Thu Aug 25 16:44:42 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
0.418333	109.531534	0.000000
0.639236	115.087421	0.005005
0.495869	118.900187	0.010010
0.392905	120.881114	0.015014
0.221314	105.174536	0.020019
0.041282	98.840439	0.025024
0.235150	82.282508	0.030029
-0.047396	86.547349	0.035034
0.149739	67.533821	0.040038
-0.490793	66.292815	0.045043
-0.399362	58.033747	0.050048
-0.896513	50.085205	0.055053
-1.630999	41.904931	0.060058
-1.613323	19.993076	0.065062
-1.911123	34.387545	0.070067
-1.791251	28.904996	0.075072
-2.163611	17.308063	0.080077
-2.324374	9.778235	0.085082
-3.076967	6.922284	0.090086
-3.457603	1.366304	0.095091
-3.485589	5.113511	0.100096
-4.066891	1.746665	0.105101
-4.049053	-1.388187	0.110106
-4.890260	-1.898551	0.115110
-4.915449	-5.675234	0.120115
-5.272560	-5.483160	0.125120
-4.786303	-11.978563	0.130125
-5.285217	-2.216009	0.135130
-5.418103	-10.341821	0.140134
-6.067833	-10.103899	0.145139
-6.305030	-3.169634	0.150144
-6.167268	-14.178918	0.155149
-6.844383	-7.447811	0.160154
-7.461462	-8.983553	0.165158
-7.855441	-7.792278	0.170163
-7.981997	-1.106304	0.175168
-7.989633	0.995715	0.180173
-8.103809	-0.555548	0.185178
-7.662378	0.615563	0.190182
-7.731666	-3.375675	0.195187
-8.716591	2.900626	0.200192
-8.694343	-4.550303	0.205197
-9.120511	-5.068748	0.210202
-9.373566	0.542382	0.215206
-10.358836	-8.569851	0.220211
-10.992000	-2.158842	0.225216
-10.373936	-6.207156	0.230221
-10.774935	0.452217	0.235226
-11.207860	-5.427764	0.240230
-11.069418	4.298205	0.245235
-11.120273	-1.578366	0.250240
-10.997270	1.901571	0.255245
-11.574384	3.507521	0.260250
-11.878608	-3.768866	0.265254
-12.349258	1.003157	0.270259
-12.733559	3.458425	0.275264
-12.354253	-2.254590	0.280269
-13.135963	0.626779	0.285274
-13.695118	-11.140183	0.290278
-13.826904	1.076883	0.295283
-13.699292	2.844497	0.300288
-13.577393	-5.204178	0.305293
-14.275145	-4.569587	0.310298
-14.410551	-4.855179	0.315302
-15.170023	-0.512467	0.320307
-15.398884	0.501075	0.325312
-15.450369	-3.467641	0.330317
-15.655335	4.473983	0.335322
-15.376730	-0.267795	0.340326
-15.588820	3.255155	0.345331
-16.084862	-0.181995	0.350336
-16.780269	-13.876490	0.355341
-16.994372	-2.677919	0.360346
-16.654985	-9.036414	0.365350
-17.141457	-0.708997	0.370355
-18.006572	7.443632	0.375360
-17.315448	1.428657	0.380365
-17.749645	-1.018432	0.385370
-18.013098	-4.416095	0.390374
-18.710592	2.599785	0.395379
-19.136293	-3.743238	0.400384
-19.596965	-3.873461	0.405389
-19.536839	9.908082	0.410394
-19.452013	6.474829	0.415398
-19.249919	-1.896463	0.420403
-19.974025	-4.089317	0.425408
-20.219948	-3.917828	0.430413
-20.645680	-4.398377	0.435418
-21.096348	-11.439842	0.440422
-21.173561	-7.080645	0.445427
-20.964232	-1.386940	0.450432
-21.026235	-0.197060	0.455437
-22.147964	2.592053	0.460442
-22.512689	-6.386454	0.465446
-22.300274	-2.145404	0.470451
-22.628106	8.859022	0.475456
-22.927390	-0.753005	0.480461
-22.854799	2.472238	0.485466
-23.455259	2.348100	0.490470
-23.572469	-3.416832	0.495475
-24.044213	-0.049352	0.500480
-23.746000	-2.832663	0.505485
-23.960655	-2.530031	0.510490
-24.995716	4.405863	0.515494
-25.477899	4.627026	0.520499
-25.712850	1.750083	0.525504
-25.329815	1.190269	0.530509
-25.586144	-1.199267	0.535514
-25.561752	-4.357291	0.540518
-25.608750	-8.927826	0.545523
-25.986336	-11.481860	0.550528
-26.520718	-6.203140	0.555533
-26.975796	8.690515	0.560538
-26.835136	-4.495903	0.565542
-26.995851	-2.208547	0.570547
-27.670792	-0.109538	0.575552
-27.888412	3.126375	0.580557
-28.636023	5.094401	0.585562
-28.715408	-0.572054	0.590566
-28.789146	3.065260	0.595571
-28.708307	0.303354	0.600576
-28.342579	-7.280485	0.605581
-29.244653	1.292387	0.610586
-29.635211	-5.986290	0.615590
-29.711137	2.672273	0.620595
-30.086439	5.221044	0.625600
-30.407863	0.218941	0.630605
-31.000061	-2.222373	0.635610
-31.364140	-4.734231	0.640614
-31.399019	-1.568080	0.645619
-31.762245	-9.002899	0.650624
-31.484737	-3.443265	0.655629
-31.625029	-7.233549	0.660634
-31.301614	-7.660635	0.665638
-31.960169	-1.185535	0.670643
-32.833595	-6.746554	0.675648
-32.893455	-1.896527	0.680653
-33.224205	2.106926	0.685658
-33.159466	-6.650967	0.690662
-33.040134	-6.799302	0.695667
-33.905946	5.032902	0.700672
-34.177438	2.095245	0.705677
-34.515212	2.341238	0.710682
-34.377686	-2.226572	0.715686
-34.594226	-2.208384	0.720691
-35.371246	-2.950267	0.725696
-35.647715	1.281964	0.730701
-35.750113	-0.407187	0.735706
-36.006311	-9.038862	0.740710
-36.092689	-3.074197	0.745715
-36.155897	-2.681399	0.750720
-36.485577	-2.952368	0.755725
-37.360911	-2.941687	0.760730
-37.128130	-3.636148	0.765734
-37.394193	-7.552258	0.770739
-37.756369	-3.547046	0.775744
-37.615056	-1.104532	0.780749
-38.186146	-0.445492	0.785754
-38.228757	-3.270313	0.790758
-38.924224	-4.240110	0.795763
-39.285762	-0.004042	0.800768
-39.082627	-5.347764	0.805773
-39.429826	-1.468285	0.810778
-39.294396	-4.425407	0.815782
-39.388864	-3.948617	0.820787
-40.176738	2.252517	0.825792
-40.346872	-5.348600	0.830797
-40.874996	3.583297	0.835802
-40.643652	-2.397601	0.840806
-40.968958	4.474541	0.845811
-41.937273	4.256181	0.850816
-41.670516	-0.034485	0.855821
-42.115551	8.147237	0.860826
-41.796703	3.516213	0.865830
-41.857946	10.065405	0.870835
-42.600468	14.408629	0.875840
-43.039458	6.855962	0.880845
-43.491332	6.192848	0.885850
-43.238471	7.162549	0.890854
-43.414725	4.080255	0.895859
-43.619111	5.343065	0.900864
-44.309019	-1.556510	0.905869
-44.904980	3.399665	0.910874
-45.072478	4.479524	0.915878
-44.983645	9.530883	0.920883
-45.186235	-0.305102	0.925888
-45.027613	-2.455932	0.930893
-45.171497	1.385363	0.935898
-45.875096	4.070997	0.940902
-46.328782	-0.034016	0.945907
-46.542193	2.764637	0.950912
-46.475661	-2.722198	0.955917
-46.613985	0.729082	0.960922
-46.976700	-5.952839	0.965926
-47.450218	-5.359708	0.970931
-47.848960	2.729336	0.975936
-47.906602	2.080381	0.980941
-48.233718	7.877125	0.985946
-48.159468	0.041561	0.990950
-48.578957	-0.787979	0.995955
-49.333428	10.767353	1.000960
-49.199235	4.906079	1.005965
-49.786673	0.784058	1.010970
-49.673861	5.072353	1.015974
-49.331735	-0.011573	1.020979
-49.806567	-4.072143	1.025984
-49.937595	-13.922496	1.030989
-51.038701	7.811211	1.035994
-51.097772	2.942008	1.040998
-50.844469	-1.498410	1.046003
-51.503679	0.199500	1.051008
-51.929785	-6.048542	1.056013
-52.212254	-4.359044	1.061018
-52.542164	-5.617073	1.066022
-52.330772	0.601493	1.071027
-52.663618	1.998327	1.076032
-52.228891	6.505102	1.081037
-52.730604	3.011895	1.086042
-53.447200	-6.870097	1.091046
-53.550962	-3.879816	1.096051
-53.734512	5.074021	1.101056
-54.210051	-0.125396	1.106061
-54.514682	1.270181	1.111066
-55.046635	-2.015806	1.116070
-55.216659	-3.805091	1.121075
-55.563642	5.709032	1.126080
-55.070521	-3.821506	1.131085
-55.586381	0.185641	1.136090
-55.608841	3.621931	1.141094
-55.747793	1.046324	1.146099
-56.490621	4.389843	1.151104
-56.584996	3.626421	1.156109
-56.553634	6.472143	1.161114
-57.010345	-2.903239	1.166118
-57.904739	-2.772509	1.171123
-58.270283	8.687079	1.176128
-58.008172	-5.663651	1.181133
-58.283075	3.437377	1.186138
-58.514311	1.578588	1.191142
-58.168083	-1.012929	1.196147
-58.482950	2.203421	1.201152
-59.418713	-0.085980	1.206157
-59.581721	-4.957877	1.211162
-59.513130	1.305210	1.216166
-59.839399	-4.635770	1.221171
-60.295845	8.429437	1.226176
-60.144380	-0.671079	1.231181
-60.940103	6.809450	1.236186
-61.166505	-5.569635	1.241190
-61.402647	-6.617729	1.246195
-61.622124	-1.094119	1.251200
-61.234672	1.382593	1.256205
-61.808073	1.225743	1.261210
-62.505308	0.743446	1.266214
-62.714226	-3.048739	1.271219
-62.770564	-0.075381	1.276224
-62.764560	-12.161844	1.281229
-63.023189	-2.987439	1.286234
-63.039942	-7.315937	1.291238
-63.709322	-2.145778	1.296243
-64.491892	-4.209243	1.301248
-64.258587	-5.587161	1.306253
-64.632286	-1.175179	1.311258
-64.583588	-7.475471	1.316262
-64.761444	-2.809438	1.321267
-64.717311	-2.123409	1.326272
-65.066034	-6.045549	1.331277
-65.296283	0.865480	1.336282
-65.621491	-1.813819	1.341286
-66.401371	-11.603631	1.346291
-66.663897	-6.639593	1.351296
-66.873049	-4.591421	1.356301
-66.799218	-3.451300	1.361306
-66.956467	-2.021868	1.366310
-67.355623	3.757688	1.371315
-68.315336	-0.315490	1.376320
-68.607624	3.469965	1.381325
-68.296092	0.728859	1.386330
-68.771210	-3.312682	1.391334
-68.808530	-4.477351	1.396339
-68.971508	0.904528	1.401344
-68.996304	-4.928666	1.406349
-68.956271	1.164889	1.411354
-69.311580	6.570578	1.416358
-69.517400	-6.406519	1.421363
-69.703282	1.449853	1.426368
-70.145524	0.740939	1.431373
-71.116714	8.065464	1.436378
-71.781623	5.423574	1.441382
-71.516090	-1.647854	1.446387
-71.376273	5.236827	1.451392
-71.743466	-2.263807	1.456397
-71.426145	-1.576293	1.461402
-71.712628	-3.815567	1.466406
-72.736381	-12.336458	1.471411
-72.834370	4.655764	1.476416
-72.956126	-6.758947	1.481421
-73.500593	-0.573807	1.486426
-73.132301	2.206465	1.491430
-73.278856	-3.155231	1.496435
-74.441930	2.054323	1.501440
-74.530441	-9.561748	1.506445
-75.263730	-4.989019	1.511450
-74.887985	-5.107929	1.516454
-74.480700	-9.097907	1.521459
-74.926086	-2.855526	1.526464
-74.961059	-14.717266	1.531469
-75.989894	-4.030118	1.536474
-76.401873	-8.176464	1.541478
-76.141005	-3.572848	1.546483
-76.404413	-3.037948	1.551488
-76.666417	-11.317529	1.556493
-76.707285	-6.027554	1.561498
-77.306422	-13.396926	1.566502
-77.426016	-13.039585	1.571507
-77.589021	-13.596099	1.576512
-77.146223	-16.762733	1.581517
-78.457435	-5.037917	1.586522
-78.964893	-13.206269	1.591526
-79.016021	-6.699799	1.596531
-78.923258	-8.897257	1.601536
-79.054143	-3.545719	1.606541
-79.232171	-7.089641	1.611546
-79.373457	-3.245591	1.616550
-80.233937	-8.099947	1.621555
-80.698374	-8.773744	1.626560
-80.687661	-11.616409	1.631565
-80.643151	-5.042666	1.636570
-80.639704	-5.365833	1.641574
-80.901930	-4.394518	1.646579
-81.974271	-6.808048	1.651584
-82.073582	-6.469704	1.656589
-82.500760	-2.713735	1.661594
-82.297713	-4.539330	1.666598
-82.133948	-3.951142	1.671603
-82.515448	5.407036	1.676608
-82.538790	0.101964	1.681613
-83.058354	-2.065987	1.686618
-83.644104	1.366816	1.691622
-83.756143	-8.015111	1.696627
-83.497720	-0.687107	1.701632
-84.234037	-11.439200	1.706637
-84.891763	-4.976886	1.711642
-85.257428	-7.330303	1.716646
-85.341170	-1.875419	1.721651
-85.396907	-5.881431	1.726656
-85.300505	-10.215004	1.731661
-85.143144	-17.199873	1.736666
-85.499001	-8.067184	1.741670
-86.124760	-5.681648	1.746675
-87.123965	0.774064	1.751680
-86.707625	-2.929431	1.756685
-86.841536	2.476367	1.761690
-86.778808	-1.004040	1.766694
-87.691443	-0.797683	1.771699
-88.115770	6.074155	1.776704
-88.021178	2.354635	1.781709
-88.285352	0.807895	1.786714
-88.214031	-2.487196	1.791718
-88.434484	3.976206	1.796723
-89.183376	0.607156	1.801728
-89.231988	0.371241	1.806733
-89.430677	4.278071	1.811738
-89.658437	-2.526234	1.816742
-89.731949	-1.654092	1.821747
-91.026752	5.306688	1.826752
-91.238362	-4.407653	1.831757
-90.791043	-1.877048	1.836762
-91.071356	-2.886582	1.841766
-90.725964	-1.561221	1.846771
-91.722601	5.169339	1.851776
-90.902641	-4.001122	1.856781
-91.827678	-4.049086	1.861786
-92.311769	-0.322163	1.866790
-92.501341	-3.702925	1.871795
-92.781693	-2.912267	1.876800
-92.969725	-4.869573	1.881805
-93.812394	11.831213	1.886810
-93.660688	-0.161026	1.891814
-93.817003	-1.629754	1.896819
-94.025857	3.528358	1.901824
-94.248384	-10.300333	1.906829
-94.135806	-1.949727	1.911834
-94.247180	-6.643050	1.916838
-95.071982	-0.141898	1.921843
-95.300855	0.011102	1.926848
-95.258907	-2.026533	1.931853
-95.661165	4.927268	1.936858
-96.319019	7.646867	1.941862
-96.519312	4.052648	1.946867
-97.104233	1.619691	1.951872
-97.065592	-4.100054	1.956877
-97.430833	-4.896962	1.961882
-97.079955	0.875799	1.966886
-97.493291	-7.114313	1.971891
-97.389270	3.974297	1.976896
-97.551570	-6.108438	1.981901
-98.146075	-5.240081	1.986906
-98.548281	-0.953347	1.991910
-98.309581	0.524774	1.996915
-98.906838	-0.207394	2.006912
-98.949853	-0.244847	2.016909
-98.800789	2.567151	2.026906
-97.718789	5.166439	2.036902
-97.416985	-0.050581	2.046899
-96.676549	-1.991113	2.056896
-96.250921	-2.073490	2.066893
-96.037949	-2.724431	2.076890
-94.867773	-3.557039	2.086886
-94.673843	-4.350715	2.096883
-94.786830	-2.755281	2.106880
-93.965883	-1.182643	2.116877
-93.402603	-4.229495	2.126874
-92.724271	3.596594	2.136870
-92.147432	-1.001447	2.146867
-91.705654	4.007502	2.156864
-91.097566	0.703370	2.166861
-90.468164	-3.988438	2.176858
-90.056712	3.261745	2.186854
-90.154906	-1.325558	2.196851
-89.620853	-2.593850	2.206848
-88.771519	-5.777390	2.216845
-87.919783	-3.661544	2.226842
-87.495161	-5.774336	2.236838
-87.750036	-1.125064	2.246835
-86.878907	0.442879	2.256832
-86.625931	-6.312385	2.266829
-85.664749	0.085045	2.276826
-84.868254	-4.990909	2.286822
-84.663572	-9.011111	2.296819
-84.633765	-7.574268	2.306816
-83.803485	1.406441	2.316813
-83.789373	5.022038	2.326810
-82.518397	2.700600	2.336806
-82.329615	1.701821	2.346803
-81.495327	7.840370	2.356800
-80.861703	-0.292355	2.366797
-80.733433	-0.755794	2.376794
-80.430245	-1.816848	2.386790
-79.852456	-3.731893	2.396787
-79.212605	7.049470	2.406784
-78.807914	0.805793	2.416781
-77.894387	1.210839	2.426778
-77.551049	0.191011	2.436774
-77.637973	6.771682	2.446771
-76.967051	5.687852	2.456768
-76.326245	-5.395239	2.466765
-75.631672	7.012146	2.476762
-74.974127	0.906246	2.486758
-74.644856	-0.966690	2.496755
-74.531774	-3.480497	2.506752
-73.653697	3.211895	2.516749
-73.381514	4.255964	2.526746
-72.570996	1.522001	2.536742
-72.062237	2.608197	2.546739
-71.807043	3.911522	2.556736
-71.473362	3.539443	2.566733
-70.667461	-0.470429	2.576730
-70.499139	-0.693054	2.586726
-69.299813	5.350284	2.596723
-69.147791	3.150325	2.606720
-69.056302	2.588112	2.616717
-68.047670	2.541097	2.626714
-67.678050	-1.175497	2.636710
-67.485506	-4.943541	2.646707
-66.975404	-0.072009	2.656704
-66.269883	4.252549	2.666701
-65.387242	2.321415	2.676698
-65.162451	0.654919	2.686694
-64.999800	5.340141	2.696691
-64.147820	0.946078	2.706688
-63.822252	6.514937	2.716685
-63.296822	3.733778	2.726682
-62.198438	-4.129645	2.736678
-62.153135	0.906584	2.746675
-62.012428	-1.852305	2.756672
-60.891758	0.287929	2.766669
-60.770843	-0.906123	2.776666
-60.392135	-2.580896	2.786662
-59.888976	-2.903503	2.796659
-59.403430	-1.509559	2.806656
-58.264965	2.018562	2.816653
-57.856565	2.619968	2.826650
-57.625555	4.212188	2.836646
-57.603809	7.386263	2.846643
-56.821883	1.175343	2.856640
-56.366175	4.477825	2.866637
-55.588564	3.253734	2.876634
-54.945038	7.920629	2.886630
-54.872975	4.336189	2.896627
-54.005902	0.348411	2.906624
-53.780069	3.281430	2.916621
-53.346283	2.966526	2.926618
-52.473682	2.329438	2.936614
-52.078666	-0.995158	2.946611
-51.668638	-0.615754	2.956608
-51.142922	4.687326	2.966605
-50.460882	2.600723	2.976602
-50.352925	5.640913	2.986598
-49.616197	2.880499	2.996595
-49.304098	-0.222029	3.006592
-48.983222	6.187039	3.016589
-47.768811	2.949464	3.026586
-47.630854	1.413784	3.036582
-47.356618	-6.944562	3.046579
-46.370918	2.791085	3.056576
-46.304772	1.808355	3.066573
-45.929656	2.218572	3.076570
-44.895501	-2.232544	3.086566
-44.894473	-2.302242	3.096563
-44.060519	-2.477107	3.106560
-43.320364	-6.242255	3.116557
-43.248884	-1.134100	3.126554
-43.012967	1.204957	3.136550
-41.991905	-4.742487	3.146547
-41.338665	-3.945025	3.156544
-41.398772	-4.410624	3.166541
-40.595761	-1.748608	3.176538
-40.373917	-3.481165	3.186534
-39.242041	-2.020597	3.196531
-38.668560	-4.099691	3.206528
-38.870609	-2.110163	3.216525
-38.482623	-2.921574	3.226522
-37.779759	0.266155	3.236518
-37.614112	-3.785947	3.246515
-36.021174	1.083816	3.256512
-35.898038	-1.083106	3.266509
-36.080628	1.296184	3.276506
-35.085753	-0.757071	3.286502
-34.600169	-3.183525	3.296499
-34.246909	0.166689	3.306496
-33.025962	0.796003	3.316493
-32.735652	0.934405	3.326490
-32.726819	7.167453	3.336486
-32.525002	2.108651	3.346483
-31.639068	3.351163	3.356480
-31.381736	3.922388	3.366477
-30.571610	2.965637	3.376474
-29.990770	4.480869	3.386470
-29.969678	5.532605	3.396467
-28.887460	5.239647	3.406464
-28.670761	-3.578525	3.416461
-28.042924	2.567036	3.426458
-27.119082	3.442477	3.436454
-26.931819	-2.358483	3.446451
-26.645509	6.010550	3.456448
-26.344710	-0.201009	3.466445
-25.635644	6.568558	3.476442
-25.402643	5.328432	3.486438
-24.182703	8.514341	3.496435
-24.077457	3.682913	3.506432
-23.829147	7.065412	3.516429
-23.378777	4.438567	3.526426
-22.381768	3.617262	3.536422
-22.147216	1.217470	3.546419
-21.268253	-0.263253	3.556416
-20.689074	1.192052	3.566413
-20.385388	2.544802	3.576410
-20.484368	7.622649	3.586406
-20.214981	-3.639835	3.596403
-19.274654	-3.216807	3.606400
-18.412685	4.821274	3.616397
-18.168526	-0.668651	3.626394
-17.426253	-2.457409	3.636390
-16.626885	-0.475900	3.646387
-16.642285	0.942685	3.656384
-16.412248	0.067324	3.666381
-15.483883	2.320061	3.676378
-14.881801	2.479305	3.686374
-14.905896	3.452590	3.696371
-13.903440	1.924008	3.706368
-13.326754	6.690080	3.716365
-13.504599	0.610537	3.726362
-12.490540	2.102241	3.736358
-12.158236	-5.413062	3.746355
-11.371360	-4.186705	3.756352
-10.592224	-0.795513	3.766349
-10.519232	-2.124608	3.776346
-10.385902	2.207246	3.786342
-9.700679	0.915272	3.796339
-9.104698	2.355273	3.806336
-8.664353	1.367764	3.816333
-7.729082	-1.737369	3.826330
-7.396842	-3.522070	3.836326
-7.182907	-1.822635	3.846323
-6.774941	-0.568587	3.856320
-6.037956	2.287513	3.866317
-5.706251	8.026479	3.876314
-5.159482	-2.313282	3.886310
-4.631288	0.648393	3.896307
-4.121538	12.783811	3.906304
-3.812091	20.499824	3.916301
-3.180688	23.328121	3.926298
-2.558057	25.007872	3.936294
-2.343470	34.009053	3.946291
-1.798717	47.916163	3.956288
-1.775528	54.451093	3.966285
-1.291014	81.834132	3.976282
-0.778820	96.620706	3.986278
-0.264249	115.034100	3.996275
0.000000	129.078741	4.001280
0.405638	141.569207	4.006285
0.475524	149.790538	4.011290
0.769048	154.743429	4.016294
0.939528	163.072394	4.021299
0.736629	172.212850	4.026304
0.962461	165.764516	4.031309
0.904392	184.610979	4.036314
1.279744	175.269643	4.041318
1.332986	189.526976	4.046323
1.182278	189.996764	4.051328
1.497994	190.266919	4.056333
1.099050	191.054016	4.061338
1.278793	196.309489	4.066342
1.182406	199.940902	4.071347
1.416911	186.878843	4.076352
1.332580	183.351836	4.081357
1.231394	193.365395	4.086362
1.431561	192.967109	4.091366
1.513383	188.692719	4.096371
1.487488	195.552824	4.101376
1.397209	192.548775	4.106381
1.291385	196.814427	4.111386
1.860182	192.875030	4.116390
1.421791	193.794861	4.121395
1.691852	187.304787	4.126400
1.604329	181.364297	4.131405
1.167522	193.496407	4.136410
1.442013	195.313795	4.141414
1.738107	192.552934	4.146419
1.420243	201.141932	4.151424
1.350509	188.380647	4.156429
1.146483	196.553167	4.161434
1.287573	190.485103	4.166438
1.004547	205.152646	4.171443
1.325788	200.812266	4.176448
1.567786	204.738679	4.181453
1.732725	201.188431	4.186458
1.393063	185.343599	4.191462
1.706495	199.841751	4.196467
1.409494	194.601641	4.201472
1.618879	212.893692	4.206477
1.572240	217.463293	4.211482
1.826826	219.176233	4.216486
1.673431	221.155581	4.221491
1.699779	223.103603	4.226496
1.988325	225.997652	4.231501
1.559258	219.215304	4.236506
1.987020	213.858467	4.241510
1.746180	204.240333	4.246515
1.380539	211.596610	4.251520
1.517737	223.613493	4.256525
1.466422	227.234685	4.261530
1.643595	219.174083	4.266534
1.780355	232.067417	4.271539
1.562281	225.846804	4.276544
1.950066	221.470683	4.281549
1.695354	221.355643	4.286554
1.464664	224.270935	4.291558
1.563386	222.034549	4.296563
1.538349	223.316730	4.301568
1.717150	237.538609	4.306573
1.600090	242.815289	4.311578
1.830033	249.821994	4.316582
1.899200	248.539380	4.321587
1.970127	253.179156	4.326592
1.981599	250.114861	4.331597
2.143727	254.547355	4.336602
2.068087	249.734463	4.341606
2.296878	258.617495	4.346611
2.046647	249.323518	4.351616
2.312192	249.506621	4.356621
2.118213	260.332038	4.361626
2.112132	255.248813	4.366630
2.157351	259.370589	4.371635
2.047710	253.243711	4.376640
2.078566	244.674502	4.381645
1.967215	250.551415	4.386650
1.845271	245.853349	4.391654
2.048467	256.996192	4.396659
2.077403	246.472043	4.401664
2.124638	253.001166	4.406669
2.149176	262.431906	4.411674
2.583843	256.789230	4.416678
2.323532	257.782404	4.421683
2.400674	257.074355	4.426688
2.563062	248.756623	4.431693
1.807870	247.843623	4.436698
1.971180	253.560441	4.441702
2.240111	252.980533	4.446707
2.102927	257.516873	4.451712
1.989597	253.617902	4.456717
2.315219	261.549274	4.461722
2.234161	250.833545	4.466726
2.185809	253.464003	4.471731
2.049400	255.162278	4.476736
2.101454	260.852237	4.481741
1.799220	265.003143	4.486746
1.761241	261.481513	4.491750
2.027645	278.616232	4.496755
2.084732	277.886013	4.501760
2.576347	273.588526	4.506765
2.114982	279.463341	4.511770
2.435707	288.176956	4.516774
2.272911	282.131164	4.521779
2.320451	284.832026	4.526784
2.743862	273.372839	4.531789
2.153471	284.715973	4.536794
2.317180	279.334049	4.541798
2.337437	278.014803	4.546803
2.413818	281.188882	4.551808
2.563295	286.461779	4.556813
2.374305	283.874987	4.561818
2.498137	290.006135	4.566822
2.544069	304.935436	4.571827
2.674449	312.562056	4.576832
2.960293	304.984274	4.581837
2.593397	295.746518	4.586842
2.531909	285.806003	4.591846
2.609594	288.517961	4.596851
2.348620	281.611173	4.601856
2.911012	302.505618	4.606861
2.668442	306.644021	4.611866
2.982565	300.020450	4.616870
2.793265	292.903107	4.621875
2.513822	292.890020	4.626880
2.659961	291.747207	4.631885
2.728681	303.806511	4.636890
2.744062	305.370274	4.641894
2.797051	306.184644	4.646899
2.833829	307.017374	4.651904
3.032402	300.797894	4.656909
2.410076	299.180686	4.661914
2.674380	292.403568	4.666918
2.884729	316.067749	4.671923
2.989098	308.331734	4.676928
2.774500	307.818094	4.681933
2.928873	318.750321	4.686938
3.392159	309.951971	4.691942
2.523506	301.824237	4.696947
2.962226	302.454780	4.701952
3.099849	307.400503	4.706957
2.733728	303.908132	4.711962
2.564919	307.743907	4.716966
2.815524	312.485263	4.721971
2.785295	318.570955	4.726976
2.955594	304.303961	4.731981
3.018787	318.616786	4.736986
3.092186	318.099151	4.741990
2.910008	314.549483	4.746995
3.006282	319.786433	4.752000
3.616221	318.555129	4.757005
3.176240	326.081291	4.762010
3.321865	315.023115	4.767014
3.243887	317.458903	4.772019
3.088731	309.867957	4.777024
2.975009	298.167040	4.782029
2.912489	306.599019	4.787034
3.079570	308.211781	4.792038
3.333752	316.530866	4.797043
3.093102	323.051336	4.802048
3.181788	315.994834	4.807053
3.192075	320.451136	4.812058
3.338467	319.877770	4.817062
3.087838	323.824447	4.822067
3.064869	306.591586	4.827072
3.382626	307.506844	4.832077
3.150019	312.751028	4.837082
3.011379	314.832480	4.842086
2.946745	312.042698	4.847091
3.048721	317.035138	4.852096
3.465226	312.524778	4.857101
2.910303	313.443889	4.862106
3.181260	317.397428	4.867110
3.163749	320.795039	4.872115
3.099450	317.549611	4.877120
2.954805	309.751369	4.882125
2.946495	323.717889	4.887130
3.228636	338.353937	4.892134
3.479768	338.608904	4.897139
3.624740	351.390302	4.902144
3.956864	344.178585	4.907149
3.324196	340.490683	4.912154
3.571320	325.585195	4.917158
3.215096	316.462818	4.922163
3.235493	316.795066	4.927168
3.519138	330.140030	4.932173
3.382671	343.756478	4.937178
3.715521	351.183708	4.942182
3.566737	350.805291	4.947187
3.636202	339.056661	4.952192
3.663441	325.273985	4.957197
3.330566	321.387250	4.962202
3.422129	334.113728	4.967206
3.407095	342.000433	4.972211
3.569736	335.539792	4.977216
3.644235	344.409076	4.982221
3.779742	348.867911	4.987226
3.663148	345.054854	4.992230
3.530912	346.132372	4.997235
3.687720	344.899296	5.002240
3.705043	339.144811	5.007245
3.111113	338.674785	5.012250
3.538720	348.013941	5.017254
3.241622	347.899214	5.022259
3.455167	348.217019	5.027264
3.363600	340.919824	5.032269
3.208767	347.274993	5.037274
4.183061	352.564211	5.042278
3.780890	353.354984	5.047283
3.503779	348.244594	5.052288
3.919757	358.525236	5.057293
3.862203	367.541776	5.062298
3.845013	363.428395	5.067302
4.067613	373.967142	5.072307
3.719139	355.136875	5.077312
3.708777	347.453621	5.082317
3.951268	360.058391	5.087322
4.033803	358.008027	5.092326
3.824655	351.741678	5.097331
3.560543	364.625148	5.102336
3.755307	368.600129	5.107341
3.780262	370.545221	5.112346
4.052134	372.242812	5.117350
4.081808	375.050893	5.122355
3.794327	378.876803	5.127360
3.916097	374.327184	5.132365
3.671983	376.830141	5.137370
3.728823	371.445950	5.142374
3.868465	372.784599	5.147379
3.747208	372.718253	5.152384
4.086266	368.805323	5.157389
3.966859	381.349749	5.162394
3.956084	374.065193	5.167398
3.863197	375.845247	5.172403
3.781089	379.246662	5.177408
4.039812	379.772529	5.182413
4.088960	397.928521	5.187418
4.260980	391.808085	5.192422
4.067745	397.280249	5.197427
4.231702	404.926959	5.202432
4.092049	394.226653	5.207437
4.112004	398.874453	5.212442
4.099411	392.865203	5.217446
4.624296	405.302368	5.222451
3.958146	401.189416	5.227456
4.257061	394.299267	5.232461
4.348702	409.661267	5.237466
4.261112	399.345117	5.242470
4.406858	394.054561	5.247475
4.149887	394.588461	5.252480
4.244238	389.078162	5.257485
4.474744	405.908571	5.262490
4.207563	389.520674	5.267494
4.429057	401.413735	5.272499
4.377712	397.796093	5.277504
4.569601	390.568364	5.282509
4.229780	387.479991	5.287514
4.128815	389.536566	5.292518
4.307081	393.887470	5.297523
4.216864	405.136492	5.302528
4.608121	398.548257	5.307533
4.590076	398.506868	5.312538
4.500019	401.495069	5.317542
4.554417	398.420860	5.322547
4.272662	404.742150	5.327552
4.695453	398.180612	5.332557
4.433265	409.146525	5.337562
4.697062	405.536453	5.342566
4.520188	406.826618	5.347571
4.558028	405.321105	5.352576
4.253042	409.817335	5.357581
4.238231	411.034650	5.362586
4.254801	408.504219	5.367590
4.389256	402.190344	5.372595
4.623713	412.192566	5.377600
4.361734	404.928373	5.382605
4.152673	404.711264	5.387610
4.516485	412.453216	5.392614
4.210317	414.165449	5.397619
4.162034	415.369025	5.402624
4.768647	421.440395	5.407629
4.373794	437.422826	5.412634
4.690798	433.412095	5.417638
4.552150	433.145986	5.422643
4.410793	444.308130	5.427648
4.672116	438.777981	5.432653
4.861549	439.039453	5.437658
4.587282	435.962947	5.442662
4.854346	443.201201	5.447667
4.565944	449.510893	5.452672
4.660584	436.986275	5.457677
4.751488	443.306139	5.462682
5.025783	444.452847	5.467686
4.922830	448.338447	5.472691
4.837192	445.491821	5.477696
5.032367	442.854305	5.482701
4.629093	448.422670	5.487706
4.658707	438.689266	5.492710
4.817687	444.916204	5.497715
4.833502	448.188390	5.502720
4.583800	438.903723	5.507725
4.514583	443.989462	5.512730
4.925214	450.161153	5.517734
5.135836	454.184290	5.522739
4.996843	467.484842	5.527744
4.926927	467.960961	5.532749
5.089440	474.418317	5.537754
5.114930	457.696590	5.542758
4.850674	445.544585	5.547763
5.064356	456.752350	5.552768
5.343073	461.932281	5.557773
5.212494	451.322271	5.562778
5.102484	436.700445	5.567782
5.030654	439.502294	5.572787
4.698692	451.811145	5.577792
5.194490	447.959064	5.582797
4.837224	461.515281	5.587802
4.816340	466.077746	5.592806
5.270439	469.224316	5.597811
4.732580	466.049896	5.602816
5.163183	463.824756	5.607821
4.808343	475.320934	5.612826
5.229528	468.968437	5.617830
5.203959	458.652027	5.622835
5.365671	468.643532	5.627840
5.235164	460.036225	5.632845
5.209362	467.997441	5.637850
5.295520	467.072829	5.642854
5.218201	466.901518	5.647859
5.395212	467.971719	5.652864
5.359076	466.556888	5.657869
5.428719	467.542668	5.662874
5.418417	464.247623	5.667878
5.374302	465.055069	5.672883
5.328456	466.963807	5.677888
5.065253	463.648274	5.682893
4.935388	471.568847	5.687898
4.927258	460.496705	5.692902
5.042605	467.075347	5.697907
4.897330	475.773481	5.702912
5.328588	487.045255	5.707917
5.391144	496.413212	5.712922
5.538049	496.532646	5.717926
5.640453	502.815926	5.722931
5.357559	501.971284	5.727936
5.459069	492.229749	5.732941
5.534115	501.725470	5.737946
5.526980	492.095874	5.742950
5.628395	502.289840	5.747955
5.702382	496.520099	5.752960
5.752027	497.157826	5.757965
5.979358	494.376054	5.762970
5.445597	492.229241	5.767974
5.582178	485.956134	5.772979
5.583666	490.628998	5.777984
6.039198	500.783299	5.782989
5.540854	491.755868	5.787994
5.363568	479.704111	5.792998
5.388701	471.423602	5.798003
5.434562	491.215917	5.803008
5.646152	498.026272	5.808013
5.256222	494.929912	5.813018
5.539214	500.143987	5.818022
5.819255	492.162061	5.823027
5.351383	496.443381	5.828032
5.613828	495.538604	5.833037
5.256836	496.100834	5.838042
5.643819	497.207743	5.843046
5.542603	498.261426	5.848051
5.579275	513.685914	5.853056
5.954528	512.285718	5.858061
5.716116	529.563051	5.863066
5.911676	524.008378	5.868070
6.174241	516.642970	5.873075
5.774045	513.045161	5.878080
5.888040	500.441534	5.883085
5.740326	502.426350	5.888090
5.641042	503.049445	5.893094
6.024697	521.330327	5.898099
5.722642	521.678299	5.903104
5.760964	524.143351	5.908109
5.839001	528.516320	5.913114
6.036011	527.359193	5.918118
6.033146	530.434998	5.923123
5.780425	532.980456	5.928128
5.686426	523.247390	5.933133
5.613246	523.170346	5.938138
6.083494	526.213152	5.943142
6.165634	531.177121	5.948147
5.920478	528.247904	5.953152
6.002643	520.502621	5.958157
5.803277	529.218747	5.963162
5.892956	518.890572	5.968166
5.931992	521.431445	5.973171
5.560830	521.359959	5.978176
6.073637	530.062581	5.983181
5.998547	528.438705	5.988186
6.064317	547.902085	5.993190
6.308351	556.352591	5.998195
6.070476	553.238725	6.003200
6.110505	561.948997	6.008205
5.873768	556.560127	6.013210
6.300112	559.211170	6.018214
6.186516	559.485320	6.023219
6.397079	570.497486	6.028224
6.405950	561.475972	6.033229
6.408698	548.174706	6.038234
6.001068	531.546084	6.043238
6.205793	528.695080	6.048243
6.042972	532.564767	6.053248
5.926729	521.825914	6.058253
6.037878	538.304977	6.063258
5.995332	550.138263	6.068262
6.296372	555.526703	6.073267
6.361549	559.866892	6.078272
6.362691	556.430826	6.083277
6.189105	550.927656	6.088282
6.055991	530.579606	6.093286
5.888997	535.285208	6.098291
6.141207	544.765849	6.103296
6.256120	554.359759	6.108301
6.443570	560.307020	6.113306
6.070767	547.634093	6.118310
6.291044	537.070303	6.123315
6.012465	534.459544	6.128320
5.951206	530.710546	6.133325
6.286163	550.030508	6.138330
5.954596	551.458821	6.143334
6.161483	556.729130	6.148339
6.463716	568.103432	6.153344
6.235206	555.917276	6.158349
6.074176	542.470826	6.163354
5.842178	533.183335	6.168358
6.264805	543.912313	6.173363
6.256637	556.091406	6.178368
6.463772	551.639102	6.183373
5.968402	546.961500	6.188378
6.067161	536.929296	6.193382
6.408915	539.008274	6.198387
6.224745	544.371490	6.203392
6.561556	530.796424	6.208397
6.440040	534.036358	6.213402
6.290864	527.785862	6.218406
6.368914	526.552459	6.223411
6.260237	528.578619	6.228416
6.178190	533.141193	6.233421
5.968936	542.963064	6.238426
6.157783	540.320198	6.243430
6.364134	533.574217	6.248435
6.517115	526.048798	6.253440
6.316896	530.462201	6.258445
6.228865	534.759948	6.263450
6.145787	529.369158	6.268454
6.202402	527.655042	6.273459
6.189765	535.253544	6.278464
6.193336	530.178219	6.283469
6.086523	536.418360	6.288474
6.013170	533.680530	6.293478
6.163357	529.167549	6.298483
6.059436	538.422402	6.303488
6.060939	534.049779	6.308493
5.911108	532.972307	6.313498
5.814673	528.111977	6.318502
5.728276	535.582826	6.323507
6.099760	540.219878	6.328512
6.234347	532.785927	6.333517
6.115363	536.110889	6.338522
5.886435	527.980895	6.343526
5.887203	531.302913	6.348531
5.723693	536.767298	6.353536
6.132844	551.911987	6.358541
6.334621	565.472442	6.363546
6.302692	564.870059	6.368550
6.396878	553.253463	6.373555
6.524530	552.179971	6.378560
6.593434	529.965224	6.383565
6.389354	539.953968	6.388570
6.126211	535.442470	6.393574
6.330710	525.102629	6.398579
5.697065	536.016085	6.403584
6.122230	528.147451	6.408589
6.005552	538.878664	6.413594
6.094260	535.428883	6.418598
6.332153	534.486821	6.423603
6.373225	538.748521	6.428608
6.364762	532.849312	6.433613
6.328334	538.670286	6.438618
5.996393	529.686369	6.443622
6.394611	527.425165	6.448627
6.274132	533.740215	6.453632
6.358645	533.961177	6.458637
6.339731	535.226602	6.463642
6.408330	528.644580	6.468646
6.223430	524.310658	6.473651
6.274546	534.237267	6.478656
6.446603	527.404909	6.483661
6.259620	523.587023	6.488666
6.114612	514.365009	6.493670
5.897299	508.757968	6.498675
5.807480	518.779420	6.503680
6.229336	525.683395	6.508685
6.240065	532.474613	6.513690
6.045047	527.987245	6.518694
6.768174	530.886023	6.523699
6.098280	525.447968	6.528704
5.918937	507.638280	6.533709
5.841502	526.801361	6.538714
5.888108	538.022700	6.543718
6.101568	534.654616	6.548723
6.017053	534.927373	6.553728
6.101930	535.274833	6.558733
5.965473	533.416954	6.563738
6.127658	531.091490	6.568742
6.164668	535.752473	6.573747
6.085225	530.816710	6.578752
5.960766	527.280102	6.583757
6.052548	533.134772	6.588762
6.118451	528.938728	6.593766
6.233850	530.480512	6.598771
6.206095	540.416318	6.603776
6.255628	530.546860	6.608781
6.219446	530.081191	6.613786
6.018220	522.987772	6.618790
6.131412	526.152963	6.623795
6.064478	529.463441	6.628800
6.341017	524.193483	6.633805
6.126622	529.918948	6.638810
6.096295	524.181361	6.643814
6.132193	525.058533	6.648819
6.268177	532.212953	6.653824
6.258624	526.130413	6.658829
6.018289	526.652219	6.663834
6.189963	536.249881	6.668838
6.359288	528.228337	6.673843
6.020557	540.120679	6.678848
6.133746	525.479629	6.683853
6.334935	524.979932	6.688858
6.543162	529.073066	6.693862
6.281951	532.287429	6.698867
5.999605	534.635041	6.703872
6.513219	529.707600	6.708877
6.421330	531.421072	6.713882
6.356392	527.520786	6.718886
6.461912	520.705183	6.723891
5.859480	518.338165	6.728896
6.205616	524.741458	6.733901
6.233349	524.136056	6.738906
5.862727	518.261958	6.743910
6.076237	525.951577	6.748915
6.159761	531.582906	6.753920
6.496634	532.049076	6.758925
6.045747	538.624711	6.763930
6.191306	538.004011	6.768934
6.267983	532.006038	6.773939
6.078826	534.038482	6.778944
5.865899	526.741243	6.783949
6.051274	530.828466	6.788954
6.109606	533.619426	6.793958
6.525866	532.832922	6.798963
5.740582	541.640857	6.803968
6.094499	524.541731	6.808973
5.926614	532.101278	6.813978
6.030723	534.761676	6.818982
6.108558	537.821674	6.823987
6.001368	535.585873	6.828992
5.846231	531.171353	6.833997
5.875555	532.748769	6.839002
5.957007	529.860130	6.844006
5.965920	525.692000	6.849011
5.727519	538.438684	6.854016
6.129672	545.690616	6.859021
6.442112	549.954094	6.864026
6.220447	554.339225	6.869030
6.264262	546.463893	6.874035
6.202172	549.526834	6.879040
5.901277	534.463420	6.884045
6.151617	541.245573	6.889050
6.040450	547.824934	6.894054
6.163712	540.076367	6.899059
5.935741	545.914699	6.904064
6.344214	555.332895	6.909069
6.258239	561.101526	6.914074
6.309719	549.270152	6.919078
6.167963	534.830397	6.924083
6.014622	540.128669	6.929088
5.977406	537.654105	6.934093
6.296251	549.924331	6.939098
6.216372	552.512315	6.944102
6.405564	531.582234	6.949107
6.006216	540.453090	6.954112
5.863863	534.505254	6.959117
6.189723	542.832197	6.964122
6.134365	546.811605	6.969126
6.301854	547.611210	6.974131
6.118809	551.370171	6.979136
6.228217	541.715960	6.984141
6.308756	549.024612	6.989146
6.115237	534.456921	6.994150
6.147085	533.132677	6.999155
5.945137	533.493439	7.004160
6.078741	541.973896	7.009165
6.198330	547.368617	7.014170
6.211965	556.288673	7.019174
6.557072	540.285611	7.024179
5.920299	544.362443	7.029184
6.379616	535.146975	7.034189
6.239600	540.405192	7.039194
6.165955	533.101947	7.044198
6.241193	521.826873	7.049203
6.045226	535.547705	7.054208
6.100018	531.685608	7.059213
5.916875	532.419923	7.064218
6.013835	535.214323	7.069222
6.398324	541.741331	7.074227
5.946944	545.871377	7.079232
5.999747	539.978385	7.084237
6.208607	553.964844	7.089242
6.119983	558.591732	7.094246
6.307231	555.069558	7.099251
6.357326	553.090695	7.104256
6.316129	540.979608	7.109261
5.956376	536.758503	7.114266
5.941477	526.348630	7.119270
6.140587	534.296782	7.124275
6.312811	557.388268	7.129280
6.035276	553.334618	7.134285
6.109310	550.260470	7.139290
6.170245	553.427526	7.144294
6.346613	549.989318	7.149299
6.067708	556.829090	7.154304
6.196325	547.387010	7.159309
6.038652	547.183993	7.164314
6.056500	560.770100	7.169318
6.291477	555.785066	7.174323
6.423504	562.699664	7.179328
6.390920	536.153651	7.184333
6.164165	538.055939	7.189338
6.095858	538.531808	7.194342
6.140314	534.952914	7.199347
5.846239	543.161848	7.204352
6.147123	533.841486	7.209357
5.809716	539.652669	7.214362
6.318123	554.367342	7.219366
6.727337	558.014524	7.224371
6.396816	548.334323	7.229376
6.318518	544.113411	7.234381
6.004091	541.305781	7.239386
5.940156	537.974832	7.244390
6.389535	530.820601	7.249395
6.305981	537.110883	7.254400
6.328005	532.472444	7.259405
6.146708	528.656830	7.264410
5.767986	531.902261	7.269414
6.050293	532.047938	7.274419
6.361022	539.734986	7.279424
6.265155	535.883838	7.284429
6.272662	535.170870	7.289434
6.489521	534.447247	7.294438
6.243695	527.278553	7.299443
6.424776	531.154470	7.304448
6.212487	531.380806	7.309453
5.990738	534.215650	7.314458
6.019836	533.455005	7.319462
6.109082	536.225303	7.324467
6.029045	530.330981	7.329472
6.155212	532.870859	7.334477
6.140408	536.002321	7.339482
6.276055	538.037660	7.344486
6.444342	534.667162	7.349491
5.913395	531.611874	7.354496
5.883293	528.857777	7.359501
6.357070	538.578955	7.364506
6.173257	535.288936	7.369510
6.187171	530.560016	7.374515
5.964859	534.521285	7.379520
6.259575	523.800301	7.384525
6.461402	530.609035	7.389530
6.285239	530.902479	7.394534
6.046528	535.043494	7.399539
5.781846	537.473764	7.404544
6.102797	534.585565	7.409549
6.104675	531.396170	7.414554
6.249215	533.670569	7.419558
6.109960	534.189193	7.424563
5.648650	535.001895	7.429568
6.316271	531.948644	7.434573
6.228732	533.977821	7.439578
6.071115	543.320186	7.444582
6.270702	529.927979	7.449587
5.997093	533.258184	7.454592
6.201047	538.601717	7.459597
6.208407	536.465031	7.464602
5.984808	530.767216	7.469606
6.232953	525.416283	7.474611
5.952223	542.557884	7.479616
6.391218	534.285270	7.484621
6.291299	529.096442	7.489626
6.081922	539.592235	7.494630
6.563303	524.877677	7.499635
6.100830	537.887267	7.504640
6.397693	536.394944	7.509645
6.113876	537.606959	7.514650
6.057248	534.898147	7.519654
6.426337	536.814648	7.524659
6.135595	539.214198	7.529664
6.641950	534.427104	7.534669
6.341104	537.078182	7.539674
6.000660	537.375220	7.544678
6.268300	534.235937	7.549683
6.339225	538.454993	7.554688
6.204057	537.020870	7.559693
6.067792	531.559316	7.564698
6.048891	539.453041	7.569702
6.527540	531.060316	7.574707
6.407002	537.065317	7.579712
6.423477	518.630129	7.584717
6.201283	520.208987	7.589722
5.957716	515.390696	7.594726
6.385260	510.489401	7.599731
5.618814	520.680147	7.604736
6.112653	517.745879	7.609741
6.356700	534.539486	7.614746
6.366107	523.372805	7.619750
6.151085	512.538699	7.624755
5.877471	515.020987	7.629760
6.417133	516.369739	7.634765
6.189165	519.411207	7.639770
6.179085	518.890827	7.644774
6.272083	508.147672	7.649779
6.257825	504.394479	7.654784
6.114254	496.162538	7.659789
6.221998	513.227426	7.664794
5.955495	497.623961	7.669798
5.763789	510.549978	7.674803
6.092357	523.546351	7.679808
6.290526	518.570258	7.684813
6.255553	530.063811	7.689818
6.286690	518.143893	7.694822
6.544425	511.424672	7.699827
6.071778	507.012448	7.704832
6.049987	492.357771	7.709837
6.228778	501.242431	7.714842
5.754210	512.906094	7.719846
6.191150	515.824398	7.724851
5.705254	529.112909	7.729856
6.250304	526.980565	7.734861
6.470024	534.270568	7.739866
6.382686	538.900413	7.744870
6.605792	522.679193	7.749875
5.840074	514.459298	7.754880
6.200514	501.481687	7.759885
5.987542	508.010543	7.764890
5.831684	508.041368	7.769894
5.957266	521.192935	7.774899
5.930867	536.785518	7.779904
6.377347	531.783172	7.784909
6.356330	534.251195	7.789914
6.420339	534.703168	7.794918
6.367571	535.217733	7.799923
6.118073	512.859899	7.804928
6.152959	502.670037	7.809933
6.128952	509.400248	7.814938
5.991976	509.867892	7.819942
6.246726	503.538297	7.824947
5.985394	525.235968	7.829952
6.261264	517.226210	7.834957
6.470262	526.001742	7.839962
6.298285	523.288858	7.844966
6.119434	503.637727	7.849971
6.334632	508.596662	7.854976
6.098859	498.490341	7.859981
6.281263	507.232064	7.864986
6.184267	505.424955	7.869990
6.116407	500.715183	7.874995
5.609650	501.645740	7.880000
6.093799	488.689885	7.885005
5.999521	509.345764	7.890010
6.220513	517.739749	7.895014
6.450568	510.797066	7.900019
5.840736	510.781959	7.905024
6.177769	512.428224	7.910029
5.885446	520.997554	7.915034
6.578418	526.473278	7.920038
6.435872	519.408632	7.925043
6.418708	506.661029	7.930048
6.362536	500.035290	7.935053
6.050492	493.750211	7.940058
5.856046	499.279545	7.945062
5.978567	502.455926	7.950067
6.163393	500.987488	7.955072
5.838392	499.155990	7.960077
