Thu Aug 25 16:56:15 2022

Number of Points = 9925

Depth (nm)	Load (N)	Time (s)
0.944180	102.550238	0.000000
1.599505	116.928284	0.005005
1.287042	118.679396	0.010010
1.663874	113.675371	0.015014
1.515572	117.991911	0.020019
1.664744	115.962723	0.025024
1.542740	104.377068	0.030029
1.347724	98.263567	0.035034
0.854890	90.602179	0.040038
0.422896	79.283412	0.045043
0.568870	74.208000	0.050048
0.546070	69.785463	0.055053
0.055456	64.126418	0.060058
-0.182948	52.090794	0.065062
-0.319624	43.029015	0.070067
-1.296805	42.103303	0.075072
-1.371641	36.610078	0.080077
-1.888060	28.923939	0.085082
-2.474640	26.592421	0.090086
-2.573972	12.586145	0.095091
-3.169574	16.928452	0.100096
-2.925937	12.647683	0.105101
-2.951688	22.497430	0.110106
-2.922049	7.828704	0.115110
-3.110012	17.444434	0.120115
-3.925566	9.150271	0.125120
-3.783971	0.595411	0.130125
-4.216423	14.460433	0.135130
-4.295781	2.779577	0.140134
-4.883157	-5.885691	0.145139
-5.294503	2.894994	0.150144
-4.700647	-3.383203	0.155149
-5.982030	9.336663	0.160154
-6.537503	8.544197	0.165158
-6.787927	-0.461771	0.170163
-6.939569	12.049448	0.175168
-6.528127	21.906625	0.180173
-7.275077	21.055574	0.185178
-7.059419	12.856102	0.190182
-6.884414	6.140488	0.195187
-7.130253	0.626610	0.200192
-7.944269	-2.770262	0.205197
-8.159194	9.067495	0.210202
-8.428446	1.244565	0.215206
-8.279904	-0.825640	0.220211
-9.215888	5.626451	0.225216
-9.525697	10.686448	0.230221
-9.878126	7.220415	0.235226
-9.594681	8.707304	0.240230
-9.636311	5.470986	0.245235
-9.778265	11.912564	0.250240
-10.131158	11.521796	0.255245
-10.912296	14.061345	0.260250
-11.201548	1.400969	0.265254
-10.923970	2.600873	0.270259
-11.273579	4.228079	0.275264
-11.485285	8.133745	0.280269
-12.267273	15.172320	0.285274
-12.644548	13.345852	0.290278
-12.540359	4.062855	0.295283
-12.800092	17.552802	0.300288
-12.510836	6.978459	0.305293
-12.943005	14.952485	0.310298
-13.777461	11.717003	0.315302
-14.109120	5.134559	0.320307
-14.350630	7.931245	0.325312
-14.165602	-0.389972	0.330317
-14.111226	4.767986	0.335322
-14.113886	5.129105	0.340326
-14.657946	-0.847413	0.345331
-15.564712	1.085391	0.350336
-15.393576	4.238204	0.355341
-15.629324	10.963398	0.360346
-15.503240	18.179236	0.365350
-16.211892	2.813102	0.370355
-16.409844	3.679387	0.375360
-17.416576	-0.633258	0.380365
-17.489274	13.425333	0.385370
-17.032120	10.772093	0.390374
-16.783440	3.450146	0.395379
-17.932938	10.460880	0.400384
-17.957897	8.860788	0.405389
-18.484956	10.743591	0.410394
-18.761367	4.392938	0.415398
-18.329068	-0.480540	0.420403
-18.310010	2.360740	0.425408
-18.841372	3.839253	0.430413
-19.901392	9.788757	0.435418
-19.857542	-0.263072	0.440422
-20.161274	4.906704	0.445427
-20.385201	8.168873	0.450432
-20.229261	5.015497	0.455437
-20.559892	8.414609	0.460442
-21.111731	10.737896	0.465446
-21.306171	2.444497	0.470451
-21.446852	11.078371	0.475456
-21.213811	4.771283	0.480461
-22.360618	3.663345	0.485466
-22.801093	5.121290	0.490470
-23.017251	3.364493	0.495475
-22.834693	13.270181	0.500480
-23.273600	-2.783622	0.505485
-22.889891	5.182787	0.510490
-23.174353	3.360762	0.515494
-23.012063	-0.910422	0.520499
-24.165693	4.784827	0.525504
-24.376765	-1.563405	0.530509
-24.553817	7.512768	0.535514
-24.733333	7.784538	0.540518
-24.584018	1.354527	0.545523
-25.136130	6.392376	0.550528
-25.807702	4.687953	0.555533
-26.283233	12.548548	0.560538
-26.093083	5.118712	0.565542
-26.196285	8.959920	0.570547
-26.329730	11.926337	0.575552
-26.197836	1.715178	0.580557
-26.875228	5.007270	0.585562
-27.438339	9.312847	0.590566
-27.604716	-1.452692	0.595571
-27.872206	5.277473	0.600576
-27.562867	0.192305	0.605581
-28.081887	5.142710	0.610586
-28.351870	4.631383	0.615590
-28.424209	6.395482	0.620595
-28.912049	10.996152	0.625600
-29.211135	6.901662	0.630605
-29.391242	8.793378	0.635610
-30.100026	0.444529	0.640614
-29.872999	3.354464	0.645619
-30.274370	14.816473	0.650624
-30.144073	10.585101	0.655629
-30.830056	13.707696	0.660634
-31.413169	-4.177482	0.665638
-31.136402	5.665982	0.670643
-31.495995	13.173052	0.675648
-31.585051	2.031561	0.680653
-31.905676	6.052369	0.685658
-32.370219	10.203296	0.690662
-32.493147	-0.347587	0.695667
-33.167715	16.007297	0.700672
-33.009354	9.493608	0.705677
-33.219588	9.643640	0.710682
-33.570798	12.406895	0.715686
-33.278646	8.852521	0.720691
-33.809576	9.764652	0.725696
-34.877118	5.603906	0.730701
-35.090589	4.507918	0.735706
-35.195730	11.380328	0.740710
-34.780207	3.298243	0.745715
-34.888677	15.324967	0.750720
-35.115058	9.583412	0.755725
-35.565942	8.315814	0.760730
-36.055614	16.403255	0.765734
-36.156732	10.294057	0.770739
-36.759091	10.980097	0.775744
-36.479219	10.306684	0.780749
-37.161916	9.692344	0.785754
-37.831723	15.267497	0.790758
-37.869529	9.974125	0.795763
-38.446784	17.315983	0.800768
-38.385739	4.831677	0.805773
-38.286436	5.293879	0.810778
-38.406670	18.325366	0.815782
-38.022513	11.390316	0.820787
-38.641317	14.942151	0.825792
-38.993681	1.367844	0.830797
-39.616902	4.964662	0.835802
-39.753442	6.200978	0.840806
-39.588011	1.198470	0.845811
-39.722748	9.341026	0.850816
-40.374231	1.884875	0.855821
-40.665925	0.206354	0.860826
-41.070410	3.781554	0.865830
-41.230398	-4.938020	0.870835
-42.140960	0.114863	0.875840
-42.113320	6.384331	0.880845
-42.359280	2.060055	0.885850
-42.369566	5.874048	0.890854
-42.195720	1.414390	0.895859
-42.484941	0.586537	0.900864
-43.107380	0.924544	0.905869
-43.239222	4.998030	0.910874
-44.040709	4.092254	0.915878
-43.213432	-0.504589	0.920883
-44.021212	3.453343	0.925888
-43.903004	5.358429	0.930893
-44.431530	1.306220	0.935898
-45.003536	8.055625	0.940902
-44.994216	4.194390	0.945907
-45.394834	11.638284	0.950912
-45.160492	-2.904315	0.955917
-45.756515	3.184460	0.960922
-46.615314	0.863965	0.965926
-46.267830	-6.128607	0.970931
-47.204049	5.663974	0.975936
-46.603676	6.262801	0.980941
-46.832587	5.824134	0.985946
-46.898772	3.872995	0.990950
-47.294444	-4.145257	0.995955
-48.252688	8.372117	1.000960
-48.083831	0.578622	1.005965
-48.456904	-2.862025	1.010970
-48.646702	7.291826	1.015974
-48.105391	4.153998	1.020979
-48.916113	13.392735	1.025984
-49.289884	10.493201	1.030989
-49.520962	0.664787	1.035994
-49.771220	5.598392	1.040998
-49.787633	0.001113	1.046003
-50.559030	2.469534	1.051008
-50.328954	8.030235	1.056013
-50.851806	-3.046444	1.061018
-51.364681	-3.396324	1.066022
-50.975898	-0.328237	1.071027
-51.671703	9.715074	1.076032
-52.256889	9.616971	1.081037
-52.518504	10.028157	1.086042
-52.438265	3.340049	1.091046
-52.223613	-1.015269	1.096051
-52.523244	7.637180	1.101056
-52.477702	-2.380109	1.106061
-53.161888	9.534336	1.111066
-53.620701	12.194228	1.116070
-53.750885	7.174762	1.121075
-54.146874	12.260918	1.126080
-53.979615	6.796210	1.131085
-55.047368	1.993255	1.136090
-55.371690	0.829215	1.141094
-55.453358	1.534910	1.146099
-55.945571	8.151590	1.151104
-55.480937	0.868574	1.156109
-55.344606	-6.669883	1.161114
-55.620395	1.504262	1.166118
-55.612404	6.520789	1.171123
-56.917282	1.900523	1.176128
-57.164784	-2.521587	1.181133
-57.207923	-3.147551	1.186138
-57.335191	10.460837	1.191142
-57.287241	2.059859	1.196147
-57.521984	-3.420950	1.201152
-58.010075	-0.746982	1.206157
-58.565696	5.490488	1.211162
-59.088460	12.516920	1.216166
-58.885007	-0.559174	1.221171
-58.744197	8.252055	1.226176
-58.749508	-3.459376	1.231181
-59.277985	5.127688	1.236186
-60.079692	10.372328	1.241190
-59.669987	-2.052706	1.246195
-60.309247	5.007795	1.251200
-60.702899	8.021310	1.256205
-61.155272	0.625714	1.261210
-61.629638	3.756281	1.266214
-61.947395	0.639163	1.271219
-62.299164	-0.523740	1.276224
-61.771701	3.794455	1.281229
-62.058224	2.776353	1.286234
-62.279502	1.267134	1.291238
-62.058450	7.256358	1.296243
-62.523309	9.825447	1.301248
-62.928850	8.095162	1.306253
-63.238951	-1.964478	1.311258
-63.301235	5.885147	1.316262
-63.260837	5.935797	1.321267
-64.401690	3.928419	1.326272
-64.535899	2.468834	1.331277
-64.821559	5.740676	1.336282
-65.136910	13.266123	1.341286
-64.961348	4.690123	1.346291
-64.855633	12.250833	1.351296
-65.392913	5.014074	1.356301
-65.909930	10.021116	1.361306
-66.159790	19.349147	1.366310
-65.804529	7.245851	1.371315
-66.679043	2.425275	1.376320
-67.206862	1.372215	1.381325
-67.560751	-3.681797	1.386330
-67.891096	11.745943	1.391334
-68.011685	0.641035	1.396339
-67.938294	3.989496	1.401344
-67.818335	-1.496271	1.406349
-67.647961	12.527391	1.411354
-68.280867	2.641717	1.416358
-68.764253	5.827481	1.421363
-69.022373	10.876215	1.426368
-69.029099	8.431702	1.431373
-69.452063	5.536714	1.436378
-69.958843	3.607156	1.441382
-70.366560	5.186521	1.446387
-70.616808	0.929358	1.451392
-70.676116	7.550972	1.456397
-70.783499	8.646677	1.461402
-70.978656	10.471149	1.466406
-70.583423	4.635361	1.471411
-71.685645	9.322808	1.476416
-71.919155	5.486968	1.481421
-72.130304	0.685837	1.486426
-72.469229	10.553005	1.491430
-72.526988	3.136706	1.496435
-73.448928	11.718987	1.501440
-73.463961	7.871059	1.506445
-73.591898	6.318741	1.511450
-73.849272	7.099424	1.516454
-73.591361	5.625853	1.521459
-74.214285	4.559222	1.526464
-73.807273	5.827428	1.531469
-74.598023	6.438584	1.536474
-75.299561	15.245761	1.541478
-75.191906	8.619796	1.546483
-75.325603	9.153308	1.551488
-75.391378	5.759424	1.556493
-75.483195	6.830543	1.561498
-76.265357	16.447625	1.566502
-76.322980	0.182224	1.571507
-76.381148	2.168729	1.576512
-76.559561	5.477551	1.581517
-76.690778	5.558255	1.586522
-77.550812	14.776247	1.591526
-78.039046	8.398677	1.596531
-77.877552	9.490217	1.601536
-77.938855	10.882425	1.606541
-78.295060	6.208426	1.611546
-78.497614	2.465813	1.616550
-78.969856	3.147286	1.621555
-79.117000	5.698230	1.626560
-79.297157	-4.657016	1.631565
-79.625603	4.009437	1.636570
-79.589770	11.467200	1.641574
-80.239802	4.596125	1.646579
-80.649611	9.975513	1.651584
-80.925350	14.043073	1.656589
-81.033253	17.692028	1.661594
-81.283914	15.576804	1.666598
-81.007564	6.377567	1.671603
-81.093433	12.503468	1.676608
-81.985036	8.109516	1.681613
-82.415914	9.303367	1.686618
-82.741278	9.028511	1.691622
-82.454418	13.121813	1.696627
-82.506569	12.728217	1.701632
-83.021821	12.581193	1.706637
-83.414615	3.246360	1.711642
-84.051244	7.560294	1.716646
-84.253694	6.408796	1.721651
-84.659138	5.004366	1.726656
-84.342915	5.704663	1.731661
-84.140879	4.205046	1.736666
-84.596842	10.749607	1.741670
-85.283876	2.416340	1.746675
-85.491230	5.929014	1.751680
-85.824884	2.725803	1.756685
-85.825688	2.593082	1.761690
-86.030486	8.715470	1.766694
-86.002310	1.886825	1.771699
-86.416747	9.896035	1.776704
-87.040960	-1.595031	1.781709
-87.056867	-2.620733	1.786714
-87.183043	10.342071	1.791718
-87.648858	3.359874	1.796723
-88.238939	7.691825	1.801728
-88.587649	0.292645	1.806733
-88.535502	7.507402	1.811738
-88.853921	3.656394	1.816742
-88.533222	7.832977	1.821747
-88.611604	5.209866	1.826752
-89.231453	5.382954	1.831757
-89.646292	0.053753	1.836762
-90.272130	13.926925	1.841766
-89.904848	9.436957	1.846771
-90.011578	15.040940	1.851776
-90.823615	8.597050	1.856781
-91.289701	7.752619	1.861786
-91.869128	8.814722	1.866790
-91.513499	10.467468	1.871795
-91.805821	12.772240	1.876800
-91.524408	18.938670	1.881805
-91.538627	9.389489	1.886810
-92.559631	16.386425	1.891814
-92.736236	8.387630	1.896819
-92.894721	16.913561	1.901824
-92.953650	17.641004	1.906829
-93.024051	10.214029	1.911834
-93.650373	14.567480	1.916838
-94.043175	7.649772	1.921843
-94.362865	11.293945	1.926848
-94.250250	2.876509	1.931853
-94.473533	3.949246	1.936858
-94.753347	10.200448	1.941862
-95.246098	9.942331	1.946867
-95.853510	13.381651	1.951872
-96.194020	5.266170	1.956877
-96.384109	0.221294	1.961882
-96.187690	11.646576	1.966886
-96.165723	0.288379	1.971891
-96.394867	3.007196	1.976896
-96.301773	-3.474112	1.981901
-96.890842	1.673932	1.986906
-97.417534	-1.252255	1.991910
-97.702896	-6.845352	1.996915
-97.738959	-1.612040	2.006912
-97.941265	6.953843	2.016909
-97.687999	7.607975	2.026906
-96.646073	1.188321	2.036902
-96.211427	0.939712	2.046899
-95.407687	4.469505	2.056896
-94.944154	4.865774	2.066893
-94.862322	6.725200	2.076890
-94.527221	14.015777	2.086886
-93.827065	14.485843	2.096883
-93.107076	3.640494	2.106880
-92.553929	1.776734	2.116877
-92.238149	1.115927	2.126874
-91.809947	7.761516	2.136870
-91.127089	-1.608140	2.146867
-91.079228	11.071564	2.156864
-90.061444	5.976675	2.166861
-89.510539	5.820724	2.176858
-89.363923	1.603613	2.186854
-88.656580	1.695582	2.196851
-88.414243	5.332350	2.206848
-87.601067	0.792215	2.216845
-86.903925	-1.680156	2.226842
-86.796630	10.036721	2.236838
-85.764359	10.160140	2.246835
-85.289252	10.434219	2.256832
-85.207102	8.013862	2.266829
-85.022771	11.485490	2.276826
-84.377665	13.453062	2.286822
-83.665204	11.934973	2.296819
-83.218333	15.428821	2.306816
-82.844237	19.507450	2.316813
-82.034654	13.181219	2.326810
-81.222253	12.822735	2.336806
-80.922716	10.751622	2.346803
-80.904953	7.175594	2.356800
-80.163193	10.227256	2.366797
-79.863825	11.073739	2.376794
-79.250949	11.601832	2.386790
-78.579578	11.547382	2.396787
-78.398314	14.937129	2.406784
-77.643520	15.135705	2.416781
-77.120223	10.130969	2.426778
-76.870713	9.331658	2.436774
-76.106206	10.947899	2.446771
-75.576351	7.440519	2.456768
-75.062554	7.059132	2.466765
-74.206843	4.973732	2.476762
-73.981555	-2.572419	2.486758
-73.906872	5.012387	2.496755
-73.459882	9.386872	2.506752
-72.788216	11.575198	2.516749
-71.940910	13.004236	2.526746
-71.549672	11.625180	2.536742
-71.458652	9.089391	2.546739
-70.535539	10.763144	2.556736
-70.331149	14.523071	2.566733
-69.236917	5.377225	2.576730
-68.663946	9.104741	2.586726
-68.675836	10.928168	2.596723
-68.481976	11.696148	2.606720
-67.565483	14.397315	2.616717
-66.899694	12.271982	2.626714
-67.077422	9.851163	2.636710
-66.061882	10.997246	2.646707
-65.613925	7.246105	2.656704
-65.145440	6.257259	2.666701
-64.365167	1.563889	2.676698
-64.205698	-1.689048	2.686694
-63.827821	2.848320	2.696691
-63.026745	5.317313	2.706688
-62.730739	5.423051	2.716685
-61.563293	1.790426	2.726682
-61.371459	2.327471	2.736678
-61.231876	8.780701	2.746675
-60.891955	5.904969	2.756672
-59.969588	6.381401	2.766669
-59.848934	-1.284572	2.776666
-59.054737	4.448359	2.786662
-58.262972	5.388751	2.796659
-58.355124	1.269241	2.806656
-57.837478	-4.143255	2.816653
-56.831702	-0.768660	2.826650
-56.566479	4.001773	2.836646
-56.060997	-4.351727	2.846643
-55.248145	-3.462156	2.856640
-55.169430	1.442038	2.866637
-54.736946	0.119877	2.876634
-54.223458	-1.899226	2.886630
-53.451257	-0.455252	2.896627
-52.832143	3.873257	2.906624
-52.401032	6.593457	2.916621
-52.408525	6.708736	2.926618
-51.504270	4.609397	2.936614
-50.920927	9.393343	2.946611
-51.004329	10.537389	2.956608
-50.099322	12.746177	2.966605
-49.727253	11.557027	2.976602
-48.612799	0.646704	2.986598
-48.157448	6.461241	2.996595
-48.098056	9.635665	3.006592
-48.026887	8.157873	3.016589
-47.117795	0.292331	3.026586
-46.889018	-3.643045	3.036582
-45.710452	9.122426	3.046579
-45.177092	4.784527	3.056576
-45.240171	5.231634	3.066573
-44.896708	4.778735	3.076570
-44.167149	2.218924	3.086566
-43.486157	4.646546	3.096563
-42.613552	6.429586	3.106560
-42.387233	9.996008	3.116557
-42.234085	9.968907	3.126554
-42.006020	3.816162	3.136550
-40.861915	5.870277	3.146547
-40.517558	10.732852	3.156544
-39.697185	12.391029	3.166541
-39.239570	11.999439	3.176538
-39.287174	7.698716	3.186534
-38.901709	7.039663	3.196531
-38.024388	9.528391	3.206528
-37.633268	4.867486	3.216525
-36.752718	4.346272	3.226522
-36.178910	10.459033	3.236518
-36.319528	2.285961	3.246515
-35.732698	6.632201	3.256512
-35.176449	9.415160	3.266509
-34.881272	11.478746	3.276506
-33.356091	8.917817	3.286502
-33.061764	0.442176	3.296499
-33.084204	10.256516	3.306496
-32.893471	5.535142	3.316493
-32.102916	3.523312	3.326490
-31.567244	6.879703	3.336486
-30.921535	12.078369	3.346483
-30.588632	5.297805	3.356480
-30.218365	9.934574	3.366477
-29.603599	6.565946	3.376474
-29.031647	7.410902	3.386470
-27.999766	8.281996	3.396467
-28.000955	8.462812	3.406464
-27.650675	4.961396	3.416461
-27.228725	0.552255	3.426458
-26.319265	4.819434	3.436454
-25.878327	0.036683	3.446451
-25.745563	8.793994	3.456448
-24.697594	-0.347766	3.466445
-24.394066	1.156974	3.476442
-24.241105	2.606110	3.486438
-23.408738	-2.184119	3.496435
-23.229425	7.361022	3.506432
-22.605408	4.437609	3.516429
-21.792097	1.253286	3.526426
-21.617947	4.153135	3.536422
-20.964964	0.239990	3.546419
-20.322510	3.212183	3.556416
-20.156732	5.457604	3.566413
-19.662736	10.382266	3.576410
-18.784109	1.837248	3.586406
-18.378147	1.083117	3.596403
-18.051588	6.604222	3.606400
-17.218212	5.434661	3.616397
-17.146814	10.181615	3.626394
-16.513545	10.494273	3.636390
-15.952508	12.836156	3.646387
-15.714121	5.649079	3.656384
-14.726244	7.445740	3.666381
-14.030034	4.564870	3.676378
-13.852241	0.624809	3.686374
-13.982340	6.185787	3.696371
-12.912972	12.163885	3.706368
-12.546095	11.403207	3.716365
-11.877557	6.733680	3.726362
-11.268638	8.513690	3.736358
-11.280767	-1.868484	3.746355
-10.281029	8.048628	3.756352
-9.837656	5.771246	3.766349
-9.901563	3.123515	3.776346
-8.908689	9.595108	3.786342
-7.956357	13.367729	3.796339
-8.017604	7.117760	3.806336
-7.794564	11.308760	3.816333
-6.980980	8.346142	3.826330
-6.669148	9.627835	3.836326
-5.542560	13.829321	3.846323
-5.484833	8.327324	3.856320
-5.298382	13.943245	3.866317
-4.479611	20.606848	3.876314
-4.134322	20.727042	3.886310
-3.948455	36.537143	3.896307
-3.224960	41.685620	3.906304
-2.643453	47.638800	3.916301
-2.284340	56.642609	3.926298
-1.986861	63.226347	3.936294
-1.096032	81.786592	3.946291
-1.087264	92.777695	3.956288
-0.531540	103.470861	3.966285
0.000000	116.087227	3.971290
0.203955	127.875251	3.976294
0.043475	122.218245	3.981299
0.235570	136.482223	3.986304
0.408306	143.545268	3.991309
0.808182	145.235393	3.996314
0.682278	149.605380	4.001318
0.864917	142.442422	4.006323
1.356076	150.186416	4.011328
1.125087	145.635126	4.016333
1.393116	143.008337	4.021338
1.265628	144.537477	4.026342
0.807778	130.210790	4.031347
0.604791	132.530053	4.036352
0.571515	130.820519	4.041357
1.139310	146.443022	4.046362
0.839971	152.203782	4.051366
0.968714	147.687878	4.056371
1.160966	144.902116	4.061376
1.215923	150.411208	4.066381
1.082157	146.255979	4.071386
0.831111	154.783828	4.076390
1.209685	143.072260	4.081395
1.014300	149.715251	4.086400
0.956027	148.215279	4.091405
1.378584	141.669638	4.096410
0.875538	145.418498	4.101414
1.271931	139.914683	4.106419
1.405255	148.768289	4.111424
1.162741	132.076139	4.116429
0.734951	128.226414	4.121434
0.989930	138.823190	4.126438
1.226538	137.666164	4.131443
1.150977	147.568078	4.136448
1.024006	146.559768	4.141453
1.185836	146.252866	4.146458
0.875302	151.873009	4.151462
0.767643	145.717330	4.156467
1.042294	151.302734	4.161472
1.160030	153.350282	4.166477
1.262577	151.657431	4.171482
1.335012	155.898265	4.176486
1.117117	146.618201	4.181491
1.207531	147.948682	4.186496
1.084699	150.464200	4.191501
1.575792	139.674653	4.196506
1.335167	146.884725	4.201510
1.063158	143.905944	4.206515
1.015963	150.506735	4.211520
1.271228	147.872453	4.216525
1.111153	149.770536	4.221530
1.445930	158.061064	4.226534
1.579213	157.341012	4.231539
1.614694	159.097724	4.236544
1.229073	157.171306	4.241549
1.380705	149.364624	4.246554
1.527853	175.847958	4.251558
1.702123	160.318036	4.256563
1.340268	162.358469	4.261568
1.324057	149.693171	4.266573
1.691641	157.174952	4.271578
1.687707	160.513414	4.276582
1.404610	149.237712	4.281587
1.266735	148.152016	4.286592
1.581281	165.146175	4.291597
1.862647	164.814216	4.296602
1.300518	160.982369	4.301606
1.616918	162.467271	4.306611
1.576253	170.386353	4.311616
1.889491	169.182516	4.316621
1.984441	159.938851	4.321626
1.447178	153.581557	4.326630
1.686085	152.762697	4.331635
1.168809	162.224456	4.336640
1.466143	163.645906	4.341645
1.655375	169.905934	4.346650
1.727752	183.062392	4.351654
1.617199	176.685690	4.356659
1.735304	172.630199	4.361664
1.690214	173.519997	4.366669
1.909906	169.717514	4.371674
1.734150	179.157409	4.376678
2.091775	177.161994	4.381683
2.100817	176.005819	4.386688
1.849776	170.571798	4.391693
1.827079	169.376304	4.396698
1.986393	170.670681	4.401702
1.860089	161.246543	4.406707
1.650255	161.592668	4.411712
1.767967	172.701361	4.416717
2.017810	175.547639	4.421722
2.056396	178.607355	4.426726
1.970096	162.776566	4.431731
1.763401	168.003951	4.436736
1.853156	172.583767	4.441741
2.083674	169.874264	4.446746
1.848584	182.107608	4.451750
1.790992	172.166488	4.456755
1.786521	182.370500	4.461760
1.769802	172.869073	4.466765
2.042427	169.849248	4.471770
1.746112	181.361344	4.476774
2.077279	173.055114	4.481779
1.879217	178.183072	4.486784
1.645798	184.499836	4.491789
1.995270	173.273706	4.496794
1.814237	176.959463	4.501798
1.620082	173.629952	4.506803
1.824965	174.553352	4.511808
2.129526	189.631833	4.516813
2.422079	189.244335	4.521818
2.323761	189.082599	4.526822
1.970635	176.023972	4.531827
1.992242	172.913760	4.536832
2.087454	198.766177	4.541837
2.309427	194.264128	4.546842
2.043503	202.072982	4.551846
2.228223	195.042557	4.556851
2.487161	200.728517	4.561856
2.328030	204.600677	4.566861
2.589658	194.606365	4.571866
2.260132	187.349626	4.576870
2.430014	179.309113	4.581875
2.056397	176.545568	4.586880
1.923291	179.224053	4.591885
2.406106	180.701866	4.596890
2.303854	181.970787	4.601894
2.365873	192.667432	4.606899
2.408868	198.925073	4.611904
2.541711	204.235314	4.616909
2.716705	193.052328	4.621914
2.544876	196.999244	4.626918
2.239007	180.839003	4.631923
2.117658	170.088448	4.636928
1.987777	180.049512	4.641933
2.376189	191.584047	4.646938
2.055069	200.347527	4.651942
2.422153	194.025698	4.656947
2.541860	202.432203	4.661952
2.273031	208.112269	4.666957
2.815561	201.959104	4.671962
2.583228	211.252854	4.676966
2.873742	200.352327	4.681971
2.704298	198.455310	4.686976
2.368464	204.671066	4.691981
2.722962	199.490179	4.696986
2.161144	201.897312	4.701990
2.563076	203.988924	4.706995
2.362605	197.838278	4.712000
2.382218	191.849307	4.717005
2.679579	196.868008	4.722010
2.538658	197.794970	4.727014
2.507715	195.066317	4.732019
2.494915	194.248927	4.737024
2.500330	194.766975	4.742029
2.531670	195.151245	4.747034
2.306902	197.467602	4.752038
2.841406	208.226271	4.757043
2.850882	212.426362	4.762048
2.604999	214.056317	4.767053
2.918695	205.502868	4.772058
2.449193	205.244262	4.777062
2.881452	207.840497	4.782067
3.033576	216.219783	4.787072
2.755960	213.719606	4.792077
2.756491	205.338613	4.797082
2.917365	210.808982	4.802086
3.210326	212.395640	4.807091
2.737217	205.616979	4.812096
2.726674	210.800989	4.817101
2.931793	204.172332	4.822106
2.587681	208.491100	4.827110
2.964363	213.873872	4.832115
2.910170	223.313727	4.837120
2.923543	222.508054	4.842125
2.919310	219.575892	4.847130
3.196513	226.287238	4.852134
3.187036	211.956672	4.857139
2.809681	208.298348	4.862144
2.886890	211.146370	4.867149
3.275616	216.691773	4.872154
3.084024	211.881189	4.877158
3.058058	203.276554	4.882163
2.780251	198.583886	4.887168
2.741721	212.532877	4.892173
3.080972	217.674738	4.897178
3.029351	231.410655	4.902182
3.213285	216.081654	4.907187
3.171262	226.930666	4.912192
2.995237	221.886680	4.917197
3.134603	223.165204	4.922202
2.710517	221.554860	4.927206
2.759932	213.254791	4.932211
3.004869	222.052980	4.937216
2.959977	227.267687	4.942221
3.357757	223.073450	4.947226
3.220440	231.169056	4.952230
3.172004	232.739603	4.957235
2.969256	231.572315	4.962240
3.147005	222.606715	4.967245
3.255729	226.800751	4.972250
3.094792	230.850373	4.977254
3.344313	223.613627	4.982259
3.340675	230.865696	4.987264
2.942655	231.627294	4.992269
3.067344	223.634972	4.997274
3.580929	241.471232	5.002278
3.433927	239.108777	5.007283
3.256448	234.182077	5.012288
3.212767	238.475926	5.017293
3.736678	240.599052	5.022298
3.579297	239.680925	5.027302
3.199033	230.464223	5.032307
3.357343	234.840320	5.037312
3.261768	245.071298	5.042317
3.730238	246.060972	5.047322
3.336741	243.784595	5.052326
3.449871	242.172336	5.057331
3.121781	240.407742	5.062336
3.483262	257.957796	5.067341
3.586163	248.048437	5.072346
3.494354	252.033448	5.077350
3.239750	251.361512	5.082355
3.746878	253.575856	5.087360
3.851933	260.817235	5.092365
3.859387	262.622641	5.097370
3.555318	260.882755	5.102374
3.868526	252.664725	5.107379
3.523188	241.835325	5.112384
3.555159	245.677551	5.117389
3.566320	247.580454	5.122394
3.780169	252.678696	5.127398
3.610502	244.359154	5.132403
3.355187	245.107884	5.137408
3.597458	255.592824	5.142413
3.570624	252.800242	5.147418
3.242800	255.654783	5.152422
3.518772	249.163709	5.157427
3.834678	249.281926	5.162432
3.434247	256.795496	5.167437
3.530654	246.570773	5.172442
3.553855	256.150383	5.177446
3.574594	249.411390	5.182451
3.667769	248.011070	5.187456
3.321192	249.745392	5.192461
3.734884	254.071990	5.197466
4.133405	266.854699	5.202470
4.038387	263.095177	5.207475
3.958350	260.488104	5.212480
3.731476	255.857046	5.217485
3.871319	253.819812	5.222490
3.785671	265.226187	5.227494
3.996670	261.861654	5.232499
4.141402	275.797799	5.237504
3.895696	268.917045	5.242509
3.676713	263.095150	5.247514
3.767423	278.855797	5.252518
4.186965	272.557358	5.257523
4.428659	270.247895	5.262528
4.005036	270.924919	5.267533
3.920370	258.694221	5.272538
3.608960	262.194775	5.277542
4.151895	270.259748	5.282547
4.369996	279.087481	5.287552
3.936884	268.486956	5.292557
4.377088	268.288299	5.297562
4.295635	270.015886	5.302566
4.096080	263.748012	5.307571
3.873321	253.889674	5.312576
3.307633	260.166774	5.317581
4.249621	268.387525	5.322586
4.293155	272.708847	5.327590
4.396907	274.189112	5.332595
4.337666	277.628012	5.337600
4.288572	279.872561	5.342605
4.257745	270.474535	5.347610
3.954297	268.563704	5.352614
3.992168	273.695853	5.357619
3.902557	268.565547	5.362624
4.004201	274.260356	5.367629
4.351503	273.389705	5.372634
3.958654	275.609017	5.377638
4.287176	276.462429	5.382643
4.200025	275.422562	5.387648
4.077194	276.432117	5.392653
4.361922	270.885646	5.397658
4.147198	279.075661	5.402662
4.469335	285.191517	5.407667
4.278349	282.598661	5.412672
4.078803	286.398075	5.417677
4.680587	281.488475	5.422682
4.275792	278.413415	5.427686
4.331752	280.843989	5.432691
4.367529	277.718883	5.437696
4.190561	276.060323	5.442701
4.552686	277.734229	5.447706
4.246582	290.576736	5.452710
4.632853	287.089821	5.457715
4.528580	286.176025	5.462720
4.310605	283.055875	5.467725
4.599700	291.951586	5.472730
4.439652	289.714558	5.477734
4.336056	293.239506	5.482739
4.624408	298.041343	5.487744
4.311064	307.338345	5.492749
4.593356	301.086712	5.497754
4.262370	310.905348	5.502758
4.398705	301.294448	5.507763
4.752889	299.536846	5.512768
4.864392	298.605060	5.517773
4.904658	303.882378	5.522778
4.482736	310.383749	5.527782
4.623210	301.079093	5.532787
4.743512	306.154042	5.537792
4.301250	300.332317	5.542797
4.353450	295.046903	5.547802
4.122651	311.996931	5.552806
4.343123	312.864111	5.557811
4.380330	314.174467	5.562816
4.294385	312.653507	5.567821
4.614656	317.994528	5.572826
4.681644	327.124378	5.577830
4.825719	324.994722	5.582835
4.822931	330.974838	5.587840
4.928327	326.377124	5.592845
5.006326	325.716348	5.597850
4.966726	325.709929	5.602854
4.767625	320.894164	5.607859
4.852387	321.083400	5.612864
4.844089	328.427990	5.617869
4.875738	318.539247	5.622874
4.877387	324.657874	5.627878
4.872109	328.967875	5.632883
4.918977	329.624968	5.637888
4.588637	334.931888	5.642893
4.832295	329.126072	5.647898
4.869956	329.743478	5.652902
5.113962	323.026425	5.657907
5.332320	316.750002	5.662912
4.934623	325.870400	5.667917
5.090417	329.272454	5.672922
4.847771	325.925201	5.677926
5.108579	325.947646	5.682931
4.631353	317.736371	5.687936
4.729587	318.663833	5.692941
4.969831	331.060090	5.697946
4.560145	324.676418	5.702950
4.601232	321.015784	5.707955
4.978596	337.275748	5.712960
5.113653	355.329623	5.717965
5.383976	351.772275	5.722970
5.154234	349.438588	5.727974
4.989906	355.760406	5.732979
5.535500	348.217786	5.737984
5.086508	345.551446	5.742989
5.415351	342.763235	5.747994
5.273696	350.733022	5.752998
5.171814	343.747444	5.758003
5.387403	336.142636	5.763008
5.114855	334.230121	5.768013
5.310040	333.098556	5.773018
5.363932	340.952276	5.778022
4.998304	345.805972	5.783027
5.577955	348.901168	5.788032
5.339158	345.793760	5.793037
5.606552	334.146944	5.798042
5.076110	340.522956	5.803046
5.028149	332.130518	5.808051
5.059226	343.341479	5.813056
5.350500	341.229888	5.818061
5.800071	354.491893	5.823066
5.218970	357.895512	5.828070
5.432958	361.215686	5.833075
5.805184	351.703845	5.838080
5.604650	357.477665	5.843085
5.760362	347.310033	5.848090
5.425777	341.575829	5.853094
5.301873	331.426707	5.858099
5.538808	324.903755	5.863104
5.215404	333.933420	5.868109
5.547175	336.447340	5.873114
5.478416	351.840721	5.878118
6.089854	361.321894	5.883123
5.618273	338.597196	5.888128
5.616958	337.341390	5.893133
5.503550	328.943389	5.898138
5.373479	326.192282	5.903142
5.339859	326.026734	5.908147
5.362119	330.408353	5.913152
5.469856	343.018373	5.918157
5.844636	346.639226	5.923162
5.552333	347.969575	5.928166
5.853252	347.169465	5.933171
5.691125	348.229474	5.938176
5.526886	356.946303	5.943181
5.731118	350.596149	5.948186
5.555508	347.722457	5.953190
5.269328	344.103604	5.958195
5.408920	352.658928	5.963200
5.250896	350.019768	5.968205
5.597488	348.212728	5.973210
5.814321	358.505556	5.978214
5.624922	355.099334	5.983219
5.468469	347.815412	5.988224
5.481126	353.805770	5.993229
5.945271	369.036574	5.998234
5.731167	379.846200	6.003238
5.832638	371.082308	6.008243
6.024658	360.833047	6.013248
5.873726	357.313227	6.018253
5.865326	351.341246	6.023258
5.542368	344.026465	6.028262
5.569184	343.803991	6.033267
5.751281	355.114687	6.038272
5.483430	364.622895	6.043277
6.218703	379.004447	6.048282
6.068377	371.697409	6.053286
5.774094	355.744007	6.058291
5.657024	354.885998	6.063296
5.537404	345.394275	6.068301
5.702158	344.824312	6.073306
5.976997	341.250440	6.078310
5.918433	345.910488	6.083315
5.994874	354.159324	6.088320
5.816421	360.619402	6.093325
6.122555	353.680626	6.098330
5.750854	351.793136	6.103334
5.924901	354.312788	6.108339
5.647213	347.013059	6.113344
5.844302	350.658591	6.118349
6.046011	345.492109	6.123354
5.865615	346.181648	6.128358
6.040577	349.659799	6.133363
6.267394	354.148581	6.138368
5.884395	354.040938	6.143373
5.965252	345.947859	6.148378
5.306169	334.503154	6.153382
5.490174	342.640216	6.158387
5.816387	345.971278	6.163392
5.461487	355.116624	6.168397
5.726560	349.187220	6.173402
5.699065	352.222517	6.178406
5.436087	349.194829	6.183411
5.621517	352.551114	6.188416
5.797564	355.361526	6.193421
5.820021	349.264486	6.198426
5.543403	349.912152	6.203430
5.719184	350.893906	6.208435
5.702422	354.351476	6.213440
5.494268	351.115877	6.218445
5.621106	344.192541	6.223450
5.822547	354.797834	6.228454
5.662158	347.017807	6.233459
5.621766	347.305749	6.238464
5.640630	362.985975	6.243469
6.069290	349.833205	6.248474
5.596609	362.141863	6.253478
5.779300	351.020850	6.258483
5.843771	357.888966	6.263488
5.541876	350.507605	6.268493
5.665397	348.071111	6.273498
5.800795	356.430937	6.278502
5.603672	356.882645	6.283507
5.856792	357.475785	6.288512
5.613271	356.735668	6.293517
5.806472	347.555607	6.298522
5.531065	345.137325	6.303526
5.899871	370.576955	6.308531
5.729585	369.714627	6.313536
5.747201	373.084555	6.318541
5.790058	362.880811	6.323546
5.727995	379.260285	6.328550
5.896031	375.991049	6.333555
5.953172	356.103715	6.338560
5.808278	359.391531	6.343565
5.756837	353.881887	6.348570
5.737687	359.326723	6.353574
5.795465	354.473864	6.358579
5.617663	357.485254	6.363584
5.409226	363.399523	6.368589
6.064495	363.113383	6.373594
5.767982	356.553775	6.378598
5.730467	357.097537	6.383603
5.612139	355.537353	6.388608
5.738927	360.086104	6.393613
5.933848	363.345989	6.398618
5.814059	353.977677	6.403622
5.395765	368.239398	6.408627
5.972733	360.609597	6.413632
5.866526	366.995081	6.418637
5.980488	354.923026	6.423642
6.104741	363.256127	6.428646
5.863474	356.289219	6.433651
6.119511	355.125972	6.438656
5.846550	360.689671	6.443661
5.728876	342.155392	6.448666
5.706160	358.379981	6.453670
5.674842	353.825828	6.458675
5.381747	354.381160	6.463680
5.428022	357.942752	6.468685
5.971021	355.162115	6.473690
5.593091	352.642832	6.478694
6.033482	354.652505	6.483699
6.098598	358.514874	6.488704
5.939036	353.800475	6.493709
5.775120	355.863701	6.498714
5.699234	356.970311	6.503718
5.543018	351.787140	6.508723
5.606034	359.848252	6.513728
5.677892	356.663694	6.518733
5.864670	357.969602	6.523738
5.860708	361.577031	6.528742
6.065185	349.588877	6.533747
5.892894	345.439638	6.538752
5.783684	358.903095	6.543757
6.165427	351.389310	6.548762
6.173648	357.241155	6.553766
6.160124	361.732795	6.558771
6.239974	353.722129	6.563776
5.647924	344.687251	6.568781
5.718632	334.358934	6.573786
5.859249	333.998403	6.578790
5.629349	331.550846	6.583795
5.753186	326.336458	6.588800
5.462908	335.205906	6.593805
5.699964	339.816471	6.598810
5.843867	342.967284	6.603814
5.594847	348.289941	6.608819
5.933009	343.817108	6.613824
5.863224	360.618565	6.618829
5.785178	341.581354	6.623834
5.696810	339.541902	6.628838
5.675221	342.781921	6.633843
5.409354	349.610040	6.638848
5.416946	350.067639	6.643853
5.764584	355.825174	6.648858
5.774311	358.449669	6.653862
5.923307	356.996300	6.658867
5.839738	356.515866	6.663872
5.640189	367.614277	6.668877
5.581649	361.710263	6.673882
5.943790	364.858524	6.678886
6.122851	359.496265	6.683891
6.055168	352.780580	6.688896
5.624453	349.396349	6.693901
5.809472	340.056218	6.698906
5.856967	349.761789	6.703910
5.708135	345.045711	6.708915
5.752569	334.908177	6.713920
5.545909	342.631874	6.718925
5.847178	354.651580	6.723930
5.455046	364.872142	6.728934
5.585894	360.656420	6.733939
5.790928	357.210543	6.738944
5.656287	353.941278	6.743949
5.781209	350.419367	6.748954
5.884394	352.605264	6.753958
5.969113	355.458460	6.758963
6.130830	361.608968	6.763968
5.943181	350.621913	6.768973
5.638583	344.139508	6.773978
5.527154	336.291701	6.778982
5.508658	353.303420	6.783987
5.806761	352.769514	6.788992
5.842565	357.531841	6.793997
6.110744	358.049854	6.799002
5.782335	354.554677	6.804006
5.351202	342.564873	6.809011
5.667030	353.361057	6.814016
5.664279	365.491681	6.819021
5.891173	361.241927	6.824026
6.018902	365.841154	6.829030
5.828102	351.931202	6.834035
5.855804	350.794239	6.839040
5.691638	344.343617	6.844045
5.789605	347.308634	6.849050
5.650081	348.441034	6.854054
5.679789	345.867374	6.859059
6.329929	352.406437	6.864064
5.316255	358.522802	6.869069
5.845851	336.840336	6.874074
5.761570	354.950723	6.879078
5.693842	347.896515	6.884083
5.697814	345.507227	6.889088
5.749509	361.834059	6.894093
6.025436	354.153349	6.899098
6.072074	345.186084	6.904102
5.581645	339.128277	6.909107
5.472062	337.028872	6.914112
5.798844	343.299049	6.919117
5.728006	346.328480	6.924122
5.777661	345.703784	6.929126
5.864601	341.324098	6.934131
5.420028	334.971199	6.939136
5.702732	355.792444	6.944141
5.955578	361.226302	6.949146
6.010603	348.575011	6.954150
5.719201	348.104995	6.959155
5.921783	338.831718	6.964160
5.638646	348.010109	6.969165
5.436325	332.035993	6.974170
5.327903	350.146994	6.979174
5.670543	358.176948	6.984179
5.724813	356.906105	6.989184
5.922041	367.569015	6.994189
5.595932	361.191218	6.999194
5.742011	365.142145	7.004198
5.450409	360.565495	7.009203
5.486568	358.177490	7.014208
5.714884	366.535417	7.019213
5.788001	357.184336	7.024218
5.800270	361.804816	7.029222
5.582600	357.216582	7.034227
5.605001	359.598639	7.039232
5.451558	361.530508	7.044237
5.565405	367.713830	7.049242
5.517687	361.197499	7.054246
5.486493	366.694845	7.059251
5.844301	366.062996	7.064256
5.995065	366.222909	7.069261
6.193520	368.422354	7.074266
5.897356	366.102236	7.079270
6.045304	363.952986	7.084275
5.914108	364.308941	7.089280
5.819986	363.260669	7.094285
5.861818	357.682624	7.099290
6.115865	358.569857	7.104294
6.054445	362.502674	7.109299
6.173558	357.940768	7.114304
5.856843	356.164888	7.119309
6.185723	350.728537	7.124314
5.932339	346.107936	7.129318
5.629554	334.926953	7.134323
5.979522	341.392817	7.139328
5.497884	337.709675	7.144333
5.778423	335.394117	7.149338
5.608577	342.881087	7.154342
5.803465	340.626406	7.159347
5.947368	333.048651	7.164352
5.549932	335.208576	7.169357
5.559171	338.165347	7.174362
5.461519	344.821572	7.179366
5.761619	353.598528	7.184371
6.002026	353.867785	7.189376
5.319642	361.770434	7.194381
5.541516	362.839882	7.199386
5.792543	368.261372	7.204390
5.915687	369.156460	7.209395
5.244911	362.427693	7.214400
5.573602	363.591140	7.219405
5.550639	367.647650	7.224410
5.639734	361.318696	7.229414
5.567609	367.993077	7.234419
5.499473	358.537574	7.239424
5.562055	365.105424	7.244429
5.561241	363.061742	7.249434
5.620630	370.436874	7.254438
5.560901	369.487620	7.259443
5.788673	372.280439	7.264448
5.470345	378.237241	7.269453
5.675289	382.909797	7.274458
5.772293	392.949329	7.279462
5.900010	395.213646	7.284467
6.019178	391.183250	7.289472
5.604028	388.856461	7.294477
6.039563	380.622371	7.299482
5.638132	372.959195	7.304486
5.694595	377.389251	7.309491
6.073019	378.013381	7.314496
5.556679	375.281657	7.319501
5.731586	365.566601	7.324506
5.775707	377.512714	7.329510
5.796621	372.355570	7.334515
5.983630	370.624154	7.339520
5.519788	369.330081	7.344525
5.814010	361.538931	7.349530
5.860587	367.713810	7.354534
5.582519	369.975263	7.359539
5.941182	367.846782	7.364544
5.653909	367.701994	7.369549
5.735293	357.052443	7.374554
5.719775	363.816032	7.379558
5.866764	370.022637	7.384563
5.734518	364.968588	7.389568
5.559354	366.995612	7.394573
5.871157	369.961931	7.399578
6.068085	376.505572	7.404582
5.930662	369.357869	7.409587
6.064053	368.856097	7.414592
5.557395	363.712011	7.419597
5.872164	366.968938	7.424602
6.001316	368.078225	7.429606
5.698779	368.419896	7.434611
5.658153	359.089799	7.439616
5.644781	372.076329	7.444621
5.783452	362.730794	7.449626
5.952536	360.799701	7.454630
5.735083	370.581598	7.459635
5.822977	366.654186	7.464640
6.122702	367.385562	7.469645
6.155699	364.241893	7.474650
5.900576	368.249355	7.479654
5.792932	370.212015	7.484659
5.967309	367.780205	7.489664
5.922671	367.119661	7.494669
6.267438	367.034035	7.499674
5.492765	355.439744	7.504678
5.912261	362.331332	7.509683
5.952241	355.949962	7.514688
5.444053	349.575387	7.519693
5.820946	358.409917	7.524698
5.816560	363.725888	7.529702
5.710112	361.151413	7.534707
5.535332	363.482105	7.539712
5.484274	365.147989	7.544717
5.888450	361.262775	7.549722
5.691906	362.274392	7.554726
5.602660	363.920948	7.559731
5.718358	352.668058	7.564736
5.774457	351.817719	7.569741
5.889096	357.061253	7.574746
5.745416	359.637015	7.579750
5.902883	363.772825	7.584755
5.915815	356.338970	7.589760
5.786858	365.091406	7.594765
5.969095	356.381307	7.599770
5.864740	360.564466	7.604774
5.780637	356.860163	7.609779
5.749846	339.451256	7.614784
5.496032	344.274777	7.619789
5.822880	356.850476	7.624794
5.600809	367.284845	7.629798
5.709283	368.764378	7.634803
5.907265	361.396443	7.639808
5.785670	363.579593	7.644813
5.865810	357.134982	7.649818
5.855047	359.753195	7.654822
5.971107	363.870182	7.659827
5.616624	343.212102	7.664832
5.357372	345.821789	7.669837
5.949026	354.742895	7.674842
5.627151	357.492113	7.679846
5.808456	365.452435	7.684851
6.216684	356.039357	7.689856
5.788153	351.933428	7.694861
5.726747	340.819028	7.699866
5.763170	346.274136	7.704870
5.520559	338.133662	7.709875
5.488243	340.511635	7.714880
5.649587	357.492016	7.719885
5.947322	360.055566	7.724890
5.641638	366.475467	7.729894
5.987616	361.821066	7.734899
5.888999	363.326718	7.739904
5.673801	364.091315	7.744909
5.813230	353.445327	7.749914
5.846935	357.255668	7.754918
5.628742	359.719715	7.759923
5.632530	358.985142	7.764928
5.556613	363.587801	7.769933
6.101992	357.551199	7.774938
5.944856	359.141951	7.779942
5.700690	344.670876	7.784947
5.810265	333.861894	7.789952
5.579671	349.540064	7.794957
5.891706	354.404647	7.799962
5.597368	355.083564	7.804966
5.985094	356.202958	7.809971
5.849669	349.994610	7.814976
5.523671	350.264024	7.819981
5.695745	352.651104	7.824986
5.763354	351.311731	7.829990
5.701558	358.357823	7.834995
6.049296	363.273763	7.840000
5.615397	353.597152	7.845005
5.626917	348.343408	7.850010
5.915170	357.853068	7.855014
5.567581	360.103266	7.860019
6.035642	353.553582	7.865024
5.839079	351.812662	7.870029
5.725999	341.687148	7.875034
5.876446	333.250967	7.880038
5.761076	339.723300	7.885043
6.085184	332.028723	7.890048
5.618774	336.515383	7.895053
5.784857	330.069971	7.900058
5.656445	334.943445	7.905062
5.216035	334.427172	7.910067
5.393072	340.837871	7.915072
5.630239	355.310104	7.920077
5.712899	354.126564	7.925082
5.701037	355.723029	7.930086
5.865905	368.232364	7.935091
5.530497	359.638172	7.940096
5.434080	359.748225	7.945101
5.739502	358.738596	7.950106
5.879696	365.446150	7.955110
5.225237	366.640249	7.960115
