Thu Aug 25 16:53:10 2022

Number of Points = 9926

Depth (nm)	Load (N)	Time (s)
1.425047	99.766778	0.000000
1.355713	89.726311	0.005005
0.725417	82.051670	0.010010
0.992214	86.891629	0.015014
0.806070	87.290992	0.020019
0.769006	84.386147	0.025024
0.438400	76.060269	0.030029
0.350301	72.005476	0.035034
0.144619	65.128027	0.040038
-0.287438	55.840444	0.045043
-0.463688	51.473597	0.050048
-0.822820	51.707073	0.055053
-1.404798	46.552740	0.060058
-1.440052	30.372393	0.065062
-1.565719	49.308367	0.070067
-1.898639	30.596175	0.075072
-2.449629	23.345736	0.080077
-2.651964	21.153336	0.085082
-2.781961	31.367435	0.090086
-3.029235	29.352919	0.095091
-3.138339	25.465945	0.100096
-3.430116	24.904250	0.105101
-3.646122	21.730057	0.110106
-4.332170	12.501275	0.115110
-5.053842	22.592937	0.120115
-5.255347	15.955300	0.125120
-4.761611	12.824930	0.130125
-5.139975	18.705597	0.135130
-5.307578	15.723139	0.140134
-5.289144	12.126235	0.145139
-6.022961	13.468791	0.150144
-5.939919	12.626904	0.155149
-6.399254	23.158356	0.160154
-6.074439	12.157664	0.165158
-7.602985	13.074243	0.170163
-7.472263	19.229488	0.175168
-7.511087	5.258041	0.180173
-7.777899	14.006592	0.185178
-7.502958	11.119313	0.190182
-8.749722	18.651492	0.195187
-9.065839	7.131125	0.200192
-8.822422	13.426900	0.205197
-9.059753	16.650043	0.210202
-8.996102	10.597291	0.215206
-9.345545	19.380937	0.220211
-9.487021	28.742613	0.225216
-9.763264	16.016921	0.230221
-10.407402	16.355164	0.235226
-10.572723	16.115344	0.240230
-10.899923	21.187559	0.245235
-11.017382	16.637503	0.250240
-10.727260	12.349455	0.255245
-11.841867	21.262482	0.260250
-11.801931	13.928951	0.265254
-12.134784	14.433557	0.270259
-12.176479	14.788140	0.275264
-12.242604	17.652262	0.280269
-12.696999	11.038432	0.285274
-13.146073	13.525954	0.290278
-13.457026	15.295803	0.295283
-13.312735	13.191465	0.300288
-13.707747	12.272620	0.305293
-13.758932	19.377026	0.310298
-14.482181	15.741305	0.315302
-15.086818	23.799304	0.320307
-15.001202	16.515563	0.325312
-15.080909	12.642968	0.330317
-15.403842	22.071036	0.335322
-15.087298	11.919533	0.340326
-15.496159	25.831482	0.345331
-15.971488	13.893130	0.350336
-16.616585	11.684683	0.355341
-16.998109	10.412546	0.360346
-16.260681	7.791328	0.365350
-16.579914	17.547846	0.370355
-17.002257	14.228813	0.375360
-17.309125	9.129465	0.380365
-17.861136	21.387039	0.385370
-17.991295	13.921971	0.390374
-18.267479	13.547660	0.395379
-18.646003	14.651049	0.400384
-19.017853	15.924236	0.405389
-19.955994	18.969282	0.410394
-19.248418	13.157325	0.415398
-19.949799	18.398900	0.420403
-20.036026	10.832036	0.425408
-20.075040	11.192526	0.430413
-20.224710	20.220120	0.435418
-19.825995	12.650040	0.440422
-20.683029	13.989756	0.445427
-20.793863	19.591222	0.450432
-21.039156	6.794250	0.455437
-21.395522	17.663908	0.460442
-21.875063	6.669026	0.465446
-22.391518	14.143724	0.470451
-22.318387	19.808116	0.475456
-22.391364	14.067838	0.480461
-22.499695	10.800847	0.485466
-22.585736	7.157038	0.490470
-23.432678	11.083141	0.495475
-23.765304	7.525425	0.500480
-24.225871	7.515365	0.505485
-24.287861	11.558926	0.510490
-24.262710	-0.540092	0.515494
-24.233619	8.446832	0.520499
-24.667571	4.990414	0.525504
-25.397643	7.142310	0.530509
-25.586006	9.668077	0.535514
-25.574293	9.637802	0.540518
-25.976748	12.927946	0.545523
-25.786085	9.895683	0.550528
-25.961791	18.864080	0.555533
-26.474906	22.256986	0.560538
-26.576075	19.691230	0.565542
-27.402772	29.935393	0.570547
-27.184499	16.739912	0.575552
-27.321923	15.448511	0.580557
-27.900184	21.686369	0.585562
-28.293450	10.469158	0.590566
-28.540335	13.750746	0.595571
-28.686705	20.484085	0.600576
-28.669209	11.034341	0.605581
-28.853137	12.205317	0.610586
-28.855020	13.404717	0.615590
-29.447551	11.716387	0.620595
-29.674092	14.007689	0.625600
-29.697958	13.900730	0.630605
-30.591790	25.841703	0.635610
-30.868520	13.935511	0.640614
-31.295548	16.400597	0.645619
-30.896885	15.756032	0.650624
-31.218975	16.255789	0.655629
-31.432198	10.366643	0.660634
-31.196753	3.369482	0.665638
-32.035328	15.738392	0.670643
-32.470414	10.722410	0.675648
-32.326690	13.370151	0.680653
-32.752352	13.753258	0.685658
-32.648082	16.350234	0.690662
-33.342462	18.841391	0.695667
-33.802416	8.210440	0.700672
-34.143148	8.241715	0.705677
-34.474273	13.520189	0.710682
-34.164239	12.677538	0.715686
-34.362856	13.414214	0.720691
-34.485868	11.845308	0.725696
-34.998337	11.201134	0.730701
-35.436520	18.185840	0.735706
-35.352833	17.960788	0.740710
-35.658048	21.200896	0.745715
-36.262620	21.536105	0.750720
-36.764809	13.214999	0.755725
-37.202969	12.866068	0.760730
-37.262497	15.640570	0.765734
-37.418644	20.698639	0.770739
-37.653796	14.268759	0.775744
-37.679708	12.463174	0.780749
-37.565904	14.223418	0.785754
-37.094542	16.411697	0.790758
-37.559579	13.390423	0.795763
-38.583835	13.554108	0.800768
-38.613255	6.104897	0.805773
-38.970621	22.900464	0.810778
-39.952385	5.463734	0.815782
-39.958885	14.823233	0.820787
-40.344761	15.696819	0.825792
-40.029015	10.063317	0.830797
-40.194891	9.051623	0.835802
-40.060430	11.333818	0.840806
-40.112930	18.077757	0.845811
-41.090574	7.860118	0.850816
-41.438095	19.348490	0.855821
-41.654005	17.784647	0.860826
-42.062566	15.972578	0.865830
-41.775410	19.455229	0.870835
-42.402882	20.145206	0.875840
-43.077158	9.316881	0.880845
-43.296796	16.498299	0.885850
-43.142377	15.762288	0.890854
-43.318105	14.078254	0.895859
-43.479036	11.765474	0.900864
-43.433484	10.565627	0.905869
-44.192923	14.952589	0.910874
-44.539740	9.596909	0.915878
-44.646672	11.496144	0.920883
-44.861332	8.511571	0.925888
-44.841420	11.605821	0.930893
-45.032653	17.333779	0.935898
-45.590989	7.857204	0.940902
-46.108819	21.210415	0.945907
-46.162244	6.206705	0.950912
-46.317673	13.919066	0.955917
-46.750856	15.246157	0.960922
-46.412269	16.689606	0.965926
-47.290618	6.399463	0.970931
-47.328631	13.780213	0.975936
-47.854042	17.203519	0.980941
-47.746025	13.146487	0.985946
-47.553174	10.202467	0.990950
-48.649780	2.844543	0.995955
-49.045305	14.466983	1.000960
-49.157773	10.279982	1.005965
-49.507527	23.258844	1.010970
-49.304208	7.740338	1.015974
-49.639237	10.580152	1.020979
-49.662521	14.677760	1.025984
-49.591437	11.971120	1.030989
-50.535625	13.887647	1.035994
-50.406313	17.872760	1.040998
-51.012322	14.307259	1.046003
-51.052190	9.308448	1.051008
-50.967516	17.179343	1.056013
-51.345257	13.840670	1.061018
-52.026084	8.882177	1.066022
-52.224109	14.478320	1.071027
-52.338848	13.765501	1.076032
-52.444791	5.113392	1.081037
-52.955743	15.260618	1.086042
-53.378507	13.798790	1.091046
-53.704911	16.564488	1.096051
-53.741681	15.453470	1.101056
-53.563776	20.076380	1.106061
-53.717479	19.413958	1.111066
-53.975434	11.003966	1.116070
-54.594031	21.481276	1.121075
-55.042781	16.220661	1.126080
-55.465448	15.432702	1.131085
-55.551790	17.784296	1.136090
-55.144976	18.112895	1.141094
-56.132707	12.990517	1.146099
-56.519599	18.318860	1.151104
-56.685176	10.302521	1.156109
-57.127973	18.888820	1.161114
-56.920842	18.685555	1.166118
-57.076565	13.916869	1.171123
-57.046966	17.585409	1.176128
-56.979747	15.524784	1.181133
-57.635933	19.892405	1.186138
-57.925864	13.872910	1.191142
-58.180201	16.042017	1.196147
-59.019285	17.647845	1.201152
-59.547148	18.100751	1.206157
-59.368377	23.125325	1.211162
-59.357922	14.451811	1.216166
-59.803624	20.279754	1.221171
-60.034469	24.384576	1.226176
-59.883973	13.230864	1.231181
-60.385138	14.998882	1.236186
-60.430270	11.092398	1.241190
-60.908715	18.266911	1.246195
-61.070467	18.482116	1.251200
-61.029528	10.196136	1.256205
-61.173987	22.165222	1.261210
-61.786412	14.339121	1.266214
-62.448068	14.661130	1.271219
-62.662239	16.529712	1.276224
-62.274164	18.911375	1.281229
-62.808126	28.363018	1.286234
-63.097962	9.726369	1.291238
-63.721768	19.524282	1.296243
-64.510062	21.068369	1.301248
-64.325150	11.013425	1.306253
-64.168731	18.901552	1.311258
-64.218317	12.319211	1.316262
-64.431050	10.672614	1.321267
-64.267590	19.923226	1.326272
-64.640584	13.793359	1.331277
-65.408636	26.774489	1.336282
-65.726010	20.746637	1.341286
-65.782679	19.322360	1.346291
-65.900299	23.099390	1.351296
-66.722409	21.070545	1.356301
-67.377530	18.439727	1.361306
-67.300968	16.134028	1.366310
-67.424291	12.869387	1.371315
-67.495453	17.265564	1.376320
-67.457699	13.415695	1.381325
-67.619966	21.967531	1.386330
-67.747740	12.588008	1.391334
-68.498986	10.003892	1.396339
-69.037490	9.265723	1.401344
-69.083538	9.554548	1.406349
-69.462637	16.511012	1.411354
-69.274688	16.889724	1.416358
-69.113573	19.882755	1.421363
-69.834419	15.500013	1.426368
-70.444507	16.139812	1.431373
-70.483998	21.764900	1.436378
-70.764379	13.845643	1.441382
-70.664448	10.277101	1.446387
-70.837114	9.598668	1.451392
-71.635875	10.897621	1.456397
-72.209786	6.982243	1.461402
-72.011380	10.254169	1.466406
-72.375493	14.920876	1.471411
-72.356986	10.523527	1.476416
-72.182500	11.008753	1.481421
-72.387943	19.254138	1.486426
-73.173396	3.602666	1.491430
-73.163685	12.719175	1.496435
-73.550112	18.686526	1.501440
-73.707509	6.995766	1.506445
-74.713034	17.486243	1.511450
-74.573437	4.084803	1.516454
-74.920903	6.572223	1.521459
-74.994005	4.340597	1.526464
-74.985004	-2.282555	1.531469
-75.082764	10.479639	1.536474
-75.694349	4.921839	1.541478
-75.876498	9.275293	1.546483
-76.536740	15.877174	1.551488
-76.414662	14.557768	1.556493
-76.786928	10.664578	1.561498
-76.872279	10.409065	1.566502
-76.904809	-3.035002	1.571507
-76.983461	12.271035	1.576512
-77.114256	8.090072	1.581517
-77.787619	13.912556	1.586522
-78.252624	11.666406	1.591526
-78.689187	-1.556166	1.596531
-78.754760	4.968351	1.601536
-78.744175	4.827520	1.606541
-79.166050	8.136526	1.611546
-79.402882	13.321131	1.616550
-80.268200	10.947879	1.621555
-80.352570	7.231044	1.626560
-80.513947	8.230807	1.631565
-81.044786	15.182573	1.636570
-80.367561	-2.444485	1.641574
-80.702101	3.169881	1.646579
-80.777336	7.354720	1.651584
-80.684765	6.482867	1.656589
-81.496015	10.102823	1.661594
-81.959087	7.011643	1.666598
-82.120189	-2.188641	1.671603
-82.421137	10.896458	1.676608
-83.045391	8.630968	1.681613
-83.646271	7.668455	1.686618
-83.692514	7.068290	1.691622
-83.265229	13.316266	1.696627
-84.187708	16.330388	1.701632
-83.821763	6.256573	1.706637
-84.239240	14.519361	1.711642
-83.955684	10.703745	1.716646
-84.152158	6.400195	1.721651
-84.815591	10.000154	1.726656
-85.082794	15.879220	1.731661
-85.231270	8.031049	1.736666
-85.543436	7.738310	1.741670
-86.455784	5.742590	1.746675
-86.638106	13.465491	1.751680
-86.820869	9.628030	1.756685
-86.824733	15.649333	1.761690
-86.818020	5.021199	1.766694
-86.946184	6.743425	1.771699
-87.043862	9.701074	1.776704
-87.538013	10.022148	1.781709
-88.322258	16.317591	1.786714
-88.094188	3.342054	1.791718
-88.061799	11.287575	1.796723
-88.527169	9.177526	1.801728
-88.967781	4.314278	1.806733
-89.527366	5.955407	1.811738
-89.453800	3.618541	1.816742
-89.594476	1.413322	1.821747
-89.962526	9.301365	1.826752
-89.798748	3.501851	1.831757
-90.526028	3.562060	1.836762
-90.885767	2.552271	1.841766
-91.184984	6.196400	1.846771
-91.348910	7.595198	1.851776
-91.046460	-1.854891	1.856781
-91.647918	4.180951	1.861786
-92.637292	5.076335	1.866790
-92.525495	0.060091	1.871795
-92.691459	7.252076	1.876800
-92.949509	3.211278	1.881805
-93.081401	5.965478	1.886810
-93.201848	7.063232	1.891814
-93.065676	5.418914	1.896819
-93.087056	10.221742	1.901824
-93.694059	5.482644	1.906829
-94.036076	10.224981	1.911834
-94.073215	8.152236	1.916838
-94.948688	9.488520	1.921843
-95.403706	10.088203	1.926848
-95.629333	-3.882429	1.931853
-95.789235	8.778767	1.936858
-96.132553	5.406230	1.941862
-95.870147	6.105470	1.946867
-95.964229	11.318326	1.951872
-95.903320	7.907760	1.956877
-96.723732	8.099622	1.961882
-97.146116	5.426014	1.966886
-97.314005	0.175183	1.971891
-97.364307	6.627704	1.976896
-97.254372	-0.460519	1.981901
-97.893263	9.697258	1.986906
-98.360050	2.104613	1.991910
-98.324740	5.490678	1.996915
-98.939299	2.103293	2.006912
-99.093893	5.913134	2.016909
-98.064354	5.137323	2.026906
-97.798077	3.923573	2.036902
-96.605593	1.566829	2.046899
-96.424484	-0.045392	2.056896
-96.182423	10.237516	2.066893
-95.096589	7.507841	2.076890
-95.236643	7.789616	2.086886
-94.668556	0.661766	2.096883
-93.540407	2.876768	2.106880
-93.175502	5.442617	2.116877
-93.538267	10.653578	2.126874
-92.432191	13.644990	2.136870
-92.014152	13.465513	2.146867
-91.596481	10.374863	2.156864
-90.835111	7.369743	2.166861
-90.553665	5.691114	2.176858
-90.336959	2.052243	2.186854
-89.096531	9.353018	2.196851
-89.234842	2.703321	2.206848
-88.714248	8.551983	2.216845
-88.149847	8.188014	2.226842
-87.442377	11.634695	2.236838
-86.616736	8.986972	2.246835
-86.748546	9.305469	2.256832
-85.903680	8.590274	2.266829
-85.101575	6.633657	2.276826
-85.346418	7.071237	2.286822
-84.479102	10.654430	2.296819
-84.151005	5.898869	2.306816
-83.510383	12.055012	2.316813
-82.556992	9.314411	2.326810
-82.027133	6.117484	2.336806
-82.109143	5.202231	2.346803
-81.947852	14.686836	2.356800
-81.206624	8.868676	2.366797
-80.403353	9.560178	2.376794
-79.811070	6.530867	2.386790
-79.412595	7.304804	2.396787
-79.227681	6.274866	2.406784
-78.480635	-1.277003	2.416781
-78.428892	8.443345	2.426778
-77.348841	8.027089	2.436774
-76.774344	1.069297	2.446771
-76.115797	16.102045	2.456768
-75.712658	8.635737	2.466765
-75.276797	7.895931	2.476762
-75.173931	13.100458	2.486758
-74.873102	12.866487	2.496755
-74.054598	10.422624	2.506752
-73.263420	11.087511	2.516749
-72.662554	12.200371	2.526746
-72.281964	10.110229	2.536742
-72.110050	11.036876	2.546739
-71.496960	11.336858	2.556736
-71.003263	19.739840	2.566733
-70.442102	11.136863	2.576730
-69.633042	16.233905	2.586726
-69.409411	11.035377	2.596723
-69.209982	12.141446	2.606720
-68.306374	16.314508	2.616717
-67.743510	10.765050	2.626714
-67.815200	9.601088	2.636710
-66.818759	8.767110	2.646707
-66.546486	14.119323	2.656704
-65.696524	14.771833	2.666701
-65.336222	16.768197	2.676698
-65.270482	14.182522	2.686694
-64.463771	8.769087	2.696691
-63.989455	13.009414	2.706688
-63.429767	10.831020	2.716685
-62.405712	11.304196	2.726682
-62.525039	13.904740	2.736678
-62.359612	18.589446	2.746675
-61.508042	14.344244	2.756672
-60.897779	11.128383	2.766669
-60.015839	20.477902	2.776666
-59.746235	16.580481	2.786662
-59.408666	18.741967	2.796659
-58.941348	14.661511	2.806656
-58.833141	21.018293	2.816653
-58.075575	22.223812	2.826650
-56.788147	18.854328	2.836646
-56.527960	21.126142	2.846643
-56.732926	16.061292	2.856640
-56.129579	9.523465	2.866637
-55.285436	7.728159	2.876634
-55.190071	13.564259	2.886630
-54.335751	10.325996	2.896627
-53.792428	12.363376	2.906624
-53.605371	15.045794	2.916621
-52.607803	13.175762	2.926618
-52.421388	14.996632	2.936614
-52.129606	17.459901	2.946611
-51.413654	12.583377	2.956608
-51.155810	24.283013	2.966605
-49.924208	16.439801	2.976602
-49.493086	19.923452	2.986598
-49.378736	19.157996	2.996595
-49.357104	18.014258	3.006592
-48.222422	12.631797	3.016589
-47.742741	17.606221	3.026586
-47.639692	19.037840	3.036582
-46.621460	18.865694	3.046579
-46.717708	18.681270	3.056576
-45.774173	12.381579	3.066573
-45.196238	23.007852	3.076570
-44.921190	14.063229	3.086566
-44.701700	17.203069	3.096563
-43.457547	21.291098	3.106560
-43.526431	16.860666	3.116557
-42.845524	18.550203	3.126554
-42.399811	26.824494	3.136550
-42.027301	21.247838	3.146547
-41.054091	18.586498	3.156544
-40.679803	11.178563	3.166541
-40.788811	19.108943	3.176538
-39.742598	17.611429	3.186534
-39.113470	15.042017	3.196531
-39.189831	17.829066	3.206528
-38.454819	14.885099	3.216525
-37.733048	15.443655	3.226522
-37.347243	11.866986	3.236518
-36.377851	16.245157	3.246515
-35.953023	16.695017	3.256512
-36.026229	13.598917	3.266509
-35.769100	13.878648	3.276506
-34.429626	11.764976	3.286502
-34.464229	8.155977	3.296499
-34.004468	11.790364	3.306496
-33.166728	13.110035	3.316493
-32.986050	16.560068	3.326490
-32.484261	21.220584	3.336486
-32.013793	16.341343	3.346483
-31.660146	22.963781	3.356480
-30.293152	16.569230	3.366477
-30.482345	16.424711	3.376474
-29.886537	19.325023	3.386470
-28.954937	16.648029	3.396467
-28.948179	18.829672	3.406464
-28.523129	22.304774	3.416461
-27.643020	19.068806	3.426458
-27.238466	13.483964	3.436454
-26.882368	17.156770	3.446451
-26.350451	11.865588	3.456448
-26.095809	18.649258	3.466445
-25.269478	15.998262	3.476442
-24.460814	21.190409	3.486438
-24.285931	18.197988	3.496435
-23.861549	22.813613	3.506432
-22.947047	21.520472	3.516429
-22.931708	24.372351	3.526426
-22.875038	20.403754	3.536422
-21.489115	18.815001	3.546419
-21.191279	15.923694	3.556416
-21.212022	19.180371	3.566413
-20.089782	21.177733	3.576410
-19.698453	20.372047	3.586406
-19.398082	18.861515	3.596403
-18.732508	20.233507	3.606400
-18.344577	19.140081	3.616397
-17.676921	15.924732	3.626394
-17.091287	16.048454	3.636390
-16.678044	18.480022	3.646387
-16.620515	17.739308	3.656384
-15.815077	13.770603	3.666381
-15.270634	20.011519	3.676378
-14.667571	19.454595	3.686374
-13.964647	14.481911	3.696371
-13.992306	15.886493	3.706368
-13.473669	17.243493	3.716365
-12.518247	22.083193	3.726362
-12.357046	18.544882	3.736358
-11.955965	17.604620	3.746355
-11.492120	18.764297	3.756352
-10.804777	21.986058	3.766349
-9.807581	16.571288	3.776346
-9.630512	21.482258	3.786342
-9.384546	16.869443	3.796339
-9.081895	15.558128	3.806336
-8.206755	14.271156	3.816333
-8.325470	17.945498	3.826330
-7.275451	19.713423	3.836326
-6.658658	16.239946	3.846323
-6.147147	15.557982	3.856320
-5.283632	19.715161	3.866317
-5.298836	23.493663	3.876314
-5.073511	20.639060	3.886310
-4.775996	28.109772	3.896307
-4.237454	38.910129	3.906304
-3.511276	43.370769	3.916301
-3.076240	57.925398	3.926298
-2.435308	66.793189	3.936294
-1.987371	79.616175	3.946291
-1.479696	82.764729	3.956288
-0.795899	89.712440	3.966285
-0.796595	101.433634	3.976282
0.000000	112.109350	3.981286
-0.156995	113.010354	3.986291
-0.173373	111.225411	3.991296
-0.144487	119.772657	3.996301
0.166057	129.607735	4.001306
0.543408	137.809322	4.006310
0.222252	140.628000	4.011315
0.504026	132.680716	4.016320
0.587723	139.979175	4.021325
0.400519	139.492842	4.026330
0.540779	131.735413	4.031334
0.414525	134.675414	4.036339
0.582289	132.425013	4.041344
0.593044	140.753644	4.046349
0.310947	146.786951	4.051354
0.505276	132.396053	4.056358
0.318845	140.663829	4.061363
0.788980	139.698010	4.066368
0.538702	141.107184	4.071373
0.394724	133.571461	4.076378
0.569328	145.968378	4.081382
0.756006	152.244618	4.086387
0.989671	154.033555	4.091392
0.618645	161.311519	4.096397
0.542350	157.897109	4.101402
0.904252	157.081128	4.106406
0.954013	165.511228	4.111411
0.798404	149.476183	4.116416
0.845046	143.755085	4.121421
0.766961	151.002966	4.126426
0.987462	146.074052	4.131430
0.480690	147.153249	4.136435
0.885089	152.547478	4.141440
1.182750	163.472941	4.146445
1.072405	153.479994	4.151450
0.936570	146.395414	4.156454
0.602374	150.399397	4.161459
0.528231	145.257217	4.166464
0.745624	156.198416	4.171469
1.370037	161.064623	4.176474
1.052450	162.322990	4.181478
0.595918	159.920460	4.186483
0.973881	154.666311	4.191488
1.331394	169.068910	4.196493
1.097501	158.737807	4.201498
1.361114	141.406366	4.206502
1.145776	138.817350	4.211507
0.878198	149.075219	4.216512
0.508686	149.247046	4.221517
0.990735	155.353620	4.226522
1.187587	147.935335	4.231526
1.166133	172.825204	4.236531
1.079299	161.518752	4.241536
1.089555	152.174472	4.246541
0.888243	163.165459	4.251546
1.331467	161.514147	4.256550
1.333811	168.208423	4.261555
1.239080	159.174822	4.266560
0.875923	157.365112	4.271565
1.020761	163.628930	4.276570
1.443548	151.777557	4.281574
1.490235	164.425486	4.286579
1.177025	154.138451	4.291584
1.004028	156.139803	4.296589
1.374275	156.663967	4.301594
1.295739	154.512265	4.306598
1.351839	154.984408	4.311603
1.206241	146.395388	4.316608
0.756704	149.101302	4.321613
1.254664	161.586773	4.326618
1.574004	165.421923	4.331622
1.324717	174.506333	4.336627
1.438879	162.076876	4.341632
1.251079	172.866433	4.346637
1.235817	167.348020	4.351642
1.500241	159.552142	4.356646
1.255567	159.410175	4.361651
1.628170	168.741998	4.366656
1.361093	169.840589	4.371661
1.107671	173.673732	4.376666
1.340832	162.095677	4.381670
1.678949	163.785990	4.386675
1.350519	172.566419	4.391680
1.578056	166.013365	4.396685
1.425137	168.201401	4.401690
1.404249	171.359021	4.406694
1.477230	175.194808	4.411699
1.556394	169.455952	4.416704
1.521247	171.729941	4.421709
1.584114	165.107774	4.426714
1.704474	162.171923	4.431718
1.503183	170.758422	4.436723
1.655129	171.819834	4.441728
1.458371	167.263180	4.446733
1.168067	168.678627	4.451738
1.796337	175.489973	4.456742
1.196526	176.586913	4.461747
1.132944	167.488315	4.466752
1.170208	167.004776	4.471757
1.544395	186.903470	4.476762
2.262542	180.491844	4.481766
1.599302	180.542011	4.486771
1.650232	166.246321	4.491776
1.863006	176.128382	4.496781
1.610414	174.652530	4.501786
1.879361	174.338338	4.506790
1.829730	177.253686	4.511795
1.810431	165.857555	4.516800
1.690047	171.004978	4.521805
1.992605	179.651745	4.526810
1.686560	172.201511	4.531814
1.887541	174.552401	4.536819
1.919625	175.202316	4.541824
1.625185	166.003846	4.546829
1.798403	174.952454	4.551834
2.240481	181.821450	4.556838
1.549126	177.370762	4.561843
1.997905	184.570908	4.566848
2.091661	190.849066	4.571853
1.758983	193.318374	4.576858
1.982413	185.535235	4.581862
1.975008	189.408930	4.586867
2.096030	187.510701	4.591872
2.153278	196.202239	4.596877
1.990505	184.407789	4.601882
1.649615	171.109974	4.606886
1.455919	174.592068	4.611891
2.100980	179.154483	4.616896
2.055672	187.159720	4.621901
1.776699	188.443677	4.626906
2.030382	183.892374	4.631910
1.828729	191.055226	4.636915
2.243569	191.240204	4.641920
2.099074	190.959152	4.646925
2.105639	188.996597	4.651930
2.183269	186.969122	4.656934
1.947348	189.919988	4.661939
2.163208	188.908584	4.666944
2.093302	189.023977	4.671949
2.018668	197.524204	4.676954
2.017597	188.086765	4.681958
2.213108	194.725474	4.686963
1.901431	191.243532	4.691968
2.093807	196.212243	4.696973
2.248694	193.967015	4.701978
2.313597	185.632901	4.706982
2.301036	191.234843	4.711987
2.440602	187.656890	4.716992
2.236952	187.226917	4.721997
1.837195	198.097156	4.727002
2.086335	204.132669	4.732006
2.374904	211.788207	4.737011
2.513386	204.584692	4.742016
2.592357	209.960324	4.747021
2.517306	209.851892	4.752026
2.088692	191.951805	4.757030
2.282480	199.460833	4.762035
2.408899	214.880459	4.767040
2.552703	213.772774	4.772045
2.391486	217.749670	4.777050
2.528465	213.552010	4.782054
2.442205	207.962448	4.787059
2.662558	206.978814	4.792064
2.437671	199.664552	4.797069
2.316713	211.538338	4.802074
2.726658	211.426684	4.807078
2.641762	212.123403	4.812083
2.391235	196.644199	4.817088
2.531269	209.084542	4.822093
2.416470	214.648726	4.827098
2.702569	213.509254	4.832102
2.212099	220.603473	4.837107
2.506242	217.324004	4.842112
2.112983	222.280074	4.847117
2.063558	216.842929	4.852122
2.579927	212.690231	4.857126
2.462801	218.615455	4.862131
2.628191	218.972398	4.867136
2.559750	211.864577	4.872141
2.657258	219.654459	4.877146
2.832386	216.200645	4.882150
2.684137	218.277222	4.887155
2.621163	216.116747	4.892160
2.499884	223.051879	4.897165
2.179673	216.679544	4.902170
2.767429	220.830161	4.907174
2.419976	229.670547	4.912179
2.544253	232.634587	4.917184
2.769582	238.009442	4.922189
2.727307	238.016100	4.927194
3.034282	228.603143	4.932198
3.055364	238.382393	4.937203
3.056672	237.490025	4.942208
2.960770	236.163628	4.947213
2.545579	235.621262	4.952218
3.288407	237.368397	4.957222
2.972911	242.809008	4.962227
3.165555	236.299361	4.967232
3.205163	230.699563	4.972237
2.861113	226.077385	4.977242
2.718451	215.905965	4.982246
2.577793	227.479121	4.987251
3.078807	234.509749	4.992256
3.238465	239.034336	4.997261
2.971134	243.211365	5.002266
3.083228	245.864099	5.007270
2.750916	244.378584	5.012275
3.192642	241.654966	5.017280
3.396489	241.066229	5.022285
2.857449	232.418588	5.027290
3.220552	233.715844	5.032294
2.934060	247.460094	5.037299
2.943024	236.407510	5.042304
3.137607	241.255662	5.047309
3.114580	234.311563	5.052314
3.259664	234.076890	5.057318
3.113078	237.548451	5.062323
3.193783	226.794686	5.067328
3.227827	231.895784	5.072333
2.955425	247.931593	5.077338
2.880619	240.679223	5.082342
3.097556	246.314828	5.087347
2.970097	246.296867	5.092352
3.108099	248.638651	5.097357
3.251509	242.737842	5.102362
3.068124	244.266259	5.107366
3.243519	243.283339	5.112371
3.051740	245.721087	5.117376
3.239777	241.771689	5.122381
3.372466	251.305665	5.127386
3.190330	233.167597	5.132390
3.017294	256.274794	5.137395
3.248139	242.678532	5.142400
3.287811	249.613767	5.147405
3.330860	250.651117	5.152410
3.170001	248.116825	5.157414
3.164339	257.087174	5.162419
3.712168	267.919720	5.167424
3.610807	267.853376	5.172429
3.356506	262.065496	5.177434
3.445106	249.687441	5.182438
3.452379	251.888353	5.187443
3.670437	250.133104	5.192448
3.748477	247.501270	5.197453
2.969578	252.457658	5.202458
3.202956	257.185838	5.207462
3.606592	264.763257	5.212467
3.747386	264.095812	5.217472
3.833353	263.636278	5.222477
3.476349	260.455660	5.227482
3.446233	256.315808	5.232486
3.713600	264.316383	5.237491
3.650984	251.354565	5.242496
3.257289	257.604715	5.247501
3.568382	258.843682	5.252506
3.900232	255.909482	5.257510
3.897169	262.902039	5.262515
3.627012	257.493139	5.267520
3.665631	257.733900	5.272525
3.132971	260.145964	5.277530
3.267727	266.189930	5.282534
3.583036	273.157919	5.287539
3.762783	269.697043	5.292544
3.995081	270.578189	5.297549
3.577047	270.782929	5.302554
3.768311	267.892901	5.307558
3.518454	280.900594	5.312563
3.383894	272.765374	5.317568
3.610979	266.690092	5.322573
3.410126	284.913580	5.327578
3.772464	274.438370	5.332582
3.631427	274.963550	5.337587
3.514799	286.330495	5.342592
3.842880	286.427825	5.347597
3.773903	290.048592	5.352602
4.172526	305.507906	5.357606
4.293521	306.453950	5.362611
4.271345	288.581835	5.367616
4.214953	278.191214	5.372621
3.596676	284.014642	5.377626
3.953927	279.636918	5.382630
3.785581	278.125710	5.387635
3.960947	279.563118	5.392640
3.849978	275.534009	5.397645
3.745841	285.525897	5.402650
3.893816	287.236523	5.407654
4.011459	297.462594	5.412659
4.226900	294.290357	5.417664
4.209344	302.585533	5.422669
4.119929	305.665327	5.427674
4.371163	294.214071	5.432678
4.090408	285.535427	5.437683
3.697854	279.202877	5.442688
4.111190	281.330680	5.447693
4.067529	290.974566	5.452698
4.241643	299.423212	5.457702
3.989488	299.212812	5.462707
3.943284	298.707546	5.467712
4.318840	294.630677	5.472717
4.123684	308.541002	5.477722
4.257963	297.513039	5.482726
4.106159	308.841216	5.487731
3.670991	313.269190	5.492736
4.103878	305.266515	5.497741
4.034158	308.014185	5.502746
4.138285	300.635676	5.507750
4.037891	297.345241	5.512755
4.192156	296.776926	5.517760
4.209046	300.131135	5.522765
4.000588	306.523125	5.527770
4.370566	299.011212	5.532774
4.277269	301.057042	5.537779
4.500177	296.469403	5.542784
4.516954	291.037682	5.547789
4.445359	306.333384	5.552794
4.507845	301.976528	5.557798
4.092667	305.265554	5.562803
4.303072	297.142714	5.567808
4.178823	297.570349	5.572813
4.357105	313.991195	5.577818
4.524767	314.312981	5.582822
4.358465	313.649357	5.587827
4.744383	316.107334	5.592832
5.068750	305.609581	5.597837
4.159651	304.632059	5.602842
4.324353	300.787547	5.607846
4.200274	303.663959	5.612851
4.325610	304.514408	5.617856
4.590031	309.611071	5.622861
4.435743	324.404040	5.627866
4.483986	319.777322	5.632870
4.667175	318.875436	5.637875
4.481465	323.118791	5.642880
4.931445	317.201562	5.647885
4.694038	319.254154	5.652890
4.742049	321.958069	5.657894
4.677992	328.185070	5.662899
4.800986	324.277483	5.667904
4.991548	316.141925	5.672909
4.691949	314.031168	5.677914
4.569048	299.743625	5.682918
4.667382	314.683671	5.687923
4.283542	310.877646	5.692928
4.547494	313.262981	5.697933
4.831243	317.258769	5.702938
4.532380	317.970034	5.707942
4.791612	315.632510	5.712947
4.472888	325.806743	5.717952
4.619002	323.730557	5.722957
4.630390	325.212644	5.727962
5.014064	319.710773	5.732966
5.009754	329.411792	5.737971
5.110451	326.105663	5.742976
5.281079	329.938839	5.747981
5.091664	327.858274	5.752986
4.951106	314.117665	5.757990
4.796814	322.912013	5.762995
4.885150	325.869045	5.768000
5.164725	320.617608	5.773005
4.749975	327.769610	5.778010
4.978216	318.742273	5.783014
5.008586	326.039672	5.788019
4.827016	326.080810	5.793024
4.905806	321.734050	5.798029
4.501539	320.797655	5.803034
5.089911	323.945266	5.808038
4.796190	332.827905	5.813043
5.040900	326.056962	5.818048
5.086873	321.892518	5.823053
4.821404	329.207796	5.828058
4.798836	323.921439	5.833062
4.882981	331.185104	5.838067
5.009611	330.519876	5.843072
4.940389	332.486005	5.848077
4.896914	326.092417	5.853082
5.057972	334.043239	5.858086
5.201217	338.348955	5.863091
5.031232	341.185108	5.868096
5.110166	351.575467	5.873101
4.923312	349.092691	5.878106
4.931428	343.814176	5.883110
4.887386	348.854773	5.888115
5.263692	345.644667	5.893120
5.232199	345.545229	5.898125
5.078071	343.924218	5.903130
5.327726	345.289879	5.908134
5.321229	348.850247	5.913139
5.057961	345.325887	5.918144
5.497835	345.029205	5.923149
5.039044	352.488681	5.928154
5.614248	353.648307	5.933158
4.933546	345.680884	5.938163
4.862690	348.552128	5.943168
5.490824	349.007417	5.948173
5.027512	354.778113	5.953178
5.091362	350.269167	5.958182
5.365926	369.418025	5.963187
5.372288	370.650960	5.968192
5.473503	368.670392	5.973197
5.538716	372.808003	5.978202
5.782021	370.779860	5.983206
5.336370	364.835260	5.988211
5.284810	360.018519	5.993216
5.464316	363.049860	5.998221
5.253110	375.149872	6.003226
5.455591	365.066661	6.008230
5.770544	375.973727	6.013235
5.703707	371.450449	6.018240
5.680611	351.553558	6.023245
5.215494	352.350986	6.028250
5.396746	349.959236	6.033254
5.351665	354.072993	6.038259
5.476511	347.535963	6.043264
5.673089	344.964637	6.048269
5.164541	355.152809	6.053274
5.482488	340.543053	6.058278
5.359614	342.296121	6.063283
5.411874	346.372479	6.068288
5.541980	345.624446	6.073293
5.249956	361.198347	6.078298
5.395091	359.362762	6.083302
5.451374	365.694311	6.088307
5.590215	370.010215	6.093312
5.626874	370.523376	6.098317
5.273983	366.193619	6.103322
5.570905	352.859011	6.108326
5.398083	356.863067	6.113331
5.339363	353.490160	6.118336
5.412551	361.207982	6.123341
5.608624	359.861139	6.128346
5.345227	357.453632	6.133350
5.178355	358.571336	6.138355
5.524476	368.948317	6.143360
5.731823	359.433838	6.148365
5.344328	363.148819	6.153370
5.520883	354.914194	6.158374
5.404770	354.948241	6.163379
5.697195	349.748567	6.168384
5.431455	344.085842	6.173389
5.298251	339.674214	6.178394
5.255414	341.231239	6.183398
5.730785	353.422984	6.188403
5.630826	355.270541	6.193408
5.460996	347.710304	6.198413
5.261093	337.848347	6.203418
5.533214	337.846875	6.208422
5.470206	340.261296	6.213427
5.211411	334.012176	6.218432
5.395793	338.880936	6.223437
5.513208	350.638369	6.228442
5.755099	336.417030	6.233446
5.629975	337.948982	6.238451
5.270553	335.091439	6.243456
5.603507	335.748005	6.248461
5.380786	335.896833	6.253466
5.671143	342.131586	6.258470
5.651187	340.847066	6.263475
5.246654	340.869353	6.268480
5.157480	336.384387	6.273485
5.019592	345.631768	6.278490
5.115998	339.317501	6.283494
5.605797	350.978624	6.288499
5.521646	347.606538	6.293504
5.729161	342.907401	6.298509
5.150459	346.184089	6.303514
5.606942	343.572041	6.308518
5.361667	351.488457	6.313523
5.303618	348.061660	6.318528
5.734718	355.872103	6.323533
5.441381	356.902051	6.328538
5.307861	335.522820	6.333542
5.437957	344.452959	6.338547
5.560945	353.861956	6.343552
5.853194	332.276810	6.348557
5.434944	339.559081	6.353562
5.737836	342.827357	6.358566
5.510123	348.238427	6.363571
5.249233	349.829617	6.368576
5.227855	350.747350	6.373581
5.147873	347.191108	6.378586
5.324157	346.366236	6.383590
5.358318	351.875484	6.388595
5.499092	364.986553	6.393600
5.671465	370.695621	6.398605
5.341363	364.995516	6.403610
5.491260	345.909944	6.408614
5.240866	348.182878	6.413619
5.356806	362.246987	6.418624
5.689291	366.418652	6.423629
5.500776	365.970484	6.428634
5.442195	353.305361	6.433638
5.492248	353.212129	6.438643
5.487552	347.590761	6.443648
5.475321	347.595876	6.448653
5.363439	350.328012	6.453658
5.702951	338.299734	6.458662
5.904385	341.039726	6.463667
5.412957	347.029966	6.468672
5.506225	339.482295	6.473677
5.517236	349.873804	6.478682
5.260744	342.668842	6.483686
5.234556	347.839523	6.488691
5.260467	344.741266	6.493696
5.339835	341.814973	6.498701
4.871396	353.120020	6.503706
5.294763	354.075640	6.508710
5.304359	367.510993	6.513715
5.480143	371.333878	6.518720
5.639682	364.297847	6.523725
5.707876	376.423687	6.528730
5.703711	363.946189	6.533734
5.504641	351.129068	6.538739
5.322115	344.282685	6.543744
5.346137	347.752847	6.548749
5.395594	357.005683	6.553754
5.548743	359.531775	6.558758
5.665155	351.619796	6.563763
5.460892	351.335450	6.568768
5.385535	347.114079	6.573773
5.283871	346.791511	6.578778
5.465780	348.022251	6.583782
5.440449	343.324794	6.588787
5.714707	346.132473	6.593792
5.322330	338.366657	6.598797
5.138793	348.779156	6.603802
5.469301	355.615079	6.608806
5.685501	364.234336	6.613811
5.776746	350.216928	6.618816
5.655618	343.541264	6.623821
5.105428	348.594725	6.628826
5.651173	339.356275	6.633830
5.174775	334.172660	6.638835
5.563365	340.088292	6.643840
5.504308	342.109779	6.648845
5.302145	349.858084	6.653850
5.390579	340.602698	6.658854
5.516937	338.982034	6.663859
5.605673	337.063537	6.668864
5.367403	333.975036	6.673869
5.207118	345.095752	6.678874
5.532363	343.143361	6.683878
5.349538	342.045715	6.688883
5.279392	349.507573	6.693888
5.722764	346.935545	6.698893
5.593865	358.592368	6.703898
5.431043	348.392392	6.708902
5.631990	345.238235	6.713907
5.459471	340.911863	6.718912
5.374767	338.859184	6.723917
5.327990	348.513082	6.728922
5.180343	336.073903	6.733926
5.527777	343.824681	6.738931
5.437866	352.188167	6.743936
5.876195	342.321123	6.748941
5.021074	348.836595	6.753946
5.338401	346.626010	6.758950
5.486664	341.325537	6.763955
5.196926	345.243502	6.768960
5.597407	357.421673	6.773965
5.666183	358.296806	6.778970
5.395939	349.195693	6.783974
5.296464	341.491554	6.788979
4.969505	348.604498	6.793984
5.380719	359.917261	6.798989
5.309909	373.428493	6.803994
5.509368	374.109140	6.808998
5.713446	373.922171	6.814003
5.730670	373.818263	6.819008
5.346160	365.984762	6.824013
5.357714	375.075863	6.829018
5.792674	373.232832	6.834022
5.721627	361.249883	6.839027
5.090203	350.009656	6.844032
5.434084	350.272194	6.849037
5.330737	355.891576	6.854042
5.477745	361.898852	6.859046
5.624004	356.098802	6.864051
5.552771	349.639951	6.869056
5.597611	342.805402	6.874061
5.544450	348.486523	6.879066
5.519892	343.102393	6.884070
5.594793	340.739962	6.889075
5.317032	352.037280	6.894080
5.444115	341.668496	6.899085
5.411911	346.640798	6.904090
5.354625	348.769578	6.909094
5.521892	345.804201	6.914099
5.509182	345.910633	6.919104
5.574433	342.461355	6.924109
5.411961	342.290687	6.929114
5.790537	339.905987	6.934118
5.488794	329.420896	6.939123
5.622930	344.004172	6.944128
5.569477	339.111801	6.949133
5.538742	347.367934	6.954138
5.622996	347.117479	6.959142
6.144886	340.739711	6.964147
5.774192	346.904028	6.969152
5.846644	339.783573	6.974157
5.320053	334.766013	6.979162
5.078062	331.178209	6.984166
5.279585	324.296971	6.989171
5.208296	346.062697	6.994176
5.403819	340.881373	6.999181
5.678123	342.524753	7.004186
5.444342	351.916879	7.009190
5.683503	347.877188	7.014195
5.396712	351.266332	7.019200
5.639574	346.691374	7.024205
5.493068	339.051554	7.029210
5.356158	337.544907	7.034214
5.622498	319.706652	7.039219
4.946634	321.805795	7.044224
5.120685	333.171520	7.049229
5.234373	349.162746	7.054234
5.216335	340.180313	7.059238
5.318094	338.398984	7.064243
5.087193	344.392698	7.069248
5.471498	337.201235	7.074253
5.264525	347.487687	7.079258
5.499373	343.489803	7.084262
5.361832	346.032965	7.089267
5.354979	341.506624	7.094272
5.594813	346.850765	7.099277
5.146323	351.091006	7.104282
5.264010	347.282325	7.109286
5.659432	345.755548	7.114291
5.449220	347.927271	7.119296
5.360926	345.758093	7.124301
5.354556	347.562512	7.129306
5.125154	347.984477	7.134310
5.476725	339.089671	7.139315
5.077520	348.627940	7.144320
5.650944	353.777443	7.149325
5.580434	355.313494	7.154330
5.605451	348.209959	7.159334
5.371358	345.563739	7.164339
4.993403	355.737777	7.169344
5.478198	360.882186	7.174349
5.686831	368.325683	7.179354
5.646024	365.608045	7.184358
5.342707	348.184891	7.189363
5.146653	349.939935	7.194368
5.646886	354.037856	7.199373
5.385870	356.524433	7.204378
5.235104	356.763231	7.209382
5.639364	363.527488	7.214387
5.221712	365.108439	7.219392
5.747096	365.902539	7.224397
5.454825	365.445317	7.229402
5.307749	344.783226	7.234406
5.584299	350.517095	7.239411
5.568484	359.194849	7.244416
5.510009	344.599775	7.249421
5.297652	346.983811	7.254426
5.079868	339.405780	7.259430
5.606784	353.446620	7.264435
5.444977	361.603070	7.269440
6.019171	364.569407	7.274445
5.196022	357.788590	7.279450
5.193800	353.657001	7.284454
5.403952	347.758355	7.289459
5.777055	358.681609	7.294464
5.513279	344.583786	7.299469
5.508696	346.890975	7.304474
5.444842	344.771752	7.309478
5.674645	341.850363	7.314483
5.365799	342.781497	7.319488
5.262871	342.626811	7.324493
5.239796	349.942086	7.329498
5.098704	348.860048	7.334502
5.466810	357.756065	7.339507
5.436471	362.645820	7.344512
5.952802	376.827545	7.349517
5.580710	368.621928	7.354522
5.338595	353.049518	7.359526
5.565399	346.468039	7.364531
5.385838	344.635872	7.369536
5.527387	336.023917	7.374541
5.272093	344.878395	7.379546
5.200668	345.240806	7.384550
5.304835	342.933902	7.389555
5.735330	347.232579	7.394560
5.487649	344.936509	7.399565
5.305348	349.014817	7.404570
5.465902	347.888680	7.409574
5.477633	336.667917	7.414579
5.355588	348.779252	7.419584
5.359951	336.199194	7.424589
5.804691	349.348049	7.429594
5.641661	344.713297	7.434598
5.438365	340.135476	7.439603
5.282878	348.097935	7.444608
5.526183	339.416250	7.449613
5.542089	345.599090	7.454618
5.638290	346.346536	7.459622
5.712408	342.547846	7.464627
5.915278	346.923317	7.469632
5.679945	345.900339	7.474637
6.012550	343.823406	7.479642
5.862605	340.056659	7.484646
6.003016	329.429523	7.489651
5.435097	321.226135	7.494656
5.476476	321.099461	7.499661
5.307013	327.827042	7.504666
5.270560	318.550106	7.509670
5.574457	313.797909	7.514675
5.122197	318.282348	7.519680
5.299071	313.271636	7.524685
5.355415	330.426628	7.529690
5.469735	335.284218	7.534694
5.710422	336.989814	7.539699
5.339189	330.498878	7.544704
5.415526	318.397950	7.549709
5.290485	322.340726	7.554714
4.939337	337.487262	7.559718
5.376843	334.628246	7.564723
5.460520	340.253122	7.569728
5.709020	340.068685	7.574733
5.712970	347.841644	7.579738
5.663297	342.470940	7.584742
5.742789	324.918226	7.589747
5.202121	324.449302	7.594752
5.315596	318.119714	7.599757
5.275902	332.704906	7.604762
5.343938	330.125247	7.609766
5.464238	334.823708	7.614771
5.599481	342.686828	7.619776
5.448914	341.454411	7.624781
5.407590	343.204193	7.629786
5.410683	335.309976	7.634790
5.487735	332.295459	7.639795
5.628401	341.116370	7.644800
5.376070	333.743076	7.649805
5.386241	327.144925	7.654810
5.555739	339.033399	7.659814
5.685834	325.000432	7.664819
5.306725	327.394774	7.669824
5.231739	314.491798	7.674829
5.204139	326.781313	7.679834
5.042037	326.085392	7.684838
5.658007	332.841778	7.689843
5.356509	342.896259	7.694848
5.831854	340.547018	7.699853
5.619043	339.330681	7.704858
5.756752	340.546199	7.709862
5.502659	331.546971	7.714867
5.468887	330.210831	7.719872
5.433167	314.530185	7.724877
5.157912	332.189562	7.729882
5.272035	330.573979	7.734886
5.539030	340.824132	7.739891
5.428919	348.599144	7.744896
5.531896	342.448366	7.749901
5.367849	341.778060	7.754906
5.302654	352.428289	7.759910
5.453544	342.302553	7.764915
5.606573	346.783913	7.769920
5.732801	339.841698	7.774925
5.606774	336.741938	7.779930
5.405446	320.501925	7.784934
5.276609	312.935279	7.789939
4.964159	324.294964	7.794944
5.402287	334.999203	7.799949
5.472220	341.072334	7.804954
5.118545	337.666547	7.809958
5.358529	336.913954	7.814963
5.727363	343.069970	7.819968
5.554247	343.154077	7.824973
5.344361	348.321902	7.829978
5.494064	343.144593	7.834982
6.028830	335.265151	7.839987
5.704517	333.006400	7.844992
5.137467	330.792010	7.849997
5.122462	323.685264	7.855002
5.388311	334.296269	7.860006
5.340598	334.661293	7.865011
5.495977	331.653487	7.870016
5.716324	335.839551	7.875021
5.787121	338.467131	7.880026
5.246628	327.775833	7.885030
5.243708	313.023380	7.890035
5.053851	330.495364	7.895040
5.730596	337.596578	7.900045
5.458984	333.377485	7.905050
5.475478	343.318866	7.910054
5.994901	341.658763	7.915059
5.518953	329.350123	7.920064
5.379643	325.774707	7.925069
