Thu Aug 25 16:47:35 2022

Number of Points = 9922

Depth (nm)	Load (N)	Time (s)
2.475708	110.238566	0.000000
2.699133	120.963665	0.005005
3.261372	124.675329	0.010010
2.923412	123.386870	0.015014
3.001880	120.160196	0.020019
3.269825	123.177643	0.025024
2.645941	116.903548	0.030029
2.658255	97.697429	0.035034
2.647179	95.658557	0.040038
2.336133	96.982339	0.045043
2.424421	79.909386	0.050048
1.663705	79.490771	0.055053
1.325721	71.387520	0.060058
1.294404	56.396120	0.065062
0.839940	54.429888	0.070067
0.665913	47.819575	0.075072
0.101730	46.623515	0.080077
-0.321701	24.657327	0.085082
-0.591171	17.302673	0.090086
-0.394994	19.641643	0.095091
-0.245357	17.849683	0.100096
-0.841280	18.980812	0.105101
-0.876744	7.992282	0.110106
-1.517828	-0.120394	0.115110
-1.919160	-2.759337	0.120115
-2.336620	-3.826520	0.125120
-2.307210	5.650743	0.130125
-2.710209	-8.241484	0.135130
-3.143697	-8.793625	0.140134
-3.384021	-4.690483	0.145139
-3.223737	-9.970587	0.150144
-3.747654	-4.981447	0.155149
-4.270513	-9.186398	0.160154
-4.317344	-11.172199	0.165158
-4.942784	5.456555	0.170163
-4.862079	-2.895762	0.175168
-5.004713	0.676379	0.180173
-5.025888	-7.558732	0.185178
-5.798392	-5.156574	0.190182
-5.934109	-1.683594	0.195187
-6.036810	-6.090420	0.200192
-6.386420	5.439406	0.205197
-6.211286	-2.506924	0.210202
-6.738653	-4.335176	0.215206
-7.442802	1.065022	0.220211
-7.681924	-5.380046	0.225216
-7.834541	1.854146	0.230221
-7.858624	3.297475	0.235226
-7.922396	-1.928542	0.240230
-8.108709	9.610503	0.245235
-8.364098	2.870586	0.250240
-9.095967	0.204338	0.255245
-9.324391	-5.530557	0.260250
-9.346498	4.837470	0.265254
-9.576690	4.784990	0.270259
-9.526880	0.496636	0.275264
-10.346964	-2.975206	0.280269
-10.854443	3.938099	0.285274
-10.868028	2.627299	0.290278
-11.230262	1.871004	0.295283
-10.887353	-0.451113	0.300288
-11.282296	7.561373	0.305293
-11.364672	-4.229725	0.310298
-11.904549	4.827368	0.315302
-12.186007	8.823062	0.320307
-12.438550	7.344058	0.325312
-12.487176	7.019518	0.330317
-12.565885	-3.519299	0.335322
-12.836053	-6.011113	0.340326
-13.492016	3.054677	0.345331
-13.594515	5.763148	0.350336
-13.761858	-1.316432	0.355341
-13.617846	4.688032	0.360346
-14.080846	0.122522	0.365350
-14.967622	9.268773	0.370355
-14.720593	1.712975	0.375360
-15.073104	8.130598	0.380365
-15.259494	-2.907043	0.385370
-16.195577	-1.137318	0.390374
-16.416079	2.190758	0.395379
-16.569872	-3.014825	0.400384
-16.863299	7.335603	0.405389
-17.067539	6.250830	0.410394
-16.930198	3.704656	0.415398
-16.496991	-0.276772	0.420403
-16.505413	-3.331620	0.425408
-16.975013	2.743677	0.430413
-17.768863	6.088823	0.435418
-17.711693	1.024191	0.440422
-18.646652	5.505095	0.445427
-18.991116	-3.941708	0.450432
-19.088049	2.660496	0.455437
-19.627744	-2.120788	0.460442
-19.598636	0.443673	0.465446
-19.608593	5.823689	0.470451
-19.457046	-8.614172	0.475456
-19.956277	2.878983	0.480461
-20.477881	0.113353	0.485466
-20.707987	1.418119	0.490470
-21.288495	9.393242	0.495475
-21.172750	5.619743	0.500480
-21.284038	13.255590	0.505485
-21.265969	-1.797281	0.510490
-21.416584	2.741062	0.515494
-22.527080	9.872241	0.520499
-22.887626	3.636023	0.525504
-22.922287	7.143791	0.530509
-22.862696	3.027912	0.535514
-22.761963	3.097589	0.540518
-23.090934	3.876840	0.545523
-23.737834	6.041020	0.550528
-24.316378	2.812908	0.555533
-24.225820	3.921897	0.560538
-24.221459	-4.744325	0.565542
-24.470976	7.282350	0.570547
-24.329720	1.404108	0.575552
-25.118078	-4.243052	0.580557
-25.114126	-6.296922	0.585562
-25.347259	-3.431942	0.590566
-26.188088	0.819076	0.595571
-26.789923	-2.588884	0.600576
-26.971044	5.038919	0.605581
-26.763016	-2.216534	0.610586
-26.931594	-3.370170	0.615590
-26.693434	2.920100	0.620595
-26.707662	-6.758780	0.625600
-27.523893	1.734168	0.630605
-28.179072	-2.899306	0.635610
-28.282789	-1.816825	0.640614
-28.565099	1.568393	0.645619
-28.132999	-1.324524	0.650624
-29.063036	5.212063	0.655629
-29.693894	4.513677	0.660634
-29.837739	3.248598	0.665638
-30.161377	11.408101	0.670643
-29.929641	7.151353	0.675648
-30.088039	2.379928	0.680653
-30.232087	-0.194922	0.685658
-30.285863	-2.439065	0.690662
-30.813655	5.081704	0.695667
-31.402730	-1.074411	0.700672
-31.828397	10.967211	0.705677
-31.206302	3.975909	0.710682
-31.327982	-1.709272	0.715686
-32.036482	4.416113	0.720691
-32.310492	0.437928	0.725696
-32.658799	6.022819	0.730701
-32.963100	1.049628	0.735706
-32.714528	-1.270363	0.740710
-33.501073	1.326988	0.745715
-34.266484	-6.155591	0.750720
-34.387244	7.135400	0.755725
-34.650599	2.880296	0.760730
-34.274809	-2.851193	0.765734
-34.516273	10.259395	0.770739
-34.247169	0.558264	0.775744
-34.758160	-0.184213	0.780749
-35.531347	1.673885	0.785754
-35.504673	-1.411772	0.790758
-35.960587	-0.947989	0.795763
-36.012681	-7.197732	0.800768
-36.821286	3.499172	0.805773
-37.315725	-3.086225	0.810778
-36.962276	-7.055155	0.815782
-37.245602	8.042512	0.820787
-37.211159	-4.573649	0.825792
-37.620814	4.004292	0.830797
-37.375822	2.396711	0.835802
-37.915654	-0.293296	0.840806
-38.630103	8.123595	0.845811
-38.374802	-7.668798	0.850816
-38.800736	4.508903	0.855821
-39.439860	4.526826	0.860826
-39.979332	3.918527	0.865830
-40.045388	12.078799	0.870835
-39.722303	-3.689417	0.875840
-40.552397	-2.546905	0.880845
-40.554988	-1.812466	0.885850
-40.482228	-1.168927	0.890854
-40.697086	13.456105	0.895859
-40.820405	5.910879	0.900864
-41.518762	5.336967	0.905869
-41.772754	1.469541	0.910874
-41.623205	-0.638780	0.915878
-41.703889	5.454674	0.920883
-42.498955	1.994734	0.925888
-42.689386	5.957181	0.930893
-43.082611	1.222552	0.935898
-43.053441	5.372055	0.940902
-43.225605	10.347213	0.945907
-44.091208	-0.061979	0.950912
-44.547439	-1.284438	0.955917
-45.025281	1.454370	0.960922
-44.519490	-8.150964	0.965926
-45.051451	8.855451	0.970931
-44.965905	-1.914746	0.975936
-45.092249	0.889209	0.980941
-45.165114	-7.366274	0.985946
-45.126371	-4.556549	0.990950
-45.977144	6.023576	0.995955
-46.052170	-1.769660	1.000960
-46.478327	6.380594	1.005965
-46.513371	3.152746	1.010970
-46.683445	-1.838312	1.015974
-47.444699	8.215256	1.020979
-47.656373	-2.609610	1.025984
-47.880652	-0.666675	1.030989
-47.879070	-2.270918	1.035994
-47.567075	-2.534902	1.040998
-48.693277	10.347316	1.046003
-49.079403	8.386204	1.051008
-49.403286	7.446729	1.056013
-49.346446	8.171857	1.061018
-49.315213	4.547643	1.066022
-49.771275	9.231925	1.071027
-49.235797	2.444021	1.076032
-49.938883	12.244867	1.081037
-50.358678	1.038154	1.086042
-50.806572	0.333248	1.091046
-51.203176	2.388607	1.096051
-51.223231	3.081490	1.101056
-52.040719	1.206952	1.106061
-52.084891	14.305610	1.111066
-52.052803	8.327413	1.116070
-52.521076	6.983454	1.121075
-52.350249	0.705108	1.126080
-52.635330	20.213359	1.131085
-52.546163	0.049343	1.136090
-52.963382	7.084549	1.141094
-54.026294	13.803312	1.146099
-53.921800	6.962715	1.151104
-54.092683	10.039407	1.156109
-54.155818	3.354791	1.161114
-54.174886	4.006391	1.166118
-54.412317	9.741590	1.171123
-54.993031	11.895401	1.176128
-55.457200	7.292111	1.181133
-55.103939	5.563160	1.186138
-54.992393	-8.517251	1.191142
-56.078537	0.922829	1.196147
-56.305775	-3.423352	1.201152
-56.790884	-2.825280	1.206157
-56.909406	9.234652	1.211162
-56.984702	-1.228767	1.216166
-57.034270	2.069362	1.221171
-57.238555	2.234288	1.226176
-58.027747	2.598432	1.231181
-58.766606	-3.518391	1.236186
-58.382506	-3.221031	1.241190
-58.593984	12.403221	1.246195
-58.758810	-0.273467	1.251200
-58.589035	11.845698	1.256205
-58.915584	2.968732	1.261210
-59.508332	-3.607586	1.266214
-60.273803	-0.035930	1.271219
-59.767652	-0.358811	1.276224
-59.965280	7.948625	1.281229
-59.909205	-0.956654	1.286234
-61.221343	8.949114	1.291238
-61.375164	0.010283	1.296243
-61.085480	5.495206	1.301248
-61.626377	7.427642	1.306253
-61.297338	6.496594	1.311258
-61.398731	-3.469185	1.316262
-62.229876	0.391174	1.321267
-62.447888	-2.013897	1.326272
-62.663391	5.793300	1.331277
-62.994707	-3.617593	1.336282
-63.774163	-4.444553	1.341286
-63.832641	10.671666	1.346291
-63.847919	-5.695265	1.351296
-63.991822	0.072732	1.356301
-64.012181	-1.414177	1.361306
-64.078954	-1.242324	1.366310
-64.629605	3.697225	1.371315
-64.898088	2.486477	1.376320
-65.200067	2.410446	1.381325
-65.553861	3.854817	1.386330
-65.379911	-6.761548	1.391334
-65.926739	10.917916	1.396339
-66.190445	4.448227	1.401344
-67.028981	11.761424	1.406349
-66.951417	5.137020	1.411354
-66.873119	0.692343	1.416358
-67.238406	9.253842	1.421363
-66.911307	1.030600	1.426368
-67.972343	4.148693	1.431373
-68.486259	6.858354	1.436378
-68.493444	1.550706	1.441382
-69.062462	6.781036	1.446387
-68.856900	-4.855855	1.451392
-68.917393	6.356582	1.456397
-68.990505	4.191400	1.461402
-68.974301	1.015634	1.466406
-69.944306	3.360159	1.471411
-69.756081	-1.490886	1.476416
-69.981602	-1.088513	1.481421
-70.441895	-3.718212	1.486426
-71.142311	-3.823561	1.491430
-71.254514	2.050201	1.496435
-71.497221	-2.214461	1.501440
-71.568008	2.558146	1.506445
-71.673834	-3.891984	1.511450
-71.691213	-3.398839	1.516454
-72.391010	1.703285	1.521459
-72.866019	-2.588253	1.526464
-73.116174	4.401792	1.531469
-73.572759	2.521325	1.536474
-73.344871	3.498062	1.541478
-73.554323	3.948538	1.546483
-73.757679	3.145204	1.551488
-73.777207	-1.714417	1.556493
-73.930897	1.546243	1.561498
-74.533379	-1.557889	1.566502
-74.964841	6.387551	1.571507
-75.089671	-8.386651	1.576512
-75.095726	-4.370838	1.581517
-75.048867	-7.507112	1.586522
-75.508071	-4.783880	1.591526
-76.267603	9.986604	1.596531
-76.269909	0.713983	1.601536
-76.457629	3.824950	1.606541
-76.762378	2.031425	1.611546
-77.334540	-0.128326	1.616550
-77.692862	2.692996	1.621555
-77.721506	2.979098	1.626560
-77.824787	2.814984	1.631565
-77.676428	-2.545508	1.636570
-78.123062	1.650073	1.641574
-78.280667	5.240379	1.646579
-78.835781	-11.060939	1.651584
-79.464282	1.224429	1.656589
-79.362444	-5.049432	1.661594
-79.278430	-4.417149	1.666598
-79.306924	-3.143973	1.671603
-80.102067	-3.566674	1.676608
-80.336227	4.483891	1.681613
-80.790916	-2.224789	1.686618
-80.791391	3.501752	1.691622
-81.012520	0.293572	1.696627
-81.252268	-1.282347	1.701632
-81.836743	5.978384	1.706637
-82.432960	-3.599808	1.711642
-82.323877	4.162854	1.716646
-82.721257	10.258475	1.721651
-82.254886	8.938909	1.726656
-82.467058	0.262326	1.731661
-82.194601	3.886484	1.736666
-82.886616	-8.217204	1.741670
-83.742516	-4.856005	1.746675
-83.910985	-1.194395	1.751680
-84.134985	-8.948463	1.756685
-84.271702	0.279573	1.761690
-84.055072	3.798583	1.766694
-84.970845	2.932874	1.771699
-85.154558	-8.817024	1.776704
-85.367941	-0.908923	1.781709
-85.428124	4.757371	1.786714
-85.865025	-2.969667	1.791718
-86.498747	5.431411	1.796723
-86.507592	2.158330	1.801728
-87.268784	8.323612	1.806733
-87.011977	1.835641	1.811738
-86.610772	4.275357	1.816742
-86.796836	17.608220	1.821747
-87.142755	8.743781	1.826752
-88.148994	8.233935	1.831757
-88.118219	6.372015	1.836762
-88.385517	3.500102	1.841766
-88.410074	9.559451	1.846771
-88.440062	3.527708	1.851776
-89.198005	4.067293	1.856781
-89.624344	-6.106994	1.861786
-89.880280	4.765903	1.866790
-90.281693	2.228219	1.871795
-90.201279	2.756662	1.876800
-90.069263	6.254130	1.881805
-90.380291	-3.099828	1.886810
-90.379000	-3.906753	1.891814
-91.221415	1.075348	1.896819
-91.643855	-1.228085	1.901824
-91.478840	-4.531571	1.906829
-91.906317	-1.693086	1.911834
-91.577137	0.852829	1.916838
-92.261137	9.679404	1.921843
-92.510400	0.777678	1.926848
-92.657759	1.272208	1.931853
-93.182916	2.145479	1.936858
-92.979947	1.863775	1.941862
-93.929138	2.287794	1.946867
-94.011269	4.667204	1.951872
-94.668916	0.486543	1.956877
-94.789883	5.254359	1.961882
-94.871155	5.488596	1.966886
-94.460954	5.775537	1.971891
-94.686661	0.815345	1.976896
-94.687880	0.309371	1.981901
-95.780670	-0.968364	1.986906
-95.691658	-1.339780	1.991910
-95.985599	4.268228	1.996915
-96.380200	0.707451	2.006912
-96.258869	-4.532056	2.016909
-95.774428	5.152173	2.026906
-95.161256	7.143764	2.036902
-94.780408	4.315486	2.046899
-93.971440	2.370470	2.056896
-93.628442	10.603828	2.066893
-92.843565	4.661625	2.076890
-92.328925	3.789104	2.086886
-92.235668	-0.061667	2.096883
-91.771556	0.258496	2.106880
-90.912231	-1.865472	2.116877
-90.819959	-0.308614	2.126874
-90.395440	0.600632	2.136870
-89.791066	2.397197	2.146867
-88.885631	9.655434	2.156864
-88.065875	6.587318	2.166861
-88.394349	4.519590	2.176858
-87.994801	2.546861	2.186854
-86.716089	2.295886	2.196851
-86.441323	-3.534705	2.206848
-86.553963	8.375031	2.216845
-85.493424	6.352583	2.226842
-85.257395	7.766538	2.236838
-84.448935	4.554473	2.246835
-83.791300	4.461006	2.256832
-83.797733	-4.252592	2.266829
-83.156723	2.920364	2.276826
-82.320166	-1.487204	2.286822
-82.193566	1.439110	2.296819
-81.617830	0.854792	2.306816
-81.244542	0.099455	2.316813
-80.697413	-2.114977	2.326810
-79.572019	-3.412651	2.336806
-79.439536	1.283554	2.346803
-79.481092	-1.833332	2.356800
-78.692374	-3.746662	2.366797
-78.426764	-2.197958	2.376794
-76.841970	-3.859056	2.386790
-76.643609	-1.403321	2.396787
-76.350882	-1.246372	2.406784
-76.582307	2.296747	2.416781
-76.083364	-0.816132	2.426778
-75.202655	-0.250800	2.436774
-74.140305	-6.844698	2.446771
-73.915759	-3.914725	2.456768
-73.830759	-1.114941	2.466765
-73.218009	2.720392	2.476762
-72.444696	-4.845089	2.486758
-72.140754	-4.553681	2.496755
-71.035094	-0.649865	2.506752
-70.757834	-5.840945	2.516749
-71.101440	5.971932	2.526746
-70.013832	-1.690315	2.536742
-69.379777	-6.506478	2.546739
-69.351014	-5.281794	2.556736
-68.550971	-4.630961	2.566733
-68.083961	-6.126414	2.576730
-67.325071	-3.707823	2.586726
-66.796014	1.518627	2.596723
-66.694952	-1.379852	2.606720
-66.054690	-6.342708	2.616717
-65.262080	1.037746	2.626714
-64.862364	3.550632	2.636710
-64.817316	1.418039	2.646707
-64.344097	-0.449022	2.656704
-63.933400	5.451714	2.666701
-62.751620	2.196994	2.676698
-62.617876	0.956502	2.686694
-61.964642	4.874191	2.696691
-61.074777	2.935509	2.706688
-60.676045	-6.098169	2.716685
-60.838065	-0.924993	2.726682
-60.415221	0.028867	2.736678
-59.468225	3.273298	2.746675
-59.097050	9.189732	2.756672
-57.982253	-1.809326	2.766669
-58.227252	1.343110	2.776666
-57.831304	3.042455	2.786662
-57.099264	3.178086	2.796659
-56.512048	6.634115	2.806656
-55.697010	6.183364	2.816653
-55.089488	10.706937	2.826650
-55.170627	6.192904	2.836646
-54.744068	8.977186	2.846643
-53.885701	8.237710	2.856640
-53.527985	9.303146	2.866637
-53.116202	0.403636	2.876634
-52.364183	2.075699	2.886630
-52.151654	7.392931	2.896627
-51.200006	4.636773	2.906624
-50.732213	4.449509	2.916621
-50.859226	10.266608	2.926618
-50.146702	8.029428	2.936614
-49.299063	9.667503	2.946611
-49.189161	7.581768	2.956608
-48.315425	0.640451	2.966605
-47.733419	4.901924	2.976602
-47.621166	5.204362	2.986598
-46.893038	6.366982	2.996595
-46.106549	2.087637	3.006592
-46.129403	10.745794	3.016589
-46.268150	6.944044	3.026586
-45.051994	13.130396	3.036582
-44.017157	12.483647	3.046579
-43.429567	9.683163	3.056576
-43.220163	9.026366	3.066573
-43.047968	12.756504	3.076570
-43.033572	6.634084	3.086566
-41.907218	9.223185	3.096563
-41.864066	0.368764	3.106560
-40.592411	5.171582	3.116557
-40.667290	-1.133252	3.126554
-40.188356	6.309030	3.136550
-39.295152	9.064544	3.146547
-39.005524	5.005604	3.156544
-38.603067	5.151696	3.166541
-37.777024	5.183900	3.176538
-37.537868	4.326037	3.186534
-36.751995	3.933711	3.196531
-36.067053	4.114737	3.206528
-36.180505	0.407228	3.216525
-35.605289	1.134473	3.226522
-34.572347	2.873395	3.236518
-34.396324	3.688532	3.246515
-34.365899	2.673305	3.256512
-33.374583	2.175929	3.266509
-33.151039	-0.529498	3.276506
-32.160018	-0.855765	3.286502
-31.545055	6.980189	3.296499
-31.548449	4.427529	3.306496
-31.381513	3.229353	3.316493
-30.321780	3.205935	3.326490
-30.186668	3.355903	3.336486
-29.157590	-0.654171	3.346483
-28.742504	7.143409	3.356480
-28.620061	-4.102472	3.366477
-28.164937	3.539945	3.376474
-27.398995	2.694576	3.386470
-26.864024	3.399618	3.396467
-25.931585	3.215580	3.406464
-25.629171	1.768093	3.416461
-25.650260	2.164283	3.426458
-25.335347	7.516160	3.436454
-24.438032	2.614397	3.446451
-24.060176	9.483303	3.456448
-23.066084	0.745979	3.466445
-22.859689	9.159139	3.476442
-22.519267	8.833443	3.486438
-22.297216	6.989898	3.496435
-21.322116	9.827617	3.506432
-20.804801	5.058255	3.516429
-19.802787	4.141051	3.526426
-19.830717	9.195018	3.536422
-19.399330	6.561563	3.546419
-19.416625	7.533704	3.556416
-18.387822	6.548946	3.566413
-17.808716	4.114093	3.576410
-17.402281	-2.320010	3.586406
-16.876744	6.781248	3.596403
-16.655522	4.890316	3.606400
-15.994493	3.624227	3.616397
-15.571527	1.733362	3.626394
-14.774936	5.004534	3.636390
-14.141371	4.107047	3.646387
-13.961642	2.919538	3.656384
-13.476202	0.274447	3.666381
-12.569967	3.854724	3.676378
-12.800434	5.975341	3.686374
-11.915218	5.190480	3.696371
-11.022063	0.568139	3.706368
-10.851696	4.143339	3.716365
-10.711654	-1.672480	3.726362
-9.898985	-2.800770	3.736358
-9.580213	7.774247	3.746355
-8.492566	7.163578	3.756352
-8.129305	3.967421	3.766349
-8.403654	6.823513	3.776346
-7.539110	1.226796	3.786342
-6.776959	6.191816	3.796339
-6.404179	6.095469	3.806336
-5.524859	7.921822	3.816333
-5.567759	10.681462	3.826330
-5.047561	9.253705	3.836326
-4.488534	22.990593	3.846323
-4.054526	23.131744	3.856320
-3.422095	28.224802	3.866317
-3.217123	34.154620	3.876314
-2.623490	46.587294	3.886310
-2.297380	52.609012	3.896307
-1.770414	60.867432	3.906304
-1.136878	76.442704	3.916301
-0.602529	83.908019	3.926298
-0.097911	106.146480	3.936294
0.000000	103.800547	3.941299
-0.403543	107.081391	3.946304
0.380482	128.361662	3.951309
0.403874	128.630121	3.956314
0.558905	130.643354	3.961318
0.556171	128.444982	3.966323
0.608977	147.353100	3.971328
0.770444	144.005849	3.976333
0.636034	148.718863	3.981338
0.658440	147.956078	3.986342
1.025484	146.547664	3.991347
0.859421	159.415593	3.996352
1.094096	152.573522	4.001357
1.310252	156.159082	4.006362
1.364466	145.428503	4.011366
1.242408	147.538937	4.016371
1.253384	158.692821	4.021376
1.359781	153.468570	4.026381
0.949886	147.129298	4.031386
1.323632	141.116504	4.036390
0.759483	136.845220	4.041395
0.856733	152.060555	4.046400
1.379285	144.790562	4.051405
1.397437	149.103180	4.056410
1.202306	137.057567	4.061414
0.799439	139.196180	4.066419
0.912292	148.312427	4.071424
1.319575	159.989520	4.076429
1.575155	159.835616	4.081434
1.521442	149.077652	4.086438
1.031796	142.583196	4.091443
1.195217	143.911735	4.096448
0.974685	136.103268	4.101453
1.225021	161.029636	4.106458
1.075448	152.934792	4.111462
1.046249	154.736445	4.116467
0.963684	162.627289	4.121472
1.158087	156.927332	4.126477
1.018249	161.122336	4.131482
1.528369	155.755733	4.136486
1.143738	156.613314	4.141491
1.291552	157.181823	4.146496
1.172777	154.014523	4.151501
1.108821	154.945248	4.156506
1.515939	151.932834	4.161510
1.095922	163.046681	4.166515
1.200587	147.122722	4.171520
1.496132	146.010253	4.176525
1.302727	157.123391	4.181530
1.694603	153.692579	4.186534
1.439107	163.663826	4.191539
1.289652	155.761955	4.196544
1.567440	160.119318	4.201549
1.395306	153.369462	4.206554
1.258529	161.313092	4.211558
1.649408	175.327652	4.216563
1.755723	175.203463	4.221568
1.719149	155.704380	4.226573
1.361884	158.911543	4.231578
1.654830	161.279663	4.236582
1.462799	159.987320	4.241587
1.237136	165.230336	4.246592
1.800162	169.074766	4.251597
1.556346	175.643100	4.256602
2.020281	174.020182	4.261606
1.652714	167.788168	4.266611
1.612645	162.574208	4.271616
1.731842	158.360367	4.276621
1.836500	161.979216	4.281626
1.992739	160.720891	4.286630
1.580078	152.401510	4.291635
1.348984	161.422956	4.296640
1.869706	155.668707	4.301645
1.868973	161.268791	4.306650
1.586449	154.052169	4.311654
1.786567	159.671403	4.316659
1.085959	159.430033	4.321664
1.872330	167.017049	4.326669
1.809626	180.248454	4.331674
1.736130	167.854727	4.336678
2.084944	183.596994	4.341683
2.058489	174.976641	4.346688
2.379463	174.081651	4.351693
2.012154	168.618401	4.356698
1.853163	154.678322	4.361702
1.724447	160.877435	4.366707
1.749750	163.334947	4.371712
1.717596	164.823848	4.376717
1.758078	176.406560	4.381722
2.181989	182.300790	4.386726
2.045144	182.224191	4.391731
1.870316	180.217294	4.396736
2.160594	177.836961	4.401741
1.793167	180.552167	4.406746
2.517030	176.677022	4.411750
2.323421	166.092829	4.416755
2.035742	161.673815	4.421760
2.030289	154.825074	4.426765
1.794807	159.531781	4.431770
1.796206	159.367082	4.436774
2.249575	170.293467	4.441779
1.937314	173.835273	4.446784
2.309356	175.311464	4.451789
1.968019	182.069089	4.456794
2.171474	183.375540	4.461798
1.945557	177.750925	4.466803
1.789747	175.690428	4.471808
2.573376	181.901625	4.476813
2.194440	182.093916	4.481818
1.931876	178.088585	4.486822
2.239632	179.808970	4.491827
2.067783	177.421950	4.496832
2.300821	174.500084	4.501837
2.210296	178.352002	4.506842
2.327036	179.482211	4.511846
2.297013	169.198258	4.516851
2.065360	175.903893	4.521856
2.515590	179.161712	4.526861
2.199389	190.366878	4.531866
2.226530	175.198537	4.536870
2.301506	180.027451	4.541875
1.891896	186.204143	4.546880
2.502784	182.311897	4.551885
2.454970	190.013807	4.556890
2.089541	171.993110	4.561894
2.193082	173.982777	4.566899
2.061906	182.526663	4.571904
2.364532	180.773992	4.576909
2.309805	184.917701	4.581914
2.382512	184.627932	4.586918
2.051317	195.136250	4.591923
2.373523	201.005291	4.596928
2.710399	198.779009	4.601933
2.632185	199.468357	4.606938
2.574219	202.366037	4.611942
2.710794	195.371639	4.616947
2.567486	203.069534	4.621952
2.410935	184.035315	4.626957
2.591420	189.224194	4.631962
2.595256	197.060385	4.636966
2.665033	200.697363	4.641971
2.731491	198.956384	4.646976
2.531188	183.950225	4.651981
2.395854	195.443436	4.656986
2.784284	191.614517	4.661990
2.969647	200.994681	4.666995
2.607247	189.573201	4.672000
2.502618	183.436027	4.677005
2.538019	193.592670	4.682010
2.607074	192.237270	4.687014
2.972072	195.786861	4.692019
2.817328	195.671937	4.697024
2.881143	195.139948	4.702029
2.455534	184.383284	4.707034
2.477286	188.148009	4.712038
2.952266	194.698641	4.717043
2.904911	199.765030	4.722048
2.971130	198.716963	4.727053
2.918950	197.124289	4.732058
2.786131	196.506048	4.737062
2.561094	187.189128	4.742067
2.482011	193.263414	4.747072
2.903554	186.085162	4.752077
2.643586	201.992435	4.757082
2.952448	200.216639	4.762086
3.085519	204.093642	4.767091
2.866771	199.578395	4.772096
2.761781	205.536519	4.777101
2.779230	203.527967	4.782106
2.594008	196.340376	4.787110
2.478987	203.046730	4.792115
2.557532	208.463562	4.797120
2.891183	205.177907	4.802125
2.736883	216.620319	4.807130
3.096431	220.553591	4.812134
3.053263	225.401028	4.817139
2.860985	226.532201	4.822144
3.207975	218.457602	4.827149
3.131981	228.011611	4.832154
3.383944	231.018925	4.837158
3.087631	217.897595	4.842163
2.939756	220.565751	4.847168
3.104999	205.594048	4.852173
3.009829	208.649420	4.857178
3.348682	220.498629	4.862182
3.600928	221.867042	4.867187
3.035353	212.280756	4.872192
3.203268	203.765978	4.877197
2.736189	207.708540	4.882202
3.293268	218.090349	4.887206
3.302635	217.440338	4.892211
3.071469	212.224666	4.897216
3.249960	217.752393	4.902221
3.312480	223.244507	4.907226
3.614420	228.876284	4.912230
3.182491	210.372413	4.917235
3.238554	204.956713	4.922240
3.328246	200.741157	4.927245
3.072847	209.655702	4.932250
3.508118	224.381531	4.937254
3.536312	218.910081	4.942259
3.158913	209.588546	4.947264
3.141466	207.199477	4.952269
3.521732	220.130548	4.957274
3.697999	223.453447	4.962278
3.588879	206.768814	4.967283
3.526665	199.062066	4.972288
3.555166	198.984871	4.977293
3.093109	208.548738	4.982298
2.998422	199.692286	4.987302
3.758125	209.128001	4.992307
3.223585	217.943915	4.997312
3.509053	221.325635	5.002317
3.611237	235.258924	5.007322
3.572045	227.219519	5.012326
3.869657	234.639531	5.017331
3.125389	228.567760	5.022336
3.529817	213.776878	5.027341
3.627998	223.268792	5.032346
3.785549	222.823357	5.037350
3.460651	217.299662	5.042355
3.143263	224.224396	5.047360
3.550678	222.986824	5.052365
3.668149	218.577083	5.057370
3.638168	222.372068	5.062374
3.695977	229.560727	5.067379
3.563076	234.899962	5.072384
3.586719	220.076987	5.077389
3.342343	219.175662	5.082394
3.321122	225.623714	5.087398
3.748241	223.177642	5.092403
3.439397	225.244584	5.097408
3.628196	218.096459	5.102413
3.370257	230.589685	5.107418
3.468170	225.597701	5.112422
3.743146	241.380063	5.117427
3.773425	248.047849	5.122432
3.973161	236.838824	5.127437
3.838370	251.536933	5.132442
3.911797	250.880047	5.137446
3.743693	246.581484	5.142451
3.797431	250.322228	5.147456
3.884745	246.787255	5.152461
3.676519	260.712251	5.157466
3.689694	243.432607	5.162470
4.091529	247.776883	5.167475
3.998032	252.635378	5.172480
3.768310	252.041809	5.177485
3.622937	256.573068	5.182490
3.845854	254.367798	5.187494
4.363133	249.718232	5.192499
4.370483	244.088686	5.197504
4.065583	248.353867	5.202509
3.825324	247.587939	5.207514
4.074596	250.614661	5.212518
4.223503	249.215107	5.217523
3.744602	249.543286	5.222528
4.289819	244.383133	5.227533
4.105143	254.128195	5.232538
3.957342	252.142365	5.237542
4.338646	252.054185	5.242547
4.177125	253.044496	5.247552
4.129112	242.902527	5.252557
3.676152	249.718797	5.257562
3.968485	256.753659	5.262566
4.318882	252.383346	5.267571
3.943349	253.704588	5.272576
4.054882	253.876979	5.277581
4.233242	260.743036	5.282586
3.975633	253.902128	5.287590
4.399368	258.012016	5.292595
4.273250	253.431621	5.297600
4.325244	255.941913	5.302605
4.424623	252.525274	5.307610
4.235833	250.324400	5.312614
4.480008	253.889770	5.317619
4.076012	254.623837	5.322624
4.186211	250.167770	5.327629
4.120565	263.918565	5.332634
4.185420	252.078917	5.337638
4.413620	254.545782	5.342643
3.963313	257.128448	5.347648
4.233050	250.556099	5.352653
4.190354	249.952210	5.357658
4.311170	245.076857	5.362662
4.271544	250.781141	5.367667
4.211216	253.679199	5.372672
4.496341	250.239785	5.377677
4.244624	250.927845	5.382682
4.570579	262.181141	5.387686
4.239955	257.591657	5.392691
4.195821	268.017074	5.397696
4.408391	274.061509	5.402701
4.391483	272.311439	5.407706
4.769524	271.885241	5.412710
4.576933	273.209458	5.417715
4.207167	277.158935	5.422720
4.349784	279.971414	5.427725
4.392182	281.929544	5.432730
4.405270	273.837634	5.437734
4.343242	278.849396	5.442739
4.184574	275.634539	5.447744
4.796174	267.543769	5.452749
4.362121	273.667373	5.457754
4.189953	274.061390	5.462758
4.603378	276.904206	5.467763
4.576830	291.000080	5.472768
4.923285	286.576591	5.477773
5.031317	284.525362	5.482778
4.681741	282.213632	5.487782
4.626847	273.815991	5.492787
4.845633	269.573865	5.497792
4.885735	273.977988	5.502797
4.488907	272.822131	5.507802
4.172215	279.424068	5.512806
4.660210	289.566801	5.517811
4.875953	299.995811	5.522816
4.936132	292.788713	5.527821
4.702060	309.261513	5.532826
4.691228	309.522682	5.537830
5.313503	299.399048	5.542835
5.141565	306.842039	5.547840
4.931572	296.829825	5.552845
4.884166	291.696073	5.557850
4.911751	294.311437	5.562854
4.878285	283.186379	5.567859
4.702100	288.823485	5.572864
5.069678	298.380799	5.577869
5.344513	299.641272	5.582874
5.117515	287.372755	5.587878
5.104937	273.314729	5.592883
4.476685	276.409344	5.597888
4.574023	292.096194	5.602893
4.582761	296.353374	5.607898
4.877727	295.763018	5.612902
5.366061	308.237449	5.617907
4.702592	305.367442	5.622912
5.027056	301.576997	5.627917
4.960305	305.304992	5.632922
5.079873	308.507074	5.637926
5.146876	302.460029	5.642931
5.259295	300.218282	5.647936
5.015144	301.439846	5.652941
5.225171	313.429527	5.657946
5.259210	302.705178	5.662950
5.351215	303.092607	5.667955
5.200576	310.642997	5.672960
4.697202	300.467936	5.677965
4.798334	298.481064	5.682970
4.804819	304.238253	5.687974
5.410315	298.916776	5.692979
5.251528	301.089932	5.697984
5.180439	302.762119	5.702989
5.237608	304.793869	5.707994
5.411151	304.127622	5.712998
5.216043	301.041860	5.718003
5.118344	305.290408	5.723008
5.215843	302.630209	5.728013
5.403488	304.018241	5.733018
5.273850	304.759945	5.738022
5.497348	303.756833	5.743027
5.052855	303.718945	5.748032
5.213130	305.981319	5.753037
5.238420	311.684943	5.758042
5.287975	322.934127	5.763046
5.472514	329.890993	5.768051
5.728564	334.172709	5.773056
5.690209	320.166142	5.778061
5.271578	312.825245	5.783066
5.462436	304.566258	5.788070
5.292458	301.008312	5.793075
5.357702	315.861797	5.798080
5.929999	316.639056	5.803085
5.795771	319.263958	5.808090
5.598463	309.632573	5.813094
5.623581	308.812408	5.818099
5.207619	307.934799	5.823104
5.387663	298.130397	5.828109
5.495539	306.475531	5.833114
5.565700	314.927821	5.838118
5.798958	310.930196	5.843123
5.663654	307.553481	5.848128
5.762162	309.528134	5.853133
5.627078	305.281331	5.858138
5.571259	308.817785	5.863142
5.664326	304.937042	5.868147
5.521138	304.450139	5.873152
5.361436	305.019378	5.878157
5.864437	324.641777	5.883162
5.569206	331.452347	5.888166
5.629274	324.251582	5.893171
5.623906	331.611536	5.898176
6.117076	318.322139	5.903181
6.009523	331.332888	5.908186
5.519539	315.403872	5.913190
5.807760	323.587876	5.918195
5.642083	330.953965	5.923200
5.806550	322.044192	5.928205
6.050810	330.592600	5.933210
5.816243	326.165223	5.938214
5.888151	336.702215	5.943219
5.737805	337.871118	5.948224
5.869742	329.213217	5.953229
5.900173	332.359665	5.958234
5.731841	329.155804	5.963238
5.928448	324.638723	5.968243
5.792916	335.236691	5.973248
5.952396	324.926119	5.978253
5.659476	328.616788	5.983258
5.721853	326.670787	5.988262
6.179028	331.291158	5.993267
5.724917	336.108099	5.998272
5.930516	331.418759	6.003277
5.842141	339.335902	6.008282
5.932150	328.694519	6.013286
5.721080	315.471173	6.018291
5.902550	327.920930	6.023296
5.649042	310.515323	6.028301
5.577893	327.544757	6.033306
5.515359	325.412679	6.038310
5.918493	321.587757	6.043315
5.882816	322.396998	6.048320
5.781845	321.384611	6.053325
5.777954	326.649876	6.058330
5.598052	316.541185	6.063334
5.792912	318.522888	6.068339
5.443982	334.444218	6.073344
5.625919	330.938696	6.078349
5.387827	325.407694	6.083354
5.466088	330.106417	6.088358
5.545901	331.486036	6.093363
5.930021	346.375008	6.098368
6.055748	348.848450	6.103373
5.722522	340.658907	6.108378
5.745827	344.322178	6.113382
5.982358	346.870010	6.118387
5.807118	335.593122	6.123392
5.465952	339.421070	6.128397
5.960267	349.591321	6.133402
6.074628	351.835584	6.138406
5.800525	345.145926	6.143411
5.943001	343.307599	6.148416
5.741090	336.872394	6.153421
5.951562	332.523985	6.158426
5.719380	331.478371	6.163430
5.789546	337.345819	6.168435
5.930075	345.410601	6.173440
6.190673	336.735702	6.178445
6.096101	328.075326	6.183450
5.958710	328.656890	6.188454
5.929089	329.585408	6.193459
5.830627	333.213971	6.198464
6.135667	329.648032	6.203469
6.098016	327.322225	6.208474
5.901777	329.931534	6.213478
6.257344	313.297383	6.218483
5.982343	325.141599	6.223488
5.969894	318.980444	6.228493
5.909705	329.541293	6.233498
5.701075	327.103066	6.238502
5.705884	320.546891	6.243507
6.012580	329.977717	6.248512
6.169788	321.423431	6.253517
5.827798	337.413280	6.258522
5.784358	326.065126	6.263526
6.105175	325.926310	6.268531
5.878377	328.704927	6.273536
6.081133	323.908465	6.278541
6.228487	303.086395	6.283546
5.644593	297.717152	6.288550
5.510162	296.456903	6.293555
5.433781	306.567848	6.298560
5.908423	314.023433	6.303565
6.178144	327.231337	6.308570
6.220205	320.422545	6.313574
6.339794	305.989436	6.318579
5.990254	299.308450	6.323584
5.779651	298.455615	6.328589
6.198071	301.614034	6.333594
5.771891	300.355203	6.338598
5.933184	289.424258	6.343603
5.895322	303.616830	6.348608
5.934139	295.141219	6.353613
5.998362	298.731630	6.358618
5.540232	292.915567	6.363622
6.302930	288.012398	6.368627
5.790710	299.387554	6.373632
5.943898	288.141497	6.378637
5.706229	304.080169	6.383642
5.587637	298.182430	6.388646
5.863567	295.323428	6.393651
5.909335	300.628362	6.398656
5.903665	300.009178	6.403661
5.453118	300.703083	6.408666
5.420381	304.001796	6.413670
5.703169	301.802959	6.418675
5.401167	301.556079	6.423680
5.712529	299.507793	6.428685
5.583915	302.922770	6.433690
5.658150	312.026169	6.438694
5.828223	322.592065	6.443699
5.738530	321.343788	6.448704
6.061610	321.827893	6.453709
6.109727	327.800035	6.458714
6.025488	310.921576	6.463718
5.938808	302.788336	6.468723
5.699151	297.165836	6.473728
5.398775	298.601858	6.478733
5.948109	318.264448	6.483738
5.989689	330.014771	6.488742
5.923509	324.017061	6.493747
6.064613	321.058954	6.498752
5.762668	296.659392	6.503757
6.003084	304.097886	6.508762
5.613934	307.753007	6.513766
5.773360	301.843345	6.518771
5.633154	310.417180	6.523776
5.740911	314.279190	6.528781
5.732629	326.609977	6.533786
6.138334	331.162481	6.538790
6.036685	321.206045	6.543795
5.680985	304.528318	6.548800
5.879609	308.423547	6.553805
5.989107	306.444855	6.558810
5.931396	300.676784	6.563814
6.119939	298.552827	6.568819
5.739189	299.356021	6.573824
5.745317	295.311728	6.578829
6.007325	294.331057	6.583834
5.876073	302.163151	6.588838
5.919929	297.344135	6.593843
5.683729	299.829984	6.598848
5.910582	291.258473	6.603853
5.658211	297.973728	6.608858
5.797857	301.580797	6.613862
5.965109	295.470589	6.618867
5.712935	292.134335	6.623872
5.864109	281.698537	6.628877
5.853940	295.013547	6.633882
5.904632	297.122243	6.638886
5.777556	292.741309	6.643891
5.721921	300.846298	6.648896
5.961439	294.199572	6.653901
6.047429	291.594963	6.658906
5.830836	298.000885	6.663910
5.847067	297.571263	6.668915
5.597255	303.890641	6.673920
5.618317	297.876106	6.678925
5.433500	300.603847	6.683930
5.857837	317.463886	6.688934
6.268294	316.377696	6.693939
5.684977	314.146878	6.698944
6.085811	312.347169	6.703949
5.759981	301.381807	6.708954
5.830952	305.853870	6.713958
5.815838	301.588271	6.718963
5.881764	303.488932	6.723968
5.895395	300.750123	6.728973
5.774267	296.058201	6.733978
5.981391	298.189844	6.738982
5.817000	288.822238	6.743987
5.759849	289.014732	6.748992
5.684238	294.367157	6.753997
5.784025	305.371172	6.759002
5.900127	315.936029	6.764006
5.978785	312.975053	6.769011
5.619946	313.306569	6.774016
6.114885	321.584736	6.779021
5.764264	309.772181	6.784026
5.750017	313.643816	6.789030
6.006850	302.198008	6.794035
5.727418	311.315690	6.799040
5.800192	302.524700	6.804045
6.194200	314.162845	6.809050
5.505260	313.087556	6.814054
5.913649	303.902286	6.819059
5.953315	304.028990	6.824064
5.443079	289.976157	6.829069
5.919996	311.551545	6.834074
5.665649	323.506422	6.839078
6.047946	320.153012	6.844083
6.198584	328.387050	6.849088
5.937676	311.615368	6.854093
6.033595	307.395648	6.859098
5.475425	298.007476	6.864102
5.659819	296.668798	6.869107
5.414657	303.344959	6.874112
5.797150	323.204542	6.879117
6.288730	320.390844	6.884122
6.025390	322.646825	6.889126
5.833644	308.544075	6.894131
5.594222	312.324437	6.899136
5.775800	314.472740	6.904141
5.889656	319.014019	6.909146
6.101926	323.299428	6.914150
5.869739	311.749897	6.919155
5.587525	314.201828	6.924160
5.975078	306.130327	6.929165
6.081428	308.299907	6.934170
5.985835	310.482147	6.939174
5.799912	297.824363	6.944179
5.425811	301.426504	6.949184
5.462649	300.126764	6.954189
6.089656	313.807037	6.959194
6.218600	315.640876	6.964198
6.445674	304.054194	6.969203
6.029598	299.541364	6.974208
5.958047	297.201889	6.979213
5.953830	301.831268	6.984218
5.736229	304.029460	6.989222
5.828016	290.904215	6.994227
5.556999	299.501705	6.999232
5.635241	294.367248	7.004237
5.850815	303.420022	7.009242
5.924739	304.560111	7.014246
6.065875	300.681329	7.019251
5.820855	299.561797	7.024256
5.874969	293.538920	7.029261
5.710821	294.200607	7.034266
5.302906	296.115397	7.039270
5.765515	288.149205	7.044275
5.758319	293.370684	7.049280
5.670052	291.631793	7.054285
5.719996	300.172666	7.059290
5.907211	316.155511	7.064294
6.465189	313.170055	7.069299
6.190004	310.359435	7.074304
6.259175	302.764937	7.079309
6.084700	302.833442	7.084314
5.933279	289.844384	7.089318
6.156539	287.601091	7.094323
5.830678	286.355017	7.099328
5.787307	289.889516	7.104333
5.705714	282.527462	7.109338
5.571522	292.378532	7.114342
5.735441	295.722362	7.119347
5.520689	288.147046	7.124352
5.557688	292.105561	7.129357
5.450736	295.115336	7.134362
5.784021	289.567588	7.139366
5.877286	287.006133	7.144371
5.615848	295.760312	7.149376
5.616206	286.303617	7.154381
5.504832	305.025652	7.159386
5.824364	316.681795	7.164390
6.517674	317.076252	7.169395
5.715384	305.780569	7.174400
5.847781	298.347014	7.179405
6.081326	293.561555	7.184410
5.986046	299.837736	7.189414
5.932273	295.850285	7.194419
6.029237	306.063787	7.199424
6.070903	298.543204	7.204429
5.974503	297.830666	7.209434
5.906481	294.228272	7.214438
6.027107	286.303008	7.219443
5.979122	294.773800	7.224448
6.106916	293.972349	7.229453
6.164562	299.987283	7.234458
6.041782	301.389151	7.239462
6.228539	293.181434	7.244467
5.666485	299.714252	7.249472
5.900040	289.113678	7.254477
5.886792	294.636669	7.259482
5.546126	289.738696	7.264486
6.238208	291.512773	7.269491
5.583992	289.875211	7.274496
5.935119	288.988147	7.279501
5.843551	292.346697	7.284506
5.779328	288.443145	7.289510
5.743232	290.733121	7.294515
5.786286	302.109864	7.299520
5.853024	291.870791	7.304525
5.978067	300.649841	7.309530
6.090380	297.117269	7.314534
6.061833	284.738564	7.319539
5.293409	278.034631	7.324544
5.644385	284.316818	7.329549
5.702496	291.546584	7.334554
5.813013	288.172487	7.339558
5.871708	291.229076	7.344563
5.831455	291.747961	7.349568
5.732265	284.385499	7.354573
5.674204	288.972689	7.359578
5.899377	289.984673	7.364582
5.903888	291.322303	7.369587
5.914522	293.073435	7.374592
5.819019	289.494330	7.379597
5.952800	286.376021	7.384602
5.766480	292.109631	7.389606
5.856443	291.216030	7.394611
5.685216	291.442217	7.399616
6.149973	293.131687	7.404621
6.013926	288.663572	7.409626
6.024015	288.715814	7.414630
6.019930	287.071303	7.419635
5.946016	284.523388	7.424640
5.943539	269.362770	7.429645
5.593546	271.100800	7.434650
5.750564	272.797356	7.439654
5.762031	285.757785	7.444659
5.676087	293.965599	7.449664
5.781794	292.914503	7.454669
5.886937	290.847907	7.459674
5.638462	292.345401	7.464678
5.728167	281.239012	7.469683
5.777342	295.180653	7.474688
5.852572	291.350165	7.479693
6.027462	286.273335	7.484698
5.757525	292.067503	7.489702
6.142745	283.512312	7.494707
5.729361	286.491003	7.499712
5.724188	285.520557	7.504717
5.836895	284.420908	7.509722
5.988516	290.686875	7.514726
6.294553	288.133212	7.519731
5.576176	299.148355	7.524736
6.036883	293.055445	7.529741
5.921333	289.226375	7.534746
5.870232	283.972978	7.539750
5.882666	272.467403	7.544755
5.662485	277.250839	7.549760
5.834352	285.086052	7.554765
5.794151	281.637493	7.559770
5.708605	290.765915	7.564774
6.160764	286.961793	7.569779
5.825690	279.035166	7.574784
6.059292	282.073840	7.579789
6.137976	263.179853	7.584794
5.725702	272.523978	7.589798
6.175390	262.718477	7.594803
5.911744	268.163632	7.599808
5.936580	264.043646	7.604813
5.782486	262.837102	7.609818
5.712675	268.821374	7.614822
5.628922	265.993422	7.619827
5.693914	263.967923	7.624832
5.819683	263.995712	7.629837
5.882160	259.275032	7.634842
5.915505	266.464375	7.639846
5.873720	266.398192	7.644851
5.889835	265.772432	7.649856
5.932276	262.279289	7.654861
5.895540	260.700009	7.659866
5.763482	275.938724	7.664870
5.507849	274.156453	7.669875
5.772411	256.907012	7.674880
5.668610	263.273102	7.679885
5.957681	261.816784	7.684890
5.667681	258.594033	7.689894
5.844797	267.735074	7.694899
5.886818	280.962801	7.699904
6.101022	276.661279	7.704909
6.043468	268.431739	7.709914
5.750053	264.956417	7.714918
5.860874	270.418831	7.719923
5.871650	271.027799	7.724928
5.677083	265.572254	7.729933
5.688595	259.986344	7.734938
5.703325	258.911539	7.739942
5.905868	262.265130	7.744947
5.734358	280.224589	7.749952
5.795472	274.580281	7.754957
5.865076	280.713559	7.759962
5.973181	294.611165	7.764966
6.045451	287.471779	7.769971
5.896345	282.942435	7.774976
5.602056	269.842895	7.779981
5.647180	274.075386	7.784986
5.900128	289.497403	7.789990
5.951583	282.785232	7.794995
5.800450	288.962591	7.800000
5.857255	276.485095	7.805005
5.741271	273.311008	7.810010
6.023253	287.532549	7.815014
5.979943	282.363355	7.820019
5.507508	279.406471	7.825024
5.500706	279.119667	7.830029
5.468696	289.761501	7.835034
5.709871	302.761883	7.840038
6.077249	293.409034	7.845043
5.730843	292.909678	7.850048
5.755234	294.399221	7.855053
5.846026	302.364207	7.860058
5.691474	297.781927	7.865062
5.803992	296.416545	7.870067
5.403487	300.462594	7.875072
5.596980	293.804097	7.880077
6.052614	299.788311	7.885082
5.679627	304.165415	7.890086
5.930131	290.999483	7.895091
5.677235	288.248651	7.900096
5.832533	290.809203	7.905101
5.793846	296.136859	7.910106
5.615362	302.935454	7.915110
6.008862	291.553663	7.920115
5.889484	291.088340	7.925120
6.155217	297.466147	7.930125
6.195109	296.067851	7.935130
6.394786	287.127268	7.940134
6.384080	290.273972	7.945152
