Thu Aug 25 17:01:32 2022

Number of Points = 9925

Depth (nm)	Load (N)	Time (s)
2.022331	98.221503	0.000000
1.821586	94.253941	0.005005
1.654797	86.531963	0.010010
1.633126	79.742716	0.015014
1.500036	88.087533	0.020019
1.481975	68.069905	0.025024
0.829166	59.971667	0.030029
0.531964	57.528354	0.035034
0.421010	54.217456	0.040038
0.133676	47.273691	0.045043
-0.185002	37.791157	0.050048
0.081579	42.406504	0.055053
-0.236139	31.218542	0.060058
0.097271	28.341066	0.065062
-0.472883	24.662355	0.070067
-0.992334	8.409161	0.075072
-1.788192	-1.732583	0.080077
-2.240402	-1.193467	0.085082
-2.375288	-10.704773	0.090086
-2.563077	-3.455586	0.095091
-2.575040	-3.912437	0.100096
-3.148588	-5.293706	0.105101
-3.500899	-5.861746	0.110106
-3.491853	-5.638512	0.115110
-4.209488	1.586125	0.120115
-4.159125	-9.805016	0.125120
-4.511999	-11.388541	0.130125
-5.122417	-10.894240	0.135130
-5.065971	-14.070001	0.140134
-5.060653	-13.687995	0.145139
-5.470015	-3.778157	0.150144
-5.170284	-10.978398	0.155149
-5.863488	-6.472112	0.160154
-6.179085	-18.663291	0.165158
-6.623573	-3.293600	0.170163
-6.973151	-8.240737	0.175168
-6.969800	-6.928272	0.180173
-7.486740	-3.063375	0.185178
-6.871311	-18.374382	0.190182
-7.243700	-4.733919	0.195187
-8.390152	-13.093301	0.200192
-8.252744	-3.329244	0.205197
-8.610242	-8.094805	0.210202
-8.462917	-11.085488	0.215206
-8.685410	-11.870022	0.220211
-9.364669	-11.200419	0.225216
-9.773794	-13.547090	0.230221
-9.906192	-2.063958	0.235226
-9.619990	-9.682862	0.240230
-9.842060	-0.368684	0.245235
-10.243668	-6.804136	0.250240
-10.334561	6.203767	0.255245
-10.976121	-0.928087	0.260250
-11.027983	-10.841545	0.265254
-11.168902	-3.555410	0.270259
-11.855885	-7.370832	0.275264
-12.278024	4.306400	0.280269
-12.614050	0.167065	0.285274
-12.615081	-14.430419	0.290278
-12.401488	-3.210308	0.295283
-12.835738	-11.292135	0.300288
-12.877675	-7.799060	0.305293
-13.612637	2.611054	0.310298
-13.816580	-4.367902	0.315302
-14.132584	-3.489456	0.320307
-14.191258	-6.213744	0.325312
-14.389355	-2.569648	0.330317
-14.661368	-0.204792	0.335322
-14.952571	-8.375473	0.340326
-15.409838	0.409240	0.345331
-15.581661	-6.011595	0.350336
-15.541924	-14.607452	0.355341
-15.767100	-0.999544	0.360346
-15.720148	-6.647893	0.365350
-17.046524	-3.697053	0.370355
-17.047048	-2.358670	0.375360
-17.258196	-8.649955	0.380365
-17.437755	-7.318322	0.385370
-16.958254	-6.792312	0.390374
-17.357442	-8.599535	0.395379
-17.952311	-3.722673	0.400384
-18.246823	-9.127693	0.405389
-18.789632	-7.960609	0.410394
-18.637605	-7.712322	0.415398
-18.864421	2.959861	0.420403
-18.900376	-5.291943	0.425408
-19.399106	-4.315265	0.430413
-20.274398	-8.408067	0.435418
-20.042359	1.945445	0.440422
-20.195638	-3.794919	0.445427
-20.350134	-5.172243	0.450432
-20.302295	-2.297514	0.455437
-21.146817	7.810227	0.460442
-21.155997	2.433263	0.465446
-21.400498	1.927426	0.470451
-21.267993	-8.989363	0.475456
-21.538104	-6.118601	0.480461
-22.310903	1.079879	0.485466
-22.309450	-10.547209	0.490470
-22.843346	-2.509797	0.495475
-22.548073	-2.992640	0.500480
-23.005922	2.058908	0.505485
-23.873957	-0.854943	0.510490
-23.790778	-8.805871	0.515494
-24.112267	2.001368	0.520499
-24.216134	-0.007153	0.525504
-24.170680	-6.310169	0.530509
-24.834377	2.389830	0.535514
-25.245541	-2.677372	0.540518
-25.734564	0.800335	0.545523
-25.462875	-1.653011	0.550528
-25.757242	-7.538948	0.555533
-25.893607	-2.689635	0.560538
-25.816576	-12.506226	0.565542
-26.372234	5.820038	0.570547
-26.887356	1.218381	0.575552
-27.115275	-0.043034	0.580557
-27.413259	0.022661	0.585562
-27.407344	-8.514114	0.590566
-27.492056	-0.986847	0.595571
-27.769458	-6.258506	0.600576
-28.244413	-3.013959	0.605581
-28.807122	-2.536623	0.610586
-28.591497	-8.717605	0.615590
-28.944905	-9.573376	0.620595
-29.210110	-8.769329	0.625600
-29.930380	-9.172146	0.630605
-30.213726	1.100766	0.635610
-29.841115	-10.559165	0.640614
-30.348898	-6.866547	0.645619
-30.417254	-2.657482	0.650624
-30.057760	-6.105356	0.655629
-31.346375	0.468423	0.660634
-31.195786	-9.514720	0.665638
-31.937871	-11.967409	0.670643
-31.957279	-3.108934	0.675648
-31.925694	-2.272296	0.680653
-32.571704	-0.573344	0.685658
-32.050871	3.027709	0.690662
-32.148696	-8.267445	0.695667
-32.717543	-4.501983	0.700672
-33.097914	-8.909614	0.705677
-33.693454	-2.381156	0.710682
-33.611810	-11.347414	0.715686
-34.384973	-10.191692	0.720691
-34.414866	-5.248330	0.725696
-34.399279	-8.670793	0.730701
-34.360856	2.516654	0.735706
-34.553235	-13.816234	0.740710
-35.669464	0.725397	0.745715
-36.093213	-9.376564	0.750720
-36.311915	-4.808582	0.755725
-35.989987	-3.938341	0.760730
-35.940650	-5.569067	0.765734
-36.311849	-4.495309	0.770739
-36.629574	-7.612444	0.775744
-36.499092	-8.708550	0.780749
-37.462017	-4.495360	0.785754
-37.640756	-4.337617	0.790758
-37.754425	3.618135	0.795763
-37.985706	2.885599	0.800768
-37.827299	0.639829	0.805773
-38.928724	5.988372	0.810778
-39.189394	-1.392985	0.815782
-39.451073	0.324841	0.820787
-39.433401	1.739468	0.825792
-39.054353	2.271725	0.830797
-39.700526	7.131318	0.835802
-39.244737	-5.307284	0.840806
-39.668553	-0.026949	0.845811
-40.466310	-7.770242	0.850816
-40.612983	-9.313307	0.855821
-41.446717	4.064087	0.860826
-41.585052	-12.223485	0.865830
-42.039323	-4.372558	0.870835
-42.218451	-0.854822	0.875840
-42.074691	0.660272	0.880845
-42.547029	3.031207	0.885850
-42.104080	-4.121873	0.890854
-42.749112	-1.951672	0.895859
-42.719007	-1.804504	0.900864
-43.194997	-8.430779	0.905869
-43.654034	-1.123274	0.910874
-43.862493	-14.020942	0.915878
-44.048143	-11.827808	0.920883
-44.075684	-9.010873	0.925888
-44.122797	-7.595588	0.930893
-44.980962	-7.964141	0.935898
-44.937509	-16.709275	0.940902
-45.229485	-14.233724	0.945907
-45.531050	-3.948470	0.950912
-45.488363	-13.949505	0.955917
-46.092888	-3.319386	0.960922
-46.345419	-15.590047	0.965926
-46.771606	-5.323232	0.970931
-46.841497	-4.897804	0.975936
-47.080411	-6.432743	0.980941
-47.311776	-0.325180	0.985946
-47.001739	-5.954639	0.990950
-47.803105	1.947513	0.995955
-48.059371	-7.997191	1.000960
-47.824745	-5.031507	1.005965
-48.517181	-7.333786	1.010970
-49.257480	-18.373239	1.015974
-49.385696	-0.186725	1.020979
-49.694172	-7.171443	1.025984
-49.721465	-3.775575	1.030989
-49.814472	-3.023820	1.035994
-49.475858	-5.107998	1.040998
-49.776766	-0.628375	1.046003
-50.446046	-2.681180	1.051008
-50.866474	-5.630360	1.056013
-51.336454	-7.075310	1.061018
-51.084577	-12.018606	1.066022
-51.180381	-6.957349	1.071027
-51.884262	-4.151499	1.076032
-52.688384	1.795871	1.081037
-52.552220	2.397823	1.086042
-52.822287	-10.392117	1.091046
-52.846947	-8.186242	1.096051
-52.678125	-8.763169	1.101056
-52.900090	-13.720804	1.106061
-53.619519	-3.616851	1.111066
-54.072705	-4.099480	1.116070
-54.048646	-5.378228	1.121075
-54.440376	-4.788475	1.126080
-54.330988	-8.124394	1.131085
-54.382626	-5.588423	1.136090
-54.944683	-5.835692	1.141094
-55.689017	-6.611225	1.146099
-55.970431	-8.066738	1.151104
-55.884307	-4.774064	1.156109
-56.352507	-3.533246	1.161114
-55.860138	-8.555354	1.166118
-56.009010	-7.393045	1.171123
-56.962639	-8.923564	1.176128
-57.293855	-7.726356	1.181133
-57.540120	-8.260390	1.186138
-57.137723	-12.670446	1.191142
-57.412067	-4.237103	1.196147
-58.254392	-1.203914	1.201152
-58.264779	-13.601101	1.206157
-58.711075	-9.180958	1.211162
-58.579163	-19.388959	1.216166
-58.539580	-10.533406	1.221171
-59.888047	-7.860675	1.226176
-60.168759	-1.697924	1.231181
-60.224306	-7.001178	1.236186
-60.208540	-10.142091	1.241190
-60.499241	-2.234535	1.246195
-60.344215	-2.258803	1.251200
-60.454313	-11.071628	1.256205
-60.771306	-3.558588	1.261210
-61.376694	-6.551553	1.266214
-61.978550	-2.233584	1.271219
-62.200792	-1.037632	1.276224
-62.184271	2.031830	1.281229
-62.321968	1.230846	1.286234
-61.909113	-2.665155	1.291238
-62.529234	-6.427773	1.296243
-63.367823	2.046527	1.301248
-63.244501	-9.862245	1.306253
-63.552957	-1.183109	1.311258
-63.462263	-5.965108	1.316262
-64.020342	-11.540799	1.321267
-64.468137	-1.093425	1.326272
-64.664527	-2.907112	1.331277
-65.280996	10.496355	1.336282
-64.570857	-6.057046	1.341286
-65.000886	-0.253715	1.346291
-65.573537	-0.483505	1.351296
-66.283938	0.238440	1.356301
-66.572588	-4.088648	1.361306
-66.482444	-4.985444	1.366310
-66.858480	-5.059379	1.371315
-66.745445	-6.908894	1.376320
-66.500397	-14.322027	1.381325
-67.943526	-5.389171	1.386330
-67.431034	-9.104629	1.391334
-67.744329	-1.674426	1.396339
-67.800600	-2.734942	1.401344
-67.638172	-11.998596	1.406349
-68.818308	0.110615	1.411354
-68.801033	-8.839229	1.416358
-69.294068	-5.911390	1.421363
-69.106827	-6.462729	1.426368
-69.368474	-4.944225	1.431373
-69.370855	-0.963799	1.436378
-69.947255	-6.754920	1.441382
-70.109712	-2.423542	1.446387
-70.306475	-8.413354	1.451392
-70.802685	-10.281301	1.456397
-71.404823	-14.777566	1.461402
-71.616856	-6.309696	1.466406
-71.903566	-4.420267	1.471411
-71.880264	2.030209	1.476416
-71.810878	-10.547159	1.481421
-71.995073	-4.776022	1.486426
-72.350180	-10.440463	1.491430
-72.855385	-5.675728	1.496435
-73.230247	-14.937449	1.501440
-73.520785	0.404954	1.506445
-73.747428	-4.156478	1.511450
-73.558550	-8.846292	1.516454
-74.199591	-3.082665	1.521459
-74.633741	-4.650287	1.526464
-74.851602	-9.830030	1.531469
-74.844516	-0.760572	1.536474
-74.801811	-11.454475	1.541478
-75.048030	1.906789	1.546483
-75.799632	-4.125801	1.551488
-76.325939	-1.107326	1.556493
-76.718490	-11.011687	1.561498
-76.751283	-7.118246	1.566502
-76.738877	-2.899690	1.571507
-76.353151	-7.076180	1.576512
-76.296331	-4.819797	1.581517
-77.228958	-5.901184	1.586522
-77.314000	-6.036534	1.591526
-77.840588	-2.663672	1.596531
-78.479431	-10.919079	1.601536
-77.939710	-4.590653	1.606541
-78.964051	2.757976	1.611546
-79.227740	-2.338657	1.616550
-79.491038	-3.923559	1.621555
-79.688914	-6.167285	1.626560
-79.426167	-12.118365	1.631565
-79.438726	-0.650851	1.636570
-79.555383	-5.973003	1.641574
-80.310482	-2.187846	1.646579
-81.115158	-1.976316	1.651584
-80.944724	-8.827262	1.656589
-81.246881	-5.828092	1.661594
-80.887328	-4.647372	1.666598
-81.573001	-12.734087	1.671603
-82.091869	-6.546676	1.676608
-82.316136	-16.268593	1.681613
-82.809862	-11.676502	1.686618
-82.834163	-10.182534	1.691622
-82.413918	-5.996246	1.696627
-82.615736	-1.848527	1.701632
-83.328602	-6.795682	1.706637
-83.843307	-10.641253	1.711642
-84.071508	-16.350887	1.716646
-84.043254	-6.724762	1.721651
-84.244316	-5.158803	1.726656
-84.396680	-17.774185	1.731661
-85.002767	-0.348034	1.736666
-85.507617	-8.023320	1.741670
-85.871849	-3.536939	1.746675
-85.899075	-14.849473	1.751680
-85.530416	-7.877309	1.756685
-85.480974	-2.022557	1.761690
-86.384418	-11.410263	1.766694
-87.082483	-3.467351	1.771699
-87.021165	-7.210191	1.776704
-86.930275	-2.538859	1.781709
-87.247506	-3.473062	1.786714
-87.256227	-12.763680	1.791718
-88.015937	-15.352807	1.796723
-88.503703	-8.281250	1.801728
-88.562948	-3.811020	1.806733
-88.714302	-0.209051	1.811738
-88.770198	-8.657042	1.816742
-88.955309	-10.459839	1.821747
-88.967177	-2.947154	1.826752
-90.058722	-6.911149	1.831757
-90.160717	-4.012945	1.836762
-90.412034	-4.653754	1.841766
-90.323832	-10.909680	1.846771
-90.403715	-12.131012	1.851776
-90.481225	-18.098376	1.856781
-91.367676	-6.307272	1.861786
-91.659749	-12.933884	1.866790
-91.729239	-1.697899	1.871795
-91.804882	-8.181255	1.876800
-91.437038	-10.538935	1.881805
-92.408535	-10.513236	1.886810
-92.742596	-8.008943	1.891814
-92.957714	-8.981293	1.896819
-93.365964	-8.221269	1.901824
-93.322619	-15.267436	1.906829
-93.615169	-0.990913	1.911834
-93.789650	-1.096429	1.916838
-94.396213	-2.817369	1.921843
-94.896357	2.661589	1.926848
-94.534361	-7.098411	1.931853
-95.013444	-1.920149	1.936858
-94.922742	-9.106618	1.941862
-94.989635	-6.922600	1.946867
-95.500628	-4.403237	1.951872
-96.045059	-8.351719	1.956877
-96.300332	-6.856360	1.961882
-96.065589	0.478478	1.966886
-96.633559	-11.505469	1.971891
-96.809110	-9.465778	1.976896
-97.547707	-10.884452	1.981901
-98.134458	-9.315006	1.986906
-98.207367	-7.107899	1.991910
-97.721755	-1.400587	1.996915
-98.083289	-11.662356	2.006912
-97.694423	-8.907046	2.016909
-97.456612	1.563416	2.026906
-96.705005	-2.662982	2.036902
-96.478029	-0.370149	2.046899
-96.235401	-3.826207	2.056896
-95.253245	-1.448966	2.066893
-95.096935	-4.698260	2.076890
-94.290586	-9.519283	2.086886
-93.870770	-10.240759	2.096883
-93.758333	-9.703963	2.106880
-92.696050	-4.998253	2.116877
-92.581222	-11.174454	2.126874
-92.198254	-11.202739	2.136870
-91.170590	-11.328875	2.146867
-91.321327	-6.043451	2.156864
-90.051361	-8.884367	2.166861
-89.740564	-9.724978	2.176858
-89.839823	-9.905784	2.186854
-89.008962	-10.235502	2.196851
-88.445338	-7.789511	2.206848
-87.925889	-3.315525	2.216845
-87.480997	-5.628012	2.226842
-86.908243	-1.244742	2.236838
-85.733973	-4.618697	2.246835
-85.819981	-4.678035	2.256832
-85.764563	-0.473463	2.266829
-85.064764	-12.015756	2.276826
-84.301432	-7.171336	2.286822
-84.185221	-0.426189	2.296819
-83.015825	-1.537552	2.306816
-82.735209	-10.283496	2.316813
-82.574741	-0.782940	2.326810
-82.006421	-6.187560	2.336806
-81.267993	-11.210182	2.346803
-81.073901	-8.611254	2.356800
-80.400979	-6.955339	2.366797
-79.598782	-2.490810	2.376794
-79.697994	-4.923949	2.386790
-78.539031	-2.507885	2.396787
-78.143189	-9.114594	2.406784
-78.207846	-5.496263	2.416781
-77.355353	-10.549430	2.426778
-76.585722	-3.637405	2.436774
-76.507211	-10.178551	2.446771
-76.036980	-9.428552	2.456768
-75.222228	-10.709260	2.466765
-75.208154	-15.941499	2.476762
-74.185163	-5.036531	2.486758
-73.716211	-9.019064	2.496755
-73.580581	-8.672803	2.506752
-72.654104	-12.825228	2.516749
-72.265930	-12.233434	2.526746
-72.360857	-9.069695	2.536742
-71.382239	-10.540805	2.546739
-71.011816	-9.664293	2.556736
-70.294610	-9.741781	2.566733
-69.973414	-12.202779	2.576730
-69.373142	-12.068707	2.586726
-68.604620	-6.955833	2.596723
-68.506733	-3.920508	2.606720
-68.095905	-5.882363	2.616717
-67.232217	-12.834812	2.626714
-66.779670	-8.885704	2.636710
-66.332267	-10.970500	2.646707
-65.570023	-4.659203	2.656704
-65.354056	-5.402590	2.666701
-65.352923	-9.663449	2.676698
-64.612136	-10.473232	2.686694
-63.696761	-10.375861	2.696691
-62.785733	-12.102478	2.706688
-62.792812	-7.026465	2.716685
-62.485036	-10.758827	2.726682
-61.768570	-10.798184	2.736678
-60.971130	-8.908352	2.746675
-60.820221	-10.750284	2.756672
-60.836419	-9.559766	2.766669
-59.882065	-6.845542	2.776666
-59.552905	-6.516933	2.786662
-58.467440	-9.569691	2.796659
-58.241409	-8.087673	2.806656
-58.252460	0.850546	2.816653
-57.316348	5.924495	2.826650
-57.232798	-1.444249	2.836646
-55.993128	-1.454712	2.846643
-55.315759	-0.141616	2.856640
-55.308729	5.923720	2.866637
-55.371590	3.361338	2.876634
-54.237925	-2.616543	2.886630
-53.947410	1.782445	2.896627
-53.114346	-6.299289	2.906624
-52.843893	-7.735464	2.916621
-52.500616	-7.694172	2.926618
-51.339113	0.705525	2.936614
-50.944198	-4.367812	2.946611
-51.023962	-1.909705	2.956608
-50.658988	-4.662668	2.966605
-49.776140	-0.378667	2.976602
-49.560394	-10.096475	2.986598
-48.838928	-1.567641	2.996595
-48.263320	-8.677692	3.006592
-47.740440	-7.628662	3.016589
-47.181590	-2.695175	3.026586
-46.750371	-3.893610	3.036582
-46.394398	-9.033704	3.046579
-45.460113	-8.568659	3.056576
-45.306231	-0.223324	3.066573
-45.321678	-3.759322	3.076570
-44.135307	-5.487899	3.086566
-43.628101	-7.005520	3.096563
-43.482832	-9.999658	3.106560
-42.749470	-4.811578	3.116557
-42.495917	-7.002216	3.126554
-41.411799	-5.882732	3.136550
-40.903113	-10.989733	3.146547
-40.566326	-4.155601	3.156544
-40.589944	-5.095868	3.166541
-40.098194	0.690777	3.176538
-39.218622	-5.133247	3.186534
-38.801851	-6.614523	3.196531
-37.908830	-13.977047	3.206528
-37.655552	-0.569259	3.216525
-37.815949	-0.962235	3.226522
-36.991081	-2.824238	3.236518
-36.328884	-7.549810	3.246515
-35.262348	1.308266	3.256512
-34.872629	-0.396855	3.266509
-35.055032	-2.535025	3.276506
-34.800205	-2.527389	3.286502
-34.040305	-4.597792	3.296499
-33.004094	-1.009398	3.306496
-32.408391	2.476956	3.316493
-32.043322	-4.691975	3.326490
-31.780143	0.959422	3.336486
-31.589129	-1.785291	3.346483
-30.269472	-3.772337	3.356480
-30.175332	-3.514609	3.366477
-30.259404	-0.406422	3.376474
-29.231274	-0.377400	3.386470
-28.976658	-0.791053	3.396467
-27.780738	-2.730200	3.406464
-27.282390	-4.705768	3.416461
-26.966249	-2.715176	3.426458
-27.258778	3.365419	3.436454
-26.325608	-8.146919	3.446451
-25.423295	-1.113121	3.456448
-25.330642	-4.967002	3.466445
-25.122577	-4.423012	3.476442
-24.331788	-5.041053	3.486438
-23.954689	-2.727389	3.496435
-23.314554	-6.850786	3.506432
-22.904245	-5.220241	3.516429
-21.920339	-7.747062	3.526426
-21.470310	-1.988726	3.536422
-21.503051	-7.672970	3.546419
-20.586180	-6.726851	3.556416
-20.232305	0.158460	3.566413
-20.013279	1.346970	3.576410
-19.006670	-0.800102	3.586406
-18.823533	-1.300758	3.596403
-18.434879	-1.668888	3.606400
-17.264573	-4.022174	3.616397
-17.020271	-5.257846	3.626394
-16.811156	-4.004427	3.636390
-16.336925	-5.165251	3.646387
-15.848349	-3.648340	3.656384
-15.154798	-4.989248	3.666381
-14.303268	-4.343338	3.676378
-13.830146	0.378670	3.686374
-13.516795	-5.112712	3.696371
-13.709650	-2.497501	3.706368
-13.233739	0.944268	3.716365
-12.350712	0.055182	3.726362
-11.420082	3.001214	3.736358
-11.046375	-3.747750	3.746355
-11.077969	-0.346841	3.756352
-9.814590	-0.994578	3.766349
-9.692817	1.805756	3.776346
-9.830680	-2.670916	3.786342
-8.745785	0.697610	3.796339
-8.155263	-0.342050	3.806336
-7.454843	5.256681	3.816333
-7.089996	-0.515205	3.826330
-6.836184	-0.124103	3.836326
-6.295707	-3.322717	3.846323
-5.473544	-3.803119	3.856320
-5.427087	-0.534817	3.866317
-4.916913	9.829630	3.876314
-4.297241	15.178086	3.886310
-3.934661	19.537281	3.896307
-3.540755	24.407925	3.906304
-2.954145	40.890174	3.916301
-2.680055	38.978251	3.926298
-2.460110	54.909739	3.936294
-1.725597	66.914857	3.946291
-1.286082	83.698964	3.956288
-0.437016	102.715607	3.966285
0.000000	119.842495	3.971290
0.252311	120.169986	3.976294
0.354524	125.880473	3.981299
0.372334	128.744110	3.986304
0.369648	118.743779	3.991309
0.087385	133.199142	3.996314
0.375834	142.787751	4.001318
0.610736	148.752706	4.006323
0.806924	155.976597	4.011328
1.131473	148.509808	4.016333
0.790312	140.002029	4.021338
0.575157	120.657476	4.026342
0.497424	122.786261	4.031347
0.389798	133.417701	4.036352
0.869816	138.363469	4.041357
0.493505	142.440484	4.046362
0.653564	150.040197	4.051366
0.762640	154.256302	4.056371
1.028814	156.685553	4.061376
1.232496	145.488592	4.066381
0.884506	136.263702	4.071386
0.966186	138.196666	4.076390
0.746003	123.114542	4.081395
0.734859	132.604551	4.086400
0.620426	131.530992	4.091405
0.456952	130.699238	4.096410
0.587402	124.566357	4.101414
0.660684	137.286037	4.106419
1.091966	146.583346	4.111424
1.041436	149.448202	4.116429
0.981427	140.801458	4.121434
1.089271	138.683817	4.126438
0.621208	133.154082	4.131443
0.314767	147.258899	4.136448
1.061692	148.154310	4.141453
0.892484	151.493349	4.146458
0.764290	148.118694	4.151462
0.992365	152.075704	4.156467
0.853742	163.120149	4.161472
1.087201	156.740160	4.166477
1.146925	157.524940	4.171482
0.796177	156.820606	4.176486
0.932989	154.056172	4.181491
0.909037	161.270264	4.186496
1.188305	151.671834	4.191501
0.982723	153.304954	4.196506
1.048863	154.990414	4.201510
1.331392	154.319736	4.206515
1.046530	154.231511	4.211520
1.026465	153.026104	4.216525
0.865449	156.503068	4.221530
0.927624	148.738861	4.226534
0.855547	157.577195	4.231539
0.832620	156.517771	4.236544
1.396436	152.006453	4.241549
1.092263	151.487813	4.246554
1.057872	155.546060	4.251558
0.806217	156.847872	4.256563
1.305092	170.212749	4.261568
1.691975	178.191395	4.266573
1.026339	167.851976	4.271578
1.436478	171.372332	4.276582
1.635668	168.088750	4.281587
1.260368	152.758817	4.286592
1.171644	147.473367	4.291597
1.423922	151.088058	4.296602
0.866710	150.912790	4.301606
1.264633	164.489636	4.306611
1.290543	173.255678	4.311616
1.557687	181.468225	4.316621
1.911113	184.696908	4.321626
1.510673	166.865163	4.326630
1.402533	154.492660	4.331635
0.967243	153.792080	4.336640
1.804022	155.651028	4.341645
1.369933	167.782664	4.346650
1.243540	164.021739	4.351654
1.426524	172.120916	4.356659
1.675451	174.714226	4.361664
1.720475	175.719613	4.366669
1.501314	165.028662	4.371674
1.611726	152.197967	4.376678
1.337046	162.425321	4.381683
1.540179	168.635710	4.386688
1.575212	162.372231	4.391693
1.369159	173.313351	4.396698
1.873440	170.934273	4.401702
1.600803	173.644104	4.406707
1.441712	178.633072	4.411712
1.981257	171.385692	4.416717
1.530411	159.095356	4.421722
1.534989	158.813082	4.426726
1.771436	173.063816	4.431731
1.490316	162.914094	4.436736
1.861032	171.901361	4.441741
1.774627	183.219217	4.446746
1.526905	171.501334	4.451750
1.686448	179.708593	4.456755
1.589610	180.350223	4.461760
1.669455	176.512688	4.466765
1.725590	181.901377	4.471770
1.647781	178.601081	4.476774
1.818078	186.971176	4.481779
1.489192	191.461559	4.486784
1.961931	178.570911	4.491789
1.834898	182.526618	4.496794
1.742728	172.973719	4.501798
1.354673	177.147496	4.506803
1.304849	185.681797	4.511808
1.694429	181.185115	4.516813
1.435499	191.027197	4.521818
1.888424	188.153117	4.526822
2.137476	199.510173	4.531827
1.607573	203.933976	4.536832
1.979314	196.494574	4.541837
2.030342	208.021871	4.546842
2.104994	214.356812	4.551846
2.370798	197.787417	4.556851
1.686576	193.503272	4.561856
1.818328	184.339234	4.566861
1.948653	197.553065	4.571866
2.117260	207.372462	4.576870
2.152705	209.081719	4.581875
2.209183	206.706359	4.586880
2.030509	187.134550	4.591885
1.768483	200.805335	4.596890
2.163165	197.266487	4.601894
2.482538	197.795448	4.606899
1.957474	201.550927	4.611904
2.283374	184.089423	4.616909
2.204354	187.933204	4.621914
2.012336	180.243612	4.626918
2.148366	183.765790	4.631923
2.018499	193.818610	4.636928
2.316055	192.493830	4.641933
1.951393	204.592465	4.646938
2.072246	206.497152	4.651942
2.423217	207.986126	4.656947
2.240217	213.159187	4.661952
2.511646	207.013681	4.666957
1.858551	207.846873	4.671962
1.893916	202.421739	4.676966
2.315267	209.056705	4.681971
2.384757	212.197001	4.686976
2.590803	204.214071	4.691981
2.692688	216.163683	4.696986
2.439761	210.131970	4.701990
2.574773	201.100293	4.706995
1.963002	194.384478	4.712000
2.276931	197.647827	4.717005
2.222733	201.411789	4.722010
2.627818	196.377990	4.727014
2.527832	202.670686	4.732019
1.874606	208.917188	4.737024
2.077560	210.549578	4.742029
2.225113	216.559881	4.747034
2.275204	207.430772	4.752038
2.096933	213.874946	4.757043
2.316621	211.005768	4.762048
2.667612	204.945875	4.767053
2.335148	208.006777	4.772058
2.148420	207.975944	4.777062
2.535369	225.911132	4.782067
2.270453	238.282069	4.787072
2.686848	234.875856	4.792077
3.077223	229.439383	4.797082
2.635909	219.536196	4.802086
2.629445	209.368724	4.807091
2.465172	215.494324	4.812096
2.401510	207.287890	4.817101
2.343140	223.685631	4.822106
2.507762	234.394700	4.827110
2.956113	238.529192	4.832115
2.517409	234.779220	4.837120
2.809065	236.242688	4.842125
2.756093	245.922813	4.847130
2.452559	248.197725	4.852134
2.654887	238.854919	4.857139
2.680786	240.989627	4.862144
2.832356	234.030806	4.867149
2.453824	243.828380	4.872154
2.531906	227.424414	4.877158
2.635015	233.492307	4.882163
2.789427	243.807503	4.887168
2.753489	237.871500	4.892173
2.709230	243.642940	4.897178
2.642359	232.842664	4.902182
2.700708	228.654138	4.907187
2.360059	240.575025	4.912192
2.420381	237.806745	4.917197
2.993747	251.751647	4.922202
3.131477	260.028801	4.927206
2.896939	268.288355	4.932211
2.832672	268.586355	4.937216
3.229649	257.457117	4.942221
2.831123	259.177426	4.947226
3.036542	251.590051	4.952230
2.998639	259.454952	4.957235
2.796515	267.257000	4.962240
3.333085	258.241472	4.967245
2.814782	260.913876	4.972250
3.028053	261.870761	4.977254
2.853796	259.211999	4.982259
2.801235	255.622989	4.987264
2.817338	253.962645	4.992269
2.762503	261.789070	4.997274
3.114094	255.817652	5.002278
3.173410	260.639541	5.007283
2.761598	264.472204	5.012288
3.144954	256.338080	5.017293
2.973263	259.060582	5.022298
3.079582	257.420905	5.027302
3.006672	258.913021	5.032307
3.074140	266.742433	5.037312
3.076221	258.364320	5.042317
3.451611	263.158833	5.047322
3.165951	255.648400	5.052326
3.504308	255.117671	5.057331
3.065031	267.746907	5.062336
3.127122	256.505621	5.067341
3.233612	266.110151	5.072346
3.177973	257.519614	5.077350
3.148122	260.438197	5.082355
2.798582	266.535893	5.087360
3.300856	268.823761	5.092365
3.115772	287.816769	5.097370
3.497260	285.352509	5.102374
3.642255	283.605527	5.107379
3.511370	287.539714	5.112384
3.666128	283.003868	5.117389
3.342488	270.557479	5.122394
3.598021	263.806989	5.127398
3.486523	259.005976	5.132403
3.160277	266.365553	5.137408
3.281561	255.393410	5.142413
3.149078	264.241262	5.147418
3.549177	275.191877	5.152422
3.188617	284.660783	5.157427
2.922193	283.095324	5.162432
3.568128	283.221936	5.167437
3.742081	285.355599	5.172442
3.855736	286.853289	5.177446
3.598415	278.237393	5.182451
3.291289	283.831729	5.187456
3.600303	281.480067	5.192461
3.137814	285.602255	5.197466
3.475021	290.162307	5.202470
3.542233	292.711338	5.207475
3.380135	295.986013	5.212480
3.379867	285.656172	5.217485
3.385224	297.978475	5.222490
3.306347	294.880810	5.227494
3.667351	297.551493	5.232499
3.641452	309.945143	5.237504
3.994614	301.692340	5.242509
3.512178	307.086355	5.247514
3.253521	299.853253	5.252518
3.831357	314.091740	5.257523
3.805065	317.186949	5.262528
3.601516	316.892990	5.267533
3.765502	316.430709	5.272538
4.087232	315.469138	5.277542
3.850810	310.542148	5.282547
3.860747	319.927712	5.287552
4.065196	312.780236	5.292557
3.620278	312.872117	5.297562
3.692339	314.733839	5.302566
3.980350	319.200364	5.307571
3.924656	322.306508	5.312576
4.149757	318.057033	5.317581
3.962271	306.449849	5.322586
3.549786	301.325815	5.327590
3.556716	297.841373	5.332595
3.616238	321.563987	5.337600
3.595122	320.099298	5.342605
3.873132	320.536665	5.347610
3.765354	319.667701	5.352614
4.041360	315.100194	5.357619
4.264304	319.241548	5.362624
4.254228	314.794797	5.367629
4.111379	322.271198	5.372634
3.984273	318.004139	5.377638
4.145687	316.893676	5.382643
4.207719	323.363515	5.387648
4.130815	315.677975	5.392653
4.302330	327.407939	5.397658
3.867568	327.355855	5.402662
3.940021	321.352220	5.407667
3.735857	328.297214	5.412672
3.953936	311.270107	5.417677
3.792598	319.034148	5.422682
3.622789	316.918861	5.427686
3.977851	324.823462	5.432691
4.067855	328.134576	5.437696
4.320247	342.901816	5.442701
4.138177	347.498951	5.447706
4.292419	342.922041	5.452710
4.372709	339.055928	5.457715
3.987954	341.337250	5.462720
3.901457	341.679865	5.467725
4.305457	342.470824	5.472730
4.331824	349.465131	5.477734
4.387890	351.345182	5.482739
4.043245	347.650053	5.487744
4.402449	343.623176	5.492749
4.073858	338.716946	5.497754
3.901536	345.704416	5.502758
4.163913	348.656322	5.507763
4.139814	348.865770	5.512768
4.359326	342.706205	5.517773
4.251830	349.642389	5.522778
4.643381	345.294059	5.527782
4.299714	342.000586	5.532787
4.225428	351.608176	5.537792
4.588879	355.180178	5.542797
4.397480	359.123863	5.547802
4.178087	356.829673	5.552806
4.282497	356.003393	5.557811
4.054540	364.616310	5.562816
4.361580	370.506760	5.567821
4.827161	378.596556	5.572826
4.763692	372.791375	5.577830
4.539304	374.693224	5.582835
4.582128	384.820336	5.587840
4.803484	376.262275	5.592845
4.570294	356.072381	5.597850
4.232494	354.992675	5.602854
4.690580	364.554825	5.607859
4.986640	368.804961	5.612864
4.625468	360.825410	5.617869
4.560089	361.844943	5.622874
4.293383	361.051499	5.627878
4.817802	367.335008	5.632883
4.552868	374.583779	5.637888
4.880561	374.573588	5.642893
4.658524	367.268280	5.647898
4.827498	371.636408	5.652902
4.859304	375.690660	5.657907
4.685916	375.581805	5.662912
4.941409	367.840998	5.667917
4.765662	374.382914	5.672922
4.312070	375.725872	5.677926
4.687896	366.564629	5.682931
3.894525	377.790890	5.687936
4.397144	381.540415	5.692941
4.894062	376.950935	5.697946
4.889838	368.953420	5.702950
4.926985	369.621521	5.707955
4.885369	371.178348	5.712960
5.033632	361.182705	5.717965
4.908670	363.995981	5.722970
5.010017	371.443632	5.727974
5.543093	365.136850	5.732979
4.889975	375.009157	5.737984
4.944041	372.308276	5.742989
4.910019	377.559285	5.747994
4.688276	374.170770	5.752998
4.745078	371.577032	5.758003
4.603464	379.157670	5.763008
4.668970	379.324604	5.768013
4.907966	374.538249	5.773018
5.307915	377.212333	5.778022
5.173281	376.625992	5.783027
4.773797	374.891542	5.788032
4.848064	372.557667	5.793037
4.920968	387.324592	5.798042
5.055757	400.841605	5.803046
5.305805	406.997269	5.808051
4.979124	410.285096	5.813056
5.221633	399.974099	5.818061
5.120245	402.846964	5.823066
5.203025	405.586567	5.828070
5.309306	404.025978	5.833075
5.135323	406.179369	5.838080
5.305255	408.202942	5.843085
5.276513	413.193698	5.848090
5.130163	410.935514	5.853094
5.724337	405.381633	5.858099
5.155539	394.023968	5.863104
4.784594	380.914178	5.868109
5.040853	393.099156	5.873114
5.273799	404.275363	5.878118
5.062841	405.064600	5.883123
4.923493	407.253694	5.888128
5.288587	399.818414	5.893133
5.238996	400.588694	5.898138
5.159098	402.537512	5.903142
5.110611	396.378789	5.908147
5.229937	404.345672	5.913152
5.255703	397.950681	5.918157
5.200082	409.064534	5.923162
5.196885	404.591372	5.928166
5.390944	403.637145	5.933171
5.464955	411.041639	5.938176
5.793432	413.543423	5.943181
5.643851	399.721871	5.948186
5.542608	409.384337	5.953190
5.744762	399.965542	5.958195
5.221117	406.872035	5.963200
5.323309	401.259195	5.968205
5.331181	398.894589	5.973210
5.213787	408.243200	5.978214
5.866333	416.408125	5.983219
5.537073	414.767076	5.988224
5.091242	406.376813	5.993229
5.670865	417.910012	5.998234
5.566190	418.774348	6.003238
5.681678	415.535474	6.008243
5.342857	406.837369	6.013248
5.532925	416.441541	6.018253
5.590472	408.924726	6.023258
5.301165	410.846242	6.028262
5.588966	418.097015	6.033267
5.772183	419.729354	6.038272
5.377475	407.797057	6.043277
5.450101	401.663650	6.048282
5.507632	404.907097	6.053286
5.889483	405.372489	6.058291
5.478848	413.276875	6.063296
5.533719	407.035513	6.068301
5.897484	405.048591	6.073306
5.625473	402.202638	6.078310
5.752529	397.930539	6.083315
5.442222	405.803383	6.088320
5.314305	398.005574	6.093325
5.608327	393.457372	6.098330
5.394895	403.915720	6.103334
5.277116	396.869320	6.108339
5.302667	396.482514	6.113344
5.368499	397.500473	6.118349
5.495598	406.228627	6.123354
5.535604	408.259902	6.128358
5.645435	398.096248	6.133363
5.328583	410.048321	6.138368
5.741199	403.912264	6.143373
5.780606	406.712449	6.148378
5.618365	416.064927	6.153382
5.640445	408.243612	6.158387
5.638575	409.914441	6.163392
5.436131	409.123582	6.168397
5.706594	398.052046	6.173402
5.098925	412.938281	6.178406
5.829432	408.084397	6.183411
5.181991	406.170489	6.188416
5.171221	406.115250	6.193421
5.535774	409.633306	6.198426
5.431459	411.279056	6.203430
5.790996	405.518322	6.208435
5.686399	413.735437	6.213440
5.591187	411.978620	6.218445
5.596259	406.203820	6.223450
5.451356	406.413213	6.228454
5.636129	403.647555	6.233459
5.647998	410.669467	6.238464
5.521981	405.937130	6.243469
5.643987	407.901771	6.248474
5.516620	403.723320	6.253478
5.855698	402.404676	6.258483
5.548198	408.097188	6.263488
5.680659	406.959617	6.268493
5.585720	404.658576	6.273498
5.637474	414.948827	6.278502
5.738407	404.128482	6.283507
5.542521	420.690323	6.288512
5.660307	406.633879	6.293517
5.659296	409.161977	6.298522
5.358435	402.220193	6.303526
5.565420	400.947556	6.308531
5.528449	413.599284	6.313536
5.798793	407.700660	6.318541
5.678549	403.438832	6.323546
5.416032	397.269350	6.328550
5.403460	396.097554	6.333555
5.538933	407.175137	6.338560
5.631824	405.357210	6.343565
5.611250	406.243171	6.348570
5.377515	407.096090	6.353574
5.592349	404.930016	6.358579
5.210322	410.121662	6.363584
5.371181	409.479530	6.368589
5.447714	402.611497	6.373594
5.576676	407.615509	6.378598
5.307141	397.457510	6.383603
5.462326	412.455181	6.388608
5.616035	401.651880	6.393613
5.688981	406.895629	6.398618
5.744590	404.112242	6.403622
5.637348	402.170644	6.408627
5.635848	407.606397	6.413632
5.589549	393.638949	6.418637
5.656241	393.581065	6.423642
5.307920	388.649438	6.428646
5.129773	383.896800	6.433651
5.337437	399.718330	6.438656
5.647662	398.600365	6.443661
5.478555	409.238438	6.448666
5.228909	410.587410	6.453670