5.660259	359.858451	7.965120
5.716891	366.955595	7.970125
5.578716	366.956211	7.975142
5.667949	370.830171	7.980160
5.535677	363.734666	7.985178
5.994542	360.150431	7.990195
5.685051	368.665884	7.995213
5.707063	355.228357	8.000230
5.865578	358.596004	8.005248
5.918573	369.664484	8.010266
6.038307	363.050196	8.015283
5.876339	359.481184	8.020301
6.002283	354.361761	8.025318
5.737298	361.835146	8.030336
5.704490	372.421616	8.035354
6.067556	367.798362	8.040371
5.753194	368.504048	8.045389
6.172494	367.639974	8.050406
5.753758	367.333233	8.055424
5.892406	374.260548	8.060442
5.733779	365.509236	8.065459
5.809672	361.173973	8.070477
5.818398	365.533911	8.075494
5.688962	355.761871	8.080512
5.794620	359.320834	8.085530
5.734213	358.538233	8.090547
5.866879	363.945401	8.095565
6.135112	356.995428	8.100582
5.743135	355.611533	8.105600
5.679325	359.493691	8.110618
5.849214	359.590179	8.115635
6.192715	361.136365	8.120653
6.030924	362.992093	8.125670
6.038529	356.963415	8.130688
6.130642	368.136217	8.135706
6.333368	364.844574	8.140723
6.160825	361.236194	8.145741
6.138960	362.565075	8.150758
6.085499	366.937913	8.155776
5.679795	368.393205	8.160794
5.816382	354.615839	8.165811
5.891353	361.329067	8.170829
5.705068	366.369648	8.175846
5.787678	360.587990	8.180864
5.659108	364.496074	8.185882
5.878796	354.890238	8.190899
5.721165	366.834307	8.195917
5.630318	358.867632	8.200934
5.951740	367.113821	8.205952
6.173959	386.480721	8.210970
6.325601	369.775582	8.215987
5.897708	365.736999	8.221005
5.626910	360.436742	8.226022
5.808368	367.789688	8.231040
6.136800	391.980905	8.236058
6.300228	387.448885	8.241075
6.331751	390.735450	8.246093
5.953922	379.247706	8.251110
5.939801	363.802451	8.256128
5.825318	374.638402	8.261146
6.189182	379.122579	8.266163
6.000365	394.577616	8.271181
5.781884	390.379986	8.276198
6.124420	389.360682	8.281216
5.783440	397.070049	8.286234
5.882860	390.629346	8.291251
6.182518	396.815082	8.296269
5.902686	385.394030	8.301286
6.204642	393.832628	8.306304
5.942063	389.859656	8.311322
5.901514	387.458185	8.316339
6.336524	396.270408	8.321357
6.150170	387.106867	8.326374
6.423227	385.492541	8.331392
5.919015	395.177750	8.336410
6.210505	396.722622	8.341427
6.095801	393.231404	8.346445
5.996753	390.106959	8.351462
5.819040	386.777091	8.356480
5.758700	392.495373	8.361498
6.352112	388.441931	8.366515
6.128904	396.906010	8.371533
6.379325	385.982539	8.376550
6.367402	392.898740	8.381568
6.164902	395.691803	8.386586
6.283854	393.426286	8.391603
5.939899	395.739744	8.396621
5.856294	396.617557	8.401638
6.097250	398.201904	8.406656
5.924336	402.612401	8.411674
6.106871	395.398132	8.416691
6.191507	395.839335	8.421709
6.586259	401.262254	8.426726
6.327178	396.499789	8.431744
6.099566	396.863684	8.436762
6.201093	397.340109	8.441779
5.955634	395.513536	8.446797
5.677566	413.743878	8.451814
6.305890	406.431355	8.456832
6.094200	421.826884	8.461850
6.776913	422.392129	8.466867
6.557899	424.395683	8.471885
6.672901	421.038881	8.476902
6.393623	406.370431	8.481920
6.334024	394.551953	8.486938
6.093819	398.913032	8.491955
5.975297	399.632217	8.496973
5.873791	408.916669	8.501990
6.316256	416.086730	8.507008
6.545644	413.412590	8.512026
6.409411	422.585726	8.517043
6.703902	420.056018	8.522061
6.157071	406.672866	8.527078
6.394601	403.552488	8.532096
6.610650	418.350825	8.537114
6.525978	410.660868	8.542131
6.169904	395.045104	8.547149
6.110483	398.068211	8.552166
6.351882	403.262697	8.557184
6.328617	417.237002	8.562202
6.188646	407.772696	8.567219
6.214675	414.982758	8.572237
6.088597	422.895148	8.577255
6.202566	412.614729	8.582272
6.308759	422.810223	8.587290
6.158563	412.820501	8.592307
5.913240	431.269790	8.597325
6.081341	424.240806	8.602343
6.055949	418.709578	8.607360
5.889749	425.318608	8.612378
6.509373	443.326277	8.617395
6.293677	442.760506	8.622413
6.388359	447.510936	8.627431
6.457658	444.593633	8.632448
6.735497	446.686599	8.637466
6.823290	448.519009	8.642483
6.717147	446.099406	8.647501
6.761392	457.544849	8.652519
6.897083	436.354620	8.657536
6.118178	425.646050	8.662554
6.256521	420.556223	8.667571
6.544224	439.736197	8.672589
6.830611	449.133462	8.677607
6.637797	433.624628	8.682624
6.420638	425.068648	8.687642
6.263721	426.595417	8.692659
6.490605	425.717307	8.697677
6.347892	436.718663	8.702695
6.672459	438.463482	8.707712
6.587182	442.472096	8.712730
6.647323	440.105335	8.717747
6.765930	455.651112	8.722765
6.288035	443.522602	8.727783
6.520428	438.904025	8.732800
6.571235	448.997760	8.737818
6.500250	452.246749	8.742835
6.635207	449.221328	8.747853
6.493059	457.382402	8.752871
6.561546	450.738242	8.757888
6.564912	440.986374	8.762906
6.259508	445.392394	8.767923
6.742956	438.023663	8.772941
6.700894	446.569836	8.777959
6.823103	447.421716	8.782976
6.731418	447.120535	8.787994
6.561684	449.880070	8.793011
6.899796	435.878563	8.798029
6.699750	443.610048	8.803047
6.764361	438.938865	8.808064
6.991924	437.988065	8.813082
6.758902	427.339130	8.818099
6.467903	422.840432	8.823117
6.718058	423.151561	8.828135
6.847472	434.208107	8.833152
6.866112	427.514962	8.838170
6.384164	420.281719	8.843187
6.570099	423.818650	8.848205
6.806770	437.398796	8.853223
6.895152	433.345579	8.858240
6.580374	446.652375	8.863258
6.511450	434.434547	8.868275
6.916553	438.423131	8.873293
6.844472	435.515358	8.878311
6.793673	442.485006	8.883328
6.989928	443.148560	8.888346
6.774661	440.439945	8.893363
7.011035	432.355696	8.898381
6.678027	438.457539	8.903399
6.566385	421.992417	8.908416
7.036791	433.431033	8.913434
6.754453	443.715817	8.918451
6.870818	430.358124	8.923469
6.442250	431.091175	8.928487
6.698474	428.040446	8.933504
7.070838	437.787149	8.938522
6.709918	441.709565	8.943539
7.147762	443.143147	8.948557
6.571725	440.011379	8.953575
6.972110	450.009317	8.958592
6.939554	446.391609	8.963610
6.998073	440.206603	8.968627
7.210482	432.962392	8.973645
6.460010	423.817791	8.978663
6.954859	422.115063	8.983680
6.826485	422.419229	8.988698
6.661980	437.835781	8.993715
6.788128	433.164424	8.998733
6.888727	442.347801	9.003751
6.876117	435.867830	9.008768
7.055144	435.883993	9.013786
6.779947	444.087998	9.018803
7.202993	440.443088	9.023821
7.208547	452.857104	9.028839
6.737244	422.834281	9.033856
7.009587	432.710261	9.038874
6.749878	446.109414	9.043891
7.180675	434.668505	9.048909
7.205527	434.172341	9.053927
6.999716	424.109276	9.058944
6.943527	417.244824	9.063962
7.016969	416.744203	9.068979
7.234975	411.575626	9.073997
6.700229	407.197172	9.079015
6.824701	407.591109	9.084032
6.782019	415.449404	9.089050
6.653354	433.886729	9.094067
7.124973	431.982513	9.099085
6.545393	441.073646	9.104103
6.983799	434.961664	9.109120
7.349399	440.474370	9.114138
7.072130	443.402230	9.119155
7.421180	441.132212	9.124173
6.950234	445.283305	9.129191
6.952287	437.302039	9.134208
7.299217	438.629947	9.139226
6.732379	440.000039	9.144243
7.369168	436.955953	9.149261
7.259164	442.899781	9.154279
7.207157	440.083535	9.159296
7.519380	442.761244	9.164314
6.949640	435.806836	9.169331
7.415778	430.526793	9.174349
6.927193	429.287416	9.179367
6.873110	421.633686	9.184384
7.259470	436.995485	9.189402
7.445275	439.724559	9.194419
7.250611	433.266803	9.199437
6.989724	421.625010	9.204455
7.020470	416.189128	9.209472
7.243353	415.182258	9.214490
6.960681	431.270566	9.219507
7.363091	436.578688	9.224525
7.115835	444.336506	9.229543
7.183976	449.728564	9.234560
7.501245	443.383096	9.239578
6.877517	438.242255	9.244595
7.039117	433.085665	9.249613
7.158065	447.738295	9.254631
7.224985	445.297888	9.259648
7.068969	445.663189	9.264666
7.008993	456.430689	9.269683
7.003062	448.794650	9.274701
6.830036	446.578029	9.279719
7.074995	448.934921	9.284736
7.154657	443.270462	9.289754
7.088182	451.839396	9.294771
7.259246	447.448175	9.299789
6.896619	466.341911	9.304807
6.892837	450.124949	9.309824
7.108765	458.958907	9.314842
6.959576	477.349000	9.319859
7.278311	467.642378	9.324877
7.117380	474.840732	9.329895
7.379667	480.000410	9.334912
7.601954	468.412270	9.339930
7.483737	486.071688	9.344947
7.327684	480.302139	9.349965
7.515497	473.449927	9.354983
7.424908	473.527268	9.360000
7.641516	471.584109	9.365018
7.609528	486.307757	9.370035
7.463874	465.092148	9.375053
7.471684	453.304094	9.380071
7.262779	447.501811	9.385088
7.192986	438.947981	9.390106
6.838717	458.247494	9.395123
7.538326	462.698022	9.400141
7.679400	464.563111	9.405159
7.536590	473.402791	9.410176
7.673354	473.400329	9.415194
7.455377	456.203915	9.420211
7.382213	444.974504	9.425229
7.058390	452.397185	9.430247
7.369586	464.618156	9.435264
7.678315	459.728838	9.440282
7.444223	473.051414	9.445299
7.686984	466.749170	9.450317
7.560035	472.976528	9.455335
7.599846	470.174294	9.460352
7.484570	449.632438	9.465370
7.151491	455.232527	9.470387
7.526946	473.783410	9.475405
7.637042	471.251028	9.480423
7.455685	477.348058	9.485440
7.411808	474.325407	9.490458
7.503642	468.933586	9.495475
7.488451	475.749346	9.500493
7.390691	480.107061	9.505511
6.902949	471.830139	9.510528
7.539819	463.702061	9.515546
7.481172	473.951814	9.520563
7.719547	466.362695	9.525581
7.409417	474.651082	9.530599
7.392954	474.164546	9.535616
7.623729	466.791212	9.540634
7.617453	469.903834	9.545651
7.485857	470.656627	9.550669
7.740236	467.874423	9.555687
7.589375	476.336671	9.560704
7.944958	465.497660	9.565722
7.752935	475.373838	9.570739
7.547622	476.728314	9.575757
7.519660	472.055848	9.580775
7.589293	478.959304	9.585792
7.856536	469.926620	9.590810
7.593477	478.251815	9.595827
7.679395	466.498851	9.600845
7.741224	472.100187	9.605863
7.385140	470.199421	9.610880
7.690283	468.415959	9.615898
7.839179	464.268047	9.620915
7.691746	467.156634	9.625933
7.753122	475.377346	9.630951
7.643375	484.230785	9.635968
7.747969	471.726969	9.640986
7.459418	478.168996	9.646003
7.485719	475.416215	9.651021
8.047797	468.972421	9.656039
7.285690	477.953316	9.661056
7.959307	485.374365	9.666074
7.627326	490.276863	9.671091
7.600094	495.917407	9.676109
7.912588	500.406508	9.681127
7.820805	497.091558	9.686144
7.787425	502.613147	9.691162
7.638002	502.418841	9.696179
7.692761	507.393293	9.701197
7.711027	504.657544	9.706215
7.722303	506.912202	9.711232
7.622478	491.855805	9.716250
7.399427	500.859549	9.721267
7.374830	494.381435	9.726285
7.817380	497.322754	9.731303
7.533430	502.482817	9.736320
7.991857	491.864361	9.741338
8.085690	500.881571	9.746355
7.979101	500.850966	9.751373
7.978899	502.517289	9.756391
7.746244	502.904066	9.761408
8.079169	496.070135	9.766426
7.588549	509.385594	9.771443
7.633246	500.021692	9.776461
7.912889	495.941649	9.781479
7.561013	508.954504	9.786496
8.247957	516.051586	9.791514
7.946122	518.023946	9.796531
7.911785	531.024934	9.801549
8.368455	531.199566	9.806567
8.117392	516.816939	9.811584
8.039334	505.742891	9.816602
7.973839	503.575686	9.821619
7.767393	500.774161	9.826637
7.904890	503.586553	9.831655
7.541700	516.752664	9.836672
8.042221	525.116031	9.841690
8.104699	521.073164	9.846707
8.229231	521.132579	9.851725
8.165883	524.304646	9.856743
8.272776	529.463439	9.861760
8.294968	509.029364	9.866778
8.081131	504.098834	9.871795
7.712401	497.523161	9.876813
8.318669	495.165498	9.881831
7.912577	503.809760	9.886848
8.118213	503.692366	9.891866
8.387708	521.193242	9.896883
8.268525	506.966684	9.901901
8.202414	499.396856	9.906919
7.652907	498.848671	9.911936
8.225703	501.147892	9.916954
8.309685	500.544632	9.921971
8.053772	508.490026	9.926989
8.295991	498.565003	9.932007
8.183152	503.540467	9.937024
8.373928	497.186397	9.942042
8.630451	496.966356	9.947059
8.079921	499.103911	9.952077
8.178734	490.457368	9.957095
8.256620	499.047887	9.962112
8.089382	493.601977	9.967130
8.374909	496.375395	9.972147
8.092158	497.208677	9.977165
8.356895	498.113968	9.982183
8.230942	501.920686	9.987200
8.034170	492.828151	9.992218
7.774366	502.989518	9.997235
7.975137	506.823941	10.002253
8.478119	515.619262	10.007271
8.403712	529.134610	10.012288
8.582585	512.765897	10.017306
8.179364	511.172313	10.022323
8.085863	506.368096	10.027341
8.304224	507.772957	10.032359
8.087140	523.677502	10.037376
8.367155	529.127905	10.042394
8.312316	523.415067	10.047411
8.367892	529.323513	10.052429
8.341976	524.196277	10.057447
8.195988	535.753628	10.062464
8.528507	531.232948	10.067482
8.746836	518.787018	10.072499
8.140820	515.457962	10.077517
8.373196	516.655501	10.082535
8.275732	529.625353	10.087552
8.261430	529.312046	10.092570
8.100298	534.983049	10.097587
8.424562	531.987914	10.102605
8.456311	532.254370	10.107623
8.418917	530.177433	10.112640
8.196268	527.675088	10.117658
8.553148	525.160836	10.122675
8.185839	533.290952	10.127693
8.484509	532.041828	10.132711
8.294634	531.200609	10.137728
8.894719	533.934215	10.142746
8.869823	531.905813	10.147763
8.639984	527.728865	10.152781
8.317813	526.920997	10.157799
8.246077	528.459675	10.162816
8.704810	519.800906	10.167834
8.800333	522.872341	10.172851
8.604048	524.361106	10.177869
8.437681	528.514988	10.182887
8.188855	531.277461	10.187904
8.551407	522.984054	10.192922
8.134320	525.148041	10.197939
8.041666	520.791810	10.202957
8.310346	520.872821	10.207975
8.135779	523.661527	10.212992
8.032861	532.128913	10.218010
8.288586	535.430869	10.223027
8.209953	552.689676	10.228045
8.640340	545.928817	10.233063
8.432187	567.944791	10.238080
8.701828	557.542068	10.243098
9.154929	551.803285	10.248115
8.477124	551.420367	10.253133
8.683764	554.647967	10.258151
8.670922	558.478000	10.263168
8.494378	560.512785	10.268186
8.744531	555.481140	10.273203
8.906282	566.722051	10.278221
8.943507	559.675650	10.283239
8.620977	557.015380	10.288256
8.779900	553.579088	10.293274
9.043916	552.288056	10.298291
8.688332	559.870392	10.303309
8.659405	554.131394	10.308327
8.558315	561.509755	10.313344
8.701364	555.358802	10.318362
8.908018	557.058991	10.323379
8.694123	556.953681	10.328397
9.106165	556.917556	10.333415
9.043219	560.569248	10.338432
8.998359	556.943978	10.343450
9.082371	540.012591	10.348467
8.390243	531.676146	10.353485
8.550940	538.817821	10.358503
8.515422	554.608739	10.363520
8.472113	556.442767	10.368538
8.692939	552.488691	10.373555
8.581887	550.252880	10.378573
8.552707	552.510727	10.383591
8.620113	558.089125	10.388608
8.425987	549.482140	10.393626
8.712465	551.854631	10.398643
8.936525	571.612762	10.403661
8.977275	564.363836	10.408679
8.948537	555.251252	10.413696
8.860943	561.750185	10.418714
8.773352	557.326880	10.423731
8.815502	578.741916	10.428749
8.847690	571.494328	10.433767
9.131043	573.911493	10.438784
9.182624	573.682537	10.443802
9.043831	552.440502	10.448819
8.996466	552.539473	10.453837
8.745271	550.833704	10.458855
8.720257	556.533880	10.463872
8.514014	576.012298	10.468890
8.895339	573.838193	10.473907
8.650954	583.984567	10.478925
8.636583	578.028685	10.483943
8.732425	575.965581	10.488960
8.672982	580.317318	10.493978
8.760676	570.577412	10.498995
8.897339	600.744498	10.504013
9.421979	608.394068	10.509031
9.321437	588.348363	10.514048
9.393580	589.375352	10.519066
9.104005	586.302816	10.524083
8.939295	587.142853	10.529101
9.043906	576.532447	10.534119
9.139590	584.416474	10.539136
8.644463	583.837674	10.544154
9.448825	585.134948	10.549171
9.052541	595.989938	10.554189
9.312716	589.110566	10.559207
9.341047	580.585475	10.564224
8.987560	583.118201	10.569242
9.259381	584.410551	10.574259
9.151669	585.554082	10.579277
8.934636	577.383019	10.584295
9.246486	587.659994	10.589312
9.370888	582.417671	10.594330
9.618921	578.418302	10.599347
9.227401	593.444523	10.604365
9.391313	586.665440	10.609383
9.593820	592.595067	10.614400
9.482549	592.937581	10.619418
9.645558	586.679349	10.624435
9.075609	585.269672	10.629453
8.864840	576.984017	10.634471
9.159867	577.884566	10.639488
8.925017	585.441685	10.644506
9.184699	583.400247	10.649523
9.266080	591.851408	10.654541
9.387547	591.409530	10.659559
9.328524	588.711125	10.664576
8.880806	594.771033	10.669594
9.406362	586.461524	10.674611
9.114409	590.284803	10.679629
9.344479	599.949748	10.684647
9.691680	607.166371	10.689664
9.221505	599.703992	10.694682
9.474745	596.634767	10.699699
9.490997	600.068931	10.704717
9.338088	599.780495	10.709735
9.094566	588.719697	10.714752
9.181128	600.294302	10.719770
9.619249	604.183076	10.724787
9.609988	605.560493	10.729805
9.810516	604.317274	10.734823
9.492472	599.961625	10.739840
9.186387	595.660907	10.744858
9.381364	589.252497	10.749875
9.498786	602.677884	10.754893
9.672883	606.567001	10.759911
9.475859	592.194781	10.764928
9.041989	593.673439	10.769946
9.760675	603.649994	10.774963
9.669349	601.988599	10.779981
9.755225	603.590951	10.784999
9.773452	590.018141	10.790016
9.439430	589.363607	10.795034
9.320864	577.753062	10.800051
9.777187	592.542299	10.805069
9.454080	588.679752	10.810087
9.769828	580.674519	10.815104
9.384079	583.515257	10.820122
9.708124	589.738265	10.825139
9.412392	594.054443	10.830157
9.614709	592.659466	10.835175
9.955606	601.353993	10.840192
9.621817	595.309297	10.845210
9.675837	588.061437	10.850227
9.576358	587.079819	10.855245
9.619998	582.399261	10.860263
10.032878	584.972858	10.865280
9.597050	589.509802	10.870298
9.640989	579.735721	10.875315
9.304117	584.140394	10.880333
9.838987	602.795822	10.885351
9.829699	607.650949	10.890368
9.610815	612.384281	10.895386
9.882206	613.683012	10.900403
9.508363	607.051294	10.905421
9.273914	610.808763	10.910439
9.647605	604.429152	10.915456
9.504356	615.427546	10.920474
9.649008	614.634895	10.925491
9.486722	615.335698	10.930509
9.525116	610.444515	10.935527
9.816504	604.712117	10.940544
9.502459	617.400386	10.945562
9.879372	610.998177	10.950579
9.951228	611.958941	10.955597
10.145716	620.657482	10.960615
10.120609	610.061068	10.965632
9.849935	616.273125	10.970650
9.800770	611.196844	10.975667
9.992856	610.358892	10.980685
9.818013	613.267576	10.985703
9.935693	614.407353	10.990720
9.888102	616.671248	10.995738
10.078561	611.380697	11.000755
9.900551	617.414134	11.005773
9.873531	618.349364	11.010791
9.912725	612.287248	11.015808
10.013842	615.086423	11.020826
9.830309	612.473794	11.025843
10.187857	616.119575	11.030861
9.906576	612.509246	11.035879
9.705185	604.304160	11.040896
9.645477	611.751798	11.045914
9.567105	615.431164	11.050931
10.336904	625.500710	11.055949
9.978509	620.933626	11.060967
10.236145	607.149722	11.065984
9.813119	608.983289	11.071002
9.974825	610.684214	11.076019
10.113667	619.157943	11.081037
10.206895	629.816336	11.086055
10.055631	621.742245	11.091072
9.677964	618.263782	11.096090
10.170271	630.008363	11.101107
10.632006	634.833878	11.106125
10.068697	624.631052	11.111143
10.163357	624.720394	11.116160
10.015313	617.270652	11.121178
9.891239	617.959156	11.126195
10.314772	627.054160	11.131213
10.319464	630.704736	11.136231
10.324821	624.890915	11.141248
10.093408	614.655028	11.146266
10.226455	604.964803	11.151283
10.039135	607.143293	11.156301
10.060057	626.280059	11.161319
10.132998	629.351895	11.166336
10.286562	632.354295	11.171354
10.234579	642.975487	11.176371
10.449887	645.138234	11.181389
10.596485	644.092812	11.186407
10.494305	620.257188	11.191424
10.264357	612.656178	11.196442
10.375163	608.277515	11.201459
10.679113	613.383367	11.206477
10.038270	610.343772	11.211495
10.265393	603.217108	11.216512
9.982764	612.362786	11.221530
10.283297	617.238799	11.226547
10.228665	633.585049	11.231565
10.279296	636.969652	11.236583
10.491879	633.452354	11.241600
10.348141	639.007055	11.246618
10.321921	641.980820	11.251635
10.496155	638.747241	11.256653
10.459913	646.566759	11.261671
10.694633	637.731592	11.266688
10.413315	630.555191	11.271706
10.412854	630.814072	11.276723
10.619602	637.254291	11.281741
10.502303	632.311757	11.286759
10.193397	618.667103	11.291776
10.142489	636.555966	11.296794
10.325042	638.730156	11.301811
10.156711	642.742361	11.306829
10.160580	642.902733	11.311847
10.420616	648.719223	11.316864
10.566765	644.076236	11.321882
10.185669	646.382922	11.326899
10.310113	642.983573	11.331917
10.094481	642.496681	11.336935
10.401723	638.876187	11.341952
10.142923	656.014999	11.346970
10.016288	657.546510	11.351987
10.894795	664.891351	11.357005
10.630763	665.522890	11.362023
10.800947	669.961747	11.367040
10.904091	668.708536	11.372058
10.677233	673.547276	11.377075
10.914356	670.180760	11.382093
10.770680	665.980812	11.387111
10.660426	660.005212	11.392128
10.709899	659.498872	11.397146
10.749168	660.562575	11.402163
10.870277	646.497073	11.407181
10.514884	650.052593	11.412199
10.672178	643.669003	11.417216
10.508924	648.014930	11.422234
10.847531	657.868030	11.427251
11.022298	654.211485	11.432269
10.632338	654.124292	11.437287
10.796988	648.440141	11.442304
11.156372	653.341658	11.447322
10.930401	641.208254	11.452339
10.923857	631.158032	11.457357
11.038082	634.497956	11.462375
10.604991	634.625806	11.467392
10.566374	633.710389	11.472410
10.885001	638.359511	11.477427
10.706998	637.314454	11.482445
10.578397	635.497950	11.487463
10.871515	638.510043	11.492480
10.726843	644.863314	11.497498
10.495030	657.472455	11.502515
10.854494	651.082433	11.507533
10.492202	662.014189	11.512551
10.615350	662.490390	11.517568
10.591428	664.078393	11.522586
10.818426	660.413663	11.527603
11.232218	651.323213	11.532621
11.256539	663.661852	11.537639
11.376658	654.358636	11.542656
10.869188	652.554153	11.547674
11.222212	662.471269	11.552691
11.371448	659.576120	11.557709
11.182064	662.455532	11.562727
11.319215	657.615135	11.567744
11.108014	655.754765	11.572762
10.685333	653.684532	11.577779
11.227776	655.919102	11.582797
11.158799	661.143359	11.587815
10.967979	650.841130	11.592832
10.996237	652.310502	11.597850
10.638742	653.218618	11.602867
11.028821	655.593826	11.607885
10.968444	653.889707	11.612903
10.941985	660.767263	11.617920
11.023645	662.881525	11.622938
11.114048	660.140762	11.627955
11.066984	652.788792	11.632973
10.953410	658.805835	11.637991
11.074344	656.432676	11.643008
10.908625	653.722576	11.648026
10.655364	660.209632	11.653043
11.218393	662.582989	11.658061
11.354439	688.209092	11.663079
11.410289	680.727376	11.668096
11.008079	665.326888	11.673114
11.015177	671.656390	11.678131
11.401834	679.163507	11.683149
11.537720	691.838138	11.688167
11.398743	679.949855	11.693184
11.548956	663.329874	11.698202
10.820785	657.924464	11.703219
11.437216	665.439755	11.708237
11.169299	665.279792	11.713255
11.456044	681.679896	11.718272
11.453612	684.381696	11.723290
11.249204	673.002291	11.728307
11.245019	683.275189	11.733325
11.029998	685.202406	11.738343
11.482419	691.108689	11.743360
11.513624	679.405183	11.748378
11.227038	691.110896	11.753395
11.279890	681.489999	11.758413
11.179407	686.368903	11.763431
11.163998	688.482597	11.768448
11.306089	686.819336	11.773466
11.526896	696.823459	11.778483
11.288760	682.691138	11.783501
11.422170	693.254910	11.788519
11.216712	687.612956	11.793536
11.551019	688.302227	11.798554
11.334659	691.406778	11.803571
11.522097	681.458680	11.808589
11.526950	690.354226	11.813607
11.144421	695.094285	11.818624
11.406963	687.125743	11.823642
11.432057	691.498975	11.828659
11.642043	696.174602	11.833677
11.677346	694.042074	11.838695
11.469829	682.028829	11.843712
11.513453	697.286761	11.848730
11.622760	709.394364	11.853747
11.630269	710.835433	11.858765
11.598676	712.995848	11.863783
11.681075	712.351803	11.868800
11.806233	707.525895	11.873818
11.543156	719.944316	11.878835
11.713023	714.101535	11.883853
11.783335	715.154066	11.888871
11.810807	715.840920	11.893888
11.924181	717.031872	11.898906
11.749027	717.993474	11.903923
12.079616	701.932179	11.908941
11.890104	693.507439	11.913959
11.726015	688.177742	11.918976
11.778384	684.019657	11.923994
11.583067	694.483455	11.929011
11.540434	685.975745	11.934029
11.603576	700.725690	11.939047
11.598482	708.966391	11.944064
12.065476	708.416724	11.949082
11.919732	715.413977	11.954099
11.753436	717.279915	11.959117
12.284525	717.613305	11.964135
11.845653	713.030404	11.969152
12.125879	705.870131	11.974170
12.051639	702.353578	11.979187
12.036569	687.735019	11.984205
11.643369	686.846754	11.989223
11.776122	680.744709	11.994240
11.743541	687.878857	11.999258
11.950635	696.625954	12.004275
12.364577	702.863319	12.009293
11.738431	696.533032	12.014311
11.991628	705.329715	12.019328
12.389074	695.544365	12.024346
12.185848	704.059107	12.029363
12.114519	677.810675	12.034381
11.937964	677.292412	12.039399
11.726166	682.188755	12.044416
12.213265	684.668687	12.049434
12.154281	673.115017	12.054451
12.091446	671.834162	12.059469
11.751889	683.096886	12.064487
12.220192	697.054351	12.069504
12.177150	692.573539	12.074522
11.987367	700.745344	12.079539
11.759616	704.798431	12.084557
11.935799	706.232007	12.089575
11.920840	718.362242	12.094592
11.807665	707.738543	12.099610
12.130291	709.531030	12.104627
12.204041	709.702545	12.109645
12.178581	703.877748	12.114663
11.876036	710.681815	12.119680
12.184631	701.579420	12.124698
12.169203	708.654084	12.129715
12.019099	701.895755	12.134733
12.270408	712.971246	12.139751
12.210889	706.340736	12.144768
12.494288	703.323573	12.149786
12.218113	712.184266	12.154803
11.994010	698.879717	12.159821
12.141309	714.629509	12.164839
12.183519	726.081755	12.169856
12.112963	736.387173	12.174874
12.352886	733.417843	12.179891
12.282975	738.796905	12.184909
12.249507	736.359564	12.189927
12.197779	743.256890	12.194944
12.577309	735.269997	12.199962
12.199574	731.703158	12.204979
12.509467	735.845585	12.209997
12.748064	729.108396	12.215015
12.535844	732.278578	12.220032
12.825249	733.517690	12.225050
12.471146	738.553111	12.230067
12.722739	734.505812	12.235085
12.433157	727.583134	12.240103
12.449399	733.819705	12.245120
12.385256	732.157195	12.250138
12.100477	736.392795	12.255155
12.226206	728.070126	12.260173
12.608369	731.513257	12.265191
12.521461	729.788041	12.270208
12.782128	733.278610	12.275226
12.428317	735.590499	12.280243
12.526819	734.416906	12.285261
12.627036	734.953507	12.290279
12.384967	745.165881	12.295296
12.878074	733.064918	12.300314
12.649416	735.720119	12.305331
12.425125	737.560431	12.310349
12.420666	732.328787	12.315367
12.602031	736.671234	12.320384
12.682037	733.319857	12.325402
12.776461	737.735887	12.330419
12.785580	733.388905	12.335437
12.443737	729.529262	12.340455
12.261338	734.275845	12.345472
12.756003	733.399946	12.350490
13.040877	745.413793	12.355507
12.499649	735.557741	12.360525
12.872425	743.647734	12.365543
13.033907	746.658380	12.370560
12.491500	740.018309	12.375578
12.806043	750.913500	12.380595
12.581571	756.970042	12.385613
12.851527	747.876833	12.390631
13.150784	755.097872	12.395648
13.288519	755.514985	12.400666
12.648161	736.292159	12.405683
12.721898	756.395943	12.410701
12.816446	748.791370	12.415719
12.772129	756.492279	12.420736
13.286131	754.830701	12.425754
13.292855	762.122824	12.430771
13.059048	757.523561	12.435789
12.790822	742.991960	12.440807
12.729935	746.375121	12.445824
13.006840	743.504137	12.450842
13.040565	749.879988	12.455859
13.088544	751.078032	12.460877
12.766880	748.597480	12.465895
13.268208	757.942297	12.470912
13.264279	754.862846	12.475930
13.351788	758.124927	12.480947
12.622597	745.543273	12.485965
13.272956	751.140848	12.490983
12.977920	761.762323	12.496000
13.042208	751.959714	12.501018
13.142651	758.037932	12.506035
13.055636	758.452389	12.511053
13.447067	755.134266	12.516071
13.398689	752.550934	12.521088
13.212690	746.514588	12.526106
13.087409	748.544518	12.531123
13.180158	747.106735	12.536141
13.015883	747.498582	12.541159
12.946021	749.567166	12.546176
13.473730	752.170134	12.551194
13.427467	756.914328	12.556211
13.427162	754.506503	12.561229
13.474915	758.510124	12.566247
12.979994	760.923022	12.571264
13.117838	754.914829	12.576282
13.348574	753.411244	12.581299
13.272738	753.729274	12.586317
13.834734	747.051863	12.591335
12.987432	749.147581	12.596352
13.281481	744.525578	12.601370
13.416573	748.944706	12.606387
13.151564	746.600447	12.611405
13.381883	739.937135	12.616423
13.434633	751.072162	12.621440
13.398543	748.742529	12.626458
13.255574	746.761004	12.631475
13.124532	748.968563	12.636493
13.208433	745.534522	12.641511
12.518845	754.990190	12.646528
12.854790	761.397589	12.651546
13.174029	772.109019	12.656563
13.426179	777.008436	12.661581
13.575989	774.895828	12.666599
13.684932	776.816478	12.671616
13.625153	770.492101	12.676634
13.786302	776.308347	12.681651
13.584131	777.573990	12.686669
13.997852	773.987280	12.691687
13.798820	770.900524	12.696704
14.004327	769.340930	12.701722
14.284983	776.738464	12.706739
14.034272	762.920478	12.711757
13.928860	747.684857	12.716775
13.410291	754.794190	12.721792
13.893938	747.276978	12.726810
13.952051	738.696653	12.731827
13.366282	752.203926	12.736845
13.625671	738.132466	12.741863
13.321779	746.984895	12.746880
13.441501	740.831222	12.751898
13.365660	754.002978	12.756915
13.467193	764.748514	12.761933
13.798678	768.521488	12.766951
13.998424	786.191344	12.771968
13.866685	769.454492	12.776986
14.316569	762.040395	12.782003
14.198492	779.198302	12.787021
14.389325	756.900820	12.792039
14.022926	752.915630	12.797056
14.008497	749.645319	12.802074
13.463206	751.763147	12.807091
13.161027	744.132372	12.812109
13.782003	758.413107	12.817127
13.981873	767.915616	12.822144
14.013158	767.396344	12.827162
14.029336	771.193473	12.832179
13.760287	785.061407	12.837197
14.227679	774.094238	12.842215
13.666492	772.257133	12.847232
13.652629	768.068380	12.852250
13.781242	783.947394	12.857267
13.672404	780.701336	12.862285
13.951812	765.765173	12.867303
14.047095	770.603959	12.872320
14.071737	770.956740	12.877338
14.043783	761.345305	12.882355
13.961912	766.025652	12.887373
14.043975	772.475989	12.892391
14.360707	771.078851	12.897408
14.096276	773.998442	12.902426
14.276220	771.338308	12.907443
14.289641	771.872730	12.912461
14.219565	768.589043	12.917479
13.654831	766.995494	12.922496
14.047500	772.977438	12.927514
14.475493	785.369680	12.932531
14.163538	794.933461	12.937549
14.463988	784.576273	12.942567
14.581121	779.322409	12.947584
13.955304	769.965591	12.952602
14.076905	775.895332	12.957619
14.053119	792.836504	12.962637
14.568921	780.731953	12.967655
14.135654	790.829142	12.972672
14.260732	795.369773	12.977690
14.643565	789.133834	12.982707
14.477121	790.649503	12.987725
14.391835	792.313404	12.992743
14.934870	798.306512	12.997760
14.425013	789.486944	13.002778
14.338507	780.960816	13.007795
14.365999	791.241436	13.012813
14.354890	788.178883	13.017831
14.681705	800.438663	13.022848
14.411257	800.619926	13.027866
14.831024	792.008158	13.032883
14.349678	793.806699	13.037901
14.748034	789.701678	13.042919
14.444834	785.820189	13.047936
14.300972	794.401413	13.052954
14.620118	789.033842	13.057971
14.521953	789.699358	13.062989
14.922706	792.145496	13.068007
14.711322	788.931283	13.073024
14.591179	789.243633	13.078042
14.651518	782.206146	13.083059
14.665813	791.693562	13.088077
14.443900	794.982040	13.093095
14.874169	789.982071	13.098112
14.466771	798.213262	13.103130
14.739929	792.354272	13.108147
14.418554	792.073293	13.113165
14.553588	790.830855	13.118183
14.939829	790.622046	13.123200
14.638828	784.912979	13.128218
14.954340	788.312914	13.133235
14.781947	793.591282	13.138253
14.693151	786.864342	13.143271
14.755400	780.927946	13.148288
14.644038	785.726529	13.153306
14.995445	790.329529	13.158323
14.953562	795.944060	13.163341
14.733473	796.439329	13.168359
15.022014	798.129868	13.173376
15.174881	799.964742	13.178394
15.016779	796.783205	13.183411
14.945729	799.300111	13.188429
14.886868	793.278544	13.193447
14.955585	788.748639	13.198464
14.977073	789.843538	13.203482
15.062125	792.885102	13.208499
14.646337	790.068993	13.213517
15.082167	788.075673	13.218535
14.979145	790.963665	13.223552
14.779129	789.413957	13.228570
15.120527	782.354525	13.233587
15.354132	796.310971	13.238605
15.069976	794.367342	13.243623
15.119812	788.641174	13.248640
14.860838	793.488134	13.253658
15.261170	785.646284	13.258675
14.884666	794.592166	13.263693
14.730434	786.452192	13.268711
15.190458	784.660212	13.273728
15.047073	800.206312	13.278746
15.414862	809.076611	13.283763
15.250077	805.132405	13.288781
15.079033	808.356110	13.293799
15.087926	818.374569	13.298816
15.342232	819.609719	13.303834
15.672916	825.418354	13.308851
15.410148	813.662989	13.313869
15.130594	805.085044	13.318887
15.439032	817.284598	13.323904
14.981752	821.891233	13.328922
15.792121	818.075107	13.333939
15.345551	827.802010	13.338957
15.421887	822.803837	13.343975
15.396831	820.450374	13.348992
15.449656	828.013016	13.354010
15.672838	823.856538	13.359027
15.329479	814.029401	13.364045
15.540167	809.818079	13.369063
15.873611	799.190622	13.374080
15.100362	797.430922	13.379098
15.393705	793.370757	13.384115
15.430586	809.273634	13.389133
15.462235	814.665208	13.394151
15.745540	817.410623	13.399168
15.347964	821.619734	13.404186
15.968557	812.708243	13.409203
15.718685	817.970355	13.414221
15.549837	815.516345	13.419239
15.774557	811.495330	13.424256
15.475259	819.501308	13.429274
15.350043	816.901603	13.434291
15.301455	819.231953	13.439309
15.554428	817.781684	13.444327
15.655592	819.422687	13.449344
15.460476	820.488408	13.454362
15.523518	812.323848	13.459379
15.436297	812.078766	13.464397
15.499565	822.726189	13.469415
15.804466	820.380990	13.474432
15.481865	821.908505	13.479450
15.565650	816.353737	13.484467
15.526755	839.110396	13.489485
15.469475	838.488231	13.494503
15.591896	847.703112	13.499520
15.592927	843.906489	13.504538
15.588866	847.085103	13.509555
15.627240	851.225916	13.514573
16.063860	847.013900	13.519591
15.974031	848.987792	13.524608
15.772728	847.226838	13.529626
16.294383	846.542369	13.534643
15.809115	846.971888	13.539661
15.648752	843.815944	13.544679
15.938034	841.886607	13.549696
15.842520	842.813645	13.554714
15.676410	838.737093	13.559731
15.925640	858.901861	13.564749
15.822323	868.373030	13.569767
16.371381	864.683045	13.574784
16.399591	865.821078	13.579802
16.452605	869.580898	13.584819
16.434997	855.328680	13.589837
16.148301	849.686779	13.594855
16.311621	839.821268	13.599872
15.988370	840.720871	13.604890
16.213071	836.952322	13.609907
16.215976	844.393402	13.614925
16.400892	837.999104	13.619943
16.450539	838.003981	13.624960
16.281827	839.772478	13.629978
16.083436	837.752288	13.634995
16.218159	836.920158	13.640013
16.323099	841.284072	13.645031
16.279643	836.774886	13.650048
16.418185	844.144221	13.655066
16.534919	834.125063	13.660083
16.434858	842.005159	13.665101
15.843048	843.821012	13.670119
16.137114	843.882268	13.675136
16.125826	854.020676	13.680154
16.065873	858.530352	13.685171
16.241250	861.368424	13.690189
16.347667	868.559763	13.695207
16.684581	863.195697	13.700224
16.556091	878.916260	13.705242
16.520868	860.936571	13.710259
16.902693	860.576972	13.715277
16.766104	860.601560	13.720295
16.601802	859.756318	13.725312
16.346804	868.418107	13.730330
16.510624	867.401532	13.735347
16.848422	864.337949	13.740365
16.637978	867.586772	13.745383
16.602885	864.329145	13.750400
16.754540	866.665997	13.755418
16.436679	858.280224	13.760435
16.870214	858.531071	13.765453
16.720558	866.065492	13.770471
16.735893	867.268659	13.775488
16.710879	865.044574	13.780506
16.683459	865.493878	13.785523
16.515435	859.464146	13.790541
16.700782	868.905867	13.795559
16.776909	861.543978	13.800576
16.412515	866.382227	13.805594
16.909029	867.393236	13.810611
16.973820	863.652892	13.815629
16.938365	865.829710	13.820647
16.791249	863.577418	13.825664
16.621124	873.949010	13.830682
16.984503	865.317639	13.835699
16.949371	869.201725	13.840717
16.811901	866.708077	13.845735
17.053835	862.510781	13.850752
16.859751	859.581028	13.855770
16.641230	862.502907	13.860787
16.729605	864.679258	13.865805
17.038283	864.416327	13.870823
17.435046	853.018356	13.875840
17.372530	869.075718	13.880858
16.816455	861.705583	13.885875
17.048042	868.141994	13.890893
16.657546	867.818194	13.895911
17.229832	876.328277	13.900928
16.983101	872.523129	13.905946
16.886750	883.899355	13.910963
17.224039	890.202446	13.915981
17.217101	893.567715	13.920999
17.492009	896.844642	13.926016
17.205012	893.086826	13.931034
17.176667	888.748831	13.936051
17.303498	885.506856	13.941069
17.157641	900.428570	13.946087
17.276421	898.519629	13.951104
16.967161	896.904975	13.956122
17.199390	891.355329	13.961139
17.232036	894.537667	13.966157
17.009434	891.277855	13.971175
17.286419	892.755615	13.976192
17.274316	882.261146	13.981210
17.381131	882.234974	13.986227
17.314328	887.600970	13.991245
17.239997	891.112499	13.996263
17.471755	887.576368	14.001280
17.860895	882.223049	14.006298
17.171081	881.397026	14.011315
17.540988	877.690926	14.016333
17.380444	886.880733	14.021351
17.573912	875.157987	14.026368
17.457430	877.136059	14.031386
17.209037	885.430741	14.036403
17.772408	887.371723	14.041421
17.414796	886.992276	14.046439
17.738018	885.256436	14.051456
17.520102	894.884432	14.056474
17.750049	896.041353	14.061491
17.870915	887.605761	14.066509
17.469408	886.826086	14.071527
17.583178	882.948673	14.076544
18.064828	906.415980	14.081562
17.435046	901.541043	14.086579
17.879818	891.094909	14.091597
17.610871	911.385106	14.096615
17.994635	902.870446	14.101632
17.847885	907.160200	14.106650
17.685140	906.838585	14.111667
18.179305	903.564300	14.116685
17.940375	907.272039	14.121703
17.975378	888.189389	14.126720
17.622971	882.535683	14.131738
17.795796	888.340669	14.136755
18.094584	899.298381	14.141773
17.683643	893.196242	14.146791
17.519401	900.149128	14.151808
17.775017	910.116358	14.156826
17.815815	906.843676	14.161843
18.177660	901.283186	14.166861
17.962885	915.117469	14.171879
17.859518	907.348175	14.176896
18.084454	908.894052	14.181914
17.857626	904.666049	14.186931
18.179541	903.618390	14.191949
18.200290	907.477950	14.196967
17.839590	896.362736	14.201984
18.095438	899.873028	14.207002
17.994859	903.650609	14.212019
17.996425	910.984627	14.217037
18.176083	908.261401	14.222055
18.084140	904.185836	14.227072
18.087957	900.597052	14.232090
17.914478	901.406919	14.237107
18.386767	927.330983	14.242125
18.523100	926.277685	14.247143
18.655877	920.778326	14.252160
18.518141	916.246021	14.257178
18.626693	904.612302	14.262195
18.384566	898.657284	14.267213
18.284137	901.065196	14.272231
18.712428	902.178416	14.277248
18.733587	905.861183	14.282266
18.212330	906.763411	14.287283
18.611377	901.291767	14.292301
18.271838	909.285155	14.297319
18.281032	897.938412	14.302336
18.531162	898.117008	14.307354
18.222627	905.537481	14.312371
18.452989	902.225631	14.317389
18.315383	908.136068	14.322407
18.668052	916.219823	14.327424
18.440711	914.942634	14.332442
18.473407	924.020130	14.337459
18.667981	921.433423	14.342477
18.908734	929.878709	14.347495
18.629578	930.553652	14.352512
18.679996	930.302783	14.357530
18.718533	936.902013	14.362547
18.784459	941.593963	14.367565
18.820612	937.122773	14.372583
18.857276	932.698842	14.377600
18.959130	930.180310	14.382618
19.063202	918.730324	14.387635
19.044182	908.372626	14.392653
18.611686	909.415584	14.397671
18.584368	901.312478	14.402688
18.803668	908.779641	14.407706
18.834519	926.469788	14.412723
18.533897	921.275024	14.417741
18.780068	930.012956	14.422759
19.022014	920.873555	14.427776
19.221931	920.018582	14.432794
19.235562	930.194155	14.437811
19.187561	930.277448	14.442829
18.858156	923.995262	14.447847
18.866601	922.065735	14.452864
19.318558	925.939790	14.457882
19.105512	926.894715	14.462899
19.272617	920.168657	14.467917
18.936845	914.846855	14.472935
19.104933	909.149459	14.477952
19.059407	916.699145	14.482970
19.449805	925.531245	14.487987
19.365808	907.275123	14.493005
18.812044	913.465363	14.498023
19.125269	924.023190	14.503040
19.298001	919.527449	14.508058
19.034665	926.237090	14.513075
19.279566	923.816070	14.518093
19.233393	924.738538	14.523111
19.364228	922.054517	14.528128
19.521427	919.300094	14.533146
19.302600	917.690204	14.538163
19.487075	918.604937	14.543181
19.236617	928.241206	14.548199
19.321282	927.565240	14.553216
19.098322	924.374907	14.558234
19.035612	922.838389	14.563251
19.040207	920.262513	14.568269
19.528322	923.957329	14.573287
18.814462	918.338152	14.578304
19.132310	913.655571	14.583322
18.943373	929.540286	14.588339
19.328498	945.707465	14.593357
19.363929	940.753538	14.598375
19.092145	947.234132	14.603392
19.593891	943.788235	14.608410
19.185075	949.056353	14.613427
19.468164	948.604923	14.618445
19.524086	951.045151	14.623463
19.731769	956.491239	14.628480
19.634724	946.136277	14.633498
19.743036	960.241873	14.638515
20.024035	956.268814	14.643533
19.799497	949.168596	14.648551
19.626535	948.299460	14.653568
19.667470	952.029632	14.658586
19.741576	964.979229	14.663603
19.979952	966.620838	14.668621
20.063626	969.211358	14.673639
19.640256	961.416437	14.678656
20.231805	955.608496	14.683674
19.820605	964.143323	14.688691
19.710671	950.240017	14.693709
19.838416	961.013123	14.698727
19.842124	971.556355	14.703744
19.982012	976.880526	14.708762
