Thu Aug 25 16:50:32 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
1.147149	95.790641	0.000000
1.016616	105.182296	0.005005
0.933929	101.499997	0.010010
1.081915	95.902264	0.015014
0.408500	89.151898	0.020019
0.523945	79.968369	0.025024
0.353228	84.538370	0.030029
0.036674	65.339546	0.035034
0.052221	54.884022	0.040038
-0.204909	64.045551	0.045043
-0.510577	48.182833	0.050048
-0.932127	46.926476	0.055053
-1.188097	36.817227	0.060058
-1.392058	29.983838	0.065062
-1.702462	32.611006	0.070067
-1.941764	14.703609	0.075072
-2.363540	19.698911	0.080077
-2.467279	20.999712	0.085082
-2.936952	9.778676	0.090086
-3.472057	12.045577	0.095091
-3.614001	6.284491	0.100096
-3.967934	10.788267	0.105101
-4.041695	12.432385	0.110106
-4.223993	5.839222	0.115110
-5.222883	4.616380	0.120115
-4.970516	1.824408	0.125120
-5.209901	6.408312	0.130125
-5.027617	3.446986	0.135130
-5.147969	4.288478	0.140134
-6.036319	0.223067	0.145139
-6.074522	6.069432	0.150144
-6.504713	15.251725	0.155149
-6.859245	6.372828	0.160154
-6.668115	4.169422	0.165158
-7.202987	8.995779	0.170163
-7.807170	9.324618	0.175168
-7.859911	15.280832	0.180173
-8.376889	9.429809	0.185178
-8.189691	9.938373	0.190182
-8.223041	16.809045	0.195187
-8.264707	3.834659	0.200192
-8.910485	13.544279	0.205197
-9.382357	9.113052	0.210202
-9.509162	6.127388	0.215206
-9.841817	13.370823	0.220211
-9.828421	8.502892	0.225216
-9.424538	16.807848	0.230221
-10.686096	9.902893	0.235226
-11.090707	11.503937	0.240230
-10.926429	15.575340	0.245235
-11.193681	6.815646	0.250240
-11.127357	5.954252	0.255245
-11.386074	5.229210	0.260250
-11.880230	-0.112854	0.265254
-12.509677	9.144949	0.270259
-12.428826	8.626130	0.275264
-12.541336	9.884012	0.280269
-12.890387	10.232987	0.285274
-12.820364	0.041045	0.290278
-13.679605	7.136031	0.295283
-13.740524	-3.165107	0.300288
-13.881267	11.217366	0.305293
-14.738484	8.909299	0.310298
-14.394644	4.030723	0.315302
-14.685212	3.288524	0.320307
-14.649978	-2.984377	0.325312
-15.245744	-0.562439	0.330317
-15.145034	10.909497	0.335322
-14.918703	4.590832	0.340326
-15.784847	10.702967	0.345331
-16.256839	5.901598	0.350336
-16.581969	9.919968	0.355341
-16.858820	11.361788	0.360346
-16.759365	6.027954	0.365350
-17.119908	13.070113	0.370355
-17.562425	15.841366	0.375360
-18.209065	14.677229	0.380365
-18.147161	14.927012	0.385370
-18.007535	7.568395	0.390374
-18.265619	10.101940	0.395379
-18.148635	8.761206	0.400384
-18.852188	12.857853	0.405389
-19.652104	18.937467	0.410394
-19.470400	9.813196	0.415398
-19.757148	12.604335	0.420403
-19.585087	7.746346	0.425408
-19.980158	-6.906406	0.430413
-20.632607	12.146878	0.435418
-20.919643	1.571117	0.440422
-21.289039	14.103811	0.445427
-21.300646	5.816594	0.450432
-21.023271	4.033111	0.455437
-21.603947	8.284511	0.460442
-21.918501	0.823053	0.465446
-22.782881	11.408487	0.470451
-22.787993	6.866161	0.475456
-22.783578	12.234448	0.480461
-22.680058	11.427338	0.485466
-22.648093	6.110406	0.490470
-23.555159	5.306616	0.495475
-24.271616	4.783010	0.500480
-24.432492	0.442264	0.505485
-24.528907	3.640179	0.510490
-24.708363	1.700484	0.515494
-24.932129	13.928783	0.520499
-24.745172	10.811699	0.525504
-24.481649	17.841499	0.530509
-24.758473	14.746462	0.535514
-25.112596	8.762356	0.540518
-25.521998	14.426438	0.545523
-26.048837	8.656057	0.550528
-26.558787	10.732354	0.555533
-26.770249	13.590792	0.560538
-26.810126	6.488093	0.565542
-27.277865	10.183956	0.570547
-27.737599	3.665903	0.575552
-28.099982	2.197799	0.580557
-28.353231	4.528104	0.585562
-28.195474	4.449655	0.590566
-28.465434	9.092135	0.595571
-28.381909	11.578482	0.600576
-28.549845	5.486110	0.605581
-29.882336	5.527268	0.610586
-30.276904	2.140632	0.615590
-29.810648	5.978053	0.620595
-29.595412	15.809030	0.625600
-29.916635	6.478824	0.630605
-30.103901	6.865726	0.635610
-30.518264	5.310853	0.640614
-31.307453	3.118680	0.645619
-31.729207	7.981097	0.650624
-31.697296	0.623542	0.655629
-31.795484	11.022484	0.660634
-31.569461	2.492391	0.665638
-31.602450	-2.080365	0.670643
-32.255934	5.602480	0.675648
-32.590580	13.472654	0.680653
-32.790465	6.493103	0.685658
-33.128556	-1.486688	0.690662
-33.943307	10.135015	0.695667
-34.061626	13.810930	0.700672
-34.582730	18.283954	0.705677
-34.760552	7.947344	0.710682
-34.514941	4.216790	0.715686
-34.886758	5.765240	0.720691
-35.014024	5.237902	0.725696
-34.850871	6.585468	0.730701
-34.845318	9.890795	0.735706
-35.125455	11.519793	0.740710
-35.579726	9.132773	0.745715
-36.294469	9.988305	0.750720
-37.144228	6.907111	0.755725
-37.074016	9.193063	0.760730
-36.913101	2.783409	0.765734
-37.282904	14.474601	0.770739
-37.474249	8.876282	0.775744
-37.469911	6.888806	0.780749
-37.749881	4.544079	0.785754
-38.356292	6.300130	0.790758
-38.764636	-0.823925	0.795763
-38.830036	0.214602	0.800768
-38.912774	2.891515	0.805773
-38.723233	7.022231	0.810778
-38.994280	2.711403	0.815782
-40.178773	11.334836	0.820787
-40.251141	8.932269	0.825792
-40.271968	6.214741	0.830797
-40.489116	11.035608	0.835802
-40.390519	-1.400760	0.840806
-41.025268	4.270154	0.845811
-41.390512	7.073592	0.850816
-41.769740	15.748023	0.855821
-42.428747	20.385025	0.860826
-41.786706	9.208103	0.865830
-42.184434	9.400191	0.870835
-42.296799	6.326844	0.875840
-42.332004	7.692836	0.880845
-43.082148	12.894613	0.885850
-42.966155	9.216005	0.890854
-43.575325	12.446808	0.895859
-43.574129	4.299958	0.900864
-44.477761	0.259093	0.905869
-44.911437	9.498876	0.910874
-44.931584	-0.584021	0.915878
-45.175400	10.169934	0.920883
-45.139818	11.556472	0.925888
-45.050109	15.604756	0.930893
-45.260806	9.680436	0.935898
-45.176691	4.750806	0.940902
-45.751016	11.462628	0.945907
-46.215309	11.788532	0.950912
-46.539916	7.780327	0.955917
-46.917468	5.400269	0.960922
-46.437019	-4.855976	0.965926
-47.506335	10.564174	0.970931
-48.082778	9.512427	0.975936
-47.918926	7.721421	0.980941
-48.427358	9.237494	0.985946
-48.266228	9.674211	0.990950
-48.072123	7.233055	0.995955
-48.542308	16.136874	1.000960
-48.866423	7.721454	1.005965
-49.366468	5.768717	1.010970
-49.053381	-3.803241	1.015974
-49.356905	5.381344	1.020979
-50.308068	10.215983	1.025984
-50.687164	9.864146	1.030989
-51.521770	14.360982	1.035994
-50.403930	1.252377	1.040998
-50.863221	2.109012	1.046003
-51.132204	8.722368	1.051008
-50.983096	4.880384	1.056013
-51.486109	14.023465	1.061018
-51.991202	-1.203672	1.066022
-52.321920	4.669542	1.071027
-52.767006	6.302239	1.076032
-52.566281	4.771213	1.081037
-53.306008	1.875263	1.086042
-53.612260	0.439494	1.091046
-53.932353	17.890456	1.096051
-54.107176	17.680619	1.101056
-53.927231	5.576353	1.106061
-54.236441	10.702712	1.111066
-53.786194	5.038665	1.116070
-54.396930	12.971081	1.121075
-55.167854	7.909670	1.126080
-55.493589	14.338930	1.131085
-55.574921	10.140745	1.136090
-55.649049	1.831691	1.141094
-55.789968	11.259721	1.146099
-56.625758	15.165117	1.151104
-56.781234	7.586984	1.156109
-56.681275	12.791601	1.161114
-56.785650	2.766194	1.166118
-57.192595	6.436712	1.171123
-57.553226	11.659714	1.176128
-58.146597	7.839156	1.181133
-58.459935	19.518339	1.186138
-57.967144	8.548303	1.191142
-58.625898	7.427197	1.196147
-58.607134	4.260538	1.201152
-58.732026	9.098586	1.206157
-59.359956	7.472774	1.211162
-59.666335	9.741803	1.216166
-60.094850	4.652051	1.221171
-59.844201	12.234359	1.226176
-59.599919	10.240924	1.231181
-60.629719	10.057486	1.236186
-60.884711	15.529694	1.241190
-61.319034	9.618269	1.246195
-61.280834	11.127784	1.251200
-61.091246	10.829210	1.256205
-61.611351	11.948477	1.261210
-61.980235	5.590199	1.266214
-62.530750	13.048105	1.271219
-62.633606	3.851368	1.276224
-62.487182	13.939897	1.281229
-62.879611	17.348713	1.286234
-63.334078	18.055896	1.291238
-63.665661	20.550340	1.296243
-63.919280	14.917485	1.301248
-63.900209	10.921868	1.306253
-64.062102	17.477318	1.311258
-65.285330	13.350489	1.316262
-65.456314	22.216920	1.321267
-64.614430	17.064147	1.326272
-65.429893	11.709156	1.331277
-65.364512	13.125827	1.336282
-65.503577	11.353811	1.341286
-65.762026	7.233999	1.346291
-66.657702	13.657651	1.351296
-66.828939	9.732983	1.356301
-67.360316	15.621823	1.361306
-67.100085	13.888481	1.366310
-67.386625	8.466433	1.371315
-67.438542	9.157996	1.376320
-67.308287	12.750669	1.381325
-68.147089	14.198285	1.386330
-68.156408	7.347066	1.391334
-68.840311	11.760176	1.396339
-69.000858	4.477071	1.401344
-68.742151	10.292730	1.406349
-69.462268	11.845137	1.411354
-69.890743	13.797938	1.416358
-70.114457	8.005375	1.421363
-70.359224	14.073933	1.426368
-70.283959	10.091658	1.431373
-70.456680	9.783415	1.436378
-70.088886	12.788371	1.441382
-71.102151	10.748372	1.446387
-71.405991	16.557266	1.451392
-71.220163	8.315046	1.456397
-71.503855	13.728475	1.461402
-71.763472	14.749978	1.466406
-72.347450	21.618341	1.471411
-72.757431	15.124131	1.476416
-72.909886	17.403843	1.481421
-73.294680	17.169960	1.486426
-73.360648	13.146538	1.491430
-73.543437	15.605012	1.496435
-74.487614	11.636941	1.501440
-74.473058	12.593337	1.506445
-74.431442	15.630420	1.511450
-74.575526	11.037104	1.516454
-74.780248	9.958752	1.521459
-74.929344	5.309275	1.526464
-74.628867	5.863363	1.531469
-75.242456	10.192689	1.536474
-75.983867	5.689808	1.541478
-76.346128	4.588684	1.546483
-76.506631	9.027350	1.551488
-76.016924	4.992791	1.556493
-77.722541	11.910351	1.561498
-77.286440	8.045544	1.566502
-77.773696	15.411280	1.571507
-77.607132	11.579214	1.576512
-77.593887	11.510753	1.581517
-77.835757	4.512476	1.586522
-77.714358	1.563854	1.591526
-78.334641	9.219353	1.596531
-78.824500	2.063781	1.601536
-78.810174	-2.956151	1.606541
-79.231927	3.611537	1.611546
-79.775241	-3.665371	1.616550
-80.276177	2.759700	1.621555
-80.553130	8.662456	1.626560
-80.500199	3.652292	1.631565
-80.849117	9.771969	1.636570
-80.879698	4.262360	1.641574
-80.670568	8.171704	1.646579
-80.926701	6.968529	1.651584
-81.399807	-0.433277	1.656589
-82.496368	12.804978	1.661594
-82.409356	5.695055	1.666598
-82.623535	7.889526	1.671603
-82.308237	5.160459	1.676608
-82.319365	8.148857	1.681613
-83.033003	12.073079	1.686618
-83.181021	6.996324	1.691622
-83.752598	8.006598	1.696627
-83.780678	9.937788	1.701632
-83.793495	11.800148	1.706637
-84.505051	12.645693	1.711642
-84.764771	8.760201	1.716646
-85.050288	10.140105	1.721651
-85.160595	13.080769	1.726656
-85.036419	10.147530	1.731661
-85.174592	17.556645	1.736666
-85.886312	17.022810	1.741670
-86.271518	6.725031	1.746675
-86.716927	10.445870	1.751680
-86.452767	12.815326	1.756685
-86.592813	19.683730	1.761690
-87.080417	11.490084	1.766694
-87.669905	12.740448	1.771699
-87.955386	18.774257	1.776704
-88.106020	18.079737	1.781709
-88.322014	18.983674	1.786714
-88.437323	13.272201	1.791718
-88.236759	11.776001	1.796723
-88.615448	16.764551	1.801728
-88.867245	15.706230	1.806733
-89.635736	19.566282	1.811738
-89.781175	14.489122	1.816742
-89.881005	22.436399	1.821747
-90.108439	14.265261	1.826752
-90.545417	15.940983	1.831757
-91.108164	17.566809	1.836762
-90.728333	8.000208	1.841766
-90.859266	12.734799	1.846771
-91.073212	17.270426	1.851776
-91.454557	9.351198	1.856781
-92.131624	9.264354	1.861786
-92.863756	13.786264	1.866790
-92.738120	21.435618	1.871795
-92.840622	14.567361	1.876800
-92.910148	10.168010	1.881805
-93.403276	21.419781	1.886810
-92.980430	13.323919	1.891814
-93.206194	12.758232	1.896819
-93.596483	13.942581	1.901824
-93.946480	17.762367	1.906829
-94.397752	12.654035	1.911834
-94.462187	15.448306	1.916838
-94.772235	19.160592	1.921843
-95.389834	8.045009	1.926848
-95.467956	4.539189	1.931853
-96.158369	13.369946	1.936858
-96.110467	17.981603	1.941862
-96.094472	8.978216	1.946867
-96.128229	17.763029	1.951872
-96.254733	6.570494	1.956877
-97.205907	16.388081	1.961882
-97.447472	12.474434	1.966886
-97.821423	17.889351	1.971891
-97.656821	17.949034	1.976896
-97.682133	9.414031	1.981901
-97.876665	19.533839	1.986906
-97.909826	4.606081	1.991910
-98.669001	11.998606	1.996915
-99.202543	16.222358	2.006912
-98.628185	14.567560	2.016909
-98.184910	10.722162	2.026906
-97.923388	17.330551	2.036902
-97.173227	16.060024	2.046899
-96.864639	11.434271	2.056896
-95.909864	16.065015	2.066893
-95.418845	13.168818	2.076890
-95.442630	13.134638	2.086886
-94.913947	12.655925	2.096883
-94.098960	12.971823	2.106880
-93.891521	17.586623	2.116877
-93.019766	26.573467	2.126874
-92.606188	21.370555	2.136870
-92.388195	13.470795	2.146867
-91.567735	17.036023	2.156864
-91.355297	19.175970	2.166861
-90.252805	17.280025	2.176858
-89.819826	18.387550	2.186854
-89.784188	18.055786	2.196851
-89.567231	11.375802	2.206848
-88.294833	17.604047	2.216845
-88.158274	15.805606	2.226842
-87.829183	16.162795	2.236838
-86.838594	13.467087	2.246835
-86.977702	8.696074	2.256832
-86.309427	7.843860	2.266829
-85.667210	11.864674	2.276826
-85.229288	9.762418	2.286822
-84.037421	7.443822	2.296819
-83.800949	4.270730	2.306816
-83.989487	1.709101	2.316813
-83.205720	4.421597	2.326810
-82.358611	4.808491	2.336806
-82.260442	2.480704	2.346803
-81.981931	7.369470	2.356800
-81.089762	6.992193	2.366797
-80.887356	5.164429	2.376794
-79.774189	8.024884	2.386790
-79.762020	8.457076	2.396787
-79.143523	6.912573	2.406784
-78.533891	1.837338	2.416781
-78.403671	12.514779	2.426778
-77.235593	7.814539	2.436774
-76.583583	5.840297	2.446771
-76.598946	6.999067	2.456768
-76.377169	12.615820	2.466765
-76.098739	10.383332	2.476762
-75.048394	7.282285	2.486758
-74.615236	14.757108	2.496755
-73.956183	11.600164	2.506752
-73.922594	6.352259	2.516749
-73.103708	11.932471	2.526746
-72.472303	17.475537	2.536742
-72.248975	9.688983	2.546739
-71.210921	13.600257	2.556736
-70.993976	11.925437	2.566733
-70.966487	13.723729	2.576730
-69.738213	17.161702	2.586726
-69.181725	6.316680	2.596723
-69.404890	7.469997	2.606720
-69.189893	8.621181	2.616717
-68.124319	15.303157	2.626714
-67.367773	9.222874	2.636710
-66.493606	8.683693	2.646707
-66.533275	8.408079	2.656704
-66.552722	6.564391	2.666701
-65.695903	8.726914	2.676698
-65.024438	11.520367	2.686694
-64.769901	4.267455	2.696691
-64.203998	7.267518	2.706688
-63.744330	13.965239	2.716685
-63.126164	6.740880	2.726682
-62.622670	10.419133	2.736678
-62.134728	15.778770	2.746675
-61.004849	11.204895	2.756672
-60.906542	10.125208	2.766669
-61.255797	12.131420	2.776666
-60.244522	12.153635	2.786662
-59.524009	9.037747	2.796659
-58.910112	6.939597	2.806656
-58.170031	7.872289	2.816653
-57.668436	3.346177	2.826650
-58.149050	8.369731	2.836646
-57.224574	7.176432	2.846643
-56.649424	9.984977	2.856640
-55.822602	12.728745	2.866637
-55.381310	10.895228	2.876634
-55.432989	11.866451	2.886630
-54.377254	18.401084	2.896627
-53.636977	21.982050	2.906624
-53.773122	21.116498	2.916621
-53.438439	16.420130	2.926618
-52.638020	17.650649	2.936614
-51.989977	14.108955	2.946611
-51.074093	9.536933	2.956608
-50.852772	13.759918	2.966605
-50.851925	18.153666	2.976602
-50.189603	10.767163	2.986598
-49.416579	8.387486	2.996595
-49.236260	16.215544	3.006592
-48.328822	4.504570	3.016589
-48.037622	13.972025	3.026586
-47.748729	19.676469	3.036582
-46.803158	7.110540	3.046579
-46.438040	9.232900	3.056576
-46.055818	9.154110	3.066573
-45.644460	12.241747	3.076570
-44.918262	7.316141	3.086566
-44.637564	11.590010	3.096563
-44.034196	9.164056	3.106560
-43.439197	14.025412	3.116557
-43.279779	9.749318	3.126554
-42.198069	7.213568	3.136550
-41.747314	10.146144	3.146547
-41.826071	13.925135	3.156544
-41.503725	15.468150	3.166541
-40.504608	7.360466	3.176538
-39.715304	13.312786	3.186534
-39.539874	13.535663	3.196531
-39.203474	3.951076	3.206528
-38.554518	8.338305	3.216525
-38.173891	5.465744	3.226522
-37.622543	4.004625	3.236518
-36.581933	7.256595	3.246515
-36.105863	5.341602	3.256512
-35.918099	7.111612	3.266509
-35.823014	6.700842	3.276506
-35.117115	5.066619	3.286502
-34.555384	4.554221	3.296499
-34.044214	3.555565	3.306496
-33.573570	6.275948	3.316493
-32.930541	17.183493	3.326490
-32.050372	9.461914	3.336486
-31.844739	4.503833	3.346483
-31.897937	3.558760	3.356480
-31.170963	6.850370	3.366477
-30.695854	6.883740	3.376474
-30.042197	6.436133	3.386470
-29.007974	-0.013940	3.396467
-28.699436	6.631435	3.406464
-28.648753	9.100839	3.416461
-28.264076	9.553860	3.426458
-27.748580	11.966273	3.436454
-26.910899	15.579496	3.446451
-25.800240	9.681316	3.456448
-25.632365	13.652915	3.466445
-25.699081	15.893624	3.476442
-25.493160	6.506878	3.486438
-24.570543	10.844895	3.496435
-24.226538	12.954726	3.506432
-23.462765	9.087622	3.516429
-23.152246	10.071785	3.526426
-22.084299	14.016397	3.536422
-21.452320	6.283022	3.546419
-21.324810	12.361213	3.556416
-21.373035	10.702600	3.566413
-20.765820	9.964496	3.576410
-19.664579	17.385332	3.586406
-19.564037	10.587369	3.596403
-18.904272	8.741796	3.606400
-18.437105	5.383670	3.616397
-18.136066	5.361951	3.626394
-17.281610	9.023231	3.636390
-16.820559	9.096817	3.646387
-16.828646	7.295698	3.656384
-15.879545	11.385645	3.666381
-15.690926	11.055254	3.676378
-14.881357	15.781622	3.686374
-14.223786	6.108696	3.696371
-14.221158	6.941529	3.706368
-13.171137	7.733796	3.716365
-12.608225	3.267769	3.726362
-12.598816	8.585179	3.736358
-12.384422	11.282359	3.746355
-11.662437	10.085945	3.756352
-10.540781	5.785796	3.766349
-10.207094	6.021891	3.776346
-9.648807	3.732885	3.786342
-9.689851	-0.907776	3.796339
-9.405919	10.322131	3.806336
-8.481316	6.116215	3.816333
-7.822612	14.417354	3.826330
-7.207066	7.627398	3.836326
-6.912718	13.502051	3.846323
-6.685727	13.577466	3.856320
-6.140555	24.646072	3.866317
-5.804064	27.454005	3.876314
-4.965342	25.951027	3.886310
-4.583217	28.593419	3.896307
-3.849982	38.903968	3.906304
-3.714806	45.788767	3.916301
-2.953132	56.595388	3.926298
-2.751127	64.109625	3.936294
-2.323536	68.002530	3.946291
-1.654088	72.906094	3.956288
-1.462613	87.302535	3.966285
-1.147931	98.293260	3.976282
-0.755785	117.004562	3.986278
0.000000	131.241793	3.991283
0.128001	136.429401	3.996288
0.590404	139.748594	4.001293
0.587415	149.841634	4.006298
0.364638	150.379637	4.011302
0.461082	149.798259	4.016307
0.732376	152.299500	4.021312
0.576708	157.243654	4.026317
0.658333	154.756826	4.031322
0.836633	151.618927	4.036326
1.154749	158.757292	4.041331
0.763390	161.058636	4.046336
0.898846	160.135782	4.051341
1.152873	158.976048	4.056346
1.092609	159.156389	4.061350
1.096177	156.995007	4.066355
1.097293	163.812878	4.071360
0.982883	152.760717	4.076365
0.934593	157.321046	4.081370
0.767433	159.283537	4.086374
1.044910	156.069985	4.091379
0.991402	162.912234	4.096384
1.072125	156.220854	4.101389
0.899337	157.421751	4.106394
1.011962	172.334141	4.111398
1.323762	174.294356	4.116403
1.047499	167.212810	4.121408
1.050896	163.675200	4.126413
1.277025	166.594814	4.131418
0.936007	168.426357	4.136422
1.265676	171.987820	4.141427
1.053534	177.004103	4.146432
1.325064	176.673706	4.151437
1.386124	179.483143	4.156442
0.937113	158.248499	4.161446
1.268534	164.100278	4.166451
1.012141	169.208916	4.171456
1.299697	186.397158	4.176461
1.346371	178.920153	4.181466
1.146934	189.214841	4.186470
1.508399	184.333454	4.191475
1.846431	176.105271	4.196480
1.015496	177.102401	4.201485
1.231097	165.457515	4.206490
1.111060	164.157070	4.211494
1.189297	171.880363	4.216499
1.619209	180.317363	4.221504
1.610588	180.644639	4.226509
1.698709	170.101744	4.231514
1.234689	166.868328	4.236518
1.275710	151.599776	4.241523
1.067295	175.557157	4.246528
1.161428	176.165730	4.251533
1.392920	183.811231	4.256538
1.227219	189.291649	4.261542
1.735671	180.989305	4.266547
1.370455	181.429402	4.271552
1.602675	187.619440	4.276557
1.969255	185.170219	4.281562
1.221790	187.464087	4.286566
1.289955	182.068662	4.291571
1.458956	189.375938	4.296576
1.399875	192.985661	4.301581
1.460396	182.709680	4.306586
1.530862	184.944994	4.311590
1.537279	180.517878	4.316595
1.473349	188.674749	4.321600
1.008545	195.809247	4.326605
1.172381	190.484252	4.331610
1.247825	196.069260	4.336614
2.086349	194.134560	4.341619
1.642579	199.968603	4.346624
1.228556	195.022055	4.351629
1.312110	193.183500	4.356634
1.769719	205.023592	4.361638
2.341935	208.891915	4.366643
1.870306	195.766454	4.371648
1.647755	192.631242	4.376653
1.773356	184.167416	4.381658
1.443170	192.657076	4.386662
1.875482	199.942083	4.391667
1.992326	204.270903	4.396672
1.643192	190.357447	4.401677
2.067963	203.499844	4.406682
1.917592	203.425380	4.411686
1.794418	183.721557	4.416691
1.754503	185.050335	4.421696
1.656920	192.918246	4.426701
1.990508	200.446516	4.431706
1.837997	214.739248	4.436710
2.121808	205.083177	4.441715
1.870852	205.540174	4.446720
1.902370	202.197470	4.451725
2.122405	202.286437	4.456730
1.869355	200.064015	4.461734
1.591691	205.011478	4.466739
1.833393	210.905804	4.471744
2.094707	210.194186	4.476749
2.222250	212.009266	4.481754
2.123844	211.436269	4.486758
2.375254	208.002162	4.491763
2.079186	196.108390	4.496768
1.581539	194.677280	4.501773
2.019074	202.676490	4.506778
2.316479	214.975132	4.511782
2.027212	211.796586	4.516787
2.013272	206.882262	4.521792
2.002184	208.709571	4.526797
2.361496	211.785498	4.531802
1.845427	216.941164	4.536806
1.841180	218.606048	4.541811
1.821972	213.069278	4.546816
1.867693	214.580796	4.551821
2.129576	220.671284	4.556826
1.955061	221.676299	4.561830
2.303670	215.686420	4.566835
2.171893	214.046120	4.571840
2.048962	215.315140	4.576845
2.439393	213.877761	4.581850
2.129202	219.928167	4.586854
2.300297	207.600516	4.591859
2.313621	221.117446	4.596864
1.963749	220.267468	4.601869
2.179118	213.808076	4.606874
2.293324	216.545915	4.611878
2.434641	209.696322	4.616883
2.752538	216.635425	4.621888
2.504711	211.045888	4.626893
2.670116	216.534548	4.631898
2.181948	224.897114	4.636902
1.995709	217.377492	4.641907
2.205549	219.616283	4.646912
2.316063	225.445747	4.651917
2.826453	232.800793	4.656922
2.433511	218.947963	4.661926
2.383844	216.389947	4.666931
2.495898	215.062626	4.671936
2.205484	216.538225	4.676941
2.741026	219.295471	4.681946
2.378186	233.649647	4.686950
2.524978	233.661503	4.691955
2.252631	238.272777	4.696960
2.340228	238.436279	4.701965
2.435114	231.960956	4.706970
2.654823	234.419670	4.711974
2.936626	236.938260	4.716979
2.362037	244.324101	4.721984
2.874126	239.697515	4.726989
2.624013	234.817024	4.731994
2.568412	240.049248	4.736998
2.481154	229.413573	4.742003
2.672445	236.992628	4.747008
2.375521	235.394021	4.752013
2.718382	233.818559	4.757018
2.220545	234.051642	4.762022
2.385389	232.937515	4.767027
2.264976	239.470730	4.772032
2.624161	239.582187	4.777037
2.459955	232.628593	4.782042
2.698234	258.031561	4.787046
3.121967	253.725706	4.792051
3.228559	247.659839	4.797056
2.622706	244.825125	4.802061
2.524405	236.747540	4.807066
2.895210	245.165357	4.812070
3.023755	245.834981	4.817075
2.620377	249.419566	4.822080
2.771751	250.139398	4.827085
3.348418	263.995210	4.832090
2.750041	252.218371	4.837094
2.935212	255.299444	4.842099
2.767853	250.788805	4.847104
2.897431	256.260944	4.852109
3.115569	248.342585	4.857114
2.960173	255.099590	4.862118
3.007041	245.733728	4.867123
2.833674	248.519794	4.872128
2.785842	251.947428	4.877133
3.302985	259.532386	4.882138
3.040289	261.361157	4.887142
3.141929	250.392146	4.892147
2.861329	245.972019	4.897152
2.757117	254.866072	4.902157
3.219646	267.815936	4.907162
3.165718	265.410444	4.912166
3.258341	265.607961	4.917171
3.174581	250.548705	4.922176
2.940941	257.143961	4.927181
3.220432	258.707442	4.932186
3.176499	268.715214	4.937190
3.395900	271.790927	4.942195
3.217241	254.471749	4.947200
3.089132	248.499605	4.952205
3.410449	244.523016	4.957210
3.071015	242.535592	4.962214
3.374818	238.178927	4.967219
3.317348	246.290518	4.972224
2.959666	237.237988	4.977229
3.258428	243.177170	4.982234
3.129183	244.197240	4.987238
3.421547	253.491073	4.992243
3.030864	260.655113	4.997248
3.311757	265.423325	5.002253
3.338506	261.103737	5.007258
3.556339	259.807296	5.012262
3.358538	261.458217	5.017267
3.483036	258.205340	5.022272
3.031352	263.768555	5.027277
3.561889	252.504546	5.032282
3.199346	263.258276	5.037286
3.822976	262.806269	5.042291
3.361635	261.929461	5.047296
3.342069	258.180290	5.052301
3.764166	258.006638	5.057306
3.486247	250.583626	5.062310
3.073677	243.795495	5.067315
3.177305	250.094290	5.072320
3.315496	260.870803	5.077325
3.406918	259.821963	5.082330
3.350664	263.785605	5.087334
3.485473	265.662828	5.092339
3.521894	269.251275	5.097344
3.586377	274.227408	5.102349
3.429683	265.339529	5.107354
3.374926	275.105386	5.112358
3.596819	268.907548	5.117363
3.590311	272.303401	5.122368
3.703787	272.855163	5.127373
3.759510	273.893710	5.132378
3.449303	271.604304	5.137382
3.900392	266.664559	5.142387
3.901514	268.107138	5.147392
3.112110	266.497105	5.152397
3.349244	263.935275	5.157402
2.966065	272.398473	5.162406
3.437788	276.190806	5.167411
3.660666	287.548865	5.172416
3.538597	291.383617	5.177421
4.026963	285.925486	5.182426
3.824511	289.583003	5.187430
3.938649	290.526975	5.192435
3.776398	289.103419	5.197440
3.915772	292.150545	5.202445
4.257886	282.418857	5.207450
3.664622	279.079117	5.212454
3.676791	263.792843	5.217459
3.948301	279.389124	5.222464
3.937650	285.493861	5.227469
4.348582	271.815600	5.232474
3.853026	265.761814	5.237478
4.010653	264.705765	5.242483
3.946075	259.995518	5.247488
3.826340	260.878054	5.252493
3.729889	258.754478	5.257498
3.423413	269.176717	5.262502
3.990582	273.491943	5.267507
3.892496	284.938256	5.272512
3.851392	296.369321	5.277517
4.126946	285.638799	5.282522
4.281641	282.292600	5.287526
4.033246	289.640006	5.292531
3.966998	291.915738	5.297536
3.829490	289.719495	5.302541
4.457684	296.878936	5.307546
4.351000	291.403304	5.312550
4.214757	286.030384	5.317555
4.081162	278.796723	5.322560
4.356682	283.799905	5.327565
4.415902	262.820870	5.332570
3.729814	261.653402	5.337574
4.089045	259.319220	5.342579
3.606057	268.902229	5.347584
3.837518	292.493445	5.352589
4.185603	286.057526	5.357594
4.476006	284.898412	5.362598
4.309360	275.097742	5.367603
4.060466	285.371760	5.372608
3.821780	287.677673	5.377613
4.061529	283.536683	5.382618
3.962075	280.337875	5.387622
4.148934	289.486903	5.392627
3.834069	284.066038	5.397632
3.834992	284.189336	5.402637
4.260985	291.462716	5.407642
4.401810	310.278127	5.412646
4.474650	303.904310	5.417651
4.743649	302.422675	5.422656
4.288343	295.695005	5.427661
4.501623	287.625526	5.432666
4.215808	291.055654	5.437670
4.625972	301.663025	5.442675
4.585466	300.524120	5.447680
4.141311	305.829898	5.452685
4.578724	299.275572	5.457690
4.290265	288.680877	5.462694
4.469428	296.271350	5.467699
4.322699	300.283978	5.472704
4.557132	300.335886	5.477709
4.738759	307.290048	5.482714
4.371101	308.527815	5.487718
4.588381	314.346907	5.492723
4.723251	315.458479	5.497728
4.709597	309.541148	5.502733
4.529675	289.811298	5.507738
4.289432	289.222556	5.512742
4.796364	301.785828	5.517747
4.787251	309.962639	5.522752
4.386270	306.171977	5.527757
4.493619	294.515494	5.532762
4.632125	303.162729	5.537766
4.506809	303.619026	5.542771
4.671012	310.227898	5.547776
4.305008	320.387404	5.552781
4.649501	309.332847	5.557786
4.340144	318.002805	5.562790
4.490860	317.893821	5.567795
4.865336	323.267496	5.572800
4.350676	324.733946	5.577805
4.330733	310.794127	5.582810
4.420537	318.563129	5.587814
4.453218	322.981096	5.592819
4.720327	340.729525	5.597824
4.909052	343.357629	5.602829
4.994949	337.481640	5.607834
5.020760	333.535514	5.612838
5.138544	332.125026	5.617843
4.801115	325.907235	5.622848
4.638114	316.969698	5.627853
5.035074	318.793196	5.632858
4.978740	332.786209	5.637862
4.944771	322.651506	5.642867
5.074187	311.924883	5.647872
4.639060	314.622255	5.652877
4.964627	316.741684	5.657882
5.000497	329.160479	5.662886
5.413697	324.900551	5.667891
5.013798	318.942493	5.672896
4.771825	313.870875	5.677901
5.055658	311.478896	5.682906
4.665563	318.532133	5.687910
5.144275	321.228695	5.692915
5.202062	335.735353	5.697920
5.273398	333.873387	5.702925
5.206375	325.683290	5.707930
5.275028	322.318926	5.712934
4.984330	324.784858	5.717939
4.804413	322.639549	5.722944
4.734531	326.820481	5.727949
5.117065	336.679211	5.732954
5.430573	346.181756	5.737958
5.160816	332.730327	5.742963
5.220871	318.021813	5.747968
5.090639	320.155710	5.752973
5.413229	325.869718	5.757978
5.132530	330.010913	5.762982
4.892987	317.503911	5.767987
5.516967	326.233284	5.772992
5.199623	336.065627	5.777997
5.241301	330.430693	5.783002
5.368263	343.711607	5.788006
5.413667	337.060496	5.793011
5.114793	332.700159	5.798016
5.024604	341.228218	5.803021
5.250933	339.895638	5.808026
5.031063	354.135759	5.813030
5.590511	353.089514	5.818035
5.250747	342.740114	5.823040
5.192196	347.219839	5.828045
5.440748	340.926048	5.833050
5.205606	345.797283	5.838054
5.086324	343.626652	5.843059
5.635024	349.052133	5.848064
5.395045	342.353984	5.853069
5.615946	348.229468	5.858074
5.318123	348.633699	5.863078
5.460130	344.055581	5.868083
5.537137	350.165588	5.873088
5.422505	355.647547	5.878093
5.216086	347.922218	5.883098
5.422276	343.305569	5.888102
5.231758	348.413427	5.893107
5.365116	344.396663	5.898112
5.334671	350.817743	5.903117
5.268953	343.234890	5.908122
5.605350	364.041406	5.913126
5.665700	370.846911	5.918131
5.986379	372.875361	5.923136
5.655907	365.400422	5.928141
5.911187	345.222661	5.933146
5.621718	348.874840	5.938150
5.517943	342.085746	5.943155
5.657326	342.756840	5.948160
5.604346	344.461009	5.953165
5.688432	343.495574	5.958170
5.699108	349.005354	5.963174
5.651040	361.057663	5.968179
6.018434	358.927839	5.973184
5.345144	359.406718	5.978189
5.802822	365.975956	5.983194
5.677505	363.214631	5.988198
5.704653	369.471666	5.993203
6.225306	372.411608	5.998208
5.751543	363.105111	6.003213
6.053342	353.968175	6.008218
5.274945	355.646798	6.013222
5.819156	362.756147	6.018227
6.035882	363.035463	6.023232
5.570875	363.257076	6.028237
5.829210	360.786825	6.033242
5.745734	363.185491	6.038246
6.009932	370.664593	6.043251
5.734782	364.563583	6.048256
5.568877	357.784218	6.053261
5.822808	365.840744	6.058266
5.952914	371.546960	6.063270
5.756891	365.344965	6.068275
5.339980	359.933738	6.073280
5.390189	368.996648	6.078285
5.827070	367.589945	6.083290
5.615194	373.352908	6.088294
5.766034	377.505596	6.093299
5.864894	371.026436	6.098304
5.495765	372.194833	6.103309
5.952073	367.773112	6.108314
5.760334	366.094735	6.113318
5.703483	368.891038	6.118323
5.592880	357.945724	6.123328
5.575626	375.109138	6.128333
5.406761	375.322316	6.133338
5.756569	368.234347	6.138342
5.432698	375.669546	6.143347
5.489028	376.995913	6.148352
5.424451	381.723371	6.153357
6.338161	392.542973	6.158362
6.014098	384.481711	6.163366
5.948152	376.066789	6.168371
5.982439	379.848587	6.173376
5.728515	373.570238	6.178381
5.920939	379.962737	6.183386
5.597420	379.826813	6.188390
5.582116	376.567346	6.193395
5.700018	371.917065	6.198400
5.568433	377.398522	6.203405
6.050360	371.308607	6.208410
5.793153	375.458788	6.213414
6.109174	368.993060	6.218419
5.511321	375.034804	6.223424
5.599259	380.741302	6.228429
5.914843	376.221403	6.233434
5.697300	367.782781	6.238438
5.946876	368.025311	6.243443
5.925742	372.347316	6.248448
5.749346	378.395794	6.253453
5.774663	372.864653	6.258458
5.601669	378.545593	6.263462
5.809153	375.418902	6.268467
5.692086	375.684077	6.273472
5.661031	375.385268	6.278477
5.632380	369.419646	6.283482
5.869056	373.574703	6.288486
5.723406	378.431924	6.293491
5.637236	369.479158	6.298496
6.098147	368.296487	6.303501
6.016537	364.386168	6.308506
6.308142	368.985046	6.313510
6.057227	371.922490	6.318515
6.352003	369.535116	6.323520
5.883101	376.901288	6.328525
6.242322	375.452968	6.333530
5.968912	376.815182	6.338534
5.933421	354.487264	6.343539
5.827257	346.894928	6.348544
5.637280	351.778070	6.353549
5.895612	339.446151	6.358554
5.694217	341.629166	6.363558
5.343486	346.989923	6.368563
6.077787	360.188345	6.373568
5.941463	359.266934	6.378573
5.587432	342.044754	6.383578
5.849882	358.598002	6.388582
5.937918	352.307210	6.393587
5.943321	360.851939	6.398592
5.723276	351.622757	6.403597
5.885849	346.471925	6.408602
5.778175	351.772454	6.413606
5.617303	351.664832	6.418611
5.822075	349.240942	6.423616
5.687974	344.946536	6.428621
5.625316	346.266234	6.433626
5.689612	348.613271	6.438630
5.978713	350.279662	6.443635
6.096941	348.840629	6.448640
5.663710	351.389009	6.453645
5.927224	341.138080	6.458650
5.896326	341.383426	6.463654
5.977434	352.380916	6.468659
5.835699	348.764766	6.473664
5.368547	360.572682	6.478669
5.916157	343.288324	6.483674
6.061771	343.730646	6.488678
5.912735	339.906829	6.493683
5.888610	345.061384	6.498688
5.677005	343.629737	6.503693
5.924227	336.564181	6.508698
5.862126	341.060280	6.513702
5.674142	345.392601	6.518707
5.824130	347.599657	6.523712
5.743509	350.725556	6.528717
5.821567	347.008529	6.533722
5.707440	340.534276	6.538726
5.378070	349.957214	6.543731
5.567189	344.931940	6.548736
5.582429	348.609145	6.553741
6.278848	331.779222	6.558746
5.980192	339.855877	6.563750
5.768685	338.228057	6.568755
5.716246	341.855753	6.573760
5.693861	345.032639	6.578765
5.949712	349.678244	6.583770
5.714007	341.941687	6.588774
5.676425	356.412683	6.593779
5.957077	340.641339	6.598784
5.597355	346.816610	6.603789
5.887377	344.923543	6.608794
5.678115	347.174232	6.613798
5.659518	343.418564	6.618803
5.594702	343.045949	6.623808
5.588245	353.636369	6.628813
5.992090	339.763009	6.633818
6.266212	331.472000	6.638822
5.670980	335.491632	6.643827
5.795370	333.314462	6.648832
5.488730	338.048197	6.653837
5.908953	337.340151	6.658842
5.752969	334.324201	6.663846
5.657082	342.014737	6.668851
5.956947	339.534819	6.673856
6.064240	350.094759	6.678861
6.058710	345.742242	6.683866
5.930235	333.413984	6.688870
5.762620	334.775437	6.693875
6.139160	328.945663	6.698880
5.616075	340.816115	6.703885
5.778311	338.914596	6.708890
5.924668	338.084940	6.713894
5.643027	343.893627	6.718899
5.812071	336.099983	6.723904
5.715539	352.592409	6.728909
5.769193	337.596973	6.733914
5.796058	343.990088	6.738918
5.965210	346.497870	6.743923
5.905878	331.722627	6.748928
5.917674	347.223615	6.753933
5.891878	335.119719	6.758938
5.911056	340.577543	6.763942
5.588887	340.102879	6.768947
5.591900	336.903825	6.773952
6.040489	341.696404	6.778957
6.072227	336.414211	6.783962
5.744690	341.094271	6.788966
5.890642	341.074620	6.793971
6.043148	326.443365	6.798976
5.874943	340.574137	6.803981
5.779183	320.543157	6.808986
5.718512	323.681744	6.813990
5.599679	320.397378	6.818995
6.067233	338.978125	6.824000
5.787702	330.264488	6.829005
5.650339	319.190509	6.834010
5.618871	323.795702	6.839014
5.576076	329.165154	6.844019
6.005880	334.188470	6.849024
5.741346	341.620686	6.854029
6.077645	336.657778	6.859034
6.064409	330.977662	6.864038
5.899732	308.866200	6.869043
5.575905	304.626841	6.874048
5.505529	315.157650	6.879053
5.593209	315.371761	6.884058
5.411497	322.610653	6.889062
5.693646	335.604648	6.894067
5.839125	333.955698	6.899072
5.937505	340.666645	6.904077
6.010048	328.879548	6.909082
5.953418	332.950834	6.914086
5.914865	337.990586	6.919091
6.063313	319.243826	6.924096
5.650061	315.527853	6.929101
5.486416	310.450291	6.934106
5.689870	320.963509	6.939110
5.478483	327.036436	6.944115
5.748902	328.724735	6.949120
5.705660	327.693827	6.954125
5.963025	338.110021	6.959130
5.965990	339.299211	6.964134
6.048391	336.122520	6.969139
5.964446	322.933057	6.974144
5.400414	321.850868	6.979149
5.880854	327.103535	6.984154
5.895457	328.192822	6.989158
5.861471	320.449979	6.994163
5.660947	309.518784	6.999168
5.585867	322.590888	7.004173
5.820929	330.188435	7.009178
6.076711	333.255295	7.014182
6.133207	322.875457	7.019187
5.852273	321.046541	7.024192
5.598953	312.702138	7.029197
5.679402	305.061597	7.034202
5.570562	313.121154	7.039206
5.567636	318.582435	7.044211
5.968833	320.304028	7.049216
6.041297	324.342430	7.054221
5.609173	314.162545	7.059226
5.585206	316.210188	7.064230
5.282124	321.984261	7.069235
5.491053	327.554723	7.074240
5.531536	330.531926	7.079245
5.755876	333.176595	7.084250
5.889381	331.440933	7.089254
5.784175	350.044993	7.094259
6.062255	339.845567	7.099264
5.425617	338.050235	7.104269
5.861097	330.433152	7.109274
5.838005	339.959960	7.114278
5.524866	334.516663	7.119283
5.916617	331.952744	7.124288
6.004626	333.226688	7.129293
5.847393	337.215659	7.134298
6.170153	332.292839	7.139302
6.094749	338.502655	7.144307
6.323222	333.313027	7.149312
5.780465	330.019149	7.154317
5.567452	310.803837	7.159322
5.757217	309.638343	7.164326
5.344895	309.427747	7.169331
5.975365	328.353124	7.174336
5.612439	334.285278	7.179341
5.848168	337.972227	7.184346
5.666492	347.928857	7.189350
5.578975	336.948300	7.194355
5.750162	337.317011	7.199360
5.535395	344.355442	7.204365
5.826995	340.807443	7.209370
6.242887	338.034092	7.214374
5.531278	341.328458	7.219379
5.945227	342.225458	7.224384
5.952202	343.977183	7.229389
5.973401	339.601497	7.234394
5.896772	330.020816	7.239398
5.869806	315.965032	7.244403
5.808737	312.174896	7.249408
5.500743	330.345625	7.254413
5.443473	330.544482	7.259418
5.684623	343.775866	7.264422
5.704122	344.516366	7.269427
5.647637	337.352859	7.274432
5.961940	350.414594	7.279437
5.910119	342.291713	7.284442
6.013920	334.514620	7.289446
5.963766	340.654040	7.294451
6.252614	334.455180	7.299456
5.861825	317.570985	7.304461
5.681730	311.705043	7.309466
5.824791	315.105944	7.314470
5.646648	321.214790	7.319475
5.679692	312.888794	7.324480
5.566587	311.454372	7.329485
5.811303	307.467625	7.334490
5.635174	310.621137	7.339494
5.977159	325.187663	7.344499
5.959259	320.682063	7.349504
5.715371	323.302015	7.354509
5.518881	310.310534	7.359514
5.627248	316.576972	7.364518
5.522661	334.801259	7.369523
5.839924	331.429578	7.374528
5.595297	330.591579	7.379533
5.878566	338.339768	7.384538
5.918956	326.912060	7.389542
5.992546	340.498734	7.394547
5.968401	336.895801	7.399552
5.822851	349.276594	7.404557
5.729499	332.155952	7.409562
5.803832	323.870940	7.414566
5.854951	320.597911	7.419571
5.615189	312.605732	7.424576
5.819550	325.380949	7.429581
5.671539	337.749465	7.434586
5.802872	338.640124	7.439590
5.529125	341.106566	7.444595
5.899777	339.969677	7.449600
6.003040	345.499752	7.454605
5.812340	339.812637	7.459610
5.777820	327.773389	7.464614
5.715816	338.084595	7.469619
5.580890	335.441842	7.474624
6.028741	341.496906	7.479629
5.854787	335.579372	7.484634
5.728818	324.035358	7.489638
5.678353	342.168913	7.494643
5.938954	340.963844	7.499648
5.948890	334.005072	7.504653
5.623814	334.407244	7.509658
5.573713	326.277773	7.514662
5.568911	341.069494	7.519667
6.287240	341.792250	7.524672
5.803064	340.650089	7.529677
5.757843	324.907672	7.534682
5.476858	322.537748	7.539686
5.834567	332.049180	7.544691
5.714025	329.179542	7.549696
5.784259	337.676136	7.554701
5.723202	331.073346	7.559706
5.986492	341.871438	7.564710
5.775034	343.793432	7.569715
6.122581	334.146288	7.574720
5.835270	326.186864	7.579725
5.652893	322.523302	7.584730
5.543713	315.599020	7.589734
5.314845	327.663815	7.594739
6.067383	339.150895	7.599744
6.013530	351.185121	7.604749
6.041536	335.554610	7.609754
5.854285	316.746553	7.614758
5.946852	319.633334	7.619763
5.833399	314.816833	7.624768
5.655266	323.051771	7.629773
5.636440	319.539759	7.634778
5.909883	312.606148	7.639782
5.714327	321.995449	7.644787
5.879076	307.128168	7.649792
5.525537	309.521683	7.654797
5.728017	317.045234	7.659802
5.624516	307.133411	7.664806
5.477683	326.158429	7.669811
5.977415	320.723818	7.674816
5.877626	332.357094	7.679821
5.994898	335.619667	7.684826
6.104424	318.106574	7.689830
5.433289	310.843225	7.694835
5.476997	314.237546	7.699840
5.547632	329.871673	7.704845
5.757094	330.727943	7.709850
6.234637	334.051130	7.714854
5.939517	336.558885	7.719859
5.870814	310.911037	7.724864
5.635524	316.506804	7.729869
5.489890	324.122867	7.734874
5.973612	329.893890	7.739878
5.621459	338.956550	7.744883
5.940541	330.016240	7.749888
5.919755	336.217497	7.754893
5.860353	329.092417	7.759898
5.629200	319.118328	7.764902
5.436805	323.903763	7.769907
5.738700	332.167899	7.774912
6.199664	340.751974	7.779917
5.873741	330.403576	7.784922
5.678567	311.989080	7.789926
5.780591	321.069157	7.794931
5.702931	318.487038	7.799936
5.543258	332.720874	7.804941
5.552346	336.041528	7.809946
5.928997	335.568104	7.814950
5.769317	343.591347	7.819955
5.669168	332.982941	7.824960
5.689023	336.013999	7.829965
5.821810	340.435268	7.834970
6.010634	340.722119	7.839974
5.762703	338.552664	7.844979
5.613288	338.063587	7.849984
5.879644	335.433892	7.854989
5.552215	335.393496	7.859994
5.733825	333.798998	7.864998
5.647443	342.222054	7.870003
6.453011	338.852959	7.875008
6.163516	340.410684	7.880013
5.552082	338.851854	7.885018
5.615950	328.749275	7.890022
5.411274	345.435814	7.895027
5.617671	341.692351	7.900032
5.514242	343.008946	7.905037
5.937233	333.330999	7.910042
5.856852	335.760814	7.915046
5.122971	349.913785	7.920051
5.536907	338.601552	7.925056
5.776321	342.000016	7.930061
5.882365	350.120836	7.935066
6.102720	340.566386	7.940070
5.768092	342.906322	7.945075
5.706868	345.219239	7.950080
5.755471	347.622519	7.955085
5.972904	342.194167	7.960090