5.665139	323.274876	7.930074
5.184752	323.280574	7.935078
5.334250	310.143107	7.940083
5.228842	316.237374	7.945088
5.398317	317.441585	7.950093
5.674223	329.829085	7.955098
5.632844	325.896631	7.960102
5.710245	315.744459	7.965107
5.435583	319.555650	7.970112
5.448564	313.131074	7.975117
5.410461	305.651458	7.980122
5.389332	314.407965	7.985139
5.460009	309.846321	7.990157
5.215930	324.524167	7.995174
5.351322	321.748009	8.000192
5.300361	319.007361	8.005210
5.549503	331.686077	8.010227
5.811979	324.973706	8.015245
5.147654	324.348847	8.020262
5.529894	316.137663	8.025280
5.382078	322.163113	8.030298
5.687850	324.327427	8.035315
5.566960	326.160965	8.040333
5.230534	329.887018	8.045350
5.584868	323.545258	8.050368
5.470665	339.405112	8.055386
5.528692	344.303268	8.060403
5.963347	338.718924	8.065421
5.824124	335.048529	8.070438
5.578058	324.802489	8.075456
5.329701	324.705739	8.080474
5.188723	316.627025	8.085491
5.698509	306.978925	8.090509
5.032218	325.058561	8.095526
5.485696	324.208071	8.100544
5.535707	334.008377	8.105562
5.060741	342.748556	8.110579
5.543534	344.061482	8.115597
5.640220	344.847932	8.120614
5.590581	345.458495	8.125632
5.432462	338.054635	8.130650
5.338775	340.066947	8.135667
5.773681	337.404802	8.140685
5.203356	344.427408	8.145702
5.508120	340.258264	8.150720
5.572407	343.126283	8.155738
5.911528	349.444673	8.160755
6.158099	341.579778	8.165773
5.646816	348.031409	8.170790
5.403343	337.308435	8.175808
5.731870	343.625327	8.180826
5.597401	340.295008	8.185843
5.481858	340.852782	8.190861
5.837570	344.385187	8.195878
5.962022	337.590297	8.200896
6.057007	336.855935	8.205914
5.857348	344.035057	8.210931
6.084218	343.248473	8.215949
6.042216	342.068521	8.220966
5.938467	328.029043	8.225984
5.776237	327.347605	8.231002
5.572835	315.469669	8.236019
5.737166	310.255888	8.241037
5.415993	306.165890	8.246054
5.191751	310.066862	8.251072
5.224949	326.307547	8.256090
5.120946	339.748490	8.261107
5.705701	334.068048	8.266125
5.586749	339.303196	8.271142
6.059312	344.597144	8.276160
5.693025	339.545386	8.281178
5.647412	342.162384	8.286195
6.003499	339.809230	8.291213
6.054485	345.090337	8.296230
6.128773	342.939123	8.301248
6.188645	332.373749	8.306266
5.715223	337.595008	8.311283
5.904606	338.789806	8.316301
5.725081	338.237308	8.321318
5.914444	333.048001	8.326336
6.005284	337.180475	8.331354
5.761852	342.643408	8.336371
5.879963	338.468796	8.341389
5.901183	336.496309	8.346406
5.573096	334.673225	8.351424
5.648395	334.137605	8.356442
5.727273	341.216281	8.361459
5.826814	335.009111	8.366477
5.540369	333.170036	8.371494
5.816037	345.453291	8.376512
5.755612	343.017075	8.381530
5.574331	347.047022	8.386547
5.700353	339.466100	8.391565
5.591500	346.122918	8.396582
5.642575	337.954144	8.401600
5.780024	341.126275	8.406618
5.322802	342.633820	8.411635
5.846070	349.475616	8.416653
6.001512	358.615641	8.421670
5.966568	353.808606	8.426688
5.910674	346.379259	8.431706
5.752535	352.501009	8.436723
6.182371	355.270730	8.441741
6.006086	348.879558	8.446758
5.718391	346.542066	8.451776
5.875603	348.076416	8.456794
5.932314	365.238091	8.461811
6.124961	355.623876	8.466829
6.007899	355.153108	8.471846
5.833130	353.435386	8.476864
5.990396	351.649863	8.481882
5.637989	351.588349	8.486899
5.812022	353.514535	8.491917
6.066048	350.432610	8.496934
5.988060	362.572475	8.501952
5.909676	360.094890	8.506970
6.294220	370.395061	8.511987
6.182959	364.530175	8.517005
6.051539	363.234845	8.522022
5.971079	371.544002	8.527040
6.243160	361.462907	8.532058
5.812453	366.876296	8.537075
6.338823	359.598707	8.542093
5.751954	358.819701	8.547110
5.875202	360.425645	8.552128
6.284924	353.336747	8.557146
6.067181	373.135471	8.562163
6.186028	359.783763	8.567181
6.338835	367.772351	8.572199
6.012039	353.518494	8.577216
5.924590	342.840498	8.582234
5.916203	358.128375	8.587251
6.061710	367.872712	8.592269
5.984103	359.130806	8.597287
5.815916	372.076907	8.602304
6.215703	369.230914	8.607322
6.045963	370.084355	8.612339
6.121452	362.962615	8.617357
6.269273	366.581245	8.622375
6.013505	371.029963	8.627392
6.278457	369.426379	8.632410
5.784929	375.259863	8.637427
6.035906	369.069979	8.642445
6.487015	362.261768	8.647463
5.969145	368.187426	8.652480
6.184927	369.027799	8.657498
6.390194	367.136924	8.662515
6.202419	352.902312	8.667533
6.203275	361.902459	8.672551
6.071448	371.481970	8.677568
6.219561	365.314517	8.682586
6.128319	366.288200	8.687603
6.344755	355.546805	8.692621
6.526002	360.599226	8.697639
6.161437	367.299272	8.702656
6.205165	371.896722	8.707674
6.187963	367.140552	8.712691
6.114679	363.664945	8.717709
6.481589	359.145236	8.722727
6.536599	366.439098	8.727744
6.336228	358.559017	8.732762
6.097917	365.122517	8.737779
6.516981	372.100568	8.742797
6.207587	352.368727	8.747815
6.153364	358.505756	8.752832
6.324576	367.573887	8.757850
6.688637	366.185146	8.762867
6.543553	353.045207	8.767885
6.344369	345.572040	8.772903
5.993824	344.995845	8.777920
6.351099	342.194386	8.782938
5.765648	348.856452	8.787955
5.995595	370.598407	8.792973
6.314302	360.380621	8.797991
6.147165	368.656020	8.803008
6.455012	366.458743	8.808026
6.494657	376.869760	8.813043
6.623617	376.041711	8.818061
6.429697	369.173617	8.823079
6.446912	373.712106	8.828096
6.695291	367.367998	8.833114
6.285439	359.754265	8.838131
6.462345	352.938528	8.843149
6.388615	345.003897	8.848167
6.113394	355.391653	8.853184
6.479326	358.180854	8.858202
6.200649	363.065499	8.863219
6.517525	366.143251	8.868237
6.630420	365.551247	8.873255
6.496160	374.215969	8.878272
6.464075	367.758015	8.883290
6.311539	368.239535	8.888307
6.208814	363.067582	8.893325
6.666823	369.215874	8.898343
6.165337	363.992791	8.903360
6.594384	364.275892	8.908378
6.637971	368.942790	8.913395
6.285923	366.662715	8.918413
6.606305	368.079984	8.923431
6.186002	367.025574	8.928448
6.581231	369.658710	8.933466
6.430613	375.078709	8.938483
6.259269	372.290643	8.943501
6.732684	358.542559	8.948519
6.493721	371.121057	8.953536
6.485062	373.893213	8.958554
6.714347	377.483303	8.963571
6.402442	371.119682	8.968589
6.716994	352.517675	8.973607
6.351536	363.143633	8.978624
6.517412	366.399677	8.983642
6.348483	373.122721	8.988659
6.567283	365.145403	8.993677
6.719904	365.373986	8.998695
6.704037	376.996049	9.003712
6.266484	362.279862	9.008730
6.663409	364.089076	9.013747
6.307313	362.626979	9.018765
6.381358	362.675372	9.023783
6.528626	375.534181	9.028800
6.295015	361.568672	9.033818
6.519278	368.564620	9.038835
6.302668	378.605538	9.043853
6.654928	360.789712	9.048871
5.987218	373.993959	9.053888
6.527937	375.906876	9.058906
6.713047	389.072186	9.063923
6.814906	388.718594	9.068941
6.931301	395.898709	9.073959
6.537071	392.145182	9.078976
6.773884	390.309322	9.083994
6.887265	383.396230	9.089011
6.373780	380.977347	9.094029
6.965735	381.667264	9.099047
6.645928	379.978577	9.104064
6.751838	378.800693	9.109082
6.558021	371.938894	9.114099
6.223900	388.817848	9.119117
6.751515	395.747343	9.124135
6.390659	398.240174	9.129152
6.459194	395.821615	9.134170
6.836597	395.790919	9.139187
6.755646	413.857827	9.144205
6.911423	396.214761	9.149223
6.988036	400.115951	9.154240
6.749579	396.697775	9.159258
7.001003	400.533707	9.164275
6.717754	406.854957	9.169293
7.127494	400.801132	9.174311
6.746936	396.247051	9.179328
7.036452	399.032453	9.184346
6.932840	400.557181	9.189363
6.611307	404.031609	9.194381
6.983970	404.705394	9.199399
6.733821	405.833365	9.204416
7.167086	401.107591	9.209434
7.112865	392.898486	9.214451
6.712997	383.938819	9.219469
6.941884	371.627044	9.224487
6.435682	367.057943	9.229504
6.851582	383.361793	9.234522
6.996221	394.845111	9.239539
6.798369	399.477263	9.244557
6.850611	389.402195	9.249575
7.078209	407.285054	9.254592
6.619191	403.601635	9.259610
7.088036	395.357911	9.264627
7.115492	392.257830	9.269645
7.016400	385.172903	9.274663
6.921355	378.339806	9.279680
6.803503	361.254037	9.284698
6.809436	366.308682	9.289715
6.935239	381.641825	9.294733
6.731795	378.622105	9.299751
7.208015	387.522539	9.304768
7.004528	389.296442	9.309786
6.659592	386.276799	9.314803
6.908188	393.628703	9.319821
6.957575	392.046268	9.324839
6.742157	397.561633	9.329856
6.787316	398.229927	9.334874
6.672326	400.892517	9.339891
6.267767	399.816704	9.344909
6.859394	395.596289	9.349927
6.566163	400.906098	9.354944
6.579344	406.234171	9.359962
6.998718	417.945855	9.364979
7.002034	424.809187	9.369997
7.564504	417.046241	9.375015
7.130548	425.527573	9.380032
7.275331	428.802711	9.385050
6.957685	420.221460	9.390067
6.767050	411.490926	9.395085
7.013454	420.657756	9.400103
7.293168	426.565763	9.405120
6.877108	429.865659	9.410138
7.142410	427.779181	9.415155
6.898058	419.025502	9.420173
7.293266	418.919434	9.425191
7.361163	428.054276	9.430208
7.113303	422.034050	9.435226
7.597822	416.479740	9.440243
7.282676	417.024608	9.445261
6.962222	410.848504	9.450279
7.040174	404.366985	9.455296
6.872830	406.419247	9.460314
7.252413	411.450074	9.465331
7.069307	429.185867	9.470349
7.516937	422.703224	9.475367
7.371908	410.951777	9.480384
7.329135	407.032728	9.485402
7.103821	395.306493	9.490419
7.216009	394.203363	9.495437
7.050820	394.301862	9.500455
7.183962	401.378372	9.505472
6.715758	405.364925	9.510490
7.199171	413.794035	9.515507
7.098583	418.262631	9.520525
7.226746	428.448372	9.525543
7.268307	425.608005	9.530560
7.095720	424.448507	9.535578
7.236164	419.490900	9.540595
7.371028	425.907591	9.545613
7.436123	419.882513	9.550631
7.331575	420.924556	9.555648
6.849084	425.869553	9.560666
6.969140	421.445311	9.565683
7.195626	428.065396	9.570701
7.592876	423.020214	9.575719
7.390553	421.609758	9.580736
7.155983	433.105179	9.585754
7.435054	425.957829	9.590771
7.273102	425.790736	9.595789
7.200655	422.567448	9.600807
7.324228	426.306653	9.605824
7.362873	423.520392	9.610842
7.742233	422.788807	9.615859
7.488161	423.412468	9.620877
7.656334	429.997510	9.625895
7.460015	426.424404	9.630912
7.289396	422.613744	9.635930
7.485624	416.328282	9.640947
7.165755	422.895115	9.645965
7.331677	425.633615	9.650983
7.262474	421.273739	9.656000
7.111809	422.506042	9.661018
7.106943	426.896527	9.666035
7.246347	421.449936	9.671053
6.958701	422.009431	9.676071
7.424191	437.387229	9.681088
6.961280	447.267962	9.686106
7.594280	445.287971	9.691123
7.646780	447.971662	9.696141
7.561648	441.219038	9.701159
7.676480	437.183771	9.706176
7.507160	453.891800	9.711194
7.831489	446.775220	9.716211
7.732307	446.503618	9.721229
7.744207	440.695149	9.726247
7.369827	429.774881	9.731264
7.528632	434.761412	9.736282
7.608413	420.554252	9.741299
7.677210	420.824371	9.746317
7.421995	431.654001	9.751335
7.434451	428.587822	9.756352
7.363851	442.219267	9.761370
7.638891	445.489779	9.766387
7.917426	458.466935	9.771405
7.773268	441.975343	9.776423
7.620963	438.351157	9.781440
7.623487	436.952785	9.786458
7.284982	428.990175	9.791475
7.464831	431.486654	9.796493
7.565990	451.800384	9.801511
8.170464	447.155070	9.806528
7.749246	447.710247	9.811546
7.646871	427.923796	9.816563
7.360245	423.017323	9.821581
7.399109	432.847831	9.826599
7.587012	428.015328	9.831616
7.189954	446.396882	9.836634
7.714746	446.990029	9.841651
7.694987	456.122841	9.846669
7.803043	450.226720	9.851687
7.539938	445.155610	9.856704
7.382938	448.569553	9.861722
7.529801	441.263032	9.866739
7.713879	444.721364	9.871757
7.501126	448.115641	9.876775
7.783430	449.702983	9.881792
7.283505	449.699296	9.886810
7.553116	442.420878	9.891827
7.711174	461.958850	9.896845
8.020956	458.249637	9.901863
7.886315	453.975745	9.906880
7.861164	448.419229	9.911898
8.016498	437.444363	9.916915
7.942095	453.973420	9.921933
7.319445	456.892282	9.926951
7.612425	445.472969	9.931968
7.822823	455.585881	9.936986
7.458868	459.991612	9.942003
8.413718	476.397294	9.947021
8.106428	473.002511	9.952039
8.277673	455.249667	9.957056
7.700349	443.932001	9.962074
7.683036	445.389563	9.967091
7.793557	448.477571	9.972109
7.958956	446.697076	9.977127
7.886135	443.366547	9.982144
7.879178	450.439780	9.987162
8.039603	448.975641	9.992179
7.813810	444.201641	9.997197
7.986153	455.289340	10.002215
7.827255	449.012171	10.007232
7.719625	452.579325	10.012250
8.065719	457.804760	10.017267
8.178316	456.739432	10.022285
7.685933	453.209552	10.027303
8.178619	454.656636	10.032320
7.957642	470.003163	10.037338
8.190466	469.300848	10.042355
8.095724	452.870930	10.047373
7.691265	449.235758	10.052391
7.718672	447.303315	10.057408
8.034648	467.384590	10.062426
8.427387	463.659223	10.067443
7.947173	473.034600	10.072461
7.987345	476.398721	10.077479
8.307954	472.015626	10.082496
7.668483	461.266261	10.087514
8.387413	459.320142	10.092531
8.132705	456.933286	10.097549
7.753355	453.382540	10.102567
8.119754	456.099101	10.107584
7.892092	464.267263	10.112602
8.062510	464.650848	10.117619
7.983941	468.961374	10.122637
7.739578	478.848907	10.127655
8.201753	472.392369	10.132672
7.874860	478.019898	10.137690
8.463137	468.523515	10.142707
8.102775	468.094020	10.147725
7.802055	468.898560	10.152743
8.427829	469.387524	10.157760
8.161690	465.888465	10.162778
8.278887	467.182944	10.167795
8.200468	463.061186	10.172813
7.765528	475.648372	10.177831
8.245255	471.117271	10.182848
8.158800	474.504387	10.187866
7.948277	474.294411	10.192883
8.234346	462.999245	10.197901
7.940797	472.364310	10.202919
8.147648	463.887051	10.207936
7.912740	472.630705	10.212954
8.161640	468.031630	10.217971
8.395731	480.422477	10.222989
8.209536	479.290355	10.228007
8.579462	474.527149	10.233024
8.367999	477.053388	10.238042
8.152456	472.754298	10.243059
8.705530	471.373803	10.248077
8.174019	473.530467	10.253095
8.421949	469.802541	10.258112
8.596789	466.695134	10.263130
8.406957	467.700049	10.268147
8.408685	471.104906	10.273165
8.060099	471.525629	10.278183
8.346535	469.344316	10.283200
8.478127	468.607369	10.288218
7.972197	468.408964	10.293235
8.302360	481.094027	10.298253
8.253295	494.681112	10.303271
8.436013	496.366113	10.308288
8.342924	500.177150	10.313306
8.521704	497.750771	10.318323
8.869840	495.682864	10.323341
8.174861	486.349663	10.328359
8.478160	475.272696	10.333376
8.365054	473.308617	10.338394
8.293208	484.295740	10.343411
8.304924	494.695423	10.348429
8.387717	498.011845	10.353447
8.565577	504.705849	10.358464
8.599861	499.509234	10.363482
8.770143	498.239206	10.368499
8.535603	502.394297	10.373517
8.723225	500.051739	10.378535
8.475674	494.694156	10.383552
8.443353	482.928158	10.388570
8.484948	483.016349	10.393587
8.683011	489.975425	10.398605
8.573767	484.353179	10.403623
8.698635	482.080416	10.408640
8.527247	477.663954	10.413658
8.434303	469.624981	10.418675
8.602517	475.916546	10.423693
8.557216	487.754730	10.428711
8.712286	495.717773	10.433728
8.554192	487.401824	10.438746
8.344035	480.037616	10.443763
8.721381	491.686507	10.448781
8.756949	504.259954	10.453799
8.583374	493.727904	10.458816
8.746108	495.352920	10.463834
8.303220	496.006168	10.468851
8.594768	500.511174	10.473869
8.307910	508.480349	10.478887
8.830094	500.597448	10.483904
8.923353	501.176159	10.488922
8.675294	504.541265	10.493939
8.796951	504.408629	10.498957
8.668812	502.970764	10.503975
8.397630	502.492582	10.508992
8.860767	501.391263	10.514010
8.584420	502.251946	10.519027
8.747508	499.316788	10.524045
8.574470	498.198381	10.529063
8.574951	502.171482	10.534080
8.873121	502.424600	10.539098
8.427830	505.741713	10.544115
8.648390	501.740359	10.549133
8.678147	507.526610	10.554151
8.883807	504.426991	10.559168
8.904624	505.616653	10.564186
8.591381	509.414849	10.569203
8.771734	500.847050	10.574221
8.907631	498.563090	10.579239
9.112643	503.182640	10.584256
8.809529	508.771739	10.589274
8.390436	508.714361	10.594291
8.794479	502.074418	10.599309
8.692928	514.461073	10.604327
9.111160	521.616038	10.609344
9.291505	512.634825	10.614362
8.772487	514.634903	10.619379
9.284087	506.728411	10.624397
9.102691	504.560434	10.629415
8.930749	512.382219	10.634432
9.127363	499.548395	10.639450
8.984998	512.219154	10.644467
9.164128	498.605433	10.649485
9.009384	505.209540	10.654503
9.205346	509.306649	10.659520
9.095750	510.169607	10.664538
9.038134	513.886727	10.669555
9.261155	508.389139	10.674573
9.193741	502.163889	10.679591
8.812927	499.396000	10.684608
9.086033	499.902352	10.689626
8.971690	509.614897	10.694643
9.091415	509.280593	10.699661
9.099299	504.441561	10.704679
8.754633	507.294787	10.709696
9.034830	492.762679	10.714714
8.653677	507.799821	10.719731
8.477060	501.209831	10.724749
8.561408	506.125997	10.729767
8.943588	517.313401	10.734784
9.079581	524.256969	10.739802
8.982157	532.029217	10.744819
9.331528	528.777689	10.749837
8.925329	535.250792	10.754855
9.006563	527.986075	10.759872
9.179880	534.560883	10.764890
9.239166	541.011548	10.769907
9.352824	537.184725	10.774925
9.259750	546.316447	10.779943
9.000734	537.344101	10.784960
9.141961	523.972985	10.789978
9.179070	533.677593	10.794995
9.333087	528.976604	10.800013
9.251931	531.182633	10.805031
8.888698	534.780384	10.810048
9.593568	530.138253	10.815066
9.179064	530.531435	10.820083
9.255962	533.223940	10.825101
9.178279	524.630287	10.830119
9.110535	531.908736	10.835136
9.357272	527.142727	10.840154
8.940919	529.735789	10.845171
8.965972	528.447489	10.850189
9.154578	527.562751	10.855207
9.256345	528.465178	10.860224
9.386910	530.212002	10.865242
9.233204	533.240438	10.870259
9.124946	527.788437	10.875277
9.211621	530.406826	10.880295
9.354254	544.834915	10.885312
9.557399	552.332860	10.890330
9.394548	553.743807	10.895347
9.594652	551.913682	10.900365
9.419962	538.257539	10.905383
8.980495	543.625016	10.910400
9.101234	547.898021	10.915418
9.033155	555.416372	10.920435
9.404464	565.229580	10.925453
9.375385	557.253146	10.930471
9.304047	561.442640	10.935488
9.373291	557.180959	10.940506
9.301002	552.998259	10.945523
9.469493	557.453133	10.950541
9.412070	551.794345	10.955559
9.343706	556.456742	10.960576
9.547763	556.352221	10.965594
9.659933	562.138201	10.970611
9.512245	556.556670	10.975629
9.612261	559.463307	10.980647
9.193307	558.266662	10.985664
9.650961	562.572089	10.990682
9.443357	562.942322	10.995699
9.483803	559.335248	11.000717
9.397776	563.362943	11.005735
9.449403	569.076360	11.010752
10.197131	573.980125	11.015770
9.601439	570.703093	11.020787
9.644878	557.473506	11.025805
9.266118	560.871724	11.030823
9.692939	570.543693	11.035840
9.895613	574.488287	11.040858
9.941004	563.347532	11.045875
9.808318	556.233086	11.050893
9.583570	551.717669	11.055911
9.533773	553.495910	11.060928
9.514990	547.190441	11.065946
9.562934	561.339889	11.070963
9.926738	568.825293	11.075981
10.188247	568.768575	11.080999
9.548178	557.277631	11.086016
9.847626	549.839861	11.091034
9.698152	557.891674	11.096051
9.691315	554.878989	11.101069
9.642290	560.036973	11.106087
9.883942	559.664630	11.111104
10.199546	561.016392	11.116122
9.701521	563.193066	11.121139
9.433783	556.251259	11.126157
9.946889	550.903867	11.131175
9.780393	566.027346	11.136192
9.943302	561.738366	11.141210
9.585022	571.053664	11.146227
9.875613	575.123338	11.151245
10.074787	581.788785	11.156263
9.551325	581.754071	11.161280
9.907243	582.534629	11.166298
9.736222	576.738997	11.171315
9.415570	583.580566	11.176333
9.860541	576.861598	11.181351
9.698352	587.651500	11.186368
9.521322	585.527011	11.191386
9.834282	580.605446	11.196403
10.045391	585.233530	11.201421
9.972743	579.842206	11.206439
9.647020	580.555994	11.211456
9.997788	577.509366	11.216474
9.924109	584.454250	11.221491
10.233421	585.974258	11.226509
10.520010	574.931405	11.231527
10.048749	580.092435	11.236544
10.433343	585.813649	11.241562
10.061955	585.168128	11.246579
9.901133	582.949581	11.251597
10.237093	584.045691	11.256615
10.132588	588.852614	11.261632
10.222336	586.181397	11.266650
10.238218	583.111499	11.271667
10.166586	579.540916	11.276685
10.740412	581.407643	11.281703
10.054729	586.005824	11.286720
9.827684	580.304175	11.291738
10.026431	578.404833	11.296755
10.139374	582.215164	11.301773
10.239673	578.993184	11.306791
10.104241	581.864131	11.311808
10.383117	573.615376	11.316826
10.218556	583.155949	11.321843
10.406189	588.286329	11.326861
10.140353	588.242808	11.331879
10.032893	585.473101	11.336896
10.138389	584.913808	11.341914
10.340413	586.734648	11.346931
9.793273	591.244851	11.351949
10.174210	583.301993	11.356967
10.045958	592.789544	11.361984
10.564006	592.758904	11.367002
10.485766	581.211474	11.372019
10.119718	580.801802	11.377037
10.586951	579.867095	11.382055
10.104849	585.730415	11.387072
10.037049	590.979713	11.392090
10.136989	585.476139	11.397107
10.276776	587.830594	11.402125
10.405785	590.764252	11.407143
10.170799	584.675681	11.412160
10.083519	579.434973	11.417178
10.042696	585.314360	11.422195
10.213477	599.958989	11.427213
10.213995	606.854387	11.432231
10.194268	610.571902	11.437248
10.501678	611.615682	11.442266
10.498478	608.179539	11.447283
10.443284	618.182678	11.452301
10.501490	617.160577	11.457319
10.436332	620.336100	11.462336
10.733000	612.680989	11.467354
10.790550	618.750101	11.472371
10.413568	615.590272	11.477389
10.377684	612.020394	11.482407
10.217892	614.163014	11.487424
10.490877	609.563285	11.492442
10.575579	611.632884	11.497459
10.562715	615.109483	11.502477
10.912738	604.779353	11.507495
10.411613	616.578588	11.512512
10.461184	610.350750	11.517530
10.364875	613.748905	11.522547
10.497224	612.355424	11.527565
10.706314	598.547585	11.532583
10.438031	614.315059	11.537600
10.551533	612.085086	11.542618
10.853906	608.433808	11.547635
10.652055	610.352643	11.552653
10.832834	606.502666	11.557671
10.740290	622.921112	11.562688
10.687512	610.325100	11.567706
10.707157	616.213958	11.572723
10.418391	621.570469	11.577741
10.591930	615.717683	11.582759
10.646154	616.450837	11.587776
10.819504	611.617409	11.592794
10.543053	614.819726	11.597811
10.564696	617.568238	11.602829
10.877671	616.045470	11.607847
10.782933	622.296235	11.612864
10.675979	621.726046	11.617882
10.905555	607.403748	11.622899
10.598084	619.346213	11.627917
10.718853	612.428719	11.632935
10.849409	615.478903	11.637952
10.794159	609.968079	11.642970
11.037921	612.871137	11.647987
10.410814	625.539030	11.653005
10.970269	611.411197	11.658023
10.768578	621.358395	11.663040
10.858097	624.711657	11.668058
11.255371	615.352421	11.673075
10.857443	618.763120	11.678093
10.922275	614.120264	11.683111
10.963648	620.220313	11.688128
10.920827	609.973823	11.693146
11.048878	615.252402	11.698163
10.779530	611.741194	11.703181
11.221127	616.699247	11.708199
10.801523	614.227752	11.713216
11.003983	617.960949	11.718234
10.922597	616.130741	11.723251
10.509603	626.556018	11.728269
10.986922	626.642213	11.733287
11.259881	635.369490	11.738304
11.095254	639.687228	11.743322
11.390966	635.446851	11.748339
11.155599	624.122829	11.753357
10.864962	619.093852	11.758375
11.164249	627.608717	11.763392
10.779819	614.297803	11.768410
10.974154	629.787680	11.773427
10.618344	632.661605	11.778445
10.956327	639.990138	11.783463
11.028882	645.589847	11.788480
10.865662	642.813089	11.793498
11.403291	635.306407	11.798515
11.198270	643.136587	11.803533
11.087280	633.083801	11.808551
11.726041	628.600328	11.813568
11.243914	641.144530	11.818586
11.503104	637.380091	11.823603
11.368605	640.096266	11.828621
11.543508	636.865742	11.833639
11.179049	647.188753	11.838656
11.024102	647.774800	11.843674
11.097162	646.371672	11.848691
10.745770	642.333667	11.853709
11.185537	628.047849	11.858727
11.459023	636.790823	11.863744
10.977182	638.062407	11.868762
11.544495	638.617341	11.873779
11.370855	641.910852	11.878797
11.144112	633.889613	11.883815
11.414398	637.687927	11.888832
11.120231	641.214917	11.893850
11.267084	638.001412	11.898867
11.246370	647.759323	11.903885
11.645775	642.915714	11.908903
11.313955	646.398112	11.913920
11.215582	642.364646	11.918938
11.309927	639.064693	11.923955
11.261521	644.695977	11.928973
11.882508	657.136783	11.933991
11.393707	649.421685	11.939008
11.080329	641.066878	11.944026
11.622057	647.195838	11.949043
11.367015	660.452403	11.954061
11.217455	665.462067	11.959079
11.740171	665.948250	11.964096
11.727300	673.934531	11.969114
11.845441	669.706188	11.974131
11.522084	657.547015	11.979149
11.497836	643.333886	11.984167
11.820689	646.461244	11.989184
11.745101	643.951624	11.994202
11.785587	637.911393	11.999219
11.383876	645.889156	12.004237
11.395505	650.469617	12.009255
11.546171	646.267741	12.014272
11.519049	665.200630	12.019290
11.740643	671.127292	12.024307
11.432821	671.352282	12.029325
11.665765	664.852696	12.034343
11.431783	666.814442	12.039360
11.581955	670.663141	12.044378
11.758455	662.528216	12.049395
11.571767	667.726735	12.054413
11.791553	666.565705	12.059431
11.508597	663.725653	12.064448
11.911699	672.467272	12.069466
12.227639	656.670258	12.074483
11.634310	672.201531	12.079501
11.673564	664.132291	12.084519
11.441926	666.541796	12.089536
11.550783	669.323988	12.094554
11.839160	663.484752	12.099571
11.563553	660.716132	12.104589
11.546336	659.197759	12.109607
11.845835	659.157179	12.114624
11.550148	665.723467	12.119642
11.894402	673.997778	12.124659
11.759786	680.800768	12.129677
12.002359	681.586466	12.134695
12.116292	683.635714	12.139712
11.783374	680.109206	12.144730
12.054254	686.574108	12.149747
11.864900	688.326891	12.154765
11.712703	693.472677	12.159783
12.258608	690.610052	12.164800
11.966974	693.136259	12.169818
12.123278	695.854216	12.174835
11.926427	692.694553	12.179853
11.905282	702.244277	12.184871
12.163593	701.736776	12.189888
12.024850	709.086382	12.194906
12.196089	694.990907	12.199923
12.151463	693.492604	12.204941
11.948034	690.002611	12.209959
12.361979	688.833249	12.214976
11.823998	689.141638	12.219994
12.242449	689.663093	12.225011
12.332085	698.135100	12.230029
12.109005	690.491961	12.235047
12.345868	681.508120	12.240064
12.120934	674.575339	12.245082
12.210795	663.973512	12.250099
12.063385	684.162350	12.255117
11.998287	691.282657	12.260135
12.394659	696.146833	12.265152
12.343536	695.012468	12.270170
12.317599	690.383814	12.275187
12.294324	688.351987	12.280205
12.477145	675.283512	12.285223
12.181390	668.282934	12.290240
11.835909	665.692521	12.295258
12.186014	676.181302	12.300275
12.252302	686.395820	12.305293
11.876511	696.903673	12.310311
12.114323	686.019873	12.315328
12.099633	699.355574	12.320346
12.194762	688.708725	12.325363
12.248303	693.591901	12.330381
12.077495	700.851852	12.335399
12.474581	687.806602	12.340416
12.125355	693.775370	12.345434
12.140770	699.131583	12.350451
12.547086	692.245059	12.355469
12.109259	712.299548	12.360487
12.582731	706.601712	12.365504
12.625363	717.889780	12.370522
12.462874	721.998918	12.375539
12.420715	718.988584	12.380557
12.569198	724.933031	12.385575
12.596082	712.917762	12.390592
12.566129	725.312280	12.395610
12.571688	712.492460	12.400627
13.039833	706.533524	12.405645
12.348314	701.810333	12.410663
12.646371	703.584580	12.415680
12.491170	703.820372	12.420698
12.498268	697.125785	12.425715
12.595449	691.578429	12.430733
12.390976	703.448007	12.435751
12.847232	708.422724	12.440768
12.588145	717.564765	12.445786
12.556484	713.681777	12.450803
12.739231	719.384167	12.455821
12.756777	729.256049	12.460839
12.660515	709.225329	12.465856
12.784065	719.654958	12.470874
13.001840	712.027944	12.475891
12.599183	691.281540	12.480909
12.485686	700.798395	12.485927
12.745473	705.475689	12.490944
12.524832	713.504008	12.495962
12.929028	717.921991	12.500979
12.873026	720.979333	12.505997
12.581420	724.944598	12.511015
12.953627	711.568711	12.516032
12.651158	715.213782	12.521050
12.698219	723.638822	12.526067
12.840527	725.664694	12.531085
12.578330	727.753945	12.536103
12.474279	720.303585	12.541120
12.663243	719.137913	12.546138
12.451521	724.741162	12.551155
12.782068	715.909885	12.556173
12.767573	724.360349	12.561191
12.918897	720.770585	12.566208
12.830464	730.034218	12.571226
13.106984	736.996877	12.576243
13.281362	739.958164	12.581261
12.834643	726.631679	12.586279
13.025813	719.983982	12.591296
12.922235	725.074822	12.596314
13.166000	732.471804	12.601331
13.134916	726.363861	12.606349
12.976630	724.634054	12.611367
13.175603	724.214746	12.616384
13.029159	724.701632	12.621402
13.398625	736.717994	12.626419
13.114897	725.568744	12.631437
12.742940	710.851459	12.636455
13.242226	726.524015	12.641472
13.463625	733.700438	12.646490
13.006349	728.214697	12.651507
13.104335	715.279407	12.656525
13.154686	719.692870	12.661543
13.204003	732.595686	12.666560
13.393143	736.002788	12.671578
13.129778	728.227089	12.676595
13.346856	723.279481	12.681613
13.211671	726.507021	12.686631
13.188103	725.917452	12.691648
13.153332	734.248020	12.696666
13.231829	738.669702	12.701683
13.404324	735.764590	12.706701
13.570117	739.200597	12.711719
13.258168	733.332320	12.716736
13.488240	738.787457	12.721754
13.377026	739.669615	12.726771
13.305428	737.099395	12.731789
13.492146	737.644536	12.736807
13.315860	728.031121	12.741824
13.640687	726.572760	12.746842
13.140339	727.601095	12.751859
13.487723	732.832721	12.756877
13.422366	744.109323	12.761895
13.260873	740.871527	12.766912
13.469704	742.145357	12.771930
13.301628	735.377215	12.776947
13.603506	738.075526	12.781965
13.362482	736.134616	12.786983
13.558266	733.531971	12.792000
13.290027	740.425348	12.797018
13.361735	742.156168	12.802035
13.435853	739.922882	12.807053
13.273280	737.774019	12.812071
13.166994	742.287770	12.817088
13.133666	743.236621	12.822106
13.152028	746.339120	12.827123
13.952494	751.969982	12.832141
13.365533	757.111320	12.837159
13.619327	757.936290	12.842176
13.787767	764.641335	12.847194
13.885810	766.147123	12.852211
13.824943	750.033520	12.857229
13.805078	749.531733	12.862247
13.679898	747.733619	12.867264
13.796627	739.267194	12.872282
13.567360	735.434098	12.877299
13.692766	739.368744	12.882317
13.596102	758.672392	12.887335
13.647014	763.249882	12.892352
13.900107	758.627985	12.897370
14.168784	772.929211	12.902387
14.179769	759.104950	12.907405
14.046578	759.201593	12.912423
13.807589	748.051631	12.917440
14.060824	743.360287	12.922458
13.670516	734.301114	12.927475
13.656306	730.623674	12.932493
13.707354	736.425599	12.937511
13.572836	753.090584	12.942528
14.009891	759.867152	12.947546
13.846798	763.682901	12.952563
14.315788	761.605497	12.957581
14.015930	765.587843	12.962599
14.209824	765.696355	12.967616
14.153684	759.182068	12.972634
13.640494	756.349671	12.977651
14.066107	752.830535	12.982669
14.095772	782.774835	12.987687
13.888914	768.801660	12.992704
14.280385	768.705644	12.997722
13.962107	767.142912	13.002739
14.157190	765.515527	13.007757
14.016193	773.518771	13.012775
13.996732	768.352589	13.017792
14.039767	760.427881	13.022810
13.808953	761.612805	13.027827
14.095949	754.047512	13.032845
14.111228	770.165174	13.037863
14.267809	768.266106	13.042880
14.350084	771.339661	13.047898
14.021536	771.479536	13.052915
14.076116	770.861942	13.057933
14.163141	769.358785	13.062951
13.877738	770.119911	13.067968
13.951881	760.558761	13.072986
13.703031	766.562320	13.078003
14.201627	777.412908	13.083021
14.242678	794.861475	13.088039
14.266120	786.949293	13.093056
14.178279	785.823831	13.098074
14.117044	795.704938	13.103091
14.157827	787.146247	13.108109
14.273873	785.613295	13.113127
14.186499	800.036601	13.118144
13.895969	784.937262	13.123162
13.872733	792.032116	13.128179
14.265883	800.137876	13.133197
14.318970	812.781380	13.138215
14.659566	817.250379	13.143232
14.925010	817.256161	13.148250
14.559961	811.194203	13.153267
14.663317	799.078531	13.158285
14.421508	791.854855	13.163303
14.430204	795.665786	13.168320
14.739183	799.792592	13.173338
14.634826	796.163977	13.178355
14.711687	783.736882	13.183373
14.805168	787.944786	13.188391
14.421962	794.007275	13.193408
14.596700	776.556527	13.198426
14.415198	787.434783	13.203443
14.548919	790.582332	13.208461
15.190036	804.099385	13.213479
14.553060	809.507354	13.218496
14.540618	792.445683	13.223514
14.608001	813.743428	13.228531
14.954717	803.833431	13.233549
14.951750	797.149850	13.238567
14.675107	799.869385	13.243584
14.394610	787.820175	13.248602
14.601726	804.939771	13.253619
14.914703	806.424510	13.258637
15.346604	812.810580	13.263655
14.960924	802.627166	13.268672
15.161502	788.085203	13.273690
14.725181	786.919665	13.278707
14.612581	782.651708	13.283725
14.945855	787.424808	13.288743
15.053193	792.391101	13.293760
14.959728	783.032926	13.298778
14.573664	794.596497	13.303795
14.813934	799.781808	13.308813
15.116359	809.097853	13.313831
15.040319	817.337095	13.318848
15.523916	816.661748	13.323866
15.296309	797.301614	13.328883
15.270919	787.939082	13.333901
15.331778	789.961944	13.338919
15.034494	787.083091	13.343936
15.453650	787.064789	13.348954
15.261158	796.587760	13.353971
15.487698	785.137615	13.358989
15.115067	784.388138	13.364007
15.065114	790.328983	13.369024
15.240261	785.763474	13.374042
15.036921	788.938586	13.379059
14.977141	796.768168	13.384077
15.231006	788.677869	13.389095
15.089331	777.484239	13.394112
15.159026	771.682387	13.399130
14.763992	788.126287	13.404147
14.884512	781.928300	13.409165
14.942873	783.594942	13.414183
14.986200	787.716030	13.419200
15.342152	792.728578	13.424218
15.370539	789.268516	13.429235
15.610425	799.291795	13.434253
15.412341	789.599710	13.439271
15.066807	779.826590	13.444288
15.132136	784.253502	13.449306
15.387857	808.630238	13.454323
15.338686	811.295199	13.459341
15.133221	808.446138	13.464359
15.430620	825.674687	13.469376
15.663070	811.181361	13.474394
15.202905	817.457890	13.479411
15.534181	814.240705	13.484429
15.646598	813.118579	13.489447
15.286557	810.520957	13.494464
15.086987	808.939623	13.499482
15.335329	807.616317	13.504499
15.422553	805.074853	13.509517
15.544659	804.266794	13.514535
15.234155	809.844521	13.519552
15.188540	803.899776	13.524570
15.498924	797.725684	13.529587
15.293203	812.514686	13.534605
15.682300	815.672721	13.539623
15.278406	819.223250	13.544640
15.783032	834.077700	13.549658
15.668989	832.479807	13.554675
15.631938	827.388948	13.559693
15.944868	826.614107	13.564711
15.872309	828.531643	13.569728
15.969448	823.927853	13.574746
15.619572	820.694311	13.579763
15.919119	807.727373	13.584781
15.674150	806.819036	13.589799
15.838533	815.434023	13.594816
15.683606	822.180288	13.599834
15.802062	831.455740	13.604851
15.892744	835.055015	13.609869
15.835391	833.962644	13.614887
15.800744	840.974097	13.619904
15.608381	833.111487	13.624922
15.918975	842.789192	13.629939
15.790413	837.264537	13.634957
15.753867	830.090737	13.639975
15.701348	838.168511	13.644992
16.185071	836.388596	13.650010
16.299469	837.513125	13.655027
15.860638	831.087174	13.660045
16.028626	838.272007	13.665063
15.765667	838.452099	13.670080
16.183853	844.871889	13.675098
15.781925	841.491862	13.680115
15.851871	836.687199	13.685133
16.176347	827.591726	13.690151
15.937930	833.274932	13.695168
16.209548	828.214607	13.700186
16.009796	839.625937	13.705203
16.401213	824.448120	13.710221
16.293526	825.765237	13.715239
16.095594	829.040497	13.720256
16.132373	828.703404	13.725274
16.219855	835.493746	13.730291
16.162988	832.570905	13.735309
16.095927	833.553448	13.740327
15.872704	825.332753	13.745344
16.102773	834.439238	13.750362
16.306612	846.771964	13.755379
16.318082	853.384870	13.760397
16.375236	851.043774	13.765415
16.304615	857.006814	13.770432
16.597663	852.757336	13.775450
16.289225	861.692584	13.780467
16.418109	866.595560	13.785485
16.883074	855.455158	13.790503
16.433080	850.160745	13.795520
16.542300	841.304123	13.800538
16.521917	833.487151	13.805555
16.213997	838.603727	13.810573
16.551724	838.970575	13.815591
16.616377	835.760446	13.820608
16.059723	829.507593	13.825626
16.409438	847.428565	13.830643
16.595475	852.979001	13.835661
17.109406	852.440914	13.840679
16.698004	847.026845	13.845696
16.453616	841.315206	13.850714
16.250195	843.796054	13.855731
16.563266	844.453947	13.860749
16.579804	847.566217	13.865767
16.517352	849.605250	13.870784
16.638770	849.961808	13.875802
16.638852	851.091625	13.880819
17.008669	853.643608	13.885837
16.756217	850.360082	13.890855
16.640195	861.925567	13.895872
16.757554	850.918527	13.900890
16.582424	850.759806	13.905907
16.532178	860.497213	13.910925
16.841527	849.548456	13.915943
16.695675	855.911454	13.920960
16.948360	851.043441	13.925978
16.973867	853.128654	13.930995
16.442801	855.635592	13.936013
17.197896	840.078884	13.941031
16.870404	849.657749	13.946048
16.946663	849.566939	13.951066
17.086833	848.169059	13.956083
16.624244	852.864898	13.961101
17.064401	849.384491	13.966119
16.922715	856.617851	13.971136
16.666901	862.414247	13.976154
16.620148	847.185140	13.981171
17.035752	875.043069	13.986189
17.142961	874.489810	13.991207
17.427612	877.402285	13.996224
17.337248	862.268363	14.001242
16.934142	859.955196	14.006259
16.775373	854.902336	14.011277
17.157691	859.210172	14.016295
17.500187	874.661268	14.021312
17.092128	861.274975	14.026330
17.188622	855.822352	14.031347
16.960810	868.762375	14.036365
17.315767	871.278818	14.041383
17.647710	884.074344	14.046400
17.205792	876.326555	14.051418
17.181554	860.806727	14.056435
17.477959	878.316354	14.061453
17.190080	863.469002	14.066471
17.284060	869.680817	14.071488
17.401608	875.636473	14.076506
17.696128	871.228966	14.081523
17.323059	873.701684	14.086541
17.062111	860.652110	14.091559
17.158418	873.983173	14.096576
17.441206	875.056074	14.101594
17.680618	878.325937	14.106611
17.391595	881.394568	14.111629
17.757629	871.604585	14.116647
17.681759	877.789365	14.121664
17.452290	881.413565	14.126682
17.618646	869.600404	14.131699
17.192946	875.868397	14.136717
17.500446	878.038821	14.141735
17.660870	871.026651	14.146752
17.561127	876.363089	14.151770
17.330401	874.152302	14.156787
17.710693	883.156379	14.161805
17.671320	875.856769	14.166823
17.421029	886.875253	14.171840
17.301006	873.260782	14.176858
17.901895	868.565429	14.181875
17.314005	880.463639	14.186893
17.590583	878.545759	14.191911
17.552274	866.764667	14.196928
17.508538	875.039900	14.201946
17.539335	874.467055	14.206963
17.843431	888.797539	14.211981
18.164667	888.545267	14.216999
17.711901	885.791745	14.222016
17.841023	895.573653	14.227034
18.292201	895.102203	14.232051
17.849544	886.044843	14.237069
17.667788	870.451854	14.242087
17.495764	875.424070	14.247104
17.566742	890.819890	14.252122
17.825054	894.607512	14.257139
17.506061	900.887198	14.262157
18.434948	894.395256	14.267175
17.958491	900.276727	14.272192
17.711870	897.317333	14.277210
18.116217	891.178981	14.282227
18.088521	901.840701	14.287245
18.259476	902.666033	14.292263
18.458528	894.394923	14.297280
17.948507	895.904473	14.302298
18.187487	899.824515	14.307315
18.004288	897.391680	14.312333
18.004648	889.833370	14.317351
18.419223	894.066732	14.322368
18.317043	899.138467	14.327386
18.124932	891.408337	14.332403
17.883244	897.634884	14.337421
18.036732	901.284294	14.342439
18.269304	895.116048	14.347456
17.942246	894.832805	14.352474
18.068688	898.413867	14.357491
18.788696	907.446782	14.362509
18.806709	905.897621	14.367527
18.793659	895.829342	14.372544
18.365006	893.870474	14.377562
18.729127	878.062560	14.382579
18.592438	890.713762	14.387597
18.371985	887.863880	14.392615
18.686093	877.678079	14.397632
18.545262	889.408419	14.402650
18.808361	889.619700	14.407667
18.513125	885.629646	14.412685
18.660209	889.030744	14.417703
18.672981	880.836165	14.422720
18.559659	885.928577	14.427738
18.743146	883.741254	14.432755
18.376276	888.368455	14.437773
18.589850	893.867251	14.442791
18.709859	889.550200	14.447808
18.675571	887.280231	14.452826
18.815647	888.640585	14.457843
18.688828	884.763002	14.462861
18.540319	891.940640	14.467879
18.619355	892.720413	14.472896
18.458419	891.357083	14.477914
18.372721	881.019324	14.482931
18.626156	894.347875	14.487949
18.657108	903.955817	14.492967
19.086463	909.884721	14.497984
19.089974	909.723256	14.503002
18.747223	898.652574	14.508019
18.944354	894.222451	14.513037
18.931142	893.255706	14.518055
18.992911	885.113409	14.523072
18.485151	904.147104	14.528090
18.966855	902.995516	14.533107
19.101626	904.905823	14.538125
18.851225	906.718685	14.543143
19.098391	910.539616	14.548160
18.849028	910.278913	14.553178
18.994299	907.886132	14.558195
18.962934	906.833867	14.563213
18.874646	920.298030	14.568231
19.264420	909.273519	14.573248
18.899322	914.209724	14.578266
19.058301	906.879023	14.583283
19.023862	908.121552	14.588301
18.666641	917.427396	14.593319
18.857130	909.798262	14.598336
18.915844	918.467726	14.603354
19.170343	926.888763	14.608371
19.143813	935.003535	14.613389
19.024345	939.544648	14.618407
19.348908	934.138320	14.623424
19.216789	944.286240	14.628442
19.312714	935.905035	14.633459
19.235241	937.801262	14.638477
19.167863	939.415034	14.643495
19.524858	928.872184	14.648512
19.156545	946.444999	14.653530
19.251774	937.530560	14.658547
19.491601	931.626258	14.663565
19.585563	942.799127	14.668583
19.576421	938.830510	14.673600
19.327528	944.477521	14.678618
19.875205	937.256324	14.683635