6.128667	517.704608	7.965082
6.426907	528.908662	7.970086
6.329649	515.607270	7.975091
6.219506	509.407614	7.980096
6.206855	500.936851	7.985101
6.243409	498.570962	7.990106
5.919560	493.790566	7.995110
6.487322	499.671890	8.000115
6.097818	504.585788	8.005133
6.143690	491.756705	8.010150
5.972012	496.186007	8.015168
5.483627	502.135532	8.020186
6.164036	520.414647	8.025203
6.300734	524.792484	8.030221
6.239393	527.314185	8.035238
6.379182	529.577157	8.040256
6.297748	519.412557	8.045274
6.412525	511.763944	8.050291
6.121722	507.849068	8.055309
6.102092	501.228216	8.060326
6.152544	520.764210	8.065344
6.258644	521.050620	8.070362
6.214229	519.047417	8.075379
6.213239	529.730014	8.080397
6.272001	534.145311	8.085414
6.418142	519.851986	8.090432
6.223208	527.554343	8.095450
6.184716	522.908811	8.100467
6.113210	523.926792	8.105485
6.433546	523.428556	8.110502
6.124551	528.712512	8.115520
5.788164	534.411014	8.120538
6.323874	524.427426	8.125555
6.270942	532.609307	8.130573
6.144609	525.336137	8.135590
6.311254	525.259611	8.140608
6.071540	527.051871	8.145626
6.169429	525.780605	8.150643
6.326236	532.537918	8.155661
6.038864	519.833612	8.160678
6.406905	532.452852	8.165696
6.294110	533.209059	8.170714
6.437094	526.297633	8.175731
6.103007	535.101077	8.180749
6.435128	532.010086	8.185766
6.692755	535.346501	8.190784
6.253718	534.424448	8.195802
6.347842	529.979041	8.200819
6.078158	528.992585	8.205837
6.254015	534.254223	8.210854
6.266333	530.522220	8.215872
6.584927	535.007259	8.220890
6.629595	522.443429	8.225907
6.406580	531.295741	8.230925
6.578820	528.592718	8.235942
6.409650	523.295476	8.240960
6.162475	529.308202	8.245978
6.512116	526.495332	8.250995
6.599419	530.126675	8.256013
6.087064	525.574323	8.261030
6.666968	523.318665	8.266048
6.262929	532.458116	8.271066
6.612400	529.560066	8.276083
6.687763	528.387003	8.281101
6.271364	529.282298	8.286118
6.523088	522.375926	8.291136
6.202218	524.010488	8.296154
6.656927	518.056921	8.301171
6.337861	521.862386	8.306189
6.567702	525.114790	8.311206
6.796974	533.571190	8.316224
6.768620	524.704770	8.321242
6.669737	523.966107	8.326259
6.344775	520.940201	8.331277
6.272376	522.460093	8.336294
6.440917	531.008058	8.341312
6.592061	532.180501	8.346330
6.172756	526.474327	8.351347
6.245093	524.503323	8.356365
6.178258	524.315058	8.361382
6.044837	528.006230	8.366400
6.025387	523.594399	8.371418
6.529380	543.867239	8.376435
6.397955	546.993215	8.381453
6.707903	557.851172	8.386470
6.885035	555.639683	8.391488
6.793033	557.194206	8.396506
6.858092	538.527010	8.401523
6.922089	536.112343	8.406541
6.604770	529.143650	8.411558
6.714980	522.066947	8.416576
6.537214	531.180412	8.421594
6.957369	526.052763	8.426611
6.694965	530.625677	8.431629
6.359245	520.860680	8.436646
6.283793	526.773915	8.441664
6.387248	529.566441	8.446682
6.683777	527.664451	8.451699
6.268281	528.894119	8.456717
6.482269	532.385692	8.461734
6.507693	542.685463	8.466752
6.601930	553.640332	8.471770
6.988022	551.777955	8.476787
6.228705	555.879624	8.481805
6.567385	549.303599	8.486822
6.703590	556.594324	8.491840
6.658401	558.706401	8.496858
6.751597	551.408291	8.501875
6.698819	558.851703	8.506893
6.944500	559.535965	8.511910
7.057719	558.000364	8.516928
6.637553	546.307766	8.521946
6.805064	526.520000	8.526963
6.410490	533.641416	8.531981
6.622946	551.542604	8.536998
6.874783	550.616444	8.542016
6.935323	561.109539	8.547034
6.613513	543.859947	8.552051
6.522043	548.630145	8.557069
6.398019	555.362040	8.562087
6.371918	553.333873	8.567104
6.071235	561.901724	8.572122
6.548946	559.390674	8.577139
6.501600	558.325199	8.582157
6.517116	555.690908	8.587175
6.393170	555.416917	8.592192
6.656512	577.504217	8.597210
6.758946	578.914669	8.602227
6.527383	582.169949	8.607245
6.440327	590.742211	8.612263
7.136977	578.259225	8.617280
6.621749	580.091502	8.622298
6.637613	580.398363	8.627315
6.679206	583.405718	8.632333
6.466973	590.599572	8.637351
6.609593	588.270410	8.642368
6.553973	582.775478	8.647386
6.825803	587.031172	8.652403
6.802236	584.002213	8.657421
6.599347	578.716550	8.662439
6.468305	586.853890	8.667456
6.631861	614.791956	8.672474
7.061275	612.764994	8.677491
7.221955	607.924131	8.682509
6.964716	608.589364	8.687527
6.876745	599.511341	8.692544
7.012751	611.267588	8.697562
6.893361	600.383053	8.702579
6.847546	596.256202	8.707597
6.650429	614.101705	8.712615
7.027825	604.373251	8.717632
6.905435	615.541981	8.722650
6.835356	608.783827	8.727667
7.307278	608.435408	8.732685
6.703642	609.202253	8.737703
7.324963	601.818218	8.742720
7.159691	600.711256	8.747738
7.083643	586.626262	8.752755
6.943503	584.060537	8.757773
6.981959	594.626539	8.762791
6.894391	580.675898	8.767808
6.855143	583.749568	8.772826
6.939153	582.193294	8.777843
7.144020	574.603123	8.782861
6.887435	572.888777	8.787879
7.053250	576.615125	8.792896
6.733661	583.819485	8.797914
7.409821	593.695435	8.802931
7.137477	583.469192	8.807949
6.927541	588.636659	8.812967
7.104068	572.224143	8.817984
7.107272	588.646524	8.823002
7.096417	586.950480	8.828019
7.064898	571.141762	8.833037
6.949216	574.890125	8.838055
7.179188	576.381579	8.843072
7.001377	584.513623	8.848090
7.114229	578.575730	8.853107
7.122677	581.727132	8.858125
6.663762	583.957685	8.863143
6.800180	586.969118	8.868160
7.051815	603.573495	8.873178
7.005275	606.247523	8.878195
7.230037	604.460911	8.883213
7.551608	605.777070	8.888231
7.541141	603.733824	8.893248
6.654703	596.425085	8.898266
7.428245	598.408886	8.903283
7.714856	593.011808	8.908301
7.274067	595.378378	8.913319
6.981037	582.643355	8.918336
7.402442	584.862209	8.923354
6.817803	576.531048	8.928371
6.753798	581.170719	8.933389
6.776317	584.222088	8.938407
7.687086	593.240769	8.943424
7.749813	602.572209	8.948442
7.671431	589.727810	8.953459
7.382140	584.496708	8.958477
7.343122	581.331315	8.963495
7.282939	578.112436	8.968512
7.412022	586.590871	8.973530
7.414897	580.338849	8.978547
7.210251	583.703521	8.983565
6.927421	583.318724	8.988583
7.445224	578.974180	8.993600
7.313392	586.123877	8.998618
7.407085	575.262775	9.003635
7.431719	581.362318	9.008653
7.364657	581.839963	9.013671
7.306474	584.253880	9.018688
7.441413	580.805612	9.023706
7.288954	593.033078	9.028723
7.507506	584.187903	9.033741
7.082843	590.263172	9.038759
7.267987	574.597229	9.043776
7.177779	586.688704	9.048794
7.399428	587.275748	9.053811
7.440391	581.267066	9.058829
7.092491	585.585147	9.063847
7.470497	578.491710	9.068864
7.315364	589.002834	9.073882
7.356128	592.382705	9.078899
7.529109	570.646901	9.083917
7.245633	580.329218	9.088935
7.183710	580.162274	9.093952
7.088762	577.333849	9.098970
7.000605	584.467235	9.103987
7.261297	579.320375	9.109005
7.292486	583.225608	9.114023
6.991591	575.089831	9.119040
7.055163	586.582856	9.124058
7.182427	599.770044	9.129075
7.766316	597.469572	9.134093
7.743731	610.670780	9.139111
7.508936	593.846163	9.144128
7.214328	593.684118	9.149146
7.171840	594.034836	9.154163
7.120692	588.371945	9.159181
7.223175	608.950765	9.164199
7.303375	609.020328	9.169216
7.446517	612.286332	9.174234
7.498045	615.330005	9.179251
7.581587	608.074410	9.184269
7.435543	617.744682	9.189287
7.384519	619.112910	9.194304
7.178039	615.440418	9.199322
7.272865	605.525863	9.204339
7.418405	602.066462	9.209357
7.596156	614.459955	9.214375
7.552615	607.710267	9.219392
7.505270	619.700374	9.224410
7.454780	613.150589	9.229427
7.739475	606.876492	9.234445
7.778829	609.650672	9.239463
7.560070	610.628613	9.244480
7.342244	612.739344	9.249498
7.626724	615.670778	9.254515
7.633012	616.935351	9.259533
7.366381	611.552367	9.264551
7.304206	605.253725	9.269568
7.602831	613.074446	9.274586
7.411210	616.074165	9.279603
7.404938	611.849596	9.284621
7.491154	629.000624	9.289639
7.426446	632.475924	9.294656
7.850087	629.585172	9.299674
8.015607	643.962452	9.304691
7.950013	612.392589	9.309709
7.294802	615.269285	9.314727
7.546253	609.123473	9.319744
7.608157	619.244003	9.324762
7.487414	631.400253	9.329779
7.639544	634.241974	9.334797
7.575844	641.267408	9.339815
7.732422	639.280036	9.344832
7.979983	637.919039	9.349850
7.523547	634.973675	9.354867
7.702448	639.499562	9.359885
7.535089	642.138877	9.364903
7.656058	631.096743	9.369920
7.808986	630.845641	9.374938
7.756575	634.984891	9.379955
7.909522	636.835559	9.384973
7.933087	644.431147	9.389991
7.892031	641.060935	9.395008
8.150518	632.834331	9.400026
7.431294	621.598797	9.405043
7.707287	623.095668	9.410061
8.029357	634.119030	9.415079
7.665199	630.064141	9.420096
7.631781	630.255648	9.425114
7.838327	634.720398	9.430131
7.910089	639.465044	9.435149
7.865520	639.910764	9.440167
7.796693	639.423007	9.445184
7.737937	647.476465	9.450202
7.703376	645.459080	9.455219
7.964704	637.755894	9.460237
7.803552	642.107844	9.465255
7.937762	645.899119	9.470272
7.568191	643.037973	9.475290
7.689095	646.683009	9.480307
7.855989	635.409613	9.485325
7.755072	643.018393	9.490343
7.837776	646.644169	9.495360
7.953898	641.229608	9.500378
7.759869	642.194208	9.505395
7.955932	641.510313	9.510413
7.838192	651.084650	9.515431
7.948327	638.592532	9.520448
7.935585	639.601312	9.525466
8.010638	642.259450	9.530483
8.053074	636.944798	9.535501
7.782989	633.758796	9.540519
7.847300	642.275809	9.545536
8.147047	641.004465	9.550554
7.648494	644.374173	9.555571
7.949317	639.025349	9.560589
7.884171	647.871917	9.565607
7.878984	646.613637	9.570624
7.923970	639.837443	9.575642
7.599115	641.946012	9.580659
7.933135	629.494561	9.585677
7.936670	635.837270	9.590695
7.910847	651.876093	9.595712
8.063071	653.247192	9.600730
8.097867	664.495465	9.605747
8.166990	663.389644	9.610765
8.212404	655.328958	9.615783
7.936161	650.543919	9.620800
8.268424	643.751114	9.625818
7.765701	643.258757	9.630835
8.401023	647.050412	9.635853
8.080704	655.283712	9.640871
8.139391	649.575189	9.645888
8.027977	647.140655	9.650906
7.616710	640.549556	9.655923
7.867083	656.254773	9.660941
8.304972	662.756655	9.665959
8.079600	670.324986	9.670976
8.104667	667.853285	9.675994
7.940710	680.597011	9.681011
8.227533	667.499674	9.686029
8.384974	669.996584	9.691047
7.992889	670.206418	9.696064
8.153165	675.379020	9.701082
8.067390	677.964532	9.706099
8.217406	659.561610	9.711117
8.076160	667.770014	9.716135
8.376600	668.751815	9.721152
8.279714	669.155240	9.726170
8.024261	676.520003	9.731187
8.166928	669.176223	9.736205
8.138147	670.367399	9.741223
8.137136	670.389727	9.746240
7.995615	665.233278	9.751258
8.046125	667.532347	9.756275
8.080211	673.564168	9.761293
8.003517	674.469360	9.766311
7.884504	681.238388	9.771328
8.143604	675.637312	9.776346
8.376267	695.940214	9.781363
8.185189	703.632575	9.786381
8.390582	707.406398	9.791399
8.195633	703.788886	9.796416
8.936616	702.404223	9.801434
8.501001	699.124223	9.806451
8.379646	679.324744	9.811469
8.249225	680.651767	9.816487
8.235396	682.765257	9.821504
8.542158	671.318444	9.826522
8.242996	669.771706	9.831539
8.306793	674.609129	9.836557
8.319731	677.128681	9.841575
7.854316	676.513713	9.846592
8.379264	679.931347	9.851610
8.490845	693.446111	9.856627
8.427446	694.945672	9.861645
8.641936	700.434837	9.866663
8.337606	696.168585	9.871680
8.406170	706.881416	9.876698
8.146356	703.703260	9.881715
8.325340	705.496206	9.886733
8.437981	702.550029	9.891751
8.448934	716.531860	9.896768
8.884954	704.297908	9.901786
8.454004	708.386031	9.906803
8.407959	707.929417	9.911821
8.647317	703.710522	9.916839
8.685754	708.962185	9.921856
8.006276	699.146808	9.926874
7.922122	706.409004	9.931891
8.583924	709.473839	9.936909
8.829847	695.338311	9.941927
8.577322	701.339309	9.946944
8.747310	709.994432	9.951962
8.518097	702.339674	9.956979
8.781011	700.029520	9.961997
8.791689	705.358115	9.967015
8.516052	705.139447	9.972032
8.572771	702.725899	9.977050
8.645248	701.546965	9.982067
8.544488	705.630691	9.987085
8.758391	703.302968	9.992103
8.704308	710.787673	9.997120
8.647372	694.651467	10.002138
8.591445	693.622042	10.007155
8.651805	693.559014	10.012173
8.615776	689.339089	10.017191
8.470958	692.060086	10.022208
8.643814	695.621253	10.027226
8.539558	699.847537	10.032243
8.898291	696.840712	10.037261
8.733668	698.501301	10.042279
8.412443	705.118982	10.047296
9.019491	696.752528	10.052314
8.745027	698.253601	10.057331
9.060947	696.534748	10.062349
9.090350	678.327431	10.067367
8.573675	672.554415	10.072384
8.456062	671.600929	10.077402
8.306491	673.767244	10.082419
8.855809	686.029985	10.087437
8.823816	689.364469	10.092455
8.612342	698.461209	10.097472
8.661100	699.766471	10.102490
8.757046	702.168878	10.107507
8.800096	700.549584	10.112525
8.751034	697.991664	10.117543
8.174728	705.738072	10.122560
8.508900	704.972574	10.127578
8.675632	703.444355	10.132595
8.390443	698.783782	10.137613
8.711909	703.094842	10.142631
8.634056	711.454280	10.147648
8.791361	705.446264	10.152666
8.936825	703.640508	10.157683
8.548128	705.206818	10.162701
8.950109	707.109992	10.167719
8.925587	704.491421	10.172736
9.015324	707.538590	10.177754
8.678419	702.488484	10.182771
8.943626	699.660415	10.187789
8.979812	705.562530	10.192807
8.382641	720.359175	10.197824
9.235955	728.708424	10.202842
8.976152	721.866344	10.207859
8.781013	715.418081	10.212877
8.998512	714.888616	10.217895
9.037722	720.307419	10.222912
9.001604	714.979806	10.227930
9.298884	713.724624	10.232947
9.241122	710.584236	10.237965
9.034956	695.364510	10.242983
8.946886	702.964991	10.248000
8.512044	696.428059	10.253018
8.373000	705.797478	10.258035
8.948401	717.696390	10.263053
9.225644	729.115002	10.268071
9.027631	724.560684	10.273088
8.845776	724.507204	10.278106
9.301070	724.246596	10.283123
8.937436	732.410977	10.288141
9.331267	722.787183	10.293159
9.036456	734.800362	10.298176
9.374493	731.231880	10.303194
9.561761	724.165115	10.308211
9.327774	712.784066	10.313229
9.379952	702.327027	10.318247
8.935604	706.451963	10.323264
9.137545	699.578570	10.328282
9.225339	702.657601	10.333299
8.867018	709.401018	10.338317
9.053430	702.548992	10.343335
9.220628	698.587559	10.348352
9.025720	700.025674	10.353370
9.147751	697.778619	10.358387
9.163496	703.033835	10.363405
9.104065	701.948154	10.368423
9.322936	710.665046	10.373440
9.135033	707.295739	10.378458
9.086125	705.286907	10.383475
9.068441	710.184443	10.388493
9.284851	708.837790	10.393511
8.826145	714.706994	10.398528
9.034855	727.689010	10.403546
9.381352	730.105814	10.408563
9.499010	733.180171	10.413581
9.895591	726.620257	10.418599
9.139342	714.074484	10.423616
9.282124	704.146050	10.428634
9.077464	700.684695	10.433651
8.778582	710.350562	10.438669
8.841692	715.920255	10.443687
9.106779	731.739998	10.448704
9.107379	733.677663	10.453722
9.753376	736.252670	10.458739
9.363594	737.844398	10.463757
9.495943	726.093516	10.468775
9.289556	741.283389	10.473792
9.369863	733.864147	10.478810
9.427977	739.362046	10.483827
9.258340	737.350035	10.488845
9.624632	738.065901	10.493863
9.673228	741.839052	10.498880
9.171840	733.103450	10.503898
9.269219	737.134047	10.508915
9.175527	737.997724	10.513933
9.479347	729.227481	10.518951
9.367982	733.114056	10.523968
9.646960	734.212835	10.528986
9.284963	740.814827	10.534003
9.288181	740.085403	10.539021
9.604407	732.190537	10.544039
9.370507	732.407145	10.549056
9.382527	725.847524	10.554074
9.733480	734.764641	10.559091
9.225118	735.267252	10.564109
9.371570	728.276309	10.569127
9.260854	729.366716	10.574144
9.376381	727.284780	10.579162
9.443509	728.669218	10.584179
9.147610	735.794187	10.589197
9.184101	730.168012	10.594215
9.588303	737.476781	10.599232
9.702759	759.799075	10.604250
9.963381	752.017054	10.609267
9.666378	737.373263	10.614285
9.817440	735.503511	10.619303
9.382830	734.063197	10.624320
9.801595	737.077754	10.629338
9.704880	726.006552	10.634355
9.373356	732.670039	10.639373
9.163264	727.656861	10.644391
9.455027	738.290558	10.649408
9.559261	750.446353	10.654426
9.736787	754.729486	10.659443
9.934838	760.132882	10.664461
9.943193	749.130410	10.669479
9.550993	746.995479	10.674496
9.568826	763.914351	10.679514
10.009616	760.342387	10.684531
9.788210	747.558154	10.689549
9.736691	733.216734	10.694567
9.445134	739.148120	10.699584
9.197193	745.615478	10.704602
9.712483	755.084373	10.709619
9.491956	759.379382	10.714637
9.660432	754.363687	10.719655
9.637187	766.959193	10.724672
9.778000	754.121358	10.729690
9.996528	742.117119	10.734707
10.025573	760.160863	10.739725
9.902180	755.137250	10.744743
10.010767	755.161340	10.749760
9.761045	750.204859	10.754778
10.328272	762.619482	10.759795
10.117335	761.219861	10.764813
9.912837	744.159979	10.769831
9.710620	739.877718	10.774848
9.832605	745.857921	10.779866
9.933887	739.943879	10.784883
9.888060	753.177236	10.789901
10.038797	756.240103	10.794919
9.899511	742.758190	10.799936
9.684407	743.915448	10.804954
9.619830	751.408126	10.809971
9.357633	760.699039	10.814989
10.019556	751.329873	10.820007
10.170944	748.166176	10.825024
9.792468	750.693417	10.830042
9.938938	747.947061	10.835059
9.973722	764.358345	10.840077
10.191331	761.900645	10.845095
9.960405	765.159014	10.850112
10.228858	755.412834	10.855130
9.896032	757.188147	10.860147
9.662394	756.880846	10.865165
10.373898	749.387946	10.870183
10.161373	760.798109	10.875200
9.826054	752.358372	10.880218
10.290601	752.433989	10.885235
9.908300	761.538591	10.890253
10.058759	764.087101	10.895271
10.213393	753.790706	10.900288
10.053713	751.770822	10.905306
10.230032	764.675888	10.910323
9.968524	764.237253	10.915341
10.169167	749.259858	10.920359
10.571604	752.611494	10.925376
10.367799	757.711776	10.930394
10.255470	760.528680	10.935411
10.063234	760.899709	10.940429
10.003485	757.668105	10.945447
10.153627	758.708175	10.950464
10.094109	761.863947	10.955482
10.353632	752.854478	10.960499
10.141219	755.049584	10.965517
10.204053	760.527816	10.970535
10.188750	756.168927	10.975552
9.872333	761.088036	10.980570
10.135574	749.991978	10.985587
10.192418	761.243170	10.990605
10.390742	747.907174	10.995623
10.081318	757.461107	11.000640
10.117877	750.629386	11.005658
10.376217	742.058769	11.010675
10.120702	755.536423	11.015693
10.191073	752.148732	11.020711
10.260575	750.500042	11.025728
10.001534	757.114311	11.030746
10.350790	748.235954	11.035763
10.405479	752.023931	11.040781
10.157690	749.620218	11.045799
9.985670	748.735213	11.050816
9.999632	751.134693	11.055834
10.415770	758.763495	11.060851
10.236737	772.544762	11.065869
10.287619	785.444251	11.070887
10.497697	788.630371	11.075904
10.229278	779.321751	11.080922
10.540832	774.353062	11.085939
10.069041	779.842481	11.090957
10.433006	787.997028	11.095975
10.588997	779.483455	11.100992
10.318289	785.884966	11.106010
10.232164	789.808625	11.111027
10.299517	790.744903	11.116045
10.489067	785.965741	11.121063
10.282658	782.788670	11.126080
10.232203	793.933617	11.131098
10.493087	782.844219	11.136115
9.922896	787.768384	11.141133
10.234827	787.823731	11.146151
10.178032	789.599979	11.151168
9.949649	802.114041	11.156186
10.634757	810.170943	11.161203
10.709288	803.172305	11.166221
10.742993	801.406141	11.171239
10.663233	803.517352	11.176256
10.531593	813.273836	11.181274
10.769582	808.802663	11.186291
10.658146	808.119604	11.191309
10.740665	808.479143	11.196327
10.849004	807.288272	11.201344
10.743580	808.068582	11.206362
11.350794	797.455094	11.211379
10.966268	796.022707	11.216397
10.634197	780.443935	11.221415
10.720767	778.480140	11.226432
10.600043	784.813969	11.231450
10.764743	777.719161	11.236467
10.684695	780.833971	11.241485
10.718234	780.683625	11.246503
10.812799	773.861742	11.251520
10.643987	780.900544	11.256538
10.733070	777.765540	11.261555
10.874865	778.803763	11.266573
10.798014	777.023366	11.271591
11.146010	776.233608	11.276608
10.669498	783.241727	11.281626
10.726250	768.990612	11.286643
10.780092	776.398474	11.291661
10.787992	771.442648	11.296679
11.059656	776.897632	11.301696
10.905759	789.854456	11.306714
10.632941	776.715336	11.311731
10.714601	782.430468	11.316749
10.857385	778.924127	11.321767
10.816459	779.145215	11.326784
10.540223	782.473803	11.331802
11.142483	778.557796	11.336819
11.083598	785.582532	11.341837
10.949340	789.658902	11.346855
10.809560	779.089881	11.351872
10.902256	778.147619	11.356890
10.827229	777.856492	11.361907
10.893136	770.553100	11.366925
10.905183	780.637352	11.371943
10.967330	772.933757	11.376960
10.897346	786.959884	11.381978
10.961350	779.609450	11.386995
10.841698	793.431922	11.392013
10.660757	808.674671	11.397031
10.923713	802.432315	11.402048
10.802906	811.502282	11.407066
11.140599	809.697956	11.412083
11.204191	811.092421	11.417101
10.913975	811.983738	11.422119
11.179466	805.810412	11.427136
10.957648	816.537248	11.432154
10.870737	808.118525	11.437171
11.049249	804.653919	11.442189
10.918402	807.044538	11.447207
11.077961	803.380928	11.452224
11.105089	812.415094	11.457242
11.404852	807.697554	11.462259
11.441952	811.128534	11.467277
10.626912	808.264574	11.472295
10.946647	811.124244	11.477312
10.781748	821.466619	11.482330
10.669073	804.853046	11.487347
11.000635	815.524735	11.492365
10.957036	829.868658	11.497383
11.623594	827.937062	11.502400
11.324229	834.279963	11.507418
11.354599	824.627855	11.512435
11.380978	818.463587	11.517453
11.335048	813.494092	11.522471
11.714484	805.267393	11.527488
11.600477	812.509063	11.532506
11.488421	802.790918	11.537523
11.016531	802.694517	11.542541
10.767549	816.161726	11.547559
11.123833	805.218315	11.552576
11.298041	812.929229	11.557594
10.962388	816.500666	11.562611
11.454102	823.682149	11.567629
11.399859	836.408794	11.572647
11.852459	827.204932	11.577664
11.605880	823.661758	11.582682
11.312131	817.490843	11.587699
11.633378	807.906779	11.592717
10.817442	816.896313	11.597735
11.516615	813.952894	11.602752
11.422507	821.854177	11.607770
11.674093	826.580165	11.612787
11.606216	819.480755	11.617805
11.307848	812.057695	11.622823
11.272089	806.225063	11.627840
11.379747	812.819768	11.632858
11.368518	827.284850	11.637875
11.497947	830.581446	11.642893
11.291567	840.829344	11.647911
11.692331	839.823030	11.652928
11.642182	837.726014	11.657946
11.592282	837.699196	11.662963
11.899143	835.483126	11.667981
11.564230	843.352720	11.672999
11.373731	835.966398	11.678016
11.753499	845.914174	11.683034
11.724769	837.798751	11.688051
11.604289	834.866987	11.693069
11.611979	835.468627	11.698087
11.860788	836.117697	11.703104
11.520617	828.600192	11.708122
11.402901	831.272783	11.713139
11.599456	828.540658	11.718157
11.745505	831.134051	11.723175
11.671987	828.895528	11.728192
11.732190	838.139123	11.733210
11.605375	832.891958	11.738227
12.015961	828.728258	11.743245
11.790921	841.402772	11.748263
11.807540	830.995410	11.753280
12.000538	834.521891	11.758298
11.907536	825.655983	11.763315
11.746394	813.499742	11.768333
11.358726	818.991772	11.773351
11.618818	814.198394	11.778368
11.751426	826.548614	11.783386
11.734945	823.903518	11.788403
11.809667	822.304497	11.793421
11.813007	828.180240	11.798439
12.046380	823.738190	11.803456
11.946609	824.555485	11.808474
11.710860	831.677380	11.813491
12.043780	822.725804	11.818509
11.710963	829.398997	11.823527
11.552996	830.799776	11.828544
12.035317	833.009117	11.833562
11.782939	836.141471	11.838579
11.791311	828.528330	11.843597
11.578361	836.505045	11.848615
11.996103	830.443557	11.853632
11.925206	829.810951	11.858650
11.735149	827.963078	11.863667
12.062162	837.246919	11.868685
11.749804	839.606021	11.873703
12.270031	834.292190	11.878720
12.049297	833.215994	11.883738
12.005233	834.147640	11.888755
11.775788	832.085029	11.893773
11.692396	841.887618	11.898791
11.834919	827.130706	11.903808
11.818634	843.357556	11.908826
12.039275	851.108549	11.913843
12.018973	859.957664	11.918861
11.873039	861.482794	11.923879
12.088243	855.276304	11.928896
12.316246	865.642352	11.933914
12.090062	861.553168	11.938931
12.192182	865.308491	11.943949
12.387315	861.784465	11.948967
12.371001	859.874652	11.953984
12.173774	856.096517	11.959002
12.021070	864.524559	11.964019
12.333701	854.837677	11.969037
12.019585	863.922180	11.974055
12.218981	855.938265	11.979072
12.105028	860.929823	11.984090
12.280866	860.675129	11.989107
12.329200	857.051026	11.994125
12.570162	860.551061	11.999143
12.427204	854.839353	12.004160
12.277520	853.802517	12.009178
12.264384	853.242912	12.014195
12.649172	850.800032	12.019213
12.159359	858.501395	12.024231
12.238434	854.831450	12.029248
12.076356	855.677444	12.034266
12.155524	859.101843	12.039283
12.372929	848.277997	12.044301
11.988517	866.307734	12.049319
12.495423	855.526889	12.054336
12.554216	855.173767	12.059354
12.127039	856.837638	12.064371
12.448024	850.993278	12.069389
12.157142	851.928882	12.074407
12.095425	858.837325	12.079424
12.504879	849.447704	12.084442
12.496048	857.616512	12.089459
12.255515	850.114946	12.094477
12.067310	848.629704	12.099495
12.511563	868.965923	12.104512
12.809525	873.634164	12.109530
12.315188	869.833150	12.114547
12.570934	872.235789	12.119565
12.369844	878.108864	12.124583
12.476363	879.275699	12.129600
12.620506	874.124926	12.134618
12.586745	874.357515	12.139635
12.617356	875.567802	12.144653
12.715028	871.096508	12.149671
12.499380	877.615659	12.154688
13.068309	879.792501	12.159706
12.643785	874.863373	12.164723
12.833234	860.657667	12.169741
12.688636	848.164290	12.174759
12.577198	858.400479	12.179776
12.765276	841.799710	12.184794
12.781733	841.992872	12.189811
13.043581	842.895523	12.194829
12.898776	856.075035	12.199847
12.668613	858.872548	12.204864
13.043245	849.128616	12.209882
12.471848	851.313707	12.214899
12.882951	851.041087	12.219917
12.523024	849.424958	12.224935
12.675713	857.363328	12.229952
12.538396	858.350612	12.234970
12.607497	860.716221	12.239987
12.897523	871.836271	12.245005
12.883124	864.169878	12.250023
12.634887	876.999532	12.255040
13.031295	876.792331	12.260058
12.994249	879.098833	12.265075
13.073090	875.684545	12.270093
13.057886	873.481062	12.275111
12.773043	872.825170	12.280128
12.811565	865.279874	12.285146
13.165881	870.693534	12.290163
13.346843	859.550339	12.295181
12.977126	854.820916	12.300199
13.126760	847.892544	12.305216
13.345152	849.439486	12.310234
12.776903	842.330102	12.315251
12.845471	839.125716	12.320269
12.852181	846.825019	12.325287
12.841710	849.285146	12.330304
13.307914	853.122279	12.335322
13.213239	859.587754	12.340339
13.323144	848.417829	12.345357
12.718908	850.989924	12.350375
12.835008	845.196603	12.355392
13.103607	854.861997	12.360410
12.864472	867.895350	12.365427
13.162599	865.383994	12.370445
13.331542	871.640909	12.375463
12.998325	874.186323	12.380480
13.430051	870.132911	12.385498
13.312871	875.797176	12.390515
13.131148	862.416498	12.395533
13.324011	864.929976	12.400551
13.053018	871.681862	12.405568
13.413901	868.671515	12.410586
13.256686	871.135702	12.415603
13.193200	869.810801	12.420621
13.130551	874.302010	12.425639
13.350192	870.783610	12.430656
13.152407	868.334175	12.435674
13.228819	878.338967	12.440691
13.150010	884.754628	12.445709
13.190466	878.906875	12.450727
13.062848	879.974694	12.455744
13.225660	876.657703	12.460762
12.951573	882.318151	12.465779
13.218019	873.812474	12.470797
13.316837	893.593765	12.475815
13.022046	884.791004	12.480832
13.550469	883.212411	12.485850
13.209806	888.662383	12.490867
13.280283	880.140069	12.495885
13.303707	883.951909	12.500903
13.334977	901.613589	12.505920
13.866591	898.150446	12.510938
13.343662	883.242127	12.515955
13.280206	880.143628	12.520973
13.711707	893.236027	12.525991
13.518458	893.487294	12.531008
13.300044	894.834431	12.536026
13.716021	898.518495	12.541043
13.740327	900.566074	12.546061
13.891144	879.284656	12.551079
13.421760	871.809470	12.556096
13.333579	869.140887	12.561114
13.461820	891.726277	12.566131
13.704899	894.421244	12.571149
13.761214	903.734910	12.576167
13.664846	900.527953	12.581184
13.939230	889.846637	12.586202
13.567223	890.337355	12.591219
13.175619	880.148563	12.596237
13.790231	893.499455	12.601255
13.637003	903.401384	12.606272
13.549974	896.286009	12.611290
13.765941	903.542287	12.616307
14.085745	908.626845	12.621325
14.065403	898.717550	12.626343
13.728058	896.031197	12.631360
13.709556	892.717365	12.636378
14.229050	901.721770	12.641395
13.830105	888.444536	12.646413
13.797395	874.586057	12.651431
13.646224	882.086046	12.656448
13.871453	885.373953	12.661466
13.851755	890.019386	12.666483
13.843145	898.816194	12.671501
13.769715	897.041560	12.676519
13.378001	904.623429	12.681536
13.727482	892.311388	12.686554
13.789914	892.816089	12.691571
13.761641	889.992947	12.696589
13.955266	894.623892	12.701607
13.979661	903.557545	12.706624
13.990934	899.349094	12.711642
13.966182	895.477654	12.716659
13.725073	894.048035	12.721677
14.308729	896.746445	12.726695
14.148211	889.759353	12.731712
14.032187	894.823829	12.736730
14.571653	895.140177	12.741747
14.154376	893.479380	12.746765
14.234198	891.314655	12.751783
14.056387	894.081879	12.756800
14.341899	896.041194	12.761818
13.988555	894.095819	12.766835
13.870978	889.210114	12.771853
13.968667	892.839904	12.776871
13.830459	891.324733	12.781888
13.668246	897.576738	12.786906
13.935390	893.669031	12.791923
13.790757	899.867789	12.796941
14.041651	895.495560	12.801959
14.089719	913.811039	12.806976
14.160133	925.539899	12.811994
13.718915	926.593738	12.817011
14.003460	923.847813	12.822029
14.124561	917.687604	12.827047
14.084210	916.971312	12.832064
14.274310	921.160995	12.837082
14.445043	924.053497	12.842099
14.309511	915.045883	12.847117
14.421473	927.591915	12.852135
14.225438	926.776937	12.857152
14.209425	923.194461	12.862170
14.205846	930.065419	12.867187
14.273067	916.497370	12.872205
14.410743	927.493000	12.877223
14.411450	932.428741	12.882240
14.362654	921.416183	12.887258
14.240810	931.698226	12.892275
14.223389	931.145601	12.897293
14.668772	942.168769	12.902311
14.596334	941.192410	12.907328
14.359643	930.281871	12.912346
14.620746	925.188498	12.917363
14.427907	922.476344	12.922381
14.722424	927.189321	12.927399
14.523227	933.554433	12.932416
14.818706	927.994916	12.937434
14.838184	922.787921	12.942451
14.462869	919.189157	12.947469
14.556742	924.886642	12.952487
14.293135	929.491404	12.957504
14.799994	926.306695	12.962522
14.965016	920.287930	12.967539
14.458701	926.944161	12.972557
14.447855	924.588507	12.977575
15.114582	930.262511	12.982592
14.909060	932.365039	12.987610
14.849187	928.306586	12.992627
14.571858	925.677099	12.997645
14.701934	916.122930	13.002663
14.942189	926.610173	13.007680
14.781796	923.438490	13.012698
14.761400	923.056749	13.017715
14.711624	920.640922	13.022733
14.957302	915.142862	13.027751
14.411338	915.471484	13.032768
14.557084	932.162187	13.037786
15.006206	943.415148	13.042803
14.601011	943.488180	13.047821
15.054374	948.400342	13.052839
14.652169	947.844888	13.057856
14.811858	947.352877	13.062874
14.962289	951.678173	13.067891
14.956109	952.405070	13.072909
15.040987	950.832849	13.077927
14.743310	951.435001	13.082944
14.966732	940.357688	13.087962
15.036944	945.213114	13.092979
14.940753	937.796194	13.097997
15.153244	939.804825	13.103015
15.183185	943.000262	13.108032
15.190603	937.722567	13.113050
15.133842	935.361482	13.118067
15.059953	942.637945	13.123085
14.979175	933.937329	13.128103
15.150899	942.772177	13.133120
14.961817	946.244934	13.138138
15.080735	945.308022	13.143155
14.980885	951.846926	13.148173
15.029695	941.920461	13.153191
14.868023	947.945176	13.158208
14.980695	951.793541	13.163226
14.914606	947.322639	13.168243
14.854721	950.996064	13.173261
15.213316	949.144267	13.178279
14.985752	945.667518	13.183296
15.137223	953.262132	13.188314
15.540528	962.603515	13.193331
15.407588	964.252853	13.198349
15.382189	948.401816	13.203367
15.471962	939.393604	13.208384
15.425787	938.551988	13.213402
15.548863	939.574219	13.218419
15.218661	943.788623	13.223437
15.555168	940.731591	13.228455
15.263435	941.862997	13.233472
15.524606	944.125938	13.238490
15.478112	934.930791	13.243507
15.220932	940.380321	13.248525
15.569630	931.779676	13.253543
15.667136	941.127935	13.258560
15.585322	946.701472	13.263578
15.616447	941.319073	13.268595
15.612600	941.234546	13.273613
15.830263	940.178019	13.278631
15.769864	937.814348	13.283648
15.893085	936.406538	13.288666
15.560950	934.211678	13.293683
15.440827	939.551370	13.298701
15.464704	931.112074	13.303719
15.713338	927.838433	13.308736
15.657001	929.980704	13.313754
15.925495	927.019538	13.318771
15.738237	941.613281	13.323789
15.837278	936.333854	13.328807
15.835264	936.864434	13.333824
16.020330	935.712027	13.338842
15.937691	937.154661	13.343859
15.786455	928.297826	13.348877
15.627737	902.510966	13.353895
15.281841	906.431170	13.358912
15.447188	920.098631	13.363930
15.920368	921.984362	13.368947
15.769761	928.354482	13.373965
15.954272	930.023507	13.378983
15.620594	937.763557	13.384000
15.649844	941.056934	13.389018
15.733447	928.975878	13.394035
15.460224	936.968393	13.399053
15.772239	929.165620	13.404071
15.489074	939.917921	13.409088
15.897585	927.075889	13.414106
15.624259	928.636764	13.419123
15.353612	945.607319	13.424141
16.028049	957.487719	13.429159
16.260924	954.052437	13.434176
15.835019	960.648744	13.439194
15.979799	964.286948	13.444211
15.702347	972.175998	13.449229
16.235866	962.773191	13.454247
16.255678	960.753564	13.459264
16.244289	966.761050	13.464282
16.083803	962.917174	13.469299
15.617797	961.734230	13.474317
15.975711	959.320794	13.479335
16.322931	959.458977	13.484352
16.463297	965.291204	13.489370
16.323274	958.625930	13.494387
16.094144	965.986687	13.499405
16.452362	958.899356	13.504423
16.308278	944.730063	13.509440
16.013434	939.449232	13.514458
16.375540	948.560373	13.519475
15.827679	956.529654	13.524493
16.359478	948.641942	13.529511
16.291991	967.303792	13.534528
16.242460	963.325764	13.539546
16.544572	961.631142	13.544563
16.422898	964.506348	13.549581
16.109482	953.557322	13.554599
16.180066	954.669830	13.559616
15.953705	961.629356	13.564634
15.892131	959.474154	13.569651
15.589004	968.620105	13.574669
15.991740	965.830408	13.579687
16.372364	966.591376	13.584704
16.426957	969.290640	13.589722
16.550223	969.934137	13.594739
16.318604	979.274022	13.599757
16.461452	978.642635	13.604775
16.843708	979.352854	13.609792
16.345175	979.857086	13.614810
16.739031	978.987550	13.619827
16.718607	982.941984	13.624845
16.527044	975.748279	13.629863
16.739639	956.360082	13.634880
16.706598	967.139483	13.639898
16.454212	955.716980	13.644915
16.450012	968.325423	13.649933
16.506739	965.258573	13.654951
16.411698	972.238554	13.659968
17.016818	982.760182	13.664986
16.795582	976.041352	13.670003
16.478421	976.646557	13.675021
16.534345	986.102342	13.680039
16.983211	988.885003	13.685056
16.499136	989.585791	13.690074
16.804864	981.301131	13.695091
16.990968	989.635121	13.700109
16.445946	988.925313	13.705127
17.001936	982.750593	13.710144
16.623618	981.295127	13.715162
16.817519	985.380086	13.720179
16.670055	990.171798	13.725197
16.886649	982.052585	13.730215
17.087333	981.134419	13.735232
16.439413	995.270196	13.740250
16.785993	976.353302	13.745267
16.610070	994.180083	13.750285
17.087795	988.052339	13.755303
16.884427	981.561086	13.760320
16.994032	976.775464	13.765338
17.373858	987.698476	13.770355
16.966439	980.223003	13.775373
17.133480	982.371307	13.780391
16.980617	981.262376	13.785408
17.118972	984.481861	13.790426
16.675850	977.557949	13.795443
17.069321	986.449595	13.800461
17.120563	991.355344	13.805479
17.302046	975.323543	13.810496
16.832457	980.872639	13.815514
17.120072	974.777842	13.820531
16.775126	989.424734	13.825549
16.836157	980.746059	13.830567
17.149313	987.147681	13.835584
17.076728	997.166417	13.840602
17.283827	1006.538565	13.845619
17.260385	1001.117361	13.850637
17.299970	1011.355221	13.855655
17.399627	1006.129327	13.860672
17.852798	1012.505864	13.865690
17.632445	1001.879906	13.870707
17.171376	993.598617	13.875725
17.352705	980.656439	13.880743
17.775043	979.769817	13.885760
17.371161	982.559852	13.890778
17.229719	983.440490	13.895795
17.125736	971.483472	13.900813
17.249043	985.962319	13.905831
17.762858	1001.847475	13.910848
17.508449	995.755543	13.915866
17.271093	977.605497	13.920883
17.471544	988.929008	13.925901
17.257645	1006.496658	13.930919
17.539741	990.890901	13.935936
17.383738	1005.908999	13.940954
17.894121	1011.534940	13.945971
18.074820	1008.417100	13.950989
17.759580	999.181974	13.956007
17.715735	988.540992	13.961024
17.320069	987.741509	13.966042
17.576116	970.931151	13.971059
17.457126	983.636488	13.976077
17.452572	1004.873178	13.981095
18.029729	1009.889040	13.986112
17.664034	1011.013103	13.991130
17.679600	1011.705036	13.996147
17.658425	1010.095777	14.001165
17.214983	1006.163679	14.006183
17.589919	1009.958340	14.011200
17.495901	1016.603655	14.016218
17.657336	1002.563176	14.021235
17.752076	1002.674645	14.026253
17.503082	1012.083542	14.031271
17.332383	1002.762650	14.036288
17.465735	1027.547059	14.041306
17.673455	1022.834418	14.046323
18.165172	1031.754876	14.051341
18.362255	1040.181845	14.056359
18.276462	1032.946298	14.061376
17.955983	1014.922850	14.066394
18.117633	1013.297569	14.071411
17.824578	1008.713887	14.076429
17.874900	1025.094572	14.081447
18.233290	1022.592688	14.086464
18.103645	1026.851430	14.091482
17.982664	1035.189373	14.096499
18.421196	1026.751338	14.101517
17.941706	1021.483634	14.106535
18.316322	1014.788198	14.111552
17.616152	1016.321282	14.116570
18.067699	1013.104198	14.121587
18.403676	1023.961517	14.126605
18.214027	1028.134984	14.131623
18.136788	1023.271325	14.136640
18.348566	1027.142049	14.141658
18.427365	1018.463727	14.146675
18.263485	1032.536317	14.151693
18.166091	1035.871645	14.156711
18.455742	1026.352377	14.161728
18.358515	1030.211555	14.166746
18.460808	1020.355563	14.171763
18.298390	1010.739872	14.176781
18.235192	1020.823425	14.181799
18.221763	1019.137210	14.186816
18.384719	1015.968498	14.191834
18.246047	1025.865058	14.196851
18.349014	1022.582665	14.201869
17.977037	1027.920817	14.206887
18.505233	1026.395898	14.211904
18.371640	1025.706834	14.216922
18.313697	1025.921123	14.221939
18.504848	1020.523095	14.226957
18.150199	1028.452668	14.231975
18.701733	1027.561580	14.236992
18.611113	1025.912707	14.242010
18.312289	1026.016411	14.247027
18.690246	1026.982932	14.252045
18.262508	1026.103264	14.257063
18.207787	1024.155268	14.262080
18.191385	1038.261561	14.267098
18.274204	1048.729361	14.272115
18.621930	1043.795956	14.277133
18.565852	1048.200970	14.282151
18.603414	1045.146577	14.287168
18.634097	1051.781833	14.292186
18.866021	1042.120119	14.297203
18.788943	1042.498357	14.302221
18.729960	1050.144922	14.307239
18.699572	1044.699545	14.312256
18.819285	1040.893803	14.317274
18.663707	1043.070571	14.322291
19.310032	1048.261804	14.327309
18.902515	1053.605532	14.332327
19.112525	1043.672688	14.337344
19.050808	1045.654865	14.342362
18.758246	1044.151242	14.347379
18.799082	1043.538992	14.352397
18.746349	1052.598415	14.357415
18.714881	1051.669281	14.362432
19.318411	1046.118269	14.367450
19.137359	1047.652073	14.372467
19.055370	1044.581696	14.377485
18.851334	1053.122014	14.382503
18.979035	1044.470733	14.387520
19.265949	1039.786705	14.392538
19.045262	1033.676852	14.397555
19.116391	1043.979219	14.402573
19.145277	1037.726118	14.407591
19.085520	1034.503933	14.412608
19.245381	1038.811993	14.417626
19.267367	1039.080033	14.422643
19.329732	1038.224562	14.427661
18.983120	1047.844438	14.432679
18.976761	1048.501937	14.437696
19.450346	1065.864097	14.442714
19.185381	1064.823220	14.447731
19.436114	1062.284548	14.452749
19.522849	1078.410262	14.457767
19.344833	1064.880524	14.462784
19.201244	1057.423643	14.467802
19.150820	1066.574233	14.472819
19.429702	1063.611417	14.477837
19.222045	1072.329041	14.482855
19.402738	1066.443475	14.487872
19.664414	1072.203081	14.492890
19.614512	1071.106416	14.497907
19.635471	1070.860206	14.502925
19.779502	1074.075662	14.507943
19.605230	1066.759287	14.512960
19.377713	1073.239342	14.517978
19.828986	1067.368187	14.522995
19.634116	1055.649422	14.528013
19.127403	1050.663692	14.533031
19.529336	1058.055002	14.538048
19.702255	1065.576875	14.543066
19.338700	1058.346967	14.548083
19.714600	1058.294460	14.553101
19.563727	1064.977103	14.558119
19.736580	1063.211203	14.563136
19.708819	1074.561058	14.568154
19.372082	1064.429837	14.573171
19.702733	1069.888293	14.578189
19.611865	1068.091127	14.583207
19.692141	1060.741184	14.588224
19.797592	1072.401533	14.593242
19.693519	1064.689142	14.598259
20.017536	1065.648337	14.603277
19.604733	1067.218453	14.608295
19.352452	1065.642243	14.613312
19.740432	1082.957871	14.618330
19.811383	1090.833410	14.623347
20.199370	1093.581444	14.628365
19.952433	1096.728770	14.633383
19.838572	1092.322123	14.638400
20.432870	1085.118856	14.643418
20.340587	1096.213739	14.648435
20.148462	1087.994411	14.653453
20.322446	1084.183312	14.658471
20.425853	1069.747918	14.663488
20.034596	1059.476916	14.668506
19.817563	1068.536843	14.673523
20.448139	1054.069359	14.678541
19.939529	1058.652579	14.683559
20.255215	1055.725025	14.688576
20.144924	1049.957641	14.693594