5.687643	335.499952	7.965094
5.783538	339.455590	7.970099
5.993148	335.724280	7.975104
5.805691	336.854719	7.980109
5.782224	341.123296	7.985114
6.197815	340.453942	7.990118
5.946664	339.721589	7.995136
5.902266	342.297389	8.000154
5.667215	349.889169	8.005171
5.764955	347.519709	8.010189
5.969695	338.130846	8.015206
5.776145	348.979181	8.020224
5.769960	346.408256	8.025242
5.655574	345.978114	8.030259
5.318352	349.647509	8.035277
5.666229	340.804256	8.040294
5.630885	338.329418	8.045312
5.405267	339.898522	8.050330
5.377211	339.117187	8.055347
5.478442	344.961631	8.060365
5.798634	355.742098	8.065382
5.738137	357.768165	8.070400
5.943383	361.279985	8.075418
6.083153	371.384995	8.080435
5.928606	365.444863	8.085453
6.026316	363.349957	8.090470
5.688861	364.699904	8.095488
5.874892	357.627140	8.100506
5.475653	367.175981	8.105523
5.316407	367.210453	8.110541
5.849744	367.376247	8.115558
5.888648	370.305069	8.120576
5.893329	368.688636	8.125594
5.931271	378.251034	8.130611
5.979859	367.804193	8.135629
6.104690	369.043839	8.140646
6.014140	377.878453	8.145664
5.986798	378.236236	8.150682
6.183971	370.069825	8.155699
6.070546	372.855259	8.160717
6.077752	366.189202	8.165734
6.075340	377.689252	8.170752
6.146502	376.034000	8.175770
6.182626	369.754727	8.180787
6.275492	373.707030	8.185805
6.290632	349.676707	8.190822
6.030595	353.084705	8.195840
5.731768	352.096489	8.200858
5.469222	352.819324	8.205875
5.604733	362.022448	8.210893
5.914166	369.279619	8.215910
5.926541	382.670816	8.220928
5.917992	379.260822	8.225946
6.187753	376.391039	8.230963
5.962354	372.813054	8.235981
5.954910	368.049065	8.240998
5.971225	374.844086	8.246016
6.032191	379.454633	8.251034
6.304145	377.764764	8.256051
6.135730	368.096686	8.261069
6.454261	369.574222	8.266086
6.051224	366.595265	8.271104
6.199283	371.895900	8.276122
6.325461	384.997872	8.281139
5.960230	374.903041	8.286157
6.261030	368.604388	8.291174
5.977027	369.002385	8.296192
6.222568	368.553717	8.301210
6.195223	354.789447	8.306227
5.815266	352.314954	8.311245
5.996894	365.177853	8.316262
6.091650	376.053614	8.321280
6.001882	371.551828	8.326298
5.992097	374.040160	8.331315
6.122289	380.397624	8.336333
5.957599	369.700180	8.341350
6.206836	374.915536	8.346368
5.871416	374.122398	8.351386
5.998913	377.949357	8.356403
5.649086	381.570242	8.361421
6.397519	375.999860	8.366438
6.230761	374.788980	8.371456
6.219569	380.303916	8.376474
6.493267	377.695445	8.381491
5.929072	376.180768	8.386509
6.020039	368.949327	8.391526
6.241735	381.941657	8.396544
6.366656	387.712976	8.401562
6.404567	381.067349	8.406579
6.090946	387.832021	8.411597
6.321798	382.301708	8.416614
6.012120	373.902288	8.421632
6.359504	376.536628	8.426650
6.388226	382.490273	8.431667
5.947321	391.250402	8.436685
6.118819	378.994974	8.441702
6.076140	375.350490	8.446720
6.282541	378.694877	8.451738
6.241406	378.597235	8.456755
6.068089	380.445324	8.461773
6.188055	374.506358	8.466790
5.716489	379.733668	8.471808
6.097755	387.162626	8.476826
6.053992	404.737721	8.481843
6.066050	403.779686	8.486861
6.052720	397.088433	8.491878
6.370742	414.139797	8.496896
6.446264	400.340440	8.501914
6.586580	400.362689	8.506931
6.121906	408.498551	8.511949
6.226100	407.989978	8.516966
6.436229	416.935289	8.521984
6.330802	415.282455	8.527002
6.338815	407.858871	8.532019
6.085947	414.481491	8.537037
6.328752	417.580342	8.542054
6.292590	422.092510	8.547072
6.122823	406.778939	8.552090
6.185014	410.865443	8.557107
6.164109	412.904247	8.562125
6.430201	409.025186	8.567143
6.252555	408.614421	8.572160
6.352853	407.551043	8.577178
6.480150	403.217208	8.582195
6.382547	410.746453	8.587213
6.651564	406.797507	8.592231
6.701180	407.780700	8.597248
6.354014	415.279621	8.602266
6.320759	410.339786	8.607283
6.419048	412.224215	8.612301
6.301620	400.326465	8.617319
6.245649	417.486923	8.622336
6.291260	411.067294	8.627354
6.400822	405.603315	8.632371
6.225199	418.055172	8.637389
6.552816	430.043183	8.642407
6.466152	433.458745	8.647424
6.360221	443.946273	8.652442
6.864012	436.855248	8.657459
6.743001	415.213004	8.662477
6.597068	420.941567	8.667495
6.396760	412.341958	8.672512
6.734192	414.119491	8.677530
6.537529	410.429699	8.682547
6.439587	408.576880	8.687565
6.347558	400.462080	8.692583
6.398416	409.022091	8.697600
6.090749	405.163502	8.702618
6.736743	415.684677	8.707635
6.222963	436.842670	8.712653
6.645256	437.136316	8.717671
6.610018	429.953027	8.722688
6.277587	436.023237	8.727706
6.742103	431.068518	8.732723
6.849685	435.128982	8.737741
6.521925	435.281375	8.742759
6.952467	437.700724	8.747776
6.607232	429.351031	8.752794
6.480494	409.959761	8.757811
6.370992	426.945580	8.762829
6.774427	428.353015	8.767847
6.774206	432.689143	8.772864
7.006157	418.540216	8.777882
6.607287	423.065034	8.782899
6.365358	418.940524	8.787917
6.141850	410.079467	8.792935
6.439971	429.046363	8.797952
6.461570	431.908479	8.802970
6.811080	438.853288	8.807987
6.642877	431.757103	8.813005
6.719308	433.477703	8.818023
6.561307	428.664704	8.823040
6.690516	431.210161	8.828058
6.714484	429.764268	8.833075
6.720779	439.262231	8.838093
6.880201	445.381610	8.843111
6.678890	435.362046	8.848128
6.313539	441.989677	8.853146
6.549284	445.080172	8.858163
6.803975	446.665547	8.863181
6.760287	434.980280	8.868199
6.912582	438.014422	8.873216
6.868973	434.518393	8.878234
6.802602	437.804545	8.883251
6.846107	439.022224	8.888269
6.561153	434.257517	8.893287
6.837823	444.328496	8.898304
6.700234	440.216035	8.903322
6.966346	443.576325	8.908339
6.757688	444.401172	8.913357
6.448208	438.602055	8.918375
6.671962	442.770549	8.923392
6.707259	446.492050	8.928410
6.483891	442.487702	8.933427
6.534129	440.513833	8.938445
6.257472	446.982403	8.943463
6.754092	458.943954	8.948480
6.620794	465.727738	8.953498
6.928568	470.312261	8.958515
6.958618	468.474095	8.963533
7.117199	467.714004	8.968551
6.968618	468.677762	8.973568
6.681636	469.038359	8.978586
6.892050	465.641377	8.983603
6.822940	467.769791	8.988621
6.853948	468.295158	8.993639
7.122400	462.695813	8.998656
6.415729	465.943439	9.003674
6.862377	473.393747	9.008691
6.981911	474.312340	9.013709
7.055285	475.938750	9.018727
6.812075	469.879932	9.023744
6.967867	477.265361	9.028762
6.833831	471.186281	9.033779
6.823484	477.793016	9.038797
6.767102	478.010186	9.043815
7.112679	469.492276	9.048832
7.046985	471.421340	9.053850
6.784237	472.759589	9.058867
6.890126	476.353271	9.063885
6.942132	478.121884	9.068903
7.160189	476.134340	9.073920
6.827203	475.820495	9.078938
7.008363	467.574498	9.083955
7.256617	473.904030	9.088973
6.772693	472.162173	9.093991
6.792852	476.406756	9.099008
6.754190	475.216825	9.104026
6.724592	468.313501	9.109043
6.801276	477.661600	9.114061
7.119169	468.002477	9.119079
6.942421	465.152149	9.124096
6.741270	474.291315	9.129114
7.043602	476.705512	9.134131
7.065571	476.045720	9.139149
6.894926	475.971525	9.144167
7.295806	482.706333	9.149184
7.340726	478.098210	9.154202
7.285722	472.776759	9.159219
7.319413	473.929707	9.164237
6.935733	475.687690	9.169255
7.129234	467.802675	9.174272
6.933973	473.295987	9.179290
7.128556	473.521171	9.184307
7.209923	473.716758	9.189325
6.985699	480.413809	9.194343
6.857976	471.982678	9.199360
7.150054	483.345137	9.204378
7.508038	486.186114	9.209395
7.158648	486.146237	9.214413
6.842860	476.479100	9.219431
6.845083	483.632975	9.224448
7.373515	493.831791	9.229466
7.123686	492.018540	9.234483
7.572372	495.397570	9.239501
6.955496	496.494663	9.244519
7.293223	499.395620	9.249536
7.334773	503.668416	9.254554
7.109331	503.596496	9.259571
7.570294	504.038718	9.264589
7.155991	488.700275	9.269607
7.235285	480.198835	9.274624
7.078210	479.529227	9.279642
7.309301	491.286252	9.284659
7.528628	487.831066	9.289677
6.899410	481.933710	9.294695
7.310572	494.217942	9.299712
7.515249	503.580714	9.304730
7.346922	495.446267	9.309747
7.302978	487.910870	9.314765
7.150226	489.724189	9.319783
7.454364	488.953914	9.324800
6.999821	489.880405	9.329818
7.208604	497.238605	9.334835
7.537154	504.152010	9.339853
7.147553	511.114825	9.344871
7.157637	510.680955	9.349888
7.271788	505.241472	9.354906
7.165986	503.481392	9.359923
7.199014	495.473186	9.364941
7.040985	509.339300	9.369959
7.007161	496.547920	9.374976
7.154117	492.495004	9.379994
7.417411	499.566955	9.385011
7.231378	503.512493	9.390029
7.187129	505.362462	9.395047
6.995796	503.429592	9.400064
7.117722	508.339888	9.405082
7.221569	530.572018	9.410099
7.407049	528.242435	9.415117
7.021437	536.858271	9.420135
7.445637	534.197795	9.425152
7.711874	534.313924	9.430170
7.690959	530.808009	9.435187
7.770517	533.339169	9.440205
7.516294	541.811345	9.445223
7.863687	529.234766	9.450240
7.682367	525.681401	9.455258
7.581860	507.980577	9.460275
7.434312	512.440793	9.465293
7.394852	508.565404	9.470311
7.436974	498.422457	9.475328
7.306600	509.633374	9.480346
7.396914	505.207480	9.485363
7.563103	514.917114	9.490381
7.653682	526.229120	9.495399
7.495412	516.174365	9.500416
7.298696	520.938931	9.505434
7.563257	528.045408	9.510451
7.707618	525.330950	9.515469
7.819697	535.595025	9.520487
7.731985	524.197464	9.525504
7.167052	516.658478	9.530522
7.318737	514.921169	9.535539
7.680993	523.347238	9.540557
7.716699	531.388975	9.545575
7.641817	531.145142	9.550592
7.723618	534.114606	9.555610
7.462504	536.247865	9.560627
7.725617	535.335694	9.565645
7.574036	533.948856	9.570663
7.852885	534.956099	9.575680
8.001677	529.801515	9.580698
7.414066	521.811645	9.585715
7.280667	518.736766	9.590733
7.680494	530.148644	9.595751
7.594573	535.716361	9.600768
7.603074	537.378188	9.605786
7.390973	537.379916	9.610803
7.127222	531.945988	9.615821
7.534090	529.916231	9.620839
7.006344	538.118838	9.625856
7.644397	533.919539	9.630874
7.286271	542.146064	9.635891
7.562526	556.259749	9.640909
7.687708	562.365598	9.645927
7.838189	559.397711	9.650944
7.687944	558.335710	9.655962
8.095681	563.775596	9.660979
7.858689	565.611589	9.665997
7.569679	561.677459	9.671015
7.723310	560.971789	9.676032
8.090196	564.205858	9.681050
7.816527	566.621955	9.686067
8.135162	551.200177	9.691085
7.949863	542.333066	9.696103
7.558622	541.870558	9.701120
7.655306	528.986123	9.706138
7.635187	542.937952	9.711155
8.146077	549.267385	9.716173
7.909082	539.979187	9.721191
7.776302	535.452541	9.726208
7.842599	539.248098	9.731226
7.811414	543.223032	9.736243
7.801342	538.364735	9.741261
7.784918	555.414987	9.746279
7.500257	566.757411	9.751296
7.888941	563.423998	9.756314
7.817208	569.298771	9.761331
7.758967	562.317848	9.766349
7.958668	568.361531	9.771367
7.811999	562.502150	9.776384
8.436996	562.587314	9.781402
8.222728	572.915167	9.786419
8.215853	563.161712	9.791437
7.799865	551.616753	9.796455
7.805643	551.660082	9.801472
8.019671	557.092447	9.806490
8.043143	568.623278	9.811507
8.356810	562.070077	9.816525
8.036378	543.280212	9.821543
8.062139	544.453342	9.826560
8.219617	541.405466	9.831578
7.809259	542.788940	9.836595
8.084368	527.730607	9.841613
7.954545	532.058663	9.846631
7.812347	539.304615	9.851648
8.381880	540.083277	9.856666
7.981189	531.764315	9.861683
7.707335	546.749979	9.866701
8.130153	548.782390	9.871719
8.217119	552.123432	9.876736
8.139312	546.600405	9.881754
7.680982	538.830113	9.886771
8.135840	554.910276	9.891789
8.284220	561.924517	9.896807
7.895059	568.218255	9.901824
8.534389	550.982136	9.906842
8.226026	551.292436	9.911859
8.018027	544.802043	9.916877
7.637539	543.167049	9.921895
8.270252	552.863567	9.926912
8.290702	560.806723	9.931930
8.279358	559.991201	9.936947
8.418282	546.961280	9.941965
8.040545	539.610704	9.946983
7.890237	536.320721	9.952000
8.229076	550.699150	9.957018
7.997314	557.914962	9.962035
8.480235	560.679571	9.967053
8.462721	563.427916	9.972071
8.290019	544.775848	9.977088
8.061157	543.195991	9.982106
7.910067	550.244526	9.987123
8.387081	551.981269	9.992141
8.215888	557.281487	9.997159
8.329916	559.368594	10.002176
8.319354	553.778224	10.007194
8.218420	564.757345	10.012211
8.101795	557.457368	10.017229
7.902372	560.571885	10.022247
8.323343	566.940660	10.027264
8.346992	561.209228	10.032282
8.463404	566.019418	10.037299
8.498700	561.608442	10.042317
8.464003	559.338599	10.047335
8.518367	560.885945	10.052352
8.319465	564.669411	10.057370
8.000530	566.429881	10.062387
8.170970	559.504647	10.067405
8.230998	571.985960	10.072423
8.264814	569.680135	10.077440
8.314101	547.988957	10.082458
8.086125	559.833735	10.087475
8.163041	560.156252	10.092493
8.164297	565.176989	10.097511
8.324307	565.413903	10.102528
8.194130	562.745610	10.107546
8.117365	573.332786	10.112563
8.099517	558.553858	10.117581
8.310331	567.417086	10.122599
8.500988	588.982436	10.127616
8.593141	584.303770	10.132634
8.245122	585.582805	10.137651
8.186676	596.776194	10.142669
8.705080	586.369223	10.147687
8.539818	595.647996	10.152704
8.672127	594.563812	10.157722
8.359534	600.122883	10.162739
8.550072	594.100204	10.167757
8.568838	589.786485	10.172775
8.255404	600.451784	10.177792
8.819967	587.411948	10.182810
8.736669	597.795035	10.187827
8.246492	585.434856	10.192845
8.228348	577.242127	10.197863
8.345063	590.222655	10.202880
8.555338	592.244193	10.207898
8.744134	594.414263	10.212915
8.293352	589.953207	10.217933
8.692814	598.673283	10.222951
8.251685	597.596896	10.227968
8.635160	584.137311	10.232986
8.529675	590.945186	10.238003
8.618653	591.975871	10.243021
8.593837	591.989280	10.248039
8.818259	602.961628	10.253056
8.580865	602.389806	10.258074
8.754589	598.957523	10.263091
8.596916	587.280548	10.268109
8.703210	594.560172	10.273127
8.426894	597.771951	10.278144
8.661696	599.543493	10.283162
8.722144	590.420103	10.288179
8.291764	594.388167	10.293197
8.852946	595.389047	10.298215
8.537037	602.441336	10.303232
8.549933	592.744727	10.308250
8.237669	599.998416	10.313267
8.324920	603.197412	10.318285
8.793267	607.927225	10.323303
8.772044	611.244204	10.328320
9.028118	609.001380	10.333338
8.683685	612.952826	10.338355
8.789734	615.372549	10.343373
8.962394	623.702139	10.348391
8.641759	613.448706	10.353408
8.759953	612.341486	10.358426
8.788030	622.154869	10.363443
8.698330	619.013165	10.368461
8.942431	617.169848	10.373479
8.637817	614.260635	10.378496
8.520023	608.229456	10.383514
8.680723	623.996010	10.388531
8.827717	617.945431	10.393549
8.951289	617.638944	10.398567
8.878755	619.335566	10.403584
9.225899	606.405521	10.408602
9.005383	609.535975	10.413619
8.942325	616.895791	10.418637
9.273334	611.406519	10.423655
8.885249	616.399911	10.428672
9.211525	615.237997	10.433690
9.161676	606.453774	10.438707
8.889351	610.031003	10.443725
8.895549	595.750051	10.448743
8.890501	596.896454	10.453760
8.804017	589.462353	10.458778
8.894288	598.394976	10.463795
8.740258	611.323267	10.468813
9.300009	611.122008	10.473831
8.895791	624.622840	10.478848
9.083361	614.475973	10.483866
8.865552	611.764598	10.488883
8.897287	615.546652	10.493901
9.373205	625.043715	10.498919
9.230383	619.622370	10.503936
9.057945	612.643541	10.508954
9.072042	615.954987	10.513971
9.009491	618.448464	10.518989
9.064356	611.288854	10.524007
8.792694	618.249010	10.529024
8.687162	621.298333	10.534042
9.065520	613.365356	10.539059
8.565956	615.068925	10.544077
9.135046	615.882374	10.549095
9.071238	613.610774	10.554112
8.916851	613.982156	10.559130
8.987156	619.822068	10.564147
8.999147	624.348833	10.569165
8.870481	615.232971	10.574183
9.197403	618.343925	10.579200
8.988767	618.263059	10.584218
9.270917	623.586940	10.589235
9.252593	621.746870	10.594253
9.218268	614.023720	10.599271
9.102155	620.255759	10.604288
8.951220	622.283402	10.609306
9.584086	637.676185	10.614323
9.142578	629.433001	10.619341
9.456540	629.355459	10.624359
9.493851	618.989134	10.629376
9.227524	620.627757	10.634394
9.106609	621.909081	10.639411
8.994212	623.277433	10.644429
9.100293	621.351599	10.649447
9.118981	633.675330	10.654464
9.453278	639.376056	10.659482
9.307552	644.899528	10.664499
9.295226	649.259696	10.669517
9.416821	639.852145	10.674535
9.588649	644.281288	10.679552
9.597194	641.786908	10.684570
9.455058	626.645544	10.689587
9.407221	627.107530	10.694605
9.283735	616.192042	10.699623
9.032381	622.347442	10.704640
9.215800	634.203549	10.709658
9.318014	640.653852	10.714675
9.428254	647.535247	10.719693
9.625188	647.987284	10.724711
9.529906	651.940727	10.729728
9.387948	643.293994	10.734746
9.570587	639.371155	10.739763
9.444310	641.956672	10.744781
9.473352	633.573486	10.749799
9.174134	639.777417	10.754816
9.673810	640.074722	10.759834
9.373612	635.823591	10.764851
9.240643	649.865768	10.769869
9.604525	635.355171	10.774887
9.537741	643.958974	10.779904
9.476017	646.938321	10.784922
9.545254	649.136598	10.789939
9.436242	649.084304	10.794957
9.505195	640.934704	10.799975
9.681921	642.844739	10.804992
9.482206	642.472140	10.810010
9.893515	642.701239	10.815027
9.640100	645.912593	10.820045
9.559093	634.375055	10.825063
9.129555	649.495650	10.830080
8.969464	647.362209	10.835098
9.498083	642.214352	10.840115
9.393658	650.328592	10.845133
9.382586	636.981279	10.850151
9.338963	647.424450	10.855168
9.441257	647.080271	10.860186
9.482144	652.893245	10.865203
9.512684	663.346895	10.870221
9.703369	669.019639	10.875239
9.725123	670.288079	10.880256
9.693903	667.698940	10.885274
9.662397	654.121285	10.890291
9.726571	678.218592	10.895309
9.829254	665.538248	10.900327
9.861235	676.319886	10.905344
9.686507	673.920489	10.910362
9.945915	678.282269	10.915379
9.732077	672.120950	10.920397
9.758071	670.046712	10.925415
9.384589	667.236643	10.930432
9.177124	666.739025	10.935450
9.198418	666.360199	10.940467
9.660869	673.896478	10.945485
9.978693	669.949296	10.950503
10.130342	669.786732	10.955520
9.907205	674.732205	10.960538
10.130513	670.812454	10.965555
9.696857	673.190515	10.970573
10.068883	670.004860	10.975591
10.354297	676.082487	10.980608
9.976085	672.670396	10.985626
10.104940	662.870374	10.990643
10.069677	678.427837	10.995661
9.872139	676.268701	11.000679
10.091004	670.317297	11.005696
9.905148	665.985128	11.010714
9.740384	660.781804	11.015731
9.731964	674.665630	11.020749
9.423841	668.711590	11.025767
9.940517	662.836604	11.030784
9.821576	676.649385	11.035802
9.951883	663.305147	11.040819
9.927756	676.923191	11.045837
9.804658	673.578426	11.050855
9.939322	678.275333	11.055872
9.934363	676.461566	11.060890
10.087687	678.299531	11.065907
9.921409	675.267647	11.070925
9.892711	669.345565	11.075943
10.238652	676.376234	11.080960
9.823703	674.734003	11.085978
10.114537	686.024202	11.090995
9.817494	673.961907	11.096013
10.014261	667.685761	11.101031
9.988537	671.227520	11.106048
9.877227	673.845410	11.111066
10.209060	674.844360	11.116083
9.945781	680.231627	11.121101
10.031352	693.428550	11.126119
10.083209	692.069786	11.131136
10.093919	704.511581	11.136154
10.143672	701.370104	11.141171
10.138723	697.179996	11.146189
10.320698	703.791395	11.151207
10.248312	702.837108	11.156224
9.995059	698.020025	11.161242
10.295560	698.752485	11.166259
10.321739	701.661264	11.171277
10.097312	695.700412	11.176295
10.152168	700.760127	11.181312
9.662469	704.560783	11.186330
10.116830	698.099098	11.191347
10.012343	710.401155	11.196365
10.103091	702.541605	11.201383
10.439751	695.170549	11.206400
10.244856	702.708849	11.211418
10.409125	703.421628	11.216435
10.264269	711.056233	11.221453
10.065008	705.706821	11.226471
10.348662	699.464388	11.231488
10.203300	702.759809	11.236506
10.214930	693.669263	11.241523
10.233210	704.027028	11.246541
9.994993	701.672290	11.251559
10.682288	710.315764	11.256576
10.289585	710.626658	11.261594
10.519041	708.965508	11.266611
10.261559	707.039824	11.271629
10.568919	720.385055	11.276647
10.628706	708.090101	11.281664
10.461112	710.470661	11.286682
10.331207	700.405046	11.291699
10.637322	701.041951	11.296717
10.530363	705.659958	11.301735
10.749110	695.451355	11.306752
10.639134	699.896263	11.311770
10.458073	698.387798	11.316787
10.641183	701.445559	11.321805
10.272257	694.229239	11.326823
10.321174	703.676482	11.331840
10.497843	698.851999	11.336858
10.354095	687.147531	11.341875
10.584973	695.272372	11.346893
10.631265	718.529929	11.351911
10.850998	706.777965	11.356928
10.356596	699.862171	11.361946
10.727607	692.286918	11.366963
10.490359	693.987264	11.371981
10.435196	700.752582	11.376999
10.997533	693.462934	11.382016
10.391427	700.399783	11.387034
10.594055	714.294754	11.392051
10.920471	716.496925	11.397069
10.679994	716.522034	11.402087
10.591082	701.741499	11.407104
10.819004	707.645107	11.412122
10.715025	698.383323	11.417139
10.596535	703.801560	11.422157
10.475107	709.744126	11.427175
10.971607	710.408007	11.432192
10.778174	708.383924	11.437210
10.832806	706.829062	11.442227
10.502718	691.502496	11.447245
10.726646	709.676580	11.452263
10.968668	716.490016	11.457280
10.899263	724.557777	11.462298
10.521591	708.503343	11.467315
10.788485	710.525490	11.472333
10.769395	719.636256	11.477351
11.285695	720.514786	11.482368
10.936843	709.322126	11.487386
10.538503	711.060337	11.492403
10.798131	717.766872	11.497421
11.051650	718.711823	11.502439
11.114133	710.872476	11.507456
10.771882	702.534810	11.512474
10.849620	696.293083	11.517491
10.899052	697.001764	11.522509
10.425022	709.061918	11.527527
10.828936	718.305223	11.532544
10.726353	724.658255	11.537562
10.586244	720.230542	11.542579
10.751224	719.949123	11.547597
10.638718	727.528174	11.552615
10.820249	724.539615	11.557632
10.613237	721.204833	11.562650
10.668666	721.694823	11.567667
10.810882	735.690795	11.572685
11.253481	752.543081	11.577703
11.332171	744.612817	11.582720
10.935559	730.262325	11.587738
10.719616	731.091483	11.592755
11.218686	747.808683	11.597773
11.018378	741.553701	11.602791
11.154824	744.401028	11.607808
10.883276	740.852290	11.612826
11.336310	742.614900	11.617843
11.350615	740.160630	11.622861
11.101573	727.986635	11.627879
11.173529	724.961596	11.632896
11.124116	720.869968	11.637914
11.014911	714.569163	11.642931
11.349807	724.429204	11.647949
11.126517	723.040964	11.652967
11.173518	722.620239	11.657984
10.927606	726.878168	11.663002
11.325072	738.530392	11.668019
11.657909	738.598218	11.673037
11.173910	728.850001	11.678055
11.271518	726.963353	11.683072
11.043647	727.459862	11.688090
11.264804	728.914816	11.693107
11.403633	734.273810	11.698125
11.106447	732.767758	11.703143
11.483266	740.980208	11.708160
11.358018	736.796316	11.713178
11.458279	722.538394	11.718195
11.257386	724.091034	11.723213
11.226741	720.564516	11.728231
11.581291	718.729130	11.733248
11.586066	719.709898	11.738266
11.635085	725.098740	11.743283
11.459294	724.394185	11.748301
11.119353	718.924799	11.753319
11.249071	715.748699	11.758336
11.386287	717.485050	11.763354
11.313278	716.919026	11.768371
11.255581	713.554539	11.773389
11.172373	721.185801	11.778407
11.599435	734.225106	11.783424
11.543367	743.228068	11.788442
11.601612	735.089570	11.793459
11.590130	719.779332	11.798477
11.383221	711.316314	11.803495
11.385845	702.255576	11.808512
11.127480	719.217660	11.813530
11.231142	737.757757	11.818547
11.563521	730.393670	11.823565
11.367879	738.137231	11.828583
11.605614	739.829432	11.833600
11.617859	744.062695	11.838618
11.931729	744.177674	11.843635
11.754204	739.661142	11.848653
11.587985	749.779596	11.853671
11.653537	748.216708	11.858688
11.486394	737.494181	11.863706
11.664284	749.281803	11.868723
11.747699	735.752353	11.873741
11.202358	735.670593	11.878759
11.373383	741.065570	11.883776
11.447741	735.805823	11.888794
11.622399	751.273654	11.893811
11.689652	740.744775	11.898829
11.786402	738.220782	11.903847
11.999217	733.671496	11.908864
11.819649	740.304842	11.913882
11.361182	741.781075	11.918899
11.627248	745.889361	11.923917
11.632198	751.442908	11.928935
11.812458	742.436370	11.933952
11.586628	751.693154	11.938970
11.343840	746.704004	11.943987
11.673684	745.693003	11.949005
11.550266	757.969658	11.954023
12.054366	756.066654	11.959040
12.095551	760.642529	11.964058
11.614466	754.485184	11.969075
12.194404	760.374681	11.974093
12.307103	757.633589	11.979111
11.718037	749.959428	11.984128
11.539251	741.971676	11.989146
11.821695	750.997343	11.994163
11.798490	753.566726	11.999181
12.037135	761.144420	12.004199
11.992396	766.327057	12.009216
12.208081	771.664552	12.014234
12.054937	752.207620	12.019251
11.857306	746.163658	12.024269
11.660919	760.963791	12.029287
12.150206	768.994528	12.034304
12.281178	768.235594	12.039322
11.826454	759.012955	12.044339
12.011761	751.899123	12.049357
11.920864	768.273275	12.054375
12.330074	757.940119	12.059392
12.135214	762.193212	12.064410
11.607850	760.830521	12.069427
12.225065	757.240357	12.074445
12.154318	771.414893	12.079463
12.210631	771.847941	12.084480
12.127548	760.607295	12.089498
11.629075	771.885518	12.094515
11.877943	773.358225	12.099533
12.036447	779.610409	12.104551
12.108169	770.204292	12.109568
12.399803	762.562550	12.114586
12.001187	772.124131	12.119603
12.354986	768.370108	12.124621
12.071427	768.506110	12.129639
12.066467	766.266296	12.134656
12.416704	770.705386	12.139674
12.372821	768.610527	12.144691
12.613217	761.772086	12.149709
12.416445	765.353287	12.154727
12.476058	761.115178	12.159744
12.589169	768.037195	12.164762
12.180984	769.123696	12.169779
12.359203	766.126182	12.174797
12.344676	768.678429	12.179815
12.328611	762.748025	12.184832
12.455787	763.801137	12.189850
11.973348	771.908387	12.194867
12.134093	771.536113	12.199885
12.429283	769.627971	12.204903
12.306407	765.835024	12.209920
12.576428	769.740724	12.214938
12.394159	769.788270	12.219955
12.371947	769.302649	12.224973
12.654937	774.456029	12.229991
12.286510	772.014385	12.235008
12.385843	772.030433	12.240026
11.934771	775.197039	12.245043
12.173408	767.165964	12.250061
12.355084	774.591642	12.255079
12.343469	770.251082	12.260096
12.446872	765.337073	12.265114
12.160022	777.405816	12.270131
12.276597	777.185630	12.275149
12.583198	790.982318	12.280167
12.772027	804.226262	12.285184
12.777086	795.218745	12.290202
12.522413	800.298583	12.295219
12.768810	788.949491	12.300237
12.752017	788.971110	12.305255
12.506952	789.817457	12.310272
12.592166	778.686132	12.315290
12.755099	796.415420	12.320307
12.454649	790.302344	12.325325
12.752251	794.273156	12.330343
12.725558	799.752779	12.335360
12.714651	790.997078	12.340378
12.502399	796.000840	12.345395
12.929228	803.517509	12.350413
12.823654	800.867416	12.355431
12.521531	793.605874	12.360448
13.008784	801.428659	12.365466
12.520137	795.619627	12.370483
12.772260	783.521706	12.375501
13.107651	787.688569	12.380519
12.614070	791.534033	12.385536
12.884607	784.990665	12.390554
12.871533	788.918634	12.395571
12.598382	787.285733	12.400589
13.075860	797.107695	12.405607
12.851736	796.098281	12.410624
13.083587	787.942026	12.415642
12.724181	797.424893	12.420659
12.952204	795.211687	12.425677
13.223760	795.835076	12.430695
12.582385	797.305257	12.435712
13.063667	795.023968	12.440730
12.927957	796.563245	12.445747
12.751518	799.721540	12.450765
13.060339	794.096833	12.455783
12.901442	799.199534	12.460800
13.000585	797.883846	12.465818
12.751698	800.381298	12.470835
12.865530	797.299192	12.475853
12.728022	805.005270	12.480871
12.613281	799.712016	12.485888
12.909354	794.325994	12.490906
12.992384	793.126441	12.495923
12.776605	796.193068	12.500941
12.907823	808.641302	12.505959
13.035677	821.396188	12.510976
13.088363	826.730837	12.515994
13.046415	826.759554	12.521011
13.259982	818.568279	12.526029
13.281566	824.030878	12.531047
12.692605	822.990262	12.536064
13.371621	832.370406	12.541082
12.852771	834.951187	12.546099
12.946945	821.953325	12.551117
12.935427	820.841169	12.556135
12.974499	830.501463	12.561152
13.457659	819.755892	12.566170
12.938127	820.487451	12.571187
12.943944	825.163559	12.576205
13.240453	821.046112	12.581223
13.018271	830.924068	12.586240
13.044659	842.404125	12.591258
13.463764	850.815130	12.596275
13.599295	855.710767	12.601293
13.307937	845.752418	12.606311
13.231582	860.653749	12.611328
13.570879	846.522381	12.616346
13.387331	848.056535	12.621363
13.564764	848.773569	12.626381
13.679810	844.978042	12.631399
13.118646	843.566991	12.636416
13.343358	842.196911	12.641434
13.513823	846.790422	12.646451
13.150168	854.494084	12.651469
13.678201	852.467399	12.656487
13.607941	854.321479	12.661504
13.364238	851.800320	12.666522
13.482079	852.047001	12.671539
13.360101	855.020045	12.676557
13.435274	859.903049	12.681575
13.444512	856.452307	12.686592
13.581578	851.854898	12.691610
13.525935	850.803303	12.696627
13.480740	842.554730	12.701645
13.767936	855.354103	12.706663
13.494083	858.335164	12.711680
13.797814	846.623596	12.716698
13.764387	858.936714	12.721715
13.568520	860.277135	12.726733
13.670620	851.977076	12.731751
13.727730	854.243552	12.736768
13.762736	843.779626	12.741786
13.638816	848.709601	12.746803
13.706850	853.316007	12.751821
13.733788	846.144899	12.756839
13.514236	847.548992	12.761856
14.010431	841.345794	12.766874
14.068824	844.899654	12.771891
13.873826	843.645829	12.776909
14.004380	839.873120	12.781927
13.605403	857.854614	12.786944
14.278177	842.907282	12.791962
13.825102	842.151492	12.796979
13.979571	845.131713	12.801997
14.297276	838.868117	12.807015
14.043313	845.090274	12.812032
14.126421	838.386903	12.817050
14.004055	822.869884	12.822067
13.780023	822.103454	12.827085
13.941955	820.645381	12.832103
13.924936	824.757015	12.837120
13.838966	826.351618	12.842138
14.207657	831.778769	12.847155
13.862371	828.856958	12.852173
14.149769	824.769339	12.857191
14.091602	829.408136	12.862208
14.043203	818.363994	12.867226
13.824280	817.868167	12.872243
14.033980	836.249739	12.877261
14.012284	839.440600	12.882279
14.000018	844.962159	12.887296
14.319019	844.454632	12.892314
14.213688	836.395368	12.897331
14.165673	847.057097	12.902349
14.459905	834.012100	12.907367
14.142910	828.236124	12.912384
14.131475	819.893908	12.917402
14.040562	819.172893	12.922419
14.120664	824.689441	12.927437
14.184537	830.981716	12.932455
14.389111	838.851964	12.937472
14.130099	834.196696	12.942490
14.283945	830.931587	12.947507
13.987382	840.158474	12.952525
14.380171	841.911598	12.957543
14.540087	845.130811	12.962560
14.230696	834.417890	12.967578
14.549229	842.125115	12.972595
14.201780	845.026186	12.977613
14.227185	843.062475	12.982631
14.361447	846.642319	12.987648
14.410696	838.088611	12.992666
14.443495	833.965141	12.997683
14.044110	844.199077	13.002701
14.501613	831.687087	13.007719
14.566432	840.156753	13.012736
14.311217	843.747126	13.017754
14.513527	839.234173	13.022771
14.654439	840.859502	13.027789
14.575857	831.959748	13.032807
14.480721	846.532646	13.037824
14.452955	838.959851	13.042842
14.570557	834.548536	13.047859
14.269500	839.919679	13.052877
14.283596	832.318237	13.057895
14.291206	837.473756	13.062912
14.255543	838.631283	13.067930
14.402654	835.562891	13.072947
14.204336	840.734898	13.077965
14.317276	828.523053	13.082983
14.544472	841.880935	13.088000
14.557444	833.102537	13.093018
14.309633	846.500133	13.098035
14.382478	868.027475	13.103053
15.004230	867.153770	13.108071
15.225213	867.251746	13.113088
14.793588	859.552869	13.118106
14.874659	843.650501	13.123123
14.938818	845.947430	13.128141
14.710722	839.393805	13.133159
14.444908	837.210632	13.138176
14.288086	846.510303	13.143194
14.850363	843.215913	13.148211
15.005046	857.755989	13.153229
14.961814	853.502414	13.158247
14.908076	845.643348	13.163264
14.873127	850.508889	13.168282
14.991240	848.073054	13.173299
14.742085	854.524838	13.178317
14.864722	844.965535	13.183335
14.809053	845.252026	13.188352
15.020844	864.804121	13.193370
14.833659	863.549070	13.198387
14.766971	870.458272	13.203405
15.335356	859.017659	13.208423
15.078868	872.858455	13.213440
15.117451	860.806563	13.218458
14.986234	843.511012	13.223475
14.996968	839.637155	13.228493
14.685546	846.256484	13.233511
15.120764	849.634538	13.238528
15.073873	859.118965	13.243546
14.884321	858.959367	13.248563
14.902588	863.993302	13.253581
14.778088	857.881037	13.258599
14.896965	855.628121	13.263616
14.966504	860.007071	13.268634
15.150413	854.625982	13.273651
14.625372	863.371119	13.278669
14.925713	862.513060	13.283687
14.895826	861.536325	13.288704
14.871996	877.556081	13.293722
15.446046	869.983655	13.298739
15.291774	882.530321	13.303757
15.986819	884.059364	13.308775
15.962737	861.625051	13.313792
15.745376	860.570392	13.318810
15.523233	854.094725	13.323827
15.136866	860.337632	13.328845
15.390137	862.005320	13.333863
15.243168	854.807807	13.338880
14.969286	855.273658	13.343898
15.286577	856.047675	13.348915
15.649122	856.647342	13.353933
15.184731	853.901980	13.358951
15.460233	856.484537	13.363968
15.191702	852.884810	13.368986
15.334558	854.689720	13.374003
15.362490	856.875559	13.379021
15.216897	863.838148	13.384039
15.322627	864.118285	13.389056
15.282098	866.873439	13.394074
15.262824	885.556030	13.399091
15.271732	890.471516	13.404109
15.545930	880.250964	13.409127
15.699371	883.149300	13.414144
15.312033	881.057748	13.419162
15.678288	870.598711	13.424179
15.568900	870.865216	13.429197
15.634705	882.500072	13.434215
15.591048	869.675251	13.439232
15.700429	880.208196	13.444250
15.887660	878.244373	13.449267
15.709247	881.705954	13.454285
15.494349	878.508080	13.459303
15.704208	876.881544	13.464320
15.830899	882.763202	13.469338
15.865272	881.486059	13.474355
15.715336	881.077252	13.479373
15.708178	880.665010	13.484391
15.859555	866.714550	13.489408
15.947656	873.571098	13.494426
16.375329	869.354192	13.499443
15.915116	877.940854	13.504461
15.844392	872.801630	13.509479
15.945603	877.412312	13.514496
15.838789	881.948289	13.519514
15.849090	878.513156	13.524531
16.177470	878.303965	13.529549
15.970789	878.150206	13.534567
15.955635	858.624199	13.539584
15.793825	869.120732	13.544602
15.855786	873.030650	13.549619
15.666275	872.359797	13.554637
15.815324	872.910863	13.559655
16.058879	874.958777	13.564672
15.668371	878.993240	13.569690
16.141971	879.032700	13.574707
15.875845	881.965216	13.579725
15.645270	885.075203	13.584743
15.842532	882.529130	13.589760
15.975570	877.427408	13.594778
15.733160	884.944826	13.599795
15.829514	881.931717	13.604813
15.975592	896.343783	13.609831
16.507627	896.175268	13.614848
16.215657	897.066839	13.619866
16.551715	895.417373	13.624883
16.232838	881.837232	13.629901
16.009803	882.711690	13.634919
16.389744	882.342939	13.639936
16.172467	886.899382	13.644954
16.413106	892.640110	13.649971
16.267370	894.534423	13.654989
16.352973	897.825250	13.660007
16.511515	885.599909	13.665024
16.012688	889.215837	13.670042
15.960073	886.816214	13.675059
15.956719	898.275720	13.680077
16.156282	894.766748	13.685095
16.424885	887.390498	13.690112
16.594513	893.663070	13.695130
16.745145	891.263159	13.700147
16.582932	892.077594	13.705165
16.134500	894.868260	13.710183
16.533269	897.942759	13.715200
16.701588	891.421679	13.720218
16.538036	887.205884	13.725235
16.793077	897.965329	13.730253
16.248192	893.304342	13.735271
16.701505	891.750116	13.740288
16.553529	900.265775	13.745306
16.359636	892.302413	13.750323
16.665693	897.139785	13.755341
16.477279	904.118566	13.760359
16.678761	896.345724	13.765376
16.382933	896.388972	13.770394
16.365345	898.427312	13.775411
16.582748	893.489095	13.780429
16.575097	893.632361	13.785447
17.068494	885.763291	13.790464
16.585534	894.675422	13.795482
16.840839	891.848850	13.800499
16.736635	885.812292	13.805517
16.823505	893.205536	13.810535
16.875280	886.450250	13.815552
16.666342	885.031346	13.820570
16.749411	892.961682	13.825587
16.609789	888.193017	13.830605
16.532907	893.443843	13.835623
16.867127	906.172768	13.840640
17.003012	918.711867	13.845658
17.029510	911.136852	13.850675
17.029992	899.510633	13.855693
16.610886	903.798896	13.860711
16.943507	917.799892	13.865728
17.010358	910.647752	13.870746
16.653531	920.521606	13.875763
16.911353	915.444504	13.880781
16.753346	921.973552	13.885799
17.061353	914.565870	13.890816
16.852733	918.287816	13.895834
16.953395	917.148610	13.900851
16.866953	914.975193	13.905869
16.852834	920.563339	13.910887
17.126865	906.615722	13.915904
16.902559	915.380037	13.920922
16.728683	920.895382	13.925939
16.913161	927.651642	13.930957
17.084398	937.770978	13.935975
17.225055	945.474560	13.940992
17.009769	945.404201	13.946010
17.047340	951.217791	13.951027
17.639606	949.181032	13.956045
17.299131	955.034921	13.961063
17.633524	943.873919	13.966080
17.568763	948.213972	13.971098
17.336568	936.365405	13.976115
17.404677	926.697835	13.981133
17.319387	928.854085	13.986151
17.316540	916.609828	13.991168
17.680899	932.852838	13.996186
17.241163	913.538466	14.001203
17.386925	917.239601	14.006221
17.295771	924.490334	14.011239
17.686767	932.198869	14.016256
17.713660	927.044334	14.021274
17.272255	924.124943	14.026291
17.532991	919.429243	14.031309
17.269373	934.678719	14.036327
18.149953	930.977828	14.041344
17.569950	934.682225	14.046362
17.451324	918.315609	14.051379
17.457524	907.669964	14.056397
17.218000	926.106235	14.061415
17.554268	937.525177	14.066432
17.873382	937.446828	14.071450
17.721223	935.274239	14.076467
17.596161	931.137610	14.081485
17.683254	939.370299	14.086503
17.592677	936.904032	14.091520
17.522928	945.224416	14.096538
17.443904	949.834953	14.101555
17.728037	943.724907	14.106573
17.644234	948.260452	14.111591
17.477696	939.740506	14.116608
17.885857	943.088102	14.121626
17.458608	946.746476	14.126643
17.778327	946.955217	14.131661
17.655653	950.243972	14.136679
17.966547	938.348182	14.141696
17.734242	940.420169	14.146714
17.674133	945.516901	14.151731
18.187664	950.255506	14.156749
17.876894	952.567011	14.161767
17.814194	946.789023	14.166784
17.974334	944.854684	14.171802
18.133730	964.102666	14.176819
18.185306	948.968548	14.181837
17.992082	940.733655	14.186855
17.985786	935.814697	14.191872
17.987487	943.584232	14.196890
17.790639	966.359489	14.201907
18.202644	961.163540	14.206925
18.457006	964.295392	14.211943
18.164400	960.885611	14.216960
18.101895	947.227382	14.221978
17.999578	961.391235	14.226995
18.289360	966.676154	14.232013
17.969157	972.867707	14.237031
18.326445	967.080714	14.242048
18.504519	968.880117	14.247066
18.175457	977.376848	14.252083
18.415936	961.181151	14.257101
18.314108	967.086017	14.262119
18.188516	967.007916	14.267136
17.922590	968.678066	14.272154
18.153417	969.645521	14.277171
18.353795	966.221615	14.282189
18.088902	974.389547	14.287207
18.132366	972.268355	14.292224
18.099449	966.435200	14.297242
18.094670	972.608891	14.302259
18.473301	965.448905	14.307277
18.063137	964.474942	14.312295
18.345628	976.849097	14.317312
18.738406	985.065471	14.322330
18.441629	988.072236	14.327347
18.674834	984.712612	14.332365
18.504287	988.277125	14.337383
18.639251	978.898860	14.342400
18.657282	983.121806	14.347418
18.669501	985.695140	14.352435
19.051339	975.549188	14.357453
18.333267	974.756014	14.362471
18.364961	970.061473	14.367488
18.671043	976.568320	14.372506
18.742662	983.427493	14.377523
18.948142	980.289970	14.382541
18.792420	982.031218	14.387559
18.929553	986.939264	14.392576
18.795835	981.920335	14.397594
18.452741	980.162672	14.402611
18.830452	979.339823	14.407629
18.879177	987.890978	14.412647
19.032320	983.682345	14.417664
18.946495	980.060277	14.422682
19.238615	983.669065	14.427699
18.997768	971.995403	14.432717
18.644811	979.902574	14.437735
18.882275	975.945825	14.442752
18.743851	984.406377	14.447770
18.669294	988.000032	14.452787
18.915647	985.102263	14.457805
19.177769	980.422109	14.462823
19.193109	987.457363	14.467840
19.298879	983.167787	14.472858
18.985399	989.825363	14.477875
19.184982	987.351497	14.482893
19.326260	994.032498	14.487911
18.918736	986.276139	14.492928
18.803100	984.905725	14.497946
19.159211	986.828717	14.502963
19.359571	985.370922	14.507981
19.197490	980.350125	14.512999
19.046111	981.323815	14.518016
19.311197	984.630719	14.523034
19.218164	988.785859	14.528051
19.400401	981.404168	14.533069
19.263604	972.481906	14.538087
19.395260	978.283920	14.543104
19.371423	973.553896	14.548122
19.243959	983.852606	14.553139
19.399747	977.137795	14.558157
19.158640	980.328345	14.563175
19.143681	976.250195	14.568192
19.283787	982.492709	14.573210
19.090679	989.434388	14.578227
19.379918	983.607558	14.583245
19.365459	980.671757	14.588263
19.395539	981.774810	14.593280
19.499885	974.553651	14.598298
19.318569	985.741289	14.603315
19.518390	977.227041	14.608333
19.395506	977.722885	14.613351
19.199658	982.440099	14.618368
19.697095	994.973097	14.623386
19.717497	1005.797775	14.628403
19.797228	1003.926523	14.633421
19.827475	1006.834714	14.638439
19.321927	1002.470499	14.643456
19.839295	1005.753658	14.648474
19.694715	1004.687586	14.653491
19.827663	1002.340926	14.658509
20.036336	1004.167098	14.663527
19.535866	1003.346140	14.668544
19.703436	1004.749552	14.673562
19.976838	1006.836987	14.678579
20.018367	999.597258	14.683597
20.162625	999.035054	14.688615
20.001017	995.207101	14.693632
19.968687	969.359286	14.698650
19.417976	980.828865	14.703667
19.633270	991.888091	14.708685
19.940763	999.644453	14.713703