20.145435	980.944971	14.713779
19.831323	975.966904	14.718797
19.851815	983.124413	14.723815
20.049128	982.553874	14.728832
20.128764	965.821591	14.733850
19.914109	985.191316	14.738867
20.220740	977.259921	14.743885
20.314542	976.932824	14.748903
20.130326	978.236693	14.753920
20.480620	967.530756	14.758938
20.433898	983.036622	14.763955
20.483707	975.012920	14.768973
20.501159	977.118343	14.773991
20.078838	964.226514	14.779008
20.498507	956.050194	14.784026
19.989932	969.252039	14.789043
20.503004	965.633946	14.794061
20.574138	965.477662	14.799079
20.127035	960.624580	14.804096
20.199133	959.395148	14.809114
20.107522	963.430118	14.814131
20.197900	963.529601	14.819149
20.361605	964.889413	14.824167
20.289304	972.045677	14.829184
20.389183	971.764966	14.834202
20.204818	966.517259	14.839219
19.908699	965.582209	14.844237
20.290094	971.446064	14.849255
20.108164	973.314477	14.854272
20.562209	978.583114	14.859290
20.606763	992.843896	14.864307
20.625877	989.057032	14.869325
20.724428	990.363937	14.874343
20.779069	996.007590	14.879360
20.991911	982.148363	14.884378
20.630284	964.099788	14.889395
21.028972	974.341290	14.894413
20.781214	967.014324	14.899431
20.648161	963.172411	14.904448
20.611248	961.199492	14.909466
20.696984	970.369690	14.914483
20.796212	981.882596	14.919501
20.960800	983.188621	14.924519
20.959132	984.148301	14.929536
20.878774	974.879485	14.934554
20.680006	969.324758	14.939571
21.180420	988.244771	14.944589
21.027866	977.380923	14.949607
20.708021	971.665280	14.954624
20.892387	970.235216	14.959642
20.914096	985.446335	14.964659
20.926480	985.914652	14.969677
21.316491	993.175219	14.974695
21.128732	996.852867	14.979712
21.163757	996.348782	14.984730
21.259813	997.081708	14.989747
21.182092	982.538998	14.994765
21.417934	977.051876	14.999783
21.294042	969.014365	15.004800
20.959333	961.988209	15.009818
20.809381	967.326230	15.014835
20.834423	983.578264	15.019853
21.109525	983.481543	15.024871
21.114214	986.068661	15.029888
21.432797	987.628276	15.034906
21.187257	982.286004	15.039923
21.410436	990.137612	15.044941
21.551523	983.005341	15.049959
21.357422	988.236674	15.054976
21.168504	988.237902	15.059994
21.244239	987.228810	15.065011
21.415025	990.910242	15.070029
21.718006	980.650377	15.075047
21.144902	984.621934	15.080064
21.341052	986.809816	15.085082
21.493689	984.191800	15.090099
21.549626	984.675385	15.095117
21.546130	988.649217	15.100135
21.432797	1000.593080	15.105152
21.972695	978.650895	15.110170
21.663416	988.832912	15.115187
21.705256	975.341319	15.120205
21.818546	982.919799	15.125223
21.657094	983.001933	15.130240
21.699447	973.193172	15.135258
22.016119	983.501179	15.140275
21.604530	983.388970	15.145293
21.673027	981.872915	15.150311
21.319006	988.637814	15.155328
21.697870	969.602190	15.160346
21.538625	985.605382	15.165363
21.644123	978.371390	15.170381
21.899197	999.494788	15.175399
21.694119	1002.916369	15.180416
21.908546	999.162019	15.185434
22.051898	1001.200382	15.190451
21.965894	1000.440698	15.195469
21.967233	1004.805105	15.200487
21.721094	1018.426626	15.205504
21.920583	1009.227558	15.210522
21.815053	1007.704053	15.215539
22.036213	1009.749161	15.220557
22.067185	1013.285242	15.225575
21.964108	1013.919977	15.230592
22.198170	1011.566917	15.235610
22.197544	1013.653087	15.240627
22.241653	1004.399469	15.245645
21.903000	1002.903022	15.250663
21.904636	1011.811856	15.255680
22.140288	999.425996	15.260698
22.014736	999.417296	15.265715
21.847000	1005.859518	15.270733
22.517422	994.727857	15.275751
21.916995	997.898947	15.280768
22.285888	1009.511635	15.285786
22.245780	1027.629576	15.290803
22.310125	1023.712539	15.295821
22.520663	1028.593299	15.300839
22.238504	1045.540478	15.305856
22.506673	1045.182904	15.310874
22.812918	1017.053867	15.315891
22.922913	1017.951872	15.320909
22.855745	1006.276189	15.325927
22.854112	1004.812147	15.330944
22.687712	1003.014150	15.335962
22.840980	998.707636	15.340979
22.622992	995.412367	15.345997
22.653434	995.726373	15.351015
22.482996	996.655691	15.356032
22.714035	981.297727	15.361050
22.670945	994.246773	15.366067
22.502815	993.127562	15.371085
22.847514	990.195424	15.376103
22.659225	986.153872	15.381120
22.685133	994.680189	15.386138
22.590112	986.694952	15.391155
22.569216	993.360321	15.396173
22.833656	993.827017	15.401191
23.132274	1010.279214	15.406208
23.082661	1006.518894	15.411226
22.911520	996.222850	15.416243
22.424697	995.876269	15.421261
23.147301	1004.324991	15.426279
22.708346	1008.849905	15.431296
23.060760	1010.823954	15.436314
22.888924	1009.623270	15.441331
22.891252	1019.074811	15.446349
23.119525	1009.890168	15.451367
22.942584	1017.189081	15.456384
23.117305	1020.494352	15.461402
23.277628	1017.064064	15.466419
22.936445	1013.986915	15.471437
22.950447	1008.651309	15.476455
23.247814	1018.829815	15.481472
23.522296	1021.904856	15.486490
23.317149	1016.685637	15.491507
23.472758	1014.120801	15.496525
23.537749	1010.626554	15.501543
23.250075	1014.840581	15.506560
23.143086	1016.447942	15.511578
23.667051	1010.969317	15.516595
23.332059	1010.280202	15.521613
23.748395	1007.926987	15.526631
23.308867	1016.163312	15.531648
23.072286	1021.795796	15.536666
23.427769	1017.419724	15.541683
23.219741	1015.180112	15.546701
23.484888	1019.373799	15.551719
23.421154	1014.744665	15.556736
23.277750	1019.826049	15.561754
23.572807	1011.079078	15.566771
23.232574	1018.087986	15.571789
23.401774	1002.682886	15.576807
23.417241	1017.749840	15.581824
23.328901	1016.952650	15.586842
23.408290	1024.905699	15.591859
23.428609	1041.827573	15.596877
23.590091	1038.220370	15.601895
23.486979	1038.495341	15.606912
24.062353	1038.301079	15.611930
24.025927	1037.066554	15.616947
23.884590	1039.512453	15.621965
24.016994	1043.114700	15.626983
23.911304	1042.553764	15.632000
24.078116	1041.129601	15.637018
24.234178	1040.227843	15.642035
23.988095	1049.450071	15.647053
24.473278	1042.980251	15.652071
24.368011	1042.854761	15.657088
23.856858	1024.375104	15.662106
24.082672	1021.824514	15.667123
24.068178	1018.680399	15.672141
23.995425	1020.102510	15.677159
23.923099	1038.007754	15.682176
24.008364	1041.702596	15.687194
24.356291	1021.188496	15.692211
24.147556	1034.273980	15.697229
24.277021	1037.548475	15.702247
24.693986	1044.429289	15.707264
24.241109	1036.332836	15.712282
24.206715	1027.394472	15.717299
24.562698	1037.863614	15.722317
24.508591	1025.753515	15.727335
24.055901	1029.485302	15.732352
23.964418	1034.331332	15.737370
24.119137	1024.770031	15.742387
23.932217	1033.399142	15.747405
24.146574	1045.414772	15.752423
24.269909	1036.546367	15.757440
24.245358	1039.387389	15.762458
24.390733	1035.886854	15.767475
24.371579	1032.216434	15.772493
24.602151	1054.400958	15.777511
24.545019	1055.618648	15.782528
24.804931	1065.575825	15.787546
24.948230	1057.449072	15.792563
24.716905	1051.924666	15.797581
24.467308	1037.563480	15.802599
24.955987	1036.303487	15.807616
24.407221	1041.457857	15.812634
24.492544	1046.105769	15.817651
24.282992	1056.758207	15.822669
24.948687	1054.454281	15.827687
25.110761	1056.944165	15.832704
24.516752	1060.107949	15.837722
24.940144	1054.992217	15.842739
24.801887	1068.401208	15.847757
24.989534	1067.267277	15.852775
25.255554	1066.291484	15.857792
25.076177	1063.902206	15.862810
25.494498	1056.085824	15.867827
25.378932	1056.009286	15.872845
25.145499	1046.565595	15.877863
24.957128	1032.835465	15.882880
24.695802	1043.215132	15.887898
25.014980	1050.448950	15.892915
25.179555	1053.929392	15.897933
24.962962	1056.185107	15.902951
25.381491	1056.088005	15.907968
25.277897	1066.316737	15.912986
25.436044	1059.964424	15.918003
25.138439	1063.482567	15.923021
25.124794	1062.067741	15.928039
25.105289	1057.172883	15.933056
25.136018	1062.479468	15.938074
24.902487	1053.660655	15.943091
25.244843	1063.342975	15.948109
25.273757	1056.654296	15.953127
25.230083	1059.211131	15.958144
25.443414	1061.080742	15.963162
25.744433	1066.101975	15.968179
25.083916	1065.277663	15.973197
25.240815	1059.279007	15.978215
25.257372	1078.161315	15.983232
25.328298	1085.916895	15.988250
25.319165	1083.611397	15.993267
25.130918	1078.837649	15.998285
25.277151	1082.825913	16.003303
25.481505	1072.893882	16.008320
25.310388	1080.741034	16.013338
25.526554	1086.785454	16.018355
25.505920	1109.836251	16.023373
25.758292	1105.763500	16.028391
25.819877	1102.446499	16.033408
25.380731	1112.693117	16.038426
25.727211	1110.704294	16.043443
25.767368	1110.215182	16.048461
25.878189	1108.392675	16.053479
25.832612	1099.557015	16.058496
25.636880	1103.545212	16.063514
26.215242	1106.380146	16.068531
25.938310	1103.229797	16.073549
25.849315	1110.802154	16.078567
26.105993	1109.035692	16.083584
26.208139	1123.707290	16.088602
26.293884	1111.673054	16.093619
25.809013	1108.261784	16.098637
25.997794	1124.339964	16.103655
26.325362	1129.139297	16.108672
26.364154	1135.874265	16.113690
26.552826	1130.123079	16.118707
26.364208	1116.670643	16.123725
26.388077	1112.365440	16.128743
26.283379	1100.184320	16.133760
26.246147	1114.688394	16.138778
26.129185	1113.548535	16.143795
26.428583	1136.798541	16.148813
26.691685	1135.242515	16.153831
26.930729	1129.786405	16.158848
25.976087	1112.048349	16.163866
26.923577	1115.576555	16.168883
26.555960	1111.196987	16.173901
26.576051	1106.955495	16.178919
26.218160	1100.251663	16.183936
26.142061	1120.991578	16.188954
26.568532	1122.569017	16.193971
26.515810	1132.733010	16.198989
27.011601	1115.976409	16.204007
26.950508	1122.332534	16.209024
26.858275	1121.182489	16.214042
26.632178	1124.247612	16.219059
26.444277	1130.554178	16.224077
26.726030	1123.806925	16.229095
26.699899	1119.746247	16.234112
26.907337	1122.702418	16.239130
26.724558	1123.687326	16.244147
26.547527	1124.093804	16.249165
26.346072	1122.402276	16.254183
26.962773	1121.128531	16.259200
26.975082	1118.109591	16.264218
26.860616	1123.107573	16.269235
27.046634	1126.518395	16.274253
27.034173	1141.570893	16.279271
27.397292	1136.066937	16.284288
27.012979	1135.322427	16.289306
27.095218	1138.863124	16.294323
26.935861	1144.808605	16.299341
27.285702	1147.448969	16.304359
27.590317	1145.498262	16.309376
27.303019	1148.519328	16.314394
27.599696	1130.121280	16.319411
27.080253	1128.845659	16.324429
27.109569	1133.341418	16.329447
27.458735	1131.980198	16.334464
27.415295	1141.132852	16.339482
27.581250	1135.435718	16.344499
27.381704	1138.272615	16.349517
27.483818	1139.951370	16.354535
27.391576	1138.605658	16.359552
27.255660	1144.976670	16.364570
27.756352	1147.748039	16.369587
27.733149	1145.539415	16.374605
27.153187	1146.280431	16.379623
27.719159	1133.445080	16.384640
27.670813	1147.913052	16.389658
27.394375	1142.487208	16.394675
27.592559	1142.544554	16.399693
27.441403	1140.005672	16.404711
27.505193	1127.785511	16.409728
27.287588	1135.485330	16.414746
27.422053	1152.310528	16.419763
27.915404	1160.347105	16.424781
27.981613	1164.480474	16.429799
28.315622	1154.262987	16.434816
28.340211	1155.581493	16.439834
28.028120	1146.964297	16.444851
28.260201	1141.951101	16.449869
27.966133	1126.400721	16.454887
28.153554	1123.796171	16.459904
27.796914	1131.066478	16.464922
27.823372	1142.991690	16.469939
28.135190	1151.896177	16.474957
28.388570	1151.165365	16.479975
28.639433	1152.685111	16.484992
28.367922	1141.041356	16.490010
28.401869	1132.849649	16.495027
28.268211	1131.276890	16.500045
28.394471	1134.757038	16.505063
28.554924	1127.435478	16.510080
28.544786	1127.566490	16.515098
27.989398	1126.678365	16.520115
28.639037	1132.108914	16.525133
28.220036	1136.517120	16.530151
28.422041	1120.586054	16.535168
28.115602	1129.562151	16.540186
28.208791	1124.690645	16.545203
28.328340	1146.302525	16.550221
28.414770	1147.882749	16.555239
28.522678	1147.181042	16.560256
28.413276	1157.464386	16.565274
28.716106	1155.233081	16.570291
28.620006	1151.113929	16.575309
28.709454	1152.438052	16.580327
29.118925	1146.497627	16.585344
28.300146	1164.838697	16.590362
28.545422	1149.061778	16.595379
28.867346	1147.818438	16.600397
28.756377	1157.167879	16.605415
28.627077	1152.015634	16.610432
28.915768	1151.948343	16.615450
28.848412	1144.712963	16.620467
29.081883	1152.332648	16.625485
28.888354	1157.260973	16.630503
28.849277	1151.264588	16.635520
28.924424	1159.571823	16.640538
28.984890	1159.350935	16.645555
29.376499	1163.234498	16.650573
29.038517	1173.642030	16.655591
29.006908	1171.548333	16.660608
29.157323	1183.018634	16.665626
29.302085	1183.106442	16.670643
29.554917	1183.688575	16.675661
29.391586	1184.089751	16.680679
29.596888	1171.415028	16.685696
29.315057	1168.420073	16.690714
28.989129	1164.567309	16.695731
29.499905	1169.656696	16.700749
29.400542	1175.700089	16.705767
29.311501	1183.149404	16.710784
29.114967	1181.027895	16.715802
29.215291	1185.433644	16.720819
29.629260	1174.995327	16.725837
29.080967	1194.161924	16.730855
29.491628	1181.133115	16.735872
29.640852	1173.579757	16.740890
29.889855	1169.191929	16.745907
29.565499	1173.967181	16.750925
29.411416	1174.710902	16.755943
29.760414	1179.046129	16.760960
29.978286	1179.122482	16.765978
29.653299	1179.593168	16.770995
29.751064	1169.210709	16.776013
29.842117	1178.244477	16.781031
29.873426	1177.254958	16.786048
29.684748	1182.113100	16.791066
29.650454	1200.372321	16.796083
30.123421	1194.172614	16.801101
30.145407	1194.276503	16.806119
30.310657	1200.054374	16.811136
30.283273	1196.789167	16.816154
30.056952	1191.090358	16.821171
30.136505	1182.664257	16.826189
30.223840	1193.355469	16.831207
30.443945	1188.751249	16.836224
30.242834	1174.376043	16.841242
29.820821	1168.316570	16.846259
30.158465	1186.157728	16.851277
30.284732	1192.623383	16.856295
30.323848	1193.788131	16.861312
30.091069	1191.372487	16.866330
30.015060	1196.304502	16.871347
30.236740	1192.189201	16.876365
30.240789	1191.989776	16.881383
30.389379	1184.849938	16.886400
30.476767	1192.009673	16.891418
30.115706	1193.985073	16.896435
29.969711	1193.108543	16.901453
30.110442	1204.255315	16.906471
30.556525	1213.508040	16.911488
30.878725	1222.635006	16.916506
30.792485	1227.691713	16.921523
30.539966	1212.522927	16.926541
30.413553	1218.718900	16.931559
30.187366	1217.889648	16.936576
30.345583	1214.614293	16.941594
30.163941	1219.528149	16.946611
30.508766	1226.647563	16.951629
30.567339	1245.198404	16.956647
30.653966	1243.818348	16.961664
30.824644	1240.241223	16.966682
30.756843	1242.028663	16.971699
30.733138	1233.757577	16.976717
30.616112	1244.086348	16.981735
30.687571	1250.137717	16.986752
31.321930	1264.098014	16.991770
31.388638	1262.954616	16.996787
31.423665	1253.888492	17.001805
31.173522	1245.308882	17.006823
31.278498	1243.196932	17.011840
31.193905	1242.389677	17.016858
30.992864	1253.132419	17.021875
31.415527	1262.133208	17.026893
31.685559	1255.078461	17.031911
31.665163	1259.885010	17.036928
31.916008	1249.677343	17.041946
31.238253	1239.403727	17.046963
31.243304	1230.777829	17.051981
31.311958	1240.512596	17.056999
31.618630	1250.516201	17.062016
31.988638	1249.019158	17.067034
31.300235	1252.548072	17.072051
31.381802	1244.377255	17.077069
31.419477	1248.852799	17.082087
31.449046	1256.911590	17.087104
31.690651	1256.832740	17.092122
31.616697	1256.797020	17.097139
32.109172	1256.117110	17.102157
31.482188	1260.968203	17.107175
31.464715	1260.140964	17.112192
31.708774	1254.942816	17.117210
31.579211	1262.300679	17.122227
31.666744	1254.400333	17.127245
31.400726	1277.571847	17.132263
31.672207	1283.462495	17.137280
32.267010	1272.074257	17.142298
32.137473	1275.954287	17.147315
32.149368	1265.414806	17.152333
32.090927	1279.092327	17.157351
32.114341	1275.484617	17.162368
32.606624	1277.118033	17.167386
32.443378	1276.487208	17.172403
32.434726	1278.786114	17.177421
32.239846	1273.350607	17.182439
32.310891	1276.164065	17.187456
32.593726	1273.904320	17.192474
32.463613	1275.082964	17.197491
32.752953	1269.019304	17.202509
32.650277	1269.268962	17.207527
32.253000	1259.967598	17.212544
32.750413	1255.408279	17.217562
32.372008	1256.957196	17.222579
32.564125	1264.021654	17.227597
32.481167	1276.213415	17.232615
32.801974	1269.510483	17.237632
32.866894	1268.518849	17.242650
32.876289	1280.746639	17.247667
32.581131	1254.731253	17.252685
32.797720	1256.950682	17.257703
32.693033	1265.933108	17.262720
32.943798	1260.809649	17.267738
32.692049	1268.713699	17.272755
32.298689	1263.350320	17.277773
32.652196	1271.522472	17.282791
32.677534	1268.135378	17.287808
32.838923	1269.224166	17.292826
32.928495	1270.090668	17.297843
32.563372	1267.765180	17.302861
32.460841	1270.722603	17.307879
32.786443	1294.675637	17.312896
32.863528	1300.394769	17.317914
32.847822	1305.453070	17.322931
33.035159	1293.178723	17.327949
33.134274	1299.793843	17.332967
32.935832	1292.275972	17.337984
32.986401	1298.150742	17.343002
33.259782	1314.588239	17.348019
33.255561	1317.441900	17.353037
33.533904	1319.244545	17.358055
33.716168	1319.045599	17.363072
33.657072	1321.188304	17.368090
33.712392	1316.063893	17.373107
33.826720	1319.438645	17.378125
33.343606	1306.268903	17.383143
33.506972	1308.755464	17.388160
33.681382	1310.776372	17.393178
33.582238	1316.592550	17.398195
33.742243	1316.384469	17.403213
33.623106	1328.361019	17.408231
33.941572	1324.845932	17.413248
33.944027	1317.773121	17.418266
33.777173	1319.434071	17.423283
33.771575	1311.769207	17.428301
33.858458	1313.734399	17.433319
33.945220	1320.865881	17.438336
34.195206	1314.735785	17.443354
33.927862	1323.854182	17.448371
33.573147	1320.403542	17.453389
33.712707	1320.410111	17.458407
33.519786	1320.260481	17.463424
33.665708	1300.263727	17.468442
33.705323	1330.188464	17.473459
33.771244	1338.756014	17.478477
34.167342	1343.099681	17.483495
33.951245	1344.345453	17.488512
34.266187	1337.387783	17.493530
34.217617	1340.100067	17.498547
34.237211	1332.573265	17.503565
34.429122	1339.839764	17.508583
34.489120	1344.838876	17.513600
34.529667	1334.582056	17.518618
34.702924	1326.065463	17.523635
34.283835	1334.264015	17.528653
34.632390	1348.707834	17.533671
34.698216	1353.825961	17.538688
34.496569	1337.516114	17.543706
34.833709	1351.671378	17.548723
35.088915	1348.163042	17.553741
35.020227	1347.867710	17.558759
34.709708	1337.154629	17.563776
34.710083	1335.311533	17.568794
34.760402	1335.695018	17.573811
35.062660	1334.628323	17.578829
35.300951	1327.486998	17.583847
34.882308	1333.075517	17.588864
35.063117	1329.152790	17.593882
34.854643	1326.282021	17.598899
34.712336	1327.655091	17.603917
34.755277	1335.301551	17.608935
35.188725	1348.008925	17.613952
35.470865	1351.215373	17.618970
35.492996	1354.456248	17.623987
35.418682	1334.585484	17.629005
35.442724	1328.866341	17.634023
35.565521	1325.580735	17.639040
35.682963	1325.085820	17.644058
35.041387	1320.777526	17.649075
35.094819	1323.069865	17.654093
35.475153	1320.842177	17.659111
35.173865	1337.262431	17.664128
35.223174	1342.234814	17.669146
35.511434	1352.039380	17.674163
35.647262	1352.021287	17.679181
35.504431	1355.297476	17.684199
35.594734	1351.067017	17.689216
35.579073	1346.401863	17.694234
35.880153	1354.115187	17.699251
35.460905	1353.205719	17.704269
35.728074	1352.747307	17.709287
35.639952	1353.427050	17.714304
36.215813	1359.396271	17.719322
35.966226	1356.115353	17.724339
35.629188	1344.491200	17.729357
35.790549	1358.484653	17.734375
35.532768	1359.392958	17.739392
35.711938	1351.683349	17.744410
35.875636	1374.276398	17.749427
35.727591	1379.844626	17.754445
36.002143	1377.677688	17.759463
35.853657	1383.274391	17.764480
35.885510	1385.907806	17.769498
36.305162	1392.390685	17.774515
35.789987	1387.027418	17.779533
36.349724	1379.860957	17.784551
36.072738	1389.419575	17.789568
36.351855	1394.393837	17.794586
36.171787	1395.289969	17.799603
36.438722	1404.289981	17.804621
37.054202	1378.551479	17.809639
36.941671	1391.656866	17.814656
37.080457	1375.662892	17.819674
36.846126	1365.202958	17.824691
36.644435	1365.458662	17.829709
37.179961	1353.842964	17.834727
36.621365	1364.029541	17.839744
36.819632	1357.519352	17.844762
36.702297	1360.324468	17.849779
36.579093	1360.094483	17.854797
36.970756	1360.474982	17.859815
36.434145	1363.087002	17.864832
36.841287	1367.618302	17.869850
36.641919	1368.580574	17.874867
36.798561	1385.377269	17.879885
36.853523	1379.044167	17.884903
36.959209	1381.082163	17.889920
37.232104	1387.584878	17.894938
36.838014	1383.878451	17.899955
37.258911	1386.589773	17.904973
37.503119	1379.179245	17.909991
37.208066	1389.760065	17.915008
37.266174	1388.482301	17.920026
37.108946	1387.367669	17.925043
37.079968	1387.716239	17.930061
37.160831	1379.031052	17.935079
37.181471	1381.615728	17.940096
37.285620	1379.021032	17.945114
37.074964	1381.793433	17.950131
37.247033	1395.996686	17.955149
37.301277	1401.160825	17.960167
37.333062	1410.140876	17.965184
37.660377	1403.282233	17.970202
37.855086	1400.891106	17.975219
37.837578	1404.201319	17.980237
37.699795	1400.375832	17.985255
37.495743	1398.716244	17.990272
37.698156	1408.319687	17.995290
37.698839	1408.859280	18.000307
37.688053	1406.645522	18.005325
38.071641	1406.910517	18.010343
37.831116	1417.186151	18.015360
38.274609	1431.438429	18.020378
38.225732	1431.338816	18.025395
38.064547	1422.723091	18.030413
38.025812	1424.389225	18.035431
37.960388	1440.469647	18.040448
37.916444	1437.781374	18.045466
37.986409	1436.978298	18.050483
37.896195	1437.560537	18.055501
38.119571	1427.502248	18.060519
38.354422	1448.013934	18.065536
38.354523	1441.152892	18.070554
38.795267	1443.782215	18.075571
38.333391	1446.552958	18.080589
38.497289	1437.280348	18.085607
38.104237	1451.616371	18.090624
38.808103	1447.564327	18.095642
39.048122	1450.891008	18.100659
38.691066	1450.391534	18.105677
38.793250	1431.392458	18.110695
38.675623	1434.778327	18.115712
38.632195	1440.049303	18.120730
38.831359	1438.812553	18.125747
38.683722	1450.411779	18.130765
39.286552	1443.349000	18.135783
39.179620	1455.528860	18.140800
38.760224	1448.907119	18.145818
38.945652	1447.312741	18.150835
39.009500	1454.463646	18.155853
38.851043	1457.303623	18.160871
39.034156	1460.768616	18.165888
39.114832	1458.666760	18.170906
39.242634	1453.941229	18.175923
39.283114	1453.452056	18.180941
39.306070	1454.186986	18.185959
39.331268	1454.504978	18.190976
39.094705	1454.497891	18.195994
39.193428	1446.703010	18.201011
39.268526	1449.335971	18.206029
39.357189	1444.749124	18.211047
39.118101	1450.432629	18.216064
39.627046	1463.304991	18.221082
39.740500	1476.999915	18.226099
39.561701	1475.352142	18.231117
39.638048	1475.488543	18.236135
39.354826	1490.659500	18.241152
39.390570	1479.519678	18.246170
39.606459	1478.015204	18.251187
39.748788	1491.118605	18.256205
39.764346	1487.811900	18.261223
39.766205	1481.073650	18.266240
39.838213	1478.540783	18.271258
40.153425	1470.421624	18.276275
39.901652	1480.493918	18.281293
39.876625	1475.293683	18.286311
39.751688	1484.093188	18.291328
39.858761	1486.572815	18.296346
40.143881	1488.115627	18.301363
40.229253	1511.519581	18.306381
40.301858	1502.441131	18.311399
40.437207	1507.453730	18.316416
40.366688	1503.967995	18.321434
40.526409	1505.407373	18.326451
40.319148	1508.447518	18.331469
40.514750	1501.707309	18.336487
40.184160	1507.783886	18.341504
40.332526	1500.678673	18.346522
40.626386	1501.225986	18.351539
40.481571	1503.325336	18.356557
40.683773	1506.291860	18.361575
40.677806	1510.925793	18.366592
40.407812	1513.338262	18.371610
40.519822	1503.376278	18.376627
40.744324	1511.837010	18.381645
40.877899	1507.126340	18.386663
40.762303	1512.443360	18.391680
40.685427	1521.027059	18.396698
41.173053	1522.383503	18.401715
40.771759	1525.577135	18.406733
41.181648	1524.203217	18.411751
41.091313	1527.165083	18.416768
40.954838	1530.137334	18.421786
41.008651	1517.328303	18.426803
41.235888	1526.741718	18.431821
41.181582	1528.719586	18.436839
41.520677	1530.427524	18.441856
41.234913	1526.057119	18.446874
41.650519	1524.811701	18.451891
41.576252	1521.755761	18.456909
41.729060	1521.823375	18.461927
41.677182	1527.723739	18.466944
41.124307	1529.438877	18.471962
41.520576	1521.483730	18.476979
41.456815	1529.525707	18.481997
41.717660	1525.031790	18.487015
41.460958	1517.343061	18.492032
41.341961	1517.472196	18.497050
41.748802	1535.255523	18.502067
41.902643	1545.889186	18.507085
42.033352	1545.414278	18.512103
42.195366	1541.415550	18.517120
41.631640	1550.915032	18.522138
42.161097	1544.400226	18.527155
41.905585	1547.602581	18.532173
42.164953	1541.354167	18.537191
42.219231	1539.815045	18.542208
41.757400	1537.984382	18.547226
41.879433	1538.804783	18.552243
41.913027	1546.951442	18.557261
42.369440	1540.735276	18.562279
42.458372	1540.109114	18.567296
41.925811	1542.938286	18.572314
42.175864	1543.331510	18.577331
42.226635	1550.093160	18.582349
42.582999	1560.508899	18.587367
42.260152	1562.866536	18.592384
42.532238	1570.789636	18.597402
42.795645	1565.241210	18.602419
42.499266	1570.965289	18.607437
42.656373	1575.497945	18.612455
42.713902	1558.894811	18.617472
42.867865	1560.294067	18.622490
42.706182	1566.154840	18.627507
42.677497	1568.056112	18.632525
42.616136	1564.449002	18.637543
43.046207	1561.039468	18.642560
42.766640	1560.755079	18.647578
43.099860	1559.872880	18.652595
42.953499	1556.926066	18.657613
43.173324	1552.911965	18.662631
43.506258	1553.030257	18.667648
43.310034	1552.830646	18.672666
43.446693	1553.086993	18.677683
43.041848	1556.521041	18.682701
43.252190	1554.345207	18.687719
43.320049	1561.826904	18.692736
43.067398	1586.063443	18.697754
43.402328	1583.047529	18.702771
43.043663	1582.753441	18.707789
43.328818	1584.876957	18.712807
43.740182	1581.205247	18.717824
43.243270	1584.233980	18.722842
43.550802	1578.640763	18.727859
43.282538	1587.434372	18.732877
43.336330	1600.570660	18.737895
43.766586	1603.217431	18.742912
43.689740	1607.243920	18.747930
43.927291	1613.805907	18.752947
43.738889	1609.092005	18.757965
43.910968	1610.870302	18.762983
43.801029	1603.369993	18.768000
43.739575	1611.506324	18.773018
44.249826	1604.666283	18.778035
44.090424	1604.464058	18.783053
44.344214	1603.168244	18.788071
44.253407	1610.283478	18.793088
44.330258	1616.693909	18.798106
44.406522	1618.496686	18.803123
44.280998	1628.893286	18.808141
44.427114	1620.942573	18.813159
44.750594	1629.056475	18.818176
44.487677	1628.864156	18.823194
44.415113	1627.322808	18.828211
44.425913	1619.617372	18.833229
44.595272	1619.556153	18.838247
45.050215	1622.931249	18.843264
44.541188	1623.421312	18.848282
44.494574	1622.645962	18.853299
44.808081	1625.014364	18.858317
44.643295	1625.090710	18.863335
44.983191	1620.496015	18.868352
44.797178	1627.487310	18.873370
44.922913	1613.628619	18.878387
45.252650	1617.578785	18.883405
45.210668	1622.739128	18.888423
45.276237	1615.962442	18.893440
44.980553	1622.002028	18.898458
45.316072	1616.316047	18.903475
45.432291	1618.491284	18.908493
45.170158	1621.439054	18.913511
45.062903	1613.707932	18.918528
45.165902	1627.767548	18.923546
45.004786	1638.270722	18.928563
45.300417	1649.633359	18.933581
45.164938	1652.106826	18.938599
45.370527	1643.386190	18.943616
45.109922	1655.053743	18.948634
45.143444	1641.080084	18.953651
45.752815	1657.585182	18.958669
45.827516	1677.074432	18.963687
46.117848	1672.276038	18.968704
46.010693	1680.400625	18.973722
45.699998	1673.001173	18.978739
46.019472	1674.573335	18.983757
45.725559	1666.363320	18.988775
46.167141	1665.852326	18.993792
45.847599	1675.502975	18.998810
46.197815	1684.098737	19.003827
46.113545	1675.354067	19.008845
45.776911	1675.088086	19.013863
46.162966	1671.950531	19.018880
45.890287	1682.073553	19.023898
46.379794	1672.415271	19.028915
46.131615	1674.000627	19.033933
46.014191	1688.959570	19.038951
46.416534	1687.072394	19.043968
46.758817	1698.692857	19.048986
46.588313	1700.351258	19.054003
46.755887	1696.159108	19.059021
46.927517	1693.916734	19.064039
46.987854	1693.749512	19.069056
47.011454	1690.416263	19.074074
47.163103	1689.171161	19.079091
47.539151	1663.450829	19.084109
46.979501	1656.418613	19.089127
47.274198	1657.666432	19.094144
47.153206	1664.347733	19.099162
47.157858	1663.371832	19.104179
47.464583	1656.835075	19.109197
46.944742	1656.462090	19.114215
47.323563	1655.594834	19.119232
47.117672	1660.588353	19.124250
47.319614	1649.103631	19.129267
47.061977	1647.979465	19.134285
46.988896	1651.109072	19.139303
47.281911	1658.290429	19.144320
47.092514	1673.544676	19.149338
47.170640	1684.256561	19.154355
47.475722	1682.078492	19.159373
47.259957	1689.693048	19.164391
47.219653	1682.718316	19.169408
47.044117	1683.522227	19.174426
47.636450	1687.873106	19.179443
48.134123	1703.423699	19.184461
47.557812	1708.730904	19.189479
48.130976	1702.610006	19.194496
47.982147	1708.443563	19.199514
48.056555	1706.898118	19.204531
47.947197	1710.648840	19.209549
47.803338	1710.826055	19.214567
48.044217	1700.679659	19.219584
48.163437	1703.065888	19.224602
48.195311	1707.375186	19.229619
48.022683	1702.147514	19.234637
48.117291	1709.656643	19.239655
48.538051	1698.775118	19.244672
48.262153	1708.478911	19.249690
48.044184	1700.591518	19.254707
48.429353	1717.431620	19.259725
48.357939	1722.151606	19.264743
48.415934	1720.675007	19.269760
48.489343	1719.842975	19.274778
48.672769	1720.344478	19.279795
49.032640	1715.636170	19.284813
48.507546	1734.537758	19.289831
48.725737	1724.170826	19.294848
48.938914	1726.185708	19.299866
48.533002	1725.734907	19.304883
48.676845	1712.488726	19.309901
48.776186	1721.022820	19.314919
48.920339	1731.989493	19.319936
49.122091	1734.160811	19.324954
49.344536	1738.408699	19.329971
49.422670	1739.687298	19.334989
49.479288	1741.609939	19.340007
49.513096	1734.986516	19.345024
49.583385	1745.532397	19.350042
49.259601	1743.960967	19.355059
49.407194	1734.990580	19.360077
49.581975	1733.729227	19.365095
49.885859	1730.099575	19.370112
49.776525	1731.230809	19.375130
49.471460	1737.606440	19.380147
49.749567	1738.001585	19.385165
49.622161	1735.884958	19.390183
49.781842	1733.354098	19.395200
50.094215	1732.869659	19.400218
49.651958	1728.034542	19.405235
50.151131	1727.751224	19.410253
50.062116	1728.279632	19.415271
49.748161	1721.177335	19.420288
49.760206	1733.247219	19.425306
49.855855	1722.189385	19.430323
50.080912	1718.859282	19.435341
49.931523	1736.300740	19.440359
50.332228	1747.126235	19.445376
50.457574	1750.751824	19.450394
50.234532	1758.569534	19.455411
50.423225	1761.386729	19.460429
50.401555	1762.314868	19.465447
50.572074	1752.880102	19.470464
50.420315	1762.857984	19.475482
50.375990	1764.780662	19.480499
50.403514	1756.166770	19.485517
50.686641	1760.228419	19.490535
50.919522	1750.670266	19.495552
50.815460	1762.452227	19.500570
50.514336	1772.074794	19.505587
50.538033	1784.603665	19.510605
50.701123	1782.106981	19.515623
51.028525	1776.832505	19.520640
51.047243	1780.692571	19.525658
50.677219	1785.746557	19.530675
51.303095	1773.557818	19.535693
51.055106	1780.315868	19.540711
51.602166	1784.888474	19.545728
51.293512	1790.087491	19.550746
51.606314	1797.530910	19.555763
51.349762	1796.365537	19.560781
51.171934	1809.238445	19.565799
51.191998	1801.203253	19.570816
51.307145	1798.464752	19.575834
51.710643	1802.640104	19.580851
51.737745	1804.718866	19.585869
51.461615	1805.885705	19.590887
51.599362	1791.346450	19.595904
52.251480	1795.618557	19.600922
51.992565	1802.602405	19.605939
51.997377	1796.381162	19.610957
51.839639	1799.047498	19.615975
52.085260	1793.129378	19.620992
52.032632	1793.244960	19.626010
51.834485	1803.722472	19.631027
52.266863	1809.442908	19.636045
52.222743	1812.665842	19.641063
52.433483	1828.555010	19.646080
52.536420	1813.415235	19.651098
52.326168	1827.334725	19.656115
52.680483	1818.123610	19.661133
52.411828	1826.816403	19.666151
52.462443	1825.760703	19.671168
52.303766	1820.669676	19.676186
52.172507	1827.753462	19.681203
52.604282	1814.982838	19.686221
52.153739	1815.148140	19.691239
52.267059	1834.906084	19.696256
52.578327	1846.916539	19.701274
52.684089	1850.106528	19.706291
52.768637	1839.631071	19.711309
52.592178	1852.118760	19.716327
53.214703	1866.769402	19.721344
53.461817	1866.219439	19.726362
53.369051	1866.751595	19.731379
53.461987	1867.333556	19.736397
53.542626	1872.597845	19.741415
53.638778	1852.403131	19.746432
53.445621	1852.256688	19.751450
53.388927	1845.729461	19.756467
53.569568	1849.027648	19.761485
53.401126	1857.682663	19.766503
53.805167	1868.059551	19.771520
53.875023	1865.987748	19.776538
53.917208	1864.450494	19.781555
53.991333	1858.764363	19.786573
53.453980	1862.765223	19.791591
53.750116	1867.364540	19.796608
53.800984	1864.945391	19.801626
53.751182	1859.193464	19.806643
53.942362	1854.044457	19.811661
54.185839	1867.406861	19.816679
53.916204	1864.782289	19.821696
53.953202	1865.268865	19.826714
53.906562	1879.954927	19.831731
54.305558	1877.086729	19.836749
54.281707	1888.370176	19.841767
54.150094	1892.307472	19.846784
54.799590	1897.343776	19.851802
54.556873	1897.400772	19.856819
54.268206	1885.740282	19.861837
54.546909	1892.665181	19.866855
54.262075	1894.745485	19.871872
54.208027	1895.129554	19.876890
54.264743	1905.851238	19.881907
55.049983	1908.732793	19.886925
55.135224	1909.290713	19.891943
55.131521	1913.034392	19.896960
55.334680	1900.630910	19.901978
55.133299	1906.008827	19.906995
55.452629	1906.615284	19.912013
55.120354	1907.876139	19.917031
55.468661	1898.486030	19.922048
55.922384	1901.782470	19.927066
55.066200	1899.650608	19.932083
55.499317	1894.485776	19.937101
55.473414	1897.241933	19.942119
55.387436	1902.182015	19.947136
55.385360	1899.673319	19.952154
55.316706	1907.861410	19.957171
55.522093	1898.279083	19.962189
55.159091	1905.115164	19.967207
55.110782	1921.423726	19.972224
55.486164	1922.971371	19.977242
55.858152	1923.812594	19.982259
55.866981	1924.543445	19.987277
55.657385	1926.441538	19.992295
55.804541	1929.271579	19.997312
56.277326	1940.048025	20.002330
55.968230	1939.266445	20.007347
56.087087	1950.309804	20.012365
56.354937	1948.759279	20.017383
56.401115	1957.219757	20.022400
56.481459	1950.232331	20.027418
56.508355	1954.009096	20.032435
56.727286	1950.313809	20.037453
56.831441	1945.159475	20.042471
56.518458	1944.870846	20.047488
56.569305	1943.780387	20.052506
56.905212	1947.420367	20.057523
56.860586	1942.876369	20.062541
56.894041	1944.026273	20.067559
56.895548	1937.565639	20.072576
56.901811	1942.573337	20.077594
56.750027	1944.241451	20.082611
56.900413	1938.044691	20.087629
57.141187	1939.051651	20.092647
57.007771	1954.082754	20.097664
57.360709	1953.421527	20.102682
57.187030	1962.910611	20.107699
57.310378	1955.553498	20.112717
57.281435	1967.816169	20.117735
57.147165	1967.426950	20.122752
57.231254	1955.304039	20.127770
57.276578	1958.623447	20.132787
57.248603	1963.380874	20.137805
57.565065	1972.300826	20.142823
57.685411	1991.502377	20.147840
57.758501	1976.969946	20.152858
57.626108	1981.390261	20.157875
58.146094	1979.131146	20.162893
58.154312	1981.086644	20.167911
58.255573	1987.073628	20.172928
58.561340	1973.495747	20.177946
58.348835	1972.212999	20.182963
58.453631	1970.059964	20.187981
58.632973	1973.825474	20.192999
58.591638	1975.542562	20.198016
58.551688	1973.421673	20.203034
58.607793	1976.802517	20.208051
58.379536	1973.196225	20.213069
58.792433	1971.446233	20.218087
58.634277	1972.796587	20.223104
58.495106	1973.001474	20.228122
58.374590	1972.294496	20.233139
58.611889	1977.256538	20.238157
58.585708	1967.293855	20.243175
58.651920	1980.649400	20.248192
58.986679	1988.947906	20.253210
58.691138	2006.863841	20.258227
58.523378	2001.730000	20.263245
58.753420	1994.655981	20.268263
58.743283	2003.775453	20.273280
59.003897	2008.995804	20.278298
58.974364	2031.215981	20.283315
59.133117	2028.628416	20.288333
59.233425	2022.821357	20.293351
59.130813	2040.470394	20.298368
59.151509	2025.605278	20.303386
59.477061	2027.056590	20.308403
59.890733	2028.472003	20.313421
59.866421	2026.332877	20.318439
59.705961	2040.210014	20.323456
59.929690	2036.561299	20.328474
60.090779	2045.360450	20.333491
60.083740	2048.924784	20.338509
60.398478	2046.956616	20.343527
60.213821	2050.349946	20.348544
60.484206	2045.453585	20.353562
60.166610	2034.037391	20.358579
60.229160	2040.374469	20.363597
60.625424	2034.432668	20.368615
60.575845	2043.217484	20.373632
60.587596	2025.686894	20.378650
60.438598	2023.706171	20.383667
60.418168	2026.433085	20.388685
60.752542	2033.368253	20.393703
60.425674	2036.856451	20.398720
61.166553	2022.099428	20.403738
61.386626	2007.566036	20.408755
61.346853	2016.437673	20.413773
61.148042	2008.098982	20.418791
61.003547	2002.677450	20.423808
61.284915	2006.004070	20.428826
61.152859	2004.607721	20.433843
61.078423	2014.078126	20.438861
61.352694	2015.755240	20.443879
61.892302	2019.019309	20.448896
61.454622	2015.038688	20.453914
61.613004	2010.841594	20.458931
61.301880	2009.173474	20.463949
61.664998	2018.572172	20.468967
61.832243	2029.406012	20.473984
61.568158	2016.517032	20.479002
61.665326	2013.352091	20.484019
61.671221	2014.386387	20.489037
61.764851	2010.376177	20.494055
61.725051	2022.725800	20.499072
61.377987	2007.081961	20.504090
61.673527	2015.254070	20.509107
61.415096	2023.386734	20.514125
61.882412	2032.068468	20.519143
62.119946	2039.779422	20.524160
61.949478	2037.915679	20.529178
62.127454	2042.918594	20.534195
62.327558	2052.696330	20.539213
62.362343	2064.677660	20.544231
62.492983	2067.365132	20.549248
62.368402	2066.216936	20.554266
62.536084	2060.336188	20.559283
62.412473	2066.241656	20.564301
62.780198	2063.646594	20.569319
62.367007	2069.133491	20.574336
62.633613	2077.366970	20.579354
62.893549	2086.308459	20.584371
62.748387	2090.995911	20.589389
62.849904	2104.614283	20.594407
63.120743	2092.821813	20.599424
62.537511	2086.402242	20.604442
62.862917	2094.579176	20.609459
62.903801	2103.996844	20.614477
63.252779	2110.636239	20.619495
63.308899	2118.700726	20.624512
63.270016	2120.010311	20.629530
63.671780	2115.926552	20.634547
63.653980	2115.320249	20.639565
63.976515	2111.043759	20.644583
63.753529	2114.225337	20.649600
63.753655	2112.451633	20.654618
63.922061	2111.547891	20.659635
63.960513	2115.553273	20.664653
63.703549	2105.544614	20.669671
63.638183	2118.712575	20.674688
63.892436	2127.888525	20.679706
64.439863	2131.801544	20.684723
63.886934	2133.923878	20.689741
64.572422	2137.054651	20.694759
64.283688	2135.774366	20.699776
64.353093	2141.463409	20.704794
64.657832	2137.240198	20.709811
64.514738	2139.929539	20.714829
64.965531	2124.078536	20.719847
64.649539	2136.203242	20.724864
64.600719	2136.188830	20.729882
64.425117	2139.233589	20.734899
64.640443	2157.110662	20.739917
64.919227	2153.841497	20.744935
65.186918	2157.343872	20.749952
64.993227	2157.812946	20.754970
64.999699	2152.768540	20.759987
64.830350	2171.356049	20.765005
65.383759	2159.885370	20.770023
64.964847	2178.515143	20.775040
65.320575	2178.298481	20.780058
65.679618	2189.010840	20.785075
65.372529	2192.533842	20.790093
65.839979	2193.473742	20.795111
65.793748	2198.985242	20.800128
65.759044	2193.432832	20.805146
65.907824	2189.821078	20.810163
65.499189	2189.607396	20.815181
65.936311	2187.613726	20.820199
65.878878	2187.909961	20.825216
65.968013	2196.319637	20.830234
66.403648	2206.723334	20.835251
66.314061	2212.876007	20.840269
66.526412	2212.299920	20.845287
66.301676	2213.193620	20.850304
66.688116	2211.936947	20.855322
66.814576	2219.564386	20.860339
66.575811	2222.394972	20.865357
66.718479	2216.874731	20.870375
66.875563	2217.639176	20.875392
66.922667	2215.261599	20.880410
66.937757	2216.105101	20.885427
66.705469	2213.045396	20.890445
66.901004	2209.489434	20.895463
66.644186	2207.102666	20.900480
66.835557	2206.735013	20.905498
66.811343	2203.756329	20.910515
66.803174	2215.147988	20.915533
67.460707	2224.320769	20.920551
67.247518	2232.307570	20.925568
67.348715	2237.578213	20.930586
67.734062	2226.948095	20.935603
67.733331	2235.883158	20.940621
67.978024	2231.218011	20.945639
68.027137	2236.171736	20.950656
67.780732	2229.869770	20.955674
68.013768	2223.682056	20.960691
67.788552	2227.245891	20.965709
68.094233	2232.926349	20.970727
67.920186	2239.278473	20.975744
67.758030	2229.987106	20.980762
67.896843	2226.184383	20.985779
67.871139	2231.108799	20.990797
67.679965	2226.111119	20.995815
68.234412	2241.697472	21.000832
68.170009	2249.938706	21.005850
68.335634	2252.248304	21.010867
68.163798	2254.607618	21.015885
68.321983	2253.172089	21.020903
68.332232	2248.922401	21.025920
67.975721	2262.855675	21.030938
68.251361	2277.658841	21.035955
68.544011	2276.000252	21.040973
68.619742	2286.384637	21.045991
68.849998	2291.111162	21.051008
69.068939	2302.199024	21.056026
69.282035	2305.918285	21.061043
69.252778	2309.170540	21.066061
69.278698	2306.982482	21.071079
69.432247	2307.324565	21.076096
69.064668	2306.132367	21.081114
69.510805	2309.250174	21.086131
69.624705	2309.027213	21.091149
69.644565	2306.540273	21.096167
69.456632	2303.836556	21.101184
69.607011	2318.441610	21.106202