5.685413	397.139148	6.458675
5.521752	413.623165	6.463680
5.482303	403.764480	6.468685
5.431853	409.043383	6.473690
5.431621	407.651348	6.478694
5.660987	402.600730	6.483699
5.586065	405.111933	6.488704
5.665978	402.429145	6.493709
5.640481	401.572596	6.498714
5.446626	403.558252	6.503718
5.888274	400.084773	6.508723
5.525179	413.970879	6.513728
5.536141	406.072211	6.518733
5.453893	405.423876	6.523738
5.492563	404.547781	6.528742
5.671874	405.623893	6.533747
5.649091	410.926936	6.538752
5.272590	393.050084	6.543757
5.713190	392.743784	6.548762
5.433141	400.823862	6.553766
5.653174	394.699000	6.558771
5.443381	391.011207	6.563776
5.540044	387.873367	6.568781
5.499068	384.931104	6.573786
5.392001	393.151760	6.578790
5.604484	395.045274	6.583795
5.518321	402.228080	6.588800
5.486173	397.509513	6.593805
5.457117	394.758375	6.598810
5.608637	402.710722	6.603814
5.695177	397.502145	6.608819
5.348184	380.902040	6.613824
5.342616	386.107463	6.618829
5.644228	397.921496	6.623834
5.519410	401.949673	6.628838
5.701550	396.510975	6.633843
5.054942	392.717612	6.638848
5.271940	394.806577	6.643853
5.497694	395.691909	6.648858
5.374995	404.709145	6.653862
5.744978	403.161025	6.658867
5.663329	404.104012	6.663872
5.609346	410.440196	6.668877
5.499639	401.196816	6.673882
5.900598	402.927919	6.678886
5.352501	389.646556	6.683891
5.672036	394.797880	6.688896
5.684352	395.346483	6.693901
5.339273	372.987882	6.698906
5.254434	383.745618	6.703910
5.760662	387.149720	6.708915
5.606131	386.446270	6.713920
5.385158	379.368588	6.718925
5.464903	384.747311	6.723930
5.206454	397.693164	6.728934
5.992195	396.737983	6.733939
5.677745	389.295282	6.738944
5.630093	384.683553	6.743949
5.315709	385.476338	6.748954
5.016464	380.239623	6.753958
5.564055	382.023682	6.758963
5.610276	398.661467	6.763968
5.492959	399.916937	6.768973
5.890545	396.377595	6.773978
5.400182	385.858721	6.778982
5.601776	373.266688	6.783987
5.547719	384.041749	6.788992
5.411148	377.029939	6.793997
5.505474	372.342183	6.799002
5.525004	387.215551	6.804006
5.570852	387.648165	6.809011
5.699371	386.027145	6.814016
5.295713	378.905317	6.819021
5.423719	383.245064	6.824026
5.452669	396.231311	6.829030
5.828818	402.091961	6.834035
5.632932	389.900726	6.839040
5.420975	390.111134	6.844045
5.490117	381.077032	6.849050
5.168128	389.141529	6.854054
5.568871	391.087806	6.859059
5.499705	396.891673	6.864064
5.583162	404.285192	6.869069
5.544709	394.581385	6.874074
5.408407	403.123011	6.879078
5.872319	404.043796	6.884083
5.406792	395.991992	6.889088
5.641912	388.874483	6.894093
5.475592	385.357056	6.899098
5.327734	380.106113	6.904102
5.440263	381.069297	6.909107
5.278945	387.716527	6.914112
5.728965	399.039059	6.919117
5.706672	407.224292	6.924122
5.438741	397.078697	6.929126
5.575735	388.805938	6.934131
5.555211	399.246714	6.939136
5.821023	395.332537	6.944141
5.417093	382.531643	6.949146
5.338357	384.515079	6.954150
5.023761	383.801906	6.959155
5.541236	397.110255	6.964160
5.783987	393.183873	6.969165
5.956916	398.228451	6.974170
5.322671	386.444434	6.979174
5.559913	382.806827	6.984179
4.781825	382.773734	6.989184
5.484241	399.767464	6.994189
5.837991	404.508458	6.999194
5.812344	408.457821	7.004198
5.417186	403.432286	7.009203
5.523421	401.106053	7.014208
5.490683	400.570187	7.019213
5.277915	400.043545	7.024218
5.459371	407.772898	7.029222
5.747857	397.347128	7.034227
5.509335	408.201727	7.039232
5.704950	407.785110	7.044237
5.556637	398.721793	7.049242
5.415232	396.228711	7.054246
5.661876	392.026464	7.059251
5.339200	395.025752	7.064256
5.750682	396.093961	7.069261
5.468817	388.067169	7.074266
5.497314	395.735059	7.079270
5.622862	374.093680	7.084275
5.436561	380.713184	7.089280
5.320794	375.435067	7.094285
5.715870	394.296158	7.099290
5.325135	394.800341	7.104294
5.605444	399.226963	7.109299
5.536257	397.776128	7.114304
5.337678	399.341731	7.119309
5.242063	406.329861	7.124314
5.694696	407.062583	7.129318
5.509775	405.987395	7.134323
5.747876	400.416538	7.139328
5.424354	393.522602	7.144333
5.471969	390.420920	7.149338
5.490202	398.017651	7.154342
5.403472	400.970479	7.159347
5.633716	403.389575	7.164352
5.321143	399.702065	7.169357
5.860241	396.159534	7.174362
5.149515	400.656010	7.179366
5.534336	400.329975	7.184371
5.593156	408.290521	7.189376
5.737436	406.689176	7.194381
5.540577	409.747848	7.199386
5.298843	407.716588	7.204390
5.538872	407.302504	7.209395
5.611620	403.931119	7.214400
5.598875	399.886575	7.219405
5.789932	402.362432	7.224410
5.425881	397.132702	7.229414
5.321562	387.198766	7.234419
5.647499	395.209206	7.239424
5.857252	398.916034	7.244429
5.723574	386.762513	7.249434
5.535283	390.493739	7.254438
5.542201	375.875706	7.259443
5.341999	386.265530	7.264448
5.291492	377.924075	7.269453
5.457685	381.419419	7.274458
5.337446	384.013652	7.279462
5.885303	381.406250	7.284467
5.749115	382.854506	7.289472
5.535954	382.897419	7.294477
5.589176	372.872367	7.299482
5.687274	380.810927	7.304486
5.592935	379.240644	7.309491
5.181303	385.278505	7.314496
5.117486	387.250112	7.319501
5.354731	384.463579	7.324506
5.614437	400.270628	7.329510
5.818785	387.535780	7.334515
5.620345	388.177518	7.339520
5.254287	381.600308	7.344525
5.378996	379.875478	7.349530
5.489122	375.128296	7.354534
5.705516	378.856227	7.359539
5.332432	387.188164	7.364544
5.372159	380.765681	7.369549
5.466320	382.630275	7.374554
5.759344	400.036174	7.379558
5.399299	389.370325	7.384563
5.330916	384.167042	7.389568
5.517912	399.055310	7.394573
5.892050	396.921227	7.399578
5.135548	389.332645	7.404582
5.439790	387.089289	7.409587
5.881937	400.425262	7.414592
5.724138	393.169992	7.419597
5.722851	379.942170	7.424602
5.345930	383.503628	7.429606
5.903274	378.227617	7.434611
5.440396	382.903561	7.439616
5.406025	381.985125	7.444621
5.493921	380.288210	7.449626
5.460914	384.795559	7.454630
5.777557	386.289927	7.459635
5.501584	388.794663	7.464640
5.316218	383.888127	7.469645
5.405119	373.313303	7.474650
5.508029	378.065117	7.479654
5.561320	375.411815	7.484659
5.587713	384.285455	7.489664
5.588084	380.615357	7.494669
5.557602	385.438695	7.499674
5.501111	386.061355	7.504678
5.502502	385.070876	7.509683
5.477218	392.158715	7.514688
5.241281	382.824389	7.519693
5.629885	380.726007	7.524698
5.163027	384.564155	7.529702
5.226813	392.463804	7.534707
5.951489	400.560471	7.539712
5.536921	399.809176	7.544717
5.862548	387.839961	7.549722
5.578610	393.614201	7.554726
5.759997	385.176296	7.559731
5.656464	396.199568	7.564736
5.563042	391.506421	7.569741
5.386185	373.658421	7.574746
5.358704	377.199929	7.579750
5.675554	375.062169	7.584755
5.460303	384.650733	7.589760
5.203254	388.573071	7.594765
5.202556	382.321442	7.599770
5.461747	388.643351	7.604774
5.332299	389.271114	7.609779
5.451961	398.070034	7.614784
5.505634	409.242695	7.619789
5.871115	410.049185	7.624794
5.592764	396.494592	7.629798
5.511012	384.984689	7.634803
5.342606	390.573141	7.639808
5.672558	406.862750	7.644813
5.977107	397.355143	7.649818
5.152518	395.051364	7.654822
5.219275	381.986892	7.659827
5.590091	396.153474	7.664832
5.660118	386.635161	7.669837
5.541963	385.062282	7.674842
5.492721	380.627979	7.679846
5.289423	382.833417	7.684851
5.635308	392.789660	7.689856
5.575686	396.026150	7.694861
5.310269	389.006049	7.699866
5.537035	402.458030	7.704870
5.896969	398.048201	7.709875
5.760556	385.784374	7.714880
4.936959	382.357275	7.719885
5.398857	384.512275	7.724890
5.576491	404.606544	7.729894
5.866483	395.246757	7.734899
5.718633	390.622252	7.739904
5.424200	378.977992	7.744909
5.655824	379.710538	7.749914
5.505817	382.404351	7.754918
5.616478	384.313818	7.759923
5.248086	372.962732	7.764928
5.380634	387.745624	7.769933
5.474796	371.797764	7.774938
5.312486	383.434532	7.779942
5.503977	397.271697	7.784947
5.444758	403.994688	7.789952
5.392473	405.432964	7.794957
5.522605	403.159935	7.799962
5.266668	409.151262	7.804966
6.020757	405.198546	7.809971
5.790934	403.804517	7.814976
5.328728	392.332073	7.819981
5.350921	384.928378	7.824986
5.514571	393.508426	7.829990
5.677924	405.258703	7.834995
5.728392	398.597242	7.840000
5.398583	388.398070	7.845005
5.424631	383.369822	7.850010
5.219968	400.964434	7.855014
5.837182	404.262562	7.860019
5.536687	392.941956	7.865024
5.620871	398.452869	7.870029
5.704317	386.559566	7.875034
5.456743	385.478377	7.880038
5.422261	380.921536	7.885043
5.435945	384.099081	7.890048
5.109075	381.540144	7.895053
5.519091	392.407018	7.900058
5.449683	407.705638	7.905062
5.627226	402.663140	7.910067
5.707751	406.909088	7.915072
5.614058	401.257335	7.920077
5.687435	387.185717	7.925082
5.131777	392.246371	7.930086
5.462363	400.828741	7.935091
5.834349	407.076034	7.940096
5.344273	398.771804	7.945101
5.358479	390.391729	7.950106
5.369217	402.466481	7.955110
5.728059	406.678315	7.960115
5.364258	402.881768	7.965120
5.513598	406.180435	7.970125
5.483097	411.449103	7.975142
5.439987	410.212503	7.980160
5.792081	407.888353	7.985178
5.617780	413.914825	7.990195
5.375841	415.458062	7.995213
5.657416	415.912581	8.000230
5.689580	413.944669	8.005248
5.659789	406.400732	8.010266
5.447045	394.713526	8.015283
5.475610	406.148771	8.020301
5.540310	403.743420	8.025318
5.504240	401.480089	8.030336
5.275558	409.471663	8.035354
5.579315	411.790928	8.040371
5.700575	405.845396	8.045389
5.694378	399.055153	8.050406
5.598941	409.370593	8.055424
5.467049	404.632365	8.060442
5.555161	396.921638	8.065459
5.591254	408.497715	8.070477
5.865542	411.755709	8.075494
5.525968	409.098121	8.080512
5.912449	403.063698	8.085530
5.738474	406.941031	8.090547
5.616710	413.407391	8.095565
5.873312	415.437402	8.100582
5.370506	404.297406	8.105600
5.694379	408.118825	8.110618
5.725539	418.859401	8.115635
5.835512	413.871837	8.120653
5.953269	401.022008	8.125670
5.758807	397.931434	8.130688
5.420698	382.713628	8.135706
5.501088	386.809875	8.140723
5.535294	400.232372	8.145741
5.863118	395.939665	8.150758
5.931726	409.688135	8.155776
5.663224	399.937844	8.160794
5.773242	392.078520	8.165811
5.299141	399.505789	8.170829
5.370833	406.017575	8.175846
5.617990	413.880947	8.180864
5.835953	413.786859	8.185882
5.587523	419.111740	8.190899
5.591857	422.077520	8.195917
5.719225	417.614245	8.200934
5.779124	419.245889	8.205952
5.793395	421.815639	8.210970
6.206312	408.070653	8.215987
5.798598	422.480739	8.221005
5.806982	417.348147	8.226022
5.750602	425.527324	8.231040
5.783016	418.563768	8.236058
5.750664	408.650239	8.241075
5.684151	412.911520	8.246093
5.611973	415.447477	8.251110
5.892564	406.740918	8.256128
5.933710	411.206235	8.261146
6.084921	404.858383	8.266163
6.014603	403.673383	8.271181
5.876412	404.256786	8.276198
5.744532	402.702738	8.281216
5.696271	408.984013	8.286234
6.027377	417.604244	8.291251
5.734594	408.473129	8.296269
5.796009	403.862403	8.301286
5.938024	397.714808	8.306304
5.823214	411.460460	8.311322
6.143850	411.485984	8.316339
5.788487	419.645732	8.321357
5.629410	420.478560	8.326374
5.654245	416.902346	8.331392
5.864007	407.099206	8.336410
5.626328	409.111987	8.341427
5.628123	413.091168	8.346445
5.647014	414.552514	8.351462
5.929676	411.762719	8.356480
5.595477	406.062117	8.361498
5.852219	407.170617	8.366515
5.367267	410.616997	8.371533
5.858703	417.473272	8.376550
6.057385	424.264966	8.381568
5.777266	446.951636	8.386586
5.962540	438.610289	8.391603
5.820245	446.758756	8.396621
5.983994	441.658618	8.401638
5.984771	439.540987	8.406656
5.921945	443.063243	8.411674
6.185186	441.447283	8.416691
5.737025	441.940400	8.421709
6.214922	431.356781	8.426726
6.173141	442.014125	8.431744
6.140997	439.175821	8.436762
5.990607	429.056715	8.441779
5.792337	428.444024	8.446797
6.429596	433.017916	8.451814
6.582318	421.721551	8.456832
5.747692	421.012906	8.461850
6.226954	408.343114	8.466867
5.626229	421.177149	8.471885
5.902041	414.109187	8.476902
6.043147	415.131665	8.481920
6.071692	420.400527	8.486938
6.273092	414.480305	8.491955
5.952773	418.472087	8.496973
5.679018	422.223047	8.501990
5.911681	432.322992	8.507008
6.059394	439.820107	8.512026
6.200243	439.214241	8.517043
5.992261	444.542260	8.522061
6.400187	446.558032	8.527078
6.244667	441.132378	8.532096
5.989022	440.979953	8.537114
6.492865	429.660127	8.542131
5.875804	425.083117	8.547149
6.296379	415.925434	8.552166
6.180060	415.353551	8.557184
5.868650	425.283121	8.562202
6.143274	424.659451	8.567219
5.613851	447.274730	8.572237
6.324921	446.980305	8.577255
6.139943	444.181726	8.582272
5.735882	444.866748	8.587290
6.263323	444.348632	8.592307
6.257197	444.264408	8.597325
6.253055	448.774700	8.602343
6.350357	445.373317	8.607360
6.061409	445.478573	8.612378
6.375409	439.941486	8.617395
6.593287	444.085632	8.622413
6.173740	447.916244	8.627431
6.257626	440.098863	8.632448
6.011603	440.822239	8.637466
6.166389	436.099045	8.642483
5.803326	448.315197	8.647501
5.738857	442.067396	8.652519
6.174505	437.865082	8.657536
5.910659	446.622726	8.662554
6.274406	440.471933	8.667571
5.930617	444.959701	8.672589
6.366575	444.203455	8.677607
6.369195	448.031037	8.682624
5.993234	440.241525	8.687642
6.351172	441.854877	8.692659
6.174154	445.824212	8.697677
6.108052	439.630316	8.702695
6.133512	444.221175	8.707712
6.361788	459.030257	8.712730
6.446383	458.142871	8.717747
6.667487	465.893584	8.722765
6.595603	449.220214	8.727783
6.425633	446.154197	8.732800
6.113754	443.110415	8.737818
6.568070	437.743846	8.742835
6.170688	449.466762	8.747853
6.357855	446.972790	8.752871
6.310234	433.138997	8.757888
6.275113	431.118509	8.762906
6.366941	431.388165	8.767923
6.376993	439.184558	8.772941
6.346424	440.473775	8.777959
6.540359	444.990900	8.782976
5.976460	446.237449	8.787994
6.431563	440.365830	8.793011
6.497365	457.800736	8.798029
6.378941	466.147442	8.803047
6.613561	460.992013	8.808064
6.409379	457.435895	8.813082
6.684287	446.612674	8.818099
6.490792	443.297880	8.823117
6.355234	441.823299	8.828135
6.201872	434.863598	8.833152
6.304247	443.361890	8.838170
6.662933	452.470120	8.843187
6.564472	454.063463	8.848205
6.281970	449.623375	8.853223
6.722520	458.305372	8.858240
6.069150	457.214878	8.863258
6.400240	450.456975	8.868275
6.447451	456.918967	8.873293
6.369372	465.906289	8.878311
6.420172	463.048674	8.883328
6.291019	463.747427	8.888346
6.712547	455.681479	8.893363
6.592905	464.751051	8.898381
6.444837	466.465777	8.903399
6.599880	456.093674	8.908416
6.673206	460.408794	8.913434
6.571057	453.968078	8.918451
6.379647	465.103314	8.923469
6.482075	463.436810	8.928487
6.604277	456.891513	8.933504
6.674758	463.258344	8.938522
6.566397	467.529350	8.943539
6.805444	463.367301	8.948557
6.606570	466.529027	8.953575
6.826678	466.213698	8.958592
6.647085	466.983470	8.963610
6.838404	463.463213	8.968627
6.498853	473.813783	8.973645
6.579165	475.499038	8.978663
6.530894	465.105137	8.983680
6.553878	467.155978	8.988698
6.675166	466.079807	8.993715
6.386482	462.660004	8.998733
6.471934	467.121549	9.003751
6.523139	460.672581	9.008768
6.549967	464.237599	9.013786
6.584352	455.900951	9.018803
6.299076	468.139642	9.023821
6.504633	466.747312	9.028839
7.053723	468.523219	9.033856
6.413060	463.845756	9.038874
6.709639	458.907836	9.043891
6.833244	459.832073	9.048909
6.319358	462.500360	9.053927
6.688015	459.157444	9.058944
6.444137	462.436674	9.063962
6.576066	462.763163	9.068979
7.005102	478.850459	9.073997
6.799569	489.337829	9.079015
6.862518	461.755834	9.084032
6.687088	462.761638	9.089050
6.632487	462.460949	9.094067
7.145687	457.470155	9.099085
6.472778	464.205924	9.104103
6.930158	473.686862	9.109120
7.166755	476.991798	9.114138
6.739274	471.220585	9.119155
6.554049	471.697752	9.124173
6.709528	462.165017	9.129191
6.975688	463.275201	9.134208
6.721069	470.914261	9.139226
6.991228	474.299145	9.144243
7.205129	468.206534	9.149261
6.735955	461.495119	9.154279
6.994868	452.056636	9.159296
6.567985	458.359382	9.164314
6.615955	461.163697	9.169331
6.725922	465.820215	9.174349
6.597409	476.579531	9.179367
6.523217	492.988682	9.184384
6.784698	495.109455	9.189402
6.554022	483.112577	9.194419
6.772238	484.441712	9.199437
6.548162	486.641718	9.204455
6.834658	482.822523	9.209472
6.541090	488.741475	9.214490
6.922548	490.190200	9.219507
6.857075	484.665218	9.224525
6.653785	485.530223	9.229543
7.141615	497.890799	9.234560
6.922424	496.956336	9.239578
7.049695	495.042940	9.244595
7.147477	482.975664	9.249613
6.783484	488.489085	9.254631
7.310319	487.904791	9.259648
7.032866	495.623179	9.264666
6.993491	490.766291	9.269683
6.991376	481.804190	9.274701
6.948773	489.182823	9.279719
7.153284	492.025731	9.284736
6.844777	483.518734	9.289754
6.985949	484.837850	9.294771
6.882607	476.074648	9.299789
7.098115	480.465326	9.304807
6.920784	489.338823	9.309824
6.788858	497.722374	9.314842
7.441032	505.859998	9.319859
7.074250	495.332948	9.324877
7.078824	498.248209	9.329895
6.923907	483.695889	9.334912
7.111227	502.512971	9.339930
7.381726	503.079680	9.344947
7.187163	487.987615	9.349965
7.137243	488.383622	9.354983
7.007805	487.296242	9.360000
6.799758	494.249520	9.365018
7.160067	498.402920	9.370035
7.480321	504.544438	9.375053
7.031115	500.487061	9.380071
6.967269	491.279008	9.385088
7.068704	495.450878	9.390106
7.133348	508.994920	9.395123
7.477251	511.929600	9.400141
6.968078	510.090676	9.405159
7.504997	512.240878	9.410176
7.204966	504.972771	9.415194
6.926248	491.894664	9.420211
7.049439	500.923051	9.425229
7.125368	513.086245	9.430247
7.072381	504.633875	9.435264
7.273208	502.431244	9.440282
7.084069	509.450993	9.445299
7.172493	513.318793	9.450317
6.996238	517.045028	9.455335
7.426548	511.322438	9.460352
7.076083	510.967119	9.465370
7.167620	510.107045	9.470387
7.242308	505.276463	9.475405
7.162691	511.130342	9.480423
7.214560	507.635081	9.485440
7.545317	520.168606	9.490458
7.472356	512.924878	9.495475
7.311426	513.180489	9.500493
7.289793	519.069467	9.505511
7.436925	516.174659	9.510528
7.468042	519.082610	9.515546
7.270011	530.187365	9.520563
7.552928	521.328908	9.525581
7.254007	525.538267	9.530599
6.908172	521.701374	9.535616
7.465279	514.295809	9.540634
7.212182	517.390301	9.545651
7.550161	510.344119	9.550669
7.244595	520.566315	9.555687
7.125254	521.544399	9.560704
7.331967	516.986617	9.565722
7.118828	519.140732	9.570739
7.492005	516.393544	9.575757
7.636034	516.064888	9.580775
7.310572	518.564805	9.585792
7.515883	509.535477	9.590810
7.327175	519.332264	9.595827
7.449721	514.882344	9.600845
7.376648	525.200659	9.605863
7.639131	518.469259	9.610880
7.622173	513.296428	9.615898
7.049733	519.420030	9.620915
7.298082	520.624526	9.625933
7.029078	520.221729	9.630951
7.333208	520.300332	9.635968
7.308101	522.008421	9.640986
7.499770	533.841070	9.646003
7.676064	537.900235	9.651021
7.576994	532.150129	9.656039
7.214852	538.026193	9.661056
7.322158	542.654746	9.666074
7.857470	547.806375	9.671091
7.847208	546.362647	9.676109
7.564138	533.638641	9.681127
7.597858	524.491023	9.686144
7.369607	524.552055	9.691162
7.857767	521.275611	9.696179
7.816983	520.306882	9.701197
7.725524	519.667984	9.706215
7.538869	518.936705	9.711232
7.703022	520.309027	9.716250
7.120046	524.603917	9.721267
7.403941	523.846248	9.726285
7.842895	521.814587	9.731303
8.078109	514.191214	9.736320
7.780208	514.218978	9.741338
7.737172	519.038338	9.746355
8.199781	518.066475	9.751373
7.402087	529.091617	9.756391
7.385895	524.527733	9.761408
7.750120	513.144523	9.766426
7.273643	515.683880	9.771443
7.713515	517.593669	9.776461
7.766549	514.764098	9.781479
7.606259	514.382138	9.786496
7.586415	514.767121	9.791514
7.577772	517.147971	9.796531
7.829631	519.039882	9.801549
7.926140	517.225978	9.806567
7.945224	520.871115	9.811584
7.581779	519.290223	9.816602
7.308899	523.855262	9.821619
7.633920	516.826887	9.826637
7.448561	526.774632	9.831655
7.643785	539.629207	9.836672
8.051856	544.358959	9.841690
8.262268	556.589473	9.846707
7.906760	537.637786	9.851725
7.754328	527.316973	9.856743
7.296825	522.942155	9.861760
7.710737	524.549900	9.866778
7.695950	549.707144	9.871795
7.749240	550.645559	9.876813
7.700671	547.910797	9.881831
7.675442	551.575507	9.886848
7.948661	538.783272	9.891866
7.822094	540.513571	9.896883
8.076302	541.988550	9.901901
8.188843	542.996576	9.906919
7.899500	543.458500	9.911936
7.967318	541.238834	9.916954
8.018522	547.207927	9.921971
8.174723	535.163020	9.926989
8.174940	539.514861	9.932007
7.996052	533.095608	9.937024
7.776687	516.880783	9.942042
7.247974	526.083908	9.947059
7.474132	536.355344	9.952077
7.444909	544.154781	9.957095
7.679741	545.427668	9.962112
7.888092	546.155595	9.967130
7.747669	552.482918	9.972147
7.271602	544.144156	9.977165
8.042150	555.674681	9.982183
8.099603	565.196239	9.987200
8.234896	556.872136	9.992218
8.078624	557.228003	9.997235
7.863729	553.477885	10.002253
8.223687	567.752029	10.007271
7.963064	560.641826	10.012288
8.106468	548.936586	10.017306
8.145465	548.927343	10.022323
8.209444	544.754835	10.027341
8.432087	543.653312	10.032359
8.034983	544.539219	10.037376
7.701797	540.870753	10.042394
7.913289	549.014328	10.047411
7.887556	550.476365	10.052429
8.424580	559.269528	10.057447
7.935542	556.108317	10.062464
8.141455	546.517142	10.067482
8.066444	551.934812	10.072499
8.491771	547.623636	10.077517
8.271868	548.964617	10.082535
8.091754	550.561296	10.087552
8.203689	535.017225	10.092570
8.062286	538.381398	10.097587
8.014552	538.256356	10.102605
7.776512	541.843955	10.107623
8.141836	555.445062	10.112640
8.537148	559.368930	10.117658
8.376455	561.931400	10.122675
8.217354	541.191151	10.127693
8.414279	542.728754	10.132711
8.232524	549.532766	10.137728
8.326361	536.367852	10.142746
8.389079	541.353684	10.147763
8.004860	535.518867	10.152781
8.184339	535.134163	10.157799
8.235787	544.893336	10.162816
8.621028	542.633404	10.167834
8.233407	548.311491	10.172851
8.059530	538.502116	10.177869
8.114291	546.345199	10.182887
8.103849	559.175208	10.187904
8.657746	557.980758	10.192922
8.606428	556.035377	10.197939
8.278201	546.512113	10.202957
8.269847	549.599822	10.207975
8.057632	544.984595	10.212992
8.417684	547.727403	10.218010
8.373159	546.535196	10.223027
7.895754	539.370605	10.228045
8.591688	557.379064	10.233063
8.041193	564.124092	10.238080
8.317306	560.956604	10.243098
8.326445	570.795004	10.248115
8.403349	567.096993	10.253133
8.486119	570.501788	10.258151
8.503764	572.316792	10.263168
8.850837	567.847459	10.268186
8.668894	579.306330	10.273203
8.400523	569.713716	10.278221
8.787912	553.741461	10.283239
8.142091	552.949580	10.288256
8.504593	550.150410	10.293274
8.397411	555.917104	10.298291
8.481256	561.881088	10.303309
8.730947	566.825010	10.308327
8.555986	550.196098	10.313344
8.100559	550.441047	10.318362
8.166738	559.203842	10.323379
8.107200	565.565833	10.328397
8.556195	564.428844	10.333415
8.327521	566.616957	10.338432
8.585611	565.894887	10.343450
8.772328	563.233711	10.348467
8.614295	560.904263	10.353485
8.562279	558.428815	10.358503
8.863122	568.297249	10.363520
8.786653	558.867077	10.368538
8.724993	570.755221	10.373555
8.596930	579.971339	10.378573
8.739541	567.284754	10.383591
8.497727	573.921461	10.388608
8.748632	573.228919	10.393626
8.947223	570.578505	10.398643
8.522851	564.358649	10.403661
8.857258	567.670368	10.408679
8.411361	563.836520	10.413696
8.764020	562.960778	10.418714
8.601509	567.660014	10.423731
8.708518	576.523718	10.428749
8.436140	567.026407	10.433767
8.517178	575.607000	10.438784
8.810362	564.837648	10.443802
8.852505	570.520990	10.448819
8.494865	569.100130	10.453837
8.327319	564.607287	10.458855
8.622555	573.277395	10.463872
8.587073	566.627377	10.468890
8.537846	564.994093	10.473907
8.580259	570.992973	10.478925
8.692704	570.483072	10.483943
8.516211	571.255519	10.488960
8.706367	569.423781	10.493978
8.862414	570.529134	10.498995
8.401006	573.959232	10.504013
8.631012	575.469564	10.509031
8.588642	596.721148	10.514048
8.949238	595.598008	10.519066
8.861774	590.177425	10.524083
8.737798	595.927829	10.529101
9.466727	591.827850	10.534119
9.325358	582.067006	10.539136
8.560477	574.969534	10.544154
8.775598	563.871586	10.549171
8.659689	571.466866	10.554189
9.238847	574.544578	10.559207
8.719431	582.909985	10.564224
9.099263	590.613792	10.569242
8.930982	574.962113	10.574259
8.643596	578.358634	10.579277
9.167675	581.798428	10.584295
8.716059	590.897987	10.589312
8.950961	589.251741	10.594330
9.373866	600.275030	10.599347
9.159924	586.053767	10.604365
9.062986	571.971974	10.609383
8.763524	571.908463	10.614400
8.923911	567.973309	10.619418
9.052160	567.959550	10.624435
8.460686	577.898370	10.629453
8.848254	584.897217	10.634471
8.975622	590.283189	10.639488
9.166852	603.640211	10.644506
9.244584	591.225707	10.649523
9.111972	590.489113	10.654541
9.252757	591.085617	10.659559
9.248228	601.292250	10.664576
9.087178	593.437439	10.669594
9.121899	589.995342	10.674611
8.968745	599.095480	10.679629
9.293309	593.414679	10.684647
9.036075	595.575712	10.689664
9.214238	592.903248	10.694682
9.238181	596.033242	10.699699
9.112449	597.375251	10.704717
9.292166	594.592090	10.709735
9.073250	592.458370	10.714752
8.943220	588.272068	10.719770
9.033706	585.020051	10.724787
9.102737	590.648693	10.729805
9.317084	589.447482	10.734823
8.989627	591.010445	10.739840
9.210988	593.118582	10.744858
9.261468	586.193155	10.749875
9.135689	591.268496	10.754893
9.426528	581.338948	10.759911
9.125711	591.904423	10.764928
9.286928	588.878009	10.769946
9.311761	590.657175	10.774963
9.416692	598.539757	10.779981
9.139761	597.289286	10.784999
9.158957	599.855134	10.790016
8.922117	593.119890	10.795034
9.186430	601.996829	10.800051
9.525884	602.492777	10.805069
9.177253	596.961633	10.810087
8.813070	599.208851	10.815104
8.894068	595.241949	10.820122
9.191755	595.801246	10.825139
8.922281	606.819412	10.830157
9.494587	614.186958	10.835175
9.621683	617.335508	10.840192
9.108389	630.575716	10.845210
9.716143	622.265919	10.850227
9.569591	627.792651	10.855245
9.434078	613.811544	10.860263
9.380923	611.686563	10.865280
9.357319	618.093436	10.870298
9.435293	614.824439	10.875315
9.400490	629.075277	10.880333
9.447387	623.324362	10.885351
9.602391	625.020019	10.890368
9.596247	619.835996	10.895386
9.550929	613.594602	10.900403
9.539276	627.560943	10.905421
9.513988	625.564139	10.910439
9.432253	617.674801	10.915456
9.699185	624.096115	10.920474
9.546031	609.439274	10.925491
9.258587	618.513125	10.930509
9.460912	617.171783	10.935527
9.631330	622.711967	10.940544
9.779385	622.038693	10.945562
9.799459	618.567327	10.950579
9.326253	612.415066	10.955597
9.688386	613.570183	10.960615
9.586048	612.428056	10.965632
9.849106	613.115856	10.970650
9.898549	604.413860	10.975667
9.313445	606.102400	10.980685
9.422050	603.639650	10.985703
9.607019	616.035139	10.990720
9.516299	617.554700	10.995738
9.816826	615.860300	11.000755
9.720873	626.990147	11.005773
9.816443	621.275788	11.010791
9.815123	624.207773	11.015808
9.690714	626.114467	11.020826
9.735258	622.929602	11.025843
9.948573	621.012179	11.030861
9.726125	611.601696	11.035879
9.862379	607.777612	11.040896
9.487020	603.907457	11.045914
9.866392	603.545081	11.050931
9.418310	622.269340	11.055949
9.776087	627.641314	11.060967
9.748490	621.059468	11.065984
9.744277	618.219915	11.071002
9.985322	612.422805	11.076019
9.901316	628.338155	11.081037
10.010048	621.769662	11.086055
9.868477	614.123231	11.091072
9.919579	622.437137	11.096090
10.089337	621.593205	11.101107
9.758385	617.943308	11.106125
9.960913	606.137249	11.111143
9.848122	609.206617	11.116160
9.779181	608.475825	11.121178
9.925195	615.095963	11.126195
9.942952	616.472296	11.131213
9.354084	614.986675	11.136231
9.511970	618.622708	11.141248
9.359999	616.368042	11.146266
9.825261	617.803647	11.151283
9.749333	625.910239	11.156301
9.342212	621.783124	11.161319
10.087403	624.973687	11.166336
9.975169	649.830759	11.171354
10.253114	640.862568	11.176371
10.259329	638.570491	11.181389
10.138773	629.131410	11.186407
10.319474	629.516533	11.191424
9.965510	625.232764	11.196442
10.056288	626.749136	11.201459
9.649786	624.594310	11.206477
9.794549	624.300251	11.211495
10.236478	631.309533	11.216512
9.816870	632.893250	11.221530
10.139294	639.413173	11.226547
10.266385	641.930564	11.231565
10.261936	647.267778	11.236583
10.249996	634.627452	11.241600
9.979553	634.524681	11.246618
10.267380	623.986508	11.251635
10.013470	632.553336	11.256653
10.135797	635.607962	11.261671
10.307135	633.103820	11.266688
9.980837	628.064631	11.271706
10.159726	632.072918	11.276723
10.344289	650.205775	11.281741
10.260719	646.198374	11.286759
9.903871	637.837732	11.291776
9.543638	648.447265	11.296794
9.815847	643.888656	11.301811
9.413800	640.742202	11.306829
9.570252	655.379662	11.311847
10.312747	658.400239	11.316864
10.559314	664.032647	11.321882
10.740769	657.774641	11.326899
10.211784	652.950240	11.331917
10.219170	638.255598	11.336935
10.333139	639.193978	11.341952
10.631814	639.920380	11.346970
10.177323	636.999895	11.351987
10.082989	647.031276	11.357005
10.295630	659.302537	11.362023
10.719893	660.981257	11.367040
10.155068	652.498559	11.372058
10.391792	652.347882	11.377075
10.363988	654.741220	11.382093
10.282295	662.176541	11.387111
10.576790	668.053907	11.392128
10.615441	674.728758	11.397146
10.441884	658.926352	11.402163
10.624794	660.030658	11.407181
10.475994	639.231876	11.412199
10.485504	637.412656	11.417216
10.137686	643.094004	11.422234
10.532483	654.049147	11.427251
10.836997	656.582922	11.432269
10.597501	647.664243	11.437287
10.761304	634.119063	11.442304
10.355977	639.241373	11.447322
10.805768	635.453365	11.452339
10.905575	636.248796	11.457357
10.529946	645.970798	11.462375
10.417708	631.667291	11.467392
10.466505	635.172096	11.472410
10.262368	634.298383	11.477427
10.459735	628.107322	11.482445
10.291140	646.898270	11.487463
10.475088	658.126294	11.492480
10.408895	659.604146	11.497498
10.630799	665.978881	11.502515
10.651302	667.001335	11.507533
10.554408	669.951458	11.512551
10.754680	663.728371	11.517568
10.422226	667.362346	11.522586
10.396098	674.321904	11.527603
10.533990	668.720820	11.532621
10.352053	664.328037	11.537639
10.934242	664.350452	11.542656
10.595429	671.283261	11.547674
10.726974	672.171551	11.552691
11.036026	665.843057	11.557709
10.527054	678.350472	11.562727
10.505447	662.356996	11.567744
10.739149	671.888867	11.572762
10.779560	671.191432	11.577779
11.160940	666.820841	11.582797
10.783924	671.395923	11.587815
10.806686	668.754108	11.592832
10.871655	672.448892	11.597850
11.171293	673.607493	11.602867
11.085796	670.029581	11.607885
10.696271	673.511551	11.612903
10.818082	666.685371	11.617920
10.696239	669.879245	11.622938
10.954342	670.419500	11.627955
10.747139	663.692209	11.632973
10.757339	661.775048	11.637991
10.811963	664.543638	11.643008
10.595334	671.959080	11.648026
10.452678	685.958616	11.653043
10.837288	690.748888	11.658061
10.965019	695.412150	11.663079
11.124980	691.906229	11.668096
10.897284	690.420818	11.673114
11.054656	698.298383	11.678131
11.298824	690.967025	11.683149
11.115144	696.692101	11.688167
11.271438	688.320464	11.693184
11.120861	696.972120	11.698202
11.423098	696.997372	11.703219
11.456632	682.872958	11.708237
11.127542	669.502809	11.713255
10.825280	668.827506	11.718272
11.105177	665.160786	11.723290
10.825058	657.012177	11.728307
11.039060	668.276524	11.733325
11.063155	682.019555	11.738343
11.372463	687.380206	11.743360
11.399850	677.201547	11.748378
11.185890	677.351859	11.753395
11.244549	654.500825	11.758413
11.009394	659.798451	11.763431
11.166849	651.458207	11.768448
11.202575	667.623078	11.773466
10.908963	647.291947	11.778483
11.447354	668.351637	11.783501
11.069237	678.979768	11.788519
11.535287	677.991580	11.793536
11.369941	677.869185	11.798554
10.856462	666.642333	11.803571
11.090753	674.141761	11.808589
11.434449	687.992512	11.813607
11.472102	684.250134	11.818624
11.306633	686.302125	11.823642
11.452417	687.819351	11.828659
11.516601	684.094906	11.833677
11.294712	674.848405	11.838695
11.278302	669.861637	11.843712
11.578213	677.966171	11.848730
11.066964	672.552001	11.853747
11.279544	674.674147	11.858765
11.317539	691.438290	11.863783
11.438948	682.633461	11.868800
11.155087	692.669316	11.873818
11.564452	688.190193	11.878835
11.309713	682.145690	11.883853
11.059520	687.341538	11.888871
11.290560	695.564169	11.893888
11.364578	691.648832	11.898906
11.137407	694.679332	11.903923
11.173286	690.845711	11.908941
11.263128	690.598125	11.913959
11.184184	691.036554	11.918976
11.569454	698.790050	11.923994
11.661319	719.537906	11.929011
11.523244	709.820658	11.934029
11.296012	704.409316	11.939047
11.650393	706.951065	11.944064
11.750564	709.160255	11.949082
11.959177	708.729957	11.954099