20.066165	1074.036871	14.698611
20.328324	1074.336710	14.703629
20.413041	1087.433093	14.708647
20.364221	1069.187140	14.713664
20.387989	1066.961747	14.718682
20.312712	1074.655058	14.723699
20.385917	1066.034396	14.728717
20.319049	1082.386157	14.733735
20.273060	1089.090247	14.738752
20.364525	1086.122078	14.743770
20.212398	1083.750668	14.748787
20.536640	1080.622948	14.753805
20.299293	1086.422875	14.758823
20.335736	1083.466483	14.763840
20.691435	1077.793341	14.768858
20.811624	1085.023673	14.773875
20.848317	1072.148274	14.778893
20.637875	1091.571129	14.783911
20.373862	1089.479189	14.788928
20.957645	1075.694380	14.793946
20.489010	1075.894120	14.798963
20.423196	1076.434699	14.803981
20.484907	1080.527769	14.808999
20.573458	1089.382033	14.814016
20.322181	1077.874068	14.819034
20.332636	1084.291594	14.824051
20.945737	1079.303977	14.829069
20.656748	1072.573634	14.834087
20.685588	1078.186681	14.839104
20.958762	1079.150688	14.844122
20.730503	1078.119838	14.849139
20.339080	1082.523753	14.854157
20.575410	1083.534559	14.859175
20.967972	1080.560241	14.864192
21.090009	1070.824208	14.869210
21.119920	1075.793284	14.874227
20.788476	1076.265027	14.879245
21.159086	1074.808977	14.884263
21.124498	1085.683368	14.889280
20.989837	1079.847208	14.894298
20.742312	1087.166714	14.899315
20.839581	1075.373760	14.904333
21.105429	1077.288838	14.909351
21.061257	1085.709447	14.914368
20.847855	1077.872165	14.919386
20.611511	1082.308588	14.924403
21.312519	1098.669443	14.929421
21.451922	1095.731632	14.934439
20.969087	1099.282003	14.939456
21.542984	1095.638624	14.944474
21.691455	1097.471106	14.949491
21.499457	1084.498981	14.954509
21.463159	1079.098702	14.959527
21.353237	1071.522927	14.964544
21.152872	1076.572266	14.969562
20.938210	1079.389475	14.974579
21.254252	1072.753689	14.979597
21.058271	1076.956562	14.984615
20.917065	1084.852717	14.989632
21.616593	1093.257794	14.994650
21.563553	1100.789838	14.999667
21.407337	1100.388346	15.004685
21.695733	1103.234039	15.009703
21.260908	1102.387036	15.014720
21.376788	1099.399260	15.019738
21.340205	1111.479531	15.024755
21.397079	1102.769890	15.029773
21.727709	1100.568999	15.034791
21.463370	1107.048523	15.039808
21.676914	1104.395748	15.044826
21.483389	1114.815363	15.049843
21.660889	1107.185072	15.054861
21.769056	1107.206074	15.059879
21.787606	1102.573545	15.064896
21.963585	1102.050574	15.069914
21.378392	1108.230066	15.074931
21.565805	1100.680278	15.079949
21.377610	1105.579391	15.084967
21.664266	1105.269461	15.089984
21.636166	1095.462261	15.095002
21.364513	1101.368556	15.100019
21.736221	1101.572334	15.105037
22.073697	1098.527746	15.110055
21.941753	1100.956446	15.115072
22.024430	1099.725395	15.120090
21.724470	1108.725750	15.125107
21.740768	1109.666888	15.130125
21.821965	1111.607745	15.135143
21.734055	1116.737308	15.140160
22.028753	1129.889187	15.145178
21.788656	1138.189035	15.150195
21.853365	1132.861279	15.155213
22.282487	1135.123178	15.160231
22.003570	1137.360309	15.165248
22.162041	1135.249506	15.170266
22.151195	1126.683011	15.175283
22.104217	1129.155208	15.180301
22.317070	1121.251121	15.185319
22.045313	1134.643239	15.190336
22.274631	1128.058892	15.195354
22.258566	1132.713285	15.200371
22.234520	1130.425947	15.205389
22.427662	1124.907651	15.210407
22.029355	1131.512319	15.215424
22.124839	1120.508591	15.220442
21.996248	1129.504198	15.225459
22.307856	1129.600624	15.230477
22.341897	1117.318917	15.235495
21.870061	1131.405120	15.240512
22.010203	1135.552187	15.245530
22.199340	1151.958578	15.250547
22.231978	1149.548743	15.255565
22.706124	1149.749095	15.260583
22.571592	1158.852948	15.265600
22.216569	1151.246112	15.270618
22.212595	1157.836344	15.275635
22.315114	1155.668031	15.280653
22.517001	1151.284484	15.285671
22.504379	1155.262981	15.290688
22.494271	1153.140718	15.295706
22.746442	1152.015654	15.300723
22.771280	1144.011623	15.305741
22.807034	1145.858615	15.310759
22.430732	1154.050419	15.315776
22.711420	1143.844506	15.320794
22.538852	1157.732356	15.325811
22.972271	1168.315713	15.330829
22.931343	1171.960966	15.335847
22.861936	1161.920352	15.340864
23.048413	1155.175444	15.345882
22.898881	1158.313830	15.350899
23.158021	1162.947204	15.355917
23.176261	1148.443037	15.360935
22.718845	1151.241485	15.365952
22.763499	1150.701219	15.370970
22.688541	1156.043366	15.375987
22.916939	1169.069958	15.381005
23.377595	1170.137143	15.386023
23.321407	1188.030566	15.391040
23.253310	1170.232514	15.396058
23.143372	1154.978383	15.401075
22.925164	1159.746509	15.406093
23.296607	1159.628427	15.411111
23.028495	1158.234576	15.416128
23.264947	1151.942601	15.421146
23.037875	1163.734008	15.426163
22.966663	1167.791117	15.431181
23.044738	1171.054795	15.436199
23.007215	1175.595793	15.441216
23.300585	1177.705392	15.446234
23.605716	1173.633878	15.451251
23.632322	1180.717960	15.456269
23.781939	1175.765065	15.461287
23.194805	1181.105414	15.466304
23.130977	1174.033631	15.471322
23.189251	1175.368996	15.476339
23.286293	1169.812094	15.481357
23.636388	1169.577432	15.486375
23.386721	1186.096789	15.491392
23.417583	1178.675642	15.496410
23.543742	1176.323736	15.501427
23.358533	1172.250151	15.506445
23.909382	1166.334959	15.511463
23.338582	1177.754183	15.516480
23.496877	1169.145387	15.521498
23.426631	1179.192262	15.526515
23.490959	1180.621356	15.531533
23.805646	1164.502241	15.536551
23.430164	1169.979844	15.541568
23.806606	1181.701950	15.546586
23.805277	1181.932618	15.551603
23.574823	1191.707946	15.556621
24.242250	1193.904112	15.561639
23.842613	1187.320455	15.566656
23.894669	1177.756279	15.571674
23.388473	1174.496716	15.576691
23.669301	1183.709078	15.581709
23.994094	1191.478616	15.586727
23.872218	1199.030954	15.591744
24.417719	1197.178251	15.596762
24.244812	1198.041737	15.601779
24.101314	1192.320537	15.606797
24.355606	1183.747188	15.611815
24.138798	1174.364000	15.616832
24.109155	1165.500620	15.621850
24.022900	1165.605734	15.626867
23.970030	1168.302930	15.631885
24.106666	1177.323278	15.636903
24.291180	1191.205702	15.641920
24.159412	1188.143100	15.646938
24.491658	1190.641098	15.651955
24.311722	1190.363245	15.656973
24.577411	1166.488264	15.661991
24.018459	1169.192167	15.667008
24.005680	1173.268525	15.672026
24.366062	1188.215335	15.677043
24.263403	1193.296737	15.682061
24.425669	1190.020802	15.687079
24.314715	1192.427290	15.692096
24.645455	1190.018081	15.697114
24.410733	1198.266620	15.702131
23.915488	1198.363229	15.707149
24.498619	1181.621351	15.712167
24.418044	1191.130190	15.717184
24.709872	1183.911158	15.722202
24.716810	1187.517355	15.727219
24.726184	1188.390152	15.732237
24.470213	1191.396893	15.737255
24.276967	1185.626683	15.742272
24.471945	1181.793340	15.747290
24.586656	1188.424950	15.752307
24.507086	1189.074989	15.757325
24.547239	1190.473157	15.762343
24.787227	1209.866594	15.767360
25.186445	1201.945894	15.772378
25.160497	1195.111174	15.777395
24.911781	1190.242777	15.782413
24.973609	1174.409432	15.787431
25.044366	1173.685189	15.792448
24.808277	1175.675765	15.797466
24.992756	1172.074450	15.802483
25.037591	1173.957893	15.807501
25.389918	1172.261696	15.812519
24.949267	1179.624122	15.817536
24.931968	1180.753570	15.822554
25.262944	1181.512860	15.827571
25.214641	1178.071096	15.832589
25.353638	1175.521513	15.837607
25.071441	1173.820588	15.842624
25.211667	1177.377497	15.847642
25.218243	1172.286063	15.852659
24.856700	1180.279900	15.857677
25.185103	1172.913125	15.862695
24.871415	1175.963622	15.867712
25.021099	1177.088999	15.872730
25.508676	1177.842687	15.877747
25.292204	1174.850165	15.882765
25.393487	1170.018457	15.887783
25.267202	1174.185186	15.892800
25.304276	1177.246999	15.897818
25.737585	1185.706456	15.902835
25.307825	1184.344241	15.907853
25.504281	1181.624703	15.912871
25.343048	1179.046417	15.917888
25.657848	1196.960621	15.922906
25.717082	1189.310954	15.927923
25.617185	1193.577698	15.932941
25.855919	1176.305941	15.937959
25.486388	1172.015074	15.942976
25.313004	1172.973312	15.947994
25.404538	1187.425740	15.953011
25.591572	1207.616450	15.958029
25.983022	1196.825088	15.963047
25.769640	1202.637076	15.968064
25.633225	1204.369034	15.973082
25.785876	1193.567750	15.978099
25.699057	1196.724720	15.983117
25.937347	1198.751430	15.988135
26.084797	1193.641074	15.993152
25.935927	1194.595471	15.998170
26.093854	1200.428180	16.003187
25.905844	1208.158147	16.008205
25.938543	1201.345794	16.013223
25.868930	1201.132709	16.018240
25.870130	1201.441879	16.023258
25.972504	1193.144801	16.028275
26.181482	1204.344032	16.033293
25.918572	1203.028260	16.038311
26.319788	1197.540460	16.043328
26.069431	1200.659935	16.048346
25.999890	1194.523190	16.053363
25.693546	1192.305321	16.058381
25.856327	1194.851964	16.063399
25.757936	1200.816354	16.068416
26.118388	1210.918846	16.073434
26.256482	1220.238800	16.078451
26.502480	1228.686599	16.083469
26.177160	1222.671973	16.088487
26.342138	1218.900129	16.093504
26.178416	1222.583567	16.098522
26.471334	1228.603425	16.103539
26.657676	1224.490549	16.108557
26.844101	1220.424999	16.113575
26.392212	1218.573926	16.118592
26.596675	1219.965287	16.123610
27.033932	1216.254928	16.128627
26.295454	1206.568437	16.133645
26.756027	1207.389476	16.138663
26.329800	1213.301091	16.143680
26.434609	1225.394001	16.148698
26.710538	1223.220602	16.153715
26.389971	1234.458639	16.158733
26.531967	1213.496954	16.163751
26.529302	1219.825062	16.168768
26.505353	1223.335117	16.173786
26.877992	1213.988946	16.178803
26.607118	1223.246743	16.183821
26.762171	1221.985407	16.188839
26.821200	1217.958754	16.193856
26.504802	1218.289282	16.198874
26.595384	1223.302544	16.203891
27.213482	1246.464908	16.208909
27.087811	1240.194925	16.213927
27.290493	1226.737965	16.218944
26.832080	1225.515941	16.223962
27.195766	1216.095429	16.228979
26.890795	1229.322403	16.233997
27.025887	1232.230007	16.239015
27.102995	1246.422803	16.244032
27.437276	1247.001690	16.249050
27.426373	1230.842007	16.254067
27.124963	1226.673003	16.259085
27.278992	1216.755147	16.264103
27.401646	1219.491123	16.269120
26.839694	1214.264684	16.274138
27.425565	1222.031201	16.279155
27.518603	1240.541947	16.284173
27.303941	1239.919227	16.289191
27.349821	1230.722078	16.294208
26.852198	1240.056437	16.299226
27.095666	1242.432648	16.304243
27.071763	1247.350241	16.309261
27.366898	1240.802879	16.314279
27.343508	1241.911195	16.319296
27.211463	1244.106391	16.324314
27.554843	1240.619026	16.329331
27.482858	1240.652474	16.334349
27.653349	1255.827917	16.339367
27.708696	1257.024886	16.344384
27.710888	1261.130478	16.349402
27.929022	1257.018925	16.354419
27.965785	1259.632660	16.359437
27.742456	1242.303843	16.364455
27.491176	1233.352074	16.369472
27.723723	1251.364430	16.374490
27.705874	1263.012664	16.379507
27.508619	1268.036321	16.384525
28.059204	1258.176234	16.389543
28.168029	1257.316630	16.394560
28.279451	1259.186493	16.399578
28.267455	1249.708057	16.404595
28.112035	1261.617695	16.409613
27.968178	1259.178691	16.414631
28.111723	1244.967249	16.419648
27.745214	1259.671391	16.424666
28.326615	1262.038840	16.429683
27.791328	1261.920808	16.434701
27.814851	1267.250713	16.439719
28.498799	1263.192412	16.444736
27.992359	1265.963843	16.449754
28.031047	1249.528120	16.454771
28.222486	1254.705476	16.459789
28.112744	1257.894452	16.464807
28.603767	1252.414656	16.469824
28.615746	1252.573809	16.474842
28.343908	1254.121854	16.479859
28.092529	1262.922163	16.484877
28.364340	1264.063126	16.489895
28.107290	1258.514336	16.494912
28.001128	1264.606203	16.499930
28.744004	1273.282296	16.504947
28.550814	1283.020276	16.509965
28.399571	1296.422036	16.514983
28.618595	1279.184828	16.520000
28.673739	1284.856937	16.525018
28.802418	1284.322437	16.530035
28.778749	1282.776663	16.535053
28.354813	1288.807869	16.540071
28.868562	1278.123533	16.545088
28.706044	1286.673237	16.550106
28.933951	1271.580676	16.555123
28.706390	1283.908745	16.560141
28.701139	1288.984380	16.565159
29.124646	1283.240587	16.570176
28.854177	1286.972323	16.575194
28.692189	1279.047997	16.580211
28.630691	1290.220231	16.585229
28.761168	1284.806383	16.590247
28.951393	1274.431525	16.595264
28.657944	1273.174183	16.600282
28.825593	1282.688363	16.605299
28.782913	1286.624259	16.610317
28.883959	1294.043875	16.615335
29.218732	1290.220165	16.620352
29.195583	1294.484376	16.625370
29.268926	1290.518582	16.630387
29.310355	1293.219957	16.635405
29.685351	1293.729348	16.640423
29.493994	1293.803591	16.645440
29.242470	1282.125113	16.650458
29.653806	1284.667540	16.655475
29.317010	1279.544665	16.660493
29.100666	1276.501610	16.665511
29.342352	1278.808675	16.670528
29.187647	1282.007856	16.675546
29.499441	1274.261775	16.680563
29.590603	1295.029360	16.685581
29.498587	1290.808597	16.690599
29.842797	1282.028601	16.695616
29.329043	1288.717689	16.700634
29.616693	1290.509449	16.705651
29.926879	1294.544700	16.710669
29.511887	1289.746511	16.715687
29.799674	1285.699781	16.720704
29.706267	1286.402486	16.725722
29.327715	1289.220158	16.730739
29.314757	1294.511605	16.735757
29.409690	1288.254380	16.740775
29.683320	1299.462477	16.745792
29.572442	1309.632561	16.750810
29.904219	1313.086898	16.755827
29.885602	1312.998371	16.760845
29.853447	1314.294264	16.765863
29.915546	1310.336540	16.770880
30.170621	1316.696886	16.775898
29.816940	1300.811762	16.780915
30.099417	1310.598311	16.785933
29.811355	1309.908190	16.790951
30.013150	1304.868186	16.795968
29.860891	1321.157802	16.800986
30.296028	1309.927164	16.806003
30.397739	1316.447245	16.811021
30.398135	1326.928121	16.816039
30.254017	1313.875742	16.821056
30.127009	1320.980792	16.826074
30.024827	1327.886288	16.831091
30.386608	1329.780050	16.836109
30.266408	1338.039114	16.841127
30.467920	1339.560341	16.846144
30.330664	1347.036252	16.851162
30.394797	1335.800608	16.856179
30.953533	1324.212910	16.861197
30.900032	1335.232434	16.866215
31.039586	1326.225694	16.871232
30.889368	1330.724426	16.876250
31.146429	1325.192899	16.881267
30.842105	1315.491976	16.886285
30.653991	1304.153856	16.891303
30.904056	1292.062254	16.896320
30.966184	1301.321566	16.901338
30.512707	1293.635417	16.906355
30.659219	1294.262662	16.911373
30.698466	1299.829964	16.916391
30.884693	1304.518982	16.921408
30.853959	1316.030408	16.926426
30.711661	1315.822398	16.931443
31.300251	1314.534157	16.936461
30.811368	1326.492929	16.941479
31.189929	1312.383472	16.946496
31.056155	1318.889955	16.951514
31.202349	1314.158473	16.956531
31.287728	1313.523455	16.961549
30.878640	1324.955306	16.966567
31.296680	1319.023002	16.971584
31.216690	1317.722744	16.976602
31.508755	1322.467771	16.981619
31.477992	1323.334239	16.986637
31.247945	1323.928962	16.991655
31.528229	1316.695905	16.996672
31.433295	1323.019571	17.001690
31.588016	1318.362495	17.006707
31.784178	1319.237592	17.011725
31.238815	1308.211074	17.016743
31.517402	1310.581792	17.021760
31.418504	1323.334717	17.026778
31.599871	1315.479660	17.031795
31.493539	1315.483775	17.036813
31.354037	1322.527665	17.041831
31.782286	1312.876072	17.046848
31.418221	1316.041786	17.051866
31.148710	1323.418484	17.056883
31.457503	1312.687342	17.061901
31.248337	1317.763375	17.066919
31.535192	1325.005563	17.071936
31.942801	1335.226974	17.076954
31.878391	1336.164990	17.081971
31.767261	1336.987244	17.086989
31.776940	1349.454920	17.092007
31.675809	1349.975794	17.097024
31.802417	1345.452509	17.102042
31.732136	1351.709204	17.107059
31.944574	1341.015234	17.112077
31.944177	1350.085544	17.117095
31.878009	1346.403539	17.122112
31.785421	1351.246712	17.127130
31.852019	1360.559006	17.132147
32.317536	1369.073468	17.137165
32.324554	1369.735194	17.142183
32.404397	1365.402276	17.147200
32.495408	1368.704991	17.152218
32.457562	1369.607287	17.157235
32.690067	1371.874775	17.162253
32.275206	1362.733967	17.167271
32.455903	1358.148553	17.172288
32.586530	1361.858488	17.177306
32.391814	1365.221750	17.182323
32.355432	1363.409705	17.187341
32.319599	1376.771351	17.192359
32.443848	1365.620948	17.197376
32.722322	1374.215213	17.202394
32.414962	1364.587325	17.207411
32.584805	1357.945937	17.212429
32.501887	1367.212230	17.217447
32.187360	1355.218513	17.222464
32.540093	1365.369641	17.227482
32.113888	1361.147571	17.232499
33.002530	1377.403544	17.237517
32.867065	1393.498082	17.242535
32.974534	1389.788863	17.247552
33.085823	1383.579537	17.252570
32.695842	1394.042719	17.257587
33.053781	1388.214487	17.262605
32.835738	1401.835085	17.267623
32.698782	1387.727442	17.272640
32.909505	1387.530395	17.277658
32.758499	1390.176724	17.282675
33.116681	1392.427680	17.287693
32.934907	1384.247621	17.292711
33.075637	1383.809064	17.297728
33.149042	1385.931061	17.302746
33.361612	1381.826663	17.307763
33.330538	1381.601226	17.312781
32.978494	1386.409317	17.317799
33.520168	1401.681369	17.322816
33.674611	1412.996578	17.327834
33.522288	1410.139139	17.332851
33.764460	1399.282677	17.337869
33.336477	1390.693046	17.342887
33.451477	1383.482703	17.347904
33.497909	1400.372450	17.352922
33.329750	1395.791190	17.357939
33.688643	1405.827762	17.362957
33.864675	1403.938249	17.367975
34.001774	1410.762103	17.372992
34.073333	1406.941737	17.378010
33.557258	1406.262090	17.383027
34.124187	1406.993888	17.388045
33.601194	1410.301290	17.393063
34.174207	1408.927117	17.398080
34.074665	1402.413131	17.403098
33.878171	1397.981484	17.408115
34.176023	1398.225242	17.413133
34.194764	1400.917564	17.418151
34.073282	1385.617705	17.423168
34.076380	1377.635911	17.428186
33.817852	1385.519020	17.433203
33.932652	1384.491209	17.438221
34.044450	1404.024868	17.443239
33.920715	1405.221502	17.448256
34.109468	1404.863788	17.453274
33.805744	1404.444373	17.458291
33.826652	1396.380881	17.463309
33.603196	1408.408578	17.468327
34.376173	1418.796864	17.473344
34.348509	1430.806523	17.478362
34.426093	1442.768141	17.483379
34.808570	1425.978575	17.488397
34.545110	1441.796550	17.493415
34.239374	1435.551555	17.498432
34.890840	1424.997041	17.503450
34.708193	1430.548656	17.508467
34.877813	1426.283712	17.513485
35.054669	1428.528367	17.518503
34.786515	1425.259864	17.523520
34.922361	1417.465546	17.528538
34.798178	1409.708817	17.533555
34.814888	1399.979640	17.538573
34.907402	1405.415547	17.543591
34.792344	1414.305030	17.548608
34.907799	1413.895681	17.553626
34.423695	1428.908732	17.558643
34.498507	1416.869752	17.563661
34.493557	1419.417459	17.568679
34.997387	1428.389871	17.573696
34.860903	1418.902447	17.578714
34.714416	1439.054152	17.583731
35.029186	1430.726841	17.588749
35.165562	1441.568350	17.593767
35.148793	1455.551948	17.598784
35.720654	1451.779423	17.603802
35.291346	1436.196376	17.608819
35.449763	1432.715863	17.613837
35.376400	1427.365469	17.618855
35.393226	1426.823243	17.623872
35.578654	1421.987751	17.628890
35.068061	1423.393329	17.633907
35.275863	1427.116433	17.638925
35.483925	1445.091794	17.643943
35.337912	1452.947836	17.648960
35.545540	1454.663784	17.653978
35.405253	1454.922539	17.658995
35.598958	1447.661968	17.664013
36.026062	1444.385519	17.669031
35.254190	1447.255372	17.674048
35.884334	1445.525090	17.679066
35.690378	1455.496824	17.684083
35.755772	1444.096805	17.689101
36.061728	1445.049384	17.694119
35.875552	1449.951430	17.699136
35.894818	1439.391814	17.704154
35.897504	1448.717324	17.709171
35.962830	1439.166709	17.714189
35.913340	1444.517576	17.719207
35.693632	1447.117871	17.724224
35.792530	1445.354053	17.729242
36.017845	1466.504781	17.734259
35.988660	1466.140184	17.739277
36.059873	1472.860770	17.744295
36.294015	1469.292642	17.749312
36.348193	1461.271248	17.754330
36.030202	1471.609580	17.759347
36.169291	1468.463464	17.764365
36.310665	1468.242567	17.769383
36.346297	1465.627082	17.774400
36.473203	1465.010800	17.779418
36.055205	1469.835559	17.784435
36.257815	1464.890061	17.789453
36.494945	1477.827144	17.794471
36.729247	1493.422002	17.799488
36.798991	1491.306124	17.804506
36.829899	1495.785986	17.809523
37.071291	1487.353376	17.814541
36.894237	1468.013052	17.819559
36.281129	1462.709343	17.824576
36.818349	1463.142827	17.829594
37.144713	1489.652351	17.834611
37.036595	1479.949000	17.839629
36.971092	1486.066130	17.844647
36.616634	1481.343616	17.849664
36.916481	1485.954916	17.854682
36.832771	1487.167377	17.859699
37.332488	1486.180242	17.864717
37.194337	1486.874186	17.869735
37.202141	1486.393335	17.874752
37.423542	1491.610249	17.879770
37.453417	1481.885276	17.884787
37.391958	1492.331758	17.889805
37.293066	1488.367658	17.894823
37.330918	1484.524153	17.899840
37.420689	1472.971966	17.904858
37.243514	1492.194374	17.909875
37.251487	1481.529200	17.914893
37.369407	1483.470655	17.919911
37.156779	1485.394470	17.924928
37.322865	1487.558765	17.929946
37.305699	1483.067440	17.934963
37.713472	1482.066308	17.939981
37.449047	1477.970348	17.944999
37.471338	1477.417796	17.950016
37.475035	1480.440708	17.955034
37.388734	1491.115154	17.960051
37.297172	1490.476293	17.965069
37.372327	1503.445085	17.970087
37.627368	1518.456017	17.975104
37.826573	1507.906039	17.980122
37.735240	1517.726023	17.985139
37.898274	1520.215865	17.990157
37.974002	1506.775430	17.995175
38.000620	1516.624272	18.000192
38.145411	1517.277041	18.005210
37.934577	1523.319120	18.010227
38.141865	1524.864706	18.015245
38.284183	1534.745925	18.020263
38.283420	1539.196045	18.025280
38.809351	1524.754047	18.030298
38.557221	1520.469949	18.035315
38.250509	1508.455968	18.040333
38.503416	1505.686509	18.045351
38.324845	1515.498068	18.050368
38.257819	1523.161875	18.055386
38.257796	1526.346331	18.060403
38.644836	1528.706398	18.065421
38.901698	1521.237076	18.070439
38.608285	1531.009829	18.075456
38.968626	1530.035061	18.080474
38.679787	1528.732794	18.085491
38.640565	1527.675455	18.090509
38.734195	1523.176229	18.095527
38.958043	1523.718777	18.100544
38.881856	1525.939972	18.105562
38.707896	1527.169731	18.110579
38.603863	1530.275805	18.115597
38.710920	1532.323116	18.120615
38.782184	1525.883314	18.125632
39.126360	1516.774987	18.130650
38.770666	1525.651733	18.135667
38.686993	1526.359234	18.140685
38.831735	1533.106194	18.145703
39.046114	1544.879180	18.150720
39.075177	1554.333163	18.155738
38.993565	1563.978069	18.160755
39.039902	1552.587279	18.165773
39.300168	1553.941520	18.170791
38.890559	1547.327731	18.175808
39.198771	1547.632988	18.180826
39.138896	1553.411571	18.185843
39.774097	1572.421571	18.190861
40.158384	1562.738861	18.195879
39.892492	1554.717078	18.200896
39.495113	1548.906146	18.205914
40.061620	1531.033553	18.210931
39.894846	1540.584487	18.215949
39.873121	1535.361677	18.220967
39.731215	1542.491241	18.225984
39.642429	1535.653612	18.231002
39.677657	1540.700884	18.236019
39.857226	1542.878853	18.241037
39.979366	1543.235355	18.246055
39.822590	1541.568395	18.251072
39.972961	1538.556206	18.256090
40.029703	1537.613226	18.261107
39.984760	1536.436856	18.266125
40.208533	1531.778373	18.271143
40.007754	1538.257561	18.276160
40.333662	1535.931120	18.281178
40.269644	1543.786979	18.286195
39.785205	1541.246656	18.291213
40.217009	1544.003676	18.296231
40.090901	1560.857488	18.301248
40.197148	1564.738552	18.306266
40.448460	1559.810645	18.311283
40.336542	1566.695666	18.316301
40.309077	1556.682975	18.321319
40.372025	1565.806589	18.326336
40.326405	1568.979261	18.331354
40.180979	1564.094579	18.336371
40.307196	1565.289933	18.341389
40.641317	1588.285784	18.346407
40.859471	1590.798560	18.351424
40.791390	1582.158758	18.356442
40.768770	1585.791759	18.361459
40.931078	1594.233908	18.366477
41.125087	1582.094086	18.371495
41.233947	1589.742987	18.376512
41.017719	1585.371193	18.381530
41.204359	1574.267692	18.386547
41.228077	1585.420446	18.391565
41.326899	1582.315335	18.396583
40.863101	1576.382249	18.401600
41.590058	1578.244072	18.406618
41.450826	1567.819673	18.411635
41.073344	1560.317172	18.416653
41.439790	1551.208495	18.421671
41.557699	1576.728272	18.426688
41.300691	1564.207821	18.431706
41.659944	1566.060979	18.436723
41.580729	1569.841707	18.441741
41.369453	1561.558885	18.446759
41.151660	1564.812184	18.451776
41.277341	1572.647802	18.456794
41.468411	1580.302755	18.461811
41.299182	1575.491229	18.466829
41.718174	1581.185325	18.471847
41.519102	1586.818460	18.476864
41.251634	1581.946582	18.481882
41.598696	1581.204279	18.486899
41.401496	1594.654490	18.491917
41.501747	1596.399899	18.496935
41.607679	1606.264768	18.501952
41.552755	1596.145897	18.506970
41.947404	1593.792898	18.511987
42.194418	1602.818260	18.517005
42.293215	1601.691953	18.522023
42.126956	1599.931793	18.527040
41.882530	1604.852476	18.532058
42.382569	1613.737208	18.537075
42.353550	1630.594809	18.542093
42.268465	1630.270528	18.547111
42.262544	1631.549709	18.552128
42.302440	1627.901525	18.557146
42.315676	1625.122259	18.562163
42.072734	1631.784822	18.567181
42.629312	1631.000223	18.572199
42.422581	1634.823035	18.577216
42.134384	1624.090564	18.582234
42.668867	1622.750816	18.587251
42.651779	1619.386133	18.592269
42.582188	1627.681584	18.597287
42.638883	1628.761595	18.602304
42.382230	1633.513778	18.607322
42.868727	1640.368188	18.612339
42.532968	1649.396514	18.617357
42.787903	1651.572156	18.622375
42.806056	1652.661364	18.627392
42.872335	1657.479728	18.632410
42.920008	1653.909220	18.637427
42.726922	1651.421068	18.642445
43.047441	1645.750104	18.647463
43.130222	1656.316101	18.652480
42.833137	1656.293295	18.657498
43.537635	1654.273617	18.662515
43.375708	1665.685894	18.667533
43.216755	1672.862365	18.672551
43.541914	1670.116276	18.677568
43.897633	1664.487132	18.682586
43.839194	1651.976536	18.687603
43.619492	1648.766676	18.692621
43.424396	1641.090388	18.697639
43.224508	1647.922947	18.702656
43.311321	1661.988313	18.707674
43.675976	1666.103483	18.712691
43.224003	1670.551743	18.717709
43.638361	1663.041905	18.722727
43.678348	1667.990631	18.727744
43.648064	1669.822776	18.732762
43.743934	1660.421903	18.737779
43.569918	1668.392886	18.742797
44.080364	1684.733644	18.747815
44.289742	1681.898390	18.752832
44.178600	1697.717974	18.757850
44.128903	1685.493182	18.762867
44.098967	1690.695881	18.767885
43.888271	1684.887216	18.772903
43.981657	1691.159414	18.777920
44.077406	1694.417262	18.782938
44.252221	1686.843954	18.787955
44.113421	1683.902296	18.792973
44.227441	1675.025623	18.797991
44.243750	1683.654801	18.803008
44.131737	1697.577766	18.808026
44.550983	1707.699732	18.813043
44.458449	1708.569585	18.818061
44.716059	1703.902601	18.823079
44.759915	1715.244797	18.828096
44.360427	1714.916122	18.833114
44.670038	1706.229708	18.838131
44.628438	1710.140280	18.843149
44.768186	1719.820021	18.848167
44.850024	1718.999339	18.853184
44.948783	1722.020021	18.858202
44.860623	1714.140743	18.863219
44.981587	1725.846429	18.868237
44.838012	1732.667041	18.873255
44.976297	1741.204547	18.878272
44.936040	1736.647344	18.883290
45.567208	1736.785233	18.888307
45.650207	1737.283580	18.893325
45.524522	1730.590522	18.898343
45.443360	1737.619122	18.903360
45.208652	1736.582930	18.908378
45.549577	1734.213083	18.913395
45.666812	1739.891388	18.918413
45.384908	1738.827875	18.923431
45.654712	1742.105802	18.928448
45.752428	1738.647365	18.933466
45.818217	1734.385992	18.938483
45.829532	1742.084958	18.943501
46.021176	1739.823712	18.948519
45.909502	1740.005399	18.953536
45.874953	1733.023488	18.958554
45.946920	1732.677754	18.963571
45.978604	1736.677842	18.968589
45.943258	1731.719057	18.973607
45.762653	1733.167636	18.978624
45.550295	1730.464727	18.983642
45.646477	1732.646317	18.988659
45.998487	1734.440663	18.993677
46.030109	1736.424072	18.998695
46.016155	1732.787459	19.003712
46.005625	1731.078631	19.008730
46.303873	1747.051880	19.013747
46.234723	1755.104308	19.018765
46.271605	1754.704106	19.023783
46.269931	1749.414972	19.028800
46.458560	1761.747594	19.033818
46.342396	1760.203646	19.038835
46.530870	1760.000614	19.043853
46.274337	1754.012903	19.048871
46.318410	1761.495292	19.053888
46.465456	1757.224339	19.058906
47.562653	1759.012393	19.063923
47.258186	1763.892030	19.068941
46.740847	1747.470379	19.073959
46.572610	1749.014857	19.078976
46.780323	1764.289048	19.083994
46.940566	1763.168883	19.089011
47.319535	1767.575344	19.094029
47.538245	1768.349095	19.099047
47.674378	1764.707896	19.104064
47.469685	1764.443380	19.109082
47.365510	1749.837977	19.114099
47.444192	1739.704404	19.119117
47.206203	1737.731392	19.124135
47.415960	1737.143149	19.129152
47.100099	1743.185976	19.134170
47.329916	1754.287608	19.139187
47.404525	1758.722817	19.144205
47.637746	1757.023136	19.149223
47.494296	1760.163830	19.154240
47.453022	1767.059951	19.159258
47.562526	1759.083408	19.164275
47.718325	1763.856215	19.169293
47.659883	1768.476385	19.174311
47.723071	1763.423254	19.179328
47.274246	1772.046450	19.184346
47.720209	1780.134955	19.189363
47.611950	1788.256646	19.194381
47.574655	1800.684656	19.199399
47.747403	1791.470497	19.204416
47.415885	1794.997293	19.209434
48.107981	1802.185651	19.214451
48.228354	1808.441038	19.219469
48.285328	1812.389840	19.224487
48.372164	1812.925461	19.229504
48.545361	1814.160811	19.234522
48.685583	1816.259767	19.239539
48.645869	1823.676409	19.244557
48.812649	1811.840520	19.249575
48.029851	1807.557440	19.254592
48.275058	1815.074615	19.259610
48.391774	1823.290469	19.264627
48.670427	1812.945631	19.269645
48.296290	1811.571494	19.274663
48.605162	1811.870341	19.279680
48.312727	1827.364969	19.284698
48.479929	1832.028703	19.289715
48.916974	1840.399519	19.294733
48.529116	1843.771038	19.299751
49.250389	1841.000734	19.304768
49.050430	1841.540262	19.309786
48.924984	1839.716875	19.314803
48.882822	1839.180722	19.319821
48.697055	1844.095435	19.324839
48.858991	1852.439928	19.329856
49.039601	1861.759867	19.334874
49.557731	1867.902459	19.339891
48.897154	1868.173304	19.344909
49.188797	1866.748503	19.349927
49.415230	1858.289659	19.354944
49.447334	1862.949319	19.359962
49.717359	1872.646603	19.364979
49.756451	1882.815607	19.369997
49.902066	1883.764929	19.375015
50.196052	1870.593005	19.380032
50.100674	1869.222529	19.385050
49.937258	1855.554194	19.390067
50.086664	1855.988488	19.395085
49.891191	1855.690966	19.400103
49.929834	1852.197577	19.405120
49.826655	1860.435278	19.410138
49.725623	1866.946296	19.415155
49.973417	1876.359866	19.420173
49.661991	1882.944883	19.425191
50.060656	1881.582213	19.430208
50.041234	1894.446177	19.435226
50.176535	1885.622874	19.440243
50.284398	1888.209781	19.445261
50.644057	1906.840401	19.450279
50.839355	1896.423361	19.455296
50.946044	1907.784238	19.460314
50.867600	1886.891021	19.465331
51.000591	1887.826541	19.470349
50.930782	1880.708075	19.475367
50.721874	1873.021228	19.480384
50.671587	1879.101392	19.485402
50.692593	1872.344269	19.490419
50.543675	1872.285622	19.495437
50.593833	1886.656730	19.500455
51.144835	1893.005634	19.505472
51.154708	1902.519616	19.510490
51.461597	1901.868808	19.515507
51.430907	1906.437325	19.520525
51.144007	1904.860151	19.525543
51.614936	1902.428884	19.530560
51.302764	1903.004931	19.535578
51.434068	1903.890220	19.540595
51.484670	1898.532887	19.545613
51.463475	1904.236089	19.550631
51.649271	1901.477084	19.555648
51.572328	1907.555122	19.560666
51.313310	1903.953715	19.565683
52.239954	1901.548886	19.570701
52.021269	1905.919623	19.575719
51.888207	1898.555421	19.580736
51.967530	1904.056668	19.585754
51.797664	1902.214986	19.590771
51.712285	1899.473221	19.595789
51.558431	1905.001534	19.600807
51.696468	1899.699934	19.605824
51.755896	1903.667308	19.610842
51.940936	1905.203789	19.615859
52.053577	1901.664081	19.620877
51.995924	1906.845938	19.625895
52.066700	1910.170860	19.630912
51.955172	1920.117313	19.635930
52.053772	1928.171940	19.640947
52.285252	1929.966255	19.645965
52.232666	1933.364161	19.650983
51.976982	1934.439482	19.656000
52.184496	1931.282565	19.661018
52.435696	1950.589836	19.666035
52.733534	1937.426728	19.671053
52.183562	1947.060009	19.676071
52.509817	1945.150059	19.681088
52.525770	1944.645827	19.686106
52.341150	1947.259632	19.691123
52.683445	1943.459855	19.696141
52.522428	1962.456155	19.701159
52.611634	1970.673231	19.706176
53.021493	1964.921893	19.711194
52.964507	1984.612029	19.716211
53.075476	1970.714410	19.721229
53.233809	1974.281265	19.726247
53.165288	1977.861572	19.731264
53.179927	1970.777180	19.736282
53.432802	1970.463062	19.741299
53.725416	1979.958034	19.746317
53.838291	1982.802966	19.751335
53.767653	1961.068929	19.756352
53.486465	1958.550352	19.761370
53.753331	1955.522998	19.766387
53.834490	1964.631338	19.771405
53.707130	1969.199237	19.776423
53.935431	1967.077397	19.781440
54.172075	1982.315681	19.786458
54.080495	1985.120057	19.791475
54.047477	1968.865336	19.796493
53.806405	1982.679345	19.801511
54.111102	1985.992879	19.806528
53.914563	1981.182367	19.811546
53.856489	1983.564895	19.816563
54.217837	1980.844650	19.821581
53.988563	1979.198475	19.826599
53.906840	1976.636020	19.831616
54.483198	1980.039544	19.836634
54.237170	1987.277123	19.841651
54.434923	1997.007890	19.846669
54.579309	2010.913018	19.851687
54.727221	2009.204588	19.856704
54.967627	2019.701919	19.861722
54.494252	2019.583644	19.866739
54.433722	2006.751211	19.871757
54.394122	2020.145487	19.876775
54.786456	2003.416960	19.881792
54.482650	2014.229945	19.886810
54.876034	2017.457000	19.891827
55.338608	2028.112047	19.896845
54.776081	2037.362303	19.901863
54.672136	2037.492285	19.906880
54.886806	2034.801326	19.911898
54.703913	2035.454960	19.916915
55.361057	2039.802124	19.921933
55.246865	2045.223272	19.926951
55.419203	2050.971944	19.931968
55.319085	2065.928519	19.936986
55.210279	2065.074570	19.942003
55.515995	2061.217379	19.947021
55.631729	2057.917016	19.952039
55.873853	2053.634253	19.957056
56.070363	2063.927030	19.962074
55.701528	2065.622895	19.967091
56.170915	2052.379172	19.972109
55.965577	2062.378274	19.977127
56.138029	2055.698348	19.982144
56.032832	2055.333024	19.987162
55.865344	2062.858154	19.992179
56.056388	2060.745297	19.997197
55.800397	2063.067318	20.002215
56.005217	2058.026630	20.007232
56.000663	2053.785671	20.012250
55.895024	2071.646695	20.017267
56.453296	2070.767132	20.022285
56.753840	2077.900176	20.027303
56.471535	2075.466971	20.032320
56.376964	2076.116236	20.037338
56.737001	2077.312863	20.042355
56.554348	2074.485318	20.047373
56.314608	2080.061857	20.052391
56.549891	2077.686425	20.057408
56.691390	2079.813616	20.062426
56.733554	2090.692372	20.067443
56.742282	2094.787663	20.072461
56.790419	2114.060648	20.077479
56.870538	2109.623357	20.082496
57.160383	2104.967000	20.087514
56.689831	2113.107727	20.092531
57.287093	2102.340388	20.097549
56.890274	2118.675356	20.102567
57.192070	2113.884569	20.107584
57.237456	2122.600928	20.112602
57.409020	2128.832626	20.117619
57.649643	2129.483029	20.122637
57.684017	2141.167835	20.127655
57.775790	2131.622178	20.132672
57.623822	2123.307710	20.137690
57.823832	2124.892363	20.142707
57.499630	2121.032857	20.147725
57.395670	2118.833658	20.152743
57.733736	2120.724912	20.157760
57.945260	2129.042828	20.162778
57.956746	2143.682154	20.167795
58.460231	2144.259813	20.172813
58.151223	2159.470119	20.177831
58.400175	2151.815567	20.182848
58.663235	2139.497278	20.187866
58.436038	2152.955762	20.192883
58.557212	2153.766904	20.197901
58.367222	2139.061010	20.202919
58.505338	2148.384601	20.207936
58.653607	2143.396935	20.212954
58.658859	2140.956541	20.217971
58.900883	2138.807282	20.222989
58.856961	2145.214771	20.228007
58.587154	2138.547297	20.233024
58.942636	2138.371748	20.238042
58.606100	2147.185831	20.243059
59.096890	2145.322672	20.248077
58.869894	2144.247375	20.253095
58.986734	2141.309773	20.258112
59.191317	2137.174895	20.263130
59.098610	2149.296220	20.268147
59.237157	2154.548403	20.273165
59.293572	2165.188265	20.278183
59.320468	2167.421793	20.283200
59.322916	2170.801653	20.288218
59.281766	2172.307319	20.293235
59.470554	2164.434949	20.298253
59.154027	2162.136494	20.303271
59.221131	2166.386771	20.308288
59.218776	2162.887122	20.313306
59.263433	2171.136518	20.318323
59.803040	2185.980339	20.323341
59.989262	2190.306641	20.328359
60.099369	2192.056878	20.333376
59.706040	2187.696902	20.338394
59.827371	2192.907608	20.343411
60.024590	2190.228829	20.348429
60.389894	2184.332911	20.353447
60.444960	2193.603259	20.358464
60.403910	2183.346172	20.363482
60.283641	2192.350474	20.368499
60.121289	2183.816680	20.373517
60.383544	2188.099508	20.378535
60.515415	2200.494978	20.383552
60.973513	2200.432751	20.388570
60.352537	2208.568684	20.393587
60.980245	2209.089009	20.398605
60.806957	2209.150954	20.403623
61.028660	2212.105115	20.408640
61.315462	2208.623275	20.413658
60.943107	2207.703304	20.418675
61.105918	2201.469843	20.423693
61.222539	2213.533166	20.428711
60.860837	2211.434304	20.433728
60.877623	2202.626258	20.438746
61.092364	2206.872350	20.443763
61.031471	2205.253426	20.448781
60.906080	2219.361944	20.453799
61.190945	2224.464979	20.458816
61.352738	2214.914619	20.463834
61.289639	2228.413726	20.468851
61.368985	2232.378053	20.473869
61.545503	2229.137570	20.478887
61.347411	2225.488678	20.483904
61.604625	2238.145428	20.488922
61.941733	2247.750347	20.493939
62.101479	2253.002393	20.498957
62.150711	2253.815344	20.503975
61.877454	2255.966509	20.508992
62.274429	2250.542178	20.514010
61.818291	2261.306588	20.519027
62.154206	2258.094779	20.524045
62.324013	2254.359836	20.529063
62.421246	2248.029326	20.534080
62.394373	2250.100859	20.539098
62.238959	2249.954858	20.544115
62.381376	2257.532509	20.549133
62.602577	2256.999267	20.554151
62.576628	2273.708654	20.559168
62.856579	2280.292687	20.564186
62.723000	2286.578561	20.569203
62.562291	2283.532928	20.574221
62.477665	2281.630510	20.579239
62.699879	2285.708176	20.584256
63.046084	2275.409299	20.589274
63.319265	2287.826875	20.594291
63.288316	2284.129691	20.599309
63.369988	2284.300028	20.604327
63.226309	2286.377241	20.609344
63.814080	2291.634828	20.614362
63.485609	2291.152988	20.619379
63.658503	2288.954577	20.624397
63.736784	2287.771475	20.629415
63.589642	2289.921822	20.634432
63.779293	2285.470483	20.639450
63.742217	2290.816500	20.644467
63.633725	2287.611193	20.649485
63.750922	2289.319298	20.654503
63.741751	2288.957861	20.659520
63.901341	2282.750126	20.664538
63.700229	2292.202687	20.669555
63.510795	2287.722370	20.674573
63.780858	2280.683052	20.679591
63.739762	2292.354533	20.684608
64.107443	2295.636165	20.689626
64.070189	2307.761532	20.694643
64.186753	2307.737036	20.699661
64.388631	2302.387442	20.704679
64.296368	2309.332789	20.709696
64.394471	2310.258017	20.714714
64.949270	2323.654075	20.719731
64.967660	2341.401251	20.724749
64.820094	2329.623741	20.729767
64.934631	2329.157706	20.734784
65.185333	2328.083300	20.739802
64.958488	2341.036891	20.744819
65.183736	2335.197585	20.749837
65.267662	2328.506179	20.754855
64.835948	2333.876166	20.759872
65.289993	2333.587334	20.764890
65.167708	2336.768997	20.769907
65.322362	2332.512496	20.774925
65.267702	2326.133167	20.779943
64.960134	2329.448009	20.784960
65.079076	2330.022801	20.789978
65.042341	2355.883527	20.794995
65.486046	2357.007100	20.800013
65.646703	2351.663950	20.805031
65.492110	2358.650643	20.810048
65.822597	2358.384326	20.815066
65.938294	2374.228930	20.820083
66.182751	2381.579187	20.825101
66.325394	2388.711845	20.830119
66.193023	2385.724878	20.835136
66.378509	2375.905606	20.840154
66.337598	2377.357597	20.845171
66.075870	2372.926459	20.850189
66.309263	2377.138108	20.855207
66.181820	2367.295279	20.860224
66.404847	2379.818616	20.865242
66.213195	2371.633340	20.870259
66.285263	2394.652348	20.875277
66.720090	2400.476783	20.880295
66.496448	2403.166202	20.885312
66.729185	2401.838960	20.890330
66.658786	2407.022958	20.895347
66.733607	2412.761776	20.900365
66.992500	2414.151017	20.905383
66.990454	2428.448678	20.910400
67.332825	2430.115206	20.915418
67.622007	2432.168803	20.920435
67.424541	2429.397175	20.925453
67.597967	2424.001506	20.930471
67.341478	2428.359354	20.935488
67.637146	2418.298712	20.940506
67.446899	2424.644010	20.945523
67.643564	2426.942499	20.950541
67.780969	2419.286373	20.955559
67.412299	2412.470167	20.960576
67.921235	2420.823681	20.965594
67.866531	2426.522830	20.970611
67.783127	2443.582239	20.975629
68.121779	2438.343733	20.980647
67.937805	2451.199159	20.985664
68.324355	2457.226857	20.990682
68.313323	2454.593291	20.995699
67.914830	2454.318097	21.000717
68.299471	2448.103450	21.005735
68.239506	2448.479035	21.010752
68.637576	2447.741333	21.015770
68.739405	2448.287248	21.020787
68.804859	2452.847153	21.025805
68.747544	2457.984930	21.030823
68.635647	2462.225448	21.035840
68.466941	2468.526357	21.040858
68.289050	2467.929391	21.045875
68.629991	2475.245633	21.050893
68.727861	2472.143675	21.055911
68.840431	2486.751663	21.060928
68.958253	2489.785268	21.065946
69.118397	2499.178182	21.070963
69.625404	2502.191844	21.075981
69.409049	2496.510046	21.080999
