25.677120
172.053668	6948.558659	25.682138
172.406691	6963.495584	25.687156
172.456092	6969.732266	25.692173
172.872541	6967.296217	25.697191
172.565266	6983.097418	25.702208
173.143073	6982.738598	25.707226
172.960498	6996.591397	25.712244
173.286433	6995.864792	25.717261
173.292045	7012.980792	25.722279
173.506542	7026.244201	25.727296
173.958256	7019.913287	25.732314
173.811426	7037.043720	25.737332
173.967033	7049.183034	25.742349
173.927432	7054.530805	25.747367
173.741900	7063.582424	25.752384
174.403999	7072.684358	25.757402
174.385640	7081.608775	25.762420
174.411216	7100.789523	25.767437
174.841796	7113.378283	25.772455
174.997396	7131.531629	25.777472
175.133145	7137.325495	25.782490
175.393141	7149.792628	25.787508
175.297908	7174.706458	25.792525
175.345034	7175.854558	25.797543
175.468997	7191.294782	25.802560
176.061560	7199.362721	25.807578
175.558032	7220.305985	25.812596
175.820395	7239.181439	25.817613
176.342257	7248.965237	25.822631
176.810005	7260.070815	25.827648
176.890287	7271.821142	25.832666
177.334808	7272.821753	25.837684
177.747002	7280.845374	25.842701
178.207620	7280.078718	25.847719
178.095331	7295.824384	25.852736
178.229608	7289.142173	25.857754
178.246211	7294.774807	25.862772
178.460989	7319.700247	25.867789
178.965538	7327.059083	25.872807
178.922148	7322.627207	25.877824
179.419351	7329.898799	25.882842
179.456528	7343.875281	25.887860
179.114779	7350.403830	25.892877
179.780695	7346.122856	25.897895
179.735853	7364.307833	25.902912
179.731314	7363.374114	25.907930
179.933188	7378.117224	25.912948
180.384631	7373.216348	25.917965
180.563738	7390.213965	25.922983
180.331563	7400.627405	25.928000
180.938206	7406.489650	25.933018
180.808107	7425.928742	25.938036
180.834828	7428.036624	25.943053
181.465710	7437.917096	25.948071
181.439832	7454.167107	25.953088
181.674145	7448.599373	25.958106
181.792432	7461.903425	25.963124
181.800496	7491.470705	25.968141
181.923673	7484.281884	25.973159
182.595331	7505.173958	25.978176
182.895745	7503.030679	25.983194
183.309880	7508.910488	25.988212
183.278268	7511.561053	25.993229
183.718265	7523.782408	25.998247
183.729834	7528.557194	26.003264
183.826916	7529.422830	26.008282
183.585819	7533.675253	26.013300
183.954441	7550.453908	26.018317
184.786246	7555.952597	26.023335
184.340790	7563.334077	26.028352
184.692692	7555.275943	26.033370
184.535671	7565.564049	26.038388
185.074167	7578.764471	26.043405
185.233150	7578.815371	26.048423
185.225592	7588.634935	26.053440
185.378020	7598.580977	26.058458
185.478538	7604.576246	26.063476
185.633057	7618.695561	26.068493
185.812327	7632.807853	26.073511
185.821112	7640.152929	26.078528
186.005019	7647.347448	26.083546
185.952018	7664.921534	26.088564
186.195752	7675.017480	26.093581
186.456500	7692.438258	26.098599
186.400405	7700.131325	26.103616
186.932136	7707.160880	26.108634
186.889660	7720.610271	26.113652
187.105421	7744.446951	26.118669
187.385364	7751.121338	26.123687
187.402683	7765.606378	26.128704
187.824598	7780.372165	26.133722
188.255883	7789.254895	26.138740
187.979571	7801.361343	26.143757
188.805748	7800.796278	26.148775
188.787675	7819.861486	26.153792
189.216648	7813.874828	26.158810
189.684294	7810.249910	26.163828
189.985145	7816.681109	26.168845
190.287892	7831.105700	26.173863
190.284526	7838.755836	26.178880
190.450963	7841.902652	26.183898
190.707398	7840.536549	26.188916
190.607904	7849.104670	26.193933
190.829139	7843.576752	26.198951
190.523821	7859.050059	26.203968
190.660977	7866.981271	26.208986
191.030129	7876.514664	26.214004
191.480858	7887.446493	26.219021
191.367141	7889.964750	26.224039
191.427604	7918.653152	26.229056
191.351833	7924.556174	26.234074
191.974345	7947.817947	26.239092
192.015872	7950.100367	26.244109
192.397896	7961.961716	26.249127
192.405213	7976.312734	26.254144
192.711087	7992.205008	26.259162
192.875775	8003.570040	26.264180
192.741890	8024.996167	26.269197
193.154058	8030.137691	26.274215
193.180761	8045.786450	26.279232
193.483673	8070.175018	26.284250
193.855052	8071.408133	26.289268
194.200256	8084.067763	26.294285
194.846271	8094.410314	26.299303
194.814483	8100.407528	26.304320
194.962730	8117.874746	26.309338
195.182350	8123.084346	26.314356
195.097640	8129.077232	26.319373
195.784989	8140.107898	26.324391
195.360633	8156.878735	26.329408
195.355336	8159.389514	26.334426
195.753369	8170.743350	26.339444
196.023227	8185.186000	26.344461
196.089651	8194.242899	26.349479
196.345478	8213.177203	26.354496
196.381162	8229.932864	26.359514
196.754673	8236.984253	26.364532
196.763789	8258.236705	26.369549
197.395288	8264.632047	26.374567
197.380795	8278.892001	26.379584
197.292693	8285.239068	26.384602
197.858305	8301.706562	26.389620
197.783070	8315.960275	26.394637
198.325122	8334.123719	26.399655
198.406787	8347.841418	26.404672
198.592663	8362.051104	26.409690
198.717995	8372.642711	26.414708
199.056597	8378.168402	26.419725
199.177230	8385.518352	26.424743
199.535288	8405.699702	26.429760
199.768606	8403.023800	26.434778
200.154253	8416.242454	26.439796
199.973856	8426.544171	26.444813
200.174903	8430.986419	26.449831
200.208251	8441.702977	26.454848
200.321805	8453.139439	26.459866
201.122661	8460.253411	26.464884
200.903858	8484.800030	26.469901
201.215087	8485.723722	26.474919
201.560981	8495.529438	26.479936
201.304674	8509.587507	26.484954
201.984050	8517.752930	26.489972
201.806428	8534.501239	26.494989
202.086632	8546.053725	26.500007
202.528189	8550.313094	26.505024
202.580771	8562.204339	26.510042
202.796224	8574.480512	26.515060
202.864109	8592.191241	26.520077
203.015759	8596.865429	26.525095
203.532718	8604.819546	26.530112
203.576530	8625.463958	26.535130
203.852794	8630.544854	26.540148
204.045378	8655.349285	26.545165
204.362792	8656.770855	26.550183
204.569251	8672.038376	26.555200
204.686595	8686.401121	26.560218
204.909618	8694.685473	26.565236
204.872083	8719.245048	26.570253
205.401927	8721.580510	26.575271
205.893325	8740.172199	26.580288
205.316309	8750.226821	26.585306
205.822558	8756.042085	26.590324
206.255309	8781.146883	26.595341
206.361538	8771.885921	26.600359
206.364018	8800.625816	26.605376
206.444765	8805.901566	26.610394
206.713333	8813.739981	26.615412
206.848719	8839.807041	26.620429
207.006307	8856.395780	26.625447
207.321328	8867.756735	26.630464
207.425681	8889.247568	26.635482
208.214389	8893.717841	26.640500
208.418155	8914.381718	26.645517
208.431548	8908.226179	26.650535
208.700043	8922.644360	26.655552
208.769900	8940.487717	26.660570
209.106538	8949.976243	26.665588
209.223519	8968.071139	26.670605
209.612302	8970.769716	26.675623
209.749473	8987.484904	26.680640
209.815847	8998.152407	26.685658
210.234197	9006.649409	26.690676
210.339562	9027.833989	26.695693
210.752832	9034.705806	26.700711
210.992577	9043.631778	26.705728
211.247868	9051.036671	26.710746
211.272031	9057.199079	26.715764
211.236835	9085.007605	26.720781
211.846242	9084.466999	26.725799
211.992844	9093.038185	26.730816
211.942557	9109.242954	26.735834
212.343996	9116.855459	26.740852
212.409897	9141.756161	26.745869
212.526215	9128.609977	26.750887
212.794057	9155.275557	26.755904
212.885945	9164.632041	26.760922
213.139445	9178.838074	26.765940
213.256131	9192.383574	26.770957
213.664513	9203.474369	26.775975
214.068025	9221.092075	26.780992
213.798655	9223.527547	26.786010
214.293963	9243.985095	26.791028
214.443797	9257.238135	26.796045
214.543011	9259.015982	26.801063
214.797059	9272.344269	26.806080
214.907215	9293.168467	26.811098
215.190108	9302.166737	26.816116
215.416243	9312.607325	26.821133
215.375907	9328.624445	26.826151
215.938177	9348.667481	26.831168
215.708877	9354.961257	26.836186
216.072345	9378.101231	26.841204
216.210173	9398.011902	26.846221
216.370201	9412.523231	26.851239
216.590618	9433.333470	26.856256
217.083296	9451.136338	26.861274
216.859962	9461.350632	26.866292
217.694096	9480.265096	26.871309
217.345208	9500.293168	26.876327
218.298590	9504.437847	26.881344
218.563910	9513.448445	26.886362
219.146771	9525.118311	26.891380
219.269716	9536.225604	26.896397
219.600508	9530.657923	26.901415
219.553199	9543.045362	26.906432
219.713491	9558.320844	26.911450
219.951518	9561.491471	26.916468
220.215685	9576.453902	26.921485
220.154157	9588.565751	26.926503
220.622409	9592.878014	26.931520
220.624529	9604.556815	26.936538
221.477611	9591.607466	26.941556
221.991591	9603.262913	26.946573
221.944805	9607.747426	26.951591
222.481588	9624.157467	26.956608
222.223832	9624.772526	26.961626
221.959252	9625.104491	26.966644
222.115908	9638.871385	26.971661
222.236366	9657.957823	26.976679
222.890044	9667.308644	26.981696
222.952891	9682.896287	26.986714
223.222497	9683.776044	26.991732
223.197222	9705.026064	26.996749
223.554034	9719.222641	27.001767
223.751293	9728.932315	27.006784
223.856927	9746.808730	27.011802
224.201445	9756.021741	27.016820
224.526944	9776.699079	27.021837
224.187648	9797.663714	27.026855
224.483989	9810.224828	27.031872
224.449574	9833.254043	27.036890
224.809904	9848.132166	27.041908
225.019763	9870.147520	27.046925
224.896726	9895.552439	27.051943
225.437578	9914.772199	27.056960
225.582845	9934.177090	27.061978
225.956513	9960.745152	27.066996
226.205236	9974.040044	27.072013
226.224537	9997.215760	27.077031
226.796710	10010.807325	27.082048
226.629198	10036.007854	27.087066
227.423048	10034.639499	27.092084
227.607902	10060.381616	27.097101
227.924165	10068.898256	27.102119
228.447924	10098.748848	27.107136
228.454394	10112.441738	27.112154
228.533016	10116.199459	27.117172
228.878169	10122.229839	27.122189
228.800405	10133.804660	27.127207
229.266167	10146.140540	27.132224
229.581917	10159.974463	27.137242
229.906440	10170.409592	27.142260
230.451714	10187.671315	27.147277
230.304745	10189.355204	27.152295
230.715342	10201.017750	27.157312
230.705514	10226.519051	27.162330
231.149946	10225.375926	27.167348
231.623218	10231.490469	27.172365
231.435034	10251.952003	27.177383
232.032377	10257.024096	27.182400
231.779628	10268.601153	27.187418
232.180117	10274.338741	27.192436
232.542290	10289.204298	27.197453
232.577810	10297.304031	27.202471
233.170474	10316.885516	27.207488
233.284733	10334.240156	27.212506
233.347951	10332.806263	27.217524
233.866109	10351.600611	27.222541
233.717119	10355.390879	27.227559
234.030676	10368.912709	27.232576
234.071962	10382.625603	27.237594
234.332751	10391.312114	27.242612
235.192502	10407.580684	27.247629
235.023660	10413.353828	27.252647
235.454597	10432.149291	27.257664
235.415850	10442.407825	27.262682
235.535096	10464.580163	27.267700
235.932281	10465.585219	27.272717
236.201368	10487.257326	27.277735
236.209156	10501.957543	27.282752
236.170359	10522.389655	27.287770
236.192978	10535.076233	27.292788
236.745354	10552.100368	27.297805
236.778633	10576.900738	27.302823
237.099946	10592.063430	27.307840
237.327255	10621.857100	27.312858
237.302963	10641.996576	27.317876
237.524689	10666.881215	27.322893
237.954161	10681.973358	27.327911
238.644948	10697.583464	27.332928
238.782739	10719.317456	27.337946
239.350277	10733.895434	27.342964
239.315504	10743.278867	27.347981
239.865772	10763.467399	27.352999
240.044503	10776.404392	27.358016
240.384605	10786.578506	27.363034
240.735198	10791.844121	27.368052
240.867842	10808.230105	27.373069
240.937837	10823.681804	27.378087
241.325188	10837.517642	27.383104
241.659626	10853.237381	27.388122
241.553149	10857.504199	27.393140
242.253497	10875.878995	27.398157
242.485018	10888.258377	27.403175
242.725337	10899.117591	27.408192
242.341146	10912.935417	27.413210
242.767323	10927.567268	27.418228
243.254196	10941.472848	27.423245
243.483982	10961.825472	27.428263
243.647191	10964.237607	27.433280
243.828375	10971.847488	27.438298
243.555611	10985.275316	27.443316
243.718338	10999.579054	27.448333
244.134947	11035.068459	27.453351
245.124872	11040.549752	27.458368
244.709297	11052.831684	27.463386
244.876385	11070.633426	27.468404
245.443579	11086.578981	27.473421
245.397830	11100.122893	27.478439
245.971683	11105.325204	27.483456
246.047880	11131.736285	27.488474
246.327701	11144.187211	27.493492
246.676708	11158.004033	27.498509
247.043809	11173.358954	27.503527
247.196513	11185.855082	27.508544
247.490924	11200.419374	27.513562
247.678070	11202.758322	27.518580
248.051011	11223.796116	27.523597
248.269658	11236.004074	27.528615
248.519855	11247.054559	27.533632
248.356562	11252.852351	27.538650
248.502194	11276.707697	27.543668
249.294197	11294.860143	27.548685
249.309269	11303.569783	27.553703
249.586830	11319.690372	27.558720
249.864469	11327.727360	27.563738
249.855916	11359.895817	27.568756
250.313362	11381.466825	27.573773
250.209963	11392.212813	27.578791
250.434595	11405.746166	27.583808
251.609583	11418.173876	27.588826
251.482116	11445.334094	27.593844
251.910239	11455.472680	27.598861
251.530642	11473.783573	27.603879
251.896220	11483.628834	27.608896
252.590885	11502.516682	27.613914
252.711105	11525.763734	27.618932
253.102564	11532.933561	27.623949
253.544862	11538.305015	27.628967
253.470540	11567.196972	27.633984
253.547537	11579.155782	27.639002
253.923597	11597.408416	27.644020
254.412887	11597.963346	27.649037
254.103645	11633.090775	27.654055
254.671749	11638.054152	27.659072
254.885105	11655.501852	27.664090
254.870562	11683.576249	27.669108
255.196029	11694.138390	27.674125
255.261394	11731.506139	27.679143
255.602393	11739.511273	27.684160
255.870024	11760.079875	27.689178
256.010381	11785.926064	27.694196
256.327173	11799.909449	27.699213
256.443871	11826.990917	27.704231
256.836279	11853.284005	27.709248
257.148773	11879.081251	27.714266
256.964762	11895.650414	27.719284
257.488971	11923.906022	27.724301
257.875806	11945.059284	27.729319
258.266845	11967.879210	27.734336
258.737466	11989.076236	27.739354
258.376821	12009.753005	27.744372
259.166936	12019.547831	27.749389
259.231094	12050.973474	27.754407
259.257634	12073.187494	27.759424
259.835168	12090.616442	27.764442
260.385517	12115.906241	27.769460
260.605446	12123.223161	27.774477
260.419372	12155.057638	27.779495
260.964150	12162.342631	27.784512
261.374169	12191.156512	27.789530
261.490294	12221.105919	27.794548
261.788053	12220.661429	27.799565
261.969767	12243.966048	27.804583
262.154136	12266.891342	27.809600
262.641500	12272.840144	27.814618
262.875975	12293.509256	27.819636
263.076538	12298.410389	27.824653
263.255798	12322.552311	27.829671
263.696557	12339.409245	27.834688
264.267584	12354.875289	27.839706
264.359603	12366.380676	27.844724
264.878866	12383.777972	27.849741
264.805029	12390.471554	27.854759
264.928815	12403.389855	27.859776
265.477442	12418.221578	27.864794
265.559352	12436.442158	27.869812
265.446013	12446.902939	27.874829
265.900327	12469.884085	27.879847
266.329541	12491.624998	27.884864
266.586629	12504.374066	27.889882
266.739930	12529.641358	27.894900
267.179822	12531.315624	27.899917
267.276867	12561.278033	27.904935
267.501188	12585.549020	27.909952
268.175807	12599.843259	27.914970
268.361843	12623.520298	27.919988
268.424115	12640.076794	27.925005
268.675202	12665.047897	27.930023
268.978391	12673.700403	27.935040
269.402638	12694.027596	27.940058
269.743458	12719.376292	27.945076
269.896350	12727.676578	27.950093
269.686908	12746.640992	27.955111
269.927999	12771.673802	27.960128
270.104267	12785.951513	27.965146
270.359488	12817.879026	27.970164
270.504925	12844.947977	27.975181
270.703062	12876.151896	27.980199
271.034359	12896.114917	27.985216
271.420746	12916.290384	27.990234
271.840369	12950.807128	27.995252
272.499039	12974.738991	28.000269
272.734672	12999.763484	28.005287
272.725649	13013.151432	28.010304
273.092854	13039.118537	28.015322
273.233037	13071.768721	28.020340
273.561725	13094.173454	28.025357
273.965344	13118.480196	28.030375
273.860687	13150.581490	28.035392
274.374420	13164.301348	28.040410
274.200550	13201.712634	28.045428
274.975275	13215.840076	28.050445
275.332067	13245.276549	28.055463
275.610270	13267.266226	28.060480
275.940226	13281.141277	28.065498
276.083957	13313.775531	28.070516
276.664078	13324.418699	28.075533
276.592769	13353.486599	28.080551
277.068371	13369.315804	28.085568
277.724005	13381.993558	28.090586
277.722308	13412.026465	28.095604
278.113723	13427.104669	28.100621
278.041610	13445.347189	28.105639
279.240368	13451.308089	28.110656
279.873600	13452.424766	28.115674
280.068440	13461.947270	28.120692
280.348742	13477.611363	28.125709
280.772608	13484.817914	28.130727
280.632289	13489.201155	28.135744
280.916609	13492.971541	28.140762
280.951412	13512.384792	28.145780
281.534818	13515.631469	28.150797
281.741721	13531.471322	28.155815
281.264513	13547.888900	28.160832
281.918830	13553.366674	28.165850
282.118268	13569.561428	28.170868
282.847084	13583.393167	28.175885
282.763642	13605.853591	28.180903
282.893930	13614.151491	28.185920
283.482487	13629.186343	28.190938
283.708703	13642.847373	28.195956
283.704751	13654.668590	28.200973
284.160721	13669.496864	28.205991
284.023353	13689.196226	28.211008
284.653923	13704.887747	28.216026
284.758834	13729.213643	28.221044
284.833539	13743.855372	28.226061
285.336865	13767.945213	28.231079
285.572200	13796.814167	28.236096
285.643853	13807.054075	28.241114
285.442812	13838.767396	28.246132
286.048941	13867.549950	28.251149
286.666155	13874.167383	28.256167
286.751523	13907.572897	28.261184
286.843495	13926.481795	28.266202
287.042006	13957.188454	28.271220
287.361629	13985.551829	28.276237
287.547663	14000.267900	28.281255
287.744078	14043.313736	28.286272
288.024452	14070.218022	28.291290
288.374655	14107.738479	28.296308
288.901617	14127.021572	28.301325
289.033993	14157.735756	28.306343
289.311675	14183.595283	28.311360
289.750297	14222.428531	28.316378
289.860886	14247.411093	28.321396
290.149170	14269.005582	28.326413
290.901327	14302.244172	28.331431
290.731395	14337.541109	28.336448
291.554930	14354.725173	28.341466
291.750386	14373.116156	28.346484
292.245545	14399.213510	28.351501
292.665936	14420.500084	28.356519
292.484573	14436.423619	28.361536
292.817836	14469.254394	28.366554
293.176300	14495.202751	28.371572
293.491400	14512.482395	28.376589
294.080733	14550.042059	28.381607
293.957374	14580.297989	28.386624
294.548253	14593.975217	28.391642
294.858421	14612.976943	28.396660
294.886653	14645.754742	28.401677
295.715939	14670.767394	28.406695
295.505459	14691.966761	28.411712
296.116726	14718.687483	28.416730
296.327993	14739.337628	28.421748
296.253041	14768.174545	28.426765
296.579457	14791.990205	28.431783
296.752539	14822.553803	28.436800
297.077928	14841.348087	28.441818
297.133463	14879.762629	28.446836
297.163670	14903.659570	28.451853
297.349666	14928.119571	28.456871
298.272796	14957.981614	28.461888
298.935538	14990.891162	28.466906
299.194580	15015.902005	28.471924
299.572688	15036.674775	28.476941
299.989120	15063.982357	28.481959
299.936890	15079.747233	28.486976
300.466952	15097.397993	28.491994
300.651073	15118.324412	28.497012
300.898148	15140.046357	28.502029
301.078728	15171.272578	28.507047
301.408152	15203.880977	28.512064
301.824178	15215.716329	28.517082
301.909516	15234.618085	28.522100
302.456718	15260.234719	28.527117
303.021658	15275.031384	28.532135
302.665952	15314.395545	28.537152
302.941485	15326.587755	28.542170
303.345158	15359.061613	28.547188
303.471481	15394.399363	28.552205
303.815025	15410.566788	28.557223
304.174734	15443.287710	28.562240
304.430489	15474.028896	28.567258
304.623234	15513.948696	28.572276
304.740679	15546.249782	28.577293
305.669985	15573.266140	28.582311
305.391108	15611.822967	28.587328
305.460080	15634.302955	28.592346
305.777684	15660.553022	28.597364
306.006671	15714.819229	28.602381
306.636467	15750.217735	28.607399
306.941123	15791.004930	28.612416
307.217466	15820.240048	28.617434
307.483082	15856.567517	28.622452
307.833330	15890.001323	28.627469
308.380527	15922.737909	28.632487
308.660994	15958.952700	28.637504
309.010780	15988.385026	28.642522
309.085791	16025.803904	28.647540
309.283594	16059.691433	28.652557
309.968203	16088.825105	28.657575
310.407398	16122.324343	28.662592
310.838603	16152.293736	28.667610
311.173087	16191.112546	28.672628
311.464017	16213.056245	28.677645
312.010045	16243.007793	28.682663
312.141810	16274.764601	28.687680
312.356996	16299.619745	28.692698
313.078442	16330.570457	28.697716
313.110212	16362.497840	28.702733
313.366425	16378.414448	28.707751
313.501829	16412.972498	28.712768
314.161151	16442.325445	28.717786
314.752038	16475.409881	28.722804
314.439229	16510.411021	28.727821
314.959094	16523.882819	28.732839
315.265291	16566.332795	28.737856
315.640855	16586.254840	28.742874
315.924000	16616.494514	28.747892
315.930770	16655.757253	28.752909
316.596031	16677.968174	28.757927
316.691547	16706.329620	28.762944
317.564918	16722.911048	28.767962
317.901531	16759.854491	28.772980
318.010171	16781.053546	28.777997
318.275749	16805.266578	28.783015
318.714667	16824.566184	28.788032
318.960653	16857.092541	28.793050
319.482946	16882.456238	28.798068
319.259857	16919.389746	28.803085
319.819319	16941.386967	28.808103
320.218670	16981.293236	28.813120
320.311287	16992.731826	28.818138
320.619439	17017.352231	28.823156
321.212132	17036.147854	28.828173
321.757885	17062.417790	28.833191
322.194638	17074.484780	28.838208
322.224750	17100.298577	28.843226
322.695465	17120.345248	28.848244
323.101713	17130.174435	28.853261
323.330843	17159.330539	28.858279
323.832942	17173.863715	28.863296
324.300626	17195.262829	28.868314
324.429427	17224.605314	28.873332
324.640387	17244.648583	28.878349
325.219110	17259.460415	28.883367
325.317605	17283.374879	28.888384
325.219818	17314.768207	28.893402
325.561354	17328.814950	28.898420
326.110664	17359.146757	28.903437
326.258230	17397.273941	28.908455
326.242038	17419.639843	28.913472
326.213239	17452.639824	28.918490
327.043065	17480.495704	28.923508