5.785283	297.799636	7.950170
5.610420	292.260319	7.955187
5.908736	288.183717	7.960205
5.934236	292.253840	7.965222
5.751213	290.834063	7.970240
5.850970	299.651432	7.975258
5.854157	292.051910	7.980275
6.109323	288.654244	7.985293
6.216037	294.261118	7.990310
5.846434	279.209314	7.995328
5.885841	275.372094	8.000346
5.610644	268.863910	8.005363
5.920902	289.706422	8.010381
5.749162	290.336119	8.015398
5.844991	293.524234	8.020416
5.812798	292.683574	8.025434
5.671379	289.395382	8.030451
5.801757	291.126437	8.035469
5.691236	294.536229	8.040486
5.904933	289.526158	8.045504
5.809859	299.074631	8.050522
5.872110	300.709065	8.055539
5.974697	292.093594	8.060557
6.061105	288.438352	8.065574
6.026147	289.917605	8.070592
5.951004	291.497828	8.075610
5.944116	302.764995	8.080627
5.854491	295.634443	8.085645
5.693361	305.439418	8.090662
6.197445	297.379565	8.095680
5.885895	300.003515	8.100698
5.790591	296.313628	8.105715
6.274300	285.123307	8.110733
5.711931	298.992643	8.115750
5.857557	295.915092	8.120768
6.023435	294.071425	8.125786
5.858486	295.031411	8.130803
6.363528	288.483020	8.135821
6.029005	297.879664	8.140838
6.107949	289.031217	8.145856
6.083616	294.734363	8.150874
5.863810	300.950968	8.155891
6.334460	288.266862	8.160909
6.061509	296.315819	8.165926
6.256491	293.845907	8.170944
6.216686	293.460869	8.175962
6.207927	296.482338	8.180979
6.221432	295.003366	8.185997
5.977028	298.187987	8.191014
6.251799	300.745317	8.196032
6.405596	296.094919	8.201050
6.165048	293.920462	8.206067
6.237007	288.983091	8.211085
5.924315	295.816997	8.216102
6.093751	291.138904	8.221120
5.941046	288.802364	8.226138
5.641780	294.472848	8.231155
5.988447	285.733931	8.236173
5.786351	302.125072	8.241190
5.738248	296.288186	8.246208
6.045562	311.245700	8.251226
6.143787	311.782606	8.256243
6.237969	318.265597	8.261261
6.380828	323.289312	8.266278
6.322483	322.096147	8.271296
6.066044	316.386570	8.276314
6.180391	315.074831	8.281331
6.297561	315.182741	8.286349
6.115267	317.224716	8.291366
6.149154	321.432385	8.296384
6.232498	317.269539	8.301402
6.018190	322.765777	8.306419
6.411564	316.724015	8.311437
6.146596	320.580883	8.316454
6.417043	313.163536	8.321472
6.457780	321.223314	8.326490
6.136367	308.467640	8.331507
6.233511	304.959033	8.336525
6.321102	309.426524	8.341542
6.151424	317.061683	8.346560
6.249348	316.702400	8.351578
6.353743	323.950642	8.356595
6.610401	312.218376	8.361613
5.929226	310.690459	8.366630
6.080819	313.443813	8.371648
6.483370	326.079558	8.376666
6.272142	316.639099	8.381683
6.063414	308.618344	8.386701
5.965571	315.570071	8.391718
6.468546	314.225842	8.396736
6.258978	327.579181	8.401754
6.239057	315.893403	8.406771
6.084304	319.152342	8.411789
6.422171	320.096663	8.416806
6.667057	321.418464	8.421824
6.700501	323.514999	8.426842
6.168646	328.155290	8.431859
6.385936	318.956952	8.436877
6.326317	323.523250	8.441894
6.287634	314.043134	8.446912
6.382672	310.894613	8.451930
6.469652	315.084494	8.456947
6.387021	317.940818	8.461965
6.536295	322.979308	8.466982
6.122949	318.780678	8.472000
6.573256	314.247916	8.477018
6.418064	309.608059	8.482035
6.710019	314.829314	8.487053
6.211045	323.058862	8.492070
6.464421	324.098471	8.497088
6.471283	319.852935	8.502106
6.549282	320.172107	8.507123
6.668390	319.828440	8.512141
6.295322	313.843652	8.517158
6.334151	313.733466	8.522176
6.232840	313.064578	8.527194
6.217644	324.465603	8.532211
6.597508	314.623266	8.537229
6.415071	321.660832	8.542246
6.156249	322.001221	8.547264
6.268774	314.488698	8.552282
5.974903	319.640800	8.557299
6.361920	315.395662	8.562317
6.067825	322.494904	8.567335
5.893277	317.608772	8.572352
6.383887	334.787644	8.577370
6.755305	345.260271	8.582387
6.675821	335.616125	8.587405
6.418004	348.071335	8.592423
6.247092	348.543116	8.597440
6.670230	340.341294	8.602458
6.644490	340.935493	8.607475
6.372920	347.078175	8.612493
6.598142	346.632675	8.617511
6.432245	347.346663	8.622528
6.466842	352.702927	8.627546
6.340847	350.886050	8.632563
6.728999	343.945703	8.637581
6.473153	344.112059	8.642599
6.633241	352.781148	8.647616
6.750884	351.727662	8.652634
6.597579	348.021606	8.657651
6.819231	342.085634	8.662669
6.772197	349.950897	8.667687
6.709075	348.464992	8.672704
6.638718	341.328247	8.677722
6.704486	337.856108	8.682739
6.839894	338.305139	8.687757
6.292047	340.464352	8.692775
6.311419	352.510066	8.697792
6.969150	341.330313	8.702810
6.637154	345.671054	8.707827
6.688533	352.567857	8.712845
6.474804	353.693278	8.717863
6.774048	346.050502	8.722880
6.862706	345.171969	8.727898
6.637758	344.333106	8.732915
6.923899	342.562107	8.737933
6.780474	344.781030	8.742951
6.543543	356.349359	8.747968
6.893477	344.933812	8.752986
6.551133	344.927530	8.758003
6.667265	349.466298	8.763021
6.550404	346.505603	8.768039
6.797313	349.348169	8.773056
6.928868	334.599643	8.778074
6.915299	347.455234	8.783091
7.062330	337.501045	8.788109
7.052487	341.620897	8.793127
6.821634	341.032265	8.798144
6.808725	329.023491	8.803162
6.460188	322.138620	8.808179
6.652260	335.763546	8.813197
6.713485	351.008957	8.818215
6.795726	348.196945	8.823232
6.983464	340.309714	8.828250
6.678784	358.086581	8.833267
6.883397	353.693291	8.838285
6.891683	350.454215	8.843303
6.704684	350.133262	8.848320
7.291508	341.419805	8.853338
7.076798	343.435305	8.858355
6.715130	326.851672	8.863373
6.786487	334.247103	8.868391
6.546869	342.843117	8.873408
6.807308	345.169172	8.878426
6.864426	346.794947	8.883443
7.151345	349.246241	8.888461
7.027449	351.364275	8.893479
6.421080	344.491391	8.898496
6.631459	349.971589	8.903514
6.622975	357.152325	8.908531
6.770164	347.952333	8.913549
7.024317	353.646576	8.918567
7.157285	351.697607	8.923584
7.083113	350.478518	8.928602
6.514609	356.064976	8.933619
6.481044	357.326269	8.938637
6.836505	351.337771	8.943655
6.862838	355.455114	8.948672
6.863074	351.832296	8.953690
7.010463	352.721257	8.958707
6.910398	341.426712	8.963725
6.742600	349.796883	8.968743
6.322754	352.390473	8.973760
7.245770	358.399635	8.978778
7.099058	359.700746	8.983795
6.802500	360.592996	8.988813
7.103880	367.728341	8.993831
6.841165	376.280653	8.998848
7.208498	367.099807	9.003866
6.850613	368.635975	9.008883
6.907022	371.678804	9.013901
7.174271	370.018059	9.018919
6.821331	373.437447	9.023936
7.067398	372.613144	9.028954
7.003556	369.142372	9.033971
6.833354	368.193945	9.038989
7.291215	368.463067	9.044007
6.723774	378.770397	9.049024
7.072318	369.280072	9.054042
7.066895	375.475736	9.059059
6.913318	373.811500	9.064077
7.483332	370.680065	9.069095
6.861416	385.906311	9.074112
7.188294	372.657700	9.079130
7.198940	379.251630	9.084147
7.370586	378.076073	9.089165
7.453354	369.072355	9.094183
7.071897	373.013757	9.099200
7.200733	376.117821	9.104218
7.072510	374.048830	9.109235
7.169037	380.979595	9.114253
7.516567	384.648992	9.119271
7.025418	386.856131	9.124288
7.144808	381.453716	9.129306
7.169134	392.154322	9.134323
7.028967	382.507036	9.139341
6.973891	382.910175	9.144359
7.012561	389.752180	9.149376
7.317188	382.474614	9.154394
7.066601	377.044964	9.159411
7.175592	379.811315	9.164429
7.034749	376.866996	9.169447
6.760143	385.869295	9.174464
7.035428	379.909129	9.179482
7.058337	379.530041	9.184499
6.779832	382.202474	9.189517
7.199059	389.959985	9.194535
7.065458	403.995749	9.199552
7.550348	410.357596	9.204570
7.477805	400.743885	9.209587
7.151566	389.289088	9.214605
7.412458	386.856174	9.219623
6.913830	386.899625	9.224640
7.418999	401.078296	9.229658
7.272701	409.258937	9.234675
7.123857	399.840216	9.239693
7.573513	407.959038	9.244711
7.319388	410.245806	9.249728
7.609880	404.696656	9.254746
7.233126	396.235133	9.259763
7.190225	398.403599	9.264781
7.225061	408.632357	9.269799
7.054039	415.314725	9.274816
7.215161	404.149628	9.279834
7.481498	405.812054	9.284851
7.413337	414.617921	9.289869
7.622547	404.458294	9.294887
7.157304	409.009273	9.299904
7.675835	402.458727	9.304922
7.699101	401.151784	9.309939
7.450705	409.320020	9.314957
7.752674	416.777182	9.319975
7.153096	405.522991	9.324992
7.573319	406.151458	9.330010
7.330678	406.019102	9.335027
7.526129	400.686815	9.340045
7.588816	401.664788	9.345063
7.484044	405.348253	9.350080
7.363563	396.357432	9.355098
7.442691	391.636658	9.360115
7.352350	403.062130	9.365133
7.768954	408.361712	9.370151
7.478400	405.377731	9.375168
7.687767	396.401499	9.380186
7.544590	392.558148	9.385203
7.412823	390.726393	9.390221
7.003152	389.020231	9.395239
7.112745	402.140584	9.400256
7.563190	402.688577	9.405274
7.410606	401.819438	9.410291
7.179003	410.436319	9.415309
7.245300	408.046514	9.420327
7.160914	410.773742	9.425344
7.383078	404.029791	9.430362
7.457543	402.213059	9.435379
7.287314	409.665309	9.440397
7.669193	419.126493	9.445415
7.634932	433.553810	9.450432
7.867842	431.005354	9.455450
7.908978	420.928856	9.460467
7.423530	416.015671	9.465485
7.795466	411.971687	9.470503
7.342403	405.219924	9.475520
7.847880	405.513144	9.480538
7.474905	414.537182	9.485555
7.505162	405.027281	9.490573
8.009327	410.085928	9.495591
7.648631	418.098195	9.500608
7.391070	412.701185	9.505626
7.766959	414.665181	9.510643
7.294958	428.665623	9.515661
7.876419	424.046013	9.520679
8.184342	442.500146	9.525696
7.625713	419.982859	9.530714
7.735956	408.901470	9.535731
7.407838	415.116150	9.540749
7.818898	425.510031	9.545767
7.661821	435.125096	9.550784
8.006597	429.961905	9.555802
8.100372	429.341341	9.560819
7.829100	422.469571	9.565837
8.133722	407.498209	9.570855
7.379499	414.417120	9.575872
7.279227	408.673577	9.580890
7.829146	415.337658	9.585907
7.658580	422.392338	9.590925
7.767042	424.076347	9.595943
7.977754	433.816820	9.600960
8.075232	430.926669	9.605978
8.068285	413.627818	9.610995
7.690515	417.900009	9.616013
7.785369	410.838335	9.621031
7.940366	414.493724	9.626048
7.812418	409.303622	9.631066
7.562880	408.623242	9.636083
7.601849	418.936565	9.641101
7.827478	424.528004	9.646119
7.620199	438.436484	9.651136
8.001808	438.594480	9.656154
8.043629	442.987125	9.661171
8.034779	431.422612	9.666189
8.124720	428.836598	9.671207
7.788030	419.444143	9.676224
7.923057	424.510140	9.681242
8.046760	421.183540	9.686259
7.784674	423.339014	9.691277
7.804538	418.561248	9.696295
7.885618	430.701487	9.701312
7.914740	444.011202	9.706330
8.023643	444.600088	9.711347
7.767144	445.855291	9.716365
7.903869	438.105397	9.721383
7.791326	439.565261	9.726400
7.627514	435.037173	9.731418
7.952940	434.112072	9.736435
7.927123	438.070348	9.741453
7.833338	436.264195	9.746471
7.673108	445.977589	9.751488
7.918947	443.685880	9.756506
8.322687	442.391904	9.761523
7.943142	451.069853	9.766541
8.002031	443.802364	9.771559
8.117611	444.308152	9.776576
7.938004	445.469258	9.781594
8.144758	443.432979	9.786611
7.687653	446.262792	9.791629
7.733392	444.747200	9.796647
7.940966	443.638593	9.801664
8.180106	456.028636	9.806682
8.242179	466.795956	9.811699
8.007116	456.431356	9.816717
8.022334	447.674866	9.821735
8.022386	451.054740	9.826752
7.899118	468.399352	9.831770
8.208116	462.014157	9.836787
8.336417	472.184127	9.841805
8.045284	458.369568	9.846823
8.224321	469.598242	9.851840
8.011615	464.822190	9.856858
8.265136	460.866175	9.861875
8.058831	472.612817	9.866893
8.269777	464.759764	9.871911
8.350248	469.771206	9.876928
8.276453	468.438441	9.881946
8.323996	464.599906	9.886963
7.869857	468.344435	9.891981
8.333264	468.230840	9.896999
8.312209	472.298831	9.902016
8.133155	465.504113	9.907034
8.274967	465.346233	9.912051
7.919382	467.629970	9.917069
8.100655	471.817737	9.922087
8.098435	470.751467	9.927104
7.861084	468.816328	9.932122
8.160742	468.911425	9.937139
8.059352	473.108767	9.942157
7.683384	471.848594	9.947175
8.165645	484.755983	9.952192
8.050529	493.288380	9.957210
8.323815	496.253068	9.962227
8.272107	503.831954	9.967245
8.354384	498.807702	9.972263
8.119352	501.864659	9.977280
7.821383	498.727189	9.982298
8.395030	499.034977	9.987315
8.094081	500.357109	9.992333
8.224104	493.169972	9.997351
8.642255	502.227887	10.002368
8.564505	497.033050	10.007386
8.694791	499.379519	10.012403
8.545551	500.810424	10.017421
8.319446	499.927553	10.022439
8.455783	491.884208	10.027456
8.387820	492.159981	10.032474
8.674331	495.217271	10.037491
8.398392	503.670729	10.042509
8.648223	498.535019	10.047527
8.696612	508.414574	10.052544
8.463432	506.055900	10.057562
8.830219	498.828509	10.062579
8.355833	506.034966	10.067597
8.508831	492.283337	10.072615
8.574983	502.384167	10.077632
8.641642	504.409247	10.082650
8.620892	499.732496	10.087667
8.628110	500.555065	10.092685
8.475538	485.961385	10.097703
8.694726	476.182005	10.102720
8.642259	482.495529	10.107738
8.288241	467.516863	10.112755
8.523116	477.092628	10.117773
8.477492	498.619147	10.122791
8.801458	501.471754	10.127808
8.298753	498.959652	10.132826
8.648337	493.388593	10.137843
8.354429	508.882285	10.142861
8.831957	508.996851	10.147879
8.936927	508.248298	10.152896
8.449731	507.466295	10.157914
8.863498	493.828441	10.162931
8.606412	491.546098	10.167949
8.459619	487.441362	10.172967
8.533450	485.182910	10.177984
8.680168	510.961714	10.183002
8.895382	503.565566	10.188019
8.281628	506.312635	10.193037
8.702437	507.701560	10.198055
8.672050	512.667268	10.203072
8.341116	509.314056	10.208090
8.254117	507.633064	10.213107
7.936106	508.617044	10.218125
8.308314	503.815606	10.223143
8.630734	504.623503	10.228160
8.745118	524.004289	10.233178
8.849956	528.014697	10.238195
8.880921	526.936913	10.243213
8.850049	520.885815	10.248231
8.884877	500.307775	10.253248
8.583394	509.973908	10.258266
8.513036	505.835101	10.263283
8.685416	517.320468	10.268301
8.709042	523.855613	10.273319
9.049588	525.017275	10.278336
8.665947	534.175587	10.283354
9.041315	523.058898	10.288371
8.965028	533.775353	10.293389
8.873440	522.220590	10.298407
8.846677	523.790096	10.303424
8.639551	535.038291	10.308442
8.998187	528.702100	10.313459
8.975975	526.092618	10.318477
8.657141	533.429348	10.323495
8.981013	528.764865	10.328512
8.754790	534.966778	10.333530
8.810548	528.826365	10.338547
9.000672	534.792629	10.343565
8.991674	538.934485	10.348583
9.198310	532.855637	10.353600
9.080753	542.843263	10.358618
8.926061	526.280663	10.363635
8.597738	530.548289	10.368653
8.760349	532.460509	10.373671
9.007546	531.951602	10.378688
8.654609	529.791569	10.383706
9.053252	540.193774	10.388723
8.865008	540.860778	10.393741
8.806654	539.897973	10.398759
9.053812	530.047909	10.403776
8.838207	532.994530	10.408794
8.748093	528.338107	10.413811
8.906430	534.091603	10.418829
8.753529	528.930622	10.423847
9.158798	530.577604	10.428864
9.056850	539.527681	10.433882
9.205519	535.076839	10.438899
9.122335	537.753405	10.443917
8.789835	541.169622	10.448935
8.973763	529.988250	10.453952
8.856054	538.353818	10.458970
9.235939	532.973658	10.463987
9.281644	533.452528	10.469005
9.228178	531.917758	10.474023
9.118888	529.438685	10.479040
8.826056	532.719297	10.484058
8.951327	543.811275	10.489075
9.184527	548.606306	10.494093
8.979339	555.335104	10.499111
8.896884	552.056560	10.504128
9.031351	565.734868	10.509146
9.129483	557.899451	10.514163
9.488088	562.330854	10.519181
8.903032	565.900255	10.524199
8.940771	553.842370	10.529216
9.266206	567.244606	10.534234
9.290014	563.356119	10.539251
9.406257	568.103208	10.544269
9.410230	564.284101	10.549287
9.627196	563.874604	10.554304
9.753925	561.778267	10.559322
9.515514	566.451536	10.564339
9.452431	553.327007	10.569357
9.115937	544.395203	10.574375
9.552051	547.713083	10.579392
9.118694	544.139228	10.584410
9.228008	543.049166	10.589427
9.713837	557.391939	10.594445
9.250706	550.430259	10.599463
9.254934	548.457260	10.604480
9.235031	553.645398	10.609498
9.392945	557.461304	10.614515
9.213822	560.862961	10.619533
9.319944	565.302366	10.624551
9.452062	551.998931	10.629568
9.137864	556.056067	10.634586
9.335483	558.164775	10.639603
9.534221	552.898199	10.644621
9.524054	565.371562	10.649639
9.545960	556.509829	10.654656
9.533851	561.737774	10.659674
9.534142	557.789858	10.664691
9.769917	550.800723	10.669709
9.406734	567.630756	10.674727
9.613967	561.643323	10.679744
9.485573	553.275356	10.684762
8.998396	554.809707	10.689779
9.151045	558.023681	10.694797
9.330717	558.352173	10.699815
9.315837	559.916665	10.704832
9.585012	551.413823	10.709850
9.312002	550.367886	10.714867
9.654439	557.380110	10.719885
9.281153	567.234249	10.724903
9.416412	555.568181	10.729920
9.367304	560.943934	10.734938
9.358050	559.389611	10.739955
9.525166	557.432114	10.744973
9.239385	564.375514	10.749991
9.518619	567.433956	10.755008
9.466606	573.911544	10.760026
9.774327	579.076758	10.765043
9.721684	578.463351	10.770061
9.572244	578.581478	10.775079
9.926015	576.840886	10.780096
9.668678	579.554212	10.785114
9.412432	576.659500	10.790131
9.384331	575.767692	10.795149
9.523750	583.395560	10.800167
9.641407	579.751142	10.805184
9.819256	580.086232	10.810202
9.784703	583.537825	10.815219
9.795540	570.057719	10.820237
9.646512	584.335882	10.825255
9.732012	576.290997	10.830272
9.914980	581.800807	10.835290
9.658857	581.657938	10.840307
9.787481	579.624419	10.845325
9.378623	583.131503	10.850343
9.706568	582.098702	10.855360
9.439122	578.057031	10.860378
9.695144	581.305305	10.865395
9.479560	577.571089	10.870413
9.736611	581.545037	10.875431
9.705020	584.636404	10.880448
9.741824	581.298144	10.885466
9.562017	581.143318	10.890483
9.921500	583.819960	10.895501
10.042012	597.797126	10.900519
10.238178	586.115183	10.905536
10.018458	589.797762	10.910554
9.820290	583.981138	10.915571
9.864304	576.283580	10.920589
9.727248	578.605675	10.925607
9.793289	572.233262	10.930624
9.991957	585.731113	10.935642
9.529554	585.232401	10.940659
9.866567	593.249036	10.945677
10.251284	606.676726	10.950695
10.199642	605.346792	10.955712
10.032418	599.291785	10.960730
10.051950	593.680890	10.965747
10.465923	582.633855	10.970765
9.713590	578.049620	10.975783
9.878434	576.569003	10.980800
9.875098	580.088288	10.985818
9.540588	597.582888	10.990835
9.962964	602.692275	10.995853
10.291527	602.565094	11.000871
10.055384	609.980417	11.005888
10.118568	618.740558	11.010906
10.303875	608.016515	11.015923
10.250764	611.979106	11.020941
10.084399	609.556301	11.025959
10.255188	594.687804	11.030976
10.226598	590.706536	11.035994
9.857298	587.662278	11.041011
10.026896	595.938675	11.046029
9.834508	603.179882	11.051047
10.140820	605.385175	11.056064
10.035009	604.294103	11.061082
9.902037	604.012017	11.066099
9.874160	602.246014	11.071117
10.098260	606.619607	11.076135
9.734359	614.610373	11.081152
10.005719	611.156461	11.086170
10.164044	613.081984	11.091187
10.381492	595.441685	11.096205
10.562882	612.243240	11.101223
10.359250	608.150538	11.106240
10.454048	609.981872	11.111258
10.512311	611.033135	11.116275
10.672725	603.642376	11.121293
9.995953	609.974867	11.126311
10.048315	605.488605	11.131328
10.353140	597.396723	11.136346
10.213906	613.920311	11.141363
10.563936	601.469480	11.146381
10.292310	610.282075	11.151399
10.389848	606.631336	11.156416
10.475929	608.344116	11.161434
10.185768	614.840097	11.166451
10.784980	600.422022	11.171469
10.240515	603.502232	11.176487
10.346349	610.232812	11.181504
10.378921	604.869179	11.186522
10.280586	607.450299	11.191539
10.297906	610.543475	11.196557
10.520504	620.919661	11.201575
10.121886	609.725373	11.206592
10.399091	609.779808	11.211610
9.882146	619.899482	11.216627
10.402917	600.535916	11.221645
10.268995	619.062616	11.226663
10.420390	626.928468	11.231680
10.952915	629.653744	11.236698
10.389870	625.797233	11.241715
10.371097	620.163929	11.246733
10.841842	635.780920	11.251751
10.033385	623.356954	11.256768
10.302652	625.801584	11.261786
10.175798	634.474743	11.266803
10.247400	633.677764	11.271821
10.591375	642.327649	11.276839
10.353424	635.592588	11.281856
10.555412	627.466312	11.286874
10.340345	640.678734	11.291891
10.534944	631.275508	11.296909
10.809533	641.059734	11.301927
10.485523	636.695552	11.306944
10.810617	631.734204	11.311962
10.556077	636.769781	11.316979
10.805341	634.913014	11.321997
10.795250	630.966708	11.327015
10.370266	641.892497	11.332032
10.716758	638.016552	11.337050
10.488315	643.515102	11.342067
10.481337	627.348988	11.347085
10.623159	646.226989	11.352103
10.447815	654.699471	11.357120
10.791513	655.769130	11.362138
10.549055	666.609531	11.367155
10.893802	667.079420	11.372173
11.155290	666.249532	11.377191
10.989322	656.394700	11.382208
10.626678	641.534004	11.387226
10.621720	652.794779	11.392243
10.691087	648.974875	11.397261
10.748574	661.639677	11.402279
10.683227	667.169485	11.407296
10.841243	660.937265	11.412314
10.702318	664.212722	11.417331
11.161602	659.299769	11.422349
10.891416	660.093226	11.427367
10.749754	665.202643	11.432384
10.799670	660.044561	11.437402
10.539661	662.745695	11.442419
10.871984	654.886165	11.447437
11.004251	660.123075	11.452455
10.835846	661.137271	11.457472
10.842705	660.965821	11.462490
10.567126	666.124623	11.467507
10.582627	657.443726	11.472525
10.635011	670.465941	11.477543
10.745293	665.730747	11.482560
10.961289	672.188468	11.487578
10.797470	685.007883	11.492595
10.692004	686.438255	11.497613
11.037695	688.874076	11.502631
10.758431	692.625965	11.507648
11.205021	688.485015	11.512666
10.945977	692.467268	11.517683
10.864972	693.780198	11.522701
11.456392	694.309269	11.527719
11.322315	700.301139	11.532736
11.245528	690.823638	11.537754
11.009085	700.549111	11.542771
11.474729	693.621735	11.547789
11.221145	697.599977	11.552807
10.861170	692.597627	11.557824
11.202951	690.224582	11.562842
11.077484	693.340144	11.567859
10.976302	691.339462	11.572877
11.329013	689.583247	11.577895
11.495137	700.744662	11.582912
11.602734	694.529797	11.587930
11.103553	688.593044	11.592947
11.263985	688.018832	11.597965
11.125633	683.726535	11.602983
10.962017	697.208649	11.608000
11.004769	692.250497	11.613018
11.114949	702.918903	11.618035
11.498463	689.004772	11.623053
11.302851	688.562085	11.628071
11.511499	700.082912	11.633088
11.655375	685.957020	11.638106
11.304369	690.199835	11.643123
11.386916	686.993244	11.648141
11.515833	679.238158	11.653159
11.250651	689.930654	11.658176
11.524825	693.696816	11.663194
11.438431	692.088296	11.668211
11.275101	678.670111	11.673229
11.575898	683.347288	11.678247
11.250703	672.144612	11.683264
11.291482	679.693302	11.688282
11.318471	686.354213	11.693299
11.304850	690.752450	11.698317
11.171647	686.863291	11.703335
11.191742	697.463756	11.708352
11.346474	683.459242	11.713370
11.120983	694.612584	11.718387
11.290066	695.359308	11.723405
11.590163	693.302065	11.728423
11.272029	695.377989	11.733440
11.424020	696.057963	11.738458
11.611377	703.069296	11.743475
11.437236	699.072939	11.748493
11.442656	693.000317	11.753511
11.314053	697.678505	11.758528
11.364960	690.109207	11.763546
11.265328	699.778530	11.768563
11.785165	715.040758	11.773581
11.839027	721.255655	11.778599
11.544514	707.125850	11.783616
11.569367	697.080150	11.788634
11.618284	702.910805	11.793651
11.454154	713.568547	11.798669
11.675011	714.799468	11.803687
11.830781	715.630330	11.808704
11.917510	716.475165	11.813722
11.637420	712.242939	11.818739
11.607506	697.424739	11.823757
11.911773	710.789373	11.828775
11.493112	709.706287	11.833792
11.716076	714.001188	11.838810
12.138936	707.449743	11.843827
11.620995	702.639399	11.848845
11.872605	704.443018	11.853863
11.663478	714.975266	11.858880
11.255814	704.741708	11.863898
11.509410	712.418014	11.868915
11.572515	716.630665	11.873933
11.807677	722.002952	11.878951
11.428748	723.012266	11.883968
11.868366	719.973787	11.888986
11.433735	723.216690	11.894003
11.480337	724.471760	11.899021
11.549037	731.192424	11.904039
11.820881	746.042251	11.909056
12.108756	747.881218	11.914074
12.164540	744.899719	11.919091
12.248611	729.656530	11.924109
12.203506	728.735820	11.929127
11.791667	723.640601	11.934144
11.858175	722.115419	11.939162
12.038989	721.878843	11.944179
11.937188	711.695187	11.949197
11.994771	710.468053	11.954215
11.995013	720.746592	11.959232
11.510397	720.570095	11.964250
11.935212	723.378534	11.969267
12.331313	742.731197	11.974285
12.477345	735.424689	11.979303
12.118858	724.444948	11.984320
11.865816	716.206889	11.989338
12.148127	710.551629	11.994355
11.763720	718.662419	11.999373
11.988201	718.210716	12.004391
12.052810	733.115093	12.009408
12.184930	738.219504	12.014426
12.324714	749.189414	12.019443
12.305199	742.470580	12.024461
12.112416	723.310202	12.029479
12.070679	721.006712	12.034496
12.234207	729.867950	12.039514
12.211056	718.220286	12.044531
12.019680	729.213668	12.049549
12.454402	728.905750	12.054567
12.056727	731.442269	12.059584
12.388754	729.531499	12.064602
12.473843	740.506818	12.069619
11.889806	742.236243	12.074637
12.378322	720.819997	12.079655
12.198928	736.532630	12.084672
12.509287	734.931371	12.089690
12.474021	722.468240	12.094707
12.150080	719.887071	12.099725
12.357222	714.085796	12.104743
12.411396	719.035155	12.109760
12.188439	725.760489	12.114778
12.331530	727.331803	12.119795
12.349266	738.371323	12.124813
12.500470	732.279002	12.129831
12.285577	739.574284	12.134848
12.514436	750.274615	12.139866
12.453463	729.932230	12.144883
12.218440	743.450815	12.149901
12.458175	749.311548	12.154919
12.545326	746.315666	12.159936
12.160716	750.551137	12.164954
12.197463	746.042039	12.169971
12.529412	742.790050	12.174989
12.822649	742.254989	12.180007
12.110567	745.557147	12.185024
12.404713	743.415623	12.190042
12.600849	742.289856	12.195059
12.174697	744.625710	12.200077
12.374296	741.495444	12.205095
12.411592	749.805266	12.210112
12.213157	744.518812	12.215130
12.464698	737.255732	12.220147
12.140566	749.611157	12.225165
12.529566	761.974777	12.230183
12.429339	770.050533	12.235200
12.497793	768.057978	12.240218
13.011189	766.241865	12.245235
12.280211	775.653538	12.250253
12.660585	767.167886	12.255271
12.870196	770.129974	12.260288
12.798169	781.312974	12.265306
12.928284	773.945827	12.270323
12.681320	770.674084	12.275341
12.950694	766.491454	12.280359
12.883353	766.805004	12.285376
12.818866	771.040816	12.290394
12.791309	772.487390	12.295411
12.684051	773.002857	12.300429
13.104320	770.781608	12.305447
12.973107	763.124048	12.310464
12.760502	740.580542	12.315482
12.860536	749.066727	12.320499
12.819157	752.468929	12.325517
12.812913	755.811977	12.330535
12.981320	750.420706	12.335552
12.556467	757.007270	12.340570
13.209451	762.853752	12.345587
12.881199	767.607422	12.350605
12.954168	770.499399	12.355623
12.889860	770.525293	12.360640
12.813119	765.450142	12.365658
12.888646	772.217090	12.370675
12.355037	770.271530	12.375693
12.878457	768.097236	12.380711
12.767265	770.487887	12.385728
12.508643	766.558401	12.390746
12.835824	772.629505	12.395763
12.730479	778.951418	12.400781
12.817751	772.932217	12.405799
12.792962	781.684131	12.410816
13.032314	787.671170	12.415834
13.002813	794.716518	12.420851
13.231359	805.404308	12.425869
13.062972	802.524196	12.430887
12.946006	804.903133	12.435904
12.964346	802.104218	12.440922
13.329695	796.271817	12.445939
12.954184	800.499562	12.450957
12.874808	797.911621	12.455975
13.014958	795.734258	12.460992
13.116052	799.530717	12.466010
13.011622	799.528182	12.471027
13.255743	803.040297	12.476045
13.248610	803.025674	12.481063
12.957585	803.320622	12.486080
12.826967	808.601921	12.491098
12.821662	803.430359	12.496115
12.646511	801.665320	12.501133
13.482062	817.411507	12.506151
13.219830	826.052321	12.511168
13.126902	831.728514	12.516186
13.218848	831.559509	12.521203
12.975593	839.064405	12.526221
13.126563	828.733780	12.531239
13.432121	826.035029	12.536256
12.978316	831.442713	12.541274
13.309199	826.470937	12.546291
13.049735	834.499086	12.551309
13.361042	828.435297	12.556327
13.400055	830.957058	12.561344
13.128519	842.578461	12.566362
13.463033	845.328484	12.571379
13.787154	853.669153	12.576397
14.079507	858.117322	12.581415
13.451385	837.336650	12.586432
13.462718	840.203581	12.591450
13.528265	830.968796	12.596467
13.710581	833.938327	12.601485
13.630451	826.007645	12.606503
13.492396	830.106672	12.611520
13.469715	831.217967	12.616538
13.240793	833.601827	12.621555
13.405692	831.161802	12.626573
13.388639	831.719942	12.631591
13.655231	845.945816	12.636608
13.448812	854.271781	12.641626
13.848000	854.398625	12.646643
13.819433	851.228349	12.651661
13.767049	850.308774	12.656679
13.877699	843.771483	12.661696
13.562499	841.684395	12.666714
14.018741	836.017623	12.671731
13.600696	836.263045	12.676749
13.866374	824.276562	12.681767
13.711051	833.800046	12.686784
14.000650	823.633898	12.691802
13.748390	823.244265	12.696819
13.512613	824.354234	12.701837
13.512718	830.839527	12.706855
14.068030	837.455586	12.711872
13.827421	842.877207	12.716890
13.881293	837.727921	12.721907
14.015985	843.898637	12.726925
13.760450	841.284641	12.731943
13.969460	827.041134	12.736960
13.544903	835.600087	12.741978
13.825588	839.409442	12.746995
13.949906	850.274538	12.752013
13.647156	853.468398	12.757031
14.313834	850.773024	12.762048
14.237250	852.015845	12.767066
13.998069	836.173107	12.772083
13.689951	841.539032	12.777101
13.929196	848.599098	12.782119
13.801922	848.903105	12.787136
13.764207	856.748194	12.792154
13.848904	848.602326	12.797171
13.913105	849.980880	12.802189
14.379025	860.066614	12.807207
14.253632	859.177412	12.812224
14.160961	856.632572	12.817242
14.297552	854.297967	12.822259
14.220820	856.266658	12.827277
14.175163	847.888745	12.832295
14.402693	852.047263	12.837312
13.834210	854.339159	12.842330
14.059910	843.321463	12.847347
13.955513	850.315450	12.852365
14.044706	853.940213	12.857383
14.531074	850.746062	12.862400
13.832575	853.197187	12.867418
14.321259	849.008579	12.872435
14.100061	858.848515	12.877453
13.715240	854.506430	12.882471
14.437110	860.017098	12.887488
14.040543	855.405450	12.892506
14.183028	844.706909	12.897523
13.979417	854.692413	12.902541
13.558761	854.379658	12.907559
14.194706	873.975754	12.912576
14.499510	883.704886	12.917594
14.671456	877.233719	12.922611
14.407583	883.157623	12.927629
14.363771	889.498337	12.932647
14.212267	882.178427	12.937664
14.464628	884.840340	12.942682
14.458408	877.860592	12.947699
14.503763	875.830619	12.952717
14.508954	883.489114	12.957735
14.620359	888.287539	12.962752
14.514272	886.672620	12.967770
14.873776	877.552701	12.972787
14.621988	878.785105	12.977805
14.351618	879.509171	12.982823
14.695476	879.632061	12.987840
14.462843	881.514726	12.992858
14.328711	873.914381	12.997875
14.688923	876.433161	13.002893
14.511252	874.352924	13.007911
14.750850	876.855888	13.012928
14.085359	884.572129	13.017946
14.668603	872.573728	13.022963
14.694031	871.439985	13.027981
14.565596	877.917032	13.032999
14.437179	877.081953	13.038016
14.548740	879.854291	13.043034
14.310353	881.043569	13.048051
14.530352	880.359030	13.053069
14.416220	881.778152	13.058087
14.754312	884.013216	13.063104
14.365816	890.445807	13.068122
14.783163	894.716608	13.073139
15.156221	894.664506	13.078157
15.085592	901.766833	13.083175
14.838664	874.441094	13.088192
14.814557	885.682924	13.093210
14.745823	870.157438	13.098227
14.792119	881.445040	13.103245
14.911939	891.458784	13.108263
15.108041	890.405598	13.113280
14.792282	889.218013	13.118298
14.873140	883.184000	13.123315
14.903612	891.441307	13.128333
14.883283	900.691206	13.133351
15.049542	899.387070	13.138368
14.837536	895.762681	13.143386
15.091994	903.009737	13.148403
15.108717	909.868003	13.153421
14.715202	900.648303	13.158439
14.944766	908.233783	13.163456
14.857261	909.913828	13.168474
14.742510	898.441347	13.173491
14.955020	906.098927	13.178509
14.821141	902.702142	13.183527
14.780024	906.435697	13.188544
14.873773	906.086525	13.193562
15.059372	903.990392	13.198579
15.014564	900.548093	13.203597
15.016843	909.750272	13.208615
15.090691	909.173840	13.213632
14.772623	932.725450	13.218650
15.346680	931.187001	13.223667
15.223093	922.401533	13.228685
15.212463	931.091339	13.233703
15.625239	925.671196	13.238720
15.311360	931.637665	13.243738
15.655206	931.788960	13.248755
15.448888	921.924525	13.253773
15.227467	912.728348	13.258791
15.528139	905.252372	13.263808
15.191915	905.390299	13.268826
15.233448	908.009508	13.273843
15.199313	903.129618	13.278861
15.301764	924.551396	13.283879
15.540452	924.807532	13.288896
15.737306	931.454542	13.293914
14.993898	915.400397	13.298931
15.584554	919.410516	13.303949
15.625085	929.812253	13.308967
15.800209	927.903956	13.313984
15.254812	915.694192	13.319002
15.273198	913.018331	13.324019
15.493982	918.471827	13.329037
15.302313	924.049909	13.334055
15.810012	922.723833	13.339072
15.709729	923.844137	13.344090
15.437489	931.729161	13.349107
15.570320	931.777816	13.354125
15.566086	936.666958	13.359143
15.458265	932.098413	13.364160
15.709287	941.507793	13.369178
15.627481	937.569500	13.374195
15.807581	932.987401	13.379213
15.461804	941.313149	13.384231
15.659751	934.430780	13.389248
15.939977	926.961154	13.394266
15.705654	926.442474	13.399283
15.748509	926.202264	13.404301
15.809883	930.882305	13.409319
15.797780	924.108592	13.414336
15.743349	930.065969	13.419354
15.855222	932.642602	13.424371
16.151249	927.180789	13.429389
15.796215	936.252770	13.434407
15.707336	924.198695	13.439424
15.632497	934.580641	13.444442
15.743487	929.933630	13.449459
15.723624	931.830301	13.454477
15.990026	924.609000	13.459495
15.840099	923.979265	13.464512
15.384318	931.829929	13.469530
15.879549	930.824549	13.474547
15.903128	926.109182	13.479565
15.842855	938.186704	13.484583
15.691267	924.608702	13.489600
15.637382	939.749571	13.494618
15.697829	943.072737	13.499635
16.182236	956.008535	13.504653
16.127879	960.962343	13.509671
16.246712	956.897933	13.514688
16.030515	959.942549	13.519706
16.054440	963.097868	13.524723
16.310546	960.416312	13.529741
16.159121	960.212853	13.534759
16.278549	948.750986	13.539776
15.957790	944.073787	13.544794
16.155166	946.681208	13.549811
16.344507	958.937390	13.554829
16.107304	964.819271	13.559847
16.335302	953.277273	13.564864
16.135983	964.521358	13.569882
16.017807	951.979538	13.574899
16.395794	955.988272	13.579917
16.682861	964.808180	13.584935
16.493131	949.595080	13.589952
16.207843	941.402995	13.594970
16.288480	945.874891	13.599987
16.212535	957.399448	13.605005
15.993761	965.168810	13.610023
16.089341	957.734414	13.615040
16.271545	968.852451	13.620058
16.587035	955.504206	13.625075
16.521308	950.231613	13.630093
16.126765	957.618248	13.635111
16.536986	951.103409	13.640128
16.393767	954.609970	13.645146
16.406607	950.609506	13.650163
16.528532	949.567939	13.655181
16.235244	963.584978	13.660199
16.237983	954.312632	13.665216
16.144991	954.977350	13.670234
16.265956	959.708024	13.675251
16.311955	970.733791	13.680269
16.545727	983.178692	13.685287
16.416195	985.212475	13.690304
16.462879	987.591043	13.695322
16.580407	994.272597	13.700339
16.540474	984.290537	13.705357
16.305684	988.985438	13.710375
16.614060	983.657376	13.715392
16.679637	986.140283	13.720410
16.702722	985.410852	13.725427
16.543720	985.805041	13.730445
16.906103	988.913646	13.735463
16.829901	987.679051	13.740480
17.108963	980.402095	13.745498
17.069528	987.404892	13.750515
16.927785	987.316683	13.755533
16.629835	986.896334	13.760551
16.493257	984.610825	13.765568
17.049895	977.460796	13.770586
16.807109	983.804316	13.775603
16.872264	971.931206	13.780621
16.779206	982.574816	13.785639
16.427122	978.682018	13.790656
17.044340	970.888168	13.795674
16.962598	986.087092	13.800691
17.024207	986.228959	13.805709
16.760224	994.936401	13.810727
16.880104	987.495030	13.815744
17.144144	988.211108	13.820762
17.025096	1006.095235	13.825779
17.293406	995.490502	13.830797
17.049208	996.093704	13.835815
17.011092	1008.167802	13.840832
17.397641	1001.050725	13.845850
17.116301	1005.724521	13.850867
17.075012	990.320867	13.855885
17.119661	982.641970	13.860903
16.981210	995.018965	13.865920
17.160540	1002.896385	13.870938
17.086436	1002.390469	13.875955
17.234630	998.472932	13.880973
17.405548	996.416960	13.885991
17.300976	1007.611512	13.891008
17.548415	1006.853240	13.896026
17.180713	1010.644298	13.901043
17.680467	1003.171804	13.906061
17.733677	1002.557576	13.911079
17.174599	991.798452	13.916096
17.128364	985.430861	13.921114
16.792236	989.226435	13.926131
17.461576	994.499218	13.931149
17.506876	1004.568884	13.936167
17.742963	1008.962789	13.941184
17.773371	1004.075914	13.946202
17.326840	998.556852	13.951219
17.630198	1001.554784	13.956237
17.747609	994.984819	13.961255
17.315161	988.270630	13.966272
17.289967	989.483317	13.971290
17.219540	995.323298	13.976307
17.368608	991.156311	13.981325
17.769326	1004.723810	13.986343
17.672554	1003.101108	13.991360
17.852660	998.724124	13.996378
17.830595	1005.238201	14.001395
17.734712	1003.549086	14.006413
17.662921	1001.199774	14.011431
17.593270	1001.419014	14.016448
17.615582	999.881798	14.021466
17.547365	1001.085447	14.026483
17.774488	998.575689	14.031501
17.734064	1001.564368	14.036519
17.710611	999.295847	14.041536
17.812248	1000.084710	14.046554
17.863949	998.637567	14.051571
18.309310	998.271172	14.056589
17.987298	1009.364091	14.061607
17.872867	1001.744826	14.066624
18.065396	1001.206602	14.071642
17.877599	1000.320859	14.076659
17.833947	984.289560	14.081677
18.029967	991.113453	14.086695
17.714304	994.647040	14.091712
18.071911	994.897168	14.096730
17.741435	994.876400	14.101747
17.996617	992.333844	14.106765
17.803614	1001.645565	14.111783
17.635583	998.045824	14.116800
17.880904	999.597988	14.121818
17.721517	998.834030	14.126835
17.979502	990.471592	14.131853
18.038271	1001.432260	14.136871
17.508516	997.100225	14.141888
17.627821	995.090210	14.146906
17.978859	1012.118031	14.151923
18.069599	1015.007264	14.156941
18.195818	1023.574685	14.161959
17.818660	1028.295059	14.166976
18.407367	1028.297534	14.171994
17.902907	1024.750500	14.177011
17.875777	1029.621164	14.182029
18.173227	1026.241983	14.187047
17.638287	1029.282901	14.192064
18.118929	1021.074916	14.197082
18.196184	1032.310424	14.202099
18.145512	1024.968345	14.207117
18.243936	1036.680233	14.212135
18.246854	1045.888694	14.217152
18.669165	1047.526744	14.222170
18.575799	1047.011221	14.227187
18.162929	1046.091311	14.232205
18.491518	1052.146511	14.237223
18.262557	1053.741433	14.242240
18.548633	1052.989729	14.247258
18.654602	1051.537234	14.252275
18.624393	1049.721057	14.257293
18.496206	1046.922971	14.262311
18.373300	1050.685151	14.267328
18.857023	1053.872588	14.272346
18.682907	1058.589560	14.277363
18.611910	1051.225407	14.282381
18.647175	1052.681097	14.287399
18.909512	1049.102280	14.292416
18.508049	1043.348918	14.297434
18.670547	1046.788661	14.302451
18.620356	1046.405233	14.307469
18.881822	1051.205438	14.312487
18.699616	1045.771181	14.317504
18.960214	1040.961841	14.322522
18.596236	1041.795256	14.327539
18.624173	1049.131514	14.332557
19.033774	1049.004257	14.337575
19.148408	1058.908452	14.342592
18.825153	1036.949970	14.347610
18.813418	1029.226238	14.352627
18.649618	1023.798571	14.357645
18.930703	1037.097653	14.362663
18.810911	1049.616933	14.367680
18.796496	1051.749455	14.372698
18.932555	1044.062521	14.377715
18.743731	1047.153356	14.382733
18.905411	1043.240008	14.387751
19.109088	1042.242432	14.392768
18.891796	1053.678742	14.397786
18.916695	1047.180059	14.402803
19.172971	1037.101065	14.407821
18.995710	1028.841519	14.412839
18.496163	1039.012352	14.417856
19.152631	1040.500101	14.422874
19.004209	1046.488022	14.427891
18.733944	1048.701657	14.432909
19.080036	1049.294427	14.437927
18.861165	1044.834772	14.442944
19.112746	1046.714173	14.447962
19.162146	1064.426794	14.452979
19.100510	1073.231961	14.457997
19.466217	1074.200366	14.463015
18.861143	1067.226008	14.468032
19.412761	1072.271099	14.473050
19.237748	1070.004225	14.478067
19.131004	1073.552432	14.483085
19.322956	1073.528706	14.488103
19.130321	1070.327293	14.493120
19.378744	1074.028141	14.498138
19.409925	1071.665841	14.503155
19.297309	1074.328163	14.508173
19.591509	1062.255000	14.513191
18.984530	1071.079338	14.518208
19.468068	1069.501410	14.523226
19.477771	1070.705478	14.528243
19.487968	1071.136276	14.533261
19.762530	1068.155160	14.538279
19.248068	1072.830784	14.543296
19.804714	1065.251518	14.548314
19.397910	1068.890920	14.553331
19.441157	1067.441940	14.558349
19.673070	1060.279638	14.563367
19.776096	1065.142542	14.568384
19.578962	1065.801490	14.573402
19.564338	1068.350625	14.578419
19.630287	1069.233448	14.583437
19.555247	1060.749583	14.588455
19.559061	1066.240274	14.593472
20.357176	1082.636365	14.598490
19.768665	1082.349905	14.603507
19.588758	1071.673339	14.608525
19.955509	1064.773939	14.613543
19.679273	1064.798323	14.618560
19.725164	1072.832385	14.623578
19.935900	1086.189865	14.628595
19.869788	1089.605473	14.633613
20.279037	1079.912753	14.638631
19.578547	1079.454484	14.643648
20.097229	1091.293071	14.648666
19.982737	1077.797505	14.653683
19.874080	1086.884609	14.658701
20.099160	1088.465200	14.663719
20.375447	1090.814119	14.668736
20.108611	1079.744058	14.673754
20.225219	1070.930350	14.678771