69.350085	2507.729981	21.086016
69.319508	2494.081378	21.091034
69.659299	2486.141023	21.096051
69.474889	2502.862826	21.101069
69.482823	2498.054856	21.106087
69.303081	2510.152186	21.111104
69.628034	2518.398856	21.116122
69.634827	2520.799697	21.121139
69.912232	2516.864785	21.126157
69.650629	2523.735750	21.131175
69.990745	2543.840859	21.136192
69.956798	2544.638449	21.141210
70.373482	2555.288376	21.146227
70.164561	2544.372499	21.151245
70.596148	2539.349803	21.156263
70.497411	2547.890112	21.161280
70.790860	2540.348357	21.166298
70.776892	2535.019888	21.171315
70.984680	2546.128618	21.176333
71.138135	2531.857797	21.181351
71.226869	2538.254110	21.186368
71.200869	2534.720219	21.191386
71.128588	2543.666680	21.196403
71.247162	2533.848337	21.201421
71.343630	2536.553902	21.206439
71.181831	2536.958067	21.211456
71.577462	2528.904793	21.216474
71.519627	2536.365598	21.221491
71.299865	2533.641634	21.226509
71.543515	2543.902052	21.231527
71.594501	2562.625902	21.236544
71.931713	2570.772836	21.241562
71.850886	2561.692698	21.246579
71.956166	2565.829779	21.251597
71.822982	2562.962843	21.256615
71.992252	2562.459822	21.261632
71.692070	2559.120379	21.266650
72.176909	2566.227900	21.271667
71.757435	2565.286886	21.276685
72.172412	2559.657649	21.281703
72.342048	2553.069509	21.286720
72.188297	2548.296326	21.291738
72.569213	2562.183760	21.296755
72.108372	2581.877856	21.301773
72.897772	2577.928993	21.306791
72.531660	2588.247098	21.311808
72.912518	2578.696941	21.316826
73.224357	2571.856115	21.321843
72.928531	2585.496106	21.326861
72.887235	2574.011089	21.331879
72.989566	2591.328748	21.336896
72.674136	2582.080206	21.341914
72.687956	2580.275953	21.346931
72.839749	2578.112375	21.351949
73.091023	2590.688245	21.356967
73.184199	2598.908144	21.361984
73.572189	2595.438781	21.367002
73.483372	2596.983512	21.372019
73.405359	2608.184401	21.377037
73.411323	2603.676547	21.382055
73.474177	2601.447997	21.387072
73.341225	2601.756116	21.392090
73.585166	2608.229134	21.397107
73.532064	2628.708405	21.402125
73.703429	2633.011894	21.407143
73.901367	2629.992071	21.412160
73.976588	2630.867246	21.417178
73.911887	2632.360859	21.422195
73.978223	2649.507468	21.427213
73.978866	2651.360116	21.432231
74.104840	2655.011082	21.437248
74.161097	2649.917758	21.442266
74.566042	2650.229975	21.447283
74.438087	2672.662068	21.452301
74.899240	2670.838219	21.457319
75.082228	2671.598671	21.462336
75.101409	2664.424922	21.467354
75.269051	2666.112535	21.472371
74.724890	2675.988316	21.477389
74.950830	2670.287665	21.482407
74.837614	2658.744427	21.487424
74.831216	2669.968852	21.492442
75.128807	2677.067880	21.497459
74.931868	2691.216382	21.502477
75.474856	2690.178223	21.507495
75.415123	2693.081873	21.512512
75.379926	2692.096426	21.517530
75.618712	2691.752943	21.522547
75.355562	2720.976276	21.527565
75.491802	2720.585736	21.532583
75.786943	2719.741059	21.537600
75.550590	2724.919587	21.542618
76.076235	2730.947678	21.547635
76.221900	2740.832195	21.552653
76.568152	2751.471180	21.557671
76.123209	2749.628321	21.562688
75.928319	2754.964483	21.567706
76.161383	2742.940852	21.572723
75.819175	2753.403646	21.577741
76.082669	2753.968429	21.582759
76.858710	2769.062903	21.587776
76.737784	2774.008740	21.592794
77.058306	2770.155391	21.597811
76.911293	2779.523983	21.602829
77.114123	2775.720634	21.607847
77.141340	2779.030449	21.612864
76.984979	2775.614776	21.617882
77.349554	2770.596204	21.622899
77.274516	2773.060398	21.627917
77.506132	2780.210834	21.632935
77.808701	2787.855148	21.637952
77.701380	2792.142369	21.642970
78.030826	2786.718991	21.647987
77.632018	2765.833915	21.653005
77.838700	2769.961469	21.658023
77.864441	2783.718506	21.663040
77.580815	2787.932351	21.668058
77.891639	2789.988911	21.673075
77.779505	2796.621940	21.678093
78.220485	2785.907088	21.683111
78.636226	2789.484276	21.688128
78.545821	2785.849960	21.693146
78.697054	2792.094542	21.698163
78.293838	2789.232003	21.703181
78.509385	2791.477082	21.708199
78.696279	2778.864140	21.713216
78.446932	2775.548254	21.718234
78.697409	2782.238088	21.723251
78.997868	2778.902340	21.728269
78.691342	2789.084976	21.733287
78.863272	2799.549305	21.738304
78.940258	2805.250035	21.743322
78.939819	2799.628998	21.748339
79.050905	2798.374444	21.753357
78.886675	2800.628526	21.758375
79.475052	2799.201350	21.763392
79.175642	2818.491667	21.768410
79.500372	2815.868567	21.773427
79.605115	2831.368109	21.778445
79.936596	2811.817258	21.783463
79.837467	2823.914792	21.788480
79.549503	2823.524432	21.793498
80.333594	2819.762566	21.798515
79.862326	2823.014772	21.803533
80.004663	2813.861668	21.808551
80.173527	2811.401862	21.813568
80.245690	2811.974530	21.818586
80.598413	2827.460466	21.823603
80.255822	2833.747715	21.828621
80.210458	2842.172490	21.833639
80.623311	2839.115805	21.838656
80.707125	2841.012254	21.843674
80.891235	2842.965581	21.848691
80.544070	2848.764341	21.853709
80.581812	2850.510198	21.858727
81.069609	2851.102966	21.863744
81.032858	2864.143929	21.868762
81.367695	2862.513444	21.873779
81.002046	2862.021630	21.878797
81.203632	2868.640251	21.883815
81.487401	2866.998829	21.888832
81.270140	2866.101866	21.893850
81.164361	2858.736152	21.898867
80.902067	2874.883446	21.903885
80.946925	2888.309322	21.908903
81.341816	2891.839299	21.913920
81.077768	2902.716022	21.918938
81.953700	2911.009110	21.923955
81.896641	2914.556245	21.928973
81.928145	2917.644478	21.933991
82.058378	2912.788830	21.939008
81.761871	2921.552830	21.944026
82.111717	2933.163475	21.949043
82.514865	2938.387056	21.954061
82.451254	2944.974662	21.959079
82.999864	2932.734187	21.964096
82.335104	2941.786297	21.969114
82.557162	2936.799476	21.974131
82.691078	2935.714927	21.979149
83.089925	2952.756073	21.984167
83.031140	2960.611730	21.989184
83.350845	2963.339195	21.994202
83.258814	2962.308982	21.999219
83.683313	2967.021075	22.004237
83.669025	2958.690962	22.009255
83.309638	2951.450161	22.014272
83.387159	2956.513298	22.019290
83.326301	2960.376659	22.024307
83.976393	2963.604700	22.029325
83.485741	2963.419684	22.034343
84.106939	2958.266168	22.039360
83.639605	2965.409405	22.044378
83.693616	2960.316345	22.049395
83.583936	2966.958520	22.054413
83.447802	2974.687428	22.059431
83.959163	2984.701000	22.064448
83.892311	2990.272825	22.069466
84.288248	2987.657482	22.074483
84.588928	2987.537858	22.079501
84.648901	3003.499059	22.084519
84.446837	2992.543961	22.089536
84.420820	3002.960516	22.094554
84.421053	3016.554447	22.099571
84.740939	3009.715352	22.104589
84.750753	3011.856974	22.109607
85.065058	3024.748364	22.114624
84.676178	3031.945616	22.119642
85.038638	3031.614314	22.124659
85.333454	3035.516653	22.129677
84.951069	3045.140038	22.134695
85.127133	3047.776396	22.139712
85.041629	3058.315928	22.144730
85.489584	3060.025943	22.149747
85.803659	3066.311389	22.154765
85.684114	3070.625842	22.159783
85.714061	3061.411316	22.164800
85.562956	3080.448271	22.169818
86.182151	3086.165139	22.174835
86.346600	3085.479798	22.179853
85.758945	3094.052777	22.184871
86.492246	3082.708046	22.189888
86.476208	3088.155159	22.194906
86.424399	3091.265944	22.199923
86.553335	3102.500997	22.204941
86.559523	3101.830981	22.209959
86.965191	3106.101030	22.214976
86.879777	3113.462238	22.219994
86.716153	3106.998703	22.225011
86.783639	3098.299058	22.230029
86.596945	3105.209006	22.235047
87.166297	3116.182535	22.240064
87.183286	3128.385175	22.245082
87.423230	3131.109381	22.250099
87.551268	3136.432935	22.255117
87.430370	3135.956423	22.260135
87.809074	3133.984479	22.265152
87.443226	3134.294376	22.270170
87.670753	3139.798032	22.275187
87.967660	3152.588083	22.280205
87.811950	3157.918225	22.285223
88.201656	3168.850494	22.290240
88.190408	3160.434593	22.295258
88.307850	3154.829695	22.300275
88.477333	3149.860522	22.305293
88.069577	3160.318039	22.310311
88.254560	3155.185467	22.315328
88.450768	3187.137184	22.320346
88.535222	3184.119269	22.325363
88.963617	3180.422528	22.330381
88.959588	3203.183052	22.335399
89.090111	3188.119927	22.340416
89.228901	3191.642743	22.345434
89.186424	3189.793594	22.350451
89.312923	3185.348773	22.355469
89.262611	3191.457789	22.360487
89.632970	3180.700113	22.365504
89.110693	3179.705733	22.370522
89.164948	3189.333378	22.375539
89.409073	3200.190631	22.380557
88.975794	3212.864719	22.385575
89.465733	3203.432863	22.390592
89.233372	3215.586253	22.395610
89.317127	3224.675887	22.400627
89.556216	3231.042577	22.405645
89.716475	3244.093979	22.410663
90.105329	3254.597181	22.415680
90.114061	3261.044160	22.420698
90.323442	3267.295579	22.425715
90.390550	3266.634950	22.430733
90.469465	3277.054161	22.435751
90.497567	3282.664856	22.440768
90.762254	3292.019710	22.445786
90.746963	3295.329966	22.450803
91.495202	3284.342586	22.455821
91.331397	3285.084803	22.460839
91.511914	3279.681456	22.465856
91.290480	3285.179746	22.470874
91.459975	3288.757740	22.475891
92.032519	3274.742613	22.480909
91.304551	3275.446968	22.485927
91.635386	3275.859186	22.490944
91.899388	3270.954079	22.495962
91.793604	3273.865037	22.500979
91.962540	3267.425092	22.505997
92.024798	3294.669884	22.511015
92.242241	3298.934751	22.516032
91.896896	3308.549316	22.521050
91.920881	3300.980026	22.526067
92.357468	3303.184226	22.531085
92.404297	3301.109602	22.536103
92.294668	3298.860645	22.541120
92.383581	3308.987930	22.546138
92.420622	3323.062392	22.551155
92.171556	3318.291313	22.556173
92.586345	3328.329677	22.561191
92.680731	3343.357838	22.566208
93.062761	3353.385567	22.571226
92.993062	3360.791758	22.576243
93.120585	3352.590748	22.581261
92.954031	3357.329264	22.586279
93.133792	3370.573392	22.591296
93.090421	3375.434646	22.596314
93.140986	3378.523128	22.601331
93.356524	3379.534171	22.606349
93.206842	3395.500159	22.611367
93.409936	3400.199710	22.616384
93.729010	3399.941483	22.621402
93.693309	3425.011346	22.626419
93.642456	3417.639955	22.631437
94.211745	3420.214760	22.636455
94.023029	3425.373399	22.641472
94.133920	3447.437619	22.646490
94.427531	3453.991538	22.651507
94.531532	3456.645559	22.656525
94.983361	3454.289680	22.661543
95.071975	3451.738203	22.666560
95.275367	3445.993497	22.671578
95.206232	3446.701951	22.676595
95.251103	3434.625282	22.681613
95.252304	3443.500706	22.686631
95.961196	3431.146408	22.691648
95.556501	3431.809589	22.696666
95.501403	3451.557843	22.701683
95.798292	3437.854064	22.706701
95.483592	3439.705698	22.711719
95.672532	3447.017745	22.716736
95.969446	3458.106762	22.721754
95.350384	3467.972612	22.726771
95.736846	3462.937796	22.731789
96.063705	3456.753954	22.736807
96.272240	3452.289902	22.741824
96.494552	3469.955738	22.746842
96.498615	3483.599921	22.751859
96.866738	3484.407154	22.756877
96.932747	3487.449047	22.761895
97.022929	3483.262348	22.766912
97.114361	3485.785778	22.771930
96.868236	3486.042203	22.776947
97.160937	3475.151329	22.781965
97.078204	3480.782607	22.786983
96.991824	3481.500076	22.792000
97.149363	3485.013700	22.797018
97.016251	3484.753722	22.802035
97.651716	3490.985808	22.807053
97.824639	3499.282000	22.812071
97.717667	3497.067321	22.817088
97.858217	3511.646505	22.822106
97.775037	3513.458718	22.827123
98.125081	3502.672471	22.832141
97.529476	3509.728701	22.837159
97.970827	3519.993423	22.842176
98.248789	3531.514714	22.847194
97.935140	3532.753866	22.852211
98.615296	3522.853316	22.857229
98.249337	3535.551800	22.862247
98.359082	3547.279366	22.867264
98.560865	3555.896164	22.872282
98.638432	3560.022035	22.877299
98.819360	3554.239782	22.882317
98.522111	3574.931975	22.887335
99.152209	3585.697425	22.892352
99.416547	3579.924191	22.897370
99.186704	3586.803206	22.902387
99.325945	3583.656700	22.907405
99.429373	3588.103628	22.912423
99.313471	3603.745717	22.917440
99.687070	3613.317243	22.922458
99.598647	3613.406927	22.927475
100.035726	3599.886224	22.932493
99.889486	3609.813795	22.937511
100.120724	3621.415059	22.942528
100.634723	3622.814931	22.947546
100.372228	3627.533829	22.952563
100.510049	3625.088246	22.957581
100.490083	3625.968914	22.962599
100.554716	3635.191160	22.967616
100.666912	3625.531043	22.972634
100.311689	3631.527005	22.977651
100.840643	3638.568072	22.982669
101.045257	3646.666829	22.987687
100.805539	3648.664553	22.992704
101.325665	3653.447067	22.997722
101.224866	3652.588631	23.002739
101.914566	3658.316733	23.007757
102.029460	3672.600213	23.012775
101.467367	3665.078404	23.017792
101.624534	3669.343333	23.022810
101.807711	3671.274804	23.027827
101.729875	3676.318295	23.032845
101.969779	3675.731582	23.037863
101.835984	3678.972097	23.042880
102.240524	3674.856044	23.047898
102.053019	3693.211262	23.052915
102.239565	3691.831196	23.057933
102.219223	3696.676303	23.062951
102.443737	3695.391291	23.067968
102.593735	3692.366179	23.072986
102.441437	3716.334210	23.078003
102.931893	3711.933242	23.083021
103.210377	3725.209508	23.088039
103.022801	3721.861673	23.093056
103.354352	3720.237941	23.098074
103.456404	3720.158904	23.103091
103.324030	3725.693875	23.108109
103.517444	3733.068464	23.113127
103.931286	3744.836894	23.118144
103.868897	3743.183345	23.123162
103.733498	3747.702449	23.128179
103.628431	3749.379234	23.133197
104.007434	3751.371567	23.138215
103.975431	3755.337893	23.143232
104.062993	3768.817703	23.148250
104.216732	3776.946585	23.153267
104.279128	3772.012958	23.158285
104.452033	3779.715885	23.163303
104.416066	3789.468458	23.168320
104.619116	3792.779318	23.173338
104.300364	3794.994604	23.178355
104.741807	3807.033354	23.183373
104.944275	3824.143967	23.188391
104.990250	3822.713318	23.193408
105.159158	3824.063112	23.198426
105.086466	3840.017429	23.203443
105.601910	3846.906031	23.208461
105.620881	3856.435400	23.213479
105.223441	3859.253265	23.218496
105.980351	3853.308081	23.223514
105.749584	3862.232678	23.228531
105.686885	3865.695659	23.233549
106.255781	3879.835578	23.238567
106.111731	3876.594524	23.243584
106.165214	3877.495261	23.248602
106.165931	3883.912155	23.253619
106.474091	3901.669123	23.258637
106.904007	3900.576020	23.263655
106.814947	3908.787190	23.268672
107.061473	3900.109612	23.273690
106.972291	3895.499556	23.278707
106.675514	3891.452299	23.283725
107.153872	3911.268982	23.288743
107.173203	3923.077242	23.293760
107.657457	3919.753526	23.298778
107.575963	3923.112146	23.303795
107.791832	3923.280412	23.308813
107.913659	3923.062551	23.313831
107.994690	3932.689554	23.318848
108.025905	3940.648321	23.323866
108.172137	3945.379019	23.328883
108.112292	3946.130226	23.333901
108.292761	3957.774381	23.338919
108.636264	3948.541843	23.343936
108.831934	3940.279388	23.348954
108.496997	3945.508428	23.353971
108.566171	3943.726931	23.358989
109.285994	3965.936268	23.364007
108.755316	3971.571593	23.369024
108.977918	3968.127885	23.374042
109.297066	3973.554315	23.379059
109.155541	3966.114839	23.384077
109.079418	3971.581100	23.389095
109.055326	3974.286831	23.394112
109.648632	3977.748061	23.399130
109.720918	3992.874916	23.404147
109.778046	3983.488373	23.409165
109.737929	3985.047686	23.414183
109.395183	3986.831171	23.419200
110.025608	3989.734218	23.424218
110.067613	4007.381482	23.429235
110.005198	4013.486359	23.434253
109.856364	4006.957056	23.439271
110.211115	4018.068921	23.444288
110.623319	4029.714693	23.449306
110.621456	4038.294186	23.454323
110.446184	4042.661789	23.459341
110.866993	4043.309288	23.464359
110.890484	4063.932847	23.469376
111.083474	4061.248145	23.474394
111.107368	4067.999208	23.479411
111.112579	4067.998470	23.484429
111.421506	4074.386081	23.489447
111.958522	4096.633689	23.494464
112.090603	4084.053680	23.499482
111.718316	4086.226885	23.504499
111.984863	4083.994648	23.509517
112.093500	4076.967301	23.514535
112.458933	4090.924626	23.519552
112.590017	4105.395297	23.524570
112.431436	4107.219381	23.529587
112.526751	4115.698461	23.534605
112.781434	4106.142022	23.539623
112.570681	4115.502350	23.544640
112.845211	4104.588695	23.549658
112.768365	4123.062736	23.554675
112.888410	4125.130404	23.559693
113.195723	4134.965108	23.564711
113.089307	4142.330023	23.569728
113.455535	4145.277645	23.574746
113.486864	4150.869165	23.579763
113.450862	4157.689618	23.584781
113.620487	4157.833568	23.589799
113.769120	4158.627875	23.594816
113.889888	4172.314264	23.599834
113.783730	4192.440627	23.604851
113.799386	4197.037182	23.609869
114.360921	4193.177341	23.614887
114.378544	4210.759181	23.619904
114.533419	4208.923198	23.624922
114.444571	4206.421513	23.629939
114.984572	4215.863127	23.634957
114.751411	4218.203937	23.639975
114.955007	4232.868518	23.644992
115.682397	4240.418485	23.650010
115.256634	4246.296285	23.655027
114.814242	4239.816047	23.660045
115.304840	4239.477278	23.665063
115.366842	4255.044709	23.670080
115.975203	4262.275593	23.675098
115.992214	4262.661249	23.680115
115.597802	4260.238994	23.685133
115.917547	4264.279736	23.690151
116.005508	4277.832461	23.695168
116.176606	4276.748322	23.700186
116.202263	4284.259894	23.705203
116.001721	4289.682615	23.710221
116.663530	4296.254910	23.715239
116.736645	4305.873881	23.720256
116.674515	4304.122390	23.725274
116.938208	4311.681906	23.730291
116.927635	4315.405105	23.735309
117.359562	4307.339048	23.740327
117.053238	4312.500580	23.745344
117.336433	4327.534698	23.750362
117.616385	4322.497395	23.755379
117.227896	4328.568239	23.760397
117.381506	4330.548604	23.765415
117.677229	4353.298331	23.770432
117.988336	4357.914924	23.775450
118.035200	4357.497320	23.780467
117.987690	4359.060979	23.785485
118.125080	4367.353667	23.790503
117.860538	4384.471690	23.795520
118.436379	4383.295726	23.800538
118.862598	4385.365959	23.805555
118.850901	4400.976626	23.810573
118.942920	4408.771405	23.815591
118.814784	4422.086636	23.820608
119.061012	4403.327080	23.825626
119.448957	4412.341244	23.830643
119.571408	4432.949718	23.835661
119.857748	4423.069349	23.840679
119.638101	4430.496311	23.845696
120.083230	4426.238004	23.850714
120.181861	4419.953865	23.855731
119.749722	4430.854679	23.860749
120.229553	4433.440494	23.865767
120.107429	4452.938350	23.870784
120.383346	4457.049132	23.875802
120.477256	4456.138056	23.880819
120.609201	4463.544669	23.885837
120.662924	4456.904558	23.890855
120.527699	4468.547997	23.895872
120.866285	4483.971284	23.900890
120.755896	4486.636951	23.905907
121.071255	4505.463433	23.910925
121.503255	4512.690485	23.915943
121.169202	4510.968950	23.920960
121.847563	4508.889941	23.925978
121.553496	4515.438466	23.930995
121.762163	4528.328542	23.936013
122.019572	4531.978236	23.941031
121.960543	4543.726577	23.946048
122.196079	4534.576944	23.951066
122.383817	4539.635884	23.956083
122.283282	4546.580227	23.961101
122.408974	4556.427831	23.966119
122.863235	4562.833881	23.971136
122.706067	4556.031070	23.976154
122.793972	4565.846722	23.981171
123.084018	4578.547320	23.986189
123.229788	4584.010566	23.991207
123.182344	4588.866471	23.996224
123.485701	4592.938263	24.001242
123.601171	4589.391276	24.006259
122.910790	4600.998672	24.011277
123.573182	4606.238944	24.016295
123.889723	4611.574435	24.021312
123.956446	4622.630788	24.026330
124.045002	4633.715293	24.031347
124.140096	4641.790620	24.036365
124.338797	4625.569807	24.041383
124.324827	4635.871778	24.046400
124.287731	4651.303561	24.051418
125.084112	4661.664824	24.056435
124.920094	4655.920482	24.061453
124.426400	4649.189299	24.066471
124.869677	4658.295926	24.071488
124.776751	4669.295250	24.076506
125.166895	4673.504977	24.081523
125.310278	4683.959088	24.086541
125.880441	4693.326784	24.091559
126.420227	4703.905037	24.096576
126.100392	4696.862510	24.101594
126.302453	4698.557551	24.106611
126.177221	4713.766456	24.111629
126.691375	4701.931075	24.116647
126.726191	4705.906078	24.121664
126.550609	4705.510690	24.126682
126.857734	4699.058060	24.131699
126.717339	4699.828230	24.136717
126.740108	4706.264054	24.141735
126.748555	4716.070140	24.146752
126.551479	4727.818131	24.151770
127.185073	4739.915783	24.156787
127.191713	4759.119175	24.161805
127.230737	4755.107496	24.166823
127.412979	4767.739889	24.171840
127.419410	4762.300246	24.176858
127.798080	4778.759161	24.181875
127.879712	4787.417466	24.186893
128.166579	4775.434567	24.191911
128.321610	4794.939872	24.196928
128.195089	4812.939445	24.201946
128.242373	4815.327933	24.206963
128.231077	4821.567116	24.211981
128.534326	4837.008866	24.216999
128.434021	4849.483563	24.222016
128.637564	4850.360839	24.227034
129.044986	4865.653717	24.232051
128.901092	4883.056335	24.237069
129.202579	4878.249092	24.242087
129.153719	4891.075606	24.247104
129.166697	4907.026905	24.252122
129.953143	4905.170820	24.257139
129.913721	4924.394228	24.262157
129.962016	4929.257320	24.267175
129.878472	4938.197255	24.272192
129.949447	4932.400228	24.277210
130.225648	4937.685318	24.282227
130.296620	4953.529719	24.287245
130.721517	4958.725231	24.292263
131.025974	4966.619543	24.297280
130.860198	4975.092581	24.302298
131.072794	4966.006302	24.307315
131.425079	4965.209394	24.312333
131.372083	4979.665409	24.317351
131.654667	4992.323273	24.322368
131.884802	4991.428708	24.327386
132.081786	4985.296264	24.332403
131.953510	4999.732523	24.337421
132.274472	4990.042131	24.342439
132.463972	4989.883101	24.347456
132.324562	5000.883594	24.352474
132.799968	5003.388116	24.357491
132.974566	5020.393743	24.362509
133.318892	5022.669434	24.367527
133.284920	5020.711440	24.372544
133.046170	5015.335387	24.377562
133.350586	5016.035883	24.382579
133.127806	5017.705972	24.387597
133.048643	5013.381311	24.392615
133.354709	5010.138980	24.397632
133.551016	5037.065510	24.402650
133.526405	5031.592772	24.407667
133.583289	5048.197042	24.412685
133.605872	5052.865330	24.417703
133.917208	5062.431597	24.422720
134.053955	5074.604156	24.427738
134.561746	5071.251296	24.432755
133.886722	5082.698760	24.437773
134.112772	5085.911556	24.442791
134.000299	5103.868179	24.447808
134.582623	5116.381316	24.452826
134.714270	5128.687287	24.457843
134.653827	5139.615517	24.462861
135.043943	5158.487783	24.467879
135.386941	5164.068665	24.472896
135.513997	5167.779946	24.477914
135.417873	5172.100696	24.482931
135.791845	5177.424201	24.487949
135.977685	5184.592232	24.492967
136.198375	5189.317903	24.497984
135.930772	5208.226975	24.503002
135.915447	5204.744553	24.508019
136.274694	5226.667858	24.513037
136.204689	5231.016095	24.518055
136.605273	5233.241963	24.523072
136.743823	5245.881533	24.528090
137.220006	5257.350772	24.533107
137.158932	5269.324020	24.538125
137.170033	5263.113280	24.543143
137.455974	5275.073202	24.548160
137.688573	5285.545247	24.553178
137.991987	5288.477646	24.558195
137.897821	5292.734985	24.563213
137.721759	5295.420527	24.568231
138.103097	5300.588240	24.573248
138.051743	5323.753412	24.578266
138.579597	5322.064066	24.583283
138.370249	5342.482491	24.588301
138.402337	5345.706782	24.593319
138.454157	5347.381229	24.598336
138.716518	5371.374858	24.603354
139.281140	5372.839546	24.608371
139.214278	5373.468801	24.613389
139.088886	5380.414198	24.618407
139.608652	5393.836971	24.623424
139.669818	5395.456296	24.628442
139.877320	5390.366919	24.633459
140.165568	5405.644199	24.638477
140.066868	5415.113903	24.643495
140.170464	5422.051850	24.648512
140.052656	5429.681071	24.653530
140.353622	5436.016749	24.658547
140.784559	5448.029828	24.663565
140.522655	5450.814071	24.668583
140.860363	5465.711168	24.673600
140.174034	5473.590465	24.678618
140.820118	5486.289581	24.683635
141.409230	5498.334732	24.688653
141.148696	5505.875861	24.693671
141.652536	5503.609436	24.698688
141.636784	5522.615112	24.703706
142.290889	5525.066458	24.708723
142.179038	5525.702766	24.713741
142.372723	5528.545069	24.718759
142.494187	5526.313293	24.723776
142.848046	5550.469596	24.728794
143.190171	5538.546989	24.733811
143.418268	5546.254647	24.738829
143.358548	5541.166056	24.743847
143.670841	5539.425233	24.748864
143.443050	5549.593914	24.753882
143.507557	5547.532049	24.758899
143.729955	5543.718749	24.763917
143.686620	5536.705180	24.768935
144.014188	5539.974757	24.773952
143.724369	5554.881852	24.778970
144.441029	5559.050103	24.783987
144.331003	5569.102489	24.789005
144.355593	5577.040912	24.794023
144.614019	5566.722365	24.799040
144.374950	5569.241045	24.804058
144.468344	5593.375078	24.809075
144.558926	5603.212966	24.814093
144.589336	5606.368119	24.819111
145.028583	5621.271532	24.824128
144.785930	5635.454736	24.829146
145.072256	5637.670144	24.834163
145.153692	5643.307936	24.839181
145.331116	5663.041099	24.844199
145.958001	5674.543813	24.849216
145.847713	5686.831243	24.854234
146.141425	5681.990285	24.859251
146.385662	5706.264983	24.864269
146.464793	5705.804413	24.869287
146.492309	5713.676147	24.874304
146.260752	5722.585990	24.879322
146.628908	5733.800978	24.884339
147.000471	5732.849498	24.889357
147.011645	5767.407454	24.894375
147.539437	5763.107481	24.899392
147.756218	5775.892998	24.904410
147.818663	5772.388814	24.909427
147.651900	5786.661260	24.914445
147.720162	5797.228793	24.919463
148.175481	5795.213002	24.924480
147.744541	5816.228565	24.929498
147.820493	5814.199601	24.934515
148.151091	5830.060909	24.939533
148.300896	5851.054977	24.944551
148.574994	5853.745837	24.949568
148.661857	5866.526517	24.954586
148.903978	5873.405053	24.959603
149.285355	5885.179961	24.964621
149.542546	5904.335833	24.969639
149.943614	5895.153276	24.974656
149.671598	5896.929016	24.979674
149.905742	5908.411331	24.984691
150.671066	5917.692266	24.989709
150.275483	5928.607180	24.994727
150.594765	5928.121608	24.999744
150.320024	5928.919189	25.004762
150.480748	5936.435536	25.009779
150.651585	5943.217937	25.014797
150.554485	5960.614248	25.019815
151.103616	5965.711669	25.024832
151.273309	5967.285631	25.029850
151.417211	5976.098895	25.034867
151.778982	5985.108472	25.039885
151.859305	6004.118537	25.044903
152.474578	6012.539139	25.049920
152.046564	6015.046442	25.054938
152.029151	6003.741763	25.059955
152.207979	6021.322189	25.064973
152.308660	6028.320803	25.069991
152.968304	6033.047373	25.075008
152.720022	6035.333958	25.080026
153.073185	6031.572676	25.085043
153.219777	6042.506890	25.090061
153.090862	6051.340834	25.095079
153.062612	6046.499714	25.100096
153.311636	6055.864763	25.105114
153.371624	6067.986875	25.110131
153.611874	6081.191935	25.115149
153.463660	6081.707688	25.120167
154.066553	6094.975901	25.125184
154.083840	6110.883381	25.130202
154.358323	6117.962130	25.135219
154.655870	6125.826461	25.140237
154.354801	6134.712669	25.145255
154.822329	6139.586166	25.150272
154.959215	6150.225228	25.155290
155.117667	6149.010378	25.160307
155.522104	6166.959666	25.165325
155.283419	6164.399109	25.170343
155.840578	6181.958300	25.175360
155.675138	6199.570734	25.180378
155.747296	6193.997254	25.185395
155.968623	6206.921259	25.190413
156.073778	6224.469227	25.195431
156.273037	6217.906693	25.200448
156.479445	6234.747472	25.205466
156.654639	6240.326564	25.210483
157.307372	6239.409929	25.215501
156.656790	6253.013533	25.220519
157.052365	6270.269816	25.225536
157.169181	6275.210921	25.230554
157.110770	6290.202317	25.235571
157.291869	6304.108144	25.240589
157.498036	6311.364981	25.245607
157.882833	6332.401706	25.250624
158.039343	6337.431314	25.255642
158.043993	6351.623678	25.260659
158.543600	6362.837400	25.265677
158.635261	6366.030440	25.270695
158.813081	6375.144793	25.275712
159.245951	6389.371118	25.280730
159.039181	6401.377401	25.285747
159.369930	6392.982191	25.290765
159.087284	6415.992413	25.295783
159.626527	6421.205158	25.300800
159.610764	6421.381331	25.305818
159.595878	6436.296577	25.310835
159.919301	6448.554451	25.315853
159.849853	6460.125715	25.320871
160.040109	6466.005571	25.325888
160.001613	6479.939621	25.330906
160.136000	6502.013330	25.335923
160.695769	6501.742615	25.340941
160.676219	6527.271953	25.345959
161.035647	6533.933480	25.350976
161.329401	6548.547916	25.355994
161.479647	6556.044061	25.361011
162.224513	6557.490084	25.366029
161.876493	6562.564070	25.371047
162.215083	6564.417838	25.376064
162.743828	6577.148728	25.381082
162.723808	6579.623756	25.386099
163.117692	6578.008956	25.391117
162.745634	6580.169784	25.396135
162.886057	6584.176004	25.401152
163.036731	6586.747408	25.406170
163.045191	6602.530422	25.411187
163.426488	6608.310945	25.416205
163.040071	6616.693032	25.421223
163.458079	6628.743641	25.426240
163.292953	6636.933225	25.431258
163.580012	6644.164894	25.436275
164.053297	6652.993175	25.441293
163.989333	6669.447377	25.446311
164.252170	6661.713000	25.451328
164.630981	6675.468173	25.456346
164.329516	6685.971024	25.461363
164.406696	6697.781485	25.466381
164.461889	6721.001180	25.471399
164.592915	6717.454504	25.476416
164.665536	6733.884209	25.481434
164.984759	6743.203887	25.486451
165.403612	6760.857909	25.491469
165.722130	6774.161698	25.496487
166.005255	6789.696645	25.501504
166.504430	6796.888830	25.506522
166.337679	6796.539362	25.511539
166.598190	6795.819897	25.516557
167.009240	6814.516966	25.521575
166.922481	6823.215243	25.526592
167.161267	6831.025946	25.531610
167.111581	6841.416832	25.536627
167.504835	6846.005407	25.541645
167.280360	6862.554380	25.546663
167.559316	6861.153290	25.551680
167.726230	6878.382831	25.556698
167.810993	6886.385003	25.561715
168.222436	6901.947297	25.566733
168.427736	6918.675228	25.571751
168.539155	6909.357602	25.576768
169.117373	6920.439389	25.581786
169.195853	6936.937810	25.586803
169.518516	6925.468795	25.591821
169.572721	6924.102910	25.596839
169.410064	6922.843608	25.601856
169.950806	6949.327534	25.606874
169.853563	6963.135406	25.611891
170.229184	6954.799207	25.616909
170.313167	6955.578513	25.621927
170.477664	6968.865533	25.626944
170.110043	6979.476779	25.631962
170.191388	6984.246845	25.636979
170.828716	6992.809665	25.641997
170.848866	7010.494821	25.647015
171.265824	7013.539147	25.652032
171.759333	7030.806060	25.657050
171.360142	7044.566589	25.662067
171.630760	7045.925948	25.667085
171.640367	7057.488358	25.672103
171.645663	7065.247346	25.677120
172.180454	7068.080648	25.682138
171.608664	7101.820090	25.687156
172.320328	7104.404703	25.692173
172.738952	7122.119091	25.697191
172.910598	7126.253130	25.702208
172.939827	7131.994267	25.707226
172.883476	7143.500768	25.712244
173.128938	7146.543571	25.717261
173.424639	7160.302658	25.722279
173.735333	7172.569325	25.727296
173.958750	7183.498498	25.732314
173.687121	7186.148774	25.737332
174.303343	7202.882040	25.742349
174.412812	7212.253760	25.747367
174.569038	7215.307398	25.752384
174.798589	7214.400193	25.757402
174.854671	7233.064905	25.762420
175.209865	7241.391072	25.767437
174.935110	7236.364112	25.772455
174.882711	7254.745929	25.777472
175.164937	7262.038582	25.782490
175.358797	7290.736709	25.787508
175.621572	7293.653702	25.792525
175.799383	7314.171510	25.797543
175.833803	7323.671852	25.802560
176.213841	7324.306927	25.807578
176.133371	7347.198241	25.812596
176.443116	7358.587540	25.817613
176.679944	7365.195967	25.822631
176.979302	7387.721599	25.827648
177.096791	7394.339261	25.832666
177.087771	7412.733381	25.837684
177.525656	7415.515623	25.842701
177.680867	7434.316544	25.847719
177.395382	7442.601109	25.852736
177.774498	7468.223987	25.857754
178.221260	7484.321088	25.862772
178.235650	7490.819186	25.867789
178.646313	7496.844793	25.872807
178.554295	7509.408394	25.877824
179.168418	7524.585878	25.882842
179.302388	7538.095924	25.887860
179.577738	7535.798757	25.892877
179.626181	7557.318934	25.897895
179.778270	7556.657468	25.902912
180.008249	7561.975819	25.907930
180.018996	7581.544578	25.912948
180.400964	7577.478556	25.917965
180.506855	7593.584957	25.922983
180.573034	7607.913873	25.928000
180.698441	7604.914072	25.933018
180.731385	7627.437536	25.938036
181.358925	7635.935894	25.943053
181.348217	7642.065447	25.948071
181.186050	7663.160972	25.953088
181.753025	7672.382326	25.958106
181.661479	7688.497641	25.963124
181.830424	7699.763986	25.968141
182.296151	7718.443938	25.973159
182.372169	7727.451786	25.978176
182.455995	7733.269797	25.983194
182.601171	7749.010275	25.988212
182.737376	7757.841385	25.993229
183.178406	7787.353966	25.998247
183.156533	7803.600533	26.003264
183.791083	7810.093142	26.008282
183.637816	7823.026455	26.013300
183.542186	7826.953116	26.018317
184.133529	7838.232298	26.023335
183.993653	7855.232994	26.028352
184.404403	7864.109541	26.033370
184.505926	7878.887749	26.038388
184.577408	7889.683289	26.043405
185.251218	7897.369467	26.048423
185.130440	7916.454053	26.053440
185.490882	7929.108066	26.058458
185.758536	7934.294339	26.063476
185.808112	7942.409823	26.068493
186.280638	7958.010798	26.073511
186.163762	7966.932169	26.078528
186.474364	7982.211252	26.083546
186.580170	7984.354204	26.088564
186.652336	7993.571153	26.093581
187.119384	8002.562075	26.098599
187.114598	8018.272605	26.103616
187.441947	8016.346085	26.108634
187.784549	8010.909643	26.113652
188.195643	8025.326917	26.118669
188.521019	8027.991125	26.123687
188.398940	8037.247998	26.128704
188.442400	8023.529991	26.133722
188.887034	8032.578110	26.138740
188.001810	8040.669601	26.143757
188.345879	8048.369615	26.148775
188.872450	8072.236984	26.153792
189.399437	8078.989637	26.158810
189.558239	8088.701355	26.163828
189.507215	8091.471896	26.168845
189.743839	8110.734318	26.173863
189.943081	8116.701695	26.178880
189.860938	8129.002129	26.183898
190.106252	8137.529030	26.188916
189.982882	8150.006420	26.193933
190.251874	8173.740631	26.198951
190.402664	8191.122309	26.203968
190.645415	8205.417712	26.208986
190.827207	8217.361143	26.214004
190.712930	8247.005653	26.219021
191.012154	8251.416729	26.224039
191.289792	8279.932783	26.229056
191.662221	8291.132882	26.234074
192.013859	8310.705836	26.239092
192.236683	8322.223006	26.244109
192.617304	8328.398823	26.249127
192.603209	8346.229536	26.254144
192.953651	8349.344494	26.259162
193.207479	8363.133139	26.264180
193.482983	8379.425182	26.269197
194.111171	8381.783116	26.274215
194.065519	8391.804853	26.279232
194.349396	8397.995850	26.284250
194.447630	8409.718865	26.289268
194.645000	8404.655507	26.294285
194.779273	8415.223673	26.299303
195.322204	8425.689938	26.304320
195.378242	8436.743948	26.309338
195.343180	8440.800164	26.314356
195.367692	8455.123636	26.319373
195.311865	8457.213035	26.324391
195.186785	8467.963934	26.329408
195.753783	8478.079170	26.334426
195.866527	8495.710197	26.339444
195.991717	8511.804902	26.344461
196.638756	8524.903789	26.349479
196.575518	8551.241534	26.354496
196.826199	8550.337271	26.359514
197.268325	8567.225342	26.364532
197.087879	8577.284082	26.369549
197.839915	8585.880195	26.374567
197.697120	8591.345644	26.379584
197.753773	8603.526775	26.384602
198.053722	8629.438342	26.389620
198.120443	8640.339254	26.394637
198.415936	8635.307819	26.399655
198.589711	8660.086817	26.404672
198.508741	8667.676874	26.409690
198.925064	8682.396934	26.414708
198.965875	8693.267207	26.419725
199.757947	8702.586418	26.424743
199.602547	8721.901419	26.429760
200.107954	8728.806082	26.434778
199.941447	8730.695003	26.439796
200.003784	8743.080554	26.444813
200.380879	8740.912534	26.449831
200.313296	8768.653073	26.454848
200.785513	8772.945615	26.459866
201.043283	8779.301848	26.464884
200.850559	8793.981650	26.469901
201.216355	8798.988616	26.474919
201.414860	8824.237544	26.479936
201.627938	8824.197927	26.484954
201.682203	8836.657421	26.489972
201.935155	8854.794083	26.494989
202.655592	8871.556743	26.500007
202.346198	8884.944639	26.505024
202.751787	8890.081158	26.510042
202.859609	8907.707034	26.515060
203.027444	8932.803052	26.520077
203.403393	8932.939983	26.525095
203.101185	8948.451629	26.530112
203.418596	8969.025177	26.535130
203.520716	8976.416185	26.540148
203.436112	8995.126813	26.545165
204.056613	9008.211257	26.550183
204.259956	9033.005065	26.555200
204.295321	9052.625193	26.560218
204.781797	9061.632533	26.565236
205.038432	9090.623557	26.570253
205.274212	9097.902113	26.575271
205.375900	9119.229482	26.580288
206.035556	9126.871035	26.585306
206.088659	9139.514037	26.590324
206.131449	9153.071119	26.595341
206.604896	9161.360687	26.600359
206.539303	9186.405212	26.605376
206.610624	9195.613419	26.610394
206.696879	9207.951330	26.615412
207.073672	9235.341950	26.620429
207.427864	9247.937857	26.625447
207.672008	9263.348387	26.630464
207.856386	9277.009670	26.635482
208.128580	9292.892584	26.640500
207.872076	9307.409129	26.645517
208.317538	9318.105868	26.650535
208.640220	9342.297289	26.655552
208.929155	9354.272027	26.660570
209.225127	9363.530371	26.665588
209.406981	9370.028151	26.670605
209.778773	9384.503160	26.675623
209.793386	9393.774023	26.680640
210.367147	9410.380182	26.685658
210.630475	9421.932736	26.690676
210.574571	9420.738628	26.695693
210.532145	9429.658508	26.700711
210.803644	9449.939834	26.705728
210.750831	9465.921171	26.710746
211.266072	9468.644252	26.715764
211.403524	9494.307794	26.720781
211.797358	9502.635246	26.725799
211.941567	9528.929247	26.730816
212.258454	9536.653085	26.735834
212.214174	9546.709960	26.740852
212.547839	9560.092319	26.745869
212.774046	9565.105575	26.750887
213.103922	9577.497129	26.755904
213.348516	9592.023800	26.760922
213.389292	9600.182433	26.765940
212.825847	9620.206390	26.770957
213.413824	9638.398683	26.775975
213.968565	9658.781103	26.780992
213.893942	9666.736827	26.786010
214.361638	9678.210163	26.791028
214.333271	9686.654358	26.796045
214.686868	9704.753981	26.801063
214.297518	9721.583918	26.806080
214.675658	9742.881322	26.811098
215.418241	9770.095444	26.816116
215.161095	9776.447436	26.821133
215.342519	9794.959321	26.826151
215.952688	9812.712587	26.831168
216.209668	9830.761163	26.836186
216.539657	9845.296755	26.841204
217.365933	9853.427166	26.846221
217.154065	9866.506847	26.851239
217.227548	9870.969463	26.856256
217.369227	9887.975267	26.861274
217.870629	9891.410998	26.866292
217.691083	9910.989919	26.871309
218.123114	9925.023346	26.876327
218.347286	9934.763679	26.881344
218.581595	9942.873199	26.886362
218.690264	9958.826502	26.891380
218.650664	9980.521150	26.896397
219.076274	9985.329623	26.901415
219.272356	10004.963465	26.906432
219.148823	10019.232396	26.911450
219.350121	10031.647553	26.916468
219.827246	10056.649271	26.921485
219.945962	10067.081886	26.926503
220.595699	10082.660048	26.931520
220.723358	10106.924060	26.936538
220.856269	10117.682855	26.941556
220.946330	10133.996015	26.946573
221.313060	10156.283962	26.951591
221.125294	10170.010515	26.956608
221.446183	10179.189584	26.961626
222.494895	10193.372887	26.966644
222.499788	10213.298969	26.971661
222.741549	10218.300493	26.976679
223.092501	10240.006880	26.981696
223.308059	10247.699527	26.986714
223.573376	10259.381745	26.991732
223.602500	10278.634716	26.996749
223.815577	10279.289744	27.001767
223.877769	10293.267718	27.006784
223.842094	10309.468114	27.011802
224.455450	10321.117951	27.016820
224.164909	10333.802966	27.021837
224.361294	10354.558037	27.026855
225.014025	10365.036618	27.031872
224.981042	10381.211395	27.036890
225.562852	10403.027051	27.041908
225.515511	10412.986988	27.046925
225.944959	10425.792929	27.051943
226.095218	10446.653211	27.056960
226.361809	10456.222980	27.061978
227.042366	10469.996859	27.066996
227.195253	10478.315133	27.072013
227.328809	10485.436584	27.077031
227.477508	10497.847662	27.082048
227.262893	10505.254162	27.087066
227.923341	10520.250030	27.092084
227.873523	10542.019552	27.097101
228.094029	10550.971400	27.102119
228.339645	10568.422540	27.107136
228.185243	10589.554892	27.112154
228.681231	10601.090675	27.117172
228.444748	10616.656555	27.122189
228.730224	10628.752642	27.127207
229.323225	10645.783159	27.132224
229.367604	10666.031921	27.137242
229.690180	10681.724988	27.142260
229.762542	10705.584801	27.147277
229.947359	10717.554624	27.152295
230.448389	10729.515966	27.157312
230.345965	10746.772348	27.162330
230.974565	10768.480059	27.167348
230.582242	10782.403298	27.172365
231.152497	10808.291338	27.177383
231.637734	10820.128909	27.182400
232.024230	10843.646032	27.187418
232.476228	10846.742349	27.192436
232.452681	10872.331962	27.197453
232.368664	10876.345855	27.202471
232.685922	10893.467159	27.207488
232.800339	10917.014367	27.212506
233.028310	10926.691470	27.217524
233.114850	10950.274663	27.222541
233.833031	10962.571575	27.227559
233.936457	10991.387465	27.232576
233.846974	11004.401401	27.237594
234.197684	11015.919151	27.242612
234.174333	11044.972859	27.247629
234.459645	11070.700656	27.252647
235.208124	11083.706521	27.257664
235.101008	11111.841959	27.262682
235.351816	11122.570231	27.267700
235.730991	11146.815134	27.272717
235.816455	11171.263962	27.277735
236.188666	11177.719921	27.282752
236.177185	11211.322172	27.287770
236.633915	11227.907238	27.292788
236.788457	11251.792762	27.297805
237.258436	11272.528093	27.302823
237.733611	11290.591261	27.307840
237.615309	11303.805693	27.312858
238.031220	11326.810432	27.317876
238.093068	11337.843145	27.322893