326.803842	17516.447370	28.928525
327.495360	17545.828542	28.933543
327.800457	17580.444222	28.938560
328.449712	17610.950289	28.943578
328.566970	17647.730792	28.948596
328.597779	17675.156183	28.953613
329.430282	17711.616293	28.958631
329.805303	17753.909635	28.963648
329.807320	17782.097780	28.968666
330.053315	17813.993998	28.973684
330.412329	17857.642009	28.978701
330.976901	17884.282846	28.983719
331.644554	17919.398277	28.988736
332.141824	17938.272901	28.993754
332.141352	17967.150311	28.998772
332.383399	17998.371479	29.003789
332.949343	18029.567229	29.008807
333.156812	18054.899653	29.013824
333.163910	18085.791347	29.018842
333.788037	18112.985430	29.023860
333.971626	18151.127404	29.028877
334.370306	18184.503895	29.033895
334.696382	18212.566091	29.038912
334.983078	18242.409740	29.043930
335.526361	18289.567711	29.048948
335.638994	18323.602056	29.053965
336.038400	18346.529368	29.058983
336.870873	18368.535989	29.064000
337.277043	18397.451422	29.069018
337.828160	18419.521127	29.074036
337.923056	18449.148749	29.079053
338.245255	18473.825663	29.084071
338.211638	18504.452738	29.089088
338.565935	18536.339495	29.094106
339.460476	18555.386245	29.099124
339.403210	18588.278893	29.104141
340.017136	18612.329056	29.109159
340.094633	18632.798998	29.114176
340.177124	18669.441571	29.119194
340.768491	18690.153283	29.124212
340.785025	18728.549995	29.129229
340.970266	18753.539333	29.134247
341.326190	18795.263015	29.139264
341.340183	18832.308325	29.144282
341.458920	18861.433733	29.149300
341.890815	18912.470834	29.154317
342.854023	18950.966088	29.159335
342.886298	18985.544873	29.164352
343.091029	19022.807062	29.169370
343.471552	19055.227576	29.174388
343.800711	19087.018086	29.179405
344.062551	19112.994109	29.184423
344.616907	19147.282910	29.189440
344.602075	19181.724109	29.194458
345.207717	19210.369422	29.199476
345.295012	19258.852111	29.204493
345.626653	19288.045892	29.209511
346.475156	19337.477269	29.214528
347.062640	19362.991948	29.219546
347.902302	19377.581307	29.224564
347.788630	19419.708415	29.229581
348.037368	19446.596723	29.234599
348.677950	19473.790131	29.239616
348.879888	19503.143547	29.244634
349.217216	19530.839433	29.249652
348.933719	19575.729178	29.254669
349.339446	19609.018551	29.259687
349.526175	19647.346179	29.264704
349.895597	19690.415402	29.269722
350.559100	19707.376604	29.274740
351.059626	19760.584902	29.279757
351.185962	19798.543201	29.284775
351.765072	19831.401435	29.289792
351.904942	19868.669075	29.294810
352.811369	19895.164343	29.299828
353.098476	19930.677871	29.304845
353.759169	19950.065891	29.309863
353.894887	19987.062726	29.314880
354.023573	20022.468554	29.319898
354.584384	20047.767170	29.324916
354.955501	20089.396459	29.329933
354.809952	20124.289426	29.334951
355.162772	20157.265790	29.339968
355.490542	20190.163996	29.344986
355.796155	20230.489654	29.350004
356.304158	20267.915208	29.355021
356.438649	20300.294186	29.360039
356.981860	20346.225071	29.365056
357.559418	20395.518331	29.370074
358.247275	20419.799236	29.375092
357.840903	20461.222549	29.380109
358.329672	20498.740011	29.385127
358.999821	20532.065351	29.390144
359.050103	20568.166823	29.395162
359.655368	20600.662103	29.400180
360.097015	20641.504356	29.405197
360.403923	20682.260387	29.410215
360.819141	20705.838784	29.415232
361.008985	20748.685722	29.420250
361.505511	20791.080334	29.425268
361.872958	20836.003675	29.430285
362.265337	20857.443883	29.435303
362.603925	20904.330615	29.440320
362.767236	20928.188838	29.445338
363.619676	20963.040696	29.450356
363.538186	21000.193511	29.455373
363.858211	21037.030761	29.460391
364.413857	21069.288167	29.465408
364.522231	21116.382064	29.470426
365.172272	21136.139400	29.475444
365.708694	21186.477323	29.480461
366.111790	21213.950450	29.485479
367.174354	21239.494252	29.490496
366.935719	21266.884736	29.495514
367.209789	21294.845761	29.500532
367.691104	21328.878118	29.505549
367.651873	21363.649206	29.510567
368.166647	21387.813093	29.515584
368.224041	21416.560144	29.520602
368.976671	21452.060364	29.525620
369.105508	21478.610070	29.530637
369.383680	21512.314401	29.535655
369.853485	21542.355545	29.540672
369.574566	21587.040633	29.545690
370.785197	21617.597716	29.550708
371.295731	21645.970824	29.555725
371.427806	21671.837863	29.560743
372.134586	21708.558917	29.565760
372.520704	21740.420622	29.570778
373.085409	21768.766466	29.575796
373.391978	21802.308875	29.580813
373.353824	21826.130234	29.585831
374.247391	21856.035971	29.590848
374.331958	21886.630844	29.595866
374.607782	21909.606957	29.600884
374.965389	21953.675028	29.605901
375.381986	21980.995456	29.610919
375.825502	22011.957657	29.615936
375.719427	22051.517441	29.620954
376.185825	22082.615182	29.625972
376.623335	22119.372859	29.630989
376.981846	22155.207787	29.636007
377.946476	22174.923208	29.641024
378.556996	22200.463240	29.646042
379.406041	22220.588581	29.651060
379.808288	22253.680766	29.656077
379.939914	22276.168062	29.661095
380.553044	22290.283251	29.666112
380.648944	22325.028540	29.671130
380.920190	22341.522675	29.676148
381.240897	22363.544448	29.681165
381.342972	22393.233755	29.686183
381.875694	22416.751558	29.691200
382.231898	22450.786486	29.696218
382.330736	22478.157374	29.701236
383.059189	22507.862479	29.706253
383.220219	22546.187124	29.711271
383.413480	22570.453370	29.716288
383.344720	22610.014739	29.721306
384.033183	22653.861927	29.726324
384.308220	22690.879915	29.731341
384.703346	22727.297811	29.736359
385.114823	22757.609016	29.741376
385.393286	22799.574481	29.746394
385.751299	22840.086827	29.751412
386.039205	22887.832949	29.756429
386.421055	22919.709855	29.761447
386.808024	22956.363254	29.766464
386.499680	23006.231488	29.771482
387.462851	23046.548357	29.776500
387.695647	23086.341479	29.781517
387.715100	23139.292997	29.786535
388.267846	23177.494308	29.791552
388.781668	23236.491930	29.796570
388.901619	23279.127792	29.801588
389.932487	23320.489920	29.806605
389.778017	23368.673001	29.811623
390.430789	23405.020182	29.816640
390.943253	23451.304329	29.821658
391.203008	23487.378300	29.826676
391.950748	23528.342860	29.831693
391.924244	23577.119369	29.836711
392.578381	23616.544223	29.841728
392.813501	23663.283058	29.846746
393.431741	23704.154516	29.851764
393.921003	23730.581259	29.856781
394.318699	23776.486017	29.861799
394.278890	23809.618433	29.866816
394.602928	23855.484355	29.871834
395.289557	23889.785953	29.876852
396.093836	23934.388785	29.881869
396.300804	23973.953901	29.886887
396.443470	24000.340499	29.891904
396.618126	24053.478668	29.896922
397.113249	24090.294152	29.901940
397.716733	24124.457510	29.906957
397.830244	24171.406164	29.911975
398.288965	24208.530904	29.916992
398.483205	24260.687031	29.922010
398.997770	24306.460947	29.927028
399.603017	24343.544026	29.932045
400.205577	24393.728039	29.937063
400.450132	24438.565018	29.942080
400.559950	24481.963376	29.947098
401.264970	24509.343209	29.952116
401.807208	24549.766968	29.957133
402.096725	24594.344467	29.962151
402.912105	24625.814928	29.967168
403.519596	24680.959800	29.972186
403.793146	24722.298104	29.977204
404.260381	24751.864200	29.982221
404.465636	24789.939750	29.987239
405.471209	24817.715306	29.992256
405.789022	24864.273356	29.997274
405.686494	24887.489115	30.002292
406.500973	24920.578028	30.007309
406.971405	24966.929138	30.012327
407.330428	24991.779052	30.017344
407.441388	25021.963808	30.022362
407.820201	25069.656655	30.027380
408.212045	25103.943308	30.032397
408.449185	25147.759225	30.037415
409.111224	25180.720769	30.042432
409.231573	25215.726358	30.047450
409.397695	25265.153014	30.052468
409.940705	25307.512045	30.057485
410.290547	25357.384138	30.062503
410.787696	25409.957148	30.067520
411.057604	25450.450654	30.072538
411.756721	25484.569748	30.077556
412.363694	25513.994998	30.082573
412.777983	25572.913965	30.087591
412.904655	25602.142819	30.092608
413.427952	25635.468116	30.097626
414.202097	25677.431484	30.102644
414.694926	25712.923109	30.107661
414.957729	25760.345041	30.112679
415.015417	25794.761050	30.117696
415.616962	25841.927876	30.122714
415.727782	25879.697955	30.127732
416.568411	25916.563786	30.132749
416.353852	25962.398794	30.137767
416.556927	26016.232895	30.142784
416.970533	26058.304087	30.147802
417.828742	26111.719822	30.152820
418.547682	26155.152772	30.157837
418.594458	26200.239531	30.162855
419.026023	26239.868720	30.167872
419.316331	26284.424550	30.172890
419.843817	26335.794388	30.177908
420.429922	26367.107561	30.182925
420.477865	26413.509208	30.187943
420.927410	26457.301013	30.192960
421.289392	26494.950736	30.197978
421.795120	26539.435462	30.202996
422.412544	26576.343779	30.208013
422.479014	26618.299862	30.213031
422.711088	26674.431741	30.218048
423.519934	26720.866594	30.223066
423.515147	26764.180360	30.228084
424.129496	26812.181719	30.233101
424.725204	26853.277992	30.238119
425.472522	26900.721505	30.243136
426.034575	26942.202450	30.248154
425.951145	26993.492673	30.253172
426.463689	27032.952718	30.258189
426.844905	27078.279778	30.263207
427.286339	27121.164149	30.268224
427.979892	27168.035230	30.273242
428.511742	27217.592654	30.278260
429.454499	27251.335264	30.283277
429.564297	27297.602830	30.288295
430.284414	27327.619762	30.293312
430.885721	27369.999259	30.298330
431.043598	27410.002266	30.303348
431.624281	27443.005524	30.308365
431.405885	27480.179131	30.313383
431.780144	27522.923177	30.318400
432.257650	27564.911636	30.323418
432.200091	27622.165988	30.328436
432.820884	27665.706033	30.333453
433.482453	27720.591574	30.338471
433.858310	27762.507873	30.343488
434.682797	27808.866914	30.348506
434.574216	27855.530226	30.353524
435.476038	27898.047049	30.358541
435.720932	27946.380740	30.363559
436.579968	27988.449366	30.368576
436.760442	28042.481988	30.373594
436.969032	28084.475713	30.378612
437.444581	28118.179168	30.383629
437.769647	28173.946649	30.388647
438.402481	28220.475701	30.393664
439.310374	28265.261489	30.398682
439.431224	28312.395567	30.403700
440.008746	28363.573061	30.408717
440.171238	28409.379792	30.413735
440.907992	28454.477237	30.418752
441.328040	28494.074693	30.423770
441.694161	28541.979948	30.428788
442.424097	28588.709537	30.433805
442.275374	28630.046089	30.438823
442.639070	28675.082356	30.443840
442.823418	28728.673717	30.448858
443.695215	28785.191587	30.453876
443.881459	28828.985480	30.458893
444.156996	28886.001560	30.463911
444.696293	28937.711114	30.468928
444.924969	28996.194985	30.473946
446.225268	29044.062547	30.478964
447.017069	29071.801576	30.483981
447.401286	29113.573948	30.488999
448.046891	29155.223290	30.494016
448.461657	29195.120015	30.499034
449.211582	29240.545822	30.504052
449.270215	29266.661658	30.509069
449.814576	29302.265247	30.514087
450.081065	29343.493949	30.519104
450.179101	29384.780725	30.524122
451.027523	29424.180135	30.529140
451.339962	29454.618031	30.534157
451.762423	29492.440796	30.539175
452.275105	29526.621157	30.544192
452.716433	29567.481581	30.549210
452.796563	29607.678045	30.554228
453.261441	29645.639835	30.559245
453.577126	29685.041013	30.564263
453.727018	29733.760421	30.569280
454.486880	29773.515717	30.574298
454.440036	29826.924906	30.579316
455.209218	29879.372012	30.584333
455.485797	29933.053202	30.589351
455.840997	29986.551541	30.594368
456.448087	30037.058514	30.599386
456.820463	30100.839233	30.604404
457.287997	30139.945677	30.609421
457.420199	30188.005186	30.614439
457.923622	30244.597406	30.619456
458.696830	30295.888128	30.624474
458.904510	30350.055296	30.629492
459.025058	30400.399150	30.634509
459.920643	30473.435808	30.639527
460.293247	30528.620648	30.644544
460.923385	30579.839662	30.649562
461.172569	30643.268380	30.654580
461.672637	30690.285282	30.659597
462.234461	30753.260791	30.664615
462.560186	30807.802600	30.669632
462.909238	30866.759671	30.674650
463.705673	30922.277433	30.679668
464.511225	30978.021494	30.684685
464.761138	31029.705756	30.689703
465.332457	31081.864500	30.694720
466.004206	31137.870169	30.699738
466.340925	31189.749847	30.704756
466.897794	31239.919928	30.709773
467.713893	31296.914886	30.714791
467.377262	31342.389067	30.719808
468.804973	31386.373230	30.724826
469.061103	31439.796010	30.729844
469.329333	31490.049835	30.734861
469.886587	31550.626212	30.739879
469.889699	31610.979791	30.744896
470.436189	31647.168688	30.749914
470.666963	31706.677696	30.754932
471.350051	31766.223500	30.759949
471.872963	31834.556653	30.764967
472.331805	31878.251081	30.769984
472.868029	31934.128396	30.775002
473.044574	31994.809946	30.780020
473.485073	32051.164067	30.785037
473.878608	32113.898210	30.790055
474.333003	32175.080452	30.795072
474.906316	32233.184409	30.800090
475.231466	32303.516206	30.805108
475.882341	32360.571562	30.810125
476.306560	32423.320794	30.815143
476.541505	32480.081266	30.820160
477.282287	32531.148667	30.825178
477.604743	32589.710163	30.830196
478.652900	32647.911595	30.835213
479.231054	32698.935336	30.840231
479.604953	32760.195117	30.845248
480.036546	32811.646703	30.850266
480.289481	32873.210257	30.855284
480.758463	32927.570793	30.860301
481.625157	32982.640486	30.865319
481.888793	33039.973300	30.870336
482.535839	33084.993726	30.875354
482.767366	33136.591245	30.880372
483.122831	33187.954522	30.885389
483.830118	33231.385261	30.890407
484.495430	33293.536653	30.895424
484.904057	33334.719390	30.900442
485.175612	33382.663272	30.905460
485.726545	33442.677108	30.910477
486.478850	33490.514326	30.915495
486.847926	33555.444148	30.920512
487.230050	33605.008714	30.925530
487.512045	33652.679713	30.930548
488.302939	33714.774746	30.935565
488.621148	33764.273828	30.940583
488.905409	33823.299959	30.945600
489.424995	33884.224074	30.950618
489.585411	33942.435369	30.955636
489.873044	34012.747150	30.960653
490.524657	34070.578384	30.965671
490.794763	34136.031296	30.970688
491.459561	34203.553298	30.975706
491.662204	34270.882353	30.980724
492.586077	34327.154225	30.985741
493.686118	34390.777157	30.990759
493.820182	34454.058411	30.995776
494.605615	34510.390391	31.000794
494.817540	34574.184590	31.005812
494.985329	34641.697318	31.010829
495.727281	34704.738689	31.015847
496.353817	34775.853492	31.020864
496.904556	34835.036715	31.025882
497.187584	34899.130570	31.030900
498.079644	34959.424072	31.035917
498.218725	35009.674923	31.040935
498.994695	35084.112123	31.045952
499.641337	35146.373058	31.050970
499.922315	35209.854856	31.055988
500.112067	35273.370101	31.061005
500.753206	35344.927127	31.066023
500.808023	35418.631179	31.071040
501.505512	35471.065593	31.076058
502.147315	35547.744785	31.081076
502.591087	35613.149764	31.086093
503.052828	35676.528766	31.091111
503.210895	35751.912366	31.096128
504.266320	35807.889353	31.101146
505.088572	35875.233940	31.106164
505.510203	35939.865652	31.111181
506.104716	35996.547634	31.116199
506.753870	36064.564887	31.121216
507.624245	36127.116130	31.126234
507.958161	36176.605735	31.131252
508.396898	36229.360762	31.136269
509.067542	36291.330422	31.141287
509.487682	36352.953781	31.146304
510.224901	36407.123159	31.151322
510.655063	36464.160932	31.156340
510.901490	36520.803976	31.161357
511.906537	36575.462987	31.166375
512.278038	36634.363121	31.171392
512.755148	36692.810568	31.176410
513.464688	36734.110859	31.181428
513.968367	36788.362045	31.186445
514.571464	36843.811881	31.191463
514.849998	36908.367760	31.196480
515.149599	36947.532136	31.201498
515.698576	37004.344068	31.206516
515.545383	37059.242633	31.211533
516.714821	37118.278382	31.216551
517.293836	37166.106764	31.221568
517.796895	37218.613864	31.226586
517.869252	37259.401591	31.231604
518.653523	37326.421554	31.236621
519.042278	37374.020936	31.241639
519.414905	37431.987204	31.246656
519.300460	37490.086827	31.251674
519.688498	37559.300610	31.256692
520.274147	37626.074380	31.261709
521.149009	37685.360182	31.266727
521.236111	37764.056570	31.271744
522.205994	37825.623351	31.276762
522.579839	37891.899933	31.281780
522.658608	37962.364945	31.286797
523.359739	38029.577184	31.291815
523.725792	38109.723536	31.296832
524.367421	38178.754144	31.301850
525.176167	38254.835093	31.306868
525.619862	38329.525338	31.311885
526.453050	38408.676362	31.316903
527.326688	38455.013312	31.321920
528.187699	38499.569016	31.326938
528.446142	38567.004035	31.331956
529.136899	38626.675398	31.336973
529.794697	38687.876145	31.341991
530.189303	38750.009959	31.347008
530.501253	38810.462083	31.352026
531.208980	38869.695107	31.357044
531.322697	38942.396514	31.362061
532.016508	39004.996438	31.367079
532.252439	39083.124128	31.372096
532.963102	39138.645234	31.377114
533.249561	39214.457214	31.382132
533.605183	39288.462590	31.387149
534.240420	39366.484490	31.392167
534.824978	39433.390496	31.397184
535.526441	39512.053930	31.402202
536.083172	39578.812962	31.407220
536.704879	39640.123235	31.412237
537.114986	39711.212399	31.417255
537.754959	39776.352655	31.422272
538.290003	39853.443364	31.427290
539.671746	39897.294287	31.432308
540.603415	39957.779028	31.437325
541.374290	40006.709367	31.442343
541.942944	40062.539668	31.447360
543.036455	40109.332690	31.452378
543.357055	40155.108489	31.457396
543.966683	40202.843929	31.462413
544.885775	40243.017683	31.467431
544.841830	40279.876594	31.472448
545.217263	40331.051499	31.477466
545.955134	40382.916036	31.482484
546.286164	40435.748805	31.487501
546.451645	40481.796234	31.492519
546.774749	40548.335526	31.497536
547.255264	40602.732719	31.502554
547.547328	40666.526096	31.507572
547.728204	40738.457715	31.512589
548.526235	40805.694994	31.517607
549.056105	40872.588683	31.522624
549.540721	40922.660053	31.527642
550.125933	40986.642458	31.532660
550.064455	41071.445662	31.537677
550.671559	41135.437721	31.542695
551.144058	41205.459440	31.547712
551.447337	41285.475525	31.552730
552.184828	41349.745047	31.557748
552.542809	41420.828957	31.562765
553.393785	41482.684039	31.567783
554.152646	41550.600156	31.572800
554.293920	41619.745336	31.577818
555.025161	41691.385162	31.582836
555.109239	41762.437178	31.587853
555.927584	41832.046214	31.592871
556.646708	41913.764074	31.597888
557.453236	41968.379235	31.602906
558.228720	42036.142451	31.607924
559.125686	42100.958429	31.612941
559.539136	42152.156925	31.617959
560.034453	42225.106741	31.622976
560.608406	42296.646671	31.627994
561.395375	42359.500933	31.633012
561.329123	42424.652143	31.638029
562.264103	42485.605066	31.643047
562.816278	42563.360412	31.648064
563.416156	42627.294689	31.653082
563.964573	42694.968990	31.658100
564.091909	42763.240752	31.663117
564.419997	42829.324428	31.668135
565.291994	42915.373714	31.673152
565.509270	42987.110891	31.678170
566.048365	43063.136954	31.683188
566.780919	43136.969768	31.688205
567.185480	43208.988265	31.693223
567.924070	43293.086449	31.698240
568.060957	43376.184921	31.703258
568.896582	43453.430928	31.708276
569.098890	43531.497474	31.713293
569.857794	43611.482245	31.718311
570.693690	43701.512527	31.723328
571.283770	43775.648093	31.728346
572.376714	43854.411230	31.733364
572.934070	43919.722173	31.738381
574.102181	43989.441349	31.743399
574.950834	44049.703647	31.748416
575.485554	44107.054962	31.753434
576.199620	44176.289196	31.758452
576.609756	44244.072103	31.763469
577.374783	44302.855366	31.768487
577.553586	44362.255615	31.773504
578.530829	44427.306192	31.778522
579.463733	44489.150519	31.783540
579.610500	44557.234972	31.788557
580.016304	44610.078657	31.793575
580.613143	44679.775603	31.798592
580.869391	44739.740355	31.803610
581.610239	44804.405237	31.808628
581.980328	44875.871533	31.813645
583.235443	44936.161125	31.818663
583.887139	44986.772176	31.823680
584.702110	45048.788338	31.828698
585.194097	45111.791465	31.833716
585.508723	45177.397128	31.838733
586.425878	45223.146914	31.843751
586.678778	45288.534841	31.848768
587.126335	45344.650476	31.853786
587.895824	45411.773362	31.858804
588.270983	45480.855957	31.863821
588.824668	45539.865344	31.868839
589.273974	45604.945094	31.873856
590.008191	45667.481684	31.878874
590.295637	45738.938366	31.883892
590.499641	45800.786604	31.888909
591.459614	45862.295208	31.893927
591.797862	45923.192843	31.898944
591.878028	45989.659969	31.903962
592.527270	46056.835241	31.908980
592.914548	46133.907681	31.913997
593.819471	46201.619010	31.919015
594.325284	46280.824241	31.924032
594.996662	46350.552651	31.929050
595.491399	46417.563413	31.934068
595.891284	46496.918839	31.939085
596.803413	46573.866298	31.944103
597.200808	46648.332537	31.949120
597.681197	46726.442558	31.954138
598.878409	46778.642317	31.959156
599.152502	46863.952710	31.964173
600.175368	46944.920221	31.969191
600.533170	47006.684408	31.974208
600.814942	47080.936104	31.979226
601.633077	47154.382842	31.984244
602.095619	47232.566992	31.989261
602.547655	47315.447208	31.994279
603.426955	47390.264276	31.999296
603.880314	47476.086634	32.004314
604.575811	47545.321485	32.009332
605.345633	47627.387573	32.014349
605.932101	47705.111088	32.019367
606.604250	47783.264304	32.024384
607.249027	47849.167641	32.029402
607.895890	47934.955098	32.034420
608.099017	48027.373002	32.039437
608.598323	48102.498659	32.044455
609.327414	48171.578315	32.049472
609.914484	48264.443175	32.054490
610.888237	48344.120079	32.059508
611.413003	48432.332649	32.064525
612.355314	48501.038269	32.069543
613.380169	48570.876301	32.074560
614.180978	48649.455203	32.079578
615.176747	48713.490297	32.084596
615.099436	48778.408551	32.089613
615.474858	48850.949445	32.094631
616.272735	48918.660329	32.099648
616.794141	49001.599072	32.104666
617.405942	49072.110698	32.109684
617.677267	49153.570713	32.114701
618.426177	49233.336541	32.119719
619.284526	49300.387413	32.124736
619.837576	49388.346156	32.129754
620.379472	49457.383086	32.134772