20.137544	1070.805266	14.683789
20.148079	1054.932676	14.688807
19.941587	1067.456084	14.693824
19.919815	1070.388202	14.698842
20.221228	1075.999531	14.703859
19.989123	1080.024986	14.708877
20.304379	1084.924073	14.713895
20.025700	1090.904015	14.718912
20.383886	1091.504358	14.723930
20.537599	1090.896472	14.728947
19.941876	1095.184035	14.733965
20.267964	1089.979402	14.738983
19.992924	1097.672428	14.744000
20.224998	1093.830093	14.749018
20.380783	1094.856636	14.754035
19.805506	1093.788595	14.759053
19.933229	1089.075804	14.764071
19.973445	1090.262470	14.769088
20.057107	1094.894879	14.774106
20.453811	1105.796351	14.779123
20.046101	1114.027738	14.784141
20.184831	1114.059690	14.789159
20.377584	1115.219302	14.794176
20.298798	1119.791962	14.799194
20.582938	1113.498797	14.804211
20.524396	1124.250695	14.809229
20.677840	1123.112658	14.814247
20.553979	1126.000819	14.819264
20.729993	1121.892697	14.824282
20.859198	1128.130646	14.829299
20.256226	1126.577777	14.834317
20.635060	1127.196978	14.839335
20.245412	1123.493075	14.844352
20.516567	1123.690477	14.849370
20.619572	1125.599477	14.854387
20.924612	1129.954206	14.859405
21.009656	1129.896736	14.864423
20.943965	1123.263892	14.869440
20.669847	1112.412709	14.874458
20.930680	1111.848000	14.879475
20.875030	1114.674976	14.884493
21.065057	1109.087701	14.889511
20.856943	1119.074057	14.894528
20.643701	1120.477167	14.899546
21.000311	1124.230505	14.904563
20.909889	1137.733042	14.909581
21.216041	1131.729921	14.914599
21.160155	1118.761645	14.919616
20.752550	1117.361209	14.924634
21.060913	1131.981566	14.929651
21.352957	1138.566401	14.934669
21.354526	1125.213565	14.939687
21.116203	1128.185934	14.944704
20.834209	1117.033015	14.949722
20.958891	1120.971018	14.954739
20.628702	1137.704895	14.959757
20.994420	1143.151530	14.964775
21.397015	1142.062820	14.969792
21.085815	1136.017565	14.974810
21.232380	1130.440249	14.979827
20.977554	1136.877231	14.984845
21.168866	1131.286591	14.989863
21.502003	1137.890235	14.994880
21.175725	1142.735214	14.999898
21.593746	1138.194683	15.004915
21.427491	1142.168807	15.009933
21.318987	1140.459566	15.014951
21.461078	1137.622274	15.019968
21.589712	1136.011582	15.024986
21.586709	1136.299278	15.030003
21.537049	1137.206530	15.035021
21.396104	1136.370245	15.040039
21.491673	1138.596002	15.045056
21.327574	1143.825839	15.050074
21.915217	1136.986480	15.055091
21.448081	1144.400345	15.060109
21.352542	1143.945122	15.065127
21.291503	1140.211820	15.070144
21.621148	1138.171989	15.075162
21.640027	1137.720931	15.080179
21.582564	1134.968556	15.085197
21.703062	1145.136976	15.090215
21.762956	1155.775660	15.095232
21.817866	1166.749657	15.100250
22.085142	1152.875471	15.105267
21.583287	1154.800346	15.110285
21.721490	1142.830469	15.115303
21.972494	1155.717773	15.120320
21.996395	1152.286751	15.125338
22.024185	1139.794514	15.130355
21.869053	1134.580057	15.135373
21.910699	1137.404417	15.140391
21.882563	1134.224556	15.145408
21.395781	1144.109416	15.150426
21.919803	1148.915848	15.155443
21.842488	1163.176924	15.160461
22.108237	1156.637309	15.165479
21.808109	1162.696377	15.170496
21.903712	1158.859631	15.175514
22.178480	1158.472624	15.180531
22.119050	1169.073205	15.185549
22.167160	1170.741494	15.190567
22.181181	1162.881120	15.195584
22.279828	1170.727073	15.200602
22.455505	1164.084799	15.205619
22.284201	1163.811866	15.210637
22.350117	1157.057400	15.215655
22.423174	1163.206325	15.220672
22.135448	1163.084181	15.225690
22.402916	1160.170435	15.230707
22.158899	1164.895231	15.235725
22.376993	1164.185734	15.240743
22.348370	1164.976078	15.245760
22.182580	1166.305483	15.250778
22.465260	1151.592568	15.255795
21.912236	1164.448060	15.260813
22.495434	1161.579522	15.265831
22.571508	1162.337682	15.270848
22.443862	1170.651451	15.275866
22.409795	1159.639547	15.280883
22.351659	1171.505446	15.285901
22.305231	1165.948889	15.290919
22.697943	1154.876432	15.295936
22.261025	1161.360888	15.300954
22.316805	1177.658775	15.305971
22.724010	1186.835523	15.310989
22.485617	1187.803907	15.316007
22.814834	1191.119723	15.321024
22.861370	1194.653406	15.326042
22.952021	1193.872354	15.331059
22.663020	1186.879985	15.336077
22.530064	1191.259172	15.341095
22.956841	1187.623004	15.346112
22.741962	1184.163114	15.351130
22.756360	1184.325003	15.356147
22.692780	1196.804019	15.361165
22.889327	1189.094923	15.366183
22.991978	1185.935588	15.371200
22.665676	1183.973279	15.376218
22.937262	1184.385216	15.381235
22.806276	1192.099894	15.386253
22.556294	1189.702735	15.391271
22.895429	1178.534512	15.396288
22.546009	1192.194439	15.401306
22.959145	1197.217081	15.406323
23.278577	1202.765664	15.411341
23.324312	1211.326851	15.416359
23.589366	1205.323833	15.421376
23.461165	1200.190347	15.426394
23.204786	1183.826113	15.431411
23.017627	1191.713700	15.436429
23.198689	1186.077310	15.441447
23.387139	1182.576318	15.446464
23.175883	1187.924013	15.451482
23.212882	1180.776424	15.456499
23.109468	1189.648157	15.461517
23.399347	1196.930810	15.466535
23.054235	1200.904567	15.471552
23.196099	1204.947198	15.476570
23.344805	1201.086343	15.481587
23.263609	1211.119138	15.486605
23.097906	1210.775897	15.491623
23.243717	1206.281155	15.496640
23.028004	1211.553814	15.501658
23.131234	1204.023439	15.506675
23.463528	1206.540329	15.511693
23.678289	1220.847210	15.516711
23.681064	1213.430405	15.521728
23.740951	1211.884128	15.526746
23.446871	1207.767588	15.531763
23.876931	1219.620146	15.536781
23.986452	1215.137400	15.541799
23.887315	1199.827838	15.546816
23.641745	1204.871635	15.551834
23.652471	1198.248881	15.556851
23.622273	1200.263969	15.561869
23.731505	1199.356925	15.566887
23.842748	1198.279146	15.571904
23.598171	1216.107408	15.576922
24.058362	1217.363985	15.581939
24.260256	1231.287867	15.586957
23.786704	1213.632146	15.591975
23.963789	1209.100944	15.596992
23.917548	1215.584171	15.602010
24.275900	1213.940635	15.607027
24.022959	1207.393905	15.612045
23.896525	1208.360528	15.617063
24.048288	1206.733582	15.622080
23.839700	1221.087858	15.627098
24.202038	1224.313281	15.632115
23.991090	1223.693095	15.637133
24.200673	1233.585666	15.642151
24.286175	1221.911182	15.647168
24.457135	1230.913522	15.652186
24.490407	1220.730504	15.657203
24.135363	1213.309800	15.662221
24.169667	1217.116813	15.667239
24.500347	1217.513180	15.672256
24.241647	1220.343584	15.677274
24.381607	1211.926950	15.682291
24.301893	1229.057184	15.687309
24.446785	1225.761831	15.692327
24.664874	1232.986316	15.697344
24.359209	1214.575272	15.702362
24.383754	1224.629378	15.707379
24.599625	1227.940869	15.712397
24.353601	1227.897401	15.717415
24.649083	1225.477890	15.722432
24.538822	1226.634491	15.727450
24.620358	1219.467285	15.732467
24.336798	1226.420059	15.737485
24.601113	1231.103098	15.742503
24.433723	1220.001588	15.747520
24.219580	1223.415169	15.752538
24.050274	1224.495811	15.757555
24.300127	1227.918747	15.762573
24.310527	1230.725925	15.767591
24.620091	1245.311472	15.772608
24.865485	1255.725483	15.777626
24.605468	1245.348554	15.782643
24.650852	1250.116395	15.787661
24.803467	1254.495036	15.792679
25.110019	1242.779592	15.797696
25.098574	1250.103167	15.802714
24.846952	1250.335141	15.807731
25.064446	1252.971014	15.812749
24.912353	1253.234733	15.817767
25.009718	1248.018552	15.822784
24.659421	1243.730924	15.827802
24.529613	1254.440416	15.832819
24.886523	1251.828234	15.837837
24.443431	1257.164935	15.842855
24.618520	1252.987499	15.847872
25.033788	1267.240910	15.852890
25.228119	1275.100320	15.857907
25.061132	1267.047346	15.862925
24.927995	1271.997804	15.867943
25.262529	1262.332472	15.872960
25.168355	1266.424723	15.877978
25.304027	1265.728135	15.882995
25.386980	1267.072225	15.888013
25.384519	1271.412050	15.893031
25.457552	1261.128102	15.898048
25.500995	1263.570332	15.903066
25.309598	1256.168153	15.908083
25.182245	1253.619222	15.913101
25.363743	1269.376767	15.918119
25.221868	1269.111844	15.923136
25.487567	1260.539782	15.928154
25.264073	1259.533382	15.933171
25.558951	1260.250953	15.938189
25.274132	1268.434752	15.943207
25.316206	1279.395050	15.948224
25.388757	1290.625145	15.953242
25.561322	1297.490702	15.958259
25.881495	1290.219802	15.963277
25.903809	1294.675676	15.968295
26.015882	1288.302108	15.973312
25.973704	1289.870941	15.978330
25.920934	1284.795042	15.983347
26.168580	1283.001582	15.988365
25.964612	1286.183196	15.993383
26.003631	1257.442395	15.998400
26.270651	1261.216111	16.003418
25.681317	1268.532403	16.008435
25.540550	1271.830350	16.013453
25.791981	1277.023523	16.018471
26.359633	1278.512586	16.023488
26.419564	1280.731321	16.028506
25.990949	1260.105095	16.033523
26.298191	1254.720324	16.038541
26.311101	1249.081857	16.043559
26.309669	1251.578456	16.048576
26.220770	1246.189481	16.053594
25.929379	1245.465129	16.058611
26.275306	1244.915487	16.063629
26.241137	1254.871509	16.068647
26.080895	1254.732546	16.073664
26.235803	1254.954475	16.078682
25.948986	1255.144625	16.083699
26.523319	1272.598473	16.088717
26.712109	1281.910482	16.093735
26.963357	1267.565330	16.098752
26.639722	1252.761130	16.103770
26.420702	1248.156276	16.108787
26.400411	1254.332482	16.113805
26.479685	1249.548341	16.118823
26.554727	1244.667031	16.123840
26.416296	1246.503415	16.128858
26.155964	1254.733866	16.133875
26.333157	1249.347381	16.138893
26.246324	1268.511184	16.143911
26.710388	1274.876606	16.148928
26.630878	1275.756982	16.153946
26.482385	1270.314218	16.158963
26.702094	1273.019178	16.163981
26.102221	1277.862877	16.168999
26.465062	1275.811518	16.174016
26.496417	1274.386476	16.179034
26.605992	1273.223744	16.184051
26.840295	1269.005466	16.189069
26.538861	1277.662106	16.194087
26.848060	1287.204571	16.199104
27.132719	1297.874397	16.204122
27.096283	1300.376488	16.209139
26.887705	1288.157877	16.214157
27.003080	1290.380549	16.219175
26.881975	1291.387369	16.224192
26.828088	1293.469298	16.229210
26.932402	1300.900993	16.234227
27.374518	1305.568817	16.239245
26.918530	1311.639731	16.244263
27.060215	1304.699762	16.249280
27.396344	1308.121819	16.254298
27.149217	1314.557657	16.259315
27.370242	1302.003473	16.264333
27.352613	1309.918200	16.269351
27.821434	1296.927546	16.274368
27.473355	1301.895909	16.279386
27.186830	1297.001805	16.284403
27.537490	1289.988071	16.289421
27.317853	1295.605366	16.294439
27.144871	1301.250068	16.299456
27.319997	1294.005049	16.304474
27.358256	1298.467893	16.309491
27.420952	1298.584346	16.314509
27.146663	1308.180371	16.319527
27.365230	1296.472366	16.324544
27.411047	1299.734772	16.329562
27.178918	1304.217890	16.334579
27.559420	1292.964217	16.339597
27.397414	1305.771168	16.344615
27.739843	1319.288076	16.349632
27.856453	1317.114339	16.354650
27.535206	1319.582158	16.359667
27.487802	1321.754596	16.364685
27.665125	1318.466769	16.369703
27.759225	1324.921734	16.374720
27.941338	1322.756669	16.379738
27.850153	1326.005831	16.384755
28.388532	1314.976726	16.389773
27.941261	1313.241648	16.394791
27.914328	1325.210062	16.399808
28.254451	1323.001304	16.404826
27.652268	1323.464937	16.409843
28.166663	1323.153996	16.414861
28.579903	1323.711008	16.419879
28.032597	1316.961039	16.424896
28.303742	1322.337337	16.429914
28.037831	1323.310040	16.434931
28.338046	1319.996645	16.439949
28.154787	1325.857569	16.444967
28.044505	1321.058926	16.449984
28.290517	1314.190972	16.455002
27.880817	1319.304700	16.460019
27.897286	1317.468559	16.465037
27.858311	1316.054533	16.470055
27.721458	1314.520137	16.475072
28.147162	1318.619311	16.480090
28.172468	1338.068588	16.485107
28.756371	1334.470891	16.490125
28.782060	1337.528166	16.495143
28.444598	1350.157502	16.500160
28.352737	1344.481770	16.505178
28.145171	1344.151397	16.510195
28.443070	1343.546159	16.515213
28.293277	1341.130124	16.520231
28.270700	1344.169715	16.525248
28.624575	1342.075570	16.530266
28.468423	1339.319691	16.535283
28.509821	1341.998948	16.540301
28.263451	1346.705224	16.545319
28.759904	1357.663809	16.550336
28.863403	1364.802156	16.555354
28.830352	1366.098154	16.560371
29.099393	1367.548801	16.565389
28.821795	1361.924256	16.570407
28.859102	1370.430033	16.575424
29.145976	1363.833382	16.580442
28.880485	1366.103114	16.585459
29.162847	1366.175682	16.590477
29.192619	1360.424080	16.595495
28.866832	1368.327153	16.600512
28.988928	1361.607991	16.605530
29.251583	1365.555990	16.610547
28.957031	1351.236324	16.615565
28.902776	1361.971913	16.620583
28.942501	1370.139625	16.625600
28.751663	1358.615650	16.630618
29.035713	1365.157639	16.635635
29.379902	1362.957707	16.640653
29.216724	1360.335475	16.645671
29.028418	1359.803259	16.650688
29.123216	1376.638036	16.655706
29.465827	1388.725325	16.660723
29.746950	1381.428948	16.665741
29.679800	1383.916926	16.670759
29.575188	1391.109982	16.675776
29.502314	1387.277492	16.680794
29.528886	1391.565458	16.685811
29.706468	1383.054483	16.690829
29.819243	1383.844774	16.695847
29.843367	1382.966835	16.700864
29.653492	1365.875614	16.705882
29.459057	1380.597045	16.710899
29.708260	1384.906935	16.715917
29.675181	1384.331461	16.720935
29.867241	1392.033482	16.725952
29.679537	1375.311158	16.730970
29.486834	1382.073024	16.735987
30.025854	1377.907969	16.741005
30.005583	1384.898451	16.746023
29.648584	1387.788465	16.751040
29.848547	1381.183333	16.756058
29.613337	1380.478577	16.761075
29.965253	1367.749196	16.766093
30.061963	1365.988844	16.771111
29.918553	1380.560264	16.776128
30.192360	1374.625249	16.781146
29.920093	1375.460089	16.786163
29.962604	1374.629764	16.791181
30.108952	1391.336552	16.796199
30.030940	1400.349583	16.801216
30.072483	1406.806501	16.806234
30.280739	1407.379852	16.811251
30.384124	1398.905742	16.816269
30.627160	1399.066527	16.821287
30.282297	1402.301797	16.826304
30.404485	1399.679031	16.831322
30.334377	1410.224620	16.836339
30.520110	1398.041988	16.841357
30.408815	1395.481053	16.846375
30.376536	1393.519992	16.851392
29.999588	1387.282972	16.856410
30.343872	1393.458911	16.861427
30.579340	1395.053682	16.866445
30.358415	1386.971234	16.871463
30.099643	1401.276709	16.876480
30.566048	1403.621130	16.881498
30.482173	1411.300117	16.886515
30.612689	1417.282329	16.891533
30.824427	1419.884414	16.896551
30.754487	1430.092302	16.901568
30.970556	1420.177191	16.906586
30.989020	1421.843836	16.911603
31.051126	1418.646629	16.916621
31.532938	1421.651389	16.921639
31.150524	1428.695473	16.926656
31.119787	1423.865403	16.931674
31.380218	1426.273658	16.936691
31.557425	1404.599246	16.941709
31.221879	1397.973865	16.946727
31.030729	1398.202677	16.951744
31.083742	1401.202031	16.956762
30.893110	1403.605212	16.961779
31.007825	1403.729295	16.966797
30.866000	1412.559817	16.971815
31.245063	1421.753720	16.976832
31.704303	1419.166509	16.981850
31.235853	1423.380557	16.986867
31.264312	1427.750290	16.991885
31.152751	1426.148803	16.996903
31.151838	1428.033089	17.001920
31.179162	1427.820553	17.006938
31.386710	1434.522884	17.011955
31.341017	1425.349405	17.016973
31.457271	1413.190272	17.021991
31.118308	1429.670163	17.027008
31.443291	1432.920413	17.032026
31.775091	1441.591531	17.037043
31.873134	1451.937222	17.042061
32.247869	1449.240164	17.047079
31.905441	1437.323303	17.052096
31.806587	1422.508992	17.057114
31.336324	1422.642675	17.062131
31.537444	1439.202063	17.067149
31.823361	1443.089628	17.072167
31.321450	1453.854384	17.077184
31.838912	1453.852245	17.082202
31.715731	1454.723693	17.087219
31.852348	1455.999426	17.092237
32.034425	1452.631930	17.097255
31.653611	1453.692074	17.102272
31.920090	1444.005748	17.107290
31.906313	1453.207566	17.112307
31.872997	1452.035651	17.117325
32.066091	1460.886309	17.122343
31.765607	1474.904874	17.127360
32.311321	1476.630934	17.132378
32.327247	1476.309724	17.137395
32.147016	1473.964716	17.142413
32.426834	1470.998490	17.147431
32.425666	1479.816475	17.152448
32.768740	1473.435052	17.157466
32.667368	1478.427929	17.162483
32.711045	1485.114926	17.167501
32.631697	1483.094954	17.172519
32.580671	1471.744671	17.177536
32.867908	1475.991816	17.182554
32.724329	1457.286868	17.187571
32.305740	1458.109922	17.192589
32.524962	1460.518326	17.197607
32.556106	1472.575574	17.202624
32.961209	1479.149133	17.207642
32.907811	1473.397903	17.212659
32.765399	1473.767410	17.217677
33.024524	1467.446482	17.222695
32.627500	1478.444140	17.227712
32.874651	1476.161564	17.232730
32.924370	1473.976197	17.237747
32.599937	1478.303399	17.242765
32.944069	1471.947058	17.247783
32.795465	1472.712031	17.252800
32.663297	1467.793695	17.257818
32.734081	1469.291193	17.262835
32.762764	1471.928278	17.267853
33.227301	1464.748305	17.272871
32.933185	1481.227528	17.277888
32.800141	1474.207454	17.282906
33.027512	1485.366076	17.287923
32.932679	1491.838080	17.292941
33.348120	1491.438494	17.297959
33.123114	1484.874661	17.302976
33.135450	1499.866766	17.307994
33.161501	1498.347858	17.313011
32.803950	1499.760983	17.318029
33.225828	1493.338802	17.323047
33.237678	1512.086595	17.328064
33.187928	1521.303553	17.333082
33.380061	1528.437546	17.338099
33.226681	1535.543621	17.343117
33.453362	1536.095155	17.348135
33.165074	1522.291950	17.353152
33.459836	1526.477964	17.358170
33.505283	1534.335568	17.363187
33.790994	1552.769081	17.368205
34.354461	1535.913134	17.373223
34.008526	1526.934976	17.378240
34.129036	1517.826932	17.383258
33.938122	1522.928530	17.388275
33.890664	1522.424736	17.393293
34.035315	1515.342202	17.398311
33.711859	1522.635874	17.403328
33.771881	1513.546778	17.408346
34.118970	1531.680303	17.413363
34.150084	1545.725868	17.418381
34.634314	1544.766364	17.423399
34.235838	1534.041711	17.428416
34.014308	1525.662633	17.433434
34.333903	1518.931404	17.438451
34.290029	1523.675430	17.443469
33.840459	1514.094945	17.448487
33.898906	1533.630765	17.453504
34.334883	1536.478615	17.458522
34.624139	1537.761998	17.463539
34.305174	1546.989589	17.468557
34.370092	1538.171127	17.473575
34.309773	1542.621074	17.478592
34.322591	1531.816201	17.483610
34.651346	1535.668671	17.488627
34.438340	1542.351723	17.493645
34.416685	1534.342133	17.498663
34.472698	1536.268007	17.503680
34.559625	1536.737290	17.508698
34.506538	1535.287586	17.513715
34.475062	1547.559833	17.518733
34.776462	1563.734376	17.523751
34.861752	1570.474849	17.528768
34.708690	1562.170237	17.533786
34.900990	1563.623456	17.538803
34.857549	1563.005417	17.543821
34.968055	1564.484075	17.548839
35.122776	1557.816536	17.553856
34.733533	1557.098034	17.558874
34.938253	1559.401421	17.563891
34.826072	1568.454605	17.568909
34.868269	1562.473762	17.573927
34.844733	1560.580744	17.578944
35.337178	1567.386818	17.583962
35.177230	1558.938112	17.588979
34.661182	1566.059994	17.593997
35.072682	1578.259702	17.599015
35.235609	1593.073647	17.604032
35.196355	1588.790853	17.609050
35.119307	1584.738056	17.614067
35.250949	1590.189944	17.619085
35.288462	1586.299089	17.624103
35.221051	1589.733932	17.629120
35.424563	1591.882869	17.634138
35.507644	1594.050675	17.639155
35.723717	1593.559242	17.644173
35.850439	1595.148977	17.649191
35.464016	1599.492233	17.654208
35.571882	1595.120110	17.659226
35.973518	1601.362880	17.664243
35.982123	1608.402577	17.669261
35.816663	1594.491704	17.674279
35.855325	1587.662446	17.679296
35.705324	1598.709841	17.684314
35.794023	1599.062077	17.689331
35.608227	1614.047448	17.694349
35.977533	1610.448605	17.699367
35.770467	1615.095141	17.704384
36.091402	1605.905155	17.709402
36.104231	1598.505551	17.714419
35.810237	1608.095355	17.719437
36.183724	1608.122087	17.724455
36.242602	1603.249525	17.729472
36.255682	1601.126690	17.734490
36.227193	1603.144712	17.739507
36.294194	1600.650491	17.744525
36.254427	1597.608078	17.749543
36.610175	1601.216477	17.754560
36.420489	1604.070843	17.759578
36.583729	1605.415003	17.764595
36.319258	1602.843321	17.769613
36.169446	1606.660328	17.774631
36.803999	1622.340888	17.779648
36.669093	1623.321484	17.784666
36.640966	1630.395349	17.789683
37.000209	1628.300331	17.794701
36.975997	1619.407426	17.799719
36.815677	1609.346044	17.804736
36.355733	1610.866744	17.809754
36.813823	1615.314384	17.814771
36.928014	1628.479101	17.819789
37.083615	1628.189656	17.824807
36.831162	1635.191366	17.829824
36.818875	1641.413791	17.834842
37.209842	1632.818769	17.839859
36.978274	1631.662124	17.844877
36.821143	1627.637645	17.849895
36.923326	1634.419679	17.854912
36.728012	1632.045453	17.859930
37.059167	1620.616260	17.864947
36.922924	1635.830585	17.869965
37.020934	1633.189482	17.874983
37.219178	1635.818961	17.880000
37.436817	1627.917012	17.885018
37.425480	1631.810164	17.890035
37.291084	1633.267235	17.895053
37.177773	1638.583938	17.900071
37.224763	1641.644239	17.905088
37.128936	1657.593909	17.910106
37.461170	1652.785808	17.915123
37.336101	1656.355937	17.920141
37.424580	1654.366459	17.925159
37.900001	1645.136467	17.930176
37.778936	1650.975128	17.935194
37.918388	1647.017792	17.940211
37.904834	1645.284157	17.945229
37.912257	1646.340290	17.950247
38.059163	1647.598645	17.955264
37.670280	1647.432381	17.960282
37.920441	1642.782317	17.965299
37.660399	1652.969621	17.970317
37.754010	1646.068611	17.975335
37.868315	1636.743716	17.980352
38.084119	1648.570166	17.985370
38.188678	1641.181420	17.990387
37.924263	1655.191319	17.995405
38.191723	1668.180563	18.000423
38.086815	1677.242130	18.005440
37.969626	1677.039610	18.010458
38.503731	1677.827021	18.015475
38.656294	1685.970884	18.020493
38.444470	1675.295802	18.025511
38.751882	1682.241371	18.030528
38.329295	1682.042516	18.035546
38.446969	1671.331591	18.040563
38.324615	1689.381028	18.045581
38.508706	1680.070425	18.050599
38.469949	1670.081486	18.055616
38.162665	1679.913266	18.060634
38.736073	1679.167016	18.065651
38.733180	1677.520075	18.070669
38.727348	1674.043116	18.075687
38.773197	1675.961130	18.080704
38.658297	1670.109013	18.085722
38.863965	1669.025879	18.090739
38.943395	1674.003107	18.095757
38.579094	1665.987179	18.100775
38.946855	1674.908413	18.105792
39.120064	1687.363294	18.110810
39.077369	1688.247390	18.115827
39.176425	1686.085827	18.120845
38.995199	1695.137269	18.125863
39.073229	1688.570065	18.130880
39.273494	1686.518885	18.135898
39.224298	1676.427430	18.140915
39.428258	1684.755757	18.145933
39.188429	1692.408803	18.150951
39.555113	1678.651189	18.155968
38.840852	1678.835725	18.160986
39.489262	1674.953283	18.166003
39.242309	1680.369837	18.171021
39.112612	1687.841514	18.176039
39.506683	1679.470060	18.181056
39.261953	1683.008447	18.186074
39.375655	1692.231442	18.191091
39.598337	1697.798496	18.196109
39.705561	1696.213201	18.201127
39.887026	1705.643351	18.206144
39.606897	1704.835158	18.211162
39.796007	1701.116198	18.216179
39.630646	1706.911321	18.221197
39.515846	1707.494270	18.226215
39.871774	1692.557985	18.231232
39.962277	1709.217011	18.236250
39.767016	1702.235001	18.241267
39.726884	1705.485699	18.246285
39.828109	1696.418459	18.251303
40.160367	1704.843465	18.256320
39.597455	1721.532291	18.261338
40.072962	1728.625121	18.266355
40.363739	1732.452024	18.271373
40.089044	1741.111009	18.276391
40.126994	1727.142915	18.281408
40.197082	1739.459345	18.286426
40.289599	1730.466039	18.291443
40.504171	1738.767480	18.296461
40.299023	1735.072413	18.301479
40.267311	1730.261349	18.306496
40.019062	1738.054599	18.311514
40.481193	1745.140064	18.316531
40.555429	1751.516239	18.321549
40.685999	1749.696893	18.326567
40.798335	1753.520198	18.331584
40.929109	1755.361794	18.336602
40.978668	1746.649785	18.341619
40.767639	1755.573374	18.346637
40.797473	1754.839699	18.351655
40.910726	1751.262010	18.356672
40.613047	1761.998107	18.361690
40.874084	1753.158279	18.366707
40.999645	1753.653075	18.371725
40.632368	1746.016300	18.376743
41.102967	1753.725332	18.381760
41.226520	1764.442771	18.386778
41.248079	1772.124330	18.391795
41.229389	1770.385175	18.396813
41.182134	1766.902064	18.401831
41.547284	1763.499515	18.406848
41.757773	1769.693392	18.411866
41.614212	1770.848933	18.416883
41.793561	1768.671624	18.421901
41.618103	1760.831208	18.426919
41.414280	1742.924404	18.431936
41.769997	1756.676263	18.436954
41.534096	1757.322373	18.441971
41.770855	1764.499965	18.446989
41.725971	1763.124701	18.452007
42.263294	1767.986028	18.457024
41.646756	1757.036613	18.462042
41.968615	1761.218438	18.467059
41.896624	1761.390712	18.472077
41.798314	1765.174435	18.477095
41.771867	1762.464444	18.482112
41.908514	1761.982295	18.487130
42.258276	1773.516422	18.492147
41.905589	1762.812861	18.497165
41.934139	1776.208870	18.502183
42.191885	1772.883111	18.507200
42.074031	1775.505328	18.512218
42.025526	1774.092759	18.517235
42.219926	1766.863466	18.522253
42.397897	1779.219829	18.527271
42.172236	1772.444538	18.532288
42.081143	1774.639656	18.537306
41.985391	1763.671762	18.542323
41.890642	1783.455933	18.547341
42.054684	1797.335692	18.552359
42.388301	1789.349225	18.557376
42.429401	1785.994287	18.562394
42.340920	1797.095286	18.567411
42.747202	1799.423932	18.572429
42.578087	1793.668637	18.577447
42.638746	1801.078976	18.582464
42.886583	1803.871135	18.587482
43.042311	1821.321676	18.592499
43.309596	1813.692754	18.597517
43.323656	1803.831174	18.602535
43.365740	1790.588268	18.607552
42.819820	1788.688704	18.612570
42.785067	1785.677033	18.617587
43.103030	1784.380625	18.622605
43.111171	1796.845666	18.627623
43.331671	1804.215182	18.632640
43.416442	1809.220014	18.637658
43.286678	1811.253926	18.642675
43.467211	1804.998846	18.647693
43.433907	1814.289122	18.652711
43.557410	1812.265735	18.657728
43.639422	1801.806489	18.662746
43.424238	1803.620238	18.667763
43.566220	1801.676014	18.672781
43.518210	1816.614718	18.677799
43.684521	1809.901085	18.682816
43.490168	1810.515439	18.687834
43.440245	1808.727522	18.692851
43.768330	1807.741973	18.697869
43.703990	1819.801791	18.702887
43.516683	1815.314905	18.707904
43.678674	1818.527643	18.712922
43.786144	1813.887268	18.717939
44.317845	1809.881063	18.722957
43.982480	1817.836329	18.727975
43.848170	1814.401565	18.732992
43.865293	1815.112181	18.738010
43.792910	1825.702556	18.743027
44.105540	1835.718181	18.748045
43.999687	1841.096895	18.753063
44.451866	1828.285204	18.758080
43.934806	1833.314904	18.763098
44.068011	1840.363574	18.768115
44.128810	1837.646215	18.773133
44.050861	1849.518822	18.778151
44.399164	1856.486457	18.783168
44.301751	1862.753856	18.788186
44.380555	1862.350200	18.793203
44.757835	1863.174815	18.798221
44.613979	1866.842610	18.803239
44.374606	1867.363026	18.808256
44.932697	1868.812612	18.813274
44.766432	1863.347203	18.818291
44.968481	1866.089737	18.823309
44.580647	1868.934162	18.828327
44.682356	1864.042194	18.833344
45.243717	1859.810408	18.838362
44.927186	1867.775370	18.843379
45.318918	1868.171657	18.848397
45.225585	1872.702602	18.853415
44.984346	1856.613111	18.858432
45.162796	1867.801728	18.863450
45.118248	1882.667356	18.868467
45.260558	1880.069773	18.873485
45.400759	1881.477529	18.878503
45.689012	1879.661868	18.883520
45.764173	1882.692548	18.888538
45.646942	1866.937094	18.893555
45.644511	1853.874697	18.898573
45.219892	1860.063965	18.903591
45.545900	1863.452999	18.908608
45.741874	1864.858328	18.913626
45.365058	1867.716806	18.918643
45.846322	1877.456706	18.923661
45.725087	1873.562257	18.928679
46.011720	1867.710284	18.933696
46.080083	1872.989123	18.938714
45.971838	1872.444347	18.943731
45.945247	1873.019794	18.948749
45.692124	1876.628966	18.953767
45.870190	1874.884222	18.958784
46.172703	1867.031992	18.963802
45.900845	1870.000267	18.968819
46.098513	1877.010447	18.973837
45.616290	1877.442671	18.978855
45.974623	1886.835737	18.983872
46.549229	1904.933995	18.988890
46.486615	1900.266593	18.993907
46.289744	1898.845699	18.998925
46.407022	1903.709754	19.003943
46.205851	1903.608758	19.008960
46.686516	1902.346816	19.013978
46.615073	1908.057855	19.018995
46.620049	1904.374015	19.024013
46.729977	1904.454667	19.029031
46.936403	1900.158554	19.034048
46.674464	1896.989941	19.039066
46.248397	1910.567740	19.044083
46.437106	1896.746319	19.049101
46.787533	1911.676329	19.054119
46.768703	1924.773736	19.059136
47.221459	1914.461480	19.064154
47.398360	1928.538156	19.069171
47.321137	1924.611551	19.074189
47.152354	1929.315290	19.079207
47.228340	1924.701912	19.084224
47.086987	1923.789908	19.089242
47.005473	1921.593488	19.094259
47.620875	1919.982206	19.099277
47.587284	1934.341193	19.104295
46.811397	1930.546145	19.109312
47.354953	1926.396035	19.114330
47.489005	1920.621604	19.119347
47.856527	1923.202511	19.124365
47.479110	1919.120955	19.129383
47.503710	1921.149630	19.134400
47.448127	1913.123094	19.139418
47.336329	1940.664504	19.144435
47.956921	1944.304068	19.149453
47.693892	1945.882312	19.154471
47.852586	1943.064385	19.159488
47.943134	1945.938019	19.164506
48.133128	1948.603554	19.169523
47.983923	1941.554268	19.174541
48.077665	1941.252419	19.179559
47.729041	1942.099247	19.184576
47.909806	1934.531170	19.189594
47.810443	1955.616544	19.194611
48.197117	1959.074994	19.199629
47.997931	1970.202912	19.204647
48.380481	1969.922090	19.209664
48.894229	1967.591371	19.214682
49.011756	1967.677145	19.219699
48.840100	1961.212083	19.224717
48.901622	1957.052277	19.229735
48.773984	1947.547360	19.234752
48.914905	1930.391147	19.239770
48.736963	1927.291425	19.244787
48.509825	1935.229786	19.249805
48.779059	1929.071227	19.254823
48.450786	1951.088778	19.259840
48.622897	1957.190896	19.264858
48.616707	1954.644973	19.269875
48.475325	1963.636654	19.274893
48.689735	1960.503858	19.279911
48.661772	1965.106642	19.284928
48.964802	1969.288310	19.289946
49.121030	1984.463419	19.294963
49.661070	1985.218355	19.299981
49.498426	1982.349775	19.304999
49.404495	1989.143734	19.310016
49.554326	1981.144949	19.315034
49.296381	1983.041161	19.320051
49.515240	1978.077154	19.325069
49.619337	1978.048258	19.330087
49.534547	1983.044989	19.335104
49.533438	1967.552141	19.340122
49.318689	1975.548544	19.345139
49.543045	1978.003555	19.350157
50.005208	1967.301601	19.355175
49.458820	1984.499361	19.360192
49.734514	1973.987577	19.365210
49.623319	1984.906044	19.370227
49.598607	1989.429423	19.375245
49.760059	2002.078885	19.380263
50.048933	2016.592559	19.385280
50.264016	1998.414722	19.390298
49.800770	2009.688188	19.395315
49.813732	2001.164840	19.400333
50.155043	2004.579909	19.405351
49.893812	2012.618327	19.410368
50.337104	2014.824430	19.415386
50.370580	2014.090173	19.420403
50.508842	2020.024033	19.425421
50.643136	2031.112365	19.430439
50.199043	2030.197291	19.435456
50.735288	2022.276812	19.440474
50.809022	2030.518398	19.445491
50.545776	2027.599295	19.450509
50.929200	2023.224924	19.455527
50.589309	2026.077641	19.460544
50.897976	2018.136012	19.465562
50.723249	2031.295794	19.470579
50.907833	2022.092243	19.475597
50.668743	2031.878814	19.480615
51.103625	2052.621801	19.485632
51.093230	2042.211610	19.490650
50.980197	2053.594347	19.495667
50.898824	2050.043937	19.500685
50.550381	2043.881121	19.505703
50.522462	2058.457088	19.510720
50.893096	2063.177341	19.515738
51.031769	2079.636644	19.520755
50.834003	2069.934350	19.525773
51.398724	2086.424745	19.530791
51.492168	2108.559466	19.535808
51.988874	2103.075325	19.540826
52.112492	2107.897414	19.545843
52.043713	2095.643724	19.550861
52.332420	2078.167545	19.555879
52.041708	2078.146853	19.560896
52.157519	2071.608307	19.565914
52.465955	2076.549766	19.570931
51.958946	2066.574005	19.575949
52.361725	2071.667953	19.580967
52.527782	2077.682691	19.585984
52.287035	2067.441132	19.591002
52.331227	2072.679632	19.596019
51.969670	2074.326977	19.601037
52.537908	2067.304102	19.606055
52.430005	2069.921647	19.611072
52.383023	2063.531696	19.616090
52.406425	2072.882654	19.621107
52.597644	2073.749056	19.626125
52.468706	2067.053182	19.631143
52.209023	2066.421664	19.636160
52.294533	2069.741113	19.641178
52.524872	2067.732519	19.646195
52.486608	2070.667384	19.651213
52.751980	2082.306459	19.656231
52.730962	2091.645451	19.661248
52.864939	2084.315035	19.666266
52.437291	2094.389981	19.671283
52.946140	2091.173158	19.676301
52.633727	2094.087858	19.681319
52.778034	2094.358801	19.686336
52.994060	2107.274365	19.691354
53.289944	2110.131634	19.696371
53.181578	2114.532441	19.701389
53.520486	2110.133463	19.706407
53.644706	2110.114039	19.711424
53.579374	2111.090072	19.716442
53.687323	2109.356292	19.721459
53.377412	2115.616044	19.726477
53.656441	2110.648886	19.731495
53.404399	2112.932384	19.736512
53.523648	2106.368037	19.741530
53.596875	2114.556087	19.746547
53.344823	2111.079747	19.751565
53.680698	2111.033474	19.756583
53.892233	2133.361181	19.761600
54.032219	2141.633466	19.766618
54.370227	2144.174845	19.771635
54.205185	2146.952845	19.776653
54.506352	2138.605203	19.781671
54.381097	2133.104881	19.786688
54.632802	2123.909698	19.791706
54.393748	2123.767294	19.796723
54.475599	2121.131807	19.801741
54.492971	2103.789641	19.806759
54.322415	2115.667466	19.811776
54.346814	2128.376363	19.816794
54.226964	2136.474743	19.821811
54.347593	2127.580986	19.826829
54.465831	2129.891685	19.831847
54.187714	2137.434144	19.836864
54.469087	2132.491861	19.841882
54.666083	2141.077134	19.846899
54.641488	2150.716544	19.851917
54.991459	2157.384207	19.856935
55.121754	2161.059606	19.861952
55.152842	2160.391996	19.866970
54.738174	2155.416737	19.871987
54.725094	2158.085715	19.877005
54.607672	2154.260041	19.882023
54.712608	2167.331921	19.887040
54.865636	2188.488487	19.892058
54.985819	2178.133505	19.897075
55.017242	2185.359218	19.902093
55.554886	2180.875433	19.907111
55.185879	2188.845601	19.912128
55.517209	2198.754348	19.917146
55.549739	2196.700987	19.922163
55.652822	2207.270406	19.927181
55.778994	2213.625985	19.932199
55.711385	2209.091841	19.937216
55.897207	2208.769249	19.942234
55.921399	2208.191088	19.947251
55.810403	2203.932011	19.952269
56.084805	2197.305449	19.957287
56.266487	2204.192019	19.962304
55.801348	2206.161745	19.967322
56.112662	2200.435198	19.972339
55.779119	2199.139844	19.977357
56.423436	2203.343841	19.982375
55.984655	2227.749269	19.987392
56.514369	2223.500267	19.992410
56.548848	2228.468910	19.997427
56.292627	2231.822994	20.002445
56.469281	2228.853872	20.007463
56.828296	2233.926319	20.012480
57.058028	2220.937744	20.017498
56.926261	2223.104572	20.022515
56.491425	2227.840605	20.027533
56.541806	2217.704839	20.032551
56.646822	2221.841845	20.037568
57.112658	2221.383854	20.042586
57.021534	2230.049028	20.047603
56.562517	2247.820383	20.052621
57.273517	2249.697367	20.057639
57.320091	2255.099665	20.062656
57.302046	2257.633724	20.067674
57.552991	2257.032659	20.072691
56.959327	2249.052404	20.077709
57.179728	2245.517796	20.082727
57.163103	2252.706879	20.087744
57.236387	2248.794495	20.092762
57.653533	2262.218353	20.097779
57.574301	2266.797686	20.102797
57.700384	2271.622589	20.107815
57.672893	2274.849317	20.112832
58.046915	2268.538512	20.117850
57.799572	2272.973756	20.122867
57.899004	2271.149768	20.127885
57.882573	2262.962292	20.132903
57.959799	2275.574646	20.137920
57.776388	2273.119566	20.142938
58.258196	2277.121803	20.147955
57.889629	2280.562932	20.152973
58.254524	2289.724787	20.157991
58.368176	2288.151058	20.163008
57.951342	2297.129253	20.168026
58.501817	2296.332920	20.173043
58.373841	2300.124559	20.178061
58.712851	2292.326392	20.183079
58.603437	2296.033063	20.188096
58.318403	2296.844694	20.193114
58.552461	2298.543920	20.198131
58.097789	2321.534872	20.203149
58.462268	2321.465180	20.208167
58.473842	2327.280122	20.213184
58.733525	2323.979208	20.218202
59.294057	2320.631160	20.223219
59.379443	2335.552551	20.228237
59.638931	2330.288564	20.233255
59.528940	2312.451705	20.238272
59.443711	2308.684075	20.243290
59.484246	2307.109176	20.248307
59.297847	2312.765764	20.253325
59.425714	2308.671229	20.258343
59.930499	2307.197178	20.263360
59.691686	2312.552680	20.268378
59.756358	2308.095625	20.273395
59.569392	2319.382806	20.278413
59.727896	2309.255297	20.283431
59.456390	2305.914524	20.288448
59.412287	2316.459727	20.293466
59.939108	2331.504475	20.298483
59.981710	2334.575051	20.303501
60.189183	2329.925187	20.308519
60.392329	2340.781995	20.313536
60.031594	2339.471953	20.318554
60.073633	2330.176958	20.323571
59.827408	2335.584125	20.328589
60.424353	2330.930050	20.333607
60.252369	2339.658444	20.338624
59.830052	2337.540617	20.343642
60.284941	2350.428401	20.348659
60.583018	2359.414549	20.353677
60.675855	2353.226673	20.358695
60.902899	2362.536408	20.363712
60.443283	2364.786180	20.368730
60.958812	2360.668769	20.373747
60.480675	2358.850049	20.378765
60.633840	2358.119119	20.383783
61.082499	2349.640963	20.388800
61.201591	2368.451751	20.393818
61.446527	2359.749863	20.398835
61.477776	2354.265982	20.403853
61.760392	2356.279531	20.408871
61.706048	2345.765586	20.413888
61.671442	2347.592126	20.418906
61.732685	2339.502910	20.423923
61.664960	2339.264226	20.428941
61.861226	2336.048993	20.433959
61.957958	2343.696925	20.438976
61.748941	2341.914945	20.443994
61.721826	2330.472000	20.449011
61.802850	2337.418578	20.454029
61.675599	2338.470603	20.459047
61.701347	2329.427493	20.464064
61.984306	2330.970724	20.469082
62.315354	2333.756242	20.474099
62.240492	2341.797168	20.479117
62.304812	2336.118745	20.484135
62.223128	2334.891227	20.489152
62.189053	2344.649003	20.494170
62.648080	2340.278492	20.499187
62.804608	2342.886207	20.504205
62.745441	2335.810035	20.509223
62.710687	2326.369267	20.514240
62.611529	2339.536372	20.519258
62.972233	2327.335166	20.524275
62.969816	2336.510408	20.529293
62.766806	2323.352851	20.534311
63.104667	2319.796669	20.539328
62.829986	2329.648944	20.544346
63.033604	2338.498388	20.549363
62.950105	2336.832455	20.554381
63.013302	2340.038674	20.559399
62.955217	2339.574395	20.564416
62.970162	2350.640594	20.569434
63.150039	2338.455088	20.574451
62.970061	2343.896064	20.579469
62.788660	2339.979378	20.584487
62.908818	2350.022291	20.589504
63.152951	2357.707102	20.594522
63.400840	2365.372390	20.599539
63.566806	2361.524364	20.604557
63.391699	2367.501124	20.609575
63.482037	2379.802197	20.614592
63.515362	2383.227720	20.619610
64.021754	2388.195061	20.624627
63.520946	2401.298895	20.629645
63.716568	2397.020137	20.634663
63.782292	2393.673853	20.639680
63.612727	2394.988158	20.644698
63.858391	2404.108785	20.649715
63.795435	2411.030608	20.654733
63.639716	2424.907297	20.659751
64.148532	2421.816667	20.664768
64.178535	2428.458816	20.669786
64.673427	2439.301536	20.674803
64.613349	2446.033552	20.679821
64.496653	2445.669982	20.684839
64.681716	2448.380550	20.689856
64.717210	2441.687178	20.694874
64.908135	2436.743203	20.699891
64.951215	2438.002101	20.704909
64.849304	2439.542519	20.709927
64.873527	2435.050740	20.714944
65.192573	2440.868044	20.719962
65.263446	2437.072774	20.724979
65.507033	2452.064160	20.729997
65.432667	2461.036121	20.735015
65.876447	2448.420988	20.740032
65.443787	2441.485351	20.745050
65.724500	2434.254893	20.750067
65.875655	2430.484920	20.755085
65.527425	2426.196680	20.760103
65.841069	2431.471972	20.765120
66.167155	2452.548082	20.770138
66.075445	2440.752232	20.775155
65.859580	2441.521470	20.780173
65.885509	2443.038703	20.785191
66.085230	2446.198301	20.790208
65.819705	2455.929277	20.795226
65.857982	2455.446742	20.800243
66.160384	2455.585613	20.805261
65.984528	2448.496117	20.810279
66.470105	2446.715764	20.815296
66.165971	2456.367574	20.820314
66.402167	2463.873774	20.825331
66.488695	2470.522864	20.830349
66.559226	2484.114816	20.835367
66.671530	2477.968033	20.840384
66.653065	2476.629605	20.845402
66.791694	2476.500614	20.850419
66.912604	2484.403622	20.855437
66.682749	2484.887845	20.860455
67.090181	2470.245837	20.865472
66.882959	2472.784316	20.870490
67.550193	2484.758364	20.875507
67.632909	2479.547279	20.880525
67.486206	2471.105535	20.885543
67.504224	2471.099594	20.890560
67.419395	2466.523897	20.895578
67.435774	2466.373030	20.900595
67.549794	2476.921959	20.905613
67.586120	2488.477250	20.910631
67.958981	2492.234647	20.915648
67.813818	2497.840646	20.920666
68.233200	2489.067179	20.925683
68.240628	2487.974028	20.930701
68.112255	2475.631575	20.935719
68.097624	2464.483266	20.940736
67.838721	2464.820545	20.945754
68.424668	2465.722963	20.950771
68.290958	2479.684618	20.955789
68.160741	2493.510023	20.960807
67.912397	2484.506623	20.965824
67.806296	2485.217636	20.970842
68.071911	2490.418411	20.975859
68.380413	2483.287731	20.980877
68.125778	2507.421664	20.985895
68.424372	2511.329570	20.990912
68.227499	2519.717931	20.995930
68.503028	2514.940579	21.000947
68.217050	2509.686254	21.005965
68.232629	2540.468924	21.010983
69.108211	2539.375466	21.016000
68.545596	2553.590590	21.021018
68.748219	2545.384447	21.026035
69.131895	2553.426217	21.031053
69.251346	2566.603423	21.036071
69.449484	2558.590501	21.041088
69.564317	2564.733362	21.046106
69.623649	2564.108654	21.051123
69.556590	2571.526697	21.056141
69.567047	2569.300007	21.061159