19.730295	937.664079	14.688653
19.390098	928.117264	14.693671
19.901715	925.585029	14.698688
19.414970	930.414063	14.703706
19.631087	928.044894	14.708723
19.336578	937.798523	14.713741
19.312104	932.809808	14.718759
19.832362	928.622544	14.723776
19.588892	935.411127	14.728794
19.594374	927.883557	14.733811
19.708115	939.744460	14.738829
19.796867	945.496363	14.743847
20.109020	940.937751	14.748864
19.993348	939.381130	14.753882
19.803251	933.187575	14.758899
19.823352	937.094582	14.763917
19.671644	936.111663	14.768935
19.775403	930.260240	14.773952
20.099337	949.021659	14.778970
19.976009	951.218568	14.783987
19.973770	945.860284	14.789005
19.803477	946.937904	14.794023
19.801910	944.517632	14.799040
19.968824	958.566702	14.804058
20.089370	964.310474	14.809075
20.453956	955.498993	14.814093
20.074065	949.985279	14.819111
20.145832	936.833025	14.824128
19.859710	938.799813	14.829146
20.150240	948.588019	14.834163
20.215283	958.515704	14.839181
19.937183	962.636699	14.844199
20.506032	968.947719	14.849216
20.184990	950.845472	14.854234
20.283298	932.775371	14.859251
20.326066	940.156594	14.864269
20.100150	940.094193	14.869287
20.429068	933.475329	14.874304
20.276610	939.558519	14.879322
20.238155	937.914059	14.884339
20.453920	942.244855	14.889357
19.861844	961.001481	14.894375
20.515857	953.044078	14.899392
20.345653	958.438918	14.904410
20.563141	957.827352	14.909427
20.663990	964.003409	14.914445
20.562240	963.075780	14.919463
20.502586	943.032750	14.924480
20.539445	946.605767	14.929498
20.826943	950.685480	14.934515
20.735216	934.207309	14.939533
20.324885	938.194378	14.944551
20.299408	929.646001	14.949568
20.507391	950.398006	14.954586
20.690193	956.005786	14.959603
20.835020	947.010986	14.964621
20.648305	953.746502	14.969639
20.496615	959.147910	14.974656
20.292584	967.549289	14.979674
20.599725	951.822823	14.984691
20.703257	954.347113	14.989709
20.379756	959.784908	14.994727
20.646677	951.499982	14.999744
20.822657	951.699667	15.004762
20.857723	951.580596	15.009779
20.790822	944.960627	15.014797
20.387171	949.716685	15.019815
20.686768	952.077709	15.024832
20.846355	950.383283	15.029850
20.607914	953.961565	15.034867
20.816379	960.048174	15.039885
20.876803	973.220828	15.044903
21.038855	969.165420	15.049920
21.284828	971.525380	15.054938
21.357458	966.707638	15.059955
21.014849	968.187807	15.064973
21.152280	968.633378	15.069991
21.214083	955.713051	15.075008
20.968915	952.409429	15.080026
21.170710	956.423675	15.085043
21.142042	967.745163	15.090061
20.876106	982.856172	15.095079
21.175099	976.791103	15.100096
21.476709	976.412515	15.105114
21.647128	971.465838	15.110131
21.438565	965.593908	15.115149
21.162131	954.175123	15.120167
21.167201	946.616051	15.125184
20.903206	962.982775	15.130202
20.964449	971.948521	15.135219
21.362992	976.361143	15.140237
21.634778	982.538827	15.145255
21.047254	974.201568	15.150272
21.577744	974.178448	15.155290
21.281311	976.213129	15.160307
21.454413	987.307352	15.165325
21.286271	983.013334	15.170343
21.260902	978.529687	15.175360
21.194435	983.460147	15.180378
21.402250	981.429951	15.185395
21.559034	984.700156	15.190413
21.427333	978.166069	15.195431
21.454694	980.184734	15.200448
21.272370	976.637726	15.205466
21.627222	991.796648	15.210483
21.890930	993.364863	15.215501
21.965402	997.708343	15.220519
21.499440	996.926140	15.225536
21.626776	999.153210	15.230554
21.680521	1005.346129	15.235571
22.086579	994.303236	15.240589
22.129933	997.089431	15.245607
21.780419	991.182771	15.250624
22.054545	984.976425	15.255642
21.678222	982.595929	15.260659
21.697199	984.041537	15.265677
21.882566	1003.146623	15.270695
22.201525	996.756520	15.275712
22.216441	999.474586	15.280730
21.896302	984.054662	15.285747
21.852484	967.449031	15.290765
21.989371	983.112321	15.295783
21.808157	1003.032253	15.300800
21.873217	998.584926	15.305818
22.108723	1001.113792	15.310835
21.904077	1000.893420	15.315853
21.992729	1001.924161	15.320871
22.143109	1009.013990	15.325888
22.381378	1000.878701	15.330906
22.060970	994.989571	15.335923
22.587426	999.827137	15.340941
22.174354	1000.299000	15.345959
22.226948	1000.016232	15.350976
22.546654	996.845010	15.355994
22.293824	992.589506	15.361011
22.541896	991.395621	15.366029
22.058825	995.286801	15.371047
22.225886	988.279856	15.376064
22.231304	996.291818	15.381082
22.130039	992.467013	15.386099
22.306255	996.049764	15.391117
21.974392	994.230358	15.396135
22.363935	991.815074	15.401152
22.518490	994.836316	15.406170
22.427958	999.085725	15.411187
22.535218	1006.570483	15.416205
22.421063	1005.404947	15.421223
22.580308	1011.461415	15.426240
22.689414	1012.258573	15.431258
22.466903	1022.935109	15.436275
22.949718	1019.365932	15.441293
22.834807	1011.361716	15.446311
22.940156	1014.961886	15.451328
22.747847	1001.626892	15.456346
22.810482	994.749918	15.461363
23.018542	991.163834	15.466381
22.713430	1000.704559	15.471399
22.703112	991.165986	15.476416
22.562128	989.496559	15.481434
22.917921	1007.700770	15.486451
22.961243	1010.764689	15.491469
23.139756	1011.683519	15.496487
23.190317	995.987748	15.501504
23.252014	982.852817	15.506522
22.888329	978.097121	15.511539
23.071929	976.976456	15.516557
23.095293	983.776900	15.521575
22.937020	981.576839	15.526592
22.913538	979.955276	15.531610
22.988563	982.979509	15.536627
22.827377	977.399961	15.541645
22.845249	1003.319582	15.546663
23.213652	996.091735	15.551680
23.574008	999.178566	15.556698
23.290923	1007.907938	15.561715
23.394133	1000.374493	15.566733
23.402220	982.712963	15.571751
23.173505	988.669258	15.576768
23.320244	981.204742	15.581786
23.252056	981.654127	15.586803
22.936111	981.605831	15.591821
22.882444	1005.889297	15.596839
23.007991	1006.772243	15.601856
23.323629	997.608640	15.606874
23.213955	1014.667617	15.611891
23.262933	1008.774257	15.616909
23.370734	1008.328201	15.621927
23.309744	1014.075185	15.626944
23.445291	1000.739318	15.631962
23.314458	1007.024275	15.636979
23.442152	1013.461237	15.641997
23.820870	1019.000471	15.647015
23.585320	1019.359311	15.652032
23.877364	1015.854740	15.657050
23.349506	1017.045194	15.662067
23.758886	1020.345259	15.667085
23.892399	1023.922083	15.672103
23.668992	1025.683389	15.677120
23.944692	1021.256704	15.682138
23.423128	1018.637020	15.687155
23.655353	1019.383328	15.692173
23.849064	1024.585468	15.697191
23.410288	1022.940604	15.702208
24.003899	1027.915983	15.707226
24.131284	1025.125192	15.712243
24.181704	1020.415059	15.717261
23.879854	1026.427009	15.722279
23.843966	1024.785294	15.727296
24.113861	1020.410012	15.732314
23.964498	1024.362525	15.737331
23.920438	1020.869587	15.742349
24.004675	1024.094360	15.747367
23.779782	1022.406518	15.752384
24.183055	1017.584295	15.757402
24.058383	1021.608679	15.762419
23.857563	1025.506136	15.767437
23.724220	1027.177590	15.772455
23.876341	1028.217324	15.777472
23.964021	1027.553508	15.782490
24.082129	1042.459225	15.787507
23.964053	1052.772268	15.792525
24.345485	1056.524855	15.797543
24.031106	1052.484112	15.802560
24.546503	1053.119782	15.807578
24.407202	1051.292290	15.812595
24.575906	1055.775659	15.817613
24.558114	1056.905134	15.822631
24.318881	1055.421512	15.827648
24.747199	1048.679732	15.832666
24.621624	1050.226891	15.837683
24.856858	1046.885854	15.842701
24.761144	1039.017477	15.847719
24.507320	1045.738294	15.852736
24.836914	1045.487867	15.857754
24.415242	1027.612753	15.862771
24.195290	1024.175776	15.867789
24.757143	1034.442240	15.872807
24.546016	1041.613970	15.877824
24.594435	1038.122318	15.882842
24.449548	1045.968499	15.887859
24.540188	1043.025668	15.892877
24.778127	1034.915663	15.897895
24.624380	1048.065122	15.902912
24.680838	1053.115201	15.907930
24.992553	1051.804041	15.912947
24.808169	1055.367561	15.917965
25.063072	1053.361538	15.922983
24.830404	1050.308411	15.928000
25.081526	1046.018117	15.933018
25.039714	1044.235314	15.938035
24.747555	1047.774692	15.943053
25.067764	1045.102013	15.948071
25.194630	1056.408657	15.953088
25.322787	1041.584337	15.958106
24.890653	1048.269975	15.963123
24.554542	1048.515180	15.968141
24.958981	1051.213250	15.973159
25.231264	1059.189740	15.978176
25.218361	1062.742174	15.983194
24.713260	1065.080965	15.988211
24.773905	1068.180051	15.993229
25.217311	1068.729168	15.998247
24.914426	1076.805250	16.003264
25.265224	1071.827128	16.008282
25.079705	1069.738625	16.013299
25.099773	1066.649053	16.018317
25.072484	1061.723860	16.023335
25.326146	1082.967494	16.028352
25.427250	1090.137661	16.033370
25.495194	1087.416136	16.038387
25.876527	1090.518631	16.043405
25.935515	1089.010373	16.048423
25.530461	1075.358352	16.053440
25.796920	1065.871051	16.058458
25.544053	1072.386595	16.063475
25.437531	1066.438683	16.068493
25.712497	1064.984952	16.073511
25.526268	1075.876747	16.078528
25.766952	1077.050935	16.083546
25.734100	1084.964788	16.088563
25.396065	1091.623075	16.093581
25.909307	1090.368702	16.098599
25.655419	1089.505929	16.103616
25.905833	1087.276537	16.108634
25.787565	1085.127001	16.113651
25.578799	1086.715601	16.118669
25.776329	1091.563702	16.123687
25.592950	1093.972014	16.128704
25.686826	1093.121028	16.133722
25.690224	1095.541103	16.138739
25.743567	1089.268325	16.143757
25.979099	1087.259021	16.148775
25.938716	1093.750749	16.153792
26.151381	1100.654126	16.158810
26.448206	1107.506449	16.163827
26.160420	1096.726842	16.168845
26.289717	1089.044101	16.173863
26.070940	1089.245676	16.178880
26.178216	1083.431522	16.183898
26.128556	1077.862872	16.188915
25.742620	1087.842352	16.193933
26.380476	1095.111466	16.198951
26.429368	1102.236169	16.203968
26.328466	1104.315970	16.208986
26.665764	1105.790612	16.214003
26.584716	1105.841215	16.219021
26.597253	1101.970154	16.224039
26.551596	1097.174065	16.229056
26.294731	1087.920229	16.234074
26.433519	1085.660989	16.239091
26.692478	1095.242777	16.244109
26.450740	1085.920299	16.249127
26.816540	1096.113371	16.254144
26.577850	1094.396124	16.259162
26.370852	1084.954591	16.264179
26.612900	1094.106671	16.269197
26.888209	1095.609960	16.274215
26.550232	1101.078468	16.279232
26.346014	1102.347611	16.284250
26.636446	1097.151716	16.289267
26.849360	1102.704330	16.294285
26.714056	1098.231565	16.299303
26.772314	1102.252554	16.304320
26.985211	1096.491277	16.309338
26.669723	1093.589978	16.314355
26.898318	1100.320440	16.319373
26.719831	1089.732002	16.324391
26.907674	1100.681971	16.329408
26.789344	1100.795222	16.334426
26.897432	1101.920757	16.339443
27.047837	1106.612139	16.344461
26.762361	1095.065287	16.349479
26.791109	1115.290129	16.354496
27.250948	1119.589039	16.359514
27.335615	1128.380775	16.364531
27.085938	1133.649260	16.369549
27.325777	1125.813481	16.374567
27.259881	1134.092306	16.379584
27.034319	1134.803044	16.384602
27.546769	1126.577402	16.389619
27.242623	1123.683789	16.394637
27.256989	1122.791608	16.399655
27.438056	1130.384778	16.404672
27.461375	1119.509075	16.409690
27.481598	1127.026456	16.414707
27.208762	1121.454888	16.419725
27.280691	1120.399049	16.424743
27.458753	1128.005312	16.429760
27.236712	1132.164901	16.434778
27.403353	1127.291359	16.439795
27.367552	1128.044952	16.444813
27.952573	1127.104388	16.449831
27.571633	1134.148121	16.454848
27.787499	1121.594868	16.459866
27.830062	1123.611167	16.464883
27.628399	1127.259461	16.469901
27.541424	1116.041269	16.474919
27.373063	1132.509932	16.479936
27.841861	1141.800084	16.484954
27.849001	1147.227158	16.489971
27.956898	1150.019044	16.494989
28.192962	1141.385404	16.500007
27.744727	1137.873715	16.505024
27.921305	1134.320939	16.510042
28.073242	1130.383847	16.515059
28.065666	1142.977127	16.520077
28.152871	1132.135590	16.525095
28.072493	1128.487370	16.530112
28.132668	1130.816500	16.535130
28.006408	1125.594362	16.540147
28.302765	1136.170735	16.545165
28.129251	1123.981454	16.550183
28.073455	1135.821711	16.555200
28.297068	1140.959238	16.560218
28.258016	1137.295074	16.565235
28.275401	1146.851621	16.570253
28.600632	1143.136692	16.575271
28.676406	1133.322615	16.580288
28.397379	1122.787780	16.585306
28.192775	1118.616211	16.590323
28.297057	1120.932117	16.595341
28.654818	1113.387145	16.600359
28.350917	1121.987286	16.605376
28.464599	1133.974564	16.610394
28.559353	1141.003731	16.615411
28.592194	1144.053537	16.620429
28.723847	1143.007274	16.625447
28.704535	1140.965308	16.630464
28.631662	1147.569447	16.635482
28.816291	1135.838457	16.640499
28.365846	1145.733399	16.645517
28.650692	1136.088541	16.650535
28.228229	1137.117317	16.655552
28.737872	1148.427164	16.660570
28.878934	1149.544379	16.665587
28.822616	1148.085741	16.670605
28.867820	1141.179883	16.675623
28.841444	1143.418431	16.680640
28.420637	1142.850059	16.685658
28.684346	1145.077872	16.690675
28.680851	1148.654096	16.695693
28.828956	1148.955984	16.700711
28.815609	1162.601099	16.705728
28.495813	1161.246859	16.710746
29.129983	1170.126095	16.715763
29.073525	1172.372516	16.720781
28.871194	1175.213012	16.725799
28.856071	1174.855642	16.730816
28.713414	1177.380665	16.735834
29.122958	1171.168818	16.740851
29.135372	1186.813918	16.745869
29.513359	1200.688093	16.750887
29.663729	1186.399834	16.755904
29.364117	1189.845730	16.760922
29.432310	1172.070450	16.765939
29.400717	1186.456925	16.770957
29.611916	1167.400035	16.775975
29.637384	1161.646012	16.780992
29.286215	1175.078969	16.786010
29.573688	1184.586909	16.791027
29.645242	1190.063865	16.796045
29.614652	1190.882918	16.801063
29.482499	1191.664233	16.806080
29.553794	1191.662565	16.811098
29.948088	1191.764930	16.816115
29.590085	1189.106970	16.821133
29.809657	1195.049903	16.826151
30.191523	1188.324817	16.831168
29.932111	1195.930222	16.836186
29.711546	1181.289816	16.841203
29.633324	1182.321466	16.846221
29.586942	1190.104937	16.851239
30.154268	1183.464408	16.856256
29.780757	1183.349388	16.861274
29.864743	1186.438526	16.866291
30.114233	1186.068100	16.871309
30.023972	1186.770265	16.876327
30.317067	1185.250567	16.881344
30.005039	1190.191155	16.886362
29.940767	1185.158110	16.891379
29.892909	1184.547083	16.896397
30.139633	1189.280202	16.901415
30.188551	1180.300312	16.906432
29.994215	1191.982426	16.911450
30.119906	1187.235208	16.916467
30.110547	1191.620273	16.921485
30.435864	1187.312010	16.926503
30.365108	1186.897082	16.931520
30.417439	1185.434041	16.936538
30.472055	1178.331028	16.941555
30.427922	1185.470339	16.946573
30.217405	1190.978866	16.951591
30.569715	1189.418330	16.956608
30.291945	1190.493869	16.961626
30.565861	1200.786608	16.966643
30.789687	1202.720865	16.971661
30.576093	1209.460688	16.976679
30.793334	1206.365446	16.981696
30.910374	1206.075734	16.986714
30.874926	1203.124228	16.991731
30.612791	1192.624577	16.996749
30.679980	1191.203391	17.001767
30.784422	1201.551086	17.006784
30.449969	1207.666037	17.011802
30.553668	1201.729325	17.016819
30.616939	1204.291518	17.021837
30.793343	1201.947471	17.026855
30.883481	1202.798104	17.031872
30.653890	1211.131015	17.036890
30.604281	1205.243569	17.041907
30.794178	1219.159851	17.046925
31.102827	1223.570841	17.051943
31.449063	1229.238311	17.056960
31.001187	1227.989343	17.061978
31.310349	1224.737680	17.066995
31.399769	1237.514652	17.072013
31.076319	1226.115682	17.077031
31.541999	1229.672063	17.082048
31.287807	1231.116308	17.087066
31.634886	1221.609982	17.092083
31.589005	1217.899532	17.097101
31.369760	1215.601694	17.102119
31.466463	1217.237122	17.107136
31.745158	1214.548832	17.112154
31.557604	1207.527932	17.117171
31.538031	1194.661208	17.122189
31.310024	1201.538991	17.127207
31.563943	1205.586153	17.132224
31.622103	1218.582612	17.137242
31.474548	1219.337938	17.142259
32.010465	1219.863098	17.147277
31.737805	1232.766227	17.152295
31.840119	1213.546460	17.157312
31.469460	1218.852861	17.162330
31.675324	1220.960354	17.167347
31.623882	1214.457788	17.172365
31.874059	1218.710675	17.177383
32.051330	1219.989485	17.182400
31.879673	1216.282962	17.187418
32.039370	1219.524352	17.192435
31.795014	1216.280516	17.197453
31.867307	1225.632836	17.202471
31.791269	1220.794135	17.207488
31.796136	1216.422459	17.212506
32.212964	1224.344817	17.217523
31.558548	1215.282595	17.222541
31.923175	1234.050563	17.227559
32.004707	1237.127471	17.232576
32.115250	1243.838613	17.237594
32.390901	1242.959139	17.242611
32.044477	1246.677477	17.247629
32.117447	1248.253509	17.252647
32.309202	1237.903631	17.257664
32.204361	1248.069540	17.262682
32.339608	1239.625225	17.267699
32.068951	1239.958010	17.272717
32.110915	1245.313383	17.277735
32.589596	1254.128658	17.282752
32.743556	1258.570204	17.287770
32.861444	1262.152680	17.292787
33.046332	1244.772471	17.297805
32.559538	1240.856532	17.302823
32.779450	1230.284488	17.307840
32.637015	1237.281426	17.312858
32.842326	1228.936595	17.317875
33.210989	1222.295619	17.322893
33.011549	1234.975831	17.327911
33.075136	1223.847594	17.332928
33.231597	1228.639049	17.337946
32.958210	1231.430724	17.342963
32.875920	1229.035684	17.347981
32.750231	1223.949132	17.352999
33.091886	1226.366722	17.358016
33.057217	1221.856067	17.363034
32.987323	1221.642982	17.368051
33.017496	1218.681192	17.373069
32.921845	1232.730590	17.378087
33.457603	1242.360611	17.383104
33.107127	1234.270122	17.388122
33.310097	1256.298261	17.393139
33.437490	1251.790611	17.398157
33.289714	1252.340837	17.403175
33.077888	1247.403479	17.408192
33.532535	1246.915699	17.413210
33.682479	1252.112139	17.418227
33.489200	1246.259813	17.423245
33.314292	1252.479175	17.428263
33.552220	1245.053913	17.433280
33.525138	1250.846155	17.438298
33.534412	1246.865116	17.443315
33.492508	1252.328309	17.448333
33.351856	1259.612165	17.453351
33.023515	1249.855027	17.458368
33.514325	1236.772603	17.463386
33.252098	1242.292404	17.468403
33.785288	1253.418742	17.473421
33.461531	1277.094772	17.478439
33.640424	1268.495276	17.483456
33.978535	1277.360990	17.488474
34.030929	1275.345645	17.493491
34.133958	1268.399118	17.498509
33.888206	1276.933416	17.503527
34.482564	1271.702475	17.508544
34.200835	1267.839612	17.513562
34.009869	1272.773878	17.518579
34.002382	1266.564220	17.523597
34.169133	1274.756164	17.528615
34.101862	1267.369243	17.533632
34.286818	1262.057277	17.538650
34.050805	1263.530236	17.543667
34.184267	1268.508349	17.548685
33.944677	1274.138226	17.553703
34.011556	1263.063100	17.558720
34.242184	1267.028715	17.563738
34.201769	1264.803841	17.568755
34.353191	1273.039214	17.573773
34.643967	1289.871604	17.578791
34.848532	1283.237380	17.583808
34.678149	1269.270720	17.588826
34.480295	1262.503887	17.593843
34.366288	1260.385221	17.598861
34.150632	1285.584418	17.603879
34.676595	1277.558570	17.608896
34.775439	1283.264818	17.613914
34.255874	1292.217579	17.618931
34.546133	1290.174432	17.623949
34.102663	1285.879295	17.628967
34.358744	1290.320629	17.633984
34.391400	1308.298054	17.639002
34.600101	1311.588589	17.644019
35.420576	1316.130858	17.649037
35.455526	1310.896031	17.654055
35.666901	1310.768270	17.659072
35.775351	1311.606571	17.664090
35.425362	1295.039137	17.669107
35.287932	1282.604243	17.674125
35.532537	1282.168306	17.679143
35.172175	1279.712681	17.684160
35.584459	1281.109316	17.689178
35.139926	1278.505926	17.694195
35.519266	1267.861542	17.699213
35.255475	1269.225240	17.704231
35.341978	1272.639059	17.709248
35.417632	1273.772842	17.714266
35.241371	1274.557916	17.719283
35.277936	1282.577750	17.724301
35.332683	1276.071148	17.729319
35.417278	1287.368781	17.734336
35.844945	1294.607791	17.739354
35.424635	1304.788445	17.744371
35.731180	1302.717497	17.749389
35.695447	1307.185621	17.754407
35.673334	1300.040929	17.759424
35.873273	1299.877089	17.764442
36.066955	1313.511973	17.769459
36.106889	1305.376063	17.774477
36.037530	1302.376203	17.779495
35.954409	1297.358703	17.784512
36.076468	1300.738554	17.789530
36.010289	1299.729590	17.794547
36.152946	1301.733383	17.799565
35.786433	1302.156930	17.804583
35.963667	1304.158461	17.809600
36.051162	1299.164724	17.814618
35.811033	1302.228921	17.819635
36.157366	1303.007859	17.824653
35.675214	1298.141244	17.829671
35.986798	1306.118000	17.834688
35.925490	1309.068971	17.839706
35.507542	1331.866701	17.844723
35.830794	1313.082446	17.849741
36.121599	1329.005959	17.854759
35.919532	1330.233753	17.859776
35.890708	1345.288981	17.864794
35.908831	1356.581293	17.869811
36.393570	1354.368806	17.874829
36.728662	1357.080945	17.879847
36.939393	1346.040036	17.884864
37.441932	1350.408056	17.889882
36.954274	1348.840250	17.894899
37.189866	1342.885982	17.899917
37.174946	1346.189468	17.904935
37.435386	1335.068191	17.909952
37.073186	1321.295652	17.914970
37.070596	1318.137000	17.919987
37.423264	1310.532781	17.925005
37.357075	1312.326289	17.930023
37.296840	1305.635711	17.935040
37.263293	1303.160437	17.940058
37.042979	1308.339163	17.945075
37.093031	1301.804883	17.950093
36.970113	1307.441739	17.955111
37.232906	1305.103079	17.960128
37.039647	1306.269529	17.965146
36.774248	1312.127534	17.970163
37.204238	1307.234774	17.975181
37.499338	1309.435598	17.980199
36.961268	1306.354533	17.985216
37.629952	1303.210636	17.990234
37.551163	1310.292308	17.995251
37.045397	1310.043367	18.000269
37.823852	1318.360407	18.005287
37.417733	1324.130006	18.010304
37.605010	1313.111727	18.015322
37.589438	1331.636397	18.020339
37.604758	1331.192199	18.025357
38.023305	1321.999684	18.030375
37.753208	1335.969193	18.035392
38.454962	1330.917077	18.040410
37.888565	1321.970403	18.045427
37.753860	1310.503935	18.050445
37.719307	1302.761564	18.055463
37.406714	1321.010854	18.060480
37.931609	1323.917322	18.065498
37.812550	1330.184767	18.070515
37.955564	1324.841483	18.075533
38.420484	1329.521518	18.080551
38.090460	1333.388789	18.085568
37.764377	1333.443069	18.090586
37.772662	1330.585681	18.095603
38.212567	1334.556394	18.100621
37.992279	1333.899792	18.105639
37.698453	1337.950750	18.110656
38.318628	1350.900277	18.115674
38.543289	1356.107133	18.120691
38.822953	1342.723184	18.125709
39.147269	1338.307740	18.130727
38.706636	1334.097357	18.135744
38.792976	1320.712154	18.140762
38.707615	1331.733474	18.145779
38.830283	1319.125253	18.150797
38.567334	1315.155290	18.155815
38.367587	1317.092806	18.160832
39.022282	1314.317187	18.165850
38.567078	1319.980860	18.170867
38.612641	1316.429639	18.175885
39.078847	1323.893007	18.180903
39.289249	1333.854933	18.185920
39.262841	1315.387402	18.190938
38.894743	1310.619683	18.195955
38.919467	1313.421471	18.200973
38.981744	1314.336437	18.205991
39.078342	1313.406115	18.211008
38.646866	1318.071951	18.216026
38.457302	1330.043753	18.221043
38.677419	1345.836339	18.226061
39.137204	1338.095400	18.231079
38.857910	1339.625641	18.236096
38.896319	1332.613472	18.241114
38.967805	1342.085905	18.246131
39.069378	1352.828631	18.251149
39.226364	1349.086369	18.256167
39.175350	1362.705979	18.261184
39.714779	1362.671992	18.266202
39.546968	1365.175735	18.271219
39.173526	1353.112299	18.276237
39.817314	1353.958250	18.281255
39.778673	1349.037912	18.286272
39.874900	1356.344657	18.291290
39.492081	1360.892422	18.296307
39.597380	1359.686168	18.301325
39.749899	1352.463599	18.306343
39.737648	1373.550418	18.311360
39.810669	1368.606268	18.316378
40.037039	1378.319553	18.321395
39.687339	1373.362734	18.326413
40.360695	1376.735123	18.331431
40.232129	1377.178197	18.336448
40.449288	1378.766364	18.341466
40.320987	1369.902511	18.346483
40.155161	1358.160010	18.351501
40.343547	1355.204969	18.356519
40.232568	1352.161126	18.361536
40.080204	1360.381017	18.366554
40.335428	1356.916865	18.371571
40.688333	1378.609226	18.376589
40.623446	1368.804434	18.381607
40.471932	1373.824069	18.386624
40.433212	1367.777066	18.391642
40.245727	1367.238405	18.396659
40.212893	1376.181223	18.401677
40.770941	1370.387873	18.406695
40.613300	1375.029755	18.411712
40.671723	1370.807448	18.416730
40.674536	1377.396658	18.421747
40.379255	1372.358726	18.426765
40.692445	1370.501334	18.431783
40.625932	1385.571968	18.436800
40.491150	1381.963780	18.441818
40.949770	1395.187972	18.446835
40.913062	1400.959679	18.451853
41.236780	1399.886466	18.456871
41.026265	1414.146516	18.461888
40.849429	1407.079674	18.466906
40.859940	1403.840055	18.471923
40.534203	1405.118790	18.476941
41.032432	1397.788388	18.481959
40.948918	1409.607922	18.486976
41.340268	1419.926572	18.491994
41.004104	1434.136893	18.497011
40.827832	1436.004468	18.502029
41.455250	1423.358119	18.507047
41.183018	1432.379500	18.512064
41.585236	1429.741256	18.517082
41.502161	1427.194826	18.522099
41.712359	1429.005005	18.527117
41.616090	1431.222980	18.532135
41.425131	1427.566777	18.537152
41.845796	1429.782659	18.542170
41.689109	1419.881763	18.547187
41.204724	1426.518919	18.552205
42.035909	1435.174909	18.557223
41.746938	1448.342693	18.562240
41.787382	1450.962149	18.567258
42.071917	1453.110996	18.572275
41.949632	1448.055406	18.577293
42.069912	1449.220080	18.582311
42.051683	1450.576877	18.587328
42.117975	1450.957864	18.592346
42.065586	1444.843545	18.597363
41.964060	1444.944697	18.602381
42.575672	1445.076136	18.607399
41.998984	1449.193527	18.612416
42.011334	1450.409827	18.617434
42.165578	1445.948416	18.622451
42.168148	1447.241991	18.627469
42.339737	1453.479722	18.632487
42.413400	1475.301162	18.637504
42.519613	1473.769692	18.642522
42.555196	1475.193803	18.647539
42.591041	1473.951084	18.652557
42.794811	1469.137907	18.657575
43.042402	1469.171737	18.662592
42.738972	1471.860853	18.667610
42.702380	1470.335978	18.672627
43.027023	1475.126397	18.677645
42.794416	1468.696306	18.682663
42.542952	1470.007592	18.687680
42.632478	1472.732976	18.692698
42.563592	1462.575291	18.697715
42.865152	1470.496884	18.702733
43.293213	1474.841888	18.707751
43.497973	1495.882226	18.712768
43.318539	1477.949770	18.717786
43.336414	1476.892912	18.722803
43.250472	1468.517860	18.727821
43.295586	1460.728223	18.732839
43.035913	1473.317049	18.737856
43.374909	1487.298548	18.742874
43.319709	1487.020038	18.747891
43.436505	1488.945848	18.752909
43.711028	1492.708967	18.757927
43.701127	1499.890380	18.762944
43.469363	1499.907790	18.767962
43.674121	1489.909198	18.772979
43.801694	1492.546569	18.777997
43.908135	1495.057857	18.783015
43.641215	1492.164661	18.788032
43.833374	1493.876683	18.793050
43.938981	1487.993229	18.798067
43.942434	1495.870016	18.803085
44.326469	1488.929873	18.808103
43.666895	1489.459302	18.813120
43.726971	1495.421014	18.818138
43.762140	1492.534140	18.823155
43.494245	1499.942176	18.828173
43.933897	1507.441341	18.833191
44.002165	1515.431065	18.838208
43.994625	1516.391696	18.843226
44.258185	1508.469978	18.848243
44.006847	1518.516975	18.853261
44.089713	1521.076143	18.858279
44.395223	1527.955672	18.863296
44.326264	1546.630947	18.868314
44.749150	1541.635090	18.873331
44.748976	1534.714098	18.878349
44.930010	1537.052750	18.883367
44.949812	1537.923887	18.888384
44.830974	1534.108031	18.893402
44.878880	1535.293518	18.898419
44.916189	1543.540583	18.903437
44.925257	1539.761493	18.908455
45.287293	1542.993332	18.913472
44.908215	1519.698551	18.918490
45.084968	1506.835559	18.923507
44.788609	1519.783634	18.928525
44.987062	1522.397281	18.933543
45.146489	1527.699619	18.938560
45.220086	1531.456355	18.943578
45.622803	1535.114187	18.948595
45.203235	1544.196580	18.953613
45.019877	1539.033762	18.958631
45.407576	1534.832414	18.963648
45.441824	1535.073248	18.968666
45.729957	1526.181944	18.973683
45.420080	1537.046052	18.978701
45.611255	1533.664489	18.983719
45.392537	1537.129335	18.988736
45.683193	1538.393561	18.993754
45.622673	1536.765126	18.998771
45.651031	1535.510951	19.003789
45.668102	1532.424924	19.008807
45.784102	1537.229113	19.013824
45.517527	1532.357061	19.018842
45.712224	1527.068738	19.023859
45.614089	1531.729742	19.028877
45.520596	1539.097845	19.033895
45.943874	1543.812866	19.038912
45.770869	1558.407998	19.043930
45.993008	1561.608107	19.048947
45.963285	1552.981197	19.053965
46.008282	1554.419619	19.058983
46.217484	1555.661892	19.064000
45.955058	1552.982589	19.069018
46.120418	1557.981033	19.074035
45.857813	1570.431524	19.079053
46.129539	1580.866845	19.084071
46.296599	1582.039978	19.089088
46.306463	1582.019531	19.094106
46.457570	1572.064015	19.099123
46.270739	1580.052708	19.104141
46.617034	1581.800552	19.109159
47.164239	1582.314489	19.114176
46.855763	1585.664013	19.119194
47.102284	1575.002386	19.124211
46.634919	1569.625266	19.129229
47.033514	1568.044823	19.134247
47.079609	1567.071905	19.139264
47.189141	1564.690950	19.144282
47.348629	1567.519002	19.149299
47.170088	1571.558261	19.154317
46.899332	1570.975832	19.159335
47.438961	1575.297070	19.164352
47.166934	1578.539890	19.169370
47.601610	1580.592641	19.174387
47.373279	1580.587422	19.179405
47.345470	1579.477751	19.184423
47.513505	1585.125916	19.189440
47.520502	1606.254177	19.194458
47.629067	1598.312519	19.199475
47.358629	1600.519931	19.204493
47.402257	1603.839540	19.209511
47.707032	1595.283285	19.214528
47.939992	1589.266229	19.219546
47.221613	1591.979347	19.224563
47.512401	1594.054644	19.229581
47.290580	1592.375733	19.234599
47.645685	1591.067204	19.239616
47.742094	1614.289663	19.244634
47.832774	1613.855744	19.249651
47.988861	1612.354321	19.254669
48.147092	1612.133893	19.259687
48.542032	1607.164488	19.264704
48.260142	1607.650526	19.269722
48.388802	1604.909942	19.274739
48.488883	1606.229278	19.279757
48.430445	1610.710503	19.284775
48.778072	1594.175511	19.289792
48.239863	1593.451937	19.294810
48.460689	1601.853323	19.299827
48.429878	1606.320751	19.304845
48.501264	1606.151801	19.309863
48.802653	1604.371978	19.314880
48.434383	1606.335928	19.319898
48.386450	1606.936798	19.324915
48.476648	1602.971405	19.329933
48.198097	1606.843294	19.334951
48.986488	1605.012417	19.339968
48.539384	1610.274101	19.344986
49.033818	1607.791807	19.350003
49.155862	1634.983665	19.355021
48.824793	1635.979212	19.360039
49.230786	1624.538288	19.365056
49.181871	1641.660930	19.370074
49.378545	1638.849721	19.375091
49.329123	1643.711416	19.380109
49.235803	1634.886135	19.385127
49.579850	1630.435968	19.390144
49.464347	1643.709269	19.395162
49.607264	1637.078262	19.400179
49.712815	1634.524341	19.405197
49.456841	1637.341753	19.410215
49.705572	1629.333938	19.415232
49.468195	1636.923452	19.420250
49.458868	1634.176078	19.425267
49.889186	1630.397246	19.430285
49.779662	1637.064116	19.435303
49.726359	1629.775847	19.440320
49.416065	1637.395723	19.445338
49.552377	1635.837432	19.450355
49.565711	1637.656385	19.455373
49.454969	1645.475386	19.460391
49.488804	1644.614844	19.465408
49.759975	1657.669773	19.470426
49.664973	1662.270355	19.475443
50.032765	1667.284453	19.480461
50.013290	1672.416036	19.485479
50.150603	1670.999606	19.490496
50.077940	1672.885688	19.495514
49.885302	1679.420419	19.500531
50.125628	1668.096947	19.505549
49.971011	1688.300670	19.510567
50.301013	1690.319338	19.515584
50.371809	1696.898014	19.520602
50.155657	1696.935070	19.525619
50.726449	1694.614381	19.530637
50.487938	1701.257299	19.535655
51.029384	1707.317243	19.540672
50.981088	1723.628773	19.545690
51.043634	1720.589241	19.550707
51.136647	1717.418696	19.555725
51.259551	1717.844471	19.560743
51.328198	1716.946912	19.565760
51.391431	1708.248555	19.570778
51.306387	1696.142858	19.575795
50.978021	1701.789933	19.580813
51.380852	1711.882878	19.585831
51.846117	1714.438970	19.590848
51.580035	1708.777790	19.595866
51.100015	1696.358411	19.600883
51.501914	1702.320289	19.605901
51.556979	1709.958695	19.610919
51.701916	1720.915768	19.615936
51.234875	1716.580035	19.620954
51.398652	1715.762252	19.625971
51.530625	1713.251520	19.630989
51.409499	1717.212384	19.636007
51.800612	1708.778256	19.641024
51.437065	1709.848328	19.646042
51.736568	1713.989457	19.651059
51.782175	1719.991383	19.656077
51.626868	1736.433307	19.661095
52.227392	1740.817633	19.666112
51.974664	1745.916350	19.671130
52.032469	1738.440205	19.676147
52.030048	1739.437918	19.681165
52.291565	1746.330736	19.686183
52.357724	1737.777083	19.691200
52.174535	1743.395114	19.696218
52.238058	1751.461430	19.701235
52.544758	1759.410751	19.706253
52.824080	1763.880123	19.711271
52.920726	1769.719424	19.716288
52.780774	1774.718423	19.721306
52.932800	1771.286141	19.726323
52.955308	1770.386340	19.731341
52.738776	1766.895030	19.736359
52.999013	1768.640597	19.741376
53.013581	1764.352480	19.746394
53.227898	1769.295972	19.751411
53.045606	1764.126610	19.756429
53.293561	1759.606255	19.761447
53.190759	1754.108840	19.766464
53.511611	1755.169521	19.771482
53.515023	1769.124918	19.776499
53.090571	1755.611122	19.781517
53.179795	1764.304621	19.786535
53.440862	1759.037392	19.791552
53.437229	1754.537520	19.796570
52.985944	1754.652444	19.801587
53.382437	1754.306317	19.806605
52.970001	1756.157273	19.811623
53.447213	1769.725992	19.816640
53.826442	1775.861871	19.821658
54.211401	1773.106354	19.826675
53.951026	1766.516393	19.831693
54.097052	1768.017904	19.836711
54.313192	1764.610294	19.841728
54.282043	1768.465548	19.846746
54.406804	1773.959595	19.851763
54.434463	1767.040465	19.856781
54.378525	1746.178544	19.861799
54.505246	1745.398126	19.866816
54.141877	1735.182276	19.871834
54.012849	1745.951899	19.876851
54.461913	1750.946976	19.881869
54.437602	1764.894089	19.886887
54.899414	1769.019270	19.891904
54.634476	1764.273138	19.896922
54.641477	1769.337480	19.901939
55.038756	1758.860421	19.906957
54.729444	1774.774207	19.911975
54.827996	1767.383191	19.916992
54.591519	1776.370738	19.922010
54.677986	1768.527148	19.927027
54.738219	1765.402758	19.932045
54.701990	1765.073931	19.937063
54.566376	1765.679075	19.942080
54.688551	1760.929101	19.947098
54.905670	1773.762194	19.952115
55.097784	1782.651035	19.957133
55.052835	1792.053581	19.962151
54.924778	1782.040694	19.967168
55.042444	1786.308166	19.972186
55.006565	1785.064038	19.977203
54.981113	1786.734438	19.982221
55.379672	1805.387231	19.987239
55.026265	1812.070283	19.992256
55.449827	1819.471109	19.997274
55.311984	1823.033800	20.002291
55.731627	1822.216953	20.007309
55.340423	1822.060514	20.012327
55.512022	1827.017027	20.017344
56.003664	1843.427121	20.022362
55.873320	1845.265450	20.027379
55.902227	1847.413368	20.032397
55.990099	1850.034920	20.037415
55.954933	1862.781362	20.042432
56.073829	1848.103004	20.047450
55.577801	1850.547776	20.052467
56.002205	1859.693771	20.057485
55.925400	1861.081869	20.062503
56.255515	1866.319693	20.067520
56.174450	1862.737707	20.072538
55.865128	1870.319656	20.077555
56.378150	1876.302054	20.082573
56.619033	1898.353449	20.087591
56.813355	1894.478983	20.092608
57.350142	1888.480502	20.097626
57.082859	1893.341682	20.102643
57.117415	1890.401188	20.107661
57.527693	1887.553317	20.112679
57.185855	1869.592260	20.117696
57.206713	1858.505040	20.122714
57.128627	1863.522775	20.127731
57.281186	1850.893718	20.132749
57.053012	1853.119787	20.137767
57.165940	1862.797457	20.142784
57.275670	1871.591944	20.147802
57.381405	1889.448042	20.152819
57.795454	1880.984992	20.157837
57.508190	1890.049985	20.162855
57.505811	1881.759485	20.167872
57.486720	1883.337372	20.172890
56.938935	1894.867021	20.177907
57.317382	1886.734619	20.182925
57.648197	1893.575608	20.187943
57.307920	1901.825187	20.192960
58.039722	1903.623127	20.197978
58.067079	1905.872287	20.202995
58.078197	1907.628494	20.208013
58.062819	1912.273474	20.213031
57.725589	1913.784434	20.218048
57.678367	1910.389655	20.223066
57.762103	1923.212192	20.228083
57.981409	1929.537295	20.233101
58.139890	1924.121977	20.238119
58.416820	1930.823089	20.243136
58.502452	1935.998244	20.248154
58.422299	1927.808277	20.253171
58.312766	1928.488241	20.258189
58.442606	1927.467467	20.263207
58.452564	1940.964346	20.268224
58.887550	1942.234392	20.273242
58.834815	1950.719831	20.278259
59.011733	1954.252169	20.283277
59.181759	1951.656542	20.288295
59.004139	1951.476106	20.293312
58.935866	1948.857849	20.298330
58.854211	1945.812467	20.303347
59.224091	1950.753729	20.308365
59.290178	1942.348324	20.313383
59.141839	1949.980829	20.318400
59.255776	1945.225785	20.323418
59.620119	1951.821684	20.328435
59.510556	1946.565129	20.333453
59.354920	1949.736127	20.338471
59.307969	1950.721892	20.343488
59.361628	1942.122759	20.348506
59.460899	1957.063750	20.353523
59.510201	1967.669856	20.358541
59.839307	1967.015522	20.363559
59.570815	1973.218234	20.368576
59.805746	1975.062468	20.373594
59.532765	1967.761140	20.378611
59.833301	1974.146121	20.383629
60.069583	1981.854089	20.388647
60.058415	1994.136080	20.393664
60.167757	1999.642081	20.398682
60.120100	2004.396292	20.403699
60.367169	2005.304434	20.408717
60.373855	1998.795632	20.413735
60.148820	2004.584415	20.418752
60.471247	1997.379153	20.423770
60.291377	2011.761117	20.428787
60.619900	2011.633934	20.433805
61.111191	2015.924982	20.438823
60.780211	2018.845730	20.443840
61.153577	2024.102073	20.448858
60.987552	2015.502608	20.453875
61.035226	2013.734092	20.458893
61.354915	2010.509044	20.463911
61.178056	2015.867371	20.468928
61.609687	2011.655874	20.473946
61.125050	2017.198133	20.478963
61.337124	2024.935161	20.483981
61.248456	2017.712241	20.488999
61.166358	2022.187807	20.494016
61.177958	2012.272841	20.499034
61.171754	2010.774720	20.504051
61.414680	2005.412424	20.509069
61.611546	2005.880272	20.514087
61.310884	2023.317298	20.519104
61.508472	2031.119719	20.524122
61.635454	2037.320458	20.529139
61.608432	2045.767197	20.534157
61.746527	2042.800987	20.539175
61.717442	2047.025236	20.544192
61.944266	2054.595851	20.549210
62.365644	2067.681198	20.554227
62.262379	2062.458339	20.559245
62.001360	2067.198653	20.564263
62.121821	2067.811028	20.569280
62.270434	2065.436508	20.574298
62.139679	2071.728136	20.579315
62.652803	2068.548518	20.584333
62.658146	2064.511104	20.589351
62.586434	2070.695643	20.594368
62.599927	2055.067873	20.599386
62.443264	2063.929440	20.604403
62.673606	2075.173176	20.609421
63.036157	2076.587136	20.614439
62.278351	2076.462882	20.619456
62.586344	2071.153494	20.624474
62.331612	2084.944436	20.629491
62.734373	2096.508339	20.634509
63.330677	2099.981311	20.639527
63.146796	2110.816555	20.644544
63.518877	2112.014413	20.649562
63.602708	2110.947183	20.654579
63.665674	2101.721613	20.659597
63.685007	2105.247110	20.664615
63.703153	2109.650183	20.669632
64.175780	2105.678415	20.674650
64.075748	2111.760099	20.679667
63.722367	2111.935430	20.684685
63.918932	2108.300429	20.689703
63.781668	2117.544025	20.694720
64.070968	2109.157223	20.699738
64.124327	2112.292349	20.704755
63.972129	2113.506070	20.709773
63.814741	2101.973215	20.714791
63.821990	2108.255859	20.719808
63.883797	2099.847894	20.724826
63.808051	2114.314621	20.729843
63.965456	2124.761859	20.734861
64.337410	2129.216811	20.739879
64.475711	2140.187804	20.744896
64.360591	2137.690478	20.749914
64.398891	2132.830461	20.754931
64.445699	2138.576696	20.759949
64.924502	2140.243871	20.764967
64.504394	2155.462077	20.769984
64.953239	2162.657095	20.775002
65.006065	2156.797473	20.780019
64.815460	2154.741198	20.785037
64.901729	2156.507748	20.790055
65.045002	2159.464679	20.795072
65.285587	2156.223594	20.800090
64.826055	2162.071260	20.805107
64.964698	2165.508642	20.810125
65.601833	2169.126723	20.815143
65.540998	2178.822320	20.820160
65.669876	2172.240657	20.825178
65.730015	2179.162037	20.830195
65.367170	2171.066746	20.835213
65.652679	2169.623902	20.840231
65.875610	2180.067219	20.845248
65.816560	2176.983538	20.850266
65.762356	2181.767226	20.855283
66.021831	2196.206747	20.860301
66.111869	2201.356040	20.865319
65.896596	2201.314056	20.870336
66.205856	2206.328010	20.875354
65.996366	2199.430087	20.880371
66.104090	2197.686862	20.885389
66.444197	2196.251243	20.890407
66.606451	2201.502841	20.895424
66.559366	2201.254609	20.900442
66.805345	2213.139824	20.905459
66.705846	2222.648980	20.910477
67.018699	2215.770209	20.915495
67.279387	2222.862175	20.920512
67.250338	2212.022419	20.925530
67.134470	2204.806842	20.930547
66.572358	2194.830168	20.935565
66.990179	2201.774420	20.940583
67.079091	2208.322040	20.945600
67.113805	2216.844402	20.950618
67.207446	2218.429905	20.955635
67.081609	2218.304474	20.960653
67.466239	2209.195726	20.965671
67.344754	2207.860830	20.970688
67.652320	2206.632298	20.975706
67.571636	2204.634542	20.980723
67.387670	2213.705606	20.985741
67.643722	2209.941333	20.990759
67.966419	2227.915268	20.995776
68.275311	2239.456097	21.000794
67.823679	2234.199397	21.005811
68.000883	2235.677127	21.010829
68.552163	2229.660483	21.015847
68.118318	2230.154562	21.020864
68.128692	2232.971366	21.025882
68.135789	2228.422353	21.030899
67.925375	2243.068087	21.035917
68.437498	2233.140858	21.040935
68.448946	2231.453743	21.045952
67.963342	2236.541742	21.050970
67.947749	2245.469667	21.055987
68.316860	2260.548531	21.061005
68.603021	2262.305866	21.066023
68.511116	2255.982847	21.071040
68.985617	2269.915323	21.076058
68.961183	2277.680046	21.081075
68.795881	2291.176242	21.086093
68.813892	2281.073913	21.091111