19.805393	993.858900	14.718720
20.162296	1001.263531	14.723738
19.652965	1000.396623	14.728755
19.983081	999.726401	14.733773
20.184438	990.924721	14.738791
20.066168	994.821879	14.743808
19.878521	992.124655	14.748826
19.857267	995.501672	14.753843
20.220376	995.845629	14.758861
20.004320	987.248210	14.763879
19.991465	989.238480	14.768896
20.172418	990.633482	14.773914
19.575735	1001.785222	14.778931
20.166275	991.657056	14.783949
20.053047	1008.161161	14.788967
20.130770	1028.712765	14.793984
20.605422	1019.606312	14.799002
20.465842	1025.450839	14.804019
20.448688	1016.560303	14.809037
20.192417	1004.693371	14.814055
19.958968	1010.546289	14.819072
20.040019	1015.024462	14.824090
20.385253	1020.079797	14.829107
20.415610	1025.339107	14.834125
20.462082	1022.769302	14.839143
20.024751	1027.101475	14.844160
20.272491	1025.500550	14.849178
20.425343	1028.298015	14.854195
20.525035	1029.317578	14.859213
20.658561	1026.030371	14.864231
20.128581	1024.930006	14.869248
20.169148	1023.039642	14.874266
20.446542	1028.061425	14.879283
20.146788	1023.958458	14.884301
20.263531	1035.399235	14.889319
20.614035	1053.036272	14.894336
20.931876	1039.242638	14.899354
20.896973	1046.370996	14.904371
20.835609	1051.190236	14.909389
20.937164	1048.911606	14.914407
20.572143	1054.182379	14.919424
20.857673	1049.571125	14.924442
20.320724	1051.918080	14.929459
21.093499	1054.287050	14.934477
21.179841	1043.903329	14.939495
21.147566	1045.773568	14.944512
21.549334	1038.590993	14.949530
20.977850	1026.091764	14.954547
20.662184	1013.568241	14.959565
20.771894	1011.247312	14.964583
20.619158	1020.713694	14.969600
20.627161	1025.727192	14.974618
21.020449	1034.644115	14.979635
20.905120	1036.726187	14.984653
21.220149	1041.830443	14.989671
21.048112	1042.804217	14.994688
21.468894	1043.401078	14.999706
21.562937	1047.798327	15.004723
21.040813	1032.479464	15.009741
21.093454	1020.570433	15.014759
21.195734	1014.914900	15.019776
21.285817	1014.601030	15.024794
20.697651	1020.698882	15.029811
20.840517	1035.550232	15.034829
21.333929	1039.017036	15.039847
21.059317	1034.503018	15.044864
21.153781	1030.565506	15.049882
21.404562	1032.732230	15.054899
21.353727	1039.828367	15.059917
21.499982	1028.851428	15.064935
21.383238	1034.190594	15.069952
21.394684	1035.741550	15.074970
21.076520	1037.845935	15.079987
21.185056	1031.450940	15.085005
21.074554	1031.155874	15.090023
21.037779	1038.174066	15.095040
21.316583	1041.235828	15.100058
21.670996	1064.114191	15.105075
21.365885	1046.747856	15.110093
21.781356	1038.486976	15.115111
21.564320	1050.683823	15.120128
21.999077	1048.378234	15.125146
21.701320	1036.637704	15.130163
21.485126	1027.027248	15.135181
21.515356	1026.760627	15.140199
21.111070	1035.423810	15.145216
21.714396	1050.894165	15.150234
22.073472	1047.751500	15.155251
21.941669	1058.805190	15.160269
21.886488	1048.475199	15.165287
21.871443	1037.078548	15.170304
21.852555	1027.159460	15.175322
21.997124	1030.472632	15.180339
21.258085	1033.274137	15.185357
21.648734	1037.410310	15.190375
21.811857	1046.641020	15.195392
21.966550	1051.754621	15.200410
21.899432	1051.171883	15.205427
21.457357	1052.355230	15.210445
21.963593	1062.930248	15.215463
22.203751	1059.799901	15.220480
22.283937	1061.942863	15.225498
22.370435	1064.091149	15.230515
22.236737	1063.736600	15.235533
22.094890	1059.769833	15.240551
21.915054	1056.219285	15.245568
22.033642	1062.260066	15.250586
22.174818	1056.945573	15.255603
22.248290	1064.167414	15.260621
22.066214	1055.463649	15.265639
21.944844	1072.193157	15.270656
21.957612	1058.687155	15.275674
22.143398	1053.630769	15.280691
21.892018	1066.656694	15.285709
22.274688	1063.421965	15.290727
22.184604	1058.465607	15.295744
22.089213	1059.200149	15.300762
22.050888	1058.616056	15.305779
21.774440	1078.749826	15.310797
22.750404	1087.253580	15.315815
22.475048	1086.791833	15.320832
22.337755	1083.136782	15.325850
22.568049	1078.117597	15.330867
22.655542	1094.116949	15.335885
22.525691	1086.493770	15.340903
22.400916	1085.844324	15.345920
22.646465	1084.136437	15.350938
22.410987	1080.127530	15.355955
22.709243	1083.890016	15.360973
22.665984	1080.971334	15.365991
22.540074	1081.735906	15.371008
22.566375	1077.338836	15.376026
22.947176	1082.338121	15.381043
22.490860	1074.324274	15.386061
22.614551	1079.793045	15.391079
22.507318	1086.872789	15.396096
22.530763	1077.483542	15.401114
22.752667	1082.608713	15.406131
22.326220	1082.287408	15.411149
22.925608	1081.022712	15.416167
22.862986	1078.511019	15.421184
22.699380	1079.530812	15.426202
23.121080	1071.663428	15.431219
22.624085	1079.075645	15.436237
22.848529	1087.466768	15.441255
22.993894	1094.112451	15.446272
22.982471	1111.863060	15.451290
23.268212	1098.273231	15.456307
22.714454	1095.907917	15.461325
23.074464	1097.110766	15.466343
23.274577	1108.355486	15.471360
23.290238	1107.472590	15.476378
23.380999	1100.026285	15.481395
23.312295	1079.280784	15.486413
23.213746	1077.983427	15.491431
23.122791	1074.125451	15.496448
23.226049	1075.507386	15.501466
23.643849	1073.513728	15.506483
23.284673	1072.651694	15.511501
23.475558	1065.748308	15.516519
23.177001	1071.444185	15.521536
23.069862	1074.055168	15.526554
23.305962	1073.693172	15.531571
23.095978	1083.127531	15.536589
23.199460	1084.916542	15.541607
23.223046	1091.300430	15.546624
23.582522	1096.142110	15.551642
23.839930	1090.197153	15.556659
23.430627	1092.189588	15.561677
23.581545	1099.074251	15.566695
23.556115	1103.310347	15.571712
23.297621	1093.526597	15.576730
23.821064	1099.450306	15.581747
23.578577	1098.753029	15.586765
23.645045	1105.426858	15.591783
23.844953	1095.249382	15.596800
23.681326	1101.877208	15.601818
23.791468	1084.994899	15.606835
23.736248	1084.804784	15.611853
23.735731	1087.591573	15.616871
23.869805	1087.494878	15.621888
23.610282	1089.400727	15.626906
23.569909	1082.634558	15.631923
23.588890	1100.156322	15.636941
23.795863	1106.031786	15.641959
23.996508	1097.163892	15.646976
23.976898	1098.322076	15.651994
23.896848	1099.840034	15.657011
23.782683	1103.443074	15.662029
24.070981	1096.514946	15.667047
23.990644	1098.821924	15.672064
23.861726	1095.326508	15.677082
24.425434	1096.929799	15.682099
24.018692	1102.358605	15.687117
24.269526	1099.289697	15.692135
23.998716	1096.583396	15.697152
23.898925	1103.119167	15.702170
24.196950	1097.716969	15.707187
24.227390	1092.533429	15.712205
23.884760	1091.757165	15.717223
24.150553	1096.657706	15.722240
24.045540	1104.219962	15.727258
24.203414	1089.703406	15.732275
23.956287	1090.578491	15.737293
23.821163	1100.992081	15.742311
24.370221	1109.846765	15.747328
24.232522	1120.273393	15.752346
24.281799	1119.801809	15.757363
24.706225	1129.821622	15.762381
24.338352	1124.943484	15.767399
24.532127	1125.105687	15.772416
24.247472	1124.828439	15.777434
24.788080	1118.690772	15.782451
24.734392	1115.221436	15.787469
24.833911	1118.516436	15.792487
24.503057	1130.576531	15.797504
24.759773	1124.521214	15.802522
24.670416	1114.041900	15.807539
24.812037	1123.897731	15.812557
24.523765	1118.224460	15.817575
25.152607	1124.210562	15.822592
24.743238	1111.130434	15.827610
24.696859	1111.024142	15.832627
24.603781	1110.555926	15.837645
24.815937	1107.565662	15.842663
25.100540	1112.740980	15.847680
24.523443	1122.150825	15.852698
24.740837	1115.322165	15.857715
24.578867	1113.709684	15.862733
24.454966	1120.514335	15.867751
24.524546	1114.971194	15.872768
24.269077	1116.046410	15.877786
24.714205	1119.770112	15.882803
24.701060	1136.896147	15.887821
24.554394	1135.928226	15.892839
25.110194	1144.362136	15.897856
24.876738	1148.075397	15.902874
25.134450	1146.450807	15.907891
25.001588	1146.989246	15.912909
24.730308	1148.859073	15.917927
25.023979	1142.318263	15.922944
25.259160	1147.867419	15.927962
25.237873	1140.391314	15.932979
25.042258	1142.274532	15.937997
25.014200	1149.625928	15.943015
25.048948	1159.160841	15.948032
24.676951	1165.310081	15.953050
25.088095	1168.073410	15.958067
25.310722	1165.977774	15.963085
25.324517	1163.046984	15.968103
25.726758	1159.001259	15.973120
25.606964	1165.937831	15.978138
25.736638	1167.151527	15.983155
25.601762	1168.289905	15.988173
25.552159	1169.708421	15.993191
25.953669	1159.846472	15.998208
25.691093	1159.720403	16.003226
25.634592	1158.665768	16.008243
25.740024	1177.108211	16.013261
25.605700	1169.009156	16.018279
25.841217	1166.393931	16.023296
25.634535	1171.144451	16.028314
25.636513	1156.526030	16.033331
25.921721	1166.914827	16.038349
25.789813	1163.830134	16.043367
25.991678	1156.379022	16.048384
25.841735	1157.469265	16.053402
25.688264	1164.758263	16.058419
26.008275	1163.553115	16.063437
25.800239	1159.666127	16.068455
25.980731	1165.634125	16.073472
25.991124	1162.015880	16.078490
25.748883	1158.251020	16.083507
25.774549	1162.617983	16.088525
25.509423	1163.309694	16.093543
25.936096	1159.421092	16.098560
25.719326	1166.795751	16.103578
25.884145	1166.861502	16.108595
26.000454	1187.097963	16.113613
26.171737	1190.934016	16.118631
26.361825	1181.991992	16.123648
26.388065	1188.634283	16.128666
26.511306	1188.586624	16.133683
26.305609	1185.586075	16.138701
26.077678	1187.237668	16.143719
26.520391	1182.740613	16.148736
26.300515	1190.330370	16.153754
26.445644	1194.243108	16.158771
26.123330	1181.083014	16.163789
26.359300	1188.052219	16.168807
26.801324	1184.934405	16.173824
26.223899	1195.205903	16.178842
26.641269	1179.957471	16.183859
26.625127	1184.024867	16.188877
26.482998	1186.183741	16.193895
26.586507	1186.852410	16.198912
26.407463	1186.845801	16.203930
26.371012	1189.360516	16.208947
26.287363	1192.296050	16.213965
26.173548	1190.272061	16.218983
26.390045	1185.239229	16.224000
26.445270	1188.714757	16.229018
26.499829	1188.384359	16.234035
26.814477	1200.905115	16.239053
26.632525	1209.495675	16.244071
26.997042	1205.979732	16.249088
27.055977	1212.310786	16.254106
27.189616	1209.875625	16.259123
27.048801	1200.199615	16.264141
26.979502	1193.914479	16.269159
27.008777	1195.345886	16.274176
26.604328	1198.104459	16.279194
26.919789	1193.157108	16.284211
26.992938	1192.681782	16.289229
27.050741	1210.267001	16.294247
27.142325	1202.889955	16.299264
27.100536	1212.869249	16.304282
27.258509	1203.723955	16.309299
27.128505	1208.175283	16.314317
26.987730	1219.397741	16.319335
27.148330	1210.564468	16.324352
27.023266	1210.060234	16.329370
27.029816	1198.499145	16.334387
27.184659	1198.610642	16.339405
26.937429	1215.953316	16.344423
27.090927	1200.560011	16.349440
27.180238	1206.933642	16.354458
27.387367	1217.429380	16.359475
27.847063	1224.139475	16.364493
27.130783	1211.561812	16.369511
27.584540	1221.801152	16.374528
27.613812	1225.593189	16.379546
27.185456	1222.861058	16.384563
27.586713	1228.068626	16.389581
27.658408	1226.646751	16.394599
27.616918	1222.970348	16.399616
27.643024	1226.242155	16.404634
27.988292	1222.268461	16.409651
28.141517	1225.188979	16.414669
27.723667	1224.774802	16.419687
27.510467	1220.509899	16.424704
27.254535	1223.573422	16.429722
27.729940	1226.052126	16.434739
27.831025	1218.298031	16.439757
27.746925	1227.270913	16.444775
27.778728	1232.208153	16.449792
28.175430	1228.548303	16.454810
27.649800	1221.062820	16.459827
28.141703	1217.520604	16.464845
27.831349	1219.822609	16.469863
28.058199	1219.563050	16.474880
27.948304	1220.186258	16.479898
27.873598	1222.145218	16.484915
28.404875	1211.997811	16.489933
27.789382	1228.609217	16.494951
27.782578	1226.416973	16.499968
28.050813	1238.004564	16.504986
27.934470	1244.246323	16.510003
28.160874	1241.667231	16.515021
28.630477	1254.684474	16.520039
28.313837	1252.433471	16.525056
28.378001	1248.948800	16.530074
28.551757	1244.418128	16.535091
28.863184	1239.411434	16.540109
28.469660	1252.851100	16.545127
28.438453	1244.234062	16.550144
28.335536	1243.104641	16.555162
28.501177	1251.164215	16.560179
28.790935	1240.259341	16.565197
28.286675	1252.965247	16.570215
28.471986	1253.368628	16.575232
28.453642	1251.777814	16.580250
28.678034	1252.367582	16.585267
28.669830	1249.979888	16.590285
28.294340	1245.762498	16.595303
28.291010	1249.464970	16.600320
28.315885	1245.781321	16.605338
28.594244	1247.826981	16.610355
28.630214	1240.149353	16.615373
28.491581	1250.939134	16.620391
28.791215	1265.235917	16.625408
29.076623	1266.671382	16.630426
28.952639	1268.928413	16.635443
29.210479	1269.626555	16.640461
29.375284	1268.227959	16.645479
28.905916	1257.602967	16.650496
28.599397	1253.302182	16.655514
28.947296	1267.402050	16.660531
29.021368	1268.293092	16.665549
29.061019	1269.735503	16.670567
28.993681	1270.658170	16.675584
29.172170	1272.075673	16.680602
28.590629	1271.298962	16.685619
28.891063	1265.801659	16.690637
29.097200	1269.506031	16.695655
28.648969	1267.127315	16.700672
29.067360	1277.249147	16.705690
29.060909	1291.047933	16.710707
29.474972	1294.413607	16.715725
29.320598	1295.368848	16.720743
29.287549	1295.146852	16.725760
29.510855	1299.195693	16.730778
29.295082	1300.498239	16.735795
29.555498	1293.905777	16.740813
29.593319	1291.731780	16.745831
29.659634	1297.433678	16.750848
29.496181	1293.211459	16.755866
29.510528	1288.535332	16.760883
29.788768	1292.534537	16.765901
29.587937	1294.137710	16.770919
29.433265	1296.544726	16.775936
29.688634	1289.984615	16.780954
29.635091	1307.202353	16.785971
29.816580	1301.979305	16.790989
29.960945	1306.782161	16.796007
30.164108	1301.880779	16.801024
29.794562	1305.463909	16.806042
29.857585	1311.112677	16.811059
29.976971	1308.288400	16.816077
30.450829	1315.160420	16.821095
30.218622	1302.020834	16.826112
30.440970	1287.008002	16.831130
29.905579	1292.823110	16.836147
30.036287	1289.832953	16.841165
30.366558	1286.959859	16.846183
30.506960	1283.633656	16.851200
30.301707	1278.881481	16.856218
30.003669	1286.729687	16.861235
30.272231	1283.755804	16.866253
30.661865	1279.469021	16.871271
30.212656	1288.458112	16.876288
30.326018	1286.764606	16.881306
30.389842	1284.605472	16.886323
30.229479	1281.051827	16.891341
30.230855	1284.763038	16.896359
30.315813	1289.357437	16.901376
30.475013	1284.185226	16.906394
30.297898	1298.723997	16.911411
30.408417	1297.365464	16.916429
30.499260	1298.108708	16.921447
30.828249	1304.653113	16.926464
31.113306	1305.511101	16.931482
30.652260	1305.419282	16.936499
30.576956	1300.653053	16.941517
30.624954	1305.739261	16.946535
30.793257	1301.199961	16.951552
30.590703	1298.113691	16.956570
30.286733	1306.906459	16.961587
30.412928	1308.874978	16.966605
30.582244	1311.515267	16.971623
30.841405	1312.787583	16.976640
30.939234	1308.338222	16.981658
30.672568	1319.801383	16.986675
30.717833	1309.591209	16.991693
31.039934	1322.417008	16.996711
31.172769	1330.374457	17.001728
31.347631	1326.417972	17.006746
30.993833	1335.108102	17.011763
30.757312	1323.102159	17.016781
31.198565	1334.176690	17.021799
31.142570	1341.097022	17.026816
31.177573	1321.224966	17.031834
30.826469	1333.733356	17.036851
30.921749	1331.812295	17.041869
31.266595	1322.912228	17.046887
30.824164	1334.825832	17.051904
31.391552	1334.247817	17.056922
31.824800	1349.347433	17.061939
31.808281	1343.678850	17.066957
31.689080	1333.582797	17.071975
31.507338	1332.112256	17.076992
31.377347	1324.971856	17.082010
31.351610	1331.960030	17.087027
31.286395	1330.133546	17.092045
31.873733	1342.321330	17.097063
31.774101	1348.961312	17.102080
31.506713	1352.446391	17.107098
31.389222	1362.693261	17.112115
31.829715	1363.517430	17.117133
31.874483	1354.727482	17.122151
31.566879	1355.372204	17.127168
31.844214	1352.409559	17.132186
31.860844	1350.873220	17.137203
31.577051	1348.635993	17.142221
31.674185	1351.571632	17.147239
31.498638	1344.776047	17.152256
31.902328	1350.488221	17.157274
32.362796	1368.947822	17.162291
32.031790	1362.662603	17.167309
32.491260	1350.153100	17.172327
32.268263	1356.051832	17.177344
32.573545	1356.496381	17.182362
32.378626	1346.699374	17.187379
32.167055	1348.155905	17.192397
32.294983	1347.517351	17.197415
32.304715	1347.146635	17.202432
32.354499	1353.157267	17.207450
32.227607	1356.516188	17.212467
32.250792	1350.005058	17.217485
32.474480	1349.228418	17.222503
32.468169	1357.182432	17.227520
32.085916	1343.141634	17.232538
32.574579	1370.720642	17.237555
32.411396	1380.939966	17.242573
32.508344	1382.963571	17.247591
32.386291	1389.701759	17.252608
32.503532	1377.040722	17.257626
32.800572	1382.624442	17.262643
32.619849	1376.116848	17.267661
32.833678	1386.498021	17.272679
32.728821	1384.747173	17.277696
32.674965	1375.401441	17.282714
32.838433	1374.113505	17.287731
32.596235	1374.312459	17.292749
32.391456	1366.896569	17.297767
32.346842	1373.960304	17.302784
32.739192	1379.020983	17.307802
32.688977	1388.083315	17.312819
32.871384	1394.300410	17.317837
33.193363	1387.471040	17.322855
33.521165	1400.037214	17.327872
33.299822	1395.773545	17.332890
33.363145	1398.042273	17.337907
33.292575	1396.863590	17.342925
33.662629	1383.796847	17.347943
33.332636	1381.046124	17.352960
33.582288	1370.302096	17.357978
33.312433	1368.870604	17.362995
33.186045	1379.355573	17.368013
33.576304	1378.325606	17.373031
33.146583	1387.715654	17.378048
33.437636	1382.156666	17.383066
33.616760	1387.449581	17.388083
33.641118	1387.796128	17.393101
33.685767	1375.821838	17.398119
33.534005	1387.386965	17.403136
33.540502	1382.140817	17.408154
33.777147	1387.778185	17.413171
33.473554	1384.676170	17.418189
33.586032	1392.674707	17.423207
32.986153	1386.374800	17.428224
33.506968	1383.907357	17.433242
33.644307	1382.216396	17.438259
33.613206	1387.728450	17.443277
33.378918	1396.084290	17.448295
33.576410	1412.379131	17.453312
33.969930	1412.964498	17.458330
33.894902	1414.065110	17.463347
33.542207	1411.548323	17.468365
33.893602	1400.905106	17.473383
33.924915	1409.607521	17.478400
33.796751	1410.583908	17.483418
34.318326	1410.880956	17.488435
34.071290	1424.821686	17.493453
34.073801	1433.326643	17.498471
33.975005	1439.149135	17.503488
34.285717	1430.879242	17.508506
34.484369	1433.297192	17.513523
34.271977	1432.323773	17.518541
34.785510	1433.723509	17.523559
34.421555	1432.527673	17.528576
34.420509	1437.015659	17.533594
34.432530	1428.215026	17.538611
34.059898	1431.959619	17.543629
34.471687	1435.398264	17.548647
34.522677	1424.656926	17.553664
34.513052	1428.533999	17.558682
34.864690	1429.182736	17.563699
34.465096	1436.971176	17.568717
34.503209	1422.653004	17.573735
34.460669	1425.784117	17.578752
34.495963	1430.591471	17.583770
34.882750	1432.658036	17.588787
34.934444	1453.261546	17.593805
35.320069	1445.024092	17.598823
35.142215	1436.199554	17.603840
35.083687	1431.058258	17.608858
34.937049	1430.876150	17.613875
34.610686	1431.350236	17.618893
35.071326	1440.490351	17.623911
34.787107	1444.233717	17.628928
34.863693	1450.161284	17.633946
35.147124	1449.788710	17.638963
35.038928	1456.852971	17.643981
35.196720	1451.936566	17.648999
35.450072	1457.561871	17.654016
35.140184	1455.268756	17.659034
35.216049	1444.656059	17.664051
35.152574	1454.547363	17.669069
35.365876	1445.648909	17.674087
35.378057	1459.861492	17.679104
35.485407	1447.934137	17.684122
35.765053	1447.855661	17.689139
35.427247	1454.728668	17.694157
35.439620	1448.863012	17.699175
35.377698	1455.434005	17.704192
35.546941	1462.937662	17.709210
35.957140	1471.918431	17.714227
36.206923	1469.054762	17.719245
36.131875	1454.779542	17.724263
36.066074	1449.626757	17.729280
35.758686	1458.388574	17.734298
35.990319	1446.012538	17.739315
35.808162	1446.647075	17.744333
35.875801	1441.356615	17.749351
35.731851	1451.210030	17.754368
35.646958	1457.052441	17.759386
35.915710	1466.560322	17.764403
35.674833	1476.526773	17.769421
36.077071	1476.810960	17.774439
36.057299	1484.069671	17.779456
36.051004	1482.786234	17.784474
36.496819	1469.988439	17.789491
36.354114	1475.211877	17.794509
36.202088	1475.955310	17.799527
35.965550	1486.877343	17.804544
36.143002	1469.614878	17.809562
36.389560	1465.495643	17.814579
36.295842	1467.151480	17.819597
36.497774	1462.584779	17.824615
36.799875	1470.048687	17.829632
36.533960	1473.786036	17.834650
36.947118	1469.145211	17.839667
36.582970	1468.971934	17.844685
36.567618	1470.173658	17.849703
36.767681	1463.565343	17.854720
36.353772	1460.584745	17.859738
37.160734	1470.705770	17.864755
36.578740	1484.272972	17.869773
36.750640	1494.600814	17.874791
37.204386	1491.421149	17.879808
37.011788	1483.179595	17.884826
36.820639	1483.815543	17.889843
36.920840	1489.183972	17.894861
36.900312	1484.469075	17.899879
36.802516	1491.711611	17.904896
36.967093	1487.785106	17.909914
37.274053	1485.101834	17.914931
36.907396	1486.948767	17.919949
36.889547	1482.227139	17.924967
36.757779	1483.128352	17.929984
37.039077	1487.026131	17.935002
37.058143	1487.256739	17.940019
37.338016	1502.140662	17.945037
37.373051	1497.619037	17.950055
37.274650	1504.145268	17.955072
37.163024	1511.860218	17.960090
37.695473	1511.407600	17.965107
37.296466	1513.941293	17.970125
37.624415	1510.386838	17.975143
37.689399	1510.834326	17.980160
37.638596	1519.997807	17.985178
38.120471	1512.799337	17.990195
37.804747	1506.972444	17.995213
37.479217	1513.477457	18.000231
37.725817	1517.626846	18.005248
37.858689	1511.388821	18.010266
37.924581	1509.806878	18.015283
37.650117	1511.800323	18.020301
37.350623	1512.904551	18.025319
37.664739	1512.823829	18.030336
38.054181	1514.517584	18.035354
37.997642	1514.173027	18.040371
37.961440	1513.616991	18.045389
37.691374	1508.313146	18.050407
38.222132	1525.802482	18.055424
37.993476	1538.083536	18.060442
38.262986	1530.236641	18.065459
38.403206	1534.137599	18.070477
38.356236	1537.133718	18.075495
38.254902	1533.255178	18.080512
38.533745	1540.782723	18.085530
38.459954	1532.128035	18.090547
38.355337	1535.884308	18.095565
38.156492	1527.719455	18.100583
38.845571	1525.070987	18.105600
38.551553	1529.349266	18.110618
38.735940	1524.554912	18.115635
38.495066	1532.795077	18.120653
38.923579	1539.200893	18.125671
38.755332	1531.706623	18.130688
38.343497	1538.483957	18.135706
38.627118	1530.035217	18.140723
38.959688	1531.157186	18.145741
38.890950	1533.159428	18.150759
38.567232	1526.831981	18.155776
38.926848	1549.647032	18.160794
39.176383	1554.780634	18.165811
39.439286	1561.436480	18.170829
39.238842	1539.552842	18.175847
38.952227	1523.243552	18.180864
38.854259	1540.891374	18.185882
39.172736	1537.660307	18.190899
39.378919	1545.148743	18.195917
39.244193	1553.034597	18.200935
39.393636	1544.269183	18.205952
39.181173	1542.999108	18.210970
39.553414	1545.490867	18.215987
39.182554	1545.457503	18.221005
39.161307	1554.808886	18.226023
39.424467	1545.325028	18.231040
39.167805	1554.527093	18.236058
39.166731	1545.797886	18.241075
38.946985	1544.749869	18.246093
39.500358	1561.973751	18.251111
39.633857	1575.892849	18.256128
39.746994	1575.944607	18.261146
39.846807	1569.033206	18.266163
39.799858	1574.342662	18.271181
39.557446	1579.878414	18.276199
40.121273	1567.847899	18.281216
39.913885	1573.125684	18.286234
39.960708	1568.150890	18.291251
40.016157	1570.970013	18.296269
39.989158	1581.979201	18.301287
40.028025	1580.713928	18.306304
39.798431	1582.662479	18.311322
40.141423	1575.788718	18.316339
40.130375	1578.015469	18.321357
39.823899	1581.730791	18.326375
40.112956	1578.040397	18.331392
40.312098	1578.204920	18.336410
40.241173	1589.934246	18.341427
40.412051	1600.385393	18.346445
40.687931	1608.494132	18.351463
40.805660	1601.718775	18.356480
40.568427	1590.255593	18.361498
40.650185	1577.495826	18.366515
40.705555	1572.339800	18.371533
40.221422	1574.274579	18.376551
40.566768	1584.745721	18.381568
40.574630	1599.249442	18.386586
40.992385	1592.711119	18.391603
40.711971	1595.677548	18.396621
40.759216	1593.928097	18.401639
40.939052	1600.379209	18.406656
40.952783	1588.371749	18.411674
40.759243	1590.999500	18.416691
41.100285	1595.736903	18.421709
40.843383	1601.988185	18.426727
41.055505	1591.180474	18.431744
41.198889	1594.323513	18.436762
40.829268	1589.451833	18.441779
41.074384	1589.511317	18.446797
40.899532	1594.582028	18.451815
41.276160	1605.218703	18.456832
41.146124	1618.920334	18.461850
41.268296	1621.883654	18.466867
41.290904	1619.525798	18.471885
41.208967	1624.376820	18.476903
41.241302	1618.406989	18.481920
41.062607	1615.105473	18.486938
41.161104	1618.321826	18.491955
41.375545	1623.000172	18.496973
41.184669	1644.490867	18.501991
41.755047	1644.628786	18.507008
41.456231	1629.163961	18.512026
41.486931	1636.954501	18.517043
41.891152	1638.434501	18.522061
41.774749	1641.141698	18.527079
41.857314	1636.401140	18.532096
41.995349	1639.753321	18.537114
41.851801	1638.731232	18.542131
41.787962	1633.505499	18.547149
41.702407	1640.238062	18.552167
42.080711	1649.665757	18.557184
41.892911	1661.148339	18.562202
41.878250	1667.604701	18.567219
42.176663	1659.339786	18.572237
42.072468	1661.606390	18.577255
42.283998	1662.261308	18.582272
41.984992	1666.871780	18.587290
42.111727	1661.565683	18.592307
42.439022	1656.764684	18.597325
42.121339	1656.767172	18.602343
42.647010	1655.340410	18.607360
42.342931	1667.526065	18.612378
42.892023	1681.342257	18.617395
43.162230	1671.475353	18.622413
42.959244	1672.223622	18.627431
43.133624	1654.052534	18.632448
42.665073	1655.640877	18.637466
42.759151	1660.631598	18.642483
42.657980	1645.501888	18.647501
42.403304	1654.577453	18.652519
42.905716	1666.059200	18.657536
43.258931	1673.433129	18.662554
42.823794	1676.272325	18.667571
43.264929	1670.939058	18.672589
43.231484	1675.571044	18.677607
43.345623	1674.050960	18.682624
43.099815	1677.804136	18.687642
43.051158	1667.046706	18.692659
43.170204	1676.906379	18.697677
43.049377	1672.832034	18.702695
43.384368	1675.762019	18.707712
43.417221	1667.901648	18.712730
43.201459	1682.853909	18.717747
43.370818	1676.225079	18.722765
43.386291	1674.007197	18.727783
43.784150	1669.166735	18.732800
43.457071	1675.110282	18.737818
43.285919	1675.130839	18.742835
43.498905	1683.795455	18.747853
43.606691	1699.050508	18.752871
43.791727	1697.462506	18.757888
43.595907	1699.292161	18.762906
44.021565	1708.216975	18.767923
43.829406	1696.942334	18.772941
43.877409	1700.314945	18.777959
44.167099	1696.441380	18.782976
44.421627	1698.023739	18.787994
44.020409	1706.024002	18.793011
44.332254	1690.810606	18.798029
43.848655	1699.366605	18.803047
44.329761	1696.520310	18.808064
44.628176	1698.319869	18.813082
44.254500	1693.836983	18.818099
44.003742	1687.580104	18.823117
43.783751	1700.285970	18.828135
44.154457	1697.942997	18.833152
44.501356	1718.166022	18.838170
44.423428	1713.927146	18.843187
44.786258	1705.715238	18.848205
44.406332	1713.945712	18.853223
44.807266	1718.159335	18.858240
45.366553	1725.516778	18.863258
44.910189	1724.770929	18.868275
45.030923	1718.197041	18.873293
44.783669	1711.137979	18.878311
44.763632	1711.860741	18.883328
45.177732	1712.436583	18.888346
44.946596	1721.098213	18.893363
45.042393	1713.231116	18.898381
44.832140	1722.088302	18.903399
44.973833	1717.912852	18.908416
45.011691	1713.529595	18.913434
45.066564	1720.287526	18.918451
44.749788	1717.184362	18.923469
44.662654	1724.504222	18.928487
44.826323	1714.057501	18.933504
45.547312	1732.202088	18.938522
45.490422	1741.761137	18.943539
45.624066	1741.910676	18.948557
45.421210	1742.608431	18.953575
45.520081	1730.735869	18.958592
45.513662	1736.764904	18.963610
44.995652	1734.068831	18.968627
45.791442	1727.212437	18.973645
45.812345	1735.329623	18.978663
45.721662	1732.620250	18.983680
46.034731	1741.297616	18.988698
45.856869	1737.607758	18.993715
45.629308	1732.265627	18.998733
45.882470	1732.730977	19.003751
45.785395	1727.390495	19.008768
46.078751	1731.819805	19.013786
46.020777	1731.342916	19.018803
46.051023	1737.473511	19.023821
46.126775	1743.581198	19.028839
46.346083	1751.168657	19.033856
46.315981	1756.178861	19.038874
46.061861	1751.929710	19.043891
46.413109	1750.189420	19.048909
46.203481	1758.219652	19.053927
46.513227	1752.348333	19.058944
46.751183	1758.181286	19.063962
46.518291	1761.998732	19.068979
46.422077	1750.869981	19.073997
46.677116	1759.357620	19.079015
46.633540	1749.568240	19.084032
46.884794	1749.784564	19.089050
46.626002	1757.232324	19.094067
46.751891	1749.130108	19.099085
46.793553	1752.980280	19.104103
46.881299	1757.151457	19.109120
46.847510	1744.914637	19.114138
46.931531	1751.611205	19.119155
47.107816	1756.185104	19.124173
46.962736	1753.938716	19.129191
47.104881	1761.923302	19.134208
47.197716	1775.826834	19.139226
47.354523	1777.607560	19.144243
47.297180	1774.157605	19.149261
47.271307	1776.061633	19.154279
47.208565	1782.980037	19.159296
47.848377	1780.449713	19.164314
47.657350	1779.962109	19.169331
47.687132	1786.594600	19.174349
47.826391	1776.587198	19.179367
47.383934	1780.772020	19.184384
47.602134	1767.028156	19.189402
47.527355	1784.533721	19.194419
47.703305	1775.432659	19.199437
47.723918	1782.205450	19.204455
47.515562	1786.404091	19.209472
47.616269	1780.925301	19.214490
47.450584	1793.982510	19.219507
47.705685	1803.420122	19.224525
47.840147	1809.644874	19.229543
48.061762	1810.052048	19.234560
48.050936	1807.980292	19.239578
47.684779	1810.070192	19.244595
47.786790	1812.900994	19.249613
47.779805	1816.635717	19.254631
48.247209	1817.020161	19.259648
48.549122	1829.606476	19.264666
48.487756	1839.980533	19.269683
48.475846	1832.155508	19.274701
48.567822	1836.004126	19.279719
48.441844	1830.447220	19.284736
48.621270	1827.244201	19.289754
48.635710	1825.379937	19.294771
48.551993	1832.071256	19.299789
48.619193	1838.584287	19.304807
48.893204	1832.043151	19.309824
49.108403	1820.452126	19.314842
48.570075	1823.474782	19.319859
48.790642	1825.766267	19.324877
49.145539	1819.092534	19.329895
48.916343	1818.083854	19.334912
49.033992	1820.041145	19.339930
49.071077	1831.333955	19.344947
49.169927	1828.285581	19.349965
49.001694	1839.799927	19.354983
49.101962	1844.833915	19.360000
49.353750	1844.630405	19.365018
49.180482	1854.867358	19.370035
49.462985	1855.965633	19.375053
49.462378	1845.658191	19.380071
49.158514	1850.970109	19.385088
49.210392	1845.309588	19.390106
49.532190	1850.027981	19.395123
49.675906	1848.023532	19.400141
50.376950	1848.074704	19.405159
49.806111	1857.667000	19.410176
49.943215	1847.262236	19.415194
49.619615	1851.153878	19.420211
49.817063	1846.161719	19.425229
50.100999	1850.816612	19.430247
49.791520	1862.646613	19.435264
50.049068	1863.770890	19.440282
50.352611	1874.173007	19.445299
50.178815	1873.689013	19.450317
50.475530	1872.269704	19.455335
50.354606	1877.799137	19.460352
50.238786	1864.555689	19.465370
50.192561	1876.761050	19.470387
49.853791	1872.241090	19.475405
50.631426	1871.118842	19.480423
49.989239	1878.247998	19.485440
50.497736	1863.256129	19.490458
50.714890	1865.526062	19.495475
50.601589	1868.011884	19.500493
50.823137	1863.208462	19.505511
51.302944	1871.986010	19.510528
51.072166	1860.862493	19.515546
51.068323	1853.815734	19.520563
51.011649	1856.731370	19.525581
51.242632	1852.327289	19.530599
51.293821	1860.891099	19.535616
51.247307	1852.907373	19.540634
51.063920	1857.259920	19.545651
51.139335	1854.196277	19.550669
51.198571	1854.587865	19.555687
51.177563	1860.676036	19.560704
51.022936	1852.254780	19.565722
51.334365	1859.947781	19.570739
51.334522	1880.228473	19.575757
51.865654	1882.487087	19.580775
51.382752	1881.262514	19.585792
51.678407	1877.899254	19.590810
51.904818	1871.078363	19.595827
51.599477	1885.760785	19.600845
52.127783	1876.973722	19.605863
52.040012	1882.778850	19.610880
51.746193	1873.558823	19.615898
51.620166	1879.657143	19.620915
51.739196	1873.503218	19.625933
52.061614	1870.353532	19.630951
51.857281	1882.555264	19.635968
52.053730	1878.923504	19.640986
51.862464	1873.982772	19.646003
51.683716	1874.408491	19.651021
51.947691	1875.957827	19.656039
51.872809	1879.750541	19.661056
52.025761	1892.890452	19.666074
51.795129	1895.173739	19.671091
52.334727	1910.689545	19.676109
52.035919	1897.102330	19.681127
52.088535	1906.881013	19.686144
52.294490	1915.496346	19.691162
52.314164	1912.157383	19.696179
52.422997	1932.607313	19.701197
53.010469	1935.450444	19.706215
52.674797	1933.287547	19.711232
53.032229	1928.623776	19.716250
52.981240	1931.942507	19.721267
53.187824	1926.671163	19.726285
53.056628	1923.194878	19.731303
52.833691	1923.573869	19.736320
52.891825	1924.243363	19.741338
52.894841	1929.172682	19.746355
53.141186	1939.009399	19.751373
53.482980	1945.069160	19.756391
53.433416	1955.173171	19.761408
53.406170	1951.043072	19.766426
53.687161	1951.535628	19.771443
53.463488	1950.816431	19.776461
53.591165	1953.277133	19.781479
53.546907	1950.415275	19.786496
53.868810	1945.731818	19.791514
54.038160	1943.205750	19.796531
53.908797	1948.695499	19.801549
54.035667	1942.922204	19.806567
53.548652	1949.269624	19.811584
53.781701	1943.523878	19.816602
54.074324	1940.236826	19.821619
53.682526	1953.761956	19.826637
53.809050	1945.255578	19.831655
53.901991	1946.964271	19.836672
53.697937	1945.329903	19.841690
53.876621	1957.964019	19.846707
54.060992	1969.072882	19.851725
54.015233	1962.146265	19.856743
54.180180	1973.138243	19.861760
53.860948	1967.207599	19.866778
54.123035	1974.037310	19.871795
53.946873	1987.913719	19.876813
54.764932	1989.688701	19.881831
54.565478	1994.267878	19.886848
54.130168	1984.984749	19.891866
54.811161	1984.919135	19.896883
54.621791	1992.239341	19.901901
55.041099	2001.282071	19.906919
55.328324	2010.721072	19.911936
54.899572	2012.511508	19.916954
55.294389	2009.091658	19.921971
54.913471	2005.992181	19.926989
55.294626	2009.770280	19.932007
55.358348	2018.534190	19.937024
55.309146	2005.860915	19.942042
55.778939	2002.789109	19.947059
55.080551	2002.390459	19.952077
55.358348	2005.209531	19.957095
55.443768	2003.334128	19.962112
55.780011	2003.376182	19.967130
56.058925	1999.680980	19.972147
55.724777	2007.519376	19.977165
56.209443	2001.036700	19.982183
56.034906	1993.246552	19.987200
55.939388	1973.435252	19.992218
55.940113	1964.317364	19.997235
55.885417	1967.128559	20.002253
55.929002	1964.568540	20.007271
55.930674	1970.473300	20.012288
55.874435	1991.356291	20.017306
56.033330	1983.409757	20.022323
56.264837	1998.522595	20.027341
56.170828	1981.901820	20.032359
55.746740	1983.139214	20.037376
55.724242	1993.706102	20.042394
56.198509	1988.752590	20.047411
55.798788	2003.771813	20.052429
56.158545	2012.240009	20.057447
56.299213	2021.477897	20.062464
56.302928	2020.940839	20.067482
56.474088	2016.940598	20.072499
56.288100	2037.831347	20.077517
56.701606	2040.073695	20.082535
56.601067	2036.725139	20.087552
56.689981	2033.002890	20.092570
56.751975	2026.169828	20.097587
56.659238	2041.686983	20.102605
57.214541	2038.668051	20.107623
57.457744	2057.796774	20.112640
57.557131	2057.109014	20.117658
57.901952	2038.289089	20.122675
57.690581	2034.153102	20.127693
57.584130	2033.851072	20.132711
57.572651	2034.796586	20.137728
57.782671	2026.302337	20.142746
57.852378	2029.520118	20.147763
57.807927	2034.106580	20.152781
57.671326	2032.871923	20.157799
57.535846	2031.106873	20.162816
57.664094	2034.356512	20.167834
57.897667	2020.505896	20.172851
57.712639	2027.699194	20.177869
57.778804	2033.934725	20.182887
57.859699	2058.239570	20.187904
57.848252	2056.767535	20.192922
58.270552	2061.981521	20.197939
57.645977	2067.236444	20.202957
57.834416	2060.582390	20.207975
58.186708	2066.432248	20.212992
58.405906	2065.274398	20.218010
58.190768	2060.106962	20.223027
57.982874	2076.633194	20.228045
58.235932	2077.982270	20.233063
58.521234	2081.642848	20.238080
58.412309	2083.932338	20.243098
58.428154	2078.189018	20.248115
58.524306	2079.903533	20.253133
58.782450	2096.344142	20.258151
58.868082	2106.038859	20.263168
59.225328	2110.975849	20.268186
58.989107	2110.290172	20.273203
59.397896	2108.916407	20.278221
59.410255	2103.293557	20.283239
59.443100	2102.303769	20.288256
59.265140	2098.784279	20.293274
59.423401	2074.770247	20.298291
59.182736	2078.046133	20.303309
59.235336	2099.423480	20.308327
59.653610	2094.923718	20.313344
59.300001	2105.488896	20.318362
59.712680	2098.263163	20.323379
59.485884	2107.416646	20.328397
59.513805	2106.424473	20.333415
59.754314	2098.405136	20.338432
59.681020	2107.793366	20.343450
60.140043	2093.522330	20.348467
59.937247	2101.990338	20.353485
59.754607	2099.266912	20.358503
59.913164	2095.214975	20.363520
59.995294	2107.630776	20.368538
59.836579	2101.375110	20.373555
60.005260	2117.113326	20.378573
60.063014	2126.897636	20.383591
60.310038	2126.830582	20.388608
60.198313	2134.290173	20.393626
60.234899	2123.891530	20.398643
59.836924	2122.341182	20.403661
60.082034	2138.092690	20.408679
60.491212	2143.652769	20.413696
60.388106	2148.646116	20.418714
60.737623	2155.345423	20.423731
60.701161	2158.939656	20.428749
60.797407	2154.045326	20.433767
61.305841	2142.872095	20.438784
60.832462	2150.388354	20.443802
61.265462	2137.642592	20.448819
60.948098	2145.080752	20.453837
61.219706	2162.649189	20.458855
61.227752	2168.865468	20.463872
61.516320	2171.140032	20.468890
61.940417	2156.505156	20.473907
61.936894	2156.953925	20.478925
61.495750	2147.529602	20.483943
61.730053	2135.225263	20.488960
61.842849	2135.769426	20.493978
61.725195	2124.681674	20.498995
61.990809	2139.896595	20.504013
61.635815	2139.305272	20.509031
62.096137	2142.143109	20.514048
62.175008	2151.873627	20.519066
62.239338	2154.502086	20.524083
62.155326	2150.210407	20.529101
61.953265	2152.495561	20.534119
61.978055	2148.133182	20.539136
62.099368	2154.981862	20.544154
61.904964	2150.303500	20.549171
61.937412	2150.535176	20.554189
61.910952	2153.824856	20.559207
62.365968	2171.986315	20.564224
61.907279	2177.739189	20.569242
62.166936	2181.741507	20.574259
62.052657	2178.249897	20.579277
62.436860	2183.024880	20.584295
62.889259	2191.008390	20.589312
62.529272	2205.967901	20.594330
62.750396	2202.038694	20.599347
62.708185	2207.066701	20.604365
62.701690	2202.112710	20.609383
63.082039	2207.106073	20.614400
62.532396	2213.412900	20.619418
62.846378	2231.236721	20.624435
62.932016	2237.497676	20.629453
63.144878	2240.459515	20.634471
63.252604	2238.728930	20.639488
63.083340	2243.073044	20.644506
63.249694	2238.420196	20.649523
63.505284	2251.847275	20.654541
63.751451	2256.927953	20.659559
63.989287	2257.903852	20.664576
63.834574	2257.555725	20.669594
63.944210	2257.784777	20.674611
64.166169	2255.401917	20.679629
64.246360	2262.708403	20.684647
63.872722	2249.508221	20.689664
63.989218	2251.648794	20.694682
64.161545	2249.396798	20.699699
64.159547	2257.931258	20.704717
64.022797	2258.053732	20.709735
64.323172	2241.648663	20.714752
64.449490	2256.904444	20.719770
64.352779	2248.890533	20.724787
64.348620	2249.756009	20.729805
64.476030	2267.751122	20.734823
65.021385	2264.118273	20.739840
64.798560	2275.594109	20.744858
64.758482	2278.497746	20.749875
64.783457	2276.335111	20.754893
64.683440	2282.426335	20.759911
64.724412	2274.820071	20.764928
64.801685	2272.974322	20.769946
64.753283	2264.905493	20.774963
65.114828	2275.825826	20.779981
65.179760	2291.170156	20.784999
65.499841	2289.526227	20.790016
65.208586	2299.545211	20.795034
65.094615	2296.075622	20.800051
65.433996	2287.090722	20.805069
65.615410	2290.433073	20.810087
65.850341	2280.524021	20.815104
65.708949	2288.430178	20.820122
65.904515	2289.804058	20.825139
66.447156	2283.684619	20.830157
65.795622	2289.492991	20.835175
66.116829	2281.959594	20.840192
65.743399	2290.176687	20.845210
66.216118	2289.010664	20.850227
65.957673	2285.648928	20.855245
65.924890	2303.937445	20.860263
66.290422	2316.523603	20.865280
66.446269	2317.474477	20.870298
66.338002	2305.378344	20.875315
66.451792	2304.369552	20.880333
66.340228	2313.211566	20.885351
66.371520	2305.909792	20.890368
66.570781	2313.598470	20.895386
66.903471	2325.924667	20.900403
67.241192	2324.334781	20.905421
67.171028	2328.527676	20.910439
67.202604	2304.384848	20.915456
66.815770	2303.650170	20.920474
67.043289	2319.272038	20.925491
67.217683	2331.304272	20.930509
66.787355	2332.981366	20.935527
67.275646	2330.866067	20.940544
67.203370	2322.797796	20.945562
67.162192	2329.826651	20.950579
67.318940	2327.905322	20.955597
67.297623	2340.176530	20.960615
67.551031	2350.482628	20.965632
67.236894	2354.230868	20.970650
67.335945	2354.865563	20.975667
67.621068	2356.342193	20.980685
67.348076	2359.377018	20.985703
67.530609	2360.484675	20.990720
67.914584	2377.300342	20.995738
67.973860	2380.835433	21.000755
68.118341	2376.255410	21.005773
68.314913	2385.901335	21.010791
68.577805	2383.452078	21.015808
68.455448	2383.903691	21.020826
68.349292	2385.567873	21.025843
68.323308	2380.408581	21.030861
68.208073	2382.459232	21.035879
68.459566	2379.042832	21.040896
68.462708	2392.711561	21.045914
68.793517	2401.954573	21.050931
69.210449	2407.459865	21.055949
68.789413	2407.888840	21.060967
69.117451	2405.546150	21.065984
69.270321	2408.599476	21.071002
69.135475	2407.692755	21.076019
69.372271	2403.265537	21.081037
69.241434	2400.764345	21.086055
69.305169	2402.446096	21.091072
69.607027	2403.430909	21.096090
69.021328	2408.799770	21.101107