70.081956	2563.475168	21.066176
69.735530	2576.119390	21.071194
69.755615	2568.342668	21.076211
69.612953	2563.375175	21.081229
69.367248	2559.152900	21.086247
69.855981	2578.912808	21.091264
69.866152	2585.182540	21.096282
70.188760	2592.457480	21.101299
70.082448	2591.445267	21.106317
70.033728	2589.379341	21.111335
70.380939	2598.837648	21.116352
70.533557	2612.489428	21.121370
70.751734	2611.079195	21.126387
70.941947	2612.924193	21.131405
70.474609	2617.292992	21.136423
71.078007	2613.502624	21.141440
70.965646	2611.954809	21.146458
70.906916	2618.131194	21.151475
71.112402	2610.413777	21.156493
71.150446	2612.112184	21.161511
71.476155	2607.620469	21.166528
71.264882	2609.900797	21.171546
71.286956	2622.342133	21.176563
71.510914	2612.368320	21.181581
71.066834	2611.118658	21.186599
71.284389	2605.813818	21.191616
71.416362	2611.508991	21.196634
71.322460	2628.715374	21.201651
71.319938	2626.752671	21.206669
71.224047	2637.874286	21.211687
71.601986	2634.488510	21.216704
71.430081	2638.113513	21.221722
71.917995	2658.025133	21.226739
71.743740	2657.784197	21.231757
71.637670	2672.133036	21.236775
72.089177	2661.864738	21.241792
72.166909	2662.985664	21.246810
71.937524	2660.162148	21.251827
72.141862	2676.797925	21.256845
72.496071	2684.686562	21.261863
72.661205	2686.800616	21.266880
72.638304	2687.053580	21.271898
72.747287	2689.911821	21.276915
72.868998	2681.872945	21.281933
72.516442	2683.856644	21.286951
72.740641	2680.684316	21.291968
72.516500	2679.147696	21.296986
72.588039	2677.880368	21.302003
72.944160	2700.148253	21.307021
72.884828	2707.312647	21.312039
73.046517	2695.760985	21.317056
73.167728	2707.138997	21.322074
73.348012	2704.434348	21.327091
73.361765	2696.901587	21.332109
73.094474	2705.222162	21.337127
73.239590	2715.255057	21.342144
73.644961	2720.822213	21.347162
73.621666	2718.436671	21.352179
73.939748	2716.575225	21.357197
73.813709	2722.894751	21.362215
73.750608	2724.962507	21.367232
73.721467	2729.130117	21.372250
74.139563	2739.227567	21.377267
74.604691	2748.194050	21.382285
74.184534	2748.758594	21.387303
74.363562	2745.785860	21.392320
74.447981	2755.803038	21.397338
74.818823	2744.139671	21.402355
74.511621	2739.990112	21.407373
74.543490	2753.610418	21.412391
74.413403	2756.035854	21.417408
74.620117	2746.083606	21.422426
74.724929	2751.287557	21.427443
75.164963	2762.694557	21.432461
74.851854	2770.356384	21.437479
75.131418	2768.876554	21.442496
74.997048	2776.226323	21.447514
75.055557	2772.754851	21.452531
75.292793	2765.357482	21.457549
74.855199	2766.533903	21.462567
75.444109	2778.469921	21.467584
75.558754	2791.632264	21.472602
75.519095	2801.204946	21.477619
76.036291	2794.047761	21.482637
75.605679	2793.891175	21.487655
75.584795	2787.967151	21.492672
75.764687	2793.547563	21.497690
75.412215	2794.496028	21.502707
75.382751	2799.307570	21.507725
75.449997	2815.194841	21.512743
76.155567	2819.291549	21.517760
76.156476	2824.385552	21.522778
76.233118	2847.603236	21.527795
76.487321	2847.601322	21.532813
76.687065	2842.599043	21.537831
76.314204	2850.491200	21.542848
76.472776	2852.672581	21.547866
76.730204	2853.714866	21.552883
76.866763	2841.466370	21.557901
77.009195	2838.029081	21.562919
77.238972	2837.630155	21.567936
77.357543	2836.734192	21.572954
77.186355	2833.134574	21.577971
77.455462	2839.300701	21.582989
77.357134	2830.664993	21.588007
77.232403	2841.646067	21.593024
77.464108	2844.885943	21.598042
77.566117	2861.910355	21.603059
77.999015	2854.838946	21.608077
77.742199	2861.895469	21.613095
77.971722	2864.791664	21.618112
78.080800	2858.042421	21.623130
77.881675	2859.781166	21.628147
77.980844	2855.719409	21.633165
77.848527	2858.530265	21.638183
77.806135	2865.000858	21.643200
78.162883	2864.837692	21.648218
77.828459	2861.370954	21.653235
78.001769	2861.918269	21.658253
77.940389	2877.030383	21.663271
78.207476	2882.098481	21.668288
78.493362	2878.692363	21.673306
78.042677	2889.547787	21.678323
78.358709	2898.010618	21.683341
78.010161	2914.228243	21.688359
78.309065	2917.975223	21.693376
78.487152	2920.317679	21.698394
78.687081	2938.289468	21.703411
78.939113	2947.346250	21.708429
78.750798	2944.165915	21.713447
78.903638	2946.468143	21.718464
79.340138	2956.610174	21.723482
79.317410	2968.935677	21.728499
79.461424	2964.264031	21.733517
79.731206	2964.161833	21.738535
79.585127	2970.083744	21.743552
79.857412	2957.908592	21.748570
79.729790	2967.813922	21.753587
79.767477	2961.022171	21.758605
80.116759	2969.801762	21.763623
80.211161	2982.127859	21.768640
80.476922	2984.074683	21.773658
80.703758	2991.064949	21.778675
80.843154	2984.067880	21.783693
80.671732	2991.208917	21.788711
80.906916	2968.440953	21.793728
80.914141	2960.047456	21.798746
80.365591	2950.989857	21.803763
81.013014	2958.782176	21.808781
80.659909	2978.535545	21.813799
80.814112	2979.827570	21.818816
80.773385	2977.615161	21.823834
80.638260	2983.039833	21.828851
80.800664	2987.202743	21.833869
80.887114	2982.458049	21.838887
80.847376	2993.470086	21.843904
81.633924	2992.611490	21.848922
81.185903	3006.477610	21.853939
81.516284	2999.744143	21.858957
81.434501	3006.836423	21.863975
81.451488	3011.893242	21.868992
81.693411	3023.189416	21.874010
81.705377	3032.293322	21.879027
81.845838	3035.373935	21.884045
81.907788	3037.018136	21.889063
81.744573	3035.879094	21.894080
82.128759	3035.885221	21.899098
81.893358	3055.134171	21.904115
82.046751	3055.050208	21.909133
82.234889	3058.069699	21.914151
82.341508	3067.165105	21.919168
82.644022	3062.206633	21.924186
82.737537	3064.960045	21.929203
82.672759	3073.160685	21.934221
82.990429	3071.725361	21.939239
82.789881	3077.583248	21.944256
83.186678	3081.709456	21.949274
83.176521	3087.307111	21.954291
83.243598	3080.624335	21.959309
83.373243	3079.859187	21.964327
83.264319	3085.128284	21.969344
83.350075	3081.557797	21.974362
83.131668	3079.237495	21.979379
83.495446	3073.167892	21.984397
83.779494	3072.596334	21.989415
83.283553	3077.793503	21.994432
83.845714	3083.105801	21.999450
83.690649	3102.282246	22.004467
83.787534	3097.226575	22.009485
83.903598	3098.783398	22.014503
83.627222	3110.040893	22.019520
84.315745	3108.676869	22.024538
83.995701	3130.606193	22.029555
84.021953	3133.196560	22.034573
84.555621	3127.188696	22.039591
84.500766	3128.390393	22.044608
84.250076	3128.104614	22.049626
84.228997	3135.203215	22.054643
84.954624	3148.289031	22.059661
84.943298	3154.082577	22.064679
84.771295	3159.165890	22.069696
85.090317	3145.398848	22.074714
84.682694	3148.259194	22.079731
84.961496	3154.114597	22.084749
85.436914	3161.612016	22.089767
85.344612	3169.182603	22.094784
85.871028	3173.405307	22.099802
85.613943	3174.768097	22.104819
85.844699	3169.861870	22.109837
86.030832	3164.905823	22.114855
86.132070	3171.704368	22.119872
86.143477	3156.445256	22.124890
86.225971	3162.615482	22.129907
86.301342	3167.612697	22.134925
86.733592	3165.518694	22.139943
86.271939	3162.081299	22.144960
86.620872	3162.373858	22.149978
86.120382	3166.375541	22.154995
86.137761	3164.011974	22.160013
86.623044	3177.482655	22.165031
86.719861	3183.915771	22.170048
87.052784	3185.820532	22.175066
87.119706	3191.229392	22.180083
87.106891	3187.579640	22.185101
87.358759	3187.780093	22.190119
86.973665	3185.833081	22.195136
87.546860	3178.521784	22.200154
87.605967	3191.850933	22.205171
87.496846	3172.453891	22.210189
87.608194	3174.453335	22.215207
87.323052	3181.817421	22.220224
87.486732	3171.874838	22.225242
87.681626	3193.941343	22.230259
87.619717	3193.831143	22.235277
87.752593	3195.388496	22.240295
87.833606	3202.594223	22.245312
88.150856	3195.376676	22.250330
87.931028	3204.450703	22.255347
88.015832	3224.205168	22.260365
88.097638	3221.045588	22.265383
88.104715	3229.007789	22.270400
88.340471	3216.462590	22.275418
88.367714	3218.569904	22.280435
88.141512	3234.825460	22.285453
88.369353	3247.531679	22.290471
88.440994	3257.636357	22.295488
88.890410	3257.622797	22.300506
88.661916	3256.617063	22.305523
88.561687	3273.828207	22.310541
89.217479	3275.003793	22.315559
89.155973	3270.660959	22.320576
89.636381	3259.204191	22.325594
89.687942	3262.999465	22.330611
89.669116	3263.236018	22.335629
90.321406	3253.434621	22.340647
89.744398	3265.689352	22.345664
89.807630	3249.569848	22.350682
89.922326	3259.652000	22.355699
89.975816	3282.930685	22.360717
90.633145	3271.619786	22.365735
90.497716	3275.283389	22.370752
90.566977	3274.944323	22.375770
90.680890	3274.172163	22.380787
90.853525	3276.518677	22.385805
90.645815	3278.056803	22.390823
90.629993	3282.777960	22.395840
90.745900	3280.799788	22.400858
90.703035	3280.503539	22.405875
90.732682	3279.088075	22.410893
90.811583	3272.962037	22.415911
90.678944	3281.324905	22.420928
91.046447	3292.888795	22.425946
91.316184	3295.478913	22.430963
91.296412	3302.959286	22.435981
91.597980	3307.416095	22.440999
91.344643	3307.907173	22.446016
91.349246	3306.470380	22.451034
91.304579	3313.847344	22.456051
91.474183	3338.746022	22.461069
91.788548	3334.527348	22.466087
91.653695	3332.755741	22.471104
91.958697	3343.407819	22.476122
92.137271	3353.366390	22.481139
92.013895	3360.976645	22.486157
92.590691	3353.560556	22.491175
92.300741	3354.249905	22.496192
92.221218	3357.885828	22.501210
92.534474	3363.382397	22.506227
93.006181	3379.838057	22.511245
93.079076	3376.515718	22.516263
92.858481	3378.118998	22.521280
92.980313	3384.639798	22.526298
93.171929	3383.079011	22.531315
93.041658	3390.772422	22.536333
93.339777	3387.569454	22.541351
93.485687	3403.968865	22.546368
93.855099	3397.806739	22.551386
93.697538	3410.611331	22.556403
93.398808	3415.582006	22.561421
93.675379	3402.152831	22.566439
93.804507	3411.427950	22.571456
93.683260	3406.639935	22.576474
93.697483	3409.948707	22.581491
93.445152	3430.049753	22.586509
93.813036	3427.801677	22.591527
94.070691	3443.855361	22.596544
94.184966	3449.430476	22.601562
94.510927	3453.293270	22.606579
94.351031	3457.487847	22.611597
94.458277	3453.778198	22.616615
94.235095	3465.908191	22.621632
94.439973	3478.728641	22.626650
94.787111	3481.997893	22.631667
94.699357	3484.104317	22.636685
95.063958	3479.644172	22.641703
94.636532	3498.087254	22.646720
95.048152	3495.743941	22.651738
95.366468	3504.405548	22.656755
95.164881	3512.103871	22.661773
95.513080	3503.189565	22.666791
95.796291	3527.240591	22.671808
96.038764	3526.763912	22.676826
96.323918	3522.303578	22.681843
96.275402	3519.814566	22.686861
96.940294	3516.977059	22.691879
96.436219	3522.740609	22.696896
96.455116	3518.413524	22.701914
96.691537	3524.259907	22.706931
96.553699	3520.099413	22.711949
97.044829	3516.575801	22.716967
96.824233	3512.175769	22.721984
96.941311	3512.147995	22.727002
96.991938	3514.816662	22.732019
96.843898	3518.210846	22.737037
96.929797	3506.443286	22.742055
97.045540	3517.652225	22.747072
96.899215	3512.902830	22.752090
97.184627	3526.133644	22.757107
97.217653	3542.588742	22.762125
97.607381	3545.920772	22.767143
97.350611	3555.190142	22.772160
97.137974	3558.215694	22.777178
97.845541	3565.973606	22.782195
97.777044	3574.749508	22.787213
97.807130	3579.097415	22.792231
97.699431	3585.969883	22.797248
97.774738	3600.098504	22.802266
98.147256	3599.734014	22.807283
98.127278	3607.198763	22.812301
98.406966	3611.321348	22.817319
98.401425	3628.243393	22.822336
98.406991	3629.164210	22.827354
98.794017	3627.411813	22.832371
98.555233	3633.256931	22.837389
99.038015	3644.512603	22.842407
98.661151	3652.399420	22.847424
98.907656	3651.789540	22.852442
99.257765	3657.485588	22.857459
99.156152	3663.747957	22.862477
99.407062	3669.964566	22.867495
99.622019	3682.553169	22.872512
99.700192	3683.885565	22.877530
99.928358	3681.409997	22.882547
99.692100	3684.126792	22.887565
99.980025	3691.268733	22.892583
99.790698	3701.420858	22.897600
100.055076	3700.404162	22.902618
100.373912	3698.406778	22.907635
100.024287	3700.210212	22.912653
100.405282	3713.953300	22.917671
100.856118	3722.291240	22.922688
100.623874	3731.326442	22.927706
100.851757	3723.421975	22.932723
101.018732	3720.618258	22.937741
100.904181	3721.273828	22.942759
101.441086	3718.096518	22.947776
101.310976	3718.173755	22.952794
101.421089	3716.234321	22.957811
101.385026	3724.386567	22.962829
101.587865	3740.016682	22.967847
101.701812	3743.900130	22.972864
101.828848	3744.306374	22.977882
101.818908	3741.546154	22.982899
101.719254	3748.385859	22.987917
102.050929	3745.985599	22.992935
102.263089	3743.616690	22.997952
102.183296	3742.859078	23.002970
102.207612	3739.900952	23.007987
102.473148	3756.919527	23.013005
102.875563	3763.383879	23.018023
103.001858	3760.990544	23.023040
102.812030	3765.499205	23.028058
103.167012	3757.609531	23.033075
103.120368	3759.725328	23.038093
103.534009	3757.015527	23.043111
103.285016	3757.139797	23.048128
102.880784	3762.780463	23.053146
103.505452	3749.845702	23.058163
102.986830	3753.616782	23.063181
103.523398	3774.680401	23.068199
103.753504	3777.327300	23.073216
103.648752	3791.364339	23.078234
103.565792	3787.513979	23.083251
104.027483	3783.152178	23.088269
103.868730	3780.977100	23.093287
104.203351	3796.037408	23.098304
104.015677	3806.729073	23.103322
104.392673	3806.212372	23.108339
104.664813	3812.813939	23.113357
104.495425	3808.992897	23.118375
104.641911	3811.835971	23.123392
104.561844	3820.616961	23.128410
104.435841	3832.608874	23.133427
104.503226	3846.953563	23.138445
104.697807	3837.987408	23.143463
105.084081	3854.254878	23.148480
105.237436	3875.056701	23.153498
105.622581	3857.178618	23.158515
105.638491	3868.892654	23.163533
105.759007	3867.781702	23.168551
105.752849	3864.951430	23.173568
105.887541	3879.178282	23.178586
106.031418	3887.242440	23.183603
105.663163	3902.725440	23.188621
105.793440	3885.092425	23.193639
105.831306	3886.090261	23.198656
105.951058	3911.991800	23.203674
106.046058	3906.873071	23.208691
105.697578	3921.144092	23.213709
105.997072	3934.290932	23.218727
106.486069	3937.007768	23.223744
106.747709	3944.056080	23.228762
106.789090	3956.441651	23.233779
107.141366	3970.896467	23.238797
107.289203	3967.186667	23.243815
107.515929	3971.462827	23.248832
107.340407	3972.408878	23.253850
107.682865	3963.239578	23.258867
107.541352	3979.690855	23.263885
108.198574	3988.201750	23.268903
108.691828	3972.563444	23.273920
108.580793	3978.814772	23.278938
108.844171	3971.684268	23.283955
108.796959	3956.086463	23.288973
108.683931	3941.265986	23.293991
108.960821	3940.307289	23.299008
108.655906	3942.179495	23.304026
109.236283	3941.406824	23.309043
108.979397	3933.530869	23.314061
109.175504	3933.942078	23.319079
109.326519	3929.234368	23.324096
109.119691	3933.250179	23.329114
109.270960	3922.251738	23.334131
109.397047	3932.061031	23.339149
109.122520	3925.841794	23.344167
109.207484	3943.583242	23.349184
109.657891	3953.464835	23.354202
109.514000	3948.326706	23.359219
109.896244	3955.968469	23.364237
109.887637	3961.247354	23.369255
109.958618	3956.413294	23.374272
109.517765	3979.798732	23.379290
109.738603	3980.221850	23.384307
110.218622	3980.781120	23.389325
109.889717	3998.505396	23.394343
110.317766	4002.134523	23.399360
110.039749	4016.385109	23.404378
110.022464	4026.598841	23.409395
110.382101	4036.624113	23.414413
110.710303	4042.484693	23.419431
110.902882	4055.096000	23.424448
111.047056	4065.571692	23.429466
111.000730	4072.403164	23.434483
111.200018	4067.956150	23.439501
111.063552	4086.300584	23.444519
111.334442	4096.705938	23.449536
111.523777	4099.958993	23.454554
111.612213	4091.697444	23.459571
111.772320	4104.146582	23.464589
112.023539	4109.776200	23.469607
112.092627	4118.152038	23.474624
112.290946	4118.215698	23.479642
112.563884	4129.883321	23.484659
112.576133	4134.571894	23.489677
112.757545	4142.106317	23.494695
113.177047	4143.565187	23.499712
113.274354	4143.692020	23.504730
113.123452	4144.217573	23.509747
113.288296	4142.913430	23.514765
113.278683	4140.995864	23.519783
113.430066	4136.414300	23.524800
113.392299	4154.396132	23.529818
113.522464	4156.913549	23.534835
113.610843	4169.970536	23.539853
113.564463	4165.341038	23.544871
113.784324	4165.372915	23.549888
113.939245	4185.199511	23.554906
114.223211	4172.674508	23.559923
114.298379	4185.809331	23.564941
114.191076	4176.236923	23.569959
114.373825	4181.530083	23.574976
114.234098	4209.177175	23.579994
114.441036	4206.572292	23.585011
114.598740	4213.337130	23.590029
114.788143	4226.312045	23.595047
115.010780	4232.359674	23.600064
114.950552	4237.649884	23.605082
115.074253	4234.035349	23.610099
115.035441	4246.181166	23.615117
115.250019	4262.778922	23.620135
115.270126	4269.527462	23.625152
115.396776	4271.366809	23.630170
115.544420	4290.759070	23.635187
116.036792	4295.555537	23.640205
115.493307	4294.797949	23.645223
115.815971	4288.194632	23.650240
115.830492	4303.974682	23.655258
116.321101	4312.941114	23.660275
116.371133	4317.882644	23.665293
116.643596	4320.658715	23.670311
116.917900	4325.965982	23.675328
116.572093	4344.703310	23.680346
117.166205	4347.135441	23.685363
117.302307	4353.846901	23.690381
117.268943	4355.739734	23.695399
118.586376	4319.956855	23.700416
118.464688	4317.731714	23.705434
118.601672	4313.256525	23.710451
118.886407	4288.711523	23.715469
118.782122	4290.659651	23.720487
118.900139	4277.002156	23.725504
118.574972	4272.870836	23.730522
118.534839	4277.163626	23.735539
118.796538	4273.416987	23.740557
118.056149	4284.792096	23.745575
118.586319	4270.119941	23.750592
118.341062	4270.442484	23.755610
118.677229	4280.320059	23.760627
118.929567	4295.295825	23.765645
118.995122	4305.174777	23.770663
119.479079	4303.473417	23.775680
119.517484	4298.900043	23.780698
119.509259	4306.628381	23.785715
119.370040	4299.412471	23.790733
119.530610	4310.949462	23.795751
119.555421	4323.713499	23.800768
119.828898	4323.613876	23.805786
119.768791	4332.729727	23.810803
119.835586	4337.558160	23.815821
120.157132	4359.334789	23.820839
120.102061	4351.951007	23.825856
120.180747	4364.053243	23.830874
120.216293	4368.413110	23.835891
120.361767	4384.655655	23.840909
120.090670	4394.461139	23.845927
120.624746	4395.548556	23.850944
120.803068	4417.417135	23.855962
120.732570	4423.968443	23.860979
121.101054	4434.330294	23.865997
121.030205	4445.010343	23.871015
121.013963	4454.637046	23.876032
120.940179	4462.833411	23.881050
121.055282	4476.208393	23.886067
121.356865	4488.869211	23.891085
121.332382	4507.051325	23.896103
121.514471	4508.967236	23.901120
121.779123	4529.307308	23.906138
122.003233	4542.491653	23.911155
122.480555	4542.082321	23.916173
122.471195	4558.077819	23.921191
122.730025	4568.646316	23.926208
122.756372	4559.062237	23.931226
122.808245	4568.249044	23.936243
123.120930	4565.779055	23.941261
123.534718	4591.562897	23.946279
123.690681	4581.049425	23.951296
124.037610	4585.701463	23.956314
123.879443	4583.390465	23.961331
124.021967	4581.979311	23.966349
123.984443	4587.262909	23.971367
123.911537	4585.348900	23.976384
123.725043	4585.289773	23.981402
123.616404	4595.300338	23.986419
123.934758	4601.626650	23.991437
124.110675	4610.749854	23.996455
124.156361	4611.535019	24.001472
124.101241	4621.382544	24.006490
124.508034	4629.891945	24.011507
124.819627	4633.678332	24.016525
124.938639	4654.019265	24.021543
125.137470	4649.872051	24.026560
125.416509	4657.729142	24.031578
125.304189	4664.817384	24.036595
125.684127	4656.573039	24.041613
125.378854	4682.883170	24.046631
125.693586	4682.751829	24.051648
125.682110	4681.345856	24.056666
125.409858	4686.808300	24.061683
126.057826	4698.528013	24.066701
126.180422	4714.057905	24.071719
126.504419	4711.677663	24.076736
126.334903	4716.211784	24.081754
126.492275	4734.371948	24.086771
126.755731	4734.415937	24.091789
126.653608	4738.885844	24.096807
127.017898	4739.668448	24.101824
127.151420	4752.838729	24.106842
127.103389	4762.429541	24.111859
127.420199	4767.143162	24.116877
127.256828	4776.092333	24.121895
127.105324	4782.940550	24.126912
127.701004	4795.366113	24.131930
127.667057	4803.777349	24.136947
127.889341	4817.413566	24.141965
127.887419	4817.246608	24.146983
127.871462	4825.017412	24.152000
128.238873	4839.909312	24.157018
128.179061	4849.287369	24.162035
128.809103	4851.470887	24.167053
128.567582	4868.926636	24.172071
128.834079	4863.323071	24.177088
129.029222	4872.771676	24.182106
129.321156	4873.054259	24.187123
129.504847	4879.919441	24.192141
129.771226	4898.757134	24.197159
130.050193	4895.418016	24.202176
130.080181	4890.549096	24.207194
129.861941	4888.001259	24.212211
130.369891	4886.775886	24.217229
130.403454	4888.677228	24.222247
130.318222	4888.277110	24.227264
130.697974	4907.198060	24.232282
130.930904	4904.049234	24.237299
131.043125	4904.779796	24.242317
130.917496	4913.634738	24.247335
131.083745	4908.264668	24.252352
131.040865	4911.835184	24.257370
130.833091	4917.268657	24.262387
131.434307	4922.288140	24.267405
131.356316	4935.677928	24.272423
131.742014	4932.429406	24.277440
131.814889	4932.818911	24.282458
132.038989	4946.259233	24.287475
132.060922	4951.931350	24.292493
132.002442	4951.145094	24.297511
132.412509	4942.858022	24.302528
132.812944	4948.480307	24.307546
132.762507	4942.531800	24.312563
133.127408	4946.398286	24.317581
133.111166	4946.385086	24.322599
133.126048	4955.877758	24.327616
133.465063	4954.328469	24.332634
133.365756	4963.012013	24.337651
133.096240	4958.268912	24.342669
133.271910	4961.262268	24.347687
133.590098	4967.525603	24.352704
133.687996	4958.779222	24.357722
133.618774	4970.908191	24.362739
133.690206	4986.392669	24.367757
133.735025	4987.847181	24.372775
134.167953	4996.816676	24.377792
134.344239	4997.082658	24.382810
134.101610	5015.457285	24.387827
134.589023	5019.127825	24.392845
134.613214	5018.786319	24.397863
134.735803	5031.342982	24.402880
134.820258	5039.846257	24.407898
134.607692	5043.074063	24.412915
135.139681	5060.623459	24.417933
135.552530	5071.846786	24.422951
135.484763	5071.639637	24.427968
135.717237	5065.773029	24.432986
135.902783	5076.864672	24.438003
136.004560	5089.494080	24.443021
136.103539	5097.010249	24.448039
136.305583	5093.099177	24.453056
136.464108	5090.549103	24.458074
136.471933	5105.589097	24.463091
136.673684	5113.830972	24.468109
136.733405	5120.182203	24.473127
136.469486	5126.511538	24.478144
136.885175	5129.060117	24.483162
137.015188	5137.269049	24.488179
137.414503	5132.941957	24.493197
137.640450	5123.853463	24.498215
137.840595	5140.665775	24.503232
138.628538	5148.193978	24.508250
138.574123	5150.197516	24.513267
138.667390	5147.291492	24.518285
138.875052	5147.360007	24.523303
138.570379	5149.939375	24.528320
139.214424	5137.249974	24.533338
138.965194	5138.826325	24.538355
139.306776	5140.089152	24.543373
139.262412	5137.842325	24.548391
139.023396	5148.122991	24.553408
138.905410	5144.893367	24.558426
139.003120	5148.523976	24.563443
139.123416	5152.820248	24.568461
139.483832	5168.038643	24.573479
139.455499	5175.069733	24.578496
139.984735	5178.446502	24.583514
139.852849	5195.089920	24.588531
139.826676	5201.442009	24.593549
140.011860	5204.699071	24.598567
139.917729	5228.944050	24.603584
140.315059	5233.525226	24.608602
140.121263	5245.683364	24.613619
140.840765	5249.595373	24.618637
140.567588	5261.791211	24.623655
140.397909	5270.053468	24.628672
141.107524	5282.603565	24.633690
140.898396	5293.937101	24.638707
141.426739	5307.247952	24.643725
141.545650	5301.894653	24.648743
141.360544	5316.804059	24.653760
141.771237	5323.154037	24.658778
141.754368	5344.101006	24.663795
142.051030	5339.250163	24.668813
142.456345	5357.002777	24.673831
142.296501	5356.301830	24.678848
142.674310	5357.950421	24.683866
142.644217	5367.002110	24.688883
142.628341	5368.182064	24.693901
142.911864	5375.903027	24.698919
142.833607	5388.103134	24.703936
143.003402	5390.014752	24.708954
143.016772	5399.747798	24.713971
143.384317	5410.789034	24.718989
143.649611	5427.338872	24.724007
143.622689	5424.691539	24.729024
144.429805	5433.763618	24.734042
144.490426	5440.891356	24.739059
144.372213	5451.175362	24.744077
144.430748	5453.906209	24.749095
144.396214	5448.703172	24.754112
144.777012	5453.167042	24.759130
144.913949	5467.243267	24.764147
144.983747	5480.651338	24.769165
145.238320	5474.733788	24.774183
145.071489	5495.713895	24.779200
145.160053	5492.151967	24.784218
145.481944	5501.117012	24.789235
145.215680	5519.394834	24.794253
145.453915	5514.881392	24.799271
145.517782	5534.367020	24.804288
146.056962	5555.160826	24.809306
146.139403	5560.419597	24.814323
146.541589	5573.308474	24.819341
146.689800	5584.548326	24.824359
146.801504	5588.688212	24.829376
146.804242	5581.771534	24.834394
146.942297	5603.256418	24.839411
147.204223	5607.915724	24.844429
147.412549	5603.460609	24.849447
147.427870	5625.359333	24.854464
147.801319	5630.607257	24.859482
147.877821	5637.890418	24.864499
147.908307	5650.237811	24.869517
148.221520	5644.222633	24.874535
148.011591	5662.068775	24.879552
148.278121	5662.450054	24.884570
148.454435	5677.464123	24.889587
148.617548	5682.467225	24.894605
148.731433	5690.173861	24.899623
148.556870	5702.405049	24.904640
148.772126	5714.297384	24.909658
148.758636	5727.412484	24.914675
149.255121	5735.507451	24.919693
149.374010	5745.631364	24.924711
149.468743	5752.441366	24.929728
149.900670	5768.198327	24.934746
149.979134	5771.775255	24.939763
150.408034	5778.163578	24.944781
150.499040	5773.793094	24.949799
150.560597	5799.188733	24.954816
151.072878	5785.338917	24.959834
151.055414	5793.122996	24.964851
151.197427	5789.773607	24.969869
151.150305	5779.755300	24.974887
151.250919	5814.435055	24.979904
151.388507	5815.224814	24.984922
151.721362	5818.992338	24.989939
151.534312	5825.133093	24.994957
151.945906	5830.154128	24.999975
152.005522	5844.435317	25.004992
151.939445	5846.620691	25.010010
152.015913	5852.477103	25.015027
152.510509	5859.653815	25.020045
152.586845	5864.061313	25.025063
152.989505	5877.742670	25.030080
152.691106	5876.084823	25.035098
153.233922	5881.937632	25.040115
153.027172	5900.054986	25.045133
153.254165	5901.335821	25.050151
153.067211	5910.709087	25.055168
153.375147	5916.762855	25.060186
153.649003	5917.288203	25.065203
153.870213	5930.991713	25.070221
154.005180	5945.595790	25.075239
153.879806	5958.409753	25.080256
154.456022	5958.306891	25.085274
154.192020	5972.679917	25.090291
154.584565	5980.892294	25.095309
154.630774	5985.787524	25.100327
154.950042	6005.170505	25.105344
155.189737	6002.475006	25.110362
155.313955	6003.876122	25.115379
155.246336	6025.636794	25.120397
155.458745	6023.744225	25.125415
155.680557	6041.605173	25.130432
155.676019	6054.810651	25.135450
155.839944	6059.485426	25.140467
155.665068	6074.902084	25.145485
156.452757	6083.087326	25.150503
156.797670	6092.102721	25.155520
157.088180	6084.177955	25.160538
157.621731	6095.304086	25.165555
157.582627	6105.235133	25.170573
157.555419	6098.872230	25.175591
157.506335	6109.483548	25.180608
157.650164	6105.297273	25.185626
158.231937	6103.956087	25.190643
158.247252	6096.308030	25.195661
158.239641	6110.732543	25.200679
158.469029	6124.801103	25.205696
158.164400	6126.373588	25.210714
158.496383	6125.052593	25.215731
158.384583	6156.126512	25.220749
158.671266	6151.791575	25.225767
158.897235	6163.275299	25.230784
159.272443	6180.045358	25.235802
159.296683	6188.179788	25.240819
159.484291	6199.694799	25.245837
159.754958	6187.119995	25.250855
159.356619	6217.370793	25.255872
159.520300	6220.612465	25.260890
159.810888	6217.896334	25.265907
159.948422	6246.011313	25.270925
160.215353	6246.480933	25.275943
159.965778	6276.115044	25.280960
160.255775	6276.937770	25.285978
160.791520	6284.550155	25.290995
160.804546	6302.687141	25.296013
161.099743	6303.824733	25.301031
161.191488	6317.694029	25.306048
161.510336	6326.372688	25.311066
161.666110	6332.365200	25.316083
161.481061	6354.836000	25.321101
161.987403	6354.851416	25.326119
161.628648	6370.833788	25.331136
162.135452	6371.212166	25.336154
162.692377	6379.105386	25.341171
162.216598	6398.199797	25.346189
162.552181	6418.183612	25.351207
162.758093	6417.305363	25.356224
162.859127	6428.237441	25.361242
163.519699	6433.213324	25.366259
163.669544	6438.212399	25.371277
163.893948	6432.485522	25.376295
164.005001	6440.947400	25.381312
164.009596	6450.455087	25.386330
164.162885	6460.135207	25.391347
164.153138	6465.336074	25.396365
164.525626	6454.790763	25.401383
164.795301	6475.921426	25.406400
164.701271	6478.733150	25.411418
164.690778	6481.140340	25.416435
164.861427	6494.021946	25.421453
164.836519	6512.405002	25.426471
165.009874	6520.945548	25.431488
165.011483	6539.851668	25.436506
165.445251	6544.285412	25.441523
165.653168	6561.467165	25.446541
165.745400	6566.655241	25.451559
165.876673	6573.882841	25.456576
166.242378	6602.833911	25.461594
166.665659	6596.112986	25.466611
166.731456	6610.040234	25.471629
166.743289	6620.282423	25.476647
166.847691	6628.338194	25.481664
167.140333	6629.248915	25.486682
167.650805	6638.172348	25.491699
167.752046	6658.979198	25.496717
167.822458	6658.321047	25.501735
167.788105	6669.672245	25.506752
167.376105	6685.009759	25.511770
168.221310	6687.516527	25.516787
168.146081	6706.280170	25.521805
168.450095	6697.090277	25.526823
168.988504	6724.486556	25.531840
168.941658	6731.044454	25.536858
169.111193	6731.807152	25.541875
169.055876	6746.953092	25.546893
169.399293	6763.933864	25.551911
169.748772	6760.008813	25.556928
169.524908	6780.614182	25.561946
170.086961	6788.364717	25.566963
169.651342	6793.730259	25.571981
170.209950	6806.870151	25.576999
170.426144	6823.362650	25.582016
170.286406	6828.464023	25.587034
170.503065	6845.098528	25.592051
170.768907	6850.130053	25.597069
170.736472	6873.284722	25.602087
171.047756	6881.911162	25.607104
171.102350	6903.467469	25.612122
171.664108	6906.675311	25.617139
171.061528	6914.532590	25.622157
171.871074	6926.904010	25.627175
172.087958	6931.094018	25.632192
172.258012	6952.891161	25.637210
172.745849	6957.622756	25.642227
172.868728	6964.510878	25.647245
172.948091	6972.734884	25.652263
173.378540	6984.913180	25.657280
173.381948	6977.727532	25.662298
173.484265	6975.179692	25.667315
174.009710	6988.470128	25.672333
174.148604	6990.108948	25.677351
174.349615	6997.770916	25.682368
174.733130	6996.918484	25.687386
174.715914	6988.776358	25.692404
174.894430	6986.582781	25.697421
175.021329	6985.862103	25.702439
174.967644	6992.597952	25.707456
175.214166	6999.435148	25.712474
175.227327	6998.665992	25.717492
175.262481	7016.257224	25.722509
175.610275	7012.723843	25.727527
175.794540	7012.745524	25.732544
175.303668	7037.538055	25.737562
175.823024	7042.877179	25.742580
176.193594	7052.068974	25.747597
176.183074	7058.599198	25.752615
176.229945	7076.535915	25.757632
176.232985	7084.869792	25.762650
176.705646	7094.692787	25.767668
176.947318	7100.309044	25.772685
177.109561	7116.955479	25.777703
177.169489	7128.917263	25.782720
177.152730	7135.713676	25.787738
177.345682	7145.359531	25.792756
177.760215	7157.682499	25.797773
177.736602	7172.189274	25.802791
177.839703	7184.573678	25.807808
177.951586	7206.819051	25.812826
178.404663	7214.470033	25.817844
178.474095	7230.562857	25.822861
178.539628	7242.242868	25.827879
178.843271	7256.752109	25.832896
179.220568	7264.282391	25.837914
179.729979	7259.539781	25.842932
180.036102	7275.305122	25.847949
180.106490	7281.560722	25.852967
180.324577	7284.863514	25.857984
180.154280	7290.437033	25.863002
180.495526	7306.016951	25.868020
180.416507	7316.712579	25.873037
180.550092	7325.764847	25.878055
181.263951	7345.766178	25.883072
181.015146	7347.456297	25.888090
180.960202	7362.706865	25.893108
181.347207	7374.611255	25.898125
181.509507	7385.152309	25.903143
181.989032	7406.772070	25.908160
181.905500	7415.994147	25.913178
182.051053	7420.179657	25.918196
182.240550	7444.458892	25.923213
182.428313	7446.712026	25.928231
182.551317	7468.359300	25.933248
182.489343	7475.387069	25.938266
183.032847	7487.317526	25.943284
182.979810	7502.394275	25.948301
182.843276	7519.709811	25.953319
183.390491	7518.007730	25.958336
183.011541	7541.949951	25.963354
183.602531	7558.109732	25.968372
184.181591	7585.276778	25.973389
183.963268	7584.698557	25.978407
184.788392	7600.733299	25.983424
184.658233	7611.080365	25.988442
184.913010	7617.499770	25.993460
185.503932	7638.092102	25.998477
185.323924	7642.937974	26.003495
185.472370	7645.629806	26.008512
185.515535	7666.484776	26.013530
186.187714	7658.259609	26.018548
186.200727	7662.930024	26.023565
186.362282	7689.326016	26.028583
186.567874	7689.780030	26.033600
186.546591	7696.195356	26.038618
186.549954	7712.453645	26.043636
187.173388	7716.024503	26.048653
186.841271	7726.419058	26.053671
187.114698	7730.682475	26.058688
186.825215	7757.578584	26.063706
187.454030	7766.029413	26.068724
187.526947	7773.231900	26.073741
187.664656	7788.187444	26.078759
188.469471	7794.735422	26.083776
188.662654	7796.444736	26.088794
189.062118	7807.460320	26.093812
189.149931	7820.437916	26.098829
189.797701	7827.632450	26.103847
189.684482	7826.374771	26.108864
189.485737	7838.478566	26.113882
189.804246	7842.144575	26.118900
189.705867	7855.773307	26.123917
189.795384	7866.629117	26.128935
190.222457	7876.210264	26.133952
190.461920	7884.990496	26.138970
190.215717	7893.878389	26.143988
190.890490	7910.281078	26.149005
190.874493	7920.051629	26.154023
191.018676	7933.847628	26.159040
190.854953	7945.964949	26.164058
191.209221	7952.681437	26.169076
192.237960	7954.070441	26.174093
192.250787	7952.470984	26.179111
192.757974	7953.745956	26.184128
192.717523	7971.072118	26.189146
192.908795	7980.680789	26.194164
193.451256	7982.117563	26.199181
193.446515	7978.374034	26.204199
193.662342	7971.871382	26.209216
193.773443	7983.487895	26.214234
193.773308	7997.101340	26.219252
194.115805	8001.013033	26.224269
193.756033	8004.987389	26.229287
194.248359	8012.850397	26.234304
194.541894	8027.484956	26.239322
194.850369	8026.167514	26.244340
195.018480	8028.966820	26.249357
195.112627	8039.566282	26.254375
195.727065	8047.258633	26.259392
195.720497	8048.026876	26.264410
195.390347	8051.456736	26.269428
195.641148	8056.001599	26.274445
195.850868	8079.501853	26.279463
196.050618	8085.661689	26.284480
196.127309	8108.463000	26.289498
196.066593	8102.467721	26.294516
196.600554	8129.276411	26.299533
196.273296	8147.275936	26.304551
196.472741	8150.616533	26.309568
196.816442	8175.058841	26.314586
196.743522	8199.042366	26.319604
196.907432	8211.531588	26.324621
197.208848	8232.697181	26.329639
197.707802	8240.177234	26.334656
197.522136	8269.387788	26.339674
197.817936	8287.217225	26.344692
197.933656	8303.098517	26.349709
198.074106	8325.656477	26.354727
198.174052	8334.304080	26.359744
198.695242	8360.313189	26.364762
199.011364	8384.210748	26.369780
199.360690	8389.055974	26.374797
199.333505	8405.988977	26.379815
199.799902	8417.957376	26.384832
199.592722	8422.697206	26.389850
199.999040	8444.692728	26.394868
200.299527	8447.585018	26.399885
199.904926	8465.267054	26.404903
200.378053	8480.707332	26.409920
200.845368	8495.772828	26.414938
200.630897	8512.949957	26.419956
200.894911	8532.650505	26.424973
200.847714	8556.182141	26.429991
201.316449	8567.124184	26.435008
201.418745	8587.146901	26.440026
201.749495	8614.152302	26.445044
201.713495	8626.644708	26.450061
202.359494	8658.466035	26.455079
202.587359	8659.191262	26.460096
202.597830	8672.806699	26.465114
203.182251	8690.654453	26.470132
204.400657	8691.887519	26.475149
204.499076	8707.023608	26.480167
204.773396	8692.839510	26.485184
204.785243	8699.417325	26.490202
204.768004	8698.813879	26.495220
205.094298	8714.817239	26.500237
204.931413	8718.593568	26.505255
205.370776	8722.089274	26.510272
205.639420	8726.331572	26.515290
205.535243	8746.610969	26.520308
205.646201	8744.172036	26.525325
205.652017	8761.526417	26.530343
206.116196	8764.033190	26.535360
206.359372	8772.930080	26.540378
206.400436	8785.356847	26.545396
206.858985	8796.985742	26.550413
206.988347	8806.806604	26.555431
206.867446	8823.464203	26.560448
207.214115	8835.795769	26.565466
207.399441	8849.399728	26.570484
207.408596	8856.432663	26.575501
207.402573	8875.181348	26.580519
208.038056	8890.359741	26.585536
208.297422	8908.236528	26.590554
208.285871	8929.897119	26.595572
208.417426	8933.621050	26.600589
208.840460	8961.862773	26.605607
208.671053	8971.607395	26.610624
209.305529	8987.951054	26.615642
208.924321	8997.239493	26.620660
209.142013	9005.256454	26.625677
209.610626	9041.125428	26.630695
209.947143	9054.270149	26.635712
210.163127	9078.348469	26.640730
210.046089	9087.917611	26.645748
210.786735	9097.854401	26.650765
211.119377	9105.682904	26.655783
211.412227	9111.885329	26.660800
212.025028	9118.669089	26.665818
211.942625	9132.896139	26.670836
212.228552	9138.588176	26.675853
212.110413	9145.859015	26.680871
212.405533	9155.022636	26.685888
212.615241	9168.300966	26.690906
212.833019	9182.582061	26.695924
213.063358	9194.240642	26.700941
213.331667	9209.672571	26.705959
213.286893	9221.923638	26.710976
213.664697	9221.078322	26.715994
213.787279	9239.756711	26.721012
214.108921	9231.453166	26.726029
214.201314	9254.581784	26.731047
214.189950	9258.725991	26.736064
214.727835	9269.433449	26.741082
214.998368	9290.279885	26.746100
215.152809	9296.027299	26.751117
214.929147	9309.698825	26.756135
214.877096	9328.575156	26.761152
215.392825	9330.669795	26.766170
215.380293	9345.508053	26.771188
215.338071	9364.869109	26.776205
215.183848	9381.731338	26.781223
215.870627	9401.514974	26.786240
216.136132	9424.919787	26.791258
216.050510	9449.222647	26.796276
216.413120	9461.419524	26.801293
216.329472	9494.202759	26.806311
216.941976	9519.615080	26.811328
217.301851	9541.142418	26.816346
217.150857	9572.758647	26.821364
217.740406	9581.727958	26.826381
218.047231	9598.786532	26.831399
218.110299	9627.211953	26.836416
218.545317	9643.101202	26.841434
218.657278	9668.885777	26.846452
219.117672	9685.670941	26.851469
218.899900	9702.123483	26.856487
219.429562	9716.018288	26.861504
219.777718	9734.207171	26.866522
219.960057	9760.669158	26.871540
219.852737	9765.576812	26.876557
220.220274	9794.507334	26.881575
220.314771	9808.934519	26.886592
220.608470	9831.252437	26.891610
220.665430	9846.822198	26.896628
221.172449	9870.227625	26.901645
221.459951	9891.226787	26.906663
221.714989	9907.940127	26.911680
222.275046	9923.633212	26.916698
222.197813	9939.511398	26.921716
222.419336	9952.968410	26.926733
222.736402	9974.632409	26.931751
223.125947	9995.344164	26.936768
223.413459	10003.473758	26.941786
223.678494	10020.340347	26.946804
223.531645	10033.372037	26.951821
223.996265	10048.587619	26.956839
223.918806	10061.914730	26.961856
224.575432	10077.349694	26.966874
224.537771	10091.014753	26.971892
224.734194	10115.245878	26.976909
224.668536	10130.901390	26.981927
224.460117	10152.853153	26.986944
225.412292	10161.794354	26.991962
225.528476	10185.141420	26.996980
225.880641	10208.407343	27.001997
226.039980	10220.232405	27.007015
226.309644	10241.351583	27.012032
226.940248	10258.915754	27.017050
227.060363	10277.617671	27.022068
227.241471	10270.551313	27.027085
227.313902	10281.973242	27.032103
227.774163	10294.995258	27.037120
227.777685	10302.152762	27.042138
228.230609	10324.493689	27.047156
228.839747	10329.071385	27.052173
229.477780	10329.865041	27.057191
229.935183	10327.396889	27.062208
230.158147	10325.347520	27.067226
230.090278	10335.777907	27.072244
229.947642	10332.017617	27.077261
230.424205	10328.090860	27.082279
230.622759	10335.644085	27.087296
230.575301	10327.969385	27.092314
230.447757	10346.097614	27.097332
230.887650	10350.367135	27.102349
231.170133	10362.147737	27.107367
231.297406	10374.467332	27.112384
231.329042	10385.403146	27.117402
231.853293	10391.118226	27.122420
232.000779	10404.587162	27.127437
231.872149	10424.029159	27.132455
231.855569	10436.889162	27.137472
232.068426	10437.698909	27.142490
232.073006	10471.887757	27.147508
232.534147	10481.243893	27.152525
232.753215	10506.277143	27.157543
232.816125	10531.173857	27.162560
232.883743	10542.580911	27.167578
233.198429	10572.468176	27.172596
233.526818	10588.024450	27.177613
233.863951	10615.240151	27.182631
233.858365	10634.401014	27.187648
234.243022	10659.149610	27.192666
234.439964	10676.576871	27.197684
234.707168	10698.783148	27.202701
234.884034	10724.432709	27.207719
235.133867	10744.090455	27.212736
235.835134	10761.404057	27.217754
235.567275	10796.772898	27.222772
235.966803	10806.786151	27.227789
236.264142	10832.590653	27.232807
236.408145	10851.961964	27.237824
236.913816	10869.574702	27.242842
236.899020	10884.654512	27.247860
237.094766	10908.766781	27.252877
237.654874	10931.094800	27.257895
237.919523	10956.061516	27.262912
237.988849	10967.484349	27.267930
238.170548	10987.762441	27.272948
238.038342	11002.775483	27.277965
239.055947	11033.153311	27.282983
239.141708	11051.785599	27.288000
239.275192	11063.267907	27.293018