68.878102	2291.845148	21.096128
68.955984	2279.555725	21.101146
69.351976	2281.775582	21.106163
69.214246	2285.306786	21.111181
69.531503	2295.751172	21.116199
69.252221	2303.379092	21.121216
69.429715	2314.555511	21.126234
69.955230	2295.198847	21.131251
69.604206	2309.696235	21.136269
69.883998	2294.219058	21.141287
70.025286	2311.003240	21.146304
69.991440	2308.685680	21.151322
69.678675	2306.620122	21.156339
69.655387	2314.236345	21.161357
69.818998	2321.062665	21.166375
70.490794	2329.049722	21.171392
70.332409	2324.640231	21.176410
70.398619	2336.124461	21.181427
70.486514	2336.571518	21.186445
70.602867	2329.780300	21.191463
70.790864	2326.806226	21.196480
70.963798	2322.054464	21.201498
70.974215	2320.932446	21.206515
71.301591	2320.350963	21.211533
71.175537	2309.305418	21.216551
71.142383	2312.242674	21.221568
71.309978	2311.960806	21.226586
71.288387	2312.541791	21.231603
70.965413	2318.898339	21.236621
71.136566	2308.074501	21.241639
71.191675	2317.777256	21.246656
70.839812	2319.602997	21.251674
71.494931	2318.982789	21.256691
71.246011	2342.111956	21.261709
71.435661	2344.398867	21.266727
71.318059	2350.281393	21.271744
71.445718	2350.857933	21.276762
71.690347	2350.036923	21.281779
71.504952	2348.469009	21.286797
71.715240	2355.089194	21.291815
71.524079	2366.550644	21.296832
71.702855	2367.674653	21.301850
72.113207	2365.811407	21.306867
72.021409	2366.337115	21.311885
71.866126	2368.352991	21.316903
72.112437	2378.088945	21.321920
71.927869	2393.494533	21.326938
72.282577	2387.287706	21.331955
72.493296	2388.981127	21.336973
72.474412	2383.934321	21.341991
72.864296	2390.460103	21.347008
72.460063	2391.454527	21.352026
72.919511	2401.463244	21.357043
72.832146	2417.106114	21.362061
73.005217	2413.796658	21.367079
72.954339	2411.923611	21.372096
72.905580	2413.307357	21.377114
73.311882	2416.122124	21.382131
73.003601	2411.502543	21.387149
72.997561	2410.531436	21.392167
73.437919	2414.827405	21.397184
73.347245	2425.095912	21.402202
73.648677	2423.306536	21.407219
73.833747	2431.117405	21.412237
73.900153	2434.076956	21.417255
74.024275	2427.382325	21.422272
74.060396	2433.095611	21.427290
74.084729	2439.684995	21.432307
74.177731	2437.202362	21.437325
74.357679	2430.634697	21.442343
74.231777	2438.125023	21.447360
74.012625	2439.611214	21.452378
74.497177	2427.043359	21.457395
74.044610	2434.761607	21.462413
74.450262	2428.388978	21.467431
74.398503	2433.203911	21.472448
74.317829	2453.662023	21.477466
74.255887	2445.437405	21.482483
74.581218	2461.807845	21.487501
74.606944	2460.686576	21.492519
74.589482	2455.364943	21.497536
74.496800	2470.932945	21.502554
74.832021	2478.442570	21.507571
74.543282	2479.702956	21.512589
74.480112	2486.353409	21.517607
75.091287	2493.131767	21.522624
75.421177	2501.027286	21.527642
76.089250	2491.018673	21.532659
76.281160	2496.290961	21.537677
76.321666	2485.739977	21.542695
76.363986	2463.208011	21.547712
76.188091	2462.973644	21.552730
76.431866	2461.303762	21.557747
76.061872	2450.334223	21.562765
76.291987	2454.571613	21.567783
76.419477	2449.924778	21.572800
76.553349	2453.927912	21.577818
76.644384	2444.246441	21.582835
76.627739	2452.278291	21.587853
76.678681	2456.187109	21.592871
76.878609	2446.065654	21.597888
76.726947	2451.110861	21.602906
76.999637	2442.363552	21.607923
76.885604	2451.164976	21.612941
76.846571	2447.229113	21.617959
77.227423	2445.285266	21.622976
76.621264	2447.968299	21.627994
76.874759	2443.560527	21.633011
76.637961	2446.286688	21.638029
76.622215	2443.527572	21.643047
77.100374	2447.827094	21.648064
76.869930	2451.975678	21.653082
76.767559	2460.153520	21.658099
77.141224	2473.868400	21.663117
77.229970	2480.542391	21.668135
77.057506	2467.020138	21.673152
77.026900	2496.550668	21.678170
77.344952	2503.504356	21.683187
77.363451	2509.343517	21.688205
77.384931	2509.434871	21.693223
77.591669	2518.457500	21.698240
77.659785	2540.053861	21.703258
78.055952	2527.184169	21.708275
78.001230	2534.281489	21.713293
77.911687	2533.932595	21.718311
78.161150	2548.301377	21.723328
77.989889	2558.279595	21.728346
78.539263	2553.778099	21.733363
78.583925	2555.043066	21.738381
78.351771	2559.611710	21.743399
78.846239	2553.572299	21.748416
78.712439	2558.223374	21.753434
78.816592	2573.271422	21.758451
78.621298	2582.707404	21.763469
78.610076	2581.178460	21.768487
78.611588	2579.877920	21.773504
78.803544	2590.843939	21.778522
79.037639	2603.829619	21.783539
79.308582	2616.355047	21.788557
79.265211	2618.953088	21.793575
79.437608	2610.578057	21.798592
79.166897	2612.170181	21.803610
79.301440	2625.969983	21.808627
79.706758	2626.496719	21.813645
79.590673	2643.040635	21.818663
79.980668	2633.530000	21.823680
79.617264	2640.416917	21.828698
79.959259	2644.889317	21.833715
80.000232	2646.041247	21.838733
80.266352	2671.640329	21.843751
80.389983	2659.513913	21.848768
80.357329	2656.735320	21.853786
80.413967	2658.033136	21.858803
80.870855	2650.503556	21.863821
80.672794	2661.186700	21.868839
80.700019	2655.356175	21.873856
80.674274	2650.322994	21.878874
81.017250	2659.905085	21.883891
81.242453	2666.482019	21.888909
81.107333	2679.124764	21.893927
81.329868	2670.909128	21.898944
81.266390	2679.027321	21.903962
81.375648	2680.443142	21.908979
81.737137	2673.345114	21.913997
81.470230	2685.096377	21.919015
81.785072	2664.222643	21.924032
81.702231	2667.382361	21.929050
81.582686	2661.293930	21.934067
81.801460	2668.095959	21.939085
81.778481	2661.171794	21.944103
82.216285	2661.620849	21.949120
82.181119	2668.150202	21.954138
82.300061	2657.694138	21.959155
82.356364	2663.947198	21.964173
82.059728	2675.194968	21.969191
82.389089	2683.317896	21.974208
82.335563	2684.165859	21.979226
82.155562	2685.065199	21.984243
82.648343	2680.705097	21.989261
82.514371	2686.552423	21.994279
82.970077	2675.185108	21.999296
82.803795	2682.479866	22.004314
83.104266	2686.924064	22.009331
82.904796	2682.647169	22.014349
82.509838	2693.528458	22.019367
82.810288	2697.802228	22.024384
83.301511	2710.908666	22.029402
82.919522	2717.479750	22.034419
83.019586	2717.369422	22.039437
82.720297	2724.287357	22.044455
83.267207	2736.731758	22.049472
83.403497	2745.115364	22.054490
83.545120	2738.335815	22.059507
84.042625	2738.027503	22.064525
84.079521	2750.330886	22.069543
84.194507	2751.215575	22.074560
84.070862	2759.532602	22.079578
84.111528	2763.654562	22.084595
84.035352	2754.125370	22.089613
84.198266	2758.086147	22.094631
84.236516	2758.045470	22.099648
84.197766	2753.326761	22.104666
84.072000	2769.525129	22.109683
84.538782	2771.134282	22.114701
84.820555	2777.004875	22.119719
84.867212	2786.917516	22.124736
85.002608	2787.028898	22.129754
84.755934	2785.287485	22.134771
84.875846	2791.953553	22.139789
85.152854	2789.580916	22.144807
85.364435	2800.070559	22.149824
85.484262	2800.054976	22.154842
85.589251	2804.229991	22.159859
85.918765	2808.846417	22.164877
85.615539	2801.356958	22.169895
85.776508	2789.937906	22.174912
86.185184	2795.340443	22.179930
86.194086	2798.962396	22.184947
86.040115	2796.404784	22.189965
86.082020	2798.048944	22.194983
86.370940	2788.560376	22.200000
86.258111	2797.298655	22.205018
86.094563	2800.190140	22.210035
86.912563	2803.268713	22.215053
86.922104	2809.251404	22.220071
86.568011	2799.418547	22.225088
86.729795	2799.434265	22.230106
86.710889	2807.277256	22.235123
86.897966	2804.890301	22.240141
86.381192	2817.618188	22.245159
86.769227	2817.835174	22.250176
86.565863	2827.976380	22.255194
86.682239	2838.717677	22.260211
87.102112	2836.076467	22.265229
87.060460	2852.577352	22.270247
87.268418	2842.479667	22.275264
87.549751	2859.731632	22.280282
87.154658	2866.153325	22.285299
87.810537	2869.478244	22.290317
87.476026	2884.936150	22.295335
87.703116	2874.690264	22.300352
87.868105	2873.865928	22.305370
87.571930	2887.174762	22.310387
88.443637	2882.430156	22.315405
88.147115	2899.428666	22.320423
88.078060	2899.423738	22.325440
88.175962	2900.431047	22.330458
87.806814	2896.076529	22.335475
88.206793	2901.963362	22.340493
87.915643	2901.794389	22.345511
88.473107	2913.290395	22.350528
88.605822	2915.983984	22.355546
88.668060	2923.647032	22.360563
89.390382	2927.296112	22.365581
89.097609	2945.146256	22.370599
88.749263	2951.008316	22.375616
89.216862	2943.723123	22.380634
89.169312	2941.824249	22.385651
89.543725	2944.669348	22.390669
89.735657	2947.782909	22.395687
89.741130	2943.271845	22.400704
89.745343	2935.926692	22.405722
89.355788	2956.105520	22.410739
89.775265	2959.622149	22.415757
89.785848	2963.306996	22.420775
89.891353	2961.532483	22.425792
89.986114	2954.261511	22.430810
90.058923	2970.978132	22.435827
90.621125	2972.796447	22.440845
90.318829	2990.629190	22.445863
90.471799	2979.154459	22.450880
90.671853	2975.449302	22.455898
90.747243	2985.935140	22.460915
90.868258	2982.264458	22.465933
90.513022	2977.699430	22.470951
90.749770	2987.765461	22.475968
91.025388	2998.040031	22.480986
91.200162	3003.349872	22.486003
91.544274	2998.062961	22.491021
91.422547	3005.104683	22.496039
90.962136	3001.663964	22.501056
91.316140	3014.710060	22.506074
91.518030	3032.817352	22.511091
91.920572	3025.242476	22.516109
92.256050	3029.087902	22.521127
91.919276	3027.641487	22.526144
92.276401	3032.307301	22.531162
91.860514	3026.546079	22.536179
92.170894	3023.836779	22.541197
92.368714	3035.739553	22.546215
92.488422	3031.472537	22.551232
92.568595	3037.747236	22.556250
92.126822	3042.424592	22.561267
92.717764	3044.595066	22.566285
92.797757	3047.590465	22.571303
92.860077	3051.024194	22.576320
93.308583	3054.533137	22.581338
93.276527	3054.623413	22.586355
93.277381	3050.356075	22.591373
92.989636	3057.067172	22.596391
93.240925	3059.044676	22.601408
93.287670	3052.295655	22.606426
93.129042	3065.251665	22.611443
93.661950	3071.067228	22.616461
93.657765	3071.737041	22.621479
93.526073	3072.366863	22.626496
93.529025	3074.395900	22.631514
93.331941	3084.384767	22.636531
93.687779	3090.774108	22.641549
93.787182	3094.568161	22.646567
93.950743	3089.113823	22.651584
94.120197	3112.137398	22.656602
94.256657	3122.339154	22.661619
94.147820	3122.870710	22.666637
94.600151	3121.306969	22.671655
94.663351	3123.408635	22.676672
94.931539	3108.724799	22.681690
94.375440	3127.888348	22.686707
95.155838	3130.429995	22.691725
94.963896	3132.701042	22.696743
94.916126	3142.590798	22.701760
95.660369	3141.205416	22.706778
95.522207	3146.419139	22.711795
95.618046	3138.497735	22.716813
96.407304	3120.759060	22.721831
96.063394	3117.079128	22.726848
96.201559	3121.946552	22.731866
96.591905	3125.076402	22.736883
96.620297	3118.844701	22.741901
96.706947	3104.672217	22.746919
96.365911	3095.244308	22.751936
96.377517	3086.392406	22.756954
96.389231	3083.104952	22.761971
95.998892	3095.188288	22.766989
96.734398	3103.790650	22.772007
96.593253	3114.540895	22.777024
96.470899	3107.411189	22.782042
96.506670	3106.979525	22.787059
96.504548	3109.735299	22.792077
96.934537	3123.527071	22.797095
96.648113	3146.644206	22.802112
96.781147	3139.073632	22.807130
96.914394	3149.708314	22.812147
96.932560	3164.571483	22.817165
97.235707	3166.278904	22.822183
97.146101	3180.814939	22.827200
97.203674	3177.255158	22.832218
97.492861	3189.323626	22.837235
97.165228	3194.418702	22.842253
97.582983	3205.482283	22.847271
97.614964	3210.918713	22.852288
98.054063	3217.414994	22.857306
98.007783	3224.536512	22.862323
98.325672	3222.034321	22.867341
98.464473	3211.928327	22.872359
98.187524	3223.586824	22.877376
98.724119	3238.974836	22.882394
98.610233	3251.100183	22.887411
98.836225	3239.222469	22.892429
99.401912	3242.473214	22.897447
99.027921	3245.192581	22.902464
99.324592	3236.087630	22.907482
99.440683	3245.702425	22.912499
99.185948	3246.982784	22.917517
99.578529	3257.431711	22.922535
99.494027	3269.467247	22.927552
99.654273	3269.369581	22.932570
99.574280	3272.172299	22.937587
99.490171	3270.787279	22.942605
99.825252	3268.171918	22.947623
100.177447	3295.361791	22.952640
99.946773	3298.418528	22.957658
99.628105	3297.568948	22.962675
100.028799	3301.217995	22.967693
100.049831	3304.137454	22.972711
100.443944	3329.518573	22.977728
100.598379	3324.766291	22.982746
100.704387	3325.636635	22.987763
100.738532	3328.673982	22.992781
101.260165	3327.740094	22.997799
101.260314	3325.739018	23.002816
101.230312	3315.937167	23.007834
101.262380	3326.767713	23.012851
101.523073	3341.653001	23.017869
101.635218	3342.244630	23.022887
101.497768	3347.309953	23.027904
102.101535	3343.591972	23.032922
101.855987	3344.268047	23.037939
101.823187	3343.916560	23.042957
101.840200	3341.167955	23.047975
102.144635	3347.811632	23.052992
101.756263	3336.875993	23.058010
102.038691	3342.345820	23.063027
102.271110	3351.674161	23.068045
102.325925	3365.625898	23.073063
102.334189	3361.316294	23.078080
102.410129	3362.144005	23.083098
102.726221	3362.179738	23.088115
102.669210	3362.706336	23.093133
103.162794	3382.116018	23.098151
102.804435	3393.389684	23.103168
102.968928	3380.091709	23.108186
103.391639	3396.687623	23.113203
103.075608	3393.123206	23.118221
103.348819	3386.404862	23.123239
103.299496	3407.319962	23.128256
103.298186	3414.447135	23.133274
103.814439	3416.364229	23.138291
103.832634	3420.461453	23.143309
104.236381	3412.668442	23.148327
103.918863	3431.349893	23.153344
103.995086	3435.040335	23.158362
104.461325	3427.764631	23.163379
104.166148	3429.174435	23.168397
104.616227	3428.734667	23.173415
104.519787	3432.303813	23.178432
104.386959	3449.109907	23.183450
104.914719	3449.649051	23.188467
104.488788	3460.494618	23.193485
104.713093	3456.716125	23.198503
104.882094	3476.381920	23.203520
105.262887	3479.592239	23.208538
105.563328	3481.811438	23.213555
105.333817	3485.527694	23.218573
105.687944	3478.891329	23.223591
105.582388	3488.484164	23.228608
105.446044	3487.050497	23.233626
105.793427	3497.544521	23.238643
105.697708	3508.878114	23.243661
106.084747	3508.381939	23.248679
105.979333	3511.264428	23.253696
106.275322	3518.963703	23.258714
106.709261	3522.115202	23.263731
106.752277	3528.184419	23.268749
106.622650	3521.238757	23.273767
106.759916	3525.992803	23.278784
106.760129	3528.360046	23.283802
107.111435	3517.949146	23.288819
107.048199	3525.998242	23.293837
107.076882	3529.251109	23.298855
107.721695	3541.137844	23.303872
107.846850	3540.130340	23.308890
108.061874	3544.641797	23.313907
107.559183	3552.649282	23.318925
107.837412	3536.978753	23.323943
107.964197	3544.489918	23.328960
107.988259	3536.854186	23.333978
108.011331	3534.410766	23.338995
108.020545	3543.193412	23.344013
108.122128	3540.286336	23.349031
108.106111	3545.345315	23.354048
107.699349	3557.459937	23.359066
108.097861	3571.288546	23.364083
108.150987	3574.060986	23.369101
108.679424	3583.118970	23.374119
108.367292	3585.443623	23.379136
108.584332	3601.986727	23.384154
108.903215	3591.107414	23.389171
109.185967	3616.080278	23.394189
109.815891	3619.422033	23.399207
109.489069	3622.639079	23.404224
109.349077	3614.359873	23.409242
109.602201	3616.349776	23.414259
109.754464	3623.667603	23.419277
109.791526	3613.375319	23.424295
109.837682	3618.522425	23.429312
109.785181	3636.796432	23.434330
109.884135	3636.149694	23.439347
110.396525	3637.903288	23.444365
110.861792	3634.958158	23.449383
110.804849	3638.555875	23.454400
110.463260	3631.469779	23.459418
111.018917	3634.715857	23.464435
110.596370	3648.834134	23.469453
110.766325	3654.179641	23.474471
110.916360	3658.672902	23.479488
110.952391	3663.509128	23.484506
111.312402	3665.472822	23.489523
111.059690	3686.663148	23.494541
111.583790	3678.923765	23.499559
111.571586	3689.420579	23.504576
111.450887	3684.102133	23.509594
111.940305	3682.977582	23.514611
112.388338	3704.228587	23.519629
112.275520	3702.207291	23.524647
112.613526	3703.423225	23.529664
112.231881	3696.984119	23.534682
112.618364	3702.122118	23.539699
112.458065	3706.395720	23.544717
112.346919	3703.815487	23.549735
112.776577	3713.412968	23.554752
112.900471	3728.856588	23.559770
113.206938	3728.685511	23.564787
113.244946	3728.285046	23.569805
113.435674	3729.997509	23.574823
113.597437	3725.389167	23.579840
113.331358	3729.830852	23.584858
113.333384	3724.717268	23.589875
113.715847	3740.470744	23.594893
113.826524	3741.226747	23.599911
114.358971	3741.225430	23.604928
114.387639	3747.082336	23.609946
114.515222	3732.445275	23.614963
114.495082	3734.613728	23.619981
114.863505	3733.473410	23.624999
114.947365	3725.326369	23.630016
114.645876	3730.761542	23.635034
114.669607	3724.432515	23.640051
114.628428	3732.481404	23.645069
115.025655	3728.991399	23.650087
114.692739	3739.667898	23.655104
114.807370	3762.716674	23.660122
114.974214	3751.589637	23.665139
115.030033	3753.904009	23.670157
115.114443	3769.713676	23.675175
115.362470	3768.418618	23.680192
115.634340	3783.264644	23.685210
115.663361	3781.132739	23.690227
115.561548	3784.942679	23.695245
116.007715	3792.164027	23.700263
115.660023	3803.903419	23.705280
115.796470	3811.807728	23.710298
116.259704	3812.953549	23.715315
116.307662	3829.491788	23.720333
116.195308	3832.536390	23.725351
116.274178	3829.014177	23.730368
116.478057	3843.198595	23.735386
116.912812	3849.689473	23.740403
117.104389	3856.994922	23.745421
117.244155	3844.126593	23.750439
117.696932	3850.987101	23.755456
117.255470	3855.999190	23.760474
117.865686	3863.469471	23.765491
117.637628	3875.815130	23.770509
117.530951	3871.359281	23.775527
118.010816	3876.735212	23.780544
117.767033	3878.550484	23.785562
117.680644	3881.067066	23.790579
118.201526	3892.007596	23.795597
118.496578	3895.622815	23.800615
118.411795	3891.927377	23.805632
118.473672	3901.831932	23.810650
118.708258	3915.433977	23.815667
118.507303	3920.263210	23.820685
118.657253	3926.438908	23.825703
118.966276	3921.602280	23.830720
119.343671	3940.017564	23.835738
119.533154	3941.449324	23.840755
119.376970	3949.904563	23.845773
119.275011	3950.788580	23.850791
119.950499	3941.030526	23.855808
119.753084	3959.337030	23.860826
119.744221	3963.795289	23.865843
120.256735	3980.560743	23.870861
120.105488	3979.568112	23.875879
120.213161	3975.416390	23.880896
120.200015	3978.158241	23.885914
120.233012	3986.924750	23.890931
120.789343	3996.805552	23.895949
120.261680	3998.362295	23.900967
120.864587	4014.258233	23.905984
120.980796	4018.737944	23.911002
121.452961	4022.824153	23.916019
121.515597	4026.286426	23.921037
121.500600	4021.165956	23.926055
121.762160	4013.596977	23.931072
121.194766	4026.286291	23.936090
121.285410	4033.276201	23.941107
122.128986	4040.545862	23.946125
121.719428	4051.982621	23.951143
122.237521	4048.176917	23.956160
122.439278	4063.403457	23.961178
122.525687	4066.227574	23.966195
122.441249	4059.053675	23.971213
122.778628	4067.128627	23.976231
123.082616	4054.815201	23.981248
122.742560	4060.894110	23.986266
123.029620	4063.800421	23.991283
123.145427	4071.013666	23.996301
123.203790	4085.808165	24.001319
123.730565	4081.139392	24.006336
123.581672	4087.213612	24.011354
123.477942	4079.427225	24.016371
123.590648	4087.060766	24.021389
123.342068	4092.030075	24.026407
123.604856	4097.004495	24.031424
123.538181	4114.703579	24.036442
123.809092	4110.286364	24.041459
124.560516	4130.319306	24.046477
124.287181	4137.675610	24.051495
124.633791	4132.006053	24.056512
124.484711	4148.307156	24.061530
124.645524	4139.191474	24.066547
125.076268	4147.529601	24.071565
125.089502	4156.412920	24.076583
125.346176	4158.197161	24.081600
125.019146	4162.850511	24.086618
125.611514	4154.446851	24.091635
125.298145	4163.476034	24.096653
125.121826	4180.062355	24.101671
125.348740	4182.466766	24.106688
125.401388	4187.701396	24.111706
125.463838	4215.742940	24.116723
125.783720	4212.129235	24.121741
125.858983	4219.898111	24.126759
126.534732	4228.728175	24.131776
126.784325	4237.823863	24.136794
126.921030	4233.875860	24.141811
126.861685	4241.839439	24.146829
126.747309	4246.345862	24.151847
127.283753	4252.129693	24.156864
127.026649	4265.143022	24.161882
127.450566	4265.941510	24.166899
127.416203	4256.070391	24.171917
127.298602	4263.168770	24.176935
127.452823	4276.666888	24.181952
127.460433	4294.013611	24.186970
127.965605	4293.805087	24.191987
127.911393	4294.287083	24.197005
127.730636	4318.888473	24.202023
128.309975	4312.570046	24.207040
128.268215	4322.847748	24.212058
128.591015	4337.825134	24.217075
128.954077	4338.251228	24.222093
128.905640	4346.459348	24.227111
129.388782	4335.269775	24.232128
129.095315	4345.609020	24.237146
129.401424	4345.134974	24.242163
129.834554	4364.359483	24.247181
129.859841	4373.556667	24.252199
130.020991	4366.344171	24.257216
129.790227	4365.869010	24.262234
129.763993	4368.654005	24.267251
130.101376	4365.179569	24.272269
129.871197	4380.025826	24.277287
130.219145	4390.551847	24.282304
129.981189	4393.319511	24.287322
129.969184	4399.991058	24.292339
130.460500	4414.440226	24.297357
130.818631	4423.878842	24.302375
130.767494	4421.636318	24.307392
130.721964	4431.955706	24.312410
131.568300	4441.500922	24.317427
131.710948	4434.026154	24.322445
131.599292	4452.578550	24.327463
131.920489	4439.072174	24.332480
131.645096	4447.953507	24.337498
131.711113	4461.797012	24.342515
132.190078	4469.685825	24.347533
131.927653	4470.194133	24.352551
132.129002	4474.051416	24.357568
132.183530	4483.026276	24.362586
132.252780	4493.832756	24.367603
132.954367	4486.800690	24.372621
132.560900	4492.998586	24.377639
132.760572	4488.428304	24.382656
133.222125	4498.804017	24.387674
133.556961	4513.501891	24.392691
133.507924	4510.271044	24.397709
133.545398	4517.585120	24.402727
133.754692	4518.193134	24.407744
133.865306	4511.386217	24.412762
133.570214	4506.969199	24.417779
133.713737	4513.597483	24.422797
133.339267	4533.848296	24.427815
133.853104	4527.906212	24.432832
134.057146	4551.655350	24.437850
133.955402	4561.734255	24.442867
134.290914	4553.664209	24.447885
134.543886	4569.302965	24.452903
134.525956	4582.683081	24.457920
134.913812	4581.094602	24.462938
134.874231	4596.649798	24.467955
135.198819	4607.217483	24.472973
135.211819	4607.146037	24.477991
135.629462	4606.821807	24.483008
135.932178	4630.075799	24.488026
135.732412	4631.634884	24.493043
136.329769	4632.169479	24.498061
136.181751	4638.186928	24.503079
136.118447	4632.215281	24.508096
136.594828	4645.508533	24.513114
136.422487	4648.764685	24.518131
136.948107	4661.472592	24.523149
136.609312	4661.554113	24.528167
136.755328	4657.418325	24.533184
136.939058	4682.386076	24.538202
136.962332	4690.040195	24.543219
137.557975	4691.010662	24.548237
137.363008	4700.747561	24.553255
137.610711	4708.941015	24.558272
137.968884	4715.965033	24.563290
137.656888	4713.425591	24.568307
137.969146	4711.820536	24.573325
137.843099	4739.226390	24.578343
138.233755	4738.480255	24.583360
138.233351	4742.081958	24.588378
138.640813	4760.202964	24.593395
138.760864	4753.807985	24.598413
138.766977	4775.864956	24.603431
138.859120	4772.804493	24.608448
139.401831	4777.476410	24.613466
139.283908	4783.063058	24.618483
139.784487	4783.748552	24.623501
139.941075	4782.249949	24.628519
140.085604	4772.953423	24.633536
139.992774	4781.478036	24.638554
139.690008	4787.889092	24.643571
140.383261	4810.431884	24.648589
140.369724	4811.598805	24.653607
140.582836	4806.726466	24.658624
140.282756	4802.837300	24.663642
140.378026	4833.582971	24.668659
140.848863	4832.707477	24.673677
140.739429	4842.737238	24.678695
140.967746	4849.866878	24.683712
141.052723	4853.429975	24.688730
140.888963	4859.651982	24.693747
141.405666	4871.581764	24.698765
141.483061	4892.879605	24.703783
141.738172	4882.839689	24.708800
141.951939	4878.803717	24.713818
142.060283	4896.895964	24.718835
142.430828	4907.469250	24.723853
142.467395	4912.318351	24.728871
142.376154	4920.230405	24.733888
142.761732	4914.021044	24.738906
142.457092	4922.673603	24.743923
143.050277	4948.085778	24.748941
142.971866	4948.760977	24.753959
143.068979	4946.046929	24.758976
143.238705	4946.768481	24.763994
143.195272	4962.526613	24.769011
143.629332	4962.818494	24.774029
143.916984	4968.887747	24.779047
143.906793	4975.571847	24.784064
144.220487	4988.679348	24.789082
143.938047	4992.126421	24.794099
144.071148	4985.984999	24.799117
144.295752	5004.835657	24.804135
144.429341	5012.927177	24.809152
144.552530	5019.969187	24.814170
144.894036	5037.434763	24.819187
145.180335	5037.216333	24.824205
145.082505	5050.593527	24.829223
145.267072	5045.413095	24.834240
145.388405	5059.595613	24.839258
145.198095	5070.070622	24.844275
145.985644	5061.935847	24.849293
146.174064	5077.755609	24.854311
146.025802	5089.818121	24.859328
146.174906	5095.157852	24.864346
146.463874	5094.746450	24.869363
146.650902	5099.856123	24.874381
146.894233	5117.460265	24.879399
146.612981	5116.809909	24.884416
147.140928	5115.707651	24.889434
146.979531	5123.192017	24.894451
147.184113	5128.968148	24.899469
147.455512	5149.131084	24.904487
147.155550	5146.056229	24.909504
147.604413	5165.601096	24.914522
147.853433	5174.185973	24.919539
147.635516	5178.390029	24.924557
147.778717	5197.038990	24.929575
148.079622	5197.392773	24.934592
148.713291	5212.565238	24.939610
148.534073	5231.053251	24.944627
148.819126	5225.841242	24.949645
149.317510	5235.892790	24.954663
149.012831	5230.034520	24.959680
149.716760	5230.009503	24.964698
149.779120	5247.752604	24.969715
149.963343	5247.553319	24.974733
150.128527	5247.732656	24.979751
150.029931	5254.067696	24.984768
150.776007	5241.946212	24.989786
150.450683	5242.458079	24.994803
150.378920	5234.543081	24.999821
150.369649	5249.238641	25.004839
150.686645	5258.977703	25.009856
150.824241	5265.919696	25.014874
150.881176	5265.595148	25.019891
150.940184	5262.410373	25.024909
150.889909	5278.567584	25.029927
151.031849	5292.245152	25.034944
151.910071	5292.394854	25.039962
152.133108	5313.755598	25.044979
152.392980	5319.071729	25.049997
152.458579	5316.627721	25.055015
152.074921	5321.766886	25.060032
152.395358	5310.062426	25.065050
152.461649	5308.805204	25.070067
152.624377	5303.189349	25.075085
152.909120	5312.532601	25.080103
152.593878	5313.437470	25.085120
153.416270	5316.651541	25.090138
153.066905	5332.461077	25.095155
153.299860	5335.701205	25.100173
153.513460	5339.522032	25.105191
153.626104	5341.745632	25.110208
153.728914	5343.285783	25.115226
153.711225	5352.111397	25.120243
153.559766	5345.919735	25.125261
153.922888	5361.958593	25.130279
153.771298	5381.092698	25.135296
154.154041	5390.022899	25.140314
154.148969	5402.962829	25.145331
154.144396	5411.477065	25.150349
154.568786	5431.584779	25.155367
154.865985	5438.302965	25.160384
155.072796	5457.204228	25.165402
155.100411	5467.534839	25.170419
155.467109	5469.144142	25.175437
155.443466	5481.521995	25.180455
155.482927	5498.369278	25.185472
156.046711	5504.259714	25.190490
156.194729	5515.215450	25.195507
156.052216	5512.551486	25.200525
156.546628	5524.586204	25.205543
156.535534	5548.070462	25.210560
156.415417	5552.884303	25.215578
156.781972	5568.922805	25.220595
156.995549	5578.365729	25.225613
157.558661	5572.115707	25.230631
157.300444	5588.561460	25.235648
157.294377	5591.065694	25.240666
157.684013	5610.001607	25.245683
157.670891	5619.975668	25.250701
158.214833	5617.365137	25.255719
158.242182	5629.943443	25.260736
158.258518	5637.554852	25.265754
158.610917	5660.063711	25.270771
158.706630	5660.165548	25.275789
158.875576	5663.330533	25.280807
158.851773	5681.384282	25.285824
159.147554	5683.023655	25.290842
159.549464	5685.132533	25.295859
159.438754	5699.620221	25.300877
159.791598	5706.673869	25.305895
159.802421	5713.317066	25.310912
160.337392	5723.303175	25.315930
160.107191	5734.053131	25.320947
160.304918	5725.931553	25.325965
160.695548	5734.324048	25.330983
160.818736	5760.028802	25.336000
160.976283	5768.644074	25.341018
161.616925	5749.388823	25.346035
161.618257	5746.093045	25.351053
162.026255	5749.103795	25.356071
162.226976	5752.352205	25.361088
162.250938	5742.357503	25.366106
162.705697	5742.469382	25.371123
162.326745	5734.940060	25.376141
162.609665	5737.462174	25.381159
162.923055	5740.099470	25.386176
162.873564	5732.834205	25.391194
163.127147	5734.047725	25.396211
163.334438	5749.221146	25.401229
163.579079	5749.681614	25.406247
163.160820	5756.922375	25.411264
163.348067	5753.272328	25.416282
163.686830	5748.654689	25.421299
163.238408	5752.595100	25.426317
163.840421	5755.341861	25.431335
163.786580	5777.557800	25.436352
163.769219	5781.654812	25.441370
164.021558	5782.357142	25.446387
164.070482	5801.277184	25.451405
164.452932	5800.980549	25.456423
164.261753	5812.084304	25.461440
164.540251	5826.454297	25.466458
164.805494	5830.917421	25.471475
164.756004	5847.428565	25.476493
165.363879	5846.171693	25.481511
165.215144	5862.578443	25.486528
165.421790	5867.694729	25.491546
165.587540	5879.620178	25.496563
165.821361	5901.724910	25.501581
166.135681	5910.012642	25.506599
166.112114	5911.739947	25.511616
166.402876	5933.936813	25.516634
166.521481	5938.179867	25.521651
166.421693	5947.953025	25.526669
167.110694	5964.200214	25.531687
167.054234	5964.872010	25.536704
167.278246	5977.034622	25.541722
167.618083	5990.208197	25.546739
167.515378	5998.959052	25.551757
167.569136	5998.571854	25.556775
168.061718	6020.112170	25.561792
168.575999	6023.535636	25.566810
168.160820	6026.094550	25.571827
168.355468	6051.356043	25.576845
168.950572	6047.601005	25.581863
169.014090	6051.903224	25.586880
168.867474	6059.994911	25.591898
169.065685	6069.134291	25.596915
169.361895	6078.087857	25.601933
169.296318	6094.421808	25.606951
169.582356	6108.080568	25.611968
169.771195	6117.540274	25.616986
170.013901	6123.601172	25.622003
169.859648	6135.826305	25.627021
170.269691	6137.997099	25.632039
170.284501	6159.804992	25.637056
170.201368	6176.328015	25.642074
170.573483	6175.515282	25.647091
170.623150	6189.952978	25.652109
171.093213	6201.701535	25.657127
171.061242	6206.953159	25.662144
171.405394	6233.147988	25.667162
171.764413	6231.538636	25.672180
171.894010	6251.081018	25.677197
172.201438	6260.531690	25.682215
172.251337	6271.077083	25.687232
172.446867	6272.302891	25.692250
172.673470	6291.508126	25.697268
172.480020	6291.285923	25.702285
172.956606	6296.852501	25.707303
173.356715	6300.694820	25.712320
173.412165	6307.208126	25.717338
173.523753	6312.424662	25.722356
173.605454	6329.853259	25.727373
174.471736	6332.666040	25.732391
174.202030	6342.693318	25.737408
174.651873	6337.054265	25.742426
174.815315	6334.973611	25.747444
174.357832	6331.916917	25.752461
174.670126	6352.854508	25.757479
175.186712	6362.629186	25.762496
174.932363	6363.152059	25.767514
175.536156	6365.412487	25.772532
175.563867	6385.627592	25.777549
175.450022	6387.943626	25.782567
175.582889	6389.810623	25.787584
175.671743	6403.648866	25.792602
176.062302	6408.389241	25.797620
176.244423	6412.016345	25.802637
176.578798	6432.076127	25.807655
176.763897	6435.746965	25.812672
176.642557	6446.837005	25.817690
177.148890	6450.991025	25.822708
177.281727	6467.704611	25.827725
177.230337	6463.157388	25.832743
177.307315	6473.752321	25.837760
177.352723	6486.000074	25.842778
177.585957	6494.098738	25.847796
177.995792	6509.787192	25.852813
178.318410	6517.158417	25.857831
178.506908	6526.031215	25.862848
178.629211	6538.746797	25.867866
179.113552	6547.475397	25.872884
179.087762	6550.216458	25.877901
179.117750	6551.954374	25.882919
179.695171	6567.133625	25.887936
179.352635	6577.333440	25.892954
179.676253	6579.710395	25.897972
179.906226	6593.264654	25.902989
180.006499	6588.980913	25.908007
180.075146	6607.671403	25.913024
180.487905	6630.162530	25.918042
180.819060	6625.182826	25.923060
180.511174	6637.208224	25.928077
180.824342	6654.916554	25.933095
180.899958	6661.597297	25.938112
181.097321	6677.385474	25.943130
181.844701	6679.392997	25.948148
181.634108	6692.441798	25.953165
182.048854	6700.038587	25.958183
181.986869	6714.964561	25.963200
181.950988	6719.891785	25.968218
182.340542	6736.309692	25.973236
182.572997	6739.550150	25.978253
182.551068	6738.211947	25.983271
183.125868	6758.654286	25.988288
183.263398	6775.417928	25.993306
183.072075	6771.776477	25.998324
183.461045	6784.867163	26.003341
183.775424	6789.666926	26.008359
184.423493	6807.345035	26.013376
184.558345	6819.181230	26.018394
184.791618	6813.077172	26.023412
184.759702	6822.499218	26.028429
184.800285	6815.260453	26.033447
184.923718	6825.510524	26.038464
184.886081	6845.089209	26.043482
184.910134	6848.201333	26.048500
185.351219	6857.770279	26.053517
185.281688	6872.574444	26.058535
185.320118	6881.212058	26.063552
185.680922	6905.438488	26.068570
185.969596	6910.662179	26.073588
185.982971	6919.060654	26.078605
186.066941	6935.390865	26.083623
186.644884	6939.069713	26.088640
186.341140	6945.150195	26.093658
186.923427	6963.498555	26.098676
187.225974	6968.619068	26.103693
187.302974	6985.392384	26.108711
187.216960	6995.665891	26.113728
187.549474	7004.702618	26.118746
187.840394	7016.151444	26.123764
187.898676	7022.582480	26.128781
187.934540	7029.496883	26.133799
188.024952	7040.017429	26.138816
187.986768	7061.329584	26.143834
188.853821	7060.587654	26.148852
188.969460	7079.788999	26.153869
189.453205	7092.546207	26.158887
189.458557	7101.779454	26.163904
189.115695	7113.024562	26.168922
189.828231	7116.432963	26.173940
189.883956	7124.335571	26.178957
190.074528	7145.583574	26.183975
190.484106	7148.127084	26.188992
190.238206	7174.349398	26.194010
190.571899	7176.109248	26.199028
191.333000	7179.888887	26.204045
191.579458	7198.425844	26.209063
191.936320	7199.920039	26.214080
191.976668	7193.584052	26.219098
192.371413	7185.093172	26.224116
192.605225	7194.214908	26.229133
192.692001	7190.798149	26.234151
192.877477	7193.960810	26.239168
192.751115	7208.003850	26.244186
193.114274	7214.049396	26.249204
193.379682	7212.691399	26.254221
193.278170	7221.174307	26.259239
193.256310	7229.335357	26.264256
193.240153	7244.519766	26.269274
193.888652	7252.187501	26.274292
193.968761	7257.819644	26.279309
193.807459	7268.894340	26.284327
194.268350	7282.817026	26.289344
193.594078	7306.356913	26.294362
194.179980	7315.805545	26.299380
194.659744	7335.909836	26.304397
194.402685	7357.654402	26.309415
194.933434	7360.639879	26.314432
194.772141	7385.406496	26.319450
195.065384	7403.589060	26.324468
195.484511	7417.909858	26.329485
195.843474	7434.929855	26.334503
196.457345	7429.378428	26.339520
196.637890	7447.338759	26.344538
197.014376	7450.957720	26.349556
196.828511	7462.513087	26.354573
197.174927	7464.135221	26.359591
197.523550	7474.628192	26.364608
197.493406	7491.216705	26.369626
197.649533	7493.733672	26.374644
197.755479	7504.476198	26.379661
197.915886	7520.719185	26.384679
198.461452	7521.085204	26.389696
198.340761	7540.709208	26.394714
198.403171	7546.603088	26.399732
198.470970	7551.148078	26.404749
198.594237	7578.247609	26.409767
199.056654	7581.856291	26.414784
198.669677	7602.447084	26.419802
199.031103	7616.480315	26.424820
199.317378	7639.614428	26.429837
199.562684	7646.335243	26.434855
199.810991	7657.125009	26.439872
199.796926	7668.123208	26.444890
200.262262	7686.256993	26.449908
200.577175	7688.758583	26.454925
200.551143	7712.762543	26.459943
200.846377	7724.839387	26.464960
201.141175	7741.216210	26.469978
201.694499	7741.514722	26.474996
202.053518	7737.875261	26.480013
202.220232	7752.652592	26.485031
202.552881	7761.257155	26.490048
202.827716	7770.426421	26.495066
202.627059	7777.485498	26.500084
203.152573	7781.128534	26.505101
203.241263	7801.319854	26.510119
203.250055	7789.103846	26.515136
203.405208	7801.291082	26.520154
203.520417	7808.944729	26.525172
203.932664	7823.993045	26.530189
203.731726	7841.682031	26.535207
204.190631	7850.626762	26.540224
204.369478	7861.926348	26.545242
204.775736	7875.886455	26.550260
204.797966	7883.933547	26.555277
205.119558	7901.161882	26.560295
205.432313	7899.853247	26.565312
205.340610	7904.562222	26.570330
205.744376	7919.008943	26.575348
205.788882	7926.004413	26.580365
206.108637	7941.553505	26.585383
206.204008	7955.028828	26.590400
206.053325	7964.129097	26.595418
206.409104	7985.200646	26.600436
206.336772	7989.950808	26.605453
206.673641	8013.914094	26.610471
207.220991	8025.336005	26.615488
207.216720	8044.386655	26.620506
207.327068	8048.909317	26.625524
207.811049	8066.216551	26.630541
207.941331	8085.299835	26.635559
208.177687	8087.015039	26.640576
208.645173	8106.247575	26.645594
208.811320	8118.313328	26.650612
209.336603	8123.951766	26.655629
209.228208	8134.185212	26.660647
209.766764	8150.135886	26.665664
209.912442	8157.500763	26.670682
209.798754	8158.819341	26.675700
210.319787	8174.678068	26.680717
210.277836	8193.018107	26.685735
210.347696	8199.450896	26.690752
210.891479	8212.240520	26.695770
210.393746	8224.583986	26.700788
210.916793	8236.417106	26.705805
210.609667	8244.257065	26.710823
210.991206	8262.897058	26.715840
211.061860	8282.311916	26.720858
211.441860	8296.102812	26.725876
212.134057	8323.212179	26.730893
212.257818	8328.986197	26.735911
212.503814	8355.789812	26.740928
212.798531	8355.437432	26.745946
212.879766	8364.406851	26.750964
213.473809	8376.333125	26.755981
213.463187	8383.659434	26.760999
213.613315	8386.628938	26.766016
214.182126	8401.883672	26.771034
214.312167	8395.741596	26.776052
214.708767	8398.631447	26.781069
214.505799	8408.573615	26.786087
214.925074	8419.899020	26.791104
214.684007	8432.110857	26.796122
215.091245	8438.367748	26.801140
215.578971	8457.654308	26.806157
215.351145	8467.597244	26.811175
215.483215	8476.255664	26.816192
215.756516	8489.173096	26.821210
215.866295	8507.915896	26.826228
216.346246	8526.041903	26.831245
216.185499	8531.254375	26.836263
216.232426	8547.983305	26.841280
216.362873	8569.532827	26.846298
216.802764	8593.638584	26.851316
216.809525	8608.198553	26.856333
217.043051	8628.453330	26.861351
217.389650	8638.353728	26.866368
217.341778	8659.962862	26.871386
217.792919	8675.716152	26.876404
218.191712	8692.020696	26.881421
218.418170	8721.486274	26.886439
219.116744	8727.536605	26.891456
219.477346	8741.154069	26.896474
219.411792	8746.910516	26.901492
219.889188	8761.592625	26.906509
219.983216	8780.556016	26.911527
220.400270	8782.205091	26.916544
220.590390	8792.420550	26.921562
220.396562	8809.998840	26.926580
220.845950	8806.341859	26.931597
221.397524	8819.683200	26.936615
221.533880	8825.565903	26.941632
221.632266	8830.242177	26.946650
221.949574	8847.096354	26.951668
222.454549	8849.277864	26.956685
222.263158	8852.979751	26.961703
222.435636	8875.552304	26.966720
222.819379	8881.260508	26.971738
222.993186	8891.102865	26.976756
222.926315	8907.420561	26.981773
222.644306	8922.420670	26.986791
223.151288	8937.736050	26.991808
223.474070	8947.719276	26.996826
223.826944	8961.164463	27.001844
224.032059	8983.400522	27.006861
223.968798	9002.783438	27.011879
224.572152	9017.802790	27.016896
224.412591	9027.915295	27.021914
224.196839	9048.405090	27.026932
224.881543	9069.378987	27.031949
225.170573	9084.081390	27.036967
225.527758	9106.486368	27.041984
225.761160	9122.725640	27.047002
225.743270	9144.586380	27.052020
226.311336	9145.757182	27.057037
226.171111	9180.199989	27.062055
226.385627	9188.353287	27.067072
226.945988	9201.081011	27.072090
226.880466	9219.198429	27.077108
227.177141	9237.262282	27.082125
227.387612	9252.434934	27.087143
227.965096	9266.498719	27.092160
228.287625	9272.074555	27.097178
228.344706	9294.435210	27.102196
228.711434	9289.834419	27.107213
228.714657	9312.115128	27.112231
228.867077	9324.240649	27.117248
229.290950	9323.435469	27.122266
229.659227	9345.744278	27.127284
230.156487	9341.325095	27.132301
230.389010	9347.331820	27.137319
230.205555	9373.721110	27.142336
230.796246	9367.815969	27.147354
230.843015	9377.798464	27.152372
231.037796	9392.212771	27.157389
231.148833	9400.101371	27.162407
231.457941	9426.100997	27.167424
231.673404	9428.514214	27.172442
231.957780	9440.758062	27.177460
231.893540	9454.164758	27.182477
231.856399	9470.809810	27.187495
231.880483	9493.586329	27.192512
232.038849	9503.684017	27.197530
232.663604	9530.815191	27.202548
233.348021	9544.710883	27.207565
233.164005	9556.999767	27.212583
233.446070	9569.799757	27.217600
234.267207	9579.863123	27.222618
234.351272	9607.407476	27.227636
234.496791	9610.842032	27.232653
234.520536	9621.655495	27.237671
234.750260	9643.986367	27.242688
235.172771	9657.932645	27.247706
235.186271	9664.804174	27.252724
235.358154	9687.519888	27.257741
235.644199	9703.511460	27.262759
235.841345	9715.134519	27.267776
236.201484	9731.458663	27.272794
236.131682	9757.057130	27.277812
236.809711	9764.250843	27.282829
237.464156	9768.897078	27.287847
237.806011	9773.358635	27.292864
238.323766	9787.356395	27.297882
238.313335	9792.583559	27.302900
238.282243	9791.126588	27.307917
239.061458	9799.775812	27.312935
238.999133	9807.420206	27.317952
239.279491	9808.648754	27.322970
239.425813	9824.201338	27.327988
239.336134	9835.332646	27.333005