620.772658	49540.805722	32.139789
621.534353	49616.502638	32.144807
622.043917	49694.808055	32.149824
622.686485	49780.704327	32.154842
623.489902	49849.853326	32.159860
623.815347	49925.746120	32.164877
624.201737	50011.177205	32.169895
624.980393	50092.497818	32.174912
625.538244	50183.774255	32.179930
626.453972	50256.829714	32.184948
626.865009	50346.237964	32.189965
627.496190	50429.601233	32.194983
628.262344	50501.592610	32.200000
628.772826	50595.282438	32.205018
629.435462	50685.759866	32.210036
630.326754	50760.908748	32.215053
630.668159	50834.543179	32.220071
631.296343	50920.920490	32.225088
631.696988	51005.365946	32.230106
632.343657	51083.559684	32.235124
632.948537	51165.442782	32.240141
633.703865	51246.676191	32.245159
634.365790	51313.270131	32.250176
634.620545	51401.726170	32.255194
635.263784	51486.369498	32.260212
636.004046	51566.397831	32.265229
636.397041	51654.997698	32.270247
637.558026	51732.904263	32.275264
637.876579	51817.909695	32.280282
638.707638	51903.645108	32.285300
639.353454	51983.594752	32.290317
639.731133	52069.768781	32.295335
640.677841	52141.142164	32.300352
641.253436	52236.979815	32.305370
642.063899	52319.265055	32.310388
642.594388	52401.372961	32.315405
643.228622	52496.354574	32.320423
643.939273	52566.083035	32.325440
644.423595	52664.075523	32.330458
645.422903	52743.700309	32.335476
645.698929	52827.450502	32.340493
646.384663	52912.237881	32.345511
647.232302	53000.974137	32.350528
647.977840	53090.308888	32.355546
648.452798	53173.117937	32.360564
649.299094	53262.412250	32.365581
649.638698	53351.324311	32.370599
650.435361	53440.665043	32.375616
650.755692	53529.897197	32.380634
651.343184	53623.485861	32.385652
652.234111	53724.924846	32.390669
652.808663	53817.769592	32.395687
653.536977	53902.079260	32.400704
654.095870	53997.040765	32.405722
654.667160	54088.260744	32.410740
655.130015	54180.706747	32.415757
655.526961	54283.402541	32.420775
656.491086	54382.826833	32.425792
657.098400	54482.345391	32.430810
657.986434	54581.466018	32.435828
658.600592	54671.175387	32.440845
658.949207	54784.202469	32.445863
659.883267	54878.925232	32.450880
660.316823	54982.314445	32.455898
661.216911	55077.979931	32.460916
661.874564	55173.943238	32.465933
662.298743	55271.177555	32.470951
663.430423	55364.637247	32.475968
664.206379	55466.304205	32.480986
665.383752	55549.593792	32.486004
666.122469	55638.546859	32.491021
666.540839	55721.215463	32.496039
667.796250	55812.138737	32.501056
668.529865	55893.271333	32.506074
669.211004	55970.672162	32.511092
669.873243	56051.506367	32.516109
670.640063	56132.406741	32.521127
671.495633	56206.369823	32.526144
671.978356	56299.124725	32.531162
672.337645	56376.684860	32.536180
673.458096	56455.777867	32.541197
673.877649	56533.968285	32.546215
674.745113	56618.974623	32.551232
675.408513	56695.810975	32.556250
675.866621	56782.394604	32.561268
676.186116	56861.367556	32.566285
676.632861	56942.757487	32.571303
677.446838	57015.754921	32.576320
677.934894	57111.195610	32.581338
678.523510	57194.127437	32.586356
679.107877	57264.079350	32.591373
679.213349	57372.840333	32.596391
680.490935	57455.677822	32.601408
680.742021	57543.885211	32.606426
681.600399	57624.358551	32.611444
682.417139	57713.788108	32.616461
682.801114	57810.760534	32.621479
683.335050	57900.830015	32.626496
684.137621	57990.686872	32.631514
684.685098	58085.476526	32.636532
685.548026	58178.369001	32.641549
686.652226	58274.660860	32.646567
687.843793	58349.615918	32.651584
688.515994	58436.874508	32.656602
689.657007	58506.407389	32.661620
690.772884	58578.102726	32.666637
691.494175	58655.284367	32.671655
692.668390	58736.218297	32.676672
692.900265	58814.331559	32.681690
693.650704	58877.489625	32.686708
694.202037	58954.312734	32.691725
694.647255	59030.684321	32.696743
695.148830	59113.794593	32.701760
695.865984	59191.978650	32.706778
696.397409	59280.275041	32.711796
697.228275	59367.366543	32.716813
697.118206	59446.630400	32.721831
697.951843	59541.507510	32.726848
698.324520	59631.501055	32.731866
698.629606	59735.937190	32.736884
699.901200	59830.170836	32.741901
700.290689	59931.663934	32.746919
700.701086	60019.273017	32.751936
701.567523	60133.661938	32.756954
702.165346	60240.016613	32.761972
703.035642	60344.980823	32.766989
703.345033	60450.280185	32.772007
704.212337	60550.498342	32.777024
704.910374	60666.561889	32.782042
705.653869	60769.060108	32.787060
706.189211	60878.801196	32.792077
706.659951	61002.592847	32.797095
707.937685	61095.399808	32.802112
708.695404	61202.132394	32.807130
709.178486	61311.567088	32.812148
709.988020	61422.964121	32.817165
710.359624	61527.188550	32.822183
711.241735	61633.099589	32.827200
712.133148	61736.312961	32.832218
712.712007	61857.464931	32.837236
713.753395	61967.125273	32.842253
713.759401	62078.499162	32.847271
714.639682	62188.533879	32.852288
715.669961	62302.818574	32.857306
716.152961	62405.579600	32.862324
717.143068	62503.108697	32.867341
717.959673	62619.776888	32.872359
719.011496	62722.810981	32.877376
719.936928	62826.390723	32.882394
720.528900	62935.980118	32.887412
721.349147	63029.923162	32.892429
722.036152	63132.522298	32.897447
722.527651	63234.221876	32.902464
723.547449	63335.611235	32.907482
724.093024	63437.030954	32.912500
724.555159	63534.729064	32.917517
725.193540	63639.199105	32.922535
725.769096	63729.656907	32.927552
726.535379	63831.018335	32.932570
727.050300	63932.742404	32.937588
727.575576	64036.965922	32.942605
728.206866	64153.062530	32.947623
729.130486	64262.510830	32.952640
729.924119	64366.358154	32.957658
730.824744	64480.128652	32.962676
731.668048	64581.772267	32.967693
731.628521	64690.537574	32.972711
732.947710	64801.350733	32.977728
734.112309	64887.871225	32.982746
735.179425	64988.873657	32.987764
736.165257	65090.864203	32.992781
736.443937	65192.389772	32.997799
737.058978	65292.482894	33.002816
737.861370	65399.941825	33.007834
738.468937	65502.531410	33.012852
739.217927	65605.498129	33.017869
739.729725	65732.022827	33.022887
740.476095	65837.232142	33.027904
741.374076	65948.230247	33.032922
741.567598	66061.073925	33.037940
742.866829	66167.679553	33.042957
743.937596	66276.955242	33.047975
744.393762	66383.263263	33.052992
745.213290	66485.310780	33.058010
745.943416	66600.276139	33.063028
746.800603	66711.258631	33.068045
747.203370	66831.974601	33.073063
748.168816	66941.776148	33.078080
749.306024	67044.592917	33.083098
749.792812	67164.898412	33.088116
750.626096	67278.597016	33.093133
751.203510	67389.145058	33.098151
752.023327	67503.144352	33.103168
752.362479	67610.140614	33.108186
753.085914	67723.934372	33.113204
754.118180	67839.845723	33.118221
754.691841	67958.355782	33.123239
755.138152	68078.842850	33.128256
756.060834	68204.631595	33.133274
757.112392	68328.843137	33.138292
757.667864	68442.058511	33.143309
758.208812	68562.406378	33.148327
759.011978	68692.578897	33.153344
759.876754	68806.564251	33.158362
760.513417	68937.080671	33.163380
761.515658	69061.980980	33.168397
761.781366	69183.951509	33.173415
762.796658	69298.668970	33.178432
763.992835	69419.557751	33.183450
764.542946	69534.083147	33.188468
765.723098	69653.519132	33.193485
766.611268	69773.223016	33.198503
767.766822	69893.309838	33.203520
768.613877	69993.391270	33.208538
768.942597	70096.391115	33.213556
770.097971	70210.419436	33.218573
770.868010	70329.156529	33.223591
771.069576	70442.322048	33.228608
772.278001	70530.228812	33.233626
772.795764	70664.369294	33.238644
773.668764	70754.305050	33.243661
774.409338	70888.158488	33.248679
775.187071	70988.963819	33.253696
776.116190	71105.957082	33.258714
776.555148	71212.895543	33.263732
777.320993	71306.548178	33.268749
777.986855	71411.463487	33.273767
778.418440	71524.990270	33.278784
779.405196	71638.937217	33.283802
779.720953	71758.879119	33.288820
780.761412	71862.585017	33.293837
781.460824	71983.392436	33.298855
782.469146	72098.946504	33.303872
783.194944	72215.140601	33.308890
783.735697	72330.452259	33.313908
784.726483	72444.136067	33.318925
785.656163	72558.817859	33.323943
786.546611	72674.164912	33.328960
787.301931	72789.812274	33.333978
787.808030	72920.292944	33.338996
788.761654	73029.248026	33.344013
789.692889	73152.468996	33.349031
790.391896	73259.970302	33.354048
791.603745	73370.089620	33.359066
792.335478	73492.545436	33.364084
793.630995	73604.729875	33.369101
794.658029	73711.801648	33.374119
795.037544	73822.939810	33.379136
796.213982	73928.279099	33.384154
796.999524	74044.180493	33.389172
797.388387	74142.652077	33.394189
798.346985	74272.283168	33.399207
798.758732	74385.609927	33.404224
799.827215	74497.972992	33.409242
800.233039	74620.573662	33.414260
801.146438	74721.549239	33.419277
802.221936	74844.844072	33.424295
802.552415	74962.087363	33.429312
803.782505	75074.579531	33.434330
805.409116	75178.219196	33.439348
806.862198	75257.920432	33.444365
808.027358	75364.901162	33.449383
808.885097	75456.894595	33.454400
809.804733	75551.500749	33.459418
810.354483	75638.666176	33.464436
811.029765	75734.881965	33.469453
811.938870	75830.364782	33.474471
812.478760	75935.114896	33.479488
813.078292	76031.938965	33.484506
813.619482	76136.246294	33.489524
814.440123	76235.848634	33.494541
815.077782	76340.268313	33.499559
815.256149	76457.389879	33.504576
815.913335	76572.207468	33.509594
816.755030	76692.925123	33.514612
817.645520	76811.938194	33.519629
818.409903	76930.794182	33.524647
818.768896	77056.858832	33.529664
819.702437	77177.931614	33.534682
820.063778	77310.913743	33.539700
820.853625	77440.776422	33.544717
821.590322	77570.318669	33.549735
822.262367	77703.621421	33.554752
823.334651	77836.608784	33.559770
824.037868	77980.675978	33.564788
824.461499	78105.189787	33.569805
825.503123	78234.598735	33.574823
826.365707	78379.415830	33.579840
827.037358	78520.425019	33.584858
827.865558	78654.480697	33.589876
827.908665	78796.210473	33.594893
829.296599	78923.579441	33.599911
830.226060	79061.953933	33.604928
831.242433	79186.037734	33.609946
831.820998	79332.665254	33.614964
832.486716	79453.333880	33.619981
833.767101	79591.199976	33.624999
834.470249	79720.871569	33.630016
835.294559	79849.878668	33.635034
836.403828	79985.163668	33.640052
837.436287	80119.283110	33.645069
838.368186	80249.858867	33.650087
838.654681	80381.689207	33.655104
839.970919	80514.157097	33.660122
840.737841	80653.502477	33.665140
841.547952	80786.456330	33.670157
842.676499	80910.352858	33.675175
843.171245	81053.125625	33.680192
844.042341	81175.505264	33.685210
844.822707	81319.387602	33.690228
846.077868	81455.847813	33.695245
847.375749	81586.866601	33.700263
847.634283	81721.330268	33.705280
848.307774	81847.646117	33.710298
849.164873	81990.759658	33.715316
849.808298	82124.328744	33.720333
850.892750	82262.555390	33.725351
851.344687	82413.590041	33.730368
852.504038	82549.969168	33.735386
853.430574	82691.859020	33.740404
854.640091	82828.991854	33.745421
855.449547	82962.095413	33.750439
856.445322	83108.740617	33.755456
856.958225	83249.253564	33.760474
857.925707	83394.878345	33.765492
858.528110	83540.028860	33.770509
859.375460	83682.100753	33.775527
860.252902	83828.071277	33.780544
860.573079	83979.920438	33.785562
861.931995	84137.449102	33.790580
862.772018	84292.056826	33.795597
863.889170	84436.003539	33.800615
864.071929	84585.317832	33.805632
864.896045	84736.496524	33.810650
865.784930	84896.624528	33.815668
866.796486	85041.072305	33.820685
867.901782	85193.299101	33.825703
868.420357	85350.066291	33.830720
869.636052	85502.999707	33.835738
871.070393	85650.020019	33.840756
871.864938	85808.799289	33.845773
872.823583	85955.920978	33.850791
873.564057	86098.566373	33.855808
874.535018	86246.878761	33.860826
875.713468	86383.209690	33.865844
876.323346	86529.451151	33.870861
877.771386	86664.233199	33.875879
878.203189	86817.410303	33.880896
879.176631	86954.789772	33.885914
879.898287	87089.966307	33.890932
880.884182	87239.878099	33.895949
881.702808	87374.242397	33.900967
882.636309	87520.146653	33.905984
884.082193	87651.600701	33.911002
884.680944	87800.372070	33.916020
885.948479	87941.892068	33.921037
886.979392	88072.804681	33.926055
887.639775	88209.301235	33.931072
888.337783	88341.090892	33.936090
889.279528	88486.922593	33.941108
889.880767	88609.680125	33.946125
890.958364	88735.874007	33.951143
891.417820	88869.084720	33.956160
892.280411	89003.791704	33.961178
893.065631	89141.844465	33.966196
893.892322	89279.118303	33.971213
895.225960	89407.708208	33.976231
896.129877	89555.718203	33.981248
896.811295	89698.821125	33.986266
897.910708	89821.036720	33.991284
899.356970	89951.550374	33.996301
900.619132	90070.902631	34.001319
901.222487	90202.842067	34.006336
902.155318	90321.904698	34.011354
903.969195	90435.164679	34.016372
905.878119	90538.169775	34.021389
906.885391	90646.905568	34.026407
907.822324	90759.112739	34.031424
908.779194	90859.847294	34.036442
909.485802	90955.678520	34.041460
910.063114	91066.637723	34.046477
911.018666	91167.449554	34.051495
911.638916	91290.189734	34.056512
912.168654	91408.128400	34.061530
913.126116	91529.232477	34.066548
913.493159	91648.655087	34.071565
914.407146	91776.281528	34.076583
915.042796	91909.541482	34.081600
915.108982	92045.654210	34.086618
916.001742	92184.350462	34.091636
916.691419	92327.008251	34.096653
917.751938	92470.470514	34.101671
918.332068	92629.623857	34.106688
919.392614	92788.538033	34.111706
919.919059	92948.816815	34.116724
920.502716	93110.823933	34.121741
921.826503	93252.195303	34.126759
922.820162	93412.859648	34.131776
923.129264	93574.646020	34.136794
924.059807	93735.081100	34.141812
925.357884	93908.996572	34.146829
926.114304	94068.814213	34.151847
926.327454	94240.974785	34.156864
927.262986	94415.989248	34.161882
928.404261	94586.498041	34.166900
929.440282	94768.343511	34.171917
930.174670	94940.857313	34.176935
931.241806	95122.446466	34.181952
931.844987	95296.250345	34.186970
933.101372	95462.030521	34.191988
934.093166	95646.347141	34.197005
935.385445	95822.112217	34.202023
936.707741	96000.243998	34.207040
937.394890	96160.171929	34.212058
938.879033	96318.809675	34.217076
939.138444	96491.850048	34.222093
940.381792	96657.993512	34.227111
941.507467	96828.897240	34.232128
943.118763	96993.159457	34.237146
944.006584	97149.334103	34.242164
945.153728	97309.183151	34.247181
946.031295	97459.643797	34.252199
947.127375	97619.679875	34.257216
947.790194	97779.733888	34.262234
948.658897	97928.588191	34.267252
949.411355	98094.816037	34.272269
950.400023	98253.731195	34.277287
951.159733	98412.784407	34.282304
951.847281	98568.591700	34.287322
953.049067	98723.812149	34.292340
953.846287	98882.735047	34.297357
954.527435	99037.594828	34.302375
955.419417	99194.171812	34.307392
955.894731	99368.740613	34.312410
957.271845	99518.435457	34.317428
958.636108	99692.993600	34.322445
959.434287	99852.631066	34.327463
960.839734	100015.419712	34.332480
961.196842	100174.291097	34.337498
962.528299	100331.907737	34.342516
963.065693	100504.558592	34.347533
964.417415	100681.913139	34.352551
965.102517	100845.731535	34.357568
965.925170	101019.303975	34.362586
967.437314	101169.745967	34.367604
968.183666	101348.352620	34.372621
969.002456	101512.039316	34.377639
969.923115	101685.422442	34.382656
970.916402	101867.175503	34.387674
972.118427	102034.227949	34.392692
972.982573	102202.335744	34.397709
973.836777	102383.023074	34.402727
974.675293	102574.439962	34.407744
975.318705	102748.569405	34.412762
976.857742	102924.993854	34.417780
977.713528	103111.593209	34.422797
978.806216	103287.417489	34.427815
979.657286	103462.380320	34.432832
980.359436	103641.285205	34.437850
981.930000	103818.001066	34.442868
982.465036	104001.092785	34.447885
983.689646	104188.971723	34.452903
984.332699	104375.078908	34.457920
985.430517	104569.129289	34.462938
986.374744	104748.483991	34.467956
987.234404	104940.342213	34.472973
987.959788	105135.671398	34.477991
988.822889	105330.561718	34.483008
989.548090	105533.158673	34.488026
990.743524	105723.117513	34.493044
991.886912	105922.937835	34.498061
993.124934	106123.289751	34.503079
994.210588	106317.250601	34.508096
995.265853	106507.020195	34.513114
996.275905	106699.004269	34.518132
997.325808	106895.218382	34.523149
998.595322	107076.132128	34.528167
999.908607	107261.617590	34.533184
1001.160896	107457.219924	34.538202
1002.592936	107627.307372	34.543220
1003.575800	107810.057803	34.548237
1004.753700	107988.365796	34.553255
1005.924438	108156.911677	34.558272
1006.884916	108334.976517	34.563290
1008.085467	108496.861973	34.568308
1009.207726	108667.725834	34.573325
1010.088230	108840.936317	34.578343
1011.138941	109006.436311	34.583360
1011.765489	109181.438223	34.588378
1013.538800	109345.304955	34.593396
1014.109348	109522.143420	34.598413
1015.308372	109687.179565	34.603431
1016.643016	109846.552062	34.608448
1017.542073	110018.028111	34.613466
1019.222860	110168.635760	34.618484
1020.039834	110326.113169	34.623501
1020.589340	110476.214448	34.628519
1021.142744	110630.145596	34.633536
1021.811979	110789.575799	34.638554
1023.372670	110948.461331	34.643572
1023.951912	111105.396059	34.648589
1025.189780	111261.746451	34.653607
1026.208809	111421.061307	34.658624
1026.791955	111590.869675	34.663642
1028.157132	111754.342228	34.668660
1028.884330	111919.285075	34.673677
1029.997582	112092.931584	34.678695
1030.810612	112267.437595	34.683712
1031.592120	112443.014696	34.688730
1032.895420	112613.235118	34.693748
1033.431753	112798.376747	34.698765
1034.197976	112967.960032	34.703783
1035.676647	113151.205753	34.708800
1036.461704	113337.807731	34.713818
1037.728015	113517.080858	34.718836
1038.738958	113705.627846	34.723853
1039.726894	113901.890525	34.728871
1040.924858	114084.030762	34.733888
1041.637165	114277.573756	34.738906
1042.891104	114454.976358	34.743924
1043.842459	114656.867356	34.748941
1044.563671	114843.385547	34.753959
1045.628156	115030.396313	34.758976
1045.899807	115239.613629	34.763994
1047.034036	115439.539746	34.769012
1047.892708	115647.335715	34.774029
1049.067581	115863.289520	34.779047
1050.309807	116061.642017	34.784064
1051.490037	116265.192856	34.789082
1052.765548	116480.094427	34.794100
1053.860112	116684.967380	34.799117
1055.185668	116893.661157	34.804135
1056.339282	117087.225816	34.809152
1057.406111	117283.899932	34.814170
1058.647813	117486.864318	34.819188
1060.049876	117693.292802	34.824205
1060.692731	117885.990221	34.829223
1061.709817	118093.521257	34.834240
1062.941685	118294.259095	34.839258
1064.164951	118487.249222	34.844276
1065.457812	118683.565423	34.849293
1066.591222	118877.205811	34.854311
1068.184241	119067.363090	34.859328
1069.337987	119259.974786	34.864346
1070.249589	119452.549250	34.869364
1071.096419	119639.058850	34.874381
1072.094895	119832.268532	34.879399
1073.594120	120024.119616	34.884416
1074.214714	120225.280384	34.889434
1075.474869	120416.549283	34.894452
1076.791438	120607.810293	34.899469
1077.682475	120796.386204	34.904487
1078.980011	120982.692174	34.909504
1079.746025	121178.938644	34.914522
1081.372586	121357.786737	34.919540
1082.417644	121552.672128	34.924557
1082.642942	121747.965905	34.929575
1083.968769	121945.790354	34.934592
1084.700283	122146.499653	34.939610
1085.891559	122334.452421	34.944628
1087.132772	122539.663410	34.949645
1087.543832	122753.111593	34.954663
1089.020769	122947.606427	34.959680
1089.991803	123138.210752	34.964698
1091.085914	123322.504520	34.969716
1092.364110	123506.351683	34.974733
1093.493620	123698.671847	34.979751
1094.428676	123883.779635	34.984768
1095.431837	124076.070645	34.989786
1096.495704	124273.985736	34.994804
1097.521751	124458.422240	34.999821
1098.138591	124662.968012	35.004839
1099.329985	124866.371897	35.009856
1100.354107	125061.582182	35.014874
1101.514310	125268.405616	35.019892
1102.922646	125470.294241	35.024909
1103.495610	125683.834103	35.029927
1105.018566	125880.860523	35.034944
1106.306168	126087.871149	35.039962
1107.191755	126290.238949	35.044980
1108.448285	126501.722283	35.049997
1109.343785	126714.861777	35.055015
1110.528241	126917.223925	35.060032
1111.642236	127139.948154	35.065050
1112.672439	127346.396411	35.070068
1113.932643	127563.961734	35.075085
1114.639553	127782.705918	35.080103
1116.128068	127998.423484	35.085120
1116.686362	128218.576134	35.090138
1118.051869	128439.618561	35.095156
1118.906941	128650.604724	35.100173
1119.825458	128884.571937	35.105191
1121.193470	129107.545990	35.110208
1122.381189	129344.886587	35.115226
1123.480766	129573.779540	35.120244
1124.396568	129802.461426	35.125261
1125.966702	130024.355553	35.130279
1127.595962	130244.731703	35.135296
1128.769338	130461.323183	35.140314
1129.769650	130684.692938	35.145332
1130.833602	130917.316276	35.150349
1131.569809	131136.187338	35.155367
1133.035314	131368.927877	35.160384
1134.233622	131600.759866	35.165402
1135.387754	131815.445196	35.170420
1136.721771	132039.467558	35.175437
1137.802946	132266.588604	35.180455
1139.156881	132492.158175	35.185472
1139.811168	132721.188261	35.190490
1141.004019	132948.523747	35.195508
1142.202112	133174.007011	35.200525
1143.388434	133411.420857	35.205543
1144.699119	133646.913156	35.210560
1145.994540	133876.775148	35.215578
1146.817854	134102.892809	35.220596
1147.991953	134326.913738	35.225613
1148.894800	134567.131671	35.230631
1150.168094	134802.115651	35.235648
1151.480774	135036.307950	35.240666
1152.729780	135257.022544	35.245684
1154.135884	135480.137318	35.250701
1154.947361	135724.410977	35.255719
1156.095121	135949.535385	35.260736
1157.317635	136177.643972	35.265754
1158.917416	136407.166648	35.270772
1160.346745	136616.235773	35.275789
1162.073805	136832.467094	35.280807
1163.098505	137039.761455	35.285824
1164.534295	137257.512402	35.290842