11.915210	695.504465	11.959117
11.787732	690.490912	11.964135
11.492591	688.198708	11.969152
11.410627	688.470351	11.974170
11.404914	687.773831	11.979187
11.827203	696.402001	11.984205
11.784602	710.196530	11.989223
11.772645	693.308413	11.994240
11.967890	681.945261	11.999258
11.961964	689.166750	12.004275
11.717899	684.032609	12.009293
11.832533	680.644246	12.014311
11.814097	687.201814	12.019328
11.823570	683.100930	12.024346
11.425482	685.085226	12.029363
11.555142	688.246009	12.034381
11.383418	688.465444	12.039399
11.833764	697.912891	12.044416
12.012070	712.294508	12.049434
11.883363	707.811322	12.054451
11.792114	693.479231	12.059469
11.438523	703.639627	12.064487
11.762092	707.019343	12.069504
11.934900	710.993886	12.074522
12.078462	719.952920	12.079539
12.063855	716.070399	12.084557
11.790519	723.460033	12.089575
11.933179	728.231419	12.094592
11.961702	718.349207	12.099610
11.790565	718.679004	12.104627
11.822228	713.006187	12.109645
11.850708	717.763901	12.114663
11.753792	713.480863	12.119680
12.102627	718.769058	12.124698
11.954224	710.871188	12.129715
12.123154	712.757178	12.134733
11.817796	714.203080	12.139751
11.834090	710.801716	12.144768
12.167912	704.807002	12.149786
12.036787	716.289557	12.154803
11.865423	718.143658	12.159821
11.717408	716.746746	12.164839
11.894508	721.982954	12.169856
11.968532	701.575225	12.174874
11.522391	711.270440	12.179891
11.879642	702.507545	12.184909
12.086763	729.249216	12.189927
12.067086	733.793571	12.194944
12.242450	738.222161	12.199962
12.181829	742.892856	12.204979
12.364778	736.861809	12.209997
12.295308	724.558640	12.215015
12.187798	734.614225	12.220032
12.277791	735.133484	12.225050
12.335059	745.242153	12.230067
12.159479	718.927912	12.235085
11.855126	723.286493	12.240103
12.036887	736.323202	12.245120
12.300432	740.539158	12.250138
12.180961	738.131060	12.255155
12.465580	736.369712	12.260173
12.526578	745.224929	12.265191
12.457086	743.881985	12.270208
12.499838	738.930110	12.275226
12.246655	739.616749	12.280243
12.278727	745.967607	12.285261
12.411475	751.513733	12.290279
12.398046	741.634925	12.295296
12.538119	738.311994	12.300314
12.305162	742.208107	12.305331
12.614168	741.755767	12.310349
12.706333	742.640764	12.315367
12.415532	737.659099	12.320384
12.341767	741.224153	12.325402
12.471631	739.054703	12.330419
12.584476	744.383036	12.335437
12.635792	738.571431	12.340455
12.157267	721.425027	12.345472
12.476302	725.957337	12.350490
12.380254	739.627718	12.355507
12.521696	741.483303	12.360525
12.661275	734.865754	12.365543
12.702606	743.888156	12.370560
12.478311	729.390687	12.375578
12.607687	740.611533	12.380595
12.694762	733.270057	12.385613
12.663640	733.950305	12.390631
12.900724	734.156181	12.395648
12.719535	728.690280	12.400666
12.798048	733.336017	12.405683
12.350285	725.510292	12.410701
12.704654	723.583381	12.415719
12.483098	735.925882	12.420736
12.519586	725.524860	12.425754
12.445411	739.327514	12.430771
12.999080	732.193802	12.435789
12.995907	742.255134	12.440807
12.798558	744.924359	12.445824
12.860719	730.050645	12.450842
12.575991	740.531635	12.455859
12.526149	733.277883	12.460877
13.098356	726.308528	12.465895
13.298682	740.102888	12.470912
13.017618	722.922388	12.475930
12.566366	721.430975	12.480947
12.725891	724.363021	12.485965
12.915920	729.855984	12.490983
12.903609	736.147520	12.496000
13.126315	728.939431	12.501018
12.649144	722.781441	12.506035
12.999519	727.132113	12.511053
13.042951	719.109508	12.516071
12.319924	724.376295	12.521088
12.910201	729.210094	12.526106
13.057552	735.729080	12.531123
12.964834	733.108506	12.536141
13.157960	731.765441	12.541159
13.017569	745.726799	12.546176
13.117508	740.267341	12.551194
13.172564	741.530541	12.556211
13.079179	744.524307	12.561229
12.795220	733.990450	12.566247
12.713868	745.878640	12.571264
12.569547	737.522523	12.576282
12.697595	740.696192	12.581299
12.951079	744.702285	12.586317
12.993193	741.883856	12.591335
13.005159	743.926988	12.596352
12.692519	738.102979	12.601370
12.824804	745.646822	12.606387
13.090585	758.446318	12.611405
12.989495	756.732779	12.616423
13.431581	766.866374	12.621440
13.791030	763.559560	12.626458
13.330429	747.802049	12.631475
13.185131	740.970354	12.636493
13.141436	736.189816	12.641511
13.197219	731.718744	12.646528
13.122495	735.059884	12.651546
12.870934	742.774321	12.656563
13.101356	761.439753	12.661581
13.488338	759.785443	12.666599
13.212598	762.776226	12.671616
13.037945	765.855314	12.676634
13.258753	763.299222	12.681651
13.092463	756.499212	12.686669
13.578934	749.139334	12.691687
13.498803	762.008810	12.696704
13.333206	751.042982	12.701722
13.352764	763.372970	12.706739
13.279447	755.337083	12.711757
13.280516	753.705368	12.716775
13.406506	757.573648	12.721792
13.479238	754.305446	12.726810
13.414375	758.471875	12.731827
13.336396	756.764182	12.736845
13.559985	752.285749	12.741863
13.576965	756.073276	12.746880
13.615176	754.640872	12.751898
13.451483	757.200683	12.756915
13.650248	757.851225	12.761933
13.539294	745.898528	12.766951
13.494697	758.973876	12.771968
13.442245	756.511093	12.776986
13.360200	759.727150	12.782003
13.362669	756.151217	12.787021
13.569799	741.567207	12.792039
13.351938	752.725700	12.797056
13.582857	752.635893	12.802074
13.444406	759.076591	12.807091
13.774696	776.205276	12.812109
14.142599	774.825356	12.817127
13.722713	763.249259	12.822144
13.690564	749.075123	12.827162
13.824803	759.774506	12.832179
13.586483	753.632731	12.837197
13.698611	748.196607	12.842215
13.715931	760.508009	12.847232
13.487878	757.375298	12.852250
13.669449	772.081504	12.857267
13.475473	777.846089	12.862285
13.766295	785.942628	12.867303
13.820568	791.340114	12.872320
13.589723	777.954491	12.877338
13.697400	793.619045	12.882355
13.534849	781.911097	12.887373
13.520446	780.187129	12.892391
13.593635	789.917783	12.897408
13.977175	779.310873	12.902426
13.592702	783.379060	12.907443
13.953092	788.248893	12.912461
14.185397	792.880017	12.917479
13.974862	784.461668	12.922496
13.941046	778.543466	12.927514
14.147418	782.601131	12.932531
13.834245	775.912491	12.937549
14.126424	779.369724	12.942567
13.885373	784.895531	12.947584
14.127317	789.083325	12.952602
14.751259	785.242753	12.957619
14.169632	787.868051	12.962637
14.422181	777.695082	12.967655
14.243728	776.599584	12.972672
14.212738	775.944891	12.977690
14.164776	778.413988	12.982707
14.114968	774.729476	12.987725
14.273956	778.737758	12.992743
14.233316	776.623421	12.997760
14.214672	784.023667	13.002778
14.435533	777.724731	13.007795
14.270650	781.809006	13.012813
14.456131	775.638692	13.017831
14.428482	779.004022	13.022848
14.313127	785.270694	13.027866
14.559013	776.222251	13.032883
14.148232	780.038936	13.037901
14.343144	777.906627	13.042919
14.343832	775.325060	13.047936
14.341242	782.508194	13.052954
14.219354	774.015999	13.057971
14.133832	780.546242	13.062989
14.525956	775.460721	13.068007
14.295116	777.472471	13.073024
14.250171	774.976950	13.078042
14.670433	769.265321	13.083059
14.098001	779.611528	13.088077
14.438776	769.778195	13.093095
14.195349	771.495267	13.098112
14.338882	768.742996	13.103130
14.338358	773.293828	13.108147
13.902786	776.180267	13.113165
14.004190	764.582454	13.118183
14.054770	781.003878	13.123200
14.406938	786.269480	13.128218
14.494602	793.589957	13.133235
14.161204	800.383110	13.138253
14.632765	794.808604	13.143271
14.492947	788.357890	13.148288
14.377672	794.678202	13.153306
14.884886	786.074810	13.158323
14.356309	793.895789	13.163341
14.651538	799.173472	13.168359
15.023586	789.508799	13.173376
14.536519	789.007616	13.178394
14.797660	786.050721	13.183411
14.681017	789.540451	13.188429
14.961690	785.617962	13.193447
14.847236	789.012674	13.198464
14.749360	800.130306	13.203482
14.695422	786.511828	13.208499
14.615113	789.891723	13.213517
14.736388	785.640753	13.218535
14.663928	780.599619	13.223552
14.956561	797.705823	13.228570
15.131271	790.177020	13.233587
14.680604	797.136871	13.238605
15.070385	790.104554	13.243623
15.039115	788.512617	13.248640
15.104911	792.481855	13.253658
15.070777	790.196081	13.258675
15.071490	796.125830	13.263693
15.126558	797.792981	13.268711
14.575672	783.024742	13.273728
15.180302	794.909628	13.278746
15.092090	781.776212	13.283763
14.956266	791.523836	13.288781
15.287430	793.210844	13.293799
15.229851	790.726769	13.298816
14.974139	791.969235	13.303834
15.079383	788.317232	13.308851
14.723297	798.317124	13.313869
14.902622	789.907117	13.318887
14.836079	794.862779	13.323904
14.802677	796.250297	13.328922
15.138595	785.218494	13.333939
14.851743	796.088019	13.338957
14.944392	790.014297	13.343975
15.034739	791.114178	13.348992
14.961324	789.481507	13.354010
15.353788	790.354170	13.359027
15.193527	798.676028	13.364045
15.016687	795.210233	13.369063
15.105492	790.831804	13.374080
14.917825	795.535042	13.379098
15.254916	809.124988	13.384115
15.203367	826.259899	13.389133
15.451436	820.982337	13.394151
15.530745	816.333986	13.399168
15.517913	813.180168	13.404186
15.476909	802.589268	13.409203
15.060023	801.486945	13.414221
15.435879	808.607637	13.419239
15.751867	809.397607	13.424256
15.363740	802.360935	13.429274
15.579086	788.687640	13.434291
15.192149	791.468629	13.439309
15.396418	783.897328	13.444327
15.259549	797.659356	13.449344
15.123342	807.959323	13.454362
15.495174	811.997382	13.459379
15.357039	814.594222	13.464397
15.388038	806.611397	13.469415
15.628828	811.825028	13.474432
15.469417	818.660356	13.479450
15.597564	815.007915	13.484467
15.343120	819.491245	13.489485
15.531904	810.142458	13.494503
15.688100	814.813915	13.499520
15.271880	810.454648	13.504538
15.466777	816.060485	13.509555
15.378287	816.752881	13.514573
15.395150	811.786106	13.519591
15.548401	815.713244	13.524608
15.490038	816.722817	13.529626
15.878635	815.914017	13.534643
15.342972	826.772050	13.539661
16.079307	824.176202	13.544679
15.930414	826.885186	13.549696
15.704687	817.383587	13.554714
15.682141	810.756698	13.559731
15.429482	823.871004	13.564749
15.972334	828.541844	13.569767
16.203006	829.594495	13.574784
15.933905	830.428800	13.579802
15.689768	813.015207	13.584819
15.615002	821.146952	13.589837
15.869038	827.052801	13.594855
16.223239	824.617813	13.599872
15.725395	830.253298	13.604890
16.098166	823.214165	13.609907
15.980914	834.984961	13.614925
15.906152	833.904772	13.619943
15.957482	837.270362	13.624960
16.102280	842.050911	13.629978
16.104953	833.144690	13.634995
16.145847	839.617277	13.640013
16.047889	824.998948	13.645031
15.909405	830.647557	13.650048
15.639362	832.725417	13.655066
15.964016	835.233971	13.660083
16.265246	827.230887	13.665101
16.103849	830.973795	13.670119
16.836355	828.552118	13.675136
16.132894	830.186637	13.680154
16.562903	832.385190	13.685171
16.411945	831.944954	13.690189
16.247729	827.628251	13.695207
16.277129	817.493378	13.700224
15.995217	822.545910	13.705242
16.261985	827.389397	13.710259
16.470251	831.516205	13.715277
16.128278	826.129115	13.720295
16.382715	819.676578	13.725312
16.193822	826.614360	13.730330
16.119133	824.319156	13.735347
16.100552	837.800746	13.740365
16.333656	826.283246	13.745383
16.206549	823.945761	13.750400
16.084775	825.710051	13.755418
16.116719	826.112174	13.760435
15.788582	825.586088	13.765453
16.152005	827.612033	13.770471
16.491122	832.444186	13.775488
16.056073	847.117676	13.780506
16.291953	843.959598	13.785523
16.879341	839.613494	13.790541
16.768720	845.399755	13.795559
16.779578	839.171571	13.800576
16.922874	847.171331	13.805594
16.636870	834.296088	13.810611
16.675731	825.355798	13.815629
16.607647	828.686447	13.820647
16.542469	824.489928	13.825664
16.630980	821.771517	13.830682
16.592805	814.298150	13.835699
16.727469	814.305477	13.840717
16.363423	831.659771	13.845735
16.902605	831.262885	13.850752
16.534780	845.471398	13.855770
17.138630	841.592936	13.860787
17.020048	833.548327	13.865805
16.945549	833.440100	13.870823
17.223907	827.520308	13.875840
16.578982	823.809106	13.880858
16.723820	823.373019	13.885875
16.834532	821.629444	13.890893
16.628606	828.816052	13.895911
16.514322	814.102458	13.900928
16.432963	837.130871	13.905946
16.834530	842.063696	13.910963
17.028831	849.935543	13.915981
16.714210	857.050829	13.920999
16.874947	852.001540	13.926016
16.671570	854.302490	13.931034
16.729150	850.948282	13.936051
17.438459	848.905784	13.941069
17.230426	857.522338	13.946087
16.999344	850.593586	13.951104
17.058092	855.176178	13.956122
16.945365	856.184803	13.961139
17.140883	852.846852	13.966157
16.911353	848.594026	13.971175
17.154355	853.883065	13.976192
17.361131	870.838686	13.981210
17.266702	849.374721	13.986227
17.304975	853.171557	13.991245
17.023339	855.314353	13.996263
17.153354	852.422173	14.001280
16.910191	860.665529	14.006298
17.439595	850.291348	14.011315
17.393088	855.840345	14.016333
17.159523	858.587847	14.021351
17.370455	848.396111	14.026368
17.198662	858.802670	14.031386
17.108172	853.862172	14.036403
17.671428	850.482383	14.041421
17.488697	854.727264	14.046439
17.166966	858.937118	14.051456
17.381426	849.180338	14.056474
17.355954	849.474691	14.061491
17.459094	856.881133	14.066509
17.220927	859.629356	14.071527
17.514737	847.846705	14.076544
17.209341	846.143077	14.081562
17.294327	856.039179	14.086579
17.313364	850.576584	14.091597
17.594227	859.766645	14.096615
17.772324	870.938913	14.101632
17.005398	860.802550	14.106650
17.379238	865.755506	14.111667
17.608589	869.452978	14.116685
17.392646	874.839177	14.121703
17.811919	874.328532	14.126720
17.602897	873.149453	14.131738
17.491185	879.402964	14.136755
17.507441	870.298932	14.141773
17.383625	876.147232	14.146791
17.488736	871.693644	14.151808
17.434788	880.996135	14.156826
17.279588	870.631375	14.161843
17.497157	872.421397	14.166861
17.671703	896.047274	14.171879
17.906346	883.380761	14.176896
17.962404	898.696883	14.181914
18.036043	896.185922	14.186931
18.348539	885.561677	14.191949
18.088526	880.843396	14.196967
18.025328	870.546273	14.201984
17.874646	871.693392	14.207002
17.661103	876.132457	14.212019
18.230016	867.434150	14.217037
17.538085	866.333891	14.222055
17.667976	876.532243	14.227072
17.965114	876.075448	14.232090
17.847786	885.211144	14.237107
18.315605	896.129748	14.242125
17.833091	901.273693	14.247143
18.354801	903.293782	14.252160
18.088292	895.515323	14.257178
18.185718	886.524800	14.262195
18.379935	868.884677	14.267213
17.868425	868.450438	14.272231
18.288415	875.497970	14.277248
18.086559	875.182475	14.282266
17.999032	873.091251	14.287283
18.202511	878.020409	14.292301
18.236753	887.738284	14.297319
18.280404	896.403786	14.302336
18.629920	887.509467	14.307354
18.309465	881.459413	14.312371
18.309493	868.851760	14.317389
17.892267	879.334656	14.322407
18.365660	888.308370	14.327424
18.178287	885.996099	14.332442
18.389514	897.261026	14.337459
18.422565	893.522480	14.342477
18.584511	899.114572	14.347495
18.497740	899.576323	14.352512
18.497019	892.961763	14.357530
18.403961	892.941651	14.362547
18.630494	879.162391	14.367565
18.777572	889.875620	14.372583
18.512595	877.959590	14.377600
18.578509	882.339092	14.382618
18.586500	886.983295	14.387635
18.800925	880.508603	14.392653
18.186993	888.002162	14.397671
18.517908	889.982714	14.402688
18.844239	886.365480	14.407706
18.506966	894.472115	14.412723
18.543826	894.245452	14.417741
18.300270	890.215725	14.422759
18.601728	891.181548	14.427776
18.789814	895.220013	14.432794
18.121494	895.479385	14.437811
18.617734	885.943529	14.442829
18.216092	895.007009	14.447847
18.290329	886.805930	14.452864
18.767569	899.430382	14.457882
19.016820	910.847153	14.462899
19.036688	912.286295	14.467917
18.615245	901.019627	14.472935
19.048541	904.574697	14.477952
19.054666	905.672002	14.482970
18.805664	899.049003	14.487987
19.068737	890.313396	14.493005
18.934965	892.098507	14.498023
19.205350	883.936126	14.503040
18.992068	881.643694	14.508058
18.945246	897.455626	14.513075
19.115221	889.343688	14.518093
18.724648	895.745040	14.523111
19.095055	892.373368	14.528128
18.975072	896.119268	14.533146
18.825783	897.689056	14.538163
18.782356	905.853800	14.543181
19.041792	920.017742	14.548199
19.090204	923.226012	14.553216
19.373430	920.846315	14.558234
19.332661	919.202205	14.563251
19.631750	912.493325	14.568269
19.597815	911.734945	14.573287
19.259074	900.941323	14.578304
19.474070	884.980005	14.583322
19.120789	886.786885	14.588339
19.421953	876.142331	14.593357
19.063403	874.576418	14.598375
19.200011	897.239392	14.603392
19.616834	897.357147	14.608410
19.214809	903.331098	14.613427
19.270060	899.926751	14.618445
19.260033	904.646367	14.623463
19.510516	911.461690	14.628480
19.906439	897.728460	14.633498
19.475465	904.022534	14.638515
19.611501	908.353185	14.643533
19.506684	905.952236	14.648551
19.075665	908.269925	14.653568
19.754802	904.303914	14.658586
20.035255	909.612348	14.663603
20.085558	895.983765	14.668621
19.523942	893.013747	14.673639
19.189470	891.021174	14.678656
19.365919	890.296105	14.683674
19.392457	908.573907	14.688691
19.771522	906.081363	14.693709
19.808740	906.637299	14.698727
19.833801	908.176615	14.703744
19.941677	896.483027	14.708762
19.631461	913.828966	14.713779
19.909155	907.959746	14.718797
19.995507	897.576059	14.723815
20.035542	900.201802	14.728832
19.929761	896.945764	14.733850
19.736548	909.735233	14.738867
20.027840	894.863351	14.743885
19.843788	899.177878	14.748903
19.667897	904.933358	14.753920
19.677225	897.272630	14.758938
19.660630	899.503295	14.763955
19.889803	899.281215	14.768973
19.694055	898.734384	14.773991
19.573023	908.214661	14.779008
20.009589	900.310263	14.784026
19.686761	908.203198	14.789043
19.770623	894.452591	14.794061
19.764502	908.484559	14.799079
20.029065	917.320591	14.804096
20.297276	927.206960	14.809114
20.270964	928.539728	14.814131
20.362461	918.354042	14.819149
20.540951	920.825548	14.824167
20.201383	905.263533	14.829184
19.988002	901.453142	14.834202
20.192490	918.068333	14.839219
20.212318	919.371780	14.844237
20.417811	925.200058	14.849255
20.176682	931.937778	14.854272
20.434893	925.866472	14.859290
20.312633	929.454942	14.864307
20.457426	927.188454	14.869325
20.348133	925.390975	14.874343
20.053440	933.733958	14.879360
20.491566	928.278261	14.884378
20.574260	930.133604	14.889395
20.380213	923.186397	14.894413
20.659638	924.345027	14.899431
20.504973	928.957920	14.904448
20.676938	918.153699	14.909466
20.049966	921.534062	14.914483
20.073455	920.653072	14.919501
20.467253	923.160274	14.924519
19.926370	928.379645	14.929536
20.544729	922.043625	14.934554
20.117710	931.126879	14.939571
20.958704	943.994179	14.944589
20.835680	953.604183	14.949607
20.382535	943.447012	14.954624
20.872288	946.680813	14.959642
20.684780	956.834265	14.964659
20.739298	949.759739	14.969677
21.101566	950.687635	14.974695
20.710673	956.438948	14.979712
20.993714	951.007543	14.984730
20.829406	951.576120	14.989747
20.839580	949.927182	14.994765
20.828578	944.825878	14.999783
20.723106	945.445198	15.004800
20.739252	948.333473	15.009818
20.704326	948.272695	15.014835
21.010318	946.170300	15.019853
21.199581	948.501264	15.024871
20.869798	945.687423	15.029888
21.111810	949.540721	15.034906
20.852344	951.212985	15.039923
20.989399	946.659697	15.044941
21.073580	944.898175	15.049959
21.268399	945.751319	15.054976
21.301496	945.345360	15.059994
21.115283	947.984468	15.065011
21.259733	949.189494	15.070029
21.122691	939.102721	15.075047
21.224887	946.903833	15.080064
21.020674	944.663622	15.085082
21.186355	951.564833	15.090099
20.963415	940.115557	15.095117
21.280556	941.400825	15.100135
20.837000	941.602891	15.105152
21.008910	944.179575	15.110170
21.479711	961.990185	15.115187
21.357335	961.526532	15.120205
21.904623	961.854226	15.125223
21.362988	960.436914	15.130240
21.606360	959.859150	15.135258
21.562582	947.965222	15.140275
21.558811	949.161912	15.145293
21.869078	938.298140	15.150311
21.449895	929.776710	15.155328
21.843587	928.648364	15.160346
21.502401	934.082607	15.165363
21.412056	929.703810	15.170381
21.450699	921.416771	15.175399
21.301341	944.525406	15.180416
21.870857	949.198413	15.185434
21.731299	956.772314	15.190451
21.677254	955.136592	15.195469
21.874338	951.886742	15.200487
21.706014	955.135288	15.205504
21.834458	952.606264	15.210522
21.634746	942.431477	15.215539
21.561989	952.320789	15.220557
21.518051	954.016090	15.225575
21.533119	967.621897	15.230592
21.650837	967.496176	15.235610
21.690030	967.313329	15.240627
21.565560	965.259441	15.245645
21.953767	951.984981	15.250663
21.919181	949.958039	15.255680
22.276336	954.695879	15.260698
22.122448	957.752811	15.265715
21.973021	960.234674	15.270733
22.015023	956.573610	15.275751
21.863240	962.912326	15.280768
21.903199	951.567021	15.285786
21.981334	955.906756	15.290803
21.936992	960.335110	15.295821
21.942417	963.688981	15.300839
22.248918	977.697269	15.305856
22.551925	976.217047	15.310874
22.624659	970.597675	15.315891
22.394560	961.689989	15.320909
22.510262	954.681616	15.325927
22.429529	949.057893	15.330944
22.422121	943.189149	15.335962
22.171835	949.186679	15.340979
22.294769	945.263622	15.345997
22.125678	944.693678	15.351015
22.032023	948.006264	15.356032
22.232842	960.831864	15.361050
22.596801	972.296976	15.366067
22.376599	979.126110	15.371085
22.615552	977.116269	15.376103
22.525976	983.612506	15.381120
22.415083	973.026144	15.386138
22.747446	972.339760	15.391155
22.402943	979.696467	15.396173
22.731452	977.514800	15.401191
22.674510	974.607711	15.406208
22.733548	973.263546	15.411226
22.960836	972.536820	15.416243
22.709125	977.101813	15.421261
22.855953	974.194356	15.426279
22.934827	961.217670	15.431296
22.543935	956.469381	15.436314
22.393174	961.192126	15.441331
22.820521	972.167613	15.446349
22.977061	966.102756	15.451367
22.864903	974.098415	15.456384
23.092203	971.850553	15.461402
22.708124	972.311550	15.466419
22.555721	980.960473	15.471437
22.940849	976.201047	15.476455
22.641877	983.891457	15.481472
22.800277	970.895992	15.486490
22.919661	979.211990	15.491507
22.806515	982.120527	15.496525
22.941318	978.435451	15.501543
22.909368	972.633660	15.506560
22.887284	973.429269	15.511578
22.963810	980.988260	15.516595
22.779825	981.522050	15.521613
23.205310	986.804628	15.526631
22.859750	991.564214	15.531648
22.985634	1004.003945	15.536666
23.225191	1007.636729	15.541683
23.180322	1007.981462	15.546701
23.328964	999.307914	15.551719
23.399039	993.654237	15.556736
23.270160	996.350642	15.561754
23.697600	992.588154	15.566771
23.469056	1000.687268	15.571789
23.590456	1000.264317	15.576807
23.852771	999.907652	15.581824
23.438664	980.582812	15.586842
23.352395	973.830143	15.591859
23.255030	971.074559	15.596877
23.566551	978.470494	15.601895
23.599491	985.443010	15.606912
23.770939	987.237115	15.611930
23.605141	976.653041	15.616947
23.105024	976.308534	15.621965
23.077551	983.814391	15.626983
23.516477	989.400984	15.632000
23.137049	990.404065	15.637018
23.286960	990.535238	15.642035
23.317052	999.351241	15.647053
23.552032	991.162799	15.652071
23.730990	1004.048661	15.657088
23.767538	1011.938985	15.662106
24.094748	1017.284308	15.667123
24.026939	1011.923635	15.672141
23.920692	1000.389763	15.677159
23.841834	989.732098	15.682176
24.183211	995.851542	15.687194
24.127533	992.985278	15.692211
24.139450	992.131345	15.697229
24.136993	994.126271	15.702247
24.170815	996.980226	15.707264
23.992430	988.881798	15.712282
24.350983	983.981364	15.717299
23.878892	989.868489	15.722317
24.136725	979.211728	15.727335
23.983205	980.245686	15.732352
23.566554	983.561548	15.737370
23.791914	982.626835	15.742387
23.908469	1008.158632	15.747405
24.064610	1015.951322	15.752423
24.241972	1017.905454	15.757440
24.218552	1020.301309	15.762458
24.625701	1008.964711	15.767475
24.439703	1012.238127	15.772493
24.542011	1011.900220	15.777511
25.117054	1013.028317	15.782528
24.264027	992.027029	15.787546
24.342432	984.699432	15.792563
24.334702	986.537389	15.797581
24.466112	985.144014	15.802599
24.462703	987.546197	15.807616
24.450483	993.869369	15.812634
24.714477	991.653625	15.817651
24.213166	994.976442	15.822669
24.509560	994.529228	15.827687
24.901285	1007.407004	15.832704
24.391792	1010.611182	15.837722
24.376040	1006.018702	15.842739
24.349526	1016.958027	15.847757
24.633444	1015.777446	15.852775
24.680330	1015.621796	15.857792
24.780314	1020.999566	15.862810
24.659871	1018.809338	15.867827
24.688968	1011.849226	15.872845
24.704697	1013.860240	15.877863
24.482547	1023.725661	15.882880
24.337313	1012.680740	15.887898
24.730993	1007.948369	15.892915
24.641010	1019.752885	15.897933
24.524646	1014.327233	15.902951
24.994063	1035.350827	15.907968
24.743879	1043.491222	15.912986
25.097532	1037.477511	15.918003
25.119106	1043.637610	15.923021
25.103370	1044.151353	15.928039
25.132905	1037.812874	15.933056
25.074980	1049.072728	15.938074
25.072522	1043.364126	15.943091
25.486109	1050.191819	15.948109
25.405511	1033.806454	15.953127
25.566906	1034.519668	15.958144
25.318114	1030.241413	15.963162
25.204816	1000.060501	15.968179
25.106252	1006.766444	15.973197
25.503225	1016.212956	15.978215
25.555377	1006.165932	15.983232
25.289759	1007.716085	15.988250
25.392862	1001.293506	15.993267
25.072666	1006.045967	15.998285
24.999338	1017.929925	16.003303
25.301401	1022.629077	16.008320
25.189290	1039.732655	16.013338
25.477198	1033.356851	16.018355
25.356868	1025.801591	16.023373
25.361361	1023.528670	16.028391
25.586099	1033.901605	16.033408
25.521930	1030.250849	16.038426
25.704153	1032.330456	16.043443
25.549664	1031.445788	16.048461
25.507827	1025.298381	16.053479
25.734200	1033.045360	16.058496
25.344910	1032.573031	16.063514
25.876623	1028.541727	16.068531
25.552811	1043.949051	16.073549
25.891448	1046.565901	16.078567
25.936330	1051.702998	16.083584
26.125637	1053.740471	16.088602
26.138320	1026.099207	16.093619
25.505568	1032.229274	16.098637
25.718086	1035.364514	16.103655
25.860727	1044.901384	16.108672
25.929505	1052.761429	16.113690
26.025921	1051.578665	16.118707
26.196952	1057.421854	16.123725
26.117751	1060.290371	16.128743
26.292634	1056.286566	16.133760
25.967930	1061.705641	16.138778
26.306906	1052.087036	16.143795
26.282689	1058.645646	16.148813
26.309831	1054.096928	16.153831
26.448424	1052.254285	16.158848
25.859143	1040.149110	16.163866
25.913985	1043.132326	16.168883
26.100850	1045.987557	16.173901
26.027688	1048.122959	16.178919
26.303768	1043.358510	16.183936
26.269246	1046.339949	16.188954
26.299221	1046.186948	16.193971
26.171627	1045.667305	16.198989
25.995713	1051.672152	16.204007
26.029169	1047.980849	16.209024
26.185929	1058.607453	16.214042
26.607135	1067.968143	16.219059
26.615875	1072.612277	16.224077
26.576240	1068.266528	16.229095
26.894962	1071.331484	16.234112
26.748287	1073.440536	16.239130
26.468402	1045.084510	16.244147
26.991049	1062.830292	16.249165
26.725618	1057.579465	16.254183
26.798146	1045.739835	16.259200
26.718711	1050.145307	16.264218
26.754249	1040.792007	16.269235
26.567476	1053.959276	16.274253
26.865084	1060.937692	16.279271
26.686824	1067.782380	16.284288
26.874337	1077.476344	16.289306
26.865609	1072.535598	16.294323
26.673811	1076.273852	16.299341
26.684944	1068.641170	16.304359
26.640920	1070.506914	16.309376
26.948086	1078.275969	16.314394
27.054776	1079.449050	16.319411
27.181468	1078.078498	16.324429
26.816115	1078.315650	16.329447
26.975117	1077.394486	16.334464
26.641861	1071.658806	16.339482
27.094129	1076.476454	16.344499
27.392707	1091.578013	16.349517
27.184715	1097.950830	16.354535
27.599402	1093.382409	16.359552
27.238312	1078.457950	16.364570
27.582011	1084.441357	16.369587
27.286494	1068.723970	16.374605
27.275590	1076.268296	16.379623
27.619388	1070.281365	16.384640
27.667802	1070.494716	16.389658
27.295781	1067.157281	16.394675
27.361174	1059.740171	16.399693
27.167539	1069.935674	16.404711
27.059879	1074.282456	16.409728
27.066092	1082.054484	16.414746
27.310217	1088.334369	16.419763
28.060003	1084.183675	16.424781
27.858192	1094.247925	16.429799
27.851753	1091.579065	16.434816
27.845249	1098.242215	16.439834
27.870827	1085.478922	16.444851
28.084073	1085.022644	16.449869
27.613155	1091.755399	16.454887
27.791116	1084.598361	16.459904
27.836144	1086.446998	16.464922
28.061204	1089.760168	16.469939
27.875093	1087.472920	16.474957
27.747132	1092.608707	16.479975
28.252929	1084.769123	16.484992
28.020712	1084.792905	16.490010
27.751148	1084.380714	16.495027
27.770268	1083.036484	16.500045
27.666583	1086.066636	16.505063
28.311145	1078.318925	16.510080
28.280484	1079.784933	16.515098
28.157767	1079.567491	16.520115
28.644387	1076.906590	16.525133
28.340069	1080.716124	16.530151
28.165177	1078.679591	16.535168
28.430904	1079.859313	16.540186
28.072013	1076.371492	16.545203
28.580318	1070.153653	16.550221
28.475148	1079.792487	16.555239
28.599815	1082.900473	16.560256
28.284828	1080.008550	16.565274
28.156369	1078.646416	16.570291
28.317565	1077.620763	16.575309
28.282723	1082.953402	16.580327
28.421217	1075.316542	16.585344
28.259048	1078.658823	16.590362
28.415310	1088.143088	16.595379
28.433932	1084.154292	16.600397
28.290955	1084.429188	16.605415
28.291195	1076.321669	16.610432
28.237831	1090.872438	16.615450
28.675063	1101.581360	16.620467
29.041435	1103.748891	16.625485
28.631613	1109.225499	16.630503
28.913911	1103.377585	16.635520
28.719097	1112.929493	16.640538
28.958433	1106.744316	16.645555
28.895288	1111.103068	16.650573
28.862975	1101.318541	16.655591
28.612247	1103.472303	16.660608
28.709660	1102.866909	16.665626
28.541561	1114.857301	16.670643
28.648548	1103.239459	16.675661
28.906277	1107.573183	16.680679
28.783138	1098.566617	16.685696
28.572027	1104.109922	16.690714
28.886853	1112.834031	16.695731
29.062871	1112.345714	16.700749
28.930926	1125.447639	16.705767
28.966784	1127.868936	16.710784
28.950906	1131.021042	16.715802
29.148181	1128.689500	16.720819
29.136097	1128.104417	16.725837
28.929514	1124.378122	16.730855
29.237153	1121.363392	16.735872
29.083459	1130.227191	16.740890
29.131282	1146.179153	16.745907
29.453723	1144.383438	16.750925
29.390758	1148.382397	16.755943
29.344343	1154.171322	16.760960
29.249450	1154.814239	16.765978
29.212207	1159.383546	16.770995
29.363123	1147.881873	16.776013
29.331357	1156.480420	16.781031
29.168544	1143.342646	16.786048
29.862373	1170.425302	16.791066
30.144018	1172.950112	16.796083
29.918733	1155.896159	16.801101
29.825371	1141.917501	16.806119
29.989812	1141.254265	16.811136
29.888106	1140.752654	16.816154
29.621171	1150.489457	16.821171
29.759470	1143.887737	16.826189
29.828754	1144.530178	16.831207
30.023391	1151.329097	16.836224
30.212966	1145.991175	16.841242
29.860700	1142.732685	16.846259
30.180833	1150.906853	16.851277
30.242416	1147.258461	16.856295
29.803818	1142.640676	16.861312
30.363309	1136.162322	16.866330
30.007679	1146.695685	16.871347
30.180259	1142.382942	16.876365
30.090262	1146.717507	16.881383
30.421362	1154.362921	16.886400
30.125435	1146.308085	16.891418
30.474816	1163.626663	16.896435
30.685388	1143.051864	16.901453
30.387903	1140.895672	16.906471
30.376778	1133.683029	16.911488
30.278801	1134.714606	16.916506
30.127832	1140.482037	16.921523
30.748688	1148.482850	16.926541
30.448705	1151.748904	16.931559
30.242635	1148.278152	16.936576
30.389886	1156.952796	16.941594
30.332488	1165.656353	16.946611
30.980329	1170.847341	16.951629
30.656861	1164.358990	16.956647
30.729314	1158.023211	16.961664
30.539408	1162.035751	16.966682
30.782503	1166.532734	16.971699
31.131818	1165.790037	16.976717
30.674388	1152.382826	16.981735
30.834240	1155.119226	16.986752
30.875510	1152.499688	16.991770
30.885801	1160.249019	16.996787
31.134015	1157.076331	17.001805
30.986660	1162.893697	17.006823
30.811598	1149.420156	17.011840
30.759749	1155.588642	17.016858
30.905163	1148.029564	17.021875
31.228366	1151.778665	17.026893
30.910065	1150.367372	17.031911
31.116045	1157.385430	17.036928
30.943577	1153.492832	17.041946
31.023195	1155.730545	17.046963
31.277298	1157.262400	17.051981
31.044725	1154.995046	17.056999
30.746554	1152.709567	17.062016
31.214843	1159.752801	17.067034
31.208443	1176.697932	17.072051
31.215665	1173.676612	17.077069
31.046869	1178.493761	17.082087
31.321395	1180.278047	17.087104
31.383719	1165.088353	17.092122
31.218935	1179.006533	17.097139
31.573859	1177.751698	17.102157
31.103535	1180.069267	17.107175
31.639706	1184.491933	17.112192
32.048997	1193.731475	17.117210
31.514948	1197.848437	17.122227
31.599141	1187.297656	17.127245
31.894275	1187.680643	17.132263
31.843057	1178.457633	17.137280
31.766981	1180.208485	17.142298
31.853622	1175.464215	17.147315