69.625826	2395.891243	21.106125
69.377225	2400.456130	21.111143
69.297908	2393.619820	21.116160
69.665913	2415.831842	21.121178
69.831294	2424.911416	21.126195
69.797852	2423.105091	21.131213
69.701903	2421.911379	21.136231
70.300141	2432.232933	21.141248
70.331432	2424.719650	21.146266
69.688415	2422.888897	21.151283
70.250784	2410.308886	21.156301
70.034208	2419.767070	21.161319
70.284859	2425.746591	21.166336
70.632691	2424.287670	21.171354
70.741190	2434.294594	21.176371
71.007842	2423.474685	21.181389
70.854580	2433.917137	21.186407
70.859159	2433.149533	21.191424
71.255917	2435.119973	21.196442
70.958337	2428.223162	21.201459
71.190051	2404.418110	21.206477
70.900019	2407.477705	21.211495
71.134987	2415.492226	21.216512
71.399240	2422.318613	21.221530
71.848871	2430.955984	21.226547
71.317259	2417.853018	21.231565
71.260978	2412.477535	21.236583
71.265325	2421.380345	21.241600
71.538569	2429.284723	21.246618
71.176113	2425.809855	21.251635
71.656757	2428.732927	21.256653
71.599414	2419.914270	21.261671
71.331433	2426.833516	21.266688
71.778193	2423.010935	21.271706
71.215855	2436.458994	21.276723
72.052803	2455.845447	21.281741
71.603224	2461.530704	21.286759
71.963962	2453.107323	21.291776
71.754866	2458.521348	21.296794
71.595071	2468.538765	21.301811
71.939247	2478.249986	21.306829
71.785686	2484.791527	21.311847
72.044285	2483.444423	21.316864
72.706906	2493.913731	21.321882
72.433024	2508.992561	21.326899
72.513291	2509.301966	21.331917
72.893918	2503.072123	21.336935
72.715667	2497.968216	21.341952
72.504782	2499.677221	21.346970
72.766209	2500.598939	21.351987
72.906490	2502.073026	21.357005
73.154339	2496.962326	21.362023
72.749504	2505.440085	21.367040
73.138001	2521.582920	21.372058
73.577346	2528.959490	21.377075
73.968901	2513.297365	21.382093
73.770525	2517.178996	21.387111
73.915033	2516.837638	21.392128
74.012433	2510.718447	21.397146
73.979239	2514.195460	21.402163
74.112756	2509.285726	21.407181
73.986040	2494.465448	21.412199
74.247412	2499.569063	21.417216
74.277481	2484.651637	21.422234
73.981825	2478.609819	21.427251
74.420723	2491.594904	21.432269
74.341371	2500.668674	21.437287
73.984081	2509.334667	21.442304
74.202949	2507.589799	21.447322
73.999484	2516.509434	21.452339
74.684797	2514.369559	21.457357
74.562561	2520.350723	21.462375
74.565796	2513.065885	21.467392
74.713033	2505.767957	21.472410
74.104585	2513.138253	21.477427
74.400991	2525.684890	21.482445
74.643913	2528.506354	21.487463
74.597654	2542.268152	21.492480
74.957092	2549.518380	21.497498
75.154384	2557.308468	21.502515
75.208659	2563.997376	21.507533
75.619939	2570.128524	21.512551
75.248168	2562.785642	21.517568
75.356987	2556.740393	21.522586
75.348085	2571.373772	21.527603
75.490309	2562.542715	21.532621
75.533487	2569.798315	21.537639
75.612960	2592.039980	21.542656
75.869710	2579.413050	21.547674
76.126996	2595.690131	21.552691
75.841971	2592.575525	21.557709
76.041300	2587.942670	21.562727
75.645481	2589.724845	21.567744
76.192717	2593.312929	21.572762
76.585550	2606.579900	21.577779
76.436014	2602.923299	21.582797
76.222152	2609.079812	21.587815
76.211972	2606.783775	21.592832
76.781512	2608.591449	21.597850
76.568854	2608.271330	21.602867
76.734662	2606.661013	21.607885
76.799740	2602.664639	21.612903
76.676917	2605.748568	21.617920
76.990256	2615.701407	21.622938
76.739505	2615.765996	21.627955
77.059483	2625.073944	21.632973
77.231679	2620.322240	21.637991
76.931870	2634.354234	21.643008
76.925213	2620.515547	21.648026
77.215885	2636.402382	21.653043
76.985847	2646.430903	21.658061
77.489174	2651.338845	21.663079
77.531421	2650.180278	21.668096
77.559715	2646.735674	21.673114
77.477802	2653.007245	21.678131
77.565211	2654.240290	21.683149
77.583218	2660.448866	21.688167
77.628945	2672.457302	21.693184
78.135957	2663.360735	21.698202
78.225247	2670.896363	21.703219
78.075313	2669.960431	21.708237
78.308960	2671.426216	21.713255
78.555266	2689.971235	21.718272
78.823392	2694.212212	21.723290
79.082857	2699.287777	21.728307
79.292545	2688.719659	21.733325
79.029496	2671.834362	21.738343
78.312027	2676.671617	21.743360
79.176605	2684.754891	21.748378
79.258411	2683.492283	21.753395
79.174386	2701.265306	21.758413
79.446457	2694.834630	21.763431
79.234325	2699.453845	21.768448
79.384888	2689.150641	21.773466
78.979233	2692.603983	21.778483
79.222152	2694.585931	21.783501
79.689232	2679.924961	21.788519
79.944998	2700.538959	21.793536
79.798735	2693.542590	21.798554
79.683881	2693.961473	21.803571
79.589600	2701.412252	21.808589
79.865356	2703.673112	21.813607
79.504016	2709.284653	21.818624
80.046482	2705.090371	21.823642
79.713225	2719.844124	21.828659
79.998170	2716.144676	21.833677
80.111288	2727.631289	21.838695
79.804732	2750.650085	21.843712
79.981608	2744.893948	21.848730
80.223730	2748.687677	21.853747
80.285310	2760.895684	21.858765
80.698659	2770.406855	21.863783
80.269280	2774.195330	21.868800
80.648300	2772.920867	21.873818
80.762843	2788.194725	21.878835
80.814553	2800.445336	21.883853
80.930667	2803.157306	21.888871
81.182077	2804.648725	21.893888
81.090219	2794.190915	21.898906
80.898706	2811.100309	21.903923
80.831251	2825.067641	21.908941
81.293574	2822.069463	21.913959
81.382841	2821.945064	21.918976
81.812321	2836.456319	21.923994
81.935481	2845.205007	21.929011
82.188013	2845.099215	21.934029
82.452490	2840.374026	21.939047
82.287426	2840.570376	21.944064
82.599247	2842.225925	21.949082
82.669960	2825.464939	21.954099
82.389487	2816.652641	21.959117
82.421550	2809.312668	21.964135
82.479008	2827.410830	21.969152
82.509128	2828.454023	21.974170
82.481331	2843.403047	21.979187
82.322327	2837.901502	21.984205
82.483814	2831.238763	21.989223
82.395098	2837.621930	21.994240
82.298327	2836.560880	21.999258
82.958441	2849.546284	22.004275
83.128778	2869.078657	22.009293
83.057163	2857.105816	22.014311
83.460904	2861.218273	22.019328
83.375877	2861.080151	22.024346
83.320962	2865.813649	22.029363
83.168087	2871.177957	22.034381
83.428288	2873.296090	22.039399
83.390571	2886.671755	22.044416
83.454698	2884.581819	22.049434
84.061048	2884.546842	22.054451
83.801265	2892.165658	22.059469
83.952797	2884.857436	22.064487
84.105352	2892.635742	22.069504
83.978835	2883.398451	22.074522
84.248400	2902.549193	22.079539
83.957007	2913.004095	22.084557
84.331244	2910.603604	22.089575
84.172147	2914.065702	22.094592
84.194707	2924.660795	22.099610
84.310793	2922.720525	22.104627
84.348193	2942.179118	22.109645
84.747819	2937.183389	22.114663
84.516063	2945.062960	22.119680
84.689747	2934.351998	22.124698
84.862656	2953.884059	22.129715
85.061894	2976.432526	22.134733
85.128950	2974.695618	22.139751
85.294509	2967.173697	22.144768
85.599620	2962.558892	22.149786
86.007410	2960.512947	22.154803
85.519018	2955.321782	22.159821
85.980710	2952.538306	22.164839
85.789726	2956.172687	22.169856
85.804754	2971.768446	22.174874
86.118370	2980.768264	22.179891
85.952328	2988.908994	22.184909
86.404919	2987.411523	22.189927
86.181138	2980.837496	22.194944
86.231100	2985.879686	22.199962
86.400116	2981.721757	22.204979
86.186483	2983.759486	22.209997
86.624932	2982.068545	22.215015
86.828944	2996.785691	22.220032
87.029398	2997.420303	22.225050
87.259552	2992.833015	22.230067
87.282754	2996.575877	22.235085
87.294092	2989.359015	22.240103
87.484261	2984.654900	22.245120
87.246919	2972.436511	22.250138
87.564248	2975.300044	22.255155
87.325110	2991.513230	22.260173
87.441767	2991.861129	22.265191
87.565929	2985.977457	22.270208
87.310940	2992.137387	22.275226
87.899037	2986.020061	22.280243
87.590942	2993.678052	22.285261
87.568506	2986.984104	22.290279
87.651704	3000.287254	22.295296
88.134354	3010.845032	22.300314
88.105229	3013.459853	22.305331
88.036849	3018.353312	22.310349
88.198266	3021.474841	22.315367
88.209238	3018.844033	22.320384
88.139935	3019.372567	22.325402
88.164839	3029.777980	22.330419
88.096300	3045.696206	22.335437
88.009140	3045.536322	22.340455
88.234279	3051.835674	22.345472
88.455264	3068.800618	22.350490
88.651451	3065.553724	22.355507
88.727951	3073.410304	22.360525
88.988648	3074.549948	22.365543
88.954833	3085.261280	22.370560
89.198614	3086.615044	22.375578
89.503008	3092.441181	22.380595
89.244823	3088.498503	22.385613
89.197080	3094.944779	22.390631
89.670834	3093.964765	22.395648
89.684558	3108.954846	22.400666
90.258997	3105.755995	22.405683
90.347869	3105.360219	22.410701
90.329295	3109.570462	22.415719
90.383577	3101.049608	22.420736
90.572163	3105.085364	22.425754
91.188171	3102.268219	22.430771
90.535518	3104.365275	22.435789
91.277466	3087.148538	22.440807
91.278391	3072.490848	22.445824
90.985814	3068.588281	22.450842
90.812704	3060.235634	22.455859
90.921382	3068.835201	22.460877
90.779808	3063.794823	22.465895
90.751137	3073.852001	22.470912
90.820546	3083.259412	22.475930
91.225835	3092.232299	22.480947
91.072315	3097.805087	22.485965
91.302639	3099.523929	22.490983
91.373055	3110.771289	22.496000
91.468422	3120.941622	22.501018
91.708793	3114.345326	22.506035
91.360894	3121.940170	22.511053
91.432322	3125.167347	22.516071
91.341963	3126.264152	22.521088
91.771168	3151.648998	22.526106
91.984692	3143.926958	22.531123
91.904955	3153.114741	22.536141
92.222562	3165.289222	22.541159
92.433945	3174.485062	22.546176
92.087853	3176.748722	22.551194
92.517003	3180.405928	22.556211
92.550540	3173.974579	22.561229
92.603238	3181.898061	22.566247
92.924674	3192.841018	22.571264
92.827742	3212.219949	22.576282
92.940481	3199.425773	22.581299
93.128256	3209.155582	22.586317
93.039674	3204.555052	22.591335
93.151514	3215.186828	22.596352
93.118356	3222.653496	22.601370
93.659616	3231.011771	22.606387
93.733293	3237.025603	22.611405
93.661979	3233.006271	22.616423
93.647406	3226.860192	22.621440
93.755979	3232.890650	22.626458
93.880260	3242.838738	22.631475
93.973859	3253.334519	22.636493
94.232305	3244.216638	22.641511
94.399014	3234.194658	22.646528
94.579394	3247.154512	22.651546
94.605542	3241.368177	22.656563
94.458087	3243.370315	22.661581
94.938303	3238.273503	22.666599
94.590385	3241.181336	22.671616
94.352547	3245.141899	22.676634
95.274386	3250.846101	22.681651
95.343073	3264.697754	22.686669
95.520849	3270.019845	22.691687
95.462711	3261.276652	22.696704
95.341003	3272.172304	22.701722
95.781740	3255.024694	22.706739
95.787571	3265.461638	22.711757
95.669207	3260.247130	22.716775
95.667208	3271.780532	22.721792
95.502231	3265.355003	22.726810
95.746071	3267.463121	22.731827
96.122082	3264.345832	22.736845
95.949261	3262.043630	22.741863
96.207784	3257.486549	22.746880
96.078090	3272.789614	22.751898
95.950603	3278.967541	22.756915
95.795989	3286.721547	22.761933
96.138708	3294.511265	22.766951
96.525295	3286.945114	22.771968
96.383377	3308.922503	22.776986
96.699288	3307.585298	22.782003
96.576288	3317.638452	22.787021
96.258969	3321.658828	22.792039
96.994055	3335.554475	22.797056
96.876179	3339.641454	22.802074
97.069551	3343.540792	22.807091
97.248005	3352.221094	22.812109
96.980495	3358.127450	22.817127
97.143261	3357.281367	22.822144
97.086684	3369.827083	22.827162
97.430163	3379.740905	22.832179
97.363478	3388.090344	22.837197
97.192056	3393.694434	22.842215
97.859206	3405.773282	22.847232
97.875427	3418.986232	22.852250
98.047099	3408.038583	22.857267
98.261209	3421.643475	22.862285
97.963638	3434.132305	22.867303
98.462256	3440.859236	22.872320
98.193667	3447.848403	22.877338
98.623225	3442.364932	22.882355
99.220285	3452.011811	22.887373
99.276764	3453.663234	22.892391
99.326403	3445.010381	22.897408
99.553240	3452.439566	22.902426
100.195848	3449.801268	22.907443
100.053564	3443.810846	22.912461
99.573770	3435.272508	22.917479
99.994973	3427.015957	22.922496
99.812266	3436.983843	22.927514
99.903407	3445.763089	22.932531
100.171836	3451.386662	22.937549
100.195583	3457.042258	22.942567
100.271303	3444.626154	22.947584
100.337175	3442.696852	22.952602
100.198950	3449.144805	22.957619
100.452993	3449.919385	22.962637
100.157592	3452.064665	22.967655
100.310310	3446.479375	22.972672
100.564058	3468.615910	22.977690
100.520905	3476.153686	22.982707
100.821161	3480.014215	22.987725
100.251069	3491.027592	22.992743
100.709820	3490.769550	22.997760
100.718066	3495.947826	23.002778
101.151884	3501.441344	23.007795
101.285416	3508.102403	23.012813
101.128302	3509.496914	23.017831
101.141521	3517.363602	23.022848
101.133719	3532.581507	23.027866
101.313282	3538.408408	23.032883
101.678182	3545.970661	23.037901
101.684874	3556.183538	23.042919
102.356191	3546.467401	23.047936
102.212002	3557.773913	23.052954
102.137095	3556.652581	23.057971
102.426448	3554.483092	23.062989
102.171014	3557.209200	23.068007
102.554161	3556.120262	23.073024
102.649798	3579.039221	23.078042
102.648818	3579.755916	23.083059
102.953436	3583.249649	23.088077
102.748192	3587.530281	23.093095
102.726065	3581.072790	23.098112
103.093002	3588.205479	23.103130
103.054353	3593.160719	23.108147
103.443775	3608.221763	23.113165
103.419398	3610.760174	23.118183
103.536586	3606.423999	23.123200
103.471980	3606.115385	23.128218
103.495620	3622.906607	23.133235
103.886434	3627.905043	23.138253
103.635476	3635.810015	23.143271
103.994654	3626.770850	23.148288
103.893892	3635.596037	23.153306
104.103858	3649.365880	23.158323
104.026078	3657.414172	23.163341
104.133382	3663.855297	23.168359
104.534359	3668.230352	23.173376
104.754329	3676.557108	23.178394
104.682546	3677.963514	23.183411
104.779904	3668.103665	23.188429
104.699090	3677.295039	23.193447
104.856898	3693.872769	23.198464
105.302549	3698.850009	23.203482
105.357764	3700.249145	23.208499
105.286901	3704.527689	23.213517
105.640911	3709.686576	23.218535
106.161978	3708.389797	23.223552
105.712652	3714.908679	23.228570
105.558029	3719.023594	23.233587
106.047097	3724.117136	23.238605
106.079650	3738.290449	23.243623
106.232791	3735.293220	23.248640
106.172750	3741.271355	23.253658
106.222364	3755.587201	23.258675
106.622555	3758.759828	23.263693
106.550774	3769.155563	23.268711
106.855970	3755.873170	23.273728
106.758570	3767.396584	23.278746
107.031433	3767.811560	23.283763
106.827972	3758.024043	23.288781
106.865636	3782.748314	23.293799
107.350048	3773.815710	23.298816
107.500823	3775.982659	23.303834
107.532017	3778.310380	23.308851
107.878164	3770.933434	23.313869
107.593682	3782.700801	23.318887
108.024602	3785.669767	23.323904
108.622162	3786.665147	23.328922
108.347276	3792.086718	23.333939
108.712203	3791.698179	23.338957
108.460213	3789.446189	23.343975
108.295972	3793.092329	23.348992
108.485062	3785.661075	23.354010
108.559328	3790.507143	23.359027
109.209303	3781.333964	23.364045
109.187102	3781.230179	23.369063
108.937740	3782.288807	23.374080
109.226962	3782.972668	23.379098
108.986338	3780.475858	23.384115
109.206921	3772.379995	23.389133
109.382930	3780.404362	23.394151
109.237097	3784.281187	23.399168
109.337368	3788.087892	23.404186
109.359879	3800.716207	23.409203
109.408910	3807.204390	23.414221
109.426271	3805.718229	23.419239
109.883025	3821.917821	23.424256
109.678003	3823.171513	23.429274
109.741132	3835.515727	23.434291
110.120345	3834.187506	23.439309
110.018872	3855.565822	23.444327
110.099292	3863.737770	23.449344
110.233162	3855.387162	23.454362
110.247471	3880.563431	23.459379
110.547406	3882.312476	23.464397
110.489247	3896.515907	23.469415
110.062948	3900.865966	23.474432
110.724402	3904.938290	23.479450
110.964840	3922.882626	23.484467
111.000047	3927.037288	23.489485
111.509260	3938.983420	23.494503
111.412146	3946.075325	23.499520
111.770925	3949.213441	23.504538
111.574584	3947.877536	23.509555
111.997777	3952.826801	23.514573
112.095881	3976.604416	23.519591
112.626175	3972.522229	23.524608
112.506236	3962.727829	23.529626
112.341354	3967.005383	23.534643
112.746380	3962.674530	23.539661
112.623508	3963.028413	23.544679
112.827547	3954.834055	23.549696
112.865891	3973.488729	23.554714
113.126320	3983.153913	23.559731
113.264776	3980.840728	23.564749
112.896802	3988.031900	23.569767
113.252270	3984.090731	23.574784
113.468832	3983.832751	23.579802
113.500186	4000.834594	23.584819
113.929339	4007.149663	23.589837
114.133364	4015.690553	23.594855
113.916714	4015.348936	23.599872
114.129538	4017.856555	23.604890
114.008335	4015.940719	23.609907
114.186148	4010.300823	23.614925
114.454724	4031.302573	23.619943
114.108858	4033.679932	23.624960
114.596958	4032.612401	23.629978
114.396155	4027.988210	23.634995
114.883595	4034.455134	23.640013
114.829182	4025.316437	23.645031
115.036335	4044.307723	23.650048
115.425796	4053.128906	23.655066
115.337012	4055.121941	23.660083
115.603928	4046.466324	23.665101
115.330997	4053.525845	23.670119
115.391034	4049.356339	23.675136
115.832951	4057.995704	23.680154
115.988880	4077.708400	23.685171
115.688498	4076.919064	23.690189
115.779679	4075.995784	23.695207
115.900167	4078.568380	23.700224
116.265280	4081.904381	23.705242
116.240108	4093.953277	23.710259
116.711282	4096.553000	23.715277
116.895230	4102.205794	23.720295
116.573570	4116.128724	23.725312
116.898607	4110.954977	23.730330
116.612340	4101.420136	23.735347
116.576397	4104.386545	23.740365
116.664325	4117.465670	23.745383
117.006527	4133.430975	23.750400
117.197837	4127.359654	23.755418
116.993309	4138.104667	23.760435
117.768798	4149.311650	23.765453
117.735816	4154.064143	23.770471
117.694490	4155.800396	23.775488
117.675261	4157.889863	23.780506
117.825840	4173.099274	23.785523
117.932601	4181.712296	23.790541
118.115869	4182.516936	23.795559
118.072408	4193.662866	23.800576
118.533795	4199.783567	23.805594
118.208708	4210.487538	23.810611
118.568614	4210.112404	23.815629
118.648244	4227.368880	23.820647
118.754144	4229.565010	23.825664
118.983033	4226.082366	23.830682
118.986739	4242.482729	23.835699
119.095702	4258.686699	23.840717
119.160549	4262.890454	23.845735
119.152278	4275.189338	23.850752
119.534869	4286.202289	23.855770
119.378501	4289.073963	23.860787
119.629074	4299.836151	23.865805
119.901793	4308.713627	23.870823
120.006951	4316.035972	23.875840
120.153844	4319.775512	23.880858
120.213405	4331.337821	23.885875
120.397186	4342.473492	23.890893
120.620847	4331.460326	23.895911
120.928054	4352.749946	23.900928
121.225840	4360.970132	23.905946
121.637372	4364.226315	23.910963
121.218165	4358.840826	23.915981
121.818934	4358.639437	23.920999
121.489449	4369.132707	23.926016
121.328810	4358.697393	23.931034
121.482019	4364.800147	23.936051
121.627366	4376.772011	23.941069
121.863900	4381.779047	23.946087
121.701994	4389.727210	23.951104
122.051978	4404.709872	23.956122
122.234621	4422.837364	23.961139
122.425577	4423.694471	23.966157
122.835363	4412.027113	23.971175
122.491192	4422.547966	23.976192
122.991805	4427.340035	23.981210
122.620952	4444.320081	23.986227
122.964128	4450.008011	23.991245
123.339073	4441.202710	23.996263
123.170264	4444.534047	24.001280
123.812565	4457.233010	24.006298
123.788822	4465.352106	24.011315
123.800389	4464.318177	24.016333
124.139680	4458.075207	24.021351
123.701675	4463.285796	24.026368
124.251237	4457.142456	24.031386
124.446176	4462.673694	24.036403
124.555234	4454.920119	24.041421
124.838818	4457.287297	24.046439
124.731293	4454.346571	24.051456
124.849435	4445.559406	24.056474
124.909770	4454.934230	24.061491
125.038858	4465.163165	24.066509
125.700888	4479.538304	24.071527
125.102101	4483.328417	24.076544
125.433202	4469.908872	24.081562
125.561875	4477.969373	24.086579
125.121643	4481.418996	24.091597
125.384640	4477.201813	24.096615
125.409777	4488.864310	24.101632
125.906549	4491.715757	24.106650
126.368454	4494.910412	24.111667
126.442318	4498.645648	24.116685
126.318971	4497.576037	24.121703
126.410692	4497.940499	24.126720
126.564243	4498.011191	24.131738
126.462794	4510.545787	24.136755
126.702975	4520.050293	24.141773
126.861300	4515.499129	24.146791
127.060146	4526.073853	24.151808
127.121574	4529.410169	24.156826
126.973197	4541.560733	24.161843
127.154839	4546.705831	24.166861
127.306412	4541.309776	24.171879
127.628663	4562.303732	24.176896
127.535790	4569.679300	24.181914
127.565689	4573.746560	24.186931
127.704792	4583.866671	24.191949
127.905954	4588.311135	24.196967
127.710444	4587.637918	24.201984
128.215734	4618.227453	24.207002
128.698400	4627.245802	24.212019
128.850190	4614.349816	24.217037
129.390385	4613.902239	24.222055
129.789545	4606.598722	24.227072
130.007715	4593.951185	24.232090
130.310986	4591.230163	24.237107
130.239015	4595.780551	24.242125
130.218647	4570.373922	24.247143
130.085404	4565.745321	24.252160
130.335796	4563.619697	24.257178
130.309168	4558.873387	24.262195
130.627681	4557.153750	24.267213
130.691761	4545.549938	24.272231
130.438394	4554.563616	24.277248
130.544643	4561.002070	24.282266
130.760920	4571.204779	24.287283
130.832582	4578.491444	24.292301
131.197164	4575.451482	24.297319
130.975545	4581.152183	24.302336
131.369873	4583.088526	24.307354
131.239875	4587.389168	24.312371
130.999761	4583.175026	24.317389
131.185897	4598.615961	24.322407
131.187622	4614.483520	24.327424
131.032767	4616.237603	24.332442
131.449533	4630.057863	24.337459
131.961832	4642.581621	24.342477
131.596501	4646.770790	24.347495
131.556720	4660.833052	24.352512
131.545671	4664.979347	24.357530
131.911034	4686.080327	24.362547
131.921535	4697.890451	24.367565
132.232399	4708.046853	24.372583
132.059541	4720.318163	24.377600
132.508856	4729.231309	24.382618
132.693324	4748.653018	24.387635
132.682627	4754.453303	24.392653
132.988581	4759.440098	24.397671
133.022028	4779.759861	24.402688
133.800814	4779.363285	24.407706
133.872583	4777.442388	24.412723
133.614561	4779.907088	24.417741
134.405391	4780.487152	24.422759
134.495370	4787.341741	24.427776
134.802403	4791.889617	24.432794
134.910455	4793.441544	24.437811
135.099169	4788.740350	24.442829
134.999140	4793.715002	24.447847
135.153125	4792.930205	24.452864
135.029516	4799.013343	24.457882
135.486314	4801.113533	24.462899
135.246407	4798.401822	24.467917
135.455184	4790.629324	24.472935
135.603551	4800.012631	24.477952
135.694106	4801.646214	24.482970
135.922354	4811.051733	24.487987
135.726682	4810.040782	24.493005
136.189388	4807.610405	24.498023
136.172678	4813.869350	24.503040
136.306126	4828.886288	24.508058
136.379112	4837.814254	24.513075
136.316111	4835.343130	24.518093
136.691402	4838.750279	24.523111
136.759022	4858.837506	24.528128
136.624581	4866.235490	24.533146
136.902077	4865.178814	24.538163
136.797918	4885.479219	24.543181
137.378242	4887.496936	24.548199
137.541874	4888.626654	24.553216
137.545898	4905.466327	24.558234
137.617087	4914.132618	24.563251
137.640355	4922.042532	24.568269
137.964898	4932.490477	24.573287
138.181600	4939.290548	24.578304
138.159741	4944.281404	24.583322
138.312891	4950.955704	24.588339
138.346741	4966.831163	24.593357
138.426386	4962.869867	24.598375
138.489161	4983.226298	24.603392
138.610628	4993.507230	24.608410
139.030966	4999.145366	24.613427
139.284564	5011.621525	24.618445
139.242954	5024.841547	24.623463
139.558307	5030.114194	24.628480
139.693648	5028.713617	24.633498
139.699894	5044.107354	24.638515
139.893616	5048.679361	24.643533
140.269265	5058.664823	24.648551
140.446965	5067.008312	24.653568
140.550649	5075.802165	24.658586
140.547735	5069.461084	24.663603
140.345238	5075.452506	24.668621
140.510576	5082.172293	24.673639
140.645147	5102.018867	24.678656
140.800859	5105.286855	24.683674
140.961978	5109.308424	24.688691
141.436471	5127.024730	24.693709
141.781532	5129.650677	24.698727
141.957216	5133.032336	24.703744
141.987818	5139.126149	24.708762
142.215674	5138.620171	24.713779
142.484261	5149.402138	24.718797
142.591565	5147.103156	24.723815
142.803999	5141.672137	24.728832
142.973662	5144.672792	24.733850
143.345741	5144.463036	24.738867
143.274050	5148.227523	24.743885
143.142292	5140.397746	24.748903
143.327764	5146.694575	24.753920
142.910732	5153.998057	24.758938
143.718848	5151.355692	24.763955
143.718682	5166.722128	24.768973
143.509364	5171.354152	24.773991
143.705904	5184.432811	24.779008
143.723593	5190.007824	24.784026
144.011086	5187.185019	24.789043
144.006050	5202.653260	24.794061
144.287686	5207.902832	24.799079
144.458470	5213.163459	24.804096
144.332804	5229.559726	24.809114
144.780493	5219.290612	24.814131
144.762636	5238.551988	24.819149
144.572663	5258.471675	24.824167
144.978987	5269.459411	24.829184
144.619168	5288.064173	24.834202
145.269444	5290.954833	24.839219
145.400595	5305.009751	24.844237
145.397452	5310.266088	24.849255
145.730594	5313.825137	24.854272
145.844562	5333.116466	24.859290
146.678833	5337.521903	24.864307
146.225932	5337.722333	24.869325
146.461311	5346.173709	24.874343
146.915117	5359.666745	24.879360
146.978757	5365.231455	24.884378
147.336638	5365.371153	24.889395
146.824267	5376.338737	24.894413
147.381286	5379.187203	24.899431
147.976831	5396.237694	24.904448
147.589571	5389.603172	24.909466
148.001966	5383.534678	24.914483
147.801491	5408.172200	24.919501
147.536865	5416.739822	24.924519
147.460712	5419.144547	24.929536
148.070594	5442.436692	24.934554
148.506675	5449.404611	24.939571
148.108762	5458.075206	24.944589
148.411483	5477.930569	24.949607
148.726688	5475.605288	24.954624
148.757076	5506.977812	24.959642
148.847814	5502.045565	24.964659
149.001820	5519.234793	24.969677
149.024779	5533.120594	24.974695
149.512521	5541.731393	24.979712
149.637913	5554.243793	24.984730
150.037670	5551.182378	24.989747
150.042948	5564.872102	24.994765
150.345980	5577.688139	24.999783
151.027413	5570.996606	25.004800
151.124205	5574.952595	25.009818
151.419863	5563.103516	25.014835
151.372796	5562.814216	25.019853
151.426902	5568.386796	25.024871
151.716635	5560.891703	25.029888
151.906165	5569.157808	25.034906
152.208904	5560.072869	25.039923
152.273418	5565.179787	25.044941
152.172571	5561.704356	25.049959
152.380711	5566.166907	25.054976
152.599668	5580.056761	25.059994
152.641723	5595.593717	25.065011
152.573009	5597.470135	25.070029
152.533245	5592.640383	25.075047
152.808766	5589.367987	25.080064
152.169551	5591.804128	25.085082
153.013590	5602.647730	25.090099
153.157576	5605.182139	25.095117
153.234630	5613.914134	25.100135
153.358682	5611.975489	25.105152
153.320219	5629.819998	25.110170
153.637263	5638.826919	25.115187
154.005744	5641.998536	25.120205
153.903852	5650.035702	25.125223
154.471487	5666.181693	25.130240
154.283369	5674.017722	25.135258
154.346374	5671.646697	25.140275
154.624520	5686.906835	25.145293
154.381768	5695.619524	25.150311
154.713055	5692.638261	25.155328
154.480571	5711.662284	25.160346
154.763419	5710.879357	25.165363
155.067201	5725.636752	25.170381
155.224918	5734.343541	25.175399
155.306752	5741.868987	25.180416
155.416619	5764.876858	25.185434
155.914381	5774.900405	25.190451
156.045775	5788.699964	25.195469
155.739023	5788.100949	25.200487
156.308191	5796.907456	25.205504
156.684308	5816.947406	25.210522
156.544350	5822.499959	25.215539
156.786044	5838.694010	25.220557
156.787065	5855.544499	25.225575
157.359049	5866.007880	25.230592
157.373220	5881.192736	25.235610
157.571233	5881.714196	25.240627
158.069294	5888.795687	25.245645
158.260758	5905.202853	25.250663
158.178078	5905.443145	25.255680
158.545466	5908.034142	25.260698
158.819199	5909.424468	25.265715
158.767090	5902.721468	25.270733
158.696175	5917.348316	25.275751
159.097260	5918.737632	25.280768
158.883457	5932.092615	25.285786
159.326403	5938.232581	25.290803
159.116945	5952.322419	25.295821
159.254477	5963.917742	25.300839
159.624185	5977.724303	25.305856
159.498784	5986.503977	25.310874
159.774066	5992.083074	25.315891
160.254593	6001.468626	25.320909
159.937850	6014.410478	25.325927
160.275081	6015.197395	25.330944
160.389667	6036.699098	25.335962
160.709676	6047.940741	25.340979
160.893327	6060.700058	25.345997
160.689052	6072.989822	25.351015
161.150356	6077.551734	25.356032
161.366150	6088.149965	25.361050
161.219326	6107.426147	25.366067
161.675392	6114.542716	25.371085
162.050032	6123.206235	25.376103
162.255197	6127.214815	25.381120
162.406733	6128.801082	25.386138
162.560732	6132.104248	25.391155
162.703944	6143.913457	25.396173
162.786938	6140.772144	25.401191
163.322984	6140.246269	25.406208
163.188899	6147.108061	25.411226
163.292271	6153.124520	25.416243
163.539973	6171.032055	25.421261
163.864691	6178.863718	25.426279
163.892783	6174.348330	25.431296
163.562436	6176.998168	25.436314
163.334898	6193.606978	25.441331
163.737045	6196.748166	25.446349
163.948836	6217.713982	25.451367
164.087746	6228.488492	25.456384
164.139283	6244.990492	25.461402
164.413249	6264.140935	25.466419
164.872518	6260.795440	25.471437
165.128170	6281.230430	25.476455
165.218948	6287.801346	25.481472
165.015597	6301.019217	25.486490
165.292312	6326.242984	25.491507
165.942006	6319.726623	25.496525
165.688922	6346.719154	25.501543
165.839704	6350.676323	25.506560
166.112780	6357.045080	25.511578
166.081135	6375.388022	25.516595
166.374946	6380.134092	25.521613
166.543844	6397.347066	25.526631
166.976463	6409.180556	25.531648
166.941899	6414.723089	25.536666
167.252568	6430.957368	25.541683
167.770896	6431.829579	25.546701
167.562980	6443.675048	25.551719
167.708368	6448.996834	25.556736
167.825989	6457.369311	25.561754
167.964262	6464.283258	25.566771
168.299736	6476.324576	25.571789
168.050163	6490.077015	25.576807
168.713901	6491.267387	25.581824
168.772229	6515.398638	25.586842
169.153493	6520.696118	25.591859
169.272615	6530.567893	25.596877
169.373916	6552.728904	25.601895
169.754372	6546.150469	25.606912
169.805554	6553.081250	25.611930
169.883570	6566.757169	25.616947
170.225544	6561.308595	25.621965
170.408777	6580.277859	25.626983
170.451148	6592.620878	25.632000
170.425456	6582.990245	25.637018
170.813461	6587.238614	25.642035
171.082252	6606.049286	25.647053
171.178704	6608.133538	25.652071
171.295574	6614.798346	25.657088
171.812611	6622.129699	25.662106
171.651189	6635.454888	25.667123
171.882928	6631.538856	25.672141
171.418198	6640.068944	25.677159
171.667432	6661.146205	25.682176
172.268709	6665.601103	25.687194
172.067643	6687.086724	25.692212
172.822365	6691.432353	25.697229
172.783951	6692.675918	25.702247
173.229645	6701.738974	25.707264
173.491658	6716.544751	25.712282
173.572835	6717.261325	25.717300
173.965407	6705.746742	25.722317
174.201027	6711.212311	25.727335
174.512325	6718.070835	25.732352
175.073049	6721.597665	25.737370
174.924209	6702.682954	25.742388
175.098519	6682.950517	25.747405
175.221479	6691.151794	25.752423
175.159286	6684.465872	25.757440
175.699377	6682.774467	25.762458
175.554727	6684.400871	25.767476
175.708444	6681.860818	25.772493
175.907979	6704.871606	25.777511
175.523385	6709.285239	25.782528
175.780879	6710.640290	25.787546
175.992612	6710.755546	25.792564
176.370109	6710.333419	25.797581
176.305374	6730.370827	25.802599
176.524996	6738.487530	25.807616
176.502145	6741.382864	25.812634
176.058198	6759.528762	25.817652
176.681693	6765.205073	25.822669
176.816454	6781.940754	25.827687
176.854577	6792.500932	25.832704
177.242189	6804.417495	25.837722
176.977285	6824.600012	25.842740
177.481353	6834.335878	25.847757
177.561833	6850.802318	25.852775
177.975066	6866.752579	25.857792
178.180368	6873.735102	25.862810
178.358026	6886.088692	25.867828
178.446460	6902.503422	25.872845
178.519482	6911.820695	25.877863
178.747298	6930.764396	25.882880
179.081281	6937.041733	25.887898
178.964799	6956.452955	25.892916
179.665879	6966.372697	25.897933
179.790786	6972.828020	25.902951
180.144252	6990.704001	25.907968
180.207382	6993.456470	25.912986
179.791020	7006.758728	25.918004
180.297413	7011.859961	25.923021
180.975432	7021.849642	25.928039
180.851818	7041.382033	25.933056
180.872980	7052.658485	25.938074
180.988930	7065.031334	25.943092
181.598385	7065.185306	25.948109
181.767943	7073.821424	25.953127
181.808193	7083.128133	25.958144
182.312331	7104.961519	25.963162
182.270018	7104.788255	25.968180
182.689394	7107.402851	25.973197
182.732252	7120.491186	25.978215
182.961235	7124.685671	25.983232
183.108294	7131.832107	25.988250
182.913931	7142.889823	25.993268
183.396150	7149.008262	25.998285
183.669909	7157.274517	26.003303
183.138396	7173.982342	26.008320
183.939718	7178.838530	26.013338
183.870217	7185.693747	26.018356
183.967687	7200.964510	26.023373
184.106443	7209.722325	26.028391
184.142681	7222.556057	26.033408
184.933630	7231.025447	26.038426
184.645235	7244.181550	26.043444
184.872057	7261.698799	26.048461
185.086366	7273.393416	26.053479
185.161898	7291.193266	26.058496
185.444139	7298.571147	26.063514
185.773471	7315.459935	26.068532
185.684204	7324.780742	26.073549
186.260795	7336.702771	26.078567
185.880337	7351.016200	26.083584
186.247117	7352.572011	26.088602
186.632300	7368.527102	26.093620
186.825956	7381.895069	26.098637
187.218924	7374.569331	26.103655
187.183572	7400.108649	26.108672
187.618737	7402.872350	26.113690
187.486800	7417.831963	26.118708
187.674444	7424.157650	26.123725
187.758543	7434.682581	26.128743
187.617256	7436.419018	26.133760
188.053544	7449.367026	26.138778
188.231494	7467.368834	26.143796
188.355552	7482.604095	26.148813
188.691950	7495.226828	26.153831
189.030209	7513.127799	26.158848
189.263038	7514.572015	26.163866
189.307055	7544.629409	26.168884
189.692990	7544.524803	26.173901
189.842680	7550.275588	26.178919
190.303163	7565.193023	26.183936
190.421359	7569.657528	26.188954
190.280437	7587.586285	26.193972
190.822227	7591.365657	26.198989
190.772122	7597.561328	26.204007
190.990705	7606.291040	26.209024
191.341904	7613.531964	26.214042
191.155887	7631.448886	26.219060
191.192698	7647.638746	26.224077
191.721747	7661.693119	26.229095
191.993608	7678.922733	26.234112
191.832962	7681.233649	26.239130
192.043852	7703.852434	26.244148
192.466933	7711.738799	26.249165
193.099824	7733.227585	26.254183
193.078201	7733.234183	26.259200
193.266126	7748.008199	26.264218
193.222323	7766.022940	26.269236
193.714085	7776.673624	26.274253
193.908056	7782.572241	26.279271
193.708213	7803.497013	26.284288
194.495260	7797.997295	26.289306
194.388225	7820.135642	26.294324
194.496902	7826.076049	26.299341
194.491221	7834.263260	26.304359
194.738008	7855.370687	26.309376
194.874791	7871.731349	26.314394
194.979315	7885.119958	26.319412
195.018241	7901.151855	26.324429
195.113797	7909.339026	26.329447
195.146499	7923.035680	26.334464
195.776622	7940.222040	26.339482
195.843355	7970.488092	26.344500
195.964307	7990.444106	26.349517
196.687513	8001.446985	26.354535
196.620306	8022.774277	26.359552
196.927285	8035.771369	26.364570
197.061113	8047.548542	26.369588
197.134367	8060.272871	26.374605
197.715043	8069.880580	26.379623
197.896253	8085.880876	26.384640
198.893004	8082.027805	26.389658
199.229892	8073.997072	26.394676
199.567740	8070.474539	26.399693
199.982922	8065.695992	26.404711
199.890647	8069.666354	26.409728
200.000298	8064.664161	26.414746
200.246975	8060.294023	26.419764
200.127257	8062.582789	26.424781
200.216836	8066.231051	26.429799
200.417874	8069.577712	26.434816
200.560125	8070.082717	26.439834
200.519334	8083.140639	26.444852
200.996109	8089.736971	26.449869
200.777411	8088.151689	26.454887
201.043002	8089.878115	26.459904
200.998105	8101.935891	26.464922
201.619342	8110.792190	26.469940
202.160344	8109.570929	26.474957
202.345224	8115.240608	26.479975
202.159782	8111.847402	26.484992
202.341505	8134.543898	26.490010
202.405223	8142.777202	26.495028
202.495564	8144.044892	26.500045
202.635705	8155.628561	26.505063
202.713398	8175.979879	26.510080
202.815836	8171.480769	26.515098
203.197799	8197.587236	26.520116
203.348767	8207.874819	26.525133
203.194715	8224.619169	26.530151
203.246990	8242.240466	26.535168
203.646448	8254.569698	26.540186
203.851811	8272.627983	26.545204
204.027692	8295.442404	26.550221
204.241615	8305.593893	26.555239
204.576655	8329.775725	26.560256
204.749064	8334.250864	26.565274
205.204608	8346.047285	26.570292
205.247885	8370.524292	26.575309
205.690999	8373.972000	26.580327
205.739131	8398.167296	26.585344
206.162980	8398.151464	26.590362
206.361518	8413.581040	26.595380
206.800015	8419.195295	26.600397
206.972296	8423.503147	26.605415
206.817390	8433.380985	26.610432
207.206334	8439.754414	26.615450
207.419113	8454.130456	26.620468
207.805190	8465.385331	26.625485
208.461065	8459.650240	26.630503
208.394516	8476.011719	26.635520
208.596042	8491.683995	26.640538
208.895617	8493.815569	26.645556
208.929590	8498.334537	26.650573
209.213906	8505.488417	26.655591
209.470832	8518.140087	26.660608
209.345319	8521.080197	26.665626
209.542856	8537.877094	26.670644
209.647461	8545.763196	26.675661
210.410445	8566.878969	26.680679
210.111505	8575.336611	26.685696
210.347346	8586.236232	26.690714
210.702325	8591.986754	26.695732
210.610353	8601.554889	26.700749
210.946641	8613.190202	26.705767
210.895064	8628.962232	26.710784
211.157743	8640.612252	26.715802
211.660659	8657.547691	26.720820
211.458376	8682.890768	26.725837
212.100282	8684.760360	26.730855
211.959568	8701.171542	26.735872
212.312119	8710.714295	26.740890
212.374757	8731.400089	26.745908
212.931598	8747.844109	26.750925
213.142143	8742.917487	26.755943
213.019954	8756.345400	26.760960
213.019331	8766.631784	26.765978
213.087845	8782.852400	26.770996
213.775818	8792.023768	26.776013
214.557858	8790.916253	26.781031
214.852348	8805.595490	26.786048
215.133027	8812.541683	26.791066
215.597790	8818.805492	26.796084
214.937227	8820.879142	26.801101
215.164509	8824.910107	26.806119
215.439256	8848.862112	26.811136
215.461561	8855.719351	26.816154
216.006491	8858.933352	26.821172
215.979500	8866.243488	26.826189
216.321052	8872.728681	26.831207
216.605207	8907.868558	26.836224
216.648866	8908.016477	26.841242
217.002857	8921.338340	26.846260
217.057068	8939.383067	26.851277
217.399634	8942.129938	26.856295
217.335117	8957.421214	26.861312
217.546412	8972.217805	26.866330
217.883511	8982.899733	26.871348
217.676013	9000.230932	26.876365
218.241649	9025.043729	26.881383
218.182864	9036.371801	26.886400
218.490078	9048.542365	26.891418
219.006130	9066.243338	26.896436
218.817094	9079.861922	26.901453
219.133765	9099.905289	26.906471
219.183160	9115.368286	26.911488
219.622787	9137.425722	26.916506
219.880718	9151.312166	26.921524
219.831788	9175.283726	26.926541
220.415312	9196.905085	26.931559
220.914887	9205.787287	26.936576
221.101014	9222.927579	26.941594
221.601728	9229.318504	26.946612
221.244569	9238.038149	26.951629
221.861193	9253.254534	26.956647
221.823408	9269.293317	26.961664
222.038728	9283.334929	26.966682
222.481381	9292.497619	26.971700
222.377042	9307.072395	26.976717
222.351885	9323.355516	26.981735
222.866467	9345.732976	26.986752
223.009467	9373.274071	26.991770
223.146011	9376.012238	26.996788
223.394258	9400.704763	27.001805
223.283049	9419.161063	27.006823
223.750726	9441.924867	27.011840
224.055547	9464.471096	27.016858
224.420593	9473.927037	27.021876
224.546573	9501.654114	27.026893
224.963477	9518.395431	27.031911
225.477097	9529.640445	27.036928
225.900457	9539.046238	27.041946
226.379588	9539.558500	27.046964
226.330525	9549.436134	27.051981
226.728489	9544.066328	27.056999
227.020233	9559.131789	27.062016
227.444228	9571.562249	27.067034
227.233410	9568.084344	27.072052
227.447666	9580.408744	27.077069
227.858032	9590.097604	27.082087
227.785613	9595.043963	27.087104
227.629382	9613.109680	27.092122
228.469416	9626.630598	27.097140
228.295686	9630.190965	27.102157
228.458884	9645.633416	27.107175
228.486655	9655.274896	27.112192
228.311381	9667.496193	27.117210
228.691727	9680.227200	27.122228
229.250627	9703.576936	27.127245
229.380659	9717.205990	27.132263
229.779699	9732.838899	27.137280
229.487739	9754.279162	27.142298
230.025788	9765.763611	27.147316
229.794156	9788.479522	27.152333
230.770927	9805.414398	27.157351
230.439519	9819.172648	27.162368
231.005543	9843.929645	27.167386
231.005144	9849.054233	27.172404
231.174292	9875.742631	27.177421
231.389214	9900.245280	27.182439
231.679057	9912.270733	27.187456
231.837719	9936.147601	27.192474
232.223341	9953.983521	27.197492
232.573526	9974.120460	27.202509
232.839607	9990.598503	27.207527
232.954150	10007.567601	27.212544
233.516846	10025.922086	27.217562
233.128700	10031.211663	27.222580
233.556451	10056.300033	27.227597
233.693760	10078.096515	27.232615
234.495254	10092.034279	27.237632
234.540036	10112.446548	27.242650
235.030579	10119.963428	27.247668
235.218719	10144.893691	27.252685
235.422188	10149.238107	27.257703
236.101746	10157.615795	27.262720
236.112214	10169.508362	27.267738
236.413529	10180.461812	27.272756
236.816421	10183.063649	27.277773
237.088796	10193.181755	27.282791
237.492622	10205.063242	27.287808
237.554217	10206.423987	27.292826
237.520184	10212.595908	27.297844
238.001627	10228.686788	27.302861
237.960821	10233.189474	27.307879
238.293904	10249.404652	27.312896
238.164895	10264.871289	27.317914
238.230457	10288.943169	27.322932
238.637537	10305.680419	27.327949
238.258951	10322.900716	27.332967
239.188284	10337.721680	27.337984
239.044786	10367.162570	27.343002