1165.507174	137475.006901	35.295860
1167.092091	137677.546474	35.300877
1168.029010	137875.239205	35.305895
1169.296025	138065.343105	35.310912
1170.709577	138274.257210	35.315930
1171.201818	138462.352046	35.320948
1172.601325	138667.082292	35.325965
1173.229699	138867.657470	35.330983
1174.403754	139080.927405	35.336000
1175.621136	139287.249786	35.341018
1176.621726	139491.233860	35.346036
1177.727055	139705.875262	35.351053
1178.723204	139924.367320	35.356071
1179.863029	140140.693144	35.361088
1180.759020	140356.626629	35.366106
1181.820672	140578.982126	35.371124
1183.210593	140803.914289	35.376141
1184.211547	141031.814634	35.381159
1185.194960	141248.715638	35.386176
1186.019355	141485.123392	35.391194
1187.418520	141709.728344	35.396212
1188.755618	141934.851697	35.401229
1190.191864	142172.791480	35.406247
1191.613566	142404.515922	35.411264
1192.765574	142634.557641	35.416282
1193.648062	142868.158168	35.421300
1195.367039	143096.894901	35.426317
1195.873726	143338.539461	35.431335
1197.165591	143583.603254	35.436352
1198.319192	143822.597863	35.441370
1199.578592	144056.804936	35.446388
1200.694128	144294.411656	35.451405
1202.147734	144547.374559	35.456423
1202.928164	144782.700727	35.461440
1204.117927	145033.460885	35.466458
1205.800724	145282.203207	35.471476
1206.772345	145524.229692	35.476493
1207.875906	145776.403138	35.481511
1209.144595	146029.224665	35.486528
1210.214387	146279.603563	35.491546
1211.645754	146513.008094	35.496564
1213.202733	146749.414821	35.501581
1214.633057	147000.464237	35.506599
1216.294796	147250.590155	35.511616
1217.407406	147487.805968	35.516634
1218.205119	147739.986072	35.521652
1219.846026	147962.905505	35.526669
1221.099167	148213.391909	35.531687
1222.236375	148449.732399	35.536704
1223.648667	148689.597593	35.541722
1224.324989	148936.001730	35.546740
1225.706478	149179.770698	35.551757
1227.065774	149428.735729	35.556775
1227.751038	149675.383034	35.561792
1228.939170	149918.550963	35.566810
1229.985040	150177.380374	35.571828
1231.360930	150431.145487	35.576845
1232.454161	150696.976681	35.581863
1233.613513	150957.696044	35.586880
1234.747080	151210.106425	35.591898
1236.169668	151470.952030	35.596916
1237.717240	151717.994010	35.601933
1238.912442	151965.688856	35.606951
1240.034533	152234.226697	35.611968
1241.892882	152471.258777	35.616986
1243.230447	152728.175814	35.622004
1244.680228	152962.785931	35.627021
1245.661839	153226.653763	35.632039
1247.036492	153454.702203	35.637056
1248.209792	153706.254439	35.642074
1249.203705	153945.560633	35.647092
1250.826588	154172.354451	35.652109
1252.032219	154412.302245	35.657127
1253.072173	154651.362986	35.662144
1254.217240	154884.048393	35.667162
1254.796586	155124.274904	35.672180
1256.335218	155356.342043	35.677197
1257.435341	155609.145398	35.682215
1258.409877	155858.872032	35.687232
1259.691002	156099.208500	35.692250
1260.359966	156366.668715	35.697268
1261.800263	156617.087329	35.702285
1263.195780	156881.237061	35.707303
1264.415681	157144.107885	35.712320
1265.672106	157405.057219	35.717338
1266.945995	157675.919702	35.722356
1268.160227	157933.805755	35.727373
1269.265306	158207.451859	35.732391
1270.431048	158477.446201	35.737408
1272.151854	158737.211409	35.742426
1273.139346	159018.090407	35.747444
1274.445142	159285.590815	35.752461
1275.860665	159559.930684	35.757479
1277.388623	159834.838154	35.762496
1279.030209	160104.054185	35.767514
1279.964823	160365.777436	35.772532
1281.366793	160639.298961	35.777549
1282.618410	160919.167621	35.782567
1283.846283	161191.373050	35.787584
1285.143766	161454.973746	35.792602
1286.389080	161747.504664	35.797620
1287.822283	162019.440257	35.802637
1288.725954	162312.547751	35.807655
1289.548019	162598.191434	35.812672
1290.975031	162875.667020	35.817690
1292.460144	163157.222816	35.822708
1294.090827	163446.374697	35.827725
1295.282963	163733.755549	35.832743
1296.997639	164010.581473	35.837760
1298.437820	164297.189553	35.842778
1299.563087	164579.137821	35.847796
1301.250832	164852.581528	35.852813
1302.896356	165127.734272	35.857831
1304.247239	165405.524335	35.862848
1305.509299	165683.380221	35.867866
1307.210454	165951.671459	35.872884
1308.841603	166218.184479	35.877901
1310.692156	166495.100851	35.882919
1312.369253	166747.375742	35.887936
1313.861698	166993.941512	35.892954
1314.945504	167257.281122	35.897972
1316.116844	167516.278387	35.902989
1317.457219	167765.714763	35.908007
1318.356587	168019.474527	35.913024
1319.940018	168276.442033	35.918042
1320.761174	168537.922958	35.923060
1322.149970	168791.037478	35.928077
1324.097900	169057.562416	35.933095
1324.922700	169313.522324	35.938112
1326.561719	169559.020139	35.943130
1327.470924	169830.281496	35.948148
1328.746366	170081.716805	35.953165
1329.845746	170344.709729	35.958183
1330.680118	170606.157891	35.963200
1332.445442	170881.542714	35.968218
1333.384740	171159.076749	35.973236
1334.766154	171426.295683	35.978253
1335.748488	171683.750098	35.983271
1336.921822	171961.898015	35.988288
1338.339449	172221.419307	35.993306
1339.200997	172496.722896	35.998324
1340.607551	172758.165083	36.003341
1342.205559	173023.031984	36.008359
1343.183049	173293.279218	36.013376
1344.393361	173554.056405	36.018394
1345.863907	173831.174053	36.023412
1346.864776	174114.207257	36.028429
1348.326847	174398.832714	36.033447
1349.774964	174668.274476	36.038464
1351.915909	174941.316539	36.043482
1353.491261	175210.740193	36.048500
1355.028316	175484.348438	36.053517
1356.345582	175760.772913	36.058535
1357.431107	176021.653802	36.063552
1358.777307	176298.888238	36.068570
1360.217302	176578.280334	36.073588
1361.631548	176857.880566	36.078605
1362.718970	177118.053469	36.083623
1364.094686	177405.763151	36.088640
1365.578507	177683.831398	36.093658
1366.605451	177968.422933	36.098676
1368.087803	178255.509242	36.103693
1369.829865	178525.565052	36.108711
1371.355294	178809.344796	36.113728
1372.406403	179103.028520	36.118746
1373.967815	179385.610805	36.123764
1375.116450	179667.115706	36.128781
1376.722718	179958.785138	36.133799
1377.829790	180243.244484	36.138816
1379.351115	180526.319192	36.143834
1380.659748	180829.441656	36.148852
1381.848113	181115.237087	36.153869
1383.490454	181406.905501	36.158887
1384.439617	181713.592068	36.163904
1385.827622	182011.575534	36.168922
1387.015969	182322.925330	36.173940
1388.146128	182630.780269	36.178957
1389.560605	182936.686804	36.183975
1390.535428	183241.723379	36.188992
1392.046488	183563.668695	36.194010
1392.996298	183886.845865	36.199028
1394.550909	184197.204602	36.204045
1396.070114	184512.852827	36.209063
1397.423528	184831.042499	36.214080
1399.356347	185151.453800	36.219098
1400.769406	185476.773307	36.224116
1401.960532	185788.387589	36.229133
1403.834809	186118.589785	36.234151
1405.069489	186439.317562	36.239168
1406.431995	186754.565420	36.244186
1408.082224	187069.311989	36.249204
1409.927890	187407.269559	36.254221
1411.262146	187760.116270	36.259239
1412.489712	188079.224494	36.264256
1414.277879	188390.803738	36.269274
1415.810192	188707.326094	36.274292
1416.606188	189014.490394	36.279309
1418.519260	189329.964310	36.284327
1420.033883	189653.045311	36.289344
1421.450822	189961.029383	36.294362
1422.301197	190269.052154	36.299380
1423.701147	190591.213915	36.304397
1425.362870	190900.990979	36.309415
1426.818732	191224.390333	36.314432
1428.281348	191539.051710	36.319450
1429.496004	191857.054797	36.324468
1430.974560	192158.430758	36.329485
1432.756784	192446.907148	36.334503
1433.585950	192756.057230	36.339520
1435.219946	193055.480572	36.344538
1436.615393	193354.078328	36.349556
1437.890955	193659.096593	36.354573
1439.589052	193961.966558	36.359591
1440.890924	194273.510217	36.364608
1442.497030	194580.104570	36.369626
1443.451501	194901.026307	36.374644
1444.840827	195214.158756	36.379661
1446.188596	195523.285019	36.384679
1447.569739	195852.397655	36.389696
1449.092660	196169.753406	36.394714
1450.621887	196490.919116	36.399732
1451.597806	196822.967824	36.404749
1453.086660	197152.447655	36.409767
1454.284922	197490.661095	36.414784
1455.689416	197815.913544	36.419802
1456.898570	198157.835459	36.424820
1458.144799	198498.533058	36.429837
1460.065699	198849.743822	36.434855
1461.367178	199191.729809	36.439872
1463.210225	199535.638537	36.444890
1465.184398	199869.290448	36.449908
1466.760724	200207.425292	36.454925
1468.613430	200531.266952	36.459943
1470.640309	200851.525674	36.464960
1472.386632	201173.353057	36.469978
1474.167425	201500.484745	36.474996
1475.698655	201831.034632	36.480013
1477.070417	202150.483842	36.485031
1478.289294	202483.192247	36.490048
1479.823160	202791.719574	36.495066
1480.988650	203130.280107	36.500084
1482.343796	203465.356822	36.505101
1483.663126	203796.578537	36.510119
1485.006805	204138.237528	36.515136
1486.293374	204468.144590	36.520154
1487.759193	204809.353795	36.525172
1489.154796	205162.437694	36.530189
1490.302390	205506.720824	36.535207
1491.568490	205866.430952	36.540224
1492.916716	206228.034063	36.545242
1494.269383	206588.976610	36.550260
1495.392814	206952.318115	36.555277
1496.953985	207312.263894	36.560295
1498.359517	207689.229294	36.565312
1500.001705	208053.329666	36.570330
1501.464483	208425.028832	36.575348
1503.284510	208797.282331	36.580365
1505.206881	209150.874362	36.585383
1506.862372	209517.413541	36.590400
1508.654713	209876.539444	36.595418
1509.886588	210242.841097	36.600436
1511.235555	210610.166457	36.605453
1512.946111	210960.771043	36.610471
1514.431696	211330.667111	36.615488
1515.887314	211696.656194	36.620506
1517.582489	212056.968641	36.625524
1519.413441	212418.936893	36.630541
1521.180901	212789.679738	36.635559
1522.504764	213146.977698	36.640576
1524.174250	213501.833999	36.645594
1525.822713	213868.125611	36.650612
1527.141788	214228.169029	36.655629
1528.950476	214581.785235	36.660647
1530.865045	214926.519286	36.665664
1532.033796	215271.802229	36.670682
1533.630933	215598.905509	36.675700
1534.825639	215944.108737	36.680717
1536.552926	216272.081293	36.685735
1537.971185	216623.829652	36.690752
1539.136359	216957.377901	36.695770
1540.472046	217305.989600	36.700788
1542.141038	217644.057558	36.705805
1543.771450	217988.965421	36.710823
1545.180489	218344.171335	36.715840
1546.408959	218691.505093	36.720858
1548.214966	219044.845608	36.725876
1549.678938	219403.777912	36.730893
1551.115757	219750.139674	36.735911
1552.492933	220129.917199	36.740928
1553.985954	220485.212706	36.745946
1555.548865	220856.578171	36.750964
1557.158717	221221.280581	36.755981
1558.538141	221596.663481	36.760999
1560.150571	221972.238677	36.766016
1561.892740	222341.747515	36.771034
1563.469372	222716.032918	36.776052
1564.623047	223092.366122	36.781069
1566.250822	223467.583634	36.786087
1568.104872	223861.666432	36.791104
1569.731932	224238.383010	36.796122
1571.450312	224621.995242	36.801140
1572.994273	225003.094387	36.806157
1574.301960	225378.895660	36.811175
1576.349624	225768.400943	36.816192
1578.034957	226143.558797	36.821210
1579.491821	226520.683087	36.826228
1580.787111	226924.405287	36.831245
1582.479370	227305.227030	36.836263
1584.606776	227686.539489	36.841280
1586.435377	228071.048729	36.846298
1588.180024	228439.591855	36.851316
1589.889271	228821.985622	36.856333
1591.899979	229191.655466	36.861351
1593.339019	229574.015046	36.866368
1594.465197	229949.208693	36.871386
1596.208174	230324.280244	36.876404
1597.795057	230711.519160	36.881421
1599.541979	231083.083976	36.886439
1600.957339	231466.310099	36.891456
1602.924082	231847.747641	36.896474
1604.755877	232226.691078	36.901492
1606.263519	232608.072970	36.906509
1608.114947	232974.590323	36.911527
1609.269575	233350.082427	36.916544
1611.495369	233720.935533	36.921562
1612.926756	234106.850140	36.926580
1614.410051	234471.442494	36.931597
1615.924309	234847.537624	36.936615
1618.009949	235222.526850	36.941632
1619.656008	235606.247208	36.946650
1621.370058	235965.416549	36.951668
1622.812722	236326.355475	36.956685
1624.810441	236695.996857	36.961703
1626.276745	237074.485283	36.966720
1627.918338	237445.705828	36.971738
1629.547894	237808.646274	36.976756
1630.830451	238191.125156	36.981773
1632.538721	238562.079957	36.986791
1634.341584	238934.315085	36.991808
1635.889086	239301.280386	36.996826
1637.548111	239677.550834	37.001844
1639.129227	240040.394573	37.006861
1640.881911	240394.370611	37.011879
1642.246614	240760.854540	37.016896
1643.081788	241109.841742	37.021914
1644.265681	241474.803362	37.026932
1645.963431	241851.090086	37.031949
1647.723478	242233.234624	37.036967
1649.197393	242606.405214	37.041984
1650.424165	242988.479576	37.047002
1652.036984	243365.894934	37.052020
1653.328918	243763.225043	37.057037
1655.065176	244156.826873	37.062055
1656.652037	244552.559809	37.067072
1658.070864	244957.031490	37.072090
1659.624739	245354.444664	37.077108
1660.845255	245773.374580	37.082125
1662.632394	246174.204407	37.087143
1664.547110	246599.349207	37.092160
1665.896645	247011.676983	37.097178
1667.691742	247433.841123	37.102196
1668.905374	247868.821943	37.107213
1670.671107	248298.380804	37.112231
1672.145845	248725.164499	37.117248
1674.019385	249162.909342	37.122266
1675.969757	249600.793452	37.127284
1677.739341	250044.826637	37.132301
1679.633932	250471.260803	37.137319
1681.613413	250912.388344	37.142336
1682.661370	251344.185505	37.147354
1684.859667	251776.233287	37.152372
1686.384749	252217.479065	37.157389
1688.263992	252660.979695	37.162407
1690.270514	253110.428480	37.167424
1691.642699	253543.108495	37.172442
1693.724542	253982.813986	37.177460
1695.887956	254418.390318	37.182477
1697.697715	254850.743863	37.187495
1699.456378	255275.610671	37.192512
1701.033326	255711.884329	37.197530
1702.861224	256146.085207	37.202548
1704.814783	256580.417400	37.207565
1706.405100	257010.359824	37.212583
1708.403570	257453.013574	37.217600
1709.724324	257883.020646	37.222618
1711.640658	258315.930320	37.227636
1713.206470	258753.973450	37.232653
1715.069819	259190.546016	37.237671
1716.826575	259619.157949	37.242688
1717.972961	260065.390075	37.247706
1720.194308	260507.108847	37.252724
1721.622952	260947.908578	37.257741
1723.730549	261378.313351	37.262759
1725.378462	261829.946564	37.267776
1727.378281	262265.597188	37.272794
1729.663392	262694.521319	37.277812
1731.351845	263113.148684	37.282829
1733.834532	263536.298250	37.287847
1735.738260	263964.718221	37.292864
1736.985206	264383.790681	37.297882
1738.941468	264805.722169	37.302900
1740.575561	265226.102203	37.307917
1742.410877	265644.163107	37.312935
1744.130819	266072.653891	37.317952
1745.249408	266489.324905	37.322970
1747.303567	266910.952900	37.327988
1748.662303	267347.723866	37.333005
1750.317355	267772.179038	37.338023
1752.060743	268199.742508	37.343040
1753.413125	268624.673029	37.348058
1755.524922	269037.952045	37.353076
1757.457243	269452.882788	37.358093
1758.998402	269873.688997	37.363111
1761.285258	270277.918817	37.368128
1762.432610	270688.293602	37.373146
1764.279851	271096.804561	37.378164
1765.405495	271516.068091	37.383181
1767.366472	271935.706860	37.388199
1769.488111	272359.458216	37.393216
1771.084349	272780.521437	37.398234
1772.839805	273196.478291	37.403252
1774.438771	273617.333790	37.408269
1775.837191	274051.247074	37.413287
1777.966826	274485.145273	37.418304
1779.010230	274928.201509	37.423322
1781.296176	275350.769291	37.428340
1782.779317	275805.942182	37.433357
1784.064474	276258.654681	37.438375
1785.873163	276707.143171	37.443392
1787.649987	277172.293700	37.448410
1789.232232	277630.767498	37.453428
1791.058851	278097.098332	37.458445
1792.339999	278570.063683	37.463463
1793.924133	279043.004096	37.468480
1795.712997	279524.873938	37.473498
1797.520153	280011.689811	37.478516
1799.245155	280496.890106	37.483533
1801.113812	280993.466837	37.488551
1802.805091	281482.652833	37.493568
1804.249423	281988.177179	37.498586
1805.900137	282484.219146	37.503604
1807.158460	282998.754911	37.508621
1809.228676	283519.000401	37.513639
1810.687420	284032.989373	37.518656
1812.207746	284557.401493	37.523674
1814.264817	285090.232271	37.528692
1816.231585	285626.501040	37.533709
1818.263621	286153.309311	37.538727
1820.513776	286670.125505	37.543744
1821.921045	287208.170458	37.548762
1824.140381	287740.903989	37.553780
1825.901723	288278.478488	37.558797
1827.691079	288809.340778	37.563815
1829.688997	289347.174049	37.568832
1831.585414	289885.755001	37.573850
1834.092877	290407.477759	37.578868
1836.264710	290929.629548	37.583885
1838.226353	291456.354733	37.588903
1840.648790	291962.005576	37.593920
1842.274920	292485.905330	37.598938
1844.410266	293001.697701	37.603956
1846.171779	293516.020773	37.608973
1848.060765	294029.633962	37.613991
1850.504574	294533.025610	37.619008
1851.956354	295051.319161	37.624026
1854.068603	295553.890708	37.629044
1855.808841	296067.306226	37.634061
1857.654544	296577.781016	37.639079
1859.455258	297080.997308	37.644096
1861.447086	297591.567095	37.649114
1863.620579	298089.917789	37.654132
1865.705046	298605.109801	37.659149
1867.492265	299111.711930	37.664167
1869.582117	299602.826823	37.669184
1871.140490	300107.170779	37.674202
1872.870866	300617.322033	37.679220
1875.186746	301117.857042	37.684237
1876.847867	301611.381774	37.689255
1878.503563	302091.575288	37.694272
1880.392635	302574.190335	37.699290
1882.062069	303054.220652	37.704308
1883.852665	303533.237599	37.709325
1885.331040	304024.026773	37.714343
1887.272780	304509.560344	37.719360
1888.868221	305016.644033	37.724378
1890.692600	305503.049630	37.729396
1892.335249	306004.861602	37.734413
1894.072879	306519.117054	37.739431
1896.010676	307017.065222	37.744448
1897.726136	307526.440196	37.749466
1899.612658	308048.753769	37.754484
1901.607245	308547.413777	37.759501
1904.045990	309064.629781	37.764519
1905.920202	309575.380068	37.769536
1907.890570	310103.597912	37.774554
1909.922272	310617.307558	37.779572
1911.736774	311129.116696	37.784589
1913.366164	311661.761602	37.789607
1915.699448	312178.757438	37.794624
1917.578622	312694.118147	37.799642
1919.839519	313217.179723	37.804660
1922.101035	313731.276247	37.809677
1923.603490	314268.022762	37.814695
1925.536408	314782.032045	37.819712
1927.590700	315314.999931	37.824730
1929.308200	315844.740404	37.829748
1930.883932	316379.090289	37.834765
1932.859882	316911.873872	37.839783
1934.818545	317445.110575	37.844800
1936.664451	317996.300275	37.849818
1938.684683	318534.082093	37.854836
1940.484434	319086.838675	37.859853
1941.830907	319637.020002	37.864871
1944.116972	320183.063265	37.869888
1946.104945	320751.806755	37.874906
1947.723647	321304.791573	37.879924
1950.080534	321863.769077	37.884941
1951.781712	322424.034379	37.889959
1954.117920	322989.013971	37.894976
1955.818081	323559.185607	37.899994
1957.776650	324119.108746	37.905012
1959.518216	324684.412008	37.910029
1961.379393	325267.043882	37.915047
1963.421465	325840.479604	37.920064
1965.585781	326406.098796	37.925082
1967.595596	326980.563643	37.930100
1969.758898	327558.700479	37.935117
1971.630296	328135.834376	37.940135
1973.675924	328708.467340	37.945152
1975.432795	329288.925879	37.950170
1977.584502	329861.474691	37.955188
1979.770168	330444.030794	37.960205
1981.518694	331024.439399	37.965223
1983.632023	331595.598634	37.970240
1985.662267	332179.395880	37.975258
1987.435280	332760.712980	37.980276
1989.924300	333344.242967	37.985293
1991.820332	333922.326609	37.990311
1993.604241	334503.183878	37.995328
1995.715506	335079.643195	38.000346
1997.660725	335662.892297	38.005364
1999.654396	336231.488543	38.010381
2001.515466	336818.283702	38.015399
2003.732840	337396.034482	38.020416
2006.058640	337980.683629	38.025434
2007.921238	338547.260410	38.030452
2010.249620	339099.602400	38.035469
2012.071512	339660.283564	38.040487
2014.403500	340206.393823	38.045504
2016.207786	340748.291944	38.050522
2018.023182	341311.712501	38.055540
2020.301204	341868.559010	38.060557
2022.325765	342420.921964	38.065575
2024.117473	342973.439372	38.070592
2026.092697	343535.429452	38.075610
2027.950314	344096.845470	38.080628
2029.835430	344654.367943	38.085645
2031.548780	345240.437398	38.090663
2033.499514	345812.207902	38.095680
2035.751319	346382.095809	38.100698
2037.375024	346962.798756	38.105716
2039.153584	347542.377015	38.110733
2040.921769	348141.877495	38.115751
2043.200962	348738.117591	38.120768
2044.887910	349342.223906	38.125786
2047.143454	349944.759500	38.130804
2049.048941	350558.926081	38.135821
2051.457974	351168.793372	38.140839
2053.450871	351768.369705	38.145856
2055.197378	352383.844893	38.150874
2057.271005	353008.587082	38.155892
2059.453496	353614.741719	38.160909
2061.337434	354235.509060	38.165927
2063.555015	354860.749958	38.170944
2065.936753	355490.566654	38.175962
2067.101434	356114.781074	38.180980
2069.488118	356758.184745	38.185997
2071.739570	357394.244756	38.191015
2073.497037	358025.856739	38.196032
2075.590240	358672.511000	38.201050
2077.660363	359316.037327	38.206068
2080.105732	359963.572258	38.211085
2082.152512	360612.777865	38.216103
2084.702685	361262.068109	38.221120
2086.686627	361900.280602	38.226138
2088.718787	362541.665384	38.231156
2091.477630	363175.521875	38.236173
2093.726479	363831.240645	38.241191
2096.184439	364460.123673	38.246208
2098.264219	365099.138924	38.251226
2100.283283	365737.566741	38.256244
2102.554266	366370.036343	38.261261
2104.471145	367018.132503	38.266279
2106.680647	367661.125377	38.271296
2108.908320	368289.479501	38.276314
2110.602694	368935.970466	38.281332
2112.818790	369582.390368	38.286349
2115.044024	370227.045626	38.291367
2116.957994	370866.540439	38.296384
2118.989403	371515.377099	38.301402
2120.737724	372165.889786	38.306420
2123.213275	372808.013757	38.311437
2125.541248	373464.815216	38.316455
2127.774157	374107.453474	38.321472