239.663476	11077.997384	27.298036
239.836386	11084.996031	27.303053
240.341254	11109.590613	27.308071
240.134716	11133.106248	27.313088
240.410117	11137.648015	27.318106
240.892999	11157.569661	27.323124
240.849697	11189.367518	27.328141
241.515636	11203.226297	27.333159
241.369054	11228.128334	27.338176
241.911714	11236.300594	27.343194
241.881502	11253.062980	27.348212
241.959731	11269.615776	27.353229
242.761179	11288.502470	27.358247
242.566958	11304.093844	27.363264
242.955472	11314.093307	27.368282
243.465034	11330.818568	27.373300
243.680156	11343.838669	27.378317
243.843433	11362.181248	27.383335
243.834456	11373.550284	27.388352
243.998260	11390.408705	27.393370
244.146750	11417.105687	27.398388
244.385068	11436.889113	27.403405
245.142619	11447.146602	27.408423
245.034258	11455.395683	27.413440
245.535955	11477.575620	27.418458
245.592245	11493.001599	27.423476
246.076094	11509.516326	27.428493
246.389358	11507.146389	27.433511
246.188740	11539.168416	27.438528
247.014621	11542.872515	27.443546
246.708285	11562.365630	27.448564
246.811199	11580.348427	27.453581
247.193226	11605.695489	27.458599
247.348852	11627.127760	27.463616
247.443986	11645.667595	27.468634
248.051246	11654.767759	27.473652
247.800122	11684.281247	27.478669
248.159772	11705.735327	27.483687
248.348098	11734.640082	27.488704
248.712897	11751.584175	27.493722
249.087139	11767.434230	27.498740
249.037883	11786.063135	27.503757
249.136500	11810.068624	27.508775
249.673488	11839.916766	27.513792
250.280894	11863.741573	27.518810
250.616252	11880.851440	27.523828
250.837509	11900.480138	27.528845
251.502895	11915.728944	27.533863
251.524508	11937.930950	27.538880
251.688003	11946.848154	27.543898
252.002501	11969.462191	27.548916
252.122931	11984.995362	27.553933
252.463910	12001.586585	27.558951
252.425797	12026.005333	27.563968
252.821263	12041.858610	27.568986
253.406743	12058.758936	27.574004
253.556458	12084.951428	27.579021
253.730944	12101.897231	27.584039
253.655492	12123.192587	27.589056
254.254924	12133.841528	27.594074
254.413812	12156.906469	27.599092
254.478376	12181.726162	27.604109
254.636674	12204.257585	27.609127
254.692596	12222.999913	27.614144
255.041267	12245.649980	27.619162
255.541557	12263.195398	27.624180
255.183842	12290.042387	27.629197
256.180110	12310.554290	27.634215
256.052094	12344.599945	27.639232
256.224966	12364.991427	27.644250
256.672845	12385.772473	27.649268
256.998864	12411.082026	27.654285
257.343388	12423.173145	27.659303
257.268223	12457.393878	27.664320
257.546572	12479.237359	27.669338
257.953299	12506.239634	27.674356
257.793438	12526.598152	27.679373
258.522162	12559.253154	27.684391
258.425694	12585.282802	27.689408
258.705579	12606.630404	27.694426
259.344800	12625.824909	27.699444
259.325818	12660.848783	27.704461
259.687112	12678.631098	27.709479
259.892705	12701.746228	27.714496
259.934339	12728.919699	27.719514
260.754287	12747.612334	27.724532
260.758066	12772.691798	27.729549
261.499674	12784.316733	27.734567
261.483667	12797.958258	27.739584
262.672424	12808.651053	27.744602
263.031790	12821.513790	27.749620
262.863542	12828.418108	27.754637
263.156049	12827.106002	27.759655
263.575933	12846.252987	27.764672
263.968877	12853.909407	27.769690
263.935870	12858.679906	27.774708
263.943048	12885.322154	27.779725
264.487572	12879.821063	27.784743
264.531126	12902.942876	27.789760
264.417342	12907.871306	27.794778
265.032552	12929.258323	27.799796
264.870344	12950.441882	27.804813
265.022106	12966.773066	27.809831
264.935068	12988.939640	27.814848
265.382069	13011.947858	27.819866
265.773672	13038.369045	27.824884
265.755154	13069.247220	27.829901
266.597406	13092.679943	27.834919
266.262812	13114.613861	27.839936
266.545193	13142.782863	27.844954
267.192408	13165.118837	27.849972
267.641974	13190.296392	27.854989
267.700502	13213.908881	27.860007
267.734932	13240.705257	27.865024
267.994470	13255.832407	27.870042
268.313284	13293.877246	27.875060
268.386323	13315.475952	27.880077
268.980787	13337.226691	27.885095
269.239678	13370.158806	27.890112
269.119976	13397.203766	27.895130
269.641280	13422.739877	27.900148
269.922243	13452.684362	27.905165
270.545502	13467.868392	27.910183
270.583619	13488.579046	27.915200
271.049530	13516.663009	27.920218
271.581240	13541.547098	27.925236
271.460408	13564.420719	27.930253
271.606479	13585.499847	27.935271
271.780034	13612.701288	27.940288
272.150893	13641.198238	27.945306
272.924827	13655.995640	27.950324
272.908650	13685.835453	27.955341
272.925710	13705.362215	27.960359
273.493282	13729.268252	27.965376
274.092648	13748.321714	27.970394
274.467367	13764.176529	27.975412
274.545719	13794.446991	27.980429
275.251257	13802.010614	27.985447
275.239308	13825.110663	27.990464
275.581231	13853.189282	27.995482
275.795792	13856.474850	28.000500
275.607332	13884.488170	28.005517
276.151608	13905.486325	28.010535
276.475560	13928.783369	28.015552
276.283104	13953.854077	28.020570
276.800292	13972.229014	28.025588
276.844812	13998.784861	28.030605
277.139234	14027.768080	28.035623
278.016661	14043.118033	28.040640
278.383419	14049.402104	28.045658
278.524194	14072.939613	28.050676
279.185352	14085.266425	28.055693
279.339728	14110.968318	28.060711
279.014680	14130.915450	28.065728
279.526993	14152.837900	28.070746
280.015162	14170.105914	28.075764
280.291767	14182.003519	28.080781
280.304404	14198.802853	28.085799
280.661446	14217.882114	28.090816
280.629781	14235.184248	28.095834
281.089810	14241.643261	28.100852
281.174345	14263.841288	28.105869
281.973888	14280.656383	28.110887
282.108424	14293.312162	28.115904
282.492536	14311.206128	28.120922
282.830626	14326.827131	28.125940
282.557407	14347.925413	28.130957
283.128402	14371.904361	28.135975
283.453533	14392.223639	28.140992
283.549157	14419.255265	28.146010
284.084659	14432.123086	28.151028
284.056385	14454.004240	28.156045
284.966639	14459.710633	28.161063
284.863683	14485.832324	28.166080
285.032458	14502.683263	28.171098
285.677974	14523.400954	28.176116
285.402343	14542.671237	28.181133
285.744699	14570.134998	28.186151
286.185982	14592.460698	28.191168
286.357153	14624.672864	28.196186
286.558759	14636.317213	28.201204
286.252124	14667.644204	28.206221
287.177209	14695.588497	28.211239
287.611341	14718.502894	28.216256
287.473339	14748.044471	28.221274
287.754812	14764.375828	28.226292
287.369939	14793.116058	28.231309
288.053701	14838.111777	28.236327
288.591598	14868.296163	28.241344
288.923173	14904.043016	28.246362
288.908473	14928.572360	28.251380
289.462844	14962.471582	28.256397
289.521455	14992.150123	28.261415
290.240630	15019.928177	28.266432
290.368022	15063.391389	28.271450
290.988855	15082.493358	28.276468
291.143455	15114.415224	28.281485
291.069653	15130.455136	28.286503
291.553351	15152.866438	28.291520
292.180778	15186.227178	28.296538
292.580873	15221.502778	28.301556
292.606662	15244.800762	28.306573
293.008249	15260.586290	28.311591
293.328413	15285.515272	28.316608
293.396327	15308.168754	28.321626
293.824444	15335.424363	28.326644
294.081320	15364.526033	28.331661
294.255632	15392.828989	28.336679
294.778951	15423.910344	28.341696
294.957080	15450.797853	28.346714
295.507828	15477.188018	28.351732
295.641117	15515.509543	28.356749
295.735984	15533.778434	28.361767
296.066431	15559.160964	28.366784
296.371308	15595.595496	28.371802
296.833858	15612.524568	28.376820
297.656992	15641.888534	28.381837
297.561615	15665.487103	28.386855
298.039251	15686.336583	28.391872
298.205694	15716.451001	28.396890
298.526760	15731.662072	28.401908
298.759482	15754.846140	28.406925
299.172919	15780.617079	28.411943
299.361825	15793.893854	28.416960
299.798109	15823.280797	28.421978
300.116981	15830.880540	28.426996
300.288005	15849.478909	28.432013
300.884951	15859.179661	28.437031
301.502493	15877.215399	28.442048
301.617478	15887.841277	28.447066
302.166720	15900.774265	28.452084
302.302145	15919.829932	28.457101
302.749289	15930.940734	28.462119
302.897277	15949.738631	28.467136
303.004812	15968.833458	28.472154
303.407731	15960.991175	28.477172
304.059912	15979.441654	28.482189
304.421429	16001.453018	28.487207
304.569972	16011.211456	28.492224
304.813896	16030.016513	28.497242
305.423659	16029.548337	28.502260
305.735622	16040.907786	28.507277
305.798164	16050.303861	28.512295
306.055815	16055.806603	28.517312
306.529637	16088.400208	28.522330
306.778447	16088.860305	28.527348
307.405217	16115.706893	28.532365
307.349375	16125.829043	28.537383
307.584444	16135.122331	28.542400
307.626271	16161.937433	28.547418
308.237528	16173.720687	28.552436
308.280546	16190.223270	28.557453
308.060050	16217.502776	28.562471
308.516714	16233.612118	28.567488
308.464729	16258.101622	28.572506
308.518589	16284.220145	28.577524
309.058859	16321.140328	28.582541
309.016092	16353.351007	28.587559
309.862667	16383.318868	28.592576
309.776154	16411.689450	28.597594
310.254540	16434.959038	28.602612
310.547035	16476.267592	28.607629
310.992876	16504.387517	28.612647
311.101625	16532.857189	28.617664
310.911739	16563.227737	28.622682
311.222033	16601.956416	28.627700
312.061807	16636.328730	28.632717
312.400528	16662.156775	28.637735
313.261516	16695.704652	28.642752
313.340557	16722.918998	28.647770
313.672848	16749.177730	28.652788
313.893020	16768.129363	28.657805
314.234071	16799.810037	28.662823
314.421700	16827.032788	28.667840
314.978438	16865.998187	28.672858
315.445249	16888.433114	28.677876
315.475317	16911.972496	28.682893
315.740249	16943.245238	28.687911
316.162946	16966.009341	28.692928
315.980743	16999.443203	28.697946
316.277895	17034.671926	28.702964
316.794227	17071.275118	28.707981
316.859664	17101.259067	28.712999
317.620516	17132.511286	28.718016
317.867604	17175.252984	28.723034
318.194299	17198.569366	28.728052
318.678156	17226.592789	28.733069
318.873672	17264.851188	28.738087
320.043584	17268.287764	28.743104
320.366143	17287.877707	28.748122
320.712833	17298.872374	28.753140
321.191934	17321.413273	28.758157
321.460765	17335.256624	28.763175
321.733548	17339.269640	28.768192
321.839253	17370.624871	28.773210
322.194518	17379.268201	28.778228
322.512632	17391.461370	28.783245
322.516569	17411.303503	28.788263
323.552907	17430.219538	28.793280
323.610106	17440.236225	28.798298
323.601240	17461.028016	28.803316
323.801675	17477.882921	28.808333
323.917154	17504.700983	28.813351
324.339386	17531.647916	28.818368
324.758584	17556.302156	28.823386
325.065829	17576.090629	28.828404
325.095563	17607.161226	28.833421
325.335208	17631.148775	28.838439
325.480773	17655.473277	28.843456
325.629727	17694.245210	28.848474
326.158587	17724.283879	28.853492
326.676219	17749.977957	28.858509
326.744028	17784.018386	28.863527
327.082650	17806.025920	28.868544
327.330029	17847.568739	28.873562
327.499422	17872.268829	28.878580
327.940673	17895.928203	28.883597
328.577847	17930.625164	28.888615
329.000688	17964.951440	28.893632
328.993612	17998.031079	28.898650
329.769322	18024.537959	28.903668
330.153982	18061.258411	28.908685
330.204385	18092.377087	28.913703
330.600375	18116.517636	28.918720
330.842054	18154.246201	28.923738
331.064158	18176.878894	28.928756
331.855157	18212.063986	28.933773
332.267294	18238.008986	28.938791
332.814807	18273.876726	28.943808
333.319922	18294.197203	28.948826
333.359804	18312.265694	28.953844
333.950080	18341.948230	28.958861
333.921567	18361.297324	28.963879
334.152105	18385.723148	28.968896
334.333505	18411.508677	28.973914
334.607794	18447.495348	28.978932
335.083316	18478.124765	28.983949
335.225009	18517.070053	28.988967
335.429219	18546.554351	28.993984
335.498284	18579.376660	28.999002
335.937196	18612.469610	29.004020
336.075574	18649.899430	29.009037
336.308133	18696.450025	29.014055
336.856065	18727.643406	29.019072
337.729197	18762.001638	29.024090
338.079226	18787.394819	29.029108
338.736257	18808.822920	29.034125
338.905852	18844.719321	29.039143
339.499906	18876.531178	29.044160
339.723835	18896.605712	29.049178
339.883154	18924.966728	29.054196
340.627572	18944.245867	29.059213
340.747360	18981.767686	29.064231
341.354748	19007.935841	29.069248
341.304593	19038.831701	29.074266
341.425309	19057.772720	29.079284
341.939638	19082.439267	29.084301
342.300349	19120.365863	29.089319
342.491196	19142.499144	29.094336
342.874593	19182.014415	29.099354
342.904494	19213.618251	29.104372
343.255539	19238.500110	29.109389
343.649529	19269.914329	29.114407
343.968077	19299.110183	29.119424
344.089495	19325.013720	29.124442
344.430011	19369.457767	29.129460
344.702155	19394.756534	29.134477
345.429875	19430.528677	29.139495
345.410024	19466.430624	29.144512
345.742651	19497.279883	29.149530
345.971442	19527.804283	29.154548
346.840400	19558.588580	29.159565
346.917126	19594.538814	29.164583
347.167744	19626.228785	29.169600
347.832794	19666.206358	29.174618
347.681425	19700.960495	29.179636
348.119919	19733.019248	29.184653
348.767126	19760.869103	29.189671
349.093526	19808.260586	29.194688
349.598424	19837.036330	29.199706
349.683641	19866.086355	29.204724
350.468981	19897.307598	29.209741
350.627045	19921.550833	29.214759
351.028128	19958.967280	29.219776
351.770020	19996.039777	29.224794
351.613153	20027.844772	29.229812
351.905722	20052.199781	29.234829
352.442278	20093.373536	29.239847
352.412356	20136.335710	29.244864
353.045360	20161.958033	29.249882
353.445592	20194.010897	29.254900
354.106637	20218.453712	29.259917
354.839531	20254.245506	29.264935
355.473270	20281.201021	29.269952
355.973925	20306.275623	29.274970
356.077693	20331.469290	29.279988
356.754489	20347.588639	29.285005
356.956647	20374.150652	29.290023
357.218663	20395.724510	29.295040
357.432003	20417.723024	29.300058
357.904940	20435.839369	29.305076
358.062808	20449.121032	29.310093
358.262547	20477.092545	29.315111
358.732013	20504.086736	29.320128
358.906822	20531.095527	29.325146
359.197113	20569.250782	29.330164
359.664739	20585.561051	29.335181
359.800366	20626.173209	29.340199
360.303985	20656.706862	29.345216
360.639710	20681.201214	29.350234
360.706701	20723.555561	29.355252
360.791881	20757.408890	29.360269
361.248507	20794.868776	29.365287
361.366898	20837.145813	29.370304
362.041631	20867.937320	29.375322
362.125520	20911.452016	29.380340
362.685160	20937.611277	29.385357
363.197703	20980.338676	29.390375
363.438504	21016.695465	29.395392
363.804623	21055.256804	29.400410
364.110049	21096.184531	29.405428
364.905545	21124.802910	29.410445
365.026272	21162.410888	29.415463
365.200748	21198.032813	29.420480
365.649527	21226.547687	29.425498
365.911437	21267.874337	29.430516
366.382084	21303.696484	29.435533
367.262772	21336.086657	29.440551
367.368911	21358.696961	29.445568
368.105421	21375.136369	29.450586
367.983972	21413.073415	29.455604
368.381109	21438.083533	29.460621
368.696419	21471.270176	29.465639
369.169791	21493.077511	29.470656
370.018469	21521.959840	29.475674
370.087481	21549.984945	29.480692
370.627826	21572.963468	29.485709
370.780993	21610.895789	29.490727
371.047906	21630.865287	29.495744
371.148107	21659.138409	29.500762
371.303547	21702.820564	29.505780
371.968796	21734.853379	29.510797
372.217029	21769.238948	29.515815
372.648941	21810.502191	29.520832
372.998435	21851.468810	29.525850
373.041121	21891.403064	29.530868
373.357495	21927.838153	29.535885
374.132929	21961.914000	29.540903
374.250533	22007.283550	29.545920
374.288154	22049.626381	29.550938
374.624302	22088.124922	29.555956
375.394771	22131.711683	29.560973
375.327441	22175.284439	29.565991
375.865947	22222.130352	29.571008
376.190185	22270.728677	29.576026
376.133533	22312.031579	29.581044
377.131283	22358.742690	29.586061
377.610924	22403.228657	29.591079
378.199640	22449.182591	29.596096
378.719970	22485.858473	29.601114
379.092866	22527.656925	29.606132
379.594034	22556.336122	29.611149
380.117149	22590.452573	29.616167
380.129615	22631.637889	29.621184
380.455741	22664.034959	29.626202
380.883895	22704.706663	29.631220
381.643166	22731.064514	29.636237
382.543774	22765.368578	29.641255
383.002180	22810.958299	29.646272
383.163381	22827.912413	29.651290
383.495326	22868.416269	29.656308
384.129745	22887.128842	29.661325
384.335275	22915.374615	29.666343
384.429282	22949.186071	29.671360
385.165063	22982.448401	29.676378
385.479139	23021.590438	29.681396
385.742732	23057.252295	29.686413
385.996834	23091.304319	29.691431
386.299220	23122.303002	29.696448
386.933054	23146.494624	29.701466
387.089632	23196.296838	29.706484
387.455644	23225.731197	29.711501
387.672129	23253.735604	29.716519
387.722130	23292.774197	29.721536
388.475186	23330.546322	29.726554
389.044940	23369.453097	29.731572
389.658223	23394.229610	29.736589
390.448567	23422.643587	29.741607
390.654756	23455.591549	29.746624
391.318239	23473.920967	29.751642
391.445517	23507.045675	29.756660
391.762650	23537.094801	29.761677
392.211379	23557.473789	29.766695
392.761335	23584.522767	29.771712
393.342635	23615.377420	29.776730
393.316791	23649.752297	29.781748
393.608338	23665.132151	29.786765
394.034477	23684.156151	29.791783
394.055544	23719.294758	29.796800
394.990265	23739.970650	29.801818
394.880233	23771.989166	29.806836
394.920994	23806.347559	29.811853
395.374703	23840.375914	29.816871
395.771467	23870.969175	29.821888
396.362985	23905.431052	29.826906
396.511033	23934.129629	29.831924
397.263758	23964.484013	29.836941
397.876872	23989.653098	29.841959
397.933920	24039.700502	29.846976
398.284794	24067.280555	29.851994
398.966451	24109.375211	29.857012
399.335288	24133.849681	29.862029
399.795067	24168.414799	29.867047
399.980269	24211.611191	29.872064
400.223314	24239.935114	29.877082
400.633096	24269.825481	29.882100
400.995372	24312.147536	29.887117
401.488750	24352.022439	29.892135
401.663817	24392.326454	29.897152
402.329707	24423.080630	29.902170
402.206560	24476.816381	29.907188
402.574152	24515.592745	29.912205
402.830648	24562.279782	29.917223
403.433909	24613.197321	29.922240
403.812228	24649.185305	29.927258
404.263532	24689.781589	29.932276
405.293549	24728.675792	29.937293
405.833940	24767.210707	29.942311
405.857674	24807.318069	29.947328
406.516240	24849.961391	29.952346
406.357000	24886.432143	29.957364
406.921031	24929.387468	29.962381
407.837340	24963.206235	29.967399
407.696587	25015.682234	29.972416
408.405011	25046.569739	29.977434
408.774907	25097.278587	29.982452
409.134287	25140.279057	29.987469
409.558310	25177.120320	29.992487
410.110600	25212.475361	29.997504
410.743685	25253.771089	30.002522
410.746239	25289.262933	30.007540
411.332956	25329.561224	30.012557
411.643533	25369.144466	30.017575
412.015870	25407.479415	30.022592
412.858537	25447.485057	30.027610
412.839032	25484.838747	30.032628
413.532835	25531.920888	30.037645
413.683737	25570.600508	30.042663
413.673612	25617.938468	30.047680
413.970639	25658.674630	30.052698
414.454082	25704.545092	30.057716
415.103994	25749.972463	30.062733
415.681182	25796.700609	30.067751
415.881061	25842.539960	30.072768
416.382623	25882.644135	30.077786
416.946451	25932.288220	30.082804
416.998265	25975.446086	30.087821
417.647961	26028.616189	30.092839
418.105438	26065.517035	30.097856
418.627372	26104.575645	30.102874
419.460243	26142.568090	30.107892
419.611170	26187.429953	30.112909
419.750306	26218.332583	30.117927
420.352482	26268.957429	30.122944
421.111499	26298.290492	30.127962
421.442512	26325.781948	30.132980
421.522298	26365.769861	30.137997
422.212184	26397.155314	30.143015
422.543561	26433.577288	30.148032
423.258177	26463.991981	30.153050
423.684843	26490.678652	30.158068
423.783379	26539.076181	30.163085
424.356761	26566.441518	30.168103
425.016240	26608.462710	30.173120
425.147891	26639.544122	30.178138
425.562079	26674.461976	30.183156
425.862375	26718.353575	30.188173
426.695297	26749.230508	30.193191
426.979012	26792.606601	30.198208
427.510239	26821.065978	30.203226
427.765004	26862.493776	30.208244
428.124864	26892.168317	30.213261
428.709893	26925.226943	30.218279
429.258654	26954.025059	30.223296
430.347970	26988.294154	30.228314
430.649281	27009.578265	30.233332
430.499427	27063.280825	30.238349
431.292879	27084.968279	30.243367
431.320363	27119.517681	30.248384
431.773291	27153.140926	30.253402
432.382064	27190.007480	30.258420
432.603755	27230.448899	30.263437
433.078386	27261.648193	30.268455
433.696168	27305.390204	30.273472
434.114529	27342.299500	30.278490
434.514973	27378.573300	30.283508
435.044556	27409.934867	30.288525
435.450722	27450.215097	30.293543
435.620960	27486.518827	30.298560
436.419821	27523.602712	30.303578
437.152204	27540.686227	30.308596
437.157823	27594.941004	30.313613
437.554135	27626.191047	30.318631
438.044154	27665.472560	30.323648
438.761475	27707.114052	30.328666
439.072659	27739.572195	30.333684
439.108257	27780.852892	30.338701
440.193574	27801.566266	30.343719
440.326443	27840.960945	30.348736
440.672503	27882.623022	30.353754
441.184414	27918.254579	30.358772
441.302729	27968.738224	30.363789
441.923766	27997.659232	30.368807
441.973715	28044.993432	30.373824
442.410603	28086.079155	30.378842
442.825648	28122.794441	30.383860
443.473629	28163.486975	30.388877
443.741947	28202.311229	30.393895
444.034260	28258.368519	30.398912
444.334235	28314.551177	30.403930
444.730327	28354.853733	30.408948
444.977171	28402.733111	30.413965
445.389112	28452.963372	30.418983
446.101450	28503.127741	30.424000
446.470395	28560.829915	30.429018
446.810786	28599.264381	30.434036
447.295728	28651.108157	30.439053
447.879613	28697.304643	30.444071
448.510117	28753.676927	30.449088
448.732865	28791.403274	30.454106
449.920710	28840.172915	30.459124
449.833079	28878.611737	30.464141
450.564330	28918.445721	30.469159
450.840898	28960.531739	30.474176
451.421898	28998.360377	30.479194
451.594463	29042.055742	30.484212
451.662378	29079.642524	30.489229
452.303335	29133.586944	30.494247
452.735163	29174.113069	30.499264
452.923232	29221.561089	30.504282
453.722893	29272.642859	30.509300
453.589054	29319.819151	30.514317
454.041092	29376.575080	30.519335
454.697296	29424.930016	30.524352
455.075920	29479.618077	30.529370
455.809715	29528.567933	30.534388
456.030293	29592.965063	30.539405
456.508263	29645.071606	30.544423
456.935307	29701.193902	30.549440
457.476191	29750.206107	30.554458
458.037345	29793.007798	30.559476
458.155532	29865.228543	30.564493
458.550270	29914.308277	30.569511
459.130071	29964.882572	30.574528
459.882174	30028.742675	30.579546
460.384087	30080.189151	30.584564
461.142936	30124.130008	30.589581
461.684363	30171.651293	30.594599
462.297422	30224.389239	30.599616
462.860225	30267.785865	30.604634
463.582947	30307.617553	30.609652
463.720420	30355.436423	30.614669
464.177337	30414.501756	30.619687
464.733189	30448.638962	30.624704
465.525029	30500.445644	30.629722
465.730307	30550.409960	30.634740
465.839824	30599.643460	30.639757
466.361295	30644.191538	30.644775
466.928679	30695.186783	30.649792
467.105092	30739.371892	30.654810
468.300073	30782.689545	30.659828
468.316343	30845.049108	30.664845
468.491661	30894.860906	30.669863
468.932522	30941.002641	30.674880
469.411264	30991.633204	30.679898
469.855498	31044.766335	30.684916
469.804203	31107.503921	30.689933
470.787394	31159.023091	30.694951
471.294947	31216.413859	30.699968
471.740579	31278.347135	30.704986
472.096014	31329.275989	30.710004
471.972204	31393.707368	30.715021
472.769225	31459.676302	30.720039
473.257233	31518.404852	30.725056
473.619960	31581.363497	30.730074
474.186042	31630.717579	30.735092
474.419884	31697.818574	30.740109
475.282325	31758.714435	30.745127
475.760933	31818.659096	30.750144
476.237680	31887.050242	30.755162
476.875178	31931.778885	30.760180
477.458556	31998.920929	30.765197
477.997080	32045.049815	30.770215
478.357162	32099.583317	30.775232
479.029577	32160.326778	30.780250
479.254350	32211.676535	30.785268
480.252262	32259.175351	30.790285
480.522771	32311.327403	30.795303
481.255392	32364.115272	30.800320
481.635341	32422.705242	30.805338
482.160882	32463.924865	30.810356
482.630660	32515.388722	30.815373
483.246196	32559.022110	30.820391
483.857806	32605.362058	30.825408
484.169454	32646.919004	30.830426
484.663415	32687.366395	30.835444
484.867790	32735.749238	30.840461
485.299772	32776.554227	30.845479
485.922169	32830.087582	30.850496
486.036861	32884.023025	30.855514
486.716332	32936.289600	30.860532
486.902470	32982.526324	30.865549
487.479115	33038.735348	30.870567
488.075129	33096.123748	30.875584
488.212963	33160.001159	30.880602
488.527953	33206.477407	30.885620
489.397948	33254.972149	30.890637
489.663953	33315.732038	30.895655
490.487367	33370.272145	30.900672
490.778012	33443.559387	30.905690
490.931296	33496.282789	30.910708
491.777803	33547.570047	30.915725
492.360719	33613.585631	30.920743
493.035723	33669.256177	30.925760
493.474963	33728.630806	30.930778
494.060696	33776.576968	30.935796
494.608616	33841.353226	30.940813
494.925277	33895.240660	30.945831
495.565256	33951.878456	30.950848
495.835534	34010.976864	30.955866
496.404894	34059.065328	30.960884
497.187737	34129.141889	30.965901
497.612072	34176.285985	30.970919
498.114983	34224.657104	30.975936
498.686488	34289.930529	30.980954
499.378584	34332.063475	30.985972
499.781824	34387.930227	30.990989
500.345284	34432.821219	30.996007
501.287209	34486.934684	31.001024
501.519008	34538.883351	31.006042
502.023980	34585.301268	31.011060
502.830585	34643.097163	31.016077
503.230418	34696.777610	31.021095
503.496205	34742.993072	31.026112
503.680817	34803.049198	31.031130
504.482771	34849.130332	31.036148
505.006472	34912.617501	31.041165
505.108945	34965.693956	31.046183
506.196849	35008.613512	31.051200
506.737004	35066.243642	31.056218
506.729437	35121.784657	31.061236
507.732877	35170.971065	31.066253
508.221894	35221.863138	31.071271
508.349492	35276.201009	31.076288
508.808847	35323.323205	31.081306
509.450962	35386.944996	31.086324
510.229891	35446.505189	31.091341
510.925982	35494.899537	31.096359
511.363534	35550.871469	31.101376
511.445691	35599.520286	31.106394
512.222272	35644.045344	31.111412
513.018293	35694.770328	31.116429
513.199507	35745.332483	31.121447
513.721062	35803.719966	31.126464
513.778879	35849.540441	31.131482
514.579869	35909.654906	31.136500
514.876962	35963.689768	31.141517
515.398469	36024.758857	31.146535
515.938137	36073.545760	31.151552
515.984075	36128.960880	31.156570
516.506307	36187.298723	31.161588
516.731577	36240.327505	31.166605
517.093855	36309.945992	31.171623
517.867851	36364.843008	31.176640
518.130364	36446.409469	31.181658
518.661046	36493.440880	31.186676
519.248488	36561.311317	31.191693
519.240835	36638.918197	31.196711
520.294568	36704.844363	31.201728
520.548581	36767.791231	31.206746
521.220884	36832.936530	31.211764
522.243874	36901.131875	31.216781
523.006225	36954.464033	31.221799
523.803733	37009.175643	31.226816
524.176186	37067.058765	31.231834
525.354305	37115.216882	31.236852
525.815405	37162.368159	31.241869
526.083617	37216.252621	31.246887
527.114801	37259.957065	31.251904
527.210594	37320.413593	31.256922
527.884093	37372.483361	31.261940
528.495851	37425.694838	31.266957
528.621088	37471.052927	31.271975
529.379781	37527.460324	31.276992
530.019875	37577.670373	31.282010
530.661181	37634.045847	31.287028
531.022957	37690.990108	31.292045
531.241262	37754.982533	31.297063
531.694913	37807.618973	31.302080
532.283852	37863.136910	31.307098
533.082627	37914.967044	31.312116
533.738521	37979.106604	31.317133
533.879036	38037.275287	31.322151
534.276505	38090.243726	31.327168
534.556870	38146.892080	31.332186
535.191930	38209.353473	31.337204
535.889718	38271.286673	31.342221
536.184115	38346.670701	31.347239
536.778948	38411.036117	31.352256
537.187347	38470.492011	31.357274
537.909947	38542.489644	31.362292
538.391456	38593.106329	31.367309
538.925030	38669.244504	31.372327
539.505702	38725.031556	31.377344
539.939455	38793.464315	31.382362
540.746490	38862.325770	31.387380
541.287634	38920.762927	31.392397
541.636583	38987.091052	31.397415
542.564181	39045.809514	31.402432
542.661864	39113.239810	31.407450
543.820878	39169.361136	31.412468
544.821260	39215.622962	31.417485
545.436312	39283.396467	31.422503
546.060617	39317.214732	31.427520
546.168165	39375.221422	31.432538
546.992979	39425.754663	31.437556
547.910239	39481.162092	31.442573
548.278338	39527.675391	31.447591
549.061732	39562.322881	31.452608
549.971400	39616.188751	31.457626
550.110801	39669.745350	31.462644
550.844267	39710.238116	31.467661
550.730727	39760.065334	31.472679
551.196654	39806.709365	31.477696
551.431314	39866.809747	31.482714
552.059229	39926.077143	31.487732
552.572392	39984.300195	31.492749
552.905288	40044.139033	31.497767
553.749154	40093.121392	31.502784
554.225090	40139.081542	31.507802
554.686978	40197.686330	31.512820
555.281849	40247.928630	31.517837
555.778325	40303.910006	31.522855
556.553435	40355.616876	31.527872
556.777109	40411.944825	31.532890
556.877206	40470.701874	31.537908
557.606643	40532.617597	31.542925
557.999443	40596.319117	31.547943
558.164721	40655.237214	31.552960
558.926834	40731.669360	31.557978
559.097292	40808.567585	31.562996
559.921061	40876.762396	31.568013
560.040793	40952.499031	31.573031
560.715571	41014.272888	31.578048
560.997692	41098.838994	31.583066
561.827069	41176.014783	31.588084
562.662703	41254.853244	31.593101
562.896293	41335.588807	31.598119
563.335146	41414.546906	31.603136
563.925138	41491.780271	31.608154
564.797497	41562.878971	31.613172
565.592999	41630.555600	31.618189
565.977727	41712.154339	31.623207
566.864629	41775.655402	31.628224
567.654083	41855.015556	31.633242
568.465553	41927.706174	31.638260
569.499538	41991.184824	31.643277
569.419799	42055.400998	31.648295
570.142227	42117.695458	31.653312
570.877177	42192.309050	31.658330
571.700243	42259.869448	31.663348
571.894732	42319.217522	31.668365
572.523800	42399.079125	31.673383
572.969368	42471.525245	31.678400
573.588946	42534.735138	31.683418
574.064222	42603.160658	31.688436
574.640000	42673.683214	31.693453
575.121292	42745.112627	31.698471
575.642458	42808.073062	31.703488
576.424250	42880.935919	31.708506
576.733766	42957.996965	31.713524
577.276675	43038.456282	31.718541
578.148429	43117.763807	31.723559
578.793400	43182.179680	31.728576
579.198190	43254.628422	31.733594
579.675774	43329.634043	31.738612
580.467242	43398.638695	31.743629
580.778184	43474.581741	31.748647
581.496000	43546.621869	31.753664
581.878650	43613.983389	31.758682
582.431652	43697.473336	31.763700
583.099161	43769.231099	31.768717
583.824505	43847.703912	31.773735
584.502944	43919.511050	31.778752
585.559140	43982.979284	31.783770
586.405852	44042.457531	31.788788
587.284658	44106.890064	31.793805
587.886106	44163.516315	31.798823
588.373015	44218.629880	31.803840
589.420022	44280.335591	31.808858
589.841953	44342.601133	31.813876
590.084385	44398.430262	31.818893
590.558539	44469.189498	31.823911
591.157246	44520.585850	31.828928
591.633502	44576.840571	31.833946
592.072579	44640.464258	31.838964
592.809648	44692.554129	31.843981
593.252848	44753.950875	31.848999
593.196143	44819.752829	31.854016
594.556132	44868.342350	31.859034
595.161577	44926.899238	31.864052
595.899664	44972.682896	31.869069
596.133008	45038.117455	31.874087
596.709373	45098.589712	31.879104
597.097523	45163.178045	31.884122
597.592692	45232.740836	31.889140
598.250592	45300.209823	31.894157
598.627406	45367.292880	31.899175
599.082075	45434.123562	31.904192
599.615618	45514.125158	31.909210
600.138986	45596.443901	31.914228
600.939501	45666.428327	31.919245
601.393615	45742.970261	31.924263
601.909332	45811.399285	31.929280
602.809971	45883.848473	31.934298
603.015007	45964.693862	31.939316
603.982183	46044.079068	31.944333
604.151808	46119.736915	31.949351
605.066526	46200.554241	31.954368
605.569977	46284.517062	31.959386
606.088513	46349.910767	31.964404
606.776949	46432.383840	31.969421
607.232582	46514.507781	31.974439
607.807634	46598.719925	31.979456
608.517321	46688.092438	31.984474
608.908948	46770.258961	31.989492
609.490315	46847.006124	31.994509
610.619969	46927.899936	31.999527
611.402192	47013.517235	32.004544
612.374234	47081.543347	32.009562
612.939757	47148.772951	32.014580
613.813435	47220.281701	32.019597
614.307217	47300.871545	32.024615
615.119071	47361.186459	32.029632
616.023024	47436.157997	32.034650
616.588129	47506.393760	32.039668
617.732525	47554.453473	32.044685
618.334465	47615.453559	32.049703
618.920464	47671.831669	32.054720
619.766287	47726.094145	32.059738
620.329917	47788.138235	32.064756
621.354851	47829.928716	32.069773
621.896106	47892.065165	32.074791
622.621603	47937.901097	32.079808
623.507769	47997.839125	32.084826
623.579169	48055.671638	32.089844
623.885575	48103.477832	32.094861
624.778937	48161.491886	32.099879
625.315808	48216.955357	32.104896
625.756587	48273.477905	32.109914
626.165186	48334.662035	32.114932
626.794229	48399.493918	32.119949
627.181180	48467.470296	32.124967
627.843090	48531.430652	32.129984
628.588964	48594.112695	32.135002
629.145189	48654.698832	32.140020
629.551517	48718.294827	32.145037
629.905705	48791.250117	32.150055
630.270430	48864.178682	32.155072
631.063215	48932.706580	32.160090
631.540568	49012.748285	32.165108
632.171416	49082.168766	32.170125
632.691297	49151.037419	32.175143
633.171516	49228.365203	32.180160
633.800345	49289.378201	32.185178
634.350892	49370.801609	32.190196
634.926537	49446.274048	32.195213
635.583181	49531.129591	32.200231
635.823382	49607.445963	32.205248
636.567817	49684.240396	32.210266
636.743268	49765.496171	32.215284
637.538955	49845.459284	32.220301
637.968634	49944.429590	32.225319
638.371098	50024.385309	32.230336
639.347134	50111.768100	32.235354
639.706408	50202.512623	32.240372
640.733472	50293.950144	32.245389
641.427618	50385.028896	32.250407
641.946244	50477.508504	32.255424
642.635169	50561.856604	32.260442
643.616608	50648.791346	32.265460
644.306923	50732.089522	32.270477
645.084991	50819.006135	32.275495
645.850646	50898.541011	32.280512
646.376009	50984.877742	32.285530
646.996447	51073.933336	32.290548
647.723338	51158.416864	32.295565
648.429017	51244.954110	32.300583
649.227865	51334.590197	32.305600
649.732882	51398.924763	32.310618
650.861306	51484.491866	32.315636
651.633602	51559.813853	32.320653
652.537448	51627.630003	32.325671
653.211587	51720.153481	32.330688
654.383532	51778.000138	32.335706
654.854024	51853.851238	32.340724
655.379466	51916.886878	32.345741
655.927064	51972.984134	32.350759
656.990574	52060.873109	32.355776
657.778838	52128.367125	32.360794
658.132525	52210.603317	32.365812
658.649860	52266.674379	32.370829
659.391381	52328.437060	32.375847
660.462193	52410.352833	32.380864
660.634596	52468.547573	32.385882
661.106758	52553.980923	32.390900
661.869295	52627.428531	32.395917
662.672778	52700.180224	32.400935
663.181459	52774.016079	32.405952
663.759824	52851.536728	32.410970
664.113801	52932.788262	32.415988
664.805875	53004.564868	32.421005
665.387619	53082.212308	32.426023
666.013016	53170.933415	32.431040
667.194865	53247.367372	32.436058
667.267649	53329.113599	32.441076
667.989149	53418.529326	32.446093
668.670572	53502.186819	32.451111
669.142101	53581.194712	32.456128
669.935816	53665.385741	32.461146
670.365348	53764.384935	32.466164
670.690568	53841.745991	32.471181
671.641152	53935.703045	32.476199
672.217354	54031.782093	32.481216
672.673275	54117.540072	32.486234
673.291465	54212.993116	32.491252
674.126274	54299.666968	32.496269
674.646527	54391.668185	32.501287
675.264598	54497.684301	32.506304
676.184666	54579.688190	32.511322
676.286106	54673.300202	32.516340
676.819692	54765.712126	32.521357
677.751124	54856.796423	32.526375
678.242069	54956.740244	32.531392
679.302421	55037.888395	32.536410
679.492258	55137.297912	32.541428
680.374159	55237.251300	32.546445
680.994136	55324.032152	32.551463
681.270420	55424.549479	32.556480
682.230036	55514.733228	32.561498
682.469934	55623.585507	32.566516
683.412544	55731.467538	32.571533
684.223485	55829.884008	32.576551
684.600157	55930.704178	32.581568
685.848693	56026.527781	32.586586
686.706749	56117.951158	32.591604
687.585835	56216.301588	32.596621
688.835480	56309.518702	32.601639
689.505942	56397.213222	32.606656
690.356919	56487.360698	32.611674
690.707895	56573.865444	32.616692
691.490872	56671.992301	32.621709
692.278381	56760.201445	32.626727
692.962910	56860.603910	32.631744
693.940906	56940.790441	32.636762
694.652428	57028.037809	32.641780
694.992095	57106.242623	32.646797
696.093591	57197.245921	32.651815
697.094193	57278.657870	32.656832
698.211396	57363.621430	32.661850
698.800281	57439.237682	32.666868
699.352407	57514.043472	32.671885
700.177540	57594.958654	32.676903
700.739906	57674.643098	32.681920
701.657068	57749.829166	32.686938
702.602138	57833.656772	32.691956
702.905062	57911.047153	32.696973
703.818455	57997.658813	32.701991
704.154096	58070.633105	32.707008
704.898599	58145.277809	32.712026
705.839534	58229.246678	32.717044
706.121542	58322.268683	32.722061
706.861112	58389.610880	32.727079
707.746312	58489.678559	32.732096
708.351564	58570.865625	32.737114
708.904768	58655.605581	32.742132
708.756284	58740.367107	32.747149
709.869970	58835.944514	32.752167
710.155819	58935.050868	32.757184
711.327266	59031.999826	32.762202
711.715037	59135.236859	32.767220
712.283935	59236.736983	32.772237
713.373428	59330.041479	32.777255
714.262492	59432.758197	32.782272
714.860029	59526.843074	32.787290
715.116001	59622.981973	32.792308
716.111268	59723.866672	32.797325
717.021417	59802.060462	32.802343
718.040263	59918.544996	32.807360
718.916215	59997.257473	32.812378
719.559379	60091.217110	32.817396
719.974382	60185.579966	32.822413
721.188621	60267.974921	32.827431
721.700843	60356.550412	32.832448
722.425856	60450.125145	32.837466
723.455127	60540.234445	32.842484
723.802939	60625.899583	32.847501
724.793816	60717.610685	32.852519
725.268692	60802.262739	32.857536
725.414738	60881.079694	32.862554
726.480817	60978.825126	32.867572
726.772739	61070.571040	32.872589
727.523263	61160.865525	32.877607
728.023544	61250.585512	32.882624
728.480758	61352.529663	32.887642
729.365978	61454.919948	32.892660
729.603781	61559.513655	32.897677
730.578108	61654.737740	32.902695
731.280957	61768.216708	32.907712
732.167498	61865.417716	32.912730
732.748807	61977.467051	32.917748
733.321209	62086.277179	32.922765
734.313766	62187.197717	32.927783
735.164596	62298.263077	32.932800
736.120682	62397.797508	32.937818
738.010555	62471.256828	32.942836
738.896864	62565.118169	32.947853
739.765361	62641.320747	32.952871
740.441540	62740.311652	32.957888
741.255455	62816.966448	32.962906
741.884100	62900.158241	32.967924
742.403586	62997.965582	32.972941
743.209548	63077.648413	32.977959
743.805801	63164.612833	32.982976
744.215257	63250.847137	32.987994
745.199169	63357.142109	32.993012
745.357382	63458.508656	32.998029
746.086622	63560.153370	33.003047
746.979133	63663.608828	33.008064
747.742296	63761.456963	33.013082
748.555967	63869.179856	33.018100
749.149626	63963.516440	33.023117
749.927617	64064.820035	33.028135
750.505612	64177.601474	33.033152
751.262664	64275.667818	33.038170
752.330556	64375.680092	33.043188
752.655827	64479.898813	33.048205
753.960051	64589.915730	33.053223
754.888360	64694.059896	33.058240
755.251494	64795.627656	33.063258
756.294505	64894.303719	33.068276
756.698924	64999.696089	33.073293
757.410665	65104.198743	33.078311
758.227930	65215.136672	33.083328
758.957416	65335.306926	33.088346
759.207519	65427.854102	33.093364
759.739209	65550.785070	33.098381
760.884156	65658.394084	33.103399
761.254099	65779.895316	33.108416
761.934260	65896.878688	33.113434
762.857467	66006.151031	33.118452
763.493671	66131.974498	33.123469
764.253740	66252.055662	33.128487
765.043916	66363.509357	33.133504
765.685162	66492.157602	33.138522
766.825074	66605.615291	33.143540
767.393066	66734.219244	33.148557
768.170495	66852.711320	33.153575
768.948894	66971.849607	33.158592
769.658146	67094.323338	33.163610
770.530074	67199.208395	33.168628
770.862975	67340.679974	33.173645
772.494917	67454.456938	33.178663
772.874661	67570.595924	33.183680
773.669238	67688.797922	33.188698
774.608169	67792.535207	33.193716
775.478794	67909.960175	33.198733
776.518735	68014.581646	33.203751
777.138174	68122.884847	33.208768
777.703524	68226.752032	33.213786
778.730011	68339.393018	33.218804
779.384976	68437.269750	33.223821
779.953850	68552.155157	33.228839
780.862054	68658.952717	33.233856
781.576193	68779.059223	33.238874
782.144438	68887.050713	33.243892
783.187271	68990.263650	33.248909
784.134229	69099.969686	33.253927
784.886042	69213.100731	33.258944
785.745188	69329.083899	33.263962
786.703375	69433.983530	33.268980
787.720793	69552.399773	33.273997
788.318002	69653.228255	33.279015
789.227703	69756.686712	33.284032
790.168497	69865.029188	33.289050
791.272102	69971.453276	33.294068
791.578447	70084.448901	33.299085
792.344677	70181.706884	33.304103