31.846621	1179.912020	17.152333
32.261103	1193.326027	17.157351
31.651945	1185.194014	17.162368
31.728558	1187.447982	17.167386
31.649148	1204.641271	17.172403
31.918107	1199.366638	17.177421
32.049136	1199.387158	17.182439
32.293673	1202.716234	17.187456
32.438992	1196.204917	17.192474
32.164908	1204.393313	17.197491
32.242570	1202.837923	17.202509
32.202672	1197.517004	17.207527
31.848150	1201.975081	17.212544
32.429478	1199.567577	17.217562
32.311871	1196.830908	17.222579
32.789926	1200.404273	17.227597
32.447330	1197.702855	17.232615
32.424539	1199.054027	17.237632
32.181945	1190.069287	17.242650
32.132312	1204.647967	17.247667
32.390230	1201.120287	17.252685
32.717404	1201.428823	17.257703
32.542091	1203.223630	17.262720
32.531175	1205.011614	17.267738
32.361998	1203.311855	17.272755
32.508109	1199.498725	17.277773
32.294131	1200.065624	17.282791
32.287238	1205.368673	17.287808
32.839492	1206.314156	17.292826
32.484637	1201.803160	17.297843
32.591468	1206.125835	17.302861
32.631425	1210.626254	17.307879
32.320939	1223.547933	17.312896
32.711446	1230.117370	17.317914
32.577747	1221.891909	17.322931
32.507056	1225.500762	17.327949
32.621599	1226.385432	17.332967
32.708655	1231.086768	17.337984
33.172279	1240.620790	17.343002
33.145369	1246.141591	17.348019
33.402929	1240.764586	17.353037
33.648850	1242.184117	17.358055
32.861643	1236.093458	17.363072
33.510684	1228.625859	17.368090
33.509599	1238.794446	17.373107
33.351332	1225.119392	17.378125
33.407013	1218.079293	17.383143
33.410953	1218.624673	17.388160
33.310600	1210.277224	17.393178
33.477740	1221.773334	17.398195
33.818971	1228.006495	17.403213
33.654295	1210.665272	17.408231
33.839194	1209.976737	17.413248
33.791115	1201.968254	17.418266
33.379721	1212.065407	17.423283
33.707078	1201.949907	17.428301
33.445546	1205.364585	17.433319
33.308378	1210.284090	17.438336
33.904842	1214.003013	17.443354
33.771873	1238.135134	17.448371
33.658513	1237.392340	17.453389
33.966144	1244.681694	17.458407
34.047387	1239.818328	17.463424
34.261548	1233.264652	17.468442
34.195306	1230.115972	17.473459
34.116571	1217.059648	17.478477
33.617759	1210.197951	17.483495
33.774292	1219.363495	17.488512
34.389434	1225.973477	17.493530
33.776913	1233.328097	17.498547
33.955876	1228.029685	17.503565
34.082973	1233.349620	17.508583
33.943313	1228.694443	17.513600
33.727093	1231.388788	17.518618
33.947343	1238.130076	17.523635
34.109128	1231.224832	17.528653
34.344241	1224.936130	17.533671
33.961256	1224.235580	17.538688
34.190967	1237.527086	17.543706
34.292044	1258.283594	17.548723
34.462450	1258.111745	17.553741
34.745946	1244.320123	17.558759
34.463153	1257.076535	17.563776
34.408157	1252.840449	17.568794
34.506700	1249.552334	17.573811
34.467378	1252.070637	17.578829
34.692321	1250.924529	17.583847
34.268395	1257.826716	17.588864
34.152207	1257.172730	17.593882
34.011950	1260.776709	17.598899
34.221431	1274.071411	17.603917
34.951984	1276.762597	17.608935
34.808195	1277.580444	17.613952
34.783471	1280.229013	17.618970
34.775292	1282.537305	17.623987
34.798270	1280.753781	17.629005
35.242877	1272.462937	17.634023
35.056532	1274.698153	17.639040
35.209732	1265.058047	17.644058
35.283021	1274.391302	17.649075
35.270362	1269.391155	17.654093
35.292811	1272.947553	17.659111
35.190671	1269.242734	17.664128
35.535447	1264.536895	17.669146
35.901141	1264.877269	17.674163
35.643766	1267.035247	17.679181
35.521273	1263.150574	17.684199
35.387760	1264.822068	17.689216
35.897256	1260.756323	17.694234
35.708352	1256.121478	17.699251
35.419439	1250.931080	17.704269
35.901863	1232.295508	17.709287
35.423907	1237.656593	17.714304
35.439819	1232.238553	17.719322
35.635030	1246.677916	17.724339
36.149029	1252.871393	17.729357
35.902484	1234.867605	17.734375
36.024915	1230.256573	17.739392
36.079045	1226.962797	17.744410
35.476843	1231.008390	17.749427
35.877929	1229.490690	17.754445
35.592221	1217.675513	17.759463
35.855892	1236.901146	17.764480
36.205023	1245.323289	17.769498
36.226330	1248.381224	17.774515
36.103577	1234.527023	17.779533
36.201320	1223.851016	17.784551
35.686148	1231.288216	17.789568
36.118936	1229.727678	17.794586
36.282975	1235.445784	17.799603
35.694011	1244.052776	17.804621
36.500811	1239.176720	17.809639
36.174558	1253.009799	17.814656
35.933625	1243.690242	17.819674
36.072212	1250.864068	17.824691
36.264326	1250.092348	17.829709
36.256280	1248.922782	17.834727
36.125793	1251.177647	17.839744
36.351081	1258.549339	17.844762
36.362802	1260.444240	17.849779
36.065686	1270.804399	17.854797
36.653787	1268.361109	17.859815
36.531413	1274.726886	17.864832
36.806398	1267.901726	17.869850
36.511253	1273.887456	17.874867
36.653030	1270.829259	17.879885
36.699350	1268.385644	17.884903
37.009575	1264.931811	17.889920
36.715647	1269.983194	17.894938
36.563343	1267.280354	17.899955
36.518472	1270.405469	17.904973
36.555674	1274.852684	17.909991
36.883849	1289.656273	17.915008
36.915843	1299.166432	17.920026
36.792118	1296.888318	17.925043
37.435050	1305.090880	17.930061
37.209088	1304.356257	17.935079
36.984442	1298.849650	17.940096
36.532683	1303.184126	17.945114
37.229985	1299.612833	17.950131
37.099338	1304.970016	17.955149
37.055431	1291.611524	17.960167
37.113082	1306.751014	17.965184
36.941683	1321.686553	17.970202
37.393005	1323.736657	17.975219
37.528119	1332.934019	17.980237
37.751946	1319.470438	17.985255
37.578774	1329.817524	17.990272
37.835042	1320.615695	17.995290
37.645331	1322.513759	18.000307
37.581714	1317.108154	18.005325
37.627668	1321.604505	18.010343
37.687995	1326.253246	18.015360
37.613335	1323.667626	18.020378
38.076414	1320.615886	18.025395
37.785907	1324.814644	18.030413
37.863212	1317.556513	18.035431
37.579318	1323.300646	18.040448
36.965882	1325.830012	18.045466
37.658841	1338.439915	18.050483
38.108423	1346.969449	18.055501
38.631416	1344.820386	18.060519
38.139890	1353.118660	18.065536
38.161310	1349.315567	18.070554
38.506339	1348.182198	18.075571
38.648226	1355.608025	18.080589
38.524991	1334.151146	18.085607
38.361405	1328.537129	18.090624
38.352545	1316.580677	18.095642
38.270032	1326.490660	18.100659
38.286348	1325.402482	18.105677
38.516732	1332.006513	18.110695
38.447123	1335.160762	18.115712
38.386742	1338.266226	18.120730
38.313760	1342.172120	18.125747
38.747423	1345.724067	18.130765
38.735851	1341.758879	18.135783
38.618240	1345.444537	18.140800
38.751525	1344.603132	18.145818
38.805040	1335.262641	18.150835
38.831438	1334.775669	18.155853
38.778670	1335.926411	18.160871
38.813997	1338.988477	18.165888
38.685260	1333.457364	18.170906
38.652363	1326.121818	18.175923
38.666917	1331.554094	18.180941
39.007701	1341.268371	18.185959
39.348614	1352.652128	18.190976
38.759366	1356.241263	18.195994
39.072248	1350.262239	18.201011
38.940408	1362.070383	18.206029
39.363338	1367.397659	18.211047
38.722230	1364.465262	18.216064
38.984785	1366.238819	18.221082
39.279251	1359.846093	18.226099
39.190085	1367.648968	18.231117
39.361991	1358.277292	18.236135
38.920968	1364.248038	18.241152
38.872056	1377.381321	18.246170
39.366159	1382.284020	18.251187
39.336406	1393.063129	18.256205
39.560781	1385.999689	18.261223
39.941135	1381.651179	18.266240
40.068475	1392.913783	18.271258
40.098781	1382.043111	18.276275
39.736161	1388.752697	18.281293
40.021090	1390.734200	18.286311
40.074365	1386.156055	18.291328
39.920267	1385.536407	18.296346
40.275891	1384.625449	18.301363
40.188672	1388.318978	18.306381
40.337260	1391.338060	18.311399
39.822630	1375.408567	18.316416
39.744651	1365.545839	18.321434
40.167562	1378.406374	18.326451
40.004241	1382.960777	18.331469
40.216019	1384.183688	18.336487
40.227685	1382.976309	18.341504
39.973526	1386.613939	18.346522
40.128147	1379.062790	18.351539
40.094726	1391.183752	18.356557
39.903780	1386.340900	18.361575
40.243070	1388.130840	18.366592
40.111054	1404.568823	18.371610
40.612843	1405.023583	18.376627
40.363446	1411.765934	18.381645
40.415780	1409.283486	18.386663
40.665667	1406.640693	18.391680
40.876978	1403.874550	18.396698
41.162843	1405.272056	18.401715
41.178470	1406.847609	18.406733
41.020305	1407.724521	18.411751
40.901852	1406.884683	18.416768
40.425882	1407.177040	18.421786
40.980525	1395.469935	18.426803
40.725124	1405.227160	18.431821
40.974058	1407.918083	18.436839
40.705340	1394.004572	18.441856
41.118000	1405.749525	18.446874
41.290215	1398.119869	18.451891
40.621118	1405.559165	18.456909
41.239567	1401.744575	18.461927
41.284634	1408.658549	18.466944
41.036838	1413.481827	18.471962
41.813369	1420.382192	18.476979
41.632376	1425.813575	18.481997
41.318268	1424.117566	18.487015
41.392858	1424.430966	18.492032
41.271258	1422.177750	18.497050
41.459065	1416.757970	18.502067
41.270749	1416.929516	18.507085
41.703146	1411.679709	18.512103
41.734388	1410.068455	18.517120
41.510071	1415.238366	18.522138
42.118231	1403.324045	18.527155
41.947967	1398.856663	18.532173
42.075924	1414.026257	18.537191
42.365210	1402.591107	18.542208
41.875844	1409.118578	18.547226
42.353288	1398.761691	18.552243
42.370407	1407.201213	18.557261
42.122740	1402.771206	18.562279
41.940442	1405.460262	18.567296
42.077908	1405.037941	18.572314
42.048271	1398.670732	18.577331
42.031924	1409.608704	18.582349
41.768557	1410.035018	18.587367
42.152771	1401.829319	18.592384
41.990453	1406.301516	18.597402
42.330777	1405.815852	18.602419
42.188057	1406.412619	18.607437
42.124924	1404.317511	18.612455
42.679561	1417.037509	18.617472
42.784530	1439.437872	18.622490
42.826387	1430.509434	18.627507
42.801992	1414.730326	18.632525
42.533668	1403.234210	18.637543
42.444545	1410.734126	18.642560
42.560424	1430.794205	18.647578
42.677170	1431.138871	18.652595
42.831767	1440.124943	18.657613
42.576969	1441.392556	18.662631
42.984802	1432.618226	18.667648
42.512042	1439.537601	18.672666
42.628841	1435.495472	18.677683
42.335134	1428.528967	18.682701
42.829111	1449.542891	18.687719
43.195343	1456.968326	18.692736
43.197007	1463.349451	18.697754
43.188319	1452.547965	18.702771
43.238752	1457.292969	18.707789
43.200425	1462.954488	18.712807
43.163907	1447.874719	18.717824
43.042245	1468.647434	18.722842
43.118983	1459.315864	18.727859
43.164228	1463.733463	18.732877
43.430867	1474.475650	18.737895
43.561475	1475.783873	18.742912
43.390461	1489.296149	18.747930
43.426822	1485.582209	18.752947
43.922486	1478.182723	18.757965
43.558227	1480.878207	18.762983
43.907297	1481.956532	18.768000
43.613243	1492.590908	18.773018
43.680721	1485.296377	18.778035
43.636810	1481.146868	18.783053
43.555369	1479.704749	18.788071
43.871163	1488.681368	18.793088
43.805397	1502.767331	18.798106
43.974023	1502.535796	18.803123
43.967509	1504.723929	18.808141
44.031841	1500.510116	18.813159
44.038596	1498.637589	18.818176
43.972629	1502.637097	18.823194
44.067487	1499.665111	18.828211
44.359208	1497.706908	18.833229
44.183604	1506.700565	18.838247
44.371915	1509.053844	18.843264
44.396398	1523.958861	18.848282
44.774733	1520.456436	18.853299
45.394109	1520.807566	18.858317
44.655398	1512.032944	18.863335
44.775292	1501.160787	18.868352
44.795137	1502.865082	18.873370
45.040293	1496.208619	18.878387
45.228625	1495.955061	18.883405
44.896212	1493.394021	18.888423
45.061640	1493.778401	18.893440
45.186034	1488.892426	18.898458
44.634061	1488.754857	18.903475
44.800400	1489.243241	18.908493
44.857540	1486.570672	18.913511
45.088468	1482.255018	18.918528
44.789546	1501.979358	18.923546
44.696676	1506.910939	18.928563
45.503597	1520.920150	18.933581
45.299774	1522.769949	18.938599
45.641322	1517.493318	18.943616
45.424777	1520.168821	18.948634
45.166311	1515.494311	18.953651
45.198522	1516.868449	18.958669
45.335431	1523.771234	18.963687
45.233173	1517.936097	18.968704
45.189965	1519.659741	18.973722
44.857204	1519.292155	18.978739
45.602945	1533.645495	18.983757
45.613107	1542.726835	18.988775
45.758564	1531.677076	18.993792
45.730721	1542.272928	18.998810
45.921473	1540.390504	19.003827
45.907058	1529.267959	19.008845
45.907711	1531.249834	19.013863
45.949460	1520.399377	19.018880
45.676715	1542.354091	19.023898
45.968517	1529.965360	19.028915
46.446259	1524.812564	19.033933
46.474616	1526.831125	19.038951
46.391311	1534.036675	19.043968
46.236728	1537.374695	19.048986
46.648349	1527.889630	19.054003
46.660246	1526.650646	19.059021
46.846547	1526.608856	19.064039
46.849559	1526.441140	19.069056
46.765144	1517.885911	19.074074
46.567575	1524.137319	19.079091
46.416512	1524.716462	19.084109
46.441163	1520.445741	19.089127
46.675724	1518.502804	19.094144
46.535310	1530.321870	19.099162
46.482872	1522.247650	19.104179
46.919691	1527.872616	19.109197
46.908521	1542.155195	19.114215
46.924463	1542.458850	19.119232
47.046307	1553.593022	19.124250
46.986764	1555.874681	19.129267
47.641491	1543.766768	19.134285
46.975174	1541.532606	19.139303
47.034126	1544.442675	19.144320
47.173871	1544.607006	19.149338
47.150403	1537.673861	19.154355
47.338973	1545.082985	19.159373
47.416427	1543.312991	19.164391
47.414853	1549.322249	19.169408
47.225367	1543.901580	19.174426
47.085234	1546.808125	19.179443
47.365739	1546.742107	19.184461
47.297485	1554.671183	19.189479
47.437360	1546.655188	19.194496
47.563229	1566.436127	19.199514
47.814939	1575.366024	19.204531
47.649775	1560.688190	19.209549
47.724849	1571.813920	19.214567
47.975374	1565.345950	19.219584
47.985136	1563.454009	19.224602
47.857733	1564.234585	19.229619
48.137774	1560.173164	19.234637
47.957919	1560.535901	19.239655
47.855208	1561.596647	19.244672
47.973805	1570.020347	19.249690
47.936934	1573.197912	19.254707
48.201228	1560.813470	19.259725
47.875914	1569.947385	19.264743
48.378867	1577.105283	19.269760
48.435086	1577.775034	19.274778
48.295346	1588.457878	19.279795
48.607256	1590.877015	19.284813
48.450791	1591.125627	19.289831
48.605879	1588.005326	19.294848
48.861428	1581.981557	19.299866
48.418196	1593.396803	19.304883
48.521949	1584.840465	19.309901
48.814318	1590.163016	19.314919
48.722700	1580.598970	19.319936
48.523300	1590.079262	19.324954
48.647647	1592.783421	19.329971
48.550358	1595.844217	19.334989
48.560335	1599.301642	19.340007
48.643858	1606.373779	19.345024
49.008718	1622.131318	19.350042
48.971782	1615.376989	19.355059
49.250064	1613.979490	19.360077
48.690828	1615.929169	19.365095
49.129172	1628.361407	19.370112
49.301533	1631.155885	19.375130
49.757820	1631.040235	19.380147
50.063104	1631.087107	19.385165
49.519276	1635.395058	19.390183
49.638002	1614.449076	19.395200
49.478857	1614.919029	19.400218
49.336155	1629.383240	19.405235
49.841157	1624.958336	19.410253
49.796479	1639.037946	19.415271
49.985773	1633.444288	19.420288
50.157914	1638.608955	19.425306
49.755606	1648.446137	19.430323
50.156706	1631.760677	19.435341
49.740069	1642.426972	19.440359
49.840693	1637.563617	19.445376
50.102162	1637.683629	19.450394
50.027461	1631.531695	19.455411
50.433505	1633.216522	19.460429
50.384607	1634.114197	19.465447
50.279915	1626.505736	19.470464
50.884879	1622.320806	19.475482
50.312200	1628.239677	19.480499
50.524400	1625.643785	19.485517
50.559272	1627.692897	19.490535
50.507725	1628.108120	19.495552
50.484200	1634.562685	19.500570
50.279690	1633.707914	19.505587
50.482532	1630.775796	19.510605
50.527481	1646.065896	19.515623
50.915586	1646.166067	19.520640
51.105011	1653.799178	19.525658
50.694090	1662.021845	19.530675
50.763770	1659.318882	19.535693
50.802627	1651.684764	19.540711
51.207728	1651.832769	19.545728
51.520356	1646.402831	19.550746
51.068367	1648.989001	19.555763
51.216448	1641.476639	19.560781
51.176667	1647.046920	19.565799
51.195904	1642.474043	19.570816
51.304659	1644.682005	19.575834
50.720937	1648.923622	19.580851
51.260051	1642.858561	19.585869
51.395798	1658.301713	19.590887
51.373601	1668.095131	19.595904
51.768306	1670.198331	19.600922
51.702718	1674.718558	19.605939
51.812662	1663.204038	19.610957
52.048305	1674.522439	19.615975
51.656453	1673.075286	19.620992
51.996439	1669.446289	19.626010
51.596875	1675.502165	19.631027
51.710731	1668.579014	19.636045
51.693157	1675.547089	19.641063
51.859990	1672.705818	19.646080
52.220019	1671.592172	19.651098
51.986630	1676.258619	19.656115
51.846730	1693.465011	19.661133
52.185749	1696.264948	19.666151
52.207992	1695.100075	19.671168
51.975897	1699.318172	19.676186
52.208407	1693.784001	19.681203
51.971533	1687.651143	19.686221
52.291296	1705.416730	19.691239
52.527723	1725.657080	19.696256
52.850668	1716.081662	19.701274
52.599961	1722.199443	19.706291
52.844957	1723.805363	19.711309
52.746289	1721.485396	19.716327
52.974493	1720.496549	19.721344
53.195585	1711.252691	19.726362
52.747840	1718.401798	19.731379
52.920297	1718.015015	19.736397
53.310246	1718.077027	19.741415
53.195819	1719.231142	19.746432
53.189747	1718.821834	19.751450
52.920302	1718.529536	19.756467
53.082629	1712.501393	19.761485
52.941380	1719.132233	19.766503
53.133934	1723.293271	19.771520
53.020721	1722.446285	19.776538
52.946064	1737.613181	19.781555
53.347019	1740.709555	19.786573
53.462364	1740.445337	19.791591
53.420390	1737.983932	19.796608
53.555759	1737.060126	19.801626
53.689353	1754.460427	19.806643
53.799938	1754.509401	19.811661
53.964983	1747.540327	19.816679
54.067077	1762.433383	19.821696
54.187382	1748.180916	19.826714
53.936520	1747.756308	19.831731
54.076865	1757.432784	19.836749
53.968435	1757.724369	19.841767
54.134906	1751.329466	19.846784
54.304441	1750.365589	19.851802
54.075404	1755.741479	19.856819
54.583266	1745.408032	19.861837
54.653778	1741.685532	19.866855
54.247437	1747.155475	19.871872
54.769519	1739.852736	19.876890
54.167266	1748.379992	19.881907
54.324029	1752.836998	19.886925
54.851098	1759.322115	19.891943
54.542259	1768.024331	19.896960
55.084451	1770.167556	19.901978
54.630903	1770.718354	19.906995
54.609963	1774.783457	19.912013
54.623294	1776.886457	19.917031
54.172167	1780.302544	19.922048
54.619989	1786.648599	19.927066
54.609692	1796.187740	19.932083
54.911841	1796.954678	19.937101
55.177852	1798.923411	19.942119
55.450467	1791.110589	19.947136
55.565178	1792.544410	19.952154
55.606548	1792.730469	19.957171
55.593391	1789.579685	19.962189
55.822994	1789.439586	19.967207
55.377285	1792.289898	19.972224
55.752389	1792.508881	19.977242
55.793803	1784.044272	19.982259
55.441653	1794.375482	19.987277
55.777003	1785.688082	19.992295
55.979363	1784.586508	19.997312
55.787441	1785.733832	20.002330
55.787421	1790.774028	20.007347
55.463256	1788.593531	20.012365
56.172525	1799.973515	20.017383
56.040714	1808.275603	20.022400
56.316092	1809.283438	20.027418
56.296444	1798.133141	20.032435
56.573567	1802.287260	20.037453
56.524933	1812.930714	20.042471
56.655123	1805.029739	20.047488
56.751330	1797.017319	20.052506
56.489868	1790.168704	20.057523
56.332265	1798.247595	20.062541
56.634706	1809.568240	20.067559
56.525988	1814.284622	20.072576
56.489471	1803.903880	20.077594
56.647236	1802.294860	20.082611
56.824566	1806.511955	20.087629
57.081082	1799.219240	20.092647
57.056399	1806.702912	20.097664
56.775171	1802.776715	20.102682
56.986873	1801.405414	20.107699
56.803174	1803.444607	20.112717
57.152165	1805.371936	20.117735
57.390220	1825.365975	20.122752
57.489920	1829.421657	20.127770
57.596867	1833.113260	20.132787
57.678981	1818.178706	20.137805
57.475913	1813.568027	20.142823
57.437874	1815.650676	20.147840
57.593494	1823.257596	20.152858
57.552368	1834.726767	20.157875
57.470588	1825.170516	20.162893
57.748320	1832.821429	20.167911
57.900253	1827.249345	20.172928
57.675540	1830.604719	20.177946
57.647965	1825.246966	20.182963
57.820435	1823.130675	20.187981
57.956670	1823.693219	20.192999
57.848582	1826.721029	20.198016
58.002127	1838.049241	20.203034
58.008505	1854.914110	20.208051
57.778102	1855.306863	20.213069
58.594357	1858.038367	20.218087
58.334109	1867.383161	20.223104
58.485926	1852.409254	20.228122
58.741269	1855.815661	20.233139
58.241481	1862.338615	20.238157
58.816662	1857.826914	20.243175
58.646546	1861.596649	20.248192
58.744340	1861.972698	20.253210
58.572256	1862.829720	20.258227
58.505551	1875.360197	20.263245
58.775461	1880.459120	20.268263
58.450335	1887.469151	20.273280
58.854875	1876.782561	20.278298
59.284151	1887.916114	20.283315
59.195156	1884.013433	20.288333
59.237663	1884.281372	20.293351
58.921853	1882.506683	20.298368
59.000863	1880.203042	20.303386
59.423144	1887.130689	20.308403
59.104932	1883.734172	20.313421
59.430985	1894.296878	20.318439
59.389180	1915.685650	20.323456
59.333620	1912.348969	20.328474
59.548140	1907.701244	20.333491
59.583835	1908.105960	20.338509
59.404848	1906.496039	20.343527
59.347091	1907.982140	20.348544
59.630080	1913.258917	20.353562
59.774028	1920.233342	20.358579
59.465920	1922.320444	20.363597
59.655267	1927.769700	20.368615
60.110405	1926.789472	20.373632
60.359137	1922.013297	20.378650
60.282196	1926.327068	20.383667
60.247595	1931.382189	20.388685
60.492493	1925.710296	20.393703
60.593375	1934.897551	20.398720
60.723266	1940.229884	20.403738
60.679477	1931.118940	20.408755
61.060266	1936.260472	20.413773
61.176456	1922.967950	20.418791
60.563957	1920.905200	20.423808
60.789102	1911.493335	20.428826
60.926391	1916.161732	20.433843
61.038676	1926.521246	20.438861
61.553956	1922.795302	20.443879
61.224083	1913.599791	20.448896
61.168692	1910.780675	20.453914
61.226477	1902.117771	20.458931
61.253038	1911.799533	20.463949
61.674900	1911.654559	20.468967
61.409189	1919.283348	20.473984
61.725761	1913.063701	20.479002
61.647949	1900.278154	20.484019
61.444830	1905.182933	20.489037
61.505231	1917.191713	20.494055
61.617477	1927.844746	20.499072
61.620707	1931.309604	20.504090
61.810109	1934.085680	20.509107
61.908405	1933.675796	20.514125
61.611653	1930.597824	20.519143
61.643615	1929.693366	20.524160
61.461199	1927.657913	20.529178
62.037388	1929.713774	20.534195
61.967119	1947.013649	20.539213
62.022997	1954.797211	20.544231
62.006050	1961.793704	20.549248
62.061636	1953.033281	20.554266
62.050942	1957.586008	20.559283
62.085472	1964.176774	20.564301
62.393194	1964.737703	20.569319
62.542067	1977.711040	20.574336
62.537239	1987.659713	20.579354
62.660066	1979.292719	20.584371
62.677970	1983.168731	20.589389
63.057984	1977.876472	20.594407
63.100308	1984.721665	20.599424
63.030538	1983.470196	20.604442
63.155919	1967.427275	20.609459
62.838339	1975.600743	20.614477
63.150394	1972.209611	20.619495
63.034588	1979.748661	20.624512
62.658960	1991.194594	20.629530
63.082029	1995.278551	20.634547
63.339128	2007.171360	20.639565
63.357998	2004.406872	20.644583
63.518131	2003.851588	20.649600
63.329997	2009.823952	20.654618
63.633338	2006.093324	20.659635
63.536119	2011.997791	20.664653
63.560585	2005.104297	20.669671
63.576218	2009.668692	20.674688
63.643421	2025.631026	20.679706
63.781187	2030.419309	20.684723
63.745298	2036.121656	20.689741
64.175387	2035.375740	20.694759
64.029873	2035.105047	20.699776
64.031092	2038.096831	20.704794
64.129387	2037.475488	20.709811
64.068376	2031.122439	20.714829
64.424652	2040.771549	20.719847
64.299234	2047.194885	20.724864
64.063139	2065.808532	20.729882
64.510245	2058.432198	20.734899
64.441952	2048.444489	20.739917
64.760805	2040.453887	20.744935
64.799366	2041.337879	20.749952
64.857987	2042.995122	20.754970
65.502086	2034.492778	20.759987
64.908903	2043.653121	20.765005
64.949512	2042.583186	20.770023
65.526370	2043.105107	20.775040
65.352856	2051.306535	20.780058
65.566776	2047.230117	20.785075
65.239070	2039.037832	20.790093
65.493058	2035.750467	20.795111
65.518732	2046.139400	20.800128
65.690498	2055.078906	20.805146
65.705472	2055.180733	20.810163
65.769648	2062.426510	20.815181
65.962674	2064.599228	20.820199
65.975839	2058.471253	20.825216
65.953960	2066.125022	20.830234
65.902719	2051.577272	20.835251
65.882332	2053.464663	20.840269
66.072685	2054.132354	20.845287
65.853891	2054.409674	20.850304
66.008250	2049.351581	20.855322
66.443268	2047.749598	20.860339
66.176597	2056.429565	20.865357
66.311936	2054.300129	20.870375
66.227163	2054.363930	20.875392
66.040391	2064.457928	20.880410
66.375601	2060.368815	20.885427
66.377770	2080.728328	20.890445
66.447086	2074.055017	20.895463
66.744089	2083.438859	20.900480
66.882383	2085.247738	20.905498
66.882168	2081.687742	20.910515
66.986800	2082.097441	20.915533
66.986211	2085.708107	20.920551
67.361991	2097.894834	20.925568
66.999147	2112.873650	20.930586
67.108776	2102.861191	20.935603
67.326946	2099.494213	20.940621
67.237463	2103.838396	20.945639
67.451722	2103.154697	20.950656
67.184104	2105.806727	20.955674
67.224577	2096.445791	20.960691
67.255352	2095.345833	20.965709
67.080600	2102.594343	20.970727
67.408992	2124.133664	20.975744
67.638798	2136.674677	20.980762
67.705870	2131.705982	20.985779
67.839573	2133.278880	20.990797
67.702003	2128.676793	20.995815
67.805924	2129.440087	21.000832
67.582708	2158.466891	21.005850
67.637973	2157.845974	21.010867
68.034890	2156.234170	21.015885
68.012630	2161.224301	21.020903
68.569273	2166.657113	21.025920
68.422400	2181.516934	21.030938
68.655550	2184.374565	21.035955
68.678618	2187.129400	21.040973
68.873553	2179.281239	21.045991
68.862144	2180.340340	21.051008
68.817897	2190.554102	21.056026
68.833414	2173.726562	21.061043
68.813394	2181.945029	21.066061
68.544790	2177.571762	21.071079
69.036255	2178.482642	21.076096
69.210092	2185.856467	21.081114
69.759287	2197.413278	21.086131
69.637534	2194.572954	21.091149
69.525508	2186.195317	21.096167
69.535298	2170.119828	21.101184
69.392422	2181.264304	21.106202
69.496729	2194.531984	21.111219
69.488009	2197.276020	21.116237
69.751377	2199.219964	21.121255
70.015240	2191.610330	21.126272
69.846310	2198.769595	21.131290
69.951954	2192.661802	21.136307
69.717501	2194.917293	21.141325
69.958356	2196.713271	21.146343
69.843563	2199.006824	21.151360
69.724858	2208.055038	21.156378
69.853905	2217.872401	21.161395
70.137382	2220.062529	21.166413
69.928756	2218.621339	21.171431
70.043579	2230.766983	21.176448
70.552009	2238.435579	21.181466
70.763294	2247.561512	21.186483
70.494643	2252.482964	21.191501
70.467533	2246.620035	21.196519
70.829942	2242.955851	21.201536
70.540244	2253.788827	21.206554
70.530906	2261.623769	21.211571
70.701120	2270.251171	21.216589
70.890307	2276.044574	21.221607
71.359191	2265.609631	21.226624
71.475256	2274.630563	21.231642
71.726396	2268.919712	21.236659
71.880809	2267.617318	21.241677
71.716332	2270.149060	21.246695
71.536920	2263.158009	21.251712
71.379045	2272.183986	21.256730
71.393472	2277.020064	21.261747
71.907462	2287.919667	21.266765
72.263298	2287.346337	21.271783
71.959356	2286.841660	21.276800
71.975756	2290.086753	21.281818
71.971775	2295.771558	21.286835
72.266165	2292.414695	21.291853
72.263013	2288.091338	21.296871
72.539547	2282.979321	21.301888
72.376068	2280.303326	21.306906
72.702426	2275.312906	21.311923
72.615577	2272.457632	21.316941
72.885813	2279.298791	21.321959
73.082504	2285.289856	21.326976
72.784088	2281.224221	21.331994
72.845159	2274.558440	21.337011
72.752971	2271.246367	21.342029
72.702661	2272.816546	21.347047
72.595338	2267.660522	21.352064
72.669171	2278.505992	21.357082
72.883838	2284.727793	21.362099
73.409195	2287.031526	21.367117
73.332360	2290.909824	21.372135
73.059138	2289.551340	21.377152
73.019827	2300.594448	21.382170
73.028745	2295.682162	21.387187
73.579896	2302.280482	21.392205
73.850203	2316.475391	21.397223
74.132021	2318.785723	21.402240
73.788254	2317.207893	21.407258
73.827988	2324.100963	21.412275
74.016048	2315.881398	21.417293
73.786089	2320.272891	21.422311
74.152411	2317.144618	21.427328
74.251788	2325.076175	21.432346
74.228596	2316.728745	21.437363
74.243501	2321.252304	21.442381
74.381454	2322.041836	21.447399
74.436042	2313.142525	21.452416
74.352748	2325.442362	21.457434
74.604314	2334.088610	21.462451
74.645726	2336.553387	21.467469
74.537177	2331.492220	21.472487
74.699946	2332.965898	21.477504
74.715159	2333.875656	21.482522
74.533199	2332.401874	21.487539
75.209811	2352.501377	21.492557
75.060610	2364.085657	21.497575
75.173880	2367.353460	21.502592
75.407068	2370.365766	21.507610
75.569896	2370.223501	21.512627
75.649608	2365.672527	21.517645
75.641464	2364.910043	21.522663
75.713907	2355.414563	21.527680
75.552860	2367.780264	21.532698
75.428859	2370.712819	21.537715
75.390916	2356.326858	21.542733
75.736048	2387.663639	21.547751
75.960411	2378.567266	21.552768
75.934796	2390.693992	21.557786
75.881280	2387.969191	21.562803
76.447889	2386.362343	21.567821
75.948719	2390.272114	21.572839
76.204961	2390.856904	21.577856
76.078561	2392.805126	21.582874
76.494966	2404.922575	21.587891
76.883489	2404.293622	21.592909
76.777434	2410.726679	21.597927
76.860886	2396.129142	21.602944
77.030214	2403.756254	21.607962
77.001960	2394.396462	21.612979
77.092787	2402.089527	21.617997
77.325717	2402.838932	21.623015
77.456543	2399.902193	21.628032
77.199098	2408.085371	21.633050
77.190335	2407.919491	21.638067
77.405503	2402.870709	21.643085
77.593263	2397.829379	21.648103
77.475097	2390.374199	21.653120
77.468190	2390.776132	21.658138
77.312609	2392.422781	21.663155
77.334376	2396.711731	21.668173
77.361301	2403.316474	21.673191
77.488049	2416.457713	21.678208
77.631213	2422.245750	21.683226
77.771724	2417.495869	21.688243
77.896429	2426.588115	21.693261
77.905290	2443.841353	21.698279
77.960842	2444.792139	21.703296
78.190378	2447.407356	21.708314
77.962672	2445.142229	21.713331
78.299932	2447.055687	21.718349
78.435452	2461.281297	21.723367
78.885499	2464.149178	21.728384
78.956833	2475.500141	21.733402
78.766978	2477.392034	21.738419
78.735707	2471.498123	21.743437
78.313043	2477.182303	21.748455
78.672675	2480.815514	21.753472
78.836409	2487.430415	21.758490
78.923233	2498.419165	21.763507
79.265548	2501.146124	21.768525
78.974311	2496.833134	21.773543
79.251810	2498.588685	21.778560
79.214385	2500.077961	21.783578
79.106168	2516.828847	21.788595
79.646688	2514.960959	21.793613
79.638839	2530.951282	21.798631
79.537167	2525.191473	21.803648
80.025352	2522.441749	21.808666
80.041435	2530.392758	21.813683
80.456873	2535.469069	21.818701
80.464990	2544.361867	21.823719
80.241811	2532.823233	21.828736
80.483880	2536.285506	21.833754
80.213004	2550.982002	21.838771
80.625947	2543.064809	21.843789
80.702256	2545.966009	21.848807
80.861005	2543.069058	21.853824
80.978673	2544.186862	21.858842
80.923133	2545.079310	21.863859
81.237943	2531.954058	21.868877
80.854572	2540.403205	21.873895
81.173642	2533.744249	21.878912
81.534739	2529.963436	21.883930
81.342578	2536.675145	21.888947
81.480915	2524.287682	21.893965
81.200796	2532.417658	21.898983
81.391271	2527.091812	21.904000
81.432574	2540.912478	21.909018
81.373775	2551.321249	21.914035
81.725184	2553.854265	21.919053
81.575326	2558.605693	21.924071
81.999426	2554.714006	21.929088
82.083683	2559.921115	21.934106
81.509163	2562.700197	21.939123
82.012389	2564.991654	21.944141
82.112288	2566.535169	21.949159
82.498830	2566.035925	21.954176
82.828606	2566.233617	21.959194
82.778182	2576.805212	21.964211
82.691227	2571.582786	21.969229
82.624680	2567.723782	21.974247
82.782810	2578.486790	21.979264
82.686138	2569.361715	21.984282
82.615351	2567.987273	21.989299
82.763017	2564.135738	21.994317
82.748482	2574.657523	21.999335
82.749231	2570.453421	22.004352
82.987830	2569.728019	22.009370
82.881261	2594.097693	22.014387
82.992015	2588.920034	22.019405
82.810903	2590.873693	22.024423
83.175454	2589.396326	22.029440
83.628072	2603.199940	22.034458
83.113661	2616.145098	22.039475
83.599063	2629.684790	22.044493
83.374984	2624.647953	22.049511
83.531252	2622.865506	22.054528
83.772186	2636.314102	22.059546
83.699596	2659.741157	22.064563
84.058546	2661.547087	22.069581
84.357852	2659.956846	22.074599
84.003526	2654.195549	22.079616
84.194458	2649.674421	22.084634
83.943974	2666.185772	22.089651
84.523974	2665.678310	22.094669
84.614984	2682.003613	22.099687
84.552839	2676.404840	22.104704
84.845714	2673.117582	22.109722
84.959898	2674.570495	22.114739
85.177342	2692.394121	22.119757
84.985469	2689.744607	22.124775
85.723377	2681.321951	22.129792
85.625951	2675.627708	22.134810
85.922768	2677.733742	22.139827
86.105404	2670.966708	22.144845
85.697192	2662.916153	22.149863
85.737878	2653.349743	22.154880
86.138000	2643.263066	22.159898
85.976254	2652.084689	22.164915
86.358918	2646.296302	22.169933
86.060513	2648.804893	22.174951
85.876283	2652.491786	22.179968
86.347429	2658.802938	22.184986
86.060870	2670.591993	22.190003
86.193634	2668.715383	22.195021
86.303671	2675.250393	22.200039
86.179381	2676.608109	22.205056
86.541042	2672.356907	22.210074
86.413300	2683.186860	22.215091
86.831116	2691.886139	22.220109