2130.036968	374759.623028	38.326490
2131.991905	375417.119872	38.331508
2134.389839	376051.148795	38.336525
2136.401358	376691.708411	38.341543
2138.729039	377338.206966	38.346560
2141.276880	377986.960582	38.351578
2143.331168	378630.481425	38.356596
2145.905069	379276.615666	38.361613
2147.569609	379905.626853	38.366631
2149.853353	380538.122817	38.371648
2152.101075	381156.121256	38.376666
2154.096140	381770.269392	38.381684
2155.846284	382380.667542	38.386701
2157.850154	382997.216594	38.391719
2160.050429	383606.400924	38.396736
2162.531484	384224.821269	38.401754
2163.710595	384854.168014	38.406772
2165.834531	385488.872038	38.411789
2167.938222	386126.880697	38.416807
2169.375202	386761.103115	38.421824
2172.202415	387397.700220	38.426842
2174.513085	388041.983724	38.431860
2176.564354	388677.656711	38.436877
2178.761166	389325.444376	38.441895
2181.004696	389970.802393	38.446912
2183.133710	390621.782209	38.451930
2185.387534	391283.915885	38.456948
2187.921309	391932.772041	38.461965
2189.910975	392593.240509	38.466983
2192.085556	393256.396193	38.472000
2194.546560	393912.400503	38.477018
2196.612084	394580.701138	38.482036
2198.794094	395243.902076	38.487053
2201.155291	395915.207443	38.492071
2202.998248	396580.955493	38.497088
2205.535779	397261.813942	38.502106
2206.921173	397942.731705	38.507124
2209.591052	398614.570105	38.512141
2211.685868	399316.496497	38.517159
2213.428279	399992.996029	38.522176
2216.375085	400675.158924	38.527194
2218.829661	401372.461922	38.532212
2221.047960	402055.507754	38.537229
2222.745156	402747.269378	38.542247
2224.912320	403440.859709	38.547264
2227.417855	404145.661704	38.552282
2229.061582	404850.930821	38.557300
2231.175006	405562.936163	38.562317
2233.870599	406266.427592	38.567335
2235.748079	406973.921259	38.572352
2238.145880	407699.577950	38.577370
2240.174889	408420.360486	38.582388
2242.576534	409127.197508	38.587405
2244.787787	409859.643115	38.592423
2247.031033	410575.818527	38.597440
2249.767138	411294.979493	38.602458
2251.854343	412024.437529	38.607476
2254.257732	412748.054386	38.612493
2256.728198	413471.029435	38.617511
2258.642955	414200.693822	38.622528
2260.765549	414929.794992	38.627546
2262.986733	415661.941329	38.632564
2265.005595	416397.584135	38.637581
2267.905469	417120.823497	38.642599
2270.337129	417860.295912	38.647616
2273.004317	418595.001944	38.652634
2274.704388	419327.203631	38.657652
2277.303683	420060.048068	38.662669
2279.456348	420789.295461	38.667687
2281.632381	421531.661168	38.672704
2283.890091	422258.058976	38.677722
2285.925714	422997.106916	38.682740
2288.488438	423728.916352	38.687757
2290.819795	424472.010728	38.692775
2292.733059	425211.553598	38.697792
2295.114782	425950.237769	38.702810
2297.618077	426694.588551	38.707828
2299.693171	427416.583556	38.712845
2302.490454	428137.327368	38.717863
2304.186072	428850.483305	38.722880
2306.604183	429560.063332	38.727898
2308.602952	430279.792697	38.732916
2311.059811	430996.947438	38.737933
2313.315268	431710.468422	38.742951
2315.262519	432432.856176	38.747968
2317.952426	433151.310581	38.752986
2319.772007	433886.450598	38.758004
2322.498769	434602.419675	38.763021
2324.709349	435333.198529	38.768039
2326.920507	436075.015783	38.773056
2329.364025	436802.063986	38.778074
2331.396462	437549.511205	38.783092
2333.752068	438295.615349	38.788109
2335.757500	439051.243213	38.793127
2337.979639	439813.879867	38.798144
2340.807219	440566.337594	38.803162
2342.876984	441314.842270	38.808180
2345.222015	442086.763316	38.813197
2347.640698	442855.357467	38.818215
2349.803558	443632.849635	38.823232
2352.183553	444400.931010	38.828250
2354.270563	445182.864910	38.833268
2356.831623	445958.277256	38.838285
2359.380481	446746.031604	38.843303
2361.561135	447529.870444	38.848320
2364.405686	448305.542402	38.853338
2366.635260	449106.121059	38.858356
2368.840620	449889.298197	38.863373
2371.487567	450684.136486	38.868391
2373.607647	451488.008837	38.873408
2375.920959	452286.109689	38.878426
2378.008856	453101.576473	38.883444
2380.553480	453917.539974	38.888461
2383.106246	454723.368475	38.893479
2384.985995	455547.790377	38.898496
2387.088334	456360.630323	38.903514
2389.428380	457188.032170	38.908532
2391.589540	458016.886177	38.913549
2394.359452	458845.756632	38.918567
2396.541070	459683.258296	38.923584
2399.344361	460515.777433	38.928602
2401.837916	461353.905565	38.933620
2404.339794	462191.940704	38.938637
2406.628466	463030.674191	38.943655
2409.036146	463880.346162	38.948672
2412.134107	464710.191745	38.953690
2414.380120	465539.070160	38.958708
2416.837194	466389.919044	38.963725
2419.386097	467215.892369	38.968743
2422.138929	468063.381086	38.973760
2424.354446	468904.101384	38.978778
2426.699291	469738.605535	38.983796
2429.823002	470575.719262	38.988813
2432.613984	471401.898959	38.993831
2434.700939	472245.040070	38.998848
2437.285837	473058.561163	39.003866
2439.867120	473880.260788	39.008884
2442.128417	474720.119685	39.013901
2444.675586	475546.882483	39.018919
2446.944094	476370.722216	39.023936
2449.234761	477200.615840	39.028954
2451.874379	478042.207366	39.033972
2453.950537	478876.231043	39.038989
2456.847485	479709.023894	39.044007
2459.295342	480545.774276	39.049024
2461.918283	481364.662083	39.054042
2464.573163	482168.332934	39.059060
2466.832950	482965.069934	39.064077
2469.455737	483750.673799	39.069095
2471.799916	484543.587727	39.074112
2474.317758	485335.375731	39.079130
2476.804142	486142.444383	39.084148
2478.972921	486934.154329	39.089165
2481.382540	487734.400261	39.094183
2483.895300	488548.793859	39.099200
2486.414168	489347.577873	39.104218
2488.938174	490157.853667	39.109236
2491.725572	490975.851712	39.114253
2493.889807	491775.318437	39.119271
2495.723596	492595.442531	39.124288
2498.606611	493411.580712	39.129306
2500.960056	494240.597868	39.134324
2503.403372	495081.689883	39.139341
2506.044442	495901.304416	39.144359
2508.118213	496739.792198	39.149376
2510.849142	497570.728846	39.154394
2513.572749	498421.605298	39.159412
2515.857861	499270.588020	39.164429
2518.435699	500112.076214	39.169447
2520.783120	500963.266032	39.174464
2523.475002	501819.787654	39.179482
2526.086314	502682.209705	39.184500
2528.360377	503542.368310	39.189517
2530.681888	504408.355529	39.194535
2533.311542	505288.129887	39.199552
2535.651491	506165.983357	39.204570
2538.010394	507040.710678	39.209588
2540.326109	507938.532663	39.214605
2542.742072	508818.172046	39.219623
2545.375502	509721.163241	39.224640
2548.038520	510621.476182	39.229658
2550.828893	511525.785207	39.234676
2552.660076	512437.528274	39.239693
2555.444766	513341.217336	39.244711
2558.173685	514262.808141	39.249728
2560.962491	515167.131516	39.254746
2563.960271	516080.614109	39.259764
2566.431829	516994.721465	39.264781
2569.220654	517891.474684	39.269799
2571.790289	518805.747039	39.274816
2574.930886	519710.871014	39.279834
2577.567633	520627.372525	39.284852
2580.047809	521535.945647	39.289869
2582.819993	522439.536953	39.294887
2585.344780	523359.739462	39.299904
2588.442541	524249.489119	39.304922
2591.312739	525142.229647	39.309940
2593.930544	526044.194129	39.314957
2596.453119	526947.468490	39.319975
2599.361235	527846.250285	39.324992
2601.806787	528745.746256	39.330010
2604.822497	529643.082239	39.335028
2606.990006	530544.105454	39.340045
2609.970733	531431.731031	39.345063
2612.494902	532335.788565	39.350080
2614.971803	533231.153550	39.355098
2617.808549	534117.060973	39.360116
2620.021593	535023.740579	39.365133
2622.519254	535915.150105	39.370151
2625.218635	536825.140459	39.375168
2628.165639	537724.435681	39.380186
2630.816421	538625.018649	39.385204
2633.301177	539522.602431	39.390221
2636.034948	540404.977553	39.395239
2638.392632	541281.628905	39.400256
2640.741727	542135.589694	39.405274
2643.870454	543006.279541	39.410292
2645.949833	543874.514031	39.415309
2648.812578	544735.541894	39.420327
2651.579210	545610.019519	39.425344
2654.599839	546463.729093	39.430362
2656.984058	547328.664445	39.435380
2659.310690	548215.064366	39.440397
2661.906836	549082.651862	39.445415
2664.498966	549960.960202	39.450432
2667.258428	550842.488678	39.455450
2670.453329	551724.236201	39.460468
2672.968065	552610.839138	39.465485
2675.637172	553498.806846	39.470503
2677.903969	554388.175757	39.475520
2681.039464	555278.846856	39.480538
2683.855839	556174.764517	39.485556
2686.481216	557070.644964	39.490573
2688.795552	557969.463520	39.495591
2691.359641	558891.676816	39.500608
2694.001444	559798.373523	39.505626
2696.365253	560715.716029	39.510644
2699.179410	561646.994444	39.515661
2701.704455	562575.539211	39.520679
2704.074336	563513.101098	39.525696
2706.522502	564448.772440	39.530714
2709.556522	565394.944617	39.535732
2711.752850	566349.784228	39.540749
2714.546624	567295.438372	39.545767
2717.382344	568251.973892	39.550784
2720.585830	569209.674168	39.555802
2723.623266	570167.771083	39.560820
2725.646429	571137.509719	39.565837
2728.482897	572097.278415	39.570855
2731.196277	573069.647821	39.575872
2734.163071	574042.594896	39.580890
2737.020073	575009.370531	39.585908
2739.664115	575988.655663	39.590925
2742.765486	576962.930925	39.595943
2745.987671	577937.202681	39.600960
2748.734969	578899.658347	39.605978
2751.847416	579861.673692	39.610996
2754.845257	580838.427929	39.616013
2757.282904	581794.079465	39.621031
2760.179052	582783.280430	39.626048
2763.300385	583748.806839	39.631066
2766.144893	584712.041807	39.636084
2768.916325	585691.201029	39.641101
2771.510984	586655.603684	39.646119
2774.715218	587615.626995	39.651136
2776.989338	588587.006121	39.656154
2779.584174	589557.398390	39.661172
2782.282712	590548.124930	39.666189
2784.823108	591512.003588	39.671207
2787.814175	592500.905498	39.676224
2790.343963	593491.386763	39.681242
2793.021953	594479.255351	39.686260
2795.297094	595472.589387	39.691277
2797.767642	596474.040342	39.696295
2800.816173	597485.792974	39.701312
2803.299275	598493.592301	39.706330
2806.040798	599499.956530	39.711348
2808.973531	600515.929267	39.716365
2811.619340	601534.893155	39.721383
2814.710426	602542.008119	39.726400
2817.422907	603559.914834	39.731418
2820.414188	604555.670524	39.736436
2823.455778	605543.039201	39.741453
2825.945419	606514.134120	39.746471
2829.166648	607483.127086	39.751488
2832.092130	608452.723173	39.756506
2835.150098	609419.064120	39.761524
2838.226011	610391.345536	39.766541
2840.754182	611356.238773	39.771559
2843.935676	612332.257517	39.776576
2846.922150	613308.162654	39.781594
2849.810433	614277.158397	39.786612
2852.796913	615243.702384	39.791629
2855.381779	616213.007399	39.796647
2858.130515	617203.225961	39.801664
2861.060510	618182.204307	39.806682
2863.968390	619159.445295	39.811700
2866.299892	620147.293219	39.816717
2868.887595	621143.521947	39.821735
2871.773540	622139.703065	39.826752
2874.207224	623155.529581	39.831770
2877.300913	624175.431055	39.836788
2879.484864	625203.187217	39.841805
2882.231484	626242.797712	39.846823
2885.208519	627286.791998	39.851840
2888.136443	628327.395778	39.856858
2891.495173	629371.553710	39.861876
2893.981311	630413.495188	39.866893
2897.206636	631463.867993	39.871911
2900.200028	632520.034091	39.876928
2902.778700	633569.331557	39.881946
2906.344835	634634.876951	39.886964
2908.791091	635702.268915	39.891981
2912.191266	636762.626769	39.896999
2915.059927	637828.817593	39.902016
2917.626127	638905.278957	39.907034
2921.142592	639969.932458	39.912052
2923.970694	641047.996667	39.917069
2926.879662	642115.732772	39.922087
2930.153721	643190.795246	39.927104
2932.836163	644264.831840	39.932122
2936.001744	645337.078170	39.937140
2939.288446	646423.740251	39.942157
2942.090328	647494.003988	39.947175
2945.003150	648572.074237	39.952192
2947.765886	649650.388831	39.957210
2950.702087	650733.217702	39.962228
2953.657970	651835.927967	39.967245
2956.362570	652930.797620	39.972263
2959.303369	654029.966393	39.977280
2962.380691	655118.853059	39.982298
2965.099360	656218.931636	39.987316
2967.955901	657321.682875	39.992333
2971.155700	658425.137929	39.997351
2974.242704	659522.073588	40.002368
2977.342972	660636.087380	40.007386
2980.344575	661736.186530	40.012404
2983.146990	662853.787970	40.017421
2985.929704	663970.011253	40.022439
2989.190481	665074.861292	40.027456
2991.919088	666195.124667	40.032474
2994.828021	667318.438872	40.037492
2997.588365	668431.966101	40.042509
3000.463043	669562.233514	40.047527
3003.352351	670692.054196	40.052544
3006.417657	671826.654782	40.057562
3009.706921	672951.905998	40.062580
3012.833702	674082.979797	40.067597
3015.615169	675211.432601	40.072615
3018.782484	676335.615508	40.077632
3021.667835	677441.819219	40.082650
3025.123898	678518.579290	40.087668
3028.201615	679604.816109	40.092685
3031.207902	680686.123546	40.097703
3033.934672	681785.400329	40.102720
3037.042414	682861.513418	40.107738
3040.427113	683941.552008	40.112756
3043.519410	685025.306375	40.117773
3046.433033	686126.310331	40.122791
3049.820762	687212.850657	40.127808
3052.598654	688308.839059	40.132826
3056.047833	689410.214372	40.137844
3058.891373	690511.735383	40.142861
3061.259764	691606.460744	40.147879
3064.525856	692723.685217	40.152896
3067.243154	693843.907242	40.157914
3070.174567	694964.140010	40.162932
3073.457509	696098.491449	40.167949
3076.160330	697224.476488	40.172967
3079.526077	698364.031175	40.177984
3082.287247	699511.026274	40.183002
3085.396581	700658.890179	40.188020
3088.312316	701807.657360	40.193037
3091.549785	702964.058502	40.198055
3094.773075	704126.316147	40.203072
3097.589731	705284.717570	40.208090
3101.144162	706456.848000	40.213108
3103.954474	707624.678881	40.218125
3106.845464	708807.073544	40.223143
3110.320212	709984.908992	40.228160
3112.928153	711184.400931	40.233178
3115.664274	712385.267246	40.238196
3118.582672	713602.928165	40.243213
3121.362849	714818.596995	40.248231
3124.754728	716040.928922	40.253248
3127.427569	717261.702482	40.258266
3130.695155	718494.359059	40.263284
3133.678958	719726.271944	40.268301
3136.709531	720977.926393	40.273319
3139.737197	722218.100698	40.278336
3142.536913	723478.147655	40.283354
3145.810930	724733.383524	40.288372
3148.873827	725998.337863	40.293389
3152.337237	727264.199554	40.298407
3155.762194	728536.595781	40.303424
3158.809084	729803.474332	40.308442
3162.567287	731073.077544	40.313460
3166.032088	732338.479081	40.318477
3168.984238	733602.812277	40.323495
3172.554614	734869.783827	40.328512
3175.548852	736136.383610	40.333530
3179.040350	737399.445696	40.338548
3182.293506	738662.181652	40.343565
3185.210152	739933.694578	40.348583
3188.577399	741204.474883	40.353600
3191.852207	742471.316877	40.358618
3194.911323	743740.378711	40.363636
3197.797621	745019.064663	40.368653
3201.437288	746299.370965	40.373671
3204.367504	747563.612707	40.378688
3207.410783	748845.671460	40.383706
3210.920745	750119.334597	40.388724
3214.603156	751387.889024	40.393741
3217.617953	752663.727915	40.398759
3221.142214	753925.775740	40.403776
3224.166638	755203.511954	40.408794
3227.503616	756457.198012	40.413812
3231.244428	757701.141022	40.418829
3234.720789	758932.412191	40.423847
3238.089479	760141.391515	40.428864
3241.443566	761344.875185	40.433882
3244.613031	762544.948797	40.438900
3247.641629	763750.762634	40.443917
3250.390823	764963.264922	40.448935
3253.626416	766172.542851	40.453952
3256.704298	767401.208960	40.458970
3259.919740	768626.650507	40.463988
3262.878219	769846.973495	40.469005
3266.058998	771074.039253	40.474023
3269.134215	772306.770049	40.479040
3272.159039	773560.261382	40.484058
3275.455912	774811.622171	40.489076
3278.445836	776057.619951	40.494093
3281.419886	777328.508161	40.499111
3284.804714	778594.256574	40.504128
3287.898345	779874.515918	40.509146
3291.272285	781157.955234	40.514164
3294.698169	782434.353711	40.519181
3297.612257	783743.004383	40.524199
3300.797142	785041.642973	40.529216
3303.722328	786360.564500	40.534234
3306.708117	787678.628859	40.539252
3310.001579	789006.187303	40.544269
3312.872869	790344.371549	40.549287
3316.268600	791694.196592	40.554304
3319.325389	793058.080583	40.559322
3322.034365	794414.521036	40.564340
3325.128656	795787.284689	40.569357
3328.379272	797172.547268	40.574375
3331.991938	798556.239557	40.579392
3334.991189	799962.619746	40.584410
3338.236557	801361.400172	40.589428
3342.003138	802770.600961	40.594445
3345.317294	804188.955108	40.599463
3349.035425	805596.908221	40.604480
3352.527582	807001.180315	40.609498
3355.850548	808425.886369	40.614516
3359.621431	809838.629646	40.619533
3362.706971	811258.261281	40.624551
3366.053128	812666.645446	40.629568
3369.619760	814096.155938	40.634586
3373.064034	815516.906310	40.639604
3376.530283	816940.923788	40.644621
3380.004160	818378.598456	40.649639
3383.587838	819805.145704	40.654656
3386.728580	821236.480721	40.659674
3390.106810	822666.281881	40.664692
3393.644473	824093.785192	40.669709
3396.885823	825533.515510	40.674727
3400.518115	826972.554711	40.679744
3403.968460	828396.448515	40.684762
3407.465531	829851.698113	40.689780
3411.067189	831278.381485	40.694797
3414.293231	832724.163806	40.699815
3418.043841	834146.173307	40.704832
3421.952033	835578.377020	40.709850
3425.640428	837002.236820	40.714868
3429.382071	838427.878250	40.719885
3432.308521	839853.692862	40.724903
3436.093811	841263.841602	40.729920
3439.277275	842683.324214	40.734938
3442.708088	844108.712428	40.739956
3446.503387	845523.740801	40.744973
3449.848856	846950.966716	40.749991
3453.672463	848358.540484	40.755008
3457.009721	849759.263744	40.760013
3460.121700	851110.802849	40.765018
3463.713812	852417.516642	40.770023
3466.357188	853674.915245	40.775028
3469.750078	854874.152271	40.780032
3472.640270	856025.424207	40.785037
3475.099740	857094.892152	40.790042
3477.795735	858106.675696	40.795047
3480.239504	859073.935616	40.800052
3482.815966	859983.968598	40.805056
3484.976830	860822.097176	40.810061
3487.380984	861609.997281	40.815066
3489.427414	862349.233159	40.820071
3491.183204	863028.024234	40.825076
3493.718464	863654.437534	40.830080
3495.644937	864228.031035	40.835085
3497.126029	864751.596652	40.840090
3498.698745	865229.217812	40.845095
3500.042302	865678.148525	40.850100
3501.390639	866058.954937	40.855104
3502.838722	866418.667165	40.860109
3503.918833	866750.988915	40.865114
3505.464850	867031.171335	40.870119
3505.887439	867288.244980	40.875124
3507.154466	867503.849808	40.880128
3508.371840	867684.116512	40.885133
3508.726880	867851.574769	40.890138
3509.547105	867987.577980	40.895143
3510.304359	868104.375532	40.900148
3511.114191	868192.972126	40.905152
3511.725554	868264.027879	40.910157
3512.188560	868310.005484	40.915162
3513.107417	868336.217345	40.920167
3513.057415	868348.389215	40.925172
3513.805781	868340.452548	40.930176
3514.262978	868315.859946	40.935181
3514.629071	868273.228342	40.940186
3515.047021	868205.583947	40.945191
3515.017423	868156.834613	40.950196
3515.762921	868070.697653	40.955200
3515.860828	867982.053864	40.960205
3515.957305	867886.650570	40.965210
3516.286845	867776.340617	40.970215
3516.477262	867657.457165	40.975220
3516.883062	867524.923455	40.980224
3516.906105	867390.129108	40.985229
3517.036971	867243.437971	40.990234
3517.380115	867099.799784	40.995239
3517.071224	866946.796617	41.000244
3517.175606	866780.495074	41.005248
3517.515969	866615.310564	41.010253
3516.875321	866453.364876	41.015258
3517.954098	866277.818381	41.020263
3517.158694	866093.963928	41.025268
3517.417054	865911.773797	41.030272
3517.654372	865727.069871	41.035277
3517.258606	865549.316595	41.040282
3517.517464	865352.137203	41.045287
3517.316700	865166.517503	41.050292
3517.280213	864967.149169	41.055296
3517.576689	864770.812985	41.060301
3516.938613	864580.991957	41.065306
3517.425952	864373.695856	41.070311
3517.319394	864182.425850	41.075316
3517.478616	863963.282834	41.080320
3517.517591	863759.898936	41.085325
3516.947021	863553.994230	41.090330
3517.161337	863347.959342	41.095335
3517.083916	863144.764807	41.100340
3517.006380	862933.929056	41.105344
3517.052150	862721.326745	41.110349
3516.694344	862512.258582	41.115354
3516.706368	862304.187979	41.120359
3516.525704	862093.240475	41.125364
3516.550613	861885.635761	41.130368
3516.368677	861686.851282	41.135373
3516.382180	861481.069997	41.140378
3516.355014	861271.807844	41.145383
3515.800180	861062.427152	41.150388
3515.534760	860850.480152	41.155392
3515.741905	860652.662068	41.160397
3515.459477	860455.493696	41.165402
3515.702467	860250.695493	41.170407
3515.398234	860054.290077	41.175412
3515.294676	859846.534414	41.180416
3515.176903	859645.348213	41.185421
3514.826729	859451.636502	41.190426
3515.079122	859250.765302	41.195431
3514.964749	859064.642498	41.200436
3514.599490	858856.504936	41.205440
3514.559456	858670.357674	41.210445
3514.149364	858483.681954	41.215450
3514.198715	858291.028946	41.220455
3513.939993	858115.536034	41.225460
3514.136073	857923.234572	41.230464
3513.944986	857727.021634	41.235469
3513.748299	857544.634363	41.240474
3513.333145	857365.467422	41.245479
3513.440119	857187.857669	41.250484
3513.491809	857010.637991	41.255488
3513.353203	856833.636061	41.260493
3513.020319	856657.819906	41.265498
3513.004340	856479.530287	41.270503
3512.951072	856311.108914	41.275508
3513.029815	856123.505962	41.280512
3512.623214	855956.967650	41.285517
3512.799135	855796.235401	41.290522
3512.746821	855613.667469	41.295527
3512.380785	855442.076580	41.300532
3512.099260	855281.594984	41.305536
3512.209255	855116.306248	41.310541
3512.077906	854957.146840	41.315546
3512.140395	854793.307776	41.320551
3512.008790	854625.042846	41.325556
3511.648327	854462.421768	41.330560
3511.642006	854311.160573	41.335565
3511.139209	854151.649879	41.340570
3511.263570	853996.101641	41.345575
3511.141506	853855.976691	41.350580
3511.190097	853707.691457	41.355584