239.608032	9839.337882	27.338023
239.552387	9855.266287	27.343040
240.109816	9867.293984	27.348058
240.359532	9879.230967	27.353076
240.270224	9893.475462	27.358093
240.811639	9907.744302	27.363111
240.339351	9925.196764	27.368128
241.190999	9935.375526	27.373146
240.831594	9960.021893	27.378164
241.074405	9974.198635	27.383181
241.709125	9994.104725	27.388199
241.682124	10025.184474	27.393216
242.109435	10028.919125	27.398234
242.593928	10052.454608	27.403252
242.689354	10063.073965	27.408269
243.122674	10077.940840	27.413287
243.397129	10084.986351	27.418304
243.210026	10104.074066	27.423322
243.752855	10122.175996	27.428340
243.655320	10138.941616	27.433357
244.298125	10140.552295	27.438375
244.376267	10163.880033	27.443392
244.752735	10165.794506	27.448410
244.990904	10180.692034	27.453428
245.510959	10190.341909	27.458445
245.703396	10192.973542	27.463463
245.947778	10211.093894	27.468480
246.663972	10211.253277	27.473498
246.435177	10211.273366	27.478516
246.337514	10224.862668	27.483533
246.793513	10236.394983	27.488551
246.824892	10256.591634	27.493568
247.294523	10265.295889	27.498586
247.392863	10281.449976	27.503604
247.468175	10292.650434	27.508621
247.902516	10320.500920	27.513639
247.714741	10341.780279	27.518656
248.103749	10351.848612	27.523674
248.572011	10360.297369	27.528692
248.624772	10388.738191	27.533709
249.046979	10405.068990	27.538727
249.244169	10418.135461	27.543744
249.240742	10427.355948	27.548762
249.610977	10455.687147	27.553780
249.845248	10485.466884	27.558797
250.189290	10499.315573	27.563815
250.362698	10506.793866	27.568832
250.733818	10519.855263	27.573850
251.752264	10532.815264	27.578868
252.247201	10537.442477	27.583885
252.403217	10546.915909	27.588903
252.716040	10552.269468	27.593920
253.046664	10547.096200	27.598938
253.346573	10554.703099	27.603956
253.035604	10568.594455	27.608973
253.423064	10580.709234	27.613991
253.461900	10590.494695	27.619008
253.581382	10604.665976	27.624026
254.032465	10614.705781	27.629044
253.808922	10626.707907	27.634061
254.323950	10644.745235	27.639079
254.082597	10660.431868	27.644096
254.396464	10669.918525	27.649114
254.584283	10696.163107	27.654132
254.608199	10723.573280	27.659149
255.264225	10739.539358	27.664167
254.808197	10760.406525	27.669184
255.259366	10780.998984	27.674202
255.540950	10810.471858	27.679220
255.693470	10839.159815	27.684237
256.235122	10858.402530	27.689255
256.121567	10886.405997	27.694272
256.899748	10906.915791	27.699290
257.204444	10938.611345	27.704308
257.712050	10949.864465	27.709325
258.251870	10969.780150	27.714343
258.274598	10973.202618	27.719360
258.915741	10981.236191	27.724378
259.541768	10994.857933	27.729396
259.534781	11013.773108	27.734413
259.588301	11018.412753	27.739431
259.791085	11035.529987	27.744448
260.133766	11040.992684	27.749466
260.402121	11050.856104	27.754484
260.648036	11078.165708	27.759501
260.978779	11080.715807	27.764519
260.789653	11102.529877	27.769536
260.956946	11110.040945	27.774554
261.522723	11128.645477	27.779572
261.460082	11145.267594	27.784589
261.636054	11155.139227	27.789607
261.632621	11186.450873	27.794624
262.437440	11203.458163	27.799642
262.025668	11208.012862	27.804660
262.038222	11237.358038	27.809677
262.690604	11262.163379	27.814695
263.030203	11281.731842	27.819712
263.095718	11303.537831	27.824730
263.372663	11331.168180	27.829748
263.577558	11355.645879	27.834765
263.781114	11380.016458	27.839783
263.970415	11408.247976	27.844800
264.564931	11424.265325	27.849818
264.697419	11455.524550	27.854836
264.733523	11477.423763	27.859853
265.172594	11501.681822	27.864871
265.279687	11526.070859	27.869888
265.692104	11552.196196	27.874906
265.901853	11572.331585	27.879924
266.237470	11604.373923	27.884941
266.687516	11613.334494	27.889959
266.868777	11644.576919	27.894976
267.555157	11666.582895	27.899994
268.020250	11679.320924	27.905012
267.953834	11701.132252	27.910029
268.518237	11708.593984	27.915047
268.761724	11747.212745	27.920064
268.965531	11750.515414	27.925082
269.380917	11769.434652	27.930100
269.498535	11792.499296	27.935117
270.221497	11807.808466	27.940135
270.373822	11823.194408	27.945152
270.862332	11829.196569	27.950170
271.066617	11850.409902	27.955188
271.482880	11865.438758	27.960205
271.422162	11876.279382	27.965223
271.995191	11892.019458	27.970240
271.896262	11907.902702	27.975258
272.155505	11921.020496	27.980276
272.131547	11933.364803	27.985293
272.332715	11944.953883	27.990311
272.703593	11980.878543	27.995328
272.742504	12004.028403	28.000346
273.518379	12024.571363	28.005364
273.503142	12040.050044	28.010381
273.826135	12059.644023	28.015399
274.280592	12078.465877	28.020416
274.950812	12095.548745	28.025434
275.532537	12097.775468	28.030452
275.556802	12105.631434	28.035469
275.694594	12125.655534	28.040487
275.768040	12144.041365	28.045504
275.963005	12162.471334	28.050522
276.641104	12175.381591	28.055540
276.324436	12204.669323	28.060557
276.515741	12217.987434	28.065575
276.988594	12239.686488	28.070592
276.627202	12264.531963	28.075610
277.095851	12279.849779	28.080628
277.332277	12316.538227	28.085645
277.805985	12332.673170	28.090663
278.052853	12354.909851	28.095680
278.673081	12384.328985	28.100698
278.548627	12403.668157	28.105716
278.519985	12427.735418	28.110733
278.983563	12442.700483	28.115751
279.481086	12480.453595	28.120768
279.941271	12494.064513	28.125786
280.173166	12509.811177	28.130804
279.876231	12527.702777	28.135821
280.475458	12539.542494	28.140839
280.479998	12565.628922	28.145856
280.795186	12594.426700	28.150874
281.067544	12613.492349	28.155892
281.329904	12644.411096	28.160909
281.714594	12667.327604	28.165927
282.183126	12690.193111	28.170944
282.141073	12714.714416	28.175962
282.485523	12731.510999	28.180980
283.181899	12763.865111	28.185997
283.178247	12787.041544	28.191015
283.624058	12810.769706	28.196032
284.170804	12833.916820	28.201050
284.473902	12849.393665	28.206068
284.945880	12867.739876	28.211085
285.091825	12894.407766	28.216103
285.787726	12907.151526	28.221120
286.103737	12916.098980	28.226138
286.630550	12932.611384	28.231156
286.767202	12941.640630	28.236173
286.917693	12951.504565	28.241191
287.265319	12972.684072	28.246208
287.401456	12981.457625	28.251226
287.713701	12991.084660	28.256244
287.917356	13014.453111	28.261261
288.045150	13026.837518	28.266279
288.649058	13042.658985	28.271296
288.879146	13059.255877	28.276314
288.917597	13073.899610	28.281332
288.919193	13097.299816	28.286349
289.252262	13119.947059	28.291367
289.737859	13136.159776	28.296384
289.937105	13164.708158	28.301402
290.365866	13187.195225	28.306420
290.704864	13208.066867	28.311437
290.957224	13225.999396	28.316455
291.327238	13246.793588	28.321472
291.102989	13272.342075	28.326490
291.714764	13282.310769	28.331508
291.903285	13303.799789	28.336525
292.603506	13326.175022	28.341543
293.047644	13346.648230	28.346560
292.958186	13368.436665	28.351578
293.116187	13376.366949	28.356596
293.792743	13401.490280	28.361613
293.988102	13422.814148	28.366631
294.145670	13440.831206	28.371648
294.312508	13462.386962	28.376666
295.109607	13473.889945	28.381684
295.343010	13493.088903	28.386701
295.627347	13507.962885	28.391719
295.803770	13523.002211	28.396736
295.952262	13542.666118	28.401754
296.630676	13554.231954	28.406772
296.425278	13582.585393	28.411789
296.980639	13603.369891	28.416807
297.243790	13617.959897	28.421824
297.190288	13634.077481	28.426842
297.648822	13656.863614	28.431860
297.896912	13686.570449	28.436877
297.737830	13708.256490	28.441895
298.363219	13728.556447	28.446912
298.181696	13763.607816	28.451930
298.616562	13794.504574	28.456948
299.165596	13813.379661	28.461965
299.243883	13836.039247	28.466983
299.506493	13854.933979	28.472000
299.559857	13886.064341	28.477018
300.227341	13905.795755	28.482036
300.583419	13936.919836	28.487053
300.790323	13966.684089	28.492071
300.777150	13981.033431	28.497088
300.980775	14017.998747	28.502106
301.328119	14045.369386	28.507124
301.865528	14070.575405	28.512141
302.254758	14102.932546	28.517159
302.490043	14124.389903	28.522176
302.697672	14152.063654	28.527194
302.709844	14177.683695	28.532212
303.034106	14207.489945	28.537229
303.631361	14242.502312	28.542247
304.150371	14263.997493	28.547264
304.175876	14304.970533	28.552282
304.653832	14328.825044	28.557300
305.124981	14355.147175	28.562317
305.310520	14386.917705	28.567335
305.541978	14400.815322	28.572352
305.966815	14447.088686	28.577370
306.387275	14459.453446	28.582388
306.569886	14489.579195	28.587405
307.074068	14512.662389	28.592423
307.065704	14543.336081	28.597440
306.979496	14571.476508	28.602458
307.440675	14598.883799	28.607476
308.297367	14628.951548	28.612493
308.457894	14668.088247	28.617511
308.785179	14686.294656	28.622528
309.138930	14721.248141	28.627546
309.348942	14744.601930	28.632564
309.645562	14772.044722	28.637581
309.822704	14799.392573	28.642599
310.241935	14830.741930	28.647616
310.408577	14864.941744	28.652634
310.684551	14891.014104	28.657652
311.462779	14917.885818	28.662669
311.816525	14944.498763	28.667687
312.424699	14960.516975	28.672704
312.684271	14988.954418	28.677722
313.453407	15008.083616	28.682740
313.434103	15027.620583	28.687757
313.586350	15040.233023	28.692775
314.107235	15058.463151	28.697792
314.231341	15094.770295	28.702810
314.869117	15103.699961	28.707828
314.894151	15123.536434	28.712845
315.444436	15146.651073	28.717863
315.828916	15171.200312	28.722880
315.959458	15191.206668	28.727898
316.441961	15203.884340	28.732916
316.572776	15229.992534	28.737933
317.042638	15254.661155	28.742951
317.275194	15278.397378	28.747968
317.433492	15299.069061	28.752986
317.388780	15322.896146	28.758004
317.883194	15340.060019	28.763021
317.824513	15372.956906	28.768039
318.289394	15388.511542	28.773056
318.919500	15419.026615	28.778074
318.987046	15451.180604	28.783092
319.150837	15480.164382	28.788109
319.364196	15517.001579	28.793127
319.758058	15530.520842	28.798144
319.941392	15556.655995	28.803162
320.243141	15582.450482	28.808180
320.679932	15604.026378	28.813197
320.716514	15637.647854	28.818215
321.587554	15661.009757	28.823232
321.612442	15689.503952	28.828250
322.314895	15712.996554	28.833268
322.689236	15742.200416	28.838285
322.574596	15766.945464	28.843303
323.123700	15788.178660	28.848320
323.295537	15821.018096	28.853338
323.402899	15848.801600	28.858356
324.134222	15876.105237	28.863373
324.287305	15898.212301	28.868391
324.608692	15922.481812	28.873408
325.022519	15951.414500	28.878426
325.382765	15982.446506	28.883444
326.057793	16004.427715	28.888461
326.311956	16029.143755	28.893479
326.978555	16050.835761	28.898496
326.893754	16074.003625	28.903514
327.332158	16094.742833	28.908532
327.468199	16117.920375	28.913549
327.396384	16147.276861	28.918567
328.334823	16173.986274	28.923584
328.247040	16200.543786	28.928602
328.806039	16227.107410	28.933620
328.814197	16257.759143	28.938637
328.939726	16285.666771	28.943655
329.473777	16315.174969	28.948672
329.764809	16343.994826	28.953690
330.014226	16378.212796	28.958708
330.713923	16402.992182	28.963725
331.098429	16430.771016	28.968743
331.632722	16457.660995	28.973760
332.356519	16477.781063	28.978778
332.244840	16500.881005	28.983796
332.663859	16524.393731	28.988813
333.009256	16551.275528	28.993831
332.737438	16573.664705	28.998848
333.601228	16592.341628	29.003866
333.875919	16617.405804	29.008884
334.390548	16639.040159	29.013901
334.521735	16675.153347	29.018919
335.087489	16703.039999	29.023936
335.462186	16730.940827	29.028954
336.372442	16739.048417	29.033972
337.236106	16736.136796	29.038989
337.868935	16745.680769	29.044007
338.427157	16738.047575	29.049024
338.472270	16750.327321	29.054042
338.659269	16772.815421	29.059060
338.622072	16781.390456	29.064077
338.974471	16785.498273	29.069095
339.228259	16802.637977	29.074112
339.307206	16815.866351	29.079130
339.709653	16837.174218	29.084148
340.438187	16844.236406	29.089165
340.136704	16870.183966	29.094183
340.566097	16883.060585	29.099200
340.472931	16910.940204	29.104218
341.181838	16923.596186	29.109236
341.653471	16944.204762	29.114253
341.564986	16969.796915	29.119271
341.804641	17001.913899	29.124288
342.011259	17018.192570	29.129306
342.084455	17050.860037	29.134324
342.631649	17067.237013	29.139341
342.750461	17102.165301	29.144359
343.037487	17124.887673	29.149376
342.934021	17161.569174	29.154394
343.201177	17195.299386	29.159412
343.747970	17230.495681	29.164429
344.179480	17261.888144	29.169447
344.352178	17290.901678	29.174464
344.973699	17318.391972	29.179482
345.200375	17345.596703	29.184500
345.833192	17362.080547	29.189517
346.289251	17396.703847	29.194535
346.716439	17432.462535	29.199552
347.193758	17450.948138	29.204570
347.169823	17477.813270	29.209588
347.944805	17508.046795	29.214605
348.368397	17537.280409	29.219623
348.592727	17554.605440	29.224640
348.995133	17576.893323	29.229658
349.178344	17620.915807	29.234676
349.259535	17626.235006	29.239693
349.811784	17656.775301	29.244711
350.017526	17694.338034	29.249728
350.518855	17714.784846	29.254746
350.838255	17755.343306	29.259764
351.289757	17779.165186	29.264781
351.495825	17809.001854	29.269799
351.901695	17837.670126	29.274816
352.230926	17884.519513	29.279834
352.374442	17910.796759	29.284852
352.689786	17929.238699	29.289869
353.131882	17966.088962	29.294887
353.713518	18003.713446	29.299904
354.056928	18023.711507	29.304922
354.496964	18058.041575	29.309940
354.918206	18079.568981	29.314957
355.579258	18097.331492	29.319975
355.892116	18130.405465	29.324992
356.272306	18156.841815	29.330010
356.464634	18176.857382	29.335028
356.722609	18205.612540	29.340045
356.990180	18222.255412	29.345063
357.496175	18262.570905	29.350080
357.869532	18287.454373	29.355098
358.295569	18315.273632	29.360116
358.778626	18337.568709	29.365133
359.176009	18369.517946	29.370151
359.197262	18400.578505	29.375168
359.465358	18411.030162	29.380186
359.762542	18457.879634	29.385204
360.476093	18479.620721	29.390221
360.685636	18504.245830	29.395239
360.997495	18530.326967	29.400256
361.548453	18558.158594	29.405274
361.534535	18590.722261	29.410292
362.169137	18600.099459	29.415309
362.450434	18640.558333	29.420327
362.779290	18659.030438	29.425344
363.306761	18687.308171	29.430362
363.646939	18728.819386	29.435380
364.026565	18749.766503	29.440397
364.699494	18765.499765	29.445415
365.061177	18788.667271	29.450432
365.663419	18811.746581	29.455450
366.316199	18831.974997	29.460468
366.485186	18835.429663	29.465485
367.123623	18868.264358	29.470503
367.322574	18876.130480	29.475520
367.626847	18892.742907	29.480538
368.055568	18910.093991	29.485556
368.481926	18928.311003	29.490573
368.741303	18933.495246	29.495591
368.650227	18957.814221	29.500608
369.030744	18969.493181	29.505626
369.109255	19003.350850	29.510644
369.308307	19028.603732	29.515661
369.806961	19046.139838	29.520679
370.191239	19066.170477	29.525696
370.552441	19097.614829	29.530714
370.544049	19129.850000	29.535732
370.777261	19159.918248	29.540749
371.234836	19184.770718	29.545767
371.577509	19223.464811	29.550784
372.080691	19254.261703	29.555802
372.168764	19287.012727	29.560820
372.172215	19328.805409	29.565837
372.904097	19366.093096	29.570855
372.970645	19401.577043	29.575872
373.820941	19439.244354	29.580890
374.061802	19477.398914	29.585908
374.566713	19512.043602	29.590925
374.932712	19545.061107	29.595943
375.101711	19589.684158	29.600960
375.712343	19617.280503	29.605978
375.637569	19659.389408	29.610996
376.102287	19693.573177	29.616013
377.155758	19726.192672	29.621031
377.365803	19757.358495	29.626048
377.826461	19785.515606	29.631066
378.439688	19821.022090	29.636084
378.930857	19852.289345	29.641101
379.380427	19874.534564	29.646119
379.359279	19910.620755	29.651136
379.914689	19927.940265	29.656154
380.327135	19974.250912	29.661172
380.470428	19999.734917	29.666189
381.291098	20040.314383	29.671207
381.472696	20067.902749	29.676224
381.942496	20087.232357	29.681242
382.249864	20133.307110	29.686260
382.667471	20157.295164	29.691277
383.173873	20186.646148	29.696295
383.101529	20219.171128	29.701312
383.515535	20240.929512	29.706330
384.175800	20278.697706	29.711348
384.997704	20311.480817	29.716365
385.621394	20341.123255	29.721383
385.426923	20372.107003	29.726400
385.780243	20394.709077	29.731418
386.169441	20429.847385	29.736436
386.437654	20459.659413	29.741453
386.851264	20488.444098	29.746471
387.050815	20524.749579	29.751488
387.672727	20548.737702	29.756506
387.924017	20590.311016	29.761524
387.993211	20613.438040	29.766541
388.424736	20648.437423	29.771559
388.896463	20682.179531	29.776576
389.532132	20713.842539	29.781594
389.503892	20758.107399	29.786612
390.241745	20788.092779	29.791629
391.138344	20818.249212	29.796647
391.102458	20861.289726	29.801664
391.641624	20887.142527	29.806682
391.570805	20919.188221	29.811700
391.874617	20958.466802	29.816717
392.694974	20983.688068	29.821735
393.299079	21018.875905	29.826752
393.514516	21043.370596	29.831770
393.585487	21068.740944	29.836788
393.914742	21104.755481	29.841805
394.138624	21134.670252	29.846823
394.394651	21167.644525	29.851840
394.853578	21198.704144	29.856858
395.000962	21238.980843	29.861876
395.301945	21284.357929	29.866893
395.589046	21317.175939	29.871911
396.032445	21373.076647	29.876928
396.456806	21408.072182	29.881946
396.747686	21451.783121	29.886964
397.222234	21498.371964	29.891981
397.907782	21539.083107	29.896999
398.402872	21590.281570	29.902016
398.582061	21613.499954	29.907034
398.662563	21662.709972	29.912052
399.390952	21699.901541	29.917069
400.166041	21744.080690	29.922087
400.225550	21790.450888	29.927104
400.790621	21822.891304	29.932122
401.639295	21859.337676	29.937140
401.811146	21894.019773	29.942157
402.584767	21932.575868	29.947175
402.609135	21969.650743	29.952192
403.089919	22000.796662	29.957210
403.783407	22027.814722	29.962228
404.529079	22067.588671	29.967245
405.157143	22096.120952	29.972263
405.841853	22123.121561	29.977280
405.872689	22150.907062	29.982298
406.525887	22180.016863	29.987316
406.420931	22213.188436	29.992333
406.809415	22230.965807	29.997351
406.938307	22273.282184	30.002368
407.352830	22305.266736	30.007386
407.781562	22346.373626	30.012404
407.955158	22387.659580	30.017421
408.454607	22417.539446	30.022439
408.754233	22463.317539	30.027456
409.170356	22499.617999	30.032474
409.348667	22544.562221	30.037492
409.213564	22586.971168	30.042509
410.115326	22635.941219	30.047527
411.058254	22687.103964	30.052544
411.478384	22721.192542	30.057562
411.612970	22764.355823	30.062580
411.418670	22809.535940	30.067597
411.768644	22844.078053	30.072615
412.223297	22904.366751	30.077632
413.059748	22946.700115	30.082650
413.112520	22991.968327	30.087668
413.143761	23031.818198	30.092685
414.179257	23087.289760	30.097703
414.708674	23126.985961	30.102720
414.593001	23181.367945	30.107738
415.482053	23225.778992	30.112756
416.144257	23275.559084	30.117773
416.661716	23314.082157	30.122791
416.913258	23356.950355	30.127808
417.640765	23392.186272	30.132826
417.985347	23434.319669	30.137844
418.232992	23483.912444	30.142861
418.493594	23512.738131	30.147879
419.013886	23557.195040	30.152896
419.294718	23603.269382	30.157914
420.068927	23639.939226	30.162932
421.149685	23670.393451	30.167949
421.805727	23690.063935	30.172967
421.768035	23715.688498	30.177984
421.999772	23752.058037	30.183002
422.693555	23780.772025	30.188020
422.940793	23822.611840	30.193037
423.556693	23841.915918	30.198055
423.708597	23871.915598	30.203072
423.945330	23904.947990	30.208090
424.780504	23932.995472	30.213108
425.011309	23972.310407	30.218125
425.306556	23993.434297	30.223143
425.746206	24039.819700	30.228160
425.781267	24079.974395	30.233178
426.120599	24108.396803	30.238196
426.422926	24160.630550	30.243213
427.161193	24196.731973	30.248231
427.648107	24247.281324	30.253248
427.766009	24281.577895	30.258266
428.469457	24329.192873	30.263284
428.715939	24377.492538	30.268301
428.968069	24411.281700	30.273319
429.398793	24452.367339	30.278336
429.791784	24496.410222	30.283354
430.321208	24542.833284	30.288372
430.556169	24592.942679	30.293389
431.189521	24631.671325	30.298407
431.858400	24676.151683	30.303424
432.316354	24715.780076	30.308442
433.250365	24760.977453	30.313460
433.738274	24793.264163	30.318477
434.138885	24832.168683	30.323495
435.010434	24862.000247	30.328512
435.162920	24890.427751	30.333530
436.388580	24918.731440	30.338548
436.813667	24940.019264	30.343565
437.237450	24966.274631	30.348583
437.621517	24993.231426	30.353600
437.832382	25021.612052	30.358618
438.344112	25051.550816	30.363636
438.320790	25080.183078	30.368653
438.977102	25107.154261	30.373671
439.485114	25145.821375	30.378688
439.647214	25170.904596	30.383706
440.709166	25186.417742	30.388724
440.766761	25239.008615	30.393741
441.153097	25258.008748	30.398759
441.573906	25292.164801	30.403776
441.677254	25336.065296	30.408794
441.988029	25361.586817	30.413812
442.540712	25405.328605	30.418829
442.818808	25436.138759	30.423847
443.046477	25490.568017	30.428864
443.222479	25528.188203	30.433882
443.845352	25568.437077	30.438900
443.804052	25618.864053	30.443917
444.406763	25665.113907	30.448935
444.569288	25712.526170	30.453952
445.055153	25760.760058	30.458970
445.839713	25809.768878	30.463988
446.015159	25858.803701	30.469005
446.421174	25908.839016	30.474023
447.264373	25961.157038	30.479040
447.126149	26010.620563	30.484058
448.112529	26053.354135	30.489076
448.455525	26099.847907	30.494093
448.761880	26147.535706	30.499111
449.698718	26182.522535	30.504128
450.159646	26231.311302	30.509146
450.748868	26257.807885	30.514164
450.996162	26306.908382	30.519181
451.009802	26334.993097	30.524199
451.618379	26378.140461	30.529216
451.895982	26427.129059	30.534234
452.467706	26466.319619	30.539252
453.080905	26512.247438	30.544269
453.246702	26553.562141	30.549287
454.073888	26601.921539	30.554304
454.475173	26646.865295	30.559322
454.487729	26685.271663	30.564340
455.235176	26744.217720	30.569357
455.670854	26797.619303	30.574375
456.416448	26834.533310	30.579392
456.299891	26886.997730	30.584410
457.003702	26928.096198	30.589428
457.348554	26982.928252	30.594445
457.907060	27026.274449	30.599463
458.354517	27072.438069	30.604480
458.800674	27111.763310	30.609498
459.557217	27158.131529	30.614516
459.767377	27209.003421	30.619533
460.299039	27255.413405	30.624551
461.201192	27310.108489	30.629568
461.314974	27349.473608	30.634586
461.615929	27388.265924	30.639604
461.915128	27446.449921	30.644621
462.300453	27497.168686	30.649639
462.951480	27542.606228	30.654656
463.738496	27599.728252	30.659674
464.165707	27641.781647	30.664692
464.590584	27697.089774	30.669709
465.014606	27748.529971	30.674727
466.089645	27785.362502	30.679744
466.175385	27828.891907	30.684762
467.164564	27860.649913	30.689780
467.664994	27901.763242	30.694797
467.881794	27943.666917	30.699815
468.620994	27982.309552	30.704832
469.116979	28030.174324	30.709850
469.915251	28063.119235	30.714868
470.278436	28106.226532	30.719885
470.779404	28135.981919	30.724903
470.629119	28167.052935	30.729920
471.372179	28227.179630	30.734938
471.939718	28261.128075	30.739956
471.750238	28300.637338	30.744973
472.600065	28346.367892	30.749991
472.973071	28390.871146	30.755008
473.447395	28428.867146	30.760026
474.368214	28466.527808	30.765044
474.551652	28507.793139	30.770061
474.997428	28559.118193	30.775079
475.113413	28601.392973	30.780096
475.583551	28659.357700	30.785114
476.526279	28696.566571	30.790132
477.218922	28735.691991	30.795149
477.487726	28778.328776	30.800167
478.189438	28814.343030	30.805184
478.437420	28853.993429	30.810202
478.991929	28888.292609	30.815220
479.349340	28932.685704	30.820237
479.571906	28978.105053	30.825255
479.955232	29029.896178	30.830272
480.124589	29084.742394	30.835290
480.647576	29127.592932	30.840308
481.334768	29178.938613	30.845325
481.681349	29223.112795	30.850343
481.997166	29266.154097	30.855360
482.357866	29316.855942	30.860378
482.683509	29364.282748	30.865396
483.337649	29412.220792	30.870413
483.504242	29458.440107	30.875431
484.400240	29504.210262	30.880448
484.778560	29556.161524	30.885466
485.190542	29606.027976	30.890484
485.467372	29665.681966	30.895501
485.618062	29718.819748	30.900519
486.372479	29775.238646	30.905536
486.879204	29839.920441	30.910554
487.306208	29882.496805	30.915572
488.021201	29955.547305	30.920589
487.854931	30004.828911	30.925607
488.767484	30061.312322	30.930624
488.802720	30131.195466	30.935642
489.281999	30191.122689	30.940660
490.211658	30260.619648	30.945677
490.297440	30320.830127	30.950695
491.091923	30371.409728	30.955712
492.063260	30433.536294	30.960730
492.285689	30492.569047	30.965748
493.023257	30545.402104	30.970765
493.080469	30603.525473	30.975783
493.933483	30656.814843	30.980800
494.289888	30719.158689	30.985818
495.264353	30773.345958	30.990836
495.552874	30836.693271	30.995853
496.130522	30890.487845	31.000871
496.720936	30935.923421	31.005888
497.735379	30980.142152	31.010906
498.534991	31025.248043	31.015924
499.156737	31064.692427	31.020941
499.849634	31123.653289	31.025959
500.783210	31156.234277	31.030976
500.889577	31203.617462	31.035994
501.066176	31244.883011	31.041012
501.552330	31291.125905	31.046029
502.100595	31321.314683	31.051047
502.610785	31367.566626	31.056064
502.992463	31417.170352	31.061082
503.641011	31457.123344	31.066100
503.834629	31496.976979	31.071117
504.349005	31564.912341	31.076135
504.655187	31605.842221	31.081152
505.170371	31660.577876	31.086170
505.797076	31706.028418	31.091188
506.034330	31762.489475	31.096205
506.207499	31820.926819	31.101223
506.859864	31878.163980	31.106240
506.876400	31930.949123	31.111258
506.878335	31990.614919	31.116276
508.164465	32057.305712	31.121293
508.655110	32119.929859	31.126311
509.058127	32171.523450	31.131328
509.626599	32243.327911	31.136346
509.933702	32297.459306	31.141364
510.297330	32357.442497	31.146381
510.824241	32422.236644	31.151399
511.669995	32488.062124	31.156416
512.189922	32552.238206	31.161434
512.675202	32615.313544	31.166452
513.324494	32679.172614	31.171469
513.390382	32735.846480	31.176487
513.909152	32787.322305	31.181504
515.036884	32842.527788	31.186522
515.441940	32899.085752	31.191540
516.503984	32942.744845	31.196557
516.798603	32981.946949	31.201575
517.887106	33030.223614	31.206592
518.654624	33071.008240	31.211610
518.705602	33119.732111	31.216628
519.292589	33157.143811	31.221645
519.245299	33227.265209	31.226663
519.944338	33260.360394	31.231680
520.388272	33304.863082	31.236698
520.906429	33364.900820	31.241716
521.208566	33403.249019	31.246733
521.431211	33464.932876	31.251751
522.068378	33514.469947	31.256768
522.531678	33578.632747	31.261786
523.318277	33633.666137	31.266804
523.475418	33689.854101	31.271821
523.839043	33759.343894	31.276839
524.641648	33823.587068	31.281856
525.205508	33878.959463	31.286874
525.123959	33942.045369	31.291892
525.932929	34008.165889	31.296909
526.272912	34068.714050	31.301927
526.938496	34139.150438	31.306944
527.703096	34206.454524	31.311962
527.921545	34273.970815	31.316980
528.448328	34330.538849	31.321997
529.299953	34401.958593	31.327015
530.030247	34463.199146	31.332032
530.819607	34519.214426	31.337050
531.016119	34588.543439	31.342068
531.641038	34642.896644	31.347085
532.134002	34705.736778	31.352103
532.881625	34761.961564	31.357120
533.886761	34829.052924	31.362138
533.804396	34894.626639	31.367156
534.419825	34936.640026	31.372173
534.734105	35008.702382	31.377191
535.608865	35064.389588	31.382208
536.194665	35138.199219	31.387226
536.262718	35201.727011	31.392244
537.181927	35251.388377	31.397261
537.722589	35323.182398	31.402279
538.221729	35384.006567	31.407296
538.614442	35439.599537	31.412314
538.784364	35511.041266	31.417332
539.592986	35567.245988	31.422349
539.919896	35638.967061	31.427367
540.558909	35709.842794	31.432384
541.083660	35770.120275	31.437402
541.492770	35841.873419	31.442420
542.340235	35914.867027	31.447437
542.942153	35970.649926	31.452455
543.737789	36040.414656	31.457472
544.421300	36107.326470	31.462490
544.424881	36166.719258	31.467508
545.199601	36224.663569	31.472525
545.846597	36291.202289	31.477543
546.353417	36355.600632	31.482560
546.791770	36415.261146	31.487578
547.221333	36484.344843	31.492596
547.722042	36549.383375	31.497613
548.262096	36609.148644	31.502631
548.563643	36679.252099	31.507648
549.349907	36752.353005	31.512666
549.719469	36817.804938	31.517684
550.486856	36870.712443	31.522701
551.544140	36934.596327	31.527719
552.512277	36974.996620	31.532736
553.374837	37032.499373	31.537754
553.975843	37081.165155	31.542772
554.280709	37124.470888	31.547789
555.059427	37175.360194	31.552807
555.102187	37220.800235	31.557824
555.774932	37271.118284	31.562842
556.037926	37323.897230	31.567860
556.490408	37373.377373	31.572877
557.064580	37436.231802	31.577895
557.117746	37490.485784	31.582912
557.880563	37542.719044	31.587930
558.130467	37603.651798	31.592948
558.804813	37662.810878	31.597965
559.810676	37731.308768	31.602983
559.901743	37793.917401	31.608000
560.425109	37869.099495	31.613018
560.865699	37938.951308	31.618036
561.361955	37998.803190	31.623053
561.867570	38068.278463	31.628071
562.120249	38139.987911	31.633088
562.837303	38219.814134	31.638106
563.375101	38293.629516	31.643124
564.259019	38372.064231	31.648141
564.944874	38439.596359	31.653159
565.268305	38513.648428	31.658176
565.930023	38580.514448	31.663194
566.178188	38653.535346	31.668212
566.741624	38719.032256	31.673229
567.048288	38791.418390	31.678247
567.689186	38869.450296	31.683264
568.666101	38956.441518	31.688282
569.182032	39034.095179	31.693300
570.003635	39094.234310	31.698317
570.913842	39172.971365	31.703335
571.614956	39239.662501	31.708352
572.272017	39309.446891	31.713370
572.449631	39382.323189	31.718388
573.193964	39441.166296	31.723405
573.872274	39514.837349	31.728423
574.572014	39585.159816	31.733440
575.243985	39643.610058	31.738458
575.792480	39714.570077	31.743476
576.636263	39769.913867	31.748493
577.054145	39833.735725	31.753511
577.782174	39902.467406	31.758528
578.681356	39957.385597	31.763546
579.447748	40013.810930	31.768564
580.179246	40058.877114	31.773581
580.901395	40122.215788	31.778599
581.230874	40172.638620	31.783616
582.041990	40216.073632	31.788634
582.681310	40280.621039	31.793652
582.844689	40330.463111	31.798669
583.503187	40389.296927	31.803687
583.783566	40448.183796	31.808704
584.605412	40487.785079	31.813722
584.918442	40556.950635	31.818740
585.819955	40618.011157	31.823757
586.119445	40676.471909	31.828775
586.789290	40737.113684	31.833792
587.123592	40795.088640	31.838810
587.354481	40855.919656	31.843828
588.212328	40921.459304	31.848845
588.769668	40987.691316	31.853863
589.131856	41051.310418	31.858880
590.489525	41101.460520	31.863898
590.891709	41165.396243	31.868916
591.476606	41214.750562	31.873933
591.990822	41261.181429	31.878951
592.448324	41318.841217	31.883968
593.026139	41368.196990	31.888986
593.225916	41436.301538	31.894004
593.727228	41498.673157	31.899021
594.561722	41557.729213	31.904039
594.699475	41619.335898	31.909056
595.447787	41681.568156	31.914074
595.893505	41755.940964	31.919092
596.507756	41817.903664	31.924109
597.217730	41891.122378	31.929127
597.263897	41957.690364	31.934144
597.765930	42021.220797	31.939162
598.288815	42110.901533	31.944180
598.482642	42181.469695	31.949197
599.290697	42256.514809	31.954215
599.813785	42345.797997	31.959232
601.201627	42407.906849	31.964250
601.506039	42499.520870	31.969268
602.031799	42568.014283	31.974285
602.492493	42649.832303	31.979303
603.196145	42730.157810	31.984320
603.935236	42806.177001	31.989338
604.790352	42894.942350	31.994356
605.732984	42962.429256	31.999373
606.268024	43026.988406	32.004391
606.989531	43093.536269	32.009408
607.830328	43159.003019	32.014426
608.308365	43236.228404	32.019444
609.033746	43302.346174	32.024461
609.994753	43370.919385	32.029479
610.103414	43447.362095	32.034496
610.978656	43507.530232	32.039514
611.232205	43584.950118	32.044532
611.670135	43646.205492	32.049549
612.633622	43714.570641	32.054567
613.155829	43790.234998	32.059584
614.094921	43874.765771	32.064602
614.605722	43941.899484	32.069620
615.124812	44008.348954	32.074637
615.836044	44084.351583	32.079655
616.033103	44161.383815	32.084672
616.669385	44227.524613	32.089690
617.357732	44302.494189	32.094708
617.642540	44385.706127	32.099725
618.381592	44457.625701	32.104743
618.925455	44538.545740	32.109760
620.014763	44607.026758	32.114778
620.504768	44680.997594	32.119796
620.951706	44757.784002	32.124813
621.761445	44841.257009	32.129831
622.020199	44921.185674	32.134848
623.246640	44989.886764	32.139866
623.763850	45067.447615	32.144884
624.043778	45150.131796	32.149901
624.930371	45219.943217	32.154919
625.465921	45304.643808	32.159936
626.230020	45373.779054	32.164954
626.738555	45456.681594	32.169972
627.028051	45530.977622	32.174989
627.629766	45607.059503	32.180007
628.012340	45696.643803	32.185024
628.442159	45767.762012	32.190042
629.431898	45866.266339	32.195060
629.638801	45954.999870	32.200077
630.591962	46032.609643	32.205095
631.070021	46119.365600	32.210112
631.520411	46199.180227	32.215130
632.379135	46283.998367	32.220148
632.817362	46358.938067	32.225165
633.641872	46432.735756	32.230183
634.487408	46510.876444	32.235200
635.462860	46595.070163	32.240218
636.440463	46656.502286	32.245236
637.029340	46719.235386	32.250253
637.863860	46778.634237	32.255271
638.525410	46852.382903	32.260288
639.276134	46917.881073	32.265306
639.538877	46992.034266	32.270324
640.270681	47068.322117	32.275341
641.114710	47135.362570	32.280359
641.538113	47205.202066	32.285376
642.276186	47279.705623	32.290394
642.649767	47349.540712	32.295412
642.798150	47424.339537	32.300429
643.681071	47499.099490	32.305447
643.801780	47582.855035	32.310464
644.477223	47678.259583	32.315482
645.310726	47759.949276	32.320500
645.815818	47843.405175	32.325517
646.527703	47925.645934	32.330535
647.037989	48020.628598	32.335552
647.496662	48104.149659	32.340570
648.604844	48185.911741	32.345588
648.886027	48281.203411	32.350605
650.093184	48363.058179	32.355623
650.156090	48454.614076	32.360640
651.084977	48533.735627	32.365658
651.973957	48629.964816	32.370676
652.046780	48719.299539	32.375693
652.838176	48803.656793	32.380711
653.422109	48901.301475	32.385728
654.086469	49000.471395	32.390746
655.188767	49086.350052	32.395764
655.468153	49165.499580	32.400781
656.327257	49259.667206	32.405799
657.052765	49354.267390	32.410816
658.035799	49444.588581	32.415834
658.816479	49521.648861	32.420852
659.299942	49615.364288	32.425869
660.100220	49694.478350	32.430887
660.774251	49789.822320	32.435904
661.332833	49863.046379	32.440922
662.283625	49943.150053	32.445940
662.758055	50036.906571	32.450957
663.666959	50109.298315	32.455975
664.093137	50207.207348	32.460992
664.814269	50287.854357	32.466010
665.832904	50362.475859	32.471028
666.349484	50452.715870	32.476045
667.481730	50528.680468	32.481063
668.222927	50603.162705	32.486080
668.733608	50679.870521	32.491098
669.577375	50751.565823	32.496116
670.201541	50839.740449	32.501133
671.234402	50914.753799	32.506151
671.723189	50986.720551	32.511168
672.066914	51052.382859	32.516186
673.057425	51121.468427	32.521204
673.269248	51208.639698	32.526221
674.482655	51277.456709	32.531239
674.853764	51353.663432	32.536256
675.147078	51442.828625	32.541274
675.927339	51515.289204	32.546292
676.265446	51601.227288	32.551309
676.753810	51676.644746	32.556327
677.261528	51753.312277	32.561344
678.134933	51836.699646	32.566362
678.658729	51918.167846	32.571380
679.183542	52008.773285	32.576397
679.917793	52088.222242	32.581415
680.418881	52174.301431	32.586432
681.106614	52261.300866	32.591450
681.793698	52349.604238	32.596468
682.046692	52441.671335	32.601485
683.017978	52526.545518	32.606503
683.133358	52621.457062	32.611520
683.668244	52724.168793	32.616538
684.692117	52815.591426	32.621556
685.696547	52924.001510	32.626573
686.773769	53013.581472	32.631591
687.181922	53105.120641	32.636608
687.834174	53191.382387	32.641626
688.995558	53279.798497	32.646644
689.356402	53376.598359	32.651661
690.386471	53471.591575	32.656679
691.122871	53552.848649	32.661696
691.762363	53631.577291	32.666714
692.851941	53714.564133	32.671732
693.747386	53810.737842	32.676749
694.580529	53894.031256	32.681767
695.250858	53959.232911	32.686784
696.082953	54042.919361	32.691802
696.935456	54121.888394	32.696820
697.952132	54195.199856	32.701837
698.826545	54262.161277	32.706855
699.601957	54336.789267	32.711872
700.154454	54418.128746	32.716890
701.253780	54474.841691	32.721908
701.460528	54558.488673	32.726925
702.428854	54632.302672	32.731943
702.672065	54711.774104	32.736960
703.007596	54796.097877	32.741978
703.780369	54864.437523	32.746996
704.413773	54947.696313	32.752013
704.874468	55028.337148	32.757031
705.644593	55115.739239	32.762048
706.041130	55211.693002	32.767066
707.108543	55296.638043	32.772084
707.482692	55387.102861	32.777101
708.312602	55475.699335	32.782119
709.174482	55563.101357	32.787136
709.654730	55656.221248	32.792154
710.842946	55733.788748	32.797172
711.552835	55829.563026	32.802189
712.116657	55902.507671	32.807207
712.968135	55990.552085	32.812224
713.537557	56075.077919	32.817242
714.104597	56166.091395	32.822260
714.362817	56262.849480	32.827277
715.137242	56352.476830	32.832295
715.962844	56440.735804	32.837312
716.472979	56548.031061	32.842330
717.108402	56629.922041	32.847348
717.728599	56737.973035	32.852365
718.402130	56829.598915	32.857383
719.093406	56926.564003	32.862400
719.728877	57028.145718	32.867418
720.386205	57131.996553	32.872436
721.505843	57228.686921	32.877453
721.962031	57330.032166	32.882471
723.010380	57426.221837	32.887488
724.081447	57523.826055	32.892506
724.596880	57602.954328	32.897524
725.571205	57689.511047	32.902541
726.026412	57777.370900	32.907559
726.892399	57862.742661	32.912576
727.435061	57957.475644	32.917594
728.004931	58038.622171	32.922612
728.526260	58133.485768	32.927629
728.721165	58230.578132	32.932647
729.839054	58327.001013	32.937664
730.202900	58430.004622	32.942682
730.776327	58540.153360	32.947700
731.347525	58637.574516	32.952717
731.974501	58748.070258	32.957735
732.724449	58858.870047	32.962752
733.232023	58976.974549	32.967770
733.909031	59081.963645	32.972788
734.607041	59199.963452	32.977805
735.185102	59321.932270	32.982823
735.970184	59442.426128	32.987840
736.532383	59558.309526	32.992858
737.919780	59678.368427	32.997876
738.372775	59799.941458	33.002893
739.650896	59908.226366	33.007911
740.680486	60008.189063	33.012928
741.606554	60119.232842	33.017946
743.063774	60210.172753	33.022964
743.838165	60319.886614	33.027981
744.602408	60420.677445	33.032999
745.582091	60503.609992	33.038016
746.183148	60609.744257	33.043034
747.115905	60711.763217	33.048052
747.832573	60808.024522	33.053069
748.667910	60904.622100	33.058087
749.438115	60996.109276	33.063104
749.938012	61095.716247	33.068122
751.172633	61184.574063	33.073140
752.119144	61274.179956	33.078157
753.100472	61364.647946	33.083175
753.891347	61454.373817	33.088192
754.215889	61544.976968	33.093210
754.875489	61641.104866	33.098228
755.577692	61731.972401	33.103245
756.149106	61827.405850	33.108263
756.863178	61914.315805	33.113280
757.678007	62013.332754	33.118298
758.657329	62098.847142	33.123316
759.220454	62204.000341	33.128333
759.450524	62299.609335	33.133351
760.153566	62398.290825	33.138368
761.797432	62488.880736	33.143386
762.568763	62590.692171	33.148404
763.256658	62694.764396	33.153421
764.071283	62786.510779	33.158439
764.723663	62870.502733	33.163456
764.893141	62981.146086	33.168474
765.822688	63074.736705	33.173492
766.429967	63175.873530	33.178509
767.267775	63277.588731	33.183527
768.172831	63375.052303	33.188544
768.986122	63481.114976	33.193562
770.072990	63571.732741	33.198580
770.660316	63677.559412	33.203597
771.415195	63769.799893	33.208615
772.643290	63858.674627	33.213632
772.824841	63964.964889	33.218650
773.766246	64052.543081	33.223668
774.236519	64156.946683	33.228685
775.134763	64257.789078	33.233703
775.880259	64346.481546	33.238720
776.274793	64451.499663	33.243738
777.387701	64545.573532	33.248756
778.141975	64629.194562	33.253773
778.597335	64727.341572	33.258791
779.863862	64822.842211	33.263808
779.901552	64924.999595	33.268826
780.975506	65020.512144	33.273844
781.951132	65123.985927	33.278861
782.273987	65230.107447	33.283879
783.113601	65334.806297	33.288896
783.999692	65435.971859	33.293914
784.855591	65530.900030	33.298932
785.750925	65630.361839	33.303949
786.255282	65734.583019	33.308967
787.592122	65831.849196	33.313984
788.243070	65944.240899	33.319002
788.964398	66043.978495	33.324020
790.169194	66147.876424	33.329037
791.012375	66251.533829	33.334055
792.528652	66333.040459	33.339072