239.420598	10376.146818	27.348020
239.804376	10395.559040	27.353037
239.568002	10419.163715	27.358055
240.171325	10445.671241	27.363072
240.344997	10463.973431	27.368090
240.551061	10481.995861	27.373108
240.577097	10513.115479	27.378125
240.825582	10529.663063	27.383143
241.663702	10541.558826	27.388160
241.773760	10549.078650	27.393178
242.242868	10564.357110	27.398196
242.924400	10573.549320	27.403213
243.353498	10590.845416	27.408231
243.624881	10588.393759	27.413248
243.573678	10598.044940	27.418266
244.015252	10600.678667	27.423284
244.286404	10614.763057	27.428301
244.159236	10622.897902	27.433319
244.564957	10620.516765	27.438336
244.762405	10632.850808	27.443354
244.856777	10642.599193	27.448372
244.790094	10653.421117	27.453389
245.143013	10668.992571	27.458407
245.402597	10674.714481	27.463424
245.320701	10691.099251	27.468442
245.464521	10702.892328	27.473460
245.646165	10712.118712	27.478477
245.564024	10737.139469	27.483495
246.426492	10754.172059	27.488512
246.101466	10777.399534	27.493530
246.793422	10801.133970	27.498548
246.957176	10811.638862	27.503565
247.034323	10833.764565	27.508583
247.277354	10843.878147	27.513600
247.352961	10865.227364	27.518618
247.880246	10889.982347	27.523636
248.018848	10905.357068	27.528653
248.039601	10924.542527	27.533671
248.733042	10940.392409	27.538688
249.012477	10968.785977	27.543706
248.895215	10986.891120	27.548724
248.991731	11003.715537	27.553741
249.384143	11030.758992	27.558759
249.854749	11052.725430	27.563776
250.032440	11067.721562	27.568794
250.358803	11080.275684	27.573812
250.732197	11098.427217	27.578829
250.900878	11116.443483	27.583847
251.353797	11141.213605	27.588864
251.510841	11161.931507	27.593882
252.108975	11178.532250	27.598900
251.892144	11192.598790	27.603917
251.884635	11218.372644	27.608935
252.148156	11233.383882	27.613952
252.449145	11270.331737	27.618970
252.867954	11288.533178	27.623988
252.922451	11317.600356	27.629005
252.691646	11341.394774	27.634023
253.270964	11356.631357	27.639040
253.846071	11392.721834	27.644058
254.156042	11412.569801	27.649076
254.685226	11432.064523	27.654093
254.557417	11459.471124	27.659111
254.991351	11472.933857	27.664128
255.386835	11506.933889	27.669146
255.301373	11524.444079	27.674164
255.294380	11541.042050	27.679181
255.690672	11570.640248	27.684199
256.051374	11581.834674	27.689216
256.672834	11607.750515	27.694234
256.832360	11627.372819	27.699252
257.339901	11635.730758	27.704269
257.502030	11645.860605	27.709287
258.033216	11666.299412	27.714304
258.145191	11689.936368	27.719322
258.218766	11696.284539	27.724340
259.007251	11714.156918	27.729357
259.062358	11742.223658	27.734375
259.699288	11747.937308	27.739392
259.773371	11759.700923	27.744410
260.092352	11764.333920	27.749428
260.386295	11776.391507	27.754445
260.503462	11794.577537	27.759463
260.680138	11800.694866	27.764480
260.564773	11820.995139	27.769498
260.682805	11831.447768	27.774516
261.055801	11857.295514	27.779533
260.986712	11868.415341	27.784551
261.490742	11885.962988	27.789568
262.032266	11903.324786	27.794586
262.278722	11916.700370	27.799604
262.511210	11933.365377	27.804621
263.171890	11946.256111	27.809639
263.882986	11945.768996	27.814656
263.593083	11961.063292	27.819674
263.484064	11966.094952	27.824692
264.187171	11969.584712	27.829709
264.477906	11997.074942	27.834727
264.571266	11998.793986	27.839744
264.572359	12005.434657	27.844762
264.416383	12019.719639	27.849780
265.146755	12034.269977	27.854797
265.300142	12051.395885	27.859815
265.312484	12076.905708	27.864832
265.485914	12101.098795	27.869850
265.681995	12123.712628	27.874868
266.173676	12137.476256	27.879885
266.211967	12170.245062	27.884903
266.468320	12189.344377	27.889920
266.847351	12205.929829	27.894938
267.164397	12229.889011	27.899956
267.716456	12245.288477	27.904973
268.213499	12257.554550	27.909991
268.805026	12278.259301	27.915008
268.669731	12289.326591	27.920026
269.143215	12305.205772	27.925044
269.671825	12307.500856	27.930061
269.579948	12339.971408	27.935079
269.603673	12344.218180	27.940096
269.880532	12372.469009	27.945114
269.917623	12389.420814	27.950132
270.509035	12399.865916	27.955149
270.673450	12429.021797	27.960167
271.008052	12444.032340	27.965184
271.093542	12462.782915	27.970202
271.100808	12486.658322	27.975220
271.525946	12509.003053	27.980237
271.770975	12530.618140	27.985255
272.161090	12545.206388	27.990272
272.558837	12566.393386	27.995290
272.771672	12591.310395	28.000308
273.243442	12617.282656	28.005325
272.918025	12627.700983	28.010343
273.836518	12659.183286	28.015360
273.886894	12679.145885	28.020378
273.852205	12698.408150	28.025396
274.310478	12723.299516	28.030413
274.556342	12750.324188	28.035431
274.688708	12774.354044	28.040448
275.125723	12792.680405	28.045466
275.158080	12820.818627	28.050484
275.879055	12841.386876	28.055501
276.050464	12868.357065	28.060519
276.146459	12881.535849	28.065536
276.368629	12906.653918	28.070554
276.671191	12939.894241	28.075572
277.041210	12951.823821	28.080589
277.510257	12968.260051	28.085607
277.646132	12991.920155	28.090624
277.778414	13006.905997	28.095642
277.858845	13028.708492	28.100660
278.505772	13052.923361	28.105677
278.862793	13088.713350	28.110695
279.226276	13103.865160	28.115712
279.434500	13123.658234	28.120730
279.721415	13145.333779	28.125748
279.701599	13149.852820	28.130765
280.091692	13180.379797	28.135783
280.242488	13198.852443	28.140800
280.468075	13218.004987	28.145818
280.857841	13245.759421	28.150836
281.385829	13253.435915	28.155853
281.536373	13276.917230	28.160871
282.019686	13295.066294	28.165888
282.178855	13312.874563	28.170906
282.444200	13339.113843	28.175924
282.777866	13349.820909	28.180941
283.108551	13366.920234	28.185959
283.377837	13392.997913	28.190976
283.794859	13412.338567	28.195994
283.655916	13434.968553	28.201012
284.338174	13449.865432	28.206029
284.460191	13469.315517	28.211047
284.695825	13488.318333	28.216064
285.021436	13497.352997	28.221082
285.355152	13534.120146	28.226100
285.468085	13548.373627	28.231117
285.593886	13568.186394	28.236135
285.791422	13595.437746	28.241152
285.984888	13617.539013	28.246170
286.603737	13640.517924	28.251188
286.784781	13673.102747	28.256205
287.139722	13703.440274	28.261223
287.389646	13725.595984	28.266240
287.816213	13738.941486	28.271258
287.457822	13768.313961	28.276276
287.856843	13802.023868	28.281293
288.360276	13832.698359	28.286311
288.836154	13861.896078	28.291328
289.296272	13875.883826	28.296346
289.525492	13904.510739	28.301364
289.748551	13931.528034	28.306381
290.433523	13951.117807	28.311399
290.388449	13980.855239	28.316416
290.833762	13984.161542	28.321434
290.971011	14016.242201	28.326452
291.174388	14036.539125	28.331469
291.125998	14062.405363	28.336487
291.472365	14092.757486	28.341504
291.978514	14122.522482	28.346522
292.061366	14153.216002	28.351540
292.911533	14176.197224	28.356557
292.938850	14199.203154	28.361575
293.202384	14223.523793	28.366592
293.651974	14247.013148	28.371610
293.893305	14275.010250	28.376628
294.128570	14307.852949	28.381645
294.333650	14336.111630	28.386663
294.034014	14359.206868	28.391680
294.636147	14381.586086	28.396698
295.232972	14424.232141	28.401716
295.564557	14457.799022	28.406733
295.616125	14473.891393	28.411751
296.000634	14500.862096	28.416768
296.681892	14517.850692	28.421786
297.480376	14539.842463	28.426804
297.877843	14562.127627	28.431821
297.916026	14568.978141	28.436839
297.944279	14587.755569	28.441856
298.497225	14606.709795	28.446874
298.894091	14629.986808	28.451892
299.078949	14652.611729	28.456909
299.026207	14670.457621	28.461927
299.634842	14697.229266	28.466944
300.069631	14707.690709	28.471962
300.032721	14729.459843	28.476980
300.468089	14742.624653	28.481997
300.728397	14763.984071	28.487015
300.760899	14781.554580	28.492032
301.253281	14799.886840	28.497050
301.030826	14827.878449	28.502068
301.549481	14842.972598	28.507085
301.864080	14870.659064	28.512103
301.992875	14901.229734	28.517120
302.319631	14914.680128	28.522138
302.700926	14943.177396	28.527156
303.314856	14958.954688	28.532173
303.902924	14970.721892	28.537191
304.061664	15002.715568	28.542208
304.160573	15010.955841	28.547226
304.335931	15030.080176	28.552244
305.078357	15054.920612	28.557261
305.157814	15085.985680	28.562279
305.196928	15105.769407	28.567296
305.752857	15125.229007	28.572314
306.287877	15142.992742	28.577332
306.334316	15145.982739	28.582349
307.225169	15174.331049	28.587367
307.363874	15194.307714	28.592384
307.466079	15207.749274	28.597402
308.115334	15242.733224	28.602420
308.142565	15252.627148	28.607437
308.415319	15271.840693	28.612455
308.487665	15302.553495	28.617472
309.140751	15320.235735	28.622490
309.163880	15341.977209	28.627508
309.476885	15352.297009	28.632525
310.662201	15368.016717	28.637543
310.517731	15397.162363	28.642560
310.755312	15403.334483	28.647578
310.833155	15427.129875	28.652596
311.229635	15450.587973	28.657613
311.401715	15464.492519	28.662631
311.948051	15482.166364	28.667648
312.643340	15482.783922	28.672666
312.737013	15495.500601	28.677684
313.148678	15518.182609	28.682701
313.861220	15528.253575	28.687719
314.079471	15553.584198	28.692736
314.154458	15561.869514	28.697754
314.110274	15573.524522	28.702772
314.857682	15594.480096	28.707789
315.357954	15617.688422	28.712807
315.086465	15629.448555	28.717824
315.561961	15644.752236	28.722842
315.467047	15671.897603	28.727860
315.938094	15702.962338	28.732877
316.158634	15712.999930	28.737895
316.331746	15739.857053	28.742912
316.408147	15755.179122	28.747930
316.964486	15782.459507	28.752948
317.069871	15806.276322	28.757965
317.309897	15836.088835	28.762983
317.294373	15872.750957	28.768000
317.694403	15892.567394	28.773018
318.182583	15924.109882	28.778036
318.748679	15956.543527	28.783053
319.576904	15980.771625	28.788071
319.828945	16006.498673	28.793088
319.769830	16024.646874	28.798106
320.132153	16056.427227	28.803124
320.413000	16072.570302	28.808141
320.585976	16103.995065	28.813159
320.561571	16123.044395	28.818176
321.074840	16148.373807	28.823194
321.393833	16184.920954	28.828212
321.520313	16205.784955	28.833229
322.162061	16225.437533	28.838247
322.179609	16261.131880	28.843264
322.548373	16290.545914	28.848282
322.952044	16317.898352	28.853300
322.961712	16344.696643	28.858317
323.443563	16374.775324	28.863335
322.951173	16406.162674	28.868352
323.914311	16443.395874	28.873370
323.962745	16487.427413	28.878388
324.483813	16515.617699	28.883405
324.815450	16538.679836	28.888423
325.009675	16577.142382	28.893440
325.476691	16607.956530	28.898458
326.296575	16643.352182	28.903476
326.546532	16676.054501	28.908493
326.766067	16706.566451	28.913511
326.686587	16741.212455	28.918528
327.369459	16772.561592	28.923546
327.715962	16808.568656	28.928564
327.776410	16843.155021	28.933581
328.334464	16869.220630	28.938599
328.607199	16909.974141	28.943616
329.114369	16934.038952	28.948634
329.572520	16968.667476	28.953652
330.153683	16995.051812	28.958669
330.654649	17011.379137	28.963687
330.671588	17046.152720	28.968704
331.252992	17081.280150	28.973722
331.686831	17097.220078	28.978740
332.051035	17117.567718	28.983757
332.734204	17135.281666	28.988775
332.880770	17166.592268	28.993792
333.004069	17174.539054	28.998810
333.732755	17200.925832	29.003828
334.065739	17224.974070	29.008845
334.482862	17236.191420	29.013863
334.288078	17268.162114	29.018880
334.611459	17296.406619	29.023898
335.330160	17318.120329	29.028916
335.797314	17337.346548	29.033933
335.923887	17361.477828	29.038951
336.076604	17381.561961	29.043968
336.111981	17402.618411	29.048986
337.030533	17432.886188	29.054004
336.964278	17447.293823	29.059021
337.526819	17471.300092	29.064039
337.775158	17496.764378	29.069056
337.772353	17528.787555	29.074074
338.787012	17539.248157	29.079092
338.347052	17573.336173	29.084109
338.740165	17591.854062	29.089127
339.391926	17629.548961	29.094144
339.723925	17647.438419	29.099162
340.011360	17672.334563	29.104180
340.053748	17711.533859	29.109197
340.363558	17734.777731	29.114215
340.326262	17769.314727	29.119232
340.965945	17803.088724	29.124250
341.380596	17831.288125	29.129268
341.062012	17874.555881	29.134285
341.619272	17900.142878	29.139303
342.391680	17927.711487	29.144320
342.395595	17962.804628	29.149338
343.243185	17998.258442	29.154356
343.727076	18019.858103	29.159373
344.396651	18031.181673	29.164391
344.485477	18053.411834	29.169408
344.481597	18078.151970	29.174426
345.344734	18094.751992	29.179444
345.713682	18129.251263	29.184461
345.811687	18146.204932	29.189479
345.957049	18177.586847	29.194496
346.044085	18205.755982	29.199514
346.151571	18236.126795	29.204532
346.337960	18267.793038	29.209549
346.873949	18290.711537	29.214567
346.985762	18335.157466	29.219584
347.345212	18377.296674	29.224602
348.149460	18407.703916	29.229620
348.060036	18434.991282	29.234637
348.698602	18470.409208	29.239655
349.131197	18507.786354	29.244672
349.397198	18537.627391	29.249690
350.069150	18569.540268	29.254708
350.606757	18607.469749	29.259725
351.254932	18627.547055	29.264743
351.600247	18649.295479	29.269760
352.135957	18669.156689	29.274778
352.695661	18682.418443	29.279796
352.946068	18701.856865	29.284813
353.545127	18713.823656	29.289831
354.165460	18731.706856	29.294848
354.175054	18747.082823	29.299866
354.603788	18771.623402	29.304884
354.706336	18802.444432	29.309901
355.029207	18813.127814	29.314919
354.973228	18829.701861	29.319936
355.390558	18866.759881	29.324954
355.719946	18887.354909	29.329972
356.023476	18917.209603	29.334989
356.229825	18938.999072	29.340007
356.610585	18975.222757	29.345024
356.820349	18998.332184	29.350042
357.542391	19027.900366	29.355060
357.153195	19060.732093	29.360077
358.143601	19090.315194	29.365095
358.676505	19115.825476	29.370112
358.538979	19153.318438	29.375130
359.064732	19185.198364	29.380148
359.445073	19220.986635	29.385165
359.465323	19250.860941	29.390183
359.824125	19285.338577	29.395200
360.152300	19310.521061	29.400218
360.943229	19345.373369	29.405236
360.940151	19380.305888	29.410253
361.445113	19410.249825	29.415271
362.076316	19456.196441	29.420288
362.047125	19478.592026	29.425306
362.632066	19510.918108	29.430324
362.731738	19550.503842	29.435341
363.036379	19584.377641	29.440359
363.458760	19611.371666	29.445376
364.009204	19637.859179	29.450394
364.946416	19662.175914	29.455412
365.095890	19692.656139	29.460429
365.477994	19720.225250	29.465447
365.934829	19744.800559	29.470464
366.352290	19767.707773	29.475482
366.740717	19787.353107	29.480500
367.396883	19820.723668	29.485517
367.473440	19852.719273	29.490535
367.540209	19867.619624	29.495552
368.042528	19895.808281	29.500570
368.502035	19915.695336	29.505588
368.541808	19947.917993	29.510605
368.847832	19977.116827	29.515623
369.082177	20002.131673	29.520640
369.280139	20026.785795	29.525658
369.563774	20062.590753	29.530676
369.782387	20099.770692	29.535693
370.227241	20132.246109	29.540711
370.613398	20156.662414	29.545728
370.438254	20203.324684	29.550746
371.418140	20234.358043	29.555764
371.644501	20275.346998	29.560781
372.076440	20308.355462	29.565799
373.050697	20333.507560	29.570816
373.383060	20363.656903	29.575834
374.306410	20382.334485	29.580852
374.746746	20409.712213	29.585869
374.995467	20432.368631	29.590887
375.385928	20458.060935	29.595904
375.629730	20488.199068	29.600922
376.026523	20505.733494	29.605940
376.197372	20533.159926	29.610957
376.268038	20560.861140	29.615975
377.055808	20591.444965	29.620992
377.322343	20629.736748	29.626010
377.283065	20656.216919	29.631028
377.776168	20674.368247	29.636045
377.963362	20717.146041	29.641063
378.739410	20750.385674	29.646080
378.864020	20794.803588	29.651098
379.185620	20824.197113	29.656116
379.358632	20865.315703	29.661133
379.238167	20900.616826	29.666151
379.960052	20934.535011	29.671168
380.378248	20978.768345	29.676186
380.815343	21024.237242	29.681204
380.998831	21074.004642	29.686221
381.419692	21107.123597	29.691239
382.155793	21138.790515	29.696256
382.353761	21172.468931	29.701274
383.446728	21207.372019	29.706292
383.678721	21241.203187	29.711309
384.094554	21274.525404	29.716327
384.564649	21288.112577	29.721344
385.041802	21320.401658	29.726362
385.279270	21353.796179	29.731380
385.977228	21390.360070	29.736397
386.191252	21416.599388	29.741415
387.031248	21450.695839	29.746432
386.895728	21483.068517	29.751450
387.450050	21510.088715	29.756468
387.874696	21541.027873	29.761485
387.981692	21567.498990	29.766503
388.705629	21593.304825	29.771520
388.756245	21628.946933	29.776538
389.042595	21663.673881	29.781556
389.245620	21697.118608	29.786573
389.466924	21724.462967	29.791591
389.945116	21758.130081	29.796608
390.097034	21805.642164	29.801626
390.801898	21839.583529	29.806644
391.438451	21882.325053	29.811661
391.316514	21922.057682	29.816679
391.777855	21954.691490	29.821696
392.018276	21994.424375	29.826714
392.771970	22024.232232	29.831732
393.245843	22058.191198	29.836749
393.696969	22074.587441	29.841767
394.200555	22105.104393	29.846784
394.641232	22146.051024	29.851802
394.896319	22164.607502	29.856820
395.289107	22199.242891	29.861837
395.334909	22219.424556	29.866855
395.765205	22251.324408	29.871872
396.098303	22295.100100	29.876890
396.526214	22318.691088	29.881908
397.293996	22347.385099	29.886925
397.848994	22383.195994	29.891943
397.865883	22409.941426	29.896960
398.646095	22454.323561	29.901978
398.372473	22491.351304	29.906996
398.714865	22527.271588	29.912013
399.238913	22562.575819	29.917031
399.771307	22593.847288	29.922048
399.736273	22637.144284	29.927066
400.302362	22695.828816	29.932084
400.866153	22714.072054	29.937101
401.445894	22756.186139	29.942119
401.725377	22798.897102	29.947136
401.836601	22844.383308	29.952154
402.283000	22880.572298	29.957172
403.034210	22922.723068	29.962189
403.092457	22962.202063	29.967207
403.869448	22998.484824	29.972224
404.009951	23040.112228	29.977242
404.564529	23085.384199	29.982260
404.723643	23119.602815	29.987277
404.988906	23159.662733	29.992295
405.686035	23200.824135	29.997312
405.873170	23248.283595	30.002330
406.391113	23293.694480	30.007348
406.716077	23336.190937	30.012365
407.389627	23378.405390	30.017383
407.837543	23410.727731	30.022400
408.241343	23452.567524	30.027418
408.808155	23492.271232	30.032436
409.518095	23530.145284	30.037453
409.863242	23567.033864	30.042471
410.577175	23599.289566	30.047488
410.973987	23633.023159	30.052506
411.174247	23667.331059	30.057524
412.127016	23692.749903	30.062541
412.196108	23729.422930	30.067559
412.639179	23764.596631	30.072576
412.783224	23802.799976	30.077594
412.998623	23838.793072	30.082612
413.710060	23866.840888	30.087629
413.745616	23910.742568	30.092647
414.198627	23938.913116	30.097664
414.655388	23985.542167	30.102682
414.731780	24025.848266	30.107700
415.293113	24065.825709	30.112717
415.342809	24108.474355	30.117735
415.783945	24154.398466	30.122752
416.277381	24195.252571	30.127770
416.743737	24241.362516	30.132788
417.453311	24285.608127	30.137805
417.883301	24325.303324	30.142823
418.624891	24367.730394	30.147840
418.585781	24404.377367	30.152858
418.783349	24437.220868	30.157876
419.564018	24475.287859	30.162893
419.669169	24519.647620	30.167911
420.388974	24553.104666	30.172928
420.738888	24591.656444	30.177946
420.980258	24640.937081	30.182964
420.989475	24674.025339	30.187981
421.638026	24709.282267	30.192999
422.091673	24751.666777	30.198016
422.356152	24803.212954	30.203034
422.893156	24839.555610	30.208052
423.525853	24879.719409	30.213069
423.973989	24926.054970	30.218087
424.602178	24955.507692	30.223104
425.258580	24992.678769	30.228122
425.732233	25035.395690	30.233140
426.153183	25065.538289	30.238157
426.367697	25100.118156	30.243175
426.546936	25141.750177	30.248192
426.834611	25178.454810	30.253210
427.207472	25224.979805	30.258228
427.677595	25262.111039	30.263245
428.056945	25315.827198	30.268263
428.328559	25353.552160	30.273280
428.660748	25409.563745	30.278298
429.136426	25463.265208	30.283316
429.884379	25503.785074	30.288333
430.006529	25542.045712	30.293351
430.480421	25581.951391	30.298368
430.938306	25640.143264	30.303386
431.398401	25697.778801	30.308404
431.965745	25738.706626	30.313421
432.131657	25780.835011	30.318439
432.485525	25829.115012	30.323456
433.345636	25883.250338	30.328474
433.838658	25934.681448	30.333492
434.367763	25971.229625	30.338509
434.732392	26017.732456	30.343527
435.348909	26061.377183	30.348544
435.842390	26098.601099	30.353562
436.228208	26141.346760	30.358580
437.056086	26168.166094	30.363597
437.383517	26216.135154	30.368615
437.983610	26250.169946	30.373632
438.781006	26283.048903	30.378650
438.906239	26320.735398	30.383668
439.806018	26354.590701	30.388685
440.100334	26397.148989	30.393703
440.633734	26413.984641	30.398720
441.336303	26440.672281	30.403738
441.550715	26470.558601	30.408756
442.531102	26496.185245	30.413773
442.935023	26530.213314	30.418791
442.875666	26564.655297	30.423808
443.128699	26590.244302	30.428826
443.783480	26611.908738	30.433844
444.340054	26642.487507	30.438861
444.439902	26672.170860	30.443879
444.842557	26708.525286	30.448896
445.372550	26748.506643	30.453914
445.517892	26791.038529	30.458932
445.796435	26831.476575	30.463949
445.726443	26871.311979	30.468967
446.689065	26905.910482	30.473984
446.920137	26949.472128	30.479002
447.320962	27000.225145	30.484020
447.459688	27032.393161	30.489037
447.901132	27088.581888	30.494055
448.428112	27128.172599	30.499072
448.780082	27169.370906	30.504090
448.812789	27221.351413	30.509108
449.381193	27272.066219	30.514125
449.814317	27319.591539	30.519143
450.206803	27368.583369	30.524160
450.735312	27413.711145	30.529178
450.963671	27467.001579	30.534196
451.826399	27510.926886	30.539213
452.443671	27567.765692	30.544231
452.908254	27615.463751	30.549248
453.376725	27651.525128	30.554266
453.579705	27701.514488	30.559284
454.222892	27734.856076	30.564301
454.781275	27782.046825	30.569319
455.079810	27828.873864	30.574336
455.496907	27869.861125	30.579354
455.924280	27917.331854	30.584372
456.516955	27964.606144	30.589389
456.983002	28008.537771	30.594407
457.562441	28051.396176	30.599424
457.694699	28091.796427	30.604442
458.219754	28141.300287	30.609460
459.088296	28195.977721	30.614477
459.342709	28243.526864	30.619495
459.651771	28290.770482	30.624512
460.335023	28329.416216	30.629530
461.003884	28373.677146	30.634548
461.352350	28426.224376	30.639565
461.920065	28478.396074	30.644583
461.920121	28518.874763	30.649600
462.369949	28560.085831	30.654618
462.920572	28615.123904	30.659636
463.532221	28661.398134	30.664653
463.825351	28713.057200	30.669671
464.330021	28769.038377	30.674688
465.490363	28795.025314	30.679706
465.770703	28843.519927	30.684724
466.446302	28885.928873	30.689741
467.005729	28936.257316	30.694759
467.153012	28979.665746	30.699776
467.880026	29011.947004	30.704794
467.806736	29061.369818	30.709812
468.233838	29103.862383	30.714829
468.755114	29160.126471	30.719847
469.443393	29193.077790	30.724864
470.256581	29239.271189	30.729882
470.481059	29285.784459	30.734900
471.010372	29323.413201	30.739917
471.315139	29371.993730	30.744935
471.752701	29412.892377	30.749952
472.588352	29447.224310	30.754970
472.604555	29507.335850	30.759988
473.244274	29553.753081	30.765005
473.499217	29604.573333	30.770023
473.710572	29655.457427	30.775040
474.559531	29703.529981	30.780058
474.952286	29756.383414	30.785076
475.643824	29798.311332	30.790093
476.656872	29840.081518	30.795111
476.847894	29887.435791	30.800128
477.290293	29922.550736	30.805146
477.254636	29974.378248	30.810164
477.877666	30014.294524	30.815181
478.547687	30062.370657	30.820199
478.873954	30113.895300	30.825216
479.504873	30157.356885	30.830234
479.799316	30208.589645	30.835252
480.084885	30252.250913	30.840269
480.553023	30298.987479	30.845287
480.863993	30348.498578	30.850304
481.641140	30383.618769	30.855322
481.985402	30441.222611	30.860340
482.595770	30485.465641	30.865357
483.679557	30517.585917	30.870375
483.662976	30562.161203	30.875392
484.342953	30596.803901	30.880410
484.681552	30635.703919	30.885428
485.206623	30679.752116	30.890445
485.617782	30714.727906	30.895463
485.994433	30765.506661	30.900480
486.242000	30807.512489	30.905498
486.678302	30865.596175	30.910516
487.178873	30914.023228	30.915533
487.710239	30952.362635	30.920551
488.146046	31009.726140	30.925568
488.847590	31061.782271	30.930586
489.099268	31109.736713	30.935604
489.725272	31162.670992	30.940621
490.301485	31216.049400	30.945639
490.294400	31267.812451	30.950656
490.822748	31317.355032	30.955674
490.933706	31383.671405	30.960692
491.494200	31441.459092	30.965709
491.593514	31501.449605	30.970727
491.840390	31568.029754	30.975744
492.596898	31629.928026	30.980762
493.192190	31697.958606	30.985780
493.898107	31755.471515	30.990797
494.991852	31823.601446	30.995815
495.141592	31882.744350	31.000832
496.023606	31931.000234	31.005850
496.675811	31995.956758	31.010868
496.733860	32052.219071	31.015885
497.452300	32105.741853	31.020903
498.100955	32169.226461	31.025920
498.615865	32214.790448	31.030938
499.202630	32269.870513	31.035956
499.408661	32323.739634	31.040973
500.441167	32377.068515	31.045991
500.746493	32433.217259	31.051008
501.081014	32483.766563	31.056026
501.624840	32540.188019	31.061044
502.071392	32589.006750	31.066061
503.124174	32647.738529	31.071079
503.267484	32697.869430	31.076096
503.863706	32752.949286	31.081114
504.305573	32809.431692	31.086132
504.733122	32865.796372	31.091149
505.350184	32916.119123	31.096167
505.563066	32979.908364	31.101184
506.110690	33034.339063	31.106202
506.658035	33089.762537	31.111220
507.038005	33142.575994	31.116237
507.372211	33203.223719	31.121255
507.752333	33272.905299	31.126272
508.052972	33331.156181	31.131290
508.969460	33395.999786	31.136308
508.986241	33460.554589	31.141325
509.621030	33518.804233	31.146343
509.702017	33595.728585	31.151360
510.775928	33652.639021	31.156378
511.808669	33719.792063	31.161396
512.272924	33774.459020	31.166413
512.632882	33831.696727	31.171431
512.967557	33889.279962	31.176448
513.746178	33943.183680	31.181466
514.763096	34002.955435	31.186484
514.777124	34057.137261	31.191501
515.496375	34106.605960	31.196519
515.818579	34175.408119	31.201536
516.203948	34217.892365	31.206554
516.707309	34281.937213	31.211572
517.448961	34340.273550	31.216589
517.627230	34384.895998	31.221607
517.892697	34450.856436	31.226624
518.488965	34499.074467	31.231642
518.758493	34565.072561	31.236660
519.304602	34623.901863	31.241677
519.927911	34681.574827	31.246695
520.500149	34752.969950	31.251712
520.832242	34817.036919	31.256730
521.437765	34879.815670	31.261748
521.537072	34942.009999	31.266765
522.427449	35003.410392	31.271783
522.954752	35074.978030	31.276800
523.944357	35137.109364	31.281818
524.700930	35183.691520	31.286836
525.175679	35237.614518	31.291853
525.881809	35285.077354	31.296871
526.197761	35354.832754	31.301888
527.429637	35404.641513	31.306906
528.189312	35446.336138	31.311924
528.886312	35500.490557	31.316941
529.467507	35538.147658	31.321959
529.844569	35582.279912	31.326976
530.737723	35627.045925	31.331994
531.423644	35667.747181	31.337012
531.482547	35718.897502	31.342029
531.950399	35759.177831	31.347047
532.467329	35813.772249	31.352064
532.868764	35853.386592	31.357082
533.105796	35918.312736	31.362100
533.356321	35966.556638	31.367117
534.100952	36028.083991	31.372135
534.652224	36077.969312	31.377152
535.688218	36120.854993	31.382170
536.264344	36170.407835	31.387188
536.618256	36229.530935	31.392205
537.434673	36275.012202	31.397223
537.785749	36322.640457	31.402240
538.112822	36370.626679	31.407258
538.573529	36423.941528	31.412276
539.114040	36476.915203	31.417293
539.559149	36526.230138	31.422311
540.049390	36581.014073	31.427328
540.060712	36646.199094	31.432346
540.986033	36699.707441	31.437364
540.839265	36770.697107	31.442381
541.837058	36832.098600	31.447399
542.443731	36902.591296	31.452416
542.319422	36961.285448	31.457434
543.052295	37023.652197	31.462452
543.106193	37104.140910	31.467469
543.987634	37165.163205	31.472487
544.164782	37238.272627	31.477504
544.264363	37322.700848	31.482522
545.074162	37390.501143	31.487540
545.772346	37478.478567	31.492557
546.466273	37548.358982	31.497575
546.752748	37630.779867	31.502592
547.343028	37699.747440	31.507610
547.813172	37776.309753	31.512628
548.454247	37857.891839	31.517645
549.109596	37928.102035	31.522663
550.037529	38008.248556	31.527680
550.507279	38076.167507	31.532698
551.032403	38140.669507	31.537716
551.454176	38204.087553	31.542733
552.224334	38270.094559	31.547751
552.901201	38332.929187	31.552768
553.227144	38401.263759	31.557786
553.945551	38461.739799	31.562804
554.269208	38532.933515	31.567821
555.096022	38596.845776	31.572839
555.652954	38663.013854	31.577856
556.101883	38725.809438	31.582874
556.793265	38787.979106	31.587892
557.383675	38869.206160	31.592909
557.949379	38915.269820	31.597927
558.660225	38978.455145	31.602944
559.141638	39040.696367	31.607962
560.656090	39099.810012	31.612980
560.342593	39164.629806	31.617997
561.349339	39218.213875	31.623015
561.702144	39282.657731	31.628032
562.360229	39357.798589	31.633050
562.800102	39409.543068	31.638068
563.568459	39471.949282	31.643085
564.203392	39535.015311	31.648103
564.617269	39607.849025	31.653120
564.964329	39671.346309	31.658138
565.933907	39721.174556	31.663156
566.314899	39785.507976	31.668173
566.989214	39842.389973	31.673191
567.659614	39914.406657	31.678208
568.127097	39965.484087	31.683226
568.409761	40030.270004	31.688244
568.894288	40103.081661	31.693261
569.649751	40172.005938	31.698279
570.153381	40234.095312	31.703296
570.537504	40314.512611	31.708314
571.191962	40367.345170	31.713332
571.332305	40440.705160	31.718349
571.982613	40506.566978	31.723367
572.421351	40580.810393	31.728384
573.250613	40655.018195	31.733402
573.691536	40717.169358	31.738420
573.848978	40804.852846	31.743437
575.021533	40876.471506	31.748455
575.954797	40948.368211	31.753472
576.151431	41024.655931	31.758490
577.125879	41088.906567	31.763508
577.347474	41153.060265	31.768525
578.529974	41217.285018	31.773543
579.060643	41294.476378	31.778560
579.556058	41359.738881	31.783578
580.327256	41428.626704	31.788596
580.693964	41490.247759	31.793613
581.557645	41560.101839	31.798631
582.141542	41625.319649	31.803648
582.050941	41695.994040	31.808666
582.947835	41762.554685	31.813684
583.378537	41829.738802	31.818701
583.761342	41901.686892	31.823719
584.626203	41973.932885	31.828736
585.047479	42046.235938	31.833754
585.815625	42121.704268	31.838772
586.449136	42181.331082	31.843789
587.048158	42245.530050	31.848807
587.835916	42318.719012	31.853824
588.323500	42382.088289	31.858842
588.904508	42442.394476	31.863860
589.532545	42512.560456	31.868877
590.131236	42577.443542	31.873895
590.509575	42640.748444	31.878912
591.130793	42707.816845	31.883930
591.655043	42782.465425	31.888948
591.765411	42842.384682	31.893965
592.520817	42915.049378	31.898983
593.201530	42976.505226	31.904000
593.600771	43046.114169	31.909018
594.069328	43113.644144	31.914036
594.666811	43182.691153	31.919053
595.261464	43258.690226	31.924071
595.829102	43326.458339	31.929088
596.590076	43409.920955	31.934106
596.987903	43470.777301	31.939124
597.379362	43551.673333	31.944141
597.843480	43633.684186	31.949159
598.765069	43708.982087	31.954176
599.658678	43781.419239	31.959194
599.909793	43868.183033	31.964212
600.526012	43943.599134	31.969229
600.950654	44019.551527	31.974247
601.682767	44100.231739	31.979264
602.273219	44185.109240	31.984282
603.318551	44247.865151	31.989300
604.481858	44309.154221	31.994317
605.077492	44381.538783	31.999335
606.336344	44439.852901	32.004352
606.692898	44514.590488	32.009370
607.236019	44583.795844	32.014388
607.832899	44645.547758	32.019405
608.339386	44709.869551	32.024423
609.177271	44774.032091	32.029440
609.813410	44840.162064	32.034458
610.417238	44895.334896	32.039476
610.754170	44965.098754	32.044493
611.116908	45037.793919	32.049511
611.909829	45106.879535	32.054528
612.662886	45171.524604	32.059546
613.663420	45232.949240	32.064564
614.476284	45287.938483	32.069581
615.200100	45339.367729	32.074599
616.087345	45402.790549	32.079616
615.892316	45458.121506	32.084634
616.974267	45514.359631	32.089652
617.166518	45580.618238	32.094669
617.890505	45656.206682	32.099687
618.295078	45715.265203	32.104704
618.646503	45798.592123	32.109722
619.191364	45866.966143	32.114740
619.442948	45941.256798	32.119757
620.075638	46007.485637	32.124775
620.628435	46090.491103	32.129792
620.518597	46173.847366	32.134810
621.378966	46264.447152	32.139828
621.675840	46351.668858	32.144845
622.298714	46438.403342	32.149863
623.299513	46523.883334	32.154880
623.665941	46617.168257	32.159898
624.249121	46702.562500	32.164916
624.823048	46794.442875	32.169933
625.229407	46876.158308	32.174951
626.015163	46973.010280	32.179968
626.738862	47068.145309	32.184986
627.152445	47168.921763	32.190004
627.750125	47252.398934	32.195021
628.336876	47346.999862	32.200039
629.215957	47423.442963	32.205056
630.320631	47520.721805	32.210074
630.755652	47597.108507	32.215092
631.982510	47676.813045	32.220109
632.733388	47754.574261	32.225127
633.349762	47824.752362	32.230144
634.232232	47894.895332	32.235162
634.882840	47970.920547	32.240180
635.472486	48039.591454	32.245197
635.912045	48104.781152	32.250215
636.505258	48171.908216	32.255232
636.936761	48246.342729	32.260250
637.555622	48320.166093	32.265268
638.116122	48402.906761	32.270285
638.424254	48474.115764	32.275303
639.508106	48557.743011	32.280320
639.765075	48641.512716	32.285338
640.758542	48715.221748	32.290356
641.235721	48791.099703	32.295373
641.847440	48871.075575	32.300391
642.407360	48945.985742	32.305408
643.100340	49042.557349	32.310426
643.851048	49124.619173	32.315444
644.572409	49202.238093	32.320461
645.015326	49285.240783	32.325479
645.833597	49365.344202	32.330496
645.844842	49450.920553	32.335514
646.574013	49536.131710	32.340532
647.549909	49629.592899	32.345549
647.386263	49730.344499	32.350567
648.568085	49823.027636	32.355584
649.179403	49912.447145	32.360602
649.442137	49999.751400	32.365620
649.783103	50101.121571	32.370637
650.552248	50206.930060	32.375655
651.440811	50312.732985	32.380672
652.268678	50412.364221	32.385690
652.757903	50505.449616	32.390708
653.471827	50612.622637	32.395725
653.863609	50706.875664	32.400743
654.696998	50807.083516	32.405760
655.514602	50916.101933	32.410778
655.655279	51004.416156	32.415796
657.015555	51107.997536	32.420813
657.701080	51206.281432	32.425831
658.341640	51305.578850	32.430848
659.441805	51392.902735	32.435866
660.626590	51485.832513	32.440884
661.567196	51571.416686	32.445901
661.876623	51656.872229	32.450919
662.746226	51740.569879	32.455936
662.920334	51826.471183	32.460954
663.959643	51916.571721	32.465972
664.520603	51996.414488	32.470989
664.848006	52092.752349	32.476007
665.639103	52179.703633	32.481024
666.081120	52275.783846	32.486042
666.442819	52363.676286	32.491060
667.229448	52453.135070	32.496077
667.608591	52555.117421	32.501095
668.239175	52658.117583	32.506112
669.007481	52753.737350	32.511130
669.522640	52850.896856	32.516148
670.714025	52942.357005	32.521165
671.729129	53020.385645	32.526183
672.875695	53096.261443	32.531200
674.019566	53185.705045	32.536218
674.526659	53261.649883	32.541236
675.508666	53337.609184	32.546253
676.005849	53427.370133	32.551271
676.759192	53497.132659	32.556288
677.401143	53575.746809	32.561306
678.158726	53636.611831	32.566324
678.733842	53705.846016	32.571341
679.202936	53777.482708	32.576359
679.497695	53848.950747	32.581376
680.101496	53922.686708	32.586394
680.285038	54007.803494	32.591412
681.210301	54083.894324	32.596429
681.250715	54177.741737	32.601447
681.652326	54268.362505	32.606464
682.925607	54346.551283	32.611482
683.459268	54438.582212	32.616500
684.852204	54512.917857	32.621517
685.473043	54599.442784	32.626535
686.531866	54671.394843	32.631552
687.291172	54748.222576	32.636570
687.944587	54824.605168	32.641588
689.051776	54897.809691	32.646605
689.511806	54972.590313	32.651623
690.075821	55052.499921	32.656640
691.251190	55133.294970	32.661658
691.651197	55205.687233	32.666676
692.438941	55275.949570	32.671693
692.631905	55362.873368	32.676711
693.273093	55443.987284	32.681728
694.129495	55519.156879	32.686746
694.886494	55604.100981	32.691764
695.769353	55673.634465	32.696781
696.264266	55767.619494	32.701799
696.870400	55851.410975	32.706816
697.514735	55940.867274	32.711834
697.846703	56020.044365	32.716852
698.806149	56111.299939	32.721869
699.421460	56195.230420	32.726887
700.048890	56285.431121	32.731904
700.566326	56371.345798	32.736922
701.404633	56466.020265	32.741940
702.187324	56552.058600	32.746957
702.951437	56646.903622	32.751975
703.229643	56736.951857	32.756992
704.251304	56824.997983	32.762010
704.918610	56905.087478	32.767028
706.087831	56982.472118	32.772045
706.616959	57082.418832	32.777063
707.386294	57169.436136	32.782080
708.409532	57249.648252	32.787098
708.815231	57338.235752	32.792116
709.867497	57423.140063	32.797133
710.247445	57512.536030	32.802151
711.144193	57595.686824	32.807168
711.856020	57684.752974	32.812186
712.163655	57775.268839	32.817204
713.051449	57862.599211	32.822221
713.344318	57960.738436	32.827239
714.140924	58061.590373	32.832256
714.737499	58154.309290	32.837274
715.073287	58262.867334	32.842292
715.697670	58348.101404	32.847309
716.167999	58466.449743	32.852327
716.999615	58565.627344	32.857344
717.496501	58664.383064	32.862362
718.390867	58767.412600	32.867380
718.986965	58883.888753	32.872397
719.648525	58987.183539	32.877415
720.084981	59093.374956	32.882432
721.055011	59211.395485	32.887450
721.674446	59320.749330	32.892468
722.363784	59419.642543	32.897485
723.145460	59531.959500	32.902503
723.913196	59642.082765	32.907520
724.837549	59739.775813	32.912538
725.319634	59855.717446	32.917556
725.940443	59960.636809	32.922573
726.573781	60067.143432	32.927591
726.993167	60166.259171	32.932608
727.913449	60274.702985	32.937626
728.701946	60382.022214	32.942644
729.630471	60483.021755	32.947661
730.767036	60593.806814	32.952679
730.831834	60705.538793	32.957696
731.950666	60801.097746	32.962714
732.245019	60908.370055	32.967732
733.118660	61016.469967	32.972749
734.173550	61138.525036	32.977767
734.813259	61247.390549	32.982784
735.576929	61356.294101	32.987802
735.845635	61471.042391	32.992820
737.181368	61594.828173	32.997837
737.718983	61702.059504	33.002855
738.651253	61818.870418	33.007872
739.399534	61918.188573	33.012890
740.088130	62041.052427	33.017908
741.431714	62138.885582	33.022925
741.921277	62243.404750	33.027943
742.569528	62349.425122	33.032960
743.636240	62458.691206	33.037978
744.633749	62561.549573	33.042996
745.682362	62655.037651	33.048013
746.397686	62756.295100	33.053031
747.108650	62852.957713	33.058048
747.969131	62953.572845	33.063066
748.631563	63060.929764	33.068084
749.671791	63162.638096	33.073101
750.088215	63263.494941	33.078119
750.969493	63362.943638	33.083136
751.516244	63460.583910	33.088154
751.970969	63563.923907	33.093172
752.825246	63676.995339	33.098189
753.512567	63787.902996	33.103207
753.865077	63915.608405	33.108224
754.963762	64004.041752	33.113242
755.587791	64122.500750	33.118260
756.338265	64235.198442	33.123277
756.654740	64355.048834	33.128295
757.590713	64474.106386	33.133312
758.777171	64572.277562	33.138330
759.703816	64682.936439	33.143348
760.816407	64781.018701	33.148365
761.468347	64887.967231	33.153383
761.971044	64991.691771	33.158400
762.880648	65099.506183	33.163418
763.210855	65209.108515	33.168436
764.490970	65313.016524	33.173453
765.141359	65430.401247	33.178471
765.561169	65540.465815	33.183488
766.492895	65651.780246	33.188506
767.094886	65761.532340	33.193524
767.942088	65877.723369	33.198541
768.650019	65987.504169	33.203559
769.133155	66113.630069	33.208576
769.972551	66224.822179	33.213594
770.588770	66334.511203	33.218612
771.036130	66459.561756	33.223629
771.393061	66578.074065	33.228647
772.082540	66702.005217	33.233664
773.255237	66831.755907	33.238682
773.963745	66962.776600	33.243700
774.863491	67080.971972	33.248717
775.361863	67194.716333	33.253735
776.344845	67316.236492	33.258752
776.875063	67435.498088	33.263770
777.607280	67559.534334	33.268788
778.123257	67669.890607	33.273805
779.249644	67804.655505	33.278823
779.697983	67925.217532	33.283840
781.084315	68049.470298	33.288858
781.844162	68167.281008	33.293876
782.522055	68286.099189	33.298893
783.422354	68408.435266	33.303911
783.967146	68529.972787	33.308928
784.872255	68650.010776	33.313946
785.791816	68775.543196	33.318964
786.733543	68903.605549	33.323981
787.184838	69025.603276	33.328999
787.940076	69150.966954	33.334016
788.765345	69276.408920	33.339034
789.654459	69406.134664	33.344052
790.544228	69528.540999	33.349069