3511.204198	853560.182134	41.360589
3510.700987	853406.748733	41.365594
3510.792725	853258.735614	41.370599
3510.493090	853111.747869	41.375604
3510.617832	852970.304485	41.380608
3510.671792	852829.643132	41.385613
3510.520296	852686.299929	41.390618
3510.322457	852543.831690	41.395623
3510.158499	852411.422889	41.400628
3509.956395	852273.111480	41.405632
3510.239952	852127.072495	41.410637
3509.904624	852006.879873	41.415642
3509.994011	851865.318213	41.420647
3509.720756	851734.653774	41.425652
3510.058361	851599.437023	41.430656
3509.695141	851472.072729	41.435661
3509.679759	851339.809874	41.440666
3509.812159	851204.035023	41.445671
3509.602463	851077.412708	41.450676
3509.079655	850946.575866	41.455680
3509.571679	850823.421191	41.460685
3509.023519	850695.197231	41.465690
3509.285023	850569.652252	41.470695
3508.865177	850446.244768	41.475700
3508.811256	850327.232321	41.480704
3508.755541	850210.057804	41.485709
3508.287436	850102.727093	41.490714
3508.412012	849987.844280	41.495719
3508.410917	849877.724603	41.500724
3508.232697	849768.599072	41.505728
3508.788484	849654.320251	41.510733
3508.180326	849547.291753	41.515738
3507.933849	849434.780616	41.520743
3507.981068	849337.331756	41.525748
3507.969876	849228.169988	41.530752
3508.155049	849118.878617	41.535757
3508.233746	849017.932364	41.540762
3508.128879	848899.383030	41.545767
3507.916966	848798.187797	41.550772
3507.490270	848691.987046	41.555776
3507.608654	848585.989775	41.560781
3507.408792	848484.302844	41.565786
3507.469921	848392.261036	41.570791
3507.449719	848294.999057	41.575796
3507.273225	848192.043961	41.580800
3507.345490	848106.583760	41.585805
3507.056541	848009.068384	41.590810
3507.243382	847903.435558	41.595815
3507.249057	847826.119996	41.600820
3507.371532	847722.431686	41.605824
3507.275841	847624.879689	41.610829
3507.045436	847527.444014	41.615834
3507.282091	847432.356024	41.620839
3506.752401	847348.529123	41.625844
3506.762781	847263.550744	41.630848
3506.724481	847175.381141	41.635853
3506.342469	847083.872490	41.640858
3506.385399	846997.625481	41.645863
3506.033378	846917.834428	41.650868
3506.473865	846848.771485	41.655872
3506.711748	846760.843174	41.660877
3506.213157	846676.904881	41.665882
3506.684818	846595.333287	41.670887
3506.163205	846514.594184	41.675892
3506.122238	846426.510630	41.680896
3506.217605	846351.681215	41.685901
3505.927689	846282.338136	41.690906
3505.933705	846197.344972	41.695911
3505.742844	846126.627781	41.700916
3505.800276	846055.967839	41.705920
3505.825394	845977.364923	41.710925
3505.733634	845903.431293	41.715930
3505.727081	845826.963510	41.720935
3505.716464	845763.870391	41.725940
3505.763881	845685.260076	41.730944
3506.023210	845609.523272	41.735949
3505.278836	845544.119418	41.740954
3505.779767	845478.326318	41.745959
3505.607037	845413.316271	41.750964
3505.686185	845338.573402	41.755968
3505.953614	845250.133199	41.760973
3505.688138	845178.253097	41.765978
3505.472898	845109.078335	41.770983
3505.077240	845046.619288	41.775988
3504.955854	844974.229503	41.780992
3505.137428	844914.974557	41.785997
3504.993233	844861.973797	41.791002
3504.757689	844793.186231	41.796007
3504.645279	844751.811862	41.801012
3505.084172	844683.305331	41.806016
3504.950176	844627.392716	41.811021
3504.612775	844570.832785	41.816026
3504.741393	844505.571709	41.821031
3504.523654	844457.135027	41.826036
3504.479920	844400.818380	41.831040
3504.839005	844338.912428	41.836045
3504.376190	844297.977418	41.841050
3504.801983	844243.427816	41.846055
3504.745083	844184.590577	41.851060
3504.298387	844134.151151	41.856064
3504.439792	844077.414681	41.861069
3504.473356	844025.638924	41.866074
3504.623068	843968.027561	41.871079
3504.517068	843922.574460	41.876084
3504.464248	843861.697392	41.881088
3504.350186	843817.505112	41.886093
3504.349060	843760.787874	41.891098
3504.283186	843712.903047	41.896103
3504.120063	843671.529012	41.901108
3503.911317	843624.344482	41.906112
3504.415430	843577.532923	41.911117
3503.981366	843523.692815	41.916122
3503.899076	843478.911285	41.921127
3503.600856	843439.301980	41.926132
3503.590071	843389.660659	41.931136
3503.612722	843352.715479	41.936141
3503.302215	843316.694792	41.941146
3503.838195	843268.227468	41.946151
3503.590692	843228.608819	41.951156
3503.517594	843192.550262	41.956160
3503.408593	843153.976050	41.961165
3503.394614	843115.095840	41.966170
3503.766555	843081.682028	41.971175
3503.536395	843040.604936	41.976180
3503.928988	843012.229693	41.981184
3503.490567	842970.602875	41.986189
3503.361702	842935.908996	41.991194
3503.772837	842891.433741	41.996199
3503.261712	842868.435329	42.001204
3503.249615	842816.171250	42.006208
3503.389839	842788.901044	42.011213
3503.152879	842747.435095	42.016218
3503.369366	842713.655624	42.021223
3503.623654	842685.591346	42.026228
3503.345939	842646.943222	42.031232
3503.418618	842599.124667	42.036237
3503.214171	842571.325500	42.041242
3503.293907	842536.499692	42.046247
3503.269344	842502.174853	42.051252
3503.178511	842459.617325	42.056256
3503.205352	842433.526901	42.061261
3503.333477	842403.347551	42.066266
3503.443776	842374.722452	42.071271
3503.551592	842340.569934	42.076276
3503.248709	842296.298796	42.081280
3503.435663	842264.751859	42.086285
3503.524925	842234.480744	42.091290
3502.998580	842192.086347	42.096295
3502.859228	842161.753618	42.101300
3503.097048	842133.398356	42.106304
3503.096483	842098.291579	42.111309
3503.073627	842071.043555	42.116314
3503.233181	842036.590250	42.121319
3502.962713	842005.307397	42.126324
3502.987897	841972.038507	42.131328
3503.066763	841939.827855	42.136333
3502.860087	841916.487183	42.141338
3503.161061	841888.605795	42.146343
3502.823414	841864.024596	42.151348
3502.785309	841841.045213	42.156352
3502.926112	841807.369384	42.161357
3502.756309	841785.477213	42.166362
3502.755990	841751.629155	42.171367
3502.742998	841725.638820	42.176372
3502.625613	841704.708023	42.181376
3503.006305	841676.522215	42.186381
3502.511172	841659.141858	42.191386
3502.683211	841624.199262	42.196391
3502.745084	841604.112984	42.201396
3502.776486	841568.901079	42.206400
3503.016104	841540.445709	42.211405
3502.284238	841513.887889	42.216410
3502.871976	841488.675520	42.221415
3502.811137	841465.698234	42.226420
3502.946703	841442.496173	42.231424
3502.915396	841415.537426	42.236429
3503.052228	841395.050753	42.241434
3502.891943	841367.239018	42.246439
3502.609289	841341.095163	42.251444
3502.687624	841312.566917	42.256448
3502.715238	841277.935836	42.261453
3502.187658	841262.499265	42.266458
3502.536346	841246.731685	42.271463
3502.368782	841228.231911	42.276468
3502.637507	841209.760875	42.281472
3502.897668	841172.570949	42.286477
3502.503100	841161.284141	42.291482
3502.933292	841130.275114	42.296487
3502.508307	841109.875279	42.301492
3502.599173	841077.270072	42.306496
3502.647054	841053.692207	42.311501
3502.624643	841033.423173	42.316506
3502.784115	841015.744597	42.321511
3502.419221	840993.201000	42.326516
3502.403752	840966.043733	42.331520
3502.487090	840934.505909	42.336525
3502.703839	840920.310084	42.341530
3502.663837	840892.380314	42.346535
3502.347811	840866.530580	42.351540
3502.527250	840850.885408	42.356544
3502.493469	840825.379378	42.361549
3502.727752	840807.591485	42.366554
3501.963190	840772.984284	42.371559
3502.002100	840769.971165	42.376564
3502.396692	840749.829981	42.381568
3502.335963	840741.497268	42.386573
3502.251615	840720.945839	42.391578
3502.209529	840698.932678	42.396583
3502.234094	840677.394037	42.401588
3502.199257	840667.990129	42.406592
3502.295907	840638.679745	42.411597
3502.456254	840620.999856	42.416602
3502.369233	840598.799338	42.421607
3502.244378	840589.312372	42.426612
3502.209822	840566.230483	42.431616
3502.832983	840552.358272	42.436621
3502.405230	840531.374837	42.441626
3502.578786	840507.387129	42.446631
3502.636922	840489.528813	42.451636
3502.070229	840462.261392	42.456640
3502.204108	840455.546982	42.461645
3502.106885	840432.765392	42.466650
3502.217481	840407.040977	42.471655
3502.189060	840402.292045	42.476660
3501.901214	840380.413128	42.481664
3502.154205	840368.926567	42.486669
3501.965271	840353.822716	42.491674
3502.354913	840339.210440	42.496679
3502.157761	840313.436717	42.501684
3502.198172	840303.050369	42.506688
3502.422735	840278.471703	42.511693
3502.171626	840271.429225	42.516698
3502.228010	840248.331883	42.521703
3502.276973	840240.951429	42.526708
3502.196509	840216.129153	42.531712
3502.223065	840192.357175	42.536717
3502.234622	840184.594451	42.541722
3502.375091	840153.334580	42.546727
3502.144433	840145.609667	42.551732
3502.323189	840124.335954	42.556736
3502.516129	840101.798773	42.561741
3502.466475	840092.299256	42.566746
3502.437842	840062.617558	42.571751
3502.196738	840053.050891	42.576756
3502.168109	840028.607785	42.581760
3502.147789	840007.655817	42.586765
3502.280549	839997.933603	42.591770
3502.268583	839975.136928	42.596775
3502.148691	839974.961677	42.601780
3502.306013	839938.847269	42.606784
3502.319698	839917.210554	42.611789
3501.931883	839902.039624	42.616794
3502.320699	839888.202505	42.621799
3502.216346	839878.808213	42.626804
3501.942744	839869.537380	42.631808
3501.899546	839851.498952	42.636813
3501.807870	839839.483144	42.641818
3501.844143	839816.387265	42.646823
3502.069154	839807.523482	42.651828
3501.751198	839794.281719	42.656832
3502.509454	839777.767095	42.661837
3502.135822	839759.586004	42.666842
3502.175700	839751.139153	42.671847
3502.317387	839724.436732	42.676852
3502.073469	839717.877567	42.681856
3501.987127	839690.822562	42.686861
3501.721885	839687.565379	42.691866
3502.142325	839672.558574	42.696871
3501.854342	839660.573091	42.701876
3502.040053	839650.745013	42.706880
3502.081770	839631.625414	42.711885
3501.994855	839618.832247	42.716890
3502.051634	839604.561268	42.721895
3502.061281	839573.512841	42.726900
3502.139205	839577.284554	42.731904
3502.351775	839559.205257	42.736909
3501.944965	839541.804861	42.741914
3502.091179	839529.654216	42.746919
3502.211791	839514.499838	42.751924
3501.891062	839495.436459	42.756928
3501.947884	839471.462819	42.761933
3501.640716	839463.748976	42.766938
3502.158902	839457.846581	42.771943
3502.024761	839432.835373	42.776948
3501.851965	839430.921937	42.781952
3502.166653	839421.946538	42.786957
3501.702096	839422.989441	42.791962
3501.658365	839406.017011	42.796967
3502.204238	839396.326263	42.801972
3502.181195	839368.580721	42.806977
3501.974487	839359.298632	42.811981
3501.794153	839344.481941	42.816986
3501.639905	839326.459277	42.821991
3501.829514	839335.064986	42.826996
3502.080109	839298.641032	42.832001
3502.020206	839289.529938	42.837005
3501.786738	839290.924845	42.842010
3502.126533	839269.331820	42.847015
3501.740522	839261.921119	42.852020
3501.602311	839253.792482	42.857025
3501.875207	839221.730795	42.862029
3501.850431	839220.182262	42.867034
3501.603802	839227.789013	42.872039
3501.509690	839202.285440	42.877044
3501.542865	839194.129930	42.882049
3501.700156	839183.432270	42.887053
3501.535866	839188.115349	42.892058
3501.569723	839182.094338	42.897063
3501.328276	839164.472927	42.902068
3501.134254	839164.794381	42.907073
3501.334251	839161.367151	42.912077
3501.632134	839159.768164	42.917082
3501.818380	839150.618379	42.922087
3501.601955	839138.911741	42.927092
3501.425464	839130.400802	42.932097
3501.666464	839131.527518	42.937101
3501.281184	839126.154145	42.942106
3501.534863	839127.278879	42.947111
3501.729652	839108.909906	42.952116
3501.618148	839081.467941	42.957121
3501.671247	839084.176519	42.962125
3501.374777	839092.664504	42.967130
3501.568984	839074.586605	42.972135
3501.523802	839068.383774	42.977140
3501.274200	839059.204950	42.982145
3502.116646	839050.049464	42.987149
3501.469720	839043.358489	42.992154
3501.750838	839030.700585	42.997159
3501.649788	839019.072706	43.002164
3501.592948	839014.327106	43.007169
3501.751946	839012.458698	43.012173
3501.412757	838990.970804	43.017178
3501.503018	838993.673614	43.022183
3501.659780	838990.156014	43.027188
3501.528914	838997.065742	43.032193
3501.999773	838973.025371	43.037197
3501.802440	838961.606494	43.042202
3502.073017	838950.793676	43.047207
3502.191102	838933.697572	43.052212
3501.527515	838928.852686	43.057217
3501.829519	838912.018866	43.062221
3501.825722	838899.114123	43.067226
3501.548529	838892.656278	43.072231
3501.904269	838889.883779	43.077236
3501.795687	838873.211066	43.082241
3502.092637	838854.243138	43.087245
3501.859023	838855.055965	43.092250
3501.977304	838839.318031	43.097255
3501.878295	838830.600482	43.102260
3502.016543	838816.897083	43.107265
3501.891345	838797.606828	43.112269
3501.809689	838804.897225	43.117274
3501.703143	838783.275178	43.122279
3501.597671	838769.124594	43.127284
3501.897150	838753.843285	43.132289
3501.689569	838745.433689	43.137293
3501.356464	838741.507341	43.142298
3501.427721	838728.008281	43.147303
3501.672556	838724.961937	43.152308
3501.564325	838727.695896	43.157313
3501.581281	838729.245856	43.162317
3501.249820	838713.286785	43.167322
3501.602347	838699.452585	43.172327
3501.511553	838697.040909	43.177332
3501.530448	838692.089140	43.182337
3501.565083	838689.754891	43.187341
3501.369798	838689.979529	43.192346
3501.467377	838662.308873	43.197351
3501.565168	838665.689914	43.202356
3501.553458	838659.869571	43.207361
3501.747826	838668.572540	43.212365
3501.304059	838663.887145	43.217370
3501.432336	838629.904143	43.222375
3500.995377	838637.832509	43.227380
3501.300301	838630.895232	43.232385
3501.600320	838626.772800	43.237389
3501.384250	838637.965909	43.242394
3501.585750	838631.529987	43.247399
3501.282565	838618.477361	43.252404
3501.232571	838607.034770	43.257409
3501.500962	838597.094993	43.262413
3501.544686	838601.066750	43.267418
3501.808565	838599.278856	43.272423
3501.742831	838586.965346	43.277428
3501.585476	838569.911255	43.282433
3502.023704	838570.036866	43.287437
3501.343461	838574.898117	43.292442
3501.519013	838553.910407	43.297447
3501.923620	838546.957451	43.302452
3501.742464	838534.661875	43.307457
3501.932837	838521.628922	43.312461
3501.467401	838513.065227	43.317466
3501.873803	838499.901418	43.322471
3501.763289	838503.703271	43.327476
3501.571690	838494.805624	43.332481
3502.082773	838469.883584	43.337485
3501.416567	838471.152244	43.342490
3501.665671	838457.818851	43.347495
3501.942173	838443.898903	43.352500
3501.943145	838443.316546	43.357505
3501.958197	838430.310801	43.362509
3501.391472	838417.104847	43.367514
3501.483282	838409.715424	43.372519
3501.680021	838401.436220	43.377524
3501.722479	838400.071045	43.382529
3501.749379	838376.485837	43.387533
3501.616852	838368.355099	43.392538
3501.988237	838370.140873	43.397543
3502.240309	838363.987883	43.402548
3501.654782	838347.291210	43.407553
3502.153444	838349.833430	43.412557
3501.922928	838330.461082	43.417562
3501.946480	838314.445444	43.422567
3501.640865	838300.130945	43.427572
3501.694829	838287.992190	43.432577
3501.759189	838275.172484	43.437581
3501.265346	838285.827415	43.442586
3501.371823	838271.836602	43.447591
3501.663777	838265.483189	43.452596
3501.440992	838257.754582	43.457601
3501.426749	838237.765863	43.462605
3501.390508	838235.539559	43.467610
3501.289853	838232.741061	43.472615
3501.592988	838241.621740	43.477620
3501.069694	838228.117445	43.482625
3501.602399	838215.030310	43.487629
3501.087219	838205.406459	43.492634
3501.402495	838207.492187	43.497639
3501.359948	838220.502793	43.502644
3501.296892	838217.698410	43.507649
3501.419311	838219.037929	43.512653
3501.113415	838223.646854	43.517658
3501.182926	838213.640486	43.522663
3501.216723	838187.627348	43.527668
3501.149345	838185.599982	43.532673
3501.734327	838185.120396	43.537677
3501.583155	838192.422408	43.542682
3501.663306	838184.743396	43.547687
3501.558039	838187.671228	43.552692
3501.578092	838169.035541	43.557697
3501.805341	838165.312349	43.562701
3501.443960	838154.111653	43.567706
3501.671646	838151.261790	43.572711
3501.939500	838134.528162	43.577716
3501.689511	838126.997729	43.582721
3501.522592	838119.454300	43.587725
3501.172383	838106.893128	43.592730
3501.643738	838101.967187	43.597735
3501.672251	838095.266591	43.602740
3501.489354	838096.071589	43.607745
3501.747689	838085.259119	43.612749
3501.846300	838077.382991	43.617754
3501.768617	838065.361409	43.622759
3501.597912	838064.514712	43.627764
3501.684961	838056.155130	43.632769
3501.520072	838030.560552	43.637773
3501.715794	838027.812674	43.642778
3501.662258	838020.833679	43.647783
3501.398181	838012.625971	43.652788
3501.337740	837993.225938	43.657793
3501.519758	837981.163590	43.662797
3501.125647	837991.706405	43.667802
3501.543759	837985.721166	43.672807
3501.426540	837987.195246	43.677812
3501.453844	837990.781785	43.682817
3501.686964	837974.441330	43.687821
3501.631147	837972.023892	43.692826
3501.656015	837963.867996	43.697831
3501.524850	837957.386303	43.702836
3501.478013	837942.254103	43.707841
3501.873142	837923.656067	43.712845
3501.345152	837941.401511	43.717850
3501.482623	837928.375533	43.722855
3501.608582	837918.262797	43.727860
3501.686348	837902.237576	43.732865
3501.655155	837889.043780	43.737869
3501.306019	837883.954772	43.742874
3501.447291	837893.928820	43.747879
3501.735794	837884.858161	43.752884
3501.501204	837874.510563	43.757889
3501.684533	837860.700872	43.762893
3501.617448	837863.331744	43.767898
3501.320777	837859.107962	43.772903
3501.653820	837836.152110	43.777908
3501.605239	837829.754418	43.782913
3501.514396	837825.692538	43.787917
3501.155792	837829.921802	43.792922
3501.449540	837818.229861	43.797927
3501.653814	837819.362574	43.802932
3501.124351	837805.081874	43.807937
3501.754509	837799.936762	43.812941
3501.423011	837802.414891	43.817946
3501.454346	837805.806810	43.822951
3501.538822	837800.844050	43.827956
3501.405516	837786.404327	43.832961
3501.279741	837775.263137	43.837965
3501.312338	837776.131542	43.842970
3501.329731	837778.555142	43.847975
3501.631454	837781.516603	43.852980
3501.172915	837767.030622	43.857985
3501.672336	837738.322349	43.862989
3501.187279	837734.904342	43.867994
3501.482156	837744.563473	43.872999
3501.440814	837739.426226	43.878004
3501.415796	837738.362604	43.883009
3501.399376	837736.715326	43.888013
3501.344475	837721.098566	43.893018
3501.474130	837719.331396	43.898023
3501.154732	837728.213107	43.903028
3501.203793	837720.635410	43.908033
3501.862564	837715.971014	43.913037
3501.314212	837718.483077	43.918042
3501.736006	837691.145443	43.923047
3501.701272	837690.277437	43.928052
3501.765104	837688.132337	43.933057
3501.696702	837680.281793	43.938061
3501.395113	837652.668850	43.943066
3501.553724	837655.070426	43.948071
3501.567467	837644.683609	43.953076
3501.434803	837650.818747	43.958081
3501.447728	837656.057642	43.963085
3501.648884	837639.818323	43.968090
3501.409580	837625.782994	43.973095
3501.552887	837627.313490	43.978100
3501.469670	837621.988580	43.983105
3501.686374	837610.502385	43.988109
3501.314449	837593.284929	43.993114
3501.571279	837583.733494	43.998119
3501.550339	837576.263611	44.003124
3501.618451	837585.667284	44.008129
3501.924877	837570.478918	44.013133
3501.626060	837547.814841	44.018138
3501.720306	837553.041114	44.023143
3501.912383	837547.090774	44.028148
3501.654858	837524.905430	44.033153
3501.615794	837509.091528	44.038157
3501.199724	837517.212218	44.043162
3501.398945	837518.831057	44.048167
3501.349728	837503.212837	44.053172
3501.243437	837498.570814	44.058177
3501.479863	837486.110739	44.063181
3501.143554	837483.348724	44.068186
3501.180377	837485.381183	44.073191
3501.444934	837481.360567	44.078196
3501.386306	837492.434153	44.083201
3501.481907	837487.954673	44.088205
3501.495069	837481.352844	44.093210
3501.396836	837465.839245	44.098215
3501.517215	837467.761592	44.103220
3501.146169	837457.531655	44.108225
3501.404799	837454.870739	44.113229
3501.405677	837459.723463	44.118234
3501.439823	837449.624286	44.123239
3501.322888	837434.792926	44.128244
3501.355481	837427.799773	44.133249
3501.556305	837427.089019	44.138253
3501.287182	837428.975209	44.143258
3501.523374	837437.091102	44.148263
3501.665554	837416.395780	44.153268
3501.467784	837400.606399	44.158273
3501.534971	837404.866459	44.163277
3501.404149	837403.819316	44.168282
3501.785927	837401.430298	44.173287
3501.159737	837370.760954	44.178292
3501.184366	837369.204216	44.183297
3501.203213	837364.348410	44.188301
3501.369400	837365.584224	44.193306
3501.137001	837364.844127	44.198311
3501.522911	837369.927910	44.203316
3500.943324	837371.086186	44.208321
3501.449218	837367.901289	44.213325
3501.520437	837373.713667	44.218330
3501.410399	837355.581065	44.223335
3501.427494	837345.484377	44.228340
3501.179552	837348.726096	44.233345
3501.456687	837336.162287	44.238349
3501.448536	837356.448778	44.243354
3501.252757	837339.300110	44.248359
3501.217285	837318.049868	44.253364
3501.264165	837320.080811	44.258369
3501.226176	837317.854437	44.263373
3500.803450	837321.802904	44.268378
3500.554335	837308.156595	44.273383
3501.058779	837321.860126	44.278388
3501.374686	837324.431365	44.283393
3501.895101	837310.567710	44.288397
3501.628751	837322.644669	44.293402
3501.789543	837316.310756	44.298407
3501.655358	837290.514084	44.303412
3501.435106	837294.333858	44.308417
3501.389049	837284.635176	44.313421
3501.246425	837287.957524	44.318426
3501.569272	837274.027609	44.323431
3501.686924	837262.167991	44.328436
3501.169418	837261.569508	44.333441
3501.595499	837259.755867	44.338445
3501.323313	837255.527826	44.343450
3501.606572	837252.571792	44.348455
3501.655000	837240.140592	44.353460
3501.286381	837226.803958	44.358465
3501.491282	837217.939479	44.363469
3501.201030	837227.108557	44.368474
3501.756233	837226.730625	44.373479
3501.379791	837208.056857	44.378484