793.126810	70294.882205	33.309120
793.865600	70408.343427	33.314138
795.003581	70523.439709	33.319156
795.801108	70628.204659	33.324173
796.667632	70735.124915	33.329191
798.041922	70829.022552	33.334208
798.593258	70936.119633	33.339226
799.553059	71033.198487	33.344244
800.075883	71142.732557	33.349261
800.785281	71256.999952	33.354279
801.646792	71367.115176	33.359296
802.292126	71477.973965	33.364314
803.457208	71575.516620	33.369332
804.107410	71686.540172	33.374349
804.736498	71789.069030	33.379367
805.499116	71898.821999	33.384384
805.918274	72019.686173	33.389402
806.630785	72135.945367	33.394420
807.549713	72255.098502	33.399437
808.346291	72370.041003	33.404455
809.181545	72490.183552	33.409472
810.275024	72604.193977	33.414490
811.260507	72720.970285	33.419508
811.971007	72837.853496	33.424525
812.813217	72946.268422	33.429543
813.565360	73054.685227	33.434560
813.792036	73174.052211	33.439578
814.668320	73291.291433	33.444596
815.248028	73409.679566	33.449613
816.243485	73547.407750	33.454631
817.354988	73668.880311	33.459648
817.825467	73787.768541	33.464666
818.956210	73906.465243	33.469684
819.730651	74041.709971	33.474701
820.363553	74150.909882	33.479719
821.389418	74276.033892	33.484736
821.985685	74405.633738	33.489754
823.050554	74515.109488	33.494772
823.664010	74640.008438	33.499789
824.458806	74759.521522	33.504807
825.235351	74885.447415	33.509824
826.528007	75016.207837	33.514842
827.765418	75116.019500	33.519860
828.477816	75230.531462	33.524877
828.980411	75360.492576	33.529895
829.962216	75470.213218	33.534912
830.268388	75592.301922	33.539930
831.200680	75709.910271	33.544948
831.899450	75819.030618	33.549965
832.877119	75939.204314	33.554983
833.583811	76056.570811	33.560000
834.085427	76170.461045	33.565018
835.136121	76283.062365	33.570036
835.819780	76420.284010	33.575053
836.581622	76534.439040	33.580071
838.233619	76643.248751	33.585088
838.932682	76757.427213	33.590106
840.001090	76870.344879	33.595124
840.456778	76987.982711	33.600141
841.444973	77104.828264	33.605159
842.133493	77219.048308	33.610176
842.815672	77348.965454	33.615194
844.056119	77455.397923	33.620212
844.806120	77589.866084	33.625229
845.284261	77702.182863	33.630247
846.575444	77821.986380	33.635264
847.092748	77949.297197	33.640282
848.002111	78072.949406	33.645300
848.654894	78199.784106	33.650317
849.436465	78325.763105	33.655335
850.286678	78455.937872	33.660352
850.648448	78592.473340	33.665370
851.916808	78716.718316	33.670388
855.279715	78795.535434	33.675405
857.257766	78884.704580	33.680423
858.608040	78970.349058	33.685440
859.310087	79061.948277	33.690458
859.891364	79139.656351	33.695476
860.572529	79219.705408	33.700493
861.357776	79311.773840	33.705511
861.917438	79400.900702	33.710528
862.003939	79497.589301	33.715546
862.963061	79596.700738	33.720564
863.518185	79696.205184	33.725581
864.043557	79813.932828	33.730599
864.791904	79911.025990	33.735616
865.211837	80034.940958	33.740634
865.977196	80145.753039	33.745652
866.410523	80266.968384	33.750669
867.018151	80398.672545	33.755687
867.994735	80521.400268	33.760704
868.624674	80654.939209	33.765722
869.075852	80795.082277	33.770740
869.959290	80931.243446	33.775757
870.112834	81068.887889	33.780775
870.990201	81210.321948	33.785792
871.722579	81361.775902	33.790810
872.926350	81509.697979	33.795828
873.471498	81669.215606	33.800845
874.092214	81810.490140	33.805863
875.674829	81960.255759	33.810880
875.931549	82122.937946	33.815898
876.966880	82277.935024	33.820916
878.299768	82417.137184	33.825933
878.988906	82565.677513	33.830951
880.724652	82690.107654	33.835968
881.759727	82827.179146	33.840986
882.665333	82968.592221	33.846004
884.021898	83100.951934	33.851021
885.090351	83238.400295	33.856039
885.878612	83357.343272	33.861056
886.693584	83490.397788	33.866074
887.634653	83618.567583	33.871092
888.801069	83748.514602	33.876109
889.610019	83872.993656	33.881127
890.754482	83984.508981	33.886144
891.657634	84093.072161	33.891162
892.153902	84199.507366	33.896180
892.981848	84317.852572	33.901197
893.603682	84447.571247	33.906215
894.590339	84565.068991	33.911232
895.191724	84690.965249	33.916250
896.262053	84823.504443	33.921268
897.217794	84945.658963	33.926285
897.748726	85077.422125	33.931303
898.702351	85204.684670	33.936320
899.313626	85351.262175	33.941338
900.015572	85487.688909	33.946356
901.180863	85624.778692	33.951373
901.708849	85768.913037	33.956391
902.465485	85897.058468	33.961408
903.396584	86059.961462	33.966426
903.956355	86206.779435	33.971444
905.040511	86347.902336	33.976461
905.871364	86516.044441	33.981479
906.881487	86662.452041	33.986496
907.290224	86820.156775	33.991514
908.200124	86966.150729	33.996532
909.058962	87114.915976	34.001549
910.022528	87284.790491	34.006567
911.012346	87446.906313	34.011584
911.879182	87609.384442	34.016602
912.971882	87770.510147	34.021620
913.565826	87929.484432	34.026637
914.235038	88101.817554	34.031655
915.594895	88268.505507	34.036672
916.396796	88427.120407	34.041690
917.488858	88602.913302	34.046708
918.724562	88748.674959	34.051725
920.032138	88908.581942	34.056743
921.443642	89052.505307	34.061760
922.380075	89213.980150	34.066778
923.387509	89374.988511	34.071796
924.384936	89525.480403	34.076813
924.992152	89676.059497	34.081831
925.892578	89821.828202	34.086848
926.701328	89975.444232	34.091866
927.546066	90131.083193	34.096884
928.619621	90288.106587	34.101901
929.153361	90458.332671	34.106919
930.451123	90607.046653	34.111936
931.398300	90774.662348	34.116954
931.786572	90940.731543	34.121972
932.590972	91097.509792	34.126989
933.596312	91262.825085	34.132007
934.658098	91424.532977	34.137024
935.631045	91593.568678	34.142042
936.383908	91774.300150	34.147060
937.196140	91933.958564	34.152077
937.896715	92100.542874	34.157095
938.896979	92271.339809	34.162112
939.936616	92442.562471	34.167130
940.688220	92620.688186	34.172148
942.095110	92793.959306	34.177165
942.781698	92972.211317	34.182183
944.431459	93120.971200	34.187200
945.519808	93294.218972	34.192218
946.124407	93455.781047	34.197236
947.271384	93618.919481	34.202253
947.874152	93782.004561	34.207271
949.113057	93954.915593	34.212288
950.398502	94106.614553	34.217306
951.732951	94248.521220	34.222324
952.882582	94374.156921	34.227341
953.794304	94519.566049	34.232359
954.925178	94669.403323	34.237376
955.776675	94808.789691	34.242394
956.579530	94954.255924	34.247412
957.657211	95095.636261	34.252429
958.222353	95247.567653	34.257447
959.139703	95390.381437	34.262464
960.021039	95540.692946	34.267482
960.561591	95692.769783	34.272500
961.694613	95842.270100	34.277517
961.870584	96014.877304	34.282535
963.304949	96173.978496	34.287552
964.311505	96338.078513	34.292570
964.738410	96499.760244	34.297588
965.616006	96667.507573	34.302605
966.296400	96847.151767	34.307623
968.012092	97011.207632	34.312640
968.618254	97174.969038	34.317658
970.067456	97353.988671	34.322676
970.926534	97522.681495	34.327693
971.757316	97683.000329	34.332711
972.810556	97854.516774	34.337728
974.070386	98023.365009	34.342746
974.824579	98190.163582	34.347764
976.437052	98351.694462	34.352781
977.456849	98521.305498	34.357799
978.743329	98673.064325	34.362816
980.249358	98834.981945	34.367834
980.819392	98998.796390	34.372852
982.074707	99159.575916	34.377869
982.755985	99314.779339	34.382887
983.872335	99476.824587	34.387904
985.430082	99618.441488	34.392922
986.583003	99772.356226	34.397940
987.926341	99921.551167	34.402957
988.462168	100076.806374	34.407975
989.238361	100220.386539	34.412992
990.270308	100368.427905	34.418010
990.797787	100539.533857	34.423028
992.141766	100693.106097	34.428045
992.859590	100859.214184	34.433063
993.628607	101015.895322	34.438080
994.642089	101181.553059	34.443098
995.283153	101346.281046	34.448116
996.385764	101519.178440	34.453133
997.249734	101688.678292	34.458151
997.941825	101862.402465	34.463168
998.642692	102034.072274	34.468186
999.609533	102218.620715	34.473204
1000.638829	102396.618270	34.478221
1001.384701	102567.814698	34.483239
1002.274939	102762.723929	34.488256
1003.394089	102945.667737	34.493274
1004.236344	103136.719650	34.498292
1005.963582	103303.797743	34.503309
1007.104775	103486.601606	34.508327
1008.044996	103653.475020	34.513344
1009.403676	103829.121086	34.518362
1010.855625	104012.779390	34.523380
1011.866429	104177.108528	34.528397
1012.536512	104354.082365	34.533415
1013.488592	104526.993620	34.538432
1014.658643	104694.787183	34.543450
1015.518736	104870.504078	34.548468
1015.985072	105032.792482	34.553485
1017.187797	105204.133737	34.558503
1017.997321	105378.149438	34.563520
1019.082168	105554.582797	34.568538
1019.645093	105725.570386	34.573556
1020.906397	105899.885740	34.578573
1021.930309	106069.534894	34.583591
1022.681687	106245.402726	34.588608
1023.741417	106431.240448	34.593626
1024.523378	106611.809686	34.598644
1025.865964	106775.135775	34.603661
1026.355411	106967.443836	34.608679
1027.543972	107155.205393	34.613696
1028.458867	107337.659685	34.618714
1029.249375	107540.778248	34.623732
1030.422368	107721.406209	34.628749
1031.240995	107918.664173	34.633767
1032.406307	108118.126144	34.638784
1033.552555	108307.954860	34.643802
1034.251718	108510.877834	34.648820
1035.640256	108705.121758	34.653837
1036.467999	108898.833197	34.658855
1037.188779	109108.908339	34.663872
1038.735002	109299.897211	34.668890
1039.498623	109511.261532	34.673908
1040.852873	109699.695670	34.678925
1042.299900	109898.451587	34.683943
1043.288566	110091.928830	34.688960
1044.553670	110289.117573	34.693978
1045.685249	110492.085747	34.698996
1046.521522	110683.472264	34.704013
1047.624331	110882.021286	34.709031
1048.291033	111076.378622	34.714048
1049.792995	111280.320533	34.719066
1050.609489	111487.198995	34.724084
1051.402000	111692.979077	34.729101
1052.134115	111893.861839	34.734119
1053.219247	112117.505609	34.739136
1054.599739	112312.645652	34.744154
1055.436829	112528.315658	34.749172
1056.942791	112742.893008	34.754189
1057.738306	112947.031081	34.759207
1058.785889	113162.329486	34.764224
1060.004967	113368.711834	34.769242
1061.166422	113595.219056	34.774260
1062.148562	113807.132574	34.779277
1063.316652	114019.538204	34.784295
1064.098095	114222.607594	34.789312
1065.258681	114442.728040	34.794330
1065.974085	114665.963429	34.799348
1067.053431	114871.653201	34.804365
1068.116309	115091.780144	34.809383
1069.153209	115319.966326	34.814400
1070.276120	115527.251018	34.819418
1071.519904	115754.557705	34.824436
1072.454767	115970.308771	34.829453
1073.774675	116194.790500	34.834471
1074.974495	116408.042009	34.839488
1076.214633	116619.461972	34.844506
1077.356772	116834.018677	34.849524
1078.731395	117038.266305	34.854541
1079.759262	117257.092400	34.859559
1081.003291	117456.923381	34.864576
1083.426110	117638.749798	34.869594
1085.008463	117832.339990	34.874612
1086.056328	118015.550420	34.879629
1087.237867	118194.922856	34.884647
1088.209452	118381.318048	34.889664
1089.491221	118564.342291	34.894682
1090.412597	118735.360972	34.899700
1091.654718	118916.338239	34.904717
1092.740685	119074.660897	34.909735
1093.066001	119248.185244	34.914752
1094.173047	119425.938815	34.919770
1095.074404	119597.433807	34.924788
1096.206850	119781.248322	34.929805
1096.918744	119960.106372	34.934823
1097.898706	120162.149268	34.939840
1098.676834	120338.588572	34.944858
1099.455359	120535.768570	34.949876
1100.342760	120728.771825	34.954893
1101.748630	120920.400984	34.959911
1102.378327	121131.078891	34.964928
1103.662146	121334.323450	34.969946
1104.524174	121541.948105	34.974964
1105.251375	121758.728445	34.979981
1106.280000	121973.344317	34.984999
1107.032859	122193.941356	34.990016
1108.629369	122412.174883	34.995034
1109.649505	122639.075360	35.000052
1110.914660	122850.906174	35.005069
1112.294211	123060.030818	35.010087
1113.284065	123285.531601	35.015104
1114.767087	123491.864104	35.020122
1115.642760	123703.747739	35.025140
1116.699583	123931.423672	35.030157
1118.074050	124146.073235	35.035175
1119.038301	124375.047472	35.040192
1120.279472	124579.863022	35.045210
1121.827926	124803.584910	35.050228
1122.468958	125023.618796	35.055245
1124.111785	125224.860587	35.060263
1124.952234	125456.905073	35.065280
1126.869677	125671.807563	35.070298
1128.595525	125872.024621	35.075316
1129.718884	126078.756477	35.080333
1130.671407	126286.962415	35.085351
1131.711301	126495.282597	35.090368
1133.053831	126692.645683	35.095386
1134.042919	126905.276761	35.100404
1134.648897	127119.288363	35.105421
1136.477618	127321.919592	35.110439
1136.958662	127546.369088	35.115456
1138.095348	127760.148657	35.120474
1138.753337	127978.267204	35.125492
1139.974994	128203.441647	35.130509
1141.345763	128418.532795	35.135527
1141.855057	128648.528196	35.140544
1143.212705	128860.604024	35.145562
1144.127514	129094.002081	35.150580
1144.902843	129329.009226	35.155597
1146.353583	129553.495246	35.160615
1147.103863	129788.661107	35.165632
1149.036621	130021.651137	35.170650
1150.008431	130259.982273	35.175668
1150.945849	130492.166397	35.180685
1152.155600	130720.654954	35.185703
1152.887480	130960.372478	35.190720
1153.963649	131191.599720	35.195738
1155.293401	131426.924902	35.200756
1156.347698	131674.792583	35.205773
1157.578053	131910.389712	35.210791
1158.675233	132160.816519	35.215808
1159.977373	132405.350521	35.220826
1161.125891	132655.645233	35.225844
1162.264013	132883.674185	35.230861
1163.675186	133120.391495	35.235879
1164.635388	133370.910080	35.240896
1165.783929	133589.779645	35.245914
1166.919085	133823.803103	35.250932
1168.047733	134052.765852	35.255949
1169.151924	134273.802869	35.260967
1170.143485	134518.955478	35.265984
1171.213019	134745.583514	35.271002
1172.750488	134978.826735	35.276020
1173.309170	135216.653005	35.281037
1174.937393	135451.496018	35.286055
1175.894066	135689.820804	35.291072
1177.431239	135929.769062	35.296090
1178.589645	136167.417595	35.301108
1179.942718	136409.034165	35.306125
1181.838412	136620.809399	35.311143
1183.156274	136860.098927	35.316160
1184.606748	137086.184069	35.321178
1185.882631	137301.777623	35.326196
1187.339766	137521.480771	35.331213
1188.272235	137748.475094	35.336231
1189.341986	137977.047997	35.341248
1190.679694	138198.727328	35.346266
1191.561027	138432.826840	35.351284
1192.377645	138658.079759	35.356301
1194.019961	138885.336491	35.361319
1195.367143	139123.897002	35.366336
1196.150507	139360.554561	35.371354
1197.080142	139597.621883	35.376372
1198.440482	139818.962637	35.381389
1199.667920	140044.627391	35.386407
1201.258106	140294.856614	35.391424
1202.709324	140529.664088	35.396442
1203.723282	140758.424124	35.401460
1204.643507	140998.456841	35.406477
1206.153950	141233.778803	35.411495
1206.940035	141476.728453	35.416512
1208.239746	141714.788947	35.421530
1209.720185	141958.914114	35.426548
1210.523687	142191.191247	35.431565
1211.780211	142435.112704	35.436583
1212.655710	142691.875305	35.441600
1213.856874	142929.792131	35.446618
1215.420796	143173.783341	35.451636
1216.372939	143422.491276	35.456653
1217.783770	143669.821402	35.461671
1219.174226	143927.766256	35.466688
1220.228945	144169.989055	35.471706
1221.914961	144412.050736	35.476724
1223.189119	144660.511335	35.481741
1224.763518	144896.640290	35.486759
1225.914656	145135.248097	35.491776
1227.180541	145366.706085	35.496794
1228.573526	145607.677056	35.501812
1229.474599	145848.370785	35.506829
1230.995868	146082.292403	35.511847
1233.647242	146286.718836	35.516864
1235.885478	146492.771920	35.521882
1237.367955	146703.983038	35.526900
1238.414672	146915.466312	35.531917
1240.092524	147116.887989	35.536935
1240.940464	147325.218212	35.541952
1241.748096	147525.406891	35.546970
1243.078512	147727.570713	35.551988
1243.662247	147936.046263	35.557005
1244.729742	148147.848579	35.562023
1245.755347	148367.604027	35.567040
1246.483726	148584.144838	35.572058
1247.410664	148813.805353	35.577076
1248.461590	149041.987752	35.582093
1249.365159	149271.869676	35.587111
1250.290430	149505.760215	35.592128
1251.419573	149725.784291	35.597146
1252.681316	149942.196323	35.602164
1253.350876	150184.646988	35.607181
1254.656012	150412.985795	35.612199
1255.597898	150661.539532	35.617216
1257.076154	150892.303070	35.622234
1259.165826	151123.708091	35.627252
1260.273465	151365.308419	35.632269
1262.077657	151579.496810	35.637287
1263.120653	151820.703053	35.642304
1264.216487	152048.903707	35.647322
1265.991687	152282.800000	35.652340
1266.599905	152526.946153	35.657357
1268.050091	152770.936179	35.662375
1269.018724	153010.965974	35.667392
1270.080700	153250.499807	35.672410
1271.330914	153504.895297	35.677428
1272.143202	153755.971154	35.682445
1273.509054	154018.741638	35.687463
1274.840181	154275.565177	35.692480
1275.190842	154543.574667	35.697498
1276.958034	154816.124035	35.702516
1277.832417	155090.464716	35.707533
1278.698790	155367.042169	35.712551
1280.114686	155646.200758	35.717568
1281.245748	155931.308242	35.722586
1282.478249	156216.553564	35.727604
1283.704676	156506.206275	35.732621
1284.993955	156787.408545	35.737639
1286.373901	157085.558230	35.742656
1287.810991	157381.504240	35.747674
1289.368974	157663.265225	35.752692
1290.411223	157955.010360	35.757709
1292.596992	158232.930702	35.762727
1293.965708	158519.612896	35.767744
1295.232933	158804.128750	35.772762
1296.440034	159080.035267	35.777780
1297.728175	159358.532868	35.782797
1299.536491	159641.964961	35.787815
1300.803438	159926.689155	35.792832
1301.993279	160215.641613	35.797850
1303.635288	160485.214725	35.802868
1304.689773	160767.322628	35.807885
1305.777459	161048.994941	35.812903
1307.257217	161344.420045	35.817920
1308.622307	161625.657918	35.822938
1309.753848	161909.333090	35.827956
1311.561374	162204.939378	35.832973
1312.712017	162477.606743	35.837991
1314.095335	162762.566621	35.843008
1315.281676	163042.327812	35.848026
1317.107281	163320.428511	35.853044
1319.281562	163580.167980	35.858061
1321.856007	163819.036790	35.863079
1323.697398	164062.249052	35.868096
1324.796031	164311.063258	35.873114
1326.386915	164558.722147	35.878132
1327.578529	164801.810276	35.883149
1328.962705	165043.040854	35.888167
1330.170987	165272.657176	35.893184
1331.114398	165531.086000	35.898202
1332.779921	165756.759947	35.903220
1333.848480	166005.483512	35.908237
1335.128852	166248.347063	35.913255
1336.153611	166498.907577	35.918272
1337.206393	166751.204060	35.923290
1338.990040	166986.055961	35.928308
1339.992685	167219.240651	35.933325
1341.101049	167457.424823	35.938343
1342.156727	167689.333083	35.943360
1343.421136	167920.269855	35.948378
1344.697863	168159.356908	35.953396
1346.128193	168407.283240	35.958413
1347.493391	168640.631695	35.963431
1348.663402	168882.810553	35.968448
1350.270834	169121.950619	35.973466
1351.311247	169371.134825	35.978484
1352.237040	169630.114695	35.983501
1353.626880	169885.416813	35.988519
1355.036710	170132.234875	35.993536
1356.053635	170396.548745	35.998554
1357.617824	170652.461087	36.003572
1359.197370	170912.181138	36.008589
1360.238253	171184.252190	36.013607
1361.406129	171442.083092	36.018624
1362.490393	171725.297744	36.023642
1365.405929	171954.998316	36.028660
1367.077512	172196.360290	36.033677
1368.349155	172454.584695	36.038695
1369.741977	172711.940245	36.043712
1370.531094	172972.819551	36.048730
1371.998300	173234.520530	36.053748
1373.082497	173503.774085	36.058765
1374.575044	173767.441043	36.063783
1375.373210	174035.712648	36.068800
1376.791938	174321.576353	36.073818
1378.000348	174595.588615	36.078836
1379.349107	174871.370273	36.083853
1380.193303	175164.056890	36.088871
1381.682498	175449.215156	36.093888
1382.346148	175741.221000	36.098906
1383.539838	176026.643393	36.103924
1384.911851	176345.702117	36.108941
1385.775397	176653.654380	36.113959
1387.226526	176965.020563	36.118976
1388.391701	177285.118405	36.123994
1390.098893	177592.408699	36.129012
1391.327662	177914.733886	36.134029
1392.707889	178226.547519	36.139047
1394.690135	178550.052393	36.144064
1395.740726	178867.837493	36.149082
1397.636197	179174.773752	36.154100
1399.369564	179492.428831	36.159117
1400.887493	179800.239069	36.164135
1402.353493	180120.071629	36.169152
1403.832693	180426.899557	36.174170
1405.565967	180721.573938	36.179188
1407.010957	181024.421753	36.184205
1408.337989	181334.197307	36.189223
1410.327584	181638.612764	36.194240
1411.517551	181932.309316	36.199258
1413.047114	182239.922713	36.204276
1414.487533	182543.842892	36.209293
1415.854865	182849.477177	36.214311
1417.605817	183137.501968	36.219328
1418.859936	183435.409261	36.224346
1420.439767	183736.212735	36.229364
1421.937989	184028.597499	36.234381
1423.420538	184332.084892	36.239399
1424.720426	184621.784763	36.244416
1426.302596	184916.724286	36.249434
1427.837229	185209.716378	36.254452
1429.043401	185504.030682	36.259469
1430.545223	185796.699401	36.264487
1431.873283	186080.201591	36.269504
1432.742519	186366.925892	36.274522
1434.081569	186653.069451	36.279540
1435.193125	186940.443169	36.284557
1436.515182	187245.513634	36.289575
1438.074879	187526.519682	36.294592
1438.992821	187907.422500	36.299610
1440.286704	188208.512323	36.304628
1441.934422	188523.187331	36.309645
1442.858622	188839.856072	36.314663
1444.217328	189148.964686	36.319680
1445.701131	189475.352040	36.324698
1446.684086	189794.046264	36.329716
1448.491328	190121.096036	36.334733
1449.614238	190445.917011	36.339751
1451.148462	190769.480688	36.344768
1452.538868	191101.170507	36.349786
1453.719522	191437.389971	36.354804
1455.384897	191762.307436	36.359821
1456.868174	192112.807346	36.364839
1458.298276	192451.048015	36.369856
1459.683656	192797.221657	36.374874
1461.046274	193133.290262	36.379892
1462.767607	193476.720688	36.384909
1464.407109	193820.342647	36.389927
1466.208067	194158.606016	36.394944
1467.711929	194510.836588	36.399962
1469.285367	194844.742927	36.404980
1471.186587	195186.219176	36.409997
1472.338460	195522.885710	36.415015
1473.975692	195863.465122	36.420032
1475.326870	196207.976565	36.425050
1476.729276	196557.053110	36.430068
1478.535248	196891.156612	36.435085
1480.248373	197240.567215	36.440103
1481.748344	197568.903198	36.445120
1482.717837	197923.588365	36.450138
1484.558402	198257.232334	36.455156
1486.369232	198605.081344	36.460173
1487.877725	198952.292613	36.465191
1490.234431	199272.039355	36.470208
1491.749802	199610.741345	36.475226
1493.253465	199933.188545	36.480244
1494.710559	200265.093277	36.485261
1496.234006	200593.762218	36.490279
1497.798211	200913.864875	36.495296
1499.257941	201253.518861	36.500314
1500.827968	201586.627859	36.505332
1502.280721	201919.146197	36.510349
1503.671587	202249.464840	36.515367
1505.606563	202574.669244	36.520384
1506.860845	202906.356810	36.525402
1508.593652	203226.462713	36.530420
1510.226618	203558.574834	36.535437
1511.173247	203891.582444	36.540455
1512.726216	204204.224370	36.545472
1514.170956	204540.889340	36.550490
1515.363825	204882.471644	36.555508
1517.376187	205221.894041	36.560525
1518.333570	205556.782587	36.565543
1519.851231	205890.542464	36.570560
1521.107860	206238.035921	36.575578
1522.691599	206581.236441	36.580596
1524.613912	206908.888653	36.585613
1525.921172	207258.763694	36.590631
1527.759114	207597.277230	36.595648
1529.450636	207936.931918	36.600666
1531.395152	208252.262047	36.605684
1533.431531	208567.324181	36.610701
1534.738785	208869.875419	36.615719
1536.092125	209183.851290	36.620736
1537.633903	209492.996829	36.625754
1538.752163	209804.596936	36.630772
1540.383447	210121.223195	36.635789
1541.808176	210439.253938	36.640807
1543.001200	210745.965977	36.645824
1544.633070	211062.364595	36.650842
1546.453614	211391.181743	36.655860
1547.908010	211709.539506	36.660877
1549.175208	212045.810999	36.665895
1551.138169	212365.690275	36.670912
1552.921141	212683.032281	36.675930
1554.660030	212985.850625	36.680948
1556.706880	213309.858493	36.685965
1557.958567	213637.141172	36.690983
1559.658502	213943.726204	36.696000
1560.907062	214271.263991	36.701018
1562.251150	214580.852079	36.706036
1563.968425	214913.270795	36.711053
1565.662068	215229.536687	36.716071
1567.312278	215548.095964	36.721088
1568.755407	215877.255879	36.726106
1569.766247	216218.067847	36.731124
1571.179622	216549.798704	36.736141
1572.971347	216899.685156	36.741159
1574.316310	217237.498722	36.746176
1575.846482	217580.897787	36.751194
1577.411496	217929.753465	36.756212
1578.908277	218270.490779	36.761229
1580.226466	218626.117554	36.766247
1582.034106	218975.875828	36.771264
1583.769934	219324.248311	36.776282
1585.008561	219671.149140	36.781300
1586.699275	220035.127082	36.786317
1587.942557	220393.484719	36.791335
1589.515411	220756.668502	36.796352
1591.065679	221113.682784	36.801370
1592.766610	221486.703568	36.806388
1594.334100	221845.595307	36.811405
1596.049440	222210.586392	36.816423
1598.020954	222566.646062	36.821440
1599.342988	222927.405598	36.826458
1601.371592	223303.195456	36.831476
1602.602752	223673.495883	36.836493
1603.933406	224042.561395	36.841511
1605.643494	224414.362015	36.846528
1607.088299	224793.495153	36.851546
1608.869761	225181.060584	36.856564
1610.174191	225550.435137	36.861581
1611.502795	225936.242339	36.866599
1613.189642	226319.707083	36.871616
1614.807064	226699.143405	36.876634
1615.982646	227100.928200	36.881652
1617.333003	227484.775699	36.886669
1618.985491	227876.197053	36.891687
1620.804581	228279.862395	36.896704
1622.754315	228665.800547	36.901722
1624.707462	229054.456273	36.906740
1626.805747	229442.606468	36.911757
1628.510159	229825.788153	36.916775
1630.450670	230207.891160	36.921792
1631.971742	230592.523820	36.926810
1633.036864	230982.308439	36.931828
1635.281276	231355.624341	36.936845
1636.421127	231748.419905	36.941863
1637.771284	232128.683573	36.946880
1639.758846	232496.348513	36.951898
1641.640996	232852.064470	36.956916
1643.899288	233207.340268	36.961933
1645.385313	233555.648998	36.966951
1647.029820	233909.597738	36.971968
1648.828724	234253.182690	36.976986
1650.320216	234622.168498	36.982004
1652.105156	234981.657859	36.987021
1653.400553	235348.184157	36.992039
1655.072372	235696.030267	36.997056
1656.759081	236065.949574	37.002074
1658.243594	236436.077987	37.007092
1659.465339	236805.764478	37.012109
1660.830241	237184.979949	37.017127
1662.542606	237562.438581	37.022144
1664.257541	237938.245148	37.027162
1665.547624	238331.570007	37.032180
1667.027173	238717.396084	37.037197
1668.698532	239112.641751	37.042215
1670.328468	239508.274422	37.047232
1672.250616	239907.315682	37.052250
1673.348228	240315.147960	37.057268
1675.062424	240718.996421	37.062285
1676.681601	241125.475674	37.067303
1678.377539	241540.858817	37.072320
1680.249776	241949.634249	37.077338
1681.647062	242372.836119	37.082356
1683.066338	242779.724987	37.087373
1685.162329	243201.088614	37.092391
1686.837100	243620.104090	37.097408
1688.073465	244058.163418	37.102426
1689.794450	244498.406882	37.107444
1691.575940	244917.453961	37.112461
1693.340654	245349.356652	37.117479
1694.988348	245792.453959	37.122496
1696.960016	246214.821766	37.127514
1698.718373	246652.641456	37.132532
1700.505333	247070.438412	37.137549
1702.055508	247511.743445	37.142567
1703.874234	247948.585358	37.147584
1705.590506	248375.687713	37.152602
1707.746831	248818.190209	37.157620
1710.040318	249236.537928	37.162637
1712.020829	249661.436570	37.167655
1714.270418	250070.491873	37.172672
1716.854042	250478.528607	37.177690
1718.905569	250881.211542	37.182708
1721.071353	251272.292276	37.187725
1723.165955	251666.685425	37.192743
1724.614627	252060.848424	37.197760
1726.112170	252441.971639	37.202778
1727.721286	252833.262518	37.207796
1730.059772	253213.540914	37.212813
1731.540300	253604.595846	37.217831
1732.923174	254007.806923	37.222848
1734.621460	254383.330725	37.227866
1736.194328	254776.857322	37.232884
1738.041169	255164.243613	37.237901
1739.357814	255566.520692	37.242919
1741.127441	255967.989050	37.247936
1742.524338	256364.485111	37.252954
1743.853793	256767.569386	37.257972
1745.308592	257174.036516	37.262989
1746.563451	257595.012120	37.268007
1748.386284	258011.630113	37.273024
1750.052096	258434.265842	37.278042
1751.647695	258851.754790	37.283060
1752.928533	259273.152435	37.288077
1754.717799	259695.688257	37.293095
1756.000568	260111.977157	37.298112
1757.885804	260511.583956	37.303130
1759.217967	260941.044877	37.308148
1760.899182	261359.883151	37.313165
1762.207404	261797.955194	37.318183
1763.844465	262234.297672	37.323200
1765.564882	262671.184176	37.328218
1767.042573	263119.104954	37.333236
1768.351657	263573.704932	37.338253
1770.265259	264021.426728	37.343271
1772.109351	264485.921039	37.348288
1773.722460	264936.225876	37.353306
1775.403699	265412.780725	37.358324
1776.954468	265885.848702	37.363341
1778.855471	266354.643440	37.368359
1780.590367	266828.567100	37.373376
1782.613001	267312.171106	37.378394
1784.244080	267795.452997	37.383412
1786.419456	268267.091040	37.388429
1788.683382	268738.433503	37.393447
1790.595098	269229.715408	37.398464
1792.550448	269687.792773	37.403482
1794.520819	270168.596550	37.408500
1796.605610	270649.659254	37.413517
1798.159207	271116.173521	37.418535
1800.251358	271603.350753	37.423552
1802.186399	272065.101812	37.428570
1803.983770	272543.786460	37.433588
1805.871853	273022.606642	37.438605
1807.509558	273504.333164	37.443623
1809.310715	273980.317108	37.448640
1811.377160	274456.510801	37.453658
1812.903717	274949.725649	37.458676
1814.754682	275424.322108	37.463693
1817.098808	275901.987746	37.468711
1818.967239	276376.753662	37.473728
1820.933461	276853.939450	37.478746
1822.603200	277334.571772	37.483764
1824.678439	277812.521957	37.488781
1827.218525	278284.961858	37.493799
1829.059958	278763.374471	37.498816
1831.309981	279212.211124	37.503834
1833.264030	279682.905628	37.508852
1834.733336	280154.003160	37.513869
1836.838788	280612.021547	37.518887
1838.703505	281077.362950	37.523904
1841.002321	281527.854018	37.528922
1842.766775	281990.208755	37.533940
1845.342352	282434.987977	37.538957
1847.390898	282891.223299	37.543975
1849.040553	283339.925414	37.548992
1851.272632	283777.182661	37.554010
1852.728033	284226.696684	37.559028
1854.603467	284678.300476	37.564045
1856.286503	285128.255469	37.569063
1857.749390	285592.284142	37.574080
1859.624606	286027.576870	37.579098
1861.832304	286487.064524	37.584116
1863.111450	286945.145377	37.589133
1865.128146	287392.011312	37.594151
1866.755476	287863.666846	37.599168
1868.412365	288318.606591	37.604186
1870.117381	288774.602052	37.609204
1872.004040	289246.079973	37.614221
1873.694196	289708.088858	37.619239
1875.114881	290171.228350	37.624256
1877.033548	290643.224067	37.629274
1878.583732	291108.570754	37.634292
1880.488902	291555.323397	37.639309
1882.142421	292012.953803	37.644327
1883.916968	292469.825532	37.649344
1885.194648	292929.031266	37.654362
1887.389672	293395.072117	37.659380
1888.939381	293876.697878	37.664397
1890.960735	294353.777431	37.669415
1892.393676	294835.515226	37.674432
1894.418536	295313.881286	37.679450
1896.450395	295796.025224	37.684468
1898.069807	296288.461203	37.689485
1900.275077	296774.987396	37.694503
1901.843129	297276.384939	37.699520
1904.692328	297741.704704	37.704538
1906.927908	298225.725695	37.709556
1908.928877	298705.514135	37.714573
1911.154518	299176.657051	37.719591
1912.770685	299675.867640	37.724608
1914.890355	300154.507882	37.729626
1916.849229	300655.102937	37.734644
1918.540461	301145.276134	37.739661
1920.290947	301644.117581	37.744679
1921.639433	302149.541394	37.749696
1923.706455	302646.775387	37.754714
1925.564948	303155.892213	37.759732
1926.922075	303662.721734	37.764749
1929.155096	304179.690079	37.769767
1930.827756	304714.611586	37.774784
1932.712915	305235.431429	37.779802
1934.414417	305768.103600	37.784820
1936.029311	306304.489735	37.789837
1938.029363	306847.790319	37.794855
1939.477605	307381.068860	37.799872
1941.778108	307929.488789	37.804890
1943.832927	308470.656270	37.809908
1945.295680	309034.272186	37.814925
1947.422015	309580.416483	37.819943
1949.291658	310137.838859	37.824960
1952.471450	310660.657985	37.829978
1955.391904	311197.928434	37.834996
1958.011841	311722.549401	37.840013
1960.015836	312255.890288	37.845031
1962.027058	312788.665608	37.850048
1963.643522	313312.512090	37.855066
1965.449471	313839.368559	37.860084
1967.272333	314380.885636	37.865101
1969.220439	314899.053324	37.870119
1970.986783	315452.469312	37.875136
1972.537336	315982.437194	37.880154
1974.529529	316531.084200	37.885172
1976.360556	317067.289150	37.890189
1978.199003	317624.600589	37.895207
1980.036247	318177.438785	37.900224
1982.042659	318728.543292	37.905242
1984.100139	319290.468645	37.910260
1985.759418	319845.495922	37.915277
1988.208754	320392.119881	37.920295
1990.155172	320947.900017	37.925312
1992.082121	321503.295317	37.930330
1993.982881	322057.469433	37.935348
1996.795244	322598.171951	37.940365
1999.398134	323134.789621	37.945383
2001.379859	323680.353071	37.950400
2003.414311	324218.720346	37.955418
2005.582505	324766.980610	37.960436
2007.353534	325313.976280	37.965453
2009.035477	325836.696951	37.970471
2011.135361	326366.398981	37.975488
2012.814684	326884.920072	37.980506
2014.592382	327405.321935	37.985524
2016.664581	327930.389992	37.990541
2018.577723	328463.391722	37.995559
2020.647097	328985.122629	38.000576
2022.581630	329515.239890	38.005594
2024.623822	330043.405000	38.010612
2026.277237	330590.650942	38.015629
2028.212592	331132.238432	38.020647
2029.902728	331676.215967	38.025664
2031.798818	332225.886827	38.030682
2034.007708	332774.841239	38.035700
2035.739093	333342.025712	38.040717
2037.648776	333889.742348	38.045735
2039.663237	334465.515848	38.050752
2042.378463	335024.124464	38.055770
2044.922538	335555.990071	38.060788
2046.721725	336130.173342	38.065805
2048.995761	336674.722586	38.070823
2051.191643	337230.233656	38.075840
2053.641944	337788.055350	38.080858
2055.793092	338346.600079	38.085876
2057.408346	338917.572204	38.090893
2059.873668	339468.897701	38.095911
2062.243709	340033.849562	38.100928
2064.490504	340581.793331	38.105946
2066.533473	341136.684392	38.110964
2068.654738	341685.645112	38.115981
2071.012825	342244.451146	38.120999
2073.245415	342797.663035	38.126016
2074.879898	343355.626026	38.131034
2076.878899	343908.248015	38.136052
2078.946668	344476.598819	38.141069
2080.945411	345043.251875	38.146087
2082.712764	345620.430311	38.151104
2084.356549	346198.936873	38.156122
2086.807857	346769.978647	38.161140
2088.051998	347360.522113	38.166157
2090.132836	347948.464560	38.171175
2091.966899	348560.803063	38.176192
2094.112008	349156.219591	38.181210
2095.938096	349757.760637	38.186228
2097.400286	350377.248440	38.191245
2099.832684	350983.464172	38.196263
2101.882640	351608.363870	38.201280
2103.246445	352240.331113	38.206298
2105.593248	352861.204779	38.211316
2107.605324	353484.958245	38.216333
2110.273142	354108.064452	38.221351
2112.482324	354733.385020	38.226368
2114.454953	355357.411873	38.231386
2116.888755	355992.483162	38.236404
2118.731729	356631.766027	38.241421
2121.418172	357256.935959	38.246439
2123.397323	357890.645185	38.251456
2125.629382	358519.916398	38.256474
2128.916552	359123.154289	38.261492
2131.161180	359743.881191	38.266509
2133.368312	360357.402584	38.271527
2135.640864	360967.428725	38.276544
2137.478010	361588.485480	38.281562
2139.406625	362200.694680	38.286580
2141.743186	362817.085423	38.291597
2144.123961	363431.707604	38.296615
2145.850380	364047.534453	38.301632
2147.399413	364676.985610	38.306650
2149.874527	365273.687133	38.311668
2152.826156	365854.412057	38.316685
2155.506389	366442.846402	38.321703
2157.629909	367018.127529	38.326720
2159.269668	367597.121897	38.331738
2161.216827	368174.485317	38.336756
2163.093612	368758.411076	38.341773
2165.108489	369341.593681	38.346791
2167.124594	369949.216092	38.351808
2169.012316	370537.385564	38.356826
2171.509566	371131.148321	38.361844
2173.251908	371735.632839	38.366861
2175.617913	372339.981275	38.371879
2177.925696	372939.587722	38.376896
2179.752864	373555.572423	38.381914
2181.700114	374161.821157	38.386932
2183.575007	374792.439503	38.391949
2185.822224	375422.452945	38.396967
2188.079264	376048.472841	38.401984
2189.798829	376682.415400	38.407002
2192.073632	377331.050049	38.412020
2193.878640	377986.480598	38.417037
2195.923190	378628.001542	38.422055
2197.947543	379290.914132	38.427072
2199.394331	379959.574223	38.432090
2201.535430	380624.689253	38.437108
2203.634817	381306.586515	38.442125
2205.767184	382005.734151	38.447143
2208.083188	382698.882357	38.452160
2210.219344	383403.563481	38.457178
2212.475872	384088.452513	38.462196
2214.353134	384787.817672	38.467213
2216.974975	385497.581957	38.472231
2219.233261	386192.999510	38.477248
2221.387798	386907.127594	38.482266
2223.856009	387615.969953	38.487284
2226.127127	388341.357815	38.492301
2228.787879	389036.911938	38.497319
2231.090453	389757.569173	38.502336
2232.820204	390481.231963	38.507354
2235.813717	391182.901954	38.512372
2237.996123	391905.844191	38.517389
2240.327144	392614.918700	38.522407
2242.787719	393324.002815	38.527424
2245.132828	394043.159657	38.532442
2247.599238	394762.377244	38.537460
2249.903615	395467.827815	38.542477
2252.122338	396183.497372	38.547495
2254.970996	396881.834399	38.552512
2257.306262	397577.699920	38.557530
2259.748211	398282.083218	38.562548
2262.146871	398991.665970	38.567565
2264.541376	399687.965707	38.572583
2266.813740	400384.263674	38.577600
2268.985677	401102.979070	38.582618
2271.491427	401795.351178	38.587636
2273.409630	402497.410665	38.592653
2275.627127	403199.705430	38.597671
2277.606887	403903.533991	38.602688
2280.020839	404622.050230	38.607706
2282.232121	405326.557412	38.612724
2284.539082	406038.213394	38.617741
2286.523748	406751.516471	38.622759
2289.157560	407458.673637	38.627776
2291.391659	408173.258370	38.632794
2293.591050	408879.324985	38.637812
2296.299790	409584.176183	38.642829
2298.027084	410295.128462	38.647847
2300.668014	410994.480659	38.652864
2302.656149	411695.177307	38.657882
2305.138422	412378.320512	38.662900
2307.451304	413057.978031	38.667917
2309.914235	413745.279816	38.672935
2312.410940	414419.705682	38.677952
2314.291040	415116.615226	38.682970
2316.385892	415802.694446	38.687988
2318.423224	416497.257963	38.693005
2320.877359	417199.876610	38.698023
2323.087715	417903.875528	38.703040
2324.938652	418606.490953	38.708058
2327.658692	419323.562534	38.713076
2329.321646	420025.198712	38.718093
2331.527464	420757.573918	38.723111
2334.014785	421479.158706	38.728128
2336.139552	422215.135766	38.733146
2338.665107	422941.871559	38.738164
2341.362545	423682.054868	38.743181
2343.414447	424411.391102	38.748199
2345.533666	425156.111095	38.753216
2347.520712	425905.172240	38.758234
2350.073398	426658.616456	38.763252
2352.272757	427407.942260	38.768269
2354.545375	428170.321327	38.773287
2356.832331	428924.024986	38.778304
2359.145096	429696.398556	38.783322
2361.219160	430459.023967	38.788340
2364.286140	431242.844447	38.793357
2366.849482	432005.838685	38.798375
2369.201363	432783.492667	38.803392
2371.440572	433554.209536	38.808410
2373.581974	434335.068695	38.813428
2376.090220	435122.711440	38.818445
2378.992291	435902.225821	38.823463
2381.762451	436687.287338	38.828480
2383.395866	437464.763692	38.833498
2386.312994	438257.771318	38.838516
2388.804683	439045.103174	38.843533
2391.248786	439821.901254	38.848551
2393.804407	440601.175731	38.853568
2396.147448	441395.555541	38.858586
2398.597611	442200.341289	38.863604
2401.278464	442982.578085	38.868621
2403.513783	443773.236228	38.873639
2406.167091	444543.086770	38.878656
2408.180977	445346.642076	38.883674
2410.704940	446140.335119	38.888692
2413.444053	446927.849288	38.893709
2416.117716	447708.471656	38.898727
2418.210006	448482.081702	38.903744
2420.903843	449290.153590	38.908762
2423.202985	450085.526730	38.913780
2425.930846	450869.942041	38.918797
2427.928200	451661.101599	38.923815
2430.605170	452458.127504	38.928832
2432.535036	453262.100211	38.933850
2435.302302	454065.148115	38.938868
2437.853805	454856.633389	38.943885
2440.200679	455645.490139	38.948903
2442.973407	456438.736897	38.953920
2445.029170	457244.475827	38.958938
2447.613954	458044.290548	38.963956
2449.994997	458846.623505	38.968973
2452.009576	459647.311055	38.973991
2454.743925	460450.926908	38.979008
2457.221828	461267.917129	38.984026
2459.234146	462066.372447	38.989044
2461.945859	462859.988452	38.994061
2464.809346	463650.264029	38.999079
2467.050156	464423.900680	39.004096
2469.251383	465191.756763	39.009114
2471.802584	465966.686304	39.014132
2474.429615	466731.428760	39.019149
2476.740751	467523.424009	39.024167
2479.551718	468284.787481	39.029184
2481.641547	469065.848673	39.034202
2484.330805	469838.306077	39.039220