238.492781	11355.956090	27.327911
239.001774	11374.326649	27.332928
239.018377	11381.766740	27.337946
239.424536	11390.418347	27.342964
239.447839	11417.892805	27.347981
239.606724	11430.953384	27.352999
239.910250	11441.916722	27.358016
239.951670	11460.802688	27.363034
240.344339	11486.365826	27.368052
240.375071	11505.840841	27.373069
240.442171	11518.802183	27.378087
240.923141	11539.435041	27.383104
241.137582	11575.121360	27.388122
241.420587	11581.695638	27.393140
241.695972	11605.654254	27.398157
242.091817	11620.588254	27.403175
242.217182	11643.042091	27.408192
242.488832	11671.257967	27.413210
242.844863	11673.235838	27.418228
243.265807	11701.415741	27.423245
243.780413	11714.158701	27.428263
244.393835	11728.806085	27.433280
244.168249	11736.685287	27.438298
244.606447	11739.578665	27.443316
244.553002	11755.950451	27.448333
244.710722	11768.777776	27.453351
245.018669	11790.205343	27.458368
245.168096	11795.187020	27.463386
245.476100	11806.427750	27.468404
245.238294	11812.382679	27.473421
245.619746	11829.112695	27.478439
246.166687	11839.352903	27.483456
246.188577	11854.437246	27.488474
246.302066	11869.140952	27.493492
246.531311	11896.451220	27.498509
246.597565	11916.037931	27.503527
246.978840	11922.840082	27.508544
246.785471	11957.154232	27.513562
247.409193	11976.511576	27.518580
247.553561	11999.543889	27.523597
247.731389	12014.597615	27.528615
248.258560	12040.813041	27.533632
248.508596	12070.052862	27.538650
248.427007	12084.629408	27.543668
248.735382	12106.069898	27.548685
248.992892	12122.077510	27.553703
249.227586	12135.066705	27.558720
249.483517	12178.023217	27.563738
249.531528	12196.378377	27.568756
250.360447	12220.301587	27.573773
250.192522	12239.726377	27.578791
250.846429	12256.821448	27.583808
250.714905	12279.316285	27.588826
251.047382	12301.214262	27.593844
251.766246	12322.357015	27.598861
251.976728	12335.337509	27.603879
252.452993	12351.721565	27.608896
252.614278	12370.292829	27.613914
252.664196	12394.695128	27.618932
253.023983	12403.989193	27.623949
253.104841	12418.164766	27.628967
253.576632	12443.931541	27.633984
253.349689	12469.937284	27.639002
253.760432	12483.843336	27.644020
254.321219	12502.661615	27.649037
254.304846	12518.185108	27.654055
254.685712	12527.122252	27.659072
254.811737	12564.349537	27.664090
255.229218	12583.648237	27.669108
255.267060	12604.768520	27.674125
255.575091	12630.349626	27.679143
255.750646	12638.605307	27.684160
256.296246	12673.875513	27.689178
256.704516	12686.740002	27.694196
256.841428	12700.265954	27.699213
256.896577	12732.856268	27.704231
257.581554	12732.010095	27.709248
257.431988	12751.571481	27.714266
257.825342	12777.341526	27.719284
258.400177	12789.519991	27.724301
258.311552	12814.945590	27.729319
258.741309	12826.212066	27.734336
258.594545	12850.456290	27.739354
259.096389	12858.799901	27.744372
259.880207	12884.486819	27.749389
259.865360	12902.745142	27.754407
260.152960	12914.119204	27.759424
260.184699	12935.016599	27.764442
260.674780	12943.103140	27.769460
260.807397	12961.366840	27.774477
261.062904	12979.270251	27.779495
261.603539	12994.710034	27.784512
261.682265	13011.014832	27.789530
261.913539	13027.873649	27.794548
261.994068	13039.501281	27.799565
262.105133	13059.716903	27.804583
262.548861	13070.280273	27.809600
262.437108	13090.300302	27.814618
262.747574	13114.037439	27.819636
263.011604	13132.691252	27.824653
263.433459	13164.283791	27.829671
263.857243	13169.516543	27.834688
263.854596	13197.455557	27.839706
263.865986	13216.183767	27.844724
264.266914	13240.551117	27.849741
264.602690	13262.329688	27.854759
264.814638	13282.052888	27.859776
265.275936	13299.286451	27.864794
265.313416	13315.133747	27.869812
265.576715	13330.541459	27.874829
265.381660	13358.119259	27.879847
265.769693	13383.417263	27.884864
266.098839	13410.960392	27.889882
266.043987	13433.994079	27.894900
266.526987	13466.559683	27.899917
266.782729	13498.371438	27.904935
267.027443	13532.092421	27.909952
267.400726	13563.961666	27.914970
267.610557	13582.782314	27.919988
268.338417	13607.923168	27.925005
267.869277	13642.005657	27.930023
268.433037	13662.034156	27.935040
268.809114	13698.397088	27.940058
268.969473	13723.993329	27.945076
269.964643	13737.540318	27.950093
269.922103	13774.745855	27.955111
270.042171	13796.044065	27.960128
270.567485	13818.384142	27.965146
270.555136	13847.080407	27.970164
270.649888	13864.564547	27.975181
270.914209	13894.878693	27.980199
271.638189	13918.801547	27.985216
271.836613	13943.725765	27.990234
272.110231	13965.094853	27.995252
272.593773	13990.179744	28.000269
273.071801	14005.930180	28.005287
273.298978	14017.295422	28.010304
273.552209	14047.715766	28.015322
273.730904	14062.587814	28.020340
274.156077	14089.308407	28.025357
274.505318	14099.198685	28.030375
275.056392	14117.202141	28.035392
275.072372	14133.827226	28.040410
274.882607	14158.092483	28.045428
275.131319	14171.406166	28.050445
275.582879	14197.235343	28.055463
276.106109	14222.273267	28.060480
276.082439	14244.030318	28.065498
276.318982	14267.966807	28.070516
277.022488	14288.293048	28.075533
276.940282	14306.222190	28.080551
277.534604	14332.919785	28.085568
277.579694	14356.491607	28.090586
277.750190	14374.690726	28.095604
277.948816	14391.078985	28.100621
277.871961	14422.957020	28.105639
278.391948	14439.061275	28.110656
278.797835	14462.147196	28.115674
279.005905	14484.300888	28.120692
279.290261	14513.368557	28.125709
279.156688	14539.713056	28.130727
279.688409	14563.009935	28.135744
280.239966	14588.223920	28.140762
280.118601	14625.519260	28.145780
280.737235	14638.339488	28.150797
280.622488	14667.330950	28.155815
281.156563	14690.858166	28.160832
281.581927	14708.442883	28.165850
281.390195	14732.557582	28.170868
282.173881	14757.624890	28.175885
282.377581	14782.309352	28.180903
282.383157	14796.163717	28.185920
283.171375	14819.676547	28.190938
283.338699	14845.301627	28.195956
283.373873	14862.341227	28.200973
283.835629	14884.752519	28.205991
284.024788	14905.940081	28.211008
284.332396	14924.746737	28.216026
284.409951	14951.560892	28.221044
285.050947	14967.488724	28.226061
285.415879	15002.845246	28.231079
285.570862	15024.003551	28.236096
285.742776	15041.312451	28.241114
285.941154	15068.717390	28.246132
285.988657	15091.967596	28.251149
286.530125	15121.321215	28.256167
286.760489	15140.920281	28.261184
287.049091	15170.951562	28.266202
287.517414	15193.324287	28.271220
288.084316	15214.478284	28.276237
288.010471	15248.476442	28.281255
288.588084	15270.718439	28.286272
288.928441	15288.354906	28.291290
289.119282	15316.263551	28.296308
289.672449	15329.738799	28.301325
289.670644	15358.141956	28.306343
289.840700	15365.025811	28.311360
290.143490	15394.559363	28.316378
290.310593	15432.003741	28.321396
290.995235	15447.931455	28.326413
290.946383	15466.671308	28.331431
291.373873	15493.125044	28.336448
291.485281	15529.842442	28.341466
291.803832	15555.729034	28.346484
291.959349	15563.398511	28.351501
292.110612	15606.799218	28.356519
292.263988	15631.183137	28.361536
292.968199	15664.368466	28.366554
292.807696	15695.247880	28.371572
293.406639	15719.451571	28.376589
293.852063	15750.782557	28.381607
294.117393	15785.148598	28.386624
294.791514	15804.138743	28.391642
294.997069	15831.786844	28.396660
295.224692	15854.962382	28.401677
295.473098	15874.729926	28.406695
295.740710	15901.964130	28.411712
296.026933	15923.491354	28.416730
295.940633	15953.667866	28.421748
296.604200	15977.056360	28.426765
296.666143	15999.518954	28.431783
296.619176	16032.494114	28.436800
297.100663	16059.028607	28.441818
297.496218	16095.573078	28.446836
297.693350	16111.776696	28.451853
297.810591	16149.912507	28.456871
298.521829	16188.596513	28.461888
298.773788	16213.272098	28.466906
298.689264	16239.895506	28.471924
298.813920	16271.350234	28.476941
299.920535	16302.006860	28.481959
300.134199	16322.882617	28.486976
300.338956	16339.919071	28.491994
300.894581	16361.407743	28.497012
301.305284	16391.254405	28.502029
301.587331	16411.718417	28.507047
302.003170	16427.865931	28.512064
302.414940	16438.647800	28.517082
303.101365	16455.599430	28.522100
302.953286	16472.978698	28.527117
303.301751	16490.100163	28.532135
303.246016	16510.380305	28.537152
303.764565	16527.573074	28.542170
303.965986	16554.505878	28.547188
304.258096	16569.002035	28.552205
304.616188	16605.250123	28.557223
304.473424	16621.002049	28.562240
304.806258	16646.451995	28.567258
305.057992	16679.100359	28.572276
305.320076	16708.200110	28.577293
305.702135	16729.321563	28.582311
306.052285	16767.311561	28.587328
306.467293	16787.069737	28.592346
306.595912	16822.403454	28.597364
306.702106	16844.699013	28.602381
307.129142	16874.708112	28.607399
307.308831	16902.235458	28.612416
307.817536	16935.491510	28.617434
308.053562	16977.482773	28.622452
308.271437	16995.743286	28.627469
308.736741	17031.337344	28.632487
308.930598	17062.690922	28.637504
309.439324	17088.840377	28.642522
309.761167	17119.782331	28.647540
309.838585	17152.038705	28.652557
310.243978	17186.113661	28.657575
310.587811	17215.529867	28.662592
311.177149	17244.478085	28.667610
311.400363	17274.582906	28.672628
312.047074	17294.273719	28.677645
312.143311	17316.552431	28.682663
312.214322	17350.048327	28.687680
312.976294	17376.992386	28.692698
313.495398	17404.277759	28.697716
313.434896	17416.934593	28.702733
313.960058	17443.467310	28.707751
314.189721	17469.471475	28.712768
314.773864	17494.681017	28.717786
314.760448	17529.157003	28.722804
315.282815	17551.211298	28.727821
315.361336	17576.765480	28.732839
315.757682	17600.014603	28.737856
316.103652	17617.244856	28.742874
315.882075	17655.531473	28.747892
316.244419	17680.750732	28.752909
316.610066	17704.724975	28.757927
316.854712	17734.429155	28.762944
317.253302	17762.845779	28.767962
317.770028	17802.413186	28.772980
318.011677	17821.605736	28.777997
318.457195	17851.581868	28.783015
318.688230	17885.786448	28.788032
318.949269	17912.512802	28.793050
319.723278	17930.661810	28.798068
320.280105	17953.077580	28.803085
320.357758	17981.873308	28.808103
320.207173	18005.954060	28.813120
320.807970	18033.271745	28.818138
320.964217	18057.967836	28.823156
321.468279	18077.858685	28.828173
321.836719	18093.910780	28.833191
322.010633	18123.797210	28.838208
322.256320	18146.716806	28.843226
322.330364	18174.584704	28.848244
322.487902	18198.844860	28.853261
322.707705	18224.864217	28.858279
323.070657	18264.974697	28.863296
323.484613	18290.129805	28.868314
323.726531	18326.809959	28.873332
324.398422	18351.545684	28.878349
324.600797	18378.762009	28.883367
324.646152	18420.912617	28.888384
325.115405	18450.620614	28.893402
325.296058	18477.543549	28.898420
325.280402	18511.781556	28.903437
325.945131	18543.562862	28.908455
326.215603	18584.465563	28.913472
326.699929	18604.189466	28.918490
327.063156	18649.127425	28.923508
327.224032	18676.369619	28.928525
327.808707	18708.959771	28.933543
328.035744	18749.256801	28.938560
328.606476	18779.505366	28.943578
328.681347	18816.016758	28.948596
329.279784	18843.607617	28.953613
329.298854	18874.005922	28.958631
329.637904	18905.984146	28.963648
330.350383	18934.069012	28.968666
330.380435	18969.090387	28.973684
330.663407	18999.801348	28.978701
331.098065	19030.330650	28.983719
331.388011	19070.252053	28.988736
331.812147	19102.103549	28.993754
332.254144	19137.686167	28.998772
332.802238	19167.566126	29.003789
333.159694	19193.407266	29.008807
333.258329	19229.997841	29.013824
333.611654	19264.318361	29.018842
333.512608	19299.158376	29.023860
333.726886	19332.609969	29.028877
334.366833	19366.411924	29.033895
334.784422	19401.506045	29.038912
335.388987	19425.672431	29.043930
335.691298	19466.609900	29.048948
335.914683	19495.144950	29.053965
336.441324	19522.065672	29.058983
336.480679	19556.284254	29.064000
337.419812	19577.763807	29.069018
338.114280	19596.684998	29.074036
338.220307	19621.498342	29.079053
338.643215	19636.108982	29.084071
339.122739	19665.930947	29.089088
339.258642	19679.455646	29.094106
339.873212	19713.445402	29.099124
339.950403	19738.895218	29.104141
340.563769	19753.425567	29.109159
340.552576	19782.383184	29.114176
340.690775	19807.185405	29.119194
341.237379	19824.228232	29.124212
341.092740	19859.329109	29.129229
341.557813	19880.327260	29.134247
341.769459	19911.556276	29.139264
341.972212	19939.343347	29.144282
342.816621	19980.064292	29.149300
343.089471	20001.680273	29.154317
343.325298	20025.721934	29.159335
343.805036	20051.924144	29.164352
344.340324	20068.672003	29.169370
344.428631	20100.628276	29.174388
344.687295	20122.530930	29.179405
345.312153	20149.917315	29.184423
345.144207	20169.871340	29.189440
345.162141	20196.329309	29.194458
345.717094	20226.077130	29.199476
346.033217	20258.080110	29.204493
346.612062	20295.374595	29.209511
346.733689	20334.888982	29.214528
346.760840	20355.134865	29.219546
347.366830	20387.465428	29.224564
347.359547	20431.334545	29.229581
347.903558	20458.961485	29.234599
348.020189	20500.107109	29.239616
348.719752	20535.076953	29.244634
348.981875	20570.658758	29.249652
349.228230	20606.685383	29.254669
350.161002	20630.719707	29.259687
350.359138	20675.264847	29.264704
350.431345	20703.831653	29.269722
350.779550	20739.880478	29.274740
350.938320	20771.163370	29.279757
351.477348	20807.492029	29.284775
351.478614	20851.417608	29.289792
351.898582	20889.553185	29.294810
352.525443	20926.279004	29.299828
352.878915	20960.381322	29.304845
353.305402	21000.493773	29.309863
352.897025	21044.743007	29.314880
353.676771	21076.573599	29.319898
354.321933	21114.238359	29.324916
354.421690	21160.619738	29.329933
355.317132	21196.962790	29.334951
354.928145	21236.306225	29.339968
355.675993	21276.191979	29.344986
356.138220	21314.536590	29.350004
356.634300	21361.734642	29.355021
356.568614	21389.022409	29.360039
356.748608	21438.127826	29.365056
357.424988	21470.423868	29.370074
357.976098	21513.936221	29.375092
358.255330	21543.419610	29.380109
358.456727	21576.099841	29.385127
359.259505	21615.099382	29.390144
359.303703	21655.513156	29.395162
360.245155	21685.878741	29.400180
360.389725	21723.705221	29.405197
360.672747	21755.482025	29.410215
361.489435	21785.766208	29.415232
361.670222	21810.564279	29.420250
362.244256	21834.630996	29.425268
362.793974	21874.094044	29.430285
363.474229	21899.110971	29.435303
362.977047	21937.139484	29.440320
363.187772	21956.321973	29.445338
363.689993	21987.843656	29.450356
364.127627	22027.804796	29.455373
364.320781	22055.754323	29.460391
364.971472	22094.443735	29.465408
364.712668	22126.230180	29.470426
365.108128	22162.615416	29.475444
365.526326	22191.913712	29.480461
366.101171	22215.026617	29.485479
366.603768	22255.249750	29.490496
367.080133	22282.744508	29.495514
367.497553	22316.396826	29.500532
367.967326	22352.789727	29.505549
368.185282	22378.966529	29.510567
368.556666	22410.547293	29.515584
368.651036	22433.621974	29.520602
369.352099	22459.957009	29.525620
369.652219	22504.749369	29.530637
369.516897	22522.893431	29.535655
370.005421	22559.113161	29.540672
370.511673	22593.977917	29.545690
370.675504	22620.106644	29.550708
370.941887	22660.317047	29.555725
371.531558	22696.919283	29.560743
371.533444	22739.395573	29.565760
372.070299	22770.325405	29.570778
372.173975	22804.173032	29.575796
372.587539	22848.777782	29.580813
372.884178	22882.740656	29.585831
373.214300	22930.808878	29.590848
373.521748	22977.256756	29.595866
374.165851	23012.031142	29.600884
374.369740	23050.059386	29.605901
375.137499	23097.465461	29.610919
375.352648	23143.643823	29.615936
375.795323	23177.868687	29.620954
376.629702	23211.078057	29.625972
376.690109	23254.475197	29.630989
377.019149	23287.346783	29.636007
377.409500	23327.141004	29.641024
377.784534	23363.683298	29.646042
378.313278	23398.432194	29.651060
378.730024	23444.636548	29.656077
379.450812	23474.495986	29.661095
379.564360	23520.564750	29.666112
379.742933	23546.610231	29.671130
380.575742	23573.772892	29.676148
380.998427	23612.614723	29.681165
381.089283	23652.595530	29.686183
381.403098	23694.058134	29.691200
381.642589	23726.957109	29.696218
382.159804	23763.768555	29.701236
382.125317	23807.358701	29.706253
382.867605	23839.711470	29.711271
383.268951	23872.553736	29.716288
383.623104	23918.712116	29.721306
384.336241	23948.466032	29.726324
384.706233	23984.612129	29.731341
385.149790	24030.200652	29.736359
385.559788	24063.124028	29.741376
386.041131	24104.137837	29.746394
386.048434	24128.492009	29.751412
386.343427	24171.367792	29.756429
386.733236	24199.845637	29.761447
387.452560	24242.990040	29.766464
387.567605	24275.138429	29.771482
388.030375	24311.055719	29.776500
388.484893	24348.895507	29.781517
388.815237	24386.280850	29.786535
389.330322	24427.606013	29.791552
389.825971	24461.692068	29.796570
390.205309	24499.973648	29.801588
390.455069	24540.455861	29.806605
390.774813	24569.450774	29.811623
391.000578	24606.233586	29.816640
391.147152	24652.331375	29.821658
391.183399	24699.874793	29.826676
391.299629	24746.173459	29.831693
392.072948	24788.394227	29.836711
392.436788	24834.945018	29.841728
392.903772	24880.904667	29.846746
393.497246	24907.468341	29.851764
393.528559	24956.946973	29.856781
394.254145	24991.907952	29.861799
394.532703	25035.938349	29.866816
394.638352	25074.447166	29.871834
395.440870	25109.775487	29.876852
395.685918	25168.277409	29.881869
396.078409	25196.579292	29.886887
396.595024	25228.666305	29.891904
397.007655	25274.818642	29.896922
397.661352	25314.379643	29.901940
397.945579	25359.092401	29.906957
398.319909	25399.917063	29.911975
399.002774	25433.273934	29.916992
399.049131	25479.692669	29.922010
399.796055	25511.276384	29.927028
400.196810	25549.878922	29.932045
400.481973	25589.725708	29.937063
401.361970	25616.220158	29.942080
401.695263	25655.263222	29.947098
402.030027	25686.646334	29.952116
402.403154	25723.673542	29.957133
402.527145	25762.831757	29.962151
402.934415	25794.424879	29.967168
403.309879	25847.586905	29.972186
404.100221	25873.451097	29.977204
404.374616	25909.748349	29.982221
404.625140	25943.167465	29.987239
405.467151	25984.754299	29.992256
405.885424	26026.957438	29.997274
406.084109	26058.950210	30.002292
406.655884	26101.325383	30.007309
406.444704	26138.786160	30.012327
407.139634	26164.589829	30.017344
407.482255	26201.730133	30.022362
408.155503	26233.364441	30.027380
408.437716	26280.639208	30.032397
408.790021	26317.936212	30.037415
409.275642	26358.669537	30.042432
409.454392	26409.089295	30.047450
410.077756	26435.827269	30.052468
410.332663	26483.233189	30.057485
410.525002	26522.565453	30.062503
411.018844	26564.884281	30.067520
411.458930	26610.681434	30.072538
411.947124	26642.421211	30.077556
411.999774	26701.147310	30.082573
412.207095	26742.266292	30.087591
412.903722	26788.959067	30.092608
412.772678	26836.457867	30.097626
413.569996	26881.485480	30.102644
414.169188	26936.429255	30.107661
414.427163	26978.570998	30.112679
414.872478	27034.303904	30.117696
414.958606	27081.421637	30.122714
415.441363	27124.482853	30.127732
416.150464	27177.570825	30.132749
416.597447	27211.100306	30.137767
417.003378	27256.803139	30.142784
417.362552	27307.854191	30.147802
417.857415	27354.175359	30.152820
418.356729	27395.028707	30.157837
418.967578	27440.206855	30.162855
419.485860	27491.182881	30.167872
419.449376	27538.118619	30.172890
419.922140	27577.377395	30.177908
420.398063	27621.262404	30.182925
421.095179	27662.534065	30.187943
421.857338	27699.649316	30.192960
421.768573	27746.246089	30.197978
422.190140	27775.501433	30.202996
422.851966	27815.287267	30.208013
423.120545	27859.413847	30.213031
423.977717	27888.221884	30.218048
424.034153	27929.518591	30.223066
424.529471	27969.387693	30.228084
424.951112	28004.945065	30.233101
424.945159	28050.240139	30.238119
425.674934	28085.224769	30.243136
425.795881	28130.936274	30.248154
426.366135	28179.478722	30.253172
427.057969	28217.414985	30.258189
427.632094	28268.093450	30.263207
428.171715	28298.108506	30.268224
428.290245	28349.300988	30.273242
428.355651	28388.106824	30.278260
428.533841	28429.391789	30.283277
428.790654	28476.473362	30.288295
429.492025	28514.446608	30.293312
429.995254	28576.280584	30.298330
430.511438	28625.938710	30.303348
431.647114	28663.964304	30.308365
431.594113	28703.383446	30.313383
432.692491	28748.867379	30.318400
432.977096	28787.361516	30.323418
433.704861	28823.852106	30.328436
433.805661	28855.807711	30.333453
434.341865	28898.055214	30.338471
434.684209	28933.923706	30.343488
435.102924	28981.170708	30.348506
435.118835	29017.709932	30.353524
436.243291	29054.202007	30.358541
436.453715	29091.747541	30.363559
437.092989	29132.759427	30.368576
437.138983	29172.208209	30.373594
437.649169	29219.100094	30.378612
437.890346	29260.364222	30.383629
438.383258	29300.615556	30.388647
439.076961	29340.911371	30.393664
439.368229	29397.420733	30.398682
439.574968	29432.047112	30.403700
440.276453	29468.802131	30.408717
440.721804	29506.355872	30.413735
440.983074	29552.497362	30.418752
441.291861	29594.573320	30.423770
441.719384	29635.176893	30.428788
442.223178	29684.150509	30.433805
442.535410	29732.642227	30.438823
443.852157	29764.819665	30.443840
444.037818	29812.863627	30.448858
444.504435	29850.812903	30.453876
445.370726	29890.545456	30.458893
445.130011	29930.571583	30.463911
446.250059	29958.405812	30.468928
446.104184	30002.703054	30.473946
446.556086	30040.914158	30.478964
446.922649	30089.322348	30.483981
446.988232	30132.082271	30.488999
447.751414	30176.376566	30.494016
448.175175	30223.676198	30.499034
448.479755	30265.608791	30.504052
449.023125	30305.411687	30.509069
449.319818	30364.837008	30.514087
449.435191	30404.568062	30.519104
449.822948	30453.081248	30.524122
450.083298	30501.519682	30.529140
450.406609	30554.057320	30.534157
450.746196	30606.225895	30.539175
451.558027	30649.375718	30.544192
451.644718	30703.562777	30.549210
452.204391	30751.544014	30.554228
453.049642	30812.401863	30.559245
453.003505	30848.600036	30.564263
453.817494	30902.901274	30.569280
454.473818	30958.851998	30.574298
455.042757	30997.331008	30.579316
455.645168	31040.963282	30.584333
456.463641	31093.614377	30.589351
456.738827	31136.002170	30.594368
457.121159	31176.944574	30.599386
457.561728	31218.137125	30.604404
458.177714	31252.658198	30.609421
458.107146	31295.233227	30.614439
458.968431	31339.097413	30.619456
459.242788	31398.598730	30.624474
459.813768	31444.183865	30.629492
460.401665	31491.125626	30.634509
460.619589	31539.478300	30.639527
461.115956	31580.239271	30.644544
461.593288	31629.461858	30.649562
462.190439	31684.513466	30.654580
462.362300	31720.716941	30.659597
462.782964	31778.141835	30.664615
463.341736	31824.134312	30.669632
463.651120	31881.829796	30.674650
463.741073	31932.510906	30.679668
464.421019	31985.919297	30.684685
465.060805	32036.830636	30.689703
465.672031	32086.501152	30.694720
466.065214	32145.688858	30.699738
466.795794	32191.402357	30.704756
467.362283	32238.292257	30.709773
467.871029	32288.232183	30.714791
468.208507	32339.109424	30.719808
468.771641	32382.845493	30.724826
468.943129	32433.970234	30.729844
469.582874	32479.843998	30.734861
469.687208	32537.390068	30.739879
470.365609	32592.646296	30.744896
470.834858	32640.917899	30.749914
471.208148	32704.295530	30.754932
472.202481	32756.417513	30.759949
472.169178	32807.714329	30.764967
472.567768	32859.980458	30.769984
473.309314	32905.700123	30.775002
473.372157	32959.972641	30.780020
474.404684	32990.663323	30.785037
474.971168	33043.618021	30.790055
475.973412	33087.255174	30.795072
476.488550	33125.746538	30.800090
476.504867	33175.651909	30.805108
477.630046	33218.922357	30.810125
477.782138	33263.793111	30.815143
478.374609	33312.862536	30.820160
478.600451	33353.580824	30.825178
479.011787	33404.847388	30.830196
479.440502	33443.245391	30.835213
479.795833	33488.072145	30.840231
480.227145	33536.731093	30.845248
480.430678	33578.724106	30.850266
480.966222	33629.219399	30.855284
481.564312	33673.079132	30.860301
481.816977	33727.968786	30.865319
482.192616	33776.396755	30.870336
482.905290	33819.423252	30.875354
483.160037	33867.149605	30.880372
483.899332	33906.726367	30.885389
483.785016	33959.530783	30.890407
484.877512	34010.742713	30.895424
485.061866	34054.193855	30.900442
485.621295	34102.012113	30.905460
486.410820	34151.880883	30.910477
486.763970	34190.367955	30.915495
487.148269	34242.096015	30.920512
487.823044	34289.283342	30.925530
487.648506	34351.367090	30.930548
488.535122	34403.642808	30.935565
488.997740	34456.686878	30.940583
489.002738	34520.222499	30.945600
489.692204	34568.514614	30.950618
490.311026	34616.463834	30.955636
490.990258	34668.064546	30.960653
491.749618	34719.937357	30.965671
492.003196	34771.744091	30.970688
492.725203	34828.801341	30.975706
492.841992	34888.937885	30.980724
493.240667	34937.693692	30.985741
493.646177	34995.958033	30.990759
494.070634	35048.092755	30.995776
495.120514	35106.970954	31.000794
495.170615	35166.574966	31.005812
496.100906	35216.986934	31.010829
496.328677	35273.635931	31.015847
496.733374	35330.965532	31.020864
497.905627	35371.754452	31.025882
498.047728	35431.066588	31.030900
498.758508	35481.007730	31.035917
499.233690	35538.162454	31.040935
499.910614	35591.871324	31.045952
500.467844	35630.872824	31.050970
500.728019	35688.396745	31.055988
501.609134	35741.928583	31.061005
502.484848	35785.237048	31.066023
503.144009	35819.126562	31.071040
503.404241	35861.949863	31.076058
503.574471	35911.369666	31.081076
504.430519	35946.815637	31.086093
504.569509	36009.354644	31.091111
504.944908	36054.923491	31.096128
505.395086	36100.309998	31.101146
505.553529	36153.134052	31.106164
506.551354	36200.787209	31.111181
507.371408	36256.739030	31.116199
507.752254	36306.019266	31.121216
508.065504	36356.568520	31.126234
508.126102	36403.774542	31.131252
509.059441	36452.083330	31.136269
509.098361	36510.023514	31.141287
509.894690	36561.509311	31.146304
510.458221	36614.580899	31.151322
510.698510	36674.134041	31.156340
511.142405	36726.535404	31.161357
511.487162	36781.475433	31.166375
512.170628	36840.649782	31.171392
512.982459	36894.638000	31.176410
513.419179	36950.240658	31.181428
514.065715	36996.578438	31.186445
514.411791	37054.471986	31.191463
514.878044	37116.261070	31.196480
515.470915	37158.332967	31.201498
515.987141	37232.217631	31.206516
516.439752	37275.797741	31.211533
516.845213	37320.529875	31.216551
517.342033	37376.143194	31.221568
517.532630	37414.048172	31.226586
517.766186	37483.652688	31.231604
518.531306	37522.511257	31.236621
518.977977	37574.977494	31.241639
519.638141	37631.444865	31.246656
520.275766	37695.649677	31.251674
520.649461	37758.428939	31.256692
521.299293	37807.670496	31.261709
521.742127	37870.401314	31.266727
521.874398	37924.947538	31.271744
522.603585	37986.767502	31.276762
522.997044	38051.239269	31.281780
524.035473	38111.025512	31.286797
524.225038	38163.457566	31.291815
524.622364	38220.201626	31.296832
525.365286	38287.199457	31.301850
525.838505	38355.719504	31.306868
526.439048	38399.689766	31.311885
526.931119	38467.859408	31.316903
527.657834	38530.800636	31.321920
528.333734	38590.202319	31.326938
528.406851	38656.604253	31.331956
529.033691	38705.092594	31.336973
529.823642	38766.930571	31.341991
530.023279	38827.994803	31.347008
530.979040	38882.768607	31.352026
531.566854	38945.789713	31.357044
531.878553	38996.952513	31.362061
532.882624	39053.432982	31.367079
533.386070	39117.346837	31.372096
534.146141	39168.578945	31.377114
534.557833	39228.833237	31.382132
535.251164	39278.324296	31.387149
535.949860	39336.409051	31.392167
536.417705	39380.958610	31.397184
537.048816	39416.236848	31.402202
537.625052	39474.549848	31.407220
538.467260	39526.826067	31.412237
538.649398	39576.543325	31.417255
538.991735	39630.422203	31.422272
539.731132	39676.681632	31.427290
539.947846	39729.372512	31.432308
540.762630	39786.289285	31.437325
540.789481	39843.487720	31.442343
541.296920	39903.754183	31.447360
542.066556	39952.235597	31.452378
542.095189	40015.745815	31.457396
542.543885	40085.318671	31.462413
543.122471	40145.833957	31.467431
543.354132	40209.426778	31.472448
544.080296	40264.157812	31.477466
544.726039	40337.628031	31.482484
545.216732	40407.366094	31.487501
545.879532	40479.360536	31.492519
546.269367	40547.748770	31.497536
546.730014	40611.901395	31.502554
547.092645	40674.595957	31.507572
547.291003	40731.390385	31.512589
548.354011	40813.992656	31.517607
548.655346	40881.219434	31.522624
549.549996	40948.068889	31.527642
550.503214	41018.862229	31.532660
551.130185	41074.540539	31.537677
552.078277	41131.560109	31.542695
552.336909	41193.614687	31.547712
553.230073	41238.139372	31.552730
553.297687	41294.538310	31.557748
553.901566	41333.302471	31.562765
554.421534	41393.058780	31.567783
555.071394	41452.788583	31.572800
555.891249	41495.402566	31.577818
556.406481	41547.039117	31.582836
557.000723	41607.246080	31.587853
557.514485	41663.974549	31.592871
557.629228	41717.141566	31.597888
558.685893	41762.742219	31.602906
559.262896	41820.517425	31.607924
559.837812	41870.020255	31.612941
560.320167	41921.738732	31.617959
560.634973	41972.800490	31.622976
561.613236	42022.816052	31.627994
561.619274	42096.322780	31.633012
562.045017	42139.765048	31.638029
562.529258	42208.763507	31.643047
563.225943	42259.487823	31.648064
564.061435	42326.287489	31.653082
564.551613	42396.303921	31.658100
565.229910	42443.027838	31.663117
565.755273	42510.951880	31.668135
566.197364	42571.096756	31.673152
567.291741	42614.365664	31.678170
567.834019	42669.080896	31.683188
568.970927	42714.898656	31.688205
569.712753	42763.839722	31.693223
569.935496	42803.690827	31.698240
570.747577	42849.104335	31.703258
571.882024	42898.161309	31.708276
572.184867	42944.850214	31.713293
572.915915	42968.138751	31.718311
573.165103	43008.783050	31.723328
573.989361	43060.785880	31.728346
574.395196	43103.739801	31.733364
574.880786	43153.360701	31.738381
575.460967	43199.728399	31.743399
575.504587	43258.621912	31.748416
576.333647	43295.456695	31.753434
576.653829	43361.587495	31.758452
577.027071	43412.630773	31.763469
577.903051	43464.278561	31.768487
578.046392	43521.253245	31.773504
578.558206	43574.267657	31.778522
578.996055	43638.236575	31.783540
579.482110	43704.557476	31.788557
579.892182	43762.680167	31.793575
580.494961	43829.153943	31.798592
581.079230	43886.275567	31.803610
581.786174	43965.143849	31.808628
581.796447	44035.341822	31.813645
582.685464	44091.448453	31.818663
583.016718	44167.662673	31.823680
583.607450	44243.653077	31.828698
584.215118	44315.833130	31.833716
584.555670	44389.345659	31.838733
585.469231	44463.382265	31.843751
585.593320	44541.268523	31.848768
586.247433	44608.603185	31.853786
586.447998	44684.264006	31.858804
587.375189	44760.260401	31.863821
588.009120	44828.465498	31.868839
588.704166	44918.301368	31.873856
589.283214	44980.765483	31.878874
589.894933	45056.046881	31.883892
590.387461	45130.094703	31.888909
591.345304	45195.928643	31.893927
591.754226	45270.578318	31.898944
592.368750	45338.977780	31.903962
593.044570	45385.278112	31.908980
593.804599	45447.392565	31.913997
594.142639	45520.814311	31.919015
594.598578	45591.624225	31.924032
595.538371	45660.106567	31.929050
595.988717	45730.512937	31.934068
596.239146	45800.520674	31.939085
597.137595	45863.671029	31.944103
597.540537	45935.704907	31.949120
598.399146	45998.241935	31.954138
599.228691	46074.251747	31.959156
599.834839	46143.565912	31.964173
600.359580	46201.771860	31.969191
600.720127	46278.304960	31.974208
601.418711	46349.996534	31.979226
602.324350	46424.584892	31.984244
602.977165	46493.778955	31.989261
603.905508	46563.771454	31.994279
604.038985	46627.638412	31.999296
604.813348	46690.380338	32.004314
605.685815	46742.017259	32.009332
606.335258	46808.100326	32.014349
607.164953	46867.563428	32.019367
607.745704	46933.183152	32.024384
608.053670	46994.657802	32.029402
609.270842	47059.096428	32.034420
609.744734	47100.092528	32.039437
610.762932	47156.648406	32.044455
611.621941	47216.360886	32.049472
611.991618	47269.956674	32.054490
612.792914	47325.281675	32.059508
612.837678	47378.479433	32.064525
614.010832	47436.960265	32.069543
614.778295	47490.393052	32.074560
615.510440	47543.603746	32.079578
615.927176	47589.424083	32.084596
616.274488	47650.831084	32.089613
616.668484	47702.190848	32.094631
617.206717	47758.848702	32.099648
618.008407	47816.009515	32.104666
618.862327	47869.644755	32.109684
618.794059	47929.010864	32.114701
619.408999	48002.776884	32.119719
619.708462	48064.976985	32.124736
620.480116	48123.389605	32.129754
621.706109	48193.973177	32.134772
621.637203	48255.472297	32.139789
621.935557	48319.470023	32.144807
622.769377	48407.330437	32.149824
623.272718	48463.369167	32.154842
624.127961	48539.319947	32.159860
624.312066	48606.765435	32.164877
624.934251	48689.699940	32.169895
625.545373	48759.546428	32.174912
626.414182	48828.574579	32.179930
627.111499	48906.006466	32.184948
627.304155	48978.690293	32.189965
628.360805	49052.169082	32.194983
628.596224	49133.394252	32.200000
629.333448	49204.905291	32.205018
630.199066	49280.350753	32.210036
630.077531	49360.772171	32.215053
631.062652	49436.458834	32.220071
631.597046	49522.358450	32.225088
632.408656	49595.023215	32.230106
633.156461	49646.262334	32.235124
633.715408	49717.859833	32.240141
634.745491	49782.265857	32.245159
635.170307	49848.095533	32.250176
636.223802	49913.801631	32.255194
636.970950	49975.835568	32.260212
637.639570	50036.002822	32.265229
637.900228	50101.137639	32.270247
637.861521	50163.655800	32.275264
638.538465	50227.802019	32.280282
639.275833	50305.118454	32.285300
639.509138	50391.460746	32.290317
640.608621	50461.457371	32.295335
641.150754	50540.956425	32.300352
641.705536	50627.806049	32.305370
642.192402	50702.727049	32.310388
642.667993	50780.870654	32.315405
643.385185	50853.041654	32.320423
644.390737	50929.248857	32.325440
644.898272	51018.688903	32.330458
645.576238	51097.592802	32.335476
646.102138	51183.386029	32.340493
647.116951	51257.422557	32.345511
648.072761	51339.941025	32.350528
648.376686	51408.780631	32.355546
649.385792	51489.532246	32.360564
649.924270	51564.795957	32.365581
650.413161	51643.016309	32.370599
651.105149	51734.727118	32.375616
651.761299	51812.206830	32.380634
652.457593	51875.557300	32.385652
653.183713	51965.175562	32.390669
653.574516	52036.401586	32.395687
654.291007	52120.371365	32.400704
654.887094	52192.135206	32.405722
655.675421	52278.929109	32.410740
656.021253	52369.228592	32.415757
656.862097	52441.207976	32.420775
657.652807	52532.703970	32.425792
658.431363	52609.850769	32.430810
659.336230	52682.251159	32.435828
659.764361	52771.640755	32.440845
660.616312	52844.638423	32.445863
661.288758	52921.385226	32.450880
661.862752	53004.304752	32.455898
662.662138	53083.215332	32.460916
662.851355	53164.151760	32.465933
663.839874	53241.989143	32.470951
664.608377	53321.683702	32.475968
665.008062	53400.544041	32.480986
665.945488	53482.642648	32.486004
666.239152	53556.603229	32.491021
667.311209	53641.389714	32.496039
667.956595	53715.169150	32.501056
668.527690	53797.484427	32.506074
669.827848	53878.901126	32.511092
670.337653	53956.214668	32.516109
671.128013	54015.449211	32.521127
671.684151	54096.337704	32.526144
671.992333	54168.348844	32.531162
672.877401	54238.808035	32.536180
673.593089	54316.805605	32.541197
674.540503	54390.615792	32.546215
675.204674	54466.400697	32.551232
675.566125	54536.284633	32.556250
676.423756	54611.387889	32.561268
677.275061	54684.543240	32.566285
677.878015	54750.460077	32.571303
678.009179	54817.792602	32.576320
678.614834	54893.777890	32.581338
680.024050	54951.411698	32.586356
680.618568	55020.899842	32.591373
680.938834	55083.811565	32.596391
681.874730	55147.652258	32.601408
682.653672	55207.049783	32.606426
683.410606	55273.950191	32.611444
683.942850	55344.702080	32.616461
684.588267	55407.797895	32.621479
685.061422	55478.154407	32.626496
685.233882	55558.715601	32.631514
686.368937	55624.709749	32.636532
687.149372	55700.062695	32.641549
687.944924	55761.515806	32.646567
688.827841	55826.550074	32.651584
689.712291	55899.267295	32.656602
690.309043	55966.928862	32.661620
690.783364	56038.850033	32.666637
691.152064	56112.775185	32.671655
692.146741	56176.881567	32.676672
692.673242	56261.750198	32.681690
693.529729	56327.270956	32.686708
694.106315	56396.620355	32.691725
694.813252	56465.645758	32.696743
695.788051	56543.768270	32.701760
695.944052	56622.898976	32.706778
696.798370	56700.952263	32.711796
697.072179	56787.659734	32.716813
697.947490	56858.969955	32.721831
698.804291	56941.529836	32.726848
699.292494	57044.596657	32.731866
699.622637	57108.018476	32.736884
700.201537	57198.989700	32.741901
700.675319	57299.110543	32.746919
701.553940	57385.320392	32.751936
702.299600	57480.513370	32.756954
703.079907	57564.422807	32.761972
703.808887	57666.346984	32.766989
704.828228	57743.567681	32.772007
706.002987	57821.055428	32.777024
706.833539	57898.179600	32.782042
707.434814	57976.245003	32.787060
708.426999	58058.831816	32.792077
709.597414	58129.156526	32.797095
710.330983	58205.625965	32.802112
710.946329	58277.057045	32.807130
711.434497	58341.590302	32.812148
712.247502	58421.199984	32.817165
712.746279	58492.884141	32.822183
713.614130	58571.529994	32.827200
714.192356	58653.626677	32.832218
715.245028	58715.433166	32.837236
715.977827	58795.208542	32.842253
716.560444	58859.943588	32.847271
717.216581	58932.769019	32.852288
717.557562	59023.569157	32.857306
718.470050	59094.633306	32.862324
718.819158	59172.621787	32.867341
719.210121	59261.870578	32.872359
720.307536	59336.951063	32.877376
720.734144	59425.821427	32.882394
721.762908	59501.141035	32.887412
722.856715	59570.576782	32.892429
723.539969	59645.938285	32.897447
724.979541	59711.433876	32.902464
725.579903	59778.124453	32.907482
726.372734	59850.507130	32.912500
727.226841	59912.936420	32.917517
727.708951	59975.493751	32.922535
728.530851	60024.566280	32.927552
729.072046	60089.716181	32.932570
729.933073	60151.651274	32.937588
730.788470	60205.086476	32.942605
731.381282	60272.304956	32.947623
731.820401	60331.907573	32.952640
732.268212	60398.623729	32.957658
732.766550	60473.016620	32.962676
733.561697	60536.532811	32.967693
733.994008	60615.778840	32.972711
734.852246	60699.667893	32.977728
735.746829	60782.215921	32.982746
736.252686	60854.051486	32.987764
736.560575	60927.310860	32.992781
737.352871	61022.345796	32.997799
737.837715	61089.374527	33.002816
738.451423	61186.185150	33.007834
739.361304	61267.827212	33.012852
740.220053	61363.207539	33.017869
740.710334	61465.792650	33.022887
741.386236	61551.264037	33.027904
741.728122	61645.080553	33.032922
742.473685	61745.955683	33.037940
743.004124	61846.883903	33.042957
743.980309	61951.110425	33.047975
744.892094	62052.207652	33.052992
745.305356	62153.706204	33.058010
746.619697	62251.671007	33.063028
747.237358	62341.927310	33.068045
747.821538	62446.717399	33.073063
748.927352	62545.311072	33.078080
749.692693	62653.536393	33.083098
750.097018	62740.700318	33.088116
751.138306	62834.278861	33.093133
751.428773	62946.302138	33.098151
752.509581	63044.667475	33.103168
753.078232	63151.324134	33.108186
754.034785	63256.242899	33.113204
754.583696	63359.839537	33.118221
755.281541	63468.579080	33.123239
756.299702	63556.466379	33.128256
757.042031	63666.510263	33.133274
757.752945	63763.746185	33.138292
758.773028	63867.157184	33.143309
759.563513	63980.626165	33.148327
760.463243	64077.624821	33.153344
761.040524	64172.661146	33.158362
761.858213	64273.433909	33.163380
762.381783	64371.885390	33.168397
763.438212	64482.174881	33.173415
764.369130	64578.727423	33.178432
764.903746	64671.436204	33.183450
765.679192	64769.906776	33.188468
767.361570	64864.943597	33.193485
767.893704	64965.213048	33.198503
768.917556	65056.903312	33.203520
769.553390	65144.925677	33.208538
770.338266	65232.741407	33.213556
771.125477	65318.904659	33.218573
771.555097	65412.746876	33.223591
772.284957	65506.162554	33.228608
773.068991	65606.863606	33.233626
774.146180	65680.484944	33.238644
775.239262	65769.184956	33.243661
776.240851	65859.488747	33.248679
776.662430	65947.085268	33.253696
777.354833	66033.784959	33.258714
777.998787	66110.356120	33.263732
778.809975	66186.027601	33.268749
779.059865	66278.293004	33.273767
779.869351	66365.975844	33.278784
780.646532	66461.533957	33.283802
781.542708	66553.382582	33.288820
782.096053	66639.257700	33.293837
783.000579	66738.063925	33.298855
783.475275	66825.636153	33.303872
784.470871	66925.866089	33.308890
785.420766	67020.360881	33.313908
786.273352	67107.444355	33.318925
787.257712	67201.377242	33.323943
787.988472	67284.523165	33.328960
788.754735	67374.476612	33.333978
789.275826	67468.590661	33.338996