3501.151955	837198.192329	44.383489
3501.345827	837188.650106	44.388493
3501.594943	837200.646734	44.393498
3501.446970	837192.807986	44.398503
3501.864986	837187.889639	44.403508
3501.493792	837173.582679	44.408513
3501.745953	837150.636840	44.413517
3501.245406	837159.838894	44.418522
3501.304088	837157.500287	44.423527
3501.480768	837156.987399	44.428532
3501.397158	837141.955979	44.433537
3501.458504	837121.175209	44.438541
3501.659618	837119.008446	44.443546
3501.165337	837127.918383	44.448551
3501.438394	837121.760839	44.453556
3501.105195	837121.521777	44.458561
3501.631638	837116.586423	44.463565
3501.345607	837113.816374	44.468570
3501.452525	837105.064108	44.473575
3501.837651	837095.977152	44.478580
3501.388356	837109.344950	44.483585
3501.448251	837102.832459	44.488589
3501.504932	837079.140405	44.493594
3501.821561	837066.278668	44.498599
3501.338451	837070.333801	44.503604
3501.113924	837075.707386	44.508609
3501.646878	837074.362298	44.513613
3501.433126	837057.312691	44.518618
3501.355007	837046.162689	44.523623
3501.356900	837040.241575	44.528628
3501.239973	837042.880599	44.533633
3501.360543	837038.299817	44.538637
3501.397901	837039.264648	44.543642
3501.282142	837045.688953	44.548647
3501.469307	837026.829451	44.553652
3501.089028	837008.835102	44.558657
3501.449285	837007.516995	44.563661
3501.679260	837017.575708	44.568666
3501.220725	837007.455736	44.573671
3501.875176	837013.177295	44.578676
3501.810122	836994.260053	44.583681
3501.528989	836972.076341	44.588685
3501.452675	836976.553267	44.593690
3501.462247	836980.628508	44.598695
3500.995847	836980.119068	44.603700
3501.363339	836971.325873	44.608705
3501.502067	836942.670168	44.613709
3501.489482	836935.101111	44.618714
3501.450765	836934.330682	44.623719
3501.582802	836935.668989	44.628724
3501.241686	836936.401805	44.633729
3501.494098	836932.188592	44.638733
3501.914395	836923.581203	44.643738
3501.199753	836910.686211	44.648743
3501.526783	836909.373278	44.653748
3501.172307	836909.719923	44.658753
3501.614176	836909.553823	44.663757
3501.269603	836891.844735	44.668762
3501.300538	836868.058804	44.673767
3501.417271	836866.778735	44.678772
3501.345766	836869.507800	44.683777
3501.630535	836875.772611	44.688781
3501.416790	836873.573545	44.693786
3501.295093	836852.529257	44.698791
3501.500921	836854.050181	44.703796
3501.185404	836852.546480	44.708801
3501.634319	836856.650193	44.713805
3501.366359	836851.838805	44.718810
3501.357900	836836.018336	44.723815
3501.191124	836819.446039	44.728820
3501.143179	836822.268509	44.733825
3501.183256	836820.418013	44.738829
3501.458499	836815.133414	44.743834
3501.348954	836810.879631	44.748839
3501.526803	836817.646552	44.753844
3501.456852	836822.510866	44.758849
3501.366486	836797.384680	44.763853
3501.460338	836791.157743	44.768858
3501.292351	836784.001057	44.773863
3501.326841	836781.083680	44.778868
3500.968629	836788.905106	44.783873
3501.629924	836783.560132	44.788877
3501.128063	836788.394923	44.793882
3500.870357	836791.056063	44.798887
3501.226828	836798.183353	44.803892
3501.501295	836795.325537	44.808897
3501.519695	836766.881934	44.813901
3501.064226	836769.865201	44.818906
3500.851305	836761.647768	44.823911
3501.211899	836753.534807	44.828916
3501.148706	836770.240380	44.833921
3500.794229	836765.345378	44.838925
3501.398594	836769.813123	44.843930
3501.457325	836769.124507	44.848935
3501.326747	836770.212701	44.853940
3501.079583	836774.522350	44.858945
3501.461018	836767.570961	44.863949
3501.043773	836752.687782	44.868954
3500.843334	836739.614969	44.873959
3501.097791	836747.049471	44.878964
3500.944864	836740.375718	44.883969
3501.270435	836736.733342	44.888973
3500.737582	836741.475946	44.893978
3501.055139	836740.746867	44.898983
3501.427008	836745.930450	44.903988
3501.271265	836741.392635	44.908993
3501.038090	836743.079280	44.913997
3501.434638	836748.744344	44.919002
3501.082591	836748.605278	44.924007
3501.110380	836752.095419	44.929012
3500.651608	836753.817327	44.934017
3501.389366	836750.304661	44.939021
3500.810749	836747.774313	44.944026
3501.206515	836742.762014	44.949031
3501.414191	836751.951049	44.954036
3501.078032	836756.759962	44.959041
3501.569886	836752.800398	44.964045
3501.203211	836738.200481	44.969050
3501.302891	836728.186909	44.974055
3501.344567	836718.764798	44.979060
3501.112659	836727.537244	44.984065
3501.202237	836725.484844	44.989069
3501.041930	836727.451308	44.994074
3501.021672	836723.862984	44.999079
3501.523049	836723.590510	45.004084
3501.191845	836728.981081	45.009089
3501.469515	836719.716217	45.014093
3501.323630	836709.449795	45.019098
3501.148891	836700.061484	45.024103
3501.435793	836694.192545	45.029108
3500.958273	836705.430138	45.034113
3501.160937	836693.167829	45.039117
3501.403151	836698.857065	45.044122
3501.181390	836694.329534	45.049127
3501.336944	836708.089019	45.054132
3501.190965	836705.005679	45.059137
3501.088018	836678.813205	45.064141
3501.157484	836676.763932	45.069146
3501.079907	836679.396964	45.074151
3501.439335	836671.866490	45.079156
3500.974106	836684.752377	45.084161
3501.171481	836685.692252	45.089165
3500.923537	836684.566220	45.094170
3501.235606	836688.691442	45.099175
3501.917693	836681.110542	45.104180
3501.343208	836686.927457	45.109185
3501.654251	836677.366104	45.114189
3501.638848	836665.817311	45.119194
3501.355828	836657.901900	45.124199
3501.683876	836653.676670	45.129204
3501.447348	836651.578152	45.134209
3501.570828	836635.057039	45.139213
3501.585446	836623.794681	45.144218
3501.258171	836616.080273	45.149223
3501.912767	836620.637349	45.154228
3500.986670	836621.461645	45.159233
3501.100636	836623.967689	45.164237
3501.342455	836612.961005	45.169242
3501.065114	836592.813763	45.174247
3501.312133	836587.145095	45.179252
3501.107524	836593.777915	45.184257
3501.597291	836593.992604	45.189261
3501.176848	836597.747044	45.194266
3501.271723	836600.838504	45.199271
3501.343424	836596.944517	45.204276
3501.440968	836593.823052	45.209281
3501.308777	836569.284867	45.214285
3501.403263	836569.658419	45.219290
3501.085996	836563.786725	45.224295
3501.472434	836556.446026	45.229300
3501.248977	836564.052537	45.234305
3501.578580	836560.215282	45.239309
3501.566730	836565.167793	45.244314
3501.281423	836547.836703	45.249319
3501.639879	836537.005789	45.254324
3501.420114	836545.970745	45.259329
3501.636136	836529.726089	45.264333
3501.494628	836529.068747	45.269338
3501.574727	836512.748221	45.274343
3501.160935	836505.823769	45.279348
3501.504479	836499.460425	45.284353
3501.292678	836500.367220	45.289357
3501.546649	836507.025523	45.294362
3501.566175	836499.062607	45.299367
3501.604542	836472.652995	45.304372
3501.159511	836459.132440	45.309377
3501.615421	836463.235334	45.314381
3501.350865	836465.606470	45.319386
3501.516224	836462.377263	45.324391
3501.341480	836439.010067	45.329396
3501.369755	836444.150552	45.334401
3501.747789	836437.878825	45.339405
3501.445586	836442.973899	45.344410
3501.411385	836437.543196	45.349415
3501.543946	836412.477617	45.354420
3501.434208	836411.232854	45.359425
3501.539378	836405.100821	45.364429
3501.311984	836405.718846	45.369434
3501.411961	836412.595474	45.374439
3501.455242	836404.337498	45.379444
3501.111788	836390.509688	45.384449
3501.458974	836379.486105	45.389453
3501.358564	836381.443318	45.394458
3501.263400	836383.399711	45.399463
3501.270783	836380.486376	45.404468
3501.312902	836383.294975	45.409473
3501.509987	836387.438381	45.414477
3501.068260	836374.305412	45.419482
3501.193924	836353.414847	45.424487
3501.417675	836350.564749	45.429492
3501.408688	836348.915927	45.434497
3501.296469	836338.643604	45.439501
3501.421368	836349.884765	45.444506
3501.382893	836344.260496	45.449511
3501.639535	836350.821482	45.454516
3501.501030	836329.292606	45.459521
3501.375741	836312.809492	45.464525
3501.312398	836317.576108	45.469530
3501.176525	836318.762285	45.474535
3501.454148	836313.088575	45.479540
3501.179246	836316.043836	45.484545
3501.364954	836299.220845	45.489549
3501.410761	836289.409111	45.494554
3501.088447	836295.381132	45.499559
3501.286645	836292.923303	45.504564
3500.937223	836292.783813	45.509569
3501.439811	836284.842174	45.514573
3501.427331	836296.299063	45.519578
3501.535464	836287.739563	45.524583
3501.767761	836274.792237	45.529588
3501.237383	836274.583957	45.534593
3501.740503	836256.837547	45.539597
3501.670988	836257.333832	45.544602
3501.401712	836240.290570	45.549607
3501.450773	836230.089925	45.554612
3501.098290	836230.824598	45.559617
3501.372560	836223.112723	45.564621
3501.404478	836225.340531	45.569626
3501.466075	836223.292334	45.574631
3501.530879	836224.447159	45.579636
3501.432846	836218.152547	45.584641
3501.575955	836208.713777	45.589645
3501.462184	836205.042682	45.594650
3501.426187	836202.330196	45.599655
3501.532038	836199.207227	45.604660
3501.499729	836183.874146	45.609665
3501.476843	836168.054165	45.614669
3501.459548	836164.659196	45.619674
3501.354135	836167.005571	45.624679
3501.668874	836165.791480	45.629684
3501.330571	836153.903864	45.634689
3501.871822	836130.714771	45.639693
3501.610128	836122.115768	45.644698
3501.443070	836128.840309	45.649703
3501.663954	836122.107430	45.654708
3501.250061	836105.765937	45.659713
3501.487311	836086.410252	45.664717
3501.398123	836090.404459	45.669722
3501.331327	836086.337633	45.674727
3501.254427	836081.495753	45.679732
3501.405993	836084.869856	45.684737
3501.384230	836083.417115	45.689741
3501.245581	836063.925959	45.694746
3501.292602	836056.055235	45.699751
3501.359300	836054.297421	45.704756
3501.360856	836057.792067	45.709761
3501.338800	836052.553274	45.714765
3501.245291	836061.693375	45.719770
3501.336328	836064.591556	45.724775
3501.339338	836056.436475	45.729780
3501.510086	836041.556682	45.734785
3501.533790	836033.980812	45.739789
3501.513630	836033.692763	45.744794
3501.439646	836033.510207	45.749799
3501.659803	836031.728397	45.754804
3501.454745	836005.160616	45.759809
3501.187758	836002.775387	45.764813
3501.433463	835989.242869	45.769818
3501.392587	835926.340927	45.774823
3501.366172	835817.904270	45.779828
3501.389587	835671.885907	45.784833
3500.764368	835456.547188	45.789837
3500.831236	835210.508344	45.794842
3499.975305	834899.645474	45.799847
3500.062514	834545.602273	45.804852
3499.434857	834159.409534	45.809857
3499.312848	833707.073560	45.814861
3498.899485	833219.298546	45.819866
3498.266814	832681.397460	45.824871
3498.119018	832086.543950	45.829876
3497.278301	831457.639335	45.834881
3496.535852	830763.359578	45.839885
3496.127075	830043.487856	45.844890
3495.631696	829266.008719	45.849895
3494.993668	828437.227061	45.854900
3493.602793	827561.397748	45.859905
3493.227824	826645.419220	45.864909
3492.205929	825679.517340	45.869914
3491.386513	824665.383893	45.874919
3490.585919	823609.249842	45.879924
3489.521704	822503.354364	45.884929
3488.479255	821353.076057	45.889933
3487.808316	820156.583930	45.894938
3486.445540	818899.512398	45.899943
3485.230589	817626.583070	45.904948
3483.679976	816298.515540	45.909953
3482.832867	814924.659562	45.914957
3481.509451	813505.072881	45.919962
3480.095174	812036.448901	45.924967
3478.890411	810523.873990	45.929972
3477.525207	808993.897558	45.934977
3476.116002	807395.481095	45.939981
3474.777272	805775.920257	45.944986
3473.132076	804093.591792	45.949991
3471.860485	802387.043190	45.954996
3469.977128	800635.663518	45.960001
3468.783297	798827.006713	45.965005
3466.784822	797006.148932	45.970010
3465.186699	795130.288609	45.975015
3463.611755	793198.510829	45.980020
3461.698046	791250.277736	45.985025
3459.627227	789242.220937	45.990029
3457.833341	787223.187520	45.995034
3456.241164	785159.173672	46.000039
3454.629988	783057.174614	46.005044
3452.361194	780927.050243	46.010049
3450.648007	778753.011685	46.015053
3448.257606	776551.626295	46.020058
3446.016892	774317.546350	46.025063
3444.059958	772028.169408	46.030068
3441.896035	769736.832500	46.035073
3439.769208	767396.744177	46.040077
3437.573396	765026.918050	46.045082
3434.887881	762621.060560	46.050087
3432.698366	760200.397768	46.055092
3430.195904	757744.165701	46.060097
3427.757741	755245.097636	46.065101
3425.335323	752737.379132	46.070106
3423.169221	750207.394646	46.075111
3420.592972	747630.925941	46.080116
3418.198748	745026.095456	46.085121
3415.230559	742398.363137	46.090125
3412.754401	739744.440501	46.095130
3410.284724	737074.185910	46.100135
3407.911653	734356.768752	46.105140
3404.852018	731632.894423	46.110145
3402.157479	728867.525738	46.115149
3399.714045	726097.253612	46.120154
3396.844598	723290.545377	46.125159
3394.366799	720450.350742	46.130164
3391.241318	717598.586442	46.135169
3388.488285	714723.771318	46.140173
3385.388427	711823.725848	46.145178
3382.632866	708900.991956	46.150183
3380.116314	705970.409881	46.155188
3376.847819	702992.295344	46.160193
3374.021184	700007.755283	46.165197
3370.972622	697012.090722	46.170202
3368.020023	693987.164413	46.175207
3365.293185	690931.940843	46.180212
3362.383167	687873.728451	46.185217
3359.075379	684779.632492	46.190221
3356.071551	681665.687674	46.195226
3353.181599	678536.427824	46.200231
3350.103902	675392.389047	46.205236
3346.709089	672236.416003	46.210241
3343.533459	669050.184732	46.215245
3340.969811	665843.750919	46.220250
3337.224478	662637.422842	46.225255
3334.067855	659391.933371	46.230260
3330.960908	656145.104630	46.235265
3327.750527	652880.890018	46.240269
3324.642289	649606.469799	46.245274
3321.205345	646312.844089	46.250279
3317.997049	643001.410685	46.255284
3314.644069	639680.894001	46.260289
3311.504143	636332.687467	46.265293
3308.372096	632977.657905	46.270298
3304.697346	629615.845355	46.275303
3301.445145	626240.463086	46.280308
3297.778830	622844.797208	46.285313
3294.384804	619439.171687	46.290317
3291.270621	616023.286685	46.295322
3287.785688	612600.844327	46.300327
3284.415667	609162.721968	46.305332
3281.009676	605716.442765	46.310337
3277.692885	602252.632809	46.315341
3274.207511	598780.487433	46.320346
3270.528400	595304.070261	46.325351
3266.906056	591799.055471	46.330356
3263.611900	588304.869643	46.335361
3260.014313	584806.697284	46.340365
3256.466780	581275.009082	46.345370
3252.843889	577745.014226	46.350375
3249.320543	574212.585242	46.355380
3245.618182	570666.583991	46.360385
3241.915036	567121.541110	46.365389
3238.598296	563569.424684	46.370394
3234.610877	560001.665409	46.375399
3231.427020	556430.392121	46.380404
3227.503142	552860.027531	46.385409
3224.101818	549263.337874	46.390413
3219.940287	545680.093679	46.395418
3216.297603	542108.459074	46.400423
3212.935722	538511.306230	46.405428
3209.382651	534921.518732	46.410433
3205.534333	531304.642074	46.415437
3202.234153	527703.494682	46.420442
3198.271251	524085.949338	46.425447
3194.732473	520452.893581	46.430452
3190.750928	516832.185796	46.435457
3187.242668	513203.185325	46.440461
3183.612892	509575.775067	46.445466
3179.358778	505933.048075	46.450471
3176.179653	502298.302895	46.455476
3172.307873	498662.750436	46.460481
3168.585317	495007.340499	46.465485
3164.769699	491365.586753	46.470490
3160.791591	487720.199188	46.475495
3157.319929	484061.080756	46.480500
3153.475103	480412.272874	46.485505
3149.833609	476757.481492	46.490509
3146.484278	473096.094771	46.495514
3142.216976	469439.080547	46.500519
3138.812552	465774.998769	46.505524
3134.646772	462115.291293	46.510529
3130.982765	458452.793697	46.515533
3127.289446	454786.385448	46.520538
3123.185672	451116.946344	46.525543
3119.360381	447453.391486	46.530548
3115.446474	443795.541407	46.535553
3111.844591	440127.901534	46.540557
3107.968076	436475.190759	46.545562
3104.011012	432807.708163	46.550567
3100.215480	429144.475027	46.555572
3096.356389	425486.555278	46.560577
3092.300745	421820.905488	46.565581
3089.082549	418173.181348	46.570586
3085.224063	414523.603800	46.575591
3081.092026	410861.627284	46.580596
3077.051830	407212.464866	46.585601
3073.617144	403556.672549	46.590605
3069.987138	399902.910299	46.595610
3065.510078	396265.200254	46.600615
3061.794396	392604.629137	46.605620
3057.597399	388970.640644	46.610625
3053.731640	385330.075239	46.615629
3049.925066	381698.702742	46.620634
3045.952986	378058.644627	46.625639
3042.657186	374432.307091	46.630644
3038.705620	370816.283378	46.635649
3034.751051	367185.640141	46.640653
3030.991513	363572.292185	46.645658
3026.542208	359953.728340	46.650663
3022.813104	356334.134865	46.655668
3018.911384	352725.355266	46.660673
3015.223858	349112.930719	46.665677
3011.456531	345520.053412	46.670682
3007.649297	341926.215778	46.675687
3003.728104	338324.396761	46.680692
2999.612632	334740.176816	46.685697
2995.321900	331148.618808	46.690701
2991.730473	327564.399292	46.695706
2987.319192	323985.378045	46.700711
2983.766920	320414.027366	46.705716
2979.529478	316860.906313	46.710721
2974.858957	313304.668227	46.715725
2971.499865	309756.450781	46.720730
2967.023538	306221.125575	46.725735
2963.542347	302695.449119	46.730740
2959.227607	299185.217808	46.735745
2955.217070	295666.315590	46.740749
2951.571310	292169.135410	46.745754
2947.367841	288678.612932	46.750759
2943.534797	285184.558729	46.755764
2939.223454	281705.675110	46.760769
2935.409643	278235.584292	46.765773
2931.339476	274769.756232	46.770778
2927.114824	271318.778115	46.775783
2923.255240	267867.047922	46.780788
2918.878874	264444.863210	46.785793
2914.651423	261016.965528	46.790797
2911.040204	257605.038877	46.795802
2906.637432	254206.997074	46.800807
2902.912798	250806.449396	46.805812
2898.615981	247424.433253	46.810817
2894.571642	244047.255832	46.815821
2890.605151	240694.946729	46.820826
2886.274800	237345.223874	46.825831
2882.056334	234005.433566	46.830836
2877.991614	230687.625445	46.835841
2873.854524	227369.431436	46.840845
2869.346844	224069.117481	46.845850
2864.838670	220784.062147	46.850855
2860.990216	217500.774123	46.855860
2856.863470	214262.374422	46.860865
2852.546102	211009.362364	46.865869
2848.871307	207789.674857	46.870874
2844.149518	204569.507206	46.875879
2840.074419	201369.180315	46.880884
2835.893087	198187.469180	46.885889
2832.159026	195001.221592	46.890893
2827.687619	191857.895236	46.895898
2823.285759	188708.119176	46.900903
2818.889750	185567.852133	46.905908
2814.741950	182463.341198	46.910913
2810.712937	179361.789346	46.915917
2806.536036	176287.332019	46.920922
2801.978854	173215.618453	46.925927
2798.342976	170156.393885	46.930932
2793.784974	167033.843663	46.935937
2789.505772	164006.777291	46.940941
2785.719511	161008.905429	46.945946
2781.304223	158028.314979	46.950951
2777.136528	155048.900612	46.955956
2772.811851	152093.079201	46.960961
2768.495298	149149.158275	46.965965
2764.528631	146226.288814	46.970970
2760.196913	143315.894693	46.975975
2756.342041	140404.056038	46.980980
2752.133550	137539.280380	46.985985
2748.056733	134658.554278	46.990989
2744.081623	131811.350499	46.995994
2740.042302	128970.155107	47.000999
2735.848059	126149.346848	47.006004
2731.510495	123337.059051	47.011009
2727.069852	120544.175353	47.016013
2722.908877	117762.969061	47.021018
2718.888889	115002.810663	47.026023
2714.967870	112247.674041	47.031028
2710.683470	109523.622423	47.036033
2706.431703	106800.704108	47.041037
2702.480807	104097.415591	47.046042
2698.280715	101419.575659	47.051047
2694.206093	98738.972431	47.056052
2689.866541	96082.271545	47.061057
2685.947985	93433.645200	47.066061
2681.699408	90815.602172	47.071066
2677.349885	88205.779981	47.076071
2673.385476	85603.545911	47.081076
2668.881296	83036.599989	47.086081
2664.451156	80465.376101	47.091085
2660.760630	77928.411312	47.096090
2656.589714	75408.899059	47.101095
2652.265605	72895.155610	47.106100
2648.022862	70402.446818	47.111105
2643.680468	67920.616724	47.116109
2639.449720	65465.336492	47.121114
2635.273266	63026.951364	47.126119
2631.611031	60600.317556	47.131124
2627.006178	58202.789720	47.136129
2622.841903	55805.175538	47.141133
2618.758075	53440.810613	47.146138
2614.391093	51093.537195	47.151143
2610.195582	48750.488458	47.156148
2605.730533	46441.671341	47.161153
2601.512965	44131.972342	47.166157
2597.173570	41852.333632	47.171162
2592.833771	39592.902332	47.176167
2588.677363	37345.100380	47.181172
2584.191497	35124.512722	47.186177
2579.973374	32923.301039	47.191181
2575.993547	30741.213090	47.196186
2571.221185	28584.211592	47.201191
2566.937369	26436.078654	47.206196
2562.397880	24322.387663	47.211201
2557.758799	22222.168188	47.216205
2553.145091	20158.411987	47.221210
2548.474235	18129.286025	47.226215
2543.734980	16112.107530	47.231220
2539.547219	14125.477840	47.236225
2534.851046	12165.227445	47.241229
2529.932321	10230.650170	47.246234
2525.321519	8334.014294	47.251239
2520.384469	6474.067276	47.256244
2514.726165	4648.405767	47.261249
2508.944549	2858.620544	47.266253
2499.211054	1227.035041	47.271258
2477.171012	-4.619131	47.276263
2413.867199	45.433075	47.281268
2368.525262	147.540222	47.286273
2351.363393	180.734298	47.291277
2353.450194	204.851955	47.296282
2364.770672	224.405516	47.301287
2379.017483	237.502592	47.306292
2390.669525	240.102882	47.311297
2396.496051	229.816836	47.316301
2398.191896	229.921750	47.321306
2397.006178	219.675969	47.326311
2393.943541	209.869357	47.331316
2389.663021	207.802287	47.336321
2385.574640	204.591476	47.341325
2382.414250	203.042064	47.346330
2378.802237	201.715172	47.351335
2376.335575	194.479324	47.356340
2373.398532	197.182025	47.361345
2370.638860	189.087152	47.366349
2368.055919	184.486024	47.371354
2364.758079	183.087842	47.376359
2362.094216	178.964466	47.381364
2358.919346	172.326662	47.386369
2355.865906	162.569274	47.391373
2352.506371	162.506410	47.396378
2348.894222	167.659156	47.401383
2345.835240	158.848638	47.406388
2342.887381	161.435971	47.411393
2339.048065	162.821289	47.416397