86.827556	2701.437330	22.225127
87.127276	2711.875242	22.230144
87.460750	2705.763142	22.235162
86.769343	2706.114516	22.240179
87.141763	2704.973619	22.245197
87.431605	2715.681356	22.250215
87.146309	2711.667222	22.255232
87.400640	2704.112521	22.260250
87.217641	2712.400952	22.265267
87.096670	2724.460781	22.270285
87.090711	2740.097500	22.275303
87.380922	2738.720142	22.280320
87.746003	2737.056466	22.285338
87.734509	2757.980687	22.290355
87.875169	2751.662066	22.295373
87.934536	2755.481250	22.300391
88.142042	2751.434085	22.305408
87.893528	2748.578815	22.310426
88.295911	2757.103797	22.315443
88.256498	2768.989912	22.320461
88.185592	2761.426175	22.325479
88.211050	2776.748696	22.330496
88.491035	2774.201989	22.335514
88.247941	2782.559835	22.340531
88.868888	2788.614004	22.345549
89.191974	2787.225180	22.350567
88.725884	2782.936359	22.355584
89.309828	2789.128886	22.360602
88.821774	2789.584118	22.365619
88.963351	2792.566661	22.370637
89.429676	2814.315604	22.375655
89.151958	2819.547937	22.380672
89.502318	2818.211649	22.385690
89.301639	2821.389849	22.390707
89.594439	2818.052077	22.395725
90.107462	2831.840091	22.400743
89.891085	2848.213704	22.405760
90.292620	2840.455980	22.410778
89.890894	2840.399006	22.415795
90.356454	2838.201961	22.420813
90.720150	2828.827879	22.425831
90.304709	2842.496245	22.430848
90.939151	2830.352780	22.435866
90.709197	2824.202666	22.440883
90.412660	2830.668871	22.445901
90.777953	2839.941412	22.450919
90.490833	2848.555526	22.455936
90.917783	2855.492289	22.460954
91.232133	2859.164235	22.465971
91.099332	2863.190297	22.470989
91.370276	2858.391459	22.476007
90.916741	2863.667132	22.481024
91.430986	2869.665453	22.486042
91.301643	2879.836125	22.491059
91.392992	2885.427276	22.496077
91.763952	2882.942050	22.501095
91.666966	2889.206576	22.506112
91.681720	2891.252672	22.511130
91.795253	2892.301709	22.516147
92.270129	2901.459270	22.521165
92.416690	2909.254287	22.526183
92.223794	2910.348178	22.531200
92.599412	2903.045827	22.536218
92.463773	2902.896665	22.541235
92.724265	2909.155691	22.546253
92.762297	2904.257614	22.551271
92.750639	2911.805986	22.556288
92.912450	2898.095289	22.561306
92.967030	2909.777398	22.566323
92.957057	2903.678010	22.571341
92.789374	2914.728982	22.576359
93.076038	2918.963929	22.581376
93.353957	2927.413806	22.586394
92.668048	2930.645953	22.591411
92.863557	2931.331808	22.596429
93.733081	2938.524355	22.601447
93.271864	2947.377259	22.606464
93.697300	2956.498408	22.611482
93.609274	2951.051947	22.616499
93.821889	2946.435817	22.621517
93.903249	2968.579819	22.626535
93.789247	2975.260507	22.631552
94.297876	2981.584838	22.636570
94.314173	2981.402403	22.641587
94.761848	2979.236549	22.646605
94.703597	2973.551855	22.651623
94.434465	2977.656114	22.656640
94.594392	2975.210251	22.661658
94.743010	2981.464736	22.666675
94.872983	2979.828404	22.671693
94.853488	2979.711545	22.676711
94.930706	2992.157125	22.681728
95.134700	3003.500262	22.686746
95.217889	3009.783945	22.691763
95.291974	3005.154785	22.696781
95.123796	3000.702457	22.701799
95.327828	3004.476935	22.706816
95.473494	3013.638788	22.711834
95.662693	3026.950595	22.716851
95.522075	3025.407153	22.721869
95.900711	3024.713450	22.726887
95.521594	3028.023798	22.731904
95.710004	3025.570309	22.736922
95.975498	3043.888598	22.741939
95.897292	3045.352746	22.746957
96.062287	3051.188065	22.751975
95.837435	3059.445336	22.756992
96.714235	3061.747769	22.762010
96.679753	3072.118312	22.767027
96.549353	3068.764735	22.772045
96.909693	3069.765646	22.777063
97.777583	3063.989481	22.782080
97.679731	3056.350936	22.787098
97.539740	3057.404984	22.792115
97.423797	3070.316442	22.797133
97.694299	3053.571225	22.802151
97.221027	3055.681175	22.807168
97.438478	3055.962754	22.812186
97.588245	3056.497968	22.817203
97.836352	3063.986769	22.822221
98.416153	3069.741325	22.827239
98.132246	3081.331388	22.832256
98.402055	3075.396421	22.837274
98.495577	3076.647448	22.842291
98.775470	3077.310619	22.847309
98.681637	3064.845536	22.852327
98.487706	3070.566657	22.857344
98.437782	3074.778626	22.862362
98.550090	3079.356553	22.867379
98.195594	3081.804552	22.872397
98.503371	3078.947293	22.877415
98.430244	3091.877309	22.882432
98.545276	3091.007121	22.887450
98.591371	3090.327641	22.892467
98.745387	3100.138418	22.897485
98.942950	3117.286986	22.902503
99.292977	3122.862932	22.907520
99.222068	3131.784182	22.912538
99.492061	3135.333729	22.917555
99.490842	3146.630200	22.922573
99.375664	3151.158567	22.927591
99.508938	3166.909561	22.932608
99.431603	3161.060516	22.937626
99.273492	3173.296901	22.942643
99.261015	3183.553592	22.947661
99.749783	3192.586032	22.952679
100.076705	3206.902181	22.957696
100.202442	3213.747399	22.962714
100.348515	3221.031311	22.967731
100.776035	3232.866670	22.972749
101.057461	3235.609595	22.977767
100.918666	3240.261622	22.982784
100.848041	3229.342522	22.987802
101.179465	3233.589469	22.992819
101.321515	3240.997114	22.997837
101.420354	3228.192417	23.002855
101.447724	3231.344428	23.007872
101.329962	3246.393096	23.012890
101.944771	3249.819205	23.017907
101.714332	3249.321919	23.022925
101.897671	3243.318382	23.027943
101.874418	3255.211753	23.032960
101.812953	3261.947442	23.037978
102.064658	3245.334401	23.042995
102.206435	3253.291287	23.048013
102.130368	3254.325862	23.053031
102.396432	3263.386916	23.058048
102.094031	3274.907406	23.063066
102.665470	3270.004568	23.068083
102.466281	3280.666164	23.073101
102.546327	3284.463282	23.078119
102.469660	3291.195051	23.083136
102.769698	3301.257657	23.088154
102.960489	3305.192088	23.093171
102.679445	3307.615984	23.098189
103.489089	3308.533892	23.103207
103.575737	3317.114920	23.108224
103.809739	3329.703452	23.113242
104.029928	3319.382619	23.118259
103.752176	3318.431926	23.123277
104.432208	3317.122860	23.128295
104.140335	3316.575228	23.133312
103.859984	3326.176427	23.138330
104.342554	3314.864445	23.143347
104.051141	3309.970529	23.148365
104.263422	3316.110999	23.153383
104.229457	3342.575553	23.158400
104.364922	3347.528676	23.163418
104.809795	3346.089168	23.168435
104.779872	3345.626747	23.173453
104.789444	3342.620476	23.178471
104.890265	3354.548131	23.183488
105.095204	3366.165947	23.188506
105.099292	3367.702447	23.193523
105.240331	3373.285964	23.198541
105.016774	3369.508200	23.203559
105.489296	3390.291040	23.208576
105.199339	3397.043639	23.213594
105.329630	3404.421630	23.218611
105.068338	3415.301351	23.223629
105.549895	3421.011443	23.228647
105.932076	3424.619222	23.233664
106.295236	3428.365703	23.238682
106.555298	3437.664508	23.243699
106.749030	3444.931575	23.248717
106.715084	3448.232108	23.253735
106.728360	3456.234467	23.258752
106.354584	3453.102014	23.263770
106.855028	3453.165667	23.268787
106.645783	3463.589065	23.273805
106.726723	3449.111011	23.278823
107.042256	3463.318678	23.283840
106.893146	3480.667095	23.288858
107.071496	3477.157755	23.293875
107.124966	3490.854145	23.298893
107.439280	3491.224715	23.303911
107.905624	3497.824142	23.308928
108.035031	3492.412891	23.313946
108.016012	3498.621224	23.318963
107.995478	3503.576736	23.323981
107.995222	3493.675413	23.328999
108.249589	3493.383079	23.334016
108.169073	3495.172725	23.339034
108.352007	3500.913847	23.344051
108.142299	3517.612121	23.349069
108.824839	3506.180314	23.354087
109.146874	3500.751508	23.359104
109.247596	3511.596663	23.364122
109.515058	3504.819186	23.369139
109.668286	3502.304863	23.374157
109.913096	3489.439235	23.379175
110.280109	3488.706305	23.384192
109.937157	3471.665428	23.389210
110.164244	3458.698441	23.394227
110.007132	3462.068774	23.399245
109.974414	3459.271114	23.404263
109.966224	3459.240856	23.409280
110.137143	3452.181830	23.414298
110.023071	3443.564048	23.419315
110.018202	3448.883223	23.424333
110.193202	3455.717658	23.429351
110.657573	3461.992280	23.434368
110.288041	3478.194766	23.439386
110.481889	3474.316865	23.444403
110.770879	3479.305942	23.449421
110.924641	3478.937836	23.454439
110.928624	3480.685836	23.459456
110.768510	3500.551584	23.464474
111.279789	3502.308485	23.469491
111.261377	3510.729311	23.474509
111.592009	3503.960874	23.479527
111.492748	3499.339809	23.484544
111.385177	3503.630347	23.489562
111.794041	3508.070389	23.494579
111.651404	3519.534440	23.499597
111.577362	3534.500747	23.504615
111.767655	3532.596097	23.509632
111.983368	3543.237033	23.514650
112.218851	3544.532134	23.519667
112.057798	3563.062969	23.524685
112.202390	3569.472950	23.529703
112.381868	3571.853138	23.534720
112.110175	3588.097208	23.539738
112.315990	3588.342744	23.544755
112.592513	3593.217020	23.549773
112.506917	3604.306053	23.554791
112.754299	3617.782779	23.559808
112.568607	3624.771634	23.564826
112.972250	3634.306867	23.569843
112.934734	3649.027663	23.574861
113.156447	3668.016279	23.579879
113.482312	3676.998733	23.584896
113.550987	3675.065777	23.589914
113.826802	3674.719578	23.594931
114.020266	3694.744775	23.599949
113.750723	3709.467251	23.604967
114.270596	3696.195402	23.609984
114.107211	3703.111353	23.615002
114.072570	3719.147957	23.620019
114.425193	3732.008571	23.625037
114.430515	3736.003717	23.630055
115.186269	3712.029549	23.635072
114.984325	3735.244693	23.640090
115.074722	3750.043378	23.645107
115.180157	3754.467891	23.650125
115.201285	3753.833330	23.655143
115.408557	3748.173077	23.660160
115.448477	3750.641438	23.665178
115.314830	3772.173054	23.670195
115.660921	3775.616114	23.675213
115.648787	3777.477141	23.680231
115.765864	3777.891245	23.685248
115.744549	3784.194726	23.690266
116.057307	3795.843272	23.695283
116.290260	3801.567184	23.700301
116.516378	3795.263219	23.705319
116.435872	3797.242277	23.710336
116.523531	3809.165981	23.715354
116.556690	3821.518031	23.720371
117.009259	3827.015004	23.725389
116.788563	3832.478579	23.730407
117.123659	3822.155240	23.735424
116.996663	3831.881029	23.740442
117.047124	3838.754059	23.745459
117.615912	3843.522644	23.750477
117.131386	3842.989395	23.755495
117.661383	3843.108392	23.760512
117.800172	3861.990261	23.765530
117.926597	3860.414378	23.770547
118.336990	3862.468040	23.775565
118.135815	3871.930867	23.780583
118.544849	3863.211992	23.785600
118.184005	3874.429535	23.790618
118.839848	3876.630972	23.795635
118.943585	3893.662408	23.800653
118.383988	3894.428727	23.805671
118.629002	3894.882761	23.810688
118.679972	3899.880837	23.815706
118.504272	3912.786475	23.820723
119.154464	3912.801420	23.825741
118.848636	3928.126317	23.830759
119.313209	3936.607396	23.835776
119.172562	3942.797060	23.840794
119.391775	3948.810403	23.845811
119.651936	3969.084279	23.850829
119.556241	3972.527151	23.855847
119.705211	3972.762660	23.860864
119.558116	3996.556636	23.865882
119.968873	4001.744573	23.870899
120.141503	4007.342275	23.875917
120.314164	4016.948619	23.880935
120.791236	4029.777322	23.885952
120.731837	4032.583236	23.890970
121.104516	4031.483254	23.895987
121.100039	4037.945163	23.901005
121.312636	4046.917139	23.906023
121.885951	4046.726336	23.911040
121.759694	4048.116025	23.916058
121.840573	4046.408380	23.921075
122.012668	4044.727478	23.926093
121.747457	4047.767648	23.931111
121.755302	4042.005979	23.936128
121.900341	4063.813077	23.941146
122.153898	4066.891921	23.946163
122.356844	4076.749222	23.951181
121.957647	4079.210669	23.956199
122.556830	4072.904977	23.961216
122.826310	4093.606806	23.966234
122.571944	4097.869979	23.971251
123.030295	4087.975393	23.976269
123.059913	4105.271154	23.981287
123.606105	4104.513287	23.986304
123.347981	4124.426635	23.991322
123.453280	4127.847516	23.996339
123.683156	4127.107640	24.001357
123.709034	4131.753035	24.006375
123.333910	4123.968092	24.011392
123.845467	4130.377596	24.016410
124.287704	4140.939204	24.021427
124.744636	4155.093699	24.026445
124.804423	4142.247128	24.031463
125.030287	4142.467437	24.036480
124.568990	4126.703901	24.041498
124.802639	4137.910535	24.046515
125.179853	4145.316429	24.051533
124.781218	4144.072141	24.056551
125.170764	4136.666111	24.061568
125.107489	4138.011218	24.066586
124.993188	4134.759083	24.071603
125.029694	4138.493761	24.076621
125.129318	4158.619396	24.081639
125.613003	4153.108256	24.086656
125.518916	4168.106632	24.091674
125.297252	4167.134479	24.096691
125.770080	4185.052139	24.101709
125.657988	4187.017249	24.106727
126.155550	4199.157915	24.111744
125.972413	4212.576275	24.116762
126.013467	4214.709937	24.121779
126.240949	4227.546320	24.126797
125.875616	4250.282687	24.131815
126.793351	4239.305983	24.136832
127.099252	4249.500771	24.141850
127.050746	4264.567841	24.146867
127.139557	4270.128253	24.151885
126.803016	4282.607979	24.156903
127.356694	4274.822654	24.161920
127.228043	4288.917486	24.166938
127.355122	4299.538032	24.171955
127.850781	4307.783995	24.176973
127.730167	4320.365645	24.181991
127.929383	4319.920960	24.187008
128.245044	4336.727066	24.192026
128.507792	4338.999616	24.197043
128.546782	4340.338187	24.202061
128.950313	4333.030893	24.207079
129.247073	4330.033126	24.212096
129.560205	4325.558723	24.217114
129.396037	4325.019458	24.222131
129.630559	4325.497243	24.227149
129.787241	4325.529536	24.232167
129.537468	4321.872467	24.237184
129.963181	4334.883040	24.242202
129.745995	4339.295112	24.247219
130.239991	4344.665809	24.252237
130.297740	4347.892167	24.257255
130.123160	4348.901203	24.262272
130.670972	4344.516288	24.267290
130.309373	4346.918220	24.272307
130.409258	4339.115582	24.277325
130.506820	4356.947007	24.282343
130.576265	4365.906847	24.287360
130.505022	4370.977861	24.292378
130.684214	4382.745561	24.297395
131.133462	4391.525965	24.302413
131.258151	4405.003561	24.307431
131.298689	4397.891995	24.312448
131.401454	4405.533540	24.317466
131.635883	4424.833448	24.322483
131.646464	4426.021808	24.327501
132.080988	4424.419704	24.332519
131.922261	4427.127606	24.337536
132.152809	4440.913761	24.342554
132.185904	4451.258724	24.347571
132.508685	4450.198101	24.352589
132.212578	4462.744214	24.357607
132.446427	4466.287061	24.362624
132.981867	4472.951778	24.367642
132.021482	4477.019470	24.372659
132.797771	4477.645963	24.377677
132.815296	4499.640856	24.382695
133.332545	4493.433083	24.387712
133.865619	4500.123433	24.392730
133.727050	4493.996309	24.397747
133.763651	4501.398896	24.402765
133.863324	4511.799749	24.407783
134.563030	4516.974132	24.412800
134.649719	4522.718031	24.417818
134.399807	4524.679516	24.422835
134.495078	4521.612276	24.427853
134.667389	4528.302339	24.432871
134.574045	4538.379918	24.437888
134.619525	4543.445319	24.442906
134.861325	4553.151593	24.447923
134.980883	4547.769981	24.452941
135.138774	4558.887736	24.457959
134.988331	4573.292383	24.462976
135.222429	4576.345954	24.467994
135.130430	4579.876743	24.473011
135.377021	4595.421836	24.478029
135.679291	4597.486211	24.483047
135.788041	4620.789539	24.488064
135.882437	4626.112446	24.493082
136.424996	4640.405419	24.498099
136.500976	4632.230775	24.503117
136.052602	4643.036372	24.508135
136.300937	4652.741676	24.513152
136.478445	4660.605200	24.518170
136.753995	4686.344570	24.523187
137.104118	4678.373165	24.528205
136.975027	4687.339016	24.533223
136.833041	4710.530227	24.538240
137.482046	4715.396957	24.543258
137.758213	4713.775447	24.548275
138.229544	4727.467280	24.553293
138.121683	4735.306101	24.558311
138.299108	4736.701926	24.563328
138.427787	4735.356043	24.568346
138.251130	4746.501073	24.573363
138.479239	4743.548716	24.578381
138.794372	4760.803526	24.583399
139.002021	4762.791205	24.588416
139.203601	4759.997672	24.593434
138.922920	4763.302377	24.598451
139.102561	4770.976223	24.603469
139.336481	4785.103018	24.608487
139.257834	4797.694206	24.613504
139.750183	4790.132918	24.618522
139.463636	4805.168284	24.623539
139.672340	4816.183539	24.628557
139.843044	4814.319705	24.633575
140.078717	4834.364800	24.638592
140.398748	4835.618342	24.643610
140.320710	4845.277027	24.648627
140.871377	4837.596104	24.653645
140.896205	4851.626290	24.658663
141.129513	4854.774729	24.663680
141.405598	4848.828735	24.668698
141.275007	4868.713446	24.673715
141.139151	4860.575044	24.678733
141.213910	4871.551343	24.683751
141.376411	4871.102928	24.688768
141.968219	4880.309468	24.693786
142.183637	4886.898213	24.698803
142.171957	4876.496032	24.703821
142.308632	4888.078170	24.708839
142.496783	4898.657933	24.713856
142.840207	4894.469052	24.718874
142.491947	4912.339301	24.723891
142.977332	4914.652803	24.728909
142.966186	4907.037772	24.733927
142.830818	4910.130343	24.738944
143.019154	4919.911478	24.743962
143.281666	4928.481500	24.748979
143.374213	4936.652015	24.753997
143.463720	4944.264298	24.759015
143.131383	4943.994416	24.764032
143.951737	4961.530116	24.769050
143.480729	4958.882960	24.774067
143.856194	4971.362088	24.779085
144.104739	4985.379424	24.784103
144.197864	4986.826355	24.789120
144.674165	4994.037149	24.794138
144.457009	5013.348456	24.799155
144.795698	5014.138226	24.804173
145.177481	5011.628926	24.809191
145.294320	5022.194680	24.814208
145.534255	5034.158464	24.819226
145.525292	5038.026714	24.824243
145.637573	5046.999119	24.829261
145.970593	5044.566898	24.834279
145.885484	5052.512772	24.839296
146.182854	5061.197345	24.844314
145.926294	5071.499654	24.849331
145.891770	5068.017047	24.854349
146.328398	5075.764398	24.859367
146.209004	5095.950636	24.864384
146.523643	5094.515618	24.869402
146.643991	5115.627082	24.874419
146.680136	5130.157609	24.879437
147.095012	5124.868452	24.884455
147.266450	5144.892386	24.889472
147.221088	5145.309875	24.894490
147.183252	5161.944850	24.899507
147.419063	5174.666959	24.904525
147.679444	5178.085839	24.909543
148.079941	5198.560065	24.914560
148.140910	5200.712820	24.919578
148.241319	5200.233089	24.924595
148.209525	5216.778782	24.929613
148.416679	5221.490754	24.934631
148.473708	5232.163855	24.939648
149.390741	5237.159195	24.944666
149.399170	5255.933513	24.949683
149.285686	5252.087602	24.954701
149.597339	5246.139064	24.959719
149.047084	5264.880965	24.964736
149.766859	5272.224185	24.969754
149.828541	5275.308043	24.974771
149.834953	5289.120486	24.979789
150.239675	5299.439275	24.984807
150.068099	5306.827454	24.989824
150.321539	5305.288369	24.994842
150.698223	5324.993092	24.999859
150.669702	5331.137250	25.004877
150.950331	5329.196166	25.009895
150.703765	5348.196769	25.014912
151.360282	5364.694738	25.019930
151.295557	5358.855635	25.024947
151.646454	5364.170140	25.029965
151.509357	5371.565570	25.034983
151.838962	5383.051508	25.040000
152.001014	5377.950250	25.045018
152.172432	5382.175425	25.050035
152.305750	5397.701069	25.055053
152.617505	5409.549679	25.060071
152.299965	5416.067436	25.065088
152.806214	5409.902116	25.070106
152.630236	5421.375743	25.075123
153.011742	5435.943950	25.080141
153.670494	5440.919835	25.085159
153.549260	5438.647116	25.090176
153.871210	5429.467643	25.095194
153.780528	5439.557928	25.100211
154.008021	5436.160469	25.105229
154.126868	5448.718008	25.110247
154.437850	5456.762993	25.115264
154.549546	5455.350272	25.120282
154.771831	5461.726653	25.125299
154.582242	5457.153963	25.130317
154.905387	5453.940384	25.135335
154.734807	5478.604898	25.140352
154.759936	5473.190458	25.145370
155.211732	5483.413591	25.150387
155.229017	5500.112841	25.155405
155.415590	5498.236982	25.160423
155.075248	5502.583396	25.165440
155.532572	5521.028813	25.170458
155.738415	5535.662501	25.175475
155.784880	5551.833219	25.180493
155.980659	5555.107614	25.185511
156.063611	5574.129431	25.190528
156.202876	5579.480311	25.195546
156.473927	5593.712401	25.200563
156.274757	5606.585032	25.205581
156.909423	5612.417044	25.210599
156.943769	5637.191718	25.215616
157.162385	5647.915508	25.220634
157.441509	5646.003038	25.225651
158.240971	5661.749686	25.230669
158.075509	5661.822981	25.235687
157.921680	5669.685187	25.240704
158.263822	5667.687082	25.245722
158.427413	5675.370137	25.250739
158.499863	5687.764647	25.255757
158.626288	5692.240009	25.260775
158.895816	5699.887538	25.265792
158.939682	5703.908644	25.270810
159.136947	5718.569076	25.275827
158.749542	5726.423706	25.280845
159.506704	5735.320673	25.285863
159.377824	5750.688822	25.290880
159.490773	5748.060547	25.295898
159.856557	5760.472286	25.300915
159.987984	5774.435973	25.305933
159.944581	5777.997260	25.310951
160.535486	5795.550773	25.315968
160.471061	5807.528024	25.320986
160.585113	5812.333653	25.326003
160.605496	5813.627896	25.331021
161.036337	5825.732755	25.336039
160.772238	5838.221130	25.341056
161.017261	5849.903704	25.346074
161.386460	5861.917228	25.351091
161.712739	5875.591614	25.356109
162.090725	5885.671856	25.361127
162.038366	5888.937835	25.366144
162.005317	5887.639303	25.371162
162.499617	5899.424909	25.376179
162.548650	5905.108852	25.381197
162.767245	5910.961950	25.386215
162.985769	5921.666975	25.391232
162.833421	5923.777472	25.396250
163.125094	5922.917361	25.401267
163.171545	5930.767242	25.406285
163.340766	5935.336975	25.411303
163.632069	5953.853034	25.416320
163.614880	5957.678573	25.421338
164.215429	5956.823735	25.426355
163.826779	5965.436280	25.431373
164.120243	5983.702647	25.436391
164.394781	5993.126767	25.441408
164.820695	5985.114513	25.446426
165.038906	5993.452064	25.451443
165.022755	6006.125838	25.456461
165.183642	6013.443275	25.461479
165.249749	6008.972442	25.466496
165.229425	6025.921134	25.471514
165.737022	6030.835631	25.476531
165.454924	6046.322734	25.481549
165.685609	6054.989819	25.486567
165.878270	6064.950826	25.491584
166.167842	6064.873916	25.496602
166.537015	6080.388445	25.501619
166.379559	6086.281572	25.506637
166.571589	6094.291810	25.511655
166.603270	6102.336641	25.516672
166.891406	6114.988074	25.521690
166.992939	6118.921318	25.526707
167.514651	6142.098756	25.531725
167.943950	6145.324046	25.536743
167.909094	6147.425633	25.541760
167.925152	6153.515730	25.546778
168.831082	6157.982731	25.551795
168.588317	6168.908536	25.556813
168.991984	6163.639781	25.561831
169.064629	6160.446384	25.566848
168.637950	6167.982205	25.571866
169.013207	6172.194570	25.576883
169.353212	6186.719371	25.581901
169.595384	6182.703901	25.586919
169.746305	6189.183265	25.591936
169.438861	6209.081353	25.596954
170.088227	6217.518770	25.601971
169.914543	6219.449550	25.606989
170.207865	6220.025509	25.612007
170.178462	6242.493901	25.617024
169.999715	6245.123129	25.622042
170.543978	6260.701928	25.627059
170.492214	6275.196628	25.632077
170.860091	6282.393355	25.637095
171.512886	6292.765391	25.642112
171.458930	6300.504889	25.647130
171.685314	6307.294467	25.652147
171.413638	6319.913784	25.657165
172.046682	6324.164719	25.662183
171.784790	6330.708805	25.667200
171.822012	6354.022393	25.672218
172.096886	6348.230789	25.677236
172.199681	6364.854295	25.682253
172.307706	6379.586060	25.687271
172.245906	6389.302994	25.692288
172.787608	6401.877020	25.697306
173.371533	6409.049420	25.702324
173.784693	6420.589216	25.707341
174.428875	6407.078116	25.712359
174.851340	6409.651061	25.717376
174.734701	6418.296968	25.722394
174.550704	6411.282933	25.727412
174.564997	6416.404248	25.732429
174.503965	6413.017085	25.737447
175.228906	6410.649562	25.742464
174.670888	6416.498216	25.747482
174.680195	6424.524597	25.752500
175.359894	6435.738531	25.757517
174.990725	6440.045484	25.762535
175.275996	6449.670196	25.767552
175.311982	6471.172103	25.772570
175.757257	6474.827437	25.777588
175.953791	6493.128439	25.782605
176.009529	6504.045561	25.787623
176.256361	6509.578744	25.792640
176.126826	6530.948810	25.797658
176.267511	6534.345659	25.802676
176.347556	6548.276947	25.807693
176.671696	6557.927194	25.812711
176.850133	6576.006978	25.817728
177.014254	6600.440622	25.822746
177.369895	6600.002950	25.827764
177.472385	6618.527163	25.832781
177.910502	6628.367944	25.837799
178.034082	6642.200934	25.842816
178.228874	6655.208305	25.847834
178.167707	6658.087505	25.852852
178.452046	6677.511408	25.857869
178.634093	6683.660913	25.862887
179.193120	6695.039128	25.867904
178.705475	6710.069674	25.872922
179.164898	6714.793022	25.877940
179.402568	6720.236154	25.882957
179.819915	6729.638281	25.887975
180.326529	6740.238672	25.892992
180.414755	6747.450982	25.898010
180.798727	6739.205050	25.903028
180.380404	6743.257752	25.908045
180.634777	6767.781658	25.913063
181.029002	6785.089129	25.918080
180.772248	6785.404025	25.923098
181.000909	6794.302231	25.928116
181.329039	6804.558107	25.933133
181.615348	6817.052466	25.938151
181.766908	6836.412103	25.943168
181.654328	6846.572886	25.948186
181.704859	6848.841119	25.953204
181.685772	6861.386510	25.958221
181.697091	6878.457307	25.963239
182.309240	6887.077653	25.968256
182.558290	6920.325137	25.973274
182.778781	6925.000735	25.978292
182.969955	6946.753538	25.983309
183.115063	6953.953860	25.988327
183.373574	6971.708953	25.993344
183.917130	6975.497367	25.998362
184.588724	6973.425414	26.003380
184.899163	6973.231584	26.008397
184.715664	6973.768619	26.013415
185.011336	6969.905601	26.018432
185.234757	6985.008075	26.023450
185.559406	6994.314369	26.028468
185.404333	6993.697829	26.033485
185.359738	6995.775783	26.038503
185.786524	6986.541229	26.043520
185.802730	7003.693457	26.048538
185.851444	7023.094658	26.053556
185.935563	7032.312375	26.058573
185.958197	7036.823268	26.063591
186.421335	7038.007195	26.068608
186.207371	7060.054057	26.073626
186.475020	7059.112423	26.078644
186.577653	7073.933983	26.083661
186.554587	7082.013077	26.088679
187.139086	7094.763977	26.093696
186.961083	7118.367963	26.098714
187.395550	7124.626448	26.103732
187.573945	7135.527886	26.108749
187.871878	7140.005147	26.113767
188.243959	7159.213769	26.118784
187.923067	7173.173614	26.123802
188.319095	7175.551924	26.128820
188.518831	7188.116924	26.133837
188.570946	7198.147920	26.138855
189.015703	7206.971431	26.143872
188.690861	7225.616870	26.148890
189.197422	7244.725589	26.153908
189.433765	7254.560435	26.158925
189.828504	7278.160137	26.163943
189.951669	7277.844109	26.168960
190.004441	7288.275987	26.173978
189.724051	7300.919438	26.178996
190.119002	7315.313404	26.184013
190.313491	7341.163916	26.189031
190.818385	7338.764457	26.194048
190.820461	7358.040723	26.199066
191.316473	7378.979132	26.204084
191.170211	7388.365712	26.209101
191.644217	7405.544461	26.214119
192.172429	7406.004738	26.219136
192.301660	7429.763038	26.224154
192.272870	7440.504537	26.229172
193.098478	7436.173249	26.234189
193.156037	7427.179427	26.239207
193.427330	7438.678949	26.244224
193.484770	7451.345347	26.249242
193.728395	7451.768126	26.254260
194.094529	7456.329490	26.259277
194.175191	7459.401272	26.264295
194.732471	7470.079388	26.269312
194.662273	7471.728896	26.274330
195.190641	7474.891550	26.279348
195.413704	7471.882725	26.284365
195.298331	7476.901525	26.289383
195.682672	7471.834320	26.294400
195.399599	7480.402616	26.299418
195.550396	7476.672685	26.304436
195.819580	7486.183652	26.309453
195.803189	7495.692007	26.314471
195.871314	7503.914849	26.319488
196.210678	7522.390235	26.324506
196.230322	7527.526806	26.329524
196.514053	7533.654352	26.334541
196.223221	7567.164375	26.339559
196.885326	7564.231978	26.344576
196.958471	7578.483986	26.349594
197.212380	7586.197892	26.354612
197.245864	7600.503486	26.359629
197.317502	7620.125872	26.364647
197.709359	7615.032195	26.369664
197.750030	7640.458926	26.374682
197.958387	7653.799525	26.379700
197.984732	7666.957125	26.384717
197.866276	7688.850865	26.389735
198.234929	7692.032265	26.394752
198.563233	7721.066749	26.399770
198.807761	7729.337826	26.404788
199.284503	7747.081579	26.409805
198.957233	7759.192829	26.414823
199.560731	7767.445572	26.419840
199.845483	7781.825597	26.424858
199.978112	7794.515178	26.429876
200.214247	7803.722094	26.434893
200.320858	7829.242938	26.439911
200.422114	7832.478880	26.444928
200.373770	7849.332613	26.449946
200.695854	7867.463774	26.454964
201.319973	7880.546822	26.459981
201.163638	7898.282557	26.464999
201.702352	7894.715924	26.470016
202.042801	7912.970536	26.475034
202.313455	7923.630677	26.480052
202.401905	7931.058097	26.485069
202.670967	7948.117920	26.490087
203.171070	7944.011150	26.495104
203.318880	7952.480590	26.500122
202.961326	7979.728673	26.505140
203.371618	7982.991999	26.510157
203.545775	7996.186663	26.515175
203.933906	8013.780385	26.520192
204.174288	8023.930719	26.525210
204.228191	8034.037660	26.530228
204.549384	8045.179305	26.535245
204.524705	8056.479326	26.540263
204.837145	8064.559960	26.545280
205.100064	8075.057231	26.550298
205.136723	8085.160586	26.555316
205.256927	8100.210688	26.560333
205.329953	8119.849173	26.565351
205.464710	8126.578008	26.570368
205.574460	8146.899020	26.575386
205.815716	8164.945265	26.580404
205.972231	8180.864268	26.585421
206.151942	8200.309325	26.590439
206.667562	8203.322563	26.595456
207.249056	8224.778941	26.600474
207.140296	8240.982653	26.605492
207.817795	8255.759305	26.610509
207.799075	8265.852491	26.615527
208.076430	8270.841553	26.620544
208.345798	8292.018563	26.625562
208.118089	8301.658308	26.630580
208.668512	8305.565898	26.635597
208.821553	8325.008951	26.640615
209.084824	8332.885875	26.645632
209.288166	8344.497638	26.650650
209.088298	8346.019150	26.655668
209.215945	8372.970797	26.660685
209.359455	8394.764345	26.665703
209.437393	8401.154893	26.670720
209.882221	8420.217675	26.675738
210.191577	8441.555921	26.680756
211.119600	8448.087987	26.685773
211.101938	8471.062400	26.690791
211.585445	8471.697043	26.695808
211.491455	8485.350810	26.700826
211.677135	8497.584243	26.705844
211.917312	8501.092158	26.710861
212.069893	8512.462561	26.715879
212.331318	8516.541758	26.720896
212.575000	8515.187059	26.725914
212.760619	8534.612599	26.730932
213.155070	8539.605491	26.735949
213.343850	8550.139904	26.740967
213.363069	8564.486363	26.745984
213.571998	8569.647243	26.751002
213.302161	8582.757177	26.756020
213.734385	8588.268259	26.761037
213.912050	8600.679819	26.766055
214.197173	8612.004261	26.771072
214.499285	8627.916626	26.776090
214.460722	8632.058630	26.781108
214.837728	8648.379188	26.786125
214.956415	8662.621739	26.791143
215.244774	8678.618389	26.796160
215.475426	8685.332405	26.801178
215.737886	8703.634744	26.806196
215.770046	8707.099513	26.811213
215.488987	8727.435027	26.816231
216.034907	8736.104509	26.821248
216.491603	8762.746282	26.826266
216.656893	8777.628852	26.831284
216.943290	8792.198839	26.836301
216.593957	8807.026292	26.841319
216.862936	8819.363705	26.846336
217.486979	8840.204785	26.851354
217.729916	8857.493703	26.856372
217.911271	8863.817694	26.861389
218.170137	8888.886759	26.866407
218.469212	8898.460074	26.871424
219.144130	8910.550834	26.876442
218.979980	8919.893632	26.881460
219.246170	8938.672364	26.886477
219.577228	8951.776827	26.891495
219.747036	8962.557556	26.896512
220.055521	8963.601666	26.901530
219.849869	8982.880591	26.906548
220.446375	8998.393541	26.911565
220.367281	9006.674844	26.916583
220.299085	9024.227353	26.921600
221.265055	9033.813083	26.926618
220.916430	9052.779807	26.931636
221.545366	9066.645950	26.936653
221.564627	9083.054507	26.941671
221.561599	9094.329666	26.946688
222.108374	9107.754062	26.951706
222.195776	9136.364383	26.956724
222.740216	9139.891059	26.961741
222.969951	9159.171421	26.966759
223.242890	9174.536298	26.971776
223.660385	9176.551577	26.976794
223.293425	9204.323880	26.981812
223.589540	9210.191145	26.986829
223.920244	9227.018321	26.991847
223.972045	9236.197997	26.996864
224.719551	9243.926833	27.001882
224.719367	9257.658034	27.006900
224.977360	9273.135840	27.011917
225.144009	9285.745337	27.016935
225.102770	9296.736132	27.021952
225.633964	9325.485605	27.026970
225.619150	9330.549140	27.031988
226.099487	9338.026239	27.037005
226.512684	9343.079559	27.042023
226.557865	9362.073310	27.047040
227.121599	9382.532939	27.052058
226.963944	9384.654129	27.057076
227.516267	9400.512173	27.062093
227.692133	9408.191707	27.067111
227.373964	9418.076685	27.072128
227.788903	9429.292885	27.077146
227.594763	9446.745542	27.082164
228.182023	9459.800757	27.087181
228.063164	9471.539476	27.092199
228.618066	9487.602418	27.097216
228.641920	9497.181269	27.102234
228.628096	9513.980586	27.107252
228.894280	9527.442928	27.112269
229.303782	9546.970220	27.117287
229.226179	9553.546556	27.122304
229.912615	9572.676868	27.127322
229.839187	9586.975482	27.132340
230.400237	9593.966435	27.137357
230.432300	9617.771176	27.142375
230.732636	9649.717847	27.147392
230.976050	9652.158280	27.152410
230.862561	9676.510023	27.157428