790.446079	67556.594657	33.344013
791.065840	67654.562579	33.349031
792.100959	67747.191523	33.354048
792.567730	67847.653503	33.359066
793.207650	67945.727017	33.364084
794.058721	68038.924031	33.369101
794.685785	68142.515284	33.374119
795.446022	68231.681199	33.379136
796.283672	68339.704204	33.384154
797.163564	68441.059913	33.389172
797.724630	68543.833637	33.394189
798.397940	68650.395679	33.399207
798.903562	68755.300119	33.404224
799.748972	68867.610846	33.409242
800.611049	68983.997263	33.414260
801.166355	69091.434419	33.419277
801.882872	69204.039064	33.424295
803.222583	69305.813724	33.429312
804.345271	69426.359488	33.434330
804.741286	69543.296301	33.439348
805.531021	69647.925570	33.444365
806.152794	69762.611757	33.449383
807.287828	69877.420708	33.454400
808.082624	69988.718386	33.459418
809.064287	70093.009106	33.464436
809.845109	70206.044942	33.469453
810.488223	70317.633730	33.474471
811.639335	70421.835906	33.479488
812.415471	70525.349995	33.484506
812.967597	70631.483192	33.489524
814.299735	70733.517909	33.494541
815.074211	70855.422949	33.499559
815.882357	70957.287291	33.504576
816.809345	71063.958791	33.509594
817.645739	71172.544672	33.514612
818.532226	71275.107223	33.519629
819.397685	71380.611787	33.524647
820.021186	71482.481747	33.529664
820.256673	71605.829843	33.534682
821.437423	71704.193774	33.539700
822.686560	71811.121826	33.544717
823.204765	71926.688603	33.549735
823.901497	72027.877933	33.554752
824.496310	72139.431351	33.559770
825.414319	72251.681900	33.564788
826.049508	72368.055549	33.569805
827.065259	72481.330349	33.574823
827.722854	72602.349831	33.579840
828.736489	72716.005937	33.584858
829.064114	72831.821821	33.589876
829.776928	72951.200347	33.594893
830.521787	73060.669595	33.599911
831.602610	73170.264009	33.604928
832.437347	73280.581377	33.609946
833.231810	73394.920672	33.614964
834.014249	73499.775366	33.619981
834.793494	73626.505567	33.624999
835.624127	73722.702545	33.630016
836.789823	73842.774122	33.635034
837.431551	73951.313195	33.640052
838.347249	74050.689964	33.645069
838.749344	74170.249257	33.650087
840.066301	74281.521231	33.655104
840.855012	74391.951721	33.660122
841.909953	74501.403644	33.665140
842.853705	74619.106786	33.670157
843.877370	74730.933216	33.675175
844.574886	74841.037827	33.680192
845.646800	74944.966165	33.685210
846.216671	75070.861956	33.690228
847.132360	75187.545954	33.695245
847.842853	75304.832604	33.700263
848.793736	75423.386831	33.705280
849.479562	75535.839517	33.710298
850.141226	75656.200785	33.715316
850.582180	75771.200896	33.720333
851.810248	75909.918125	33.725351
852.784574	76022.048972	33.730368
853.591778	76151.510154	33.735386
853.952160	76277.596361	33.740404
855.132647	76405.733553	33.745421
855.805090	76532.962827	33.750439
856.694111	76665.669217	33.755456
857.830116	76786.480586	33.760474
858.816121	76917.032166	33.765492
860.195344	77037.375856	33.770509
860.923033	77144.888177	33.775527
861.892686	77260.445180	33.780544
862.971084	77382.142290	33.785562
863.659103	77498.491808	33.790580
864.743598	77610.168546	33.795597
865.639391	77733.289298	33.800615
866.649001	77843.382523	33.805632
867.572736	77954.503096	33.810650
868.522818	78083.900377	33.815668
869.472016	78184.971915	33.820685
870.068862	78306.102432	33.825703
870.694236	78418.779139	33.830720
871.702116	78533.676745	33.835738
872.304952	78655.745329	33.840756
873.516262	78766.773470	33.845773
873.605959	78892.863394	33.850791
874.578321	79016.041224	33.855808
875.493835	79135.516542	33.860826
876.341037	79277.655001	33.865844
877.644969	79394.017415	33.870861
878.331347	79508.602007	33.875879
879.332784	79633.893744	33.880896
879.972954	79767.363499	33.885914
880.645884	79892.948551	33.890932
881.483094	80022.005146	33.895949
882.791614	80157.652573	33.900967
883.406444	80282.906406	33.905984
884.757710	80394.590605	33.911002
884.828945	80525.365803	33.916020
886.178649	80650.518881	33.921037
886.750111	80782.534577	33.926055
887.953349	80907.318979	33.931072
888.428797	81029.658622	33.936090
888.932814	81158.088458	33.941108
889.849105	81286.048893	33.946125
890.693652	81410.841013	33.951143
891.402594	81538.036859	33.956160
892.278598	81672.188261	33.961178
893.071176	81807.607693	33.966196
894.157336	81938.673981	33.971213
895.182912	82082.103740	33.976231
895.727727	82211.989043	33.981248
896.487356	82338.927148	33.986266
897.531629	82484.129847	33.991284
898.557950	82620.517518	33.996301
899.693080	82756.939487	34.001319
900.501539	82889.054611	34.006336
901.630356	83023.502249	34.011354
902.232836	83157.247357	34.016372
902.842514	83293.374050	34.021389
904.794708	83439.275720	34.026407
905.195185	83560.675037	34.031424
906.336571	83708.757706	34.036442
906.908241	83846.945661	34.041460
907.776443	83986.532342	34.046477
909.159392	84125.544932	34.051495
909.510870	84261.944731	34.056512
910.969971	84388.909129	34.061530
911.644822	84546.167055	34.066548
912.124679	84679.609004	34.071565
913.371612	84834.776863	34.076583
914.457908	84982.165116	34.081600
915.382918	85113.600640	34.086618
915.900338	85263.563008	34.091636
916.783208	85404.446748	34.096653
918.199277	85545.323715	34.101671
918.786269	85698.546725	34.106688
920.493413	85831.586392	34.111706
921.219844	85968.353687	34.116724
922.274589	86108.390257	34.121741
923.245800	86250.746877	34.126759
923.911649	86390.402173	34.131776
924.920451	86531.588449	34.136794
925.839138	86674.487585	34.141812
926.750118	86817.756119	34.146829
927.803961	86952.778678	34.151847
928.707877	87094.706410	34.156864
930.203282	87225.086372	34.161882
931.069892	87369.809200	34.166900
931.930698	87496.893514	34.171917
933.060839	87635.544272	34.176935
933.707431	87768.188536	34.181952
934.962955	87895.288799	34.186970
936.009140	88044.004057	34.191988
937.459115	88168.565848	34.197005
938.546476	88294.325496	34.202023
939.161409	88423.213818	34.207040
940.457184	88535.711350	34.212058
941.513233	88666.052414	34.217076
942.201136	88786.262552	34.222093
943.184775	88913.447774	34.227111
944.216753	89033.452959	34.232128
944.867825	89148.182846	34.237146
946.166995	89281.935654	34.242164
946.881332	89394.489454	34.247181
947.742454	89525.827972	34.252199
948.514508	89656.331893	34.257216
949.414644	89782.367937	34.262234
949.793392	89912.592373	34.267252
950.591625	90043.245962	34.272269
951.580256	90170.435751	34.277287
952.335362	90307.763580	34.282304
953.350133	90429.158490	34.287322
953.876186	90565.103897	34.292340
954.898906	90704.178640	34.297357
955.726757	90833.297483	34.302375
956.295797	90982.241485	34.307392
957.507837	91115.306359	34.312410
958.466088	91256.003339	34.317428
959.220489	91409.432399	34.322445
960.020202	91551.410315	34.327463
960.710140	91713.304711	34.332480
961.291436	91859.285316	34.337498
962.273244	92019.171116	34.342516
963.473875	92176.425223	34.347533
964.644502	92323.570552	34.352551
965.338565	92491.019883	34.357568
966.231982	92646.588090	34.362586
967.180452	92808.663286	34.367604
967.883125	92968.813228	34.372621
969.114193	93141.860348	34.377639
969.714531	93303.599743	34.382656
970.849590	93471.619122	34.387674
971.788797	93646.248453	34.392692
973.173418	93808.285976	34.397709
974.839519	93966.338284	34.402727
975.705168	94128.915054	34.407744
977.264818	94275.298997	34.412762
978.308690	94427.417619	34.417780
979.277198	94576.227815	34.422797
980.212099	94734.170367	34.427815
980.764221	94891.730007	34.432832
982.173696	95046.798534	34.437850
983.192124	95196.072875	34.442868
984.516290	95356.556156	34.447885
985.308819	95507.540558	34.452903
986.070212	95662.713613	34.457920
987.394064	95811.816313	34.462938
988.517368	95963.980694	34.467956
989.296218	96116.972985	34.472973
990.555422	96268.902070	34.477991
991.015258	96437.245987	34.483008
992.397051	96582.857311	34.488026
993.429492	96738.652402	34.493044
993.997969	96895.864602	34.498061
995.109162	97046.514935	34.503079
996.003030	97210.954045	34.508096
996.794782	97365.319426	34.513114
997.867789	97533.421047	34.518132
998.782911	97695.831073	34.523149
1000.401449	97849.638346	34.528167
1001.312637	98009.185632	34.533184
1002.341835	98157.800418	34.538202
1003.247592	98320.481306	34.543220
1004.129094	98483.914762	34.548237
1005.530060	98637.430291	34.553255
1006.191977	98795.055572	34.558272
1007.716321	98939.412998	34.563290
1008.869337	99098.686978	34.568308
1009.419043	99256.103896	34.573325
1010.737557	99408.051346	34.578343
1011.550995	99576.419842	34.583360
1012.647871	99721.925286	34.588378
1013.352945	99875.923320	34.593396
1014.168417	100040.680801	34.598413
1015.397301	100203.675577	34.603431
1016.023588	100364.204607	34.608448
1017.288930	100528.767349	34.613466
1018.144390	100688.045023	34.618484
1019.216063	100845.730232	34.623501
1020.293041	100995.402863	34.628519
1020.774909	101147.400696	34.633536
1021.826824	101295.138876	34.638554
1022.901306	101458.011955	34.643572
1023.944095	101619.293343	34.648589
1025.185494	101773.317783	34.653607
1025.873950	101934.402627	34.658624
1026.566165	102099.595485	34.663642
1027.555635	102262.105499	34.668660
1028.803861	102435.238479	34.673677
1030.037812	102595.188818	34.678695
1030.815900	102769.018404	34.683712
1031.881212	102928.819254	34.688730
1032.794266	103099.599216	34.693748
1033.715261	103271.722773	34.698765
1034.897474	103440.522472	34.703783
1036.021914	103603.499721	34.708800
1037.404299	103771.432938	34.713818
1038.579227	103943.659672	34.718836
1039.467420	104107.411755	34.723853
1041.171057	104274.688598	34.728871
1042.030622	104439.765428	34.733888
1042.969379	104598.414896	34.738906
1043.736080	104781.360532	34.743924
1044.666593	104953.503912	34.748941
1045.687972	105113.956040	34.753959
1046.577766	105290.938437	34.758976
1047.784799	105477.419920	34.763994
1048.870771	105653.359115	34.769012
1049.775752	105824.965688	34.774029
1050.965890	105995.349248	34.779047
1052.127489	106181.930467	34.784064
1053.172345	106360.948311	34.789082
1054.120875	106537.192547	34.794100
1055.733737	106695.594109	34.799117
1057.298970	106864.046609	34.804135
1058.525194	107039.844185	34.809152
1059.487396	107198.273856	34.814170
1060.359114	107368.929668	34.819188
1061.648631	107538.722042	34.824205
1062.699188	107700.855571	34.829223
1063.590783	107870.534348	34.834240
1064.436162	108041.818956	34.839258
1065.476364	108210.487037	34.844276
1066.454632	108388.092915	34.849293
1067.700879	108554.536630	34.854311
1068.456601	108738.139138	34.859328
1069.579067	108913.670809	34.864346
1070.568711	109088.374525	34.869364
1071.010334	109271.217421	34.874381
1072.489061	109452.364476	34.879399
1073.708573	109634.478781	34.884416
1074.244909	109831.119644	34.889434
1075.060069	110013.438708	34.894452
1076.250801	110203.638503	34.899469
1077.568098	110381.822790	34.904487
1078.558015	110577.166685	34.909504
1079.714488	110767.045149	34.914522
1080.605674	110949.344448	34.919540
1081.499115	111143.501797	34.924557
1082.707069	111331.206627	34.929575
1083.886265	111534.249392	34.934592
1084.711137	111723.931231	34.939610
1085.748820	111915.102603	34.944628
1086.295365	112113.365104	34.949645
1088.150793	112310.764305	34.954663
1088.646440	112510.089582	34.959680
1090.076194	112699.922832	34.964698
1091.239417	112884.205868	34.969716
1092.645973	113076.555843	34.974733
1093.073406	113253.029407	34.979751
1094.417051	113437.325056	34.984768
1095.625977	113630.584006	34.989786
1097.229072	113810.985399	34.994804
1097.906210	113998.305260	34.999821
1099.092125	114176.490869	35.004839
1100.029158	114371.927028	35.009856
1100.983724	114559.865838	35.014874
1102.209112	114746.558321	35.019892
1103.209767	114949.559371	35.024909
1104.532919	115137.532207	35.029927
1105.425974	115333.145234	35.034944
1106.605835	115524.402066	35.039962
1107.912516	115727.283375	35.044980
1108.652286	115915.592476	35.049997
1110.037478	116110.041774	35.055015
1110.880281	116306.314652	35.060032
1112.198677	116507.790502	35.065050
1113.492388	116704.400754	35.070068
1114.584443	116910.759388	35.075085
1115.757914	117093.818857	35.080103
1116.816056	117308.175806	35.085120
1118.041903	117509.671522	35.090138
1119.316239	117703.347344	35.095156
1120.212804	117914.054653	35.100173
1121.889719	118114.341401	35.105191
1122.660544	118305.257868	35.110208
1123.977819	118491.929287	35.115226
1125.371026	118696.855242	35.120244
1126.111723	118899.398298	35.125261
1127.062180	119103.596628	35.130279
1128.496032	119311.259366	35.135296
1129.582282	119512.191357	35.140314
1130.621830	119710.505971	35.145332
1131.700710	119915.868188	35.150349
1132.812993	120114.731623	35.155367
1134.269272	120313.377321	35.160384
1135.210870	120520.743086	35.165402
1136.675403	120726.607364	35.170420
1137.561904	120939.108746	35.175437
1138.677466	121144.839589	35.180455
1139.859676	121346.489115	35.185472
1140.978901	121550.952995	35.190490
1142.245304	121753.936080	35.195508
1142.856910	121957.695052	35.200525
1143.920760	122173.892197	35.205543
1145.687708	122377.168010	35.210560
1147.162129	122583.243452	35.215578
1148.363211	122777.412814	35.220596
1149.782186	122980.289514	35.225613
1150.958722	123171.902120	35.230631
1152.510215	123369.064114	35.235648
1153.670688	123566.567388	35.240666
1154.932858	123750.633903	35.245684
1156.022219	123952.564948	35.250701
1157.080355	124141.156071	35.255719
1158.330738	124327.738933	35.260736
1159.253181	124525.436419	35.265754
1160.551625	124714.132149	35.270772
1161.545247	124905.604052	35.275789
1162.679799	125101.659974	35.280807
1163.774750	125301.123026	35.285824
1164.489909	125500.811438	35.290842
1166.161695	125692.802519	35.295860
1167.162628	125890.392863	35.300877
1168.714431	126063.958027	35.305895
1169.795358	126240.718595	35.310912
1170.845411	126421.950528	35.315930
1172.260065	126606.259848	35.320948
1172.892792	126790.831958	35.325965
1174.705634	126955.441079	35.330983
1176.114891	127125.620225	35.336000
1176.933721	127317.080000	35.341018
1178.124527	127495.592244	35.346036
1179.201237	127682.623564	35.351053
1180.027438	127862.387058	35.356071
1180.991334	128049.780241	35.361088
1181.411387	128256.569638	35.366106
1183.232836	128443.766896	35.371124
1183.740493	128649.821327	35.376141
1184.862951	128856.998528	35.381159
1186.093895	129067.344364	35.386176
1186.800755	129281.237037	35.391194
1187.860077	129491.091645	35.396212
1189.075925	129719.180601	35.401229
1190.268499	129935.677663	35.406247
1191.646963	130159.937143	35.411264
1192.515717	130387.398851	35.416282
1193.688153	130604.156206	35.421300
1194.799880	130830.770184	35.426317
1195.233370	131075.813361	35.431335
1196.700027	131308.578838	35.436352
1197.534754	131549.438177	35.441370
1199.295640	131785.712902	35.446388
1200.332787	132043.520449	35.451405
1201.272324	132278.137336	35.456423
1202.535018	132518.275218	35.461440
1203.969853	132773.880419	35.466458
1205.662356	133011.771246	35.471476
1206.892221	133251.283824	35.476493
1208.155973	133490.678192	35.481511
1209.525774	133735.132857	35.486528
1210.645728	133967.903260	35.491546
1212.088336	134216.282784	35.496564
1213.250714	134449.975366	35.501581
1214.385987	134691.363118	35.506599
1215.381806	134936.365085	35.511616
1216.746484	135179.546808	35.516634
1218.197444	135422.094547	35.521652
1219.518924	135671.148221	35.526669
1220.367749	135906.014102	35.531687
1221.960641	136148.264325	35.536704
1223.215677	136404.019875	35.541722
1224.508104	136638.007927	35.546740
1226.189681	136874.017395	35.551757
1227.040743	137117.404054	35.556775
1228.504455	137355.734285	35.561792
1229.866078	137602.216075	35.566810
1231.452364	137827.687164	35.571828
1232.732878	138070.973525	35.576845
1233.691018	138302.357363	35.581863
1235.228986	138526.291173	35.586880
1236.027120	138766.610975	35.591898
1237.542437	138994.954136	35.596916
1239.113887	139234.723789	35.601933
1240.088299	139460.780743	35.606951
1241.668049	139697.784888	35.611968
1242.698800	139926.246461	35.616986
1244.099392	140157.493967	35.622004
1245.076583	140381.930432	35.627021
1246.173095	140615.512101	35.632039
1247.573666	140851.166696	35.637056
1248.041787	141085.001300	35.642074
1249.436994	141309.008603	35.647092
1250.873257	141527.629467	35.652109
1252.160824	141755.805685	35.657127
1253.417662	141982.972479	35.662144
1254.710017	142204.626734	35.667162
1256.040656	142424.714958	35.672180
1257.169148	142651.790718	35.677197
1258.136608	142879.463848	35.682215
1259.833011	143103.698730	35.687232
1260.667040	143330.646019	35.692250
1261.880952	143567.942046	35.697268
1263.218157	143808.621284	35.702285
1264.422187	144034.257372	35.707303
1265.504905	144273.265288	35.712320
1266.722720	144522.647866	35.717338
1268.180074	144756.687659	35.722356
1269.317490	145001.414539	35.727373
1271.122810	145246.786879	35.732391
1272.258562	145476.349256	35.737408
1273.060237	145726.754800	35.742426
1274.455239	145980.444833	35.747444
1275.462951	146226.073648	35.752461
1276.504416	146471.876043	35.757479
1277.715491	146738.341761	35.762496
1279.128785	146999.915955	35.767514
1280.290137	147240.448516	35.772532
1281.497660	147511.919626	35.777549
1282.348206	147777.165128	35.782567
1283.877030	148033.598546	35.787584
1285.116144	148314.778825	35.792602
1287.168539	148563.707545	35.797620
1288.367341	148815.652353	35.802637
1289.707727	149081.843145	35.807655
1291.062955	149329.145627	35.812672
1292.619258	149611.374696	35.817690
1294.365454	149865.561597	35.822708
1295.541836	150118.049140	35.827725
1296.525581	150386.434674	35.832743
1297.888526	150640.393252	35.837760
1299.231320	150898.468842	35.842778
1300.407406	151157.650692	35.847796
1301.686451	151425.588902	35.852813
1302.978742	151683.434902	35.857831
1304.152283	151946.467022	35.862848
1305.434165	152230.770850	35.867866
1306.933154	152492.967592	35.872884
1308.100004	152759.520776	35.877901
1309.368494	153032.736324	35.882919
1310.677425	153287.591345	35.887936
1312.015101	153567.742261	35.892954
1313.001662	153846.210425	35.897972
1314.368783	154117.080033	35.902989
1315.424691	154403.016921	35.908007
1316.868294	154677.444282	35.913024
1318.101485	154954.571698	35.918042
1319.562717	155234.305182	35.923060
1321.258296	155510.512344	35.928077
1322.492732	155790.817166	35.933095
1324.159359	156065.063820	35.938112
1325.254141	156335.453224	35.943130
1326.308338	156610.293369	35.948148
1328.064719	156886.167399	35.953165
1329.225943	157160.383980	35.958183
1330.513087	157425.060935	35.963200
1331.949364	157700.595284	35.968218
1333.104783	157980.440376	35.973236
1334.798124	158253.626513	35.978253
1336.003846	158515.248777	35.983271
1337.395609	158774.278615	35.988288
1339.012260	159029.338824	35.993306
1340.638573	159277.606603	35.998324
1342.129392	159528.727647	36.003341
1343.346008	159796.256978	36.008359
1344.566885	160034.155643	36.013376
1345.465933	160300.061045	36.018394
1346.698844	160554.019593	36.023412
1348.257014	160807.217297	36.028429
1349.294927	161074.386482	36.033447
1350.816922	161330.994373	36.038464
1352.302542	161603.465976	36.043482
1353.371252	161870.316278	36.048500
1354.743271	162144.966247	36.053517
1355.707218	162405.791937	36.058535
1357.519628	162677.556740	36.063552
1359.241710	162940.297256	36.068570
1360.192501	163218.001253	36.073588
1361.793372	163485.638215	36.078605
1363.134391	163755.157880	36.083623
1364.678176	164024.481852	36.088640
1365.808070	164295.027059	36.093658
1366.901094	164567.750201	36.098676
1368.936827	164848.439870	36.103693
1370.186931	165136.909626	36.108711
1371.529878	165416.072252	36.113728
1372.736676	165699.345615	36.118746
1373.605611	165973.175990	36.123764
1375.193582	166261.254798	36.128781
1376.521466	166552.943286	36.133799
1377.486174	166841.820382	36.138816
1379.041786	167125.692521	36.143834
1380.485557	167424.133899	36.148852
1381.908944	167708.600445	36.153869
1383.411322	168012.342435	36.158887
1384.776125	168296.731625	36.163904
1386.181588	168587.794231	36.168922
1387.897619	168882.174133	36.173940
1389.309327	169164.248536	36.178957
1390.939305	169454.416078	36.183975
1392.283830	169729.887941	36.188992
1393.730280	170018.016789	36.194010
1394.957972	170316.313491	36.199028
1396.299975	170607.673412	36.204045
1397.837383	170911.041071	36.209063
1399.295306	171189.687659	36.214080
1400.488645	171478.712496	36.219098
1401.991951	171771.435707	36.224116
1403.616115	172059.239833	36.229133
1405.061629	172358.056508	36.234151
1406.771637	172638.116467	36.239168
1408.072005	172926.241163	36.244186
1409.536646	173216.207793	36.249204
1410.925557	173506.707963	36.254221
1412.315582	173797.158236	36.259239
1413.892765	174085.091475	36.264256
1414.784732	174373.679021	36.269274
1416.288400	174675.847678	36.274292
1418.017479	174958.096938	36.279309
1419.162405	175258.812849	36.284327
1420.703132	175543.442781	36.289344
1422.112350	175837.503686	36.294362
1423.172688	176137.512254	36.299380
1424.454876	176424.725349	36.304397
1425.756027	176737.866564	36.309415
1427.204621	177033.487427	36.314432
1428.884916	177336.311187	36.319450
1429.905003	177643.150505	36.324468
1431.452937	177932.968416	36.329485
1432.196217	178231.421313	36.334503
1433.670061	178524.097289	36.339520
1435.535889	178819.608193	36.344538
1436.669729	179113.406046	36.349556
1438.060491	179408.840899	36.354573
1438.901901	179709.950198	36.359591
1440.306025	180011.480387	36.364608
1441.926515	180320.724050	36.369626
1443.047317	180637.234584	36.374644
1444.734735	180949.847827	36.379661
1446.051528	181263.510667	36.384679
1446.917532	181585.397933	36.389696
1448.277125	181904.085067	36.394714
1449.561666	182243.052898	36.399732
1451.501455	182569.575744	36.404749
1452.751431	182906.976645	36.409767
1454.440103	183230.213839	36.414784
1455.860670	183557.786449	36.419802
1457.023982	183901.198457	36.424820
1458.845728	184227.135782	36.429837
1460.053397	184569.882793	36.434855
1461.898248	184913.090023	36.439872
1463.373156	185251.606685	36.444890
1464.557848	185600.253377	36.449908
1466.044919	185947.279165	36.454925
1467.090842	186293.079793	36.459943
1468.870765	186644.633951	36.464960
1470.727856	186979.946896	36.469978
1471.871210	187342.347002	36.474996
1473.827185	187686.180952	36.480013
1474.935449	188038.556001	36.485031
1476.715716	188456.892070	36.490048
1478.230707	188806.107124	36.495066
1479.253475	189165.585724	36.500084
1481.095857	189517.164746	36.505101
1482.271009	189877.815553	36.510119
1483.837482	190232.030768	36.515136
1486.207697	190582.971618	36.520154
1487.530118	190930.470650	36.525172
1489.206053	191278.575780	36.530189
1490.685742	191629.151089	36.535207
1491.980490	191982.880635	36.540224
1493.877595	192324.095972	36.545242
1495.521298	192681.557612	36.550260
1497.376614	193010.207978	36.555277
1498.792297	193378.045432	36.560295
1499.973567	193720.240220	36.565312
1501.456660	194071.964875	36.570330
1502.579344	194425.651968	36.575348
1504.263911	194779.658482	36.580365
1505.470893	195128.762031	36.585383
1506.895712	195478.467418	36.590400
1508.953459	195829.700325	36.595418
1510.389394	196195.637284	36.600436
1511.970554	196543.441177	36.605453
1513.377255	196913.956845	36.610471
1514.690733	197263.379282	36.615488
1516.445114	197617.813891	36.620506
1517.558906	197986.472998	36.625524
1519.344530	198336.738539	36.630541
1520.597847	198690.060223	36.635559
1521.982150	199065.817547	36.640576
1523.683939	199421.153668	36.645594
1525.176165	199791.713827	36.650612
1526.694391	200156.047250	36.655629
1528.060798	200521.954785	36.660647
1529.831725	200880.687190	36.665664
1531.350048	201227.647831	36.670682
1532.747290	201586.338613	36.675700
1534.344629	201915.151007	36.680717
1536.121567	202255.087582	36.685735
1537.530287	202607.732880	36.690752
1539.377992	202946.465776	36.695770
1540.983396	203293.366050	36.700788
1542.058852	203644.947791	36.705805
1543.711264	203995.423779	36.710823
1544.661580	204339.659609	36.715840
1546.525883	204698.867648	36.720858
1547.746618	205064.680184	36.725876
1549.454357	205424.168055	36.730893
1550.958592	205783.688405	36.735911
1552.166055	206146.761425	36.740928
1553.658936	206513.931080	36.745946
1555.041489	206891.152821	36.750964
1556.286936	207275.433314	36.755981
1557.977833	207648.060916	36.760999
1559.478367	208030.676950	36.766016
1561.477872	208416.771958	36.771034
1562.892773	208804.102221	36.776052
1564.348583	209182.154488	36.781069
1566.092460	209575.455032	36.786087
1567.551245	209950.205529	36.791104
1569.289492	210341.882284	36.796122
1570.851219	210740.014293	36.801140
1572.418880	211123.284909	36.806157
1574.155004	211522.762504	36.811175
1576.197988	211910.303756	36.816192
1577.889268	212290.330281	36.821210
1579.034855	212680.426281	36.826228
1580.579164	213069.545817	36.831245
1582.286663	213460.824979	36.836263
1584.159454	213847.048785	36.841280
1585.951125	214233.234895	36.846298
1587.410369	214624.681201	36.851316
1588.990117	215017.760291	36.856333
1591.063357	215404.284569	36.861351
1592.923949	215796.101076	36.866368
1594.419916	216176.822722	36.871386
1596.297333	216561.829051	36.876404
1598.355550	216936.696658	36.881421
1600.009471	217329.715397	36.886439
1601.301570	217702.544145	36.891456
1602.695637	218082.140040	36.896474
1604.369578	218470.177304	36.901492
1605.929510	218850.535262	36.906509
1607.419659	219242.691812	36.911527
1608.824725	219622.413949	36.916544
1610.872424	219994.871783	36.921562
1612.230465	220386.668568	36.926580
1614.162977	220768.950736	36.931597
1615.808151	221157.756063	36.936615
1617.407469	221537.270837	36.941632
1618.764854	221921.421740	36.946650
1620.727514	222300.981518	36.951668
1622.565302	222675.581745	36.956685
1624.690379	223059.841456	36.961703
1626.115035	223432.194735	36.966720
1628.079176	223802.913997	36.971738
1629.539625	224182.324121	36.976756
1630.849709	224553.755527	36.981773
1632.745864	224936.196824	36.986791
1634.085033	225319.030149	36.991808
1635.704834	225684.265329	36.996826
1636.872763	226073.247820	37.001844
1638.305753	226444.685386	37.006861
1639.703522	226819.659591	37.011879
1641.025296	227212.352276	37.016896
1642.922735	227566.111973	37.021914
1644.493707	227931.583156	37.026932
1646.112160	228304.032938	37.031949
1647.815871	228674.411545	37.036967
1649.494475	229057.470584	37.041984
1651.164661	229431.486968	37.047002
1652.579546	229808.718666	37.052020
1653.840173	230191.766461	37.057037
1655.630543	230585.045199	37.062055
1657.110097	230973.367792	37.067072
1658.687134	231359.363157	37.072090
1660.159348	231756.374617	37.077108
1661.702815	232156.448552	37.082125
1663.289346	232567.159720	37.087143
1665.011105	232970.456888	37.092160
1666.527521	233382.397800	37.097178
1667.926927	233803.806922	37.102196
1669.280474	234224.968812	37.107213
1671.623197	234640.234248	37.112231
1672.912367	235062.802629	37.117248
1674.381522	235488.213040	37.122266
1676.334127	235918.526472	37.127284
1677.400609	236348.597038	37.132301
1679.658225	236775.787907	37.137319
1681.286424	237218.827020	37.142336
1682.851180	237645.820406	37.147354
1684.526711	238091.010267	37.152372
1686.474949	238520.355827	37.157389
1688.217204	238960.021442	37.162407
1689.940750	239403.449050	37.167424
1691.673843	239842.505093	37.172442
1693.511936	240282.814186	37.177460
1695.243873	240731.598491	37.182477
1696.627244	241163.111532	37.187495
1698.299754	241624.554441	37.192512
1700.115663	242073.094629	37.197530
1701.670821	242523.529226	37.202548
1703.404702	242980.692225	37.207565
1705.078337	243432.249668	37.212583
1706.564780	243887.595143	37.217600
1708.510587	244334.408602	37.222618
1710.582884	244794.817289	37.227636
1711.958516	245254.597302	37.232653
1714.125660	245712.448818	37.237671
1715.387268	246167.926122	37.242688
1717.488827	246630.891719	37.247706
1719.129864	247090.041664	37.252724
1721.123068	247554.241282	37.257741
1722.870014	247993.888662	37.262759
1724.516304	248453.872651	37.267776
1726.431205	248911.501789	37.272794
1728.395486	249374.964512	37.277812
1729.800413	249829.165486	37.282829
1731.790962	250286.398039	37.287847
1733.712354	250746.332752	37.292864
1735.325699	251191.200164	37.297882
1737.468785	251641.165414	37.302900
1738.973034	252101.669486	37.307917
1740.887581	252548.238590	37.312935
1742.657582	253005.269078	37.317952
1744.129700	253453.657410	37.322970
1746.014379	253901.751180	37.327988
1747.822853	254349.347437	37.333005
1749.648478	254792.494343	37.338023
1751.107194	255255.713463	37.343040
1753.474125	255696.512027	37.348058
1755.176058	256124.890452	37.353076
1756.684394	256552.484952	37.358093
1758.718714	256980.706968	37.363111
1760.195932	257407.084273	37.368128
1761.997999	257831.504253	37.373146
1764.127164	258264.609451	37.378164
1765.559552	258686.112486	37.383181
1767.210102	259125.461897	37.388199
1768.714588	259555.790011	37.393216
1770.674817	259985.130840	37.398234
1772.677234	260428.230433	37.403252
1773.969839	260864.124167	37.408269
1775.918325	261302.809215	37.413287
1777.537134	261750.967534	37.418304
1779.091884	262200.226277	37.423322
1780.847102	262649.604222	37.428340
1782.420431	263099.796169	37.433357
1784.162302	263550.010664	37.438375
1785.466076	264015.175873	37.443392
1787.186847	264475.244713	37.448410
1789.321796	264947.971703	37.453428
1790.419663	265415.778993	37.458445
1793.258804	265891.236125	37.463463
1794.647367	266376.264768	37.468480
1796.819900	266843.592458	37.473498
1798.623939	267319.738099	37.478516
1799.738701	267799.697441	37.483533
1801.600497	268265.416011	37.488551
1803.403777	268763.067000	37.493568
1805.052156	269250.300984	37.498586
1806.938051	269733.202992	37.503604
1808.675762	270241.955211	37.508621
1810.101686	270735.514774	37.513639
1811.871073	271237.170482	37.518656
1813.737016	271746.300471	37.523674
1815.616029	272260.022360	37.528692
1817.083706	272773.069063	37.533709
1819.416557	273282.116989	37.538727
1821.054048	273788.426238	37.543744
1822.932081	274299.520158	37.548762
1824.816736	274812.108294	37.553780
1826.654589	275326.275135	37.558797
1828.812709	275837.518856	37.563815
1831.264848	276340.002511	37.568832
1833.256965	276852.687920	37.573850
1835.567578	277353.054070	37.578868
1837.025958	277870.362193	37.583885
1838.824583	278372.909739	37.588903
1840.250942	278889.479582	37.593920
1842.305530	279399.776638	37.598938
1844.226831	279901.329889	37.603956
1845.829102	280423.677107	37.608973
1847.563791	280937.137255	37.613991
1849.407732	281454.335064	37.619008
1851.307459	281962.023072	37.624026
1853.627755	282475.075987	37.629044
1855.225629	283000.782753	37.634061
1857.476933	283512.289953	37.639079
1859.599538	284022.289955	37.644096
1861.624048	284527.070569	37.649114
1863.681202	285031.029799	37.654132
1865.372635	285533.239648	37.659149
1867.464924	286036.627286	37.664167
1869.309372	286538.551779	37.669184
1870.684402	287039.428683	37.674202
1872.690341	287547.465189	37.679220
1874.476117	288055.303679	37.684237
1877.092716	288540.612778	37.689255
1879.007098	289023.514349	37.694272
1880.871750	289489.611045	37.699290
1882.427938	289970.377844	37.704308
1884.030469	290458.801771	37.709325
1886.034216	290939.110264	37.714343
1887.849906	291412.487477	37.719360
1889.641293	291893.431165	37.724378
1891.349856	292377.913257	37.729396
1893.074711	292867.898542	37.734413
1895.162540	293357.112143	37.739431
1896.658529	293851.746142	37.744448
1898.358847	294355.458797	37.749466
1900.146299	294859.204299	37.754484
1902.038880	295373.262266	37.759501
1903.705957	295872.219383	37.764519
1906.066409	296377.309235	37.769536
1907.244917	296897.812460	37.774554
1909.229915	297418.768658	37.779572
1910.674273	297955.088022	37.784589
1912.683396	298487.988141	37.789607
1914.560251	299015.623327	37.794624
1916.495988	299544.894416	37.799642
1919.072041	300086.195048	37.804660
1920.741997	300622.123226	37.809677
1922.782166	301156.744248	37.814695
1924.327795	301692.300453	37.819712
1926.219545	302246.633290	37.824730
1928.421698	302788.269832	37.829748
1930.351520	303338.777435	37.834765
1932.485860	303888.130302	37.839783
1934.053472	304442.186022	37.844800
1935.670289	305012.042511	37.849818
1938.168699	305561.295182	37.854836
1939.721594	306126.732388	37.859853
1941.901553	306677.215809	37.864871
1943.677842	307234.939786	37.869888
1945.435988	307804.336484	37.874906
1947.951495	308378.506962	37.879924
1950.056177	308947.836214	37.884941
1951.912386	309501.613133	37.889959
1953.662480	310071.720769	37.894976
1955.755161	310633.189122	37.899994
1957.446055	311205.424573	37.905012
1959.061238	311793.731019	37.910029
1961.546413	312368.416959	37.915047
1963.616912	312936.384214	37.920064
1965.924069	313521.185116	37.925082
1968.061772	314079.432739	37.930100
1970.080061	314671.522779	37.935117
1972.233416	315223.662975	37.940135
1974.229277	315793.662243	37.945152
1976.270270	316362.555968	37.950170
1978.476853	316933.852834	37.955188
1980.069726	317504.477053	37.960205
1982.145663	318078.038222	37.965223
1984.253479	318642.400450	37.970240
1986.153237	319217.141600	37.975258
1988.387086	319787.813409	37.980276
1990.414049	320353.536344	37.985293
1992.453872	320913.058145	37.990311
1994.527500	321482.895054	37.995328
1996.136399	322057.262999	38.000346
1998.323797	322617.703437	38.005364
2000.397532	323193.962320	38.010381
2002.087583	323770.552366	38.015399
2003.943295	324344.241245	38.020416
2005.735723	324912.146933	38.025434
2007.962411	325479.494705	38.030452
2010.010591	326030.522598	38.035469
2011.700792	326592.306040	38.040487
2013.132734	327151.432629	38.045504
2015.083301	327711.332887	38.050522
2017.263406	328274.309991	38.055540
2019.169226	328839.859065	38.060557
2020.784761	329411.407457	38.065575
2022.688572	329994.039812	38.070592
2024.737743	330567.685232	38.075610
2026.962266	331140.736585	38.080628
2028.886014	331729.073128	38.085645
2031.011619	332304.050609	38.090663
2033.257544	332898.939867	38.095680
2035.012143	333486.032671	38.100698
2036.939728	334078.999821	38.105716
2038.895471	334678.878321	38.110733
2040.841279	335280.930220	38.115751
2043.007482	335879.310502	38.120768
2044.896031	336488.225859	38.125786
2047.006340	337093.773554	38.130804
2048.959893	337711.257137	38.135821
2051.257673	338320.635844	38.140839
2053.631167	338923.626054	38.145856
2055.491478	339546.419176	38.150874
2057.843318	340158.649582	38.155892
2060.412822	340768.831709	38.160909
2061.885945	341380.214651	38.165927
2064.231934	341993.073517	38.170944
2066.259984	342613.452920	38.175962
2068.038789	343233.353007	38.180980
2069.970418	343862.297045	38.185997
2072.345783	344493.239641	38.191015
2074.313104	345126.212444	38.196032
2076.394851	345750.685667	38.201050
2078.537000	346367.809300	38.206068
2081.084328	347002.634152	38.211085
2083.432312	347643.208925	38.216103
2085.531520	348258.960407	38.221120
2087.812598	348881.543597	38.226138
2090.186522	349519.339470	38.231156
2091.915350	350144.495354	38.236173
2093.999635	350769.532921	38.241191
2096.021214	351391.906013	38.246208
2097.490203	352028.678609	38.251226
2099.936988	352671.674697	38.256244
2102.434709	353309.832779	38.261261
2104.630721	353950.636555	38.266279
2106.606789	354583.780078	38.271296
2108.470310	355221.288925	38.276314
2111.163680	355842.430303	38.281332
2113.243754	356487.636822	38.286349
2115.551436	357110.587713	38.291367
2117.857044	357739.483470	38.296384
2119.869185	358368.336204	38.301402
2122.224829	359005.512581	38.306420
2124.370155	359632.189127	38.311437
2126.312540	360263.041411	38.316455
2128.475553	360898.611167	38.321472
2130.732770	361531.998271	38.326490
2132.979808	362153.765157	38.331508
2134.972760	362787.597758	38.336525
2137.084158	363417.520498	38.341543
2139.542331	364046.691204	38.346560
2141.678425	364684.490256	38.351578
2143.473601	365303.625522	38.356596
2145.803486	365932.370105	38.361613
2147.936961	366551.324392	38.366631
2150.069781	367175.105668	38.371648
2152.011521	367790.540765	38.376666
2154.467757	368394.580303	38.381684
2156.518987	369002.445971	38.386701
2158.486066	369597.667450	38.391719
2160.521479	370211.286883	38.396736
2162.731898	370823.091831	38.401754
2164.193485	371421.368894	38.406772
2166.815159	372037.846277	38.411789
2168.532222	372666.536933	38.416807
2170.387887	373283.081011	38.421824
2172.546941	373910.407283	38.426842
2174.574676	374541.463896	38.431860
2176.744382	375172.711664	38.436877
2178.802043	375817.642354	38.441895
2181.293652	376464.313701	38.446912
2182.950296	377113.683991	38.451930
2184.506564	377768.095217	38.456948
2187.009251	378432.626706	38.461965
2188.973971	379098.264235	38.466983
2190.960852	379768.998118	38.472000
2193.476667	380437.783104	38.477018
2195.401536	381123.512188	38.482036
2197.739125	381800.673839	38.487053
2199.875969	382481.800236	38.492071
2202.232036	383163.710136	38.497088
2204.428695	383862.189932	38.502106
2206.159874	384541.425765	38.507124
2208.909189	385248.695592	38.512141
2210.909290	385948.921617	38.517159
2213.118600	386654.387995	38.522176
2215.286478	387359.613152	38.527194
2217.452698	388063.881795	38.532212
2219.714262	388773.306384	38.537229
2221.626871	389507.578961	38.542247
2223.881667	390207.265909	38.547264
2226.017095	390947.360129	38.552282
2228.192591	391669.753849	38.557300
2230.612578	392382.315503	38.562317
2232.890902	393119.232712	38.567335
2235.351734	393849.010527	38.572352
2237.878562	394577.692644	38.577370
2240.003080	395309.655710	38.582388
2242.473999	396041.997747	38.587405
2244.850426	396761.523853	38.592423
2247.340119	397485.920800	38.597440
2249.766884	398224.479396	38.602458
2252.285748	398954.799823	38.607476
2254.742848	399667.491752	38.612493
2256.893787	400398.178777	38.617511
2259.035401	401118.113695	38.622528
2261.134776	401846.333401	38.627546
2263.304293	402578.163101	38.632564
2265.497660	403310.876615	38.637581
2267.533523	404049.309985	38.642599
2269.976869	404784.770918	38.647616
2271.868378	405518.269966	38.652634
2274.319347	406257.679429	38.657652
2276.587233	406999.370195	38.662669
2278.375745	407750.978386	38.667687
2280.945855	408488.878327	38.672704
2283.250348	409237.268803	38.677722
2285.248996	409976.928635	38.682740
2288.157013	410730.789890	38.687757
2289.985934	411485.906922	38.692775
2292.790939	412231.030508	38.697792
2295.309997	412978.753181	38.702810
2297.523974	413715.317946	38.707828
2299.928878	414444.492732	38.712845
2302.270554	415166.722616	38.717863
2304.999245	415872.478995	38.722880
2307.078235	416595.004933	38.727898
2309.592686	417302.972665	38.732916
2312.077621	418018.912310	38.737933
2314.087130	418720.235175	38.742951
2316.307789	419438.746928	38.747968
2318.666783	420146.743962	38.752986
2320.409399	420866.292567	38.758004
2322.410232	421596.445554	38.763021
2324.813810	422327.268138	38.768039
2327.230222	423061.096526	38.773056
2329.409452	423791.750222	38.778074
2331.584799	424534.563409	38.783092
2333.733012	425271.893282	38.788109
2335.495688	426024.474178	38.793127
2338.345518	426773.368579	38.798144
2340.438072	427516.438740	38.803162
2342.759392	428284.013355	38.808180
2345.496502	429043.607634	38.813197
2347.866167	429805.656542	38.818215
2350.250568	430572.980988	38.823232
2352.419571	431345.515154	38.828250
2354.616284	432117.306945	38.833268
2357.119636	432890.536430	38.838285
2359.486847	433681.242363	38.843303
2361.692190	434446.370498	38.848320
2364.366642	435233.073673	38.853338
2366.719426	436025.100728	38.858356
2369.185709	436809.548437	38.863373
2371.441090	437598.847460	38.868391
2373.786182	438392.596374	38.873408
2376.174791	439188.679763	38.878426
2378.085005	439981.823657	38.883444
2380.741795	440792.246145	38.888461
2382.863039	441606.506016	38.893479
2385.055144	442413.495732	38.898496
2387.730273	443231.689465	38.903514
2390.055913	444042.274727	38.908532
2392.953819	444855.563227	38.913549
2395.219285	445683.460076	38.918567
2397.690274	446500.984726	38.923584
2400.102905	447312.169247	38.928602
2402.411472	448132.978954	38.933620
2405.019547	448955.774881	38.938637
2407.444675	449774.269872	38.943655
2410.277901	450593.522043	38.948672
2413.279185	451412.356950	38.953690
2415.943423	452225.501922	38.958708
2418.562553	453039.626368	38.963725
2421.185496	453849.674155	38.968743
2423.140524	454650.551360	38.973760
2425.937938	455446.565852	38.978778
2428.121455	456258.035055	38.983796
2430.987230	457058.861408	38.988813
2433.462215	457866.878750	38.993831
2436.193109	458661.848013	38.998848
2438.449729	459464.424666	39.003866
2441.227557	460268.900836	39.008884
2443.547187	461073.965933	39.013901
2445.841240	461862.597958	39.018919
2448.046618	462656.908835	39.023936
2450.748871	463454.131988	39.028954
2453.238852	464262.248230	39.033972
2455.988047	465046.422647	39.038989
2458.257398	465840.573460	39.044007
2460.867587	466634.027882	39.049024
2463.083785	467426.194625	39.054042
2465.007310	468197.436887	39.059060
2467.578436	468962.539858	39.064077
2470.032528	469744.924815	39.069095
2472.456872	470514.013412	39.074112
2474.372332	471292.071632	39.079130
2476.833070	472070.915187	39.084148