69.830779	2322.231794	21.111219
69.998563	2320.655886	21.116237
69.897996	2325.854015	21.121255
69.538214	2334.545549	21.126272
70.033451	2335.601036	21.131290
69.902242	2326.718221	21.136307
69.979521	2327.154314	21.141325
70.063690	2346.570216	21.146343
70.040715	2353.315319	21.151360
70.474051	2349.920908	21.156378
70.534619	2358.944267	21.161395
69.923440	2359.128426	21.166413
70.166769	2367.902227	21.171431
70.987468	2367.013051	21.176448
70.866338	2384.217156	21.181466
70.844392	2379.697899	21.186483
70.836948	2386.427956	21.191501
70.873322	2380.674985	21.196519
71.230433	2374.502498	21.201536
70.953961	2373.943026	21.206554
70.942092	2377.104197	21.211571
70.829000	2387.439321	21.216589
70.981144	2388.668498	21.221607
71.102345	2397.398325	21.226624
71.177038	2393.801294	21.231642
70.918385	2407.062871	21.236659
71.482028	2411.557296	21.241677
71.557163	2414.357668	21.246695
71.555316	2418.457804	21.251712
71.582642	2420.309360	21.256730
72.177929	2430.249472	21.261747
72.272248	2443.714578	21.266765
72.383572	2436.015135	21.271783
72.410419	2439.681546	21.276800
72.191885	2438.649042	21.281818
72.784518	2436.773008	21.286835
72.570906	2444.308641	21.291853
72.567851	2428.556883	21.296871
72.766972	2423.835704	21.301888
72.488112	2416.484609	21.306906
72.907135	2419.461502	21.311923
73.347349	2426.304494	21.316941
73.451323	2414.891443	21.321959
72.979947	2400.311417	21.326976
72.745433	2402.333396	21.331994
73.149485	2397.352875	21.337011
73.275935	2397.301534	21.342029
73.296066	2391.061904	21.347047
73.300568	2392.954907	21.352064
73.157779	2403.158979	21.357082
73.828702	2399.941952	21.362099
73.564434	2412.008241	21.367117
73.560116	2417.623706	21.372135
73.571881	2412.486870	21.377152
73.737188	2416.728091	21.382170
74.092477	2415.280605	21.387187
73.868776	2421.795223	21.392205
73.601852	2419.687749	21.397223
73.596849	2418.965810	21.402240
73.866599	2420.943504	21.407258
73.834494	2421.967996	21.412275
73.595387	2429.318250	21.417293
74.140710	2436.851752	21.422311
74.003046	2442.371340	21.427328
73.857128	2446.841229	21.432346
74.033006	2448.353900	21.437363
74.345097	2469.283889	21.442381
74.284279	2469.706904	21.447399
74.364569	2468.835886	21.452416
74.407914	2481.046551	21.457434
74.989618	2486.052616	21.462451
74.739328	2492.000163	21.467469
74.975543	2499.812519	21.472487
75.191291	2497.171773	21.477504
74.800229	2492.820783	21.482522
75.122951	2503.195001	21.487539
74.999740	2504.003374	21.492557
74.881953	2509.807077	21.497575
75.301380	2516.694390	21.502592
75.083892	2527.266881	21.507610
75.531654	2517.955554	21.512627
75.409953	2513.814849	21.517645
75.288297	2538.704406	21.522663
75.489538	2542.166770	21.527680
75.674930	2549.494751	21.532698
76.285698	2546.271343	21.537715
75.958744	2551.590221	21.542733
76.109301	2548.508351	21.547751
76.324986	2548.136882	21.552768
76.463555	2552.543289	21.557786
76.488863	2552.009122	21.562803
76.349127	2551.390347	21.567821
76.627233	2570.709828	21.572839
76.923588	2567.447304	21.577856
77.019314	2572.106608	21.582874
76.807531	2575.333853	21.587891
76.989832	2570.858296	21.592909
76.728289	2571.470569	21.597927
77.020720	2573.488912	21.602944
76.790718	2574.184617	21.607962
77.310380	2567.109184	21.612979
77.272063	2566.424021	21.617997
77.147006	2566.424709	21.623015
77.234736	2556.241859	21.628032
77.050649	2563.602484	21.633050
77.350683	2576.966025	21.638067
77.752334	2590.938575	21.643085
77.330613	2584.515611	21.648103
77.883092	2583.968285	21.653120
77.700719	2585.114171	21.658138
77.818656	2580.468794	21.663155
77.870822	2580.820455	21.668173
78.092041	2591.437871	21.673191
78.160708	2581.485237	21.678208
78.201302	2586.352021	21.683226
77.901618	2584.230723	21.688243
78.085958	2603.088348	21.693261
77.925409	2615.829723	21.698279
78.161907	2611.522410	21.703296
78.228024	2619.516120	21.708314
78.453577	2630.461121	21.713331
78.442240	2642.405876	21.718349
78.912231	2649.032824	21.723367
78.909309	2646.719840	21.728384
79.012536	2649.440100	21.733402
79.037725	2663.705245	21.738419
79.274258	2636.632447	21.743437
79.120485	2646.525917	21.748455
79.275884	2639.545401	21.753472
79.262557	2649.047596	21.758490
79.580969	2657.352131	21.763507
79.591954	2666.194042	21.768525
79.771033	2669.025511	21.773543
79.786214	2662.837062	21.778560
79.930242	2665.109067	21.783578
80.016611	2658.508632	21.788595
79.827152	2659.690350	21.793613
79.939968	2663.576894	21.798631
80.112391	2651.670075	21.803648
80.046683	2655.445716	21.808666
79.857510	2657.555304	21.813683
80.391732	2667.413587	21.818701
80.539507	2680.179293	21.823719
80.107450	2682.639399	21.828736
80.149526	2687.540696	21.833754
80.238262	2696.761806	21.838771
80.570911	2686.016585	21.843789
80.621356	2704.585990	21.848807
80.892563	2706.453021	21.853824
80.756733	2708.936156	21.858842
80.923652	2712.536490	21.863859
81.559286	2708.220275	21.868877
81.198555	2711.486661	21.873895
81.314467	2709.609541	21.878912
81.396240	2702.779408	21.883930
81.450285	2720.145760	21.888947
81.460203	2719.771808	21.893965
81.100815	2737.269229	21.898983
81.762055	2727.135302	21.904000
81.803889	2728.025136	21.909018
81.708186	2724.770354	21.914035
81.910842	2741.261272	21.919053
81.671539	2738.707566	21.924071
81.973559	2748.327685	21.929088
81.545143	2756.774523	21.934106
81.702941	2758.059651	21.939123
82.237076	2761.892832	21.944141
82.285687	2784.130101	21.949159
82.445005	2774.456685	21.954176
81.981435	2777.837037	21.959194
82.226372	2785.140003	21.964211
82.558708	2782.092738	21.969229
82.629627	2797.401837	21.974247
83.195576	2798.638803	21.979264
83.021482	2805.486656	21.984282
83.422165	2804.716923	21.989299
83.297556	2804.026333	21.994317
83.120718	2806.512750	21.999335
83.362204	2799.521841	22.004352
83.149594	2803.961236	22.009370
83.477174	2792.658099	22.014387
83.532046	2794.666344	22.019405
83.090563	2802.259921	22.024423
83.456416	2813.552328	22.029440
83.362890	2822.000383	22.034458
83.243287	2823.931812	22.039475
83.457633	2829.680426	22.044493
83.439129	2848.680556	22.049511
83.880134	2849.065988	22.054528
84.015913	2857.563351	22.059546
84.034342	2859.441596	22.064563
84.531803	2868.112702	22.069581
84.420551	2872.826606	22.074599
84.756038	2867.127616	22.079616
84.965347	2869.891257	22.084634
84.646161	2867.997071	22.089651
84.595561	2869.819851	22.094669
84.917653	2873.780964	22.099687
85.208945	2875.745865	22.104704
85.188886	2874.300339	22.109722
85.253155	2875.287664	22.114739
85.323108	2874.115250	22.119757
85.236239	2872.673879	22.124775
85.561464	2879.150003	22.129792
85.390933	2883.365046	22.134810
85.495804	2887.944094	22.139827
85.973808	2887.572552	22.144845
85.744345	2896.591121	22.149863
85.921077	2885.283154	22.154880
86.002496	2889.016855	22.159898
85.819972	2890.235376	22.164915
86.098460	2881.622657	22.169933
86.477214	2902.668955	22.174951
86.343111	2907.045576	22.179968
86.519655	2907.677598	22.184986
86.298127	2908.962199	22.190003
86.638851	2910.565863	22.195021
86.394791	2912.804016	22.200039
86.775296	2904.225803	22.205056
86.944726	2903.669045	22.210074
86.530093	2902.086493	22.215091
86.832202	2910.901851	22.220109
86.935942	2923.740909	22.225127
87.385337	2933.271757	22.230144
87.067389	2933.391039	22.235162
87.274311	2936.009879	22.240179
87.697227	2935.331344	22.245197
87.159285	2930.043767	22.250215
87.582895	2923.052683	22.255232
87.863697	2932.729881	22.260250
87.560952	2947.409594	22.265267
87.939365	2945.589166	22.270285
87.772080	2957.653249	22.275303
88.165139	2949.240327	22.280320
88.380149	2955.386562	22.285338
88.231218	2954.939649	22.290355
88.252422	2941.418250	22.295373
88.240505	2949.168679	22.300391
88.497742	2944.094231	22.305408
88.455514	2951.439100	22.310426
88.565543	2971.830056	22.315443
88.914605	2980.537092	22.320461
88.566165	2974.396036	22.325479
88.807218	2973.424057	22.330496
88.860572	2974.189006	22.335514
88.946174	2978.124069	22.340531
89.062575	2964.571957	22.345549
88.647648	2984.767425	22.350567
89.035533	2994.200630	22.355584
89.045232	3001.332229	22.360602
89.046861	3003.834899	22.365619
89.281499	2995.992805	22.370637
89.685605	3015.813801	22.375655
89.377628	3025.747419	22.380672
89.904289	3030.866418	22.385690
89.785559	3029.972899	22.390707
89.674151	3022.358602	22.395725
89.519308	3041.443420	22.400743
89.763337	3047.155891	22.405760
90.233629	3052.807664	22.410778
89.981340	3056.931401	22.415795
90.218897	3059.315053	22.420813
90.455099	3071.903058	22.425831
90.339203	3083.542549	22.430848
90.487883	3075.669699	22.435866
90.476714	3085.351692	22.440883
90.552293	3083.638665	22.445901
90.797177	3104.346360	22.450919
90.708575	3107.008369	22.455936
91.364236	3109.383335	22.460954
90.752255	3109.539216	22.465971
91.135198	3111.092096	22.470989
91.617753	3121.776194	22.476007
91.562738	3125.572351	22.481024
91.560442	3131.642223	22.486042
91.932530	3128.995829	22.491059
91.849247	3133.440293	22.496077
92.058669	3131.924073	22.501095
91.975186	3133.556344	22.506112
91.739061	3134.041559	22.511130
92.055207	3150.773884	22.516147
92.444678	3143.772283	22.521165
92.277571	3148.621260	22.526183
92.407234	3158.016101	22.531200
92.357630	3156.770869	22.536218
92.308454	3168.589337	22.541235
92.612909	3177.871584	22.546253
92.523587	3181.114469	22.551271
92.565199	3187.590951	22.556288
92.859106	3186.919995	22.561306
92.764543	3198.717187	22.566323
93.256586	3207.136805	22.571341
93.394085	3205.357253	22.576359
93.484983	3205.769140	22.581376
93.798037	3204.710119	22.586394
93.575845	3208.374672	22.591411
93.748944	3189.785571	22.596429
93.762551	3214.156177	22.601447
93.933225	3223.759254	22.606464
94.010774	3218.965384	22.611482
93.700001	3223.341354	22.616499
94.249237	3219.095370	22.621517
94.036797	3231.949465	22.626535
94.185414	3230.206043	22.631552
94.389937	3235.495510	22.636570
94.466708	3258.811554	22.641587
94.322474	3260.311322	22.646605
94.567226	3258.593868	22.651623
94.423868	3256.198650	22.656640
94.843028	3264.563432	22.661658
94.686396	3287.433170	22.666675
95.228891	3285.539658	22.671693
95.377023	3281.340719	22.676711
94.852912	3279.611158	22.681728
95.013871	3285.519784	22.686746
95.094474	3295.174885	22.691763
95.653347	3302.927571	22.696781
95.600227	3308.926558	22.701799
95.281669	3314.736724	22.706816
95.557198	3304.145276	22.711834
95.515203	3314.876951	22.716851
96.025686	3321.977562	22.721869
96.152700	3316.759287	22.726887
96.249930	3326.995714	22.731904
96.557575	3318.346657	22.736922
96.697554	3323.602074	22.741939
96.887265	3324.260455	22.746957
96.534346	3325.549888	22.751975
96.147504	3322.949775	22.756992
96.701514	3321.376397	22.762010
96.619463	3350.332481	22.767027
96.893848	3347.814990	22.772045
96.655397	3354.439567	22.777063
96.606848	3360.078037	22.782080
96.935586	3362.993484	22.787098
97.055784	3379.115992	22.792115
97.196212	3378.121883	22.797133
97.295250	3375.322543	22.802151
97.758603	3391.463895	22.807168
97.530945	3398.127829	22.812186
97.632487	3407.666083	22.817203
97.799995	3402.621348	22.822221
98.153001	3400.261972	22.827239
97.821982	3424.986704	22.832256
98.197093	3421.888443	22.837274
98.085294	3425.324271	22.842291
98.199308	3423.194871	22.847309
98.484119	3428.099371	22.852327
98.709824	3444.356911	22.857344
99.194711	3449.772957	22.862362
98.902417	3451.652600	22.867379
98.777450	3447.802572	22.872397
99.080238	3445.447903	22.877415
99.012999	3445.635222	22.882432
99.562173	3443.472362	22.887450
99.349598	3449.518471	22.892467
99.447081	3458.609192	22.897485
99.799952	3461.451435	22.902503
99.484028	3475.682287	22.907520
99.494002	3465.350136	22.912538
99.280865	3471.020738	22.917555
99.824089	3472.835765	22.922573
100.160004	3475.967892	22.927591
100.245002	3495.470122	22.932608
100.529799	3489.485341	22.937626
100.548226	3503.575455	22.942643
100.217365	3499.924959	22.947661
100.712212	3494.851008	22.952679
100.775999	3496.813746	22.957696
100.838413	3485.030929	22.962714
100.502866	3496.320027	22.967731
100.978627	3515.713713	22.972749
101.065310	3507.219125	22.977767
100.890134	3516.412563	22.982784
100.904925	3518.288290	22.987802
100.829672	3516.513633	22.992819
100.987662	3532.652452	22.997837
101.215805	3535.902476	23.002855
101.339260	3538.023156	23.007872
101.614975	3539.927445	23.012890
101.696246	3554.676894	23.017907
101.697628	3577.373894	23.022925
102.104627	3574.545212	23.027943
101.584748	3574.595130	23.032960
102.030651	3572.764069	23.037978
102.095865	3588.361958	23.042995
102.222212	3598.404597	23.048013
102.660038	3599.238747	23.053031
102.858302	3598.434414	23.058048
103.448426	3581.635503	23.063066
103.349642	3587.944744	23.068083
103.111357	3584.585891	23.073101
103.548542	3581.351625	23.078119
103.286791	3576.740228	23.083136
104.100829	3574.892523	23.088154
104.178472	3570.130108	23.093171
103.913119	3567.154259	23.098189
103.916345	3567.532545	23.103207
104.009064	3574.806024	23.108224
104.262736	3566.837604	23.113242
104.157202	3569.944220	23.118259
104.228081	3563.292224	23.123277
104.384439	3565.997986	23.128295
104.138745	3566.532055	23.133312
104.663507	3559.468067	23.138330
104.455904	3566.267799	23.143347
104.456524	3568.003716	23.148365
104.391663	3557.863148	23.153383
104.689326	3566.632178	23.158400
104.874437	3565.583714	23.163418
104.634271	3585.042294	23.168435
104.729620	3594.123948	23.173453
104.774591	3590.676528	23.178471
104.695216	3602.496853	23.183488
105.359361	3608.131058	23.188506
105.395269	3613.816345	23.193523
104.952574	3622.234256	23.198541
105.727947	3628.131956	23.203559
106.031264	3636.092111	23.208576
105.952488	3642.429800	23.213594
106.064070	3643.889520	23.218611
105.923711	3647.257268	23.223629
106.181093	3638.726406	23.228647
105.951063	3655.898281	23.233664
105.978322	3660.464434	23.238682
106.148614	3672.138375	23.243699
106.135078	3670.278280	23.248717
106.309113	3683.460377	23.253735
106.045631	3696.651058	23.258752
106.765633	3695.515628	23.263770
106.972338	3716.813933	23.268787
106.897740	3732.784207	23.273805
106.916566	3731.730221	23.278823
106.691518	3742.361418	23.283840
107.267223	3744.572243	23.288858
106.957355	3753.307135	23.293875
106.741304	3769.930876	23.298893
106.866305	3779.030072	23.303911
107.098209	3780.126909	23.308928
107.732054	3805.688937	23.313946
108.054268	3813.336885	23.318963
108.019577	3814.595433	23.323981
108.083168	3810.958827	23.328999
108.085658	3830.155550	23.334016
108.503515	3832.406898	23.339034
108.493093	3839.093773	23.344051
108.537893	3840.488219	23.349069
109.232755	3845.748390	23.354087
108.716409	3840.621290	23.359104
108.660354	3849.486908	23.364122
109.281193	3861.024099	23.369139
109.327139	3875.116503	23.374157
109.712294	3862.253896	23.379175
109.702667	3876.774807	23.384192
109.873841	3857.137404	23.389210
109.894400	3855.401361	23.394227
109.843071	3864.023204	23.399245
110.047836	3872.503925	23.404263
109.952781	3871.991733	23.409280
109.996259	3879.670753	23.414298
110.295309	3890.396684	23.419315
110.157978	3893.271607	23.424333
110.467279	3881.781274	23.429351
110.458008	3889.594818	23.434368
110.681868	3895.007705	23.439386
110.608456	3898.323978	23.444403
110.838097	3897.745133	23.449421
111.317237	3899.939543	23.454439
111.125069	3897.485603	23.459456
111.106510	3908.453844	23.464474
111.496269	3907.376454	23.469491
111.674233	3929.844221	23.474509
111.647543	3921.095752	23.479527
111.882954	3928.896230	23.484544
111.936009	3919.778595	23.489562
112.325059	3923.764172	23.494579
111.988386	3920.130281	23.499597
112.581447	3915.716296	23.504615
112.041294	3914.497363	23.509632
112.278473	3934.181389	23.514650
112.650339	3939.340685	23.519667
112.703188	3946.910948	23.524685
112.595795	3942.376279	23.529703
112.663359	3937.006163	23.534720
112.909404	3949.668992	23.539738
113.524484	3959.900400	23.544755
113.016988	3968.319153	23.549773
113.170305	3965.126138	23.554791
113.656685	3958.636162	23.559808
113.106904	3956.320307	23.564826
113.692602	3973.705573	23.569843
113.664306	3986.158896	23.574861
113.825588	3988.882889	23.579879
113.857016	3991.109576	23.584896
114.001811	3993.826684	23.589914
114.321789	3987.122881	23.594931
114.081631	4005.256220	23.599949
113.897880	4001.595198	23.604967
114.152794	4018.580966	23.609984
114.305439	4022.518379	23.615002
114.722229	4035.924682	23.620019
114.504550	4052.788824	23.625037
114.781947	4040.870960	23.630055
114.898366	4046.587959	23.635072
114.813786	4070.309096	23.640090
115.250689	4069.833501	23.645107
114.988801	4079.599494	23.650125
115.211845	4077.446623	23.655143
115.119717	4100.203117	23.660160
115.585353	4100.086008	23.665178
115.821531	4107.646555	23.670195
115.787088	4127.682676	23.675213
115.883835	4120.701311	23.680231
115.993092	4132.391423	23.685248
115.722901	4134.558063	23.690266
115.963624	4151.448329	23.695283
115.927277	4160.298385	23.700301
116.495323	4156.895165	23.705319
116.439260	4173.696221	23.710336
116.610546	4179.332068	23.715354
117.246789	4184.740407	23.720371
116.654663	4191.281814	23.725389
116.869985	4194.941148	23.730407
117.171938	4208.447638	23.735424
117.246897	4215.061303	23.740442
117.588206	4210.039619	23.745459
117.596984	4224.586332	23.750477
118.121824	4228.361316	23.755495
118.002842	4232.436024	23.760512
118.202165	4232.329073	23.765530
118.675718	4215.964494	23.770547
118.593360	4220.677376	23.775565
118.906737	4212.412084	23.780583
118.800021	4219.366702	23.785600
118.571456	4215.160280	23.790618
118.929683	4224.279977	23.795635
118.922034	4250.905854	23.800653
119.169033	4256.321537	23.805671
119.343968	4251.881442	23.810688
119.505259	4244.744721	23.815706
119.687684	4245.669421	23.820723
119.869180	4243.955474	23.825741
119.908912	4250.565201	23.830759
120.049891	4241.433630	23.835776
119.939237	4255.191028	23.840794
120.393182	4262.203021	23.845811
120.385166	4272.431220	23.850829
120.369631	4276.707526	23.855847
120.418725	4277.015512	23.860864
120.153146	4276.372201	23.865882
120.537553	4270.188486	23.870899
120.621389	4281.538623	23.875917
120.508413	4288.588941	23.880935
120.930151	4288.485023	23.885952
120.902268	4293.470314	23.890970
121.359699	4302.082101	23.895987
121.028136	4316.896848	23.901005
121.327844	4314.990769	23.906023
121.341633	4309.663689	23.911040
121.335455	4324.780989	23.916058
121.475134	4329.175031	23.921075
121.298283	4340.184114	23.926093
121.435601	4353.798574	23.931111
121.710737	4367.625031	23.936128
121.693557	4380.547197	23.941146
121.938117	4391.490290	23.946163
122.227701	4406.621294	23.951181
122.265988	4414.408674	23.956199
122.772282	4434.527710	23.961216
122.399142	4430.760543	23.966234
122.591530	4431.898333	23.971251
122.864190	4450.251637	23.976269
123.308608	4457.271512	23.981287
123.407639	4455.368450	23.986304
123.387316	4455.513707	23.991322
123.953390	4461.880070	23.996339
123.643480	4481.568333	24.001357
124.019539	4481.600986	24.006375
124.005107	4486.669448	24.011392
123.894613	4485.323186	24.016410
124.459380	4475.032959	24.021427
124.329267	4488.080214	24.026445
124.275047	4494.123955	24.031463
124.661935	4491.774916	24.036480
124.422740	4508.387175	24.041498
124.921110	4502.602184	24.046515
124.871101	4513.073835	24.051533
124.759791	4525.568941	24.056551
124.987677	4535.599348	24.061568
125.101076	4544.583956	24.066586
125.472758	4539.027131	24.071603
125.625310	4550.448740	24.076621
125.628290	4553.462766	24.081639
125.533647	4552.110859	24.086656
125.509814	4569.128187	24.091674
125.938040	4567.422903	24.096691
125.969135	4586.382361	24.101709
125.938483	4589.407975	24.106727
126.436856	4602.258997	24.111744
126.459687	4624.038556	24.116762
126.392111	4613.957796	24.121779
126.468400	4628.415343	24.126797
126.721825	4638.132467	24.131815
127.215159	4635.791985	24.136832
127.027224	4641.544229	24.141850
127.356336	4644.459827	24.146867
127.374472	4651.855901	24.151885
128.164725	4645.737894	24.156903
128.575907	4646.648872	24.161920
128.573904	4650.418103	24.166938
128.432462	4651.636615	24.171955
128.706343	4655.144825	24.176973
128.602347	4648.936490	24.181991
128.421588	4644.403670	24.187008
128.605523	4646.609701	24.192026
128.452730	4644.187368	24.197043
128.417195	4653.552049	24.202061
129.010423	4658.541141	24.207079
129.087002	4670.277754	24.212096
128.967056	4683.333026	24.217114
129.007693	4689.851233	24.222131
129.547831	4691.793133	24.227149
129.753740	4688.178247	24.232167
129.739231	4679.048722	24.237184
129.486116	4693.289622	24.242202
129.587497	4714.106867	24.247219
129.699235	4719.565977	24.252237
129.797700	4717.088487	24.257255
129.960119	4734.698626	24.262272
130.050678	4744.820108	24.267290
130.678218	4755.731829	24.272307
130.989050	4780.439914	24.277325
130.560007	4776.858199	24.282343
130.883535	4772.104297	24.287360
130.636810	4787.698426	24.292378
130.992216	4794.366218	24.297395
131.101877	4796.268250	24.302413
131.168596	4803.953489	24.307431
132.510096	4795.836204	24.312448
132.395605	4806.116105	24.317466
132.846273	4802.178762	24.322483
132.913433	4795.489020	24.327501
132.525430	4781.569504	24.332519
132.881422	4767.154654	24.337536
133.134226	4773.847982	24.342554
133.184913	4777.186008	24.347571
133.130726	4769.022242	24.352589
132.576595	4774.440487	24.357607
133.062380	4781.229892	24.362624
132.740631	4796.725304	24.367642
132.943039	4798.189828	24.372659
133.447000	4805.683462	24.377677
133.434154	4799.012566	24.382695
133.717870	4816.275501	24.387712
133.517382	4828.273425	24.392730
133.795039	4825.742595	24.397747
134.152521	4829.556553	24.402765
134.087856	4833.995358	24.407783
134.121509	4846.556357	24.412800
133.919593	4852.200377	24.417818
134.145043	4860.700416	24.422835
134.263317	4870.441996	24.427853
134.130673	4885.541695	24.432871
134.476828	4894.660466	24.437888
134.578723	4908.886951	24.442906
134.611515	4905.179195	24.447923
135.097878	4932.028546	24.452941
135.218067	4944.793859	24.457959
135.347202	4946.951694	24.462976
135.380310	4958.247070	24.467994
135.443249	4970.068084	24.473011
135.836760	4973.794357	24.478029
135.776053	4989.807750	24.483047
135.853660	4998.637204	24.488064
136.073911	5008.116667	24.493082
136.191849	5016.175918	24.498099
136.321407	5026.269350	24.503117
136.798284	5031.617686	24.508135
136.811651	5046.413707	24.513152
136.913865	5050.794855	24.518170
137.448979	5058.975006	24.523187
137.195218	5060.138541	24.528205
137.400063	5078.155879	24.533223
137.568599	5081.620701	24.538240
137.629188	5089.575332	24.543258
137.555856	5097.850824	24.548275
137.703877	5104.434427	24.553293
137.952354	5106.513608	24.558311
138.374438	5119.717863	24.563328
138.064417	5130.372650	24.568346
138.287540	5131.972846	24.573363
138.774217	5143.434023	24.578381
138.775414	5164.791475	24.583399
138.729124	5154.539781	24.588416
138.784759	5166.191610	24.593434
139.365833	5185.914657	24.598451
139.815292	5182.286771	24.603469
139.577223	5181.402370	24.608487
140.004251	5177.228748	24.613504
140.060667	5188.391194	24.618522
140.034725	5194.629603	24.623539
140.666845	5203.728981	24.628557
140.502915	5206.425192	24.633575
140.482757	5202.596250	24.638592
140.796827	5204.153795	24.643610
140.849859	5219.515091	24.648627
140.954829	5228.027864	24.653645
140.873245	5243.381859	24.658663
141.248448	5232.126571	24.663680
141.281549	5243.011763	24.668698
141.412899	5255.096870	24.673715
141.502303	5260.471255	24.678733
141.712575	5270.858371	24.683751
141.786691	5265.256404	24.688768
142.194779	5269.842214	24.693786
142.073009	5296.383329	24.698803
142.076029	5285.394654	24.703821
142.077211	5278.939192	24.708839
142.343431	5288.383190	24.713856
142.591857	5310.497551	24.718874
142.793111	5308.294289	24.723891
143.153897	5304.888609	24.728909
143.166751	5309.359578	24.733927
143.176661	5316.078533	24.738944
143.469537	5327.260838	24.743962
143.405591	5323.830153	24.748979
143.590515	5327.728071	24.753997
144.076529	5331.547253	24.759015
144.303938	5342.793486	24.764032
144.164697	5352.225280	24.769050
144.111370	5360.541950	24.774067
144.296081	5356.084273	24.779085
144.286999	5362.661016	24.784103
144.515988	5373.960684	24.789120
144.287095	5381.701950	24.794138
144.853878	5389.558468	24.799155
145.300071	5400.413761	24.804173
145.196093	5417.712751	24.809191
145.617922	5407.254997	24.814208
145.280983	5423.100550	24.819226
145.558387	5434.818819	24.824243
145.895542	5440.987801	24.829261
145.524785	5452.068968	24.834279
145.568684	5459.994809	24.839296
145.652711	5474.199281	24.844314
145.556933	5485.808745	24.849331
146.234993	5499.667639	24.854349
146.126201	5519.739034	24.859367
146.685013	5516.131832	24.864384
146.661527	5527.524813	24.869402
146.668288	5549.538431	24.874419
146.863668	5550.094995	24.879437
147.144658	5573.066345	24.884455
147.670262	5580.190735	24.889472
147.403136	5581.065980	24.894490
147.178963	5609.561794	24.899507
147.943368	5610.319629	24.904525
147.883552	5624.328942	24.909543
147.865866	5630.547266	24.914560
148.396065	5641.550532	24.919578
148.320711	5657.506827	24.924595
148.518537	5659.814977	24.929613
148.703159	5667.324274	24.934631
149.206086	5682.969026	24.939648
149.188925	5682.138378	24.944666
148.915351	5693.977856	24.949683
149.461944	5704.757624	24.954701
149.631486	5720.369407	24.959719
149.962710	5721.921154	24.964736
150.204038	5715.841444	24.969754
150.349377	5737.874615	24.974771
150.659043	5731.137069	24.979789
150.447859	5744.785070	24.984807
150.651657	5740.081244	24.989824
151.083681	5738.817201	24.994842
150.731448	5756.957208	24.999859
151.679617	5765.499124	25.004877
151.508678	5766.558181	25.009895
151.723464	5763.014299	25.014912
151.924687	5760.249093	25.019930
151.545978	5757.865160	25.024947
152.308620	5766.897023	25.029965
152.077168	5774.168504	25.034983
152.036256	5781.855234	25.040000
152.020028	5785.800547	25.045018
152.472394	5788.412918	25.050035
152.684311	5787.609511	25.055053
152.204207	5807.224847	25.060071
152.389095	5807.786221	25.065088
152.571925	5806.892668	25.070106
152.662240	5830.377192	25.075123
152.843935	5845.892476	25.080141
152.838765	5854.495401	25.085159
153.511597	5857.442581	25.090176
153.853136	5858.298244	25.095194
153.811068	5870.653995	25.100211
153.883700	5885.592934	25.105229
154.275378	5895.633155	25.110247
154.309742	5906.995212	25.115264
154.612063	5897.395595	25.120282
154.843273	5915.419100	25.125299
155.171641	5911.989978	25.130317
154.760358	5923.548132	25.135335
155.331270	5926.208243	25.140352
155.431188	5934.131827	25.145370
155.174194	5936.141928	25.150387
155.874211	5940.000318	25.155405
155.614210	5939.883245	25.160423
155.813489	5969.932689	25.165440
156.189527	5965.204978	25.170458
156.051889	5962.846386	25.175475
156.559581	5977.780376	25.180493
156.293428	5992.965040	25.185511
156.838213	5995.837601	25.190528
156.903264	5996.379873	25.195546
156.854166	6017.010676	25.200563
157.191584	6025.692594	25.205581
157.143836	6032.483981	25.210599
156.983998	6042.604372	25.215616
157.565082	6058.350845	25.220634
157.342025	6072.168258	25.225651
157.698293	6074.855705	25.230669
157.834781	6080.330285	25.235687
157.857892	6089.566557	25.240704
158.336432	6106.263541	25.245722
157.978756	6115.985646	25.250739
158.438743	6129.730817	25.255757
158.562322	6138.105358	25.260775
159.015726	6153.237404	25.265792
159.031070	6163.655566	25.270810
159.469050	6166.797429	25.275827
159.573693	6174.057452	25.280845
159.981360	6167.781068	25.285863
160.401356	6169.192676	25.290880
161.068844	6162.102178	25.295898
160.725242	6163.800723	25.300915
161.416639	6161.375360	25.305933
161.172341	6167.326317	25.310951
161.254492	6159.591991	25.315968
161.523613	6151.935707	25.320986
161.587720	6154.798365	25.326003
162.026232	6164.812457	25.331021
161.790899	6160.543507	25.336039
161.762676	6160.200714	25.341056
162.038118	6145.257593	25.346074
162.041717	6161.173546	25.351091
162.291881	6166.797653	25.356109
162.169075	6182.963873	25.361127
162.345792	6187.459894	25.366144
162.544462	6184.897059	25.371162
162.703169	6203.778226	25.376179
162.705349	6211.392092	25.381197
162.955691	6209.165249	25.386215
163.357754	6211.110011	25.391232
163.225650	6209.239821	25.396250
163.338815	6230.520997	25.401267
163.459001	6231.761760	25.406285
163.567835	6249.924725	25.411303
163.446253	6247.787712	25.416320
163.840472	6259.639738	25.421338
163.799041	6275.215596	25.426355
164.069072	6289.094822	25.431373
164.265682	6295.582853	25.436391
164.275486	6304.871827	25.441408
164.597991	6308.489543	25.446426
164.729559	6318.242439	25.451443
165.066601	6329.847766	25.456461
164.958503	6343.158066	25.461479
165.060733	6349.679843	25.466496
165.390995	6362.634212	25.471514
165.451261	6374.895351	25.476531
165.592190	6382.209751	25.481549
165.760838	6399.637425	25.486567
165.802669	6413.423066	25.491584
166.295644	6424.855653	25.496602
166.574348	6432.322115	25.501619
166.518450	6450.908846	25.506637
166.871511	6456.617941	25.511655
167.037313	6476.527404	25.516672
167.058026	6472.994849	25.521690
167.008728	6484.594506	25.526707
167.328689	6505.521605	25.531725
167.937180	6505.505230	25.536743
167.702978	6527.235774	25.541760
168.107157	6525.613005	25.546778
168.177451	6542.667931	25.551795
168.147734	6549.810251	25.556813
168.514944	6566.215725	25.561831
168.521316	6576.155685	25.566848
168.947039	6590.572668	25.571866
169.205373	6600.656266	25.576883
169.590409	6603.263522	25.581901
169.454535	6618.778702	25.586919
169.330450	6626.996541	25.591936
169.591395	6634.857318	25.596954
170.080886	6654.990912	25.601971
170.424702	6645.782171	25.606989
170.812905	6656.843023	25.612007
170.578062	6673.636502	25.617024
170.833477	6675.850524	25.622042
171.295479	6681.773075	25.627059
171.231252	6691.310607	25.632077
171.190245	6697.466652	25.637095
171.527477	6698.004188	25.642112
171.717385	6704.840669	25.647130
171.524292	6718.467616	25.652147
171.624425	6714.622669	25.657165
172.166546	6738.548990	25.662183
172.370001	6756.640808	25.667200
172.730687	6759.760159	25.672218
172.993213	6758.254269	25.677236
172.810593	6752.003869	25.682253
173.265027	6766.217609	25.687271
173.583298	6768.263952	25.692288
173.622176	6770.391948	25.697306
173.323906	6777.570114	25.702324
173.781512	6783.086148	25.707341
174.039108	6793.372009	25.712359
173.871991	6802.385889	25.717376
174.252917	6809.160916	25.722394
174.518582	6812.737128	25.727412
174.225499	6833.318677	25.732429
174.534588	6825.883149	25.737447
174.422208	6843.033267	25.742464
174.975586	6854.099931	25.747482
175.048534	6855.357609	25.752500
175.048377	6878.144188	25.757517
175.583524	6877.687868	25.762535
175.277424	6901.807267	25.767552
175.575567	6905.125856	25.772570
176.017931	6915.000853	25.777588
175.920519	6914.851986	25.782605
176.423026	6936.407616	25.787623
176.468611	6934.335885	25.792640
176.998365	6945.103242	25.797658
177.017481	6958.693964	25.802676
177.186091	6972.362298	25.807693
177.542162	6972.732732	25.812711
177.409305	6983.487111	25.817728
177.551768	6992.465213	25.822746
177.584437	7000.800722	25.827764
177.714072	7018.939090	25.832781
177.887238	7020.711442	25.837799
178.127370	7033.803527	25.842816
178.495094	7046.648333	25.847834
178.152190	7054.386062	25.852852
178.399697	7074.580125	25.857869
179.001245	7082.949671	25.862887
179.168457	7099.847868	25.867904
178.832727	7111.230766	25.872922
179.665757	7122.171701	25.877940
179.692778	7132.591740	25.882957
180.007878	7138.644789	25.887975
180.360487	7168.015528	25.892992
180.470356	7168.276159	25.898010
180.458662	7175.359073	25.903028
180.717906	7187.510657	25.908045
180.911787	7192.847144	25.913063
180.934333	7195.508117	25.918080
181.021293	7210.306982	25.923098
181.273768	7214.358883	25.928116
181.250422	7231.893192	25.933133
181.505776	7237.472618	25.938151
181.827367	7255.830547	25.943168
182.140664	7266.783539	25.948186
181.955098	7279.045909	25.953204
182.154508	7296.037108	25.958221
182.747113	7308.392262	25.963239
182.768447	7321.831370	25.968256
182.770370	7334.459027	25.973274
182.607949	7339.851375	25.978292
182.930512	7356.911733	25.983309
183.364327	7367.208192	25.988327
183.527322	7394.045521	25.993344
184.004227	7391.221100	25.998362
184.225197	7410.942984	26.003380
184.300616	7425.904837	26.008397
184.668438	7428.293919	26.013415
184.681273	7446.735136	26.018432
184.543525	7455.479546	26.023450
185.261190	7467.748919	26.028468
185.088243	7480.691358	26.033485
185.601378	7484.895062	26.038503
185.460782	7495.906669	26.043520
185.472444	7502.768215	26.048538
185.907955	7509.898007	26.053556
186.052847	7530.528528	26.058573
186.722564	7533.725881	26.063591
186.970101	7542.526783	26.068608
186.858059	7542.490698	26.073626
186.889102	7557.510122	26.078644
186.951093	7566.977821	26.083661
187.043579	7573.517344	26.088679
187.303947	7584.081031	26.093696
187.221481	7589.593521	26.098714
187.769431	7605.592767	26.103732
187.695596	7622.765983	26.108749
188.275281	7628.430471	26.113767
188.298193	7648.357273	26.118784
188.593778	7645.479137	26.123802
189.179811	7642.309251	26.128820
189.549971	7651.611906	26.133837
190.100169	7650.701757	26.138855
189.970513	7656.966720	26.143872
190.005034	7650.675683	26.148890
190.434484	7646.166487	26.153908
190.186851	7648.431023	26.158925
190.175560	7648.922165	26.163943
190.143448	7667.061253	26.168960
190.514309	7668.537507	26.173978
190.684329	7683.052235	26.178996
190.881813	7691.273839	26.184013
190.936532	7703.078960	26.189031
191.050814	7720.661626	26.194048
191.420748	7722.924135	26.199066
191.928512	7731.690674	26.204084
191.725471	7758.746887	26.209101
192.216268	7759.670817	26.214119
192.102707	7768.023267	26.219136
192.291578	7781.048145	26.224154
192.485976	7802.087946	26.229172
192.129281	7808.006524	26.234189
192.826330	7823.856319	26.239207
192.547258	7837.143968	26.244224
192.820003	7858.319942	26.249242
193.213801	7880.992372	26.254260
193.415439	7901.049301	26.259277
193.596507	7915.328856	26.264295
193.746209	7930.636231	26.269312
193.872725	7940.466549	26.274330
194.192959	7959.437867	26.279348
194.388375	7971.590497	26.284365
194.845574	7992.374662	26.289383
194.635917	8004.376090	26.294400
194.934281	8023.811836	26.299418
195.347549	8041.404796	26.304436
195.603718	8052.676602	26.309453
196.100346	8060.598939	26.314471
195.984237	8077.684486	26.319488
196.252444	8092.521964	26.324506
196.273109	8082.236048	26.329524
196.783646	8097.910086	26.334541
197.319712	8108.595054	26.339559
197.280138	8111.445846	26.344576
197.803656	8124.945779	26.349594
198.155433	8123.697311	26.354612
197.984021	8135.045623	26.359629
198.468473	8128.125127	26.364647
198.705348	8134.500159	26.369664
198.503470	8152.145393	26.374682
199.060474	8153.314700	26.379700
198.585524	8160.682091	26.384717
198.910673	8165.341615	26.389735
198.810463	8183.621320	26.394752
199.187097	8180.654634	26.399770
199.638644	8197.127280	26.404788
199.719203	8215.962767	26.409805
200.010737	8216.722197	26.414823
199.843034	8230.077922	26.419840
200.047863	8247.624804	26.424858
200.191244	8250.516413	26.429876
200.436298	8271.176270	26.434893
200.815540	8269.642505	26.439911
200.819701	8294.936926	26.444928
201.114154	8290.931768	26.449946
201.907280	8288.673319	26.454964
202.306189	8308.017842	26.459981
202.311797	8298.921252	26.464999
202.321391	8314.636066	26.470016
202.436704	8320.102004	26.475034
202.917206	8321.103349	26.480052
202.568848	8330.664139	26.485069
203.073959	8333.227577	26.490087
203.353348	8341.575555	26.495104
203.628927	8361.829773	26.500122
204.025950	8357.098172	26.505140
203.894307	8367.534291	26.510157
203.781872	8366.551118	26.515175
204.135943	8385.160813	26.520192
204.034046	8408.309348	26.525210
204.364995	8409.744560	26.530228
204.281707	8429.957199	26.535245
204.551870	8440.260955	26.540263
204.843857	8448.272348	26.545280
204.746009	8467.821146	26.550298
204.835038	8477.862839	26.555316
205.565703	8503.709897	26.560333
205.620067	8512.803570	26.565351
206.062951	8522.420463	26.570368
206.161629	8539.734834	26.575386
206.249408	8556.350033	26.580404
206.391105	8578.046197	26.585421
206.591231	8591.729736	26.590439
207.237928	8605.542230	26.595456
206.865851	8631.458032	26.600474
207.253481	8645.099608	26.605492
207.348090	8657.268481	26.610509
207.700014	8673.116246	26.615527
207.989541	8678.128774	26.620544
208.608612	8701.991919	26.625562
208.824600	8709.027122	26.630580
208.631699	8713.840558	26.635597
208.967438	8732.065136	26.640615
209.026117	8741.530798	26.645632
209.095266	8764.766641	26.650650
209.199627	8775.004998	26.655668
209.751706	8785.230053	26.660685
210.010250	8800.789461	26.665703
210.459152	8823.890114	26.670720
210.383822	8836.751904	26.675738
210.457279	8849.874546	26.680756
210.600886	8869.471186	26.685773
211.019623	8883.480619	26.690791
211.391870	8890.194631	26.695808
211.521687	8900.517473	26.700826
211.636665	8910.735298	26.705844
211.929516	8933.323801	26.710861
212.162818	8940.236404	26.715879
212.720682	8956.693072	26.720896
212.647349	8981.845863	26.725914
212.896969	8981.620512	26.730932
212.950082	8998.149975	26.735949
213.189311	9006.280379	26.740967
213.713700	9013.412619	26.745984
213.504849	9040.474766	26.751002
213.442453	9032.180946	26.756020
213.423937	9050.549738	26.761037
213.833300	9070.461729	26.766055
214.087562	9074.242236	26.771072
214.222939	9095.949467	26.776090
214.665003	9105.746757	26.781108
215.052394	9126.325281	26.786125
215.125291	9150.214577	26.791143
215.436947	9156.631921	26.796160
215.525032	9178.428746	26.801178
215.943569	9181.075329	26.806196
216.128653	9203.008538	26.811213
216.216812	9207.730711	26.816231
216.927978	9219.522364	26.821248
216.360098	9236.954435	26.826266
216.952501	9241.357668	26.831284
216.931365	9272.463672	26.836301
217.142125	9285.258852	26.841319
217.964478	9295.391332	26.846336
217.811873	9308.732836	26.851354
218.034067	9318.160547	26.856372
218.342303	9329.500749	26.861389
218.523797	9349.189837	26.866407
219.000249	9356.228685	26.871424
219.123042	9375.469184	26.876442
219.365310	9380.536666	26.881460
219.289201	9402.665737	26.886477
219.106099	9411.645499	26.891495
219.416330	9423.282236	26.896512
219.597744	9448.490469	26.901530
220.194416	9470.302682	26.906548
220.158765	9483.512325	26.911565
220.610722	9502.909775	26.916583
221.007133	9514.687779	26.921600
220.795903	9532.992515	26.926618
221.233128	9550.355828	26.931636
221.554882	9564.453588	26.936653
222.634110	9569.794150	26.941671
222.882903	9558.391861	26.946688
222.991958	9577.685239	26.951706
223.411062	9584.158518	26.956724
223.846886	9586.764564	26.961741
223.829850	9597.458108	26.966759
223.856483	9603.310886	26.971776
223.822692	9604.228691	26.976794
224.010816	9615.382655	26.981812
224.265188	9629.898323	26.986829
224.591132	9631.770134	26.991847
224.880961	9640.729594	26.996864
225.008749	9652.988642	27.001882
224.719081	9655.016885	27.006900
225.219027	9667.599685	27.011917
225.376388	9680.068820	27.016935
225.348849	9689.267464	27.021952
225.551787	9708.296836	27.026970
226.001856	9721.424242	27.031988
226.295841	9739.646879	27.037005
226.168934	9760.723448	27.042023
226.571619	9766.192154	27.047040
226.636062	9770.570872	27.052058
227.007697	9795.497184	27.057076
227.087859	9817.936951	27.062093
227.074785	9832.920923	27.067111
227.623068	9841.413741	27.072128
228.114154	9868.730541	27.077146
227.986491	9880.174098	27.082164
228.236808	9886.310822	27.087181
228.199759	9902.741545	27.092199
228.561693	9911.077300	27.097216
228.642037	9924.370121	27.102234
229.088684	9948.211362	27.107252
229.572443	9970.262872	27.112269
230.020661	9975.538219	27.117287
230.226047	9988.183168	27.122304
230.078351	10010.545194	27.127322
230.131388	10013.309147	27.132340
230.313987	10024.811541	27.137357
230.831734	10056.465920	27.142375
230.594223	10058.953337	27.147392
230.797816	10092.327279	27.152410
230.721092	10108.391819	27.157428
231.181606	10128.511638	27.162445
231.261535	10159.350690	27.167463
231.785849	10170.591249	27.172480
231.988705	10195.156167	27.177498
232.341215	10204.781777	27.182516
232.819371	10224.340064	27.187533
232.888508	10255.335680	27.192551
233.421315	10268.456826	27.197568
233.679948	10286.047724	27.202586
233.947358	10299.586208	27.207604
234.271426	10314.457759	27.212621
234.142883	10331.724139	27.217639
234.658426	10338.665671	27.222656
234.622763	10362.393548	27.227674
235.169563	10379.468924	27.232692
235.658365	10382.894050	27.237709
235.371446	10400.393698	27.242727
235.786075	10418.658092	27.247744
236.088349	10440.264962	27.252762
236.367408	10447.227793	27.257780
236.546258	10453.596926	27.262797
236.908438	10473.473606	27.267815
237.187634	10492.378160	27.272832
237.439500	10499.512620	27.277850
237.969059	10505.226902	27.282868
238.457024	10507.553365	27.287885
238.365141	10526.285586	27.292903
239.010731	10533.314175	27.297920
239.458384	10544.907983	27.302938
239.190175	10550.693575	27.307956
239.553647	10554.709880	27.312973
239.395861	10569.808680	27.317991
239.783460	10577.859694	27.323008
239.985568	10596.223861	27.328026
240.200450	10603.613600	27.333044
240.677179	10621.565340	27.338061