2487.024065	470634.076626	39.044237
2489.183827	471417.738369	39.049255
2491.697686	472200.298543	39.054272
2494.582943	472979.283648	39.059290
2496.969575	473772.679697	39.064308
2499.929657	474556.619396	39.069325
2501.875179	475349.200168	39.074343
2504.511026	476139.768478	39.079360
2506.796013	476938.065706	39.084378
2509.426916	477751.694305	39.089396
2512.246061	478555.926444	39.094413
2514.269609	479362.812826	39.099431
2516.738859	480171.150731	39.104448
2519.273650	481002.923060	39.109466
2521.270940	481818.255561	39.114484
2523.940670	482640.596350	39.119501
2526.323958	483479.718921	39.124519
2528.671054	484317.542084	39.129536
2530.951929	485163.795104	39.134554
2533.095683	486007.554357	39.139572
2535.885990	486853.785957	39.144589
2538.493914	487706.498057	39.149607
2541.244521	488568.963313	39.154624
2543.651316	489432.743121	39.159642
2546.153218	490299.027675	39.164660
2549.099356	491155.119839	39.169677
2551.657347	492025.678329	39.174695
2554.580451	492892.452909	39.179712
2556.920787	493777.598530	39.184730
2559.575315	494633.235428	39.189748
2562.052540	495509.444593	39.194765
2564.413737	496393.877228	39.199783
2567.015067	497265.028766	39.204800
2570.056698	498140.036908	39.209818
2572.299848	499024.732556	39.214836
2575.038360	499919.465131	39.219853
2577.286163	500808.884134	39.224871
2579.714109	501701.743574	39.229888
2582.326585	502589.285007	39.234906
2584.992451	503485.570153	39.239924
2587.535536	504385.341044	39.244941
2590.474160	505288.314497	39.249959
2593.139180	506178.745267	39.254976
2595.677545	507067.379195	39.259994
2598.548072	507969.689924	39.265012
2602.591749	508822.611453	39.270029
2606.113409	509687.635448	39.275047
2609.398363	510534.887588	39.280064
2611.570802	511402.380804	39.285082
2614.177447	512259.190677	39.290100
2616.949114	513102.896901	39.295117
2619.354380	513963.304258	39.300135
2621.696096	514816.326594	39.305152
2624.455587	515676.823122	39.310170
2626.622085	516534.040178	39.315188
2629.305712	517384.084318	39.320205
2631.786495	518246.624719	39.325223
2634.288819	519112.173415	39.330240
2636.796310	519963.994116	39.335258
2639.314243	520801.083188	39.340276
2641.942561	521634.534687	39.345293
2644.044563	522471.886485	39.350311
2646.403037	523298.190911	39.355328
2648.965503	524137.678088	39.360346
2651.760337	524998.731967	39.365364
2653.969895	525848.717982	39.370381
2656.275562	526688.888005	39.375399
2659.157978	527540.870578	39.380416
2662.007347	528411.288857	39.385434
2664.557825	529276.974601	39.390452
2667.351547	530136.437462	39.395469
2669.795378	531014.129310	39.400487
2672.068362	531887.118272	39.405504
2674.753217	532768.319927	39.410522
2677.677985	533657.809509	39.415540
2680.304181	534537.543856	39.420557
2682.169709	535430.290009	39.425575
2685.123115	536332.241840	39.430592
2688.179350	537237.928994	39.435610
2690.244207	538156.004534	39.440628
2693.055719	539065.866336	39.445645
2695.492190	539987.716235	39.450663
2698.170706	540916.235774	39.455680
2701.280855	541843.113873	39.460698
2703.850161	542784.408690	39.465716
2706.241451	543716.177845	39.470733
2709.247699	544670.507681	39.475751
2711.830450	545617.305686	39.480768
2714.905463	546565.459164	39.485786
2717.263672	547524.636369	39.490804
2720.122644	548475.134440	39.495821
2722.922013	549432.890019	39.500839
2725.697079	550386.362170	39.505856
2728.619602	551348.160488	39.510874
2731.554123	552320.810814	39.515892
2734.410615	553273.291684	39.520909
2736.951241	554223.491002	39.525927
2740.210781	555188.340120	39.530944
2743.356618	556145.310478	39.535962
2746.031245	557101.425991	39.540980
2748.908100	558052.772685	39.545997
2751.783024	559021.982823	39.551015
2754.754296	559973.211001	39.556032
2757.614354	560932.396262	39.561050
2760.725087	561889.861134	39.566068
2763.373279	562843.813776	39.571085
2766.140228	563802.729175	39.576103
2768.998208	564758.646666	39.581120
2771.551372	565718.740148	39.586138
2773.954648	566690.245259	39.591156
2776.596049	567636.495128	39.596173
2779.596433	568613.803943	39.601191
2782.150641	569580.836341	39.606208
2784.909473	570548.806469	39.611226
2787.399329	571538.711180	39.616244
2790.163231	572508.016083	39.621261
2793.068242	573493.231325	39.626279
2795.462596	574478.891148	39.631296
2798.569159	575463.502958	39.636314
2801.133799	576458.070186	39.641332
2803.527724	577439.618389	39.646349
2806.670469	578432.119046	39.651367
2809.622215	579420.909803	39.656384
2812.844465	580407.569748	39.661402
2815.341175	581403.757633	39.666420
2818.953399	582375.427845	39.671437
2822.588167	583331.708006	39.676455
2825.539655	584279.862065	39.681472
2828.751036	585196.746982	39.686490
2831.203196	586125.221491	39.691508
2834.019847	587040.913503	39.696525
2836.388641	587968.544099	39.701543
2839.203152	588899.124271	39.706560
2841.932383	589817.844039	39.711578
2844.533137	590758.941689	39.716596
2847.233884	591700.041300	39.721613
2850.051968	592639.491237	39.726631
2852.505970	593582.312592	39.731648
2855.393822	594532.775179	39.736666
2858.220111	595509.983854	39.741684
2860.935713	596463.547150	39.746701
2863.846904	597422.387170	39.751719
2866.941155	598389.849692	39.756736
2870.037150	599355.675175	39.761754
2872.849185	600332.339522	39.766772
2875.339606	601304.719847	39.771789
2878.110065	602293.437515	39.776807
2880.874826	603278.867875	39.781824
2883.786026	604273.164598	39.786842
2885.926789	605271.478217	39.791860
2888.790478	606285.349054	39.796877
2891.544962	607308.217027	39.801895
2894.325167	608337.114823	39.806912
2897.053591	609366.216455	39.811930
2899.615711	610408.955855	39.816948
2902.280006	611449.128687	39.821965
2905.380719	612506.828511	39.826983
2907.827179	613572.497435	39.832000
2910.681229	614632.505948	39.837018
2913.553403	615711.142946	39.842036
2916.172823	616785.018000	39.847053
2919.477483	617873.571997	39.852071
2921.915839	618956.760483	39.857088
2925.683184	620044.456178	39.862106
2928.429468	621141.508584	39.867124
2931.364689	622226.852109	39.872141
2934.510349	623329.675900	39.877159
2937.460229	624422.445267	39.882176
2941.052655	625522.412113	39.887194
2943.602625	626614.351213	39.892212
2946.575295	627716.656616	39.897229
2949.782190	628830.648191	39.902247
2952.628895	629932.919856	39.907264
2956.009673	631039.411460	39.912282
2958.633216	632148.183139	39.917300
2961.897676	633254.487005	39.922317
2965.055435	634358.639402	39.927335
2968.269614	635470.962748	39.932352
2971.303710	636567.863266	39.937370
2974.324350	637683.090857	39.942388
2977.407733	638776.444564	39.947405
2980.305517	639877.556662	39.952423
2983.142664	640993.066812	39.957440
2985.727414	642097.695641	39.962458
2988.578709	643225.116481	39.967476
2991.506547	644345.678975	39.972493
2994.170349	645471.663366	39.977511
2996.743698	646599.462538	39.982528
3000.013829	647723.785317	39.987546
3003.224271	648856.275757	39.992564
3006.122251	649986.638499	39.997581
3009.554106	651115.834196	40.002599
3012.394231	652256.006410	40.007616
3015.585541	653374.183343	40.012634
3018.773083	654498.279472	40.017652
3021.896302	655589.334568	40.022669
3024.715251	656679.212996	40.027687
3027.035197	657775.439030	40.032704
3030.389623	658851.570024	40.037722
3033.379813	659954.222100	40.042740
3035.997394	661051.388369	40.047757
3039.182329	662144.957246	40.052775
3041.868898	663257.464543	40.057792
3044.709486	664372.634158	40.062810
3048.084124	665484.752609	40.067828
3050.998133	666602.949777	40.072845
3054.011965	667723.467000	40.077863
3056.929765	668856.048383	40.082880
3060.741418	669972.582814	40.087898
3063.962853	671100.264647	40.092916
3066.863644	672230.673709	40.097933
3069.901849	673362.201166	40.102951
3072.751950	674517.632627	40.107968
3075.616595	675664.090492	40.112986
3078.591253	676813.398155	40.118004
3081.660445	677968.675725	40.123021
3084.467091	679127.896872	40.128039
3086.774277	680298.422456	40.133056
3090.108635	681492.827130	40.138074
3093.479766	682668.648275	40.143092
3096.386260	683854.866966	40.148109
3099.781112	685049.647284	40.153127
3102.774835	686252.233728	40.158144
3105.850841	687440.934120	40.163162
3109.079519	688645.561217	40.168180
3112.294007	689856.937296	40.173197
3115.724638	691059.154067	40.178215
3118.562960	692284.173133	40.183232
3121.343463	693484.802280	40.188250
3124.787184	694712.576136	40.193268
3127.914122	695950.837087	40.198285
3130.952388	697178.549804	40.203303
3133.770960	698419.249079	40.208320
3137.002230	699658.113279	40.213338
3139.815134	700895.568816	40.218356
3142.771151	702144.610535	40.223373
3146.018041	703403.086814	40.228391
3149.233256	704670.204000	40.233408
3152.713657	705918.080554	40.238426
3155.829664	707177.560272	40.243444
3159.043441	708439.241588	40.248461
3162.367379	709702.726304	40.253479
3165.601568	710970.855015	40.258496
3168.534687	712244.890508	40.263514
3171.763424	713520.693618	40.268532
3175.257584	714775.101640	40.273549
3178.894973	716051.412276	40.278567
3181.416454	717336.014523	40.283584
3184.526486	718610.310703	40.288602
3187.935034	719882.379393	40.293620
3191.294122	721168.182678	40.298637
3194.401688	722436.477079	40.303655
3197.622696	723715.718984	40.308672
3201.392605	724987.473681	40.313690
3204.702950	726267.700076	40.318708
3207.950441	727537.927743	40.323725
3211.503166	728794.315191	40.328743
3214.364767	730061.570661	40.333760
3217.663715	731319.838663	40.338778
3221.285938	732584.827451	40.343796
3224.482209	733851.045173	40.348813
3228.044219	735112.222119	40.353831
3231.257363	736356.282898	40.358848
3234.489897	737570.401257	40.363866
3238.040266	738774.296248	40.368884
3241.344867	739969.092027	40.373901
3244.780263	741166.325274	40.378919
3247.373348	742369.976871	40.383936
3250.804092	743568.929184	40.388954
3253.910880	744763.561880	40.393972
3257.016554	745973.607262	40.398989
3260.495675	747176.374206	40.404007
3263.470030	748405.418586	40.409024
3266.944856	749602.237057	40.414042
3270.015697	750817.117577	40.419060
3272.913026	752046.385179	40.424077
3277.055985	753271.470943	40.429095
3279.628494	754499.042945	40.434112
3282.494599	755741.454619	40.439130
3285.867650	756977.982248	40.444148
3289.217432	758233.309500	40.449165
3292.318626	759481.544227	40.454183
3295.179212	760745.906366	40.459200
3298.853753	762004.624043	40.464218
3301.703027	763284.005455	40.469236
3304.722632	764568.706525	40.474253
3308.020853	765842.554053	40.479271
3311.029797	767149.686509	40.484288
3314.125615	768448.729650	40.489306
3317.375508	769756.015959	40.494324
3320.510174	771083.907447	40.499341
3323.894951	772396.147786	40.504359
3326.756245	773742.148572	40.509376
3330.450195	775080.225642	40.514394
3334.035190	776422.894577	40.519412
3337.303512	777764.711754	40.524429
3340.969733	779105.565172	40.529447
3344.402858	780457.031228	40.534464
3347.587963	781797.520935	40.539482
3351.035858	783153.715269	40.544500
3354.224153	784504.647051	40.549517
3357.778939	785859.981418	40.554535
3361.628544	787228.020825	40.559552
3364.942114	788573.713821	40.564570
3368.179476	789940.360760	40.569588
3371.262824	791313.623638	40.574605
3375.196173	792677.788369	40.579623
3378.598352	794042.921591	40.584640
3382.333004	795424.822304	40.589658
3386.149508	796766.951910	40.594676
3389.622290	798133.408440	40.599693
3392.934069	799485.575473	40.604711
3396.213241	800857.768521	40.609728
3399.679449	802226.475387	40.614746
3403.094826	803588.035602	40.619764
3406.175141	804957.387300	40.624781
3409.553869	806330.630900	40.629799
3413.230913	807694.046709	40.634816
3416.105870	809068.284860	40.639834
3419.363831	810452.471562	40.644852
3422.975783	811833.188214	40.649869
3426.399216	813211.881642	40.654887
3429.807592	814605.141546	40.659904
3432.518045	815983.821816	40.664922
3436.456159	817364.919169	40.669940
3439.723142	818758.050037	40.674957
3443.178246	820149.964618	40.679975
3446.728476	821541.842045	40.684992
3450.114679	822930.616552	40.690010
3453.630449	824321.094367	40.695028
3456.529156	825702.232141	40.700032
3460.342708	827023.351901	40.705037
3463.312130	828325.654091	40.710042
3466.732779	829567.450221	40.715047
3470.115655	830738.942285	40.720052
3472.800847	831859.120201	40.725056
3475.407402	832897.125049	40.730061
3478.162523	833905.599368	40.735066
3480.827995	834841.677307	40.740071
3483.560548	835713.620133	40.745076
3485.987853	836537.821800	40.750080
3488.033908	837294.028416	40.755085
3490.072913	837984.827458	40.760090
3492.219214	838634.191904	40.765095
3494.301912	839234.205665	40.770100
3495.926261	839779.609284	40.775104
3497.952194	840266.790949	40.780109
3499.533858	840723.640124	40.785114
3501.046878	841135.070658	40.790119
3502.888706	841493.076642	40.795124
3504.092449	841809.651112	40.800128
3505.136396	842084.725955	40.805133
3505.956149	842342.173320	40.810138
3506.744003	842556.752502	40.815143
3508.398301	842743.455081	40.820148
3509.158051	842913.710207	40.825152
3510.086421	843026.530846	40.830157
3510.703927	843133.289213	40.835162
3511.278073	843210.478986	40.840167
3511.555377	843268.418866	40.845172
3512.486949	843313.651032	40.850176
3513.320940	843324.089400	40.855181
3513.629765	843321.617151	40.860186
3514.058859	843302.448863	40.865191
3514.270824	843261.110316	40.870196
3515.019274	843225.796229	40.875200
3515.467261	843149.610521	40.880205
3515.686289	843074.914090	40.885210
3515.941539	842981.108763	40.890215
3516.595918	842870.755036	40.895220
3516.312441	842763.164037	40.900224
3516.895109	842644.962756	40.905229
3517.365440	842506.606142	40.910234
3517.074642	842358.570673	40.915239
3517.498331	842212.068444	40.920244
3517.595886	842055.042618	40.925248
3517.401078	841893.403099	40.930253
3517.675500	841710.542699	40.935258
3517.507268	841546.464873	40.940263
3517.952902	841370.938428	40.945268
3517.969118	841182.476518	40.950272
3517.719597	840992.983167	40.955277
3517.929608	840802.538906	40.960282
3517.700007	840607.307001	40.965287
3517.968312	840405.200259	40.970292
3517.442027	840200.882567	40.975296
3517.809490	839994.574842	40.980301
3517.714915	839807.347750	40.985306
3517.668766	839601.091017	40.990311
3517.721722	839388.116918	40.995316
3517.582697	839187.487794	41.000320
3517.444926	838967.736478	41.005325
3517.470745	838767.940722	41.010330
3517.230479	838552.071479	41.015335
3517.321394	838336.627849	41.020340
3516.985629	838125.513133	41.025344
3517.135527	837907.521588	41.030349
3517.195553	837686.527495	41.035354
3516.623216	837480.764820	41.040359
3516.796106	837264.881432	41.045364
3516.944273	837052.973688	41.050368
3516.379626	836850.197022	41.055373
3516.538149	836640.311415	41.060378
3515.932942	836428.596367	41.065383
3516.331654	836217.493497	41.070388
3516.453608	836010.795043	41.075392
3516.346556	835796.941091	41.080397
3516.110136	835576.886167	41.085402
3515.742463	835378.009356	41.090407
3515.833972	835170.995413	41.095412
3515.532762	834958.986678	41.100416
3515.620491	834759.532677	41.105421
3515.349554	834550.806187	41.110426
3515.313896	834348.930243	41.115431
3515.377052	834142.662116	41.120436
3514.890435	833944.727485	41.125440
3514.964092	833741.940040	41.130445
3514.418262	833536.523240	41.135450
3514.577283	833350.122479	41.140455
3514.164377	833147.293926	41.145460
3514.170184	832967.412715	41.150464
3514.481995	832762.223934	41.155469
3514.162324	832573.154249	41.160474
3513.804328	832381.170467	41.165479
3514.140050	832191.986376	41.170484
3513.579484	832016.050971	41.175488
3513.709624	831826.207539	41.180493
3513.918076	831634.500037	41.185498
3513.826311	831452.160123	41.190503
3513.641956	831263.514010	41.195508
3513.614419	831070.756792	41.200512
3513.528492	830889.856393	41.205517
3513.184855	830705.881576	41.210522
3512.913410	830526.165286	41.215527
3512.961571	830338.522822	41.220532
3512.790399	830167.234102	41.225536
3512.574682	829994.101141	41.230541
3512.489403	829817.152833	41.235546
3512.353167	829643.317167	41.240551
3511.977388	829490.408762	41.245556
3511.915676	829321.411463	41.250560
3511.821275	829144.347761	41.255565
3511.753057	828985.741506	41.260570
3511.118750	828841.896112	41.265575
3511.728161	828675.400193	41.270580
3511.784601	828518.414614	41.275584
3511.772211	828348.702132	41.280589
3511.906039	828197.819979	41.285594
3511.098471	828028.903312	41.290599
3511.412628	827874.971503	41.295604
3511.165317	827717.818320	41.300608
3510.909990	827571.453278	41.305613
3510.852476	827425.539884	41.310618
3510.749355	827262.422107	41.315623
3510.378904	827113.730765	41.320628
3510.164050	826969.483833	41.325632
3510.078753	826835.422119	41.330637
3509.974321	826690.665193	41.335642
3509.933965	826548.033918	41.340647
3509.826228	826416.008365	41.345652
3509.865636	826281.720522	41.350656
3509.864238	826152.103543	41.355661
3509.996920	826017.503595	41.360666
3509.390629	825894.588053	41.365671
3509.736423	825762.185741	41.370676
3509.253385	825625.339537	41.375680
3509.171308	825491.831296	41.380685
3509.152378	825371.050124	41.385690
3509.162598	825245.302125	41.390695
3509.081057	825117.718046	41.395700
3508.621335	825000.694145	41.400704
3508.413294	824884.795763	41.405709
3508.609708	824774.862094	41.410714
3508.685177	824645.395685	41.415719
3508.728725	824525.560685	41.420724
3508.533807	824407.025079	41.425728
3508.287441	824297.832931	41.430733
3508.346094	824187.132114	41.435738
3508.255672	824065.947299	41.440743
3508.281445	823949.313771	41.445748
3507.918744	823834.100603	41.450752
3507.999548	823730.683715	41.455757
3507.777080	823635.775704	41.460762
3507.614512	823534.728235	41.465767
3507.691246	823419.341307	41.470772
3507.687099	823306.591508	41.475776
3507.589287	823207.182345	41.480781
3507.446501	823096.298774	41.485786
3507.014032	823011.337182	41.490791
3507.506490	822901.226382	41.495796
3507.084472	822809.352779	41.500800
3507.464558	822720.271197	41.505805
3507.677886	822621.971445	41.510810
3507.063946	822524.869697	41.515815
3506.953179	822413.774219	41.520820
3506.963694	822323.285201	41.525824
3506.751676	822236.332454	41.530829
3506.582511	822139.738897	41.535834
3506.773203	822045.617461	41.540839
3506.685593	821958.154820	41.545844
3506.861654	821876.682698	41.550848
3506.737227	821785.914960	41.555853
3506.505733	821700.319993	41.560858
3506.265254	821613.460208	41.565863
3506.197997	821530.756517	41.570868
3506.010860	821439.506920	41.575872
3505.761385	821366.268857	41.580877
3506.145208	821289.816836	41.585882
3506.474573	821218.238206	41.590887
3506.191994	821117.656381	41.595892
3505.898847	821047.827493	41.600896
3505.621793	820964.175808	41.605901
3505.779110	820881.720270	41.610906
3505.498343	820822.105668	41.615911
3505.439064	820733.939973	41.620916
3505.375345	820666.893307	41.625920
3505.159241	820600.356365	41.630925
3505.293277	820534.737244	41.635930
3505.257394	820467.100094	41.640935
3505.370597	820395.059076	41.645940
3505.217780	820339.215655	41.650944
3505.140077	820268.662961	41.655949
3505.307002	820201.088528	41.660954
3505.278105	820144.834650	41.665959
3505.381889	820069.773980	41.670964
3504.917762	820000.057302	41.675968
3504.957801	819937.950624	41.680973
3505.066822	819873.399098	41.685978
3505.127688	819824.720608	41.690983
3504.825376	819749.622196	41.695988
3504.882947	819693.545375	41.700992
3504.500615	819634.227207	41.705997
3504.634063	819577.650768	41.711002
3504.667202	819519.726688	41.716007
3504.534414	819453.553749	41.721012
3504.600768	819407.888794	41.726016
3504.802188	819338.644689	41.731021
3504.293889	819289.953621	41.736026
3504.362977	819231.826535	41.741031
3504.612044	819169.582125	41.746036
3504.347552	819118.515225	41.751040
3504.333813	819065.169648	41.756045
3504.382538	819017.168161	41.761050
3504.024630	818971.079552	41.766055
3504.278788	818917.885532	41.771060
3504.194318	818869.611665	41.776064
3503.926525	818818.153391	41.781069
3504.124577	818767.011287	41.786074
3504.356829	818713.916299	41.791079
3504.414353	818659.679890	41.796084
3503.944486	818607.569958	41.801088
3503.879350	818559.972160	41.806093
3504.197044	818509.977535	41.811098
3503.783507	818474.603416	41.816103
3504.202820	818426.831507	41.821108
3503.937362	818374.200857	41.826112
3503.790099	818314.249128	41.831117
3503.658263	818271.527648	41.836122
3503.487224	818232.024997	41.841127
3503.677248	818193.439292	41.846132
3503.710280	818150.593843	41.851136
3504.248844	818105.624401	41.856141
3503.561015	818058.412192	41.861146
3503.731221	818019.244306	41.866151
3503.631406	817970.186904	41.871156
3503.884132	817940.839738	41.876160
3503.642086	817892.096057	41.881165
3503.873895	817846.004265	41.886170
3503.359770	817802.852472	41.891175
3503.421466	817757.760319	41.896180
3503.440499	817723.677485	41.901184
3503.381379	817685.030200	41.906189
3503.594189	817644.587458	41.911194
3503.395077	817603.527233	41.916199
3503.609239	817569.997294	41.921204
3503.663644	817528.994320	41.926208
3503.613718	817479.827872	41.931213
3503.212771	817442.011512	41.936218
3503.059844	817410.875118	41.941223
3503.324493	817362.924462	41.946228
3503.163155	817338.118524	41.951232
3503.381211	817298.549109	41.956237
3503.604849	817261.802552	41.961242
3503.106355	817230.232380	41.966247
3503.408891	817185.195806	41.971252
3503.174795	817153.778673	41.976256
3503.211666	817111.996648	41.981261
3503.440203	817082.064929	41.986266
3503.067441	817036.840702	41.991271
3502.932885	816998.687852	41.996276
3503.113139	816967.399771	42.001280
3503.451209	816942.222035	42.006285
3503.347448	816905.427171	42.011290
3503.101696	816872.841830	42.016295
3503.169616	816824.917784	42.021300
3502.856202	816789.518404	42.026304
3503.006775	816759.889483	42.031309
3502.841373	816723.103176	42.036314
3502.968217	816712.955123	42.041319
3502.740303	816672.672350	42.046324
3503.062780	816647.203697	42.051328
3502.850866	816629.999117	42.056333
3502.560817	816595.958422	42.061338
3502.965092	816573.008794	42.066343
3502.664888	816540.040664	42.071348
3502.601011	816502.165891	42.076352
3502.872329	816483.716681	42.081357
3503.146453	816436.926107	42.086362
3502.377436	816413.087995	42.091367
3502.602231	816384.516998	42.096372
3502.794729	816352.347384	42.101376
3502.777318	816330.826285	42.106381
3502.925804	816301.000723	42.111386
3502.455912	816280.426725	42.116391
3502.505403	816248.376324	42.121396
3502.505775	816223.638056	42.126400
3502.353708	816206.520345	42.131405
3502.268063	816174.588084	42.136410
3502.102930	816157.374884	42.141415
3502.638986	816136.643159	42.146420
3502.537210	816108.121947	42.151424
3502.440181	816089.339566	42.156429
3502.448575	816059.924338	42.161434
3502.260073	816045.733803	42.166439
3502.742897	816020.432323	42.171444
3502.283844	815995.667570	42.176448
3502.106803	815983.033474	42.181453
3502.350843	815948.321355	42.186458
3502.295585	815933.427941	42.191463
3502.332669	815917.448659	42.196468
3502.276292	815903.042345	42.201472
3502.518230	815878.654546	42.206477
3502.140449	815850.467501	42.211482
3501.976330	815838.220694	42.216487
3502.049468	815813.956430	42.221492
3502.276100	815793.077134	42.226496
3502.108052	815776.447747	42.231501
3502.273921	815752.071345	42.236506
3502.162463	815735.043392	42.241511
3502.552897	815710.047307	42.246516
3502.249178	815693.731116	42.251520
3502.230491	815682.630107	42.256525
3502.281098	815653.595978	42.261530
3502.232752	815627.499308	42.266535
3502.299379	815604.891120	42.271540
3502.188891	815590.297733	42.276544
3501.759954	815567.377258	42.281549
3502.180775	815557.668398	42.286554
3501.778935	815540.880118	42.291559
3502.014456	815519.706303	42.296564
3501.727115	815497.737495	42.301568
3501.946535	815493.904390	42.306573
3502.154990	815480.527170	42.311578
3502.169637	815462.212475	42.316583
3502.086082	815430.470890	42.321588
3501.824557	815427.686999	42.326592
3501.975154	815418.117573	42.331597
3502.443556	815389.309127	42.336602
3502.181223	815373.277850	42.341607
3501.953140	815354.318926	42.346612
3501.892781	815340.009342	42.351616
3502.286314	815321.927233	42.356621
3502.163921	815310.159910	42.361626
3501.922427	815294.417400	42.366631
3502.038454	815272.676972	42.371636
3502.157930	815251.910030	42.376640
3501.473812	815241.009666	42.381645
3501.865500	815222.245687	42.386650
3501.665104	815203.866439	42.391655
3501.758575	815195.766765	42.396660
3501.962831	815197.780502	42.401664
3501.957998	815179.955079	42.406669
3501.867026	815173.540198	42.411674
3501.993561	815141.277245	42.416679
3501.924399	815134.956327	42.421684
3501.952067	815114.203278	42.426688
3501.550045	815089.913067	42.431693
3501.824656	815078.862548	42.436698
3501.461674	815064.794465	42.441703
3501.788903	815045.552968	42.446708
3501.734588	815051.503703	42.451712
3501.562460	815036.041936	42.456717
3501.664007	815017.907180	42.461722
3501.705286	815025.888683	42.466727
3501.437290	814995.829751	42.471732
3501.738288	814977.468872	42.476736
3501.596645	814976.224665	42.481741
3501.441739	814976.151504	42.486746
3501.555907	814965.125865	42.491751
3501.758977	814946.780204	42.496756
3501.762728	814938.889052	42.501760
3501.804862	814925.926306	42.506765
3501.730428	814903.045385	42.511770
3501.523985	814902.882863	42.516775
3501.874176	814893.671097	42.521780
3501.644391	814877.243793	42.526784
3501.452718	814873.766821	42.531789
3501.644511	814861.365042	42.536794
3501.554939	814860.892001	42.541799
3501.537282	814844.236619	42.546804
3502.059611	814843.960172	42.551808
3501.927217	814828.589097	42.556813
3502.005595	814810.457362	42.561818
3501.992594	814798.477139	42.566823
3501.529556	814778.189352	42.571828
3501.539475	814771.953121	42.576832
3501.497535	814751.404585	42.581837
3501.554827	814736.101047	42.586842
3501.836266	814740.246066	42.591847
3501.801125	814720.962801	42.596852
3501.558412	814709.407990	42.601856
3501.572652	814705.021968	42.606861
3501.339813	814684.210797	42.611866
3501.607811	814677.641872	42.616871
3501.956589	814672.131923	42.621876
3502.073572	814662.469178	42.626880
3501.630688	814645.587480	42.631885
3501.646350	814631.361808	42.636890
3501.680705	814622.588696	42.641895
3501.651359	814593.464719	42.646900
3501.933721	814597.512269	42.651904
3501.599320	814570.871379	42.656909
3501.833611	814561.774665	42.661914
3501.549309	814556.461000	42.666919
3501.484388	814539.909615	42.671924
3502.000021	814534.665727	42.676928
3501.769491	814529.343632	42.681933
3501.627441	814507.056358	42.686938
3501.744912	814496.419065	42.691943
3501.627907	814487.864268	42.696948
3501.908597	814471.648364	42.701952
3501.668995	814459.118381	42.706957
3502.038291	814439.673604	42.711962
3501.437731	814424.277295	42.716967
3501.776735	814426.075375	42.721972
3501.868354	814421.677058	42.726976
3501.634402	814397.844993	42.731981
3501.658512	814386.832415	42.736986
3501.462747	814392.416193	42.741991
3501.658056	814366.860709	42.746996
3501.561113	814358.400022	42.752000
3501.936664	814346.553043	42.757005
3502.033882	814333.580459	42.762010
3501.779700	814325.728854	42.767015
3501.587941	814315.431866	42.772020
3501.633634	814293.601606	42.777024
3501.552364	814296.634522	42.782029
3501.478354	814284.273152	42.787034
3501.875670	814269.986998	42.792039
3501.469656	814253.683027	42.797044
3501.453239	814252.906226	42.802049
3501.817843	814253.336397	42.807053
3501.724085	814225.389882	42.812058
3501.466063	814219.974395	42.817063
3501.279503	814208.897009	42.822068
3501.549019	814194.046102	42.827073
3501.477621	814189.575680	42.832077
3501.838440	814187.083649	42.837082
3501.412458	814173.120827	42.842087
3501.518330	814155.080323	42.847092
3501.326074	814152.772163	42.852097
3501.357304	814155.495279	42.857101
3501.707008	814147.256767	42.862106
3501.635040	814133.433371	42.867111
3501.473454	814117.870255	42.872116
3501.235289	814119.953505	42.877121
3501.162621	814119.770047	42.882125
3501.802193	814097.456557	42.887130
3501.522705	814088.634328	42.892135
3501.428615	814089.331072	42.897140
3501.910347	814080.194980	42.902145
3501.450216	814067.211542	42.907149
3501.528631	814056.871894	42.912154
3501.673436	814055.387865	42.917159
3501.958354	814038.585610	42.922164
3501.671680	814027.523552	42.927169
3501.712784	814021.866274	42.932173
3501.443292	813987.808127	42.937178
3501.710396	813994.391629	42.942183
3501.617331	813991.288466	42.947188
3501.735197	813976.363322	42.952193
3501.520126	813963.731079	42.957197
3501.656543	813951.043866	42.962202
3501.332936	813951.776503	42.967207
3501.384659	813925.754514	42.972212
3501.505181	813921.253899	42.977217
3501.345169	813925.273610	42.982221
3501.622942	813911.395051	42.987226
3501.409662	813903.049365	42.992231
3501.483612	813890.274363	42.997236
3501.552789	813886.171473	43.002241
3500.868607	813889.396265	43.007245
3501.601642	813896.101898	43.012250
3501.237074	813872.093384	43.017255
3501.418565	813862.809049	43.022260
3501.446504	813857.251112	43.027265
3501.402972	813863.493585	43.032269
3501.545364	813851.097530	43.037274
3501.443297	813825.781190	43.042279
3501.229142	813818.312418	43.047284
3501.270336	813816.844530	43.052289
3501.081479	813815.607470	43.057293
3501.394985	813813.317554	43.062298
3501.339963	813804.946998	43.067303
3501.255018	813796.970838	43.072308
3501.233120	813790.543738	43.077313
3500.979456	813794.773038	43.082317
3501.107490	813801.475917	43.087322
3501.001903	813791.944055	43.092327
3501.250086	813783.038908	43.097332
3501.044608	813787.065815	43.102337
3500.713197	813777.179501	43.107341
3501.324275	813773.381559	43.112346
3500.800679	813778.919696	43.117351
3501.155965	813772.628481	43.122356
3501.223422	813782.458707	43.127361
3500.967102	813776.263103	43.132365
3501.267884	813772.318800	43.137370
3500.958834	813783.279645	43.142375
3501.338641	813783.902342	43.147380
3501.247085	813778.655313	43.152385
3501.176773	813762.395013	43.157389
3501.525464	813749.187042	43.162394
3501.283808	813746.886454	43.167399
3501.215462	813747.676643	43.172404
3501.453671	813749.977847	43.177409
3501.037986	813737.279073	43.182413
3501.191610	813717.281171	43.187418
3500.975961	813734.658137	43.192423
3501.289331	813725.645284	43.197428
3501.279435	813717.072689	43.202433
3501.339031	813720.765899	43.207437
3501.085323	813722.461973	43.212442
3501.304632	813726.714816	43.217447
3501.006419	813702.890148	43.222452
3501.365731	813700.787900	43.227457
3501.219226	813703.149260	43.232461
3501.352091	813694.944054	43.237466
3501.355759	813710.825286	43.242471
3501.328734	813690.173499	43.247476
3501.485962	813663.841627	43.252481
3501.053352	813665.760552	43.257485
3501.350689	813659.088544	43.262490
3501.203581	813674.896003	43.267495
3501.355529	813671.364641	43.272500
3501.041463	813659.136997	43.277505
3500.716798	813653.244259	43.282509
3501.064622	813634.774695	43.287514
3501.324063	813633.077778	43.292519
3501.355485	813637.165183	43.297524
3501.198778	813640.697383	43.302529
3500.911024	813638.793700	43.307533
3501.445054	813640.464091	43.312538
3501.329730	813645.159041	43.317543
3501.023922	813633.027489	43.322548
3501.104049	813614.892019	43.327553
3501.274881	813619.055079	43.332557
3501.358725	813617.093301	43.337562
3501.149462	813619.074761	43.342567
3501.309891	813628.306083	43.347572
3501.453742	813614.740109	43.352577
3501.084144	813609.536403	43.357581
3501.208422	813594.024732	43.362586
3501.093648	813588.878609	43.367591
3501.030308	813588.401369	43.372596
3501.448159	813582.002749	43.377601
3500.995667	813593.083784	43.382605
3501.108563	813588.096942	43.387610
3501.217039	813583.208224	43.392615
3501.240662	813573.168651	43.397620
3501.232422	813561.282752	43.402625
3501.217319	813559.628733	43.407629
3501.495166	813560.462265	43.412634
3501.195060	813567.524631	43.417639
3501.087880	813551.561856	43.422644
3501.534541	813541.748412	43.427649
3501.205550	813537.512664	43.432653
3501.173443	813537.517721	43.437658
3501.496236	813528.892861	43.442663
3501.042148	813536.174207	43.447668
3501.218455	813517.146488	43.452673
3500.876411	813504.045980	43.457677
3501.383248	813499.776985	43.462682
3501.316599	813503.295184	43.467687
3501.227608	813504.283506	43.472692
3501.423038	813495.970823	43.477697
3501.231852	813493.272500	43.482701
3500.975212	813473.727705	43.487706
3501.077017	813479.558089	43.492711
3501.171795	813474.086801	43.497716
3501.074791	813474.491754	43.502721
3501.149725	813485.977718	43.507725
3501.362295	813481.852149	43.512730
3501.207002	813481.681587	43.517735
3501.467685	813461.763573	43.522740
3501.314008	813453.115654	43.527745
3500.936041	813457.656925	43.532749
3501.239306	813449.619637	43.537754
3501.256600	813448.740029	43.542759
3501.016881	813450.433988	43.547764
3501.677442	813456.956552	43.552769
3501.329057	813428.559095	43.557773
3501.503259	813420.736823	43.562778
3501.446114	813434.971805	43.567783
3501.397458	813424.358663	43.572788
3501.223155	813403.631516	43.577793
3501.231813	813396.419724	43.582797
3501.115481	813393.514779	43.587802
3501.620701	813398.600103	43.592807
3501.278403	813393.002192	43.597812
3501.787953	813393.799527	43.602817
3501.067619	813373.157635	43.607821
3501.146373	813363.888623	43.612826
3501.261210	813360.265450	43.617831
3501.133785	813369.054954	43.622836
3501.639801	813362.057694	43.627841
3501.349923	813351.287257	43.632845
3501.085788	813341.487175	43.637850
3501.163744	813346.054695	43.642855
3500.897172	813342.003935	43.647860
3501.335565	813339.109688	43.652865
3500.989504	813348.030840	43.657869
3501.070665	813353.182492	43.662874
3501.227613	813351.891280	43.667879
3500.849418	813346.396378	43.672884
3501.311119	813316.994823	43.677889
3500.873689	813325.930289	43.682893
3501.423750	813327.013621	43.687898
3501.090957	813331.255600	43.692903
3500.818948	813324.964560	43.697908
3500.930044	813321.829149	43.702913
3501.225753	813331.526962	43.707917
3501.143810	813329.785891	43.712922
3501.180091	813332.898335	43.717927
3500.748395	813309.385354	43.722932
3501.239101	813307.652199	43.727937
3500.748153	813309.093147	43.732941
3500.956362	813297.952435	43.737946
3500.848130	813303.328615	43.742951
3500.508549	813300.166204	43.747956
3500.896500	813310.726594	43.752961
3501.157591	813310.101176	43.757965
3501.129274	813308.644037	43.762970
3501.049413	813311.482326	43.767975
3501.097941	813311.085017	43.772980
3501.169102	813311.756013	43.777985
3500.838584	813321.941495	43.782989
3501.279112	813320.021307	43.787994
3501.261391	813314.859787	43.792999
3501.265820	813309.110159	43.798004
3501.136157	813289.155177	43.803009
3500.917174	813293.964034	43.808013
3500.966109	813281.386583	43.813018
3501.027209	813286.443985	43.818023
3501.267353	813292.740121	43.823028
3501.389574	813289.213193	43.828033
3500.976921	813295.806254	43.833037
3500.986407	813286.937718	43.838042
3501.418722	813287.454820	43.843047
3500.851937	813265.716723	43.848052
3501.267214	813258.343768	43.853057
3501.023758	813257.894658	43.858061
3501.209758	813253.578211	43.863066
3501.107104	813264.410254	43.868071
3500.722591	813261.059965	43.873076
3500.895179	813259.961172	43.878081
3500.946958	813261.804495	43.883085
3501.060293	813255.063383	43.888090
3501.315065	813257.459622	43.893095
3501.218007	813261.469916	43.898100
3501.636168	813243.085647	43.903105
3501.243062	813236.813448	43.908109
3501.223973	813236.134380	43.913114
3501.376828	813243.028860	43.918119
3501.204729	813242.373712	43.923124
3501.340980	813243.131982	43.928129
3501.369862	813225.198279	43.933133
3501.486552	813216.994977	43.938138
3501.273603	813214.982028	43.943143
3500.875495	813208.223373	43.948148
3501.272976	813212.838483	43.953153
3500.802286	813213.106984	43.958157
3501.333607	813207.080014	43.963162
3501.435621	813202.874103	43.968167
3501.165909	813187.617901	43.973172
3501.052975	813185.784192	43.978177
3501.015759	813191.636577	43.983181
3501.165870	813182.161257	43.988186
3501.007462	813185.596536	43.993191
3501.362247	813189.926011	43.998196
3501.586408	813166.115082	44.003201
3501.599479	813164.066784	44.008205
3501.674152	813155.090430	44.013210
3501.263038	813140.245987	44.018215
3501.330870	813126.593400	44.023220
3501.373623	813122.006927	44.028225
3501.514006	813121.497804	44.033229
3501.362045	813133.896870	44.038234
3501.165242	813119.700979	44.043239
3500.811990	813099.293127	44.048244
3501.203086	813086.077137	44.053249
3500.827549	813090.131072	44.058253
3500.861799	813086.812669	44.063258
3501.335776	813097.554860	44.068263
3500.929357	813093.428355	44.073268
3501.437591	813096.856915	44.078273
3501.414929	813113.815655	44.083277
3501.166963	813108.397628	44.088282
3501.379555	813090.239934	44.093287
3501.296663	813074.661922	44.098292
3501.550178	813072.576007	44.103297
3501.465797	813077.461432	44.108301
3501.441585	813059.925332	44.113306
3501.344648	813048.831881	44.118311
3500.905886	813039.448400	44.123316
3501.342220	813048.540003	44.128321
3500.911210	813052.505189	44.133325
3501.263531	813047.772825	44.138330
3501.217671	813051.677805	44.143335
3501.266159	813045.238937	44.148340
3501.699914	813026.266932	44.153345
3501.480116	813023.962656	44.158349
3501.481682	813016.946427	44.163354
3501.445883	813016.464837	44.168359
3501.280419	812997.294080	44.173364
3501.365159	812981.299851	44.178369
3500.755787	812982.661937	44.183373
3501.149531	812984.256995	44.188378
3501.710759	812988.359448	44.193383
3501.108052	812982.509539	44.198388
3501.363296	812962.103564	44.203393
3501.206736	812964.466772	44.208397
3501.261499	812952.472425	44.213402
3501.360100	812956.842110	44.218407
3500.897137	812954.770712	44.223412
3501.328140	812956.165062	44.228417
3501.165309	812961.452623	44.233421
3501.071295	812944.511786	44.238426
3501.103506	812940.901288	44.243431
3500.994895	812940.041290	44.248436
3501.239835	812923.632087	44.253441
3501.204298	812941.860105	44.258445
3501.160014	812932.122460	44.263450
3501.211049	812943.320816	44.268455
3501.368725	812942.321746	44.273460
3501.442928	812923.795422	44.278465
3501.433862	812912.687993	44.283469
3501.463169	812902.646458	44.288474
3501.439212	812909.081713	44.293479
3501.345973	812893.212528	44.298484
3501.219810	812871.501627	44.303489
3500.928782	812882.266329	44.308493
3501.090358	812872.593857	44.313498
3501.142660	812881.258502	44.318503
3501.165144	812884.860560	44.323508
3501.084376	812878.149387	44.328513
3500.907859	812875.838290	44.333517
3501.259396	812875.296140	44.338522
3501.082410	812862.558273	44.343527
3501.262442	812853.565018	44.348532
3501.319149	812841.180365	44.353537
3501.292236	812843.036113	44.358541
3501.179339	812848.998095	44.363546
3501.418719	812847.206659	44.368551
3501.262341	812826.474800	44.373556
3501.214309	812821.609956	44.378561
3501.002334	812818.524798	44.383565
3501.200228	812818.396453	44.388570
3500.956889	812836.072576	44.393575
3500.956031	812826.035634	44.398580
3501.126822	812825.034496	44.403585
3501.180291	812833.114338	44.408589
3501.250654	812816.147459	44.413594
3501.282970	812807.956813	44.418599
3500.905999	812796.516898	44.423604
3501.154089	812785.174148	44.428609
3501.267148	812799.968654	44.433613
3501.537229	812797.100474	44.438618
3500.906530	812800.025103	44.443623
3501.049477	812805.752235	44.448628
3500.985418	812798.843468	44.453633
3500.911508	812785.407193	44.458637
3500.997220	812769.217375	44.463642
3501.033062	812773.207204	44.468647
3501.100686	812768.714034	44.473652
3500.968231	812763.959791	44.478657
3500.755220	812770.814536	44.483661
3500.733944	812771.012797	44.488666
3500.707421	812772.088916	44.493671
3500.566464	812768.602837	44.498676
3500.979495	812768.343412	44.503681
3501.065455	812779.634049	44.508685
3500.907067	812770.791027	44.513690
3501.131142	812771.633075	44.518695
3500.932993	812779.362524	44.523700
3501.024446	812788.410971	44.528705
3501.212374	812793.351497	44.533709
3501.107811	812781.771523	44.538714
3501.296568	812785.055301	44.543719
3501.093000	812780.019842	44.548724
3501.265874	812751.245483	44.553729
3501.250176	812756.900011	44.558733
3501.226670	812754.564951	44.563738
3501.060970	812762.094452	44.568743
3501.369916	812755.809470	44.573748
3501.488554	812744.584332	44.578753
3501.548466	812732.783659	44.583757
3501.173950	812735.668269	44.588762
3501.413087	812733.487042	44.593767
3501.026541	812726.336259	44.598772
3501.273348	812727.174760	44.603777
3501.590364	812716.990504	44.608781
3501.683799	812701.091652	44.613786
3501.219829	812690.542190	44.618791
3501.551638	812694.485803	44.623796
3501.528836	812676.753512	44.628801
3501.029449	812670.594806	44.633805
3501.173536	812661.801796	44.638810
3501.394260	812662.352032	44.643815
3500.991818	812662.512431	44.648820
3501.187866	812662.579273	44.653825
3501.201848	812667.449639	44.658829
3501.404147	812646.271315	44.663834
3501.303227	812635.275205	44.668839
3501.106365	812628.192108	44.673844
3501.590608	812628.018998	44.678849
3501.693876	812629.172303	44.683853
3501.289472	812610.524969	44.688858
3501.281515	812605.068986	44.693863
3501.319169	812600.190575	44.698868
3501.309953	812592.006140	44.703873