231.419960	9691.451880	27.162445
231.749376	9701.882823	27.167463
231.733445	9722.035804	27.172480
232.067063	9731.136844	27.177498
232.234128	9761.355388	27.182516
232.802922	9770.871113	27.187533
233.072046	9786.180261	27.192551
233.272998	9808.196957	27.197568
233.273238	9814.650681	27.202586
233.266629	9834.161369	27.207604
233.635945	9854.153104	27.212621
234.180705	9870.176919	27.217639
234.401403	9878.844211	27.222656
234.944607	9888.127199	27.227674
234.824620	9902.755405	27.232692
235.183222	9926.610424	27.237709
235.353723	9930.678919	27.242727
235.458737	9948.293570	27.247744
236.030191	9951.011027	27.252762
236.167503	9967.458703	27.257780
236.449449	9987.562148	27.262797
236.596942	9989.218822	27.267815
237.353833	10015.562769	27.272832
237.579337	10007.769635	27.277850
237.709649	10028.149473	27.282868
237.701107	10036.309669	27.287885
237.778131	10040.695947	27.292903
238.218634	10067.471583	27.297920
238.444098	10072.617662	27.302938
238.469733	10088.925067	27.307956
238.927190	10103.655575	27.312973
239.233655	10117.156237	27.317991
239.251775	10132.637603	27.323008
239.317069	10141.840871	27.328026
239.482685	10158.685278	27.333044
240.097024	10178.297971	27.338061
239.949913	10184.383380	27.343079
240.048116	10209.198377	27.348096
240.353886	10225.379922	27.353114
240.727298	10239.779538	27.358132
240.853588	10257.277479	27.363149
241.075366	10274.087933	27.368167
241.328395	10302.112063	27.373184
241.753001	10314.628169	27.378202
241.622475	10336.397454	27.383220
242.051219	10348.139348	27.388237
242.517695	10362.420284	27.393255
242.597875	10386.853124	27.398272
242.869369	10399.165932	27.403290
243.280092	10425.097377	27.408308
243.388631	10440.388013	27.413325
243.665618	10461.430526	27.418343
244.031997	10477.694363	27.423360
244.275514	10481.464207	27.428378
244.334291	10504.132342	27.433396
244.579230	10520.273152	27.438413
244.754632	10531.057070	27.443431
245.011763	10543.599566	27.448448
245.301899	10558.921843	27.453466
245.819057	10589.500519	27.458484
245.421248	10597.030439	27.463501
246.259562	10609.317742	27.468519
245.976600	10624.802475	27.473536
246.549350	10637.633448	27.478554
247.148321	10663.813598	27.483572
246.699865	10677.698162	27.488589
247.360603	10695.422229	27.493607
247.296418	10712.865179	27.498624
247.778361	10735.025245	27.503642
248.160610	10738.208204	27.508660
248.767660	10752.956840	27.513677
248.883912	10758.827512	27.518695
249.208899	10785.034964	27.523712
249.632013	10779.354545	27.528730
249.813209	10787.131697	27.533748
249.517693	10811.854449	27.538765
249.884113	10818.415349	27.543783
250.372332	10835.108787	27.548800
250.569124	10838.481852	27.553818
250.667521	10855.634230	27.558836
250.496200	10874.979192	27.563853
251.068547	10887.999856	27.568871
250.976104	10906.239968	27.573888
251.447574	10930.934295	27.578906
251.866713	10952.286639	27.583924
251.557896	10966.746327	27.588941
252.063148	10994.814079	27.593959
252.379457	11015.030078	27.598976
252.522438	11038.809778	27.603994
252.895109	11057.952878	27.609012
253.288328	11081.434506	27.614029
253.660394	11101.793430	27.619047
253.827935	11127.457653	27.624064
253.973679	11149.355113	27.629082
254.056785	11166.020737	27.634100
254.262974	11187.681423	27.639117
254.791582	11194.125478	27.644135
255.012872	11214.088177	27.649152
255.649287	11239.584374	27.654170
256.035895	11250.367197	27.659188
256.260120	11261.892251	27.664205
256.783744	11266.313057	27.669223
257.126578	11284.715858	27.674240
257.288241	11286.995644	27.679258
257.728126	11303.314995	27.684276
257.427290	11314.439211	27.689293
257.850007	11317.947486	27.694311
258.356285	11335.424798	27.699328
258.263534	11346.557487	27.704346
258.661431	11363.063454	27.709364
258.816179	11375.319410	27.714381
259.280744	11395.433652	27.719399
259.057962	11409.460230	27.724416
259.273113	11426.282230	27.729434
259.783476	11437.525741	27.734452
259.836260	11463.618900	27.739469
260.493868	11467.121983	27.744487
260.354429	11500.694286	27.749504
260.482445	11519.910918	27.754522
260.726368	11535.983293	27.759540
260.916999	11543.342465	27.764557
261.546532	11541.279782	27.769575
261.922162	11560.972372	27.774592
262.449272	11576.454137	27.779610
262.982371	11565.817606	27.784628
262.838855	11587.824044	27.789645
263.133880	11597.923562	27.794663
263.305870	11601.420644	27.799680
263.710204	11623.076054	27.804698
263.937134	11629.636988	27.809716
264.018479	11633.546148	27.814733
264.211015	11645.458485	27.819751
264.450170	11667.004040	27.824768
264.213753	11680.000381	27.829786
264.784920	11693.107050	27.834804
264.862047	11718.953604	27.839821
264.927080	11735.556252	27.844839
265.138215	11755.492697	27.849856
265.453918	11782.966092	27.854874
265.723717	11795.520072	27.859892
265.923157	11818.704574	27.864909
266.490126	11841.932578	27.869927
266.558927	11865.573372	27.874944
266.932279	11883.198329	27.879962
267.350230	11904.851930	27.884980
266.967595	11931.023418	27.889997
267.327341	11955.714491	27.895015
268.044160	11972.865744	27.900032
267.773078	11994.958954	27.905050
268.129140	12018.021275	27.910068
268.472200	12055.301998	27.915085
268.945718	12080.275401	27.920103
268.797089	12110.784017	27.925120
268.767746	12145.972799	27.930138
269.490870	12170.029352	27.935156
269.473501	12211.273048	27.940173
269.896495	12233.355699	27.945191
270.507039	12256.043718	27.950208
270.880291	12275.813216	27.955226
271.318537	12298.904058	27.960244
271.094715	12330.413205	27.965261
271.999422	12353.311045	27.970279
272.263537	12375.324016	27.975296
272.662468	12398.822185	27.980314
273.104449	12404.806553	27.985332
273.209306	12431.353937	27.990349
274.075292	12441.910774	27.995367
274.247065	12447.577490	28.000384
274.605362	12453.549721	28.005402
275.315811	12468.491930	28.010420
275.026582	12482.709709	28.015437
275.536683	12491.989710	28.020455
275.254107	12504.902269	28.025472
275.614963	12522.905567	28.030490
275.924729	12536.142195	28.035508
275.997231	12555.390683	28.040525
276.184317	12575.657023	28.045543
276.702442	12591.614713	28.050560
277.200662	12605.162918	28.055578
277.766039	12612.568015	28.060596
277.607821	12634.379028	28.065613
277.831994	12647.989140	28.070631
277.808854	12656.838020	28.075648
278.151936	12678.251608	28.080666
278.536792	12697.561837	28.085684
278.714001	12726.656193	28.090701
278.762956	12734.060130	28.095719
279.114826	12752.687161	28.100736
279.305543	12778.558423	28.105754
279.258372	12793.032201	28.110772
279.641951	12812.330116	28.115789
280.091703	12840.955636	28.120807
280.755549	12851.197000	28.125824
280.670285	12874.556871	28.130842
281.311208	12890.138733	28.135860
281.359078	12915.574660	28.140877
281.467657	12934.258929	28.145895
281.823583	12944.144364	28.150912
281.830380	12967.493086	28.155930
282.492489	12986.791758	28.160948
282.782552	13001.733928	28.165965
283.296505	13021.144267	28.170983
283.343847	13044.420415	28.176000
283.439923	13069.681627	28.181018
283.810600	13073.861557	28.186036
284.151142	13108.520492	28.191053
284.560274	13121.315640	28.196071
284.735861	13142.519145	28.201088
285.220428	13162.411084	28.206106
285.531936	13173.481519	28.211124
285.888358	13196.321007	28.216141
286.533895	13200.353696	28.221159
286.872298	13208.220910	28.226176
286.944589	13229.829125	28.231194
287.320095	13233.367264	28.236212
288.040821	13239.213496	28.241229
288.256703	13253.352726	28.246247
288.563296	13263.760808	28.251264
288.656066	13271.205461	28.256282
288.405651	13288.345216	28.261300
288.844580	13303.722213	28.266317
289.232832	13321.428288	28.271335
289.655747	13331.755025	28.276352
289.645586	13357.298533	28.281370
289.819188	13368.551744	28.286388
289.998947	13391.068603	28.291405
290.116158	13421.866116	28.296423
290.865042	13445.149707	28.301440
290.720178	13463.169962	28.306458
290.974562	13483.047768	28.311476
291.430831	13513.056497	28.316493
291.572622	13532.847779	28.321511
291.752558	13546.869695	28.326528
291.583347	13587.429612	28.331546
292.151204	13611.180733	28.336564
292.501980	13647.266485	28.341581
292.503974	13675.293900	28.346599
292.852936	13704.504964	28.351616
293.077697	13742.053868	28.356634
293.783143	13762.856100	28.361652
293.996838	13788.886201	28.366669
294.147530	13826.677415	28.371687
294.500934	13847.010645	28.376704
294.502508	13876.093221	28.381722
295.079577	13899.442181	28.386740
295.078967	13942.537654	28.391757
295.305660	13974.727424	28.396775
295.996523	14004.134879	28.401792
295.927727	14039.990239	28.406810
296.403049	14073.284465	28.411828
296.621331	14107.509605	28.416845
296.910704	14135.881129	28.421863
297.500248	14164.733083	28.426880
297.420044	14203.252844	28.431898
297.962102	14222.050489	28.436916
298.611199	14258.700190	28.441933
298.745755	14274.968880	28.446951
299.377822	14295.738977	28.451968
299.491693	14329.156592	28.456986
299.442318	14339.886311	28.462004
299.940970	14370.909841	28.467021
300.163143	14386.858560	28.472039
300.888896	14406.113970	28.477056
301.358914	14426.464291	28.482074
301.720767	14446.218891	28.487092
302.009487	14467.551427	28.492109
301.961644	14487.433411	28.497127
302.545789	14496.892292	28.502144
302.543961	14520.774845	28.507162
303.549459	14539.601270	28.512180
303.777318	14552.760549	28.517197
304.103775	14563.362041	28.522215
304.794020	14575.207731	28.527232
304.764890	14601.175918	28.532250
305.125985	14597.594818	28.537268
305.572526	14614.973988	28.542285
305.332756	14639.721414	28.547303
305.945404	14651.787750	28.552320
306.034811	14668.761815	28.557338
306.388901	14694.629041	28.562356
306.570968	14706.775494	28.567373
306.566821	14723.720047	28.572391
307.019446	14740.728867	28.577408
307.223665	14772.238167	28.582426
307.482649	14799.468999	28.587444
307.728740	14823.976326	28.592461
307.569020	14847.675577	28.597479
308.633630	14862.371550	28.602496
308.867204	14889.622283	28.607514
309.521447	14919.058997	28.612532
309.946248	14932.993044	28.617549
309.905532	14957.267542	28.622567
310.310260	14970.620482	28.627584
310.655791	15004.404089	28.632602
311.386725	15021.524319	28.637620
311.324035	15038.083537	28.642637
311.409847	15068.683339	28.647655
311.727115	15080.755160	28.652672
311.709882	15112.511315	28.657690
311.977376	15135.812380	28.662708
312.428012	15167.972239	28.667725
312.489487	15190.440268	28.672743
313.579964	15214.124156	28.677760
313.629825	15235.384425	28.682778
313.696898	15259.304481	28.687796
314.116622	15274.622916	28.692813
314.154198	15313.164360	28.697831
314.460981	15333.781253	28.702848
314.656960	15360.994329	28.707866
314.832442	15392.114358	28.712884
315.447487	15414.240110	28.717901
315.773771	15459.097521	28.722919
315.883353	15475.819631	28.727936
316.123015	15512.779069	28.732954
316.601291	15539.843953	28.737972
317.380278	15572.376277	28.742989
317.445179	15594.642106	28.748007
317.777029	15623.874579	28.753024
318.090884	15660.371032	28.758042
318.292452	15692.277057	28.763060
318.807400	15714.393569	28.768077
319.169883	15725.454346	28.773095
319.613899	15742.376972	28.778112
319.762274	15784.632070	28.783130
320.053668	15806.246778	28.788148
320.467618	15824.352271	28.793165
320.857245	15851.876817	28.798183
320.981380	15866.294504	28.803200
321.384341	15880.014733	28.808218
321.772217	15917.261258	28.813236
321.815032	15929.250269	28.818253
322.082523	15959.017632	28.823271
322.517681	15983.594737	28.828288
322.792008	16010.196357	28.833306
323.144339	16032.572433	28.838324
323.574206	16065.807764	28.843341
323.890810	16088.893835	28.848359
324.180777	16113.591762	28.853376
324.392368	16143.687171	28.858394
324.552049	16176.415443	28.863412
325.236322	16200.998022	28.868429
325.372503	16226.490849	28.873447
326.476765	16233.260223	28.878464
326.973132	16245.418429	28.883482
327.278745	16264.773114	28.888500
328.049733	16283.593782	28.893517
327.977157	16297.619370	28.898535
328.066387	16307.680987	28.903552
328.512371	16331.644095	28.908570
329.012962	16340.940107	28.913588
328.954003	16358.602190	28.918605
328.949324	16378.757318	28.923623
329.384008	16406.029237	28.928640
329.705752	16428.290542	28.933658
329.923533	16460.811211	28.938676
330.377561	16480.272364	28.943693
330.423024	16503.691990	28.948711
330.908099	16527.737657	28.953728
331.034342	16558.320862	28.958746
331.869679	16576.035728	28.963764
332.927314	16592.092302	28.968781
332.816954	16625.940699	28.973799
333.131424	16634.675362	28.978816
333.473093	16649.043768	28.983834
333.687681	16673.381512	28.988852
334.485066	16681.696270	28.993869
334.609472	16698.593999	28.998887
334.921623	16714.116790	29.003904
335.020346	16739.287674	29.008922
335.248537	16750.145822	29.013940
335.694406	16776.731106	29.018957
336.048965	16805.418545	29.023975
336.153338	16821.649903	29.028992
336.424759	16848.316309	29.034010
337.041279	16868.061941	29.039028
337.197528	16890.526585	29.044045
337.588180	16919.499128	29.049063
337.273061	16944.577176	29.054080
338.190380	16960.681308	29.059098
338.508930	16987.428964	29.064116
339.226908	17009.451992	29.069133
339.265575	17034.247318	29.074151
339.462072	17054.261086	29.079168
340.051231	17082.008825	29.084186
339.955699	17101.202926	29.089204
340.440515	17133.319658	29.094221
340.491738	17158.732266	29.099239
340.783799	17185.939188	29.104256
341.094704	17209.548670	29.109274
341.405345	17243.120571	29.114292
342.122397	17272.592120	29.119309
342.458761	17298.888888	29.124327
342.692994	17319.977278	29.129344
343.131351	17340.825246	29.134362
343.142631	17372.586974	29.139380
343.493641	17398.755238	29.144397
343.620478	17435.672863	29.149415
344.068861	17453.840829	29.154432
344.314481	17483.462354	29.159450
344.464831	17515.379417	29.164468
345.113179	17548.494637	29.169485
345.102581	17587.348245	29.174503
345.059717	17622.340734	29.179520
346.026010	17658.495548	29.184538
346.270347	17690.688779	29.189556
346.789452	17715.795083	29.194573
347.289090	17747.461975	29.199591
347.259941	17779.894034	29.204608
347.796467	17808.327028	29.209626
348.376328	17836.500576	29.214644
348.698553	17864.512363	29.219661
349.449758	17899.703158	29.224679
349.447854	17931.031958	29.229696
349.791163	17952.685161	29.234714
349.934375	17995.457620	29.239732
350.295218	18016.350044	29.244749
350.719046	18048.711597	29.249767
350.996396	18080.502298	29.254784
351.519551	18118.117247	29.259802
351.783901	18153.182602	29.264820
352.497713	18178.277958	29.269837
352.674535	18207.437546	29.274855
353.207321	18239.523328	29.279872
353.458894	18255.979216	29.284890
353.497051	18294.239062	29.289908
354.341512	18315.776263	29.294925
354.619195	18344.124235	29.299943
355.202286	18380.460459	29.304960
355.455454	18410.025356	29.309978
355.515795	18435.867808	29.314996
355.859857	18459.682101	29.320013
356.382549	18484.529813	29.325031
356.682060	18512.969378	29.330048
357.406727	18539.548159	29.335066
357.315182	18576.698008	29.340084
357.998266	18597.249967	29.345101
358.467854	18624.108893	29.350119
358.814698	18652.876088	29.355136
359.312883	18666.501254	29.360154
359.220508	18707.239959	29.365172
359.845652	18729.399526	29.370189
359.851886	18758.605613	29.375207
359.991885	18795.814376	29.380224
360.777523	18822.055469	29.385242
360.797231	18848.542929	29.390260
361.760211	18881.194164	29.395277
362.048320	18908.442026	29.400295
361.830060	18935.061646	29.405312
362.662822	18965.490590	29.410330
363.055349	18994.895553	29.415348
363.734713	19017.356530	29.420365
363.686119	19044.076079	29.425383
363.896167	19084.856650	29.430400
364.380464	19106.343742	29.435418
364.736153	19130.523472	29.440436
365.134416	19166.479451	29.445453
365.291883	19200.066089	29.450471
365.940738	19217.945270	29.455488
366.042251	19240.572834	29.460506
366.489820	19283.850104	29.465524
367.164688	19297.100550	29.470541
367.393535	19324.092921	29.475559
367.808073	19356.243291	29.480576
368.005467	19379.671015	29.485594
368.097184	19397.877715	29.490612
368.459760	19421.380702	29.495629
368.838344	19454.465610	29.500647
369.287268	19473.816847	29.505664
369.619015	19505.159090	29.510682
370.044804	19543.765018	29.515700
370.176415	19578.038701	29.520717
370.633702	19605.115719	29.525735
371.225656	19632.405449	29.530752
371.987041	19654.494184	29.535770
371.965649	19688.564577	29.540788
372.455640	19709.425952	29.545805
372.613751	19742.381612	29.550823
372.413264	19781.894824	29.555840
373.031793	19799.362294	29.560858
373.004480	19844.414761	29.565876
373.643584	19869.839908	29.570893
374.271146	19911.491885	29.575911
374.416954	19950.831149	29.580928
375.006521	19986.133171	29.585946
375.748573	20023.117280	29.590964
375.800448	20050.466918	29.595981
376.311528	20076.348342	29.600999
376.708074	20102.279333	29.606016
377.205103	20134.822426	29.611034
377.478460	20168.032431	29.616052
377.584119	20207.902911	29.621069
378.891899	20243.130806	29.626087
378.870726	20274.832837	29.631104
379.082774	20298.354138	29.636122
379.650686	20341.829716	29.641140
380.281764	20359.763275	29.646157
380.328268	20395.283783	29.651175
380.412547	20419.374933	29.656192
381.119089	20459.227622	29.661210
381.165105	20494.438787	29.666228
381.665770	20527.241012	29.671245
382.081325	20564.928075	29.676263
382.154177	20606.940106	29.681280
382.896067	20638.087230	29.686298
383.039793	20677.529368	29.691316
383.418852	20709.940251	29.696333
384.114053	20745.050177	29.701351
384.139384	20786.463467	29.706368
384.950722	20812.974903	29.711386
384.930437	20856.411065	29.716404
385.068094	20884.835198	29.721421
385.894156	20921.150722	29.726439
386.062220	20960.817078	29.731456
386.937103	20997.289376	29.736474
387.377337	21023.814996	29.741492
387.987906	21051.937828	29.746509
388.352703	21088.445963	29.751527
388.469362	21125.416376	29.756544
388.985368	21140.228363	29.761562
389.187069	21179.321221	29.766580
389.806301	21209.003603	29.771597
390.273269	21248.554215	29.776615
390.280291	21284.126737	29.781632
391.082732	21300.176651	29.786650
391.352923	21335.044591	29.791668
392.260028	21366.097485	29.796685
392.532101	21378.546788	29.801703
392.776140	21413.178855	29.806720
393.360186	21419.109047	29.811738
393.832560	21447.007663	29.816756
394.135517	21459.458499	29.821773
394.136241	21490.470321	29.826791
394.384361	21513.943192	29.831808
394.798510	21535.842012	29.836826
395.196308	21569.426645	29.841844
395.417359	21598.786544	29.846861
395.838413	21621.891246	29.851879
396.077385	21660.448449	29.856896
396.495528	21685.089126	29.861914
396.796006	21723.523081	29.866932
396.786405	21749.665190	29.871949
397.502788	21787.332742	29.876967
397.911171	21828.713491	29.881984
397.976006	21863.614529	29.887002
398.623406	21902.215647	29.892020
398.709251	21947.855474	29.897037
399.448785	21983.845294	29.902055
399.941202	22009.650041	29.907072
400.319386	22043.238550	29.912090
400.715588	22079.396061	29.917108
400.765755	22120.473355	29.922125
401.511574	22157.208130	29.927143
401.650545	22200.615978	29.932160
402.178957	22251.810984	29.937178
402.779395	22284.208731	29.942196
403.044888	22325.075790	29.947213
403.413731	22348.619206	29.952231
404.159734	22388.652860	29.957248
404.846299	22427.248867	29.962266
405.056175	22454.747695	29.967284
405.306038	22496.211537	29.972301
406.124015	22518.421009	29.977319
406.360315	22561.492132	29.982336
406.629466	22594.195037	29.987354
406.818424	22629.646690	29.992372
407.372383	22680.181621	29.997389
407.657324	22714.335627	30.002407
408.150720	22745.948377	30.007424
408.513660	22786.895908	30.012442
409.155796	22819.370146	30.017460
409.341495	22854.696328	30.022477
410.301168	22896.820752	30.027495
410.497357	22935.620939	30.032512
410.429940	22975.947485	30.037530
410.969408	23012.804635	30.042548
411.017114	23046.800477	30.047565
412.043151	23084.472546	30.052583
412.185725	23132.918231	30.057600
412.459487	23172.932649	30.062618
413.148995	23209.779300	30.067636
413.023519	23252.548389	30.072653
413.809929	23289.057729	30.077671
414.337035	23333.070769	30.082688
414.280266	23376.549754	30.087706
415.003736	23412.835368	30.092724
415.452062	23458.055363	30.097741
415.689427	23487.225918	30.102759
416.273698	23525.663139	30.107776
416.636118	23576.476798	30.112794
417.476497	23609.963961	30.117812
417.470236	23653.663134	30.122829
417.826967	23701.703813	30.127847
418.603462	23739.852244	30.132864
418.830532	23782.756827	30.137882
419.424748	23826.848915	30.142900
419.768704	23863.340138	30.147917
420.479837	23890.237922	30.152935
420.687046	23917.745504	30.157952
421.144028	23953.618844	30.162970
421.681955	23987.615334	30.167988
421.640791	24029.266974	30.173005
422.697501	24055.902310	30.178023
422.898525	24081.199273	30.183040
423.005297	24118.258949	30.188058
423.269432	24139.166699	30.193076
423.576678	24192.038078	30.198093
424.192904	24233.751480	30.203111
424.465934	24269.047524	30.208128
424.459142	24321.317521	30.213146
425.174422	24355.400608	30.218164
425.381007	24402.398481	30.223181
426.183627	24445.631424	30.228199
426.162568	24489.758148	30.233216
426.931117	24530.569885	30.238234
427.760971	24570.398880	30.243252
427.716974	24632.944909	30.248269
428.606348	24656.915089	30.253287
429.772295	24690.593216	30.258304
430.293537	24715.967217	30.263322
430.829512	24735.044542	30.268340
431.245732	24774.199329	30.273357
431.621788	24798.875731	30.278375
432.244523	24825.908694	30.283392
432.423035	24852.493057	30.288410
432.691094	24885.313635	30.293428
432.933035	24926.613125	30.298445
433.633527	24962.879872	30.303463
434.170210	24990.855538	30.308480
434.156338	25014.601079	30.313498
434.719210	25050.263882	30.318516
435.432909	25078.578492	30.323533
436.222852	25099.847270	30.328551
436.812332	25123.277242	30.333568
437.135611	25152.923388	30.338586
437.308263	25168.285109	30.343604
437.661406	25210.281902	30.348621
438.156027	25246.467650	30.353639
438.363683	25275.696019	30.358656
438.543271	25319.875293	30.363674
439.160113	25355.953616	30.368692
439.307548	25399.228038	30.373709
439.643871	25433.043679	30.378727
440.455881	25467.271502	30.383744
440.353670	25510.458867	30.388762
440.801251	25546.140607	30.393780
440.789522	25598.206133	30.398797
441.027192	25631.765801	30.403815
441.732758	25691.840366	30.408832
441.914676	25736.942903	30.413850
442.715578	25787.187874	30.418868
443.118771	25835.074696	30.423885
443.465357	25891.066466	30.428903
443.965272	25934.501706	30.433920
444.485759	25988.924415	30.438938
445.115786	26031.922360	30.443956
445.110191	26089.094816	30.448973
445.761269	26147.485482	30.453991
446.122565	26189.084865	30.459008
446.528087	26237.907654	30.464026
447.154754	26277.127199	30.469044
447.124823	26329.557704	30.474061
447.582982	26381.014427	30.479079
448.395853	26431.183282	30.484096
449.060707	26482.639490	30.489114
449.551923	26529.559812	30.494132
450.218002	26573.425454	30.499149
450.965028	26603.209604	30.504167
451.460377	26634.366797	30.509184
451.865426	26666.353497	30.514202
452.287216	26698.969654	30.519220
452.407896	26729.275555	30.524237
453.365637	26766.055117	30.529255
453.538167	26812.798480	30.534272
453.938726	26854.418359	30.539290
454.111410	26894.847868	30.544308
455.178708	26930.491867	30.549325
455.039325	26980.646903	30.554343
455.624110	27011.013259	30.559360
455.705298	27058.523620	30.564378
456.340243	27105.277391	30.569396
456.691799	27151.595305	30.574413
456.816117	27196.299280	30.579431
457.833844	27236.508623	30.584448
458.385033	27291.391411	30.589466
458.511574	27335.298963	30.594484
458.694343	27382.598233	30.599501
459.147000	27436.751026	30.604519
459.927191	27477.080217	30.609536
460.079785	27528.954298	30.614554
460.652172	27582.216489	30.619572
460.776166	27639.373002	30.624589
461.499315	27695.114825	30.629607
462.204659	27730.475609	30.634624
462.483287	27788.802916	30.639642
463.654170	27821.183451	30.644660
463.947968	27874.060235	30.649677
464.614799	27906.873813	30.654695
465.310861	27947.305601	30.659712
465.615936	27988.791058	30.664730
466.395793	28029.412146	30.669748
466.729004	28069.553371	30.674765
467.131218	28112.427063	30.679783
467.700342	28154.453005	30.684800
467.909456	28195.637875	30.689818
468.556944	28233.265102	30.694836
468.968358	28274.911464	30.699853
469.272682	28323.919447	30.704871
469.666646	28364.854476	30.709888
469.892178	28403.243395	30.714906
470.312582	28455.235899	30.719924
470.678522	28511.459394	30.724941
471.136852	28562.694049	30.729959
471.832874	28604.972838	30.734976
472.378675	28651.624019	30.739994
473.060370	28693.386922	30.745012
473.738181	28741.205961	30.750029
474.297308	28781.382726	30.755047
475.094704	28811.459304	30.760064
475.461771	28855.149137	30.765082
476.184841	28886.703930	30.770100
476.930269	28923.324694	30.775117
477.215094	28959.006308	30.780135
478.042408	28982.479341	30.785152
478.227940	29020.218295	30.790170
478.514813	29042.796288	30.795188
478.940982	29083.727709	30.800205
479.760465	29103.997346	30.805223
480.088393	29130.292094	30.810240
480.559028	29170.268566	30.815258
481.192267	29201.724136	30.820276
481.903903	29234.305268	30.825293
481.756988	29273.961476	30.830311
482.114434	29295.725915	30.835328
482.318852	29333.892322	30.840346
483.035468	29375.404621	30.845364
483.634879	29402.011178	30.850381
484.489845	29417.869745	30.855399
485.020797	29441.509824	30.860416
485.113571	29476.824186	30.865434
485.312719	29504.511272	30.870452
486.271436	29526.586336	30.875469
486.384122	29570.140538	30.880487
486.942347	29601.039563	30.885504
486.812868	29645.295578	30.890522
487.232754	29685.957370	30.895540
488.002115	29724.579640	30.900557
488.148901	29775.891401	30.905575
488.511944	29817.384116	30.910592
488.760911	29878.041904	30.915610
489.093495	29934.110160	30.920628
489.363405	29985.068128	30.925645
489.463592	30037.746918	30.930663
490.442205	30093.885098	30.935680
490.782359	30156.703961	30.940698
491.508360	30213.413026	30.945716
492.260229	30261.306178	30.950733
493.567823	30290.780339	30.955751
494.767515	30325.366497	30.960768
494.964290	30365.976073	30.965786
495.522514	30401.648971	30.970804
496.849625	30432.902923	30.975821
496.955269	30459.227861	30.980839
497.619885	30488.980013	30.985856
498.073797	30520.434078	30.990874
498.067708	30554.362400	30.995892
498.960269	30597.727083	31.000909
499.019659	30620.860796	31.005927
499.018764	30654.699967	31.010944
499.588319	30692.198508	31.015962
500.202283	30746.884734	31.020980
500.751547	30783.343564	31.025997
500.895489	30836.504292	31.031015
501.251219	30878.082461	31.036032
501.449968	30928.061407	31.041050
501.775293	30987.964539	31.046068
502.582233	31037.810562	31.051085
502.898325	31094.725320	31.056103
503.106744	31145.967604	31.061120
503.768267	31195.685062	31.066138
504.364680	31260.610182	31.071156
505.060229	31316.100627	31.076173
505.188585	31367.823804	31.081191
506.069879	31426.067010	31.086208
506.164902	31479.224399	31.091226
506.648237	31535.564174	31.096244
507.442368	31586.178455	31.101261
508.055583	31652.714223	31.106279
508.644946	31703.443043	31.111296
509.145452	31751.631881	31.116314
509.652556	31800.363476	31.121332
510.225321	31849.103866	31.126349
510.428711	31904.413767	31.131367
510.901682	31954.466021	31.136384
511.339470	32016.516587	31.141402
511.985641	32067.812692	31.146420
512.347733	32123.749476	31.151437
512.836278	32191.589846	31.156455
513.745624	32243.591156	31.161472
514.340842	32283.503548	31.166490
514.555462	32335.677118	31.171508
515.484202	32384.957275	31.176525
516.126333	32445.649484	31.181543
516.153379	32487.990414	31.186560
516.884021	32533.900680	31.191578
517.372288	32578.717353	31.196596
517.950115	32629.399654	31.201613
517.976052	32684.688834	31.206631
518.763615	32734.801159	31.211648
518.883738	32788.849367	31.216666
519.500545	32840.556585	31.221684
520.284524	32888.836411	31.226701
520.772855	32935.259673	31.231719
521.787194	32988.093566	31.236736
522.240229	33034.724886	31.241754
522.802994	33090.240844	31.246772
523.289091	33128.268942	31.251789
523.774305	33193.818100	31.256807
524.197488	33235.352465	31.261824
524.488330	33280.182592	31.266842
525.067056	33335.551285	31.271860
525.930543	33383.674386	31.276877
525.930124	33453.049557	31.281895
526.712034	33501.659880	31.286912
526.974978	33554.220897	31.291930
527.169805	33616.396443	31.296948
527.789547	33670.444534	31.301965
528.051394	33745.804858	31.306983
528.483167	33805.806865	31.312000
528.853821	33867.007242	31.317018
529.643310	33945.124431	31.322036
530.351017	34014.694021	31.327053
530.943198	34080.532666	31.332071
531.438067	34131.964998	31.337088
531.918201	34198.276783	31.342106
532.510859	34262.743922	31.347124
533.093849	34320.795318	31.352141
533.900703	34391.261076	31.357159
534.813690	34444.772058	31.362176
535.082477	34503.271492	31.367194
535.427078	34568.960755	31.372212
536.372097	34622.808596	31.377229
536.847981	34690.779140	31.382247
537.354899	34743.469295	31.387264
537.915609	34807.481538	31.392282
538.144798	34863.199831	31.397300
538.734103	34929.262865	31.402317
539.437075	34994.208133	31.407335
540.176671	35048.152458	31.412352
540.850173	35101.222073	31.417370
540.829959	35162.974274	31.422388
541.605779	35223.893817	31.427405
542.026624	35290.363733	31.432423
542.661444	35338.394323	31.437440
543.133831	35405.665860	31.442458
544.535749	35460.544463	31.447476
545.224501	35500.745482	31.452493
545.682412	35560.065486	31.457511
546.461985	35610.514692	31.462528
547.110029	35648.439764	31.467546
547.413174	35687.626619	31.472564
548.063769	35737.628424	31.477581
548.782915	35778.881156	31.482599
549.755788	35821.801456	31.487616
550.259839	35857.119060	31.492634
550.564399	35897.349386	31.497652
551.040628	35938.520334	31.502669
551.757969	35981.689641	31.507687
552.326328	36023.194095	31.512704
553.078925	36066.693178	31.517722
553.131826	36101.557025	31.522740
553.628376	36145.456789	31.527757
553.957124	36186.689255	31.532775
553.998184	36237.078563	31.537792
555.100454	36282.262196	31.542810
555.043929	36335.076157	31.547828
555.287830	36372.148949	31.552845
555.425914	36432.830380	31.557863
555.969128	36493.739401	31.562880
556.687164	36552.300573	31.567898
557.054238	36616.487696	31.572916
557.858257	36672.658172	31.577933
559.039703	36729.964794	31.582951
559.579869	36782.825519	31.587968
560.525516	36821.926475	31.592986
560.752237	36883.069551	31.598004
561.720717	36925.885266	31.603021
561.944845	36976.336170	31.608039
562.766122	37032.378420	31.613056
563.705604	37074.395900	31.618074
563.882849	37131.898815	31.623092
564.441383	37184.542658	31.628109
564.607732	37235.502773	31.633127
564.588394	37294.219401	31.638144
565.375711	37358.102633	31.643162
565.870638	37426.350823	31.648180
566.313505	37482.807633	31.653197
566.660421	37543.560675	31.658215
567.328395	37608.310701	31.663232
567.788669	37674.181112	31.668250
568.442448	37745.004436	31.673268
569.141336	37816.630355	31.678285
569.523680	37879.952522	31.683303
570.007215	37959.416051	31.688320
570.963331	38027.056401	31.693338
571.333384	38098.652551	31.698356
571.870176	38162.627998	31.703373
572.671636	38226.625421	31.708391
572.885139	38301.358055	31.713408
573.598644	38370.403418	31.718426
573.905960	38449.852084	31.723444
574.920093	38507.113767	31.728461
575.693303	38579.122657	31.733479
576.481468	38635.395604	31.738496
577.969211	38679.265465	31.743514
578.246834	38724.090133	31.748532
578.997488	38775.550498	31.753549
579.646415	38835.121568	31.758567
580.376220	38889.222555	31.763584
581.022520	38942.894077	31.768602
581.462079	39003.465968	31.773620
581.882023	39056.901292	31.778637
582.358535	39106.685248	31.783655
582.599887	39166.536078	31.788672
583.170202	39222.351395	31.793690
583.453478	39287.229944	31.798708
584.219838	39350.255957	31.803725
584.905749	39404.162732	31.808743
584.905833	39474.271964	31.813760
585.654821	39544.574016	31.818778
586.004679	39619.270863	31.823796
586.567474	39676.840322	31.828813
587.024496	39748.883643	31.833831
587.883616	39815.336849	31.838848
588.356557	39876.158914	31.843866
588.939134	39948.278094	31.848884
589.820853	40014.203454	31.853901
589.955600	40075.180229	31.858919
590.627617	40156.918013	31.863936
591.143453	40215.261493	31.868954
591.625496	40280.225707	31.873972
592.259437	40343.667446	31.878989
592.740865	40414.589727	31.884007
593.384432	40481.116668	31.889024
594.222644	40546.936611	31.894042
595.612256	40597.567585	31.899060
596.258368	40644.855634	31.904077
596.912084	40695.829768	31.909095
597.382017	40768.728239	31.914112
597.881325	40821.092942	31.919130
598.422512	40876.006324	31.924148
599.015614	40930.576513	31.929165
599.782118	40997.737201	31.934183
599.774270	41051.940114	31.939200