240.066784	10631.954578	27.343079
240.539079	10650.630118	27.348096
240.843376	10667.778481	27.353114
241.033911	10690.217791	27.358132
241.419351	10689.949044	27.363149
241.512230	10708.399899	27.368167
241.971881	10720.440310	27.373184
242.214912	10736.685799	27.378202
242.612162	10757.378253	27.383220
242.785875	10769.318241	27.388237
242.594978	10781.627953	27.393255
242.984929	10790.989081	27.398272
243.247510	10807.784144	27.403290
243.782007	10828.082582	27.408308
243.668829	10836.038489	27.413325
243.730981	10855.940473	27.418343
243.829718	10875.322061	27.423360
244.199766	10880.347833	27.428378
244.231285	10909.651645	27.433396
244.539274	10923.070551	27.438413
244.870499	10947.666868	27.443431
245.358164	10953.630987	27.448448
245.358986	10971.894436	27.453466
245.412733	10984.604863	27.458484
245.882789	11000.284539	27.463501
245.689240	11032.895079	27.468519
246.130237	11048.187805	27.473536
246.694465	11078.264142	27.478554
246.884879	11082.099268	27.483572
246.807845	11106.702913	27.488589
247.092329	11134.350745	27.493607
247.360825	11148.754863	27.498624
247.530265	11166.250044	27.503642
247.584265	11195.816021	27.508660
248.057539	11211.072247	27.513677
248.553655	11240.439572	27.518695
248.712784	11267.200993	27.523712
248.863218	11286.063367	27.528730
249.275279	11312.737866	27.533748
250.029828	11319.238144	27.538765
249.726303	11346.119519	27.543783
250.368808	11363.682871	27.548800
250.523373	11373.643230	27.553818
251.133966	11386.456157	27.558836
251.619784	11406.216571	27.563853
251.533518	11417.133562	27.568871
251.749221	11431.050413	27.573888
252.135696	11450.618030	27.578906
252.426351	11460.152932	27.583924
252.787638	11467.946365	27.588941
252.790403	11480.181988	27.593959
253.125377	11496.666347	27.598976
253.763469	11503.361765	27.603994
253.781210	11518.007541	27.609012
254.184723	11527.723733	27.614029
254.250266	11543.852472	27.619047
254.654357	11549.627781	27.624064
254.576701	11564.967443	27.629082
254.864945	11588.333515	27.634100
254.983279	11604.109846	27.639117
254.906213	11617.198013	27.644135
255.171351	11635.127033	27.649152
255.506361	11650.692629	27.654170
255.805923	11676.930557	27.659188
256.085671	11692.002766	27.664205
256.355721	11720.901022	27.669223
256.499338	11731.548512	27.674240
256.450963	11756.050625	27.679258
256.860661	11774.626572	27.684276
257.323577	11786.212444	27.689293
257.385689	11807.918509	27.694311
257.814662	11826.311496	27.699328
258.800024	11842.978472	27.704346
258.492366	11864.382544	27.709364
259.000936	11881.114771	27.714381
259.127061	11900.603646	27.719399
259.197856	11920.375934	27.724416
259.682272	11928.194478	27.729434
259.485653	11948.914964	27.734452
260.097427	11957.922994	27.739469
260.210535	11987.803047	27.744487
260.634153	12004.273966	27.749504
261.003201	12020.794498	27.754522
261.285727	12040.615847	27.759540
261.196089	12046.478127	27.764557
261.588389	12072.866284	27.769575
262.020828	12081.131967	27.774592
262.475181	12089.078443	27.779610
262.493173	12106.225603	27.784628
263.024778	12109.486458	27.789645
263.332142	12130.860800	27.794663
263.413005	12132.644950	27.799680
263.585883	12148.223724	27.804698
263.814914	12156.303417	27.809716
264.216533	12173.709480	27.814733
264.287950	12197.814465	27.819751
264.656310	12220.227745	27.824768
264.814673	12216.400968	27.829786
264.868931	12235.601456	27.834804
265.131606	12255.056676	27.839821
265.209175	12276.290343	27.844839
265.572874	12293.882454	27.849856
266.068990	12316.484252	27.854874
265.722214	12343.658024	27.859892
266.348452	12362.143789	27.864909
266.333366	12383.076308	27.869927
266.615900	12400.753863	27.874944
267.208734	12426.470060	27.879962
267.368548	12454.038309	27.884980
267.916790	12469.703809	27.889997
268.163555	12484.980765	27.895015
268.753137	12498.347211	27.900032
269.214021	12500.551858	27.905050
269.678542	12521.848342	27.910068
269.722288	12527.355144	27.915085
270.046689	12542.329461	27.920103
269.857977	12571.862986	27.925120
270.610559	12578.815591	27.930138
270.769063	12598.293799	27.935156
271.113185	12600.191489	27.940173
270.689400	12622.328287	27.945191
270.945311	12647.181781	27.950208
271.738568	12658.530130	27.955226
272.169405	12691.478353	27.960244
272.242774	12693.254256	27.965261
272.394326	12713.134722	27.970279
272.527026	12728.066586	27.975296
272.700124	12750.725821	27.980314
272.698195	12770.851444	27.985332
273.182189	12797.586252	27.990349
273.346192	12823.648063	27.995367
273.630553	12834.261496	28.000384
273.948112	12870.647794	28.005402
273.963597	12885.310773	28.010420
274.680624	12908.535522	28.015437
274.757678	12936.594285	28.020455
275.211808	12961.767670	28.025472
275.986091	12974.230775	28.030490
275.972676	12994.607911	28.035508
276.192555	13000.017785	28.040525
276.521200	13024.958277	28.045543
276.367401	13053.672333	28.050560
276.791228	13067.440945	28.055578
277.126851	13091.073040	28.060596
277.768695	13117.647781	28.065613
277.815498	13128.191223	28.070631
277.651334	13151.699575	28.075648
278.491845	13173.193690	28.080666
278.701135	13200.859489	28.085684
278.690903	13201.366399	28.090701
279.062854	13229.515192	28.095719
279.397492	13257.054066	28.100736
279.536172	13274.398121	28.105754
279.944641	13289.530393	28.110772
280.584597	13300.394709	28.115789
280.477098	13320.957465	28.120807
280.683020	13342.500653	28.125824
281.021727	13349.906813	28.130842
281.051103	13381.371707	28.135860
281.280682	13395.900487	28.140877
281.668887	13419.846871	28.145895
281.772831	13435.715409	28.150912
281.911979	13463.916809	28.155930
282.183983	13492.198495	28.160948
282.799291	13513.361945	28.165965
283.085185	13544.303747	28.170983
283.049587	13568.749358	28.176000
283.228696	13588.408521	28.181018
283.565104	13621.426840	28.186036
284.186501	13643.495839	28.191053
284.487811	13661.187421	28.196071
284.535612	13683.886347	28.201088
284.772250	13708.741093	28.206106
285.098015	13744.830925	28.211124
285.525484	13761.429096	28.216141
285.814871	13779.820589	28.221159
285.987651	13817.504083	28.226176
286.738451	13842.938500	28.231194
286.767271	13867.159653	28.236212
286.975629	13892.205396	28.241229
287.658699	13913.778703	28.246247
287.708138	13936.632420	28.251264
288.058224	13951.528034	28.256282
288.666630	13984.605435	28.261300
288.699915	14011.257811	28.266317
288.893209	14025.281143	28.271335
289.166471	14063.928398	28.276352
289.327495	14081.613924	28.281370
289.553309	14112.054446	28.286388
289.818889	14127.699279	28.291405
290.222855	14159.384694	28.296423
290.375371	14193.231819	28.301440
290.833673	14213.782702	28.306458
291.179565	14236.006082	28.311476
291.606940	14258.823089	28.316493
292.126324	14284.758596	28.321511
291.876650	14316.350858	28.326528
292.328809	14333.545712	28.331546
292.425363	14358.634847	28.336564
292.713642	14391.911537	28.341581
293.194646	14407.797615	28.346599
293.203855	14438.016776	28.351616
293.668335	14464.447488	28.356634
294.094391	14494.415107	28.361652
294.306973	14515.532224	28.366669
294.519099	14543.777479	28.371687
295.040491	14577.933853	28.376704
295.844465	14590.557602	28.381722
296.151756	14607.257451	28.386740
296.655671	14622.571643	28.391757
297.051456	14639.996679	28.396775
297.304168	14650.957174	28.401792
298.018888	14669.541872	28.406810
298.179401	14686.337422	28.411828
298.208371	14698.258351	28.416845
298.343726	14708.131886	28.421863
298.556327	14724.290824	28.426880
298.991951	14743.933104	28.431898
299.123153	14759.327898	28.436916
298.854267	14776.806647	28.441933
299.586205	14791.835756	28.446951
299.432667	14818.281655	28.451968
299.967704	14833.534293	28.456986
300.169945	14858.841240	28.462004
300.151840	14888.383210	28.467021
300.515547	14900.093916	28.472039
300.367440	14933.038809	28.477056
300.766551	14950.258321	28.482074
301.156991	14990.180825	28.487092
301.721436	15017.155657	28.492109
302.209155	15031.878960	28.497127
302.213145	15059.462761	28.502144
302.558559	15080.325981	28.507162
302.743714	15112.157794	28.512180
303.105727	15145.916940	28.517197
303.551167	15161.168084	28.522215
303.558556	15214.968612	28.527232
304.156334	15234.244899	28.532250
304.511419	15254.212993	28.537268
304.427652	15284.953385	28.542285
304.960596	15308.708922	28.547303
304.907033	15337.350700	28.552320
305.574828	15367.095479	28.557338
306.089475	15401.298598	28.562356
305.973874	15438.253512	28.567373
306.588512	15468.417360	28.572391
306.979691	15507.099594	28.577408
307.154891	15522.191225	28.582426
307.295535	15541.438363	28.587444
307.751185	15576.380617	28.592461
308.503588	15596.855335	28.597479
308.576292	15628.073946	28.602496
308.722947	15644.304000	28.607514
309.247961	15670.869025	28.612532
309.683236	15695.546796	28.617549
310.280722	15714.804664	28.622567
310.305398	15739.821591	28.627584
310.754919	15769.885444	28.632602
311.028529	15788.609816	28.637620
311.536137	15802.619958	28.642637
312.335612	15814.092410	28.647655
312.547105	15831.427382	28.652672
312.625297	15851.673196	28.657690
313.187501	15866.265455	28.662708
313.162039	15882.863780	28.667725
313.375177	15905.485749	28.672743
313.527140	15926.544432	28.677760
314.035283	15948.289575	28.682778
314.248336	15974.727017	28.687796
314.479133	15999.980461	28.692813
314.918596	16015.236381	28.697831
315.332567	16036.241509	28.702848
315.543461	16063.358476	28.707866
315.757931	16083.106260	28.712884
316.113565	16105.235533	28.717901
316.447502	16124.452977	28.722919
316.345215	16143.558741	28.727936
316.606125	16174.192868	28.732954
316.907858	16201.864323	28.737972
317.369698	16228.547404	28.742989
318.312996	16254.068589	28.748007
318.915923	16271.503724	28.753024
318.972840	16282.208403	28.758042
319.476187	16301.137332	28.763060
319.827420	16319.862697	28.768077
320.187034	16333.618464	28.773095
320.818708	16357.460908	28.778112
320.828803	16366.833767	28.783130
321.205219	16379.361439	28.788148
321.102828	16386.022988	28.793165
321.745909	16402.706547	28.798183
321.861087	16418.452618	28.803200
321.887415	16432.664951	28.808218
321.998742	16448.181079	28.813236
322.300872	16474.861094	28.818253
322.574931	16489.720061	28.823271
322.663700	16516.262995	28.828288
322.707489	16545.722011	28.833306
323.250603	16569.824956	28.838324
323.408745	16610.058849	28.843341
323.750828	16617.939535	28.848359
324.247135	16645.615893	28.853376
324.562333	16685.616878	28.858394
324.816932	16713.460697	28.863412
325.367695	16746.934088	28.868429
325.717911	16763.426945	28.873447
326.172118	16798.987566	28.878464
326.295826	16821.690950	28.883482
326.619346	16846.769893	28.888500
326.479008	16879.148354	28.893517
327.280860	16904.859966	28.898535
327.240031	16943.186351	28.903552
327.531197	16975.945902	28.908570
327.530417	17010.501103	28.913588
327.722321	17053.971355	28.918605
328.279813	17087.510614	28.923623
328.914077	17125.952714	28.928640
329.117995	17156.332004	28.933658
329.675030	17194.868463	28.938676
330.021988	17229.041086	28.943693
330.474812	17263.317214	28.948711
330.944525	17293.831969	28.953728
330.859935	17324.054562	28.958746
331.248284	17350.280070	28.963764
331.628131	17394.366011	28.968781
331.611504	17424.382277	28.973799
332.352247	17455.075938	28.978816
332.540191	17496.185116	28.983834
333.031664	17523.285452	28.988852
333.376854	17563.580470	28.993869
333.856789	17593.822450	28.998887
333.984634	17632.919767	29.003904
334.684508	17665.395354	29.008922
334.949852	17682.499286	29.013940
334.849785	17729.093370	29.018957
335.347465	17765.448114	29.023975
335.876334	17796.674583	29.028992
335.982944	17827.645057	29.034010
336.539707	17853.901722	29.039028
337.137056	17886.684343	29.044045
337.642884	17911.685569	29.049063
337.646034	17941.168867	29.054080
338.319306	17961.052021	29.059098
339.080337	17986.815692	29.064116
339.168408	18012.842750	29.069133
339.481802	18038.708197	29.074151
339.643443	18056.321470	29.079168
340.097375	18090.573619	29.084186
340.507269	18114.699359	29.089204
340.656012	18137.956308	29.094221
340.767618	18170.303774	29.099239
341.303666	18202.426868	29.104256
341.498150	18232.834592	29.109274
342.420790	18250.170897	29.114292
342.368972	18284.313081	29.119309
342.783210	18294.185834	29.124327
343.483692	18321.222957	29.129344
344.019207	18334.058653	29.134362
344.286795	18334.907555	29.139380
344.490438	18366.944003	29.144397
344.719137	18376.744779	29.149415
345.176771	18398.254208	29.154432
345.700900	18414.143165	29.159450
345.948084	18426.000627	29.164468
346.251436	18455.462950	29.169485
346.560430	18466.565269	29.174503
346.610664	18483.792050	29.179520
346.903085	18504.240835	29.184538
347.289581	18519.014255	29.189556
347.576671	18550.772591	29.194573
347.605525	18577.738382	29.199591
348.049910	18594.025359	29.204608
348.446209	18635.514961	29.209626
348.865727	18655.223775	29.214644
348.999683	18685.768043	29.219661
349.179794	18717.278063	29.224679
349.614632	18743.877237	29.229696
349.580324	18777.948047	29.234714
350.653936	18809.697323	29.239732
350.684726	18840.940314	29.244749
351.104797	18862.557226	29.249767
351.251409	18897.598117	29.254784
351.189802	18926.227508	29.259802
352.410275	18949.677665	29.264820
352.484420	18990.277128	29.269837
352.503609	19020.707223	29.274855
353.274464	19053.957428	29.279872
353.257533	19082.864355	29.284890
353.989319	19123.923373	29.289908
353.953849	19166.107207	29.294925
354.197296	19201.329329	29.299943
354.688744	19220.446201	29.304960
354.985992	19256.784585	29.309978
355.631637	19296.878181	29.314996
355.768700	19339.016408	29.320013
356.127681	19374.549279	29.325031
357.107091	19388.491282	29.330048
357.274472	19413.313689	29.335066
358.114975	19440.469432	29.340084
358.009661	19480.384091	29.345101
358.257723	19492.020934	29.350119
358.711287	19527.956256	29.355136
359.037476	19557.460892	29.360154
359.861358	19588.069087	29.365172
359.924759	19616.711496	29.370189
360.376395	19637.427160	29.375207
360.717583	19660.099789	29.380224
360.862238	19694.352657	29.385242
361.592310	19728.179027	29.390260
361.673384	19762.220840	29.395277
361.756097	19789.123002	29.400295
361.976516	19826.889733	29.405312
362.420278	19856.073133	29.410330
363.067999	19889.280869	29.415348
363.445291	19917.811369	29.420365
363.619466	19946.639089	29.425383
364.151961	19976.137313	29.430400
364.108939	20017.768164	29.435418
364.229182	20035.661390	29.440436
364.569797	20079.437324	29.445453
365.045445	20117.556363	29.450471
365.860158	20157.549423	29.455488
365.963461	20192.814235	29.460506
366.223214	20215.613991	29.465524
366.983692	20262.009815	29.470541
367.509800	20294.864511	29.475559
367.795229	20316.068161	29.480576
367.852018	20353.223390	29.485594
368.461418	20379.690037	29.490612
368.902586	20412.804648	29.495629
368.729353	20436.721322	29.500647
368.872872	20460.607364	29.505664
369.204597	20506.097904	29.510682
369.943570	20539.772641	29.515700
370.061719	20580.520143	29.520717
370.742551	20623.687982	29.525735
370.772981	20652.444478	29.530752
371.169061	20680.960507	29.535770
371.814702	20727.394374	29.540788
372.185002	20772.734165	29.545805
372.667682	20798.545155	29.550823
372.603049	20839.005901	29.555840
373.071941	20885.745838	29.560858
373.800825	20914.753463	29.565876
374.037439	20955.331540	29.570893
374.347207	20984.708205	29.575911
374.727920	21012.020290	29.580928
375.584269	21052.463582	29.585946
376.119590	21079.163922	29.590964
376.736423	21109.263534	29.595981
376.748322	21136.481918	29.600999
377.086222	21155.283530	29.606016
377.028081	21200.129064	29.611034
377.644386	21227.000157	29.616052
378.219851	21269.718345	29.621069
378.691858	21294.173163	29.626087
379.431502	21321.006110	29.631104
379.832322	21352.302549	29.636122
380.536701	21375.255155	29.641140
380.734308	21411.726867	29.646157
380.928925	21427.158083	29.651175
380.997036	21445.111304	29.656192
381.446043	21484.911603	29.661210
382.140222	21515.410431	29.666228
382.748579	21535.478003	29.671245
382.927121	21558.829122	29.676263
383.762072	21587.024972	29.681280
383.823448	21599.147251	29.686298
384.391579	21624.187698	29.691316
384.691410	21656.315548	29.696333
384.906324	21671.693227	29.701351
385.264978	21704.134195	29.706368
385.288442	21734.176055	29.711386
385.037799	21767.262295	29.716404
385.472484	21795.192565	29.721421
385.978685	21849.094395	29.726439
386.225011	21877.357586	29.731456
386.520136	21932.202606	29.736474
387.063090	21969.866053	29.741492
387.750978	22002.906777	29.746509
387.761589	22044.931585	29.751527
388.293689	22080.075732	29.756544
387.907063	22127.969946	29.761562
388.455073	22160.464147	29.766580
388.638584	22209.918475	29.771597
389.227132	22258.709189	29.776615
389.716749	22300.545768	29.781632
389.826426	22351.187329	29.786650
390.462552	22397.266434	29.791668
391.107881	22444.677502	29.796685
391.202256	22496.541387	29.801703
391.737708	22526.289405	29.806720
392.141596	22578.313549	29.811738
392.585189	22614.414036	29.816756
392.681376	22655.365137	29.821773
393.216819	22696.291752	29.826791
393.920659	22737.154160	29.831808
394.022620	22772.777647	29.836826
394.330857	22823.515690	29.841844
394.767097	22873.045824	29.846861
395.117366	22910.071413	29.851879
395.461834	22947.116938	29.856896
395.904949	22998.346147	29.861914
396.320204	23039.879973	29.866932
397.299156	23081.325590	29.871949
397.269754	23130.240513	29.876967
397.894069	23166.749717	29.881984
398.135169	23205.499133	29.887002
398.473652	23242.944254	29.892020
398.906418	23282.927640	29.897037
399.079912	23331.849190	29.902055
399.675868	23380.692050	29.907072
400.192756	23427.455738	29.912090
400.794433	23469.580546	29.917108
401.419548	23499.151673	29.922125
401.443608	23554.606038	29.927143
402.053331	23584.938019	29.932160
402.642737	23626.951335	29.937178
403.236625	23653.999854	29.942196
404.016103	23679.433185	29.947213
404.067908	23717.789850	29.952231
404.900410	23735.416869	29.957248
405.122537	23764.729225	29.962266
405.768698	23800.926520	29.967284
406.308782	23832.862270	29.972301
406.215907	23871.020712	29.977319
407.025066	23899.103823	29.982336
407.089989	23937.825381	29.987354
407.644058	23965.822154	29.992372
408.449565	23985.349452	29.997389
409.410325	23999.171274	30.002407
410.284532	24004.646039	30.007424
410.823321	24023.753833	30.012442
411.018683	24037.758764	30.017460
411.129774	24051.069126	30.022477
410.941916	24081.210818	30.027495
411.911647	24095.776999	30.032512
411.718127	24125.445685	30.037530
412.144538	24147.528717	30.042548
412.612665	24174.553404	30.047565
412.731293	24206.682156	30.052583
413.289920	24231.600989	30.057600
413.801727	24268.654352	30.062618
413.715027	24309.043454	30.067636
414.016955	24330.640623	30.072653
414.436422	24374.129304	30.077671
414.686573	24408.335871	30.082688
414.810058	24436.331232	30.087706
414.551952	24484.912432	30.092724
415.465906	24531.275249	30.097741
415.579756	24589.909817	30.102759
416.222059	24631.322912	30.107776
416.717982	24685.575279	30.112794
417.267063	24716.954901	30.117812
417.717083	24754.909913	30.122829
418.156597	24802.295623	30.127847
418.249405	24840.382584	30.132864
418.685970	24876.722090	30.137882
419.205880	24929.132320	30.142900
420.056945	24965.324905	30.147917
420.453529	25004.628544	30.152935
420.815566	25043.741759	30.157952
420.844399	25069.281797	30.162970
421.270493	25125.290547	30.167988
421.740561	25159.849454	30.173005
421.970048	25201.296786	30.178023
422.359727	25237.688526	30.183040
422.819143	25280.256534	30.188058
423.045862	25321.881502	30.193076
423.731446	25358.511505	30.198093
424.168210	25410.139708	30.203111
424.187710	25451.772122	30.208128
424.507213	25500.461211	30.213146
425.083440	25552.889523	30.218164
425.694970	25599.498094	30.223181
425.984852	25652.091593	30.228199
426.307257	25697.557524	30.233216
426.848813	25736.966283	30.238234
427.362352	25798.303594	30.243252
427.931709	25837.891476	30.248269
428.368454	25893.439328	30.253287
428.858525	25932.433091	30.258304
429.314995	25982.858862	30.263322
429.623293	26026.090439	30.268340
429.739730	26072.493245	30.273357
430.078327	26130.850602	30.278375
430.752738	26181.514497	30.283392
431.216581	26236.724080	30.288410
431.368159	26282.995461	30.293428
432.314173	26332.763971	30.298445
432.796908	26389.456252	30.303463
433.309565	26435.431256	30.308480
433.782832	26475.667458	30.313498
434.035867	26523.895404	30.318516
434.694335	26573.437775	30.323533
435.234585	26614.434831	30.328551
435.519964	26655.901668	30.333568
436.003231	26704.251988	30.338586
436.374988	26749.731511	30.343604
437.099701	26791.654398	30.348621
437.309580	26854.123241	30.353639
437.589282	26900.515008	30.358656
438.430680	26933.470300	30.363674
438.539968	26986.032343	30.368692
439.079981	27025.165755	30.373709
439.782851	27083.550960	30.378727
439.848921	27121.937139	30.383744
440.519639	27166.542794	30.388762
440.542505	27225.692241	30.393780
441.456679	27266.297061	30.398797
441.507340	27319.412706	30.403815
442.199524	27365.077274	30.408832
442.480149	27416.930979	30.413850
442.540520	27472.295603	30.418868
443.277907	27501.362024	30.423885
443.834602	27552.212111	30.428903
444.125267	27603.944629	30.433920
445.073837	27651.522736	30.438938
445.369368	27704.038497	30.443956
446.095558	27751.228189	30.448973
446.208750	27792.774877	30.453991
446.600200	27827.875260	30.459008
447.605480	27879.408056	30.464026
447.707235	27921.519335	30.469044
448.353248	27972.685155	30.474061
448.629154	28019.838544	30.479079
449.441291	28058.640567	30.484096
449.391652	28105.548071	30.489114
449.325567	28145.872053	30.494132
449.796896	28179.342422	30.499149
450.334722	28235.146308	30.504167
450.694538	28275.391194	30.509184
451.128412	28328.853969	30.514202
451.431177	28375.504629	30.519220
452.199916	28420.887775	30.524237
453.121995	28452.233723	30.529255
454.098949	28497.843581	30.534272
454.510295	28527.297538	30.539290
454.814182	28566.565705	30.544308
455.566235	28599.006735	30.549325
456.113390	28635.329329	30.554343
456.198860	28660.890289	30.559360
456.846256	28697.121441	30.564378
457.127900	28738.833290	30.569396
457.502127	28774.310930	30.574413
457.768304	28816.063284	30.579431
457.963513	28855.146755	30.584448
458.322611	28899.432068	30.589466
458.987887	28956.987829	30.594484
459.484005	28999.715898	30.599501
460.453853	29036.004601	30.604519
460.616114	29077.482997	30.609536
461.275306	29118.472775	30.614554
461.645246	29163.401705	30.619572
461.836049	29207.872069	30.624589
462.358421	29247.454975	30.629607
462.827713	29294.505153	30.634624
463.236784	29342.279154	30.639642
463.494286	29387.238826	30.644660
464.014969	29432.353329	30.649677
464.231721	29489.727988	30.654695
464.678171	29546.428391	30.659712
465.400328	29588.964252	30.664730
465.209758	29639.664751	30.669748
466.353125	29682.994515	30.674765
466.753076	29736.150206	30.679783
467.271152	29778.775315	30.684800
468.072570	29817.291570	30.689818
468.487380	29872.063523	30.694836
468.951373	29912.579756	30.699853
469.682640	29959.242748	30.704871
470.408358	29984.825175	30.709888
471.405555	30021.459008	30.714906
471.845080	30065.437130	30.719924
472.672512	30090.586550	30.724941
473.080568	30113.399578	30.729959
473.228339	30145.261317	30.734976
474.107619	30180.447350	30.739994
474.398269	30217.931796	30.745012
474.432189	30249.628208	30.750029
474.512183	30282.727122	30.755047
474.444597	30319.604116	30.760064
475.168753	30371.092383	30.765082
475.918965	30411.672231	30.770100
476.027938	30459.767645	30.775117
476.233168	30504.598865	30.780135
476.816775	30558.258907	30.785152
477.413284	30597.276503	30.790170
477.757078	30661.518614	30.795188
478.354971	30709.790890	30.800205
478.394364	30755.862360	30.805223
478.969197	30818.930896	30.810240
479.500011	30864.470484	30.815258
479.574325	30918.375589	30.820276
480.073062	30977.006130	30.825293
480.514921	31024.083507	30.830311
480.555917	31081.970550	30.835328
481.389941	31137.786477	30.840346
481.269490	31202.286301	30.845364
482.190321	31252.721844	30.850381
482.860823	31305.150123	30.855399
483.242141	31364.748404	30.860416
483.753280	31415.330692	30.865434
484.414044	31481.238882	30.870452
484.665553	31522.366823	30.875469
485.606179	31580.455722	30.880487
485.624200	31632.797368	30.885504
486.576027	31689.949192	30.890522
486.621812	31755.859745	30.895540
486.639562	31807.455895	30.900557
487.389402	31863.034079	30.905575
488.113566	31927.486042	30.910592
488.759028	31975.962430	30.915610
489.127612	32034.445643	30.920628
489.648627	32084.623406	30.925645
490.082488	32140.017907	30.930663
490.400345	32204.256197	30.935680
491.030639	32256.048325	30.940698
491.505444	32328.702271	30.945716
492.268333	32393.415131	30.950733
493.117135	32445.103962	30.955751
493.263137	32508.004539	30.960768
493.792527	32550.899093	30.965786
494.737312	32610.204047	30.970804
495.281453	32664.805048	30.975821
495.908268	32721.441612	30.980839
496.489349	32781.568995	30.985856
497.056655	32820.753386	30.990874
497.447960	32870.738398	30.995892
497.635928	32923.107230	31.000909
498.014627	32967.404477	31.005927
498.609886	33023.224913	31.010944
498.774738	33081.053836	31.015962
499.492531	33147.179625	31.020980
499.964012	33208.071422	31.025997
500.592412	33252.557763	31.031015
500.549814	33310.261751	31.036032
501.469888	33363.692965	31.041050
502.241086	33425.606922	31.046068
502.350753	33488.661541	31.051085
502.701715	33546.393048	31.056103
503.166587	33617.086750	31.061120
504.344566	33668.486790	31.066138
504.770144	33732.795077	31.071156
505.506235	33774.388949	31.076173
506.468574	33802.569151	31.081191
507.088726	33855.871563	31.086208
508.017331	33890.588279	31.091226
508.423670	33932.872682	31.096244
508.734136	33979.768647	31.101261
509.089232	34030.116146	31.106279
509.405914	34077.030321	31.111296
510.089841	34118.260013	31.116314
510.106877	34170.437430	31.121332
510.704882	34211.402569	31.126349
511.547905	34270.955765	31.131367
512.032226	34322.111980	31.136384
512.599671	34348.666628	31.141402
513.383032	34393.643242	31.146420
513.275304	34441.680579	31.151437
513.871493	34491.017728	31.156455
514.116376	34539.904201	31.161472
514.791437	34586.023623	31.166490
515.186995	34649.043251	31.171508
515.294864	34696.396159	31.176525
515.766646	34743.464557	31.181543
516.023759	34806.955252	31.186560
516.724499	34855.385367	31.191578
517.391153	34906.748381	31.196596
517.417049	34963.959300	31.201613
518.111241	35013.048373	31.206631
518.233809	35081.227200	31.211648
518.520087	35144.771243	31.216666
519.303679	35212.088216	31.221684
519.433424	35275.359992	31.226701
520.027481	35339.305338	31.231719
520.678260	35406.131571	31.236736
521.770151	35464.245454	31.241754
522.123197	35526.471331	31.246772
522.532762	35585.546014	31.251789
522.874187	35649.127188	31.256807
523.347188	35709.678185	31.261824
524.437476	35780.900814	31.266842
524.763763	35839.135632	31.271860
524.987615	35907.364472	31.276877
526.111050	35962.964515	31.281895
526.154085	36033.548978	31.286912
526.753865	36095.105559	31.291930
527.729030	36160.523880	31.296948
528.330645	36216.275868	31.301965
528.752197	36282.742394	31.306983
528.786681	36353.689675	31.312000
529.357520	36411.761289	31.317018
530.059886	36477.216984	31.322036
530.794237	36550.394906	31.327053
531.335161	36609.932419	31.332071
531.839739	36674.768398	31.337088
532.380737	36738.884333	31.342106
533.033883	36813.517591	31.347124
533.149259	36868.632897	31.352141
533.972979	36932.230878	31.357159
534.359182	37002.454942	31.362176
535.187868	37053.127471	31.367194
535.980846	37114.694669	31.372212
536.315573	37179.274221	31.377229
537.025479	37236.143804	31.382247
537.538454	37303.965050	31.387264
538.258029	37362.110798	31.392282
538.802312	37415.832395	31.397300
539.453857	37476.113811	31.402317
539.906945	37537.084129	31.407335
539.889231	37604.685909	31.412352
540.469075	37655.980606	31.417370
541.221888	37730.095553	31.422388
541.658286	37797.411811	31.427405
542.350372	37859.053857	31.432423
543.095044	37916.413040	31.437440
543.786797	37959.413247	31.442458
544.513986	38031.572903	31.447476
544.916433	38073.651123	31.452493
545.832001	38140.400156	31.457511
545.893619	38199.163437	31.462528
546.257758	38255.185571	31.467546
547.246725	38309.522720	31.472564
547.814957	38372.924674	31.477581
548.140519	38422.825518	31.482599
548.591160	38490.881596	31.487616
549.347198	38545.306410	31.492634
549.755879	38592.538608	31.497652
550.389783	38656.841748	31.502669
551.023023	38709.167704	31.507687
551.225765	38780.191486	31.512704
551.553650	38836.619212	31.517722
552.141622	38886.328251	31.522740
552.196645	38954.852482	31.527757
553.300518	39006.118907	31.532775
553.642427	39070.140158	31.537792
554.355318	39122.890996	31.542810
554.639593	39181.976216	31.547828
555.285691	39247.683137	31.552845
555.761991	39304.386065	31.557863
556.222314	39368.573049	31.562880
556.749793	39434.115712	31.567898
557.184353	39506.901613	31.572916
557.717338	39575.175867	31.577933
558.427693	39640.330034	31.582951
558.612881	39710.847349	31.587968
559.265660	39776.529525	31.592986
560.148306	39828.983551	31.598004
560.439142	39916.611007	31.603021
561.189782	39970.338251	31.608039
561.686520	40057.466029	31.613056
562.161965	40124.068752	31.618074
562.767194	40187.419618	31.623092
563.322165	40267.569699	31.628109
563.912502	40338.386078	31.633127
564.280773	40410.262018	31.638144
564.833716	40481.166932	31.643162
565.682452	40545.682340	31.648180
566.118238	40625.934620	31.653197
566.577438	40692.851519	31.658215
567.246482	40766.850821	31.663232
567.802712	40844.510967	31.668250
568.363432	40916.200314	31.673268
568.720800	40996.592724	31.678285
569.386602	41066.786158	31.683303
569.968792	41146.637940	31.688320
570.518762	41225.672857	31.693338
571.311058	41309.521117	31.698356
571.861434	41383.028787	31.703373
573.082958	41456.842695	31.708391
573.261368	41528.068967	31.713408
573.683133	41602.913056	31.718426
574.540836	41672.332051	31.723444
575.041297	41758.960030	31.728461
575.737378	41810.720679	31.733479
576.661021	41870.219010	31.738496
577.347486	41939.507547	31.743514
577.962745	42005.227585	31.748532
578.492683	42079.291043	31.753549
579.121378	42133.175514	31.758567
579.658636	42201.621732	31.763584
580.392443	42272.858301	31.768602
580.924935	42330.237034	31.773620
581.121303	42407.642811	31.778637
582.010830	42464.580152	31.783655
582.600837	42535.751540	31.788672
583.264816	42598.530910	31.793690
584.044074	42664.341076	31.798708
584.814268	42721.234518	31.803725
585.468168	42777.994518	31.808743
585.971312	42839.996478	31.813760
585.994803	42898.620221	31.818778
586.820055	42960.059736	31.823796
587.070879	43036.776069	31.828813
587.403284	43094.175470	31.833831
588.574921	43156.326626	31.838848
589.267340	43233.119957	31.843866
589.969900	43288.349270	31.848884
590.025430	43359.328700	31.853901
590.695516	43419.826029	31.858919
591.857600	43466.773630	31.863936
592.144347	43525.332496	31.868954
592.877143	43586.668047	31.873972
592.758946	43646.125591	31.878989
593.549486	43709.634675	31.884007
593.850040	43772.790554	31.889024
594.199810	43839.715155	31.894042
594.924330	43903.020068	31.899060
595.241505	43981.462427	31.904077
596.027178	44047.857630	31.909095
596.491163	44128.118216	31.914112
596.859780	44202.017938	31.919130
597.652685	44271.569091	31.924148
598.361891	44349.211262	31.929165
598.530649	44421.764047	31.934183
599.074103	44507.567379	31.939200
599.502642	44586.595351	31.944218
600.177540	44659.866665	31.949236
600.551096	44745.805054	31.954253
601.178630	44832.652845	31.959271
602.205921	44919.577532	31.964288
602.901593	44998.128647	31.969306
603.605388	45068.170661	31.974324
604.731014	45151.266433	31.979341
605.316071	45228.621135	31.984359
605.946626	45294.430734	31.989376
606.458365	45380.153812	31.994394
607.512726	45424.592084	31.999412
607.935183	45504.231522	32.004429
608.523542	45588.317652	32.009447
609.413340	45652.278498	32.014464
609.890502	45727.728745	32.019482
610.463195	45807.086364	32.024500
611.030994	45876.911813	32.029517
611.791118	45951.597336	32.034535
612.558622	46017.969594	32.039552
612.733560	46094.512190	32.044570
613.230484	46165.241600	32.049588
613.530242	46243.802137	32.054605
614.353679	46327.158340	32.059623
615.199260	46404.027128	32.064640
615.506568	46480.379496	32.069658
616.254402	46559.497242	32.074676
616.402684	46638.253678	32.079693
617.267562	46717.347321	32.084711
617.872064	46807.002510	32.089728
618.286056	46892.885819	32.094746
619.047871	46966.397752	32.099764
619.295821	47051.105675	32.104781
620.001817	47141.353614	32.109799
620.664961	47230.558452	32.114816
621.045961	47323.173449	32.119834
622.071122	47407.710372	32.124852
622.528397	47495.948924	32.129869
623.101760	47583.068839	32.134887
623.582328	47674.113369	32.139904
624.412282	47764.287430	32.144922
625.407027	47847.419946	32.149940
625.847470	47932.834880	32.154957
626.617033	48015.395928	32.159975
627.407824	48095.448628	32.164992
627.880148	48186.256084	32.170010
628.881725	48262.208356	32.175028
629.204084	48338.140721	32.180045
629.582582	48418.619741	32.185063
630.521921	48497.948328	32.190080
631.353760	48586.132437	32.195098
631.947182	48659.391506	32.200116
632.621092	48734.884200	32.205133
633.098027	48808.769357	32.210151
634.138597	48874.651670	32.215168
634.349743	48946.256965	32.220186
635.252260	49015.957389	32.225204
636.329958	49078.905155	32.230221
636.862681	49149.897634	32.235239
637.410449	49217.003271	32.240256
637.694860	49291.983052	32.245274
638.596486	49366.505782	32.250292
638.907978	49438.438549	32.255309
639.528732	49517.643406	32.260327
640.298723	49586.151540	32.265344
641.142761	49656.040221	32.270362
642.338697	49711.941908	32.275380
643.192237	49776.160460	32.280397
643.776063	49857.093222	32.285415
644.493878	49908.862772	32.290432
645.528325	49968.649887	32.295450
646.060959	50021.404081	32.300468
646.999957	50092.993864	32.305485
647.667603	50155.357104	32.310503
648.404191	50202.682722	32.315520
648.599515	50264.734270	32.320538
649.015840	50327.200604	32.325556
649.557864	50396.417530	32.330573
649.853177	50465.527774	32.335591
650.517950	50537.952785	32.340608
650.842641	50620.472653	32.345626
651.276417	50687.992714	32.350644
651.921267	50763.762358	32.355661
652.643413	50852.465859	32.360679
653.119804	50930.122664	32.365696
653.422817	51025.510875	32.370714
653.994733	51104.557981	32.375732
654.696702	51204.851458	32.380749
654.934779	51292.664352	32.385767
655.868596	51380.722959	32.390784
656.526297	51481.081507	32.395802
656.734665	51569.899845	32.400820
657.068451	51670.765519	32.405837
657.852350	51773.889687	32.410855
658.670551	51879.723485	32.415872
659.182957	51983.751653	32.420890
660.112639	52074.540742	32.425908
660.282982	52186.153300	32.430925
660.742754	52287.210719	32.435943
661.476238	52384.669517	32.440960
662.095486	52504.844339	32.445978
663.252819	52612.881034	32.450996
663.871829	52715.503644	32.456013
664.641962	52815.723759	32.461031
665.418353	52913.741218	32.466048
665.950826	53011.183477	32.471066
666.695611	53115.294181	32.476084
668.109441	53200.538145	32.481101
668.809262	53306.960120	32.486119
669.678658	53391.264903	32.491136
670.650548	53470.345961	32.496154
671.241074	53560.826894	32.501172
672.303768	53645.614890	32.506189
672.692867	53725.699318	32.511207
673.611651	53801.910519	32.516224
674.162051	53896.195899	32.521242
674.837969	53987.323223	32.526260
675.241990	54067.646945	32.531277
675.936062	54152.975436	32.536295
676.747443	54239.108535	32.541312
677.285029	54308.780712	32.546330
678.105533	54375.390198	32.551348
679.040734	54456.195272	32.556365
679.536229	54536.601185	32.561383
680.056196	54619.617144	32.566400
680.724791	54697.939784	32.571418
680.739452	54786.306989	32.576436
681.542427	54865.235647	32.581453
681.692388	54950.645892	32.586471
682.321849	55045.815775	32.591488
682.847518	55141.932580	32.596506
683.611632	55248.340563	32.601524
684.527196	55338.404002	32.606541
684.816694	55448.051471	32.611559
685.748118	55536.910750	32.616576
686.452903	55636.982185	32.621594
687.188598	55733.239358	32.626612
688.051648	55834.280432	32.631629
688.878524	55938.510933	32.636647
689.071098	56028.500340	32.641664
689.666867	56139.121942	32.646682
690.376095	56241.081178	32.651700
691.462886	56342.342512	32.656717
691.890820	56453.542455	32.661735
692.575643	56553.633509	32.666752
693.392992	56659.773628	32.671770
694.425227	56749.026673	32.676788
695.565061	56836.193639	32.681805
696.607179	56936.211349	32.686823
697.573376	57017.513906	32.691840
698.419050	57106.575982	32.696858
699.177480	57190.114153	32.701876
699.997192	57271.396205	32.706893
700.377057	57358.475220	32.711911
701.461070	57431.900024	32.716928
701.993039	57519.829216	32.721946
702.253335	57615.763325	32.726964
702.818480	57697.067691	32.731981
703.164048	57800.337332	32.736999
704.093768	57884.629574	32.742016
704.955672	57987.268514	32.747034
705.325605	58077.478317	32.752052
706.125815	58180.203687	32.757069
706.379122	58266.926035	32.762087
707.522424	58362.775460	32.767104
708.140695	58471.916855	32.772122
709.070297	58557.357072	32.777140
710.357164	58641.956796	32.782157
711.114911	58734.266636	32.787175
711.971591	58826.365121	32.792192
712.462123	58918.603576	32.797210
712.928352	58999.725257	32.802228
713.971056	59094.473004	32.807245
714.565631	59182.733886	32.812263
715.301751	59267.200500	32.817280
715.710538	59358.807807	32.822298
716.320254	59457.618743	32.827316
717.031034	59556.686426	32.832333
717.537753	59653.533106	32.837351
718.328980	59746.404877	32.842368
719.044395	59843.523452	32.847386
719.468273	59938.054895	32.852404
719.948124	60046.110979	32.857421
720.799384	60153.862514	32.862439
721.303157	60251.895693	32.867456
722.553084	60355.116828	32.872474
722.974143	60454.872829	32.877492
723.675809	60555.895581	32.882509
724.226489	60655.524489	32.887527
724.943306	60743.012261	32.892544
725.543788	60844.457160	32.897562
726.406827	60938.157752	32.902580
727.168597	61038.027342	32.907597
727.347383	61145.806242	32.912615
728.832543	61250.038755	32.917632
729.432562	61345.560836	32.922650
729.765554	61445.302986	32.927668
730.546453	61551.204268	32.932685
730.906745	61662.957657	32.937703
731.641412	61766.797132	32.942720
732.556519	61879.749648	32.947738
732.939451	61985.765752	32.952756
733.715019	62086.029889	32.957773
734.619689	62210.424385	32.962791
734.795185	62326.520651	32.967808
736.001099	62445.760557	32.972826
736.626323	62563.116881	32.977844
737.469523	62679.844562	32.982861
737.792946	62799.616847	32.987879
738.735680	62920.122020	32.992896
739.553122	63043.692382	32.997914
739.946102	63163.594792	33.002932
741.172387	63283.417928	33.007949
741.337692	63405.300642	33.012967
742.142622	63536.731709	33.017984
743.447828	63652.163437	33.023002
743.939100	63781.777353	33.028020
744.722236	63901.812121	33.033037
745.445634	64030.454020	33.038055
745.918182	64155.843835	33.043072
747.214595	64280.320236	33.048090
747.791557	64398.876591	33.053108
748.830362	64511.283512	33.058125
749.948800	64641.069542	33.063143
750.818050	64759.974343	33.068160
751.508755	64875.406622	33.073178
752.286181	64986.299166	33.078196
753.106252	65105.599488	33.083213
753.916803	65218.159260	33.088231
754.650992	65326.584614	33.093248
755.576103	65446.845086	33.098266
756.576802	65563.783091	33.103284
757.713706	65660.598763	33.108301
758.867960	65752.815627	33.113319
760.012789	65849.282563	33.118336
761.202939	65947.097659	33.123354
762.060178	66032.543281	33.128372
762.811167	66112.592563	33.133389
763.544183	66214.412013	33.138407
764.761624	66296.370535	33.143424
765.353679	66383.568327	33.148442
765.930663	66465.241471	33.153460
766.259363	66561.680625	33.158477
767.244945	66662.550591	33.163495
767.660530	66752.848027	33.168512
768.518433	66846.482857	33.173530
768.703177	66939.438335	33.178548
769.704071	67038.509238	33.183565
770.028323	67150.735827	33.188583
770.774681	67243.553811	33.193600
771.688805	67349.420632	33.198618
771.941071	67456.056355	33.203636
772.492016	67557.612077	33.208653
773.035355	67677.822546	33.213671
773.678701	67799.176622	33.218688
774.334198	67902.680168	33.223706
774.934873	68021.274999	33.228724
775.572804	68138.857785	33.233741
776.092959	68255.167855	33.238759
777.073084	68373.939166	33.243776
778.051681	68486.322386	33.248794
778.478788	68597.899653	33.253812
779.084119	68715.806765	33.258829
780.509469	68822.733003	33.263847
781.390728	68938.122119	33.268864
782.575120	69051.602664	33.273882
783.424531	69170.531073	33.278900
784.151519	69285.439327	33.283917
784.554105	69390.641104	33.288935
785.181258	69498.904556	33.293952
786.025099	69624.699952	33.298970
786.658254	69746.330700	33.303988
787.635178	69854.426879	33.309005
788.554929	69969.415614	33.314023
789.204131	70084.333241	33.319040
790.117101	70205.593035	33.324058
790.699762	70329.805326	33.329076
791.535245	70452.598161	33.334093
792.493406	70563.454792	33.339111
793.095635	70693.250915	33.344128