791.261082	69659.346116	33.354087
792.563255	69790.465494	33.359104
793.432599	69900.877255	33.364122
793.979799	70026.689324	33.369140
794.839545	70146.855311	33.374157
795.946710	70260.524143	33.379175
796.552395	70389.317653	33.384192
797.533277	70504.096483	33.389210
798.572615	70624.489838	33.394228
799.438221	70746.734693	33.399245
800.085372	70861.402704	33.404263
800.933323	70981.143760	33.409280
801.454316	71111.271235	33.414298
802.304446	71233.976723	33.419316
803.085745	71344.319699	33.424333
804.067558	71468.056866	33.429351
804.997597	71589.168343	33.434368
806.036819	71708.160835	33.439386
806.670114	71823.506469	33.444404
807.350535	71943.480779	33.449421
808.752926	72060.112877	33.454439
809.457234	72181.769040	33.459456
810.440267	72284.219045	33.464474
810.855893	72409.328506	33.469492
811.760103	72525.850682	33.474509
812.672513	72634.151997	33.479527
813.309353	72762.660908	33.484544
814.304307	72878.283812	33.489562
814.704333	73008.388897	33.494580
815.502258	73123.423087	33.499597
815.951962	73241.020183	33.504615
816.575589	73380.933604	33.509632
817.864961	73501.908883	33.514650
818.393404	73632.718875	33.519668
818.691942	73756.016387	33.524685
820.134267	73878.084054	33.529703
820.940861	74019.682125	33.534720
822.007199	74141.379209	33.539738
822.904569	74268.258589	33.544756
823.682851	74390.407238	33.549773
824.757743	74516.955997	33.554791
825.468166	74648.008443	33.559808
826.343662	74758.477489	33.564826
827.352904	74877.058152	33.569844
828.011527	74997.366269	33.574861
828.771529	75122.155814	33.579879
829.792400	75246.309737	33.584896
830.955715	75356.457489	33.589914
832.100373	75457.070279	33.594932
832.300314	75565.216326	33.599949
833.360843	75662.549593	33.604967
834.249515	75766.953111	33.609984
835.845496	75875.616495	33.615002
836.132871	75982.610458	33.620020
836.332286	76082.360195	33.625037
837.936852	76193.240301	33.630055
838.288740	76318.694632	33.635072
838.598720	76431.222520	33.640090
839.813783	76542.899761	33.645108
839.983846	76668.257495	33.650125
840.558023	76788.574108	33.655143
841.468737	76919.479491	33.660160
842.228914	77044.037148	33.665178
842.892855	77173.601594	33.670196
843.645069	77312.805820	33.675213
844.811614	77451.502494	33.680231
845.234270	77585.515144	33.685248
846.172376	77724.033607	33.690266
846.960394	77858.307080	33.695284
847.820968	77994.102709	33.700301
849.006241	78136.676402	33.705319
849.884634	78278.994844	33.710336
850.365940	78409.252468	33.715354
851.110398	78542.535284	33.720372
852.889984	78679.887968	33.725389
854.082429	78799.584487	33.730407
854.875892	78921.320317	33.735424
855.945699	79040.352970	33.740442
857.157271	79172.146774	33.745460
857.856632	79299.359260	33.750477
858.934558	79417.670135	33.755495
859.743723	79542.446774	33.760512
860.946923	79664.375082	33.765530
861.463895	79780.127505	33.770548
861.851883	79902.716608	33.775565
863.071904	80020.703735	33.780583
863.738682	80149.914273	33.785600
864.839820	80276.916277	33.790618
866.303166	80406.269325	33.795636
866.544084	80534.040663	33.800653
867.801788	80655.419978	33.805671
868.239653	80785.366114	33.810688
868.820488	80919.218042	33.815706
869.493385	81054.728589	33.820724
870.377511	81178.474542	33.825741
871.433103	81308.060301	33.830759
871.897935	81449.889544	33.835776
872.710892	81582.682021	33.840794
873.635524	81714.038599	33.845812
874.397663	81870.216487	33.850829
875.409926	82009.530172	33.855847
875.631016	82158.496391	33.860864
876.569024	82292.374921	33.865882
877.417297	82444.031882	33.870900
877.975259	82599.612242	33.875917
878.668257	82742.299150	33.880935
879.752264	82900.738325	33.885952
880.944992	83052.053169	33.890970
881.825496	83190.468321	33.895988
882.589884	83351.684232	33.901005
884.078793	83489.980228	33.906023
884.770739	83646.863075	33.911040
885.968009	83789.159481	33.916058
886.898812	83931.967142	33.921076
887.713425	84068.040056	33.926093
888.560654	84197.810984	33.931111
889.230471	84333.185573	33.936128
890.391738	84463.250645	33.941146
891.367708	84597.919639	33.946164
892.235739	84734.291447	33.951181
892.839129	84853.307555	33.956199
893.517002	85001.849565	33.961216
894.241582	85152.893979	33.966234
895.025434	85282.172845	33.971252
895.909749	85436.767102	33.976269
896.621017	85572.736570	33.981287
897.726450	85724.243862	33.986304
898.415814	85874.790675	33.991322
899.291877	86014.094430	33.996340
900.461680	86176.251036	34.001357
901.675732	86308.850511	34.006375
902.478461	86465.819997	34.011392
903.256703	86620.589210	34.016410
904.457972	86765.459381	34.021428
904.926165	86924.840736	34.026445
905.420592	87069.607658	34.031463
906.546928	87234.906997	34.036480
907.309258	87388.846374	34.041498
908.441715	87547.518815	34.046516
909.371034	87721.494401	34.051533
910.252076	87874.606678	34.056551
911.467049	88033.028030	34.061568
911.929368	88201.617615	34.066586
913.010649	88353.877287	34.071604
913.776847	88513.474017	34.076621
914.802758	88675.413465	34.081639
915.755275	88841.344634	34.086656
916.981940	89002.265927	34.091674
918.267585	89164.826374	34.096692
918.812275	89319.696980	34.101709
919.701879	89485.464158	34.106727
921.244515	89637.366670	34.111744
922.320611	89796.668276	34.116762
923.201406	89940.945133	34.121780
923.968582	90099.536305	34.126797
925.386326	90233.300111	34.131815
926.545690	90386.140911	34.136832
927.571398	90534.440849	34.141850
928.770219	90667.328350	34.146868
929.384276	90819.040039	34.151885
930.318422	90957.774915	34.156903
931.277888	91116.860966	34.161920
931.600561	91265.452008	34.166938
932.535818	91405.861745	34.171956
933.311323	91560.352859	34.176973
934.595360	91721.203674	34.181991
935.576569	91879.441141	34.187008
936.053413	92044.070265	34.192026
937.153543	92187.322216	34.197044
938.597702	92341.167594	34.202061
939.464146	92479.894670	34.207079
940.484433	92626.279135	34.212096
941.889727	92771.437943	34.217114
942.953263	92914.813106	34.222132
943.562605	93061.859711	34.227149
944.748728	93203.581973	34.232167
945.527282	93350.793589	34.237184
946.354483	93491.926954	34.242202
947.196776	93642.032563	34.247220
947.986336	93790.917669	34.252237
948.634234	93938.760955	34.257255
950.087551	94096.416252	34.262272
950.529358	94241.289212	34.267290
951.497170	94379.172402	34.272308
952.202591	94524.715232	34.277325
953.186417	94667.160356	34.282343
954.132344	94812.704903	34.287360
955.088378	94953.533217	34.292378
956.061912	95101.533862	34.297396
957.088939	95257.005523	34.302413
958.236794	95400.150831	34.307431
958.514702	95547.603364	34.312448
959.278340	95704.550861	34.317466
960.533683	95855.616552	34.322484
960.961890	96010.108252	34.327501
961.590956	96172.910143	34.332519
963.058907	96346.685864	34.337536
963.735103	96509.469439	34.342554
964.582781	96676.511599	34.347572
965.121212	96855.823098	34.352589
966.239236	97035.932216	34.357607
967.368752	97208.130402	34.362624
968.044602	97378.955423	34.367642
969.275223	97567.543251	34.372660
969.979973	97754.160900	34.377677
970.746857	97922.363174	34.382695
971.880258	98111.806114	34.387712
972.750454	98303.598596	34.392730
973.959415	98482.218450	34.397748
975.008544	98665.123834	34.402765
976.159072	98844.895797	34.407783
977.275200	99016.890322	34.412800
978.194915	99207.805722	34.417818
979.321506	99384.719374	34.422836
980.240841	99572.543708	34.427853
981.246713	99755.119761	34.432871
982.803577	99939.867189	34.437888
983.361265	100114.351060	34.442906
984.170528	100303.768898	34.447924
984.890165	100500.757855	34.452941
985.692503	100679.085864	34.457959
986.914703	100866.261720	34.462976
988.017510	101068.911878	34.467994
989.087979	101247.175649	34.473012
990.179014	101442.844323	34.478029
990.869467	101632.415244	34.483047
992.283218	101808.789970	34.488064
993.431418	101999.901487	34.493082
994.423688	102192.623337	34.498100
995.325308	102378.602835	34.503117
995.982988	102570.073380	34.508135
997.367161	102751.034753	34.513152
998.025247	102949.886428	34.518170
998.966613	103142.051224	34.523188
1000.334698	103333.288152	34.528205
1001.194541	103528.865892	34.533223
1002.503521	103714.408714	34.538240
1003.151412	103895.821243	34.543258
1004.748817	104082.931199	34.548276
1005.629792	104274.592116	34.553293
1006.751961	104464.149629	34.558311
1008.023753	104640.231927	34.563328
1008.892683	104812.549020	34.568346
1010.493682	104992.144545	34.573364
1011.276729	105178.310333	34.578381
1012.242741	105360.061328	34.583399
1014.058052	105524.676789	34.588416
1014.567081	105700.719196	34.593434
1015.594245	105869.517265	34.598452
1016.895149	106038.717109	34.603469
1018.353750	106202.415346	34.608487
1019.985749	106344.708656	34.613504
1020.536610	106504.264607	34.618522
1021.194898	106652.113373	34.623540
1022.248410	106807.027178	34.628557
1023.382053	106959.646688	34.633575
1024.430556	107117.288936	34.638592
1025.278467	107280.162272	34.643610
1026.187209	107424.678247	34.648628
1026.882452	107587.323327	34.653645
1027.782471	107763.505316	34.658663
1028.875160	107916.325681	34.663680
1029.889112	108082.879546	34.668698
1030.900820	108250.487064	34.673716
1032.106814	108413.892986	34.678733
1032.366857	108595.200995	34.683751
1033.458337	108764.269478	34.688768
1034.100640	108952.367197	34.693786
1035.296993	109139.402740	34.698804
1036.244300	109310.626857	34.703821
1037.100058	109501.826346	34.708839
1038.231222	109682.838743	34.713856
1039.343445	109871.616011	34.718874
1040.209568	110061.916545	34.723892
1041.817472	110244.619902	34.728909
1042.128904	110434.666888	34.733927
1043.650563	110604.805529	34.738944
1045.445537	110795.662072	34.743962
1046.468659	110981.085887	34.748980
1047.449407	111154.850053	34.753997
1048.097267	111348.729882	34.759015
1049.246936	111532.475429	34.764032
1049.810948	111730.923269	34.769050
1050.754320	111917.924320	34.774068
1052.212054	112114.040358	34.779085
1052.862461	112317.500037	34.784103
1054.059827	112505.352132	34.789120
1054.888996	112702.559002	34.794138
1055.732470	112893.119129	34.799156
1057.259932	113100.098434	34.804173
1058.262799	113311.967740	34.809191
1059.664404	113508.975234	34.814208
1060.896299	113710.943930	34.819226
1061.791557	113909.060160	34.824244
1063.040238	114102.023636	34.829261
1063.808005	114297.282928	34.834279
1065.045910	114485.138903	34.839296
1066.326170	114690.326904	34.844314
1066.927585	114885.551952	34.849332
1068.116811	115079.544520	34.854349
1069.077195	115278.786742	34.859367
1070.770934	115468.998864	34.864384
1071.961289	115667.243242	34.869402
1072.718466	115866.114568	34.874420
1073.712582	116065.102064	34.879437
1074.324353	116269.376112	34.884455
1075.672146	116458.886447	34.889472
1076.719485	116661.673879	34.894490
1077.684609	116864.018665	34.899508
1079.269610	117068.664739	34.904525
1080.258673	117264.919694	34.909543
1081.767328	117441.484911	34.914560
1082.960964	117630.302306	34.919578
1084.134728	117825.732168	34.924596
1085.829475	118010.769254	34.929613
1086.047804	118213.707508	34.934631
1087.384576	118395.301667	34.939648
1088.283645	118586.503847	34.944666
1089.250012	118767.117652	34.949684
1090.201699	118949.548488	34.954701
1090.364970	119151.536327	34.959719
1092.045252	119331.178476	34.964736
1093.458797	119516.469842	34.969754
1094.402161	119711.285825	34.974772
1095.739090	119897.859493	34.979789
1096.833738	120084.636897	34.984807
1097.678128	120270.338111	34.989824
1098.625401	120457.812687	34.994842
1099.290902	120654.706515	34.999860
1100.396482	120862.720692	35.004877
1101.045311	121072.304336	35.009895
1102.111652	121266.677578	35.014912
1103.431919	121475.067332	35.019930
1103.902307	121702.264103	35.024948
1104.820747	121907.433551	35.029965
1105.676917	122126.923060	35.034983
1106.591576	122341.825141	35.040000
1107.985162	122573.728285	35.045018
1108.903507	122803.246160	35.050036
1110.212620	123034.048876	35.055053
1111.330057	123255.952089	35.060071
1112.944488	123475.977326	35.065088
1114.273326	123705.283896	35.070106
1115.202871	123937.013901	35.075124
1116.306628	124151.464806	35.080141
1117.396644	124386.952751	35.085159
1118.827704	124608.243463	35.090176
1119.901993	124840.767923	35.095194
1121.014664	125061.996783	35.100212
1122.196513	125281.389160	35.105229
1123.774987	125511.516897	35.110247
1124.788380	125729.390297	35.115264
1126.498078	125949.033480	35.120282
1127.334925	126175.525794	35.125300
1129.094006	126384.303696	35.130317
1130.115806	126602.649829	35.135335
1131.256581	126817.755999	35.140352
1132.735919	127024.538334	35.145370
1133.318361	127248.297901	35.150388
1135.122794	127443.574976	35.155405
1136.198291	127662.692203	35.160423
1137.486043	127878.922710	35.165440
1138.547282	128092.132142	35.170458
1139.433659	128300.218939	35.175476
1140.620254	128506.064831	35.180493
1142.104793	128718.107361	35.185511
1142.903027	128932.402607	35.190528
1144.059675	129143.064903	35.195546
1144.714951	129371.544203	35.200564
1146.072321	129580.451714	35.205581
1147.072039	129807.420335	35.210599
1147.670284	130025.520703	35.215616
1148.708841	130249.338982	35.220634
1149.831362	130487.419369	35.225652
1150.974606	130713.355276	35.230669
1152.556319	130946.570198	35.235687
1153.524837	131167.105281	35.240704
1154.879377	131406.359804	35.245722
1155.455908	131632.630312	35.250740
1156.612651	131862.655773	35.255757
1157.882545	132105.860824	35.260775
1158.777460	132335.409533	35.265792
1159.995115	132574.590386	35.270810
1161.208838	132812.174373	35.275828
1162.549821	133044.638811	35.280845
1163.523461	133286.056893	35.285863
1164.661335	133513.441970	35.290880
1166.216330	133740.039636	35.295898
1166.856922	133965.766480	35.300916
1168.431753	134182.021686	35.305933
1169.555319	134412.674702	35.310951
1170.747208	134639.790589	35.315968
1171.519966	134857.506992	35.320986
1172.796462	135086.007713	35.326004
1174.147590	135309.993146	35.331021
1175.134774	135542.119892	35.336039
1176.241841	135763.645937	35.341056
1177.574155	136001.190210	35.346074
1178.611659	136246.002325	35.351092
1179.910974	136466.016984	35.356109
1181.010711	136700.543060	35.361127
1182.315575	136940.507572	35.366144
1183.509462	137165.529219	35.371162
1184.791875	137411.667024	35.376180
1186.268766	137646.214998	35.381197
1187.364078	137885.366974	35.386215
1188.564390	138133.792994	35.391232
1189.782757	138361.633831	35.396250
1191.004647	138599.678278	35.401268
1192.553089	138827.786964	35.406285
1194.016821	139053.892227	35.411303
1195.819252	139280.681602	35.416320
1197.528502	139484.935439	35.421338
1198.974087	139698.736737	35.426356
1200.589084	139910.190073	35.431373
1201.683867	140115.253489	35.436391
1202.997869	140330.791472	35.441408
1204.559969	140535.669314	35.446426
1205.308365	140742.972471	35.451444
1206.298011	140950.289516	35.456461
1207.356134	141174.031641	35.461479
1207.982403	141389.098228	35.466496
1209.175720	141598.810165	35.471514
1210.043988	141838.258657	35.476532
1211.051921	142060.324780	35.481549
1212.468559	142299.499315	35.486567
1213.825216	142524.241587	35.491584
1214.897672	142746.986049	35.496602
1215.833986	142987.406732	35.501620
1217.166194	143224.479486	35.506637
1218.071592	143465.148462	35.511655
1218.989994	143708.253373	35.516672
1220.723175	143944.797191	35.521690
1221.518774	144184.078032	35.526708
1222.768543	144425.839982	35.531725
1224.085615	144667.440252	35.536743
1224.963351	144914.821856	35.541760
1226.421754	145153.419698	35.546778
1227.511560	145406.685003	35.551796
1229.027831	145644.628787	35.556813
1230.765779	145885.191657	35.561831
1232.055346	146122.893922	35.566848
1233.700618	146358.853516	35.571866
1234.896174	146593.742270	35.576884
1236.056746	146820.628611	35.581901
1237.538921	147054.954193	35.586919
1238.803966	147293.541454	35.591936
1240.193169	147516.511100	35.596954
1241.034881	147755.534822	35.601972
1242.393402	147980.008978	35.606989
1243.608644	148212.274522	35.612007
1244.470177	148449.178583	35.617024
1245.862338	148680.974236	35.622042
1247.040561	148920.534416	35.627060
1248.629930	149141.892956	35.632077
1250.037642	149365.489445	35.637095
1251.333225	149586.273848	35.642112
1252.533527	149791.664535	35.647130
1253.613100	150013.157239	35.652148
1254.626767	150228.149505	35.657165
1255.581108	150450.196715	35.662183
1256.344168	150687.240289	35.667200
1257.872431	150910.748125	35.672218
1259.016709	151152.862193	35.677236
1259.790119	151391.214619	35.682253
1261.232416	151635.886338	35.687271
1261.818758	151880.375787	35.692288
1263.100696	152136.816467	35.697306
1264.428005	152373.639321	35.702324
1265.518487	152645.433709	35.707341
1266.557998	152910.585784	35.712359
1267.476217	153168.814492	35.717376
1268.544129	153423.301598	35.722394
1270.016076	153702.340422	35.727412
1271.094154	153977.900603	35.732429
1271.911176	154251.966976	35.737447
1273.419273	154538.062197	35.742464
1274.548026	154813.593064	35.747482
1275.912025	155107.368343	35.752500
1277.165832	155381.498643	35.757517
1278.768870	155676.915044	35.762535
1280.079244	155955.177590	35.767552
1281.238856	156241.056447	35.772570
1282.368489	156533.898077	35.777588
1283.975068	156824.914613	35.782605
1285.202020	157111.929652	35.787623
1286.654515	157409.041282	35.792640
1288.197371	157691.820333	35.797658
1289.844896	157979.065662	35.802676
1291.131700	158258.954899	35.807693
1293.071495	158524.613533	35.812711
1294.990315	158792.612520	35.817728
1297.106658	159060.848358	35.822746
1298.369534	159320.598864	35.827764
1299.712371	159557.080086	35.832781
1301.382755	159811.754204	35.837799
1302.359873	160077.570222	35.842816
1303.624997	160329.453416	35.847834
1304.748183	160597.559352	35.852852
1306.325071	160859.146044	35.857869
1307.337211	161105.409701	35.862887
1308.449401	161383.055115	35.867904
1309.367407	161654.676257	35.872922
1310.659675	161925.224298	35.877940
1311.770248	162197.528555	35.882957
1313.293832	162457.657405	35.887975
1314.626265	162736.302546	35.892992
1316.258302	162992.950559	35.898010
1317.143027	163265.269243	35.903028
1318.265375	163537.818476	35.908045
1319.857802	163812.974143	35.913063
1320.906270	164086.324360	35.918080
1322.371831	164357.477433	35.923098
1323.654173	164639.452167	35.928116
1324.800446	164910.365437	35.933133
1326.511829	165188.275945	35.938151
1327.228876	165474.468989	35.943168
1328.565188	165748.161777	35.948186
1330.132029	166041.054910	35.953204
1331.375937	166329.746461	35.958221
1332.673468	166598.725547	35.963239
1334.002243	166882.403614	35.968256
1335.112489	167158.257722	35.973274
1336.501473	167438.817902	35.978292
1337.256834	167722.195517	35.983309
1338.773376	167986.942964	35.988327
1339.975824	168263.409099	35.993344
1341.417597	168545.387448	35.998362
1342.646114	168813.293813	36.003380
1344.032408	169098.063671	36.008397
1345.062829	169378.065418	36.013415
1346.270847	169665.036618	36.018432
1347.832273	169950.975929	36.023450
1349.050516	170232.195869	36.028468
1350.480931	170521.954399	36.033485
1352.254356	170808.651072	36.038503
1353.637677	171097.365318	36.043520
1355.076953	171380.688158	36.048538
1356.824422	171670.668140	36.053556
1357.936289	171956.088687	36.058573
1359.430478	172234.860359	36.063591
1360.843845	172528.273468	36.068608
1362.421614	172810.678385	36.073626
1363.357228	173099.000443	36.078644
1364.062704	173404.362026	36.083661
1365.771142	173691.955795	36.088679
1366.920422	173996.666096	36.093696
1368.305636	174291.321906	36.098714
1370.127286	174595.332441	36.103732
1370.793308	174901.620200	36.108749
1372.583856	175200.190394	36.113767
1374.135244	175516.170252	36.118784
1375.516672	175817.219395	36.123802
1377.082400	176120.094740	36.128820
1378.041154	176423.104292	36.133837
1379.366916	176741.117780	36.138855
1380.592897	177051.732203	36.143872
1382.294505	177357.193926	36.148890
1383.407945	177675.599715	36.153908
1384.973273	177988.907319	36.158925
1386.314243	178288.257303	36.163943
1387.718464	178609.897265	36.168960
1388.978489	178934.049927	36.173978
1390.633002	179242.878131	36.178996
1392.191852	179570.999161	36.184013
1394.068841	179882.563100	36.189031
1395.370775	180198.891321	36.194048
1396.586454	180509.214853	36.199066
1398.189423	180817.345392	36.204084
1399.596230	181130.993645	36.209101
1401.314216	181437.711364	36.214119
1402.563983	181747.220988	36.219136
1404.009352	182057.564559	36.224154
1405.336970	182376.588425	36.229172
1406.711906	182686.818088	36.234189
1408.284566	182982.007271	36.239207
1409.639414	183301.842707	36.244224
1410.950452	183627.807138	36.249242
1412.577172	183932.693049	36.254260
1414.006570	184251.859547	36.259277
1415.521016	184545.005242	36.264295
1416.838263	184871.582365	36.269312
1417.976556	185176.980307	36.274330
1419.717397	185493.130298	36.279348
1421.362804	185806.095896	36.284365
1423.267273	186115.948572	36.289383
1424.244580	186414.314366	36.294400
1425.470812	186723.360621	36.299418
1427.407782	187027.394420	36.304436
1428.571198	187336.604687	36.309453
1430.378616	187617.292790	36.314471
1431.605485	187975.617954	36.319488
1433.174304	188272.905742	36.324506
1434.725890	188553.788691	36.329524
1435.701493	188839.309097	36.334541
1437.242061	189124.589401	36.339559
1438.224026	189425.883719	36.344576
1439.423488	189726.128784	36.349594
1441.183698	190016.914180	36.354612
1442.326983	190322.579838	36.359629
1443.683488	190620.669016	36.364647
1444.877935	190926.709245	36.369664
1446.130118	191239.802561	36.374682
1447.753476	191552.940200	36.379700
1448.611938	191865.842761	36.384717
1450.150851	192182.703728	36.389735
1451.336248	192508.231697	36.394752
1452.624831	192844.387309	36.399770
1454.797933	193160.338673	36.404788
1455.970840	193483.305627	36.409805
1457.947236	193807.951105	36.414823
1459.529183	194125.191216	36.419840
1461.209709	194448.919357	36.424858
1462.655792	194774.793284	36.429876
1464.095797	195099.475095	36.434893
1465.547266	195409.016704	36.439911
1466.964413	195739.342712	36.444928
1468.648218	196069.170547	36.449946
1470.255097	196379.452046	36.454964
1471.491006	196715.117639	36.459981
1473.269055	197036.017033	36.464999
1474.450802	197365.291414	36.470016
1475.617645	197698.937965	36.475034
1478.158054	198008.670418	36.480052
1479.449176	198333.687736	36.485069
1481.395885	198653.522763	36.490087
1482.447358	198978.985395	36.495104
1483.742621	199311.751728	36.500122
1486.078070	199629.521163	36.505140
1487.265414	199955.980631	36.510157
1488.672678	200274.938107	36.515175
1490.105638	200598.616993	36.520192
1491.439226	200922.591489	36.525210
1493.097671	201240.622433	36.530228
1494.643083	201574.624335	36.535245
1496.067694	201892.235846	36.540263
1497.906064	202228.047529	36.545280
1498.945073	202559.234693	36.550298
1500.683938	202883.124014	36.555316
1501.506121	203222.983189	36.560333
1503.118838	203554.996859	36.565351
1504.280565	203905.320818	36.570368
1505.697583	204235.689733	36.575386
1507.200204	204579.991926	36.580404
1508.831820	204916.602883	36.585421
1510.589903	205260.078783	36.590439
1512.416913	205599.073564	36.595456
1513.987454	205923.299133	36.600474
1515.948668	206246.397130	36.605492
1517.326394	206581.754975	36.610509
1518.994696	206920.700491	36.615527
1520.306925	207256.349046	36.620544
1521.750355	207573.001435	36.625562
1522.990344	207902.997350	36.630580
1524.418831	208255.623869	36.635597
1526.032075	208593.488119	36.640615
1527.355136	208923.980499	36.645632
1528.897535	209273.262828	36.650650
1530.235001	209603.906264	36.655668
1531.348339	209945.661061	36.660685
1532.707888	210272.745408	36.665703
1534.185056	210603.266604	36.670720
1536.267125	210931.534226	36.675738
1538.134228	211258.641907	36.680756
1539.652061	211598.125321	36.685773
1541.288389	211926.794071	36.690791
1542.601567	212251.398374	36.695808
1544.070062	212576.994847	36.700826
1545.787945	212902.323985	36.705844
1547.511072	213238.347555	36.710861
1549.137798	213571.693757	36.715879
1550.360607	213901.928032	36.720896
1552.078270	214235.590874	36.725914
1553.442538	214572.129140	36.730932
1554.851587	214928.323200	36.735949
1556.609235	215261.091547	36.740967
1557.942876	215607.593769	36.745984
1559.288971	215947.336909	36.751002
1561.316101	216298.456261	36.756020
1562.677395	216639.366126	36.761037
1564.298890	216982.598072	36.766055
1565.865813	217350.836229	36.771072
1567.126953	217708.681499	36.776090
1568.871427	218058.982605	36.781108
1570.035981	218423.575493	36.786125
1571.830127	218777.324194	36.791143
1573.641877	219130.435240	36.796160
1574.858051	219496.748139	36.801178
1576.344829	219861.443829	36.806196
1577.831655	220239.019520	36.811213
1579.482643	220607.297226	36.816231
1580.899246	220976.881971	36.821248
1582.382110	221367.211590	36.826266
1584.229815	221722.020202	36.831284
1585.580427	222109.271489	36.836301
1587.309208	222501.696942	36.841319
1589.011308	222872.838066	36.846336
1590.525035	223265.907063	36.851354
1591.668513	223629.793986	36.856372
1593.395362	224026.208504	36.861389
1594.819801	224407.554967	36.866407
1596.566822	224802.543778	36.871424
1598.236720	225191.219058	36.876442
1600.163307	225578.126691	36.881460
1601.939184	225967.318862	36.886477
1603.444408	226358.204631	36.891495
1605.096660	226735.679397	36.896512
1606.781944	227129.153512	36.901530
1608.629221	227512.110321	36.906548
1610.509942	227898.592980	36.911565
1612.279540	228281.129901	36.916583
1614.319389	228649.499767	36.921600
1615.876956	229034.787879	36.926618
1618.016209	229402.608460	36.931636
1620.320065	229756.024465	36.936653
1621.469859	230126.692443	36.941671
1623.308305	230479.698316	36.946688
1624.987320	230850.232331	36.951706
1626.516742	231220.764165	36.956724
1627.971895	231588.741622	36.961741
1629.328925	231955.667260	36.966759
1630.791355	232326.412175	36.971776
1632.402890	232686.540085	36.976794
1633.899119	233048.032212	36.981812
1635.429512	233430.603963	36.986829
1636.847237	233799.754411	36.991847
1638.399313	234178.740239	36.996864
1639.883492	234540.258552	37.001882
1641.741328	234900.219267	37.006900
1643.346846	235260.066741	37.011917
1644.689003	235622.444681	37.016935
1646.278572	235984.021457	37.021952
1647.552240	236346.968321	37.026970
1649.101470	236709.820894	37.031988
1650.368009	237082.319920	37.037005
1651.802693	237471.787254	37.042023
1653.296759	237856.519773	37.047040
1655.018105	238253.105134	37.052058
1656.698491	238642.685031	37.057076
1658.128416	239040.051694	37.062093
1659.414119	239432.664544	37.067111
1661.199498	239846.410522	37.072128
1662.529532	240257.077128	37.077146
1663.969113	240672.374785	37.082164
1665.328413	241087.608145	37.087181
1667.265734	241512.429023	37.092199
1668.725480	241936.282389	37.097216
1670.685299	242366.280541	37.102234
1672.229833	242786.892944	37.107252
1673.801007	243213.419338	37.112269
1675.716958	243645.327226	37.117287
1677.210790	244081.059977	37.122304
1679.130579	244514.438928	37.127322
1681.509584	244929.505858	37.132340
1683.660534	245361.068684	37.137357
1685.414772	245793.556370	37.142375
1687.402190	246212.365364	37.147392
1688.940466	246639.321793	37.152410
1690.952458	247055.711858	37.157428
1692.830795	247477.710475	37.162445
1694.319499	247902.410957	37.167463
1696.819550	248313.793710	37.172480
1698.089267	248729.051390	37.177498
1699.875622	249141.661596	37.182516
1701.785162	249551.558891	37.187533
1703.295866	249985.116233	37.192551
1705.182931	250399.866776	37.197568
1706.945695	250825.685605	37.202586
1709.072049	251230.616771	37.207604
1710.508591	251644.596320	37.212621
1712.512251	252052.668989	37.217639
1714.437613	252455.393041	37.222656
1716.033881	252864.060712	37.227674
1717.957227	253273.488922	37.232692
1720.288851	253669.465459	37.237709
1721.533243	254089.945689	37.242727
1723.621493	254482.452649	37.247744
1725.031657	254890.686456	37.252762
1726.509576	255302.972655	37.257780
1728.071895	255711.510420	37.262797
1729.466055	256135.847354	37.267815
1731.292676	256546.347886	37.272832
1732.583476	256964.043248	37.277850
1734.487232	257385.807078	37.282868
1735.902264	257812.141929	37.287885
1737.210632	258250.074744	37.292903
1739.418007	258674.301398	37.297920
1741.109227	259099.623373	37.302938
1742.681775	259536.799022	37.307956
1744.222858	259964.783068	37.312973
1745.653536	260395.856265	37.317991
1747.518398	260836.511976	37.323008
1749.469469	261273.291697	37.328026
1750.948010	261721.497461	37.333044
1752.948684	262150.747632	37.338061
1754.190946	262587.658548	37.343079
1755.962323	263002.895213	37.348096
1757.878425	263419.072819	37.353114
1759.547829	263844.761410	37.358132
1761.615339	264257.203724	37.363149
1763.601432	264669.631755	37.368167
1765.738297	265083.025117	37.373184
1767.499812	265510.013244	37.378202
1769.052765	265934.593912	37.383220
1770.708150	266356.997854	37.388237
1772.254478	266787.976437	37.393255
1774.066590	267218.911541	37.398272
1775.837196	267646.905004	37.403290
1777.356569	268087.812862	37.408308
1779.381526	268520.969289	37.413325
1780.761599	268958.796308	37.418343
1782.584721	269408.082652	37.423360
1784.162088	269858.878348	37.428378
1785.297295	270304.686858	37.433396
1787.284791	270765.852373	37.438413
1788.998568	271236.912588	37.443431
1790.480102	271702.317632	37.448448
1792.319223	272168.654750	37.453466
1793.672447	272645.275041	37.458484
1795.445178	273119.134972	37.463501
1797.410762	273610.536694	37.468519
1799.056622	274086.696790	37.473536
1800.604715	274578.208976	37.478554
1802.318491	275076.777906	37.483572
1804.556459	275570.715854	37.488589
1806.434761	276063.157916	37.493607
1808.542713	276558.786305	37.498624
1810.596671	277045.328377	37.503642
1812.454480	277544.316584	37.508660
1814.273248	278027.207009	37.513677
1816.317009	278514.401805	37.518695
1818.208774	279003.521921	37.523712
1820.415110	279487.231330	37.528730
1821.960976	279991.813909	37.533748
1824.228718	280472.104451	37.538765
1825.647867	280973.881385	37.543783
1827.650507	281460.174653	37.548800
1829.603027	281945.177410	37.553818
1831.617163	282437.531496	37.558836
1833.019427	282924.365912	37.563853
1834.960425	283417.410287	37.568871
1837.091924	283914.205004	37.573888
1839.157564	284409.635246	37.578906
1840.919711	284913.412939	37.583924
1842.854453	285410.075315	37.588941
1844.813310	285902.642064	37.593959
1846.391796	286395.188551	37.598976
1848.342408	286886.606698	37.603994
1850.031638	287388.574424	37.609012
1851.978124	287877.522802	37.614029
1853.972667	288359.020221	37.619047
1856.028574	288871.304359	37.624064
1857.667526	289376.717823	37.629082
1859.418791	289865.046875	37.634100
1861.428787	290356.454750	37.639117
1863.394752	290839.131256	37.644135
1865.407573	291333.628666	37.649152
1867.363649	291837.906264	37.654170
1868.794192	292331.496544	37.659188
1871.259949	292823.397442	37.664205
1873.842431	293298.518871	37.669223
1876.433580	293765.891382	37.674240
1878.362957	294236.486657	37.679258
1879.928687	294685.148132	37.684276
1881.564523	295136.740324	37.689293
1883.505635	295589.169862	37.694311
1885.080041	296036.575547	37.699328
1886.900929	296493.459810	37.704346
1888.744406	296956.658531	37.709364
1890.501717	297407.173015	37.714381
1891.766364	297874.085286	37.719399
1893.196162	298347.543193	37.724416
1895.025356	298822.584763	37.729434
1896.212469	299309.299221	37.734452
1898.011454	299795.532838	37.739469
1899.466870	300297.428643	37.744487
1901.457487	300793.092576	37.749504
1904.212668	301293.861866	37.754522
1906.119934	301778.613734	37.759540
1908.221549	302276.429779	37.764557
1909.876735	302778.093421	37.769575
1911.872644	303280.714374	37.774592
1913.450327	303788.269838	37.779610
1915.000419	304313.416229	37.784628
1917.192968	304814.671565	37.789645
1919.030616	305345.550068	37.794663
1920.626718	305874.353968	37.799680
1922.523950	306389.931128	37.804698
1924.276197	306919.181930	37.809716
1926.059992	307453.270356	37.814733
1927.935683	307992.592895	37.819751
1930.109316	308532.015210	37.824768
1932.261922	309065.977689	37.829786
1933.843555	309624.415712	37.834804
1935.962410	310165.427549	37.839821
1938.044413	310714.891056	37.844839
1939.334711	311266.629504	37.849856
1941.396180	311815.296697	37.854874
1943.556131	312375.947063	37.859892
1945.341596	312934.796553	37.864909
1947.207715	313503.651759	37.869927
1948.860405	314068.193451	37.874944
1951.037512	314625.869887	37.879962
1952.508896	315213.140247	37.884980
1955.020098	315782.652933	37.889997
1957.404730	316354.944452	37.895015
1959.095592	316936.346374	37.900032
1961.037806	317510.773278	37.905050
1962.997285	318094.833381	37.910068
1964.968477	318672.818792	37.915085
1967.415855	319245.342199	37.920103
1969.264183	319820.438650	37.925120
1971.535859	320385.894459	37.930138
1973.292454	320971.089489	37.935156
1975.787535	321529.339284	37.940173
1977.930164	322105.196309	37.945191
1979.880883	322673.006365	37.950208
1982.163791	323238.777548	37.955226
1983.884666	323807.394725	37.960244
1986.203422	324366.471581	37.965261
1988.174884	324945.335512	37.970279
1990.501752	325515.990960	37.975296
1992.326679	326074.385907	37.980314
1994.175361	326640.685525	37.985332
1996.174997	327204.492483	37.990349
1998.567624	327771.477538	37.995367
2000.469607	328338.607382	38.000384
2002.251855	328896.487524	38.005402
2004.060407	329463.235245	38.010420
2006.083034	330031.920110	38.015437
2008.072052	330582.640254	38.020455
2010.069075	331131.676933	38.025472
2012.712900	331666.093587	38.030490
2014.068762	332204.331988	38.035508
2016.163544	332745.339143	38.040525
2018.401659	333295.245607	38.045543
2020.044077	333835.496162	38.050560
2022.286195	334368.415497	38.055578
2023.772087	334921.079356	38.060596
2025.388545	335476.149728	38.065613
2027.476224	336039.001469	38.070631
2029.072169	336606.182935	38.075648
2031.450199	337165.217860	38.080666
2033.021978	337750.952578	38.085684
2035.563738	338308.904312	38.090701
2037.814124	338876.759556	38.095719
2040.859325	339428.857508	38.100736
2045.405765	339930.239331	38.105754
2047.949862	340463.098237	38.110772
2050.180612	340978.802407	38.115789
2052.449257	341498.398841	38.120807
2054.214115	342028.566117	38.125824
2056.454033	342530.423884	38.130842
2057.915423	343046.167183	38.135860
2059.779564	343576.092398	38.140877
2061.309116	344102.714257	38.145895
2063.294314	344633.821486	38.150912
2065.305550	345179.979822	38.155930
2066.718578	345721.201889	38.160948
2068.684175	346260.046567	38.165965
2070.866748	346805.999655	38.170983
2072.213961	347367.289156	38.176000
2073.990589	347924.115213	38.181018
2075.785220	348501.671001	38.186036
2077.517449	349074.662298	38.191053
2079.559075	349655.176625	38.196071
2081.355677	350255.749814	38.201088
2083.833538	350836.453780	38.206106
2085.564594	351430.575318	38.211124
2087.527914	352028.959765	38.216141
2090.301732	352608.317802	38.221159
2092.076150	353203.287112	38.226176
2093.645142	353804.007130	38.231194
2095.717302	354415.614520	38.236212
2098.018765	355006.715337	38.241229
2099.641094	355631.603016	38.246247
2101.826931	356254.083105	38.251264
2103.826453	356865.729980	38.256282
2106.043589	357493.250300	38.261300
2107.888245	358122.108895	38.266317
2110.129797	358756.317080	38.271335
2111.977466	359390.497637	38.276352
2114.082410	360024.447241	38.281370
2116.613899	360658.164708	38.286388
2118.442532	361284.678964	38.291405
2121.411066	361918.909692	38.296423
2122.957093	362573.068174	38.301440
2125.193112	363195.372489	38.306458
2127.192007	363842.614231	38.311476
2129.313477	364480.267914	38.316493
2131.538170	365124.531439	38.321511
2133.281143	365772.910862	38.326528
2135.701619	366411.032928	38.331546
2137.791656	367063.282421	38.336564
2139.565229	367715.541235	38.341581
2142.223817	368356.471583	38.346599
2143.959325	369023.479793	38.351616
2146.148542	369666.354409	38.356634
2148.483433	370321.886178	38.361652
2150.218087	370948.307120	38.366669
2152.764624	371567.745861	38.371687
2154.557510	372201.629357	38.376704
2156.790215	372827.955302	38.381722
2159.213443	373450.867534	38.386740
2161.019108	374080.119998	38.391757
2163.721287	374697.766475	38.396775
2165.963200	375338.828844	38.401792
2168.349086	375969.137481	38.406810
2170.386558	376600.043196	38.411828
2173.056361	377223.843464	38.416845
2175.096308	377834.327277	38.421863
2177.405925	378472.796332	38.426880
2179.627084	379102.904806	38.431898
2181.313277	379742.909881	38.436916
2183.604322	380369.329621	38.441933
2186.313560	380997.821869	38.446951
2188.050670	381654.793007	38.451968
2190.194348	382298.969607	38.456986
2193.006241	382934.566501	38.462004
2195.106981	383574.665676	38.467021
2197.489143	384219.314064	38.472039
2199.531653	384872.913619	38.477056
2201.691033	385503.306514	38.482074
2203.510901	386158.807077	38.487092
2205.789712	386808.571812	38.492109
2207.593491	387464.294108	38.497127
2209.964891	388130.823973	38.502144
2212.094419	388784.814713	38.507162
2214.251925	389464.331844	38.512180
2215.927694	390135.448952	38.517197
2218.660357	390806.483685	38.522215
2220.810696	391487.515799	38.527232
2222.271412	392177.396575	38.532250
2224.557828	392863.584266	38.537268
2226.165926	393559.377374	38.542285
2229.115599	394260.206062	38.547303
2231.422540	394966.177691	38.552320
2233.774553	395657.439485	38.557338
2236.092752	396359.216648	38.562356
2238.104865	397059.856541	38.567373
2240.708982	397766.052765	38.572391
2242.694725	398467.566091	38.577408
2244.937155	399170.384960	38.582426
2247.843682	399869.788550	38.587444
2249.659499	400589.892050	38.592461
2252.452702	401283.905277	38.597479
2254.447235	402001.051687	38.602496
2256.836264	402709.914803	38.607514
2259.130299	403410.420042	38.612532
2261.205178	404127.335245	38.617549
2263.531121	404825.666219	38.622567
2265.752425	405542.716035	38.627584
2268.123982	406257.391667	38.632602
2270.952263	406971.112775	38.637620
2273.165396	407675.242485	38.642637
2275.679205	408380.314802	38.647655
2278.242392	409081.157299	38.652672
2280.946631	409767.737940	38.657690
2283.407284	410457.168477	38.662708
2285.826225	411151.238325	38.667725
2288.854486	411830.418084	38.672743
2291.021801	412514.871388	38.677760
2293.279126	413203.083031	38.682778
2295.814295	413885.968219	38.687796
2297.461494	414557.892488	38.692813
2300.000111	415240.076333	38.697831
2302.347699	415923.937390	38.702848
2304.023138	416568.985517	38.707866
2306.600314	417221.914886	38.712884
2308.337130	417893.365460	38.717901
2310.685507	418549.020558	38.722919
2313.048100	419210.974591	38.727936
2315.327597	419864.980779	38.732954
2317.647366	420532.108403	38.737972
2319.736670	421200.868780	38.742989
2322.043522	421855.819163	38.748007
2324.058093	422540.678658	38.753024
2326.082186	423225.614896	38.758042
2328.598964	423906.406111	38.763060
2330.546363	424601.825014	38.768077
2332.969918	425276.770410	38.773095
2335.536531	425964.714588	38.778112
2337.725263	426658.710438	38.783130
2340.268252	427350.705826	38.788148
2342.714641	428050.477335	38.793165
2344.988559	428749.391882	38.798183
2347.164507	429453.604701	38.803200
2349.048736	430154.451469	38.808218
2351.264061	430871.041974	38.813236
2353.820629	431600.441335	38.818253
2356.126865	432304.380087	38.823271
2358.290512	433032.624982	38.828288
2360.442183	433770.143270	38.833306
2362.900784	434512.841100	38.838324
2365.267928	435258.202890	38.843341
2367.357323	435993.018196	38.848359
2369.371182	436745.451826	38.853376
2371.462388	437506.231201	38.858394
2374.095192	438264.116526	38.863412
2376.140758	439033.936315	38.868429
2378.607067	439803.305238	38.873447
2381.503589	440575.859112	38.878464
2383.694500	441343.894448	38.883482
2385.801526	442116.760722	38.888500
2388.039207	442907.556953	38.893517
2390.120840	443694.909121	38.898535
2392.581030	444484.744415	38.903552
2394.823459	445272.307063	38.908570
2397.788564	446073.005364	38.913588
2400.330725	446869.947055	38.918605
2403.055679	447660.361281	38.923623
2405.284729	448453.292959	38.928640
2407.763816	449252.614072	38.933658
2410.776850	450046.362909	38.938676
2413.423666	450837.306387	38.943693
2416.158130	451632.543115	38.948711
2418.761595	452421.908390	38.953728
2421.020789	453210.484620	38.958746
2423.883602	453985.149732	38.963764
2426.263406	454769.396912	38.968781
2429.058471	455545.316290	38.973799
2431.504773	456322.467170	38.978816
2434.003928	457098.918962	38.983834
2436.532823	457868.871151	38.988852
2439.253915	458648.247026	38.993869
2441.275349	459418.562770	38.998887
2443.570061	460196.572636	39.003904
2446.138302	460974.857597	39.008922
2449.183602	461742.738791	39.013940
2451.561832	462508.318176	39.018957
2454.363831	463272.081243	39.023975
2456.585072	464038.675486	39.028992
2458.772686	464810.133730	39.034010
2461.596466	465564.405715	39.039028
2463.957830	466331.983133	39.044045
2466.024570	467069.557688	39.049063
2468.561851	467802.032268	39.054080
2470.685654	468552.243083	39.059098
2473.497691	469278.354922	39.064116
2475.381525	470020.264918	39.069133
2477.692160	470765.655282	39.074151
2480.373251	471511.004170	39.079168
2482.088812	472269.530646	39.084186