600.743176	41112.346417	31.944218
601.266515	41179.786081	31.949236
601.779563	41238.613398	31.954253
602.421978	41303.214001	31.959271
602.684087	41371.846255	31.964288
603.876921	41440.010400	31.969306
604.319526	41513.067416	31.974324
604.418775	41583.231120	31.979341
605.383345	41642.482134	31.984359
605.996127	41712.268559	31.989376
606.619665	41768.278113	31.994394
606.809591	41844.310507	31.999412
607.621317	41917.709521	32.004429
608.922489	41978.382412	32.009447
608.996931	42060.809094	32.014464
609.255295	42120.203620	32.019482
609.960676	42189.034643	32.024500
610.783916	42251.029144	32.029517
611.182425	42315.266121	32.034535
611.722494	42399.980352	32.039552
612.816029	42470.187233	32.044570
613.063565	42545.669069	32.049588
613.967900	42624.995125	32.054605
614.341008	42691.096733	32.059623
614.931645	42774.318090	32.064640
615.757434	42849.723051	32.069658
616.095385	42910.568335	32.074676
616.977967	42987.482900	32.079693
617.333444	43057.940064	32.084711
617.480201	43146.475895	32.089728
618.474631	43217.428065	32.094746
618.714378	43294.760632	32.099764
619.355936	43377.084417	32.104781
619.868241	43455.538704	32.109799
620.069655	43548.134728	32.114816
620.753807	43626.872646	32.119834
621.423047	43724.703086	32.124852
622.032447	43809.525697	32.129869
623.007999	43894.664487	32.134887
623.573596	43989.805051	32.139904
624.129841	44075.737624	32.144922
624.927298	44158.077834	32.149940
625.545532	44238.567744	32.154957
626.537874	44319.366234	32.159975
627.018398	44406.026722	32.164992
627.718149	44481.963000	32.170010
628.272982	44575.899563	32.175028
629.176065	44647.148923	32.180045
629.897063	44717.111293	32.185063
630.631855	44787.406982	32.190080
631.456100	44865.184807	32.195098
631.891874	44929.284330	32.200116
632.425925	45005.545643	32.205133
633.663080	45066.622877	32.210151
634.113717	45135.363749	32.215168
634.457980	45201.692395	32.220186
634.810473	45273.466453	32.225204
635.699514	45348.813031	32.230221
636.642337	45417.528292	32.235239
636.777537	45491.424601	32.240256
637.521831	45551.359453	32.245274
638.042521	45620.451413	32.250292
638.540676	45711.852275	32.255309
639.183256	45773.378802	32.260327
639.397789	45867.703013	32.265344
640.062746	45939.455564	32.270362
641.077304	46011.197875	32.275380
641.746233	46090.908392	32.280397
642.406310	46172.866323	32.285415
643.478783	46253.355581	32.290432
643.511478	46326.549507	32.295450
644.544996	46401.212742	32.300468
644.829088	46487.855083	32.305485
645.769248	46555.119222	32.310503
646.401093	46639.885754	32.315520
646.901776	46721.554328	32.320538
647.529173	46792.891618	32.325556
647.795073	46885.864547	32.330573
648.984541	46954.046092	32.335591
649.994582	47031.055800	32.340608
651.054485	47101.124333	32.345626
651.970109	47174.144766	32.350644
652.298498	47250.388938	32.355661
653.075888	47317.706141	32.360679
653.685514	47396.709340	32.365696
653.818869	47478.191435	32.370714
654.405787	47547.209318	32.375732
655.123796	47628.935692	32.380749
655.545000	47708.545189	32.385767
656.053148	47795.954568	32.390784
656.680931	47888.058804	32.395802
657.863994	47961.862331	32.400820
658.897770	48028.869445	32.405837
659.872732	48090.242660	32.410855
660.553853	48165.896898	32.415872
661.317481	48228.163998	32.420890
662.161121	48288.906673	32.425908
662.921711	48358.981671	32.430925
663.922198	48425.185352	32.435943
664.573481	48481.941230	32.440960
664.709894	48552.601726	32.445978
665.856825	48611.146682	32.450996
666.249936	48670.967633	32.456013
667.037691	48736.572858	32.461031
667.521610	48801.200917	32.466048
667.990979	48866.154103	32.471066
669.253872	48930.780745	32.476084
669.695546	49009.037629	32.481101
670.108319	49060.049570	32.486119
670.189538	49139.306048	32.491136
670.916056	49212.729581	32.496154
671.655864	49284.923848	32.501172
672.139665	49366.136344	32.506189
672.492697	49440.422615	32.511207
673.135814	49516.150534	32.516224
673.323382	49606.078219	32.521242
673.712632	49687.401561	32.526260
674.594297	49774.013404	32.531277
674.975366	49869.555534	32.536295
675.523742	49952.221536	32.541312
675.945387	50047.802339	32.546330
676.764780	50131.831162	32.551348
677.218992	50223.282296	32.556365
678.004235	50311.189344	32.561383
678.540921	50403.938005	32.566400
679.180801	50500.359658	32.571418
679.894432	50584.166252	32.576436
680.502943	50676.752904	32.581453
681.509130	50771.270752	32.586471
682.559332	50861.106189	32.591488
683.232974	50942.009766	32.596506
684.335992	51020.309102	32.601524
685.891836	51096.373818	32.606541
687.075871	51158.298278	32.611559
687.648999	51231.486501	32.616576
687.982806	51294.455624	32.621594
688.985932	51370.259786	32.626612
689.681890	51458.988760	32.631629
690.258922	51508.063149	32.636647
690.547985	51595.660464	32.641664
690.998815	51683.637739	32.646682
691.777014	51747.519267	32.651700
691.859038	51831.207808	32.656717
692.957863	51914.129963	32.661735
693.998086	51994.840587	32.666752
694.991061	52069.534950	32.671770
696.949552	52103.454640	32.676788
698.072612	52158.158782	32.681805
698.619151	52215.857754	32.686823
699.212523	52269.253012	32.691840
699.884621	52328.451252	32.696858
700.028088	52392.800957	32.701876
700.382750	52448.904319	32.706893
701.044757	52526.145116	32.711911
701.866423	52594.685738	32.716928
702.088349	52675.685057	32.721946
702.763444	52744.375626	32.726964
703.367614	52814.437996	32.731981
704.357784	52890.116241	32.736999
705.052805	52968.808740	32.742016
705.243350	53047.276765	32.747034
705.830430	53128.764665	32.752052
706.236667	53219.652899	32.757069
706.832216	53297.957088	32.762087
707.437953	53392.409050	32.767104
707.966959	53487.379651	32.772122
708.743864	53574.186568	32.777140
709.386709	53665.324232	32.782157
710.055597	53758.945121	32.787175
710.674084	53855.415612	32.792192
711.718629	53951.743839	32.797210
712.426369	54037.708990	32.802228
713.016912	54132.084026	32.807245
713.257977	54225.533289	32.812263
713.927844	54324.959270	32.817280
714.459272	54432.311394	32.822298
715.360725	54530.012313	32.827316
715.451361	54631.738874	32.832333
716.267787	54744.401569	32.837351
717.478183	54864.413676	32.842368
717.722504	54979.293424	32.847386
718.220547	55078.679858	32.852404
718.957244	55190.996432	32.857421
719.359482	55302.834316	32.862439
720.749417	55410.974057	32.867456
721.142382	55527.617826	32.872474
722.008091	55629.847477	32.877492
723.207454	55740.638607	32.882509
723.941657	55835.213083	32.887527
724.805459	55932.261146	32.892544
725.274138	56030.263829	32.897562
725.829154	56123.595433	32.902580
726.551439	56226.558919	32.907597
727.521559	56322.395777	32.912615
728.225186	56426.597161	32.917632
729.046892	56528.818561	32.922650
729.803404	56636.398513	32.927668
730.383095	56725.526217	32.932685
731.311607	56815.675545	32.937703
732.447736	56912.552026	32.942720
732.615162	57023.143610	32.947738
733.414040	57125.516691	32.952756
734.456861	57222.548270	32.957773
734.944411	57330.129142	32.962791
735.481473	57427.633151	32.967808
736.222083	57534.415813	32.972826
737.187965	57634.537053	32.977844
737.486938	57744.161969	32.982861
738.343088	57853.636837	32.987879
739.359148	57947.529910	32.992896
740.318633	58073.369641	32.997914
740.810108	58166.257078	33.002932
741.911490	58271.726973	33.007949
742.884718	58381.711228	33.012967
743.771861	58482.107809	33.017984
744.222271	58576.788131	33.023002
745.008538	58680.422990	33.028020
745.707047	58780.818698	33.033037
746.355030	58891.172666	33.038055
747.404550	58994.723334	33.043072
747.882890	59101.889435	33.048090
748.678112	59196.670080	33.053108
749.575366	59301.397876	33.058125
750.103604	59416.210009	33.063143
750.896212	59511.941730	33.068160
751.346729	59624.925091	33.073178
752.140401	59735.728459	33.078196
752.890984	59846.773277	33.083213
753.413335	59965.215840	33.088231
754.447508	60077.198405	33.093248
754.865977	60194.563292	33.098266
756.144862	60295.437694	33.103284
757.305397	60395.381566	33.108301
758.055276	60503.581030	33.113319
759.321682	60589.918841	33.118336
760.612869	60681.722141	33.123354
761.717075	60771.042070	33.128372
762.306127	60859.278278	33.133389
763.000283	60961.639579	33.138407
763.574499	61044.745137	33.143424
764.286497	61138.938643	33.148442
764.995965	61226.163488	33.153460
765.860686	61318.333459	33.158477
766.508560	61409.714814	33.163495
767.345984	61500.193265	33.168512
767.984019	61603.958651	33.173530
768.762901	61695.928246	33.178548
769.356460	61793.675044	33.183565
769.783747	61888.751580	33.188583
770.320516	61994.794358	33.193600
771.088796	62101.541981	33.198618
771.428277	62191.733775	33.203636
772.246188	62302.373969	33.208653
772.702216	62420.781729	33.213671
773.732588	62529.414584	33.218688
774.418323	62643.552389	33.223706
775.222612	62747.081282	33.228724
775.775925	62844.996778	33.233741
776.410647	62953.731423	33.238759
777.546606	63056.241094	33.243776
777.913371	63165.385792	33.248794
779.199419	63252.685732	33.253812
780.946440	63349.422377	33.258829
781.730516	63447.449704	33.263847
782.601397	63535.625968	33.268864
783.338662	63629.723666	33.273882
784.218490	63715.063012	33.278900
785.321238	63796.411035	33.283917
785.780591	63883.310850	33.288935
786.764146	63968.818409	33.293952
787.565581	64063.553426	33.298970
787.938712	64160.438709	33.303988
788.782668	64252.667105	33.309005
789.232267	64361.671091	33.314023
790.235504	64452.552126	33.319040
790.789252	64559.147579	33.324058
791.815841	64656.211003	33.329076
792.166988	64754.102301	33.334093
792.714852	64874.197640	33.339111
793.847623	64975.550747	33.344128
794.270655	65084.416401	33.349146
795.117281	65189.417543	33.354164
795.978748	65296.550380	33.359181
796.665378	65403.913645	33.364199
797.544292	65520.870619	33.369216
797.964720	65640.552697	33.374234
798.784555	65758.336741	33.379252
799.395709	65876.546546	33.384269
800.246468	65992.243851	33.389287
801.002938	66117.282465	33.394304
802.034496	66244.070387	33.399322
802.569343	66364.472388	33.404340
803.505525	66477.853902	33.409357
803.923271	66603.790020	33.414375
805.051219	66727.393203	33.419392
806.419915	66850.091872	33.424410
806.740851	66971.498948	33.429428
807.629780	67090.019111	33.434445
808.369120	67214.135039	33.439463
809.493531	67331.543077	33.444480
810.239207	67459.337865	33.449498
810.650592	67576.966315	33.454516
812.033469	67693.740359	33.459533
812.719489	67814.486410	33.464551
814.128836	67923.488321	33.469568
814.774029	68048.097901	33.474586
814.634991	68168.702539	33.479604
815.837525	68289.857486	33.484621
816.868757	68422.196595	33.489639
817.772767	68535.161665	33.494656
818.334434	68650.169064	33.499674
819.192597	68780.472896	33.504692
820.097116	68905.767847	33.509709
820.522452	69037.673091	33.514727
821.350407	69164.361662	33.519744
822.092493	69288.259181	33.524762
822.764947	69429.340911	33.529780
823.820356	69557.686460	33.534797
824.263639	69683.380325	33.539815
825.328903	69801.062130	33.544832
826.627426	69935.444067	33.549850
826.916997	70062.487267	33.554868
827.600145	70193.826084	33.559885
828.481639	70320.119288	33.564903
829.670492	70446.466290	33.569920
830.212568	70567.633958	33.574938
831.079161	70682.912870	33.579956
831.759175	70806.795652	33.584973
832.764919	70939.138879	33.589991
833.573548	71057.303463	33.595008
834.420856	71177.222969	33.600026
835.070128	71307.584790	33.605044
836.248258	71423.654070	33.610061
836.742534	71558.778193	33.615079
837.542820	71678.618688	33.620096
838.466027	71805.849735	33.625114
839.560731	71940.919791	33.630132
840.312403	72062.568135	33.635149
841.188849	72194.785926	33.640167
842.121153	72331.377943	33.645184
843.082481	72449.056217	33.650202
843.494796	72583.907097	33.655220
844.580550	72702.542275	33.660237
845.427918	72848.244315	33.665255
846.381259	72979.782683	33.670272
847.381690	73108.299814	33.675290
847.733517	73253.651021	33.680308
848.784390	73381.908251	33.685325
849.533730	73517.331722	33.690343
849.980695	73662.885584	33.695360
851.094008	73787.537760	33.700378
852.106811	73919.312106	33.705396
853.746615	74040.969750	33.710413
854.694481	74174.946819	33.715431
855.371241	74306.813688	33.720448
856.657145	74435.482494	33.725466
857.189956	74565.891177	33.730484
858.298662	74684.366890	33.735501
859.014048	74814.684856	33.740519
859.214529	74950.619505	33.745536
860.354770	75076.996145	33.750554
861.521070	75214.047584	33.755572
862.461527	75339.278703	33.760589
863.262789	75480.619453	33.765607
864.540177	75602.784255	33.770624
865.792433	75713.312346	33.775642
866.494543	75841.863926	33.780660
867.895042	75954.776576	33.785677
868.616222	76073.585073	33.790695
869.539896	76186.877369	33.795712
870.497710	76309.728768	33.800730
871.060510	76434.428703	33.805748
872.092124	76553.317361	33.810765
872.486053	76675.637990	33.815783
873.858037	76795.791848	33.820800
874.637193	76907.919002	33.825818
875.186639	77044.303526	33.830836
876.297742	77160.357446	33.835853
876.720618	77283.284320	33.840871
877.396635	77413.367547	33.845888
878.231005	77540.664952	33.850906
878.782035	77669.603500	33.855924
879.671981	77806.166520	33.860941
880.383682	77931.559375	33.865959
880.906347	78077.251732	33.870976
882.484689	78204.955121	33.875994
883.053856	78351.401748	33.881012
884.234406	78479.599423	33.886029
884.532179	78623.138220	33.891047
885.570225	78762.862601	33.896064
886.187370	78897.662120	33.901082
886.773694	79043.362267	33.906100
888.231346	79182.478304	33.911117
889.209101	79312.953975	33.916135
889.968263	79435.533717	33.921152
891.070458	79568.296852	33.926170
892.107326	79684.220979	33.931188
892.966821	79809.143104	33.936205
893.818440	79939.502101	33.941223
894.292272	80075.862738	33.946240
895.760185	80196.725856	33.951258
896.330317	80341.333096	33.956276
897.430212	80471.034898	33.961293
897.918785	80605.457384	33.966311
899.002809	80739.825286	33.971328
900.200363	80870.780600	33.976346
900.610944	81011.970145	33.981364
902.207006	81142.420889	33.986381
902.653026	81281.553740	33.991399
903.565347	81420.487566	33.996416
904.358474	81560.416323	34.001434
905.125785	81708.116514	34.006452
906.415072	81826.429936	34.011469
907.063986	81978.267839	34.016487
907.894234	82122.691452	34.021504
909.069720	82259.624318	34.026522
909.801059	82407.485830	34.031540
911.178657	82538.484038	34.036557
913.182215	82647.224296	34.041575
913.980383	82782.748998	34.046592
915.140587	82911.185518	34.051610
915.888963	83046.529213	34.056628
916.748794	83171.440834	34.061645
917.579307	83291.339998	34.066663
918.033610	83432.914865	34.071680
919.210065	83559.869281	34.076698
919.889167	83702.183199	34.081716
920.782703	83830.260136	34.086733
921.499881	83977.726527	34.091751
921.909427	84117.651880	34.096768
922.838136	84264.009578	34.101786
923.665032	84423.460624	34.106804
924.458473	84568.966739	34.111821
925.015828	84717.386942	34.116839
925.742688	84872.193086	34.121856
927.006113	85033.492530	34.126874
927.881408	85192.534755	34.131892
928.490854	85356.802161	34.136909
929.702332	85507.189461	34.141927
930.707610	85656.203264	34.146944
931.832335	85828.287142	34.151962
932.878361	85988.738907	34.156980
933.603764	86135.771487	34.161997
934.639761	86295.656274	34.167015
935.579445	86457.622564	34.172032
936.428035	86606.070166	34.177050
937.771755	86774.260328	34.182068
938.276753	86925.538561	34.187085
939.317022	87083.817603	34.192103
940.233677	87244.575300	34.197120
941.046995	87397.797257	34.202138
941.793550	87557.227339	34.207156
942.893989	87715.652428	34.212173
944.054427	87876.692218	34.217191
944.997299	88034.966273	34.222208
946.349906	88196.269189	34.227226
947.269165	88363.077505	34.232244
948.534229	88506.780502	34.237261
950.089570	88642.087229	34.242279
951.341452	88782.080431	34.247296
952.611317	88906.344124	34.252314
953.346023	89034.937643	34.257332
954.314106	89158.375190	34.262349
955.061745	89277.462808	34.267367
955.462919	89408.492736	34.272384
956.802330	89534.826587	34.277402
957.201632	89669.609276	34.282420
958.182536	89807.457210	34.287437
958.932361	89949.308785	34.292455
959.523838	90105.861885	34.297472
961.012595	90233.417315	34.302490
962.298451	90371.866451	34.307508
963.194249	90518.222382	34.312525
964.015740	90663.918943	34.317543
964.676575	90801.821550	34.322560
965.727906	90948.611477	34.327578
966.211484	91102.461739	34.332596
966.816780	91262.833567	34.337613
967.929414	91419.983611	34.342631
968.673884	91581.235199	34.347648
969.705202	91747.880013	34.352666
970.346788	91912.280021	34.357684
971.269506	92078.449346	34.362701
972.533500	92249.154321	34.367719
973.562555	92407.894193	34.372736
974.628922	92575.057696	34.377754
975.353081	92745.152856	34.382772
976.391061	92919.636006	34.387789
977.535308	93090.693968	34.392807
978.420416	93267.192982	34.397824
979.141889	93427.634032	34.402842
979.767588	93597.635248	34.407860
980.920014	93781.206074	34.412877
981.932662	93956.510274	34.417895
982.715561	94146.871676	34.422912
983.903861	94319.830848	34.427930
984.674703	94507.217635	34.432948
985.297393	94679.836405	34.437965
986.657584	94866.169739	34.442983
988.074512	95047.475738	34.448000
989.058306	95228.508360	34.453018
990.322556	95404.123572	34.458036
991.409814	95583.925174	34.463053
992.669741	95763.916265	34.468071
993.319677	95949.657408	34.473088
994.195079	96113.891015	34.478106
995.355837	96300.783834	34.483124
996.366799	96473.174228	34.488141
997.896530	96642.023706	34.493159
998.941844	96813.726060	34.498176
999.697419	96987.464914	34.503194
1001.454838	97159.260473	34.508212
1001.858297	97341.460934	34.513229
1003.089325	97502.375511	34.518247
1003.790363	97678.509897	34.523264
1004.867819	97851.835455	34.528282
1005.895407	98024.218998	34.533300
1007.107704	98192.099593	34.538317
1008.061271	98365.814968	34.543335
1009.510784	98536.512556	34.548352
1009.867917	98708.130035	34.553370
1011.330630	98875.265082	34.558388
1012.801548	99029.456222	34.563405
1014.055606	99186.204843	34.568423
1014.960294	99357.486509	34.573440
1016.247772	99512.405938	34.578458
1017.148314	99674.359327	34.583476
1018.004597	99827.154564	34.588493
1018.983460	99960.293672	34.593511
1019.850554	100129.354045	34.598528
1020.876734	100274.175872	34.603546
1021.424722	100423.903459	34.608564
1022.793641	100587.740455	34.613581
1023.436039	100738.012530	34.618599
1024.114883	100903.619963	34.623616
1025.006358	101069.587965	34.628634
1026.216545	101237.218456	34.633652
1026.921013	101402.380666	34.638669
1028.204621	101568.226407	34.643687
1028.846484	101736.823228	34.648704
1029.405651	101921.484700	34.653722
1030.769072	102083.960770	34.658740
1032.109596	102271.164341	34.663757
1033.004865	102441.677583	34.668775
1033.846796	102616.878477	34.673792
1035.452462	102779.966653	34.678810
1036.456048	102963.271129	34.683828
1037.019364	103140.115933	34.688845
1038.353047	103326.895452	34.693863
1039.177642	103514.440389	34.698880
1040.087946	103685.084442	34.703898
1040.901133	103876.094578	34.708916
1041.688429	104067.680420	34.713933
1042.812340	104258.745520	34.718951
1043.780439	104461.463069	34.723968
1044.556695	104653.206129	34.728986
1045.975604	104850.847066	34.734004
1046.756373	105044.772517	34.739021
1048.087649	105247.704200	34.744039
1048.856210	105450.573041	34.749056
1049.676357	105646.258250	34.754074
1051.354768	105850.508606	34.759092
1052.565405	106046.870416	34.764109
1053.464332	106245.146121	34.769127
1054.491655	106455.220725	34.774144
1055.203974	106649.254794	34.779162
1056.764487	106856.547505	34.784180
1057.438146	107045.707971	34.789197
1058.644437	107255.581930	34.794215
1059.824793	107457.941707	34.799232
1060.928140	107662.394337	34.804250
1061.984524	107869.962279	34.809268
1062.877379	108071.444971	34.814285
1064.300444	108263.652267	34.819303
1065.345725	108462.906913	34.824320
1067.071299	108662.233724	34.829338
1069.119560	108849.413500	34.834356
1070.104315	109026.007259	34.839373
1071.698187	109195.252954	34.844391
1073.295154	109375.556960	34.849408
1074.319809	109552.032993	34.854426
1075.214163	109717.497587	34.859444
1076.028562	109890.495518	34.864461
1077.286436	110054.281568	34.869479
1078.606122	110225.325184	34.874496
1079.290938	110409.569050	34.879514
1080.451598	110577.126478	34.884532
1081.620230	110752.431944	34.889549
1082.304017	110921.967907	34.894567
1083.500078	111101.417723	34.899584
1084.399957	111269.272876	34.904602
1086.251609	111435.927212	34.909620
1087.017133	111603.893746	34.914637
1087.757678	111777.051927	34.919655
1088.939682	111953.692813	34.924672
1090.053310	112128.480998	34.929690
1090.840342	112283.600331	34.934708
1091.682855	112459.497874	34.939725
1092.437837	112623.196898	34.944743
1093.500922	112798.807915	34.949760
1094.196609	112987.692415	34.954778
1094.716947	113160.054670	34.959796
1095.613872	113352.016775	34.964813
1096.643988	113543.236132	34.969831
1097.552290	113740.017908	34.974848
1098.237193	113941.033720	34.979866
1099.319285	114134.239232	34.984884
1100.482897	114345.239820	34.989901
1101.597941	114545.329167	34.994919
1102.631956	114754.652875	34.999936
1103.646146	114963.169156	35.004954
1105.114677	115174.456524	35.009972
1105.795482	115388.468495	35.014989
1106.844677	115607.953971	35.020007
1107.968112	115821.480593	35.025024
1109.178998	116045.255705	35.030042
1110.214861	116261.741135	35.035060
1111.375222	116488.000109	35.040077
1112.504383	116695.734409	35.045095
1113.717384	116924.385002	35.050112
1114.976323	117149.871509	35.055130
1116.261513	117364.637317	35.060148
1117.408177	117584.360120	35.065165
1119.117558	117790.386069	35.070183
1120.293090	118001.494276	35.075200
1121.775489	118218.479154	35.080218
1122.533713	118423.756870	35.085236
1123.875448	118638.356146	35.090253
1124.952664	118851.970600	35.095271
1126.058665	119060.989944	35.100288
1127.006279	119287.971232	35.105306
1128.007350	119500.624507	35.110324
1129.070691	119728.262562	35.115341
1130.326623	119947.068552	35.120359
1131.635421	120161.351687	35.125376
1132.789586	120392.543886	35.130394
1133.839107	120609.128008	35.135412
1134.725396	120827.083509	35.140429
1136.158928	121055.495931	35.145447
1136.995123	121278.929106	35.150464
1137.912833	121496.084249	35.155482
1139.124913	121712.725149	35.160500
1140.561042	121951.519029	35.165517
1141.571696	122175.741860	35.170535
1143.024632	122392.589817	35.175552
1144.353222	122613.987213	35.180570
1145.856996	122832.123555	35.185588
1147.462047	123049.268433	35.190605
1148.264924	123262.797743	35.195623
1149.573348	123476.807231	35.200640
1150.255601	123699.491638	35.205658
1151.882278	123911.360433	35.210676
1152.792506	124136.320441	35.215693
1153.807524	124364.449541	35.220711
1154.883743	124568.808923	35.225728
1156.208974	124788.493530	35.230746
1157.273255	125007.712724	35.235764
1158.348952	125232.538744	35.240781
1159.198979	125456.525961	35.245799
1160.304082	125672.519954	35.250816
1161.189355	125901.832480	35.255834
1162.600529	126131.469935	35.260852
1163.210805	126357.821293	35.265869
1164.705557	126596.481294	35.270887
1165.720224	126806.507181	35.275904
1166.381136	127034.541689	35.280922
1167.836130	127256.731245	35.285940
1169.035977	127467.251660	35.290957
1170.667580	127688.565834	35.295975
1171.790276	127907.423388	35.300992
1172.304714	128135.588350	35.306010
1173.993390	128351.784081	35.311028
1175.522319	128574.819132	35.316045
1176.660193	128798.271835	35.321063
1178.099199	129000.921582	35.326080
1179.460730	129216.843085	35.331098
1180.995726	129435.161899	35.336116
1182.323922	129649.314532	35.341133
1183.731528	129842.064008	35.346151
1185.574233	130031.675757	35.351168
1186.863941	130238.021591	35.356186
1188.181122	130439.403080	35.361204
1189.276190	130641.809959	35.366221
1190.073629	130842.500723	35.371239
1191.222147	131047.870178	35.376256
1192.135117	131253.556626	35.381274
1193.560067	131454.418450	35.386292
1195.204041	131667.377057	35.391309
1195.994871	131878.325908	35.396327
1197.022537	132081.244912	35.401344
1198.002058	132290.440570	35.406362
1199.148508	132497.466708	35.411380
1200.226789	132717.650026	35.416397
1201.149052	132934.141049	35.421415
1202.461391	133162.651869	35.426432
1203.275696	133384.440567	35.431450
1204.276066	133604.132940	35.436468
1205.611045	133840.828111	35.441485
1206.409607	134079.917934	35.446503
1207.990200	134312.618149	35.451520
1209.337345	134539.684020	35.456538
1210.552531	134768.776610	35.461556
1211.933667	135001.993816	35.466573
1212.657850	135237.408829	35.471591
1214.357219	135468.738655	35.476608
1215.108083	135706.385281	35.481626
1216.639870	135948.111174	35.486644
1217.745302	136182.710021	35.491661
1218.535198	136425.036784	35.496679
1220.015322	136664.173142	35.501696
1221.099256	136909.933452	35.506714
1221.863482	137150.643745	35.511732
1223.339750	137396.256394	35.516749
1224.213182	137657.243620	35.521767
1225.682860	137904.014787	35.526784
1226.660322	138171.511365	35.531802
1228.046299	138422.016617	35.536820
1229.417639	138669.505183	35.541837
1230.723359	138925.901338	35.546855
1231.635675	139185.456961	35.551872
1232.647824	139441.381555	35.556890
1234.412791	139700.451182	35.561908
1235.406930	139953.652856	35.566925
1236.758292	140198.563617	35.571943
1237.908949	140448.964123	35.576960
1239.507222	140717.101251	35.581978
1240.750453	140966.791957	35.586996
1241.939506	141212.405907	35.592013
1242.908924	141473.779804	35.597031
1244.794971	141727.434962	35.602048
1246.165668	141976.044840	35.607066
1247.592327	142210.991345	35.612084
1249.085257	142440.522069	35.617101
1250.002718	142678.786825	35.622119
1251.504743	142905.678468	35.627136
1252.234612	143147.312715	35.632154
1253.831235	143372.478325	35.637172
1254.747725	143610.582719	35.642189
1255.546359	143865.091749	35.647207
1256.996886	144099.421571	35.652224
1257.996438	144348.101440	35.657242
1259.411368	144592.046880	35.662260
1260.617514	144836.914620	35.667277
1261.830029	145090.171999	35.672295
1262.812085	145322.194716	35.677312
1264.513347	145580.442180	35.682330
1265.945794	145831.257294	35.687348
1267.524315	146076.504230	35.692365
1268.621832	146331.042288	35.697383
1269.847742	146566.243625	35.702400
1271.288416	146822.240781	35.707418
1272.287350	147068.446235	35.712436
1274.171421	147314.615835	35.717453
1274.779235	147574.757923	35.722471
1276.384144	147821.684394	35.727488
1277.756332	148078.586909	35.732506
1278.857721	148341.029070	35.737524
1280.310421	148585.622068	35.742541
1281.383640	148840.658445	35.747559
1282.403952	149093.356111	35.752576
1283.571627	149363.776852	35.757594
1285.019301	149624.102139	35.762612
1286.205702	149893.735633	35.767629
1287.383870	150166.062737	35.772647
1288.523269	150437.940314	35.777664
1289.574205	150706.190084	35.782682
1290.836063	150981.414951	35.787700
1292.384582	151262.549595	35.792717
1293.558776	151546.359151	35.797735
1294.864471	151821.885998	35.802752
1296.005898	152090.674166	35.807770
1297.195206	152375.767659	35.812788
1298.522001	152653.973705	35.817805
1299.856056	152941.383086	35.822823
1301.563154	153221.436494	35.827840
1303.071486	153498.234643	35.832858
1304.518394	153779.385140	35.837876
1306.188286	154055.069012	35.842893
1307.512256	154323.978863	35.847911
1309.385618	154572.924717	35.852928
1311.308743	154843.063409	35.857946
1312.555553	155097.415836	35.862964
1314.170425	155346.659368	35.867981
1315.165322	155613.951050	35.872999
1317.436081	155841.513356	35.878016
1318.899651	156088.282901	35.883034
1320.735184	156334.246268	35.888052
1321.454857	156573.619041	35.893069
1322.932459	156817.393476	35.898087
1323.978785	157064.689409	35.903104
1325.235556	157302.749638	35.908122
1326.059671	157556.988396	35.913140
1327.490992	157805.039589	35.918157
1328.364585	158048.278818	35.923175
1329.283006	158305.755889	35.928192
1331.055635	158569.117831	35.933210
1331.697333	158841.252581	35.938228
1332.949757	159098.896524	35.943245
1334.088240	159361.155078	35.948263
1335.242073	159620.746314	35.953280
1336.670656	159889.080851	35.958298
1337.867003	160145.582635	35.963316
1338.762853	160392.268092	35.968333
1339.926787	160665.776367	35.973351
1340.832531	160931.924692	35.978368
1342.323474	161200.216971	35.983386
1343.825630	161480.163304	35.988404
1345.206633	161745.516979	35.993421
1346.179074	162032.658278	35.998439
1347.514757	162297.729317	36.003456
1348.707355	162579.557092	36.008474
1349.714445	162876.332925	36.013492
1351.075894	163153.299569	36.018509
1352.685722	163454.300331	36.023527
1353.987172	163745.688949	36.028544
1355.330975	164035.167783	36.033562
1356.648265	164333.717168	36.038580
1358.673076	164620.095616	36.043597
1360.204912	164923.311685	36.048615
1361.745121	165221.449223	36.053632
1363.426736	165504.101593	36.058650
1364.768287	165784.865789	36.063668
1366.677378	166064.882075	36.068685
1367.902420	166339.864426	36.073703
1369.214939	166629.181454	36.078720
1370.625839	166918.789008	36.083738
1371.668496	167211.959721	36.088756
1373.127910	167491.239535	36.093773
1374.021677	167793.349169	36.098791
1375.452134	168081.866504	36.103808
1377.189048	168366.286686	36.108826
1378.520749	168661.792480	36.113844
1380.297323	168938.526989	36.118861
1382.166245	169231.957577	36.123879
1383.306746	169512.831536	36.128896
1385.276149	169798.960470	36.133914
1386.408083	170092.268615	36.138932
1387.621458	170368.017410	36.143949
1389.404983	170653.454994	36.148967
1391.076679	170929.743603	36.153984
1392.588051	171205.042522	36.159002
1393.817977	171467.181041	36.164020
1395.957997	171740.021762	36.169037
1397.294326	172005.002439	36.174055
1398.750352	172283.297869	36.179072
1400.956597	172529.884919	36.184090
1402.136397	172791.489810	36.189108
1403.737347	173052.547144	36.194125
1405.161010	173309.430109	36.199143
1406.562546	173564.019057	36.204160
1407.633576	173828.920493	36.209178
1408.955114	174093.910582	36.214196
1410.286000	174352.728848	36.219213
1411.493587	174627.884262	36.224231
1412.258544	174896.519577	36.229248
1413.963556	175162.672183	36.234266
1414.982989	175443.320018	36.239284
1416.427711	175719.076917	36.244301
1417.733585	176003.884947	36.249319
1418.743999	176279.762488	36.254336
1420.131601	176563.302509	36.259354
1421.293684	176851.551801	36.264372
1422.676406	177140.580243	36.269389
1423.823198	177423.652909	36.274407
1425.063871	177723.397696	36.279424
1427.153291	178011.074015	36.284442
1428.190633	178298.331828	36.289460
1430.026642	178586.583063	36.294477
1431.233970	178861.676202	36.299495
1432.449447	179144.642146	36.304512
1434.228189	179424.600111	36.309530
1435.230282	179707.829826	36.314548
1436.635524	179982.235117	36.319565
1438.493964	180261.167312	36.324583
1439.088481	180550.482745	36.329600
1440.712129	180838.850677	36.334618
1441.591901	181141.228678	36.339636
1443.108876	181434.669380	36.344653
1444.420766	181737.616639	36.349671
1446.027912	182038.816977	36.354688
1447.301177	182347.029688	36.359706
1448.685729	182652.228960	36.364724
1450.326822	182961.529012	36.369741
1451.643915	183267.121771	36.374759
1452.961953	183580.766729	36.379776
1453.987613	183888.692930	36.384794
1455.555958	184215.482701	36.389812
1457.003088	184543.181480	36.394829
1458.739220	184859.685922	36.399847
1459.873885	185198.128727	36.404864
1461.868673	185514.137541	36.409882
1463.497215	185842.751888	36.414900
1464.621477	186166.696528	36.419917
1466.644978	186486.208922	36.424935
1467.913448	186811.656947	36.429952
1470.635328	187103.655838	36.434970
1472.111961	187418.329115	36.439988
1473.656652	187740.129977	36.445005
1475.123803	188113.505528	36.450023
1476.962021	188416.009383	36.455040
1478.321321	188730.349198	36.460058
1479.714563	189043.693983	36.465076
1481.174142	189357.689658	36.470093
1482.233643	189672.485422	36.475111
1483.972598	189983.848273	36.480128
1485.103670	190300.920570	36.485146
1486.624528	190627.051451	36.490164
1487.671171	190939.592020	36.495181
1489.415193	191275.443524	36.500199
1490.491701	191612.416465	36.505216
1492.269146	191930.230149	36.510234
1493.090671	192262.088461	36.515252
1494.928690	192599.884753	36.520269
1496.489147	192932.848436	36.525287
1498.060345	193284.049173	36.530304
1499.712239	193613.672808	36.535322
1501.124643	193940.388246	36.540340
1502.795853	194275.446363	36.545357
1504.269396	194612.390553	36.550375
1505.289574	194951.337046	36.555392
1506.950950	195288.456746	36.560410
1508.305676	195629.689493	36.565428
1509.905179	195982.747241	36.570445
1511.597919	196321.083823	36.575463
1512.903459	196675.332387	36.580480
1514.434149	197010.342968	36.585498
1515.903193	197354.330763	36.590516