794.055575	70810.453403	33.349146
794.628987	70941.154473	33.354164
795.434060	71062.903734	33.359181
796.189929	71173.022051	33.364199
796.568394	71311.050574	33.369216
797.531601	71443.250913	33.374234
797.930803	71575.920191	33.379252
798.772109	71705.620544	33.384269
799.618194	71855.002825	33.389287
800.696905	71992.659286	33.394304
801.468991	72126.704138	33.399322
801.780221	72266.394699	33.404340
802.806215	72414.080103	33.409357
803.602531	72547.401344	33.414375
804.762428	72682.224216	33.419392
805.821248	72811.579279	33.424410
806.635286	72950.751399	33.429428
807.433627	73071.459686	33.434445
808.354263	73203.802135	33.439463
809.172292	73333.729415	33.444480
810.121143	73471.565869	33.449498
810.568544	73609.785545	33.454516
811.216594	73739.209431	33.459533
812.339330	73880.098674	33.464551
813.038208	74015.785793	33.469568
813.931590	74146.807201	33.474586
814.895401	74281.858855	33.479604
815.625101	74415.681184	33.484621
816.610576	74558.153477	33.489639
817.266692	74699.006086	33.494656
818.285461	74824.779794	33.499674
818.888071	74967.326870	33.504692
820.074795	75095.127576	33.509709
820.713559	75229.867540	33.514727
821.529634	75362.097666	33.519744
822.528785	75489.752270	33.524762
823.402356	75615.780407	33.529780
824.536895	75741.388248	33.534797
825.736513	75863.680314	33.539815
826.899710	75988.322097	33.544832
828.051223	76097.651376	33.549850
828.771543	76198.751428	33.554868
829.808652	76312.913122	33.559885
830.895923	76418.770187	33.564903
831.398055	76523.313183	33.569920
832.005061	76625.775330	33.574938
832.441434	76728.986639	33.579956
833.193443	76838.546131	33.584973
834.231575	76953.293063	33.589991
834.818622	77069.035865	33.595008
835.322227	77170.654831	33.600026
836.077972	77286.954862	33.605044
837.274950	77403.072283	33.610061
838.133232	77526.717395	33.615079
838.562218	77640.865847	33.620096
839.469239	77759.487797	33.625114
840.231297	77885.125824	33.630132
841.032230	78003.106688	33.635149
841.859188	78134.829142	33.640167
842.549197	78254.526010	33.645184
843.033544	78383.098190	33.650202
843.799556	78509.029816	33.655220
844.545574	78643.997847	33.660237
845.742907	78777.147594	33.665255
846.202048	78921.752068	33.670272
847.389044	79057.109136	33.675290
847.983047	79198.590085	33.680308
848.720401	79323.833115	33.685325
849.461962	79464.747551	33.690343
850.308535	79612.360841	33.695360
851.502416	79742.601883	33.700378
852.111214	79894.510713	33.705396
853.075767	80040.967574	33.710413
853.877051	80180.292621	33.715431
854.524977	80324.482067	33.720448
855.868081	80463.787032	33.725466
856.412178	80601.938185	33.730484
857.660789	80747.505410	33.735501
858.416656	80884.826614	33.740519
859.186031	81032.117402	33.745536
860.470209	81169.369941	33.750554
860.894754	81321.758793	33.755572
861.661220	81459.841330	33.760589
862.835587	81597.442565	33.765607
863.714747	81742.794048	33.770624
864.474872	81884.553951	33.775642
865.525470	82034.935442	33.780660
866.301815	82186.843086	33.785677
867.162925	82329.628358	33.790695
867.996484	82471.189642	33.795712
868.981544	82598.739816	33.800730
870.455934	82746.182543	33.805748
871.197682	82886.911352	33.810765
872.160217	83029.443517	33.815783
872.683626	83170.803432	33.820800
873.621698	83306.371966	33.825818
874.848292	83451.487722	33.830836
875.436235	83584.641604	33.835853
876.052389	83729.322178	33.840871
877.011052	83880.082584	33.845888
877.969713	84023.545285	33.850906
878.498629	84170.699916	33.855924
879.225312	84311.095964	33.860941
880.126370	84462.704739	33.865959
880.702239	84620.472779	33.870976
881.422014	84770.400936	33.875994
882.822012	84925.773433	33.881012
883.460937	85075.285002	33.886029
884.758476	85226.164115	33.891047
885.170112	85380.413986	33.896064
886.171230	85525.930301	33.901082
887.286990	85676.561442	33.906100
887.967278	85818.644734	33.911117
889.345095	85955.690151	33.916135
890.350110	86088.726905	33.921152
891.005843	86222.744010	33.926170
891.833578	86360.270292	33.931188
892.855844	86505.712157	33.936205
893.925252	86638.171088	33.941223
894.267637	86780.438689	33.946240
895.277987	86918.775367	33.951258
895.762109	87061.440321	33.956276
896.378287	87218.696557	33.961293
897.577376	87369.678201	33.966311
898.412442	87533.035312	33.971328
899.167030	87676.281850	33.976346
900.474092	87824.258186	33.981364
901.194880	87973.188806	33.986381
902.223647	88121.222877	33.991399
903.235165	88281.400976	33.996416
904.647963	88423.128711	34.001434
905.942535	88567.777747	34.006452
907.293272	88695.170701	34.011469
908.591128	88822.534462	34.016487
909.799120	88958.454533	34.021504
910.662354	89083.656993	34.026522
911.542557	89218.374928	34.031540
912.406540	89364.463968	34.036557
913.144248	89481.804955	34.041575
914.085186	89623.257435	34.046592
915.250803	89745.069538	34.051610
915.869915	89869.502412	34.056628
916.571670	90011.463095	34.061645
917.848785	90143.879825	34.066663
918.228689	90288.211487	34.071680
919.068714	90434.537618	34.076698
919.480802	90578.168572	34.081716
919.979362	90731.241388	34.086733
920.979178	90875.884362	34.091751
921.821222	91035.406671	34.096768
922.689674	91189.437811	34.101786
923.381968	91341.773632	34.106804
924.153488	91510.308126	34.111821
925.295712	91657.530748	34.116839
925.989656	91822.074047	34.121856
927.301229	91972.605030	34.126874
928.862041	92126.684608	34.131892
929.785339	92279.926868	34.136909
931.047068	92427.387991	34.141927
931.853269	92575.668955	34.146944
933.059339	92729.084661	34.151962
934.246988	92874.620307	34.156980
934.931232	93027.662920	34.161997
935.853420	93159.958254	34.167015
937.308685	93305.454041	34.172032
938.229558	93435.241124	34.177050
939.358409	93584.870693	34.182068
939.773828	93724.954244	34.187085
940.531175	93863.907503	34.192103
941.395510	94013.022855	34.197120
942.207888	94158.940208	34.202138
943.733834	94306.432345	34.207156
944.374967	94455.001705	34.212173
945.341440	94594.762076	34.217191
946.517215	94746.139127	34.222208
947.200548	94886.046543	34.227226
948.141788	95028.981715	34.232244
948.487329	95185.827347	34.237261
949.530011	95337.988654	34.242279
950.077360	95496.059147	34.247296
950.739040	95644.022512	34.252314
952.147580	95787.699243	34.257332
952.667490	95943.874895	34.262349
953.908518	96091.331350	34.267367
954.735179	96232.464597	34.272384
956.028740	96377.708519	34.277402
957.105574	96530.922387	34.282420
957.688029	96684.227080	34.287437
958.959487	96831.986468	34.292455
960.024296	96971.856125	34.297472
960.492547	97125.561131	34.302490
961.638495	97275.269068	34.307508
962.349845	97443.160656	34.312525
963.468493	97594.142033	34.317543
964.188775	97765.697488	34.322560
964.991801	97923.651355	34.327578
966.590889	98073.254067	34.332596
967.655370	98239.687426	34.337613
968.673623	98387.582426	34.342631
969.495895	98548.819714	34.347648
970.703994	98705.142061	34.352666
971.633233	98849.097862	34.357684
972.605080	99002.504862	34.362701
973.939365	99155.196627	34.367719
974.950858	99314.962917	34.372736
976.103498	99467.393022	34.377754
976.807263	99623.038144	34.382772
977.599421	99787.354298	34.387789
978.642839	99940.970071	34.392807
979.752311	100101.903926	34.397824
979.957537	100258.542947	34.402842
980.721603	100424.857132	34.407860
981.929314	100593.727024	34.412877
982.884100	100765.451893	34.417895
983.786649	100930.212942	34.422912
984.821305	101113.476795	34.427930
985.945262	101280.803950	34.432948
986.719593	101459.774576	34.437965
987.564023	101629.365959	34.442983
988.745966	101796.509167	34.448000
989.377660	101986.243541	34.453018
990.277565	102156.361445	34.458036
991.302193	102347.709934	34.463053
992.347072	102525.249346	34.468071
993.184568	102728.559912	34.473088
993.942953	102910.228780	34.478106
995.209402	103088.750817	34.483124
996.033174	103281.239195	34.488141
997.204450	103461.223525	34.493159
998.141779	103651.680304	34.498176
999.240671	103840.908357	34.503194
1000.565703	104021.112532	34.508212
1001.563375	104198.503419	34.513229
1002.428156	104383.485602	34.518247
1003.617041	104571.372356	34.523264
1004.418302	104768.513456	34.528282
1005.578426	104944.234508	34.533300
1006.536187	105129.206224	34.538317
1007.589092	105330.039002	34.543335
1008.727852	105502.913373	34.548352
1009.490993	105695.006621	34.553370
1010.500444	105875.625138	34.558388
1011.329654	106065.136115	34.563405
1012.352860	106247.960762	34.568423
1013.374844	106445.292598	34.573440
1014.573520	106626.658947	34.578458
1016.126467	106810.899921	34.583476
1016.901770	106989.925235	34.588493
1017.938611	107163.622825	34.593511
1019.472488	107327.099139	34.598528
1020.269091	107493.684254	34.603546
1021.818069	107651.960750	34.608564
1022.842005	107818.816173	34.613581
1023.973099	107982.257207	34.618599
1024.704308	108142.807013	34.623616
1025.457542	108309.669137	34.628634
1026.524206	108482.354217	34.633652
1027.547709	108660.461655	34.638669
1028.417432	108831.949253	34.643687
1029.120656	109005.898517	34.648704
1030.191899	109178.079081	34.653722
1031.337634	109356.665490	34.658740
1031.918634	109540.946325	34.663757
1032.773455	109730.232406	34.668775
1033.814021	109913.885265	34.673792
1035.277800	110108.074489	34.678810
1036.054923	110281.917045	34.683828
1037.158420	110475.758889	34.688845
1038.128696	110664.892405	34.693863
1039.194637	110849.509951	34.698880
1040.039011	111050.725521	34.703898
1041.350890	111241.495295	34.708916
1042.118673	111431.920091	34.713933
1043.344846	111630.136952	34.718951
1044.400287	111831.945293	34.723968
1045.313411	112022.261699	34.728986
1046.333248	112209.645506	34.734004
1047.862200	112421.769725	34.739021
1048.094951	112614.821009	34.744039
1049.488672	112812.054298	34.749056
1050.254907	113022.005944	34.754074
1051.447994	113219.792847	34.759092
1052.658337	113427.419819	34.764109
1053.894897	113642.032022	34.769127
1054.998614	113835.663667	34.774144
1055.410992	114048.720493	34.779162
1056.509077	114256.648780	34.784180
1057.537003	114465.007769	34.789197
1058.671641	114681.645934	34.794215
1059.637583	114887.873591	34.799232
1060.989684	115103.960187	34.804250
1061.983181	115313.217186	34.809268
1062.737003	115529.171634	34.814285
1063.517467	115740.924965	34.819303
1065.145032	115963.619547	34.824320
1065.824418	116180.819731	34.829338
1066.948689	116393.334691	34.834356
1067.761571	116616.059246	34.839373
1069.391316	116820.265780	34.844391
1070.944106	117031.613786	34.849408
1072.372231	117249.945962	34.854426
1073.850111	117456.615039	34.859444
1075.784160	117648.576448	34.864461
1076.736485	117837.458085	34.869479
1077.993491	118029.603529	34.874496
1078.651839	118226.993470	34.879514
1079.903851	118411.074455	34.884532
1080.816565	118596.135409	34.889549
1081.646691	118797.852147	34.894567
1083.218985	118984.181635	34.899584
1084.203612	119183.884756	34.904602
1085.243723	119369.069032	34.909620
1086.304703	119561.176765	34.914637
1087.323488	119752.873466	34.919655
1088.407227	119941.250217	34.924672
1089.469934	120127.791875	34.929690
1090.457522	120309.158060	34.934708
1091.911455	120489.970054	34.939725
1092.330091	120673.063375	34.944743
1093.624454	120850.997157	34.949760
1094.417143	121047.632101	34.954778
1095.392469	121226.454763	34.959796
1096.572114	121426.341873	34.964813
1097.123550	121612.526698	34.969831
1098.123386	121817.277065	34.974848
1098.815987	122028.558875	34.979866
1099.792990	122221.301772	34.984884
1101.069212	122428.739434	34.989901
1101.774517	122645.210963	34.994919
1103.012108	122843.396303	34.999936
1103.992287	123064.711093	35.004954
1105.476137	123269.443936	35.009972
1106.761072	123479.778099	35.014989
1108.062748	123694.969487	35.020007
1109.311027	123891.242770	35.025024
1109.971318	124109.112064	35.030042
1111.127157	124330.545896	35.035060
1112.586504	124531.445096	35.040077
1112.910238	124760.204670	35.045095
1114.241387	124973.812481	35.050112
1116.141990	125189.615830	35.055130
1117.274575	125404.677877	35.060148
1118.781647	125616.155554	35.065165
1119.410114	125830.575629	35.070183
1121.090904	126043.017877	35.075200
1121.770584	126254.501515	35.080218
1122.978871	126461.628008	35.085236
1124.109018	126679.500923	35.090253
1124.525376	126908.663984	35.095271
1126.161124	127116.551496	35.100288
1127.115996	127347.840229	35.105306
1128.442306	127569.188760	35.110324
1129.983862	127791.989182	35.115341
1130.767368	128006.903753	35.120359
1131.903112	128223.591269	35.125376
1133.214028	128446.520093	35.130394
1134.365225	128658.601881	35.135412
1135.529940	128870.796808	35.140429
1136.506148	129100.429792	35.145447
1137.598630	129318.880609	35.150464
1138.790670	129544.079563	35.155482
1139.914299	129765.293739	35.160500
1141.534723	129987.750833	35.165517
1142.748178	130204.195246	35.170535
1143.897385	130422.109937	35.175552
1144.848024	130650.867106	35.180570
1145.579209	130863.761537	35.185588
1147.600875	131064.642227	35.190605
1148.816705	131284.606347	35.195623
1150.078176	131500.301142	35.200640
1151.012221	131721.834197	35.205658
1151.844255	131934.641967	35.210676
1153.299683	132151.375458	35.215693
1154.116028	132383.956667	35.220711
1155.425171	132596.553389	35.225728
1156.298567	132811.960128	35.230746
1157.359313	133034.698107	35.235764
1158.624695	133249.157396	35.240781
1159.883807	133480.050896	35.245799
1161.150569	133701.694106	35.250816
1162.198998	133923.715206	35.255834
1162.973075	134149.181050	35.260852
1164.364106	134373.003363	35.265869
1165.366481	134590.263841	35.270887
1166.756441	134813.682464	35.275904
1167.237008	135029.237553	35.280922
1168.513310	135235.355044	35.285940
1169.855282	135451.855900	35.290957
1170.835679	135678.248810	35.295975
1172.007354	135894.676919	35.300992
1173.311054	136124.028875	35.306010
1174.477112	136334.064341	35.311028
1175.613986	136551.224323	35.316045
1176.549637	136787.058262	35.321063
1177.730051	137005.038413	35.326080
1178.668832	137230.328789	35.331098
1180.096966	137461.178043	35.336116
1181.625560	137690.566045	35.341133
1182.429084	137914.180438	35.346151
1183.300031	138151.135490	35.351168
1184.500306	138397.113763	35.356186
1185.492070	138631.958430	35.361204
1186.799014	138869.242256	35.366221
1187.952402	139127.630254	35.371239
1189.248956	139362.900394	35.376256
1190.175992	139605.780479	35.381274
1191.324138	139855.746677	35.386292
1192.481632	140102.108540	35.391309
1193.918109	140355.268361	35.396327
1194.774318	140607.606610	35.401344
1196.117916	140860.034865	35.406362
1197.076312	141114.796437	35.411380
1198.228463	141362.447380	35.416397
1199.737426	141616.770049	35.421415
1201.482984	141878.265631	35.426432
1203.238552	142121.498257	35.431450
1203.615369	142381.078656	35.436468
1205.199906	142627.805309	35.441485
1206.494932	142874.147008	35.446503
1207.843379	143128.261496	35.451520
1209.049733	143381.815715	35.456538
1210.367541	143633.056582	35.461556
1211.556457	143877.579569	35.466573
1212.616324	144133.787730	35.471591
1214.142688	144375.963102	35.476608
1215.366208	144624.571092	35.481626
1216.267952	144880.414351	35.486644
1218.051797	145119.519590	35.491661
1218.821928	145371.070621	35.496679
1220.116498	145626.284989	35.501696
1221.436492	145882.372416	35.506714
1222.663586	146136.863738	35.511732
1224.834970	146375.254178	35.516749
1225.817188	146618.896155	35.521767
1226.913131	146866.037295	35.526784
1228.649452	147105.616142	35.531802
1229.675709	147343.949135	35.536820
1230.662436	147576.476159	35.541837
1231.662375	147823.954175	35.546855
1232.900569	148079.227507	35.551872
1233.935254	148324.024252	35.556890
1235.412935	148569.577819	35.561908
1236.711317	148816.125253	35.566925
1237.652890	149069.241203	35.571943
1238.968635	149321.601657	35.576960
1239.688276	149569.626705	35.581978
1240.821868	149825.242094	35.586996
1242.471114	150092.316148	35.592013
1243.860763	150347.754294	35.597031
1244.904961	150598.221137	35.602048
1246.045610	150858.321045	35.607066
1247.212280	151112.502942	35.612084
1248.444973	151349.704391	35.617101
1249.450731	151599.115558	35.622119
1250.987579	151840.790428	35.627136
1252.185213	152086.111775	35.632154
1253.234289	152335.976444	35.637172
1254.670261	152580.386783	35.642189
1256.013345	152829.179426	35.647207
1257.257406	153080.400521	35.652224
1258.294137	153326.577585	35.657242
1259.319904	153579.612227	35.662260
1260.806547	153819.310498	35.667277
1262.538124	154067.324197	35.672295
1263.991847	154309.136907	35.677312
1265.499628	154563.522203	35.682330
1266.525262	154803.550637	35.687348
1267.874807	155038.311970	35.692365
1269.777182	155281.442208	35.697383
1270.972312	155522.983110	35.702400
1272.945402	155739.813909	35.707418
1274.552067	155970.692302	35.712436
1275.751981	156189.372255	35.717453
1277.248968	156426.756561	35.722471
1278.535902	156658.906384	35.727488
1279.608949	156884.425835	35.732506
1280.778648	157122.232299	35.737524
1282.264585	157341.722273	35.742541
1283.681542	157584.125495	35.747559
1284.345198	157807.033870	35.752576
1285.950600	158045.385138	35.757594
1286.795948	158285.493984	35.762612
1288.478479	158518.325372	35.767629
1289.360672	158759.763304	35.772647
1290.868907	159005.915678	35.777664
1291.858626	159243.949056	35.782682
1292.650483	159502.314147	35.787700
1293.903777	159743.355063	35.792717
1295.040861	160003.915280	35.797735
1295.905596	160264.392259	35.802752
1297.044016	160527.912493	35.807770
1297.924151	160789.074793	35.812788
1299.457844	161072.391325	35.817805
1300.336309	161345.972520	35.822823
1301.614115	161619.136894	35.827840
1302.874980	161899.478216	35.832858
1303.920309	162180.743207	35.837876
1305.377053	162460.738907	35.842893
1306.742669	162758.791059	35.847911
1307.635836	163036.236690	35.852928
1309.143107	163328.175167	35.857946
1310.002582	163619.581533	35.862964
1311.627063	163903.873827	35.867981
1312.888652	164210.074392	35.872999
1314.458614	164511.213046	35.878016
1315.784220	164791.150279	35.883034
1317.147093	165090.546450	35.888052
1318.745351	165370.519580	35.893069
1320.421232	165669.856610	35.898087
1322.368865	165949.904393	35.903104
1323.828732	166236.898545	35.908122
1324.727878	166519.817147	35.913140
1326.203083	166796.006336	35.918157
1327.491738	167076.745875	35.923175
1328.870383	167369.356691	35.928192
1330.583796	167631.761210	35.933210
1331.579949	167913.438649	35.938228
1333.041605	168197.444067	35.943245
1334.292394	168478.575999	35.948263
1335.368353	168752.435573	35.953280
1337.253482	168998.743724	35.958298
1338.436939	169264.576522	35.963316
1339.835256	169507.674031	35.968333
1341.425518	169773.445003	35.973351
1342.369975	170036.638893	35.978368
1344.272531	170292.217705	35.983386
1345.568172	170549.771612	35.988404
1346.919439	170812.498257	35.993421
1348.396098	171072.361959	35.998439
1349.608355	171323.430466	36.003456
1351.294969	171577.320601	36.008474
1352.576461	171849.051654	36.013492
1353.474067	172103.460670	36.018509
1354.828865	172360.973389	36.023527
1355.902084	172631.089110	36.028544
1357.506161	172892.373902	36.033562
1358.249729	173171.215686	36.038580
1359.639761	173449.309679	36.043597
1360.895347	173728.136783	36.048615
1362.174877	174012.560923	36.053632
1363.402219	174290.137321	36.058650
1364.944205	174572.693861	36.063668
1366.106662	174854.180668	36.068685
1367.296478	175151.676529	36.073703
1368.796519	175441.874252	36.078720
1370.128908	175728.492945	36.083738
1371.179817	176027.042284	36.088756
1372.449651	176336.618672	36.093773
1373.994302	176629.099278	36.098791
1375.151121	176934.060660	36.103808
1376.397208	177244.621890	36.108826
1377.594714	177556.639489	36.113844
1379.079682	177871.559295	36.118861
1380.365221	178177.012914	36.123879
1381.376817	178503.006105	36.128896
1383.157209	178814.022702	36.133914
1384.487148	179135.092117	36.138932
1385.838605	179462.737300	36.143949
1387.127391	179785.948904	36.148967
1388.191804	180112.904864	36.153984
1389.651808	180431.799764	36.159002
1391.083717	180768.529531	36.164020
1392.660498	181097.135884	36.169037
1393.969421	181429.341069	36.174055
1395.096160	181772.751168	36.179072
1396.727026	182101.073216	36.184090
1397.763996	182430.860875	36.189108
1399.172707	182768.845995	36.194125
1400.762723	183104.340263	36.199143
1402.276143	183450.311929	36.204160
1404.153581	183784.163439	36.209178
1406.342063	184106.207737	36.214196
1407.355362	184427.395669	36.219213
1409.378705	184747.715365	36.224231
1410.610384	185080.275351	36.229248
1412.600102	185392.017463	36.234266
1414.615043	185712.011327	36.239284
1415.985371	186011.457442	36.244301
1417.637095	186316.575234	36.249319
1419.001734	186621.840447	36.254336
1420.484581	186927.494432	36.259354
1421.748648	187241.159012	36.264372
1423.179631	187546.645086	36.269389
1424.774960	187884.897373	36.274407
1425.973889	188240.916434	36.279424
1427.428598	188536.978225	36.284442
1428.754376	188845.938770	36.289460
1430.022665	189136.189335	36.294477
1431.513689	189436.464223	36.299495
1432.523040	189733.513272	36.304512
1433.669714	190020.330700	36.309530
1434.883469	190314.047218	36.314548
1436.405474	190624.912273	36.319565
1437.792809	190922.184596	36.324583
1438.982843	191238.386509	36.329600
1440.206234	191542.239362	36.334618
1441.704505	191857.531035	36.339636
1442.652517	192183.349330	36.344653
1444.285138	192493.541468	36.349671
1445.424992	192822.201698	36.354688
1446.744012	193141.080803	36.359706
1447.938689	193478.751472	36.364724
1449.484965	193815.504361	36.369741
1450.893539	194144.278335	36.374759
1452.074550	194490.793349	36.379776
1453.635642	194832.067931	36.384794
1454.968572	195168.121026	36.389812
1456.017343	195519.917458	36.394829
1457.485785	195874.875084	36.399847
1458.896512	196242.187765	36.404864
1460.607330	196584.814942	36.409882
1462.379484	196940.692978	36.414900
1463.930752	197295.336381	36.419917
1465.415111	197646.638090	36.424935
1466.781074	198008.704118	36.429952
1469.090863	198349.412758	36.434970
1471.375583	198683.801015	36.439988
1472.829861	199022.917730	36.445005
1475.086236	199343.340778	36.450023
1476.624780	199683.106186	36.455040
1478.255766	200009.724956	36.460058
1479.764785	200344.746189	36.465076
1481.013582	200668.708068	36.470093
1482.487260	200998.096867	36.475111
1484.179126	201323.870436	36.480128
1486.003142	201654.170965	36.485146
1487.782938	201978.890516	36.490164
1489.305075	202281.373046	36.495181
1491.055897	202597.664657	36.500199
1492.318928	202916.192384	36.505216
1493.707395	203236.275994	36.510234
1495.198519	203558.173079	36.515252
1496.507201	203890.311141	36.520269
1498.004999	204214.443729	36.525287
1499.306190	204542.621265	36.530304
1500.744172	204863.893779	36.535322
1501.984652	205199.626532	36.540340
1503.574776	205530.783402	36.545357
1505.075693	205857.001193	36.550375
1506.296204	206186.565762	36.555392
1507.653976	206516.922250	36.560410
1508.840025	206867.984188	36.565428
1509.874755	207214.904258	36.570445
1511.201707	207561.652108	36.575463
1512.573559	207917.436973	36.580480
1514.194522	208281.617248	36.585498
1515.560813	208640.808092	36.590516
1516.795729	209005.583338	36.595533
1518.032372	209363.042691	36.600551
1519.616902	209741.939318	36.605568
1520.878174	210108.439428	36.610586
1522.526886	210477.267319	36.615604
1524.038852	210857.675671	36.620621
1525.794828	211225.217586	36.625639
1526.987889	211605.244979	36.630656
1528.536764	211967.155248	36.635674
1530.465860	212309.623513	36.640692
1532.351255	212664.876997	36.645709
1534.538027	213009.083933	36.650727
1536.181800	213350.937458	36.655744
1537.452332	213693.561043	36.660762
1538.754052	214029.067042	36.665780
1540.196059	214388.710333	36.670797
1541.647134	214734.558315	36.675815
1542.855147	215083.620117	36.680832
1544.456317	215440.927728	36.685850
1546.166001	215803.502656	36.690868
1547.408951	216172.095431	36.695885
1549.052866	216537.221638	36.700903
1550.228921	216910.169533	36.705920
1551.918262	217275.568635	36.710938
1553.502275	217637.148492	36.715956
1554.918541	218019.611469	36.720973
1556.459100	218386.152384	36.725991
1558.094593	218763.983428	36.731008
1559.356241	219144.566028	36.736026
1561.454422	219514.703904	36.741044
1562.790899	219897.612375	36.746061
1564.653801	220271.369418	36.751079
1566.099880	220663.889225	36.756096
1567.719176	221045.814019	36.761114
1569.060147	221431.059643	36.766132
1570.596775	221832.914438	36.771149
1572.409456	222217.934081	36.776167
1574.039352	222595.615261	36.781184
1575.408381	222989.164098	36.786202
1577.070286	223381.447788	36.791220
1578.731216	223776.145088	36.796237
1580.488055	224154.314780	36.801255
1581.875303	224565.059582	36.806272
1583.954443	224946.201984	36.811290
1585.787124	225332.082725	36.816308
1586.912408	225727.676916	36.821325
1588.415440	226123.237375	36.826343
1589.942547	226518.590800	36.831360
1591.456500	226918.696797	36.836378
1593.737968	227308.978254	36.841396
1595.321947	227708.107793	36.846413
1597.026372	228097.768074	36.851431
1598.335301	228499.226819	36.856448
1600.377596	228892.288943	36.861466
1602.099099	229290.634365	36.866484
1603.296322	229686.343450	36.871501
1605.011584	230074.350087	36.876519
1606.575302	230474.929839	36.881536
1608.443694	230873.200750	36.886554
1609.863706	231265.520872	36.891572
1611.207533	231668.623968	36.896589
1612.764517	232063.792824	36.901607
1614.502503	232478.214671	36.906624
1616.152947	232877.356763	36.911642
1617.926935	233277.698610	36.916660
1619.178960	233681.907004	36.921677
1620.559454	234085.663091	36.926695
1622.256323	234505.627757	36.931712
1623.778167	234918.607967	36.936730
1625.346357	235315.347511	36.941748
1627.088819	235733.169905	36.946765
1628.653953	236145.583208	36.951783
1629.922611	236560.303383	36.956800
1631.571685	236978.037390	36.961818
1633.667290	237389.629548	36.966836
1634.964718	237808.636947	36.971853
1636.641264	238210.386262	36.976871
1638.396242	238614.205881	36.981888
1640.306205	239029.787933	36.986906
1642.136757	239406.463727	36.991924
1643.892302	239794.582310	36.996941
1645.558664	240175.855398	37.001959
1647.358802	240559.063077	37.006976
1649.264801	240950.382701	37.011994
1650.938596	241334.167898	37.017012
1652.796813	241723.105915	37.022029
1654.317672	242116.592483	37.027047
1655.902907	242500.974006	37.032064
1657.454013	242888.002170	37.037082
1658.654564	243275.719625	37.042100
1660.127196	243677.238489	37.047117
1661.877811	244083.361868	37.052135
1663.498865	244482.188717	37.057152
1664.894411	244897.612790	37.062170
1666.471747	245310.086258	37.067188
1668.500765	245723.123273	37.072205
1669.485804	246134.773244	37.077223
1671.057177	246552.782870	37.082240
1672.102181	246979.282225	37.087258
1674.042118	247415.141118	37.092276
1675.844092	247850.995168	37.097293
1677.704090	248282.266648	37.102311
1679.487799	248724.065600	37.107328
1680.944390	249160.199103	37.112346
1682.801728	249589.562585	37.117364
1684.513537	250030.581940	37.122381
1686.482396	250473.668264	37.127399
1688.489682	250903.868528	37.132416
1690.016713	251339.223179	37.137434
1691.693851	251776.305860	37.142452
1693.597340	252215.536435	37.147469
1695.238370	252650.183690	37.152487
1696.794562	253091.269578	37.157504
1697.975668	253544.808817	37.162522
1699.949874	253989.179579	37.167540
1701.371478	254449.866946	37.172557
1702.909019	254906.343429	37.177575
1704.857328	255356.403801	37.182592
1706.446110	255833.571200	37.187610
1708.099828	256274.199964	37.192628
1709.536274	256741.202097	37.197645
1711.231503	257213.775653	37.202663
1712.696770	257676.324725	37.207680
1714.394105	258151.231334	37.212698
1716.812942	258610.859045	37.217716
1718.742095	259071.476080	37.222733
1720.367155	259538.997061	37.227751
1722.322071	260007.353599	37.232768
1723.917524	260480.590566	37.237786
1725.880463	260945.513053	37.242804
1727.668614	261408.403600	37.247821
1729.668661	261856.654139	37.252839
1731.594903	262306.108216	37.257856
1733.562167	262775.518214	37.262874
1735.191012	263230.577571	37.267892
1737.028252	263680.598691	37.272909
1738.847547	264139.332702	37.277927
1740.739915	264580.273781	37.282944
1742.230305	265036.312199	37.287962
1744.324546	265484.024802	37.292980
1746.114465	265939.453533	37.297997
1747.715787	266392.344428	37.303015
1749.715394	266838.491070	37.308032
1751.106605	267296.465038	37.313050
1752.903191	267732.657718	37.318068
1754.384757	268166.383277	37.323085
1756.109793	268607.916816	37.328103
1758.100514	269038.333127	37.333120
1759.601667	269477.916547	37.338138
1761.327266	269913.678467	37.343156
1762.981698	270348.789104	37.348173
1764.334133	270785.163994	37.353191
1766.466115	271231.827755	37.358208
1767.580800	271678.826241	37.363226
1769.366203	272127.368321	37.368244
1770.972739	272586.704460	37.373261
1772.789083	273043.871974	37.378279
1774.602448	273500.123221	37.383296
1776.277081	273969.422229	37.388314
1777.944980	274431.049899	37.393332
1779.740880	274895.118425	37.398349
1781.227274	275362.458093	37.403367
1783.333766	275834.599498	37.408384
1784.811506	276314.556908	37.413402
1786.501972	276777.894672	37.418420
1788.413668	277265.955895	37.423437
1790.531077	277746.693379	37.428455
1792.493717	278233.648576	37.433472
1794.182621	278710.637821	37.438490
1796.182692	279197.149325	37.443508
1798.098965	279680.598033	37.448525
1799.469595	280169.334923	37.453543
1801.838984	280642.091512	37.458560
1803.379967	281132.903129	37.463578
1805.497250	281621.615127	37.468596
1807.228102	282108.759076	37.473613
1809.030563	282603.557459	37.478631
1810.611089	283107.909761	37.483648
1812.169301	283598.143164	37.488666
1814.658184	284084.240749	37.493684
1816.696380	284576.677557	37.498701
1818.445267	285074.234702	37.503719
1820.692936	285562.746520	37.508736
1822.017855	286064.197066	37.513754
1823.602862	286559.839094	37.518772
1825.555642	287056.486356	37.523789
1827.186384	287555.389379	37.528807
1829.397092	288062.297842	37.533824
1830.851309	288568.965240	37.538842
1832.386510	289064.545324	37.543860
1834.611965	289571.922043	37.548877
1836.174383	290076.249967	37.553895
1838.966459	290576.090390	37.558912
1841.192319	291060.349400	37.563930
1843.656716	291545.252843	37.568948
1845.866272	292040.196086	37.573965
1847.564292	292519.930574	37.578983
1849.690627	292994.236996	37.584000
1851.799985	293462.347271	37.589018
1853.761586	293939.845698	37.594036
1855.837927	294411.406645	37.599053
1857.514652	294885.082861	37.604071
1859.047767	295353.344515	37.609088
1860.345563	295836.618495	37.614106
1862.328507	296311.834664	37.619124
1864.140251	296800.072431	37.624141
1865.580797	297282.397931	37.629159
1867.466538	297768.407047	37.634176
1868.570840	298263.546806	37.639194
1870.799911	298754.698089	37.644212
1872.509653	299255.167175	37.649229
1874.401716	299743.823701	37.654247
1876.064528	300234.898077	37.659264
1878.262446	300711.160193	37.664282
1879.915797	301196.591565	37.669300
1881.728395	301674.860186	37.674317
1883.259684	302146.796728	37.679335
1885.309165	302613.139342	37.684352
1886.908041	303117.296190	37.689370
1888.598171	303604.578274	37.694388
1890.284538	304086.880972	37.699405
1892.116577	304587.027081	37.704423
1894.055879	305100.122898	37.709440
1895.575078	305598.201194	37.714458
1897.116807	306122.162508	37.719476
1898.911373	306633.412457	37.724493
1900.098473	307162.748948	37.729511
1901.848401	307690.697216	37.734528
1903.461309	308234.144722	37.739546
1905.561348	308775.860142	37.744564
1907.935358	309325.344372	37.749581
1909.028164	309877.357970	37.754599
1911.076001	310426.753806	37.759616
1912.753513	310988.206602	37.764634
1914.457334	311558.049740	37.769652
1916.686769	312125.367224	37.774669
1918.494396	312696.119430	37.779687
1921.150467	313269.980534	37.784704
1922.967300	313844.041978	37.789722
1924.612499	314409.824064	37.794740
1926.826087	314990.077789	37.799757
1928.952312	315565.642708	37.804775
1931.330445	316124.842560	37.809792
1933.621704	316704.326120	37.814810
1935.490591	317270.570291	37.819828
1937.506586	317847.544234	37.824845
1939.394840	318417.526524	37.829863
1941.491078	318987.215078	37.834880
1943.101204	319567.731832	37.839898
1945.167298	320148.930726	37.844916
1947.230054	320723.448459	37.849933
1949.249606	321303.979187	37.854951
1951.470421	321880.816474	37.859968
1953.513029	322457.724502	37.864986
1955.046160	323034.602809	37.870004
1957.396495	323614.237903	37.875021
1959.170543	324195.096868	37.880039
1961.114483	324771.429987	37.885056
1963.279522	325364.111304	37.890074
1965.076133	325947.986617	37.895092
1967.715745	326521.623476	37.900109
1969.350870	327100.255337	37.905127
1971.515671	327688.437105	37.910144
1973.636160	328265.809028	37.915162
1975.933331	328838.958709	37.920180
1977.935827	329412.780399	37.925197
1979.884239	329989.265977	37.930215
1981.938233	330561.413661	37.935232
1984.090611	331130.645396	37.940250
1986.092932	331698.090997	37.945268
1988.721059	332267.662693	37.950285
1990.744483	332838.005411	37.955303
1992.823308	333403.587109	37.960320
1994.920045	333963.246921	37.965338
1997.159236	334516.661181	37.970356
1998.889070	335074.332400	37.975373
2000.676346	335632.239906	37.980391
2002.876568	336183.276330	37.985408
2004.403232	336747.650613	37.990426
2006.250927	337312.904452	37.995444
2008.778198	337859.831367	38.000461
2010.714268	338401.592102	38.005479
2012.751744	338936.582023	38.010496
2014.532207	339468.611268	38.015514
2016.309828	340005.933908	38.020532
2017.671134	340551.683247	38.025549
2020.033248	341110.379892	38.030567
2021.719397	341662.021347	38.035584
2023.438658	342221.029122	38.040602
2025.368701	342785.574384	38.045620
2027.066509	343342.132796	38.050637
2028.824782	343919.290670	38.055655
2030.601761	344495.421511	38.060672
2032.755536	345061.390625	38.065690
2034.770001	345655.926327	38.070708
2037.335510	346234.541628	38.075725
2039.110168	346815.933305	38.080743
2041.324924	347407.718743	38.085760
2043.394698	347991.807757	38.090778
2045.154989	348585.621181	38.095796
2047.121027	349179.949565	38.100813
2049.078558	349790.039849	38.105831
2051.160750	350394.495701	38.110848
2053.096670	351007.659922	38.115866
2054.512266	351621.603850	38.120884
2057.081673	352240.629165	38.125901
2059.321805	352855.713544	38.130919
2061.311953	353471.408281	38.135936
2063.673735	354092.154115	38.140954
2065.530683	354709.924490	38.145972
2068.087437	355332.085786	38.150989
2069.921199	355959.975716	38.156007
2071.994953	356587.460521	38.161024
2074.357108	357201.705541	38.166042
2076.277200	357831.065014	38.171060
2078.524769	358454.301958	38.176077
2080.268542	359085.817860	38.181095
2082.130402	359708.430422	38.186112
2084.940873	360352.579034	38.191130
2086.856958	360997.563489	38.196148
2089.432025	361624.004266	38.201165
2090.995878	362251.578560	38.206183
2093.175101	362893.743482	38.211200
2095.701538	363527.172271	38.216218
2097.250924	364166.924208	38.221236
2099.456563	364806.635517	38.226253
2101.591542	365449.207575	38.231271
2104.249179	366088.870617	38.236288
2106.608773	366725.601112	38.241306
2108.410727	367358.248769	38.246324
2110.685920	367993.342457	38.251341
2112.799204	368645.830604	38.256359
2114.954762	369289.149550	38.261376
2116.632219	369922.494401	38.266394
2118.706865	370578.820731	38.271412
2121.114739	371217.241736	38.276429
2123.150926	371869.210955	38.281447
2125.403251	372504.560892	38.286464
2128.438324	373148.590660	38.291482
2130.532938	373786.925304	38.296500
2133.062656	374409.722733	38.301517
2134.732737	375048.676970	38.306535
2136.955735	375678.916209	38.311552
2139.183282	376310.508003	38.316570
2140.579811	376948.573406	38.321588
2142.798917	377580.693920	38.326605
2144.917291	378233.358828	38.331623
2146.768827	378875.081275	38.336640
2148.869892	379507.047711	38.341658
2151.044998	380143.394697	38.346676
2152.956563	380762.189284	38.351693
2154.772010	381388.810644	38.356711
2156.923205	382018.580973	38.361728
2159.186206	382643.025155	38.366746
2161.072516	383276.149420	38.371764
2163.707862	383908.583728	38.376781
2165.546714	384544.064704	38.381799
2167.171100	385185.894487	38.386816
2169.036387	385825.745736	38.391834
2170.742113	386501.564596	38.396852
2172.904251	387142.779395	38.401869
2175.090512	387818.082480	38.406887
2176.931138	388491.851448	38.411904
2179.094498	389168.893952	38.416922
2181.157723	389844.465048	38.421940
2183.211726	390533.336865	38.426957
2185.480090	391229.194290	38.431975
2187.564283	391927.086109	38.436992
2189.662813	392618.879621	38.442010
2191.558089	393331.798807	38.447028
2193.858619	394030.254402	38.452045
2195.970067	394750.945494	38.457063
2198.283014	395474.064101	38.462080
2200.314292	396188.902121	38.467098
2202.448628	396922.889192	38.472116
2204.882381	397641.923432	38.477133
2206.936464	398375.422188	38.482151
2209.410575	399129.080185	38.487168
2212.060530	399831.713732	38.492186
2214.449817	400577.593447	38.497204
2216.875841	401300.312257	38.502221
2219.230863	402035.166703	38.507239
2221.512351	402765.555241	38.512256
2223.922308	403495.495416	38.517274
2225.944372	404230.280635	38.522292
2228.267165	404966.614369	38.527309
2230.490439	405701.067212	38.532327
2232.769674	406445.810393	38.537344
2235.212601	407175.120160	38.542362
2237.372471	407929.143224	38.547380
2239.836669	408658.502139	38.552397
2242.664156	409386.515194	38.557415
2245.135681	410119.568739	38.562432
2247.420908	410844.076576	38.567450
2249.790076	411575.781836	38.572468
2252.237246	412299.709951	38.577485
2254.277768	413030.355121	38.582503
2256.504809	413754.521825	38.587520
2258.606120	414478.936686	38.592538
2261.446518	415201.693883	38.597556
2263.972662	415928.319899	38.602573
2265.972184	416645.949610	38.607591
2268.895727	417368.164746	38.612608
2271.739069	418089.710147	38.617626
2273.987471	418796.758280	38.622644
2276.239936	419514.806747	38.627661
2278.592258	420226.442847	38.632679
2280.548551	420937.307359	38.637696
2282.830429	421635.707385	38.642714
2285.120816	422353.550289	38.647732
2287.012520	423055.098183	38.652749
2289.703719	423766.103798	38.657767
2291.747757	424486.337295	38.662784
2294.550455	425185.950175	38.667802
2296.754623	425902.366879	38.672820
2299.320940	426600.855393	38.677837
2301.109562	427300.907293	38.682855
2302.424220	427994.740393	38.687872
2305.099243	428670.997841	38.692890
2306.991252	429374.145383	38.697908
2309.460798	430062.822363	38.702925
2311.134538	430754.531370	38.707943
2313.264517	431459.437475	38.712960
2315.731423	432161.384649	38.717978
2317.809574	432881.662621	38.722996
2319.936354	433589.676235	38.728013
2322.411951	434305.644574	38.733031
2324.651765	435014.801184	38.738048
2327.043010	435740.128694	38.743066
2329.523191	436467.941343	38.748084
2331.466554	437194.648088	38.753101
2333.921227	437926.804978	38.758119
2336.139336	438668.418613	38.763136
2338.238152	439418.105344	38.768154
2340.376599	440165.735232	38.773172
2342.565016	440914.034772	38.778189
2344.919193	441668.946552	38.783207
2346.911424	442439.594193	38.788224
2348.939023	443196.768168	38.793242
2350.826372	443985.703713	38.798260
2353.423198	444760.958490	38.803277
2356.248990	445552.558973	38.808295
2358.463640	446337.251354	38.813312
2360.853324	447133.447310	38.818330
2363.320035	447937.777112	38.823348
2365.467255	448737.020984	38.828365
2368.117427	449536.958659	38.833383
2370.329120	450347.835566	38.838400
2372.670799	451134.622281	38.843418
2375.664479	451950.908455	38.848436
2378.090034	452755.634392	38.853453
2380.669413	453563.177202	38.858471
2383.522179	454368.520084	38.863488
2386.025649	455165.046991	38.868506
2388.518205	455970.473609	38.873524
2390.690461	456770.613412	38.878541
2393.236341	457564.046204	38.883559
2395.642000	458370.939801	38.888576
2398.610975	459161.154511	38.893594
2401.358144	459959.795142	38.898612
2403.801436	460760.161792	38.903629
2406.404110	461554.007178	38.908647
2408.737393	462356.889515	38.913664
2411.059560	463136.980447	38.918682
2413.722808	463945.184980	38.923700
2416.176106	464746.724163	38.928717
2418.941738	465532.436542	38.933735
2420.742558	466329.613120	38.938752
2423.114456	467128.528650	38.943770
2425.561165	467930.521370	38.948788
2427.442402	468732.664571	38.953805
2429.838488	469536.302194	38.958823
2432.320444	470352.999706	38.963840
2434.587011	471166.916532	38.968858
2436.801459	471988.869430	38.973876
2439.005264	472805.286118	38.978893
2441.583306	473620.897260	38.983911
2443.604874	474455.865276	38.988928
2446.323160	475266.077202	38.993946
2449.113643	476099.377507	38.998964
2451.507017	476935.973336	39.003981
2454.054340	477743.162636	39.008999
2456.643308	478566.888441	39.014016
2458.969528	479390.562097	39.019034
2461.525361	480212.191181	39.024052
2463.423101	481016.895671	39.029069
2466.183419	481810.487825	39.034087
2468.300977	482613.715147	39.039104
2471.231573	483419.091915	39.044122
2473.323785	484223.701427	39.049140
2475.411563	485029.428705	39.054157
2477.781937	485833.003974	39.059175
2480.075664	486664.158141	39.064192
2482.262465	487476.744706	39.069210
2484.743721	488307.729910	39.074228