793.621948	66428.276703	33.344090
794.190090	66512.445935	33.349108
795.164581	66588.238657	33.354125
795.723527	66674.043368	33.359143
796.514513	66760.913708	33.364160
797.505144	66854.749373	33.369178
798.061970	66947.387010	33.374196
798.844726	67036.121037	33.379213
799.664573	67125.052174	33.384231
800.604228	67206.518927	33.389248
801.444080	67309.193422	33.394266
801.937793	67402.982277	33.399284
802.671768	67493.441396	33.404301
803.207821	67586.819068	33.409319
804.076380	67693.150307	33.414336
804.799276	67798.048500	33.419354
805.550999	67898.605361	33.424372
806.307678	67989.258954	33.429389
806.909634	68097.881390	33.434407
807.636478	68196.626086	33.439424
808.122053	68312.314963	33.444442
809.250783	68420.704306	33.449460
809.719971	68526.613968	33.454477
810.308317	68645.283230	33.459495
811.337014	68752.562546	33.464512
811.877741	68867.599411	33.469530
812.315773	69001.439946	33.474548
813.406566	69109.660820	33.479565
813.855875	69223.966399	33.484583
814.894563	69343.119226	33.489600
816.104407	69469.508749	33.494618
816.634043	69589.128675	33.499636
817.740637	69704.922816	33.504653
818.171889	69826.990799	33.509671
819.115895	69954.982030	33.514688
820.106918	70074.937202	33.519706
820.790089	70191.914288	33.524724
821.656621	70322.249739	33.529741
822.097593	70445.104297	33.534759
823.044541	70571.552990	33.539776
823.690344	70699.227280	33.544794
824.209296	70828.657149	33.549812
825.220273	70953.476548	33.554829
825.947984	71089.764761	33.559847
826.664440	71221.052725	33.564864
827.412775	71351.791751	33.569882
828.500964	71480.882390	33.574900
829.377269	71602.496324	33.579917
829.835167	71743.997607	33.584935
830.381311	71859.927020	33.589952
831.287293	71984.983060	33.594970
832.219796	72115.481717	33.599988
832.892152	72234.838035	33.605005
833.728469	72380.146469	33.610023
834.388059	72512.146364	33.615040
835.043292	72646.414773	33.620058
836.014341	72790.159128	33.625076
837.241121	72928.113889	33.630093
837.661124	73062.889873	33.635111
838.590126	73207.339694	33.640128
839.589205	73346.662213	33.645146
840.141978	73480.355562	33.650164
841.629568	73604.998833	33.655181
842.768974	73733.737756	33.660199
844.119532	73865.458830	33.665216
845.287877	73980.641405	33.670234
846.390071	74098.710124	33.675252
847.364995	74229.237825	33.680269
848.264243	74342.994776	33.685287
849.349599	74454.785071	33.690304
849.781100	74576.089570	33.695322
850.398107	74691.893530	33.700340
851.683984	74815.054004	33.705357
852.005412	74948.816227	33.710375
852.794074	75073.943104	33.715392
853.504462	75208.988405	33.720410
854.069496	75332.441451	33.725428
855.351733	75459.494222	33.730445
855.521223	75602.581131	33.735463
856.228991	75736.438759	33.740480
857.364188	75869.052060	33.745498
857.917375	76008.914204	33.750516
859.410356	76140.269407	33.755533
860.359218	76282.211797	33.760551
861.262775	76408.124893	33.765568
862.057160	76543.822397	33.770586
862.841190	76685.184650	33.775604
864.573185	76794.438491	33.780621
865.444526	76928.061015	33.785639
866.591841	77049.885210	33.790656
867.202320	77173.276152	33.795674
868.232512	77301.871805	33.800692
868.889426	77418.415878	33.805709
869.732254	77552.767992	33.810727
870.557036	77668.602766	33.815744
871.534165	77791.977084	33.820762
872.230859	77920.159130	33.825780
873.022411	78040.548577	33.830797
874.097110	78179.111327	33.835815
874.964953	78304.341968	33.840832
875.890633	78433.035286	33.845850
876.523222	78557.429784	33.850868
877.534417	78672.517482	33.855885
878.330061	78814.015553	33.860903
878.905990	78940.358950	33.865920
879.742257	79077.607984	33.870938
880.331261	79208.346622	33.875956
881.118040	79344.806589	33.880973
881.715867	79488.872855	33.885991
882.789233	79624.617865	33.891008
883.794226	79771.966466	33.896026
884.369843	79912.731766	33.901044
885.367327	80047.160453	33.906061
886.574351	80199.496690	33.911079
887.180125	80322.978425	33.916096
888.143006	80454.817274	33.921114
889.074818	80589.448891	33.926132
889.867631	80716.070439	33.931149
891.018222	80851.441898	33.936167
891.942903	80976.282899	33.941184
893.087311	81097.808598	33.946202
893.630932	81244.134921	33.951220
894.349115	81370.809112	33.956237
895.681281	81490.191245	33.961255
896.504283	81625.744421	33.966272
898.170805	81743.136773	33.971290
898.751947	81879.831327	33.976308
899.758057	82000.609698	33.981325
900.460074	82136.437668	33.986343
901.067619	82253.035017	33.991360
902.347237	82382.121861	33.996378
903.157538	82520.342065	34.001396
903.957245	82651.367816	34.006413
904.568475	82785.565954	34.011431
905.555807	82917.298437	34.016448
906.769628	83052.442461	34.021466
907.033691	83192.335275	34.026484
908.160946	83330.725183	34.031501
908.951025	83472.450280	34.036519
909.751943	83615.302085	34.041536
910.753251	83755.703087	34.046554
911.595043	83899.842340	34.051572
912.765625	84035.517286	34.056589
913.621994	84181.923782	34.061607
914.156213	84332.993758	34.066624
915.196971	84471.542094	34.071642
916.080207	84626.613744	34.076660
916.549912	84781.979060	34.081677
917.361537	84931.450158	34.086695
918.342668	85083.898625	34.091712
919.811076	85243.456358	34.096730
920.622122	85397.985898	34.101748
922.076945	85533.560022	34.106765
923.412570	85679.987767	34.111783
924.453512	85819.138096	34.116800
925.661686	85951.204689	34.121818
926.328386	86091.200571	34.126836
927.522112	86228.098677	34.131853
928.404951	86373.333607	34.136871
929.095745	86507.321170	34.141888
930.865333	86643.307372	34.146906
931.286898	86779.746045	34.151924
932.191041	86913.385256	34.156941
933.127765	87047.691608	34.161959
933.423404	87198.522355	34.166976
934.197245	87332.513357	34.171994
935.240485	87481.390994	34.177012
936.188422	87635.036519	34.182029
937.337359	87770.009931	34.187047
938.014230	87925.891777	34.192064
938.851223	88068.709105	34.197082
939.653834	88231.682291	34.202100
940.597491	88375.865737	34.207117
941.439285	88527.175358	34.212135
942.364159	88671.946139	34.217152
943.869572	88823.280094	34.222170
944.755349	88974.851242	34.227188
945.535694	89121.750583	34.232205
946.851670	89264.371931	34.237223
947.775313	89414.672059	34.242240
948.796052	89554.071298	34.247258
949.413621	89706.461231	34.252276
949.929385	89853.798472	34.257293
951.078372	89999.174276	34.262311
951.730232	90159.152612	34.267328
952.827674	90285.882276	34.272346
953.623439	90427.399284	34.277364
954.196459	90576.847621	34.282381
955.061520	90732.955457	34.287399
955.594540	90900.890191	34.292416
956.793680	91051.877785	34.297434
957.905908	91211.916363	34.302452
958.686532	91371.285280	34.307469
959.637294	91533.302655	34.312487
960.285823	91702.161634	34.317504
961.586646	91852.072652	34.322522
962.275532	92023.702779	34.327540
963.658521	92187.443056	34.332557
965.111939	92335.127198	34.337575
966.038906	92500.917788	34.342592
967.179294	92657.245893	34.347610
968.213790	92819.700606	34.352628
969.655559	92977.415404	34.357645
970.782724	93109.462944	34.362663
971.714495	93252.796982	34.367680
972.963778	93400.961846	34.372698
973.953263	93550.232805	34.377716
975.047131	93695.140578	34.382733
976.223444	93834.382998	34.387751
976.980493	93978.242096	34.392768
978.167525	94127.484916	34.397786
978.803999	94270.679785	34.402804
979.931581	94417.499643	34.407821
981.054835	94571.267030	34.412839
981.681149	94714.148648	34.417856
982.940282	94853.078464	34.422874
984.384271	95003.147201	34.427892
985.233613	95138.922839	34.432909
986.525199	95277.114274	34.437927
988.084694	95414.833397	34.442944
989.381436	95538.447998	34.447962
989.826091	95678.497728	34.452980
990.929478	95810.585842	34.457997
992.317258	95933.338458	34.463015
993.180628	96070.827205	34.468032
993.646799	96208.315361	34.473050
994.476622	96349.651447	34.478068
995.375659	96496.301355	34.483085
996.527081	96633.519285	34.488103
997.275626	96791.121102	34.493120
998.156514	96926.760087	34.498138
998.879143	97073.376910	34.503156
999.175813	97227.996617	34.508173
1000.399796	97383.245162	34.513191
1001.090944	97540.770955	34.518208
1001.740060	97715.658555	34.523226
1002.645117	97874.876545	34.528244
1003.709112	98036.846678	34.533261
1004.863567	98198.664023	34.538279
1005.440442	98378.193641	34.543296
1006.287006	98547.274168	34.548314
1007.064677	98725.468555	34.553332
1007.737783	98917.840745	34.558349
1008.980170	99100.959276	34.563367
1009.986473	99282.417045	34.568384
1010.824980	99477.124665	34.573402
1011.529689	99647.209339	34.578420
1012.915707	99831.475856	34.583437
1014.025387	100024.432841	34.588455
1014.804173	100218.114698	34.593472
1016.064428	100397.016086	34.598490
1016.785449	100584.015292	34.603508
1017.511442	100753.760125	34.608525
1019.182250	100917.728885	34.613543
1020.493030	101101.950988	34.618560
1021.257982	101268.269315	34.623578
1022.344270	101445.707666	34.628596
1023.083000	101617.572241	34.633613
1023.896729	101791.809499	34.638631
1025.413740	101982.863235	34.643648
1026.061015	102158.180798	34.648666
1027.316953	102336.408810	34.653684
1028.097174	102529.495524	34.658701
1029.399975	102708.288740	34.663719
1030.157379	102900.113316	34.668736
1030.830521	103087.438529	34.673754
1032.156580	103274.421674	34.678772
1033.388958	103478.765369	34.683789
1034.351448	103649.996863	34.688807
1035.614089	103842.914234	34.693824
1036.837532	104022.563749	34.698842
1038.062699	104218.151776	34.703860
1038.970279	104401.973533	34.708877
1040.093517	104583.213971	34.713895
1041.217435	104768.702898	34.718912
1042.807043	104955.616120	34.723930
1043.160701	105144.080598	34.728948
1043.884905	105327.961467	34.733965
1045.601034	105519.295880	34.738983
1046.738518	105707.425214	34.744000
1048.071737	105891.949217	34.749018
1049.177521	106069.903575	34.754036
1049.769135	106260.733496	34.759053
1050.742390	106448.068429	34.764071
1052.106139	106634.011834	34.769088
1053.723236	106816.505602	34.774106
1054.402675	107002.621543	34.779124
1055.194485	107181.822782	34.784141
1057.017800	107366.062434	34.789159
1057.987762	107553.175660	34.794176
1058.818547	107727.643808	34.799194
1060.142768	107909.681999	34.804212
1060.797569	108097.342053	34.809229
1062.005905	108267.949603	34.814247
1063.400845	108448.508582	34.819264
1064.774435	108636.059010	34.824282
1066.029078	108816.996929	34.829300
1067.143963	108988.167919	34.834317
1068.405457	109155.867540	34.839335
1069.239812	109334.921054	34.844352
1070.530353	109499.663066	34.849370
1071.731884	109674.970599	34.854388
1072.839655	109845.373329	34.859405
1074.142230	110012.360454	34.864423
1074.911290	110168.792164	34.869440
1075.775875	110340.402050	34.874458
1077.346873	110511.331503	34.879476
1077.985985	110684.005561	34.884493
1079.211288	110853.202674	34.889511
1080.198710	111037.934936	34.894528
1081.223693	111212.136366	34.899546
1081.938233	111383.812828	34.904564
1083.603404	111552.500532	34.909581
1084.566984	111719.092205	34.914599
1085.757064	111892.954057	34.919616
1086.777405	112066.171173	34.924634
1087.824738	112241.819876	34.929652
1088.770188	112412.425173	34.934669
1089.463036	112586.647233	34.939687
1090.253888	112754.741892	34.944704
1091.465234	112922.314934	34.949722
1092.521084	113090.027237	34.954740
1093.067048	113263.539967	34.959757
1094.300401	113435.791793	34.964775
1095.187337	113620.591090	34.969792
1096.285028	113804.559316	34.974810
1097.243863	113977.338624	34.979828
1098.337275	114166.445872	34.984845
1099.249121	114347.110333	34.989863
1099.953248	114537.612147	34.994880
1100.910712	114738.576849	34.999898
1101.907972	114927.994782	35.004916
1102.977349	115132.508067	35.009933
1104.078030	115335.140461	35.014951
1105.742403	115529.517657	35.019968
1107.028800	115719.870996	35.024986
1108.503825	115916.651657	35.030004
1109.532721	116104.459854	35.035021
1110.656203	116279.228155	35.040039
1111.888464	116482.759424	35.045056
1113.374311	116673.479603	35.050074
1114.559983	116862.142240	35.055092
1115.845618	117051.563891	35.060109
1117.104401	117234.420439	35.065127
1118.152306	117422.206898	35.070144
1119.071889	117607.845413	35.075162
1120.123954	117803.268899	35.080180
1121.071087	117991.961850	35.085197
1122.204342	118181.780866	35.090215
1123.487913	118381.471036	35.095232
1124.348854	118586.264105	35.100250
1125.362871	118775.597374	35.105268
1126.537766	118986.837860	35.110285
1127.660051	119179.289244	35.115303
1128.878309	119371.016231	35.120320
1129.884916	119574.789696	35.125338
1131.368936	119766.020398	35.130356
1132.398495	119982.058569	35.135373
1133.449308	120173.257629	35.140391
1134.809230	120376.739000	35.145408
1135.372214	120581.525908	35.150426
1136.618899	120779.813581	35.155444
1137.662574	120995.246297	35.160461
1138.872195	121204.387730	35.165479
1140.218305	121398.108989	35.170496
1141.035536	121612.971664	35.175514
1142.187454	121825.588543	35.180532
1143.194173	122045.662992	35.185549
1144.464145	122251.324729	35.190567
1145.489576	122468.455559	35.195584
1146.542673	122687.549529	35.200602
1147.554501	122898.316627	35.205620
1148.845225	123117.667540	35.210637
1150.206068	123333.329775	35.215655
1151.213605	123559.615891	35.220672
1152.382866	123780.321484	35.225690
1153.493707	123991.687781	35.230708
1154.269746	124217.569834	35.235725
1155.571380	124453.963885	35.240743
1157.604127	124637.013101	35.245760
1159.266928	124841.561017	35.250778
1160.682155	125045.958426	35.255796
1162.409026	125252.071500	35.260813
1163.549517	125427.525208	35.265831
1164.802222	125621.065892	35.270848
1165.813622	125825.149833	35.275866
1167.018971	126018.674438	35.280884
1167.844827	126198.887489	35.285901
1169.534205	126367.700230	35.290919
1170.961223	126528.003772	35.295936
1171.595472	126714.567148	35.300954
1172.794272	126885.945453	35.305972
1173.746979	127070.963516	35.310989
1174.914648	127253.373268	35.316007
1176.536000	127420.526262	35.321024
1177.707210	127601.059286	35.326042
1179.123091	127768.258530	35.331060
1180.032108	127947.248189	35.336077
1181.303974	128130.267146	35.341095
1182.505977	128304.416638	35.346112
1183.219797	128495.187756	35.351130
1184.601246	128665.428280	35.356148
1185.480440	128849.844034	35.361165
1186.614937	129044.903630	35.366183
1187.799376	129233.574387	35.371200
1188.711638	129427.274885	35.376218
1189.947339	129624.592413	35.381236
1190.862597	129824.815795	35.386253
1191.955210	130039.527364	35.391271
1193.125264	130235.931776	35.396288
1194.087124	130445.083124	35.401306
1194.932337	130661.371793	35.406324
1196.074459	130872.324091	35.411341
1197.154457	131086.484586	35.416359
1198.143477	131310.290820	35.421376
1199.039070	131530.978802	35.426394
1200.920422	131755.853040	35.431412
1202.038648	131969.440926	35.436429
1203.000487	132194.677078	35.441447
1204.186392	132421.566901	35.446464
1205.281652	132650.971764	35.451482
1206.885760	132873.839578	35.456500
1208.061749	133099.072220	35.461517
1209.264875	133327.778521	35.466535
1210.394213	133553.287243	35.471552
1211.718558	133787.750422	35.476570
1212.931718	134017.981390	35.481588
1214.188083	134246.265340	35.486605
1215.311630	134486.435680	35.491623
1216.477026	134704.965495	35.496640
1217.924922	134944.465732	35.501658
1219.023336	135174.631771	35.506676
1219.986299	135405.568866	35.511693
1221.352661	135640.162028	35.516711
1222.694993	135881.472975	35.521728
1223.742206	136127.069757	35.526746
1224.868282	136358.861741	35.531764
1226.272854	136610.179013	35.536781
1227.139920	136842.978415	35.541799
1228.358217	137085.558727	35.546816
1229.747207	137338.367135	35.551834
1231.279672	137569.670131	35.556852
1232.417934	137824.157457	35.561869
1233.278853	138061.989247	35.566887
1234.430648	138309.256361	35.571904
1236.163486	138562.601337	35.576922
1237.131154	138799.836403	35.581940
1238.648663	139038.344472	35.586957
1239.754812	139277.006974	35.591975
1241.017865	139519.453301	35.596992
1242.270103	139768.895125	35.602010
1243.706294	140017.154599	35.607028
1244.593771	140261.884376	35.612045
1245.528654	140512.217350	35.617063
1247.318496	140752.176197	35.622080
1248.495403	140994.656171	35.627098
1249.792993	141216.419334	35.632116
1251.185241	141454.438718	35.637133
1252.529132	141669.825758	35.642151
1253.803734	141897.116291	35.647168
1254.803660	142133.817060	35.652186
1255.972532	142370.061018	35.657204
1257.275515	142605.714004	35.662221
1258.124593	142842.061053	35.667239
1259.821839	143080.865535	35.672256
1261.390446	143320.998540	35.677274
1262.478408	143551.079992	35.682292
1263.900094	143793.345092	35.687309
1265.091873	144038.198403	35.692327
1265.879034	144272.188562	35.697344
1266.968655	144507.198583	35.702362
1268.162244	144759.251432	35.707380
1269.797340	145008.342638	35.712397
1270.816168	145260.438027	35.717415
1272.331594	145501.110134	35.722432
1273.519001	145761.291898	35.727450
1274.751193	146006.478381	35.732468
1276.490179	146255.648251	35.737485
1277.630031	146512.731635	35.742503
1279.130586	146752.231532	35.747520
1280.503168	147003.759697	35.752538
1281.559578	147250.642311	35.757556
1283.043231	147504.617865	35.762573
1284.461524	147759.176054	35.767591
1285.439333	148000.819721	35.772608
1286.741711	148260.107492	35.777626
1287.995413	148511.598023	35.782644
1289.034850	148773.556892	35.787661
1290.411485	149037.393603	35.792679
1291.313088	149288.422501	35.797696
1292.728424	149568.858315	35.802714
1294.184199	149824.042475	35.807732
1295.488396	150080.254335	35.812749
1297.039842	150349.312426	35.817767
1298.707234	150607.627786	35.822784
1300.202395	150866.034795	35.827802
1301.155227	151132.816775	35.832820
1302.903803	151387.035792	35.837837
1303.635308	151643.471554	35.842855
1304.892214	151905.614578	35.847872
1306.346193	152164.161048	35.852890
1307.644487	152430.641325	35.857908
1308.816782	152690.503704	35.862925
1309.839096	152968.428824	35.867943
1311.436011	153237.760398	35.872960
1312.655434	153508.167867	35.877978
1313.723126	153785.048980	35.882996
1315.209346	154050.390395	35.888013
1316.464419	154319.387075	35.893031
1317.857055	154581.838620	35.898048
1319.191599	154859.622522	35.903066
1320.438014	155139.528823	35.908084
1321.728692	155406.366938	35.913101
1322.907787	155684.724975	35.918119
1325.042348	155947.256965	35.923136
1325.741627	156227.393754	35.928154
1327.265205	156506.171455	35.933172
1328.543680	156765.616634	35.938189
1330.261761	157036.965338	35.943207
1331.941398	157296.857825	35.948224
1333.512718	157557.428529	35.953242
1334.826843	157830.595954	35.958260
1336.318941	158074.195408	35.963277
1337.296348	158333.631004	35.968295
1338.620739	158577.703055	35.973312
1339.650033	158823.066399	35.978330
1340.771874	159079.511876	35.983348
1342.155442	159334.622531	35.988365
1343.115470	159593.532967	35.993383
1344.305672	159852.992440	35.998400
1345.276851	160124.116310	36.003418
1346.693636	160388.747676	36.008436
1348.023908	160656.986541	36.013453
1349.167182	160937.938736	36.018471
1350.545561	161209.168577	36.023488
1351.865974	161490.285920	36.028506
1352.959253	161785.049933	36.033524
1354.603182	162056.432236	36.038541
1355.768029	162343.912887	36.043559
1357.070390	162634.483796	36.048576
1358.466677	162920.902401	36.053594
1360.080363	163215.362926	36.058612
1361.563834	163482.688155	36.063629
1362.607751	163780.579469	36.068647
1364.245830	164066.000294	36.073664
1365.972052	164351.954484	36.078682
1367.398812	164644.406508	36.083700
1368.771341	164940.562942	36.088717
1370.269771	165222.531730	36.093735
1371.880934	165510.184771	36.098752
1373.154231	165803.935468	36.103770
1374.618468	166090.115750	36.108788
1376.113926	166363.037023	36.113805
1377.698399	166646.826516	36.118823
1379.009947	166930.571009	36.123840
1380.897863	167206.494079	36.128858
1382.094717	167495.007415	36.133876
1383.973662	167763.925405	36.138893
1385.025876	168057.580528	36.143911
1386.171075	168332.595787	36.148928
1387.442603	168614.144010	36.153946
1388.617542	168906.475601	36.158964
1390.295535	169176.382629	36.163981
1391.671024	169482.944061	36.168999
1392.532977	169768.662069	36.174016
1394.232674	170057.767213	36.179034
1395.258558	170349.873955	36.184052
1396.938385	170649.015432	36.189069
1397.985341	170943.432130	36.194087
1399.111083	171241.583415	36.199104
1400.984544	171540.380695	36.204122
1402.500871	171851.373968	36.209140
1404.180561	172141.874302	36.214157
1405.579120	172443.492143	36.219175
1406.746222	172740.106378	36.224192
1408.563064	173023.782563	36.229210
1410.169031	173319.949378	36.234228
1411.169305	173614.307430	36.239245
1412.483812	173910.331615	36.244263
1413.902470	174207.686589	36.249280
1415.313083	174506.059771	36.254298
1416.797297	174811.228717	36.259316
1418.213615	175099.101879	36.264333
1419.649188	175404.560028	36.269351
1420.916684	175699.848946	36.274368
1422.285445	176002.246804	36.279386
1423.489217	176306.843004	36.284404
1425.033913	176603.336188	36.289421
1426.659664	176904.668527	36.294439
1427.884790	177214.496425	36.299456
1429.379267	177516.181647	36.304474
1430.909578	177805.747910	36.309492
1432.983140	178073.820298	36.314509
1434.382210	178349.872238	36.319527
1435.961255	178618.836426	36.324544
1437.778386	178893.478593	36.329562
1438.666077	179179.543578	36.334580
1440.606117	179456.022274	36.339597
1441.690796	179732.051563	36.344615
1442.891068	180016.317871	36.349632
1443.836175	180297.170910	36.354650
1445.857625	180582.199388	36.359668
1447.137016	180857.541287	36.364685
1448.510455	181150.571727	36.369703
1449.617927	181439.784208	36.374720
1451.006407	181737.715984	36.379738
1452.448712	182032.846470	36.384756
1453.848788	182326.612976	36.389773
1455.612136	182621.187078	36.394791
1457.013933	182924.504970	36.399808
1458.262774	183224.444344	36.404826
1459.747616	183532.119702	36.409844
1460.870243	183829.566222	36.414861
1462.234275	184143.358105	36.419879
1463.441029	184462.407773	36.424896
1464.965871	184777.319433	36.429914
1466.628992	185095.690107	36.434932
1468.229872	185415.620869	36.439949
1469.246100	185737.447482	36.444967
1470.308739	186068.284592	36.449984
1471.948823	186395.730450	36.455002
1473.467299	186723.958346	36.460020
1474.976461	187052.290315	36.465037
1476.462519	187397.517666	36.470055
1477.233748	187738.311454	36.475072
1479.134480	188078.726325	36.480090
1480.342742	188503.298848	36.485108
1481.828815	188832.198591	36.490125
1483.421838	189181.935996	36.495143
1484.995246	189523.905114	36.500160
1486.899154	189875.399402	36.505178
1488.373625	190219.849897	36.510196
1489.617242	190561.772105	36.515213
1491.262437	190903.530853	36.520231
1493.123847	191247.822192	36.525248
1494.724854	191596.905182	36.530266
1496.142277	191945.560698	36.535284
1497.823082	192286.987580	36.540301
1499.692001	192624.601246	36.545319
1500.821531	192973.939734	36.550336
1502.771163	193317.181614	36.555354
1504.459882	193642.049537	36.560372
1506.155454	193976.976020	36.565389
1507.766523	194309.630487	36.570407
1508.973026	194651.417333	36.575424
1510.719744	194981.232723	36.580442
1512.371775	195318.353912	36.585460
1513.846923	195648.950067	36.590477
1515.477370	195976.652346	36.595495
1516.546891	196320.217510	36.600512
1518.064927	196649.691658	36.605530
1519.577993	196999.056802	36.610548
1521.033362	197327.043615	36.615565
1522.525896	197660.131094	36.620583
1523.795916	198015.353699	36.625600
1525.260651	198341.512366	36.630618
1526.560279	198700.567627	36.635636
1527.808130	199046.676832	36.640653
1529.797248	199383.195840	36.645671
1530.955401	199728.355311	36.650688
1532.465005	200059.844985	36.655706
1534.108384	200387.504075	36.660724
1535.333709	200725.694963	36.665741
1536.964393	201059.377697	36.670759
1538.060723	201399.673118	36.675776
1539.669736	201740.498632	36.680794
1541.137988	202085.792270	36.685812
1542.607040	202433.398083	36.690829
1544.551927	202779.304337	36.695847
1545.789701	203132.028197	36.700864
1547.382926	203477.812991	36.705882
1548.888463	203837.151765	36.710900
1550.125318	204186.168961	36.715917
1551.965750	204540.020455	36.720935
1553.143576	204903.553143	36.725952
1555.537311	205247.183583	36.730970
1557.455500	205595.842590	36.735988
1558.896118	205966.931505	36.741005
1560.661128	206309.518969	36.746023
1562.150113	206656.875137	36.751040
1564.192923	207012.401170	36.756058
1565.672885	207360.598153	36.761076
1566.877829	207706.781055	36.766093
1569.049882	208062.923575	36.771111
1570.484761	208417.632406	36.776128
1572.040197	208763.914413	36.781146
1574.080635	209104.989537	36.786164
1575.638932	209467.631781	36.791181
1577.068610	209817.313551	36.796199
1578.118193	210171.348442	36.801216
1579.823319	210541.717209	36.806234
1581.425692	210894.015296	36.811252
1582.547346	211263.688823	36.816269
1584.274054	211621.201456	36.821287
1585.393922	212000.529517	36.826304
1587.256667	212354.541437	36.831322
1588.958924	212731.264285	36.836340
1590.329525	213097.446160	36.841357
1592.724301	213458.133379	36.846375
1593.824773	213836.653692	36.851392
1595.763554	214201.960297	36.856410
1597.787247	214569.311677	36.861428
1599.059782	214943.106503	36.866445
1601.069518	215315.566927	36.871463
1602.226900	215688.745370	36.876480
1603.708345	216047.596473	36.881498
1605.627627	216421.469228	36.886516
1606.601892	216799.148338	36.891533
1608.684079	217158.134920	36.896551
1609.973814	217546.053802	36.901568
1611.593522	217915.198638	36.906586
1613.164298	218298.475964	36.911604
1614.437052	218679.844077	36.916621
1617.046718	219052.238827	36.921639
1618.589694	219427.315719	36.926656
1620.447458	219789.844782	36.931674
1621.821514	220168.632073	36.936692
1623.399040	220552.849563	36.941709
1625.280110	220918.093717	36.946727
1626.726915	221303.449760	36.951744
1628.398397	221667.380578	36.956762
1630.050207	222053.416118	36.961780
1631.647840	222429.527265	36.966797
1633.514849	222807.527061	36.971815
1634.874572	223180.220669	36.976832
1636.386593	223558.377793	36.981850
1638.248892	223918.265432	36.986868
1639.833012	224284.852518	36.991885
1641.659048	224629.249412	36.996903
1643.086144	224983.489332	37.001920
1645.060545	225336.957697	37.006938
1647.538931	225662.326480	37.011956
1648.767302	225999.551351	37.016973
1650.737156	226339.784864	37.021991
1652.233834	226687.586601	37.027008
1653.981435	227041.420600	37.032026
1655.584931	227382.066978	37.037044
1657.067133	227739.473559	37.042061
1658.273332	228087.498348	37.047079
1659.681691	228450.556021	37.052096
1661.368674	228803.128923	37.057114
1662.983660	229168.440407	37.062132
1664.086868	229538.125136	37.067149
1665.873398	229906.762835	37.072167
1667.442848	230281.607525	37.077184
1668.804435	230662.352895	37.082202
1670.223034	231040.955216	37.087220
1671.608210	231437.192918	37.092237
1672.931557	231833.592481	37.097255
1674.602171	232237.736454	37.102272
1676.204062	232642.017922	37.107290
1677.796530	233052.651543	37.112308
1679.381149	233469.510020	37.117325
1681.523065	233862.375905	37.122343
1682.997828	234276.583476	37.127360
1684.662192	234687.382288	37.132378
1686.281573	235104.818139	37.137396
1687.725482	235532.010668	37.142413
1689.178653	235951.503958	37.147431
1690.847565	236379.676495	37.152448
1692.867788	236805.431013	37.157466
1694.728611	237236.874975	37.162484
1696.559381	237664.969817	37.167501
1698.312413	238090.916963	37.172519
1699.980390	238522.440225	37.177536
1701.582720	238950.518278	37.182554
1703.158742	239386.754346	37.187572
1705.347489	239807.499392	37.192589
1707.711682	240227.301830	37.197607
1709.854120	240640.558856	37.202624
1711.903118	241053.702844	37.207642
1714.334118	241458.860572	37.212660
1716.587260	241864.705966	37.217677
1718.467588	242253.334863	37.222695
1720.186043	242662.056948	37.227712
1721.787038	243059.924175	37.232730
1723.469869	243459.606925	37.237748
1725.271847	243860.794498	37.242765
1727.076371	244248.720592	37.247783
1728.915847	244637.199381	37.252800
1730.571211	245026.722380	37.257818
1732.139367	245419.611463	37.262836
1733.623339	245817.593511	37.267853
1735.440521	246207.165124	37.272871
1736.698705	246617.399596	37.277888
1738.513673	247016.216492	37.282906
1740.146657	247420.014517	37.287924
1741.624071	247832.980902	37.292941
1743.417186	248237.590343	37.297959
1745.068622	248647.784154	37.302976
1746.441072	249066.403427	37.307994
1748.514187	249474.090669	37.313012
1749.775249	249891.734652	37.318029
1751.720172	250296.213870	37.323047
1753.190970	250710.520674	37.328064
1754.514481	251113.951995	37.333082
1756.320025	251515.579523	37.338100
1757.885246	251930.376390	37.343117
1759.479840	252340.036371	37.348135
1761.089331	252744.561757	37.353152
1762.649986	253163.826649	37.358170
1764.538989	253582.353116	37.363188
1765.814584	254006.613492	37.368205
1767.505704	254426.895757	37.373223
1769.227757	254861.828504	37.378240
1770.707013	255298.855377	37.383258
1772.671841	255729.683172	37.388276
1774.353169	256185.675646	37.393293
1776.231468	256615.929884	37.398311
1777.974921	257061.393565	37.403328
1779.984118	257518.600110	37.408346
1782.283370	257957.090057	37.413364
1783.940223	258399.565290	37.418381
1785.475611	258841.270523	37.423399
1787.479305	259294.966099	37.428416
1789.241031	259739.553684	37.433434
1791.193527	260186.395773	37.438452
1792.573644	260645.340011	37.443469
1794.267831	261103.674476	37.448487
1796.346394	261561.692949	37.453504
1797.973755	262020.211959	37.458522
1799.933690	262490.411731	37.463540
1801.393737	262961.221102	37.468557
1803.558301	263418.126224	37.473575
1805.183482	263890.226468	37.478592
1806.634975	264365.272705	37.483610
1808.944431	264844.144803	37.488628
1810.843442	265321.046976	37.493645
1812.490830	265789.071250	37.498663
1814.385880	266265.766404	37.503680
1816.187116	266744.277264	37.508698
1818.191603	267210.943639	37.513716
1819.862549	267700.290020	37.518733
1821.773150	268184.084967	37.523751
1823.846802	268665.566099	37.528768
1825.553421	269155.864541	37.533786
1827.226310	269633.695277	37.538804
1829.164400	270119.304564	37.543821
1830.961651	270603.079266	37.548839
1832.849185	271090.469091	37.553856
1834.199030	271595.972547	37.558874
1836.246450	272080.512794	37.563892
1838.353380	272570.577608	37.568909
1840.493361	273066.780536	37.573927
1842.266479	273544.599885	37.578944
1843.982514	274044.545979	37.583962
1845.989522	274525.853293	37.588980
1847.811340	275024.405539	37.593997
1849.786685	275509.902464	37.599015
1851.670803	276006.712016	37.604032
1853.515889	276498.191464	37.609050
1855.583449	276987.880760	37.614068
1857.191013	277468.141038	37.619085
1859.044002	277946.099767	37.624103
1861.320342	278448.089434	37.629120
1862.945876	278952.615583	37.634138
1865.134398	279433.636143	37.639156
1866.957861	279926.290778	37.644173
1868.948455	280415.030633	37.649191
1870.935354	280894.778200	37.654208
1872.662927	281377.001058	37.659226
1874.857735	281856.074920	37.664244
1876.873112	282344.721800	37.669261
1878.488551	282800.568365	37.674279
1880.523987	283266.478337	37.679296
1882.154344	283737.958985	37.684314
1884.142934	284184.799697	37.689332
1886.316353	284646.844476	37.694349
1888.395115	285093.741369	37.699367
1890.021388	285555.814839	37.704384
1891.477188	286017.277013	37.709402
1893.292893	286472.839443	37.714420
1895.373096	286938.209568	37.719437
1896.932577	287409.904347	37.724455
1898.887833	287880.949796	37.729472
1900.570412	288372.881093	37.734490
1902.830308	288827.570533	37.739508
1904.352061	289323.836289	37.744525
1906.122166	289809.039571	37.749543
1907.872405	290287.742158	37.754560
1909.670921	290779.763676	37.759578
1912.131915	291258.880818	37.764596
1914.192050	291749.279498	37.769613
1915.982120	292243.626594	37.774631
1918.316560	292728.667958	37.779648
1919.572962	293223.141357	37.784666
1921.451275	293719.722261	37.789684
1923.566148	294227.585639	37.794701
1925.038828	294728.106139	37.799719
1926.985177	295224.536820	37.804736
1928.927578	295743.610558	37.809754
1931.309428	296240.142137	37.814772
1933.387301	296747.430804	37.819789
1935.009032	297269.638290	37.824807
1937.105585	297770.796404	37.829824
1939.303210	298267.516812	37.834842
1941.252430	298771.507045	37.839860
1943.651646	299287.278039	37.844877
1945.180072	299796.909913	37.849895
1947.294373	300312.563534	37.854912
1949.107397	300834.809072	37.859930
1951.182412	301348.250366	37.864948
1953.377111	301862.861150	37.869965
1954.882427	302376.508628	37.874983
1957.318046	302891.224055	37.880000
1959.117254	303418.828097	37.885018
1961.286657	303932.762612	37.890036
1963.042259	304447.746774	37.895053
1965.205538	304965.378123	37.900071
1967.153184	305492.582380	37.905088
1969.081014	306015.342104	37.910106
1970.595493	306539.506418	37.915124
1972.533449	307064.157429	37.920141
1974.358729	307595.318595	37.925159
1976.185015	308127.539981	37.930176
1977.763752	308671.698711	37.935194
1979.796547	309205.399035	37.940212
1982.075697	309755.172445	37.945229
1983.634585	310297.615477	37.950247
1985.632521	310843.207104	37.955264
1987.566870	311395.325350	37.960282
1989.711744	311940.881372	37.965300
1991.761986	312495.354399	37.970317
1993.523363	313045.729082	37.975335
1995.860937	313584.586174	37.980352
1997.515456	314151.486689	37.985370
1999.334990	314696.426751	37.990388
2001.231804	315258.174413	37.995405
2004.013117	315820.055884	38.000423
2005.648235	316368.380031	38.005440
2007.937875	316913.016760	38.010458
2009.800624	317452.232037	38.015476
2011.719937	317989.122549	38.020493
2013.531189	318525.414360	38.025511
2016.172287	319047.511049	38.030528
2017.518175	319584.801570	38.035546
2019.536256	320125.964287	38.040564
2021.736539	320665.797513	38.045581
2023.121185	321217.830241	38.050599
2025.178263	321757.291405	38.055616
2026.947485	322311.736465	38.060634
2029.227497	322864.089704	38.065652
2031.200672	323420.924110	38.070669
2033.230309	323969.597230	38.075687
2035.609707	324521.100906	38.080704
2037.751769	325085.625323	38.085722
2039.523532	325642.613418	38.090740
2042.139083	326189.338268	38.095757
2044.066823	326767.244072	38.100775
2046.780148	327316.754601	38.105792
2048.805700	327874.839190	38.110810
2050.643505	328435.000355	38.115828
2052.612812	328994.016691	38.120845
2054.215943	329563.154344	38.125863
2056.290075	330128.125464	38.130880
2058.365848	330697.223337	38.135898
2061.682407	331253.358026	38.140916
2063.905415	331817.646910	38.145933
2066.022557	332375.601927	38.150951
2067.947085	332941.442974	38.155968
2069.987740	333507.054444	38.160986
2072.024351	334066.087925	38.166004
2074.490900	334630.043062	38.171021
2076.050365	335197.353112	38.176039
2078.607257	335755.163701	38.181056
2080.255454	336329.037675	38.186074
2082.447338	336899.799133	38.191092
2084.663480	337476.204235	38.196109
2086.007425	338052.305438	38.201127
2088.651502	338626.494646	38.206144
2090.682840	339204.321450	38.211162
2092.569601	339783.074603	38.216180
2094.788723	340370.668699	38.221197
2096.429184	340947.792786	38.226215
2098.908193	341534.286975	38.231232
2100.937770	342124.544439	38.236250
2102.577416	342713.813097	38.241268
2104.929974	343304.050710	38.246285
2106.888164	343922.084062	38.251303
2109.172093	344509.446007	38.256320
2111.353519	345103.610195	38.261338
2113.271296	345708.253117	38.266356
2115.201069	346306.264775	38.271373
2117.048708	346913.610400	38.276391
2119.457870	347518.321390	38.281408
2121.124571	348131.784319	38.286426
2122.999906	348753.139868	38.291444
2124.951512	349358.801662	38.296461
2127.376419	349996.326374	38.301479
2129.686129	350614.079604	38.306496
2131.879096	351235.921443	38.311514
2134.020980	351850.888306	38.316532
2136.693822	352482.037418	38.321549
2138.291805	353096.482333	38.326567
2140.417277	353708.069411	38.331584
2142.548185	354332.218536	38.336602
2144.828057	354957.244652	38.341620
2147.380902	355566.345731	38.346637
2149.722665	356178.560729	38.351655
2152.066054	356766.807417	38.356672
2154.331492	357352.545477	38.361690
2156.794899	357922.575549	38.366708
2159.322994	358492.331405	38.371725
2161.973697	359057.697519	38.376743
2164.091123	359622.756318	38.381760
2166.567613	360191.144942	38.386778
2168.549222	360763.807850	38.391796
2170.795447	361315.659678	38.396813
2172.666155	361879.852862	38.401831
2174.883917	362443.702251	38.406848
2176.840091	363014.602400	38.411866
2178.656398	363595.929980	38.416884
2180.762207	364176.845948	38.421901
2182.388117	364770.091711	38.426919
2184.488440	365349.084444	38.431936
2186.662913	365955.651973	38.436954
2188.591841	366552.741948	38.441972
2190.944847	367164.400512	38.446989
2192.857636	367757.489339	38.452007
2194.710829	368381.465013	38.457024
2196.638912	369008.151949	38.462042
2198.545791	369635.715175	38.467060
2200.678817	370248.456602	38.472077
2202.558846	370896.900204	38.477095
2204.927101	371539.956821	38.482112
2207.087907	372187.388937	38.487130
2209.433700	372842.580521	38.492148
2211.556121	373486.339721	38.497165
2213.768627	374149.223015	38.502183
2215.985082	374803.399860	38.507200
2218.313873	375454.731311	38.512218
2220.503856	376122.991377	38.517236
2223.082298	376786.259554	38.522253
2225.241992	377456.315116	38.527271
2228.031144	378107.206213	38.532288
2230.194167	378768.134270	38.537306
2232.117335	379433.212129	38.542324
2235.050546	380095.100977	38.547341
2237.202329	380763.098270	38.552359
2239.274710	381428.811352	38.557376
2241.784153	382084.232026	38.562394
2244.325418	382755.789644	38.567412
2247.148957	383402.643212	38.572429
2249.444157	384056.173085	38.577447
2251.879222	384714.222842	38.582464
2254.290054	385359.293348	38.587482
2256.054928	386015.742807	38.592500
2258.947872	386662.806490	38.597517
2261.284468	387322.247171	38.602535
2263.211778	387973.707545	38.607552
2265.621685	388624.417052	38.612570
2267.642015	389295.300070	38.617588
2269.883187	389937.873656	38.622605
2272.082447	390604.540662	38.627623
2274.462404	391255.615868	38.632640
2276.310944	391921.086595	38.637658
2278.444246	392586.393303	38.642676
2280.749365	393246.946053	38.647693
2282.750202	393912.996462	38.652711
2285.023181	394588.554826	38.657728
2287.459013	395252.171036	38.662746
2289.421028	395944.902613	38.667764
2291.662232	396618.332727	38.672781
2293.334717	397310.462171	38.677799
2295.901406	397996.862949	38.682816
2297.874492	398679.793038	38.687834
2299.808183	399364.430383	38.692852
2302.662332	400032.503422	38.697869
2304.877546	400699.341119	38.702887
2306.959694	401356.765994	38.707904
2309.667652	402014.985223	38.712922
2311.774168	402684.464879	38.717940
2313.950167	403347.638322	38.722957
2316.461397	404018.179513	38.727975
2319.183796	404697.220490	38.732992
2321.067750	405358.761290	38.738010
2323.352903	406036.160290	38.743028
2325.806642	406719.685988	38.748045
2328.909073	407401.723029	38.753063
2330.600049	408062.859767	38.758080
2333.759267	408738.977205	38.763098
2335.777773	409416.061895	38.768116
2338.332615	410081.506109	38.773133
2340.610885	410778.341445	38.778151
2342.367204	411458.136049	38.783168
2344.913871	412150.534557	38.788186
2347.367725	412843.127789	38.793204
2349.679757	413523.832961	38.798221
2351.434643	414230.098863	38.803239
2353.661057	414930.450557	38.808256
2356.220279	415637.960449	38.813274
2358.193413	416355.199335	38.818292
2360.785148	417089.716253	38.823309
2363.193736	417810.024078	38.828327
2365.566409	418528.542675	38.833344
2367.966056	419246.931224	38.838362
2371.224379	419949.887994	38.843380
2373.854266	420664.853805	38.848397
2376.443451	421378.941603	38.853415
2379.495611	422065.373414	38.858432
2382.282826	422766.790942	38.863450
2384.624268	423470.276674	38.868468
2386.788038	424171.086163	38.873485
2389.210223	424889.223586	38.878503
2391.375708	425578.052086	38.883520
2394.193148	426285.309203	38.888538
2396.567723	426989.627982	38.893556
2399.690547	427675.909307	38.898573
2402.056483	428364.711853	38.903591
2403.970357	429070.646856	38.908608
2406.829812	429754.117422	38.913626
2408.821235	430444.675394	38.918644
2411.333042	431155.901237	38.923661
2413.795133	431860.841852	38.928679
2416.009907	432582.676112	38.933696
2418.242778	433286.590244	38.938714
2420.170858	433997.450000	38.943732
2422.599104	434713.107237	38.948749
2424.978321	435434.102017	38.953767
2426.867072	436152.670430	38.958784
2429.467285	436884.490710	38.963802
2431.565268	437608.782419	38.968820
2433.748330	438346.826514	38.973837
2436.292779	439084.583216	38.978855
2438.096722	439836.875877	38.983872
2440.489756	440588.793695	38.988890
2442.702043	441344.953009	38.993908
2444.996855	442101.775982	38.998925
2447.498581	442862.879881	39.003943
2449.797737	443631.964877	39.008960
2452.384967	444380.062227	39.013978
2454.745582	445164.276731	39.018996
2457.277936	445936.410795	39.024013
2459.531751	446709.717327	39.029031
2462.002170	447473.160110	39.034048
2464.482730	448218.995878	39.039066
2466.800035	448975.683003	39.044084
2469.333213	449703.169664	39.049101
2471.821494	450456.334135	39.054119
2474.093955	451205.764417	39.059136
2476.629989	451956.384146	39.064154
2479.270816	452716.093596	39.069172
2481.862600	453464.671823	39.074189
2484.556858	454207.901750	39.079207