2484.683154	473015.025963	39.089204
2486.682668	473799.102765	39.094221
2489.223432	474566.014914	39.099239
2492.086865	475328.756241	39.104256
2494.219558	476122.530511	39.109274
2496.710873	476887.070807	39.114292
2498.615706	477691.641471	39.119309
2501.086436	478477.532908	39.124327
2503.941611	479271.944509	39.129344
2505.940213	480079.151565	39.134362
2509.136747	480872.068277	39.139380
2511.667655	481685.409571	39.144397
2514.391481	482479.125216	39.149415
2516.890969	483296.469478	39.154432
2519.396704	484099.660699	39.159450
2522.497873	484898.131922	39.164468
2525.115116	485717.950092	39.169485
2527.203567	486530.804249	39.174503
2529.943953	487343.966777	39.179520
2532.610825	488161.077273	39.184538
2535.009226	488984.180395	39.189556
2537.654743	489802.515782	39.194573
2540.145855	490632.113532	39.199591
2542.676505	491452.996668	39.204608
2545.195181	492286.628962	39.209626
2548.233439	493112.076091	39.214644
2550.743589	493926.481691	39.219661
2553.583538	494745.222362	39.224679
2556.664120	495568.764345	39.229696
2559.508482	496377.142514	39.234714
2562.431441	497197.647809	39.239732
2564.653361	498018.770757	39.244749
2567.332535	498834.087774	39.249767
2569.552399	499651.646006	39.254784
2571.933245	500472.757296	39.259802
2574.506016	501293.691503	39.264820
2577.499615	502136.607724	39.269837
2579.961865	502959.175845	39.274855
2582.369141	503775.465496	39.279872
2585.158325	504613.487938	39.284890
2588.003919	505436.860468	39.289908
2590.470038	506265.024664	39.294925
2593.085250	507087.583048	39.299943
2595.679927	507920.913221	39.304960
2598.078401	508756.136541	39.309978
2600.780486	509568.375210	39.314996
2603.184241	510400.129807	39.320013
2605.884686	511251.404244	39.325031
2608.647416	512084.964010	39.330048
2610.871368	512921.525243	39.335066
2613.326364	513750.054480	39.340084
2616.450576	514590.950245	39.345101
2619.259457	515442.805362	39.350119
2621.916590	516269.240915	39.355136
2624.228153	517105.434071	39.360154
2626.835580	517935.949579	39.365172
2629.705142	518785.727038	39.370189
2631.891764	519621.131827	39.375207
2635.018836	520456.991415	39.380224
2637.797735	521287.827729	39.385242
2639.744863	522095.423764	39.390260
2642.884295	522900.774598	39.395277
2645.557893	523692.431385	39.400295
2648.440358	524481.445913	39.405312
2650.973371	525281.823620	39.410330
2653.882400	526076.065252	39.415348
2656.554955	526884.915643	39.420365
2658.600088	527694.919770	39.425383
2661.671371	528498.334048	39.430400
2663.678526	529309.751570	39.435418
2666.459607	530118.938479	39.440436
2669.212901	530937.772617	39.445453
2671.484139	531757.835899	39.450471
2674.525399	532577.475854	39.455488
2677.289760	533408.304810	39.460506
2679.713070	534244.004003	39.465524
2682.051191	535083.427769	39.470541
2684.220315	535917.903090	39.475559
2687.285660	536771.460779	39.480576
2689.773463	537623.495567	39.485594
2692.223752	538477.687672	39.490612
2695.070679	539346.315386	39.495629
2697.397276	540221.388711	39.500647
2700.153492	541078.820168	39.505664
2702.290473	541976.333465	39.510682
2704.991162	542855.530591	39.515700
2707.636641	543745.361275	39.520717
2710.160048	544667.506493	39.525735
2712.740738	545562.886416	39.530752
2715.342732	546472.193380	39.535770
2718.241628	547383.593910	39.540788
2721.245393	548296.415199	39.545805
2723.829211	549214.550226	39.550823
2726.914135	550132.889039	39.555840
2729.286673	551069.873128	39.560858
2732.309767	551988.733573	39.565876
2734.939124	552928.191520	39.570893
2737.224461	553865.223986	39.575911
2740.344872	554807.767545	39.580928
2742.751127	555748.945410	39.585946
2745.695891	556695.528396	39.590964
2748.641028	557637.125000	39.595981
2751.311036	558588.762585	39.600999
2754.250643	559529.458535	39.606016
2756.644132	560495.717879	39.611034
2759.162060	561464.233326	39.616052
2762.551636	562433.083787	39.621069
2765.159313	563392.559378	39.626087
2767.654920	564357.333073	39.631104
2770.248343	565343.747526	39.636122
2772.927292	566313.839486	39.641140
2775.844474	567294.078192	39.646157
2778.289445	568282.268684	39.651175
2781.042948	569265.119315	39.656192
2783.615392	570261.781110	39.661210
2786.174650	571240.587964	39.666228
2789.375570	572234.226321	39.671245
2792.112594	573233.906263	39.676263
2795.318595	574227.169269	39.681280
2798.122302	575221.408707	39.686298
2800.798172	576216.831317	39.691316
2803.958618	577212.039948	39.696333
2806.618630	578208.088870	39.701351
2809.371679	579200.632952	39.706368
2812.329881	580204.410392	39.711386
2815.492839	581198.512637	39.716404
2818.770682	582177.605177	39.721421
2821.660117	583146.320788	39.726439
2824.732113	584097.622744	39.731456
2827.402356	585042.605646	39.736474
2830.364947	585981.762253	39.741492
2833.568902	586912.802410	39.746509
2835.751779	587855.968306	39.751527
2838.982783	588780.046614	39.756544
2841.517741	589730.990727	39.761562
2844.030208	590673.109931	39.766580
2847.345017	591606.327283	39.771597
2849.839866	592572.565630	39.776615
2852.751430	593527.661254	39.781632
2855.382269	594490.657569	39.786650
2857.701547	595449.320011	39.791668
2860.433133	596414.373832	39.796685
2863.314147	597384.010421	39.801703
2866.501966	598360.750234	39.806720
2869.628308	599342.351898	39.811738
2872.287216	600314.948502	39.816756
2875.562984	601295.195547	39.821773
2878.511195	602276.998954	39.826791
2881.894726	603257.543604	39.831808
2884.709050	604238.733324	39.836826
2887.604390	605210.984938	39.841844
2890.895439	606186.475937	39.846861
2893.918177	607167.554047	39.851879
2896.934794	608160.112852	39.856896
2899.679313	609144.936176	39.861914
2902.690758	610122.839482	39.866932
2906.240437	611098.071022	39.871949
2908.966835	612088.147981	39.876967
2911.837083	613061.002889	39.881984
2914.983716	614061.092331	39.887002
2917.752501	615051.021446	39.892020
2920.570823	616039.349719	39.897037
2923.273110	617027.698188	39.902055
2926.329781	618031.641936	39.907072
2929.193772	619031.527922	39.912090
2932.026152	620037.347181	39.917108
2934.542775	621043.512144	39.922125
2936.889840	622062.802541	39.927143
2939.616972	623073.310478	39.932160
2941.901254	624117.452898	39.937178
2944.943074	625148.317511	39.942196
2948.161162	626198.067706	39.947213
2950.919800	627264.207335	39.952231
2953.621001	628314.008841	39.957248
2956.882524	629383.321532	39.962266
2959.650426	630442.538471	39.967284
2962.332627	631491.499343	39.972301
2964.961515	632561.951032	39.977319
2967.766041	633636.037000	39.982336
2971.853701	634718.209398	39.987354
2974.489447	635791.780007	39.992372
2977.747683	636869.359650	39.997389
2980.486910	637964.901602	40.002407
2983.408490	639038.506355	40.007424
2986.362204	640120.138068	40.012442
2989.493826	641211.361762	40.017460
2992.285377	642291.375725	40.022477
2995.264592	643386.693728	40.027495
2998.580765	644465.776732	40.032512
3002.126754	645545.493192	40.037530
3004.670606	646634.233748	40.042548
3008.113107	647714.159678	40.047565
3011.126535	648805.997819	40.052583
3014.024424	649878.501198	40.057600
3017.266152	650961.949847	40.062618
3020.180920	652036.580688	40.067636
3023.099558	653090.527246	40.072653
3026.335404	654134.769190	40.077671
3029.155485	655162.474242	40.082688
3032.583729	656202.326407	40.087706
3035.126543	657246.266343	40.092724
3038.374699	658292.455604	40.097741
3041.183791	659321.670935	40.102759
3043.934944	660374.640434	40.107776
3047.527412	661429.437146	40.112794
3050.352134	662481.649088	40.117812
3053.035077	663534.749868	40.122829
3056.214815	664600.143744	40.127847
3059.340871	665659.913146	40.132864
3062.623857	666722.653307	40.137882
3065.188287	667796.530231	40.142900
3068.128093	668866.300596	40.147917
3071.630196	669947.101402	40.152935
3074.227772	671024.588909	40.157952
3077.310221	672121.784202	40.162970
3080.617388	673229.109209	40.167988
3083.721147	674308.287241	40.173005
3086.277739	675421.143489	40.178023
3089.462639	676540.145014	40.183040
3092.449804	677669.230718	40.188058
3094.854879	678788.653050	40.193076
3098.256984	679914.801054	40.198093
3100.829772	681064.488385	40.203111
3103.726574	682203.279003	40.208128
3107.109481	683362.968022	40.213146
3110.027616	684526.329461	40.218164
3113.611452	685690.859608	40.223181
3116.209869	686867.251783	40.228199
3119.468546	688024.384206	40.233216
3122.538237	689186.230528	40.238234
3125.482026	690376.311704	40.243252
3129.023032	691551.446342	40.248269
3132.091039	692756.191645	40.253287
3135.262636	693931.438825	40.258304
3138.648963	695126.494972	40.263322
3141.717004	696326.316672	40.268340
3144.839687	697508.367628	40.273357
3148.219520	698715.937789	40.278375
3151.491991	699921.615962	40.283392
3154.578786	701116.626059	40.288410
3157.170585	702320.668764	40.293428
3160.716104	703528.182164	40.298445
3164.254915	704745.779350	40.303463
3167.343210	705952.207715	40.308480
3171.324204	707154.563696	40.313498
3174.903388	708355.418749	40.318516
3177.802365	709542.140782	40.323533
3181.635144	710745.403671	40.328551
3185.176391	711935.510718	40.333568
3188.771534	713116.357367	40.338586
3191.903591	714301.484899	40.343604
3194.891409	715472.211386	40.348621
3198.667133	716655.401088	40.353639
3202.475796	717818.155010	40.358656
3206.369676	718959.537697	40.363674
3209.224983	720114.557357	40.368692
3212.564121	721256.375604	40.373709
3215.924952	722415.894635	40.378727
3219.676773	723554.646471	40.383744
3223.021457	724690.141389	40.388762
3225.645713	725841.083135	40.393780
3228.877411	726963.311361	40.398797
3231.575496	728112.223262	40.403815
3234.426137	729253.950523	40.408832
3237.653576	730351.077412	40.413850
3240.539557	731473.720907	40.418868
3243.381746	732568.222772	40.423885
3246.725324	733692.084367	40.428903
3249.395355	734813.227064	40.433920
3253.124152	735913.292858	40.438938
3255.743804	737038.727458	40.443956
3259.258297	738156.578511	40.448973
3262.354277	739300.708173	40.453991
3265.158384	740440.775706	40.459008
3267.963957	741571.039402	40.464026
3271.404879	742742.475261	40.469044
3273.245623	743899.390900	40.474061
3277.053744	745085.760572	40.479079
3280.121608	746267.634603	40.484096
3283.580437	747456.026897	40.489114
3286.758288	748644.660050	40.494132
3290.388086	749838.962439	40.499149
3294.048390	751039.487034	40.504167
3297.058708	752257.812349	40.509184
3300.559667	753456.730079	40.514202
3303.264274	754673.415784	40.519220
3306.707544	755881.689910	40.524237
3309.804031	757112.846236	40.529255
3312.842189	758347.521213	40.534272
3316.727512	759586.011733	40.539290
3320.073574	760839.405956	40.544308
3323.521217	762077.965986	40.549325
3326.323843	763327.669384	40.554343
3329.776033	764581.795999	40.559360
3333.332067	765837.491198	40.564378
3336.487345	767103.690210	40.569396
3339.898476	768371.525606	40.574413
3342.981667	769646.223690	40.579431
3345.960175	770929.995000	40.584448
3349.883148	772198.414265	40.589466
3353.045935	773494.683877	40.594484
3356.390452	774788.381143	40.599501
3359.949435	776075.054090	40.604519
3362.967385	777382.530570	40.609536
3366.102506	778677.131212	40.614554
3369.826788	779985.703141	40.619572
3373.268474	781285.322819	40.624589
3376.743415	782599.626512	40.629607
3380.103506	783914.568535	40.634624
3383.395557	785214.082634	40.639642
3386.663232	786537.208950	40.644660
3390.483321	787856.423333	40.649677
3394.464648	789173.203014	40.654695
3397.902757	790485.366629	40.659712
3401.673846	791786.294235	40.664730
3404.832363	793096.614411	40.669748
3408.184983	794405.861849	40.674765
3411.635153	795712.784507	40.679783
3415.136204	797020.946876	40.684800
3418.726862	798329.610712	40.689818
3422.248354	799637.290024	40.694836
3425.535188	800932.373419	40.699853
3429.243981	802235.357162	40.704871
3432.409649	803549.014731	40.709888
3436.151600	804853.115528	40.714906
3439.696300	806164.813356	40.719924
3442.736904	807467.466874	40.724941
3445.969748	808773.713383	40.729959
3449.100045	810084.665600	40.734976
3452.578849	811404.915927	40.739994
3456.229837	812719.224685	40.745012
3459.663859	814009.144254	40.750016
3463.130586	815264.149515	40.755021
3466.746198	816465.411586	40.760026
3469.838851	817613.942271	40.765031
3473.083262	818709.080657	40.770036
3476.327664	819733.551736	40.775040
3479.208437	820696.011622	40.780045
3481.618783	821605.458256	40.785050
3484.691418	822433.521573	40.790055
3487.093951	823221.496842	40.795060
3489.346379	823946.945189	40.800064
3491.897310	824594.742746	40.805069
3493.400842	825219.100225	40.810074
3495.367797	825781.279948	40.815079
3497.165158	826287.523823	40.820084
3498.960682	826751.139868	40.825088
3500.223393	827172.706880	40.830093
3501.638764	827558.251028	40.835098
3503.299099	827878.795924	40.840103
3504.603938	828170.703716	40.845108
3505.579796	828435.140807	40.850112
3507.131838	828665.457001	40.855117
3507.864566	828852.251984	40.860122
3508.900574	828994.673945	40.865127
3509.974090	829139.905225	40.870132
3511.036644	829244.995804	40.875136
3511.966545	829317.255885	40.880141
3512.856769	829362.211779	40.885146
3513.208274	829381.205535	40.890151
3513.563472	829394.561832	40.895156
3514.381673	829378.981291	40.900160
3514.426664	829343.015063	40.905165
3514.881896	829308.442314	40.910170
3515.481754	829238.178457	40.915175
3516.013070	829168.604836	40.920180
3516.256709	829083.330370	40.925184
3516.426806	828976.392134	40.930189
3516.875309	828859.980572	40.935194
3517.155444	828732.318234	40.940199
3517.490911	828605.908157	40.945204
3517.692453	828464.061368	40.950208
3517.841292	828307.833335	40.955213
3517.855382	828135.194434	40.960218
3518.185960	827972.222105	40.965223
3518.469474	827789.713134	40.970228
3518.281240	827621.271409	40.975232
3518.776615	827425.983249	40.980237
3518.448048	827241.803617	40.985242
3518.464014	827027.813955	40.990247
3518.401766	826831.232768	40.995252
3518.008366	826624.585009	41.000256
3518.458871	826426.354929	41.005261
3518.801536	826226.093292	41.010266
3518.312837	826015.064118	41.015271
3518.243526	825792.390052	41.020276
3518.151041	825581.089461	41.025280
3518.212314	825363.922480	41.030285
3517.922662	825144.760305	41.035290
3517.953633	824920.871779	41.040295
3518.136364	824701.230849	41.045300
3518.190362	824490.745068	41.050304
3518.125112	824266.069535	41.055309
3517.482506	824057.720411	41.060314
3517.677509	823815.284210	41.065319
3517.744012	823595.524568	41.070324
3517.218799	823365.732174	41.075328
3517.339376	823148.866574	41.080333
3516.658418	822937.664117	41.085338
3517.044344	822708.580316	41.090343
3516.671862	822499.455027	41.095348
3516.315850	822294.114739	41.100352
3516.395454	822067.390145	41.105357
3516.450710	821858.760041	41.110362
3516.001541	821649.131318	41.115367
3516.511116	821423.678165	41.120372
3515.869348	821211.047937	41.125376
3516.383152	820991.125368	41.130381
3515.986705	820781.848202	41.135386
3515.704956	820571.378089	41.140391
3515.471646	820355.832064	41.145396
3515.373903	820157.680011	41.150400
3515.061561	819948.069447	41.155405
3515.473259	819744.373665	41.160410
3515.343572	819536.667405	41.165415
3515.312679	819344.708816	41.170420
3514.761508	819125.762502	41.175424
3514.926735	818925.388198	41.180429
3514.658508	818730.721810	41.185434
3514.636337	818525.690807	41.190439
3514.471543	818325.251342	41.195444
3514.368731	818129.371878	41.200448
3514.382551	817937.167993	41.205453
3513.554981	817742.071181	41.210458
3513.686071	817550.518598	41.215463
3513.931062	817369.848549	41.220468
3513.359106	817181.121044	41.225472
3513.761394	816999.733998	41.230477
3513.496207	816808.610047	41.235482
3513.374279	816614.244001	41.240487
3513.325245	816438.462322	41.245492
3512.844416	816264.204097	41.250496
3513.140671	816085.047064	41.255501
3512.687738	815905.709800	41.260506
3512.335937	815731.319105	41.265511
3512.170185	815557.284072	41.270516
3512.125102	815380.595303	41.275520
3512.717957	815214.127358	41.280525
3511.775190	815040.491614	41.285530
3512.105357	814868.697790	41.290535
3511.990740	814714.796392	41.295540
3511.296969	814551.142218	41.300544
3511.443721	814378.097115	41.305549
3511.283249	814228.477561	41.310554
3511.388555	814066.634317	41.315559
3510.738586	813919.422178	41.320564
3510.749448	813768.985409	41.325568
3510.698627	813614.267504	41.330573
3510.471262	813474.286506	41.335578
3510.380603	813325.803725	41.340583
3510.591241	813189.353180	41.345588
3510.433264	813038.243173	41.350592
3510.607746	812883.179676	41.355597
3510.464465	812749.016164	41.360602
3510.257579	812596.928685	41.365607
3509.985710	812470.770340	41.370612
3510.259418	812327.956741	41.375616
3510.119804	812182.962978	41.380621
3509.994315	812045.565547	41.385626
3509.743105	811913.935029	41.390631
3509.465913	811780.064142	41.395636
3509.556544	811639.700134	41.400640
3509.747184	811504.775594	41.405645
3509.072695	811375.149334	41.410650
3508.848577	811256.659315	41.415655
3509.097202	811131.659874	41.420660
3508.750026	810996.126188	41.425664
3508.864920	810875.431523	41.430669
3508.798532	810755.347767	41.435674
3508.653684	810642.682602	41.440679
3508.726616	810519.355675	41.445684
3508.520780	810395.777457	41.450688
3508.436133	810275.492446	41.455693
3508.287535	810171.203355	41.460698
3508.392274	810055.953980	41.465703
3508.447125	809942.562660	41.470708
3508.459327	809829.663442	41.475712
3508.721463	809708.240977	41.480717
3508.372787	809605.436260	41.485722
3508.110231	809479.021527	41.490727
3507.764526	809373.775082	41.495732
3507.527849	809255.054421	41.500736
3507.470305	809141.763803	41.505741
3507.580649	809047.653690	41.510746
3507.717277	808950.807850	41.515751
3507.399985	808849.936094	41.520756
3507.517175	808745.630681	41.525760
3507.560945	808641.286271	41.530765
3507.235018	808548.943412	41.535770
3507.470755	808432.230014	41.540775
3507.305143	808330.497384	41.545780
3506.744786	808233.164418	41.550784
3507.158037	808142.601702	41.555789
3506.817637	808052.106746	41.560794
3506.643430	807963.193647	41.565799
3506.776100	807869.891492	41.570804
3506.572652	807781.760615	41.575808
3506.732041	807687.476342	41.580813
3506.284784	807595.626190	41.585818
3506.866629	807510.587234	41.590823
3506.446690	807421.802488	41.595828
3506.157352	807341.091294	41.600832
3506.336259	807252.356863	41.605837
3506.433309	807169.095965	41.610842
3506.200643	807072.084086	41.615847
3506.397167	806991.828953	41.620852
3506.210960	806908.560151	41.625856
3506.378057	806836.452178	41.630861
3505.917904	806759.905761	41.635866
3505.480999	806670.088966	41.640871
3505.887905	806598.330976	41.645876
3505.561409	806520.248845	41.650880
3505.440928	806435.793031	41.655885
3505.104637	806373.805782	41.660890
3504.993508	806301.247496	41.665895
3505.291280	806236.184556	41.670900
3505.299515	806166.191133	41.675904
3505.616109	806101.953061	41.680909
3505.183315	806034.514699	41.685914
3505.367115	805956.101989	41.690919
3505.045399	805893.815122	41.695924
3504.984578	805829.047967	41.700928
3505.045007	805759.578472	41.705933
3504.819801	805712.347259	41.710938
3505.076353	805639.675176	41.715943
3504.949216	805570.281718	41.720948
3504.835562	805510.641470	41.725952
3504.866747	805442.831624	41.730957
3504.733652	805388.851851	41.735962
3504.366904	805330.956829	41.740967
3504.791047	805275.425536	41.745972
3504.700543	805214.071519	41.750976
3504.497326	805152.588181	41.755981
3504.010464	805091.880344	41.760986
3504.256105	805034.033244	41.765991
3504.533245	804977.010032	41.770996
3504.645085	804933.232832	41.776000
3504.893247	804878.213443	41.781005
3504.121427	804819.157463	41.786010
3503.818791	804765.052555	41.791015
3503.869905	804715.087522	41.796020
3503.817524	804669.285152	41.801024
3503.820268	804615.521533	41.806029
3503.873588	804567.262549	41.811034
3504.074294	804512.735305	41.816039
3503.734060	804470.879546	41.821044
3504.074020	804440.333706	41.826048
3503.970376	804381.657107	41.831053
3503.891688	804338.637449	41.836058
3504.089440	804280.400698	41.841063
3504.121567	804239.558588	41.846068
3503.775300	804192.286248	41.851072
3503.763906	804140.570038	41.856077
3503.907662	804107.272203	41.861082
3503.634697	804047.155267	41.866087
3503.996869	804000.161092	41.871092
3503.488704	803954.961561	41.876096
3503.660436	803912.046262	41.881101
3503.649716	803873.843311	41.886106
3503.889165	803828.379637	41.891111
3503.942470	803788.019265	41.896116
3503.525174	803737.680672	41.901120
3503.548722	803689.517304	41.906125
3503.488477	803664.690455	41.911130
3503.488866	803612.138624	41.916135
3503.436955	803575.013813	41.921140
3503.754428	803543.979262	41.926144
3503.837640	803499.757563	41.931149
3503.036063	803459.138387	41.936154
3503.413839	803417.651444	41.941159
3503.544508	803372.933486	41.946164
3503.234029	803331.895154	41.951168
3503.181051	803294.280912	41.956173
3502.474275	803260.770050	41.961178
3502.924067	803216.001110	41.966183
3503.069111	803182.747063	41.971188
3502.888495	803161.743331	41.976192
3503.197194	803122.900385	41.981197
3503.004555	803102.337524	41.986202
3502.746285	803054.799020	41.991207
3502.846454	803029.115044	41.996212
3503.058317	803003.852701	42.001216
3502.995363	802964.334901	42.006221
3502.825908	802937.619112	42.011226
3502.982032	802902.312279	42.016231
3503.007533	802872.100922	42.021236
3502.851304	802849.530737	42.026240
3502.496297	802804.006319	42.031245
3502.609950	802787.201042	42.036250
3502.705368	802757.905438	42.041255
3502.736809	802721.933884	42.046260
3502.234114	802698.148483	42.051264
3502.790780	802668.682766	42.056269
3502.498609	802651.354948	42.061274
3502.572958	802627.479079	42.066279
3502.853666	802594.786404	42.071284
3502.582528	802566.864899	42.076288
3502.599066	802537.092590	42.081293
3502.133155	802507.932396	42.086298
3502.748962	802486.948361	42.091303
3502.369874	802458.115992	42.096308
3502.322491	802438.162737	42.101312
3502.675262	802413.461689	42.106317
3502.693864	802383.932366	42.111322
3502.501633	802345.943892	42.116327
3502.473500	802339.945389	42.121332
3502.709567	802318.727341	42.126336
3502.771464	802292.655962	42.131341
3502.409975	802257.475300	42.136346
3502.426970	802239.902817	42.141351
3502.544776	802213.041491	42.146356
3502.346449	802195.112101	42.151360
3502.249478	802153.691201	42.156365
3502.296679	802138.651628	42.161370
3502.306461	802121.519203	42.166375
3502.336809	802095.598375	42.171380
3502.345470	802079.832592	42.176384
3502.850388	802048.078217	42.181389
3502.580938	802025.522828	42.186394
3502.122099	801995.334248	42.191399
3502.452784	801974.588345	42.196404
3502.402219	801945.263046	42.201408
3502.315622	801922.434673	42.206413
3502.665647	801908.469799	42.211418
3502.493770	801890.096152	42.216423
3502.507250	801860.321181	42.221428
3502.916735	801823.602181	42.226432
3502.696154	801799.476487	42.231437
3502.153068	801788.286633	42.236442
3502.348573	801748.525703	42.241447
3502.174114	801733.568641	42.246452
3502.235775	801714.962747	42.251456
3502.191008	801698.521051	42.256461
3501.910612	801683.873290	42.261466
3502.117192	801663.926738	42.266471
3502.209954	801639.068122	42.271476
3502.159960	801625.213978	42.276480
3502.396166	801587.105226	42.281485
3501.854641	801573.669479	42.286490
3502.083595	801550.936888	42.291495
3502.321387	801539.380475	42.296500
3502.218650	801512.989994	42.301504
3502.398626	801497.293623	42.306509
3502.146725	801479.858718	42.311514
3501.941840	801453.191092	42.316519
3502.179292	801431.823468	42.321524
3502.024345	801422.427130	42.326528
3502.195776	801395.846875	42.331533
3501.984654	801367.666706	42.336538
3501.926806	801357.278856	42.341543
3501.909749	801341.368846	42.346548
3501.591173	801327.897730	42.351552
3501.940185	801310.710114	42.356557
3501.889341	801296.806581	42.361562
3502.180187	801279.676787	42.366567
3501.987120	801257.350820	42.371572
3501.815258	801243.319651	42.376576
3501.889151	801228.224962	42.381581
3502.060653	801211.992278	42.386586
3501.858840	801200.162286	42.391591
3502.185283	801186.150722	42.396596
3501.730855	801170.747980	42.401600
3502.149605	801148.716502	42.406605
3502.112075	801132.662735	42.411610
3502.312820	801115.644218	42.416615
3501.924481	801087.832222	42.421620
3501.840289	801075.056145	42.426624
3502.166963	801065.828068	42.431629
3501.919518	801043.851558	42.436634
3501.929580	801031.402361	42.441639
3501.977366	801016.067184	42.446644
3501.772541	801005.018336	42.451648
3501.601747	800981.858079	42.456653
3501.899335	800968.729221	42.461658
3501.778857	800956.837251	42.466663
3502.031053	800925.214477	42.471668
3501.775831	800924.912720	42.476672
3502.042000	800899.438357	42.481677
3501.575432	800882.962880	42.486682
3501.680174	800875.233691	42.491687
3501.774951	800861.208822	42.496692
3501.780009	800858.767296	42.501696
3501.820004	800831.912364	42.506701
3501.814384	800835.965021	42.511706
3501.955759	800824.910560	42.516711
3501.495513	800795.790506	42.521716
3501.599872	800776.589429	42.526720
3501.529159	800773.573919	42.531725
3501.670946	800762.568103	42.536730
3501.532273	800743.356102	42.541735
3501.839489	800745.065529	42.546740
3501.633897	800720.689356	42.551744
3501.694622	800707.450543	42.556749
3501.262100	800712.058182	42.561754
3501.535236	800697.126369	42.566759
3501.615267	800674.999772	42.571764
3501.386035	800683.041670	42.576768
3501.523242	800668.082222	42.581773
3501.430782	800659.602526	42.586778
3501.589112	800646.982957	42.591783
3501.470575	800646.074010	42.596788
3501.062151	800638.327121	42.601792
3501.481447	800621.321953	42.606797
3501.448686	800611.465969	42.611802
3500.971071	800603.973943	42.616807
3501.444193	800602.581959	42.621812
3501.295271	800593.378736	42.626816
3501.529378	800578.696840	42.631821
3501.334448	800573.210940	42.636826
3501.377670	800567.004355	42.641831
3501.703160	800564.512627	42.646836
3501.559512	800553.502257	42.651840
3501.392096	800539.322400	42.656845
3501.243091	800543.397656	42.661850
3501.709818	800535.562656	42.666855
3501.884035	800512.151502	42.671860
3501.691714	800521.554746	42.676864
3501.685986	800501.344873	42.681869
3501.705116	800476.005091	42.686874
3501.315892	800463.080207	42.691879
3501.569762	800460.453179	42.696884
3501.619786	800434.522580	42.701888
3501.487184	800434.641000	42.706893
3501.352943	800439.788030	42.711898
3501.651015	800417.821741	42.716903
3501.960104	800399.173365	42.721908
3501.538963	800397.628216	42.726912
3501.864232	800377.219754	42.731917
3501.643978	800369.052569	42.736922
3501.520351	800354.719002	42.741927
3501.601428	800332.249327	42.746932
3501.214243	800338.851751	42.751936
3501.620330	800329.903129	42.756941
3501.568029	800316.290624	42.761946
3501.671316	800298.357607	42.766951
3501.661133	800292.305566	42.771956
3501.788869	800286.671341	42.776960
3502.132622	800274.754359	42.781965
3501.559697	800262.053068	42.786970
3501.655024	800251.297744	42.791975
3501.911007	800239.199136	42.796980
3501.538979	800225.978164	42.801985
3501.652998	800199.694871	42.806989
3501.421561	800196.411290	42.811994
3501.668949	800192.759931	42.816999
3501.668396	800181.433629	42.822004
3501.904844	800163.821169	42.827009
3501.823917	800147.137054	42.832013
3501.298341	800128.911302	42.837018
3501.551140	800117.935855	42.842023
3502.083078	800118.682718	42.847028
3501.497658	800101.247384	42.852033
3501.372229	800088.768724	42.857037
3501.364512	800096.142043	42.862042
3501.219419	800081.030077	42.867047
3501.556528	800064.915083	42.872052
3501.574658	800069.550371	42.877057
3501.243612	800052.172783	42.882061
3501.288831	800043.719575	42.887066
3501.063907	800029.157008	42.892071
3501.380170	800025.885365	42.897076
3501.501000	800023.571892	42.902081
3501.505901	800016.199037	42.907085
3501.331154	800010.563033	42.912090
3501.499804	800007.900323	42.917095
3501.385821	799992.636820	42.922100
3501.397153	799996.882644	42.927105
3501.777888	799987.058711	42.932109
3501.736978	799973.394878	42.937114
3501.471483	799963.916042	42.942119
3501.729016	799944.346785	42.947124
3501.711672	799927.261580	42.952129
3501.951745	799926.003533	42.957133
3501.639990	799914.627765	42.962138
3501.861379	799897.407516	42.967143
3501.396271	799890.254459	42.972148
3500.992403	799877.770093	42.977153
3501.130279	799857.975162	42.982157
3501.535202	799857.472507	42.987162
3502.076653	799851.431466	42.992167
3501.865058	799829.445202	42.997172
3501.663338	799829.672083	43.002177
3501.867476	799815.481373	43.007181
3501.505692	799794.885531	43.012186
3501.426219	799789.283264	43.017191
3501.747788	799781.518871	43.022196
3501.229313	799769.198681	43.027201
3501.715981	799751.204213	43.032205
3501.350079	799754.581507	43.037210
3501.485595	799745.625552	43.042215
3501.678346	799720.988025	43.047220
3501.717287	799717.222511	43.052225
3501.818752	799709.053019	43.057229
3501.660054	799695.797607	43.062234
3501.279323	799685.994603	43.067239
3501.863459	799683.755057	43.072244
3501.619670	799657.964914	43.077249
3501.722811	799649.941559	43.082253
3501.710525	799648.967034	43.087258
3501.372404	799625.632754	43.092263
3501.401499	799625.823560	43.097268
3501.276716	799617.298719	43.102273
3501.513257	799601.247116	43.107277
3501.380150	799590.135798	43.112282
3501.328223	799582.771331	43.117287
3501.648888	799576.813376	43.122292
3501.292587	799567.982882	43.127297
3501.491766	799546.224391	43.132301
3501.327477	799544.150620	43.137306
3501.187801	799547.053226	43.142311
3501.630664	799544.982195	43.147316
3501.263243	799534.786273	43.152321
3501.403728	799520.263085	43.157325
3501.589460	799523.651917	43.162330
3501.396163	799507.032538	43.167335
3501.803963	799484.167053	43.172340
3501.528482	799485.919087	43.177345
3501.884762	799476.049377	43.182349
3501.675344	799457.576992	43.187354
3501.680742	799455.330187	43.192359
3501.942353	799445.963494	43.197364
3501.586690	799425.365513	43.202369
3501.769983	799404.780868	43.207373
3501.686031	799394.149796	43.212378
3501.516978	799384.117934	43.217383
3501.353073	799365.540516	43.222388
3501.301582	799367.794664	43.227393
3501.707081	799342.536512	43.232397
3501.540193	799340.414254	43.237402
3501.539254	799337.728954	43.242407
3501.723369	799327.739449	43.247412
3501.234880	799309.652057	43.252417
3501.547542	799299.593587	43.257421
3501.638179	799317.450343	43.262426
3501.784719	799282.076319	43.267431
3501.332883	799279.852101	43.272436
3501.439857	799282.520957	43.277441
3501.220843	799256.139400	43.282445
3501.540890	799245.298445	43.287450
3501.171260	799235.151221	43.292455
3501.366115	799232.532926	43.297460
3501.161352	799235.348188	43.302465
3501.356909	799205.971935	43.307469
3501.349435	799204.117681	43.312474
3501.304668	799198.167676	43.317479
3501.500138	799192.570739	43.322484
3501.182946	799180.706237	43.327489
3501.446242	799176.710023	43.332493
3501.544355	799177.866623	43.337498
3501.487673	799168.646944	43.342503
3501.551983	799159.603651	43.347508
3501.416308	799146.636482	43.352513
3501.210069	799138.416712	43.357517
3501.131291	799136.671243	43.362522
3501.175095	799139.789492	43.367527
3501.389217	799124.863275	43.372532
3501.097245	799108.893069	43.377537
3501.419238	799096.782007	43.382541
3500.950331	799103.349630	43.387546
3501.237514	799103.158303	43.392551
3501.153100	799110.935369	43.397556
3500.639942	799118.584133	43.402561
3500.663818	799117.848019	43.407565
3500.866004	799125.043148	43.412570
3501.249628	799115.559247	43.417575
3501.294324	799102.905596	43.422580
3501.492872	799081.536273	43.427585
3501.498421	799077.238485	43.432589
3501.196326	799096.377977	43.437594
3501.331536	799083.661310	43.442599
3501.385135	799056.699200	43.447604
3501.402707	799070.319901	43.452609
3501.338669	799060.075800	43.457613
3501.378743	799059.288318	43.462618
3501.341797	799035.074719	43.467623
3501.491764	799026.066679	43.472628
3501.096725	799027.398057	43.477633
3500.777473	799023.151006	43.482637
3501.360676	799023.645848	43.487642
3500.914558	799009.115552	43.492647
3501.391262	798993.562026	43.497652
3501.124669	798995.898759	43.502657
3501.661320	798995.082473	43.507661
3501.236042	799006.184552	43.512666
3501.304917	798997.628617	43.517671
3501.557335	798965.556740	43.522676
3501.280512	798969.994775	43.527681
3501.517440	798963.658708	43.532685
3501.359003	798962.120965	43.537690
3501.380877	798947.029069	43.542695
3501.820995	798926.842228	43.547700
3501.516046	798941.197244	43.552705
3501.888601	798920.630303	43.557709
3501.628072	798907.340356	43.562714
3501.328547	798909.975251	43.567719
3501.319350	798880.092389	43.572724
3501.072875	798870.169490	43.577729
3501.421011	798862.595169	43.582733
3501.233957	798864.089390	43.587738
3501.419407	798863.669806	43.592743
3501.349458	798847.761908	43.597748
3501.003965	798830.432110	43.602753
3501.050611	798824.369809	43.607757
3501.315677	798821.203230	43.612762
3501.305898	798827.455203	43.617767
3501.351126	798825.104290	43.622772
3501.379497	798814.503536	43.627777
3501.241822	798795.920378	43.632781
3501.022979	798805.916237	43.637786
3501.277676	798802.507114	43.642791
3501.427028	798805.218374	43.647796
3500.983805	798798.011843	43.652801
3501.473158	798774.642791	43.657805
3501.313630	798772.665688	43.662810
3500.992681	798767.442102	43.667815
3501.500128	798770.829873	43.672820
3500.785241	798772.797278	43.677825
3500.982784	798772.668788	43.682829
3501.124799	798758.583135	43.687834
3501.253039	798737.077169	43.692839
3501.453363	798723.519475	43.697844
3501.519400	798740.746856	43.702849
3501.212153	798733.470164	43.707853
3501.033128	798720.655410	43.712858
3500.576820	798711.644044	43.717863
3501.224706	798708.661728	43.722868
3501.107449	798710.438064	43.727873
3501.095752	798707.412359	43.732877
3501.187794	798717.213261	43.737882
3501.166046	798722.051078	43.742887
3501.109181	798717.567480	43.747892
3500.879275	798723.463308	43.752897
3501.285070	798705.478580	43.757901
3500.819337	798688.216028	43.762906
3501.330668	798682.959933	43.767911
3501.278514	798678.670901	43.772916
3500.716008	798686.230220	43.777921
3501.223164	798689.325087	43.782925
3501.490380	798690.601838	43.787930
3501.442760	798679.866245	43.792935
3501.317384	798657.667178	43.797940
3501.290362	798654.692676	43.802945
3501.529750	798654.801805	43.807949
3501.130693	798651.055307	43.812954
3500.936397	798636.435971	43.817959
3501.162035	798629.075858	43.822964
3500.962347	798623.491370	43.827969
3501.008443	798614.157166	43.832973
3501.277242	798622.758594	43.837978
3500.725759	798622.258864	43.842983
3501.148555	798621.850996	43.847988
3500.941283	798627.938703	43.852993
3500.983608	798620.900233	43.857997
3501.156359	798628.393515	43.863002
3501.139554	798601.489345	43.868007
3501.609362	798585.740590	43.873012
3501.472409	798596.309967	43.878017
3501.361684	798589.393054	43.883021
3501.248307	798566.801135	43.888026
3501.458375	798559.980542	43.893031
3501.399263	798542.507537	43.898036
3500.720211	798557.605548	43.903041
3501.237958	798550.883348	43.908045
3501.064249	798565.902344	43.913050
3501.300492	798552.192177	43.918055
3501.541673	798526.858865	43.923060
3500.812901	798526.875175	43.928065
3500.851779	798528.480653	43.933069
3501.122169	798532.149776	43.938074
3501.299635	798529.338584	43.943079
3501.198807	798527.108062	43.948084
3501.217361	798518.657028	43.953089
3501.133487	798497.378758	43.958093
3501.216693	798496.877468	43.963098
3500.935249	798503.562890	43.968103
3501.121558	798499.675964	43.973108
3500.983114	798514.103563	43.978113
3501.055562	798504.520914	43.983117
3501.019783	798506.821739	43.988122
3501.010477	798508.630089	43.993127
3501.509900	798488.725615	43.998132
3500.771937	798483.518152	44.003137
3501.285738	798481.191534	44.008141
3500.796390	798476.189369	44.013146
3500.954368	798486.126816	44.018151
3501.089829	798479.903807	44.023156
3500.776987	798485.568646	44.028161
3501.215486	798479.981938	44.033165
3501.360472	798489.677241	44.038170
3501.174313	798474.519095	44.043175
3501.097641	798457.195105	44.048180
3501.175613	798452.299573	44.053185
3501.256837	798457.512164	44.058189
3501.352764	798458.669236	44.063194
3501.166845	798444.780665	44.068199
3501.532435	798431.147691	44.073204
3501.174261	798433.059432	44.078209
3501.118539	798428.038278	44.083213
3501.264777	798423.864566	44.088218
3501.128743	798436.094423	44.093223
3501.069989	798411.784229	44.098228
3501.144400	798403.519649	44.103233
3501.309548	798393.873511	44.108237
3501.734692	798405.380854	44.113242
3501.095448	798401.183412	44.118247
3501.340161	798381.025419	44.123252
3501.416050	798374.176772	44.128257
3501.299635	798361.156179	44.133261
3501.245435	798367.952721	44.138266
3501.029348	798364.568129	44.143271
3501.223762	798354.087168	44.148276
3501.392915	798345.172852	44.153281
3501.379310	798329.352540	44.158285
3501.301145	798325.506852	44.163290
3501.257222	798330.983283	44.168295
3500.963230	798326.048132	44.173300
3501.067796	798302.932872	44.178305
3500.938343	798288.888634	44.183309
3501.452603	798296.133575	44.188314
3501.168854	798293.443215	44.193319
3501.748440	798293.303831	44.198324
3500.946629	798288.155023	44.203329
3501.376859	798278.125428	44.208333
3501.451605	798271.814040	44.213338
3501.026870	798280.084822	44.218343
3501.298300	798267.687106	44.223348
3501.184851	798271.465217	44.228353
3501.195143	798255.934001	44.233357
3501.530060	798242.451932	44.238362
3501.172916	798231.812816	44.243367
3501.183706	798229.271729	44.248372
3501.332006	798234.962370	44.253377
3501.406375	798215.416518	44.258381
3501.326481	798204.538674	44.263386
3501.169053	798207.102801	44.268391
3501.382663	798201.941697	44.273396
3501.529792	798200.356002	44.278401
3501.417214	798178.788156	44.283405
3501.142781	798161.836142	44.288410
3501.057111	798158.138037	44.293415
3501.240238	798163.237263	44.298420
3501.234344	798160.845265	44.303425
3501.293028	798157.808300	44.308429
3501.322510	798131.871666	44.313434
3500.736713	798139.679440	44.318439
3500.870869	798139.560849	44.323444
3500.815030	798141.767266	44.328449
3501.011066	798133.287984	44.333453
3501.114991	798140.304229	44.338458
3500.779965	798141.382217	44.343463
3501.003689	798131.726532	44.348468
3501.296789	798134.562115	44.353473
3500.977353	798135.930685	44.358477
3501.070425	798124.439632	44.363482
3501.338119	798119.514190	44.368487
3501.260462	798116.400847	44.373492
3501.128154	798115.933217	44.378497
3501.291866	798116.151861	44.383501
3501.395168	798120.042687	44.388506
3500.964032	798107.021943	44.393511
3501.473261	798089.361196	44.398516
3501.071235	798088.056666	44.403521
3500.945165	798089.101998	44.408525
3501.278936	798085.777814	44.413530
3501.150165	798079.986421	44.418535
3501.157113	798070.266859	44.423540
3501.122939	798054.497926	44.428545
3500.836262	798056.789295	44.433549
3501.280173	798061.359465	44.438554
3500.974310	798054.814342	44.443559
3501.356574	798062.910410	44.448564
3501.218343	798061.173943	44.453569
3501.144210	798065.873929	44.458573
3500.933787	798034.553509	44.463578
3500.901723	798028.551604	44.468583
3501.106597	798029.496375	44.473588
3500.948385	798025.760696	44.478593
3501.152112	798037.742844	44.483597
3501.019836	798034.589161	44.488602
3500.847345	798039.304542	44.493607
3501.230431	798039.635407	44.498612
3501.050608	798034.535674	44.503617
3501.072000	798018.660293	44.508621
3501.178486	798003.943669	44.513626
3501.038955	797998.691096	44.518631
3501.231523	797997.147087	44.523636
3501.252297	798002.613682	44.528641
3501.327012	798007.729978	44.533645
3501.443206	798004.195578	44.538650
3501.133709	797994.427694	44.543655
3501.456447	797985.195851	44.548660
3501.277931	797981.854022	44.553665
3501.096763	797980.319594	44.558669
3501.384937	797972.900126	44.563674
3501.152354	797963.169009	44.568679
3501.357108	797945.995007	44.573684
3501.229912	797950.166156	44.578689
3501.187795	797943.286664	44.583693
3500.948406	797944.545084	44.588698
3501.033287	797944.190004	44.593703
3501.356350	797940.427880	44.598708
3501.050170	797917.033587	44.603713
3501.410551	797916.440086	44.608717
3501.271886	797913.824562	44.613722
3500.954328	797912.311439	44.618727
3500.929107	797917.101563	44.623732
3501.056518	797923.479477	44.628737
3501.342103	797903.753152	44.633741
3501.235211	797890.046388	44.638746
3501.042355	797890.906839	44.643751
3500.921261	797883.746599	44.648756
3500.802703	797890.749055	44.653761
3501.058193	797890.123111	44.658765
3501.088526	797881.718242	44.663770
3501.348791	797884.656745	44.668775
3501.406071	797880.057045	44.673780
3501.421287	797866.917203	44.678785
3501.242629	797853.368095	44.683789
3500.732766	797855.303714	44.688794
3501.217731	797864.311909	44.693799
3501.088357	797857.104096	44.698804
3501.358412	797867.562198	44.703809
3501.150500	797832.968236	44.708813
3501.096143	797826.090532	44.713818
3501.147222	797824.275568	44.718823
3500.942265	797818.740044	44.723828
3501.221613	797832.468946	44.728833
3500.933273	797830.218656	44.733837
3501.136084	797830.919585	44.738842
3500.868461	797828.324185	44.743847
3500.839220	797811.430599	44.748852