2487.266006	489140.879767	39.079245
2489.763450	489966.532991	39.084263
2492.047783	490811.616326	39.089280
2494.813716	491652.195263	39.094298
2497.607467	492497.960462	39.099316
2500.202620	493342.802512	39.104333
2502.783420	494168.715472	39.109351
2505.644271	495019.362971	39.114368
2508.187785	495859.286696	39.119386
2510.973188	496698.772448	39.124404
2513.238025	497553.948986	39.129421
2515.727962	498398.015714	39.134439
2518.075109	499258.768602	39.139456
2520.241459	500117.636589	39.144474
2522.926069	500989.056685	39.149492
2525.226463	501856.760105	39.154509
2527.701100	502716.180929	39.159527
2530.533513	503595.070452	39.164544
2532.887023	504472.169538	39.169562
2535.304629	505348.701678	39.174580
2537.958216	506232.338015	39.179597
2540.927370	507107.971208	39.184615
2543.360032	507991.079813	39.189632
2546.111049	508884.043807	39.194650
2548.603193	509763.762280	39.199668
2551.165059	510653.373838	39.204685
2554.090435	511539.803944	39.209703
2556.160471	512435.213190	39.214720
2559.249877	513328.745786	39.219738
2561.778304	514221.353045	39.224756
2564.526991	515119.600353	39.229773
2566.757465	516011.182951	39.234791
2569.395272	516905.710732	39.239808
2572.196083	517801.511861	39.244826
2575.393548	518682.613970	39.249844
2578.486801	519568.299708	39.254861
2581.670288	520435.064849	39.259879
2584.833531	521310.321636	39.264896
2587.636638	522183.818853	39.269914
2589.931064	523043.619673	39.274932
2592.777131	523913.831429	39.279949
2595.444644	524769.744299	39.284967
2597.471104	525629.269611	39.289984
2600.121587	526506.376345	39.295002
2602.623588	527373.250041	39.300020
2604.867617	528251.811431	39.305037
2607.089446	529118.413024	39.310055
2609.766333	530005.529277	39.315072
2611.643335	530890.902318	39.320090
2614.458919	531767.279888	39.325108
2617.245716	532666.601887	39.330125
2619.830532	533565.441041	39.335143
2622.153692	534458.986493	39.340160
2624.588708	535352.000510	39.345178
2627.239640	536262.087759	39.350196
2629.679280	537162.505079	39.355213
2632.194519	538053.309844	39.360231
2634.887786	538951.904399	39.365248
2637.160809	539832.433165	39.370266
2639.258972	540713.730834	39.375284
2641.527283	541607.284776	39.380301
2644.032129	542507.963687	39.385319
2646.550163	543407.522058	39.390336
2648.584966	544311.606474	39.395354
2650.769080	545215.802505	39.400372
2653.349655	546153.730586	39.405389
2656.131608	547085.787729	39.410407
2658.610005	548026.799649	39.415424
2661.449647	548965.225591	39.420442
2663.985435	549908.842502	39.425460
2666.320256	550859.387895	39.430477
2669.084382	551813.652693	39.435495
2671.527601	552775.062051	39.440512
2674.406898	553741.440249	39.445530
2677.147674	554708.815355	39.450548
2679.474696	555695.324544	39.455565
2682.541529	556676.825373	39.460583
2685.180229	557661.920818	39.465600
2687.321793	558653.977978	39.470618
2690.187562	559651.450967	39.475636
2693.205464	560659.137233	39.480653
2696.341467	561649.585291	39.485671
2699.141328	562654.129040	39.490688
2701.833830	563658.102589	39.495706
2704.547198	564652.570528	39.500724
2707.600895	565670.839175	39.505741
2710.584676	566677.061086	39.510759
2713.321000	567680.630445	39.515776
2715.607261	568688.939371	39.520794
2718.778680	569696.270532	39.525812
2721.223929	570717.693410	39.530829
2723.937455	571727.270236	39.535847
2727.028822	572754.316244	39.540864
2729.879749	573779.405236	39.545882
2732.580331	574794.316589	39.550900
2734.948277	575827.452121	39.555917
2737.865905	576846.247738	39.560935
2740.532903	577858.236275	39.565952
2743.756367	578895.357878	39.570970
2746.675687	579929.329398	39.575988
2749.242490	580961.309295	39.581005
2752.157363	581988.737825	39.586023
2755.401947	583016.219214	39.591040
2758.018944	584041.052851	39.596058
2760.541376	585070.055164	39.601076
2763.609656	586105.574052	39.606093
2766.272827	587132.160538	39.611111
2769.100626	588159.723946	39.616128
2771.792401	589204.003197	39.621146
2775.218435	590229.927148	39.626164
2777.828123	591256.130890	39.631181
2780.285313	592280.711634	39.636199
2783.525388	593313.115012	39.641216
2785.853485	594351.905085	39.646234
2788.869561	595369.408467	39.651252
2791.701667	596416.958358	39.656269
2794.614676	597447.912519	39.661287
2797.272237	598479.804522	39.666304
2800.038881	599520.415431	39.671322
2802.738323	600547.803899	39.676340
2805.823100	601581.470551	39.681357
2808.722320	602619.655691	39.686375
2812.252436	603632.734404	39.691392
2814.964141	604655.124003	39.696410
2817.985941	605674.419954	39.701428
2820.804404	606687.709554	39.706445
2823.839402	607657.362659	39.711463
2826.985219	608641.871758	39.716480
2829.430593	609612.529155	39.721498
2832.212111	610585.385593	39.726516
2834.758489	611558.434984	39.731533
2837.613542	612535.631009	39.736551
2840.428392	613515.979688	39.741568
2842.962846	614502.708102	39.746586
2845.470167	615497.718655	39.751604
2848.207841	616490.151983	39.756621
2851.091022	617481.965587	39.761639
2854.084972	618488.763157	39.766656
2856.373576	619498.259827	39.771674
2859.068816	620514.216781	39.776692
2861.519519	621541.267120	39.781709
2864.393108	622566.649855	39.786727
2867.798155	623589.700677	39.791744
2869.976822	624641.274488	39.796762
2872.584187	625673.495651	39.801780
2875.244863	626740.006246	39.806797
2877.905665	627808.092515	39.811815
2880.814338	628881.249375	39.816832
2883.387902	629964.045820	39.821850
2886.276656	631043.336573	39.826868
2888.733500	632135.462761	39.831885
2891.507375	633229.106621	39.836903
2894.609790	634334.315714	39.841920
2897.540192	635435.045510	39.846938
2901.190027	636548.915782	39.851956
2903.978720	637662.043488	39.856973
2907.043270	638773.902622	39.861991
2909.594682	639891.428861	39.867008
2912.312478	641018.839064	39.872026
2915.565998	642147.819187	39.877044
2918.253375	643273.669260	39.882061
2920.996430	644414.334085	39.887079
2924.070304	645549.936700	39.892096
2927.047956	646692.023278	39.897114
2930.322318	647828.605839	39.902132
2933.744688	648958.864733	39.907149
2936.761505	650105.587514	39.912167
2939.782573	651243.921415	39.917184
2942.749502	652382.816589	39.922202
2945.565806	653522.188173	39.927220
2948.982764	654656.953596	39.932237
2952.202543	655800.095266	39.937255
2955.309290	656932.885055	39.942272
2958.188379	658074.103001	39.947290
2961.485791	659198.884246	39.952308
2964.214482	660341.076407	39.957325
2966.777216	661481.312304	39.962343
2970.107055	662620.735972	39.967360
2972.827988	663772.655247	39.972378
2975.920035	664915.638490	39.977396
2978.871372	666074.013942	39.982413
2981.844990	667217.509083	39.987431
2985.065606	668362.897767	39.992448
2987.834529	669510.684522	39.997466
2990.857694	670649.359923	40.002484
2993.536520	671816.628009	40.007501
2996.439755	672966.611316	40.012519
2999.628462	674127.690395	40.017536
3002.308573	675296.170738	40.022554
3005.191310	676464.856074	40.027572
3007.866444	677626.085652	40.032589
3010.965953	678793.774021	40.037607
3014.130074	679957.628506	40.042624
3016.538120	681110.502837	40.047642
3020.152286	682253.133516	40.052660
3023.320987	683389.048173	40.057677
3026.053002	684519.781440	40.062695
3029.467398	685653.470600	40.067712
3032.158471	686785.387655	40.072730
3035.392029	687912.120478	40.077748
3038.173215	689039.759965	40.082765
3040.761876	690181.910352	40.087783
3044.049715	691327.451443	40.092800
3046.778518	692483.596669	40.097818
3049.670065	693642.370496	40.102836
3052.585872	694791.884454	40.107853
3055.179290	695972.857252	40.112871
3058.670608	697144.478314	40.117888
3061.749955	698330.960210	40.122906
3064.511059	699513.614052	40.127924
3067.294054	700703.053269	40.132941
3070.560001	701906.508932	40.137959
3073.670142	703106.698586	40.142976
3076.564430	704309.703188	40.147994
3079.874848	705515.964940	40.153012
3082.695357	706737.958366	40.158029
3085.522387	707955.717256	40.163047
3088.963481	709173.389906	40.168064
3092.182947	710410.635844	40.173082
3095.080878	711650.547945	40.178100
3098.344364	712903.567366	40.183117
3101.348646	714143.363739	40.188135
3105.075066	715379.399994	40.193152
3108.290402	716627.293945	40.198170
3111.280076	717856.644640	40.203188
3114.911670	719111.315432	40.208205
3117.789715	720353.537005	40.213223
3121.280332	721585.809754	40.218240
3123.836851	722855.057013	40.223258
3127.179625	724105.607835	40.228276
3130.340144	725364.792388	40.233293
3133.198204	726634.494652	40.238311
3136.209889	727897.366505	40.243328
3139.198292	729161.654212	40.248346
3142.421526	730443.007124	40.253364
3145.838440	731704.488184	40.258381
3148.494605	733000.738145	40.263399
3152.348876	734269.634285	40.268416
3155.125388	735549.149019	40.273434
3158.287936	736833.248170	40.278452
3162.164229	738109.052497	40.283469
3164.732090	739410.092954	40.288487
3168.118892	740683.120465	40.293504
3171.701733	741978.635040	40.298522
3174.558960	743249.776535	40.303540
3177.983187	744535.434292	40.308557
3181.267111	745828.445778	40.313575
3184.921618	747099.623808	40.318592
3188.262539	748378.183788	40.323610
3191.165081	749655.947676	40.328628
3194.856604	750929.289781	40.333645
3197.588157	752214.031552	40.338663
3201.120290	753485.129108	40.343680
3204.221118	754764.744679	40.348698
3207.793321	756050.036016	40.353716
3210.826440	757328.611505	40.358733
3213.620151	758608.903950	40.363751
3217.474764	759871.455695	40.368768
3220.796109	761141.749708	40.373786
3224.443924	762412.398957	40.378804
3227.552142	763672.913050	40.383821
3230.929451	764932.716416	40.388839
3234.115587	766155.220879	40.393856
3237.169542	767366.128086	40.398874
3240.376157	768577.533161	40.403892
3243.838809	769779.537343	40.408909
3247.041070	770995.556180	40.413927
3250.170087	772207.507515	40.418944
3253.485719	773426.108847	40.423962
3256.510721	774646.004404	40.428980
3259.608962	775871.094959	40.433997
3263.031934	777101.875290	40.439015
3266.599418	778309.445790	40.444032
3269.791482	779541.527827	40.449050
3272.899462	780767.683141	40.454068
3276.091992	781994.724398	40.459085
3279.145689	783239.089740	40.464103
3282.041787	784480.807174	40.469120
3285.217042	785727.081077	40.474138
3288.200988	786987.594352	40.479156
3291.751502	788251.974766	40.484173
3294.537182	789525.939211	40.489191
3297.543936	790816.983716	40.494208
3300.787507	792119.780509	40.499226
3303.855331	793411.767604	40.504244
3306.929566	794709.346780	40.509261
3309.579809	796032.559610	40.514279
3312.895512	797360.611822	40.519296
3316.054603	798695.332854	40.524314
3318.952042	800039.412551	40.529332
3322.244728	801392.108617	40.534349
3325.313963	802762.273284	40.539367
3328.459473	804136.853704	40.544384
3331.253265	805517.907915	40.549402
3334.705311	806912.277851	40.554420
3338.244275	808294.169472	40.559437
3341.055908	809707.867835	40.564455
3344.357361	811109.311661	40.569472
3347.521293	812534.960537	40.574490
3350.976934	813955.964113	40.579508
3354.315586	815379.286736	40.584525
3357.593775	816819.099039	40.589543
3361.008698	818257.488603	40.594560
3364.236561	819700.622769	40.599578
3367.440872	821154.392843	40.604596
3371.081131	822606.199395	40.609613
3374.968686	824075.185782	40.614631
3378.340606	825524.500751	40.619648
3381.931798	826977.316927	40.624666
3385.038928	828432.674135	40.629684
3388.210799	829890.289835	40.634701
3391.740645	831365.136060	40.639719
3394.896927	832831.542376	40.644736
3398.408104	834303.928955	40.649754
3401.674238	835785.385903	40.654772
3405.747347	837256.959353	40.659789
3408.851556	838735.677327	40.664807
3412.076227	840221.169612	40.669824
3415.741994	841697.224252	40.674842
3419.123581	843187.365628	40.679860
3422.419787	844669.698665	40.684877
3426.130537	846158.263251	40.689895
3429.880215	847647.603503	40.694912
3433.724232	849131.525420	40.699930
3436.621531	850612.802655	40.704948
3440.419329	852087.477768	40.709965
3443.855240	853580.756621	40.714983
3447.232097	855058.022684	40.720000
3451.184768	856534.723348	40.725018
3454.018875	858006.596238	40.730023
3457.714153	859422.730832	40.735028
3460.895260	860806.114033	40.740032
3464.263622	862122.833043	40.745037
3467.625709	863370.064768	40.750042
3470.818832	864566.331195	40.755047
3474.012987	865701.206253	40.760052
3476.969159	866769.259455	40.765056
3479.658569	867758.077949	40.770061
3482.668155	868695.895840	40.775066
3485.076510	869574.678323	40.780071
3487.983417	870368.321326	40.785076
3489.913127	871109.030478	40.790080
3492.188932	871795.848047	40.795085
3494.583188	872425.935311	40.800090
3496.316820	872994.127947	40.805095
3498.434933	873517.353223	40.810100
3500.053881	873996.726320	40.815104
3501.434051	874411.580892	40.820109
3503.130739	874786.240968	40.825114
3504.356388	875126.333848	40.830119
3505.760621	875410.938264	40.835124
3506.982986	875683.312079	40.840128
3507.714530	875899.446777	40.845133
3509.086129	876088.479512	40.850138
3510.240976	876241.485134	40.855143
3511.188273	876365.406050	40.860148
3511.874840	876465.168877	40.865152
3512.650734	876548.046414	40.870157
3513.539764	876590.032981	40.875162
3514.370687	876605.712156	40.880167
3514.759972	876602.277461	40.885172
3515.069800	876580.250625	40.890176
3515.706253	876546.797761	40.895181
3516.264944	876493.113233	40.900186
3516.547894	876418.167004	40.905191
3516.934745	876326.044118	40.910196
3516.922344	876246.321663	40.915200
3517.592037	876127.158441	40.920205
3517.714867	875991.206921	40.925210
3517.837319	875870.002749	40.930215
3518.314185	875723.769928	40.935220
3518.137510	875576.478434	40.940224
3518.587081	875406.137854	40.945229
3518.752078	875241.814574	40.950234
3519.178476	875057.485955	40.955239
3519.187221	874863.766680	40.960244
3518.826799	874686.105716	40.965248
3519.333070	874487.184724	40.970253
3519.174012	874278.427610	40.975258
3519.213828	874075.032219	40.980263
3519.151535	873860.747154	40.985268
3519.272278	873652.019182	40.990272
3519.003166	873435.145930	40.995277
3519.766008	873218.006443	41.000282
3519.121020	873001.753766	41.005287
3519.313584	872765.683294	41.010292
3519.267480	872533.884674	41.015296
3519.205236	872297.641246	41.020301
3519.523081	872067.213377	41.025306
3518.921622	871843.480272	41.030311
3519.212898	871597.986387	41.035316
3518.951445	871364.050120	41.040320
3518.884278	871129.784196	41.045325
3519.153028	870884.744912	41.050330
3518.892799	870649.234557	41.055335
3519.340359	870408.585429	41.060340
3518.657093	870161.347142	41.065344
3518.486759	869911.315384	41.070349
3518.593677	869671.652922	41.075354
3518.398241	869437.722189	41.080359
3518.027870	869189.909447	41.085364
3517.869367	868955.566700	41.090368
3517.684766	868716.584646	41.095373
3517.685133	868481.038832	41.100378
3517.622860	868253.602379	41.105383
3517.576648	868002.790260	41.110388
3517.201870	867779.534902	41.115392
3517.131560	867555.933417	41.120397
3517.098100	867323.337474	41.125402
3516.891247	867087.765620	41.130407
3516.740554	866850.050688	41.135412
3516.703712	866634.711948	41.140416
3516.534270	866410.887306	41.145421
3516.260679	866189.001581	41.150426
3516.002335	865962.855198	41.155431
3515.935311	865720.443651	41.160436
3515.838064	865507.872246	41.165440
3515.605349	865302.172027	41.170445
3515.635439	865088.502414	41.175450
3515.302543	864877.682832	41.180455
3515.312232	864661.971697	41.185460
3515.172020	864452.265355	41.190464
3515.084382	864244.088774	41.195469
3515.031272	864029.812491	41.200474
3514.702255	863826.102481	41.205479
3514.807466	863624.829392	41.210484
3514.591178	863408.139579	41.215488
3514.273553	863208.753663	41.220493
3514.186724	863003.333536	41.225498
3513.863042	862806.446821	41.230503
3513.963199	862616.155013	41.235508
3513.734368	862424.555282	41.240512
3513.749607	862231.847846	41.245517
3514.007900	862040.062353	41.250522
3513.652679	861851.169161	41.255527
3513.438022	861649.586055	41.260532
3513.292057	861465.383376	41.265536
3513.428006	861280.454041	41.270541
3512.931170	861084.501309	41.275546
3512.730758	860920.008827	41.280551
3512.612448	860716.347599	41.285556
3512.640547	860545.138345	41.290560
3512.843814	860368.096024	41.295565
3512.459545	860187.466255	41.300570
3512.358613	860012.007291	41.305575
3512.277059	859833.639357	41.310580
3511.956574	859667.969292	41.315584
3511.634696	859507.709296	41.320589
3511.896719	859333.816481	41.325594
3511.627848	859174.215693	41.330599
3511.495815	859008.497035	41.335604
3511.465316	858842.564297	41.340608
3511.294977	858684.384951	41.345613
3511.569761	858519.942401	41.350618
3511.410107	858358.754462	41.355623
3511.221446	858194.375004	41.360628
3510.846359	858039.111201	41.365632
3510.644753	857884.009503	41.370637
3510.939540	857731.147300	41.375642
3510.595925	857590.761341	41.380647
3510.378044	857432.361387	41.385652
3510.282859	857287.383066	41.390656
3510.170815	857141.146221	41.395661
3510.231367	856990.719157	41.400666
3509.893798	856855.731293	41.405671
3509.878588	856713.434551	41.410676
3509.665833	856583.257642	41.415680
3509.765043	856447.321239	41.420685
3509.878821	856307.606315	41.425690
3509.756497	856163.571299	41.430695
3509.821685	856016.987882	41.435700
3509.463829	855884.979599	41.440704
3509.230301	855758.754069	41.445709
3509.436741	855626.071112	41.450714
3508.807385	855494.967118	41.455719
3508.948937	855367.029475	41.460724
3508.486751	855239.086603	41.465728
3508.532780	855125.576098	41.470733
3508.764895	855001.873813	41.475738
3508.608316	854894.873775	41.480743
3508.420474	854773.457901	41.485748
3508.441227	854650.168190	41.490752
3508.308958	854526.899763	41.495757
3508.349362	854415.021309	41.500762
3508.058109	854297.579400	41.505767
3508.361569	854185.945718	41.510772
3508.206792	854077.091402	41.515776
3507.814773	853949.592841	41.520781
3507.853312	853851.059919	41.525786
3507.608674	853744.439446	41.530791
3507.774758	853633.010127	41.535796
3507.610711	853525.211537	41.540800
3506.933780	853420.201309	41.545805
3507.512421	853323.026848	41.550810
3507.492129	853219.749427	41.555815
3507.480627	853114.629627	41.560820
3507.490114	853010.375832	41.565824
3507.150768	852910.433951	41.570829
3507.017783	852809.586856	41.575834
3507.158254	852713.535493	41.580839
3507.194067	852605.591712	41.585844
3507.225879	852514.394353	41.590848
3507.212737	852411.682241	41.595853
3506.822685	852313.480549	41.600858
3506.637844	852224.539153	41.605863
3506.859826	852123.721437	41.610868
3507.107090	852035.290477	41.615872
3506.501605	851941.279237	41.620877
3506.556600	851853.553284	41.625882
3506.213249	851761.628169	41.630887
3506.441561	851668.256724	41.635892
3506.289429	851584.722433	41.640896
3506.242611	851499.524452	41.645901
3506.349535	851409.363040	41.650906
3505.902098	851325.387044	41.655911
3506.012428	851238.030445	41.660916
3506.259283	851162.658194	41.665920
3505.918820	851080.695375	41.670925
3506.282633	850994.360639	41.675930
3505.703814	850920.469982	41.680935
3505.985279	850828.335572	41.685940
3505.877179	850753.788194	41.690944
3505.682128	850680.899707	41.695949
3505.634157	850599.755923	41.700954
3505.544676	850532.562627	41.705959
3505.361659	850450.469459	41.710964
3505.447336	850373.950068	41.715968
3505.343183	850305.497472	41.720973
3505.431541	850234.980211	41.725978
3505.056320	850162.210229	41.730983
3505.102070	850087.727105	41.735988
3505.205643	850022.628405	41.740992
3504.877220	849960.308323	41.745997
3504.956199	849886.689088	41.751002
3505.115901	849835.235609	41.756007
3505.334111	849765.564038	41.761012
3505.401107	849701.048583	41.766016
3504.941474	849636.227313	41.771021
3505.260708	849554.236698	41.776026
3504.991213	849492.967830	41.781031
3505.335032	849413.392851	41.786036
3504.849803	849349.928428	41.791040
3504.791582	849294.532949	41.796045
3504.804512	849228.858377	41.801050
3504.553727	849170.392210	41.806055
3504.690007	849112.446138	41.811060
3504.416677	849050.107699	41.816064
3504.638612	849000.961905	41.821069
3504.755486	848925.871609	41.826074
3504.509065	848860.427165	41.831079
3504.532302	848798.620890	41.836084
3504.488029	848745.930375	41.841088
3504.305991	848692.485945	41.846093
3504.635655	848631.598718	41.851098
3504.142377	848573.745708	41.856103
3504.444124	848523.227186	41.861108
3503.962455	848464.015029	41.866112
3503.714064	848412.128410	41.871117
3504.081587	848362.954488	41.876122
3503.799056	848317.272496	41.881127
3504.146327	848271.007302	41.886132
3503.750111	848214.879374	41.891136
3503.674917	848175.945433	41.896141
3503.577016	848121.223175	41.901146
3503.333799	848086.093263	41.906151
3503.791824	848038.646337	41.911156
3503.650515	847998.171425	41.916160
3503.337337	847954.332163	41.921165
3504.081004	847913.524558	41.926170
3503.876731	847866.954847	41.931175
3503.840480	847814.835987	41.936180
3504.113376	847765.187400	41.941184
3503.433195	847719.175339	41.946189
3503.817780	847676.968902	41.951194
3503.456036	847641.079732	41.956199
3503.845557	847584.629141	41.961204
3503.781190	847539.778973	41.966208
3503.585857	847492.817319	41.971213
3503.642976	847443.684193	41.976218
3503.618169	847412.391781	41.981223
3503.592505	847357.457294	41.986228
3503.668483	847316.071648	41.991232
3503.601891	847278.293115	41.996237
3503.923214	847223.593817	42.001242
3503.171401	847188.828700	42.006247
3503.443047	847147.798864	42.011252
3503.168883	847106.369571	42.016256
3503.274543	847066.818583	42.021261
3503.571987	847027.528047	42.026266
3503.343396	846992.873771	42.031271
3502.992718	846946.222711	42.036276
3503.070693	846908.709896	42.041280
3503.067538	846865.589213	42.046285
3503.028596	846833.714504	42.051290
3503.056309	846807.546477	42.056295
3502.915404	846775.881198	42.061300
3503.245589	846736.680498	42.066304
3503.268540	846709.543737	42.071309
3503.459007	846661.255341	42.076314
3502.761750	846627.544310	42.081319
3502.755887	846593.337381	42.086324
3503.031580	846563.447053	42.091328
3503.105242	846533.685062	42.096333
3502.981478	846494.844429	42.101338
3502.940550	846466.941265	42.106343
3503.255194	846429.969842	42.111348
3503.334491	846399.431016	42.116352
3502.859655	846354.539020	42.121357
3503.152876	846317.570238	42.126362
3502.633650	846279.274549	42.131367
3502.975401	846244.042126	42.136372
3502.984699	846212.737972	42.141376
3502.651877	846187.205010	42.146381
3502.690211	846145.041671	42.151386
3502.463290	846121.914716	42.156391
3502.228049	846087.449948	42.161396
3502.486416	846070.352560	42.166400
3502.336773	846040.429143	42.171405
3502.327715	846014.360238	42.176410
3502.575188	845986.700454	42.181415
3502.371293	845963.860025	42.186420
3502.615711	845940.561758	42.191424
3502.523203	845917.897573	42.196429
3502.719974	845899.840141	42.201434
3502.581354	845866.231230	42.206439
3502.590995	845837.735656	42.211444
3502.569700	845814.284587	42.216448
3502.300669	845795.815053	42.221453
3502.787280	845763.755452	42.226458
3502.550736	845735.394785	42.231463
3502.735983	845707.161889	42.236468
3502.534657	845679.183129	42.241472
3502.475283	845660.195786	42.246477
3502.437850	845627.926598	42.251482
3502.305902	845608.078130	42.256487
3502.237860	845570.579581	42.261492
3502.364437	845552.144361	42.266496
3502.132904	845529.500407	42.271501
3502.233774	845502.152032	42.276506
3502.173431	845485.102763	42.281511
3502.344887	845460.844753	42.286516
3502.089852	845445.861233	42.291520
3502.272387	845425.672211	42.296525
3502.481386	845395.398663	42.301530
3502.409003	845384.941967	42.306535
3502.189456	845350.567341	42.311540
3502.164186	845334.190640	42.316544
3502.102331	845312.294742	42.321549
3502.425833	845289.078459	42.326554
3502.271549	845277.180453	42.331559
3502.002710	845254.832055	42.336564
3502.088579	845234.754417	42.341568
3502.247976	845199.641169	42.346573
3502.261030	845180.059375	42.351578
3502.094836	845160.505535	42.356583
3502.170222	845149.152948	42.361588
3502.265941	845118.992615	42.366592
3502.047866	845097.411129	42.371597
3502.187981	845064.141777	42.376602
3502.063185	845054.468138	42.381607
3502.408543	845027.757861	42.386612
3502.136597	845006.378325	42.391616
3502.032829	844991.369997	42.396621
3502.171634	844959.845052	42.401626
3501.976594	844947.274214	42.406631
3502.102833	844929.515630	42.411636
3502.283872	844916.692070	42.416640
3501.918429	844906.571135	42.421645
3502.035476	844878.344920	42.426650
3502.113819	844861.078291	42.431655
3501.898515	844840.949454	42.436660
3501.878099	844820.983954	42.441664
3501.924090	844802.849790	42.446669
3501.889151	844783.952731	42.451674
3502.265083	844775.654403	42.456679
3502.192008	844752.594936	42.461684
3501.854191	844729.189013	42.466688
3502.003854	844721.410666	42.471693
3501.913292	844698.353719	42.476698
3501.774268	844692.656153	42.481703
3501.812861	844661.339150	42.486708
3502.094705	844657.611466	42.491712
3501.835444	844640.590841	42.496717
3501.856317	844619.357999	42.501722
3501.755421	844609.098256	42.506727
3501.885492	844585.424742	42.511732
3501.662387	844583.520857	42.516736
3502.023827	844560.489652	42.521741
3501.602382	844554.836101	42.526746
3501.766562	844539.881673	42.531751
3501.766106	844514.095588	42.536756
3502.079031	844503.286268	42.541760
3501.995720	844492.829691	42.546765
3501.868485	844472.298059	42.551770
3501.511589	844458.200410	42.556775
3502.267126	844432.101906	42.561780
3501.848445	844422.667050	42.566784
3501.833908	844403.183925	42.571789
3501.933977	844396.673156	42.576794
3501.516977	844368.140206	42.581799
3502.027165	844351.870953	42.586804
3501.999362	844327.445533	42.591808
3501.695902	844315.762784	42.596813
3501.864854	844311.373922	42.601818
3501.750538	844287.737414	42.606823
3501.920547	844272.490564	42.611828
3501.755133	844253.127471	42.616832
3501.883814	844247.969296	42.621837
3501.690814	844233.069925	42.626842
3501.628147	844221.543239	42.631847
3501.776679	844199.416417	42.636852
3501.655144	844194.588147	42.641856
3501.730186	844178.677278	42.646861
3501.455080	844152.253916	42.651866
3501.429345	844154.293852	42.656871
3501.484129	844136.059312	42.661876
3501.518129	844125.292903	42.666880
3501.686943	844128.174960	42.671885
3501.933261	844108.068398	42.676890
3501.482757	844092.336396	42.681895
3501.647525	844081.452517	42.686900
3501.793097	844062.621871	42.691904
3501.377138	844053.864632	42.696909
3501.810877	844047.979958	42.701914
3501.693072	844032.195787	42.706919
3501.694423	844015.035662	42.711924
3501.915701	844019.654653	42.716928
3501.940027	844001.133611	42.721933
3501.573364	843982.964479	42.726938
3501.515593	843960.772060	42.731943
3501.762503	843949.972048	42.736948
3501.651509	843945.044975	42.741952
3501.489700	843934.211876	42.746957
3501.901961	843921.446957	42.751962
3501.878296	843904.484322	42.756967
3501.725027	843885.312021	42.761972
3501.668828	843880.958036	42.766976
3501.529357	843863.916435	42.771981
3501.615804	843836.562574	42.776986
3501.631603	843840.341260	42.781991
3501.774075	843830.332970	42.786996
3501.674710	843795.154843	42.792001
3501.592872	843799.239676	42.797005
3501.689678	843785.263393	42.802010
3501.544086	843767.349894	42.807015
3501.633803	843755.313709	42.812020
3501.445086	843748.459555	42.817025
3501.489573	843731.582722	42.822029
3501.652588	843716.335528	42.827034
3501.665765	843720.987285	42.832039
3501.592256	843699.668927	42.837044
3501.486217	843693.577419	42.842049
3501.577349	843688.327672	42.847053
3501.603662	843664.084949	42.852058
3501.444284	843656.256554	42.857063
3501.233473	843657.743863	42.862068
3501.516325	843642.380790	42.867073
3501.512338	843629.777266	42.872077
3501.642568	843618.897934	42.877082
3501.336311	843625.926632	42.882087
3501.788349	843606.174024	42.887092
3501.714314	843592.902681	42.892097
3501.478922	843591.969950	42.897101
3501.854695	843570.871762	42.902106
3501.312044	843555.831420	42.907111
3501.611040	843557.142104	42.912116
3501.944271	843546.812645	42.917121
3501.350907	843532.652781	42.922125
3501.181089	843528.219338	42.927130
3500.863453	843522.160728	42.932135
3501.158945	843518.236284	42.937140
3501.367902	843491.540372	42.942145
3501.043807	843487.906676	42.947149
3501.316472	843486.797550	42.952154
3501.353447	843487.567463	42.957159
3501.454686	843485.709473	42.962164
3501.477024	843469.417098	42.967169
3501.376517	843457.506999	42.972173
3501.459637	843456.039665	42.977178
3501.724080	843441.648531	42.982183
3501.166808	843426.125349	42.987188
3501.480220	843416.089636	42.992193
3501.507964	843415.212701	42.997197
3501.650867	843398.222570	43.002202
3501.557748	843390.771300	43.007207
3501.387007	843386.434854	43.012212
3501.314925	843383.246495	43.017217
3501.144707	843366.499138	43.022221
3501.548029	843352.376956	43.027226
3501.427373	843351.038410	43.032231
3501.796790	843338.278933	43.037236
3501.903649	843319.936769	43.042241
3501.658143	843309.503444	43.047245
3501.664894	843299.903314	43.052250
3501.407668	843274.442823	43.057255
3501.513373	843268.899542	43.062260
3501.686894	843268.484603	43.067265
3501.455764	843253.782635	43.072269
3501.340877	843240.904731	43.077274
3501.272542	843244.212142	43.082279
3500.994780	843230.971830	43.087284
3501.178821	843207.769157	43.092289
3501.162503	843203.214511	43.097293
3501.251934	843196.994970	43.102298
3501.041080	843202.942668	43.107303
3501.248841	843196.122855	43.112308
3501.430428	843197.936787	43.117313
3500.974501	843197.426315	43.122317
3501.261086	843173.722666	43.127322
3500.945009	843172.414627	43.132327
3501.198776	843169.756993	43.137332
3501.079628	843170.648315	43.142337
3501.082350	843163.860516	43.147341
3501.318440	843166.829494	43.152346
3501.261458	843155.299832	43.157351
3501.246296	843139.691150	43.162356
3500.935521	843146.139342	43.167361
3501.062071	843146.992261	43.172365
3501.345470	843145.396579	43.177370
3501.480714	843145.472433	43.182375
3501.199840	843128.838662	43.187380
3501.164416	843107.415245	43.192385
3501.277710	843113.797181	43.197389
3501.161713	843108.385370	43.202394
3501.328678	843108.844121	43.207399
3501.380260	843093.515775	43.212404
3501.523998	843087.093701	43.217409
3501.271117	843084.418263	43.222413
3501.362691	843084.403980	43.227418
3501.188844	843082.782794	43.232423
3500.785256	843053.659583	43.237428
3501.218561	843052.137408	43.242433
3500.822333	843050.260081	43.247437
3501.424584	843047.450953	43.252442
3500.872580	843053.743024	43.257447
3500.789379	843054.434815	43.262452
3501.147254	843063.008763	43.267457
3500.635473	843070.167211	43.272461
3500.758235	843073.347881	43.277466
3501.181830	843078.129918	43.282471
3501.139130	843066.888744	43.287476
3501.221156	843037.883473	43.292481
3501.098072	843037.030060	43.297485
3501.075883	843038.972861	43.302490
3501.002876	843033.263365	43.307495
3501.133266	843036.927688	43.312500
3501.119322	843025.875871	43.317505
3500.799516	843036.398133	43.322509
3501.413800	843019.139295	43.327514
3500.755406	843015.266666	43.332519
3501.112825	843002.896203	43.337524
3501.047548	843004.457889	43.342529
3500.868603	843004.291962	43.347533
3501.162201	843001.531061	43.352538
3501.101932	843007.067553	43.357543
3501.328747	843012.850060	43.362548
3501.439684	842992.469967	43.367553
3501.289589	842988.808760	43.372557
3501.410880	842975.699426	43.377562
3501.156595	842978.454257	43.382567
3501.133671	842973.997433	43.387572
3501.459469	842963.668119	43.392577
3501.281390	842955.647782	43.397581
3501.088984	842950.053836	43.402586
3501.186002	842954.014327	43.407591
3501.605068	842945.997598	43.412596
3501.456706	842924.882073	43.417601
3501.176188	842925.022922	43.422605
3501.072624	842916.603015	43.427610
3500.969559	842922.049310	43.432615
3500.865467	842919.932340	43.437620
3501.001483	842914.093087	43.442625
3500.786776	842903.266358	43.447629
3500.886109	842889.481494	43.452634
3501.216092	842887.393625	43.457639
3500.900501	842885.988476	43.462644
3501.230098	842887.294531	43.467649
3500.968477	842888.111199	43.472653
3500.998562	842897.415402	43.477658
3501.103838	842901.471605	43.482663
3500.876949	842902.767679	43.487668
3500.903483	842906.060449	43.492673
3500.992822	842905.270778	43.497677
3501.152441	842895.064289	43.502682
3501.335907	842879.132966	43.507687
3500.993790	842873.950222	43.512692
3501.192861	842872.270682	43.517697
3501.294541	842874.775981	43.522701
3500.891560	842871.542103	43.527706
3501.092084	842866.080590	43.532711
3501.011209	842861.244868	43.537716
3501.153541	842856.762123	43.542721
3500.950051	842841.860868	43.547725
3501.033125	842842.235787	43.552730
3501.124217	842846.682118	43.557735
3501.239738	842845.985314	43.562740
3501.251452	842844.819896	43.567745
3500.853874	842853.512243	43.572749
3500.828129	842845.080069	43.577754
3501.025823	842824.297961	43.582759
3501.160722	842819.816350	43.587764
3501.113948	842815.847978	43.592769
3501.026180	842816.055667	43.597773
3501.352711	842810.380468	43.602778
3501.117382	842825.059555	43.607783
3500.703906	842818.336419	43.612788
3501.349348	842824.441547	43.617793
3500.968846	842808.598193	43.622797
3500.959949	842790.951263	43.627802
3500.830842	842790.777538	43.632807
3500.933831	842789.791780	43.637812
3501.405853	842791.269531	43.642817
3500.891146	842786.792472	43.647821
3500.762528	842789.139869	43.652826
3500.908174	842797.262536	43.657831
3501.185551	842798.091929	43.662836
3501.087284	842791.319488	43.667841
3500.887971	842775.059844	43.672845
3501.375176	842753.165566	43.677850
3501.431155	842765.762899	43.682855
3501.064019	842758.159724	43.687860
3501.348053	842759.666870	43.692865
3500.982144	842766.221062	43.697869
3501.118150	842749.908931	43.702874
3501.339018	842732.613790	43.707879
3501.081284	842734.399571	43.712884
3501.125245	842725.568451	43.717889
3500.828374	842744.427075	43.722893
3501.185165	842735.934948	43.727898
3501.187078	842747.377131	43.732903
3500.887882	842719.302617	43.737908
3501.032108	842714.528557	43.742913
3501.082679	842709.090340	43.747917
3500.827666	842711.554496	43.752922
3500.782642	842709.331246	43.757927
3501.075321	842710.158260	43.762932
3501.217903	842713.917849	43.767937
3501.088264	842715.683613	43.772941
3501.019878	842716.470097	43.777946
3501.050344	842718.016892	43.782951
3501.189509	842703.255664	43.787956
3501.073595	842680.194779	43.792961
3500.635504	842688.602787	43.797965
3501.124132	842682.223331	43.802970
3500.973075	842688.356139	43.807975
3500.992080	842692.716884	43.812980
3501.132761	842689.785802	43.817985
3500.927501	842704.654430	43.822989
3501.418069	842694.395862	43.827994
3501.323624	842670.361875	43.832999
3501.341697	842664.346871	43.838004
3501.058945	842664.585045	43.843009
3501.125016	842663.992921	43.848013
3501.272208	842662.903261	43.853018
3501.293297	842661.348456	43.858023
3500.954721	842649.958797	43.863028
3501.054746	842649.652278	43.868033
3501.150115	842656.037513	43.873037
3501.324555	842651.161708	43.878042
3501.228383	842650.691916	43.883047
3500.981085	842643.845631	43.888052
3500.910059	842626.304892	43.893057
3501.210449	842612.584926	43.898061
3501.449496	842608.765679	43.903066
3501.268754	842609.569741	43.908071
3501.072324	842612.897528	43.913076
3501.424701	842611.484868	43.918081
3501.042452	842597.386715	43.923085
3501.116524	842580.792883	43.928090
3501.361458	842587.057840	43.933095
3501.060394	842588.947410	43.938100
3501.516376	842578.791022	43.943105
3501.139634	842584.280408	43.948109
3501.304002	842560.205516	43.953114
3501.151524	842553.441276	43.958119
3501.031111	842551.617643	43.963124
3501.203755	842548.584522	43.968129
3501.080865	842547.343114	43.973133
3500.916638	842546.593032	43.978138
3501.050765	842547.153936	43.983143
3500.976932	842541.347119	43.988148
3501.353287	842519.081413	43.993153
3500.577345	842520.366422	43.998157
3501.015845	842517.194753	44.003162
3500.976167	842517.394934	44.008167
3500.785371	842519.946104	44.013172
3501.203666	842518.717065	44.018177
3501.018122	842528.249505	44.023181
3500.727931	842519.761231	44.028186
3500.835243	842519.744488	44.033191
3500.719454	842527.908394	44.038196
3500.841532	842527.210528	44.043201
3501.032016	842538.332718	44.048205
3501.240647	842525.402679	44.053210
3500.865435	842503.351371	44.058215
3500.864905	842498.696740	44.063220
3501.148647	842500.785843	44.068225
3501.014393	842502.164495	44.073229
3500.921668	842500.918361	44.078234
3500.996105	842512.446637	44.083239
3500.997033	842508.373627	44.088244
3501.615364	842508.373975	44.093249
3500.997422	842490.045563	44.098253
3501.143346	842482.749725	44.103258
3501.301319	842478.458197	44.108263
3500.960667	842481.711629	44.113268
3501.013090	842483.061104	44.118273
3500.695505	842478.649967	44.123277
3500.692594	842473.510817	44.128282
3501.113379	842487.409358	44.133287
3500.669933	842481.175389	44.138292
3500.996127	842480.542585	44.143297
3501.035141	842479.857699	44.148301
3501.088229	842464.139587	44.153306
3500.881977	842455.638100	44.158311
3500.552057	842454.913908	44.163316
3501.194484	842457.431830	44.168321
3500.815115	842458.557885	44.173325
3500.885752	842457.577129	44.178330
3500.929435	842463.291830	44.183335
3500.692737	842467.595738	44.188340
3500.991050	842468.518881	44.193345
3500.764457	842474.469770	44.198349
3501.016760	842465.120821	44.203354
3501.227256	842473.815643	44.208359
3500.877574	842482.888941	44.213364
3501.154600	842470.432961	44.218369
3501.189725	842467.033398	44.223373
3501.061184	842446.494909	44.228378
3501.183356	842441.239203	44.233383
3500.610851	842443.947049	44.238388
3501.389386	842445.280002	44.243393
3500.827192	842462.338479	44.248397
3500.919044	842447.777958	44.253402
3500.939651	842450.684010	44.258407
3501.105690	842448.621618	44.263412
3501.177537	842442.597982	44.268417
3501.184671	842426.111154	44.273421
3500.882379	842412.097034	44.278426
3500.903618	842415.487881	44.283431
3500.582545	842420.677790	44.288436
3500.795559	842421.711251	44.293441
3501.090671	842428.162483	44.298445
3501.128572	842431.453742	44.303450
3501.225290	842426.395952	44.308455
3501.078075	842437.959021	44.313460
3501.183431	842422.620528	44.318465
3501.249101	842407.967028	44.323469
3501.253904	842391.771395	44.328474
3501.435254	842400.179955	44.333479
3501.218900	842395.268053	44.338484
3501.302245	842372.368769	44.343489
3500.877153	842357.403954	44.348493
3501.005786	842353.213899	44.353498
3500.872656	842362.835387	44.358503
3500.753170	842365.278500	44.363508
3501.125225	842369.972199	44.368513
3501.092689	842372.498692	44.373517
3501.203303	842370.250985	44.378522
3501.441234	842367.789422	44.383527
3500.857636	842349.843108	44.388532
3501.486056	842332.289136	44.393537
3501.240267	842329.418289	44.398541
3501.118206	842331.764841	44.403546
3501.052598	842343.606268	44.408551
3500.783828	842334.241590	44.413556
3500.884929	842341.402083	44.418561
3500.976365	842350.406628	44.423565
3500.944399	842337.804718	44.428570
3501.226527	842327.384148	44.433575
3501.109745	842311.304277	44.438580
3501.126355	842297.724919	44.443585
3501.225411	842299.358079	44.448589
3501.049920	842306.270919	44.453594
3501.180695	842306.541439	44.458599
3500.994853	842307.928200	44.463604
3501.204266	842301.301054	44.468609
3501.099055	842296.177741	44.473613
3501.044745	842284.548983	44.478618
3501.310065	842272.773260	44.483623
3500.942356	842275.934055	44.488628
3501.433133	842282.742772	44.493633
3501.364546	842276.062077	44.498637
3501.288901	842252.896251	44.503642
3500.943437	842251.786550	44.508647
3501.212602	842248.932144	44.513652
3501.379467	842247.839333	44.518657
3501.322115	842257.158213	44.523661
3501.020691	842235.288324	44.528666
3501.220535	842228.565614	44.533671
3500.889686	842220.083264	44.538676
3501.094199	842220.633197	44.543681
3500.645807	842224.291523	44.548685
3501.027185	842225.201722	44.553690
3501.149663	842237.692808	44.558695
3500.684257	842226.419133	44.563700
3501.146850	842223.146564	44.568705
3501.010075	842231.314159	44.573709
3500.998793	842207.071331	44.578714
3500.901697	842205.825817	44.583719
3500.770935	842200.221521	44.588724
3501.011053	842199.505166	44.593729
3501.057505	842205.801556	44.598733
3501.157628	842205.301043	44.603738
3501.080839	842207.155674	44.608743
3500.919039	842205.047466	44.613748
3501.293173	842198.588414	44.618753
3501.093928	842204.050404	44.623757
3501.296281	842178.319381	44.628762
3501.390722	842179.565378	44.633767
3501.032677	842179.136484	44.638772
3501.572997	842181.282573	44.643777
3501.307670	842165.031567	44.648781
3500.743703	842154.161077	44.653786
3501.158585	842139.646282	44.658791
3501.168119	842145.463608	44.663796
3501.438159	842143.481833	44.668801
3501.135156	842149.251032	44.673805
3501.197823	842144.974161	44.678810
3501.137189	842121.514534	44.683815
3500.955525	842123.288605	44.688820
3501.116794	842109.783182	44.693825
3500.978263	842109.222987	44.698829
3501.243539	842102.780848	44.703834
3501.087378	842106.005643	44.708839
3500.754070	842119.053130	44.713844
3501.385027	842114.784384	44.718849
3500.966202	842101.272641	44.723853
3501.072335	842085.254290	44.728858
3501.177986	842073.697092	44.733863