2487.051942	454965.265484	39.084224
2489.463128	455722.205790	39.089242
2491.774413	456488.163836	39.094260
2494.704471	457245.057808	39.099277
2496.917617	458014.850257	39.104295
2499.549658	458774.550294	39.109312
2502.212601	459546.273251	39.114330
2504.852827	460320.134990	39.119348
2507.008264	461087.629013	39.124365
2509.623706	461863.493606	39.129383
2512.167465	462656.135945	39.134400
2514.565809	463442.961730	39.139418
2516.719537	464233.219807	39.144436
2518.721010	465028.711295	39.149453
2521.181119	465829.289328	39.154471
2523.345840	466654.138922	39.159488
2525.510218	467468.455810	39.164506
2528.352895	468291.957918	39.169524
2530.694647	469125.635143	39.174541
2533.617012	469945.259520	39.179559
2536.374631	470783.831058	39.184576
2539.302074	471622.131328	39.189594
2541.132620	472446.793606	39.194612
2544.578039	473279.330135	39.199629
2547.354318	474103.508124	39.204647
2549.554504	474937.969120	39.209664
2552.697963	475766.441419	39.214682
2555.483555	476594.826014	39.219700
2558.171349	477431.450314	39.224717
2560.987840	478248.552898	39.229735
2563.576324	479082.635755	39.234752
2566.155282	479921.968396	39.239770
2568.655971	480751.289292	39.244788
2571.052855	481589.553390	39.249805
2574.633004	482401.180546	39.254823
2576.940792	483226.872732	39.259840
2580.078180	484042.464535	39.264858
2582.706169	484859.755830	39.269876
2585.278606	485686.686342	39.274893
2587.878811	486506.766555	39.279911
2590.244874	487339.535029	39.284928
2592.848682	488156.906602	39.289946
2595.294032	488985.744266	39.294964
2597.920891	489817.933523	39.299981
2600.685942	490642.903173	39.304999
2603.020424	491461.951965	39.310016
2605.698364	492279.895195	39.315034
2608.885731	493110.304052	39.320052
2611.380672	493929.847607	39.325069
2614.208694	494743.906091	39.330087
2616.141895	495578.552899	39.335104
2619.076565	496406.047936	39.340122
2621.390235	497229.918451	39.345140
2624.130903	498061.026100	39.350157
2626.570295	498887.955537	39.355175
2629.093942	499736.570646	39.360192
2631.390818	500553.511587	39.365210
2634.524890	501389.904884	39.370228
2636.892216	502213.686999	39.375245
2639.420610	503023.607687	39.380263
2642.279540	503836.702074	39.385280
2644.874930	504637.815434	39.390298
2647.175280	505440.439577	39.395316
2649.695504	506254.858335	39.400333
2652.268434	507060.317073	39.405351
2654.239526	507875.684638	39.410368
2657.106689	508691.921443	39.415386
2659.365114	509524.906646	39.420404
2662.061246	510357.773997	39.425421
2664.762226	511184.505149	39.430439
2667.042894	512033.130819	39.435456
2669.788935	512873.233439	39.440474
2672.075178	513726.482138	39.445492
2674.783743	514593.943201	39.450509
2677.636102	515457.857796	39.455527
2680.272216	516324.517196	39.460544
2682.640428	517193.878516	39.465562
2685.521849	518071.147703	39.470580
2688.416400	518957.859023	39.475597
2691.176210	519831.916957	39.480615
2693.900684	520717.685212	39.485632
2696.316014	521606.107343	39.490650
2699.244819	522495.898127	39.495668
2701.346596	523390.633598	39.500685
2704.580439	524289.754971	39.505703
2706.997945	525200.198174	39.510720
2709.527751	526102.372020	39.515738
2712.419809	527023.568417	39.520756
2714.946229	527945.712122	39.525773
2717.595283	528863.251195	39.530791
2720.510225	529803.236579	39.535808
2722.694723	530730.260601	39.540826
2725.597958	531674.733539	39.545844
2728.435513	532609.958403	39.550861
2731.229436	533542.210144	39.555879
2733.834519	534499.578868	39.560896
2736.657970	535441.579685	39.565914
2739.490577	536392.295140	39.570932
2742.206378	537349.132458	39.575949
2745.412699	538287.500246	39.580967
2748.319662	539252.245690	39.585984
2751.005786	540210.528201	39.591002
2753.692804	541165.375498	39.596020
2756.540506	542126.447694	39.601037
2759.399062	543074.599616	39.606055
2761.761529	544027.272565	39.611072
2764.857727	544995.510488	39.616090
2767.475580	545958.831636	39.621108
2770.223304	546927.474709	39.626125
2773.108702	547891.054747	39.631143
2775.721344	548863.328314	39.636160
2778.675295	549839.433036	39.641178
2781.375830	550813.343196	39.646196
2783.991613	551785.684514	39.651213
2787.122414	552757.666852	39.656231
2789.808819	553736.659028	39.661248
2792.607845	554713.799657	39.666266
2795.441383	555688.048549	39.671284
2798.172296	556665.191337	39.676301
2801.263559	557656.831527	39.681319
2804.511705	558636.337930	39.686336
2806.919482	559604.871372	39.691354
2810.107155	560585.629129	39.696372
2812.225361	561567.775159	39.701389
2815.876725	562530.313016	39.706407
2818.888058	563502.589481	39.711424
2821.548718	564453.302779	39.716442
2824.873860	565379.544668	39.721460
2827.582840	566321.583758	39.726477
2830.640459	567232.996463	39.731495
2833.600202	568160.375097	39.736512
2836.298278	569061.935790	39.741530
2839.787174	569974.115558	39.746548
2842.072434	570899.325972	39.751565
2844.990927	571820.958731	39.756583
2847.680703	572744.704837	39.761600
2849.555666	573669.404061	39.766618
2852.337942	574596.037732	39.771636
2855.364758	575538.669360	39.776653
2858.223229	576482.599307	39.781671
2861.103967	577422.944342	39.786688
2863.481270	578389.802529	39.791706
2866.282048	579343.355254	39.796724
2868.920056	580315.708012	39.801741
2871.769840	581280.090545	39.806759
2874.957569	582255.387917	39.811776
2877.675321	583244.123464	39.816794
2880.461574	584215.909809	39.821812
2883.180646	585205.668555	39.826829
2886.684884	586180.367942	39.831847
2889.283233	587188.362126	39.836864
2891.828746	588189.973552	39.841882
2895.101881	589182.133070	39.846900
2897.786585	590192.433156	39.851917
2900.523816	591195.135288	39.856935
2904.004444	592210.817584	39.861952
2906.466331	593217.570530	39.866970
2909.632658	594235.257862	39.871988
2912.684244	595244.324778	39.877005
2915.568615	596273.199262	39.882023
2918.746723	597297.233615	39.887040
2921.837815	598315.439862	39.892058
2924.790007	599345.502198	39.897076
2927.408730	600380.058577	39.902093
2930.161503	601407.453148	39.907111
2933.567777	602440.034994	39.912128
2936.196774	603484.763626	39.917146
2938.924035	604511.306488	39.922164
2942.350532	605561.190238	39.927181
2945.191434	606595.441887	39.932199
2948.305034	607642.667475	39.937216
2950.957864	608688.910265	39.942234
2954.194252	609737.747824	39.947252
2957.022833	610787.488704	39.952269
2959.987712	611837.797892	39.957287
2963.427949	612895.851956	39.962304
2965.777727	613932.975558	39.967322
2969.203123	614990.512866	39.972340
2972.174422	616053.642426	39.977357
2975.103581	617111.581733	39.982375
2978.018370	618154.011580	39.987392
2980.710701	619221.382273	39.992410
2983.914385	620277.646254	39.997428
2986.904625	621351.267959	40.002445
2990.027994	622419.670782	40.007463
2992.953166	623477.528416	40.012480
2995.463475	624544.998780	40.017498
2998.584345	625616.987971	40.022516
3001.398946	626688.409169	40.027533
3004.492228	627768.829596	40.032551
3007.487688	628849.294149	40.037568
3010.386354	629928.607650	40.042586
3013.403215	630996.931590	40.047604
3015.883937	632088.560543	40.052621
3019.534854	633162.515872	40.057639
3022.594877	634210.968503	40.062656
3025.723894	635255.513937	40.067674
3028.750418	636291.155839	40.072692
3031.730382	637333.903729	40.077709
3034.650462	638375.600870	40.082727
3037.739877	639413.675360	40.087744
3040.214382	640462.819098	40.092762
3043.045356	641508.160266	40.097780
3046.070096	642564.538910	40.102797
3049.094766	643627.259290	40.107815
3052.694427	644690.314789	40.112832
3055.247892	645767.325859	40.117850
3058.101722	646841.431513	40.122868
3061.114237	647923.683838	40.127885
3064.184687	649004.160198	40.132903
3067.120869	650094.861311	40.137920
3070.133118	651192.770425	40.142938
3073.407315	652278.538603	40.147956
3076.807038	653377.910798	40.152973
3079.618262	654489.255699	40.157991
3082.637693	655598.495232	40.163008
3085.326044	656716.484531	40.168026
3088.641024	657843.119817	40.173044
3091.356546	658972.237596	40.178061
3094.405350	660098.878073	40.183079
3097.609912	661237.852772	40.188096
3100.444904	662396.381292	40.193114
3103.738930	663534.203383	40.198132
3106.838412	664684.405452	40.203149
3109.752281	665853.476090	40.208167
3113.250571	667011.343191	40.213184
3116.115982	668173.121350	40.218202
3120.173116	669325.884839	40.223220
3123.775726	670485.306015	40.228237
3127.069584	671647.890524	40.233255
3130.293780	672788.035224	40.238272
3133.449031	673956.523032	40.243290
3136.799224	675122.592551	40.248308
3139.949126	676261.990458	40.253325
3143.271341	677417.252570	40.258343
3146.674698	678567.047736	40.263360
3149.829686	679733.210344	40.268378
3152.717694	680886.781128	40.273396
3155.831957	682038.872185	40.278413
3158.966379	683203.865685	40.283431
3162.021940	684363.910710	40.288448
3165.354335	685536.267157	40.293466
3167.984766	686703.226820	40.298484
3171.638768	687870.753000	40.303501
3174.668697	689050.327078	40.308519
3177.796530	690229.223282	40.313536
3180.552663	691413.347937	40.318554
3183.410522	692598.719619	40.323572
3186.544282	693796.577551	40.328589
3189.639345	694980.529651	40.333607
3193.232978	696176.583063	40.338624
3196.287490	697373.977354	40.343642
3199.368752	698566.745563	40.348660
3202.633371	699770.815303	40.353677
3205.835509	700968.493710	40.358695
3208.792748	702171.956118	40.363712
3211.986607	703385.566547	40.368730
3215.330835	704585.051688	40.373748
3218.934757	705785.154576	40.378765
3222.506937	706997.514362	40.383783
3225.362224	708186.911404	40.388800
3228.862392	709399.013157	40.393818
3232.052991	710600.768559	40.398836
3235.184407	711783.415164	40.403853
3238.233267	712930.991307	40.408871
3241.459314	714097.053451	40.413888
3244.325589	715261.666643	40.418906
3247.586967	716426.979855	40.423924
3250.561747	717596.892703	40.428941
3253.343954	718772.323922	40.433959
3256.649151	719960.103732	40.438976
3259.354922	721143.164367	40.443994
3262.364028	722351.994181	40.449012
3266.222675	723553.361265	40.454029
3268.580871	724769.048881	40.459047
3272.037121	725980.236220	40.464064
3274.902090	727218.239981	40.469082
3278.167796	728449.287007	40.474100
3281.379594	729696.817888	40.479117
3284.580750	730949.209429	40.484135
3287.977142	732198.902356	40.489152
3291.090302	733451.577375	40.494170
3294.340133	734711.541973	40.499188
3298.285102	735971.724939	40.504205
3301.526239	737250.232328	40.509223
3304.987995	738510.156724	40.514240
3308.529774	739786.163096	40.519258
3311.901568	741049.449350	40.524276
3315.685072	742331.065809	40.529293
3318.626146	743610.968749	40.534311
3322.424265	744888.058201	40.539328
3325.845151	746173.964279	40.544346
3329.142310	747450.435318	40.549364
3333.022765	748738.463476	40.554381
3336.323167	750012.223406	40.559399
3339.321432	751290.905631	40.564416
3342.590582	752582.116492	40.569434
3346.127044	753867.756700	40.574452
3349.854361	755167.449242	40.579469
3352.867540	756462.996369	40.584487
3356.362487	757750.194410	40.589504
3360.330196	759049.724458	40.594522
3363.434900	760336.902942	40.599540
3367.019707	761632.194307	40.604557
3370.672786	762914.846352	40.609575
3374.421993	764199.744475	40.614592
3377.946241	765489.384399	40.619610
3381.141425	766776.682665	40.624628
3384.903365	768063.603904	40.629645
3387.692424	769361.591478	40.634663
3391.214957	770643.029291	40.639680
3394.732206	771935.183090	40.644698
3397.609042	773233.158117	40.649716
3401.149753	774534.448860	40.654733
3404.565354	775841.179873	40.659751
3407.668989	777146.144232	40.664768
3411.290380	778460.840513	40.669786
3414.207457	779776.563015	40.674804
3417.323566	781077.003825	40.679821
3420.683140	782417.144992	40.684839
3423.916517	783730.870628	40.689856
3427.225138	785062.482724	40.694874
3430.862821	786389.921663	40.699892
3434.439451	787721.934610	40.704909
3437.893820	789047.552169	40.709927
3441.454071	790369.911770	40.714944
3444.836933	791699.347200	40.719962
3448.504233	793030.223674	40.724980
3451.762408	794353.874668	40.729997
3455.110361	795697.758378	40.735015
3458.048412	797009.913503	40.740020
3461.726974	798299.935247	40.745024
3464.906856	799539.389625	40.750029
3468.568939	800708.820314	40.755034
3471.182271	801830.712001	40.760039
3474.208253	802876.556526	40.765044
3476.884457	803879.005903	40.770048
3480.129794	804822.910607	40.775053
3482.597267	805701.872901	40.780058
3484.774106	806513.502203	40.785063
3487.606527	807279.913853	40.790068
3489.926129	807986.239440	40.795072
3492.258462	808625.200841	40.800077
3494.200220	809214.822092	40.805082
3496.128764	809752.230579	40.810087
3498.058508	810240.069486	40.815092
3499.356419	810675.817233	40.820096
3500.901871	811068.509803	40.825101
3502.466059	811426.378429	40.830106
3504.049410	811754.692046	40.835111
3505.077321	812015.340743	40.840116
3506.635387	812260.497632	40.845120
3507.593309	812468.804052	40.850125
3508.603921	812630.319099	40.855130
3509.259559	812777.852902	40.860135
3510.074259	812883.553794	40.865140
3510.936785	812974.920958	40.870144
3511.666694	813036.879348	40.875149
3512.526886	813070.850400	40.880154
3513.223146	813094.322992	40.885159
3513.746227	813084.691778	40.890164
3514.283134	813057.031240	40.895168
3515.021646	813026.610616	40.900173
3515.469044	812954.138918	40.905178
3515.601078	812876.745888	40.910183
3515.825625	812786.571718	40.915188
3516.566922	812685.888341	40.920192
3516.679824	812573.315039	40.925197
3517.093402	812446.951768	40.930202
3517.090850	812323.964498	40.935207
3517.219605	812171.814447	40.940212
3517.881086	812015.679027	40.945216
3517.852403	811861.889265	40.950221
3518.312062	811693.204692	40.955226
3518.047962	811513.614853	40.960231
3518.181301	811326.939853	40.965236
3518.266838	811142.313743	40.970240
3518.132536	810941.827866	40.975245
3518.243515	810739.542625	40.980250
3517.905915	810539.953063	40.985255
3517.910415	810338.159008	40.990260
3518.076261	810129.314037	40.995264
3518.164812	809925.543861	41.000269
3518.404060	809721.158580	41.005274
3518.292196	809509.021654	41.010279
3518.333239	809283.105857	41.015284
3518.355325	809065.375457	41.020288
3518.076221	808850.219886	41.025293
3517.948531	808614.653174	41.030298
3517.646188	808388.271543	41.035303
3517.697094	808172.358734	41.040308
3518.003086	807945.524873	41.045312
3517.345304	807720.052641	41.050317
3517.734464	807496.505628	41.055322
3517.695000	807282.966158	41.060327
3517.389873	807052.538408	41.065332
3517.417091	806814.052026	41.070336
3516.967985	806597.042073	41.075341
3516.925642	806361.280806	41.080346
3516.592498	806145.798084	41.085351
3516.579414	805907.479110	41.090356
3516.519926	805688.523723	41.095360
3516.537798	805471.353600	41.100365
3516.346733	805246.257232	41.105370
3516.049034	805025.462577	41.110375
3515.948703	804819.996891	41.115380
3515.557967	804607.788573	41.120384
3515.513716	804395.958136	41.125389
3515.376847	804177.011750	41.130394
3515.111117	803974.472140	41.135399
3515.257167	803757.126074	41.140404
3515.376441	803546.120200	41.145408
3514.922814	803347.786508	41.150413
3514.950063	803126.729049	41.155418
3514.604708	802934.807030	41.160423
3514.571367	802723.017092	41.165428
3514.638895	802523.697983	41.170432
3514.283068	802327.367134	41.175437
3514.501230	802122.301872	41.180442
3514.293427	801935.062616	41.185447
3514.031286	801730.596807	41.190452
3513.910363	801526.102413	41.195456
3513.730131	801341.428503	41.200461
3513.560122	801138.930757	41.205466
3513.449750	800954.430065	41.210471
3513.008185	800768.706629	41.215476
3513.335175	800576.804279	41.220480
3512.864205	800400.057278	41.225485
3513.024128	800204.801439	41.230490
3512.951703	800031.838865	41.235495
3512.684147	799849.576899	41.240500
3513.102970	799672.475555	41.245504
3512.478911	799491.528641	41.250509
3512.335158	799301.224349	41.255514
3512.235427	799135.663791	41.260519
3511.816384	798959.113314	41.265524
3511.818019	798791.037742	41.270528
3511.715749	798623.560034	41.275533
3511.667580	798452.797659	41.280538
3511.688731	798291.152116	41.285543
3511.335443	798126.484378	41.290548
3511.704438	797961.601864	41.295552
3511.099246	797793.644075	41.300557
3511.257991	797643.584499	41.305562
3511.082065	797487.029048	41.310567
3510.595899	797325.829441	41.315572
3510.980535	797155.893215	41.320576
3510.620436	797009.221432	41.325581
3510.476258	796854.746075	41.330586
3510.192869	796706.785466	41.335591
3510.022065	796555.726448	41.340596
3510.084702	796410.782438	41.345600
3509.194288	796272.969778	41.350605
3509.739721	796136.395278	41.355610
3509.931830	796012.281638	41.360615
3509.675348	795861.219865	41.365620
3509.699253	795724.669395	41.370624
3509.370970	795601.801778	41.375629
3509.520781	795450.373818	41.380634
3509.762626	795313.340940	41.385639
3509.196715	795174.379390	41.390644
3509.262475	795038.052266	41.395648
3509.006573	794908.564197	41.400653
3508.879478	794784.623632	41.405658
3508.852382	794659.150343	41.410663
3508.663626	794534.383998	41.415668
3508.792113	794402.871258	41.420672
3508.348062	794289.476658	41.425677
3508.543625	794161.075933	41.430682
3508.201239	794057.678969	41.435687
3508.116184	793921.352077	41.440692
3508.269200	793808.100117	41.445696
3508.004576	793700.433749	41.450701
3508.074440	793576.879280	41.455706
3508.202372	793463.087686	41.460711
3507.835359	793345.999295	41.465716
3507.600000	793216.523307	41.470720
3507.684993	793118.665089	41.475725
3507.633008	793004.502648	41.480730
3507.579452	792888.236806	41.485735
3507.611764	792783.832470	41.490740
3507.625013	792679.087308	41.495744
3507.062464	792571.888822	41.500749
3507.194510	792457.736954	41.505754
3507.003445	792371.690531	41.510759
3506.986334	792268.214411	41.515764
3506.969519	792171.140032	41.520768
3506.728133	792085.195473	41.525773
3507.075147	791972.125824	41.530778
3506.589270	791875.951401	41.535783
3506.614691	791772.216387	41.540788
3506.702491	791680.984478	41.545792
3506.628524	791594.176272	41.550797
3506.567944	791491.085768	41.555802
3506.634408	791404.057550	41.560807
3506.437012	791310.567396	41.565812
3506.298893	791205.186812	41.570816
3505.770410	791120.790030	41.575821
3506.046662	791043.453117	41.580826
3506.002039	790956.534113	41.585831
3505.695533	790867.943721	41.590836
3505.765561	790784.280196	41.595840
3505.688374	790710.905931	41.600845
3505.869490	790628.005323	41.605850
3505.417018	790555.079124	41.610855
3505.331251	790477.009852	41.615860
3505.942695	790398.977348	41.620864
3505.436551	790325.861418	41.625869
3505.242526	790243.992510	41.630874
3505.376769	790161.288931	41.635879
3505.449459	790088.911115	41.640884
3505.147660	790004.024482	41.645888
3504.977542	789949.530534	41.650893
3505.209401	789872.675778	41.655898
3504.956963	789807.093630	41.660903
3504.991591	789743.519716	41.665908
3504.906310	789667.103332	41.670912
3504.851152	789603.004202	41.675917
3504.878832	789533.219023	41.680922
3504.957687	789477.361930	41.685927
3504.655801	789397.895515	41.690932
3504.430920	789321.790358	41.695936
3504.682832	789269.523217	41.700941
3504.488354	789201.676459	41.705946
3504.256288	789146.060776	41.710951
3504.467730	789082.061616	41.715956
3504.522980	789019.211055	41.720960
3504.350072	788958.058330	41.725965
3504.596852	788901.192010	41.730970
3503.992943	788841.768362	41.735975
3504.124575	788779.148104	41.740980
3504.381490	788720.371298	41.745984
3504.192898	788665.233832	41.750989
3504.122041	788605.431284	41.755994
3503.812976	788553.441798	41.760999
3503.848443	788502.180577	41.766004
3504.392811	788445.508358	41.771008
3504.213428	788396.431886	41.776013
3503.943425	788335.386388	41.781018
3503.799129	788281.706080	41.786023
3503.736629	788228.795114	41.791028
3504.085417	788171.613109	41.796032
3503.879057	788128.408151	41.801037
3503.703898	788066.513853	41.806042
3503.741133	788030.949285	41.811047
3503.451667	787979.979367	41.816052
3503.801236	787922.110313	41.821056
3503.371022	787879.868062	41.826061
3503.610667	787836.395824	41.831066
3503.645711	787788.601975	41.836071
3503.363953	787742.324722	41.841076
3503.414430	787691.641838	41.846080
3503.477517	787646.337208	41.851085
3503.681052	787601.646206	41.856090
3503.471087	787562.155648	41.861095
3503.492644	787509.861689	41.866100
3503.675343	787457.884539	41.871104
3503.439486	787412.478292	41.876109
3503.700394	787365.820076	41.881114
3503.039007	787327.817269	41.886119
3503.320154	787272.154497	41.891124
3503.495589	787234.705186	41.896128
3503.294542	787200.983361	41.901133
3503.267741	787150.112741	41.906138
3503.040997	787110.084005	41.911143
3502.641257	787077.713414	41.916148
3503.194018	787031.349653	41.921152
3502.964610	786989.657353	41.926157
3503.184976	786945.399571	41.931162
3502.717014	786920.083324	41.936167
3502.847408	786866.055068	41.941172
3502.877784	786827.598804	41.946176
3502.530613	786805.492000	41.951181
3502.687933	786760.557948	41.956186
3502.874899	786731.518430	41.961191
3502.669703	786697.354396	41.966196
3502.964434	786666.976866	41.971200
3502.585456	786635.921758	41.976205
3502.610286	786599.813301	41.981210
3502.590305	786571.147889	41.986215
3502.261990	786533.186292	41.991220
3502.596953	786512.390639	41.996224
3502.197131	786476.690355	42.001229
3502.455379	786447.589529	42.006234
3502.367448	786424.560304	42.011239
3502.421497	786394.708389	42.016244
3502.097878	786361.343917	42.021248
3502.439830	786335.311734	42.026253
3502.291132	786306.176054	42.031258
3502.669533	786288.553006	42.036263
3502.754731	786254.977317	42.041268
3502.607582	786214.001152	42.046272
3502.501784	786189.114745	42.051277
3502.189128	786153.056613	42.056282
3501.924571	786127.460906	42.061287
3502.099725	786101.062474	42.066292
3501.812187	786070.724312	42.071296
3501.952833	786056.513727	42.076301
3502.060125	786038.198500	42.081306
3502.067227	786015.691192	42.086311
3501.982832	786002.200643	42.091316
3502.303782	785961.345451	42.096320
3501.907640	785942.766169	42.101325
3501.932485	785916.243717	42.106330
3502.289478	785895.100200	42.111335
3502.166086	785873.053155	42.116340
3502.050532	785852.815144	42.121344
3502.078423	785823.698669	42.126349
3502.230952	785801.461470	42.131354
3502.091819	785780.297287	42.136359
3501.702881	785757.802086	42.141364
3502.275066	785732.905841	42.146368
3502.458169	785704.596371	42.151373
3502.312383	785676.631767	42.156378
3502.358599	785644.086598	42.161383
3502.542307	785616.314881	42.166388
3502.211721	785582.898652	42.171392
3502.329394	785555.185932	42.176397
3502.305107	785529.012126	42.181402
3502.040782	785513.444710	42.186407
3502.167377	785483.626291	42.191412
3501.959381	785465.554495	42.196416
3501.862874	785443.942200	42.201421
3502.011179	785401.300114	42.206426
3501.937152	785388.932115	42.211431
3502.218234	785371.860100	42.216436
3502.282563	785340.680694	42.221440
3502.037981	785325.843725	42.226445
3501.806697	785294.025266	42.231450
3502.027710	785286.063765	42.236455
3501.982807	785259.158139	42.241460
3501.901785	785233.677091	42.246464
3501.136653	785210.847381	42.251469
3501.748866	785197.686697	42.256474
3501.619716	785176.665827	42.261479
3501.128704	785160.741555	42.266484
3501.472919	785146.790804	42.271488
3501.055419	785144.703047	42.276493
3501.150808	785127.463701	42.281498
3501.475965	785124.525846	42.286503
3501.463778	785103.877928	42.291508
3501.465092	785090.323195	42.296512
3501.838143	785080.771810	42.301517
3501.877868	785056.837083	42.306522
3501.698066	785046.197662	42.311527
3501.432856	785021.038194	42.316532
3501.963058	784993.552252	42.321536
3501.676190	784986.354865	42.326541
3501.500051	784964.019444	42.331546
3501.928409	784946.140366	42.336551
3501.311183	784936.107427	42.341556
3501.755196	784907.900586	42.346560
3501.590700	784902.494567	42.351565
3501.668541	784875.763942	42.356570
3501.673143	784866.123042	42.361575
3501.314695	784848.219891	42.366580
3501.919993	784833.151096	42.371584
3501.714875	784818.942985	42.376589
3501.849251	784799.788213	42.381594
3501.457901	784786.489985	42.386599
3501.500740	784767.691980	42.391604
3501.752032	784761.242132	42.396608
3501.374800	784745.935243	42.401613
3501.390968	784721.905122	42.406618
3501.464682	784707.799995	42.411623
3501.168298	784686.412227	42.416628
3501.427906	784677.318429	42.421632
3501.272977	784665.891525	42.426637
3501.462608	784652.502210	42.431642
3501.536981	784650.190592	42.436647
3501.408795	784631.614685	42.441652
3501.860639	784620.092852	42.446656
3500.987938	784599.088515	42.451661
3501.369985	784580.285893	42.456666
3501.518007	784574.928627	42.461671
3501.433395	784567.992792	42.466676
3501.480480	784550.319068	42.471680
3501.107222	784550.671075	42.476685
3501.577690	784533.371559	42.481690
3501.763614	784523.897570	42.486695
3501.526632	784503.478681	42.491700
3501.546868	784482.676955	42.496704
3501.257552	784474.255945	42.501709
3501.120416	784452.597841	42.506714
3501.273657	784435.054032	42.511719
3501.109353	784424.019685	42.516724
3501.640613	784418.896016	42.521728
3501.089731	784410.809444	42.526733
3501.337090	784397.361654	42.531738
3500.989542	784387.383601	42.536743
3501.008677	784368.783931	42.541748
3501.538148	784354.998322	42.546752
3501.426868	784355.064691	42.551757
3501.577957	784334.829315	42.556762
3501.402450	784332.214076	42.561767
3501.161851	784324.274650	42.566772
3501.520363	784293.093291	42.571776
3501.403558	784296.341581	42.576781
3501.123280	784274.215880	42.581786
3501.223217	784261.867531	42.586791
3500.835596	784264.717713	42.591796
3501.129330	784260.805605	42.596800
3501.192618	784261.431960	42.601805
3501.523322	784236.910465	42.606810
3501.248102	784219.530946	42.611815
3500.982329	784221.725881	42.616820
3501.184564	784195.364601	42.621824
3500.983678	784198.919721	42.626829
3501.105432	784191.021372	42.631834
3501.273608	784186.443687	42.636839
3500.995601	784167.645204	42.641844
3501.190913	784167.370006	42.646848
3501.027734	784167.199787	42.651853
3501.283980	784154.337402	42.656858
3501.086245	784134.107006	42.661863
3501.094807	784130.533043	42.666868
3501.187659	784122.737013	42.671872
3501.183305	784111.775025	42.676877
3501.134438	784093.674624	42.681882
3501.084737	784096.472053	42.686887
3500.861478	784088.823280	42.691892
3500.966678	784072.069079	42.696896
3500.897322	784070.464903	42.701901
3501.025311	784064.082600	42.706906
3501.215672	784050.104670	42.711911
3500.927405	784053.575644	42.716916
3501.112397	784033.725585	42.721920
3501.032718	784032.661367	42.726925
3501.049889	784038.972136	42.731930
3501.042888	784028.059366	42.736935
3500.944308	784015.839477	42.741940
3501.125240	784003.233281	42.746944
3500.840425	784005.920677	42.751949
3500.982200	784001.689582	42.756954
3501.035610	783987.977638	42.761959
3500.862455	783973.664841	42.766964
3500.909257	783953.934029	42.771968
3500.937847	783965.381973	42.776973
3501.212311	783958.046778	42.781978
3501.236656	783949.135593	42.786983
3501.077018	783937.512407	42.791988
3501.308202	783924.066194	42.796993
3501.065606	783930.613441	42.801997
3500.948703	783914.823463	42.807002
3501.066155	783907.659584	42.812007
3500.979326	783915.650761	42.817012
3501.235299	783904.207258	42.822017
3500.802831	783891.843567	42.827021
3500.854359	783874.901493	42.832026
3501.151954	783871.135382	42.837031
3501.169194	783872.062627	42.842036
3501.262653	783857.805788	42.847041
3501.125363	783845.200097	42.852045
3501.063843	783833.169850	42.857050
3501.088645	783838.207106	42.862055
3501.197648	783836.574992	42.867060
3501.309510	783817.861404	42.872065
3501.080511	783805.955174	42.877069
3500.922557	783804.952099	42.882074
3500.975839	783799.364308	42.887079
3501.246392	783785.862720	42.892084
3501.234200	783766.972610	42.897089
3500.983118	783769.507996	42.902093
3500.959667	783760.897690	42.907098
3501.144397	783745.941139	42.912103
3501.032200	783738.225657	42.917108
3501.035461	783736.512162	42.922113
3501.233343	783731.097484	42.927117
3501.205724	783713.335333	42.932122
3501.030326	783707.881100	42.937127
3500.907606	783701.978136	42.942132
3500.982362	783688.409070	42.947137
3501.219731	783683.575506	42.952141
3501.135180	783680.015858	42.957146
3501.016382	783683.754194	42.962151
3500.779584	783691.818026	42.967156
3501.059056	783663.974261	42.972161
3500.815615	783656.474976	42.977165
3501.031833	783651.106311	42.982170
3500.971356	783645.731951	42.987175
3500.934761	783657.288502	42.992180
3501.169481	783640.268252	42.997185
3500.789566	783622.463042	43.002189
3501.152169	783607.576265	43.007194
3501.132217	783611.201301	43.012199
3500.919678	783607.465844	43.017204
3501.439492	783591.135068	43.022209
3501.424540	783589.130715	43.027213
3500.990961	783581.612124	43.032218
3500.913864	783559.648065	43.037223
3500.825529	783554.914268	43.042228
3500.911816	783542.762502	43.047233
3500.519973	783551.438077	43.052237
3501.048222	783539.217217	43.057242
3501.030085	783544.457186	43.062247
3500.897033	783528.619873	43.067252
3501.136754	783518.206096	43.072257
3501.224305	783512.270093	43.077261
3500.585473	783520.103307	43.082266
3500.928426	783512.169579	43.087271
3500.737807	783498.690557	43.092276
3501.216417	783486.085798	43.097281
3501.115384	783486.640024	43.102285
3500.987615	783486.464250	43.107290
3501.022368	783480.340691	43.112295
3500.656600	783459.596116	43.117300
3500.661709	783444.569078	43.122305
3500.724469	783449.747530	43.127309
3500.816379	783453.453056	43.132314
3500.922050	783453.240790	43.137319
3500.884771	783453.050869	43.142324
3500.967880	783440.263122	43.147329
3501.159346	783423.200136	43.152333
3500.967780	783422.104364	43.157338
3500.752171	783421.012351	43.162343
3500.343238	783434.144810	43.167348
3500.962852	783428.027668	43.172353
3501.091695	783426.930756	43.177357
3501.055105	783418.371008	43.182362
3501.236776	783409.532400	43.187367
3500.953661	783412.317657	43.192372
3501.500651	783389.717077	43.197377
3501.204920	783382.764063	43.202381
3500.855956	783368.624286	43.207386
3501.188335	783369.600231	43.212391
3500.603777	783353.686245	43.217396
3500.902843	783339.983515	43.222401
3500.949141	783337.871619	43.227405
3501.027200	783330.811173	43.232410
3501.166633	783329.516804	43.237415
3501.090233	783315.774826	43.242420
3501.294342	783301.401610	43.247425
3501.213771	783298.624281	43.252429
3501.145664	783294.523443	43.257434
3501.168109	783274.549699	43.262439
3500.937289	783256.671257	43.267444
3501.354549	783257.487110	43.272449
3500.984162	783250.349839	43.277453
3501.133802	783240.879706	43.282458
3501.094873	783234.375863	43.287463
3500.869731	783236.613711	43.292468
3501.143669	783226.830445	43.297473
3500.939355	783218.884025	43.302477
3501.088257	783205.645020	43.307482
3500.903179	783197.695568	43.312487
3501.078777	783201.877625	43.317492
3500.997092	783185.590942	43.322497
3500.736620	783173.688502	43.327501
3500.809244	783165.258199	43.332506
3500.573192	783169.210941	43.337511
3500.863128	783179.885165	43.342516
3500.896178	783168.426306	43.347521
3500.787774	783178.477535	43.352525
3500.573055	783154.624703	43.357530
3500.945101	783147.077577	43.362535
3500.820881	783145.922283	43.367540
3501.012856	783141.829643	43.372545
3500.823831	783155.760382	43.377549
3500.682464	783148.685097	43.382554
3500.970113	783148.199636	43.387559
3501.189781	783129.809904	43.392564
3501.193754	783113.558603	43.397569
3500.820984	783119.931197	43.402573
3500.793130	783113.131818	43.407578
3500.990273	783103.947752	43.412583
3500.585953	783085.998079	43.417588
3500.832904	783083.854737	43.422593
3500.762706	783080.439369	43.427597
3500.591663	783085.507807	43.432602
3500.751281	783083.182324	43.437607
3500.680168	783090.339910	43.442612
3501.201255	783083.699430	43.447617
3500.921933	783072.778720	43.452621
3500.763395	783065.950772	43.457626
3500.943433	783058.629356	43.462631
3500.616418	783065.288540	43.467636
3501.048850	783048.872207	43.472641
3500.961019	783051.871827	43.477645
3500.687845	783040.020082	43.482650
3500.863806	783032.111891	43.487655
3500.756977	783024.150000	43.492660
3500.876948	783025.061304	43.497665
3501.318940	783029.740262	43.502669
3500.770682	783022.532655	43.507674
3501.128738	783002.750378	43.512679
3500.933542	782992.305873	43.517684
3501.256226	782994.311317	43.522689
3501.224386	782994.610022	43.527693
3500.916445	782973.610149	43.532698
3501.295727	782966.453282	43.537703
3500.625885	782967.243314	43.542708
3501.043945	782962.087292	43.547713
3501.273409	782953.828001	43.552717
3500.796273	782937.259886	43.557722
3501.346456	782943.243623	43.562727
3500.983166	782947.265335	43.567732
3501.097082	782931.436948	43.572737
3501.407478	782908.186439	43.577741
3500.892192	782909.343912	43.582746
3501.276472	782903.556783	43.587751
3500.982727	782885.638234	43.592756
3501.020638	782873.199116	43.597761
3501.160948	782871.023427	43.602765
3501.095786	782865.404421	43.607770
3501.224769	782853.538428	43.612775
3501.020367	782843.144079	43.617780
3500.797540	782831.137241	43.622785
3500.839533	782836.759966	43.627789
3500.978102	782832.822336	43.632794
3501.166442	782814.142934	43.637799
3501.129918	782807.197747	43.642804
3501.025461	782801.486930	43.647809
3501.214898	782806.841880	43.652813
3501.127206	782792.953740	43.657818
3501.203356	782777.473545	43.662823
3501.108300	782777.439488	43.667828
3500.947648	782752.108252	43.672833
3500.849588	782750.214540	43.677837
3501.027255	782746.760254	43.682842
3501.171650	782737.290229	43.687847
3500.865107	782744.093382	43.692852
3501.262249	782734.436990	43.697857
3501.228222	782716.379486	43.702861
3501.252124	782709.228948	43.707866
3501.313670	782708.093489	43.712871
3501.175972	782700.674499	43.717876
3501.325871	782693.308444	43.722881
3500.826648	782685.945951	43.727885
3500.755510	782687.034030	43.732890
3501.241590	782676.972044	43.737895
3500.548372	782662.444022	43.742900
3500.694249	782652.630985	43.747905
3500.809142	782647.962678	43.752909
3500.862878	782644.087150	43.757914
3501.124759	782649.675659	43.762919
3500.849939	782642.865455	43.767924
3501.029060	782621.641482	43.772929
3501.052112	782608.323066	43.777933
3500.782265	782609.050607	43.782938
3500.430203	782617.721167	43.787943
3500.844338	782622.160011	43.792948
3501.226425	782605.897321	43.797953
3500.838693	782594.111641	43.802957
3500.758804	782590.844393	43.807962
3500.866930	782596.212223	43.812967
3500.587780	782591.067003	43.817972
3500.938409	782582.641460	43.822977
3500.822636	782589.072285	43.827981
3500.707936	782575.873242	43.832986
3500.697781	782564.273246	43.837991
3500.698584	782557.860438	43.842996
3500.519577	782550.007168	43.848001
3500.916556	782563.406965	43.853005
3500.581871	782562.676085	43.858010
3500.987539	782558.696542	43.863015
3500.814908	782566.066366	43.868020
3501.112946	782548.299163	43.873025
3500.895710	782534.724449	43.878029
3500.836301	782529.838545	43.883034
3500.751205	782516.879519	43.888039
3500.939162	782521.696453	43.893044
3500.862536	782522.393798	43.898049
3500.912114	782507.602465	43.903053
3500.682205	782493.148504	43.908058
3500.653068	782497.656725	43.913063
3500.657606	782504.754159	43.918068
3501.035881	782494.366086	43.923073
3500.582301	782491.010347	43.928077
3500.849911	782509.619443	43.933082
3501.054422	782497.936823	43.938087
3500.959282	782482.335864	43.943092
3500.857130	782471.141709	43.948097
3500.881280	782468.739286	43.953101
3500.433778	782469.837281	43.958106
3501.041341	782465.091831	43.963111
3500.846117	782461.695691	43.968116
3500.833596	782453.081990	43.973121
3501.096546	782433.802430	43.978125
3500.780049	782433.411363	43.983130
3501.059234	782435.864356	43.988135
3500.658903	782447.528810	43.993140
3500.951650	782435.097995	43.998145
3500.697278	782416.241924	44.003149
3500.494832	782402.811489	44.008154
3501.017276	782403.072526	44.013159
3500.997520	782424.663972	44.018164
3500.702696	782409.779402	44.023169
3500.878726	782408.723902	44.028173
3500.598493	782413.614103	44.033178
3500.870312	782399.326274	44.038183
3500.924052	782388.450284	44.043188
3500.885728	782382.484003	44.048193
3500.758711	782382.552847	44.053197
3500.774996	782391.508791	44.058202
3500.837444	782377.204691	44.063207
3500.529304	782388.952742	44.068212
3500.666889	782381.735130	44.073217
3500.912356	782355.457746	44.078221
3500.967761	782353.490977	44.083226
3500.907517	782363.389040	44.088231
3500.968919	782361.666103	44.093236
3500.691305	782355.198716	44.098241
3501.005696	782347.561801	44.103245
3500.695145	782330.036015	44.108250
3500.856277	782319.436848	44.113255
3500.450620	782320.773094	44.118260
3500.224104	782320.514814	44.123265
3500.489866	782320.962842	44.128269
3500.334197	782332.001806	44.133274
3500.842515	782323.796057	44.138279
3500.822961	782324.876131	44.143284
3500.795314	782321.160000	44.148289
3500.996150	782317.701873	44.153293
3500.710598	782328.859052	44.158298
3500.793637	782309.215628	44.163303
3500.570538	782304.746779	44.168308
3500.783345	782301.825266	44.173313
3500.785369	782299.964734	44.178317
3500.725998	782303.743502	44.183322
3500.643743	782309.581908	44.188327
3500.890462	782298.283974	44.193332
3500.900236	782308.024311	44.198337
3500.713927	782292.045529	44.203341
3500.795725	782273.136503	44.208346
3500.838371	782266.961646	44.213351
3500.734937	782285.433553	44.218356
3500.706727	782282.843432	44.223361
3501.149732	782282.872123	44.228365
3500.644547	782278.692123	44.233370
3500.769717	782254.342356	44.238375
3500.824562	782246.501127	44.243380
3500.724652	782245.684556	44.248385
3501.124543	782247.139663	44.253389
3500.865279	782249.432125	44.258394
3500.763124	782245.238055	44.263399
3500.977159	782238.987426	44.268404
3501.175393	782218.003959	44.273409
3501.074060	782227.027464	44.278413
3500.728782	782227.375200	44.283418
3501.245508	782224.210326	44.288423
3501.198528	782214.573660	44.293428
3501.122122	782196.472422	44.298433
3500.924325	782192.978637	44.303437
3501.010194	782188.657230	44.308442
3501.175226	782174.630390	44.313447
3500.955323	782166.391423	44.318452
3500.734822	782161.971026	44.323457
3500.668754	782158.162900	44.328461
3500.628266	782153.028989	44.333466
3500.985886	782157.721754	44.338471
3500.429170	782158.690005	44.343476
3500.648107	782134.765741	44.348481
3500.998530	782129.374883	44.353485
3500.794207	782117.951332	44.358490
3500.997076	782122.668313	44.363495
3500.742865	782130.589876	44.368500
3500.802404	782115.110746	44.373505
3500.787245	782122.260620	44.378509
3500.734324	782104.400238	44.383514
3500.141472	782086.722122	44.388519
3500.401257	782093.878002	44.393524
3500.416807	782092.064253	44.398529
3500.461416	782093.330156	44.403533
3500.389970	782098.530635	44.408538
3500.742376	782095.293478	44.413543
3500.801316	782108.110613	44.418548
3500.533061	782105.655857	44.423553
3500.907625	782106.184804	44.428557
3500.487193	782103.851747	44.433562
3500.720868	782111.648110	44.438567
3500.977723	782116.797254	44.443572
3500.871675	782102.029353	44.448577
3500.985518	782092.465282	44.453581
3500.870685	782088.273096	44.458586
3500.893216	782077.744168	44.463591
3500.845051	782085.339841	44.468596
3501.097591	782076.390488	44.473601
3500.500223	782064.244997	44.478605
3500.492276	782047.356546	44.483610
3500.482895	782042.952023	44.488615
3500.877427	782042.009179	44.493620
3500.727427	782038.214105	44.498625
3500.931761	782040.874769	44.503629
3500.346347	782045.910854	44.508634
3500.888934	782043.476192	44.513639
3500.528643	782045.001222	44.518644
3500.653062	782051.003369	44.523649
3500.653183	782057.318675	44.528653
3500.519553	782059.248871	44.533658
3500.627010	782055.462517	44.538663
3500.436988	782063.520992	44.543668
3500.919693	782053.213824	44.548673
3500.801765	782027.236739	44.553677
3500.619426	782033.042075	44.558682
3500.662492	782025.153473	44.563687
3500.532402	782034.867115	44.568692
3500.411775	782034.396447	44.573697
3500.679530	782028.235137	44.578701
3500.613151	782035.539977	44.583706
3500.740609	782040.709409	44.588711
3500.443341	782035.958238	44.593716
3500.484971	782035.315338	44.598721
3500.762224	782034.635605	44.603725
3500.574615	782040.490715	44.608730
3500.710235	782020.593446	44.613735
3500.715312	782014.375273	44.618740
3500.889964	782011.704379	44.623745
3500.980300	782014.187050	44.628749
3500.776001	782008.833854	44.633754
3501.013698	782000.718974	44.638759
3500.694419	782004.146891	44.643764
3500.677123	781974.482160	44.648769
3500.713080	781977.316040	44.653773
3500.763397	781984.651650	44.658778
3500.875313	781977.192835	44.663783
3500.621229	781983.988555	44.668788
3500.677298	781979.818541	44.673793
3500.719759	781983.630527	44.678797
3500.529828	781987.136145	44.683802
3500.781692	781983.033439	44.688807
3500.661859	781996.710990	44.693812
3500.767088	781966.782291	44.698817
3500.420957	781967.962429	44.703821
3500.467294	781962.276278	44.708826
3500.614469	781949.867321	44.713831
3500.447070	781954.642303	44.718836
3500.742030	781959.638743	44.723841
3500.840007	781958.203725	44.728845
3500.676808	781963.320739	44.733850
3500.695450	781959.695084	44.738855