3501.216963	812603.617422	44.708877
3501.391329	812584.099926	44.713882
3501.140873	812587.160113	44.718887
3501.128413	812572.349454	44.723892
3501.145317	812573.126464	44.728897
3501.328290	812578.360289	44.733901
3501.178354	812569.223306	44.738906
3501.394187	812560.321487	44.743911
3500.733385	812555.259870	44.748916
3501.049422	812548.778670	44.753921
3501.519185	812551.336480	44.758925
3501.016838	812543.229068	44.763930
3500.763212	812554.378292	44.768935
3500.795120	812558.368872	44.773940
3501.268986	812546.600591	44.778945
3501.409939	812553.692596	44.783949
3501.317262	812551.563177	44.788954
3501.485470	812525.127361	44.793959
3501.148518	812518.455850	44.798964
3501.267926	812511.810444	44.803969
3501.325717	812519.987466	44.808973
3501.292884	812517.946133	44.813978
3501.253686	812517.270131	44.818983
3501.336320	812512.482074	44.823988
3501.082264	812488.645882	44.828993
3501.113357	812485.522562	44.833997
3501.189813	812486.095367	44.839002
3501.235810	812488.134728	44.844007
3501.203110	812494.571774	44.849012
3501.464270	812480.692657	44.854017
3501.363290	812476.810353	44.859021
3501.406936	812460.821223	44.864026
3501.355884	812461.121602	44.869031
3501.176260	812458.031208	44.874036
3501.299453	812453.431672	44.879041
3501.176383	812442.146325	44.884045
3501.334318	812431.011939	44.889050
3501.466196	812432.648077	44.894055
3501.148517	812432.892683	44.899060
3501.398778	812431.196884	44.904065
3501.263266	812423.811604	44.909069
3501.272340	812400.031397	44.914074
3501.505511	812392.296083	44.919079
3501.245104	812391.654647	44.924084
3501.460935	812383.629670	44.929089
3501.129365	812382.804448	44.934093
3501.217404	812369.829240	44.939098
3501.380576	812363.956476	44.944103
3501.127021	812360.975046	44.949108
3501.682279	812361.278105	44.954113
3500.958464	812363.340391	44.959117
3501.486727	812355.558903	44.964122
3501.362201	812343.688876	44.969127
3500.912496	812343.954123	44.974132
3501.470502	812326.519872	44.979137
3501.221835	812334.745042	44.984141
3501.242336	812333.572410	44.989146
3501.076460	812330.089982	44.994151
3501.401535	812322.145305	44.999156
3501.185066	812304.442237	45.004161
3501.250926	812309.597139	45.009165
3501.065919	812300.660158	45.014170
3501.315929	812303.837159	45.019175
3500.859128	812306.929737	45.024180
3501.373877	812305.192559	45.029185
3500.966826	812302.332552	45.034189
3501.046085	812281.562057	45.039194
3500.853065	812272.041550	45.044199
3500.897704	812273.301543	45.049204
3500.896688	812270.572961	45.054209
3500.857732	812270.286720	45.059213
3500.716078	812276.935933	45.064218
3501.246656	812279.386894	45.069223
3501.043885	812291.990475	45.074228
3501.630892	812274.259178	45.079233
3501.131864	812286.616712	45.084237
3500.987262	812283.423301	45.089242
3501.500308	812284.220244	45.094247
3501.191300	812268.870490	45.099252
3501.409622	812252.366242	45.104257
3501.118710	812251.534646	45.109261
3501.163308	812247.629443	45.114266
3501.309622	812244.000708	45.119271
3500.853689	812250.601621	45.124276
3501.237680	812246.350993	45.129281
3501.310892	812240.297264	45.134285
3501.191377	812223.650838	45.139290
3501.306704	812217.298131	45.144295
3501.006118	812220.951073	45.149300
3501.480411	812215.321908	45.154305
3501.006160	812225.336714	45.159309
3501.038764	812219.191855	45.164314
3501.349342	812194.778996	45.169319
3501.253809	812186.997357	45.174324
3501.430436	812181.317236	45.179329
3501.076951	812185.855588	45.184333
3501.332490	812193.709749	45.189338
3501.298732	812193.520149	45.194343
3501.324900	812172.270305	45.199348
3501.091819	812154.569411	45.204353
3501.269078	812148.499329	45.209357
3501.559257	812152.644710	45.214362
3501.226031	812155.133294	45.219367
3501.342234	812147.903257	45.224372
3501.519082	812126.044952	45.229377
3501.293985	812127.347140	45.234381
3500.996519	812123.885167	45.239386
3501.689095	812125.823572	45.244391
3501.687987	812120.658473	45.249396
3501.682054	812095.417579	45.254401
3501.446762	812092.628083	45.259405
3501.484805	812087.846674	45.264410
3501.236900	812075.313211	45.269415
3501.248137	812065.565542	45.274420
3501.582549	812051.186730	45.279425
3501.330531	812059.120403	45.284429
3501.291042	812058.152017	45.289434
3501.625264	812041.531639	45.294439
3501.085233	812027.484387	45.299444
3501.343959	812017.600496	45.304449
3501.310908	812029.983149	45.309453
3501.148625	812027.182211	45.314458
3501.351687	812014.967972	45.319463
3500.967126	812012.591616	45.324468
3501.260789	811994.905391	45.329473
3501.172434	811993.749713	45.334477
3500.936736	812002.265670	45.339482
3501.404400	812010.769125	45.344487
3501.077063	812005.849849	45.349492
3501.237600	812007.871462	45.354497
3501.347933	811995.769143	45.359501
3501.374044	811979.878991	45.364506
3501.212005	811976.590688	45.369511
3501.163136	811978.645045	45.374516
3501.349660	811980.272761	45.379521
3501.038891	811973.694034	45.384525
3501.134221	811957.500622	45.389530
3501.062701	811939.286560	45.394535
3501.211239	811941.699916	45.399540
3501.128464	811944.246892	45.404545
3501.218527	811941.211545	45.409549
3501.201716	811943.845671	45.414554
3501.497151	811941.850297	45.419559
3501.187743	811934.296701	45.424564
3501.206634	811907.491785	45.429569
3501.235775	811910.021280	45.434573
3501.199394	811909.832081	45.439578
3501.126433	811911.110530	45.444583
3501.214886	811912.168823	45.449588
3501.581890	811899.051574	45.454593
3501.124094	811886.648007	45.459597
3501.039870	811884.224652	45.464602
3501.132572	811871.540075	45.469607
3500.849710	811879.088946	45.474612
3501.012106	811872.143758	45.479617
3501.105697	811880.413480	45.484621
3501.046148	811878.473577	45.489626
3500.915778	811875.667582	45.494631
3501.071635	811887.923523	45.499636
3501.320074	811870.633868	45.504641
3501.034288	811884.030942	45.509645
3501.297500	811863.425236	45.514650
3501.200793	811860.613972	45.519655
3501.169965	811850.190306	45.524660
3501.338807	811853.087837	45.529665
3501.417933	811854.439986	45.534669
3501.123919	811849.320452	45.539674
3501.511135	811833.373482	45.544679
3501.073359	811816.775728	45.549684
3501.350097	811811.956796	45.554689
3501.387060	811813.705399	45.559693
3501.043196	811816.488167	45.564698
3501.528669	811805.983719	45.569703
3501.420848	811797.423809	45.574708
3501.095712	811783.732271	45.579713
3501.107941	811791.235117	45.584717
3501.105377	811784.608012	45.589722
3501.355194	811786.420812	45.594727
3501.710274	811787.534911	45.599732
3501.616473	811760.552057	45.604737
3501.503013	811754.527042	45.609741
3501.244894	811750.181530	45.614746
3501.613640	811741.449582	45.619751
3501.321640	811722.684570	45.624756
3501.213668	811717.048520	45.629761
3501.125318	811713.261234	45.634765
3501.155337	811713.159114	45.639770
3501.371342	811717.901171	45.644775
3501.125816	811706.731109	45.649780
3501.272645	811684.583569	45.654785
3501.481166	811691.178660	45.659789
3501.205794	811692.488794	45.664794
3501.220672	811684.201946	45.669799
3501.262539	811687.509265	45.674804
3501.456146	811665.354345	45.679809
3501.007229	811659.674075	45.684813
3501.002148	811648.466322	45.689818
3500.883469	811655.502463	45.694823
3500.687998	811659.626626	45.699828
3500.836642	811656.581985	45.704833
3500.697643	811643.933169	45.709837
3500.760918	811596.554607	45.714842
3500.584851	811499.796846	45.719847
3500.657479	811350.657196	45.724852
3500.869608	811148.076799	45.729857
3500.429882	810910.694954	45.734861
3499.761921	810612.218874	45.739866
3499.529237	810262.382407	45.744871
3498.942278	809877.971855	45.749876
3498.990305	809433.573747	45.754881
3498.473442	808932.580810	45.759885
3497.947473	808405.220324	45.764890
3497.883799	807817.912257	45.769895
3497.133825	807187.790675	45.774900
3496.740438	806499.316470	45.779905
3495.848380	805770.457386	45.784909
3495.234336	804994.394808	45.789914
3494.409263	804168.309483	45.794919
3493.408875	803302.960772	45.799924
3493.065539	802386.782685	45.804929
3492.013849	801422.993489	45.809933
3491.091337	800433.409645	45.814938
3490.368211	799374.650424	45.819943
3489.134774	798279.610484	45.824948
3488.269513	797123.126413	45.829953
3487.161143	795944.099537	45.834957
3486.060881	794700.799573	45.839962
3485.466153	793422.044726	45.844967
3483.885753	792089.179742	45.849972
3482.806858	790720.176499	45.854977
3481.570641	789307.438645	45.859981
3480.223864	787844.866439	45.864986
3478.918158	786343.020706	45.869991
3477.193148	784795.194750	45.874996
3475.890433	783204.407685	45.880001
3474.518563	781585.884381	45.885005
3472.989425	779911.314518	45.890010
3471.729359	778195.139322	45.895015
3469.687412	776448.419283	45.900020
3468.159822	774653.776527	45.905025
3466.537109	772834.409037	45.910029
3464.686460	770966.635495	45.915034
3462.916834	769059.248111	45.920039
3460.996102	767115.883222	45.925044
3458.785905	765151.061392	45.930049
3456.772140	763145.692575	45.935053
3454.962957	761107.059931	45.940058
3453.026252	759037.743381	45.945063
3450.678759	756932.702135	45.950068
3448.876663	754775.243472	45.955073
3446.511493	752606.106416	45.960077
3444.708829	750400.124292	45.965082
3442.666325	748161.770456	45.970087
3440.127355	745888.696348	45.975092
3438.186156	743577.256096	45.980097
3435.630728	741243.807339	45.985101
3433.403765	738884.491335	45.990106
3431.195524	736489.579685	45.995111
3428.733073	734067.513461	46.000116
3426.632136	731611.123618	46.005121
3424.066554	729130.769343	46.010125
3421.724693	726607.674029	46.015130
3419.084019	724070.655958	46.020135
3416.550327	721503.300823	46.025140
3413.738984	718903.322323	46.030145
3411.374408	716274.976744	46.035149
3408.826789	713653.725777	46.040154
3406.592897	710979.189271	46.045159
3403.744693	708279.604268	46.050164
3401.125258	705552.494092	46.055169
3398.484153	702798.964683	46.060173
3395.665320	700022.732670	46.065178
3392.921424	697221.711181	46.070183
3390.204981	694393.015337	46.075188
3387.584345	691545.830570	46.080193
3384.825563	688666.696706	46.085197
3381.628418	685775.124762	46.090202
3379.464907	682852.771195	46.095207
3376.082420	679910.286369	46.100212
3373.371952	676948.254805	46.105217
3370.518568	673965.599613	46.110221
3367.581534	670960.857314	46.115226
3364.825481	667919.261332	46.120231
3361.976086	664866.228531	46.125236
3358.694419	661796.586684	46.130241
3355.260158	658717.894975	46.135245
3352.094992	655600.824293	46.140250
3349.542842	652472.820266	46.145255
3346.205608	649334.298563	46.150260
3342.661185	646176.299485	46.155265
3339.696914	642996.197426	46.160269
3336.999978	639818.704835	46.165274
3333.961894	636608.422482	46.170279
3330.360399	633375.887182	46.175284
3327.409890	630118.351150	46.180289
3323.776781	626855.176753	46.185293
3320.760946	623590.709301	46.190298
3317.530937	620293.717267	46.195303
3314.162535	616989.051400	46.200308
3310.666880	613673.663574	46.205313
3307.693447	610342.651862	46.210317
3304.285706	606998.562014	46.215322
3300.761194	603633.286534	46.220327
3297.138018	600265.632116	46.225332
3293.808796	596877.822045	46.230337
3290.453123	593475.908087	46.235341
3287.150386	590087.079488	46.240346
3284.090444	586661.615745	46.245351
3280.187380	583241.171780	46.250356
3277.188525	579796.104414	46.255361
3273.631820	576339.923796	46.260365
3269.182449	572877.149243	46.265370
3266.073586	569396.996930	46.270375
3262.705896	565929.285400	46.275380
3259.434399	562439.629546	46.280385
3255.928167	558957.914420	46.285389
3252.011486	555441.069626	46.290394
3248.205656	551933.229640	46.295399
3245.036073	548421.359433	46.300404
3241.541587	544892.691732	46.305409
3237.822799	541359.031277	46.310413
3234.349441	537829.622392	46.315418
3230.733241	534283.298674	46.320423
3226.766423	530736.807497	46.325428
3223.047771	527171.633347	46.330433
3219.716833	523601.857623	46.335437
3216.078344	520047.905840	46.340442
3212.770769	516459.801138	46.345447
3209.041378	512882.216997	46.350452
3204.943526	509292.269457	46.355457
3201.563106	505704.874477	46.360461
3197.937951	502108.087104	46.365466
3193.977566	498499.706113	46.370471
3190.694303	494903.707485	46.375476
3186.780239	491286.990988	46.380481
3182.793250	487684.669728	46.385485
3179.324937	484060.805924	46.390490
3175.655475	480436.428892	46.395495
3171.694666	476810.503503	46.400500
3167.935286	473184.177389	46.405505
3164.182644	469558.605640	46.410509
3160.802148	465924.387667	46.415514
3156.830454	462288.206578	46.420519
3152.933672	458657.761326	46.425524
3148.917407	455028.442516	46.430529
3145.281061	451381.861489	46.435533
3141.371207	447744.398335	46.440538
3137.543321	444095.051198	46.445543
3133.590902	440473.515313	46.450548
3130.058255	436837.789388	46.455553
3126.297160	433194.363086	46.460557
3122.709797	429557.827155	46.465562
3119.145140	425912.762122	46.470567
3114.924159	422278.596752	46.475572
3111.117972	418640.122501	46.480577
3107.195396	414994.896829	46.485581
3103.275294	411356.351153	46.490586
3099.681644	407713.949374	46.495591
3095.766029	404080.944415	46.500596
3092.123315	400435.185395	46.505601
3088.211800	396802.394005	46.510605
3084.096277	393172.476673	46.515610
3079.857053	389540.915742	46.520615
3076.381063	385916.799821	46.525620
3072.373757	382291.053163	46.530625
3068.734323	378666.543080	46.535629
3064.208797	375047.364179	46.540634
3060.897146	371428.655079	46.545639
3057.077578	367826.118290	46.550644
3053.036426	364211.116755	46.555649
3049.055117	360603.129827	46.560653
3045.227488	357007.113004	46.565658
3041.321289	353395.057306	46.570663
3037.158009	349801.492535	46.575668
3033.576247	346215.780040	46.580673
3029.642606	342630.706285	46.585677
3025.513980	339043.690078	46.590682
3021.668295	335455.862794	46.595687
3017.579467	331890.080904	46.600692
3013.908384	328309.198561	46.605697
3009.652790	324752.478060	46.610701
3005.495191	321183.094456	46.615706
3001.738155	317632.048109	46.620711
2997.681729	314085.749552	46.625716
2993.779240	310550.806939	46.630721
2989.821600	307012.302934	46.635725
2985.168371	303495.517779	46.640730
2981.531158	299985.080770	46.645735
2977.263037	296475.076265	46.650740
2973.375304	292986.153296	46.655745
2969.519539	289500.663102	46.660749
2965.318218	286022.647074	46.665754
2961.526520	282537.665347	46.670759
2956.916363	279078.177103	46.675764
2953.285045	275624.971973	46.680769
2949.318378	272178.037263	46.685773
2944.864968	268743.162120	46.690778
2940.946540	265310.980093	46.695783
2936.861064	261899.589338	46.700788
2932.583081	258505.058398	46.705793
2928.544224	255100.336600	46.710797
2924.509117	251725.860029	46.715802
2920.543305	248339.379596	46.720807
2915.991364	244983.614232	46.725812
2911.833803	241636.340538	46.730817
2907.884057	238302.232517	46.735821
2903.425532	234976.598184	46.740826
2899.656728	231660.023408	46.745831
2894.826803	228357.630219	46.750836
2890.801586	225065.926693	46.755841
2886.822150	221808.344443	46.760845
2882.550441	218556.521331	46.765850
2878.579788	215314.167752	46.770855
2874.143941	212088.211792	46.775860
2869.722211	208866.565249	46.780865
2865.369758	205658.192222	46.785869
2861.788090	202478.372874	46.790874
2857.511761	199307.274858	46.795879
2853.332536	196151.224678	46.800884
2849.251625	193002.563659	46.805889
2844.959643	189874.996656	46.810893
2840.341409	186762.996288	46.815898
2836.303915	183652.014314	46.820903
2831.963735	180570.409063	46.825908
2827.921106	177493.774748	46.830913
2823.634607	174435.111431	46.835917
2819.640529	171418.629216	46.840922
2815.661947	168299.180243	46.845927
2810.680162	165269.800630	46.850932
2806.396639	162269.072213	46.855937
2802.587665	159300.431055	46.860941
2798.560416	156347.353004	46.865946
2794.928251	153386.787518	46.870951
2790.313003	150457.975155	46.875956
2786.318801	147532.747193	46.880961
2781.878106	144629.662999	46.885965
2777.749965	141738.783445	46.890970
2774.092420	138859.858621	46.895975
2769.336865	136002.615608	46.900980
2764.995939	133157.024157	46.905985
2761.261361	130327.662591	46.910989
2757.038475	127516.294506	46.915994
2752.937403	124707.818157	46.920999
2748.671117	121931.610946	46.926004
2744.549225	119159.238540	46.931009
2740.318018	116404.796408	46.936013
2735.840034	113656.990801	46.941018
2731.776657	110937.209015	46.946023
2727.879625	108239.945541	46.951028
2723.633046	105543.466491	46.956033
2719.340620	102862.410571	46.961037
2715.265353	100208.367631	46.966042
2711.336038	97568.879192	46.971047
2707.358922	94926.947638	46.976052
2703.309977	92309.762348	46.981057
2699.239891	89702.066410	46.986061
2694.961058	87113.762835	46.991066
2690.503525	84534.365603	46.996071
2686.375216	81982.177897	47.001076
2682.509935	79439.945636	47.006081
2678.253432	76906.362822	47.011085
2673.623984	74402.331100	47.016090
2669.570632	71899.584522	47.021095
2665.802303	69437.532126	47.026100
2661.356409	66961.192616	47.031105
2657.045181	64528.866210	47.036109
2652.533311	62103.316648	47.041114
2648.760962	59696.385994	47.046119
2644.229796	57300.419421	47.051124
2640.021393	54927.004732	47.056129
2635.721505	52585.535516	47.061133
2631.300162	50253.364170	47.066138
2627.393682	47936.816841	47.071143
2622.974656	45637.936261	47.076148
2618.446045	43366.372338	47.081153
2613.845018	41099.090259	47.086157
2609.557756	38861.810560	47.091162
2605.487625	36646.934508	47.096167
2601.152940	34449.386116	47.101172
2596.331113	32277.995076	47.106177
2592.122455	30122.766882	47.111181
2587.600049	28007.677324	47.116186
2583.263687	25899.765549	47.121191
2578.673333	23826.388190	47.126196
2574.071963	21760.556129	47.131201
2569.766210	19734.786186	47.136205
2564.733294	17742.565101	47.141210
2559.959614	15764.968702	47.146215
2554.894895	13826.571189	47.151220
2549.963058	11919.964059	47.156225
2545.271619	10055.170265	47.161229
2539.039378	8230.710463	47.166234
2533.562464	6453.289003	47.171239
2526.411799	4763.401804	47.176244
2515.521062	3223.184906	47.181249
2502.199671	1832.826995	47.186253
2488.066913	594.388691	47.191258
2455.015569	32.993416	47.196263
2405.913758	207.334501	47.201268
2383.280033	203.544674	47.206273
2378.597118	201.040671	47.211277
2385.135456	221.630290	47.216282
2394.960419	229.388781	47.221287
2404.884490	225.672199	47.226292
2411.124295	222.206110	47.231297
2413.747975	219.296235	47.236301
2412.437606	222.873963	47.241306
2410.164936	225.634086	47.246311
2407.026754	208.622476	47.251316
2403.288218	211.305022	47.256321
2399.749025	205.363290	47.261325
2396.448143	206.629559	47.266330
2393.910246	195.677802	47.271335
2390.928046	201.510313	47.276340
2387.797740	206.644631	47.281345
2385.025152	198.086680	47.286349
2382.129964	203.813828	47.291354
2379.323683	189.844597	47.296359
2376.157741	192.776106	47.301364
2372.982534	192.621123	47.306369
2370.117493	183.527133	47.311373
2366.655506	193.576216	47.316378
2363.189676	180.162615	47.321383
2359.869234	184.323733	47.326388
2356.505569	184.732933	47.331393
2353.613061	184.122426	47.336397
2350.324876	186.576337	47.341402
2347.151441	185.370679	47.346407
2343.862873	186.182602	47.351412
2340.221043	189.501793	47.356417
2336.865913	190.814532	47.361421
2333.799614	192.774973	47.366426
2330.706285	183.770496	47.371431
2327.551471	192.778076	47.376436
2323.931864	194.739658	47.381441
2320.299464	192.890776	47.386445
2316.917533	198.940868	47.391450
2313.091034	190.541498	47.396455
2310.042592	196.526762	47.401460
2307.136242	190.985955	47.406465
2304.085001	187.109867	47.411469
2300.293621	194.866070	47.416474
2296.530106	183.479652	47.421479
2292.921302	183.101453	47.426484
2289.421139	200.787787	47.431489
2286.227854	184.648611	47.436493
2282.536239	193.132719	47.441498
2279.937483	183.323194	47.446503
2276.885969	193.779495	47.451508
2273.010540	191.791475	47.456513
2269.127923	189.127512	47.461517
2265.460819	183.889246	47.466522
2262.514320	175.662285	47.471527
2259.049034	187.499491	47.476532
2255.616091	189.871668	47.481537
2252.084931	182.672686	47.486541
2248.241274	196.568662	47.491546
2244.708689	185.086023	47.496551
2241.678760	178.966603	47.501556
2238.032807	193.973805	47.506561
2235.009217	190.118723	47.511565
2231.518451	202.165582	47.516570
2228.316869	192.621232	47.521575
2224.740183	187.992116	47.526580
2221.408252	195.951714	47.531585
2218.175270	183.561639	47.536589
2214.396263	178.695255	47.541594
2210.843971	178.235473	47.546599
2206.873327	188.139537	47.551604
2203.611592	186.840165	47.556609
2200.713798	182.240888	47.561613
2196.568321	182.987600	47.566618
2193.486248	181.002038	47.571623
2190.147222	176.788187	47.576628
2186.944186	174.419742	47.581633
2183.611299	178.519575	47.586637
2179.227431	177.813410	47.591642
2175.587308	181.100744	47.596647
2172.632040	180.727904	47.601652
2169.090445	190.182023	47.606657
2165.766272	187.380103	47.611661
2161.882784	190.325855	47.616666
2159.352421	182.403990	47.621671
2155.488277	188.096118	47.626676
2151.756428	185.234598	47.631681
2148.480757	178.350036	47.636685
2144.550787	186.406383	47.641690
2141.289171	178.086393	47.646695
2137.875138	176.750758	47.651700
2134.101635	185.817210	47.656705
2131.042008	186.700945	47.661709
2127.087414	183.494622	47.666714
2124.071297	174.319951	47.671719
2120.651861	182.169868	47.676724
2116.573478	184.513355	47.681729
2113.761176	174.762613	47.686733
2110.040728	177.002639	47.691738
2106.620187	171.466422	47.696743
2103.066056	177.378985	47.701748
2099.500736	176.734610	47.706753
2096.238660	177.643703	47.711757
2092.554844	181.374512	47.716762
2089.172660	171.659162	47.721767
2085.775365	169.726120	47.726772
2082.155449	178.692618	47.731777
2078.514129	168.587535	47.736781
2074.685509	175.947810	47.741786
2071.514176	181.256302	47.746791
2068.032363	174.631824	47.751796
2064.328424	179.257999	47.756801
2061.312115	170.934462	47.761805
2057.957454	180.428958	47.766810
2054.646098	177.552302	47.771815
2051.099014	178.031425	47.776820
2047.392551	180.487590	47.781825
2043.799215	177.908169	47.786829
2040.298100	173.074305	47.791834
2036.829052	173.148903	47.796839
2033.032214	176.520915	47.801844
2029.582399	181.711636	47.806849
2026.768355	171.233509	47.811853
2023.072211	182.505752	47.816858
2019.369701	177.595836	47.821863
2015.924424	176.752365	47.826868
2012.524504	175.895470	47.831873
2008.843724	174.269412	47.836877
2005.180806	176.487815	47.841882
2001.885583	171.586946	47.846887
1998.737994	179.675938	47.851892
1995.025700	178.709735	47.856897
1991.311342	177.667924	47.861901
1987.938408	183.431941	47.866906
1984.333665	175.763672	47.871911
1981.047663	169.099098	47.876916
1977.177186	167.021828	47.881921
1974.067540	166.692184	47.886925
1970.400892	168.898526	47.891930
1967.025670	173.400524	47.896935
1963.503695	165.140331	47.901940
1959.862936	174.866283	47.906945
1956.633593	173.938420	47.911949
1952.772387	169.372916	47.916954
1949.536458	164.067307	47.921959
1946.057477	169.626455	47.926964
1942.726632	165.873336	47.931969
1939.237636	163.521245	47.936973
1935.426161	169.746213	47.941978
1931.911910	163.550825	47.946983
1928.405384	163.685109	47.951988
1925.167786	168.959710	47.956993
1921.710741	159.170724	47.961997
1918.126230	173.073666	47.967002
1914.791838	159.959258	47.972007
1910.966295	159.672054	47.977012
1907.287392	170.799247	47.982017
1903.893071	170.444566	47.987021
1900.762504	168.178772	47.992026
1897.224083	165.119397	47.997031
1893.437994	163.231442	48.002036
1889.843140	170.615301	48.007041
1886.848221	165.610531	48.012045
1882.748513	156.292303	48.017050
1879.297325	160.866324	48.022055
1876.297040	159.092696	48.027060
1872.977582	171.138116	48.032065
1869.349680	162.578153	48.037069
1865.548557	173.563128	48.042074
1861.795157	169.366780	48.047079
1858.779675	169.031926	48.052084
1854.810834	166.735971	48.057089
1851.691376	157.128312	48.062093
1848.184912	162.388057	48.067098
1844.745311	164.400716	48.072103
1841.156561	153.430113	48.077108
1837.525620	162.433196	48.082113
1834.000614	163.237976	48.087117
1830.434001	164.223280	48.092122
1826.944153	163.371029	48.097127
1823.541404	159.926607	48.102132
1820.279622	162.202522	48.107137
1816.641092	162.417613	48.112141
1813.155085	159.967020	48.117146
1809.593454	159.053239	48.122151
1806.289709	157.782718	48.127156
1802.545215	160.393614	48.132161
1799.027157	163.623994	48.137165
1795.695737	160.443675	48.142170
1792.042654	162.464449	48.147175
1789.200391	155.407795	48.152180
1785.295563	160.622329	48.157185
1781.839938	146.935320	48.162189
1777.912712	156.952922	48.167194
1774.397522	153.965892	48.172199
1771.285223	146.704727	48.177204
1767.780746	151.087794	48.182209
1764.295445	151.870565	48.187213
1760.875910	161.071543	48.192218
1757.014685	151.124415	48.197223
1753.333813	152.485142	48.202228
1750.124298	155.860244	48.207233
1746.667413	159.701180	48.212237
1742.992309	157.678851	48.217242
1739.444583	159.891968	48.222247
1736.502628	166.202387	48.227252
1732.727699	162.468220	48.232257
1729.039596	165.718906	48.237261
1725.721481	166.709650	48.242266
1721.940833	166.573681	48.247271
1718.637214	161.304060	48.252276
1714.795385	156.099689	48.257281
1711.622323	161.753398	48.262285
1708.015186	165.687467	48.267290
1704.761258	166.212577	48.272295
1701.396513	158.652409	48.277300
1697.453886	163.945657	48.282305
1694.369931	159.831274	48.287309
1690.645584	163.774201	48.292314
1687.027168	159.392279	48.297319
1684.076489	155.617722	48.302324
1680.409887	164.310044	48.307329
1676.969830	149.332957	48.312333
1673.175885	157.206789	48.317338
1669.377491	152.043099	48.322343
1665.725588	155.218534	48.327348
1662.526105	159.807009	48.332353
1659.023612	155.618935	48.337357
1655.820621	153.146251	48.342362
1652.057132	153.659376	48.347367
1648.788417	157.799932	48.352372
1645.222423	152.995360	48.357377
1641.736811	154.566018	48.362381
1638.319306	152.867254	48.367386
1634.560740	151.519273	48.372391
1631.146351	153.774833	48.377396
1627.085272	157.618617	48.382401
1624.475960	156.378678	48.387405
1620.616583	154.239699	48.392410
1616.957363	156.872114	48.397415
1613.812059	149.334589	48.402420
1609.785412	154.637851	48.407425
1606.662886	152.374059	48.412429
1602.992220	155.457537	48.417434
1599.437975	146.019275	48.422439
1596.360770	149.889417	48.427444
1592.469657	152.994746	48.432449
1588.910975	146.300238	48.437453
1585.426720	152.651271	48.442458
1582.320163	143.832666	48.447463
1578.636933	153.432474	48.452468
1575.047382	153.579871	48.457473
1572.052146	151.672666	48.462477
1568.383820	161.238509	48.467482
1564.582624	152.073036	48.472487
1561.312733	149.614020	48.477492
1557.475114	147.810192	48.482497
1553.983474	153.111995	48.487501
1550.390368	155.161428	48.492506
1546.854929	153.148952	48.497511
1543.707505	154.122527	48.502516
1539.703564	153.471068	48.507521
1536.802730	143.247172	48.512525
1532.983321	150.900396	48.517530
1529.636875	154.641852	48.522535
1526.686396	141.499176	48.527540
1522.796391	145.414299	48.532545
1519.269522	156.603211	48.537549
1515.509673	143.071516	48.542554
1511.911247	151.031853	48.547559
1508.537121	142.922728	48.552564
1504.773903	148.191119	48.557569
1501.394771	142.110805	48.562573
1497.548084	148.540739	48.567578
1494.361268	152.390100	48.572583
1491.374930	154.458478	48.577588
1487.601313	158.662290	48.582593
1484.042698	147.627020	48.587597
1481.179118	149.619237	48.592602
1477.356894	149.806252	48.597607
1473.705559	148.602905	48.602612
1470.063044	154.096032	48.607617
1466.400518	143.538959	48.612621
1462.529329	149.251383	48.617626
1459.331651	147.796692	48.622631
1456.461452	139.064531	48.627636
1452.486914	146.938219	48.632641
1449.012565	144.514410	48.637645
1445.611971	145.992728	48.642650
1442.343302	149.146216	48.647655
1438.562582	141.667092	48.652660
1434.941183	148.953984	48.657665
1431.671307	142.321906	48.662669
1428.204247	143.304419	48.667674
1424.665774	142.431447	48.672679
1421.028693	140.504533	48.677684
1417.135063	147.837207	48.682689
1413.877310	143.019282	48.687693
1410.354854	143.017027	48.692698
1406.801061	149.189166	48.697703
1403.586558	139.447869	48.702708
1400.061501	147.589746	48.707713
1396.640904	150.052002	48.712717
1393.104121	150.333577	48.717722
1389.465755	146.894560	48.722727
1386.131669	143.496503	48.727732
1382.616100	143.192615	48.732737
1379.080072	141.145492	48.737741
1375.631109	151.338289	48.742746
1371.943199	147.350199	48.747751
1368.682357	148.835140	48.752756
1365.005996	144.465585	48.757761
1361.537339	142.661030	48.762765
1357.842878	145.795771	48.767770
1354.320711	153.168399	48.772775
1350.960351	145.117296	48.777780
1347.193425	156.160327	48.782785
1343.756284	146.362151	48.787789
1340.395601	143.189742	48.792794
1337.252909	152.613251	48.797799
1333.970863	150.937684	48.802804
1330.155919	152.354350	48.807809
1326.612735	143.082161	48.812813
1322.816448	149.361890	48.817818
1318.993306	154.623906	48.822823
1315.766240	148.114886	48.827828
1312.333718	147.835989	48.832833
1308.833323	155.546917	48.837837
1305.404174	144.431350	48.842842
1302.105468	149.873873	48.847847
1298.685851	135.469596	48.852852
1294.649286	146.013831	48.857857
1291.253042	139.104190	48.862861
1287.781316	142.457195	48.867866
1284.387173	144.099075	48.872871
1281.531052	135.820369	48.877876
1277.075718	140.589725	48.882881
1273.960988	134.885738	48.887885
1270.573314	134.843451	48.892890
1266.987355	138.448468	48.897895
1263.580620	133.998782	48.902900
1260.031447	137.696121	48.907905
1256.474028	135.551151	48.912909
1252.890933	139.532221	48.917914
1248.794309	138.968159	48.922919
1245.996244	133.894833	48.927924
1242.678623	135.882261	48.932929
1238.581110	137.501388	48.937933
1235.561731	143.928445	48.942938
1231.846520	141.248187	48.947943
1228.699443	135.970070	48.952948
1224.948117	145.745155	48.957953
1221.590837	140.069666	48.962957
1218.000026	142.992071	48.967962
1214.331094	142.088978	48.972967
1211.019490	143.854006	48.977972
1207.175634	140.716160	48.982977
1203.659570	135.837512	48.987981
1200.153685	127.559319	48.992986
1197.056602	140.702709	48.997991
1193.271842	129.557451	49.002996
1189.561299	138.497234	49.008001
1186.482108	133.012348	49.013005
1182.999616	131.637144	49.018010
1179.226755	133.047277	49.023015
1175.889827	131.332902	49.028020
1172.187007	144.450906	49.033025
1168.669583	128.382014	49.038029
1165.707265	136.271334	49.043034
1161.852819	136.583742	49.048039
1158.233362	136.293036	49.053044
1154.725245	140.939460	49.058049
1151.306972	136.953543	49.063053
1148.274369	139.152650	49.068058
1144.248034	131.674150	49.073063
1141.063346	129.629063	49.078068
1137.319142	136.989053	49.083073
1133.663823	135.049288	49.088077
1130.353960	139.819708	49.093082
1126.544082	142.099383	49.098087
1123.353614	139.216790	49.103092
1119.749403	138.278290	49.108097
1116.312252	137.395896	49.113101
1112.974406	143.882336	49.118106
1109.081753	131.959888	49.123111
1105.901792	143.565998	49.128116
1102.193972	142.881013	49.133121
1098.668623	142.047235	49.138125
1095.199637	139.948595	49.143130
1091.425182	140.008055	49.148135
1088.635410	139.040134	49.153140
1084.693417	143.874736	49.158145
1081.301126	132.984467	49.163149
1077.857856	144.337573	49.168154
1074.313992	147.284317	49.173159
1071.017234	133.803736	49.178164
1067.172982	146.633858	49.183169
1063.887732	137.118920	49.188173
1060.363403	143.334009	49.193178
1056.700861	134.858934	49.198183
1053.310070	138.727702	49.203188
1049.612969	142.242625	49.208193
1046.353829	132.846998	49.213197
1042.804588	137.718201	49.218202
1038.939584	135.732208	49.223207
1035.476451	128.269988	49.228212
1032.133446	143.827951	49.233217
1028.811082	127.272999	49.238221
1025.309063	136.237132	49.243226
1021.303121	137.683819	49.248231
1018.294957	126.347452	49.253236
1015.009618	130.234522	49.258241
1011.309333	132.446459	49.263245
1007.775723	131.000228	49.268250
1004.202548	138.064558	49.273255
1000.557334	125.423205	49.278260
996.609774	141.771873	49.283265
993.533021	129.025696	49.288269
990.748128	136.071010	49.293274
987.339717	138.553639	49.298279
983.348337	129.620713	49.303284
979.341419	135.098283	49.308289
976.268761	122.019276	49.313293
972.512593	136.483978	49.318298
968.875174	129.226250	49.323303
965.690200	129.342161	49.328308
962.283328	133.466581	49.333313
958.666690	133.744998	49.338317
955.145538	132.929602	49.343322
951.430655	128.563092	49.348327
948.391652	132.247093	49.353332
944.708442	140.246181	49.358337
941.235322	131.817433	49.363341
937.739063	131.839723	49.368346
934.012498	138.108663	49.373351
930.437374	123.630844	49.378356
926.713128	138.033613	49.383361
923.304831	129.930089	49.388365
920.532231	131.126749	49.393370
916.884987	130.293145	49.398375
913.496652	132.177856	49.403380
909.427714	140.278484	49.408385
905.914215	134.054931	49.413389
902.321764	125.907487	49.418394
899.145963	126.148537	49.423399
895.869012	120.125241	49.428404
892.219848	129.621826	49.433409
888.992612	128.289022	49.438413
885.281788	130.730451	49.443418
881.449534	131.738701	49.448423
878.190716	127.958884	49.453428
874.543754	132.393017	49.458433
870.411251	128.658260	49.463437
867.755812	131.908892	49.468442
864.018399	128.820968	49.473447
860.624045	135.458700	49.478452
856.804186	129.422352	49.483457
853.277097	131.085196	49.488461
850.076868	123.531270	49.493466
846.656041	128.414065	49.498471
843.455022	132.129794	49.503476
839.478849	135.514481	49.508481
836.002336	135.758348	49.513485
832.687981	131.167814	49.518490
828.839973	125.594642	49.523495
825.433182	123.378799	49.528500
822.076618	135.458722	49.533505
818.155379	126.780658	49.538509
815.324365	125.727528	49.543514
811.602590	131.223786	49.548519
808.558226	122.240733	49.553524
804.705408	131.519294	49.558529
801.254850	121.986071	49.563533
796.973930	122.479308	49.568538
793.635894	126.456958	49.573543
790.371057	124.187260	49.578548
787.076147	124.000902	49.583553
783.800283	122.024005	49.588557
780.508345	118.262070	49.593562
776.676803	131.299088	49.598567
772.989495	119.265571	49.603572
769.221271	126.158032	49.608577
765.716520	129.718864	49.613581
762.376976	126.546532	49.618586
758.807115	131.316651	49.623591
755.832054	121.892488	49.628596
752.074720	121.863981	49.633601
748.576580	128.309185	49.638605
744.710760	125.814073	49.643610
741.071899	124.896967	49.648615
737.556495	122.742460	49.653620
734.401434	127.602655	49.658625
731.012807	131.018762	49.663629
727.825209	121.469704	49.668634
723.930006	125.126498	49.673639
720.298425	124.182950	49.678644
716.890733	129.161809	49.683649
713.305026	123.300836	49.688653
710.060580	122.913610	49.693658
706.654182	131.249079	49.698663
703.304907	122.794720	49.703668
699.379344	122.223093	49.708673
695.842944	119.587827	49.713677
692.372778	118.982851	49.718682
688.659158	130.799179	49.723687
685.236943	125.842775	49.728692
681.838156	126.688307	49.733697
678.220202	120.253423	49.738701
675.109005	122.794017	49.743706
671.149322	123.524909	49.748711
668.083542	125.884383	49.753716
664.647061	128.200671	49.758721
660.656307	127.322889	49.763725
657.689688	117.274174	49.768730
654.204950	126.033222	49.773735
650.591779	121.796452	49.778740
646.535704	125.959371	49.783745
642.845827	126.429718	49.788749
639.510801	120.026472	49.793754
636.580670	122.880413	49.798759
633.567956	116.610194	49.803764
629.501502	124.137879	49.808769
625.851241	113.598287	49.813773
622.522162	111.797467	49.818778
618.419112	112.455922	49.823783
615.263087	117.392233	49.828788
612.037263	123.829633	49.833793
608.251003	126.330438	49.838797
605.353783	109.911616	49.843802
601.297506	121.474740	49.848807
597.728249	115.263225	49.853812
594.324507	119.086712	49.858817
590.722438	125.371071	49.863821
587.505248	112.748322	49.868826
583.763922	121.440005	49.873831
580.386261	110.595147	49.878836
576.854951	114.033650	49.883841
573.089094	117.521546	49.888845
569.588355	111.726428	49.893850
566.233019	121.702284	49.898855
563.152891	115.512255	49.903860
559.313232	122.938005	49.908865
555.974802	116.661882	49.913869
552.084734	117.154128	49.918874
548.416160	123.262252	49.923879
545.447169	113.976436	49.928884
541.747234	115.913243	49.933889
538.472239	121.931252	49.938893
534.773588	109.940769	49.943898
531.082698	119.573712	49.948903
527.405601	111.654844	49.953908
524.090037	116.230186	49.958913
520.429578	122.197840	49.963917
517.589368	124.696041	49.968922
514.065538	122.710626	49.973927
510.319094	116.852775	49.978932
506.700686	120.548560	49.983937
503.214416	116.975362	49.988941
499.997763	109.977826	49.993946
495.959562	115.482624	49.998951
493.048034	109.003622	50.003956
489.217289	115.928117	50.008961
485.542175	106.452367	50.013965
482.109348	118.060250	50.018970
478.492205	110.356646	50.023975
475.189161	110.016649	50.028980
471.435636	115.483195	50.033985
468.142448	120.187931	50.038989
465.093876	112.426914	50.043994
461.261736	127.947709	50.048999
457.859231	114.164454	50.054004
454.191174	110.230603	50.059009
450.365876	117.435839	50.064013
447.365126	115.017337	50.069018
443.663524	112.319467	50.074023
440.072767	108.088773	50.079028
436.387705	110.219447	50.084033
433.169768	109.891445	50.089037
429.941829	122.789725	50.094042
426.171131	123.446828	50.099047
422.815363	107.931999	50.104052
418.997612	113.076425	50.109057
415.679975	110.786667	50.114061
411.992751	101.588104	50.119066
408.424452	116.162729	50.124071
405.440717	110.660031	50.129076
401.743970	115.728562	50.134081
398.101500	109.788040	50.139085
394.623587	109.010384	50.144090
391.371959	112.914518	50.149095
387.692825	102.847817	50.154100
384.071357	113.903134	50.159105
380.407915	105.191250	50.164109
376.998303	110.765313	50.169114
373.727806	117.510343	50.174119
370.596900	110.056497	50.179124
366.346935	113.076129	50.184129
362.688399	114.342123	50.189133
359.716154	107.875847	50.194138
356.058873	113.542499	50.199143
352.744471	107.534789	50.204148
349.192765	111.691590	50.209153
345.153972	120.857064	50.214157
342.293235	113.101476	50.219162
338.614060	110.748157	50.224167
335.000370	103.313007	50.229172
331.452032	105.238805	50.234177
327.854993	110.978288	50.239181
324.695803	107.809519	50.244186
321.123988	118.800133	50.249191
317.867929	111.198232	50.254196
314.202038	119.726327	50.259201
310.732254	115.527359	50.264205
307.154501	106.659715	50.269210
303.132609	114.044498	50.274215
299.740136	108.422370	50.279220
296.108255	115.366404	50.284225
292.688425	112.906039	50.289229
289.598241	113.614787	50.294234
285.908944	116.923119	50.299239
282.854614	112.757160	50.304244
279.436745	106.405018	50.309249
275.575219	112.657359	50.314253
272.447291	115.039349	50.319258
268.260321	115.122641	50.324263
264.799746	104.224484	50.329268
261.323832	105.645411	50.334273
257.911458	113.760480	50.339277
254.718784	110.827940	50.344282
251.353256	113.576194	50.349287
247.482465	110.022214	50.354292
243.867685	108.538386	50.359297
240.119760	111.786317	50.364301
237.121844	112.876103	50.369306
233.366752	110.734043	50.374311
230.231196	114.673832	50.379316
226.613579	115.844884	50.384321
222.973176	112.450979	50.389325
219.641837	111.280267	50.394330
216.256263	119.014661	50.399335
212.679501	108.378341	50.404340
209.020115	113.605608	50.409345
205.270535	118.268032	50.414349
201.850791	109.556021	50.419354
198.018152	116.927017	50.424359
194.677200	116.925262	50.429364
191.284562	111.720827	50.434369
188.108073	118.966887	50.439373
184.453865	107.235386	50.444378
180.513372	114.056964	50.449383
177.236985	111.814622	50.454388
173.702778	118.439675	50.459393
169.992585	118.056008	50.464397
167.008984	115.638086	50.469402
163.271778	119.706957	50.474407
160.025906	109.199161	50.479412
156.462892	118.005426	50.484417
153.031498	112.604596	50.489421
149.465137	113.109579	50.494426
145.855824	114.608398	50.499431
142.785440	114.693991	50.504436
139.179984	117.957608	50.509441
135.180275	118.976584	50.514445
131.718619	111.929002	50.519450
128.318957	112.433188	50.524455
124.976551	100.966088	50.529460
121.199950	112.422284	50.534465
117.536145	113.366495	50.539469
114.454847	110.185604	50.544474
110.936476	115.957135	50.549479
107.534056	108.957233	50.554484
103.824827	115.593911	50.559489
100.277869	118.161835	50.564493
96.912832	110.406260	50.569498
93.378669	119.625647	50.574503
89.718128	108.641843	50.579508
86.241763	112.657221	50.584513
82.958916	120.910246	50.589517
79.423010	101.915171	50.594522
75.684337	117.415101	50.599527
72.057986	113.205966	50.604532
68.776386	111.284028	50.609537
65.431474	113.092635	50.614541
61.761351	116.312630	50.619546
58.278945	116.877264	50.624551
54.901769	103.938150	50.629556
51.230330	107.825915	50.634561
47.610027	116.685484	50.639565
44.238317	103.274115	50.644570
40.804673	108.890023	50.649575
37.442544	105.743672	50.654580
33.566592	114.526240	50.659585
30.000450	119.596596	50.664589
26.930965	112.079487	50.669594
23.310349	107.872640	50.674599
19.758528	113.219168	50.679604
16.455246	102.767896	50.684609
12.636470	106.621812	50.689613
9.282275	108.966576	50.694618
5.455566	108.151978	50.699623
2.233044	110.273631	50.704628