3501.109268	842083.018023	44.738868
3501.310669	842080.174130	44.743873
3501.088597	842090.197888	44.748877
3500.902266	842088.190453	44.753882
3501.231075	842076.210454	44.758887
3500.967939	842066.941451	44.763892
3501.177256	842060.508014	44.768897
3500.435420	842067.897587	44.773901
3500.648773	842067.379362	44.778906
3500.995075	842063.252057	44.783911
3500.669335	842065.533572	44.788916
3500.975316	842057.242381	44.793921
3500.841109	842057.651316	44.798925
3501.128403	842067.498507	44.803930
3501.142254	842065.556753	44.808935
3501.032722	842063.828248	44.813940
3501.276439	842067.281499	44.818945
3501.259484	842055.258526	44.823949
3501.154263	842039.661015	44.828954
3500.852318	842032.822560	44.833959
3500.921796	842039.406473	44.838964
3501.450597	842034.862695	44.843969
3500.901168	842040.379575	44.848973
3501.029215	842032.116164	44.853978
3501.238003	842031.986576	44.858983
3501.180632	842018.612105	44.863988
3501.276757	842001.625273	44.868993
3500.849592	842004.795505	44.873997
3500.981438	842008.169296	44.879002
3501.105749	842004.755526	44.884007
3501.396924	842007.716483	44.889012
3501.649956	841997.784792	44.894017
3501.199413	841986.508333	44.899021
3501.414949	841982.498396	44.904026
3501.239546	841978.743532	44.909031
3500.960577	841971.416503	44.914036
3501.051990	841952.490615	44.919041
3501.496893	841939.134432	44.924045
3501.181212	841944.905810	44.929050
3501.280752	841944.696316	44.934055
3501.396368	841942.059733	44.939060
3501.362652	841926.838678	44.944065
3501.259771	841920.550875	44.949069
3501.011256	841909.145703	44.954074
3501.366206	841906.956610	44.959079
3501.419558	841915.191903	44.964084
3501.348766	841884.944078	44.969089
3500.880108	841877.549599	44.974093
3501.076216	841876.549134	44.979098
3501.103181	841872.859553	44.984103
3501.222158	841880.114795	44.989108
3501.768638	841871.688767	44.994113
3501.058265	841863.362213	44.999117
3501.396639	841846.240083	45.004122
3501.419187	841847.012467	45.009127
3501.279347	841849.071035	45.014132
3501.534419	841838.556851	45.019137
3501.399757	841817.144268	45.024141
3501.200070	841817.369485	45.029146
3501.402977	841814.137289	45.034151
3501.387635	841813.751779	45.039156
3501.420120	841788.530542	45.044161
3501.216250	841782.258378	45.049165
3501.252788	841783.028583	45.054170
3501.286069	841780.695756	45.059175
3500.864436	841777.173226	45.064180
3501.006662	841763.282047	45.069185
3500.841025	841760.107434	45.074189
3501.026045	841744.560759	45.079194
3501.534502	841750.106510	45.084199
3500.893652	841753.989179	45.089204
3501.391415	841751.195789	45.094209
3501.684827	841757.551038	45.099213
3501.472788	841742.260397	45.104218
3501.786728	841723.298993	45.109223
3501.457579	841715.785515	45.114228
3501.401899	841690.286681	45.119233
3501.080140	841689.852074	45.124237
3501.157626	841688.288198	45.129242
3501.618807	841679.972221	45.134247
3501.493235	841666.607614	45.139252
3501.491044	841649.538154	45.144257
3501.419458	841657.599361	45.149261
3501.205483	841649.679844	45.154266
3500.958078	841629.933000	45.159271
3501.214998	841621.842847	45.164276
3500.845238	841610.747016	45.169281
3501.098666	841610.513455	45.174285
3501.000166	841615.572282	45.179290
3501.228426	841607.971533	45.184295
3500.917505	841612.966580	45.189300
3500.879185	841610.450902	45.194305
3501.091086	841617.206999	45.199309
3501.093569	841613.521084	45.204314
3501.101479	841593.734207	45.209319
3501.363259	841589.037856	45.214324
3501.365006	841577.204966	45.219329
3501.137009	841588.588342	45.224333
3500.815832	841586.116870	45.229338
3501.127556	841592.566424	45.234343
3500.844656	841588.731126	45.239348
3500.994651	841570.667761	45.244353
3501.351738	841567.702298	45.249357
3501.048821	841559.311617	45.254362
3501.099396	841559.109765	45.259367
3501.077064	841564.835654	45.264372
3500.976080	841560.874912	45.269377
3500.685562	841567.030680	45.274381
3500.535421	841565.211386	45.279386
3500.912814	841564.473499	45.284391
3501.031934	841569.692326	45.289396
3501.109809	841569.971152	45.294401
3501.270598	841562.671859	45.299405
3501.473930	841544.600077	45.304410
3501.155954	841536.599676	45.309415
3500.928876	841543.521468	45.314420
3501.299903	841538.904989	45.319425
3501.151949	841538.831159	45.324429
3500.997330	841524.985825	45.329434
3501.282082	841515.436329	45.334439
3500.866086	841514.628479	45.339444
3501.147092	841497.708292	45.344449
3501.063264	841504.898707	45.349453
3500.712112	841496.806448	45.354458
3500.852553	841497.851419	45.359463
3500.657925	841506.320027	45.364468
3501.098357	841490.538780	45.369473
3500.822083	841511.046946	45.374477
3500.933969	841521.116450	45.379482
3501.115152	841505.375768	45.384487
3501.089019	841495.971828	45.389492
3500.965968	841474.071236	45.394497
3500.999793	841484.637958	45.399501
3501.357076	841483.903205	45.404506
3501.199644	841476.556560	45.409511
3501.123683	841481.127026	45.414516
3501.240121	841472.476687	45.419521
3500.819453	841460.030659	45.424525
3500.851083	841459.249819	45.429530
3500.987573	841438.472414	45.434535
3500.705264	841444.821007	45.439540
3501.219778	841433.004664	45.444545
3501.016893	841443.996427	45.449549
3500.901869	841436.643103	45.454554
3500.960612	841446.333076	45.459559
3501.045046	841447.483803	45.464564
3500.887917	841453.521845	45.469569
3500.935339	841458.751978	45.474573
3500.901241	841451.289031	45.479578
3500.853790	841450.423561	45.484583
3500.789391	841455.477194	45.489588
3501.332861	841450.445727	45.494593
3501.245470	841435.910737	45.499597
3501.047568	841419.453155	45.504602
3500.999633	841421.303520	45.509607
3501.044766	841418.871707	45.514612
3501.102094	841419.153752	45.519617
3501.355576	841425.806576	45.524621
3501.288305	841423.489327	45.529626
3501.547835	841398.812888	45.534631
3501.121204	841402.662295	45.539636
3501.435346	841393.786952	45.544641
3501.386634	841396.316391	45.549645
3501.194412	841375.493158	45.554650
3501.517248	841366.713408	45.559655
3501.392752	841360.816357	45.564660
3501.255769	841351.914480	45.569665
3501.099450	841338.844917	45.574669
3501.229347	841334.750939	45.579674
3501.143126	841325.744093	45.584679
3500.992936	841323.148787	45.589684
3501.095149	841324.587739	45.594689
3501.267902	841337.072870	45.599693
3500.994613	841324.506525	45.604698
3501.167991	841327.874213	45.609703
3501.166772	841311.482578	45.614708
3501.251342	841299.248213	45.619713
3500.998562	841300.742662	45.624717
3500.865610	841289.900190	45.629722
3501.197740	841301.002571	45.634727
3501.059498	841296.368521	45.639732
3501.200220	841282.864426	45.644737
3501.004896	841271.740689	45.649741
3500.815069	841269.733519	45.654746
3500.898337	841271.466427	45.659751
3501.148171	841271.427405	45.664756
3501.188301	841270.257235	45.669761
3501.019215	841266.985900	45.674765
3501.232274	841263.557831	45.679770
3501.329384	841262.087770	45.684775
3501.192057	841246.881163	45.689780
3501.123465	841233.215686	45.694785
3501.274548	841237.459864	45.699789
3501.266290	841227.276747	45.704794
3501.016623	841232.165542	45.709799
3500.930891	841227.426234	45.714804
3501.284273	841207.390073	45.719809
3501.181838	841211.576904	45.724813
3501.203893	841202.843931	45.729818
3501.328296	841193.124993	45.734823
3500.810715	841174.291817	45.739828
3500.667915	841115.825525	45.744833
3501.061254	841004.507952	45.749837
3500.744245	840857.312141	45.754842
3500.688979	840663.995052	45.759847
3500.390795	840409.206792	45.764852
3500.516746	840105.252860	45.769857
3499.808881	839760.568963	45.774861
3499.931928	839368.872215	45.779866
3499.417883	838904.087042	45.784871
3498.801934	838413.177593	45.789876
3498.546010	837847.443422	45.794881
3497.745384	837253.787635	45.799885
3496.957604	836623.960931	45.804890
3496.669818	835933.120204	45.809895
3496.151337	835201.845314	45.814900
3495.579898	834409.507431	45.819905
3495.058981	833589.572490	45.824909
3494.092605	832717.240935	45.829914
3493.617038	831789.137957	45.834919
3492.545027	830822.994714	45.839924
3491.358242	829799.670711	45.844929
3490.497777	828739.188174	45.849933
3489.492835	827628.477708	45.854938
3488.761102	826462.682554	45.859943
3487.820221	825251.864119	45.864948
3486.681378	823999.009954	45.869953
3485.638102	822705.411168	45.874957
3483.995764	821359.862957	45.879962
3482.821753	819972.872188	45.884967
3481.966462	818558.649646	45.889972
3480.968484	817081.900512	45.894977
3479.429738	815569.527390	45.899981
3478.241126	813997.690917	45.904986
3476.782140	812377.457040	45.909991
3475.129454	810731.198212	45.914996
3473.780357	809034.636296	45.920001
3472.019278	807302.815699	45.925005
3470.548345	805530.965426	45.930010
3469.092989	803714.022365	45.935015
3467.257678	801867.728153	45.940020
3465.652400	799966.137195	45.945025
3464.095475	798032.575448	45.950029
3462.173041	796058.288084	45.955034
3460.638706	794039.457700	45.960039
3458.890708	791988.262702	45.965044
3456.828271	789893.004747	45.970049
3455.138031	787778.874785	45.975053
3452.843096	785621.741686	45.980058
3451.315303	783423.212312	45.985063
3448.893840	781200.303033	45.990068
3446.642581	778926.378507	45.995073
3444.712331	776640.661615	46.000077
3442.476677	774301.631397	46.005082
3440.456485	771940.779350	46.010087
3437.838503	769553.849362	46.015092
3435.585761	767124.330114	46.020097
3433.804054	764676.558026	46.025101
3431.041415	762188.651644	46.030106
3428.924864	759678.442337	46.035111
3426.177959	757130.486663	46.040116
3423.943983	754558.234412	46.045121
3421.504292	751953.615127	46.050125
3419.194176	749322.400007	46.055130
3416.775272	746664.209424	46.060135
3414.234915	743977.298866	46.065140
3411.774874	741242.603828	46.070145
3409.341464	738498.459660	46.075149
3406.543408	735726.197729	46.080154
3403.929688	732920.925580	46.085159
3401.259184	730096.557886	46.090164
3398.661424	727243.045106	46.095169
3395.693839	724366.599991	46.100173
3393.122022	721466.738734	46.105178
3390.665333	718531.583173	46.110183
3387.583988	715598.323424	46.115188
3384.937299	712611.888893	46.120193
3381.969843	709608.441889	46.125197
3379.132603	706591.957135	46.130202
3376.335477	703544.330833	46.135207
3373.370002	700477.152722	46.140212
3370.486301	697391.608352	46.145217
3367.504141	694283.899297	46.150221
3364.712560	691156.838841	46.155226
3361.736672	687990.641002	46.160231
3358.565473	684820.437957	46.165236
3355.882373	681628.910748	46.170241
3352.735093	678418.229098	46.175245
3349.437911	675174.776202	46.180250
3346.539044	671927.945854	46.185255
3343.270216	668659.627554	46.190260
3340.401440	665365.213093	46.195265
3337.020997	662059.397360	46.200269
3333.652252	658738.265846	46.205274
3330.782329	655396.062757	46.210279
3327.278572	652051.074924	46.215284
3324.007344	648680.514002	46.220289
3320.965994	645299.260432	46.225293
3317.383254	641895.472751	46.230298
3314.576956	638468.034259	46.235303
3311.092884	635036.760074	46.240308
3307.728809	631587.512553	46.245313
3304.376681	628139.916964	46.250317
3300.781740	624664.767494	46.255322
3297.494906	621181.340698	46.260327
3293.916532	617686.635950	46.265332
3290.564423	614181.422407	46.270337
3287.291695	610663.474423	46.275341
3284.387081	607130.645343	46.280346
3280.569934	603589.737346	46.285351
3277.037279	600036.212957	46.290356
3274.183112	596458.995226	46.295361
3270.425735	592875.249646	46.300365
3266.588108	589288.160683	46.305370
3263.012339	585683.049595	46.310375
3259.639762	582074.209711	46.315380
3256.006730	578451.441827	46.320385
3252.629715	574833.628669	46.325389
3248.688587	571204.355574	46.330394
3245.523454	567560.403242	46.335399
3241.373391	563913.144441	46.340404
3238.196693	560254.396760	46.345409
3234.875720	556598.156000	46.350413
3230.870241	552930.499068	46.355418
3227.404383	549252.092340	46.360423
3223.405767	545582.621216	46.365428
3219.712982	541890.835425	46.370433
3216.292382	538202.096855	46.375437
3212.484728	534501.474133	46.380442
3209.192236	530799.604857	46.385447
3205.146230	527104.154296	46.390452
3201.613126	523385.773453	46.395457
3197.976010	519655.791311	46.400461
3194.037074	515945.999964	46.405466
3190.625952	512213.038472	46.410471
3186.821436	508492.350403	46.415476
3183.072582	504760.077649	46.420481
3179.338805	501030.208994	46.425485
3175.846010	497289.753002	46.430490
3172.074865	493542.684137	46.435495
3168.019781	489809.817850	46.440500
3164.663979	486045.665288	46.445505
3161.126900	482291.885836	46.450509
3156.904501	478539.483276	46.455514
3153.286337	474777.453519	46.460519
3149.403886	471017.416615	46.465524
3145.736215	467270.337424	46.470529
3141.952818	463513.376385	46.475533
3137.893693	459735.991586	46.480538
3134.303212	455970.555264	46.485543
3130.311676	452213.833872	46.490548
3126.698491	448446.385633	46.495553
3123.057618	444678.762908	46.500557
3119.129280	440915.122405	46.505562
3115.361715	437143.303138	46.510567
3111.359078	433384.960040	46.515572
3107.306725	429624.325198	46.520577
3103.518712	425862.882396	46.525581
3099.386302	422097.292694	46.530586
3095.815123	418337.870978	46.535591
3091.882686	414591.472665	46.540596
3088.091581	410826.895762	46.545601
3084.251730	407085.114212	46.550605
3080.406415	403333.622015	46.555610
3076.775123	399581.578762	46.560615
3072.739816	395829.652518	46.565620
3069.009562	392089.523031	46.570625
3064.729526	388344.689575	46.575629
3060.794704	384601.065979	46.580634
3056.964325	380871.146390	46.585639
3052.855107	377143.911292	46.590644
3048.929543	373424.509561	46.595649
3045.272300	369696.990505	46.600653
3040.930168	365979.755214	46.605658
3037.089815	362272.126748	46.610663
3033.263952	358564.566008	46.615668
3029.479197	354863.105288	46.620673
3025.494466	351163.577483	46.625677
3021.520429	347469.979649	46.630682
3017.823154	343779.182850	46.635687
3013.546617	340097.691322	46.640692
3009.618617	336407.039957	46.645697
3005.683180	332741.145319	46.650701
3001.284693	329061.385590	46.655706
2997.331327	325404.079305	46.660711
2993.128963	321759.711570	46.665716
2989.277995	318103.855800	46.670721
2985.521764	314479.256570	46.675725
2981.057558	310848.042260	46.680730
2977.320004	307225.013097	46.685735
2973.387498	303611.421114	46.690740
2969.163713	300010.018316	46.695745
2965.416703	296405.884795	46.700749
2961.317399	292831.437831	46.705754
2957.199355	289237.282294	46.710759
2953.121654	285677.743482	46.715764
2949.162317	282119.602038	46.720769
2944.731498	278572.636329	46.725773
2940.061484	275029.667956	46.730778
2936.402470	271492.880845	46.735783
2932.259362	267980.344765	46.740788
2928.543405	264484.826099	46.745793
2924.143230	260992.301425	46.750797
2919.770745	257505.700549	46.755802
2915.673676	254027.746000	46.760807
2911.235385	250579.351753	46.765812
2907.110451	247140.333622	46.770817
2903.279953	243701.460206	46.775821
2898.827368	240296.553936	46.780826
2894.772726	236885.939079	46.785831
2890.736919	233501.520481	46.790836
2886.516077	230113.898022	46.795841
2882.100483	226752.117392	46.800845
2877.809079	223402.639618	46.805850
2873.902086	220061.332687	46.810855
2869.345215	216747.112474	46.815860
2865.462368	213439.074393	46.820865
2860.892203	210145.131492	46.825869
2856.932218	206858.747605	46.830874
2852.931642	203598.980798	46.835879
2848.454510	200361.093170	46.840884
2844.262050	197117.443347	46.845889
2840.073556	193896.631365	46.850893
2835.328737	190699.770051	46.855898
2831.448323	187504.107136	46.860903
2826.931074	184335.883924	46.865908
2822.577457	181187.163366	46.870913
2818.103647	178045.875589	46.875917
2813.928834	174938.823464	46.880922
2809.965236	171836.986857	46.885927
2806.074344	168668.344647	46.890932
2801.864134	165602.486769	46.895937
2797.557128	162542.533992	46.900941
2793.480187	159510.982436	46.905946
2789.142625	156477.060863	46.910951
2784.461736	153480.038124	46.915956
2780.383512	150483.269375	46.920961
2776.206432	147516.545995	46.925965
2771.945655	144560.004197	46.930970
2768.007363	141624.451107	46.935975
2763.761983	138707.303167	46.940980
2759.233340	135800.111933	46.945985
2755.260204	132908.106092	46.950989
2751.050396	130040.762113	46.955994
2746.679970	127185.209531	46.960999
2742.642265	124345.737082	46.966004
2738.085337	121519.262715	46.971009
2733.853703	118716.746340	46.976013
2729.846667	115935.088544	46.981018
2725.568013	113164.538941	46.986023
2721.260791	110406.181130	46.991028
2717.193198	107675.994032	46.996033
2712.965435	104955.008689	47.001037
2708.712513	102254.176429	47.006042
2704.585016	99563.725160	47.011047
2699.946656	96901.968599	47.016052
2695.805051	94255.085758	47.021057
2691.765643	91631.080935	47.026061
2687.278847	89013.254524	47.031066
2683.278033	86416.099094	47.036071
2678.868636	83853.651062	47.041076
2674.770459	81290.861494	47.046081
2670.701111	78746.335240	47.051085
2666.492793	76227.819301	47.056090
2662.537922	73708.784809	47.061095
2658.301199	71219.781245	47.066100
2653.875593	68750.562548	47.071105
2649.638721	66284.151452	47.076109
2645.396280	63852.627315	47.081114
2641.555731	61427.081986	47.086119
2636.974867	59026.041573	47.091124
2632.708477	56634.527871	47.096129
2628.643348	54274.606406	47.101133
2624.424777	51922.746375	47.106138
2619.879020	49596.089931	47.111143
2615.400488	47284.809734	47.116148
2610.912242	44983.684171	47.121153
2607.019597	42712.162512	47.126157
2602.175245	40459.657169	47.131162
2598.454009	38228.300657	47.136167
2593.852846	36027.201634	47.141172
2589.942945	33832.033305	47.146177
2585.598753	31659.064925	47.151181
2581.081002	29504.062433	47.156186
2577.167368	27384.884902	47.161191
2572.666597	25275.554522	47.166196
2568.152481	23183.634128	47.171201
2563.813705	21113.291090	47.176205
2559.126440	19083.168247	47.181210
2554.948401	17053.422855	47.186215
2550.228314	15060.831422	47.191220
2545.502417	13098.408055	47.196225
2540.941305	11160.391859	47.201229
2535.474449	9253.630097	47.206234
2531.046664	7381.501401	47.211239
2525.505024	5536.371076	47.216244
2520.187033	3727.428365	47.221249
2514.816281	1981.789615	47.226253
2508.392751	294.203088	47.231258
2461.212044	-276.909878	47.236263
2385.342793	235.459409	47.241268
2358.397333	247.394712	47.246273
2356.326630	227.751421	47.251277
2367.034102	252.124607	47.256282
2382.491503	249.412220	47.261287
2395.710467	250.941614	47.266292
2403.968127	247.030126	47.271297
2407.484683	236.444187	47.276301
2406.777928	240.889305	47.281306
2404.047534	231.853297	47.286311
2399.771070	234.778183	47.291316
2395.885558	222.755840	47.296321
2392.323245	219.231752	47.301325
2388.701681	219.700261	47.306330
2385.760500	217.622979	47.311335
2382.782780	228.785931	47.316340
2380.024381	221.658975	47.321345
2377.956100	210.649550	47.326349
2375.393232	224.161642	47.331354
2372.035431	220.384094	47.336359
2368.779405	224.152302	47.341364
2365.977431	224.650794	47.346369
2362.664540	207.751942	47.351373
2359.140140	215.447379	47.356378
2355.977202	199.259100	47.361383
2352.866887	202.071168	47.366388
2349.948469	197.981276	47.371393
2346.743100	200.941100	47.376397
2342.674472	199.366095	47.381402
2339.923527	193.111226	47.386407
2336.130222	196.761004	47.391412
2332.740951	198.107550	47.396417
2330.054031	194.275688	47.401421
2326.276939	199.701031	47.406426
2323.436129	204.315485	47.411431
2319.577299	199.831702	47.416436
2316.331282	195.574765	47.421441
2313.213321	202.665599	47.426445
2309.675330	196.616130	47.431450
2306.777083	197.620099	47.436455
2302.923986	207.436145	47.441460
2299.643514	200.545930	47.446465
2296.544155	199.556484	47.451469
2292.840987	199.784681	47.456474
2289.757517	189.778874	47.461479
2285.944279	202.939229	47.466484
2282.362407	204.828470	47.471489
2279.216927	196.765493	47.476493
2275.893769	204.799635	47.481498
2272.568976	207.091602	47.486503
2269.148812	207.557115	47.491508
2265.518643	199.414941	47.496513
2262.262596	195.580387	47.501517
2258.249373	216.548848	47.506522
2254.987219	206.488739	47.511527
2251.680115	201.817419	47.516532
2248.059678	196.929358	47.521537
2245.159728	192.577172	47.526541
2241.871959	205.073174	47.531546
2238.455349	195.065718	47.536551
2235.181267	201.652629	47.541556
2231.201157	202.088696	47.546561
2227.486768	199.233893	47.551565
2223.529379	213.081235	47.556570
2220.836315	200.394678	47.561575
2217.336000	215.733466	47.566580
2214.460790	193.096552	47.571585
2210.600420	194.722492	47.576589
2207.037801	206.590763	47.581594
2203.746710	200.429934	47.586599
2200.176231	196.144702	47.591604
2196.345514	196.671307	47.596609
2193.391671	195.219347	47.601613
2189.588065	204.230382	47.606618
2186.040022	194.582046	47.611623
2182.522800	190.209393	47.616628
2179.155614	198.187166	47.621633
2176.143239	192.821168	47.626637
2172.161564	202.040408	47.631642
2168.892661	200.283395	47.636647
2165.704465	196.390797	47.641652
2161.746863	191.248628	47.646657
2158.939541	186.562425	47.651661
2155.226005	189.269600	47.656666
2151.437574	194.867616	47.661671
2148.217748	188.831707	47.666676
2144.274830	200.936667	47.671681
2141.167201	186.261660	47.676685
2137.340281	186.502944	47.681690
2134.489151	190.710911	47.686695
2130.775072	192.747438	47.691700
2127.157226	188.048852	47.696705
2123.952362	184.908716	47.701709
2120.058180	188.893893	47.706714
2116.949178	189.377209	47.711719
2113.776607	186.133943	47.716724
2109.934672	181.824780	47.721729
2106.443734	187.651517	47.726733
2102.876589	190.775581	47.731738
2099.374424	174.624692	47.736743
2095.562421	189.015632	47.741748
2092.093647	194.339015	47.746753
2089.052556	186.417971	47.751757
2085.327100	187.200237	47.756762
2082.093578	191.034598	47.761767
2078.473524	181.992387	47.766772
2074.958590	187.411584	47.771777
2071.808135	185.401944	47.776781
2068.201828	183.463631	47.781786
2064.351297	174.571392	47.786791
2061.156293	181.772410	47.791796
2057.293604	183.579104	47.796801
2054.047575	185.096315	47.801805
2050.574983	184.228619	47.806810
2047.201175	178.811650	47.811815
2043.675200	186.099263	47.816820
2039.807328	175.928382	47.821825
2036.528990	178.440942	47.826829
2033.010717	186.714479	47.831834
2029.819473	176.061228	47.836839
2025.957441	176.387142	47.841844
2022.866520	180.284628	47.846849
2019.637941	180.891089	47.851853
2015.771671	180.091333	47.856858
2012.247100	181.272477	47.861863
2008.785765	179.621560	47.866868
2005.050556	182.771950	47.871873
2001.743064	169.248296	47.876877
1997.741133	176.050390	47.881882
1994.684808	177.449345	47.886887
1991.055503	180.342714	47.891892
1987.731076	175.987426	47.896897
1984.322739	174.011839	47.901901
1981.083827	174.781285	47.906906
1977.539914	171.159560	47.911911
1973.937362	173.564677	47.916916
1970.488300	167.678607	47.921921
1966.849432	179.688565	47.926925
1963.047499	175.192862	47.931930
1959.952699	173.506755	47.936935
1956.494486	177.278227	47.941940
1952.569673	182.331309	47.946945
1949.734128	170.261973	47.951949
1945.577375	181.894216	47.956954
1942.078721	176.892304	47.961959
1938.927950	175.974288	47.966964
1935.642162	173.527108	47.971969
1932.230430	166.145034	47.976973
1927.753590	169.626641	47.981978
1924.466836	171.621677	47.986983
1921.546941	174.337616	47.991988
1918.061404	171.621133	47.996993
1914.553403	171.923326	48.001997
1910.935998	167.177300	48.007002
1907.809273	170.210355	48.012007
1904.039110	179.665492	48.017012
1900.526848	175.523132	48.022017
1897.058838	166.166138	48.027021
1893.462434	183.693568	48.032026
1889.898013	174.626915	48.037031
1886.098598	174.348274	48.042036
1882.364543	174.733309	48.047041
1879.653595	175.239827	48.052045
1875.910171	176.395148	48.057050
1872.526062	175.896493	48.062055
1869.119151	166.536277	48.067060
1865.518245	168.890548	48.072065
1862.373545	173.261577	48.077069
1858.610711	176.603004	48.082074
1855.146352	174.743799	48.087079
1851.537072	173.964002	48.092084
1848.126932	168.704659	48.097089
1844.646870	162.649478	48.102093
1840.782683	167.946214	48.107098
1837.434996	164.151461	48.112103
1833.835512	166.037269	48.117108
1830.661405	173.000943	48.122113
1827.045969	170.646517	48.127117
1823.502411	171.027073	48.132122
1819.911513	172.237640	48.137127
1816.539601	168.187248	48.142132
1812.826461	176.393253	48.147137
1809.828134	163.678711	48.152141
1805.827198	172.255631	48.157146
1802.466443	170.155597	48.162151
1799.154047	170.598065	48.167156
1795.379338	162.700191	48.172161
1792.485044	164.532604	48.177165
1788.058585	174.466976	48.182170
1784.831190	170.318046	48.187175
1781.405835	164.304949	48.192180
1777.754919	167.923125	48.197185
1774.512460	166.940412	48.202189
1771.007631	169.985219	48.207194
1767.714001	161.591277	48.212199
1763.874700	161.920056	48.217204
1760.218549	171.854111	48.222209
1757.045738	167.180941	48.227213
1753.563242	169.861578	48.232218
1750.425620	166.435790	48.237223
1746.715716	168.762864	48.242228
1742.665497	169.210083	48.247233
1739.772817	161.468436	48.252237
1736.188055	173.599695	48.257242
1732.607570	171.239834	48.262247
1729.073733	164.003504	48.267252
1725.045916	167.506670	48.272257
1722.115199	169.667515	48.277261
1718.545130	169.460614	48.282266
1715.488754	160.399957	48.287271
1711.936528	156.760651	48.292276
1708.088871	164.582760	48.297281
1704.264451	162.425607	48.302285
1700.684654	164.102728	48.307290
1697.480824	154.884817	48.312295
1693.748693	165.014281	48.317300
1690.354816	161.328053	48.322305
1687.238081	156.529071	48.327309
1683.598750	154.089853	48.332314
1680.102182	155.320506	48.337319
1676.758204	153.103994	48.342324
1672.797952	156.327676	48.347329
1669.684718	160.193939	48.352333
1665.815260	156.911193	48.357338
1662.453526	158.209338	48.362343
1659.098288	153.979221	48.367348
1655.502139	158.313385	48.372353
1652.302515	150.284444	48.377357
1648.701697	158.998108	48.382362
1645.218394	151.301478	48.387367
1641.344921	150.461862	48.392372
1637.753649	155.168602	48.397377
1634.856166	157.760879	48.402381
1631.036907	168.717107	48.407386
1627.606836	150.324667	48.412391
1624.141107	157.071428	48.417396
1620.245132	162.211853	48.422401
1616.677946	147.156596	48.427405
1613.401440	158.239854	48.432410
1609.925627	151.016644	48.437415
1606.605978	149.100078	48.442420
1603.242092	155.735989	48.447425
1599.667676	151.394661	48.452429
1596.022613	151.778526	48.457434
1592.172798	156.051168	48.462439
1588.875504	152.811784	48.467444
1584.969770	152.398032	48.472449
1582.169380	147.824831	48.477453
1578.450420	153.877226	48.482458
1574.964174	153.109911	48.487463
1571.345873	151.866542	48.492468
1567.832350	147.069595	48.497473
1564.473657	149.322776	48.502477
1561.218796	145.130772	48.507482
1557.779118	148.247705	48.512487
1554.559996	146.309095	48.517492
1550.466021	150.866746	48.522497
1547.065791	147.662472	48.527501
1543.084615	157.849936	48.532506
1539.483703	143.692203	48.537511
1536.523953	146.832104	48.542516
1532.968480	156.187290	48.547521
1529.901841	148.425492	48.552525
1525.992853	152.400525	48.557530
1522.379736	151.567663	48.562535
1519.487395	156.585834	48.567540
1515.335168	151.895204	48.572545
1512.108753	146.395261	48.577549
1508.472070	149.071632	48.582554
1505.276852	148.840937	48.587559
1501.366613	151.917643	48.592564
1497.740324	154.503803	48.597569
1494.658526	146.102132	48.602573
1490.679722	150.084941	48.607578
1487.167399	149.929197	48.612583
1484.083008	151.351671	48.617588
1480.235764	155.905531	48.622593
1477.112313	143.568237	48.627597
1473.525830	162.495759	48.632602
1469.762575	145.582448	48.637607
1466.482433	153.840995	48.642612
1462.746202	155.327539	48.647617
1459.701066	147.265001	48.652621
1455.760812	157.183488	48.657626
1452.205967	149.880961	48.662631
1448.574431	145.219595	48.667636
1445.518671	147.150141	48.672641
1442.168879	142.890780	48.677645
1438.316800	146.992981	48.682650
1435.225169	141.003722	48.687655
1431.877653	142.897680	48.692660
1427.877264	151.389201	48.697665
1424.401818	143.568045	48.702669
1420.796322	148.742163	48.707674
1417.258141	146.910491	48.712679
1414.101566	146.964850	48.717684
1410.885349	156.624479	48.722689
1407.319928	146.944418	48.727693
1403.319924	153.018713	48.732698
1399.577733	141.471187	48.737703
1396.294206	150.935703	48.742708
1392.772301	140.723642	48.747713
1389.456442	137.715035	48.752717
1385.582360	145.000356	48.757722
1381.628728	150.346044	48.762727
1379.296583	141.216451	48.767732
1375.337652	147.031218	48.772737
1372.393830	137.244384	48.777741
1368.395330	150.731331	48.782746
1364.866717	152.292981	48.787751
1361.231488	144.683530	48.792756
1357.055152	143.122622	48.797761
1354.588785	138.136533	48.802765
1350.925836	142.690061	48.807770
1347.544478	148.022110	48.812775
1344.318443	145.249400	48.817780
1340.231963	151.299287	48.822785
1336.899556	137.273637	48.827789
1333.421617	158.231193	48.832794
1330.155263	154.022086	48.837799
1326.382914	151.869590	48.842804
1322.685494	156.381068	48.847809
1319.397591	150.682007	48.852813
1316.029751	152.038168	48.857818
1312.099969	154.675065	48.862823
1309.094256	140.449584	48.867828
1305.181786	156.242178	48.872833
1301.835523	142.120631	48.877837
1298.107854	152.717748	48.882842
1294.580834	145.284381	48.887847
1291.756928	145.036758	48.892852
1287.934547	149.327357	48.897857
1284.535315	144.522123	48.902861
1280.911357	142.251501	48.907866
1277.234014	147.541318	48.912871
1273.724953	141.614300	48.917876
1269.882327	148.625810	48.922881
1266.748325	141.285959	48.927885
1263.465123	149.130572	48.932890
1259.778793	150.989039	48.937895
1256.270420	157.239531	48.942900
1252.970406	154.127246	48.947905
1249.171171	137.748054	48.952909
1245.873293	143.547966	48.957914
1242.275456	154.738560	48.962919
1238.860752	146.110685	48.967924
1235.221972	155.659333	48.972929
1231.963161	137.749672	48.977933
1228.111456	140.292117	48.982938
1225.131101	148.620854	48.987943
1221.515969	142.878146	48.992948
1217.461891	144.686628	48.997953
1214.136595	146.320907	49.002957
1210.711859	144.876524	49.007962
1207.312013	142.124746	49.012967
1203.942334	146.072412	49.017972
1200.363004	157.548031	49.022977
1197.045213	144.725574	49.027981
1193.278449	147.501514	49.032986
1189.575336	139.678135	49.037991
1186.096441	141.602232	49.042996
1182.897151	149.968418	49.048001
1179.455521	140.183659	49.053005
1175.729745	146.673857	49.058010
1172.283581	139.721444	49.063015
1168.832322	133.149492	49.068020
1164.915231	138.897667	49.073025
1161.683584	139.688378	49.078029
1158.074201	143.676750	49.083034
1154.276547	141.461846	49.088039
1151.136439	136.913498	49.093044
1147.673320	139.664062	49.098049
1144.606206	135.651632	49.103053
1141.184454	143.078195	49.108058
1137.049116	143.111865	49.113063
1133.810047	146.244984	49.118068
1130.066212	137.852190	49.123073
1126.662440	135.699022	49.128077
1123.016990	142.705020	49.133082
1119.602407	141.692526	49.138087
1116.261286	141.465817	49.143092
1112.945183	134.898039	49.148097
1109.467423	131.541550	49.153101
1105.914883	137.178886	49.158106
1102.197801	141.896000	49.163111
1098.642395	138.845907	49.168116
1094.958003	142.744801	49.173121
1091.925523	136.635674	49.178125
1088.154058	144.044236	49.183130
1084.517901	138.583297	49.188135
1081.042843	139.418471	49.193140
1077.514989	139.818976	49.198145
1074.284773	141.368811	49.203149
1070.484393	142.106223	49.208154
1066.702696	145.314827	49.213159
1063.648311	139.845070	49.218164
1059.757960	147.047624	49.223169
1056.516203	141.176924	49.228173
1053.196942	144.161267	49.233178
1049.782683	148.283645	49.238183
1046.067230	137.114931	49.243188
1042.903857	138.417023	49.248193
1039.553760	134.059786	49.253197
1035.976684	142.450355	49.258202
1032.220954	146.768575	49.263207
1028.722306	138.327948	49.268212
1024.798743	145.127579	49.273217
1021.627296	145.551398	49.278221
1018.112231	143.994675	49.283226
1014.660690	139.741917	49.288231
1011.363585	138.166890	49.293236
1007.209225	150.441288	49.298241
1004.034682	136.900454	49.303245
1000.748809	138.652020	49.308250
996.788684	144.172871	49.313255
993.337680	134.392830	49.318260
989.929010	143.576476	49.323265
986.682246	134.846489	49.328269
983.420419	136.508872	49.333274
979.587222	140.712686	49.338279
976.190037	133.853931	49.343284
972.265698	137.328518	49.348289
969.391113	127.860044	49.353293
965.321019	132.876091	49.358298
961.883717	134.711493	49.363303
958.978786	139.655840	49.368308
954.965801	142.559006	49.373313
951.541925	138.159570	49.378317
948.050186	138.083058	49.383322
944.406763	148.705052	49.388327
940.957915	131.651057	49.393332
937.238114	142.212241	49.398337
934.124981	135.239422	49.403341
930.715966	139.765986	49.408346
927.348704	138.939146	49.413351
923.557619	127.864600	49.418356
919.902329	138.523256	49.423361
916.607488	135.062269	49.428365
913.237152	136.112065	49.433370
909.293318	135.739353	49.438375
905.985923	133.156716	49.443380
902.240354	138.764231	49.448385
898.951835	132.717416	49.453389
895.259340	135.902623	49.458394
892.275368	135.294196	49.463399
888.989335	130.635916	49.468404
884.847720	131.901407	49.473409
881.582442	126.062939	49.478413
877.821242	137.108357	49.483418
874.642111	135.071972	49.488423
870.948336	120.150829	49.493428
867.355518	137.073576	49.498433
864.029815	131.959599	49.503437
860.470848	137.458812	49.508442
856.667962	137.836025	49.513447
853.535437	138.937191	49.518452
850.142543	144.100350	49.523457
846.531771	137.328878	49.528461
842.629997	141.632068	49.533466
838.845464	140.022696	49.538471
836.220660	134.280108	49.543476
832.583743	143.233779	49.548481
829.163596	136.375517	49.553485
825.919235	133.166094	49.558490
821.678431	135.434256	49.563495
818.657283	135.505569	49.568500
814.497706	135.068603	49.573505
811.208007	127.342020	49.578509
807.588864	137.412905	49.583514
804.067895	140.862359	49.588519
801.261197	136.565658	49.593524
797.587981	143.968423	49.598529
794.411616	131.168309	49.603533
790.542749	138.886456	49.608538
786.657810	143.996970	49.613543
782.978857	134.107184	49.618548
779.217203	142.833626	49.623553
776.303843	134.545074	49.628557
773.091311	130.555551	49.633562
769.914146	139.949783	49.638567
765.870323	134.904006	49.643572
762.258577	145.160416	49.648577
758.917529	125.950896	49.653581
755.597667	133.839349	49.658586
751.969272	135.976839	49.663591
748.915754	127.919061	49.668596
744.915207	135.382592	49.673601
741.399144	125.179415	49.678605
738.050907	129.658555	49.683610
734.223230	136.417961	49.688615
730.874064	123.610140	49.693620
726.666819	124.784734	49.698625
723.555301	128.828168	49.703629
720.356912	118.913785	49.708634
716.814379	136.236825	49.713639
713.426175	128.433959	49.718644
709.734624	135.222676	49.723649
706.208433	119.803967	49.728653
703.019784	124.985803	49.733658
699.481811	128.200668	49.738663
696.188015	126.830888	49.743668
692.204423	124.876259	49.748673
688.893146	118.655925	49.753677
685.371691	128.951994	49.758682
681.524390	126.150269	49.763687
678.135855	117.616633	49.768692
674.564790	128.034372	49.773697
671.212743	116.951316	49.778701
667.756573	130.786968	49.783706
664.039146	127.275199	49.788711
660.899620	122.530791	49.793716
657.449319	124.121557	49.798721
654.070349	124.400825	49.803725
650.270630	133.557219	49.808730
646.677224	128.507402	49.813735
643.212969	131.369050	49.818740
639.667434	141.482245	49.823745
636.123294	129.125788	49.828749
632.824931	126.484892	49.833754
629.712370	125.191160	49.838759
626.090473	120.601406	49.843764
622.193013	125.248857	49.848769
618.703658	126.206663	49.853773
615.193290	122.817515	49.858778
611.548446	125.043055	49.863783
608.117286	114.589365	49.868788
604.367247	130.302905	49.873793
601.147551	120.749421	49.878797
597.642639	119.979065	49.883802
593.952138	122.040916	49.888807
590.775284	124.420963	49.893812
587.076017	125.759677	49.898817
584.250753	127.214613	49.903821
580.285115	126.516421	49.908826
576.580479	133.386328	49.913831
573.510554	122.600821	49.918836
569.865345	118.897447	49.923841
566.589260	119.081539	49.928845
562.835812	123.801372	49.933850
558.873159	131.325475	49.938855
555.578426	121.394614	49.943860
551.376436	131.041158	49.948865
548.587200	130.307430	49.953869
545.348384	125.936127	49.958874
541.589840	122.282154	49.963879
538.353633	117.654178	49.968884
534.513675	129.060053	49.973889
531.236582	126.396883	49.978893
527.880438	131.332920	49.983898
524.209784	123.387712	49.988903
520.644681	115.751851	49.993908
517.277507	132.778546	49.998913
513.538692	120.844959	50.003917
509.882767	122.695780	50.008922
506.451237	126.378105	50.013927
503.398607	125.761578	50.018932
499.529280	123.248128	50.023937
496.275961	124.526521	50.028941
492.822369	122.033382	50.033946
489.033746	122.009872	50.038951
485.355832	119.694243	50.043956
482.224134	121.693924	50.048961
478.744304	112.798186	50.053965
475.064332	116.269492	50.058970
471.634101	124.577116	50.063975
468.347511	108.133904	50.068980
464.411319	118.760753	50.073985
461.092855	112.101873	50.078989
457.480363	114.831777	50.083994
453.802020	127.231110	50.088999
450.742750	117.639911	50.094004
447.041631	122.288315	50.099009
443.572512	122.236926	50.104013
440.162817	114.646364	50.109018
436.738782	123.380142	50.114023
432.977267	120.742267	50.119028
429.328636	122.364182	50.124033
425.912324	116.669784	50.129037
422.912544	102.715887	50.134042
418.952476	128.488479	50.139047
415.592707	121.453264	50.144052
412.094238	125.509945	50.149057
408.551128	117.478377	50.154061
404.790871	124.790496	50.159066
401.121302	115.785305	50.164071
398.212308	115.171626	50.169076
394.186736	120.060699	50.174081
391.141423	115.358589	50.179085
387.562578	125.366336	50.184090
383.926750	123.050486	50.189095
380.857361	118.440736	50.194100
377.041887	117.054715	50.199105
373.402192	117.270521	50.204109
370.019916	116.594943	50.209114
366.435581	113.622455	50.214119
363.569018	112.147914	50.219124
359.610928	113.970193	50.224129
356.127561	121.830587	50.229133
352.222925	127.105703	50.234138
348.206287	123.305580	50.239143
345.389025	119.412500	50.244148
342.083315	123.265002	50.249153
338.738994	110.947011	50.254157
335.129902	111.765491	50.259162
331.278438	112.979448	50.264167
327.876258	116.369330	50.269172
324.323863	114.666871	50.274177
320.919232	109.011821	50.279181
317.428959	110.770328	50.284186
313.729895	120.803255	50.289191
310.954746	116.413202	50.294196
306.973554	124.424363	50.299201
303.476117	116.072474	50.304205
299.950935	121.212237	50.309210
296.156039	115.966349	50.314215
292.876055	110.630312	50.319220
289.288712	119.699769	50.324225
285.825346	112.813722	50.329229
282.373991	123.503895	50.334234
278.870168	127.937956	50.339239
275.663959	120.673100	50.344244
272.041266	111.249337	50.349249
268.771144	112.992358	50.354253
265.054144	112.375583	50.359258
261.267428	118.328297	50.364263
258.299068	117.233575	50.369268
253.878999	118.830872	50.374273
250.721765	123.577649	50.379277
247.555790	113.250270	50.384282
243.841528	125.791337	50.389287
240.308911	110.766200	50.394292
236.577312	115.713690	50.399297
233.544623	111.898693	50.404301
229.966577	106.682144	50.409306
226.261708	118.285254	50.414311
223.072700	116.788506	50.419316
219.484681	113.639486	50.424321
215.882074	118.743950	50.429325
212.096643	121.440929	50.434330
208.293385	129.433746	50.439335
204.988607	126.566230	50.444340
201.904231	127.647416	50.449345
198.061828	123.250587	50.454349
194.947483	118.758685	50.459354
191.552037	118.759130	50.464359
187.728572	108.895456	50.469364
184.474187	131.153302	50.474369
180.744118	116.905783	50.479373
177.037293	122.032916	50.484378
173.586642	120.308253	50.489383
170.776270	123.956660	50.494388
167.084642	131.925678	50.499393
163.543364	126.250970	50.504397
159.769524	122.172453	50.509402
156.117094	118.302712	50.514407
152.991584	120.510345	50.519412
149.249859	127.338756	50.524417
146.057752	125.095864	50.529421
142.273315	125.062355	50.534426
138.391613	122.364345	50.539431
135.036809	125.708910	50.544436
131.555799	118.113841	50.549441
128.180218	118.585768	50.554445
125.039758	119.375206	50.559450
121.422770	122.355884	50.564455
117.938750	113.321766	50.569460
114.259206	121.871044	50.574465
110.258574	116.821995	50.579469
107.227005	116.607274	50.584474
103.175604	119.133992	50.589479
100.387309	118.004787	50.594484
96.567389	120.716708	50.599489
93.338199	117.932309	50.604493
89.943944	117.999046	50.609498
86.355950	123.325900	50.614503
82.909310	115.057908	50.619508
79.655744	117.042016	50.624513
75.792276	118.359205	50.629517
72.411273	117.003327	50.634522
68.531212	124.103381	50.639527
64.901793	118.189425	50.644532
61.564778	116.810841	50.649537
58.203965	116.780601	50.654541
54.815139	113.220789	50.659546
51.033543	117.261847	50.664551
47.927694	117.846570	50.669556
44.451454	126.784808	50.674561
40.562615	117.352235	50.679565
37.390209	114.027445	50.684570
33.482853	118.948767	50.689575
30.447202	121.556820	50.694580
26.602367	117.173112	50.699585
23.077266	116.216323	50.704589
19.587452	120.781161	50.709594
15.818101	121.871656	50.714599
12.552923	115.625407	50.719604
9.147518	125.568135	50.724609
5.566056	113.505764	50.729613
2.614554	115.202123	50.734618