3500.850592	797809.475322	44.753857
3500.965753	797801.887349	44.758861
3500.685766	797800.417165	44.763866
3500.657242	797796.075013	44.768871
3501.021636	797802.318323	44.773876
3500.930127	797802.430359	44.778881
3500.950747	797810.827472	44.783885
3500.857727	797804.346500	44.788890
3500.678144	797809.258511	44.793895
3500.841003	797801.565404	44.798900
3500.798012	797812.170209	44.803905
3501.239715	797807.168492	44.808909
3501.192292	797804.782855	44.813914
3501.067914	797817.305090	44.818919
3500.865445	797816.408857	44.823924
3500.815773	797819.395840	44.828929
3501.061534	797824.241349	44.833933
3500.866128	797824.955691	44.838938
3500.937418	797812.441876	44.843943
3500.745613	797793.717781	44.848948
3500.881732	797794.917530	44.853953
3500.861117	797776.508497	44.858957
3501.015568	797788.254615	44.863962
3500.677303	797792.312343	44.868967
3500.929560	797792.907869	44.873972
3500.972777	797788.456820	44.878977
3500.888783	797793.646934	44.883981
3501.047998	797786.247412	44.888986
3501.201643	797790.863152	44.893991
3501.348824	797797.042744	44.898996
3501.066338	797803.191820	44.904001
3500.776765	797799.036994	44.909005
3501.025661	797785.372068	44.914010
3500.639606	797779.229912	44.919015
3501.388232	797766.219413	44.924020
3500.945032	797768.584188	44.929025
3500.917435	797772.007295	44.934029
3500.812250	797773.244769	44.939034
3500.996009	797777.953488	44.944039
3501.290894	797767.602392	44.949044
3500.905092	797774.939784	44.954049
3500.838638	797778.271283	44.959053
3501.444285	797776.711488	44.964058
3500.961720	797769.509950	44.969063
3501.239773	797750.858799	44.974068
3500.920032	797739.724631	44.979073
3500.811148	797743.990728	44.984077
3501.136669	797737.932655	44.989082
3500.896355	797748.910285	44.994087
3501.287978	797744.404742	44.999092
3501.214956	797751.253712	45.004097
3501.487061	797741.003813	45.009101
3501.017508	797727.011520	45.014106
3500.974031	797711.487403	45.019111
3501.292813	797701.425504	45.024116
3500.763310	797709.420348	45.029121
3501.210351	797705.980587	45.034125
3501.224092	797716.772038	45.039130
3500.939742	797711.786067	45.044135
3500.880206	797698.657569	45.049140
3500.719123	797697.168773	45.054145
3500.683860	797688.822748	45.059149
3501.058800	797683.587175	45.064154
3500.654549	797697.227867	45.069159
3500.897193	797687.324366	45.074164
3501.164606	797687.331457	45.079169
3500.972942	797687.556831	45.084173
3500.994468	797684.525453	45.089178
3500.984039	797697.323146	45.094183
3500.791649	797696.376480	45.099188
3501.154416	797702.375943	45.104193
3501.182475	797699.392392	45.109197
3500.875461	797696.900775	45.114202
3500.857646	797692.996437	45.119207
3501.046549	797690.915692	45.124212
3500.903266	797680.925992	45.129217
3500.994550	797674.757957	45.134221
3501.214571	797669.888469	45.139226
3500.902838	797678.581908	45.144231
3501.341693	797667.035990	45.149236
3501.225703	797675.894192	45.154241
3501.067726	797675.186343	45.159245
3501.051956	797678.558810	45.164250
3500.776609	797676.550633	45.169255
3501.193933	797660.856682	45.174260
3501.117910	797646.607337	45.179265
3500.847689	797643.963428	45.184269
3501.057027	797637.728063	45.189274
3500.949166	797640.821905	45.194279
3501.015220	797651.019207	45.199284
3500.807103	797637.816132	45.204289
3500.770462	797644.464167	45.209293
3501.172147	797637.319613	45.214298
3501.041886	797651.992052	45.219303
3501.503273	797642.591529	45.224308
3501.101038	797629.467623	45.229313
3501.119124	797606.216875	45.234317
3501.032746	797612.677357	45.239322
3500.935227	797625.684166	45.244327
3501.145065	797622.818684	45.249332
3500.940575	797615.475822	45.254337
3501.081899	797622.877505	45.259341
3501.131972	797624.823340	45.264346
3501.050596	797614.286616	45.269351
3501.387051	797588.983586	45.274356
3501.603033	797586.947416	45.279361
3501.546310	797592.670674	45.284365
3501.468667	797584.282298	45.289370
3501.414799	797576.427442	45.294375
3501.520156	797566.594059	45.299380
3501.417572	797558.258389	45.304385
3501.241188	797548.029454	45.309389
3501.114192	797532.566806	45.314394
3500.888480	797523.957294	45.319399
3501.276300	797524.433973	45.324404
3500.892519	797530.354935	45.329409
3501.237465	797534.403703	45.334413
3501.973471	797536.144657	45.339418
3501.364053	797514.261536	45.344423
3501.169785	797507.454206	45.349428
3501.089366	797501.996623	45.354433
3501.238761	797506.369025	45.359437
3501.445399	797493.296184	45.364442
3501.178531	797481.323004	45.369447
3501.559139	797464.755177	45.374452
3501.434108	797467.216846	45.379457
3501.085203	797463.706017	45.384461
3501.241942	797456.013457	45.389466
3501.234319	797446.588286	45.394471
3501.127560	797429.119723	45.399476
3501.362035	797431.183315	45.404481
3501.065744	797432.597252	45.409485
3501.126289	797424.089384	45.414490
3500.723180	797428.450524	45.419495
3500.826670	797425.845788	45.424500
3500.976910	797432.025252	45.429505
3500.972550	797428.314018	45.434509
3500.930044	797404.730128	45.439514
3500.793368	797394.641268	45.444519
3500.732217	797394.357829	45.449524
3501.278964	797403.943115	45.454529
3501.029499	797395.630197	45.459533
3501.130471	797390.193007	45.464538
3501.077968	797406.709841	45.469543
3501.250506	797394.521285	45.474548
3501.196533	797398.241764	45.479553
3501.022010	797382.541977	45.484557
3500.893384	797368.593295	45.489562
3501.327771	797373.849237	45.494567
3501.312267	797368.820974	45.499572
3501.309490	797363.693033	45.504577
3501.150047	797365.915909	45.509581
3501.433671	797361.475828	45.514586
3501.011453	797347.231100	45.519591
3500.910085	797338.211163	45.524596
3500.870910	797339.438400	45.529601
3501.203274	797344.173049	45.534605
3500.897546	797341.729934	45.539610
3500.872962	797353.114091	45.544615
3500.998971	797348.307901	45.549620
3501.264433	797342.600746	45.554625
3501.452935	797336.075296	45.559629
3501.052359	797311.765564	45.564634
3500.755190	797306.195172	45.569639
3500.642986	797307.482673	45.574644
3501.154553	797313.117341	45.579649
3500.845480	797308.623348	45.584653
3500.825057	797308.187010	45.589658
3500.984060	797316.074706	45.594663
3500.671421	797309.969467	45.599668
3500.760530	797309.027581	45.604673
3500.443451	797318.796873	45.609677
3500.995936	797316.903386	45.614682
3501.151197	797325.280081	45.619687
3501.187386	797324.395313	45.624692
3501.234687	797318.771083	45.629697
3500.892266	797324.148498	45.634701
3501.324772	797307.816371	45.639706
3501.472795	797307.939812	45.644711
3501.631222	797287.254641	45.649716
3501.126544	797284.940291	45.654721
3501.180666	797280.536031	45.659725
3500.955665	797252.144673	45.664730
3500.950789	797250.338296	45.669735
3501.403921	797248.704537	45.674740
3501.685215	797261.164429	45.679745
3501.225904	797258.159175	45.684749
3501.316327	797247.594999	45.689754
3501.254286	797227.237159	45.694759
3501.348101	797219.505313	45.699764
3500.955457	797216.050028	45.704769
3501.219355	797222.211925	45.709773
3501.208596	797213.812614	45.714778
3501.349398	797217.014315	45.719783
3501.173904	797201.509615	45.724788
3501.158896	797192.866724	45.729793
3500.925871	797193.635856	45.734797
3501.197199	797191.932816	45.739802
3501.097337	797200.007651	45.744807
3501.213243	797204.043588	45.749812
3500.928246	797188.116383	45.754817
3501.105365	797170.260840	45.759821
3501.332536	797110.000879	45.764826
3501.126405	797013.272262	45.769831
3501.394391	796853.896620	45.774836
3500.872159	796646.281657	45.779841
3500.362599	796391.469612	45.784845
3500.231441	796078.357251	45.789850
3499.464246	795732.987663	45.794855
3499.383462	795341.859778	45.799860
3499.290363	794890.562978	45.804865
3498.620806	794394.516448	45.809869
3498.355777	793856.097810	45.814874
3498.009192	793280.602028	45.819879
3497.507295	792639.828576	45.824884
3496.950245	791949.385206	45.829889
3496.272635	791215.084256	45.834893
3495.226010	790423.308524	45.839898
3494.382123	789602.848106	45.844903
3493.839073	788736.706560	45.849908
3493.071129	787817.709133	45.854913
3491.891021	786860.245945	45.859917
3491.274750	785857.347037	45.864922
3490.206793	784805.872254	45.869927
3489.275460	783696.211863	45.874932
3488.291629	782556.073814	45.879937
3487.277306	781362.428000	45.884941
3486.180422	780125.881002	45.889946
3484.899256	778849.707265	45.894951
3483.839755	777513.099233	45.899956
3482.700328	776145.811300	45.904961
3481.165468	774718.910783	45.909965
3480.353048	773268.460811	45.914970
3478.640173	771764.988879	45.919975
3476.889672	770213.573595	45.924980
3475.419429	768634.883262	45.929985
3473.750889	767013.176645	45.934989
3472.315423	765363.276469	45.939994
3471.005074	763672.958173	45.944999
3469.367766	761929.498607	45.950004
3467.184391	760151.605804	45.955009
3465.328998	758338.381853	45.960013
3463.734865	756486.028268	45.965018
3461.574583	754605.360683	45.970023
3460.074874	752679.647762	45.975028
3458.044817	750729.204471	45.980033
3455.795522	748750.619327	45.985037
3454.074052	746714.527046	45.990042
3452.138218	744665.885697	45.995047
3449.692590	742570.713585	46.000052
3447.710734	740452.607838	46.005057
3445.803996	738293.582648	46.010061
3443.998306	736111.685671	46.015066
3441.489092	733888.886698	46.020071
3439.318999	731629.377712	46.025076
3437.259593	729342.585201	46.030081
3435.062192	727020.781182	46.035085
3432.801543	724669.156919	46.040090
3430.197248	722304.122487	46.045095
3427.688781	719886.490116	46.050100
3425.428626	717455.561036	46.055105
3423.091191	714992.304534	46.060109
3420.882993	712498.738296	46.065114
3417.903091	709976.808511	46.070119
3415.813968	707431.426322	46.075124
3412.990214	704858.721864	46.080129
3410.374034	702257.190207	46.085133
3407.808983	699619.060191	46.090138
3405.339906	696980.448441	46.095143
3402.871349	694290.247816	46.100148
3400.329058	691582.521180	46.105153
3397.649694	688848.542031	46.110157
3395.499158	686091.409911	46.115162
3392.258278	683304.862813	46.120167
3389.251517	680487.926394	46.125172
3386.393059	677658.461263	46.130177
3383.233571	674797.016635	46.135181
3380.922971	671919.531851	46.140186
3377.922469	669032.201664	46.145191
3375.025982	666123.068959	46.150196
3372.229144	663186.004033	46.155201
3369.075035	660218.570953	46.160205
3366.629932	657229.088813	46.165210
3363.247566	654242.488810	46.170215
3359.987045	651208.925307	46.175220
3357.052881	648172.655887	46.180225
3353.829462	645113.305016	46.185229
3351.203059	642041.784084	46.190234
3347.994483	638950.496424	46.195239
3344.849425	635825.814564	46.200244
3341.497275	632702.429799	46.205249
3338.352180	629566.862960	46.210253
3335.325223	626404.797478	46.215258
3332.063988	623233.800039	46.220263
3328.753384	620027.266571	46.225268
3325.976664	616813.264181	46.230273
3322.545910	613589.831612	46.235277
3319.603625	610348.440289	46.240282
3315.901550	607091.778916	46.245287
3312.264230	603819.363539	46.250292
3309.267281	600542.961106	46.255297
3305.948086	597245.055243	46.260301
3302.453980	593927.866504	46.265306
3298.654660	590620.664202	46.270311
3295.290929	587284.164105	46.275316
3292.259930	583948.542687	46.280321
3288.769114	580595.131568	46.285325
3285.630946	577238.544524	46.290330
3281.968561	573875.163453	46.295335
3278.333479	570481.870329	46.300340
3274.895146	567081.163906	46.305345
3271.001794	563682.892685	46.310349
3267.779340	560263.786832	46.315354
3264.181480	556855.507536	46.320359
3260.769266	553422.704162	46.325364
3257.227005	549989.246641	46.330369
3253.839775	546545.344843	46.335373
3250.153522	543088.758240	46.340378
3246.672567	539634.654721	46.345383
3243.013396	536158.445490	46.350388
3239.530677	532684.787493	46.355393
3235.719296	529201.939080	46.360397
3232.416898	525712.845955	46.365402
3228.323712	522221.647901	46.370407
3224.946279	518719.047553	46.375412
3221.516916	515214.947329	46.380417
3217.910866	511693.594672	46.385421
3214.142397	508158.768556	46.390426
3210.243583	504646.687540	46.395431
3206.620021	501120.127105	46.400436
3203.024524	497589.171079	46.405441
3199.144026	494040.397413	46.410445
3195.753911	490497.922419	46.415450
3191.992845	486959.472626	46.420455
3188.112631	483396.984339	46.425460
3184.574528	479851.109377	46.430465
3181.051085	476287.502127	46.435469
3177.286885	472713.633948	46.440474
3173.649312	469164.190929	46.445479
3169.586302	465588.306213	46.450484
3165.967396	462006.427552	46.455489
3162.145713	458453.525983	46.460493
3158.069641	454864.506961	46.465498
3154.340411	451287.758361	46.470503
3150.770504	447709.254181	46.475508
3147.103898	444130.766957	46.480513
3142.992060	440557.731688	46.485517
3139.462782	436972.019106	46.490522
3135.397530	433394.480920	46.495527
3131.363445	429821.193330	46.500532
3128.152751	426242.720387	46.505537
3124.091305	422648.839145	46.510541
3120.191186	419077.067351	46.515546
3116.338965	415503.966357	46.520551
3112.845943	411925.187219	46.525556
3108.758429	408340.126976	46.530561
3104.744978	404760.714220	46.535565
3101.244462	401187.249886	46.540570
3096.974031	397612.285359	46.545575
3093.446437	394035.087299	46.550580
3089.873315	390469.852155	46.555585
3085.627894	386906.793563	46.560589
3081.641738	383332.067043	46.565594
3077.722812	379771.382956	46.570599
3074.188898	376195.069485	46.575604
3070.007884	372631.691710	46.580609
3066.084320	369079.397067	46.585613
3061.972258	365528.666711	46.590618
3058.119380	361979.416990	46.595623
3054.094905	358439.783094	46.600628
3050.118824	354897.799310	46.605633
3046.036369	351373.606803	46.610637
3042.336789	347839.664624	46.615642
3038.662442	344319.147622	46.620647
3034.703578	340797.040894	46.625652
3030.508640	337276.729378	46.630657
3026.725372	333774.425187	46.635661
3022.482543	330262.480369	46.640666
3018.405010	326779.316621	46.645671
3014.317501	323282.420013	46.650676
3010.536270	319785.893385	46.655681
3006.287819	316304.727144	46.660685
3002.546238	312821.836603	46.665690
2998.023442	309368.885636	46.670695
2994.575276	305907.071370	46.675700
2990.528434	302451.730508	46.680705
2986.399814	299021.704510	46.685709
2982.468459	295577.333294	46.690714
2978.294612	292161.686634	46.695719
2974.046559	288743.161538	46.700724
2970.080115	285327.159660	46.705729
2965.996925	281936.717488	46.710733
2962.432544	278540.432941	46.715738
2958.175540	275159.306120	46.720743
2953.498045	271788.417127	46.725748
2949.843547	268425.972114	46.730753
2945.593326	265072.285419	46.735757
2941.516093	261725.719067	46.740762
2937.395715	258403.022139	46.745767
2932.887145	255086.153109	46.750772
2928.874786	251771.010219	46.755777
2924.610971	248484.383752	46.760781
2920.754140	245194.957626	46.765786
2916.538598	241920.382252	46.770791
2912.326664	238663.284406	46.775796
2908.684810	235419.382243	46.780801
2904.003968	232188.885190	46.785805
2900.032261	228959.939978	46.790810
2895.855615	225748.412218	46.795815
2891.898632	222547.188777	46.800820
2887.279167	219365.915532	46.805825
2882.956814	216202.030558	46.810829
2878.721906	213043.807594	46.815834
2874.828027	209898.651305	46.820839
2870.546209	206779.111285	46.825844
2866.516520	203658.862213	46.830849
2862.376293	200558.851365	46.835853
2858.425460	197466.024587	46.840858
2853.863423	194387.491618	46.845863
2849.698948	191326.411419	46.850868
2845.645971	188289.862782	46.855873
2840.934859	185263.201803	46.860877
2837.078747	182244.389895	46.865882
2832.774030	179236.896146	46.870887
2828.447121	176260.163056	46.875892
2824.297400	173283.622591	46.880897
2820.042751	170313.550220	46.885901
2816.097941	167311.609611	46.890906
2811.724771	164385.930590	46.895911
2807.613732	161471.563957	46.900916
2803.207760	158573.794286	46.905921
2799.157636	155700.045163	46.910925
2795.382080	152834.410940	46.915930
2791.127932	149994.155577	46.920935
2786.768379	147153.530508	46.925940
2782.366227	144329.658632	46.930945
2778.121340	141535.286039	46.935949
2774.232668	138744.923419	46.940954
2770.431069	135979.062044	46.945959
2766.259837	133214.837508	46.950964
2762.535777	130468.422064	46.955969
2757.889010	127737.856632	46.960973
2753.929229	125004.868711	46.965978
2749.824998	122306.985003	46.970983
2745.406898	119596.769157	46.975988
2741.607011	116919.759865	46.980993
2737.037947	114267.576252	46.985997
2733.118235	111609.760746	46.991002
2729.017460	108982.873372	46.996007
2724.794603	106364.668233	47.001012
2720.745448	103763.821723	47.006017
2716.416536	101178.206206	47.011021
2712.729148	98604.170483	47.016026
2708.296126	96041.170474	47.021031
2704.301513	93483.634536	47.026036
2700.251940	90951.032764	47.031041
2696.165463	88433.348316	47.036045
2692.102141	85930.495807	47.041050
2687.937230	83439.738280	47.046055
2683.827921	80960.670830	47.051060
2679.908233	78511.372241	47.056065
2675.441577	76069.169905	47.061069
2671.174927	73632.501106	47.066074
2667.077347	71224.076162	47.071079
2662.964542	68823.745037	47.076084
2659.087064	66441.721238	47.081089
2654.552297	64077.127173	47.086093
2650.583724	61722.141512	47.091098
2646.347289	59394.454260	47.096103
2642.091354	57079.078946	47.101108
2638.058577	54770.647725	47.106113
2633.907610	52482.347226	47.111117
2629.551155	50201.863040	47.116122
2625.596929	47963.129914	47.121127
2621.503454	45720.578530	47.126132
2616.918437	43501.574670	47.131137
2612.483602	41305.899634	47.136141
2608.463417	39100.975796	47.141146
2603.885374	36948.848358	47.146151
2599.579262	34800.798416	47.151156
2595.773385	32675.660883	47.156161
2591.454598	30570.845512	47.161165
2587.004952	28470.724892	47.166170
2582.786967	26410.822449	47.171175
2578.307638	24353.222126	47.176180
2574.009551	22324.533633	47.181185
2569.023262	20326.222912	47.186189
2565.423653	18328.207977	47.191194
2561.111473	16370.192901	47.196199
2556.397425	14435.745969	47.201204
2551.819282	12518.306551	47.206209
2547.013115	10634.848789	47.211213
2542.327028	8776.579734	47.216218
2537.079532	6951.718504	47.221223
2528.536449	5261.235072	47.226228
2515.605010	3742.741911	47.231233
2502.534179	2316.211002	47.236237
2486.682162	1127.361657	47.241242
2461.841573	334.265546	47.246247
2421.504955	218.553996	47.251252
2393.348771	231.893595	47.256257
2382.624097	235.795642	47.261261
2385.134310	233.397092	47.266266
2392.739913	233.302016	47.271271
2400.714815	241.985894	47.276276
2407.956487	239.609654	47.281281
2411.003434	233.403253	47.286285
2411.411775	228.546146	47.291290
2409.429993	222.196262	47.296295
2406.363062	236.777521	47.301300
2403.283812	219.633315	47.306305
2399.726183	229.260768	47.311309
2396.508065	217.365023	47.316314
2393.576304	224.224251	47.321319
2390.297207	225.920581	47.326324
2387.906245	219.441718	47.331329
2384.800603	222.610592	47.336333
2382.259464	218.765425	47.341338
2378.937981	222.214850	47.346343
2375.838338	218.852543	47.351348
2373.054042	209.198576	47.356353
2369.857981	216.497802	47.361357
2366.469537	205.774047	47.366362
2363.177671	219.934891	47.371367
2360.052111	226.311896	47.376372
2356.887116	213.537792	47.381377
2353.514560	216.590236	47.386381
2350.153308	211.032006	47.391386
2346.847236	221.107349	47.396391
2343.785902	219.314670	47.401396
2340.604467	210.377766	47.406401
2337.126405	220.929288	47.411405
2333.367272	217.284176	47.416410
2330.654188	213.883556	47.421415
2326.859891	215.679487	47.426420
2323.706662	216.805629	47.431425
2320.334731	213.565036	47.436429
2316.904409	210.887259	47.441434
2313.878460	213.825374	47.446439
2310.815174	213.396641	47.451444
2307.309914	209.857361	47.456449
2302.892625	218.040550	47.461453
2299.920090	206.552536	47.466458
2296.143246	216.185827	47.471463
2292.838349	213.406173	47.476468
2290.188159	205.015789	47.481473
2286.357888	206.402893	47.486477
2283.250109	201.134077	47.491482
2279.711155	209.461438	47.496487
2276.208178	210.177222	47.501492
2272.763806	208.359067	47.506497
2269.120108	219.524998	47.511501
2265.610279	209.554291	47.516506
2262.630713	203.173884	47.521511
2258.991950	205.679522	47.526516
2255.874005	207.644916	47.531521
2252.438523	206.920077	47.536525
2248.842780	200.098221	47.541530
2244.569481	210.799487	47.546535
2241.006045	200.802380	47.551540
2237.869679	206.719171	47.556545
2234.501304	215.102119	47.561549
2231.290343	209.431829	47.566554
2228.358919	205.337708	47.571559
2225.208960	204.966854	47.576564
2221.321960	202.376379	47.581569
2218.264534	206.303406	47.586573
2214.377997	190.456248	47.591578
2210.761838	200.573796	47.596583
2206.833240	207.082798	47.601588
2203.547865	192.290072	47.606593
2200.510375	199.362032	47.611597
2197.016108	198.244598	47.616602
2193.335421	192.679457	47.621607
2189.697008	191.185931	47.626612
2186.338136	195.514481	47.631617
2183.293261	200.489955	47.636621
2179.544577	193.018154	47.641626
2176.071508	190.090842	47.646631
2172.492742	195.241603	47.651636
2169.021768	186.185555	47.656641
2165.308529	195.502023	47.661645
2162.178562	193.862513	47.666650
2158.719210	191.822107	47.671655
2155.214222	198.758407	47.676660
2151.788008	186.180305	47.681665
2148.212465	193.934430	47.686669
2144.945374	192.075926	47.691674
2141.498434	186.584971	47.696679
2137.643714	188.814375	47.701684
2134.181604	186.575086	47.706689
2130.656648	194.786389	47.711693
2127.481742	186.025731	47.716698
2124.307265	189.945781	47.721703
2120.595453	191.883902	47.726708
2117.132055	192.337270	47.731713
2113.620857	192.671563	47.736717
2109.936052	191.697870	47.741722
2106.353668	194.580724	47.746727
2102.822013	186.749121	47.751732
2099.792386	187.878131	47.756737
2095.919713	190.224258	47.761741
2092.570911	191.219707	47.766746
2089.330230	178.995435	47.771751
2085.693722	185.455600	47.776756
2081.987968	187.886349	47.781761
2078.096373	184.496192	47.786765
2074.985184	198.138401	47.791770
2071.528557	190.427952	47.796775
2068.218356	203.860851	47.801780
2064.888909	196.057733	47.806785
2061.083410	191.473989	47.811789
2057.796499	187.261536	47.816794
2054.168705	192.103614	47.821799
2050.618134	199.553293	47.826804
2047.527823	188.710259	47.831809
2043.701350	195.481747	47.836813
2040.473508	185.938439	47.841818
2037.240550	193.661134	47.846823
2033.108284	196.857851	47.851828
2029.712243	200.670223	47.856833
2026.037835	193.063472	47.861837
2022.677945	189.814772	47.866842
2019.428451	190.405549	47.871847
2015.817993	192.650560	47.876852
2012.798438	191.272238	47.881857
2008.961099	189.379617	47.886861
2005.409135	188.979980	47.891866
2001.871296	189.052714	47.896871
1997.994484	189.789115	47.901876
1994.797599	193.393156	47.906881
1991.347721	186.482141	47.911885
1987.642637	188.245240	47.916890
1984.881123	189.028598	47.921895
1980.869893	184.897873	47.926900
1977.842192	179.132563	47.931905
1974.051307	180.494627	47.936909
1970.189757	181.617805	47.941914
1966.534183	180.430774	47.946919
1963.216571	184.202415	47.951924
1959.628040	180.464316	47.956929
1956.253865	183.181752	47.961933
1953.078578	185.140379	47.966938
1949.659583	177.613927	47.971943
1945.985230	179.160252	47.976948
1942.637634	183.313089	47.981953
1939.138858	189.236035	47.986957
1935.575460	179.805393	47.991962
1932.368998	189.273579	47.996967
1928.099236	181.247491	48.001972
1925.107202	175.403851	48.006977
1922.033018	185.341736	48.011981
1917.866845	176.340796	48.016986
1914.544944	182.843530	48.021991
1911.074716	182.415316	48.026996
1907.680573	176.789633	48.032001
1903.714013	183.703308	48.037005
1900.523346	179.004436	48.042010
1896.912512	173.472781	48.047015
1893.473814	185.502074	48.052020
1890.097608	187.017581	48.057025
1886.376791	186.954466	48.062029
1883.011218	178.258543	48.067034
1879.865257	180.497349	48.072039
1875.780964	188.283699	48.077044
1872.289870	172.381174	48.082049
1868.930072	181.170990	48.087053
1865.962893	184.460698	48.092058
1862.135240	183.654985	48.097063
1858.524944	177.923936	48.102068
1855.348957	178.572864	48.107073
1851.605186	177.564197	48.112077
1848.162318	182.076830	48.117082
1844.672268	171.062315	48.122087
1840.936236	175.307604	48.127092
1837.449569	168.158796	48.132097
1833.739459	176.680726	48.137101
1830.661723	175.147045	48.142106
1827.479556	176.002599	48.147111
1823.539628	170.759764	48.152116
1819.945760	177.225985	48.157121
1816.528468	187.910472	48.162125
1813.218055	173.745130	48.167130
1809.932775	179.998543	48.172135
1806.230620	180.068582	48.177140
1802.740714	175.346969	48.182145
1798.954229	179.793163	48.187149
1795.344418	178.279482	48.192154
1792.089641	175.172609	48.197159
1788.463061	170.197136	48.202164
1785.268995	163.214539	48.207169
1781.509202	171.620866	48.212173
1778.036847	169.848393	48.217178
1774.765924	180.952918	48.222183
1771.109682	179.614197	48.227188
1767.968958	180.767013	48.232193
1764.333756	180.877210	48.237197
1760.593348	176.799112	48.242202
1757.265712	182.385267	48.247207
1753.717799	188.806353	48.252212
1750.140419	173.328690	48.257217
1746.518329	172.070058	48.262221
1742.614969	174.633085	48.267226
1739.431370	170.616557	48.272231
1735.850148	179.757443	48.277236
1732.714606	170.297897	48.282241
1729.200266	177.922324	48.287245
1725.647065	172.922736	48.292250
1722.545626	170.010195	48.297255
1718.742141	172.810708	48.302260
1714.822200	161.521839	48.307265
1711.229877	166.867844	48.312269
1707.971183	169.000950	48.317274
1705.008322	162.981974	48.322279
1700.529174	169.599433	48.327284
1698.023997	154.241918	48.332289
1694.241108	155.254804	48.337293
1690.533372	162.760802	48.342298
1687.217650	160.581022	48.347303
1683.553212	170.886582	48.352308
1679.999063	165.431568	48.357313
1676.380645	156.215309	48.362317
1673.018941	158.168388	48.367322
1669.600887	160.421361	48.372327
1666.109494	169.263456	48.377332
1662.660125	162.539166	48.382337
1658.993135	161.062961	48.387341
1655.783676	165.434709	48.392346
1652.362963	167.074317	48.397351
1648.265886	167.690291	48.402356
1644.938656	156.545982	48.407361
1641.236117	168.809609	48.412365
1637.790029	164.565273	48.417370
1634.695565	163.274725	48.422375
1631.000197	166.751228	48.427380
1627.777304	159.475801	48.432385
1623.898669	163.287883	48.437389
1620.739291	160.719813	48.442394
1617.188772	160.082797	48.447399
1613.649161	156.786444	48.452404
1610.155584	164.936010	48.457409
1606.755740	162.665017	48.462413
1603.081330	161.114061	48.467418
1599.572466	169.908286	48.472423
1595.687897	161.543661	48.477428
1592.539534	166.779086	48.482433
1589.031021	165.705221	48.487437
1585.432423	163.250201	48.492442
1582.112200	167.341905	48.497447
1578.579668	169.239491	48.502452
1575.315710	157.041239	48.507457
1571.346499	154.505024	48.512461
1567.792502	161.635808	48.517466
1564.385141	150.690746	48.522471
1560.838323	165.758495	48.527476
1557.730010	162.872396	48.532481
1554.341076	168.597915	48.537485
1550.902688	166.519640	48.542490
1547.163733	152.873940	48.547495
1543.465468	166.098729	48.552500
1540.115272	160.545409	48.557505
1536.651944	157.354207	48.562509
1532.848033	158.667843	48.567514
1530.075457	156.716325	48.572519
1526.214550	168.913018	48.577524
1522.713577	158.447707	48.582529
1518.832310	157.584076	48.587533
1515.191689	170.246181	48.592538
1511.788477	165.694615	48.597543
1508.088629	167.770278	48.602548
1505.032168	157.877659	48.607553
1501.706145	157.531421	48.612557
1498.331835	163.501445	48.617562
1494.826452	156.308252	48.622567
1490.970593	161.009019	48.627572
1487.970189	164.452723	48.632577
1483.847444	162.750519	48.637581
1480.224585	154.942952	48.642586
1477.041624	155.899979	48.647591
1473.355052	159.030299	48.652596
1470.067987	151.815601	48.657601
1466.168644	157.073690	48.662605
1462.766833	153.920345	48.667610
1459.728357	147.862674	48.672615
1456.062867	160.883029	48.677620
1452.715986	151.080187	48.682625
1449.149796	156.811332	48.687629
1445.467008	146.877572	48.692634
1442.207877	159.457826	48.697639
1438.411727	158.210735	48.702644
1435.009032	159.461604	48.707649
1431.281898	157.460210	48.712653
1428.104640	155.856812	48.717658
1424.694319	152.815548	48.722663
1420.817713	156.659021	48.727668
1417.146555	152.563900	48.732673
1414.168352	158.253638	48.737677
1410.398809	154.085333	48.742682
1407.299357	162.603543	48.747687
1403.504111	158.230449	48.752692
1399.909706	152.069989	48.757697
1396.272696	154.749638	48.762701
1392.633074	158.894557	48.767706
1389.518449	157.233910	48.772711
1385.380260	167.857324	48.777716
1382.567744	153.351655	48.782721
1379.614954	151.121499	48.787725
1375.848118	159.218988	48.792730
1372.012141	159.680302	48.797735
1368.139369	159.552576	48.802740
1364.831074	157.083837	48.807745
1361.359976	161.015719	48.812749
1357.949237	154.956241	48.817754
1354.591539	152.675578	48.822759
1351.344128	154.604540	48.827764
1347.846875	158.154532	48.832769
1344.040779	156.921690	48.837773
1340.093044	156.552603	48.842778
1336.833643	152.671476	48.847783
1333.130327	153.659382	48.852788
1329.773278	148.293886	48.857793
1326.450798	159.007927	48.862797
1322.858638	155.352906	48.867802
1319.371114	158.119917	48.872807
1315.812217	155.576526	48.877812
1312.521319	149.365428	48.882817
1309.205706	156.832302	48.887821
1305.583844	163.505539	48.892826
1301.928821	153.260603	48.897831
1297.972588	161.128330	48.902836
1294.876836	158.265666	48.907841
1291.405153	158.802864	48.912845
1287.958007	154.872049	48.917850
1284.379144	150.585360	48.922855
1280.834881	154.535048	48.927860
1277.686181	150.535370	48.932865
1273.813138	156.213363	48.937869
1270.197507	162.031400	48.942874
1267.082198	147.721885	48.947879
1263.264006	158.111737	48.952884
1259.698798	154.579075	48.957889
1256.374087	166.391338	48.962893
1253.174364	154.198991	48.967898
1249.915966	141.990529	48.972903
1245.901187	154.505617	48.977908
1242.230460	145.829269	48.982913
1238.599810	151.270004	48.987917
1235.368823	150.339488	48.992922
1231.679096	152.404173	48.997927
1227.993152	161.716612	49.002932
1224.579026	150.434228	49.007937
1221.267427	147.950240	49.012941
1217.829317	152.908411	49.017946
1214.672504	143.316371	49.022951
1211.039615	145.571485	49.027956
1207.486410	142.726684	49.032961
1203.811538	146.304527	49.037965
1200.414318	153.825335	49.042970
1197.308566	147.126541	49.047975
1193.012038	151.845777	49.052980
1189.796716	143.468327	49.057985
1186.057343	145.869838	49.062989
1182.457109	146.424036	49.067994
1179.024858	131.895267	49.072999
1175.563488	149.819306	49.078004
1172.273959	140.605575	49.083009
1168.750980	144.267221	49.088013
1164.988851	138.123631	49.093018
1161.884211	143.225768	49.098023
1158.674671	150.160370	49.103028
1154.835753	139.115376	49.108033
1151.701302	145.009977	49.113037
1148.035250	145.030313	49.118042
1144.090617	144.243195	49.123047
1140.975010	143.854646	49.128052
1137.434929	142.222729	49.133057
1133.840896	137.261419	49.138061
1130.074764	149.038404	49.143066
1126.887681	146.582413	49.148071
1122.999645	147.785983	49.153076
1119.617531	147.189223	49.158081
1115.992081	134.908575	49.163085
1112.723284	151.312315	49.168090
1109.135594	144.891495	49.173095
1105.643917	143.786698	49.178100
1102.259754	138.798871	49.183105
1098.610444	152.848189	49.188109
1095.175163	154.097947	49.193114
1092.259360	140.940553	49.198119
1088.103261	148.393539	49.203124
1084.981770	145.512832	49.208129
1081.281817	151.429552	49.213133
1077.578272	142.226896	49.218138
1074.284325	138.098172	49.223143
1070.364238	151.898819	49.228148
1067.401056	142.738442	49.233153
1063.791874	141.629912	49.238157
1060.228311	148.645279	49.243162
1056.890315	142.568211	49.248167
1053.370792	153.642206	49.253172
1049.942187	138.745918	49.258177
1046.142339	139.932548	49.263181
1042.632428	148.113299	49.268186
1039.010666	137.233686	49.273191
1035.761423	145.459049	49.278196
1032.600924	141.524586	49.283201
1028.386604	146.193050	49.288205
1025.008149	152.625777	49.293210
1021.563704	144.483590	49.298215
1017.882926	148.426264	49.303220
1014.526957	150.783627	49.308225
1011.379989	143.306730	49.313229
1007.809724	149.165202	49.318234
1004.547072	143.361103	49.323239
1000.583435	145.576328	49.328244
997.264816	145.403115	49.333249
993.599210	143.601076	49.338253
989.827055	143.258427	49.343258
986.196026	135.971233	49.348263
982.946076	151.606403	49.353268
979.677154	143.613926	49.358273
976.191849	144.979128	49.363277
972.579317	156.387256	49.368282
969.053724	151.456425	49.373287
965.683277	150.310551	49.378292
962.532371	152.221362	49.383297
958.951355	151.108461	49.388301
955.212718	144.954957	49.393306
951.823588	139.373169	49.398311
948.250748	148.158601	49.403316
944.531475	143.773812	49.408321
940.768052	148.055328	49.413325
937.476733	149.564180	49.418330
934.318845	138.286107	49.423335
930.343972	147.169298	49.428340
926.805524	150.444297	49.433345
923.583405	149.392275	49.438349
920.162650	150.342420	49.443354
916.753967	140.198308	49.448359
912.927501	147.856014	49.453364
909.440712	141.546035	49.458369
905.906202	152.761624	49.463373
902.489005	151.502869	49.468378
899.219179	140.584031	49.473383
895.695425	147.026891	49.478388
892.496251	144.183727	49.483393
888.538026	151.583657	49.488397
885.015459	148.265939	49.493402
881.218959	144.174851	49.498407
877.668595	146.701907	49.503412
874.330150	144.934111	49.508417
871.134799	139.863026	49.513421
867.792490	143.021909	49.518426
864.470777	141.738725	49.523431
860.520215	149.564581	49.528436
857.045205	137.880610	49.533441
853.473415	133.244974	49.538445
849.959237	138.936522	49.543450
846.391092	133.727667	49.548455
842.742425	140.566597	49.553460
839.501041	150.549869	49.558465
836.088128	139.947702	49.563469
832.315605	136.286326	49.568474
829.054373	141.909798	49.573479
825.699315	144.808094	49.578484
822.238233	134.048961	49.583489
818.635972	143.753381	49.588493
814.897730	147.594392	49.593498
811.586244	137.938156	49.598503
807.559256	146.842205	49.603508
804.222277	137.136180	49.608513
800.938841	141.535574	49.613517
797.327739	139.519433	49.618522
794.398973	131.983147	49.623527
790.880434	143.711965	49.628532
786.936937	143.298151	49.633537
783.240293	141.380834	49.638541
780.189403	140.669053	49.643546
776.490180	133.386306	49.648551
772.905830	149.399757	49.653556
769.508966	137.820651	49.658561
765.944386	144.700225	49.663565
761.705360	143.079829	49.668570
759.207935	133.375233	49.673575
755.693889	142.081910	49.678580
752.005260	132.604989	49.683585
748.531455	130.007372	49.688589
744.582155	131.657294	49.693594
741.286354	139.038960	49.698599
737.706749	133.888895	49.703604
734.099500	133.324369	49.708609
730.953420	132.364915	49.713613
727.469720	139.946856	49.718618
724.164009	138.847883	49.723623
720.262102	142.720886	49.728628
716.940368	132.987205	49.733633
713.677372	136.393150	49.738637
709.818988	136.753831	49.743642
706.186225	136.104725	49.748647
702.804251	138.349203	49.753652
699.424872	130.782281	49.758657
695.788160	139.698015	49.763661
691.979013	137.880614	49.768666
688.905108	131.702230	49.773671
685.287640	136.533630	49.778676
682.066712	130.042909	49.783681
678.592769	128.416633	49.788685
675.060359	138.341114	49.793690
671.713888	131.778308	49.798695
667.749275	139.511514	49.803700
664.108300	137.000223	49.808705
660.743752	140.260736	49.813709
657.057688	142.923021	49.818714
653.643100	132.824251	49.823719
650.616753	135.183898	49.828724
647.596899	135.846725	49.833729
643.489236	136.556527	49.838733
639.522808	138.702732	49.843738
636.378223	131.260420	49.848743
632.535907	136.471908	49.853748
629.310233	135.142133	49.858753
625.452677	135.800119	49.863757
622.174106	131.571086	49.868762
618.721288	134.544874	49.873767
615.154681	142.646046	49.878772
611.681758	136.134706	49.883777
608.223955	126.624871	49.888781
604.959019	134.435183	49.893786
601.456748	131.873721	49.898791
597.731457	140.702117	49.903796
594.044355	130.111373	49.908801
590.775623	133.923224	49.913805
587.403658	131.667233	49.918810
584.048484	132.528133	49.923815
580.439615	135.997783	49.928820
577.129839	131.093436	49.933825
573.240977	136.119244	49.938829
569.459256	138.344118	49.943834
566.341013	127.335258	49.948839
562.872600	141.479767	49.953844
559.379674	133.753515	49.958849
555.794340	136.235543	49.963853
552.147702	134.063714	49.968858
549.048118	129.316287	49.973863
544.981870	133.873170	49.978868
541.637804	131.590680	49.983873
538.261761	129.253088	49.988877
534.684038	139.216346	49.993882
531.286632	122.606987	49.998887
527.604249	129.134919	50.003892
524.040776	126.902621	50.008897
520.694747	127.958267	50.013901
517.323710	129.226643	50.018906
513.890551	124.907971	50.023911
509.902217	126.959581	50.028916
506.463606	128.206907	50.033921
502.839369	130.796289	50.038925
499.601173	142.781841	50.043930
496.522184	129.030165	50.048935
492.767075	132.570209	50.053940
489.201294	127.595263	50.058945
485.979179	131.096122	50.063949
482.066985	139.014178	50.068954
478.908892	131.289305	50.073959
474.890800	133.598696	50.078964
471.627375	122.096920	50.083969
468.032905	129.231209	50.088973
464.171442	143.079799	50.093978
461.380631	131.361623	50.098983
457.496079	140.885739	50.103988
454.321205	134.811848	50.108993
450.756368	128.900283	50.113997
447.228907	142.566845	50.119002
444.073208	126.859320	50.124007
440.104611	130.733386	50.129012
436.601046	128.599310	50.134017
433.120267	130.479702	50.139021
429.383931	142.954593	50.144026
426.366346	125.131002	50.149031
422.895173	138.908976	50.154036
419.082428	135.133861	50.159041
415.355426	130.544874	50.164045
411.811803	124.892601	50.169050
408.698924	122.083563	50.174055
404.967242	128.964115	50.179060
400.919592	128.876838	50.184065
397.931445	115.832337	50.189069
394.525695	128.767983	50.194074
391.751527	118.195700	50.199079
388.170308	131.174654	50.204084
383.971974	129.987836	50.209089
380.785390	120.878560	50.214093
376.925657	131.433376	50.219098
373.793802	125.963397	50.224103
369.938027	120.704896	50.229108
366.502861	118.835386	50.234113
363.027121	116.753932	50.239117
358.868638	127.437808	50.244122
356.176767	126.109941	50.249127
352.547800	130.319990	50.254132
349.294318	122.958136	50.259137
345.620157	118.712089	50.264141
342.028410	133.347377	50.269146
338.797605	126.333155	50.274151
334.685817	137.288146	50.279156
330.861793	126.798080	50.284161
328.116337	120.558901	50.289165
324.574416	128.602510	50.294170
321.284281	131.202902	50.299175
317.343909	134.699269	50.304180
314.069452	125.742992	50.309185
310.592270	119.580478	50.314189
306.954691	126.354573	50.319194
303.462535	129.973724	50.324199
300.382465	127.713251	50.329204
296.617697	127.913908	50.334209
293.035648	122.568271	50.339213
289.262935	131.847128	50.344218
285.978394	118.633967	50.349223
282.335326	128.053870	50.354228
278.437614	124.500943	50.359233
275.112866	116.640915	50.364237
271.826616	126.444693	50.369242
268.332882	116.412297	50.374247
264.767384	123.902788	50.379252
261.633411	126.877377	50.384257
258.391901	121.563831	50.389261
254.761906	120.465217	50.394266
251.435261	117.199337	50.399271
247.378478	126.845415	50.404276
243.712323	122.417823	50.409281
240.324385	114.922056	50.414285
236.958274	128.557063	50.419290
233.543002	115.161927	50.424295
230.080596	128.267847	50.429300
226.351747	122.692132	50.434305
222.773717	125.616074	50.439309
219.092936	125.794115	50.444314
216.172290	118.171368	50.449319
212.597360	124.932517	50.454324
209.044844	116.855097	50.459329
205.469991	125.011473	50.464333
201.902940	127.145916	50.469338
198.449033	128.231236	50.474343
194.714104	122.055368	50.479348
191.299234	124.365294	50.484353
187.903438	122.581439	50.489357
184.346775	127.988795	50.494362
181.024895	118.435726	50.499367
177.498143	119.038913	50.504372
173.969418	117.914978	50.509377
170.387480	123.047883	50.514381
167.006206	132.246476	50.519386
163.404233	123.582027	50.524391
159.607401	119.276189	50.529396
155.748874	122.756636	50.534401
152.609664	125.292312	50.539405
149.436599	124.558762	50.544410
146.003891	128.042105	50.549415
141.969888	127.617447	50.554420
138.612495	118.807126	50.559425
135.446130	124.665887	50.564429
131.861952	123.446250	50.569434
128.410566	124.319228	50.574439
124.795037	130.017407	50.579444
121.238728	126.914112	50.584449
117.719897	128.427257	50.589453
114.048320	121.225923	50.594458
110.748169	122.347300	50.599463
107.620552	126.757308	50.604468
104.168742	122.033603	50.609473
100.518840	132.106382	50.614477
96.591169	132.145983	50.619482
93.185136	123.207258	50.624487
89.379037	112.898020	50.629492
86.052948	114.991592	50.634497
82.873048	118.492297	50.639501
79.035966	127.189681	50.644506
75.715813	124.631545	50.649511
72.104626	122.090534	50.654516
69.149939	126.403857	50.659521
65.735164	111.436325	50.664525
61.758662	126.394563	50.669530
58.128576	117.307462	50.674535
54.416895	120.220770	50.679540
50.914165	118.554967	50.684545
47.889211	114.656600	50.689549
44.112354	126.403951	50.694554
40.876773	115.144797	50.699559
37.272867	120.578589	50.704564
33.524831	110.076785	50.709569
30.611588	120.448618	50.714573
26.569407	121.186409	50.719578
23.485220	122.552395	50.724583
19.791688	123.109011	50.729588
15.898137	122.323880	50.734593
12.701293	116.291587	50.739597
9.231774	123.523516	50.744602
5.793301	114.922119	50.749607
2.258899	123.844191	50.754612