2479.435244	472848.892533	39.089165
2481.851355	473639.064004	39.094183
2483.988482	474427.727875	39.099200
2486.463867	475216.602745	39.104218
2488.749568	476015.349962	39.109236
2491.441787	476803.608674	39.114253
2494.020193	477610.498098	39.119271
2496.433232	478415.053681	39.124288
2499.104241	479218.217536	39.129306
2501.252679	480038.508804	39.134324
2503.573649	480849.557544	39.139341
2505.886081	481677.751231	39.144359
2508.329477	482512.179922	39.149376
2510.633481	483349.558877	39.154394
2512.664115	484187.993632	39.159412
2515.282131	485031.732866	39.164429
2517.493203	485900.731865	39.169447
2519.980004	486755.431231	39.174464
2522.961689	487620.887187	39.179482
2524.969912	488494.053001	39.184500
2527.804626	489363.815637	39.189517
2530.520882	490244.980766	39.194535
2532.994514	491123.815620	39.199552
2535.872631	491993.823054	39.204570
2538.084081	492876.524835	39.209588
2540.785156	493755.421859	39.214605
2543.109440	494655.575630	39.219623
2545.674909	495538.567990	39.224640
2548.581014	496432.883528	39.229658
2550.652862	497336.538901	39.234676
2553.779729	498226.028918	39.239693
2556.395375	499126.166483	39.244711
2558.477032	500029.503267	39.249728
2561.156075	500934.049554	39.254746
2563.632674	501845.214635	39.259764
2566.148367	502752.038405	39.264781
2568.978662	503661.574006	39.269799
2571.694649	504572.428509	39.274816
2574.326993	505482.282081	39.279834
2577.214855	506405.421120	39.284852
2580.109615	507304.450639	39.289869
2582.897063	508209.023994	39.294887
2585.142429	509118.956406	39.299904
2588.187970	510030.918061	39.304922
2590.582969	510949.008153	39.309940
2593.018858	511856.570315	39.314957
2595.672552	512777.366403	39.319975
2597.813299	513692.046537	39.324992
2600.771959	514617.651126	39.330010
2602.988486	515538.030144	39.335028
2605.864036	516463.372772	39.340045
2608.393493	517387.399880	39.345063
2610.781453	518310.632515	39.350080
2613.557936	519236.456182	39.355098
2615.908832	520172.335982	39.360116
2618.248279	521101.669184	39.365133
2621.428130	522022.313417	39.370151
2624.230780	522956.069673	39.375168
2627.099568	523876.584935	39.380186
2629.710489	524809.387401	39.385204
2632.358246	525725.036043	39.390221
2635.184641	526641.196360	39.395239
2637.796550	527539.291922	39.400256
2641.023993	528429.745293	39.405274
2643.123686	529314.035966	39.410292
2646.105274	530189.339432	39.415309
2648.424974	531074.832658	39.420327
2650.734475	531954.743101	39.425344
2653.940265	532840.379137	39.430362
2656.438076	533733.697491	39.435380
2659.339952	534623.024671	39.440397
2662.134367	535507.688218	39.445415
2664.477691	536403.706846	39.450432
2667.153033	537277.473232	39.455450
2669.737445	538177.746989	39.460468
2672.232313	539079.175510	39.465485
2674.373244	539985.162277	39.470503
2677.043418	540899.984190	39.475520
2680.143668	541814.471603	39.480538
2682.483177	542745.569614	39.485556
2685.114232	543664.210164	39.490573
2688.107512	544580.167736	39.495591
2691.043563	545499.528169	39.500608
2694.113787	546421.608458	39.505626
2697.039501	547347.956101	39.510644
2700.016233	548267.906639	39.515661
2702.277086	549193.617357	39.520679
2704.911382	550130.733413	39.525696
2707.527479	551053.088498	39.530714
2710.486934	551996.679187	39.535732
2713.664895	552924.620407	39.540749
2716.602460	553854.884174	39.545767
2719.066834	554794.423725	39.550784
2721.712709	555734.112073	39.555802
2724.241284	556683.518381	39.560820
2726.911651	557603.058436	39.565837
2729.736503	558564.647240	39.570855
2731.775211	559527.233164	39.575872
2734.478445	560475.106916	39.580890
2737.426299	561442.004265	39.585908
2739.926485	562406.988548	39.590925
2742.909614	563387.796991	39.595943
2745.561270	564361.011890	39.600960
2748.157707	565328.344595	39.605978
2750.317297	566323.308447	39.610996
2752.950708	567304.592759	39.616013
2756.001706	568310.863491	39.621031
2758.093006	569306.232032	39.626048
2761.003042	570299.233621	39.631066
2763.750781	571319.805753	39.636084
2766.528269	572324.415380	39.641101
2769.257238	573335.800410	39.646119
2772.221665	574358.568364	39.651136
2775.122678	575364.040333	39.656154
2777.509452	576399.773746	39.661172
2780.350207	577409.525357	39.666189
2782.991215	578434.825003	39.671207
2785.575601	579471.794156	39.676224
2788.628370	580498.340185	39.681242
2791.353237	581528.243252	39.686260
2794.076589	582560.400951	39.691277
2796.973759	583601.285159	39.696295
2799.903853	584642.465608	39.701312
2802.710929	585676.917360	39.706330
2805.329521	586713.899965	39.711348
2808.227040	587758.837411	39.716365
2811.340269	588799.142506	39.721383
2813.997196	589843.166924	39.726400
2817.220051	590873.010661	39.731418
2820.030085	591903.020180	39.736436
2822.574830	592904.895353	39.741453
2825.699394	593898.743147	39.746471
2828.288056	594895.529095	39.751488
2830.870424	595901.512295	39.756506
2833.570706	596911.626472	39.761524
2836.882031	597911.311780	39.766541
2840.080890	598911.818548	39.771559
2842.541357	599915.141328	39.776576
2845.684719	600913.868161	39.781594
2848.383921	601924.898256	39.786612
2851.667808	602926.155769	39.791629
2854.421210	603933.288655	39.796647
2857.051567	604945.832006	39.801664
2860.169836	605950.964713	39.806682
2862.984527	606965.326642	39.811700
2866.200848	607985.811282	39.816717
2868.624375	609007.315771	39.821735
2871.233616	610032.130492	39.826752
2874.477142	611051.556137	39.831770
2877.395024	612089.530620	39.836788
2880.085416	613121.849662	39.841805
2882.713436	614165.988550	39.846823
2885.193694	615215.376254	39.851840
2888.134373	616271.610471	39.856858
2891.046797	617333.170180	39.861876
2893.754348	618395.097407	39.866893
2896.995827	619460.365640	39.871911
2899.532812	620531.508849	39.876928
2902.314167	621600.006776	39.881946
2905.421168	622680.691761	39.886964
2908.120846	623757.984375	39.891981
2911.039609	624841.499017	39.896999
2914.156913	625948.864700	39.902016
2916.918587	627035.496492	39.907034
2919.378548	628138.732159	39.912052
2922.238014	629240.385753	39.917069
2925.559062	630348.511189	39.922087
2928.090108	631470.717085	39.927104
2931.324988	632577.503896	39.932122
2934.503186	633698.650816	39.937140
2937.182003	634823.873324	39.942157
2940.345953	635939.833086	39.947175
2943.206042	637073.167527	39.952192
2946.215143	638204.253898	39.957210
2949.310743	639338.124838	39.962228
2951.724670	640469.230762	39.967245
2954.823134	641607.152618	39.972263
2957.681663	642752.827353	39.977280
2960.636299	643896.854913	39.982298
2963.662010	645037.996940	39.987316
2966.495737	646195.326856	39.992333
2970.004715	647333.823832	39.997351
2973.028839	648475.882164	40.002368
2976.375226	649615.413207	40.007386
2979.209616	650770.129744	40.012404
2982.506714	651904.118044	40.017421
2985.865051	653038.402093	40.022439
2988.732604	654182.798577	40.027456
2992.001372	655312.938843	40.032474
2995.174010	656455.410684	40.037492
2997.880386	657597.164877	40.042509
3001.199415	658728.058479	40.047527
3004.416111	659857.584386	40.052544
3007.430014	660987.445135	40.057562
3010.446779	662116.913568	40.062580
3013.350548	663246.305102	40.067597
3016.292273	664363.396393	40.072615
3019.230845	665492.990399	40.077632
3021.973571	666593.317623	40.082650
3025.134799	667684.964211	40.087668
3027.848593	668777.238083	40.092685
3031.186426	669861.298160	40.097703
3034.034966	670954.863102	40.102720
3036.941558	672038.569520	40.107738
3040.093957	673136.270116	40.112756
3043.123324	674240.883833	40.117773
3046.122198	675343.081843	40.122791
3048.479372	676448.011462	40.127808
3051.779478	677571.813042	40.132826
3055.143862	678686.396080	40.137844
3057.775749	679800.798765	40.142861
3060.532481	680925.775785	40.147879
3063.559758	682063.180275	40.152896
3066.533814	683196.629256	40.157914
3069.726907	684339.390246	40.162932
3072.608747	685497.379192	40.167949
3075.898403	686637.832061	40.172967
3078.695026	687804.614754	40.177984
3081.476407	688964.560323	40.183002
3084.498328	690136.962643	40.188020
3087.419217	691313.119494	40.193037
3090.724353	692496.313923	40.198055
3093.812144	693681.793282	40.203072
3097.154542	694862.959824	40.208090
3100.670420	696041.952008	40.213108
3103.281571	697234.153502	40.218125
3107.131637	698430.875799	40.223143
3110.137014	699620.787526	40.228160
3113.507464	700816.144914	40.233178
3116.943771	702015.708170	40.238196
3120.056014	703200.284815	40.243213
3123.459956	704393.474803	40.248231
3126.717451	705595.934390	40.253248
3130.178796	706789.496533	40.258266
3133.015052	707985.985980	40.263284
3135.621799	709174.142399	40.268301
3139.255263	710383.362852	40.273319
3141.833900	711604.445772	40.278336
3144.943504	712819.635127	40.283354
3148.057285	714049.225931	40.288372
3151.042125	715263.462806	40.293389
3154.538331	716490.193165	40.298407
3157.165753	717729.133544	40.303424
3160.305992	718947.203353	40.308442
3163.826061	720185.806800	40.313460
3166.673272	721427.763059	40.318477
3169.927308	722669.355937	40.323495
3173.154759	723916.363506	40.328512
3176.117536	725156.514034	40.333530
3179.684038	726411.771912	40.338548
3182.910518	727655.016134	40.343565
3185.954310	728891.098084	40.348583
3189.224664	730145.240551	40.353600
3192.155293	731385.849148	40.358618
3195.503015	732637.890415	40.363636
3198.467771	733901.040540	40.368653
3201.557886	735150.438528	40.373671
3204.706133	736414.312731	40.378688
3207.826024	737672.324434	40.383706
3211.131740	738944.586691	40.388724
3214.679555	740210.008624	40.393741
3218.213616	741463.033948	40.398759
3221.398349	742721.644849	40.403776
3224.842979	743975.284626	40.408794
3228.355987	745215.983458	40.413812
3231.740408	746464.048831	40.418829
3234.834828	747686.082756	40.423847
3237.947837	748898.927979	40.428864
3240.768678	750097.878625	40.433882
3244.343739	751302.249806	40.438900
3246.909696	752519.081391	40.443917
3250.118129	753730.554902	40.448935
3253.000266	754952.805553	40.453952
3255.840053	756181.469505	40.458970
3258.758863	757416.817874	40.463988
3261.933860	758673.861134	40.469005
3264.966705	759917.426268	40.474023
3268.231218	761166.416748	40.479040
3271.656219	762441.261233	40.484058
3275.018596	763709.958383	40.489076
3277.972084	764982.061998	40.494093
3281.217239	766262.452369	40.499111
3284.394636	767539.974163	40.504128
3287.660393	768832.559835	40.509146
3291.279887	770118.243854	40.514164
3294.343833	771416.587954	40.519181
3298.182493	772709.430510	40.524199
3301.499449	774011.692218	40.529216
3304.656098	775320.182172	40.534234
3307.940431	776635.681806	40.539252
3311.452088	777961.932969	40.544269
3314.980424	779274.145014	40.549287
3318.469590	780595.143230	40.554304
3321.551691	781913.112970	40.559322
3324.803335	783234.556170	40.564340
3327.812470	784570.614886	40.569357
3331.067282	785911.247437	40.574375
3334.820536	787249.384496	40.579392
3337.939222	788591.545640	40.584410
3341.843319	789926.336586	40.589428
3345.025499	791282.084235	40.594445
3348.599787	792613.650269	40.599463
3351.950210	793958.238611	40.604480
3355.488451	795307.296474	40.609498
3359.300701	796648.820855	40.614516
3362.678026	798001.924468	40.619533
3366.212999	799349.265827	40.624551
3369.550497	800698.645315	40.629568
3372.650477	802044.712004	40.634586
3376.285757	803387.979069	40.639604
3379.428356	804742.330747	40.644621
3382.789423	806094.803987	40.649639
3386.334483	807447.252847	40.654656
3389.839878	808802.483375	40.659674
3393.177402	810154.532643	40.664692
3396.429739	811516.708042	40.669709
3399.824635	812874.581102	40.674727
3403.055400	814245.304934	40.679744
3406.391875	815609.591088	40.684762
3409.434144	816974.013438	40.689780
3413.103916	818354.547796	40.694797
3415.858565	819726.956432	40.699815
3419.632976	821105.987360	40.704832
3423.105628	822481.069294	40.709850
3426.802334	823860.660146	40.714868
3430.297820	825243.561329	40.719885
3433.769757	826621.401349	40.724903
3437.591371	827997.517986	40.729920
3440.579313	829388.963825	40.734938
3444.085028	830758.106297	40.739956
3447.017461	832150.089433	40.744973
3450.471795	833542.929082	40.749991
3453.820273	834935.753241	40.755008
3456.938184	836308.523270	40.760013
3460.649875	837641.027388	40.765018
3463.705101	838929.865898	40.770023
3467.128706	840159.578226	40.775028
3470.065438	841336.832603	40.780032
3473.302083	842456.397051	40.785037
3476.301349	843500.062765	40.790042
3478.670371	844503.411651	40.795047
3481.441329	845424.236836	40.800052
3483.840801	846303.013058	40.805056
3486.271220	847105.975545	40.810061
3488.701599	847848.758793	40.815066
3491.025179	848549.905306	40.820071
3493.290730	849182.687961	40.825076
3495.727309	849763.752064	40.830080
3497.728320	850299.696475	40.835085
3499.920944	850756.736165	40.840090
3501.670787	851171.687853	40.845095
3503.106523	851546.864222	40.850100
3504.675566	851881.912581	40.855104
3505.600050	852181.414907	40.860109
3506.798382	852417.642382	40.865114
3507.769558	852652.637239	40.870119
3508.943436	852839.867236	40.875124
3510.483865	852997.025865	40.880128
3511.096294	853126.737890	40.885133
3512.009313	853209.647401	40.890138
3512.365496	853296.611371	40.895143
3513.210144	853341.392228	40.900148
3513.959719	853360.343614	40.905152
3514.446870	853362.009835	40.910157
3515.396498	853347.245535	40.915162
3515.651747	853312.553221	40.920167
3516.079429	853258.281013	40.925172
3516.064887	853192.171409	40.930176
3516.794226	853114.328986	40.935181
3517.140742	853015.152616	40.940186
3516.986981	852905.694971	40.945191
3517.219238	852784.074451	40.950196
3517.820451	852669.557329	40.955200
3517.838941	852545.254651	40.960205
3517.999525	852386.849920	40.965210
3518.570883	852228.860712	40.970215
3518.665543	852069.392668	40.975220
3518.562445	851895.331554	40.980224
3518.849568	851719.945534	40.985229
3518.926183	851544.974419	40.990234
3519.042420	851355.467706	40.995239
3519.223360	851158.101392	41.000244
3519.086223	850957.679397	41.005248
3519.166747	850760.024752	41.010253
3518.977994	850542.165702	41.015258
3518.915192	850336.481235	41.020263
3519.203737	850124.148900	41.025268
3518.906078	849909.866570	41.030272
3518.955737	849690.873001	41.035277
3518.940627	849465.004328	41.040282
3518.861599	849246.304740	41.045287
3518.768522	849019.849826	41.050292
3518.993189	848797.986220	41.055296
3518.615001	848580.373994	41.060301
3518.507604	848352.829814	41.065306
3518.790338	848129.381679	41.070311
3518.625478	847903.088419	41.075316
3518.434434	847674.949601	41.080320
3518.224399	847446.320386	41.085325
3518.136544	847210.299003	41.090330
3517.951452	846989.496651	41.095335
3517.950440	846766.040791	41.100340
3518.119228	846542.259143	41.105344
3518.074975	846309.974055	41.110349
3517.899349	846069.365583	41.115354
3517.547629	845838.175940	41.120359
3517.582740	845617.675164	41.125364
3517.756356	845391.231937	41.130368
3517.225342	845167.119529	41.135373
3517.410865	844936.973584	41.140378
3516.981587	844708.756557	41.145383
3517.029542	844485.303150	41.150388
3517.082894	844261.549580	41.155392
3516.704412	844045.417020	41.160397
3516.902164	843828.410831	41.165402
3516.604433	843610.795415	41.170407
3515.963175	843385.081060	41.175412
3515.956028	843173.900383	41.180416
3515.763446	842961.092703	41.185421
3516.257709	842740.412369	41.190426
3515.416874	842540.490918	41.195431
3515.037652	842325.847020	41.200436
3515.502109	842118.433957	41.205440
3515.149190	841917.639309	41.210445
3515.094656	841708.547297	41.215450
3515.064862	841509.434050	41.220455
3514.949760	841306.932663	41.225460
3515.246583	841105.135936	41.230464
3514.604870	840907.456064	41.235469
3514.369248	840704.661928	41.240474
3514.346914	840517.736626	41.245479
3514.011178	840320.183348	41.250484
3514.059630	840128.966296	41.255488
3514.091915	839948.223346	41.260493
3514.232286	839755.039566	41.265498
3513.707016	839578.932433	41.270503
3513.258639	839382.820900	41.275508
3513.111961	839197.134791	41.280512
3513.276206	839016.536935	41.285517
3512.968735	838837.656917	41.290522
3513.095829	838670.153944	41.295527
3512.644424	838499.340307	41.300532
3512.671194	838314.764028	41.305536
3512.358302	838150.226490	41.310541
3512.403789	837980.678938	41.315546
3512.168289	837811.752794	41.320551
3511.983903	837649.898778	41.325556
3511.776251	837493.479144	41.330560
3511.606885	837340.058237	41.335565
3512.005514	837173.344293	41.340570
3511.681718	837025.374865	41.345575
3511.313906	836868.381507	41.350580
3511.607125	836707.009666	41.355584
3510.891050	836554.915946	41.360589
3511.638840	836402.492447	41.365594
3510.807104	836259.631286	41.370599
3511.074877	836104.557108	41.375604
3511.001718	835949.338047	41.380608
3511.020963	835803.420531	41.385613
3510.947129	835653.921836	41.390618
3510.913524	835512.277265	41.395623
3510.701290	835361.530763	41.400628
3510.700190	835223.952098	41.405632
3510.346303	835079.337484	41.410637
3510.382174	834936.891695	41.415642
3509.390446	834810.624596	41.420647
3509.597130	834679.797927	41.425652
3510.016156	834551.848326	41.430656
3509.485261	834429.870835	41.435661
3509.624858	834293.316999	41.440666
3509.474828	834164.185695	41.445671
3509.454604	834037.750460	41.450676
3509.491414	833910.915193	41.455680
3509.113117	833802.011474	41.460685
3509.175675	833667.397776	41.465690
3509.067724	833550.289321	41.470695
3508.942041	833422.303712	41.475700
3509.039096	833295.640297	41.480704
3508.592455	833187.027494	41.485709
3508.647152	833065.513520	41.490714
3509.092039	832950.540912	41.495719
3508.633838	832830.073660	41.500724
3508.438551	832718.013499	41.505728
3508.490630	832601.735776	41.510733
3508.273291	832499.679914	41.515738
3507.963604	832384.717334	41.520743
3508.119548	832279.296674	41.525748
3508.153657	832172.727514	41.530752
3508.196462	832071.498018	41.535757
3507.911652	831954.871911	41.540762
3507.769520	831858.039292	41.545767
3507.491659	831755.494562	41.550772
3507.865922	831659.355224	41.555776
3507.826925	831566.970729	41.560781
3507.545132	831449.557171	41.565786
3507.289379	831355.260247	41.570791
3507.092212	831262.701512	41.575796
3507.403034	831170.159108	41.580800
3507.347039	831068.928253	41.585805
3507.102850	830985.602802	41.590810
3507.585885	830894.875329	41.595815
3506.991544	830798.387903	41.600820
3507.118644	830712.182882	41.605824
3506.736204	830617.699923	41.610829
3506.714704	830528.794840	41.615834
3506.826599	830450.264772	41.620839
3506.872042	830357.751431	41.625844
3506.666577	830266.053281	41.630848
3506.523196	830177.842307	41.635853
3506.462495	830093.892845	41.640858
3506.340440	830015.490887	41.645863
3506.583549	829940.334883	41.650868
3506.202670	829855.849105	41.655872
3506.217170	829782.378927	41.660877
3506.156715	829696.188765	41.665882
3505.825581	829623.256597	41.670887
3506.014915	829549.853454	41.675892
3506.278478	829473.133516	41.680896
3505.649368	829395.483099	41.685901
3506.030246	829328.072901	41.690906
3505.779025	829256.192890	41.695911
3505.798971	829175.328146	41.700916
3505.986506	829121.260920	41.705920
3505.356133	829054.880489	41.710925
3505.411104	828980.908317	41.715930
3505.237564	828900.556125	41.720935
3505.255076	828850.789629	41.725940
3505.407010	828773.495130	41.730944
3505.475625	828726.441132	41.735949
3505.231066	828650.859408	41.740954
3505.328733	828597.287560	41.745959
3505.466384	828530.198133	41.750964
3505.591839	828473.510433	41.755968
3505.463090	828403.253602	41.760973
3505.458846	828333.170902	41.765978
3505.336169	828264.758390	41.770983
3505.187210	828203.445239	41.775988
3505.270889	828147.247058	41.780992
3505.107604	828073.492374	41.785997
3504.902876	828022.295719	41.791002
3504.988645	827966.289957	41.796007
3504.355464	827903.785754	41.801012
3504.590074	827852.616203	41.806016
3504.333950	827807.161238	41.811021
3504.861440	827744.668386	41.816026
3504.636210	827702.999122	41.821031
3504.778623	827644.745630	41.826036
3504.841611	827587.962232	41.831040
3504.701739	827530.335067	41.836045
3504.896470	827474.988269	41.841050
3505.140504	827430.327260	41.846055
3504.631926	827373.922868	41.851060
3504.749666	827306.434189	41.856064
3504.454829	827259.717325	41.861069
3504.229463	827198.211548	41.866074
3504.427833	827155.694544	41.871079
3504.106232	827103.925098	41.876084
3504.898228	827048.383839	41.881088
3504.614851	827011.094014	41.886093
3504.557518	826947.517719	41.891098
3504.361730	826903.796640	41.896103
3503.955950	826842.023791	41.901108
3504.065376	826799.032068	41.906112
3503.731579	826760.290167	41.911117
3504.313715	826713.529253	41.916122
3504.129341	826677.583124	41.921127
3503.680658	826640.414101	41.926132
3503.980267	826593.890898	41.931136
3503.940753	826555.004458	41.936141
3504.252947	826501.672338	41.941146
3503.831862	826451.274159	41.946151
3504.189470	826412.908137	41.951156
3504.000438	826368.793228	41.956160
3503.410688	826328.727304	41.961165
3504.117137	826276.401180	41.966170
3503.867724	826231.516825	41.971175
3503.532226	826199.675464	41.976180
3503.644373	826159.109752	41.981184
3503.509106	826139.488796	41.986189
3503.748573	826101.333764	41.991194
3503.412102	826074.937301	41.996199
3503.446476	826035.160841	42.001204
3503.606327	825995.364508	42.006208
3503.554131	825966.978319	42.011213
3503.633392	825927.485866	42.016218
3503.699243	825892.079445	42.021223
3503.477130	825851.174971	42.026228
3503.553475	825814.891273	42.031232
3503.232019	825779.447500	42.036237
3503.259495	825743.851730	42.041242
3503.119476	825708.379182	42.046247
3503.270431	825680.251640	42.051252
3503.169373	825642.049729	42.056256
3503.156963	825613.655679	42.061261
3503.532786	825579.949442	42.066266
3503.363230	825549.342964	42.071271
3503.228846	825514.840892	42.076276
3503.064683	825483.941498	42.081280
3503.021864	825456.037715	42.086285
3503.376210	825433.809466	42.091290
3502.844125	825399.077159	42.096295
3503.087618	825375.601772	42.101300
3502.994816	825342.745492	42.106304
3503.430529	825319.531595	42.111309
3503.424292	825286.661482	42.116314
3503.377152	825256.034400	42.121319
3502.886360	825216.529215	42.126324
3502.401585	825194.723031	42.131328
3502.687338	825173.282589	42.136333
3503.106151	825141.026028	42.141338
3503.237627	825116.011084	42.146343
3503.260384	825094.222458	42.151348
3503.268966	825057.944864	42.156352
3502.881975	825036.414597	42.161357
3502.989264	825002.066365	42.166362
3502.585517	824977.329035	42.171367
3502.958901	824961.612324	42.176372
3503.072214	824926.581925	42.181376
3502.704070	824909.327612	42.186381
3502.997457	824877.867339	42.191386
3503.075931	824859.181446	42.196391
3502.804028	824823.432603	42.201396
3503.146814	824799.842229	42.206400
3502.741362	824782.885170	42.211405
3503.017751	824745.202216	42.216410
3502.781592	824725.397968	42.221415
3503.074975	824701.814941	42.226420
3502.749586	824671.617476	42.231424
3502.531599	824646.947032	42.236429
3502.862871	824622.774203	42.241434
3502.624188	824601.024692	42.246439
3502.288257	824574.427129	42.251444
3502.852451	824560.041253	42.256448
3502.423253	824531.123751	42.261453
3502.749710	824519.206549	42.266458
3502.789278	824493.522580	42.271463
3502.831037	824462.585837	42.276468
3502.904270	824435.145585	42.281472
3502.553661	824422.166846	42.286477
3502.402084	824388.828303	42.291482
3502.506786	824378.015423	42.296487
3502.599880	824362.438263	42.301492
3502.680938	824331.591982	42.306496
3502.414129	824310.137635	42.311501
3502.444804	824291.749287	42.316506
3502.705928	824274.103007	42.321511
3502.638864	824259.717842	42.326516
3502.795601	824233.139049	42.331520
3502.266034	824221.355085	42.336525
3502.486065	824199.337901	42.341530
3502.635361	824187.642290	42.346535
3502.746781	824153.775007	42.351540
3502.572212	824144.561696	42.356544
3502.306274	824130.110044	42.361549
3502.610689	824099.324951	42.366554
3502.362774	824082.924948	42.371559
3502.273028	824064.068385	42.376564
3502.870263	824035.182629	42.381568
3502.041271	824018.970561	42.386573
3502.447834	824000.717127	42.391578
3502.488710	823984.660807	42.396583
3502.072240	823958.267702	42.401588
3502.417157	823943.525573	42.406592
3502.515593	823932.129247	42.411597
3502.309458	823910.858563	42.416602
3502.511460	823899.543261	42.421607
3502.230325	823873.517732	42.426612
3502.612161	823858.380529	42.431616
3502.245479	823838.204714	42.436621
3502.493971	823823.963748	42.441626
3502.707638	823803.307996	42.446631
3502.083209	823779.281245	42.451636
3502.505606	823765.207511	42.456640
3501.900310	823752.753544	42.461645
3502.016527	823738.143950	42.466650
3502.247960	823736.162313	42.471655
3502.515013	823714.525148	42.476660
3502.318544	823694.905916	42.481664
3501.784610	823679.619596	42.486669
3502.054818	823661.289193	42.491674
3502.293935	823645.687387	42.496679
3502.096876	823636.865940	42.501684
3502.263909	823615.925012	42.506688
3502.201887	823617.685803	42.511693
3502.148913	823599.600293	42.516698
3502.361548	823596.746040	42.521703
3502.424912	823584.673599	42.526708
3502.248122	823557.171226	42.531712
3502.156768	823546.776650	42.536717
3502.203377	823528.869925	42.541722
3502.016853	823529.580121	42.546727
3501.999056	823501.468964	42.551732
3501.985042	823483.279741	42.556736
3502.256748	823476.816806	42.561741
3502.457005	823459.372264	42.566746
3502.603386	823449.134923	42.571751
3502.666710	823425.777524	42.576756
3502.376586	823405.491034	42.581760
3502.255848	823387.415492	42.586765
3502.503130	823366.850301	42.591770
3502.172055	823348.029262	42.596775
3502.041892	823331.316991	42.601780
3502.183218	823325.944395	42.606784
3502.251398	823304.239592	42.611789
3502.544824	823288.433824	42.616794
3502.219486	823263.385453	42.621799
3502.204491	823258.523657	42.626804
3502.281364	823240.416792	42.631808
3501.883196	823234.252888	42.636813
3502.142230	823218.160462	42.641818
3502.327426	823204.608953	42.646823
3502.183657	823195.875826	42.651828
3502.110619	823182.072779	42.656832
3502.097190	823160.963941	42.661837
3501.902419	823146.693414	42.666842
3501.514748	823135.274313	42.671847
3501.993347	823120.703891	42.676852
3502.333307	823109.754718	42.681856
3501.687386	823119.973582	42.686861
3501.631506	823092.839374	42.691866
3502.028783	823086.161827	42.696871
3501.956078	823082.184496	42.701876
3502.375312	823075.308931	42.706880
3501.785325	823054.095279	42.711885
3502.068552	823035.955554	42.716890
3501.703752	823036.499098	42.721895
3502.014231	823018.063196	42.726900
3501.933524	822995.991426	42.731904
3501.650859	823008.877768	42.736909
3501.575387	823002.565897	42.741914
3501.882663	822979.168666	42.746919
3502.164278	822973.871122	42.751924
3502.223267	822966.176150	42.756928
3502.466222	822950.766562	42.761933
3502.155313	822924.838950	42.766938
3501.745097	822920.914275	42.771943
3502.332947	822905.547949	42.776948
3502.324270	822896.793278	42.781952
3502.036187	822876.796589	42.786957
3502.280306	822864.305316	42.791962
3501.942223	822864.747406	42.796967
3502.099059	822840.594841	42.801972
3501.965296	822831.956922	42.806977
3501.696394	822822.561785	42.811981
3501.908900	822796.357227	42.816986
3502.274066	822791.824801	42.821991
3501.986748	822789.534789	42.826996
3502.079661	822759.457094	42.832001
3501.792776	822762.420786	42.837005
3501.968691	822752.566839	42.842010
3502.194210	822734.435248	42.847015
3501.653819	822717.201675	42.852020
3501.971720	822711.898235	42.857025
3502.086962	822702.734744	42.862029
3501.998286	822685.235883	42.867034
3501.986835	822682.902706	42.872039
3501.777056	822667.174008	42.877044
3501.862142	822644.880472	42.882049
3501.381732	822643.204354	42.887053
3501.576583	822645.314443	42.892058
3501.902107	822643.998811	42.897063
3502.045285	822629.674253	42.902068
3502.578094	822619.472420	42.907073
3501.970759	822609.351504	42.912077
3502.198857	822584.311142	42.917082
3502.146409	822580.038434	42.922087
3501.840696	822557.708378	42.927092
3502.299775	822534.966800	42.932097
3501.971983	822544.553105	42.937101
3502.047493	822531.795628	42.942106
3501.738519	822517.736083	42.947111
3501.800865	822504.202238	42.952116
3501.979786	822502.325716	42.957121
3501.621990	822491.484522	42.962125
3501.645476	822476.983726	42.967130
3502.031964	822475.269342	42.972135
3501.981512	822465.255728	42.977140
3501.787568	822451.956426	42.982145
3501.778937	822446.606507	42.987149
3502.037721	822440.630996	42.992154
3501.920958	822435.589862	42.997159
3501.614902	822417.443137	43.002164
3502.048219	822414.748439	43.007169
3501.527345	822413.565070	43.012173
3501.632632	822400.705369	43.017178
3502.031425	822379.626708	43.022183
3501.425248	822382.056703	43.027188
3501.699822	822371.602935	43.032193
3501.309226	822375.653306	43.037197
3501.357285	822369.710667	43.042202
3501.556405	822378.144579	43.047207
3501.138631	822350.869071	43.052212
3501.444194	822344.886155	43.057217
3501.751590	822354.470760	43.062221
3501.724059	822353.696752	43.067226
3501.967248	822350.934449	43.072231
3501.585160	822345.837419	43.077236
3501.441790	822324.064928	43.082241
3501.540313	822327.357777	43.087245
3501.765974	822312.435793	43.092250
3501.953577	822327.293330	43.097255
3501.682971	822323.930239	43.102260
3502.185620	822304.975669	43.107265
3501.498958	822297.007224	43.112269
3501.641163	822285.503707	43.117274
3501.740260	822299.012951	43.122279
3501.331606	822287.595548	43.127284
3501.646073	822262.053876	43.132289
3501.644870	822262.832543	43.137293
3501.594664	822249.704934	43.142298
3501.480811	822250.209311	43.147303
3501.414173	822254.209119	43.152308
3501.720896	822254.647751	43.157313
3501.543423	822237.258796	43.162317
3501.596097	822229.953093	43.167322
3501.303444	822219.101233	43.172327
3501.752249	822225.647607	43.177332
3501.663273	822220.115449	43.182337
3502.046350	822232.218236	43.187341
3501.592531	822206.212628	43.192346
3501.849563	822203.740000	43.197351
3502.010025	822201.185165	43.202356
3502.082188	822182.005610	43.207361
3501.603196	822169.625968	43.212365
3501.633187	822159.599281	43.217370
3501.297631	822161.111340	43.222375
3501.469947	822155.830184	43.227380
3501.671021	822151.614849	43.232385
3501.483293	822140.746448	43.237389
3501.695693	822125.242272	43.242394
3501.601660	822126.327375	43.247399
3501.683911	822127.190316	43.252404
3501.655991	822127.194758	43.257409
3502.007062	822131.615860	43.262413
3502.042598	822113.122931	43.267418
3501.760637	822093.998459	43.272423
3501.758753	822095.263768	43.277428
3502.234344	822077.966880	43.282433
3501.788680	822059.257102	43.287437
3501.527931	822061.535918	43.292442
3502.079768	822067.482536	43.297447
3501.297038	822040.943825	43.302452
3501.815374	822024.710446	43.307457
3501.778701	822036.976538	43.312461
3501.725334	822027.546490	43.317466
3502.014434	822016.895244	43.322471
3501.838174	822000.575774	43.327476
3501.894007	821992.198948	43.332481
3501.954249	821997.735959	43.337485
3501.640479	821968.788323	43.342490
3502.057523	821965.414843	43.347495
3501.848608	821963.696091	43.352500
3501.572179	821953.619665	43.357505
3501.545244	821937.665905	43.362509
3501.751995	821940.455516	43.367514
3501.612841	821932.109090	43.372519
3501.757660	821931.113475	43.377524
3501.585218	821939.508768	43.382529
3501.993971	821917.745836	43.387533
3501.713122	821906.891579	43.392538
3501.667669	821902.617306	43.397543
3501.218785	821903.466001	43.402548
3501.769751	821903.282645	43.407553
3501.802519	821884.205627	43.412557
3501.764651	821871.756426	43.417562
3501.210363	821863.961333	43.422567
3501.226687	821874.273335	43.427572
3501.725923	821869.135442	43.432577
3501.280045	821877.087031	43.437581
3502.028633	821861.984908	43.442586
3501.984793	821846.617394	43.447591
3501.561551	821853.884328	43.452596
3501.495466	821834.044154	43.457601
3501.711004	821842.865463	43.462605
3501.374925	821830.560102	43.467610
3501.734465	821813.669844	43.472615
3501.488097	821813.416513	43.477620
3501.581668	821812.623506	43.482625
3501.220167	821820.561977	43.487629
3501.052845	821805.602893	43.492634
3501.614151	821812.715968	43.497639
3501.500547	821806.603444	43.502644
3501.911807	821807.804228	43.507649
3501.475126	821794.736063	43.512653
3501.461746	821777.028233	43.517658
3501.713625	821778.740477	43.522663
3501.387979	821779.667230	43.527668
3501.744015	821770.659329	43.532673
3501.534909	821764.950924	43.537677
3501.407080	821749.693606	43.542682
3501.206762	821750.016922	43.547687
3501.671255	821758.410202	43.552692
3501.702793	821757.529577	43.557697
3501.346110	821754.958092	43.562701
3502.053646	821745.895207	43.567706
3502.016610	821726.536688	43.572711
3501.866474	821723.543667	43.577716
3501.915301	821727.428458	43.582721
3501.845812	821712.648471	43.587725
3501.936823	821694.242923	43.592730
3501.993288	821685.476345	43.597735
3501.875980	821694.641826	43.602740
3501.586888	821665.299667	43.607745
3501.641794	821662.274564	43.612749
3501.907767	821655.907934	43.617754
3501.855175	821650.174956	43.622759
3501.546495	821636.405275	43.627764
3501.924785	821620.484659	43.632769
3501.895066	821622.338278	43.637773
3501.897322	821610.952691	43.642778
3501.808159	821597.051297	43.647783
3501.479168	821589.804498	43.652788
3501.787405	821580.219927	43.657793
3501.840452	821592.278257	43.662797
3501.656278	821573.428811	43.667802
3501.780373	821550.054795	43.672807
3501.346400	821553.431300	43.677812
3501.546786	821557.584440	43.682817
3501.474902	821559.833914	43.687821
3501.067893	821559.119126	43.692826
3501.163888	821563.093958	43.697831
3501.161230	821560.661671	43.702836
3501.236686	821554.130096	43.707841
3501.315386	821560.345795	43.712845
3501.487649	821561.292056	43.717850
3501.705145	821551.332381	43.722855
3501.443541	821531.716420	43.727860
3501.981392	821530.659303	43.732865
3501.436226	821535.220939	43.737869
3501.801345	821527.281693	43.742874
3501.876418	821514.522179	43.747879
3501.589206	821504.154765	43.752884
3501.776682	821494.783564	43.757889
3501.512528	821502.123351	43.762893
3501.927536	821494.078951	43.767898
3501.502670	821469.622697	43.772903
3501.606145	821474.374919	43.777908
3501.972622	821468.965513	43.782913
3501.438384	821475.277113	43.787917
3501.549001	821478.860464	43.792922
3501.742883	821476.786670	43.797927
3501.570324	821451.317776	43.802932
3501.817733	821454.977071	43.807937
3501.533188	821449.766729	43.812941
3501.656822	821454.418502	43.817946
3501.816132	821435.806880	43.822951
3501.546903	821413.953532	43.827956
3501.866940	821410.497605	43.832961
3501.619260	821410.244460	43.837965
3501.414138	821404.437783	43.842970
3501.747771	821406.137353	43.847975
3501.324266	821381.583223	43.852980
3501.363580	821376.516821	43.857985
3501.314428	821382.266114	43.862989
3501.368657	821374.472585	43.867994
3502.126749	821378.830608	43.872999
3501.898357	821374.973822	43.878004
3502.071703	821359.765772	43.883009
3501.824266	821359.901844	43.888013
3501.971428	821345.476367	43.893018
3501.502736	821333.482684	43.898023
3501.922071	821320.279695	43.903028
3502.144616	821315.087285	43.908033
3501.822264	821326.037037	43.913037
3501.695410	821307.080500	43.918042
3501.801279	821296.553973	43.923047
3501.489344	821284.049112	43.928052
3501.639988	821287.139740	43.933057
3501.566265	821282.577509	43.938061
3501.419631	821274.328674	43.943066
3501.687514	821251.028364	43.948071
3501.398688	821253.506495	43.953076
3501.639730	821259.405171	43.958081
3501.646784	821261.155834	43.963085
3502.027003	821261.485739	43.968090
3501.846571	821240.396422	43.973095
3501.519178	821240.447678	43.978100
3501.862446	821222.877137	43.983105
3501.709718	821239.931466	43.988109
3501.749642	821203.918165	43.993114
3501.874360	821192.415345	43.998119
3501.669571	821194.685727	44.003124
3501.911980	821193.480107	44.008129
3501.713123	821189.132002	44.013133
3501.628923	821167.054219	44.018138
3501.753833	821156.913747	44.023143
3501.803047	821163.523726	44.028148
3502.190317	821155.872494	44.033153
3501.774043	821138.712400	44.038157
3501.822833	821130.432824	44.043162
3501.665948	821124.326387	44.048167
3501.527613	821125.710543	44.053172
3501.537551	821105.953459	44.058177
3501.392470	821100.721020	44.063181
3501.225825	821090.528696	44.068186
3502.009228	821090.600949	44.073191
3501.643594	821103.309596	44.078196
3501.930798	821093.824879	44.083201
3502.015872	821088.167176	44.088205
3501.783073	821068.642556	44.093210
3501.952037	821064.820779	44.098215
3501.965746	821066.375818	44.103220
3501.690163	821034.498247	44.108225
3501.773240	821034.582658	44.113229
3501.735028	821028.068296	44.118234
3501.547110	821014.083704	44.123239
3501.422391	820998.726720	44.128244
3501.388075	820980.922556	44.133249
3501.505778	820991.317507	44.138253
3501.502092	820997.935933	44.143258
3501.421950	821000.089581	44.148263
3501.181022	821001.197842	44.153268
3501.449226	820998.236391	44.158273
3501.451909	820999.111930	44.163277
3501.534309	820996.179523	44.168282
3501.866465	820964.985151	44.173287
3501.575507	820961.235206	44.178292
3501.799366	820953.414628	44.183297
3501.849021	820955.645323	44.188301
3501.310171	820958.941219	44.193306
3501.387628	820943.163209	44.198311
3501.574122	820945.372516	44.203316
3501.917915	820938.117097	44.208321
3501.468933	820940.036460	44.213325
3501.613373	820928.432745	44.218330
3501.639764	820925.606381	44.223335
3501.337152	820918.062701	44.228340
3501.645927	820904.778788	44.233345
3501.305857	820902.204342	44.238349
3501.409727	820900.047107	44.243354
3501.686622	820902.436941	44.248359
3501.615664	820901.085608	44.253364
3501.392615	820898.784833	44.258369
3501.234084	820887.228401	44.263373
3501.204618	820878.960721	44.268378
3501.634102	820868.188232	44.273383
3501.345809	820873.099482	44.278388
3501.839213	820870.881344	44.283393
3501.981305	820877.087823	44.288397
3501.577693	820878.318858	44.293402
3501.945931	820859.770163	44.298407
3501.864293	820851.802569	44.303412
3501.831970	820832.635152	44.308417
3501.570629	820844.841411	44.313421
3501.422891	820823.064297	44.318426
3501.847909	820810.735241	44.323431
3501.468928	820809.918654	44.328436
3501.624970	820806.585353	44.333441
3501.781343	820813.081633	44.338445
3502.040227	820804.282162	44.343450
3501.432371	820784.717948	44.348455
3501.751329	820791.286159	44.353460
3501.605916	820777.099739	44.358465
3501.510036	820778.380011	44.363469
3501.586026	820773.404705	44.368474
3501.837002	820753.316843	44.373479
3501.745502	820745.837274	44.378484
3501.714909	820746.815375	44.383489
3501.724000	820752.361501	44.388493
3501.961817	820726.241518	44.393498
3501.870956	820710.489226	44.398503
3501.755881	820720.434399	44.403508
3501.751929	820699.607617	44.408513
3501.793724	820690.452621	44.413517
3501.917377	820674.958680	44.418522
3501.925163	820672.621735	44.423527
3501.916820	820671.941840	44.428532
3501.918116	820648.486283	44.433537
3501.661553	820642.394950	44.438541
3501.744006	820634.109446	44.443546
3501.834075	820637.696500	44.448551
3501.325603	820623.079849	44.453556
3501.755087	820613.182852	44.458561
3501.787062	820613.177932	44.463565
3501.731458	820608.223064	44.468570
3501.743235	820597.904708	44.473575
3501.706045	820589.345868	44.478580
3501.833340	820574.435065	44.483585
3501.584587	820579.827000	44.488589
3501.627357	820567.849195	44.493594
3501.732061	820557.029610	44.498599
3501.631335	820546.144791	44.503604
3501.907079	820532.475936	44.508609
3501.482144	820532.639767	44.513613
3501.622929	820533.591112	44.518618
3501.678485	820510.905170	44.523623
3501.554925	820503.722301	44.528628
3501.296708	820500.064282	44.533633
3501.659976	820497.574374	44.538637
3501.552635	820496.423295	44.543642
3501.635660	820500.108858	44.548647
3501.487368	820499.548149	44.553652
3501.630611	820469.354089	44.558657
3501.556931	820470.825611	44.563661
3501.781949	820469.427915	44.568666
3501.434641	820468.217015	44.573671
3501.404478	820477.954647	44.578676
3502.025398	820471.628646	44.583681
3501.374407	820452.654089	44.588685
3501.761684	820437.118342	44.593690
3502.118249	820434.921443	44.598695
3501.320389	820439.523376	44.603700
3501.461377	820431.325779	44.608705
3501.668093	820417.570131	44.613709
3501.618789	820428.868101	44.618714
3502.115066	820420.030976	44.623719
3501.983335	820423.068851	44.628724
3502.098064	820393.073534	44.633729
3501.591773	820383.711773	44.638733
3501.754510	820388.844889	44.643738
3501.776689	820371.711445	44.648743
3501.675614	820370.267373	44.653748
3501.614583	820351.686931	44.658753
3501.785738	820342.608529	44.663757
3501.654689	820343.407736	44.668762
3501.833558	820344.255826	44.673767
3501.838104	820326.541031	44.678772
3502.041275	820312.883036	44.683777
3501.612940	820313.728719	44.688781
3501.418408	820308.600666	44.693786
3501.710335	820287.044925	44.698791
3501.464941	820284.844742	44.703796
3501.503092	820277.733663	44.708801
3501.493046	820279.584609	44.713805
3501.684980	820283.155945	44.718810
3501.537807	820280.356418	44.723815
3501.507356	820286.298471	44.728820
3501.463579	820257.689913	44.733825
3501.747189	820247.523143	44.738829
3501.634065	820248.319559	44.743834
3501.852193	820239.720323	44.748839
3501.569685	820239.180571	44.753844