3500.601730	781965.731407	44.743860
3500.638341	781962.886247	44.748865
3500.554609	781961.185896	44.753869
3500.512162	781953.849098	44.758874
3500.673379	781958.817489	44.763879
3500.468458	781945.092783	44.768884
3500.650797	781939.287439	44.773889
3500.979967	781940.557844	44.778893
3500.688089	781948.632379	44.783898
3500.503186	781939.457486	44.788903
3500.601810	781946.344978	44.793908
3500.703696	781944.958302	44.798913
3500.539119	781948.459977	44.803917
3500.566756	781948.700473	44.808922
3500.996048	781940.310787	44.813927
3500.846929	781953.111786	44.818932
3500.624630	781930.430724	44.823937
3500.692160	781920.824691	44.828941
3500.635133	781921.665904	44.833946
3500.560274	781911.837334	44.838951
3500.989821	781918.673124	44.843956
3500.736418	781918.859641	44.848961
3500.750447	781908.723430	44.853965
3500.699695	781919.746671	44.858970
3500.909774	781918.783687	44.863975
3500.671560	781898.210143	44.868980
3500.703292	781888.511746	44.873985
3500.783331	781884.484797	44.878989
3500.713340	781890.272694	44.883994
3500.668893	781879.068527	44.888999
3500.848137	781888.195499	44.894004
3500.639461	781890.724958	44.899009
3501.020414	781890.714398	44.904013
3500.846377	781866.801652	44.909018
3500.790623	781852.857610	44.914023
3500.707885	781857.913169	44.919028
3501.003733	781853.264979	44.924033
3500.707990	781855.954934	44.929037
3500.678748	781862.421885	44.934042
3500.565095	781854.998196	44.939047
3500.900871	781843.930362	44.944052
3500.832481	781825.533124	44.949057
3500.828780	781822.008802	44.954061
3500.914348	781832.276515	44.959066
3500.880857	781832.379699	44.964071
3500.669110	781825.314012	44.969076
3500.851387	781829.251102	44.974081
3500.888232	781816.320614	44.979085
3500.951117	781808.134913	44.984090
3500.442853	781803.122814	44.989095
3500.460736	781807.134573	44.994100
3500.404779	781807.583972	44.999105
3500.949464	781808.820714	45.004109
3500.670382	781811.410166	45.009114
3500.942128	781809.507334	45.014119
3500.941479	781807.744999	45.019124
3500.810122	781793.763694	45.024129
3500.882160	781780.387016	45.029133
3500.712939	781779.189560	45.034138
3500.670821	781768.572337	45.039143
3500.914382	781781.948729	45.044148
3500.717499	781774.880666	45.049153
3501.088646	781767.381094	45.054157
3500.999651	781763.967990	45.059162
3500.704166	781750.403915	45.064167
3500.720389	781744.624371	45.069172
3500.386117	781743.942289	45.074177
3500.474371	781750.586813	45.079181
3500.418442	781762.345491	45.084186
3500.418416	781750.595629	45.089191
3500.688280	781763.821072	45.094196
3500.524389	781759.832180	45.099201
3500.883988	781761.440569	45.104205
3500.825093	781767.765374	45.109210
3500.739292	781743.104026	45.114215
3500.386093	781732.192667	45.119220
3500.989881	781729.748327	45.124225
3500.947504	781717.025864	45.129229
3500.458240	781728.215885	45.134234
3500.727495	781729.544656	45.139239
3500.831518	781728.255518	45.144244
3500.811680	781733.399255	45.149249
3501.120458	781726.496884	45.154253
3501.038091	781711.577545	45.159258
3501.087746	781695.756285	45.164263
3500.999014	781699.686858	45.169268
3500.628909	781701.605164	45.174273
3501.090952	781702.022554	45.179277
3500.363654	781677.852911	45.184282
3500.341271	781669.729329	45.189287
3500.627155	781666.649242	45.194292
3500.678927	781662.332828	45.199297
3500.852999	781665.194208	45.204301
3500.946096	781663.025511	45.209306
3500.884313	781662.888327	45.214311
3501.013110	781673.247443	45.219316
3500.920776	781660.777475	45.224321
3501.003728	781638.684169	45.229325
3500.472858	781638.669272	45.234330
3500.917008	781643.397835	45.239335
3501.004045	781644.608232	45.244340
3500.711296	781633.442469	45.249345
3500.956198	781609.169561	45.254349
3501.115347	781608.655126	45.259354
3501.412928	781602.292928	45.264359
3500.897905	781604.674546	45.269364
3500.719082	781587.713730	45.274369
3500.860441	781572.073679	45.279373
3500.654968	781569.070358	45.284378
3500.938059	781566.333377	45.289383
3500.982472	781561.871170	45.294388
3500.975137	781568.237063	45.299393
3501.137084	781560.378289	45.304397
3500.797539	781542.267458	45.309402
3500.471364	781533.260969	45.314407
3501.022756	781539.441628	45.319412
3501.043021	781530.821616	45.324417
3500.925251	781532.504686	45.329421
3500.985287	781520.402314	45.334426
3500.937727	781504.057242	45.339431
3501.006474	781512.124886	45.344436
3500.625046	781509.589680	45.349441
3500.936869	781506.211708	45.354445
3501.065418	781511.822016	45.359450
3501.096938	781482.441235	45.364455
3500.997556	781477.071211	45.369460
3500.717939	781467.616716	45.374465
3501.075713	781470.253624	45.379469
3500.718503	781466.490616	45.384474
3500.448462	781443.129924	45.389479
3500.560913	781435.474583	45.394484
3500.811749	781445.668094	45.399489
3500.971000	781431.836446	45.404493
3500.805157	781436.121949	45.409498
3500.942946	781432.869066	45.414503
3501.026332	781436.136403	45.419508
3500.840125	781419.078393	45.424513
3500.948482	781409.122524	45.429517
3500.470370	781412.869330	45.434522
3500.703129	781412.881940	45.439527
3500.875344	781412.463370	45.444532
3500.649245	781399.132537	45.449537
3500.658350	781405.838737	45.454541
3500.730884	781408.079614	45.459546
3501.102430	781391.913556	45.464551
3500.816070	781386.327885	45.469556
3500.609684	781380.778668	45.474561
3500.885141	781374.076989	45.479565
3500.631396	781374.949021	45.484570
3500.858598	781367.716311	45.489575
3500.737554	781374.198084	45.494580
3500.676705	781377.439037	45.499585
3500.728889	781354.811037	45.504589
3500.643644	781349.144936	45.509594
3500.431610	781347.023836	45.514599
3500.677015	781348.846023	45.519604
3500.411372	781349.034465	45.524609
3500.810975	781349.314759	45.529613
3500.831733	781357.194247	45.534618
3500.993320	781360.547319	45.539623
3500.770774	781357.595532	45.544628
3500.531805	781349.897106	45.549633
3500.851669	781333.934831	45.554637
3500.767990	781325.134959	45.559642
3500.552705	781322.524749	45.564647
3500.617233	781328.536907	45.569652
3500.704882	781334.643368	45.574657
3501.164351	781328.843137	45.579661
3501.056897	781331.748670	45.584666
3500.749555	781313.925952	45.589671
3500.913363	781308.465689	45.594676
3500.700354	781295.181564	45.599681
3501.045814	781291.847189	45.604685
3500.878425	781300.098885	45.609690
3500.988775	781295.773077	45.614695
3501.082439	781291.596759	45.619700
3500.809352	781270.830892	45.624705
3501.231264	781273.702660	45.629709
3500.749355	781267.559921	45.634714
3501.077727	781261.682203	45.639719
3500.818954	781250.755297	45.644724
3500.800366	781235.041541	45.649729
3500.607949	781222.537441	45.654733
3500.476113	781231.371205	45.659738
3500.683897	781239.368481	45.664743
3500.431049	781222.712082	45.669748
3500.449498	781230.836889	45.674753
3500.818735	781233.276253	45.679757
3500.149320	781237.591639	45.684762
3500.237087	781238.214456	45.689767
3500.606835	781234.386638	45.694772
3500.258064	781239.973866	45.699777
3500.380408	781242.255974	45.704781
3500.437072	781253.508327	45.709786
3500.681162	781237.851438	45.714791
3500.658746	781237.659129	45.719796
3500.678375	781242.552264	45.724801
3500.879402	781251.823585	45.729805
3500.822082	781247.132264	45.734810
3500.594295	781224.939285	45.739815
3500.625418	781221.702975	45.744820
3500.850648	781209.672143	45.749825
3500.574480	781139.993223	45.754829
3500.386341	781054.239959	45.759834
3500.300931	780902.906862	45.764839
3500.481929	780700.457755	45.769844
3499.800743	780440.698672	45.774849
3500.019690	780147.489548	45.779853
3499.359827	779808.371381	45.784858
3498.858738	779403.487075	45.789863
3498.909918	778958.868763	45.794868
3498.324428	778476.261902	45.799873
3497.892408	777939.369578	45.804877
3497.119564	777362.904157	45.809882
3496.742893	776719.695432	45.814887
3496.174756	776039.804073	45.819892
3495.276939	775320.790515	45.824897
3495.089510	774531.652430	45.829901
3493.973683	773716.295352	45.834906
3493.365251	772859.141575	45.839911
3492.286869	771950.571637	45.844916
3491.881802	770985.679115	45.849921
3490.883402	769973.123007	45.854925
3489.988859	768925.085226	45.859930
3488.728142	767825.287039	45.864935
3487.949646	766680.686115	45.869940
3486.650570	765487.197068	45.874945
3485.825669	764253.621965	45.879949
3484.691427	762986.641009	45.884954
3483.726221	761658.713992	45.889959
3482.054998	760283.056531	45.894964
3480.286612	758880.619190	45.899969
3479.504945	757432.203619	45.904973
3477.641880	755936.877349	45.909978
3476.448911	754410.803870	45.914983
3474.810188	752847.993655	45.919988
3473.100462	751231.449263	45.924993
3472.108601	749581.227568	45.929997
3469.851793	747885.957163	45.935002
3468.302692	746139.738711	45.940007
3466.586372	744384.511729	45.945012
3465.008822	742585.169794	45.950017
3463.282490	740746.947108	45.955021
3461.337728	738871.058712	45.960026
3459.511085	736955.651521	45.965031
3457.799375	735009.716470	45.970036
3455.962084	733028.339840	45.975041
3454.033167	730999.557480	45.980045
3451.599323	728943.324880	45.985050
3450.052351	726849.093168	45.990055
3447.827619	724736.621428	45.995060
3445.466615	722576.934218	46.000065
3443.801424	720376.777628	46.005069
3441.320828	718162.831443	46.010074
3439.048494	715902.120366	46.015079
3437.171417	713618.251220	46.020084
3434.788091	711292.216281	46.025089
3432.820516	708943.964614	46.030093
3430.037279	706572.090046	46.035098
3428.063407	704158.854397	46.040103
3425.413695	701714.158101	46.045108
3422.982446	699253.829337	46.050113
3420.885831	696760.456312	46.055117
3418.271637	694239.843987	46.060122
3415.652939	691681.187282	46.065127
3413.542832	689104.155336	46.070132
3410.504262	686499.539065	46.075137
3408.502521	683855.403116	46.080141
3405.658530	681201.781759	46.085146
3402.902513	678511.276076	46.090151
3400.260502	675796.464368	46.095156
3397.337777	673059.626283	46.100161
3395.312746	670293.159869	46.105165
3392.307303	667505.388153	46.110170
3389.331102	664689.875080	46.115175
3386.819896	661849.566145	46.120180
3384.099614	658992.509351	46.125185
3381.417062	656099.448244	46.130189
3378.356962	653200.785653	46.135194
3375.234055	650270.680142	46.140199
3372.378233	647325.445234	46.145204
3369.669804	644361.604754	46.150209
3366.381045	641369.792015	46.155213
3363.612161	638361.233705	46.160218
3360.675204	635326.503139	46.165223
3357.472879	632274.179863	46.170228
3354.497214	629205.426041	46.175233
3351.429343	626120.384117	46.180237
3348.530302	623027.995328	46.185242
3345.491623	619892.791593	46.190247
3342.142285	616748.548049	46.195252
3338.779442	613580.872469	46.200257
3335.945857	610401.967543	46.205261
3332.715684	607231.333679	46.210266
3329.430967	604016.299169	46.215271
3326.347373	600793.928361	46.220276
3323.025284	597559.736897	46.225281
3319.906915	594299.031040	46.230285
3316.508723	591028.854027	46.235290
3313.321341	587750.282873	46.240295
3310.056266	584459.655755	46.245300
3306.265895	581146.762988	46.250305
3303.302976	577810.179411	46.255309
3299.757688	574483.427803	46.260314
3296.395235	571124.753880	46.265319
3292.944167	567768.920688	46.270324
3289.407754	564396.306894	46.275329
3286.238119	561010.604978	46.280333
3282.471755	557605.986079	46.285338
3279.025271	554208.736934	46.290343
3275.880206	550795.501200	46.295348
3272.133236	547370.289569	46.300353
3268.731969	543933.055381	46.305357
3265.284716	540502.477050	46.310362
3261.371155	537053.322196	46.315367
3257.962775	533585.636235	46.320372
3254.350466	530120.171674	46.325377
3251.003655	526639.793533	46.330381
3247.274947	523177.199002	46.335386
3243.630274	519672.472481	46.340391
3240.065383	516181.242532	46.345396
3236.406543	512680.919758	46.350401
3232.923482	509158.303726	46.355405
3229.123318	505651.400878	46.360410
3225.422005	502134.688492	46.365415
3222.012590	498599.914246	46.370420
3217.910110	495067.524315	46.375425
3214.881581	491530.641104	46.380429
3211.118161	487981.222688	46.385434
3207.105060	484441.928757	46.390439
3203.562657	480881.186116	46.395444
3199.645020	477334.754859	46.400449
3196.335175	473763.982715	46.405453
3192.315492	470200.571674	46.410458
3188.731777	466631.867634	46.415463
3185.303352	463064.296515	46.420468
3182.013505	459481.531494	46.425473
3178.037121	455889.321116	46.430477
3173.984434	452308.682617	46.435482
3169.987412	448713.845993	46.440487
3166.773046	445125.056471	46.445492
3162.863734	441521.087081	46.450497
3159.148811	437916.795769	46.455501
3155.377420	434326.267700	46.460506
3151.301278	430724.477781	46.465511
3147.789769	427115.401108	46.470516
3143.857974	423515.066419	46.475521
3140.342307	419907.844998	46.480525
3136.018102	416311.431573	46.485530
3132.412953	412708.411155	46.490535
3128.667234	409106.840123	46.495540
3124.443611	405499.427240	46.500545
3120.951195	401888.022188	46.505549
3117.042013	398291.541602	46.510554
3113.289922	394689.864820	46.515559
3109.497199	391087.753443	46.520564
3105.568278	387493.230829	46.525569
3101.592335	383890.149768	46.530573
3097.563021	380296.447445	46.535578
3093.583748	376703.234192	46.540583
3090.333339	373109.526681	46.545588
3085.847336	369524.179302	46.550593
3082.027813	365931.436365	46.555597
3078.237820	362346.169689	46.560602
3074.358398	358764.803444	46.565607
3070.530612	355191.166277	46.570612
3066.558226	351631.530621	46.575617
3063.041645	348045.397714	46.580621
3058.738987	344486.101968	46.585626
3054.719763	340912.049483	46.590631
3051.156231	337353.506956	46.595636
3046.708399	333803.070093	46.600641
3043.032400	330252.099906	46.605645
3039.233461	326698.864953	46.610650
3034.976608	323152.662480	46.615655
3030.983025	319611.026519	46.620660
3026.829442	316081.159495	46.625665
3023.105315	312542.423186	46.630669
3019.075822	309018.581745	46.635674
3015.183949	305501.283640	46.640679
3011.345354	301988.390870	46.645684
3007.022355	298497.332071	46.650689
3003.101881	295002.376677	46.655693
2999.255165	291510.942472	46.660698
2995.241825	288021.041585	46.665703
2990.993285	284544.380669	46.670708
2986.381432	281091.506820	46.675713
2982.700553	277624.193313	46.680717
2978.323992	274183.212092	46.685722
2974.578870	270751.716472	46.690727
2970.131727	267335.782628	46.695732
2966.014915	263925.125780	46.700737
2961.982698	260524.174617	46.705741
2957.807963	257135.878297	46.710746
2953.792694	253748.663855	46.715751
2949.567657	250374.466279	46.720756
2945.175716	247022.533855	46.725761
2941.190749	243668.821979	46.730765
2937.117687	240337.408380	46.735770
2932.829613	237025.190232	46.740775
2928.370363	233711.591390	46.745780
2923.996503	230416.548264	46.750785
2920.281957	227128.799250	46.755789
2915.855866	223867.414589	46.760794
2911.927264	220613.799626	46.765799
2907.901196	217378.599887	46.770804
2903.394532	214148.665054	46.775809
2899.241431	210922.548440	46.780813
2895.207087	207725.686582	46.785818
2891.161837	204533.504821	46.790823
2887.128292	201340.837502	46.795828
2882.829335	198180.333470	46.800833
2878.691779	195024.733852	46.805837
2874.837088	191880.979137	46.810842
2870.079119	188761.739394	46.815847
2866.311042	185642.100133	46.820852
2861.494571	182543.012959	46.825857
2857.393466	179440.501757	46.830861
2852.923291	176379.938260	46.835866
2848.450574	173333.490069	46.840871
2844.761413	170304.654873	46.845876
2840.796140	167192.799547	46.850881
2836.837301	164169.328733	46.855885
2832.520326	161181.676271	46.860890
2827.975716	158200.435431	46.865895
2823.674129	155233.110731	46.870900
2819.118064	152281.515097	46.875905
2815.190403	149357.272811	46.880909
2810.989786	146454.367760	46.885914
2806.662305	143547.852920	46.890919
2803.033173	140668.803773	46.895924
2798.463990	137800.658219	46.900929
2794.575830	134951.066888	46.905933
2790.211762	132116.269430	46.910938
2785.682949	129291.882386	46.915943
2781.794132	126469.655729	46.920948
2777.780050	123684.143285	46.925953
2773.935539	120912.176094	46.930957
2769.460694	118148.095574	46.935962
2765.267775	115397.370270	46.940967
2761.405413	112669.721661	46.945972
2757.031907	109951.817251	46.950977
2752.859782	107230.810043	46.955981
2748.615177	104541.935127	46.960986
2744.248500	101875.626205	46.965991
2739.901191	99205.678163	46.970996
2735.976496	96569.473682	46.976001
2731.966441	93945.904605	46.981005
2727.828961	91330.379028	46.986010
2723.433985	88733.389096	46.991015
2719.802752	86149.794520	46.996020
2715.217087	83600.698278	47.001025
2711.276040	81036.141593	47.006029
2707.091652	78509.679601	47.011034
2702.726195	75987.260567	47.016039
2698.846968	73479.881707	47.021044
2694.701084	70998.110590	47.026049
2690.617787	68523.628724	47.031053
2686.371576	66062.998400	47.036058
2682.141136	63617.194269	47.041063
2677.858031	61195.238208	47.046068
2673.332224	58799.777359	47.051073
2669.433578	56401.706075	47.056077
2665.416705	54025.526884	47.061082
2660.937017	51660.404556	47.066087
2656.740315	49318.306218	47.071092
2652.465120	47011.716054	47.076097
2647.953575	44703.329091	47.081101
2644.072791	42420.591422	47.086106
2639.505715	40155.994015	47.091111
2635.193147	37904.359536	47.096116
2630.587994	35673.893041	47.101121
2626.618292	33464.787904	47.106125
2622.259470	31281.250398	47.111130
2617.811206	29114.292752	47.116135
2613.155961	26960.800463	47.121140
2608.789162	24842.730867	47.126145
2604.186454	22756.001347	47.131149
2599.929657	20681.870568	47.136154
2595.015019	18637.152268	47.141159
2590.339672	16607.905156	47.146164
2585.030808	14639.500580	47.151169
2579.155532	12709.090685	47.156173
2570.011988	10917.717124	47.161178
2560.227826	9196.950024	47.166183
2550.863996	7545.605162	47.171188
2541.428035	6020.352610	47.176193
2532.335207	4586.665729	47.181197
2520.193285	3348.388658	47.186202
2506.659496	2289.525111	47.191207
2493.783053	1368.735839	47.196212
2480.598490	632.290807	47.201217
2465.502017	121.352367	47.206221
2434.483394	240.930038	47.211226
2420.812572	242.992752	47.216231
2418.200092	234.574239	47.221236
2421.456762	234.855781	47.226241
2426.903085	246.516973	47.231245
2431.819606	241.005221	47.236250
2434.659808	242.509899	47.241255
2435.198651	224.954675	47.246260
2433.176318	237.160946	47.251265
2430.486127	227.523839	47.256269
2427.421522	232.837701	47.261274
2424.307969	233.644361	47.266279
2421.468216	217.623797	47.271284
2417.972664	224.368707	47.276289
2415.052519	224.252899	47.281293
2412.326016	219.946295	47.286298
2409.155464	217.936531	47.291303
2406.453467	219.479274	47.296308
2403.324458	223.139013	47.301313
2400.419145	211.121537	47.306317
2397.607654	228.652678	47.311322
2393.781266	216.981781	47.316327
2390.910112	216.798201	47.321332
2387.746254	214.183095	47.326337
2384.387817	216.986516	47.331341
2381.442126	221.971722	47.336346
2378.063434	215.982730	47.341351
2374.602910	215.720506	47.346356
2370.725272	218.791824	47.351361
2367.675144	223.755406	47.356365
2364.723405	214.371224	47.361370
2361.196869	213.708028	47.366375
2357.764790	210.929241	47.371380
2354.558037	231.686101	47.376385
2351.440828	220.185860	47.381389
2348.402881	210.011548	47.386394
2344.837009	226.037640	47.391399
2341.957260	216.556778	47.396404
2337.746972	220.173713	47.401409
2334.155146	208.583215	47.406413
2330.816233	212.196712	47.411418
2327.408185	222.221551	47.416423
2324.487643	216.654467	47.421428
2320.500221	223.182112	47.426433
2318.039291	207.510473	47.431437
2314.755313	211.134363	47.436442
2310.927448	207.082356	47.441447
2307.732907	215.213434	47.446452
2303.483358	213.612962	47.451457
2299.935290	207.659990	47.456461
2297.070826	213.942350	47.461466
2293.477629	221.202460	47.466471
2289.949500	215.629198	47.471476
2286.767089	207.062613	47.476481
2283.343909	207.072997	47.481485
2280.081476	212.057155	47.486490
2276.221057	211.848034	47.491495
2272.580880	208.737987	47.496500
2268.776053	216.518448	47.501505
2265.493647	207.644799	47.506509
2262.595560	204.406000	47.511514
2259.484628	203.836009	47.516519
2256.070818	206.799994	47.521524
2252.046066	207.625867	47.526529
2248.746764	209.619613	47.531533
2245.640155	208.178884	47.536538
2241.781187	214.544078	47.541543
2238.935172	209.332373	47.546548
2235.120381	210.457610	47.551553
2231.059023	201.534998	47.556557
2228.113734	205.548863	47.561562
2224.477105	205.643281	47.566567
2221.441606	201.954577	47.571572
2217.781027	200.280977	47.576577
2214.476972	203.284751	47.581581
2210.771523	203.949947	47.586586
2206.819210	207.358878	47.591591
2203.412949	208.170263	47.596596
2199.979915	201.031864	47.601601
2196.818274	205.209304	47.606605
2193.786488	200.080466	47.611610
2189.734285	210.414927	47.616615
2186.783294	196.161501	47.621620
2182.826232	196.502228	47.626625
2179.662336	205.691596	47.631629
2176.377765	201.260399	47.636634
2172.749694	200.736542	47.641639
2168.464485	193.358152	47.646644
2165.529275	212.322906	47.651649
2161.901020	200.386997	47.656653
2158.356736	200.634675	47.661658
2154.754541	209.690139	47.666663
2151.605195	204.484791	47.671668
2148.126923	198.394404	47.676673
2144.675557	204.097878	47.681677
2141.511681	201.792913	47.686682
2138.131710	201.967430	47.691687
2134.287916	196.579669	47.696692
2130.766601	198.639822	47.701697
2127.307816	195.453991	47.706701
2123.832730	194.621466	47.711706
2120.368003	201.807727	47.716711
2116.600746	187.957308	47.721716
2113.103111	200.046385	47.726721
2109.759906	196.102130	47.731725
2106.505331	196.263366	47.736730
2102.917648	194.075346	47.741735
2099.623922	196.428941	47.746740
2095.613866	194.095032	47.751745
2092.248792	199.310437	47.756749
2088.812877	199.322875	47.761754
2085.416776	203.935675	47.766759
2082.281167	198.006841	47.771764
2078.218441	204.106558	47.776769
2074.595257	191.923119	47.781773
2071.370353	193.209222	47.786778
2067.714039	198.960603	47.791783
2064.786098	197.896948	47.796788
2061.008356	194.836980	47.801793
2057.378412	191.121114	47.806797
2054.211007	200.184500	47.811802
2050.443610	194.582332	47.816807
2046.962491	188.369041	47.821812
2043.043991	195.208692	47.826817
2039.690967	192.281599	47.831821
2036.824512	189.961769	47.836826
2033.426627	188.519224	47.841831
2030.076194	186.781343	47.846836
2026.167264	192.005930	47.851841
2022.576723	193.026545	47.856845
2019.105265	190.073697	47.861850
2015.187821	188.886467	47.866855
2012.241083	196.950354	47.871860
2008.723241	194.776750	47.876865
2005.121687	190.237021	47.881869
2001.457741	191.844952	47.886874
1997.941381	195.733084	47.891879
1994.381231	195.866235	47.896884
1991.420959	188.229987	47.901889
1987.754460	201.481343	47.906893
1984.192220	193.565953	47.911898
1980.553129	194.287283	47.916903
1977.218013	192.180015	47.921908
1973.845787	187.689838	47.926913
1970.604246	181.521350	47.931917
1966.694477	181.066954	47.936922
1963.018718	194.186877	47.941927
1959.481631	179.262776	47.946932
1956.164117	191.576806	47.951937
1952.699755	187.426932	47.956941
1949.199102	184.042065	47.961946
1945.589789	185.768020	47.966951
1942.293036	177.792127	47.971956
1939.037168	184.341450	47.976961
1934.920614	176.588759	47.981965
1931.885583	167.176659	47.986970
1928.048188	179.809328	47.991975
1924.647752	189.105361	47.996980
1921.297519	194.286850	48.001985
1917.897312	187.307949	48.006989
1914.651762	180.466207	48.011994
1910.790593	187.980318	48.016999
1907.159733	179.082251	48.022004
1903.941355	193.174688	48.027009
1900.485931	182.382491	48.032013
1896.636437	183.956215	48.037018
1892.609903	189.718120	48.042023
1889.817759	187.424670	48.047028
1886.498643	185.618659	48.052033
1883.121972	194.629403	48.057037
1879.306672	185.624160	48.062042
1875.332650	184.917253	48.067047
1872.285405	177.380085	48.072052
1869.186956	186.141639	48.077057
1865.201467	188.388410	48.082061
1862.062336	187.759672	48.087066
1858.401911	178.587833	48.092071
1855.010346	180.165843	48.097076
1851.163687	188.547763	48.102081
1847.906978	187.010418	48.107085
1844.297065	182.117708	48.112090
1840.790683	181.204751	48.117095
1837.014136	175.474389	48.122100
1833.548078	182.072449	48.127105
1830.133528	182.344226	48.132109
1827.097475	176.244880	48.137114
1823.076622	182.812700	48.142119
1819.842891	169.960984	48.147124
1816.509222	173.039104	48.152129
1812.628063	176.468667	48.157133
1809.630270	171.866172	48.162138
1805.882554	176.274633	48.167143
1802.678514	179.481174	48.172148
1798.968196	177.755396	48.177153
1795.085974	182.656326	48.182157
1792.016111	181.966148	48.187162
1788.150735	184.605451	48.192167
1784.552869	173.247123	48.197172
1781.022282	173.366228	48.202177
1777.852974	171.941784	48.207181
1774.188711	171.199096	48.212186
1770.620123	178.395366	48.217191
1767.222453	175.079875	48.222196
1763.993067	177.331745	48.227201
1760.212988	173.620507	48.232205
1756.909994	166.582169	48.237210
1753.279421	172.785201	48.242215
1750.230349	165.495149	48.247220
1746.164641	165.995414	48.252225
1743.021559	169.875822	48.257229
1739.464979	174.453714	48.262234
1735.621404	174.375036	48.267239
1732.633484	171.261196	48.272244
1728.948470	169.873182	48.277249
1725.003091	175.533850	48.282253
1722.006524	171.402606	48.287258
1718.103502	168.359217	48.292263
1714.767140	154.498531	48.297268
1711.335873	170.835834	48.302273
1707.538460	171.218192	48.307277
1704.344286	161.141367	48.312282
1700.573024	177.427482	48.317287
1697.703936	172.225895	48.322292
1693.858511	169.148191	48.327297
1690.297586	163.301888	48.332301
1686.867805	167.078479	48.337306
1683.284661	167.389346	48.342311
1680.020612	161.477603	48.347316
1676.441840	164.097398	48.352321
1672.807695	164.637720	48.357325
1669.511948	158.832186	48.362330
1665.568546	169.260484	48.367335
1662.092953	162.473829	48.372340
1658.669034	160.206559	48.377345
1655.580909	171.023039	48.382349
1652.255772	160.498481	48.387354
1648.257253	160.216289	48.392359
1644.555808	157.435622	48.397364
1640.890400	163.191706	48.402369
1637.745439	171.378436	48.407373
1634.341643	159.512069	48.412378
1630.376811	167.823953	48.417383
1627.362244	160.424140	48.422388
1623.913274	159.635156	48.427393
1620.015761	160.466660	48.432397
1616.816144	159.183058	48.437402
1612.979475	161.890695	48.442407
1609.564147	161.349558	48.447412
1606.177490	163.711511	48.452417
1602.910631	164.953697	48.457421
1599.416570	158.682503	48.462426
1595.911138	161.857174	48.467431
1592.455078	162.442420	48.472436
1588.986307	160.878241	48.477441
1585.348536	166.940075	48.482445
1581.875180	155.315582	48.487450
1578.140061	165.996051	48.492455
1574.939616	162.023321	48.497460
1570.944840	160.234583	48.502465
1567.478684	163.235432	48.507469
1564.484538	152.706569	48.512474
1560.780673	155.997732	48.517479
1557.255017	155.068910	48.522484
1553.838078	163.893028	48.527489
1549.974637	160.172778	48.532493
1547.126831	166.269173	48.537498
1543.050240	159.636747	48.542503
1539.925699	160.192269	48.547508
1536.654907	155.369999	48.552513
1532.668982	157.234132	48.557517
1529.206539	162.297240	48.562522
1525.376662	161.985537	48.567527
1522.319752	156.243918	48.572532
1518.536941	158.917848	48.577537
1515.254478	156.919562	48.582541
1511.918774	144.318082	48.587546
1508.149055	163.995625	48.592551
1504.590367	157.399217	48.597556
1501.133293	162.167255	48.602561
1497.642589	162.099876	48.607565
1494.552213	154.490510	48.612570
1490.819796	157.697579	48.617575
1487.143799	151.100559	48.622580
1483.794397	155.987793	48.627585
1480.082126	165.117593	48.632589
1476.780394	159.199168	48.637594
1472.815479	163.271563	48.642599
1469.387853	167.696471	48.647604
1466.337602	153.740491	48.652609
1462.979996	158.410711	48.657613
1459.767012	148.466653	48.662618
1455.609556	164.756312	48.667623
1452.135070	162.310363	48.672628
1449.063335	157.244990	48.677633
1445.215556	152.022673	48.682637
1441.574938	157.116859	48.687642
1438.037928	168.231443	48.692647
1434.868147	163.858481	48.697652
1431.272626	153.901542	48.702657
1427.787212	155.538670	48.707661
1424.410095	149.040431	48.712666
1420.676585	162.134699	48.717671
1416.916023	155.987555	48.722676
1413.595319	164.951675	48.727681
1409.679664	164.539544	48.732685
1406.616281	154.831522	48.737690
1403.132770	160.407343	48.742695
1399.600494	159.470121	48.747700
1396.354419	160.190248	48.752705
1392.267524	166.676794	48.757709
1389.199950	156.358813	48.762714
1385.760427	158.811370	48.767719
1382.099033	162.165551	48.772724
1378.597825	159.011949	48.777729
1375.203475	156.170661	48.782733
1371.819352	150.704950	48.787738
1367.972007	154.825418	48.792743
1364.917585	155.221317	48.797748
1361.219860	154.192946	48.802753
1357.401003	151.854726	48.807757
1354.675039	147.678087	48.812762
1350.640792	155.077079	48.817767
1347.110649	162.897052	48.822772
1343.320054	151.651368	48.827777
1339.650619	160.920038	48.832781
1336.551746	151.249239	48.837786
1332.817997	158.474647	48.842791
1329.773725	146.087060	48.847796
1326.524324	146.143324	48.852801
1322.755881	151.399928	48.857805
1319.009157	156.991666	48.862810
1315.355915	159.794086	48.867815
1311.965049	150.330362	48.872820
1308.554912	146.257675	48.877825
1305.258203	155.629361	48.882829
1302.129480	149.668105	48.887834
1298.124263	162.393641	48.892839
1294.835566	152.619692	48.897844
1291.055936	157.216818	48.902849
1287.359540	158.330186	48.907853
1284.159554	152.462351	48.912858
1280.413215	154.795289	48.917863
1277.085474	150.244630	48.922868
1273.632105	150.858038	48.927873
1269.522576	161.673134	48.932877
1266.445286	146.791311	48.937882
1263.177861	147.742618	48.942887
1259.581745	145.809343	48.947892
1255.913562	142.587015	48.952897
1252.279266	155.941045	48.957901
1248.996771	146.454058	48.962906
1245.311212	156.335897	48.967911
1242.048619	159.089843	48.972916
1238.657558	148.544150	48.977921
1234.911234	151.636422	48.982925
1231.936582	148.432084	48.987930
1228.127911	154.255018	48.992935
1224.634313	148.876109	48.997940
1221.063619	150.124850	49.002945
1217.479071	154.163100	49.007949
1214.152160	153.870857	49.012954
1210.264463	156.912502	49.017959
1207.031825	155.703810	49.022964
1203.351531	145.763414	49.027969
1199.981629	154.191106	49.032973
1196.594755	142.705121	49.037978
1192.902324	152.230536	49.042983
1189.422633	151.319962	49.047988
1186.171597	149.569979	49.052993
1182.637346	151.369863	49.057997
1179.270928	143.579205	49.063002
1175.460463	156.233153	49.068007
1171.699115	159.296163	49.073012
1168.524900	149.086721	49.078017
1164.756035	147.579169	49.083021
1161.389715	148.814919	49.088026
1157.902116	148.383333	49.093031
1154.584928	139.642158	49.098036
1151.139140	154.672006	49.103041
1147.328106	151.810615	49.108045
1143.943640	148.901426	49.113050
1140.322385	148.323088	49.118055
1136.915485	150.802257	49.123060
1133.563795	146.998905	49.128065
1129.870895	152.389284	49.133069
1126.195764	145.251271	49.138074
1122.844352	148.148875	49.143079
1119.863859	143.904590	49.148084
1116.211376	144.916230	49.153089
1112.472395	145.555427	49.158093
1109.367313	148.243622	49.163098
1105.678739	144.559464	49.168103
1101.772401	141.086576	49.173108
1098.313801	146.399152	49.178113
1094.556017	147.753161	49.183117
1091.168284	141.471862	49.188122
1087.975200	142.585598	49.193127
1084.198318	146.698297	49.198132
1081.116497	146.010216	49.203137
1077.090696	151.111040	49.208141
1073.890080	143.133112	49.213146
1070.277611	150.330120	49.218151
1067.184222	139.541746	49.223156
1063.503055	138.099602	49.228161
1059.452583	146.637048	49.233165
1056.660611	152.069899	49.238170
1053.189513	151.113736	49.243175
1049.213292	140.561670	49.248180
1045.761771	141.260291	49.253185
1042.350402	144.607080	49.258189
1038.900885	136.785201	49.263194
1035.135034	150.416151	49.268199
1031.654313	145.278920	49.273204
1028.310443	137.051353	49.278209
1024.996850	150.779179	49.283213
1021.816632	134.268400	49.288218
1017.758921	146.856693	49.293223
1014.642755	143.529050	49.298228
1011.016811	134.478768	49.303233
1007.226806	134.898198	49.308237
1003.860427	142.297144	49.313242
1000.369650	138.066358	49.318247
996.372750	143.327204	49.323252
993.402814	137.622787	49.328257
989.457209	140.205334	49.333261
986.305183	136.570099	49.338266
983.074435	141.676188	49.343271
979.390123	146.970357	49.348276
976.254516	142.728263	49.353281
972.233196	140.845857	49.358285
968.884045	142.113785	49.363290
965.149741	152.594973	49.368295
961.791239	141.316629	49.373300
958.700574	144.765095	49.378305
954.522320	149.529158	49.383309
951.078426	138.612212	49.388314
947.572217	145.064940	49.393319
944.381278	147.678041	49.398324
940.775964	139.975512	49.403329
937.033859	151.134988	49.408333
933.541158	147.008934	49.413338
930.141513	141.447754	49.418343
927.071732	151.090895	49.423348
923.572922	147.453030	49.428353
919.736385	148.904861	49.433357
916.635453	134.928598	49.438362
912.596893	149.190753	49.443367
909.359551	142.661347	49.448372
906.088480	136.864906	49.453377
901.968138	148.687907	49.458381
898.777878	144.046265	49.463386
895.272894	146.835108	49.468391
891.786894	143.249037	49.473396
888.297579	140.375348	49.478401
884.249062	146.362507	49.483405
881.096337	137.908915	49.488410
877.680996	141.787902	49.493415
874.139485	148.524598	49.498420
870.480529	139.818076	49.503425
867.384859	141.400695	49.508429
863.581631	142.587899	49.513434
860.025838	149.931126	49.518439
856.872422	144.046675	49.523444
853.392874	144.395406	49.528449
849.799825	143.850730	49.533453
846.448875	146.723041	49.538458
842.397954	150.138405	49.543463
838.999567	135.636102	49.548468
835.389735	138.567936	49.553473
831.977029	147.768076	49.558477
828.906316	138.972625	49.563482
825.464894	137.730322	49.568487
821.643150	136.152097	49.573492
818.151574	138.495932	49.578497
814.695037	144.146804	49.583501
811.394087	144.284081	49.588506
807.892300	147.151551	49.593511
803.774688	151.042455	49.598516
800.776924	143.722587	49.603521
796.961266	143.402620	49.608525
793.810839	133.509167	49.613530
790.056309	140.469074	49.618535
786.416275	137.900607	49.623540
783.230499	139.573296	49.628545
779.525028	144.462714	49.633549
776.332905	135.778049	49.638554
772.513556	145.057702	49.643559
768.811868	144.068152	49.648564
765.694358	139.449972	49.653569
762.393702	150.511896	49.658573
758.826244	137.782537	49.663578
754.820415	143.278995	49.668583
751.415856	144.077938	49.673588
748.313685	144.215748	49.678593
744.484492	150.117994	49.683597
741.315877	131.286456	49.688602
737.601566	142.042993	49.693607
733.697871	142.274688	49.698612
730.798540	143.070451	49.703617
727.101003	146.512781	49.708621
724.018513	133.024111	49.713626
720.144862	146.491690	49.718631
716.557018	138.558732	49.723636
713.119923	135.082138	49.728641
709.459167	138.404815	49.733645
706.197408	139.415534	49.738650
702.577633	142.004119	49.743655
699.120459	136.951928	49.748660
695.777340	143.812638	49.753665
691.876308	143.787664	49.758669
688.291434	137.385544	49.763674
684.800185	138.096845	49.768679
681.342979	143.627639	49.773684
678.233479	138.622252	49.778689
674.084230	134.861724	49.783693
671.065929	134.584621	49.788698
667.980281	131.717408	49.793703
664.239911	136.577529	49.798708
660.739865	132.035117	49.803713
656.900512	138.340788	49.808717
653.314292	128.990220	49.813722
649.733877	137.011258	49.818727
646.468736	138.974837	49.823732
642.938632	136.177238	49.828737
639.161362	143.004715	49.833741
636.288389	128.689157	49.838746
632.615227	132.070754	49.843751
629.090572	136.087167	49.848756
625.927895	131.419167	49.853761
621.840165	133.796324	49.858765
618.280945	126.380964	49.863770
614.941768	115.131409	49.868775
611.364881	129.090379	49.873780
608.070544	123.534993	49.878785
604.450246	125.544716	49.883789
601.077432	125.206097	49.888794
597.211198	121.692357	49.893799
593.521001	130.872740	49.898804
590.475533	130.533478	49.903809
587.121387	135.086361	49.908813
583.666003	129.148074	49.913818
579.906881	135.488663	49.918823
576.277984	126.445379	49.923828
572.990265	129.042117	49.928833
569.328453	132.706702	49.933837
565.938096	124.736563	49.938842
562.271415	122.039486	49.943847
558.931147	119.152081	49.948852
555.778561	116.320706	49.953857
551.973234	123.586044	49.958861
548.769777	119.854624	49.963866
544.886771	121.351848	49.968871
541.318861	129.326666	49.973876
537.747116	124.010913	49.978881
533.832736	131.018088	49.983885
530.768562	120.851814	49.988890
527.689390	132.600449	49.993895
524.146740	127.248506	49.998900
520.805263	125.041524	50.003905
517.093299	127.647778	50.008909
513.451847	121.472907	50.013914
509.832902	123.773524	50.018919
505.839673	118.748432	50.023924
502.409432	120.418372	50.028929
499.123209	124.609460	50.033933
495.919363	129.809559	50.038938
492.400384	126.864747	50.043943
488.831692	117.628578	50.048948
485.655628	115.781688	50.053953
482.091908	121.797469	50.058957
478.313006	124.629361	50.063962
474.797914	119.266799	50.068967
471.198601	117.695017	50.073972
467.853608	116.985089	50.078977
464.552581	132.134780	50.083981
460.867930	120.929913	50.088986
457.536794	122.967168	50.093991
453.821541	119.451992	50.098996
450.163728	116.269513	50.104001
446.540138	128.657104	50.109005
443.441577	123.067957	50.114010
439.608859	124.449779	50.119015
435.812459	122.168551	50.124020
432.700080	115.300233	50.129025
429.449007	126.120343	50.134029
426.105915	118.497212	50.139034
422.791802	121.202540	50.144039
418.827315	126.278191	50.149044
415.203508	114.434223	50.154049
411.745157	125.131777	50.159053
408.185567	116.719977	50.164058
404.559174	124.416092	50.169063
400.979498	117.728551	50.174068
398.031288	122.717791	50.179073
394.354305	127.678814	50.184077
390.989018	123.915855	50.189082
387.330914	128.146249	50.194087
383.442359	124.898698	50.199092
380.183426	121.229818	50.204097
376.621928	122.714718	50.209101
373.239278	112.139650	50.214106
369.758046	116.525843	50.219111
366.214996	120.402858	50.224116
362.951808	116.136693	50.229121
358.873148	121.913633	50.234125
356.028832	116.863675	50.239130
352.548339	119.088880	50.244135
348.891855	117.415372	50.249140
345.218262	120.426977	50.254145
341.301598	131.629788	50.259149
337.735587	120.966394	50.264154
334.798966	123.577819	50.269159
331.566078	116.927739	50.274164
327.997739	111.918439	50.279169
324.121643	119.618892	50.284173
320.593022	116.261206	50.289178
317.247009	114.937718	50.294183
313.708555	119.456283	50.299188
310.402935	116.244006	50.304193
306.619065	114.919506	50.309197
302.826885	107.363620	50.314202
299.875416	114.488963	50.319207
295.947372	122.305134	50.324212
292.514812	113.952586	50.329217
288.723524	120.197073	50.334221
285.451974	109.857750	50.339226
282.066816	103.557421	50.344231
278.616548	118.638773	50.349236
275.568141	111.912363	50.354241
271.310345	117.258647	50.359245
268.389148	118.504077	50.364250
264.568593	120.390275	50.369255
260.943597	118.306905	50.374260
257.687676	113.087341	50.379265
254.207312	122.171687	50.384269
250.756526	107.462773	50.389274
247.181942	125.173748	50.394279
243.743190	123.599056	50.399284
240.397541	107.181043	50.404289
236.925569	124.154599	50.409293
233.125417	115.030746	50.414298
229.321076	108.631588	50.419303
225.585096	113.899310	50.424308
222.539985	118.767736	50.429313
218.932433	119.652462	50.434317
215.484785	113.225904	50.439322
212.395244	121.764976	50.444327
208.772057	116.267603	50.449332
205.432556	117.961404	50.454337
201.774164	114.820255	50.459341
198.056630	112.596384	50.464346
194.498690	120.841838	50.469351
190.612703	115.765301	50.474356
187.503059	114.382687	50.479361
183.696560	123.087870	50.484365
180.672183	113.560933	50.489370
177.046922	121.759992	50.494375
173.446641	121.802026	50.499380
170.170435	111.295803	50.504385
166.666950	120.962773	50.509389
163.232522	112.484025	50.514394
159.625544	118.051108	50.519399
156.115486	119.335043	50.524404
152.416614	126.830625	50.529409
148.978966	123.360682	50.534413
145.805190	126.790779	50.539418
142.301867	124.546026	50.544423
138.134402	124.863597	50.549428
134.940457	114.224277	50.554433
131.340079	117.724375	50.559437
127.848310	118.872576	50.564442
124.506960	119.933936	50.569447
120.749237	124.145235	50.574452
117.542431	124.119319	50.579457
113.407068	126.133996	50.584461
110.224305	120.561340	50.589466
106.862935	119.534573	50.594471
103.569842	127.643653	50.599476
99.999128	119.774751	50.604481
96.429049	122.143804	50.609485
93.073488	121.783694	50.614490
89.295183	118.126699	50.619495
85.875796	114.059130	50.624500
82.553849	115.316785	50.629505
78.678090	126.642992	50.634509
75.575106	116.998699	50.639514
72.031553	122.166730	50.644519
68.328598	123.186688	50.649524
65.230129	113.858074	50.654529
61.193629	125.146194	50.659533
57.993046	126.220327	50.664538
54.387042	127.060584	50.669543
50.474631	123.728342	50.674548
47.924500	120.075096	50.679553
43.588506	125.772262	50.684557
40.528876	116.393278	50.689562
37.394565	119.535650	50.694567
33.337715	121.803821	50.699572
29.752767	116.215118	50.704577
25.947760	123.129417	50.709581
22.997457	111.129510	50.714586
19.822155	112.471782	50.719591
15.998469	120.648201	50.724596
12.657980	116.514516	50.729601
8.542615	117.953461	50.734605
4.960573	112.829393	50.739610
2.035614	115.802931	50.744615