2335.990671	162.401102	47.421402
2332.430223	171.487945	47.426407
2329.241729	153.032079	47.431412
2326.145820	167.408999	47.436417
2323.104899	163.056716	47.441421
2320.057101	158.651724	47.446426
2315.754951	162.827220	47.451431
2312.917405	169.579936	47.456436
2309.686557	171.300357	47.461441
2306.202975	173.357722	47.466445
2303.010863	169.858030	47.471450
2299.533668	168.035496	47.476455
2296.721904	173.996380	47.481460
2292.724548	165.848394	47.486465
2289.426254	179.804559	47.491469
2286.083853	170.971955	47.496474
2282.273049	178.974808	47.501479
2279.322287	175.209565	47.506484
2275.786305	182.359475	47.511489
2272.103277	172.991686	47.516493
2269.347416	174.615659	47.521498
2265.542651	185.449237	47.526503
2262.036436	172.140084	47.531508
2258.839626	174.567064	47.536513
2254.925574	185.205763	47.541517
2251.433868	169.692294	47.546522
2248.547085	176.800753	47.551527
2245.736841	178.009283	47.556532
2241.712956	181.850197	47.561537
2237.817036	180.710147	47.566541
2234.726778	176.852842	47.571546
2231.015600	180.496133	47.576551
2227.583815	180.855913	47.581556
2224.730941	178.056170	47.586561
2220.836993	178.358541	47.591565
2217.796691	169.659039	47.596570
2213.998553	168.187313	47.601575
2210.692724	167.942077	47.606580
2207.241124	176.474065	47.611585
2204.017052	174.311392	47.616589
2200.231281	169.851047	47.621594
2196.539824	179.923403	47.626599
2193.625764	169.739287	47.631604
2189.592795	178.077492	47.636609
2186.002860	175.041890	47.641613
2183.285636	176.637691	47.646618
2179.224780	179.104965	47.651623
2176.006493	168.813426	47.656628
2172.519202	169.590046	47.661633
2169.072920	169.575612	47.666637
2165.932537	171.212314	47.671642
2161.968193	175.632417	47.676647
2158.942672	170.265336	47.681652
2155.258400	171.287925	47.686657
2151.464047	175.298606	47.691661
2148.324657	171.559752	47.696666
2144.716748	175.924092	47.701671
2141.148145	169.025255	47.706676
2137.984775	171.478674	47.711681
2134.120511	181.040226	47.716685
2130.792474	161.312254	47.721690
2127.618454	168.459350	47.726695
2123.845422	175.905823	47.731700
2120.445854	169.024840	47.736705
2116.799503	174.018484	47.741709
2114.133343	173.676355	47.746714
2110.262924	173.854857	47.751719
2106.654368	171.252483	47.756724
2102.807990	173.923514	47.761729
2099.346327	170.918495	47.766733
2095.973531	165.472891	47.771738
2092.296939	173.676265	47.776743
2089.146138	171.511656	47.781748
2085.606146	176.880986	47.786753
2082.528743	172.069396	47.791757
2079.129077	168.431403	47.796762
2075.481128	176.725217	47.801767
2071.815057	168.057240	47.806772
2067.909274	170.690119	47.811777
2064.059564	171.877834	47.816781
2060.929832	170.459771	47.821786
2057.287545	171.516953	47.826791
2054.744471	174.034694	47.831796
2051.044672	168.504225	47.836801
2047.328595	175.717174	47.841805
2043.787928	169.513217	47.846810
2039.982811	173.851496	47.851815
2036.937941	170.746480	47.856820
2033.323554	165.373503	47.861825
2030.138861	180.276917	47.866829
2026.907165	162.707492	47.871834
2022.769397	181.006157	47.876839
2019.539592	179.382295	47.881844
2015.629427	175.783072	47.886849
2012.009310	176.957026	47.891853
2008.665427	172.788291	47.896858
2005.443594	179.053855	47.901863
2002.039034	168.152431	47.906868
1998.585319	173.318453	47.911873
1994.773604	171.225652	47.916877
1991.586260	176.542991	47.921882
1987.757802	173.946594	47.926887
1984.484524	175.819283	47.931892
1981.143843	163.509449	47.936897
1977.680507	176.893524	47.941901
1974.242215	173.669749	47.946906
1970.478348	180.327033	47.951911
1967.130074	168.477149	47.956916
1963.494787	170.434965	47.961921
1960.066555	171.816200	47.966925
1956.912322	166.551588	47.971930
1953.210104	172.721485	47.976935
1949.685320	171.241883	47.981940
1945.848111	169.890269	47.986945
1942.326321	172.200503	47.991949
1939.271502	157.552162	47.996954
1935.530296	169.518021	48.001959
1932.179779	169.320993	48.006964
1928.501229	167.144102	48.011969
1925.160570	163.917723	48.016973
1921.771930	163.172990	48.021978
1918.236840	170.351325	48.026983
1914.445563	166.651280	48.031988
1911.107443	171.786582	48.036993
1907.605840	166.500413	48.041997
1904.381120	157.333162	48.047002
1900.496610	162.974759	48.052007
1897.231581	163.159847	48.057012
1893.930997	161.778064	48.062017
1890.308320	164.410996	48.067021
1886.520882	160.963471	48.072026
1882.949504	171.279711	48.077031
1879.632159	161.845379	48.082036
1875.864763	162.444456	48.087041
1872.277169	169.165932	48.092045
1869.355642	161.979279	48.097050
1865.748159	166.248717	48.102055
1862.458326	162.970113	48.107060
1858.819326	164.238824	48.112065
1855.244306	168.044427	48.117069
1852.115072	160.940905	48.122074
1848.384647	160.040868	48.127079
1844.435397	162.512941	48.132084
1841.308759	161.796838	48.137089
1837.801682	162.402649	48.142093
1834.294059	151.656644	48.147098
1830.437795	160.103342	48.152103
1826.731630	156.488095	48.157108
1823.746337	159.429439	48.162113
1820.381363	155.732325	48.167117
1817.069549	164.913266	48.172122
1813.308320	157.570129	48.177127
1809.684951	154.815155	48.182132
1806.282292	161.548836	48.187137
1802.652641	152.546240	48.192141
1799.449424	155.100901	48.197146
1795.911608	159.248723	48.202151
1792.184218	157.291504	48.207156
1788.337408	152.261894	48.212161
1785.149179	159.047447	48.217165
1781.466868	149.578525	48.222170
1778.362255	151.703296	48.227175
1774.711521	159.415472	48.232180
1771.286531	156.518731	48.237185
1767.601853	155.731790	48.242189
1764.404542	151.432638	48.247194
1760.728139	154.684641	48.252199
1757.281360	147.330289	48.257204
1753.696006	151.858895	48.262209
1750.484211	160.932445	48.267213
1746.876637	155.583828	48.272218
1743.325650	154.500719	48.277223
1739.526877	153.446898	48.282228
1736.135415	158.226749	48.287233
1732.768053	149.980426	48.292237
1729.396137	144.022283	48.297242
1725.810808	157.672270	48.302247
1722.369937	159.125161	48.307252
1718.869250	156.958479	48.312257
1715.038447	151.591026	48.317261
1711.826476	151.805835	48.322266
1708.058435	151.886202	48.327271
1704.656923	150.944233	48.332276
1701.563386	151.789098	48.337281
1697.858455	154.128071	48.342285
1693.962747	143.869987	48.347290
1690.478520	151.277706	48.352295
1687.370835	148.809077	48.357300
1684.182141	143.996063	48.362305
1680.461292	156.711788	48.367309
1676.529216	151.458280	48.372314
1672.895431	155.627486	48.377319
1669.671777	152.367068	48.382324
1666.118008	146.038764	48.387329
1662.804895	150.107163	48.392333
1659.348344	152.524337	48.397338
1655.573955	152.469671	48.402343
1652.180982	152.159153	48.407348
1649.000513	144.079775	48.412353
1645.241973	152.504903	48.417357
1641.862922	151.511983	48.422362
1638.271394	148.087682	48.427367
1634.511687	154.905764	48.432372
1631.846110	143.009304	48.437377
1627.841277	143.610829	48.442381
1624.144695	137.909191	48.447386
1620.408731	156.154531	48.452391
1617.014558	148.564204	48.457396
1613.921677	144.622095	48.462401
1610.177417	144.781036	48.467405
1606.738077	135.277334	48.472410
1603.251443	145.630989	48.477415
1599.754062	142.555811	48.482420
1596.279434	152.923412	48.487425
1592.583276	148.784657	48.492429
1589.265965	141.941636	48.497434
1585.562679	147.982086	48.502439
1582.307821	149.254044	48.507444
1579.117834	142.868839	48.512449
1575.429585	149.039820	48.517453
1571.925435	144.858366	48.522458
1567.577550	155.201298	48.527463
1564.248300	150.970324	48.532468
1561.297218	144.835642	48.537473
1557.848902	145.808847	48.542477
1554.715034	144.277694	48.547482
1550.606763	155.320304	48.552487
1547.563046	157.517870	48.557492
1543.548072	147.025415	48.562497
1539.805419	154.704585	48.567501
1536.559491	146.894929	48.572506
1532.815427	157.646415	48.577511
1529.884991	149.164103	48.582516
1526.777416	146.483532	48.587521
1523.368793	156.999015	48.592525
1519.309857	148.873679	48.597530
1515.249980	157.924997	48.602535
1511.556638	155.779053	48.607540
1508.362503	157.256671	48.612545
1505.192145	152.358588	48.617549
1501.954776	150.992352	48.622554
1498.363344	149.156339	48.627559
1494.736778	148.094641	48.632564
1491.654517	145.558820	48.637569
1487.675730	151.322876	48.642573
1484.115918	143.378870	48.647578
1480.318641	155.211240	48.652583
1477.060743	156.765289	48.657588
1473.651865	144.766926	48.662593
1470.440710	142.105752	48.667597
1466.869219	144.705498	48.672602
1463.537867	141.411390	48.677607
1459.643175	140.878905	48.682612
1456.037691	152.178209	48.687617
1452.555435	145.832470	48.692621
1449.368161	141.883046	48.697626
1445.403188	136.331064	48.702631
1441.986503	140.124664	48.707636
1438.642926	139.597674	48.712641
1435.233196	137.913583	48.717645
1432.058747	136.078767	48.722650
1428.305355	148.489589	48.727655
1424.528751	139.165308	48.732660
1421.288675	135.780996	48.737665
1417.611635	141.105525	48.742669
1414.195670	136.157337	48.747674
1409.998876	143.496331	48.752679
1406.962172	130.588678	48.757684
1404.056878	133.716930	48.762689
1399.903794	143.510551	48.767693
1396.693755	131.386192	48.772698
1392.964046	144.815232	48.777703
1389.548526	141.951952	48.782708
1386.334790	137.111328	48.787713
1382.535795	145.144220	48.792717
1379.245963	137.139017	48.797722
1375.580093	142.787687	48.802727
1371.814992	137.441738	48.807732
1368.347421	139.987283	48.812737
1365.275872	146.568008	48.817741
1361.807406	132.974965	48.822746
1358.145877	147.842381	48.827751
1355.031043	145.802099	48.832756
1351.259866	136.072033	48.837761
1347.437786	141.868553	48.842765
1344.285654	136.974008	48.847770
1340.290906	146.167046	48.852775
1336.799665	140.509316	48.857780
1333.382496	137.611513	48.862785
1329.967075	144.290369	48.867789
1326.504311	137.761294	48.872794
1323.418588	141.094988	48.877799
1319.619950	138.190465	48.882804
1316.264834	136.608602	48.887809
1312.774262	131.719591	48.892813
1309.071179	139.408452	48.897818
1305.446000	140.029768	48.902823
1301.859276	144.647316	48.907828
1298.759806	144.246680	48.912833
1294.831858	138.660494	48.917837
1291.667379	137.602468	48.922842
1287.724466	144.076002	48.927847
1284.422764	136.480831	48.932852
1280.881439	141.739865	48.937857
1277.631412	138.135693	48.942861
1274.095165	133.902434	48.947866
1270.463620	146.756141	48.952871
1266.797289	141.628898	48.957876
1263.728731	132.285605	48.962881
1260.272623	145.330155	48.967885
1256.758032	134.661437	48.972890
1252.964400	137.587102	48.977895
1249.528334	135.094097	48.982900
1245.966299	139.350284	48.987905
1242.549992	139.894631	48.992909
1239.085050	136.336774	48.997914
1235.367195	131.733318	49.002919
1232.140255	123.550652	49.007924
1228.508052	137.037233	49.012929
1224.922386	140.917467	49.017933
1221.267330	136.886330	49.022938
1218.252704	138.057517	49.027943
1214.606379	133.208747	49.032948
1211.180293	129.309454	49.037953
1207.363571	136.914892	49.042957
1203.807449	136.848374	49.047962
1200.278916	133.540939	49.052967
1197.193719	136.577185	49.057972
1193.699019	134.049086	49.062977
1190.136926	141.216026	49.067981
1186.791466	129.717252	49.072986
1183.152469	138.962214	49.077991
1179.330156	133.748696	49.082996
1175.794707	130.866307	49.088001
1172.251216	141.168860	49.093005
1168.967791	129.220609	49.098010
1165.328933	137.522733	49.103015
1162.113577	130.388671	49.108020
1158.632178	131.376682	49.113025
1154.662932	127.401090	49.118029
1151.140541	132.492680	49.123034
1147.746960	132.176103	49.128039
1144.547834	131.120387	49.133044
1140.998670	129.673374	49.138049
1137.467206	138.271912	49.143053
1134.279616	137.774390	49.148058
1130.675066	133.074144	49.153063
1127.064787	144.706484	49.158068
1123.481819	135.076776	49.163073
1119.717052	146.046755	49.168077
1116.431602	135.949682	49.173082
1112.726722	140.911665	49.178087
1109.525123	135.968001	49.183092
1105.963480	139.977395	49.188097
1102.142413	130.403961	49.193101
1098.877294	134.585235	49.198106
1095.370398	135.200765	49.203111
1092.112381	134.458014	49.208116
1088.761220	132.385220	49.213121
1084.837896	138.526719	49.218125
1081.557931	132.389917	49.223130
1077.711630	131.476678	49.228135
1074.249867	133.170342	49.233140
1070.857579	131.088175	49.238145
1066.901538	153.297563	49.243149
1063.903854	136.770847	49.248154
1060.504308	130.133910	49.253159
1057.094863	136.935296	49.258164
1053.688607	137.905252	49.263169
1049.608023	134.592558	49.268173
1046.139622	133.686605	49.273178
1042.514931	139.154925	49.278183
1039.136455	129.056634	49.283188
1036.661171	127.273842	49.288193
1032.079649	129.076399	49.293197
1028.977236	118.542582	49.298202
1025.638586	129.328800	49.303207
1022.052432	128.767168	49.308212
1018.708677	124.105233	49.313217
1014.524969	127.417933	49.318221
1011.120495	127.106275	49.323226
1007.481275	134.405570	49.328231
1004.206567	129.732829	49.333236
1001.067928	121.327620	49.338241
997.396368	133.276474	49.343245
993.983663	118.080320	49.348250
989.970467	123.429145	49.353255
986.447302	131.855578	49.358260
983.788051	117.139421	49.363265
979.617149	127.758561	49.368269
976.426123	128.707499	49.373274
972.774274	134.901444	49.378279
969.201006	136.739157	49.383284
965.886384	126.868189	49.388289
962.069376	125.210077	49.393293
958.746576	123.303738	49.398298
955.273885	129.327264	49.403303
951.689564	131.891228	49.408308
948.452116	123.492019	49.413313
944.713730	130.838499	49.418317
941.635480	129.412741	49.423322
937.788115	133.751674	49.428327
934.487554	136.888159	49.433332
931.004946	139.426714	49.438337
927.048759	140.175932	49.443341
924.001006	130.895958	49.448346
920.159720	139.698100	49.453351
916.571088	133.150941	49.458356
913.050867	130.471920	49.463361
909.460443	135.520457	49.468365
906.182261	131.038126	49.473370
902.649480	127.968762	49.478375
899.320689	130.935669	49.483380
896.102220	129.364200	49.488385
892.271016	137.165004	49.493389
888.782491	125.824813	49.498394
885.202107	130.191563	49.503399
881.720259	128.158293	49.508404
878.551850	124.022626	49.513409
874.467754	134.330814	49.518413
871.261783	122.348427	49.523418
867.359899	123.728257	49.528423
863.925728	123.513054	49.533428
860.611673	119.400201	49.538433
857.106148	122.894678	49.543437
853.661047	122.472377	49.548442
850.006173	131.802182	49.553447
846.721430	129.434334	49.558452
843.439694	131.504857	49.563457
840.286143	134.194401	49.568461
836.268978	118.210272	49.573466
832.515399	127.318249	49.578471
828.889598	134.431999	49.583476
825.688219	131.949862	49.588481
821.838656	115.778143	49.593485
818.714933	119.820299	49.598490
815.248557	118.439544	49.603495
811.692329	118.034662	49.608500
808.317846	120.135538	49.613505
804.668416	121.077220	49.618509
801.453123	115.303740	49.623514
797.588113	122.331566	49.628519
793.961611	119.602797	49.633524
790.891589	121.817357	49.638529
786.979554	130.225650	49.643533
783.466002	129.057942	49.648538
779.864510	129.814953	49.653543
776.354697	130.035579	49.658548
773.534347	125.060818	49.663553
769.860124	130.312353	49.668557
765.967382	117.323899	49.673562
762.647840	128.262220	49.678567
759.026762	120.682484	49.683572
755.788695	128.738467	49.688577
752.084665	125.749767	49.693581
748.869073	121.820858	49.698586
744.976172	120.731555	49.703591
741.609348	113.624552	49.708596
738.087624	123.920646	49.713601
734.299386	131.040880	49.718605
730.880959	127.555037	49.723610
727.378444	127.809341	49.728615
724.444535	127.329182	49.733620
720.850825	123.677800	49.738625
717.000348	126.267711	49.743629
713.414103	124.320460	49.748634
709.959546	125.320248	49.753639
706.236379	126.112161	49.758644
703.190735	126.174701	49.763649
699.788321	124.888379	49.768653
696.055697	114.820402	49.773658
692.577913	116.355354	49.778663
689.117410	129.533603	49.783668
685.731179	120.904702	49.788673
681.632694	124.289617	49.793677
678.623716	109.476499	49.798682
675.056214	115.771227	49.803687
671.633843	126.067601	49.808692
668.399713	110.973366	49.813697
664.334469	119.206370	49.818701
660.725167	120.040582	49.823706
657.529048	111.094017	49.828711
653.952866	114.400309	49.833716
650.910228	107.884831	49.838721
647.073755	114.427338	49.843725
643.624284	115.287146	49.848730
639.610979	114.083865	49.853735
636.538382	114.100027	49.858740
633.019726	111.604378	49.863745
629.522309	117.992551	49.868749
625.962281	111.516982	49.873754
622.422828	121.281201	49.878759
618.968616	117.832648	49.883764
615.360715	113.193263	49.888769
611.635022	121.256048	49.893773
608.491938	109.839754	49.898778
604.909269	113.232502	49.903783
601.415286	112.441459	49.908788
597.541259	108.596750	49.913793
594.356466	120.346089	49.918797
591.000978	117.147846	49.923802
587.680248	113.422132	49.928807
583.840735	119.857571	49.933812
580.848577	115.241990	49.938817
577.058862	115.750143	49.943821
573.413984	112.540283	49.948826
569.859794	108.870124	49.953831
566.465080	117.371476	49.958836
562.829273	114.482908	49.963841
559.200598	117.693051	49.968845
555.862270	112.777350	49.973850
552.287447	118.718919	49.978855
548.946582	119.966720	49.983860
545.575985	114.084787	49.988865
541.979677	116.451457	49.993869
538.513730	112.144220	49.998874
534.740844	116.750050	50.003879
531.437447	115.951332	50.008884
528.090401	109.603803	50.013889
524.184066	114.695619	50.018893
520.840024	115.064388	50.023898
517.422447	112.432730	50.028903
513.294975	116.135472	50.033908
510.430343	111.604349	50.038913
506.968241	113.611484	50.043917
503.489468	104.763045	50.048922
499.953118	114.374949	50.053927
496.429495	117.590807	50.058932
493.153437	113.725255	50.063937
489.066219	110.208221	50.068941
485.966679	111.086046	50.073946
482.418547	115.628219	50.078951
478.666263	114.282886	50.083956
475.396154	109.859580	50.088961
471.836237	119.848515	50.093965
468.493826	108.817851	50.098970
464.912328	114.463097	50.103975
461.146868	110.446419	50.108980
457.912651	112.250197	50.113985
454.237478	116.774313	50.118989
450.761955	118.543122	50.123994
447.394555	116.042840	50.128999
443.807604	119.588181	50.134004
440.778288	115.639708	50.139009
436.835312	114.204037	50.144013
433.232882	109.516420	50.149018
429.553269	110.070664	50.154023
426.013254	108.562390	50.159028
423.043924	112.928501	50.164033
419.025107	115.494276	50.169037
415.910549	113.969985	50.174042
412.183780	112.278993	50.179047
408.631111	120.140736	50.184052
405.426766	113.584242	50.189057
401.793395	109.344418	50.194061
398.289882	113.449354	50.199066
394.636369	118.362412	50.204071
391.220548	116.989724	50.209076
387.826881	109.485278	50.214081
384.104111	110.312061	50.219085
381.002331	110.775813	50.224090
377.048389	123.117095	50.229095
373.286796	113.411328	50.234100
370.159613	115.356560	50.239105
366.826845	111.259493	50.244109
363.447310	110.513893	50.249114
360.067562	108.157953	50.254119
356.462428	109.519985	50.259124
353.043143	104.569595	50.264129
349.011517	112.373500	50.269133
345.747439	115.858810	50.274138
342.123894	114.578793	50.279143
338.572295	106.045563	50.284148
335.465499	106.361419	50.289153
331.430085	111.065398	50.294157
328.192474	104.757763	50.299162
324.581587	105.674613	50.304167
321.230300	110.277758	50.309172
317.874366	104.940967	50.314177
313.886107	108.906728	50.319181
310.999315	103.518597	50.324186
306.840393	109.494799	50.329191
303.349089	113.822487	50.334196
300.449703	112.220238	50.339201
296.718719	114.067087	50.344205
293.362839	114.184691	50.349210
289.743304	101.865566	50.354215
285.884872	114.229876	50.359220
282.436950	111.403748	50.364225
278.802944	111.020752	50.369229
275.538336	110.579891	50.374234
272.290726	116.005220	50.379239
268.885194	116.978510	50.384244
265.388625	107.392640	50.389249
261.486571	111.256332	50.394253
258.416510	112.512436	50.399258
254.844051	107.244393	50.404263
251.079642	115.781608	50.409268
247.873534	102.825091	50.414273
243.832890	115.338184	50.419277
240.423837	108.010224	50.424282
236.672427	123.543738	50.429287
233.218899	108.300589	50.434292
230.102464	108.225681	50.439297
226.492227	121.962188	50.444301
223.328601	108.416885	50.449306
219.706558	112.714463	50.454311
215.656646	106.894801	50.459316
212.677620	115.271027	50.464321
208.948051	103.003983	50.469325
205.721446	103.199446	50.474330
202.025379	110.549037	50.479335
198.556764	116.603807	50.484340
195.231989	108.981086	50.489345
191.502628	105.123396	50.494349
187.851659	107.441815	50.499354
184.231438	108.973961	50.504359
180.768830	114.167243	50.509364
177.463202	110.524753	50.514369
174.297008	116.155661	50.519373
170.749128	107.530178	50.524378
167.224091	110.907732	50.529383
163.161062	123.607866	50.534388
160.612334	102.857207	50.539393
156.787565	115.450407	50.544397
153.009920	113.621965	50.549402
149.476145	102.254436	50.554407
145.761593	108.316113	50.559412
142.293368	104.411207	50.564417
138.868651	109.389755	50.569421
135.658248	105.042658	50.574426
132.101830	110.168393	50.579431
128.197478	109.103305	50.584436
125.480329	104.008210	50.589441
121.482005	108.845673	50.594445
118.101232	108.258553	50.599450
114.151365	107.526474	50.604455
110.506378	121.588003	50.609460
107.530871	109.797664	50.614465
103.952102	110.620986	50.619469
100.297932	108.001256	50.624474
97.262941	107.280876	50.629479
93.793335	107.213891	50.634484
90.206042	107.981605	50.639489
86.303596	106.707428	50.644493
83.047097	105.680067	50.649498
79.478140	111.174787	50.654503
76.063799	106.400915	50.659508
72.122048	103.800945	50.664513
68.774774	113.702905	50.669517
65.697299	101.254677	50.674522
62.124151	100.523712	50.679527
58.282865	111.142160	50.684532
55.485262	109.625291	50.689537
51.301211	107.126569	50.694541
47.633757	105.141704	50.699546
44.174803	103.779079	50.704551
40.616371	109.604361	50.709556
37.516428	104.778083	50.714561
34.019688	110.448168	50.719565
30.454322	112.484317	50.724570
27.024287	104.973079	50.729575
23.174229	108.116870	50.734580
20.023958	101.055356	50.739585
16.521578	111.120839	50.744589
12.840802	109.403835	50.749594
9.400710	107.389691	50.754599
6.100333	118.356850	50.759604
2.246814	102.853794	50.764609