3501.445207	820226.838921	44.758849
3501.813774	820219.870789	44.763853
3501.511937	820215.148762	44.768858
3501.944869	820207.099896	44.773863
3501.331944	820207.293120	44.778868
3501.482789	820202.986982	44.783873
3501.239212	820180.541254	44.788877
3501.061629	820180.861091	44.793882
3501.869182	820171.098957	44.798887
3501.926599	820183.159358	44.803892
3501.492391	820178.263329	44.808897
3501.445911	820183.039989	44.813901
3502.008541	820175.262807	44.818906
3501.565457	820156.644169	44.823911
3501.770904	820150.674792	44.828916
3502.018756	820146.450784	44.833921
3501.693941	820142.218961	44.838925
3501.624645	820131.425832	44.843930
3501.964073	820117.162102	44.848935
3501.238750	820110.462180	44.853940
3501.774363	820111.254537	44.858945
3501.722987	820104.838593	44.863949
3501.541928	820082.382735	44.868954
3501.829123	820081.656576	44.873959
3501.287560	820079.015944	44.878964
3501.613286	820068.550293	44.883969
3501.952159	820075.505496	44.888973
3501.469786	820048.035212	44.893978
3501.594349	820046.458456	44.898983
3501.596405	820041.591455	44.903988
3501.704549	820040.503940	44.908993
3501.669042	820049.561736	44.913997
3501.525524	820035.957325	44.919002
3501.680271	820015.103429	44.924007
3501.335255	820005.813215	44.929012
3501.867668	819999.889917	44.934017
3501.156566	820005.841303	44.939021
3501.530759	820006.853580	44.944026
3501.881054	820006.701563	44.949031
3501.359081	819990.236139	44.954036
3501.314766	819967.077135	44.959041
3501.389582	819969.693598	44.964045
3501.541238	819980.376954	44.969050
3501.816635	819973.520447	44.974055
3501.665471	819980.455026	44.979060
3501.367377	819972.617469	44.984065
3501.565965	819975.993272	44.989069
3501.413514	819957.523272	44.994074
3501.657577	819953.007716	44.999079
3501.564078	819954.774468	45.004084
3501.638372	819944.445249	45.009089
3501.499254	819951.767323	45.014093
3501.484743	819950.309620	45.019098
3501.329233	819930.087957	45.024103
3501.273923	819923.672439	45.029108
3501.442745	819915.761821	45.034113
3501.625883	819921.184149	45.039117
3501.462104	819913.130846	45.044122
3501.807109	819907.820781	45.049127
3501.604497	819919.727669	45.054132
3501.895681	819913.647325	45.059137
3501.452062	819896.974729	45.064141
3501.495936	819898.525348	45.069146
3501.984877	819889.493943	45.074151
3501.465117	819894.831497	45.079156
3501.817457	819889.714945	45.084161
3501.669433	819865.014368	45.089165
3501.546260	819859.680110	45.094170
3501.286634	819857.092645	45.099175
3501.311658	819861.371686	45.104180
3501.811953	819865.479090	45.109185
3501.618533	819865.996093	45.114189
3501.458659	819838.766477	45.119194
3501.786329	819827.034717	45.124199
3501.493958	819828.735254	45.129204
3501.579619	819819.280096	45.134209
3501.593766	819819.083285	45.139213
3501.348804	819823.015201	45.144218
3501.474149	819816.376655	45.149223
3501.474330	819792.528670	45.154228
3501.735532	819796.576157	45.159233
3501.571410	819790.956224	45.164237
3501.546403	819792.128280	45.169242
3501.534852	819793.492911	45.174247
3501.563963	819791.346977	45.179252
3501.389902	819766.260720	45.184257
3501.619679	819766.711576	45.189261
3501.418643	819757.106461	45.194266
3501.700339	819766.504444	45.199271
3501.376205	819762.661609	45.204276
3501.664908	819759.793708	45.209281
3501.503106	819766.146151	45.214285
3501.566529	819746.960399	45.219290
3501.547178	819727.203486	45.224295
3501.471307	819733.931890	45.229300
3501.660336	819726.699252	45.234305
3501.332889	819732.104222	45.239309
3501.229721	819735.722008	45.244314
3501.489763	819734.221336	45.249319
3501.495371	819723.999826	45.254324
3501.723891	819718.221108	45.259329
3501.410696	819704.739832	45.264333
3501.462102	819704.342512	45.269338
3501.440982	819704.735253	45.274343
3501.188110	819700.881240	45.279348
3501.400887	819699.485288	45.284353
3500.990724	819696.337243	45.289357
3501.206319	819694.551488	45.294362
3501.648762	819694.579743	45.299367
3501.090820	819701.967583	45.304372
3501.308604	819696.677225	45.309377
3501.279216	819707.486696	45.314381
3501.134036	819705.075957	45.319386
3501.625005	819706.848754	45.324391
3501.473480	819685.652264	45.329396
3501.484091	819675.916596	45.334401
3501.589898	819679.501748	45.339405
3501.104499	819668.578175	45.344410
3501.473982	819667.644425	45.349415
3501.334911	819676.621614	45.354420
3501.428295	819667.457040	45.359425
3501.481727	819680.492455	45.364429
3501.583475	819662.468540	45.369434
3501.731613	819645.216054	45.374439
3501.726190	819639.571174	45.379444
3501.517374	819637.657064	45.384449
3501.714066	819642.201445	45.389453
3501.731668	819636.844988	45.394458
3501.878448	819617.061754	45.399463
3501.647089	819619.142177	45.404468
3502.209523	819613.505848	45.409473
3501.699536	819608.913233	45.414477
3501.628504	819585.854320	45.419482
3501.674724	819573.971394	45.424487
3501.636693	819581.083418	45.429492
3501.670131	819574.653665	45.434497
3501.438629	819574.397904	45.439501
3501.552227	819558.902741	45.444506
3501.673401	819545.742588	45.449511
3501.356650	819542.871890	45.454516
3501.757324	819537.260779	45.459521
3501.455088	819543.830088	45.464525
3501.629732	819542.634749	45.469530
3501.625034	819539.909956	45.474535
3501.557456	819512.567132	45.479540
3501.502723	819511.115613	45.484545
3501.526486	819513.545564	45.489549
3501.431480	819515.702050	45.494554
3501.546229	819515.392159	45.499559
3501.735599	819507.477809	45.504564
3501.856055	819484.388584	45.509569
3501.816383	819480.793136	45.514573
3501.884554	819473.968473	45.519578
3501.809610	819476.219180	45.524583
3501.589355	819449.970732	45.529588
3502.075426	819444.930255	45.534593
3501.858110	819442.530689	45.539597
3501.727021	819435.542443	45.544602
3501.915972	819410.105961	45.549607
3501.871491	819406.511221	45.554612
3501.628190	819401.000655	45.559617
3501.819682	819408.076998	45.564621
3501.591157	819393.121628	45.569626
3501.844850	819378.090841	45.574631
3501.516585	819376.390012	45.579636
3501.253703	819375.944456	45.584641
3501.474488	819380.387919	45.589645
3501.331095	819388.392745	45.594650
3501.699326	819376.848485	45.599655
3501.403536	819349.540616	45.604660
3501.333650	819346.047159	45.609665
3501.688751	819348.522725	45.614669
3501.440539	819347.588143	45.619674
3501.716228	819340.146817	45.624679
3501.386402	819345.941877	45.629684
3501.241620	819333.991003	45.634689
3501.302298	819338.654216	45.639693
3501.650355	819342.104349	45.644698
3501.498930	819318.083543	45.649703
3501.287395	819316.364450	45.654708
3501.524221	819310.584055	45.659713
3501.696580	819311.335963	45.664717
3501.670653	819309.977240	45.669722
3501.659060	819305.306487	45.674727
3501.361262	819294.255576	45.679732
3501.753788	819276.087736	45.684737
3501.647997	819279.706198	45.689741
3501.371998	819281.014933	45.694746
3501.301388	819272.848883	45.699751
3501.629568	819284.576668	45.704756
3501.795813	819279.196666	45.709761
3501.548689	819259.473867	45.714765
3501.411335	819251.902307	45.719770
3501.394496	819247.232331	45.724775
3500.908360	819244.777362	45.729780
3501.074944	819239.591967	45.734785
3500.922712	819246.040794	45.739789
3501.201889	819247.360098	45.744794
3501.432441	819248.881698	45.749799
3501.074152	819252.150256	45.754804
3501.244423	819251.831674	45.759809
3501.279304	819259.127365	45.764813
3500.927163	819236.111091	45.769818
3501.422945	819187.164852	45.774823
3501.142251	819079.832349	45.779828
3500.968226	818932.274806	45.784833
3500.910195	818745.948229	45.789837
3500.533638	818486.743918	45.794842
3500.438101	818183.086845	45.799847
3500.315264	817843.976716	45.804852
3500.209471	817436.682529	45.809857
3499.530448	816992.056294	45.814861
3499.027010	816497.896518	45.819866
3498.887347	815951.142658	45.824871
3498.249579	815361.948763	45.829876
3497.637315	814724.375908	45.834881
3497.162957	814044.432405	45.839885
3496.215813	813302.029857	45.844890
3495.787014	812524.862763	45.849895
3494.688897	811700.628498	45.854900
3493.830502	810822.732990	45.859905
3493.370883	809908.775466	45.864909
3492.201777	808942.434961	45.869914
3491.632037	807933.137952	45.874919
3490.720198	806883.303668	45.879924
3489.492813	805773.933473	45.884929
3488.824742	804634.376159	45.889933
3487.791170	803436.410141	45.894938
3486.639840	802188.114982	45.899943
3485.216489	800897.296543	45.904948
3484.396509	799568.577989	45.909953
3482.860286	798196.722247	45.914957
3481.836851	796776.674724	45.919962
3480.393916	795309.234534	45.924967
3478.911284	793804.964701	45.929972
3477.717420	792253.817940	45.934977
3476.132980	790665.646907	45.939981
3475.115926	789028.441426	45.944986
3473.215224	787349.094966	45.949991
3471.504124	785631.519239	45.954996
3470.049526	783877.388837	45.960001
3468.259934	782087.013993	45.965005
3466.475706	780251.010182	45.970010
3465.142247	778384.995851	45.975015
3463.048755	776469.245078	45.980020
3461.262999	774527.223057	45.985025
3459.286864	772550.849554	45.990029
3457.911338	770536.688017	45.995034
3455.959721	768480.820443	46.000039
3453.938268	766398.638812	46.005044
3451.363816	764267.963071	46.010049
3449.468691	762112.470210	46.015053
3447.129558	759921.265616	46.020058
3445.243692	757704.594438	46.025063
3442.640606	755459.424866	46.030068
3440.543238	753170.400692	46.035073
3438.305500	750860.697768	46.040077
3436.105464	748522.007873	46.045082
3433.919919	746152.686655	46.050087
3430.914265	743756.284584	46.055092
3428.982684	741324.062812	46.060097
3427.260113	738869.770138	46.065101
3424.510139	736370.472763	46.070106
3421.586325	733845.860946	46.075111
3419.092383	731302.279061	46.080116
3416.968406	728722.310709	46.085121
3414.175451	726125.132505	46.090125
3411.860691	723495.300914	46.095130
3409.270754	720837.497736	46.100135
3406.283747	718168.364444	46.105140
3403.610130	715462.387112	46.110145
3401.265336	712722.743884	46.115149
3398.080546	709967.339491	46.120154
3395.680580	707192.397930	46.125159
3392.989915	704390.898974	46.130164
3389.991958	701564.605915	46.135169
3387.223346	698713.118518	46.140173
3384.368916	695841.221732	46.145178
3382.342803	692945.636663	46.150183
3378.813399	690033.203703	46.155188
3376.040961	687093.889847	46.160193
3372.952161	684128.784708	46.165197
3369.958702	681137.407438	46.170202
3367.017338	678135.480338	46.175207
3363.573338	675130.088673	46.180212
3361.154845	672080.315669	46.185217
3358.136467	669029.409412	46.190221
3354.955842	665949.422433	46.195226
3352.125332	662846.319227	46.200231
3349.077910	659733.504294	46.205236
3345.858184	656583.800051	46.210241
3342.663099	653427.809566	46.215245
3339.846588	650246.757119	46.220250
3336.363113	647058.323732	46.225255
3332.899021	643856.673437	46.230260
3329.741622	640644.449075	46.235265
3326.533287	637410.286466	46.240269
3323.297708	634166.190724	46.245274
3320.257698	630881.339298	46.250279
3317.106248	627602.120510	46.255284
3313.651650	624309.406226	46.260289
3310.349646	621010.364530	46.265293
3306.922758	617682.757974	46.270298
3304.179591	614335.239031	46.275303
3300.063211	610989.120054	46.280308
3296.797577	607629.560698	46.285313
3293.363901	604251.814812	46.290317
3290.030571	600879.656707	46.295322
3286.847788	597470.289584	46.300327
3283.230446	594072.909445	46.305332
3279.807377	590654.777465	46.310337
3276.076082	587223.881497	46.315341
3272.637950	583795.315677	46.320346
3268.906359	580344.564568	46.325351
3265.432810	576898.267763	46.330356
3262.290954	573428.682610	46.335361
3258.795277	569953.774295	46.340365
3254.346781	566474.848182	46.345370
3251.524951	562987.390825	46.350375
3247.776199	559492.157452	46.355380
3244.407723	555988.144439	46.360385
3240.885649	552479.963273	46.365389
3236.605320	548962.889893	46.370394
3233.550990	545446.626658	46.375399
3229.552234	541922.923027	46.380404
3226.133099	538386.161775	46.385409
3222.604210	534842.240482	46.390413
3218.937919	531308.943078	46.395418
3215.554689	527752.581738	46.400423
3211.562757	524193.893494	46.405428
3207.801697	520630.136991	46.410433
3203.989361	517061.868561	46.415437
3200.344568	513490.373473	46.420442
3197.022651	509918.209073	46.425447
3193.355185	506345.441150	46.430452
3189.487660	502766.458126	46.435457
3186.144470	499174.744892	46.440461
3181.894326	495587.640819	46.445466
3178.570576	491986.344215	46.450471
3174.639349	488395.389524	46.455476
3171.202486	484783.506249	46.460481
3167.176963	481176.681031	46.465485
3163.586867	477569.058622	46.470490
3159.775294	473956.254560	46.475495
3155.901490	470351.297702	46.480500
3152.295868	466731.901825	46.485505
3148.451893	463118.433113	46.490509
3144.785334	459498.447015	46.495514
3141.239776	455878.336781	46.500519
3136.992977	452256.674142	46.505524
3133.439920	448632.037239	46.510529
3129.600612	445006.260852	46.515533
3125.657595	441379.733197	46.520538
3122.253935	437762.344683	46.525543
3118.216586	434141.021991	46.530548
3114.169231	430522.569229	46.535553
3110.506100	426885.955451	46.540557
3106.720495	423275.669144	46.545562
3102.870782	419650.861791	46.550567
3098.928602	416039.483749	46.555572
3095.302340	412411.312302	46.560577
3091.616973	408794.360532	46.565581
3087.455120	405176.737685	46.570586
3083.577851	401552.653101	46.575591
3079.633838	397936.787169	46.580596
3075.706475	394338.482353	46.585601
3071.843733	390728.052304	46.590605
3067.924224	387126.822268	46.595610
3064.292374	383524.216999	46.600615
3060.290861	379925.403934	46.605620
3056.261218	376331.714405	46.610625
3052.810306	372735.929543	46.615629
3048.502438	369152.688957	46.620634
3044.858543	365562.461413	46.625639
3040.527400	361987.167850	46.630644
3036.540417	358399.420411	46.635649
3032.603933	354832.999909	46.640653
3028.818846	351267.395784	46.645658
3025.134149	347702.627579	46.650663
3021.031939	344146.898357	46.655668
3017.113252	340588.736635	46.660673
3013.377409	337042.546338	46.665677
3009.191011	333492.240683	46.670682
3005.215576	329952.580023	46.675687
3001.218305	326420.282453	46.680692
2996.915571	322882.227670	46.685697
2993.065779	319363.188176	46.690701
2989.060424	315855.794280	46.695706
2985.310697	312344.575233	46.700711
2981.059912	308857.218487	46.705716
2976.865885	305358.609247	46.710721
2973.009044	301876.885748	46.715725
2969.194881	298409.409895	46.720730
2964.876937	294937.367913	46.725735
2960.785406	291501.587215	46.730740
2957.127135	288045.537798	46.735745
2953.358806	284600.777571	46.740749
2949.087860	281163.153466	46.745754
2945.264363	277726.493787	46.750759
2940.674816	274311.673150	46.755764
2936.851148	270913.397482	46.760769
2932.851667	267509.876152	46.765773
2928.605656	264131.075328	46.770778
2924.639070	260743.361707	46.775783
2919.946530	257386.347755	46.780788
2916.326834	254024.900423	46.785793
2911.761214	250689.064402	46.790797
2907.403931	247351.470663	46.795802
2903.672710	244035.366038	46.800807
2899.468791	240726.084346	46.805812
2895.283194	237443.168754	46.810817
2891.261234	234161.595715	46.815821
2886.933043	230904.089288	46.820826
2882.998131	227633.618850	46.825831
2878.608972	224396.780931	46.830836
2874.104862	221162.025667	46.835841
2870.172773	217947.744308	46.840845
2865.914200	214755.435069	46.845850
2862.005802	211567.477308	46.850855
2857.804528	208397.859560	46.855860
2853.507747	205247.169332	46.860865
2849.499096	202093.400560	46.865869
2845.056698	198969.882855	46.870874
2840.736385	195836.705588	46.875879
2836.836032	192747.537695	46.880884
2832.443987	189664.404545	46.885889
2828.050656	186592.863804	46.890893
2823.738126	183528.910965	46.895898
2819.339779	180489.791351	46.900903
2815.481800	177470.497354	46.905908
2811.051647	174469.476332	46.910913
2807.043426	171485.737284	46.915917
2802.962685	168433.195772	46.920922
2798.860764	165445.055356	46.925927
2794.628478	162507.304712	46.930932
2790.674986	159573.613671	46.935937
2786.339317	156652.605771	46.940941
2782.132702	153755.761131	46.945946
2777.975243	150864.451095	46.950951
2773.580755	147983.650194	46.955956
2769.395630	145138.678359	46.960961
2765.248005	142288.604124	46.965965
2760.971446	139467.825233	46.970970
2757.204108	136661.751525	46.975975
2752.764597	133875.074010	46.980980
2748.706510	131093.280650	46.985985
2744.472418	128331.396236	46.990989
2740.131666	125580.393419	46.995994
2736.047257	122854.679072	47.000999
2731.868886	120143.154725	47.006004
2727.625417	117439.434188	47.011009
2723.574897	114750.283180	47.016013
2718.992147	112083.661728	47.021018
2715.055559	109431.655377	47.026023
2710.839982	106801.147921	47.031028
2706.563280	104189.651574	47.036033
2702.605770	101582.006504	47.041037
2698.253832	98996.274004	47.046042
2694.364200	96420.398379	47.051047
2690.290487	93871.968386	47.056052
2686.282480	91326.329588	47.061057
2681.882406	88803.174432	47.066061
2677.596230	86298.648913	47.071066
2673.670447	83801.560055	47.076071
2669.335820	81326.637803	47.081076
2665.088550	78859.043780	47.086081
2660.830751	76412.777904	47.091085
2656.736109	73995.277982	47.096090
2652.364240	71581.162335	47.101095
2648.074307	69193.891585	47.106100
2643.644548	66822.203882	47.111105
2639.867030	64464.533598	47.116109
2635.366589	62138.230931	47.121114
2631.464136	59817.014487	47.126119
2627.416799	57516.262771	47.131124
2622.887467	55225.087417	47.136129
2618.704432	52960.627988	47.141133
2614.245002	50707.575006	47.146138
2610.354523	48476.667648	47.151143
2605.972205	46269.013220	47.156148
2601.280181	44072.504615	47.161153
2596.989820	41887.530946	47.166157
2592.584350	39734.835841	47.171162
2588.391901	37595.360521	47.176167
2584.064877	35493.196241	47.181172
2579.435111	33410.042165	47.186177
2575.214600	31339.642146	47.191181
2570.650010	29294.457648	47.196186
2566.567647	27269.005970	47.201191
2561.953177	25283.274052	47.206196
2557.554262	23294.332783	47.211201
2553.035684	21331.181492	47.216205
2548.756504	19407.484632	47.221210
2544.040996	17506.750417	47.226215
2539.835692	15628.753042	47.231220
2534.858785	13774.283328	47.236225
2529.925376	11950.452196	47.241229
2524.779758	10169.001935	47.246234
2518.832994	8440.842635	47.251239
2510.185707	6823.339219	47.256244
2499.968174	5308.713856	47.261249
2489.846256	3883.722814	47.266253
2479.963114	2566.942175	47.271258
2470.433977	1357.179248	47.276263
2459.652947	312.743746	47.281268
2420.238787	145.804237	47.286273
2384.105473	204.920102	47.291277
2368.343445	222.354331	47.296282
2366.856487	228.456027	47.301287
2372.608448	235.310919	47.306292
2381.340463	239.421616	47.311297
2388.652540	235.715036	47.316301
2392.935731	239.022045	47.321306
2394.324806	217.398006	47.326311
2392.640816	228.152950	47.331316
2389.971446	218.411413	47.336321
2386.107478	215.032654	47.341325
2382.522175	218.045628	47.346330
2379.497305	214.431194	47.351335
2376.249196	215.385520	47.356340
2373.198806	208.282162	47.361345
2370.497132	215.001011	47.366349
2367.651295	210.539128	47.371354
2364.684758	207.029474	47.376359
2362.094250	211.307404	47.381364
2358.856043	211.212943	47.386369
2355.837836	211.432092	47.391373
2352.561537	203.484527	47.396378
2349.238988	203.048910	47.401383
2345.626728	208.230201	47.406388
2342.383932	205.649658	47.411393
2339.352128	204.001089	47.416397
2336.003219	200.257025	47.421402
2333.523990	202.315493	47.426407
2329.728579	205.348696	47.431412
2326.151356	204.481512	47.436417
2323.590455	204.293755	47.441421
2319.818044	200.739343	47.446426
2316.691527	205.107465	47.451431
2313.030927	209.957793	47.456436
2309.476701	207.052646	47.461441
2306.294364	203.564115	47.466445
2302.995618	206.421544	47.471450
2299.882853	204.605312	47.476455
2296.569827	204.968681	47.481460
2293.123910	196.917959	47.486465
2289.462244	196.016541	47.491469
2285.468083	203.155918	47.496474
2282.588470	199.044210	47.501479
2279.400037	202.463375	47.506484
2276.305113	202.966640	47.511489
2273.356580	197.198358	47.516493
2269.376948	198.441175	47.521498
2265.985508	192.963661	47.526503
2262.192464	191.029238	47.531508
2258.684074	196.630913	47.536513
2255.315303	195.620405	47.541517
2252.100593	210.307069	47.546522
2249.112142	196.518298	47.551527
2245.053248	203.569735	47.556532
2241.087561	196.188834	47.561537
2238.327095	191.878159	47.566541
2234.898402	193.329031	47.571546
2231.391725	186.847631	47.576551
2227.896762	200.872597	47.581556
2224.241231	195.120028	47.586561
2221.114260	197.086867	47.591565
2217.617231	207.767953	47.596570
2214.539265	196.517970	47.601575
2210.771481	192.292136	47.606580
2207.491407	198.902181	47.611585
2204.374479	193.849992	47.616589
2200.348091	196.574511	47.621594
2196.883918	187.767358	47.626599
2193.628063	193.645925	47.631604
2190.260601	196.390744	47.636609
2186.825556	190.818838	47.641613
2182.945088	194.302007	47.646618
2179.419547	192.971190	47.651623
2176.382378	186.242339	47.656628
2172.529882	191.850417	47.661633
2169.635355	191.521899	47.666637
2165.718190	193.545946	47.671642
2162.406340	188.739413	47.676647
2158.924142	185.541468	47.681652
2155.208710	194.371069	47.686657
2152.162103	182.046825	47.691661
2148.453994	199.015910	47.696666
2144.942413	184.340896	47.701671
2141.238498	196.642624	47.706676
2137.604504	195.433196	47.711681
2134.773827	191.949815	47.716685
2130.876404	189.588831	47.721690
2127.487119	190.672888	47.726695
2124.005876	198.409126	47.731700
2120.638608	188.201067	47.736705
2117.404106	192.712686	47.741709
2113.565544	183.407307	47.746714
2110.511547	189.649793	47.751719
2106.883514	185.367332	47.756724
2103.054383	187.931301	47.761729
2100.136326	177.130933	47.766733
2096.728482	189.421143	47.771738
2092.698200	175.349358	47.776743
2088.988260	183.722517	47.781748
2085.567906	188.867521	47.786753
2082.269609	183.277422	47.791757
2078.617223	192.236388	47.796762
2075.435350	182.075275	47.801767
2071.840360	192.237021	47.806772
2068.193006	178.915278	47.811777
2065.528392	178.544487	47.816781
2061.512041	180.274029	47.821786
2057.643356	184.229974	47.826791
2054.643582	183.332641	47.831796
2051.225887	183.389748	47.836801
2047.600201	181.625377	47.841805
2043.594804	185.963398	47.846810
2040.360583	180.100689	47.851815
2037.105854	187.175057	47.856820
2033.428291	188.639620	47.861825
2030.219665	176.976715	47.866829
2026.746841	181.870507	47.871834
2023.017873	179.002300	47.876839
2019.420701	177.518225	47.881844
2015.573109	169.853190	47.886849
2012.776846	163.621400	47.891853
2009.428881	181.597198	47.896858
2005.823537	178.276204	47.901863
2002.039270	177.947746	47.906868
1998.355742	174.781363	47.911873
1995.400856	175.057144	47.916877
1991.670244	183.939781	47.921882
1988.241844	172.751062	47.926887
1984.793122	178.046068	47.931892
1981.206456	171.140673	47.936897
1978.192299	164.753158	47.941901
1973.775281	176.736213	47.946906
1970.812162	165.556960	47.951911
1967.193424	167.363527	47.956916
1963.646575	168.953196	47.961921
1960.387933	164.524405	47.966925
1956.777839	180.165173	47.971930
1953.227886	172.276412	47.976935
1949.729889	174.124205	47.981940
1946.344155	182.949723	47.986945
1942.982875	170.706448	47.991949
1939.096966	177.876440	47.996954
1935.943840	173.314081	48.001959
1932.598978	176.659732	48.006964
1928.745283	176.541488	48.011969
1925.294820	172.512895	48.016973
1921.664516	169.970985	48.021978
1918.021656	174.034008	48.026983
1914.751092	181.417776	48.031988
1910.976107	177.892401	48.036993
1908.279437	168.879847	48.041997
1904.214831	173.834638	48.047002
1900.953620	171.168537	48.052007
1897.217263	174.920321	48.057012
1893.964833	173.967657	48.062017
1890.525430	169.310904	48.067021
1887.004572	172.158908	48.072026
1883.490879	168.159210	48.077031
1879.755671	174.128682	48.082036
1876.202307	173.039613	48.087041
1872.919121	164.935130	48.092045
1869.063755	173.789860	48.097050
1866.076329	163.905305	48.102055
1862.618702	174.944132	48.107060
1858.865744	175.132862	48.112065
1855.421067	173.935040	48.117069
1851.445132	179.850442	48.122074
1848.266774	176.817039	48.127079
1844.863481	165.956661	48.132084
1841.221496	168.307926	48.137089
1838.184481	162.240422	48.142093
1834.270464	174.024577	48.147098
1831.103223	167.031461	48.152103
1827.482712	165.016417	48.157108
1823.859744	168.475224	48.162113
1820.475682	167.574822	48.167117
1817.223021	170.738392	48.172122
1813.685418	161.012726	48.177127
1809.957321	161.713291	48.182132
1806.367951	168.292731	48.187137
1803.052892	157.687495	48.192141
1799.048298	156.637431	48.197146
1795.871551	161.051502	48.202151
1792.185584	159.957904	48.207156
1788.665557	162.682418	48.212161
1785.240524	157.820971	48.217165
1781.990264	169.823975	48.222170
1778.515934	162.458146	48.227175
1775.390120	166.503574	48.232180
1771.163342	165.792020	48.237185
1767.467745	159.277099	48.242189
1764.439733	163.734343	48.247194
1761.204088	165.329159	48.252199
1757.602761	159.381636	48.257204
1754.069149	170.081191	48.262209
1750.547920	156.132414	48.267213
1746.329078	164.354341	48.272218
1743.455119	168.236972	48.277223
1739.833371	169.104421	48.282228
1736.464759	163.373594	48.287233
1732.681092	155.872694	48.292237
1729.372091	167.935522	48.297242
1726.055304	159.744605	48.302247
1722.318994	169.147073	48.307252
1719.002425	174.162034	48.312257
1715.789051	168.536636	48.317261
1712.051479	159.617452	48.322266
1708.826770	152.203098	48.327271
1705.213741	156.302646	48.332276
1701.446844	161.397579	48.337281
1697.845786	159.120103	48.342285
1694.074470	161.630866	48.347290
1690.894451	156.705799	48.352295
1687.263061	162.222467	48.357300
1683.767540	161.848935	48.362305
1680.688095	161.653902	48.367309
1676.732651	164.323206	48.372314
1673.472439	165.817487	48.377319
1670.221113	171.277844	48.382324
1666.462519	167.509550	48.387329
1663.314274	158.725952	48.392333
1659.249423	155.847179	48.397338
1656.005970	158.117147	48.402343
1652.722980	156.913074	48.407348
1648.799762	159.359039	48.412353
1645.465481	162.741081	48.417357
1641.847254	170.328026	48.422362
1638.318470	152.754717	48.427367
1634.422354	154.320059	48.432372
1631.123367	159.825850	48.437377
1627.985704	151.708184	48.442381
1624.624961	159.352909	48.447386
1621.013163	164.749470	48.452391
1617.319013	154.997771	48.457396
1613.550567	166.341570	48.462401
1610.384706	152.416338	48.467405
1607.228849	161.838721	48.472410
1604.077483	153.723208	48.477415
1600.148900	149.250702	48.482420
1596.123327	145.970330	48.487425
1592.828731	149.523350	48.492429
1589.303543	156.693934	48.497434
1585.859371	152.053865	48.502439
1582.560732	161.419505	48.507444
1578.804201	157.103580	48.512449
1575.767925	157.135947	48.517453
1571.690046	159.489085	48.522458
1568.280921	151.512009	48.527463
1564.778497	155.935985	48.532468
1561.087961	157.380591	48.537473
1558.030712	150.133079	48.542477
1554.085975	152.452728	48.547482
1551.288618	152.846351	48.552487
1547.390255	155.225185	48.557492
1543.625597	155.453827	48.562497
1540.185601	153.483405	48.567501
1536.866504	162.390337	48.572506
1533.608180	148.890913	48.577511
1529.928519	159.524790	48.582516
1526.186898	159.284747	48.587521
1523.085901	149.743982	48.592525
1518.951673	161.768334	48.597530
1515.823264	157.537623	48.602535
1512.641370	160.914836	48.607540
1509.120287	153.929771	48.612545
1505.961538	138.462692	48.617549
1501.971288	156.374562	48.622554
1498.627638	150.310883	48.627559
1494.896402	149.015668	48.632564
1490.843311	145.594112	48.637569
1487.299821	155.191091	48.642573
1484.311200	153.804952	48.647578
1481.257832	151.856294	48.652583
1477.396855	147.366933	48.657588
1474.041639	147.066428	48.662593
1470.556183	142.331625	48.667597
1466.778046	151.974828	48.672602
1463.374643	149.388085	48.677607
1459.989273	141.109939	48.682612
1456.246516	149.111902	48.687617
1453.421995	143.776927	48.692621
1449.516428	146.932065	48.697626
1445.594646	148.080704	48.702631
1442.294275	146.752869	48.707636
1438.553868	159.335712	48.712641
1435.321232	141.200455	48.717645
1431.629055	150.077218	48.722650
1428.252708	149.425687	48.727655
1424.672676	153.839707	48.732660
1421.357033	145.683542	48.737665
1418.063583	144.683671	48.742669
1414.320921	145.358183	48.747674
1410.718399	147.257312	48.752679
1407.689331	143.390754	48.757684
1404.024907	148.308385	48.762689
1400.659822	139.862569	48.767693
1396.776155	147.010223	48.772698
1393.538238	148.953528	48.777703
1389.792330	143.177494	48.782708
1385.982634	146.700471	48.787713
1382.590669	145.494565	48.792717
1379.402446	145.724787	48.797722
1375.879523	152.986828	48.802727
1372.309766	141.681315	48.807732
1368.230855	147.581352	48.812737
1365.142944	145.106615	48.817741
1361.674220	151.616674	48.822746
1358.237989	149.864034	48.827751
1354.960614	146.371728	48.832756
1351.462623	152.130215	48.837761
1347.567502	143.413041	48.842765
1344.180401	155.342636	48.847770
1341.002822	147.996979	48.852775
1337.023241	148.733918	48.857780
1333.619053	152.842023	48.862785
1330.581443	143.253448	48.867789
1326.777869	152.264744	48.872794
1323.404302	146.012824	48.877799
1319.682079	146.383607	48.882804
1316.118816	149.953457	48.887809
1312.699289	145.249524	48.892813
1309.203184	146.502426	48.897818
1306.205889	141.675451	48.902823
1302.425107	147.899010	48.907828
1298.750562	148.271829	48.912833
1295.205448	147.368346	48.917837
1291.367833	146.709975	48.922842
1288.049780	150.671728	48.927847
1284.782202	149.683672	48.932852
1281.372603	155.532750	48.937857
1278.206609	151.140326	48.942861
1274.345713	154.918138	48.947866
1270.513415	143.970153	48.952871
1266.904694	146.860583	48.957876
1263.058661	156.318320	48.962881
1259.759235	148.985441	48.967885
1256.786999	143.417386	48.972890
1253.620964	144.612308	48.977895
1250.190194	150.214766	48.982900
1246.652556	147.256802	48.987905
1242.986511	142.980640	48.992909
1239.001590	140.902644	48.997914
1235.617753	148.563740	49.002919
1232.435527	143.927096	49.007924
1228.702217	142.980331	49.012929
1224.935969	133.771634	49.017933
1221.326962	137.965621	49.022938
1217.851100	148.896712	49.027943
1214.637308	147.922406	49.032948
1210.927954	149.797200	49.037953
1207.903840	141.880229	49.042957
1204.330982	150.798494	49.047962
1200.630284	143.936596	49.052967
1197.321799	140.749784	49.057972
1193.672519	143.561165	49.062977
1190.311435	140.882475	49.067981
1186.461671	146.414502	49.072986
1183.289807	136.821696	49.077991
1179.634623	150.644137	49.082996
1175.945420	145.859088	49.088001
1172.585150	152.494597	49.093005
1168.612753	145.365193	49.098010
1165.905349	151.094880	49.103015
1162.375906	140.691172	49.108020
1158.777029	143.225749	49.113025
1155.424345	134.385782	49.118029
1151.627886	145.553746	49.123034
1147.838589	141.673416	49.128039
1144.441906	140.471498	49.133044
1140.960083	146.499606	49.138049
1137.814839	142.483646	49.143053
1133.948670	149.125600	49.148058
1130.665983	138.794010	49.153063
1127.368743	140.408156	49.158068
1123.445371	135.387704	49.163073
1120.285937	137.416885	49.168077
1116.694228	139.175216	49.173082
1113.127665	136.949515	49.178087
1109.852152	136.674623	49.183092
1106.214532	144.739328	49.188097
1102.998458	141.035034	49.193101
1098.909630	142.469396	49.198106
1095.937356	144.655948	49.203111
1092.137492	144.121464	49.208116
1088.548470	136.748577	49.213121
1084.958083	133.093404	49.218125
1081.358006	135.568082	49.223130
1077.616863	131.620133	49.228135
1074.626814	142.791579	49.233140
1070.946208	140.131322	49.238145
1067.548871	132.864479	49.243149
1064.115612	136.284339	49.248154
1060.496428	129.381273	49.253159
1057.025871	145.933691	49.258164
1053.449569	142.399713	49.263169
1049.917855	140.851967	49.268173
1046.485975	135.634372	49.273178
1043.078327	136.860863	49.278183
1039.500330	137.206008	49.283188
1036.075287	145.414625	49.288193
1032.779207	135.246532	49.293197
1028.705666	136.956946	49.298202
1025.663468	140.397850	49.303207
1022.303485	135.858722	49.308212
1018.494627	138.362948	49.313217
1015.023524	134.138621	49.318221
1011.341444	138.302991	49.323226
1008.007447	142.653313	49.328231
1005.056946	134.566706	49.333236
1000.745204	137.146513	49.338241
997.511445	134.609316	49.343245
993.801121	139.819012	49.348250
990.641060	146.246050	49.353255
986.985435	141.943054	49.358260
983.699038	142.467194	49.363265
979.869104	137.242347	49.368269
976.439600	138.690587	49.373274
972.901896	139.715998	49.378279
969.486598	133.689063	49.383284
965.809245	139.962979	49.388289
962.633980	140.577295	49.393293
958.708087	139.173564	49.398298
955.326762	135.539494	49.403303
951.776842	138.876416	49.408308
948.369588	146.794366	49.413313
945.090601	134.608279	49.418317
941.468350	139.367595	49.423322
938.217555	139.152169	49.428327
934.731918	142.156322	49.433332
930.940975	139.706393	49.438337
927.498819	140.944655	49.443341
923.309758	138.601360	49.448346
920.549382	137.768136	49.453351
917.137143	135.575297	49.458356
913.497511	143.754274	49.463361
909.977302	132.245067	49.468365
906.332238	145.509159	49.473370
902.842729	143.556219	49.478375
899.007081	143.324815	49.483380
895.712843	138.664708	49.488385
892.737052	130.101206	49.493389
888.785220	138.442972	49.498394
885.140129	136.137906	49.503399
881.992307	135.260956	49.508404
878.076025	139.740463	49.513409
874.749028	146.532202	49.518413
871.421180	139.615233	49.523418
868.232649	138.247942	49.528423
864.868310	139.439239	49.533428
860.771359	142.539142	49.538433
857.571024	131.495576	49.543437
854.043041	133.601534	49.548442
850.285264	132.491070	49.553447
846.883805	138.693349	49.558452
843.010251	140.103600	49.563457
840.017656	130.065245	49.568461
836.311676	139.665697	49.573466
832.733843	130.155596	49.578471
829.719090	131.981875	49.583476
825.875940	131.856083	49.588481
822.722142	129.258972	49.593485
819.041009	132.898066	49.598490
815.609196	131.904256	49.603495
811.888981	132.085091	49.608500
807.873153	137.121225	49.613505
804.778991	128.288387	49.618509
801.034996	123.423498	49.623514
797.703609	121.705274	49.628519
794.461949	130.676193	49.633524
790.575239	127.228901	49.638529
787.756054	128.708185	49.643533
783.681718	131.931130	49.648538
780.512633	136.236715	49.653543
776.818899	124.390913	49.658548
772.984329	137.554995	49.663553
770.013435	128.848403	49.668557
766.569366	131.200685	49.673562
762.634647	133.939858	49.678567
759.501080	131.203557	49.683572
755.657794	128.423373	49.688577
752.055077	125.877606	49.693581
748.650338	126.005900	49.698586
745.021218	130.851781	49.703591
741.698497	133.900091	49.708596
738.069829	137.230437	49.713601
734.779476	135.651344	49.718605
731.426637	131.642736	49.723610
728.016166	128.424618	49.728615
724.433236	130.371545	49.733620
720.796761	139.170195	49.738625
717.651959	128.329972	49.743629
713.518843	129.189289	49.748634
710.099528	134.793281	49.753639
706.611741	129.287185	49.758644
702.994207	127.550531	49.763649
700.013634	131.225493	49.768653
696.084069	134.441621	49.773658
692.730408	127.769225	49.778663
689.479185	122.631060	49.783668
685.898289	127.912342	49.788673
681.877077	122.467651	49.793677
678.465247	125.371746	49.798682
675.167015	131.168761	49.803687
671.827992	121.327105	49.808692
668.157251	130.795535	49.813697
664.801802	123.035081	49.818701
660.961776	128.553111	49.823706
657.392526	123.616627	49.828711
654.700452	127.372972	49.833716
650.641228	132.890534	49.838721
647.278605	126.286002	49.843725
643.450336	124.892430	49.848730
640.150335	122.027213	49.853735
636.765667	121.975232	49.858740
633.259991	122.075083	49.863745
630.242849	124.749699	49.868749
626.330587	129.244489	49.873754
622.667154	119.735243	49.878759
618.923953	124.804682	49.883764
615.059128	130.873953	49.888769
612.105003	118.706756	49.893773
608.637953	125.507847	49.898778
605.419407	124.044110	49.903783
601.625962	119.177566	49.908788
597.968380	124.268405	49.913793
594.443149	122.650220	49.918797
590.957615	133.022993	49.923802
587.682505	129.891301	49.928807
584.354838	127.808735	49.933812
580.628584	125.383630	49.938817
577.016488	122.915337	49.943821
573.753391	123.331565	49.948826
569.925661	128.407934	49.953831
566.426880	123.947679	49.958836
562.884222	130.751137	49.963841
559.755691	121.601078	49.968845
556.405283	122.891543	49.973850
552.648087	118.405330	49.978855
549.140241	118.477079	49.983860
545.091178	124.306306	49.988865
541.951266	119.543079	49.993869
538.468005	123.325294	49.998874
535.359711	121.809513	50.003879
532.133091	124.222734	50.008884
528.068440	130.503673	50.013889
524.678531	115.035313	50.018893
521.005954	118.508657	50.023898
517.434093	117.337577	50.028903
513.686707	114.495025	50.033908
510.001215	126.560136	50.038913
507.069558	116.892040	50.043917
503.634398	117.771848	50.048922
500.252603	115.738924	50.053927
496.853283	118.321578	50.058932
493.058576	130.005162	50.063937
489.493367	118.683554	50.068941
486.312197	116.872317	50.073946
482.685262	124.267976	50.078951
479.446049	116.144545	50.083956
475.321004	125.760123	50.088961
472.059727	114.678828	50.093965
468.308850	126.118267	50.098970
465.085901	117.340550	50.103975
461.794696	120.852260	50.108980
457.749225	127.348524	50.113985
454.533923	118.674018	50.118989
450.709839	120.820175	50.123994
447.350650	123.124473	50.128999
444.024072	127.638330	50.134004
440.213450	119.180466	50.139009
437.065782	112.808120	50.144013
433.294926	127.028522	50.149018
430.130685	124.126303	50.154023
426.643012	122.796537	50.159028
423.095617	118.881807	50.164033
419.582336	115.895059	50.169037
415.858249	118.958889	50.174042
412.605441	118.057420	50.179047
408.821570	120.529495	50.184052
405.243573	129.211513	50.189057
401.910780	110.795097	50.194061
398.661860	123.434108	50.199066
395.150806	119.440930	50.204071
391.504780	121.470634	50.209076
387.559555	123.208678	50.214081
384.524137	118.913207	50.219085
380.769321	120.678377	50.224090
377.490172	119.429866	50.229095
374.080443	123.380958	50.234100
370.427080	130.110070	50.239105
367.079288	115.131911	50.244109
363.029994	122.384959	50.249114
359.291869	115.231924	50.254119
356.440741	117.940732	50.259124
352.717615	116.942113	50.264129
349.717481	112.584181	50.269133
346.281091	117.716393	50.274138
342.449265	118.886191	50.279143
338.905848	110.462458	50.284148
335.353847	119.118275	50.289153
331.604661	119.012776	50.294157
328.542272	107.397352	50.299162
325.203084	119.408268	50.304167
321.569830	120.825384	50.309172
318.135971	121.227325	50.314177
314.627692	119.059261	50.319181
310.551271	118.233064	50.324186
306.789160	121.707860	50.329191
303.519698	127.611218	50.334196
300.138676	119.038671	50.339201
297.220923	118.938986	50.344205
293.238085	119.502865	50.349210
289.789345	118.201858	50.354215
286.464367	125.021928	50.359220
282.345865	127.859692	50.364225
279.405879	113.656103	50.369229
276.115475	123.454224	50.374234
272.610633	111.392434	50.379239
268.425110	108.314904	50.384244
265.323914	117.400004	50.389249
261.965629	116.021563	50.394253
258.115314	117.260733	50.399258
254.494495	120.558390	50.404263
251.276394	115.503802	50.409268
247.815444	130.422370	50.414273
244.433133	113.235022	50.419277
240.721107	118.325027	50.424282
237.324776	122.761293	50.429287
234.110019	116.092650	50.434292
230.344452	120.156485	50.439297
226.877955	110.167329	50.444301
223.311284	117.177142	50.449306
219.463546	114.774392	50.454311
216.242446	108.056133	50.459316
212.713499	116.265446	50.464321
209.544989	115.005994	50.469325
206.014028	116.100243	50.474330
202.357681	113.964915	50.479335
198.640088	115.021965	50.484340
194.760409	121.403773	50.489345
191.469827	111.614868	50.494349
187.762840	122.803907	50.499354
184.610643	121.943711	50.504359
181.174835	127.370124	50.509364
177.809882	125.233447	50.514369
174.593258	113.294234	50.519373
170.534731	123.503792	50.524378
167.087107	113.533853	50.529383
163.913425	123.234625	50.534388
160.241553	122.576077	50.539393
156.613774	115.051509	50.544397
153.193957	111.809783	50.549402
149.573397	114.161463	50.554407
146.629106	112.120251	50.559412
142.865921	111.124836	50.564417
139.697361	115.443191	50.569421
135.310305	111.796180	50.574426
131.744861	121.178681	50.579431
128.649780	107.739795	50.584436
124.902825	111.050934	50.589441
121.836418	110.911321	50.594445
118.322476	112.474344	50.599450
114.599024	109.969913	50.604455
111.223691	113.703733	50.609460
107.538081	114.800103	50.614465
104.172055	109.610565	50.619469
101.091280	119.749219	50.624474
97.287149	119.307575	50.629479
93.664078	116.297037	50.634484
90.208384	113.371011	50.639489
86.386607	112.147515	50.644493
82.892499	108.806727	50.649498
79.184427	115.535019	50.654503
76.189986	108.787635	50.659508
72.341109	115.300706	50.664513
68.683422	115.684028	50.669517
65.641624	124.978182	50.674522
62.321728	113.763893	50.679527
58.792332	113.383627	50.684532
55.133630	122.530825	50.689537
52.047166	114.896186	50.694541
48.202303	113.258704	50.699546
44.594309	119.477778	50.704551
41.303300	117.316918	50.709556
37.274463	112.519162	50.714561
34.225933	118.223470	50.719565
30.786006	112.697524	50.724570
27.048551	108.486879	50.729575
23.547539	102.622493	50.734580
19.632248	118.488670	50.739585
16.348481	114.061409	50.744589
13.040979	113.219283	50.749594
9.689664	115.778773	50.754599
6.023036	105.061775	50.759604
2.442783	111.437869	50.764609