1517.194466	197702.233654	36.595533
1518.995142	198042.741917	36.600551
1521.176262	198374.910405	36.605568
1523.563095	198704.761252	36.610586
1524.975094	199035.273417	36.615604
1526.582121	199361.945458	36.620621
1528.135142	199693.961059	36.625639
1530.081145	200024.950564	36.630656
1531.563380	200337.647564	36.635674
1532.939378	200651.403278	36.640692
1534.420439	200943.195589	36.645709
1536.112300	201239.324610	36.650727
1537.409142	201553.526235	36.655744
1538.648438	201851.657723	36.660762
1540.134911	202159.048326	36.665780
1541.245603	202467.590582	36.670797
1542.752368	202776.731845	36.675815
1544.071915	203102.592421	36.680832
1545.532875	203427.872582	36.685850
1546.900626	203758.350038	36.690868
1547.943877	204084.916033	36.695885
1549.516875	204425.701415	36.700903
1550.764354	204768.062502	36.705920
1552.009506	205113.803116	36.710938
1553.598188	205466.882790	36.715956
1554.789687	205824.165906	36.720973
1556.706716	206179.176824	36.725991
1557.870425	206531.664319	36.731008
1559.967009	206896.631693	36.736026
1561.227281	207250.680211	36.741044
1562.810949	207632.952346	36.746061
1564.435019	207992.711580	36.751079
1565.803188	208361.936000	36.756096
1567.312320	208729.792549	36.761114
1568.844900	209100.846788	36.766132
1570.269316	209475.906819	36.771149
1572.151840	209848.050521	36.776167
1573.931624	210231.058070	36.781184
1575.388495	210606.038406	36.786202
1577.286446	210985.853082	36.791220
1578.864909	211352.508447	36.796237
1580.744225	211723.918449	36.801255
1582.253244	212103.490594	36.806272
1584.106672	212471.069615	36.811290
1585.968903	212844.820759	36.816308
1587.525897	213224.361320	36.821325
1589.468763	213591.876785	36.826343
1590.996730	213957.450677	36.831360
1592.770135	214321.665532	36.836378
1594.316275	214688.939354	36.841396
1595.683768	215070.797842	36.846413
1597.391490	215437.411978	36.851431
1599.041292	215805.077057	36.856448
1601.045638	216176.370516	36.861466
1602.709658	216542.001676	36.866484
1604.339333	216915.920157	36.871501
1606.168873	217272.609209	36.876519
1607.658565	217643.374653	36.881536
1609.424229	218012.191868	36.886554
1611.273198	218378.481295	36.891572
1612.910525	218739.418430	36.896589
1614.223305	219098.475863	36.901607
1615.663951	219471.206225	36.906624
1617.238223	219830.553367	36.911642
1618.842083	220195.510335	36.916660
1620.372951	220578.693573	36.921677
1622.073438	220946.887458	36.926695
1623.293918	221324.048020	36.931712
1624.923842	221693.548830	36.936730
1626.819810	222060.289887	36.941748
1628.261260	222451.490081	36.946765
1629.710194	222812.636193	36.951783
1631.520926	223185.894313	36.956800
1633.195667	223561.765001	36.961818
1634.975804	223939.727791	36.966836
1636.152720	224314.838155	36.971853
1637.552458	224695.502578	36.976871
1639.421731	225059.352244	36.981888
1640.579490	225429.664289	36.986906
1642.505324	225792.285706	36.991924
1643.961327	226163.287768	36.996941
1645.589431	226524.736334	37.001959
1647.037179	226905.393163	37.006976
1648.197139	227278.321324	37.011994
1649.508115	227652.775430	37.017012
1651.205931	228057.984040	37.022029
1652.693113	228440.184022	37.027047
1654.161105	228830.998864	37.032064
1656.229873	229224.132935	37.037082
1658.078595	229617.402907	37.042100
1659.408736	230030.111729	37.047117
1660.925421	230415.202410	37.052135
1662.886943	230822.629606	37.057152
1664.999140	231225.409471	37.062170
1666.191349	231623.480915	37.067188
1667.209707	232035.043408	37.072205
1669.819373	232438.354350	37.077223
1671.801079	232845.777094	37.082240
1673.324887	233252.686898	37.087258
1675.288991	233646.596904	37.092276
1676.799976	234063.237731	37.097293
1678.371426	234468.665634	37.102311
1679.795378	234879.349430	37.107328
1681.581555	235292.414903	37.112346
1683.714663	235697.880750	37.117364
1685.381616	236108.931734	37.122381
1687.397052	236517.488977	37.127399
1689.083985	236941.339363	37.132416
1690.626703	237349.182113	37.137434
1692.452809	237772.018951	37.142452
1693.870430	238192.150175	37.147469
1695.747004	238600.929849	37.152487
1697.215431	239023.592350	37.157504
1698.648721	239444.430696	37.162522
1700.362880	239863.725670	37.167540
1701.827590	240298.656727	37.172557
1704.075074	240724.649628	37.177575
1706.554567	241137.167189	37.182592
1708.336610	241549.132747	37.187610
1710.013872	241962.079346	37.192628
1711.636738	242381.918018	37.197645
1713.608708	242796.823917	37.202663
1715.380726	243209.982151	37.207680
1716.768858	243625.994041	37.212698
1719.079974	244042.165550	37.217716
1720.639658	244457.234510	37.222733
1722.489342	244872.003249	37.227751
1723.885895	245284.682829	37.232768
1725.135535	245704.395731	37.237786
1727.353036	246124.438942	37.242804
1728.593518	246550.857798	37.247821
1730.284853	246982.717518	37.252839
1731.798333	247409.625176	37.257856
1733.428473	247854.650969	37.262874
1735.076148	248277.598208	37.267892
1736.492360	248722.020259	37.272909
1738.228773	249159.786468	37.277927
1740.029320	249589.412800	37.282944
1741.414966	250033.277370	37.287962
1743.331476	250480.309140	37.292980
1744.910767	250926.173147	37.297997
1746.921844	251370.342609	37.303015
1748.608012	251816.797018	37.308032
1749.962552	252260.380815	37.313050
1752.035182	252705.552855	37.318068
1754.250895	253133.758262	37.323085
1755.461911	253564.227968	37.328103
1757.618615	253984.387796	37.333120
1759.392663	254409.102315	37.338138
1761.666673	254831.070165	37.343156
1763.065583	255255.256570	37.348173
1764.876748	255681.891859	37.353191
1766.497790	256104.288154	37.358208
1768.162927	256549.130716	37.363226
1770.038410	256958.275908	37.368244
1771.720816	257398.464477	37.373261
1773.458278	257830.971868	37.378279
1775.515248	258260.074876	37.383296
1777.040209	258703.737988	37.388314
1778.650335	259143.449082	37.393332
1780.269706	259588.897616	37.398349
1782.329319	260030.160739	37.403367
1784.117345	260475.401735	37.408384
1785.593561	260923.382226	37.413402
1788.054742	261363.612225	37.418420
1790.049227	261811.736715	37.423437
1791.788873	262254.082724	37.428455
1793.904374	262688.418031	37.433472
1795.383248	263133.849263	37.438490
1797.450549	263575.224251	37.443508
1799.701189	264021.597803	37.448525
1801.405984	264463.838591	37.453543
1804.015229	264891.864818	37.458560
1805.410048	265328.410200	37.463578
1807.759048	265767.547488	37.468596
1808.842197	266203.045713	37.473613
1810.744728	266652.764114	37.478631
1812.943590	267086.356755	37.483648
1814.410835	267532.481830	37.488666
1816.257816	267978.037454	37.493684
1818.077528	268426.744653	37.498701
1820.004448	268876.728252	37.503719
1821.801986	269307.630603	37.508736
1823.346597	269762.977932	37.513754
1825.221863	270205.318382	37.518772
1826.470190	270648.669096	37.523789
1828.447102	271111.662904	37.528807
1830.640862	271571.471092	37.533824
1832.034346	272031.021145	37.538842
1833.886600	272491.919231	37.543860
1835.553560	272956.069271	37.548877
1837.326813	273433.279543	37.553895
1839.030579	273899.958362	37.558912
1840.797158	274373.304055	37.563930
1842.894306	274847.281028	37.568948
1844.648596	275318.489931	37.573965
1846.153099	275798.293694	37.578983
1848.139331	276279.416004	37.584000
1849.784877	276755.560355	37.589018
1851.259580	277234.547496	37.594036
1853.027416	277726.386770	37.599053
1855.029262	278210.161384	37.604071
1857.150701	278696.428371	37.609088
1858.857932	279190.299397	37.614106
1860.825399	279680.723567	37.619124
1862.720017	280163.867648	37.624141
1864.902149	280656.892861	37.629159
1867.130059	281130.607891	37.634176
1869.160518	281621.466434	37.639194
1870.974622	282086.859897	37.644212
1872.800560	282572.284249	37.649229
1874.994245	283061.913887	37.654247
1876.586296	283542.695752	37.659264
1878.377790	284009.806882	37.664282
1879.964600	284471.741298	37.669300
1881.972357	284939.142423	37.674317
1883.190271	285402.702659	37.679335
1885.132418	285872.139070	37.684352
1887.356160	286346.505070	37.689370
1889.005005	286824.182474	37.694388
1890.978475	287302.440442	37.699405
1892.306880	287774.295533	37.704423
1894.298454	288256.200140	37.709440
1896.273623	288739.830351	37.714458
1897.848955	289226.794968	37.719476
1899.718832	289723.942414	37.724493
1901.434747	290219.485023	37.729511
1903.866040	290709.808243	37.734528
1905.797869	291201.653017	37.739546
1907.630655	291699.222205	37.744564
1910.009867	292185.352466	37.749581
1912.013596	292681.845915	37.754599
1913.925448	293178.375054	37.759616
1915.977861	293674.878093	37.764634
1917.803610	294174.205285	37.769652
1919.441452	294674.065447	37.774669
1921.179680	295179.008813	37.779687
1923.197095	295683.421738	37.784704
1925.022561	296194.283575	37.789722
1927.184909	296712.044527	37.794740
1928.748324	297240.735154	37.799757
1930.765180	297761.149665	37.804775
1932.430673	298280.776549	37.809792
1934.612108	298815.474058	37.814810
1936.194921	299339.242114	37.819828
1938.126202	299864.930830	37.824845
1939.611378	300401.118149	37.829863
1942.069361	300920.875361	37.834880
1943.921037	301470.119433	37.839898
1946.070319	302008.877758	37.844916
1948.144178	302539.823685	37.849933
1949.994884	303085.522624	37.854951
1952.535867	303628.569375	37.859968
1954.510994	304156.468167	37.864986
1956.795062	304693.197785	37.870004
1958.721997	305225.027751	37.875021
1960.655045	305762.841817	37.880039
1963.130558	306284.472060	37.885056
1965.377699	306813.544573	37.890074
1967.063894	307344.806052	37.895092
1969.344475	307862.465174	37.900109
1970.819509	308397.454291	37.905127
1973.441534	308914.845850	37.910144
1975.378883	309443.101021	37.915162
1977.208574	309972.179488	37.920180
1979.716176	310500.613059	37.925197
1981.398464	311019.651971	37.930215
1983.205937	311535.340726	37.935232
1985.312996	312050.976979	37.940250
1987.203940	312584.940620	37.945268
1989.701681	313087.103502	37.950285
1991.838113	313618.986460	37.955303
1993.890306	314130.369827	37.960320
1995.763708	314652.460115	37.965338
1997.668918	315164.184844	37.970356
1999.935162	315679.324181	37.975373
2002.255203	316197.672261	37.980391
2003.802313	316713.698983	37.985408
2006.094532	317231.988658	37.990426
2007.827993	317744.827405	37.995444
2010.067751	318239.664681	38.000461
2011.531307	318746.443442	38.005479
2013.674372	319232.732589	38.010496
2015.708199	319720.378316	38.015514
2017.190155	320211.657517	38.020532
2019.309767	320703.897107	38.025549
2021.085577	321211.917580	38.030567
2023.220697	321707.847945	38.035584
2024.790447	322222.689065	38.040602
2026.529644	322744.348483	38.045620
2028.574923	323267.374455	38.050637
2030.219687	323796.267122	38.055655
2032.291319	324325.517587	38.060672
2033.919419	324854.932125	38.065690
2035.859707	325386.067067	38.070708
2037.654605	325923.763938	38.075725
2039.768248	326491.190756	38.080743
2041.734553	327030.571367	38.085760
2043.696068	327590.394884	38.090778
2045.567433	328146.672672	38.095796
2047.943491	328699.616220	38.100813
2049.795724	329258.773596	38.105831
2052.216064	329827.982126	38.110848
2054.339198	330387.613723	38.115866
2056.428613	330957.187280	38.120884
2058.567563	331522.939324	38.125901
2060.260904	332100.675954	38.130919
2062.631808	332659.144845	38.135936
2065.582214	333228.778146	38.140954
2067.479388	333792.783848	38.145972
2069.967561	334352.756714	38.150989
2071.622985	334924.342556	38.156007
2073.996185	335492.814080	38.161024
2075.837330	336059.584481	38.166042
2078.100342	336638.227275	38.171060
2080.361188	337210.443882	38.176077
2082.224021	337778.122745	38.181095
2084.229534	338356.068271	38.186112
2086.249107	338941.865112	38.191130
2088.213298	339515.562669	38.196148
2090.207052	340102.891672	38.201165
2091.974310	340688.394906	38.206183
2093.966427	341282.983623	38.211200
2096.211845	341876.533522	38.216218
2098.121729	342469.060643	38.221236
2100.672290	343061.832468	38.226253
2103.106357	343655.246354	38.231271
2105.797126	344237.831823	38.236288
2107.820432	344822.312317	38.241306
2110.146758	345404.174090	38.246324
2112.468384	345992.467710	38.251341
2114.654249	346567.535279	38.256359
2116.643206	347146.047099	38.261376
2119.612111	347731.597078	38.266394
2121.700865	348308.881278	38.271412
2123.929549	348878.196916	38.276429
2125.766200	349449.009329	38.281447
2128.253278	350017.630874	38.286464
2130.779284	350587.250615	38.291482
2132.483171	351164.012233	38.296500
2134.814230	351715.868938	38.301517
2136.426814	352283.116949	38.306535
2138.413757	352858.384077	38.311552
2140.475806	353428.076775	38.316570
2142.490460	354006.893549	38.321588
2144.734760	354581.024368	38.326605
2146.572262	355166.185563	38.331623
2148.709161	355743.962517	38.336640
2150.827111	356318.131933	38.341658
2152.728512	356888.192525	38.346676
2154.895243	357439.366274	38.351693
2157.203986	358002.700902	38.356711
2158.983710	358552.166109	38.361728
2161.253334	359109.859016	38.366746
2162.947758	359684.538665	38.371764
2165.017027	360244.726110	38.376781
2166.991603	360826.361396	38.381799
2168.783372	361415.161669	38.386816
2170.741293	361990.364295	38.391834
2172.391147	362592.900944	38.396852
2174.593812	363193.083150	38.401869
2176.658396	363794.972797	38.406887
2179.139251	364402.639386	38.411904
2181.082958	365008.248522	38.416922
2182.967872	365626.703007	38.421940
2185.199295	366249.322213	38.426957
2187.652781	366873.008255	38.431975
2189.462567	367505.904221	38.436992
2191.718828	368131.849035	38.442010
2193.597208	368773.144511	38.447028
2196.202739	369403.035678	38.452045
2198.428387	370056.613290	38.457063
2200.683522	370686.783889	38.462080
2202.681723	371334.615457	38.467098
2204.714185	371983.262689	38.472116
2207.356128	372623.818389	38.477133
2209.737908	373274.635579	38.482151
2211.977587	373926.498300	38.487168
2215.003463	374591.067127	38.492186
2216.715573	375238.902101	38.497204
2219.250926	375888.594124	38.502221
2221.403542	376540.736970	38.507239
2223.481740	377194.522199	38.512256
2226.113315	377850.332707	38.517274
2228.088428	378505.115175	38.522292
2230.193062	379174.628758	38.527309
2232.569671	379831.240655	38.532327
2234.931145	380490.472714	38.537344
2237.629600	381156.676717	38.542362
2239.286460	381825.407412	38.547380
2241.639312	382479.550211	38.552397
2243.929543	383157.645025	38.557415
2246.224396	383829.161847	38.562432
2248.585389	384488.874522	38.567450
2250.253519	385166.481577	38.572468
2252.585189	385840.775938	38.577485
2254.749287	386521.941062	38.582503
2256.905896	387212.078350	38.587520
2259.351044	387889.186778	38.592538
2261.989705	388562.271145	38.597556
2264.594231	389231.797757	38.602573
2267.299617	389908.481232	38.607591
2269.716808	390586.355859	38.612608
2272.501211	391244.659258	38.617626
2274.590527	391906.091748	38.622644
2277.019620	392567.301196	38.627661
2279.187242	393225.596821	38.632679
2281.694744	393888.681889	38.637696
2284.520988	394533.877183	38.642714
2286.543732	395189.255792	38.647732
2288.754705	395837.347306	38.652749
2291.728748	396493.047461	38.657767
2293.731606	397135.516613	38.662784
2295.879001	397781.843588	38.667802
2298.009085	398430.787787	38.672820
2300.187007	399097.625922	38.677837
2302.547604	399731.058865	38.682855
2304.717274	400370.325348	38.687872
2306.824654	400986.047616	38.692890
2308.931533	401615.824294	38.697908
2310.940196	402248.838289	38.702925
2313.109927	402878.671659	38.707943
2315.112022	403530.124361	38.712960
2317.335490	404168.719762	38.717978
2319.117776	404821.384349	38.722996
2321.542007	405473.676596	38.728013
2323.795187	406133.617895	38.733031
2326.358821	406787.165823	38.738048
2328.947215	407443.271380	38.743066
2331.391719	408103.832842	38.748084
2333.661746	408765.009058	38.753101
2336.193444	409424.657210	38.758119
2338.182338	410091.807955	38.763136
2340.682342	410760.376225	38.768154
2342.630518	411446.666948	38.773172
2345.045251	412127.298065	38.778189
2347.310271	412800.595810	38.783207
2349.271056	413500.832551	38.788224
2351.597751	414193.047298	38.793242
2353.534261	414905.534269	38.798260
2356.088145	415614.157779	38.803277
2358.615326	416320.789182	38.808295
2360.451130	417042.425893	38.813312
2362.752523	417754.355427	38.818330
2365.217789	418474.934158	38.823348
2367.984946	419196.856908	38.828365
2370.645622	419922.918195	38.833383
2372.913796	420657.359548	38.838400
2375.240576	421365.672410	38.843418
2377.687395	422097.506166	38.848436
2379.918443	422836.173818	38.853453
2382.657293	423560.577746	38.858471
2384.771953	424292.890521	38.863488
2387.273388	425031.941877	38.868506
2389.590203	425777.061983	38.873524
2391.857929	426517.258320	38.878541
2394.614781	427257.199183	38.883559
2396.742471	428007.978598	38.888576
2399.541067	428746.088402	38.893594
2401.764326	429490.528689	38.898612
2404.102680	430248.469286	38.903629
2407.131463	430995.506819	38.908647
2409.047932	431743.346937	38.913664
2411.140857	432499.874312	38.918682
2413.918359	433244.237107	38.923700
2415.907311	434009.414583	38.928717
2418.584678	434772.988598	38.933735
2421.083717	435535.195855	38.938752
2423.981826	436279.725859	38.943770
2426.356882	437044.671597	38.948788
2428.900526	437793.341298	38.953805
2431.394664	438546.586919	38.958823
2433.537701	439303.191922	38.963840
2436.331449	440059.159558	38.968858
2438.589621	440816.291919	38.973876
2440.913745	441572.524542	38.978893
2443.833385	442332.775490	38.983911
2446.320074	443084.021369	38.988928
2448.741599	443841.661711	38.993946
2451.229420	444594.260266	38.998964
2453.165087	445348.126499	39.003981
2456.285314	446108.291399	39.008999
2458.412292	446862.115763	39.014016
2460.954430	447619.984900	39.019034
2463.142367	448378.635195	39.024052
2465.499669	449118.644834	39.029069
2467.402069	449850.060834	39.034087
2470.070362	450589.203841	39.039104
2472.378662	451326.807418	39.044122
2474.734460	452064.019610	39.049140
2476.762376	452820.436742	39.054157
2479.061023	453577.536431	39.059175
2481.413283	454332.424558	39.064192
2484.262631	455086.344369	39.069210
2486.453594	455858.657555	39.074228
2488.646572	456626.999280	39.079245
2491.549654	457391.662974	39.084263
2493.630980	458163.991879	39.089280
2496.405226	458932.342366	39.094298
2498.479852	459730.340428	39.099316
2500.494874	460524.425080	39.104333
2503.301185	461311.284654	39.109351
2505.655974	462110.389305	39.114368
2508.305110	462921.166424	39.119386
2510.725414	463725.583391	39.124404
2513.163124	464534.298003	39.129421
2515.371368	465356.983714	39.134439
2517.917055	466179.778000	39.139456
2520.695719	467009.506856	39.144474
2523.181583	467840.198457	39.149492
2525.354379	468681.136289	39.154509
2528.001431	469515.803969	39.159527
2530.331507	470360.716742	39.164544
2532.767831	471206.628371	39.169562
2535.701121	472066.840759	39.174580
2538.004851	472918.685154	39.179597
2540.277864	473766.960033	39.184615
2542.765244	474634.265897	39.189632
2545.598943	475503.134620	39.194650
2548.688309	476367.479831	39.199668
2550.946085	477242.192286	39.204685
2553.479994	478100.934772	39.209703
2556.348610	478978.430256	39.214720
2558.964143	479852.842027	39.219738
2561.288924	480734.407584	39.224756
2564.238108	481613.306105	39.229773
2566.744288	482474.989548	39.234791
2569.549958	483356.483305	39.239808
2572.162763	484230.701182	39.244826
2575.402432	485097.415258	39.249844
2578.778978	485971.667094	39.254861
2580.977750	486831.594204	39.259879
2583.832567	487697.718020	39.264896
2586.045757	488561.928425	39.269914
2588.644815	489425.979020	39.274932
2590.764000	490304.763180	39.279949
2593.816354	491172.773409	39.284967
2596.629719	492048.476538	39.289984
2598.956349	492911.816068	39.295002
2601.493301	493776.382161	39.300020
2604.217822	494658.190685	39.305037
2607.069838	495526.382395	39.310055
2609.664404	496400.957708	39.315072
2612.161360	497272.072958	39.320090
2614.709768	498131.499447	39.325108
2617.527664	499011.875319	39.330125
2620.283602	499875.647120	39.335143
2623.095381	500754.559660	39.340160
2625.426310	501618.747350	39.345178
2628.355694	502482.236216	39.350196
2630.887894	503356.353933	39.355213
2633.751480	504217.081813	39.360231
2636.387847	505071.403070	39.365248
2638.688263	505902.379402	39.370266
2641.506757	506745.049633	39.375284
2643.626561	507585.817020	39.380301
2646.668599	508415.624614	39.385319
2649.170260	509255.025556	39.390336
2651.823152	510087.210051	39.395354
2653.963003	510923.750958	39.400372
2656.270194	511783.351080	39.405389
2659.389043	512619.737765	39.410407
2661.853722	513472.721241	39.415424
2664.187613	514335.578799	39.420442
2666.362981	515198.658613	39.425460
2669.025519	516075.485060	39.430477
2671.561489	516939.857153	39.435495
2673.915857	517837.583881	39.440512
2675.963127	518727.909950	39.445530
2678.869924	519631.413936	39.450548
2681.034374	520547.991670	39.455565
2683.593502	521474.095142	39.460583
2686.233667	522406.655382	39.465600
2688.821143	523330.063405	39.470618
2691.502584	524266.206269	39.475636
2693.701548	525220.044967	39.480653
2696.748107	526153.787066	39.485671
2699.804267	527110.118941	39.490688
2702.392947	528067.157842	39.495706
2704.858976	529018.620908	39.500724
2707.685843	529981.410116	39.505741
2710.430034	530947.255076	39.510759
2713.216994	531916.235687	39.515776
2715.839066	532898.978917	39.520794
2718.975825	533868.511941	39.525812
2722.084385	534847.666502	39.530829
2725.018491	535824.112864	39.535847
2728.490847	536773.292464	39.540864
2731.187160	537750.482181	39.545882
2734.599746	538712.627793	39.550900
2737.353591	539664.414290	39.555917
2740.038934	540623.015128	39.560935
2743.198685	541579.612095	39.565952
2746.060248	542535.129054	39.570970
2749.164649	543481.052268	39.575988
2752.019287	544453.231688	39.581005
2754.398075	545405.242881	39.586023
2757.663775	546350.270388	39.591040
2760.175644	547309.036628	39.596058
2763.198615	548255.912232	39.601076
2765.602503	549224.075318	39.606093
2768.443006	550162.557371	39.611111
2771.333977	551119.211190	39.616128
2773.707907	552074.567013	39.621146
2776.693315	553042.335698	39.626164
2779.538866	554012.805933	39.631181
2781.809530	554963.838844	39.636199
2784.756407	555925.567295	39.641216
2787.323984	556905.821619	39.646234
2790.284171	557869.797258	39.651252
2792.646901	558845.514023	39.656269
2795.576169	559815.049221	39.661287
2798.732869	560805.061256	39.666304
2801.284919	561771.638966	39.671322
2804.694564	562746.869647	39.676340
2807.005886	563725.045995	39.681357
2810.211055	564681.113394	39.686375
2813.059865	565650.579772	39.691392
2816.077565	566634.260783	39.696410
2818.719998	567593.531473	39.701428
2821.323644	568553.129037	39.706445
2824.055780	569495.654634	39.711463
2827.117184	570436.649607	39.716480
2829.411088	571372.981891	39.721498
2832.176967	572306.510741	39.726516
2834.406537	573262.168033	39.731533
2836.902163	574203.690937	39.736551
2839.307555	575165.865927	39.741568
2842.075603	576137.108567	39.746586
2845.184069	577106.312868	39.751604
2847.852438	578085.057221	39.756621
2850.389668	579064.586719	39.761639
2853.024395	580055.168788	39.766656
2855.916343	581054.574643	39.771674
2859.190217	582046.329267	39.776692
2861.848447	583049.291983	39.781709
2864.205223	584052.960441	39.786727
2867.353516	585073.711584	39.791744
2870.337248	586091.693736	39.796762
2873.062306	587113.470207	39.801780
2875.774894	588134.202978	39.806797
2878.669399	589170.153859	39.811815
2881.534567	590196.215648	39.816832
2884.721015	591243.015485	39.821850
2887.791328	592277.091168	39.826868
2890.593585	593336.287111	39.831885
2893.176015	594371.934998	39.836903
2896.289867	595428.776303	39.841920
2899.055043	596485.067437	39.846938
2902.103249	597548.249937	39.851956
2904.627017	598607.712288	39.856973
2907.681612	599688.752942	39.861991
2910.931301	600757.870074	39.867008
2913.584014	601839.649924	39.872026
2916.562854	602916.924143	39.877044
2919.402556	604001.344724	39.882061
2922.009787	605093.522470	39.887079
2925.192305	606193.228462	39.892096
2927.977468	607284.447575	39.897114
2930.815348	608384.222281	39.902132
2933.859069	609491.478031	39.907149
2936.563473	610601.060473	39.912167
2940.189429	611701.301550	39.917184
2942.868760	612809.948089	39.922202
2946.245166	613916.569012	39.927220
2949.232373	615023.527912	39.932237
2952.056237	616126.003715	39.937255
2955.639250	617227.591358	39.942272
2958.608592	618341.063944	39.947290
2961.897967	619438.914458	39.952308
2964.747306	620540.448986	39.957325
2967.790613	621651.545063	39.962343
2970.943203	622745.064054	39.967360
2973.813181	623852.601057	39.972378
2976.545510	624952.912593	39.977396
2980.089503	626064.028001	39.982413
2982.383386	627172.672665	39.987431
2985.684036	628280.236680	39.992448
2988.035154	629396.334601	39.997466
2991.377042	630513.840748	40.002484
2994.163263	631622.644278	40.007501
2997.608646	632741.268407	40.012519
3000.876508	633853.271276	40.017536
3003.426839	634980.181648	40.022554
3006.709932	636096.745650	40.027572
3009.551105	637218.817818	40.032589
3012.203177	638344.317233	40.037607
3015.375442	639457.616625	40.042624
3017.709437	640578.422872	40.047642
3021.232075	641661.821716	40.052660
3023.951782	642755.957485	40.057677
3026.770608	643847.662742	40.062695
3030.029146	644935.990142	40.067712
3032.809595	646034.202569	40.072730
3035.355580	647123.874340	40.077748
3038.429358	648227.145485	40.082765
3041.397941	649323.445369	40.087783
3044.395198	650432.969983	40.092800
3048.071915	651536.442925	40.097818
3050.890908	652638.227738	40.102836
3054.213878	653755.240900	40.107853
3056.950983	654877.469840	40.112871
3060.730998	655994.134453	40.117888
3063.716492	657107.012565	40.122906
3066.888446	658218.581957	40.127924
3070.318098	659345.602690	40.132941
3072.993197	660473.194192	40.137959
3076.340600	661596.172147	40.142976
3079.294945	662738.859521	40.147994
3082.322054	663873.601558	40.153012
3085.437546	665002.233154	40.158029
3087.917701	666160.864857	40.163047
3091.046382	667300.750816	40.168064
3093.974591	668465.798709	40.173082
3096.864044	669630.151602	40.178100
3099.846372	670795.077122	40.183117
3102.680719	671981.967111	40.188135
3105.803324	673157.204957	40.193152
3108.580651	674343.481354	40.198170
3111.984217	675531.377838	40.203188
3115.301876	676737.197525	40.208205
3118.040151	677938.382120	40.213223
3121.275567	679141.844109	40.218240
3124.077941	680359.508092	40.223258
3127.361264	681584.889604	40.228276
3130.281233	682799.955953	40.233293
3133.389799	684034.805858	40.238311
3136.602166	685267.577631	40.243328
3139.363541	686498.160499	40.248346
3142.688338	687744.793594	40.253364
3145.887290	688989.973483	40.258381
3149.234380	690247.995045	40.263399
3152.359851	691486.333518	40.268416
3155.629544	692744.480200	40.273434
3159.003534	693985.664967	40.278452
3162.019026	695236.302894	40.283469
3165.459949	696491.869674	40.288487
3168.565271	697751.987417	40.293504
3172.065862	699010.365751	40.298522
3175.064012	700258.750688	40.303540
3178.571866	701520.291528	40.308557
3182.024187	702778.137970	40.313575
3185.432418	704024.194917	40.318592
3188.590264	705274.932608	40.323610
3191.655358	706522.379736	40.328628
3195.063305	707765.926478	40.333645
3198.273750	709024.155486	40.338663
3201.644971	710288.323285	40.343680
3204.973822	711546.821126	40.348698
3208.523226	712777.917321	40.353716
3212.102588	714015.420308	40.358733
3215.125080	715254.933165	40.363751
3218.410508	716491.989726	40.368768
3221.623012	717735.708772	40.373786
3224.685846	718985.458076	40.378804
3228.152961	720214.796468	40.383821
3231.297076	721445.909245	40.388839
3234.075725	722645.270129	40.393856
3237.219641	723845.665633	40.398874
3240.387105	725037.401916	40.403892
3243.570611	726224.174840	40.408909
3246.469546	727435.065786	40.413927
3250.153012	728634.963663	40.418944
3252.555037	729838.412597	40.423962
3255.680230	731059.557123	40.428980
3258.957352	732273.938481	40.433997
3262.046651	733497.444586	40.439015
3265.254485	734733.955263	40.444032
3268.159392	735971.143108	40.449050
3270.860916	737222.407759	40.454068
3274.443912	738466.689506	40.459085
3277.172150	739740.518069	40.464103
3280.389874	741003.145073	40.469120
3283.100011	742291.612733	40.474138
3286.450969	743586.774365	40.479156
3290.047232	744867.921579	40.484173
3293.341227	746171.026589	40.489191
3296.666780	747472.125490	40.494208
3300.319594	748779.121022	40.499226
3303.999657	750086.659899	40.504244
3307.426100	751381.542127	40.509261
3310.774738	752694.542749	40.514279
3314.398359	753992.598933	40.519296
3317.983960	755291.061535	40.524314
3321.559903	756605.510920	40.529332
3324.938057	757907.104327	40.534349
3327.764305	759227.994321	40.539367
3331.726781	760546.940168	40.544384
3335.395847	761852.607466	40.549402
3338.308112	763173.475655	40.554420
3341.523068	764496.347327	40.559437
3344.751740	765828.509908	40.564455
3347.991389	767144.950452	40.569472
3351.400014	768487.779943	40.574490
3354.492302	769826.483787	40.579508
3358.055660	771159.864505	40.584525
3360.939798	772503.849934	40.589543
3364.722998	773855.301818	40.594560
3368.075228	775199.220925	40.599578
3371.212011	776549.798636	40.604596
3374.759344	777904.635832	40.609613
3378.558853	779264.193489	40.614631
3382.031533	780621.378731	40.619648
3385.692582	781966.247684	40.624666
3388.744060	783332.130332	40.629684
3392.304463	784674.663744	40.634701
3395.485115	786042.167423	40.639719
3398.893526	787397.887744	40.644736
3402.244872	788777.242223	40.649754
3405.812186	790129.206530	40.654772
3408.823047	791496.047287	40.659789
3411.921422	792876.239934	40.664807
3415.190978	794261.963535	40.669824
3418.935226	795635.428336	40.674842
3421.961289	797020.310715	40.679860
3425.220820	798411.680213	40.684877
3428.654624	799802.430882	40.689895
3432.257055	801189.057469	40.694912
3435.887806	802574.991087	40.699930
3438.973972	803971.076324	40.704948
3443.057673	805361.494394	40.709965
3446.205256	806759.684708	40.714983
3449.603071	808148.336141	40.720000
3453.062055	809530.741406	40.725018
3456.106527	810918.475597	40.730023
3459.706475	812262.465530	40.735028
3462.408460	813566.164753	40.740032
3465.527256	814800.264589	40.745037
3468.882406	815995.319395	40.750042
3472.140452	817125.110418	40.755047
3475.019503	818187.866818	40.760052
3478.123726	819184.112229	40.765056
3480.877064	820119.127063	40.770061
3483.755967	821004.153398	40.775066
3485.868171	821807.240773	40.780071
3488.358595	822566.381778	40.785076
3490.626611	823259.894838	40.790080
3492.521823	823896.580213	40.795085
3494.549713	824489.118136	40.800090
3496.366456	825030.183643	40.805095
3498.242826	825507.980984	40.810100
3499.880137	825952.521965	40.815104
3501.598135	826344.122431	40.820109
3502.918474	826697.937865	40.825114
3503.589250	827008.958555	40.830119
3505.456825	827278.944051	40.835124
3506.404270	827532.340284	40.840128
3507.316088	827745.096848	40.845133
3508.283107	827921.772658	40.850138
3509.613761	828072.334998	40.855143
3510.454625	828177.866948	40.860148
3510.709747	828279.017246	40.865152
3511.301159	828337.927332	40.870157
3512.293504	828388.803597	40.875162
3512.798857	828417.885211	40.880167
3513.423664	828418.759582	40.885172
3514.169814	828407.756365	40.890176
3514.521746	828371.250558	40.895181
3515.015567	828326.362884	40.900186
3515.080143	828261.323534	40.905191
3515.451863	828173.878224	40.910196
3515.818773	828092.556450	40.915200
3515.904294	828004.861831	40.920205
3516.240567	827890.394020	40.925210
3516.385554	827777.314926	40.930215
3516.788820	827644.264506	40.935220
3517.076774	827507.534990	40.940224
3517.388442	827349.605043	40.945229
3517.211838	827195.150076	40.950234
3517.190771	827041.736340	40.955239
3517.548985	826872.022668	40.960244
3517.450070	826689.833169	40.965248
3517.626865	826513.137361	40.970253
3517.678591	826321.676264	40.975258
3517.275990	826148.852653	40.980263
3517.477474	825962.996696	40.985268
3517.752360	825771.094492	40.990272
3517.767814	825574.364470	40.995277
3517.954601	825367.195557	41.000282
3517.553048	825170.420477	41.005287
3517.991607	824958.043920	41.010292
3517.790681	824749.942153	41.015296
3517.814127	824539.852971	41.020301
3517.820097	824316.628282	41.025306
3517.213686	824105.552732	41.030311
3517.683111	823886.519833	41.035316
3517.206359	823666.167867	41.040320
3517.193442	823455.366275	41.045325
3517.268356	823236.760991	41.050330
3517.054551	823015.955446	41.055335
3517.020564	822805.329420	41.060340
3517.052742	822590.015707	41.065344
3516.897141	822368.204858	41.070349
3517.313069	822146.004769	41.075354
3517.003447	821925.369657	41.080359
3516.575744	821707.469733	41.085364
3516.600807	821485.404228	41.090368
3516.755276	821262.434659	41.095373
3516.733131	821042.988120	41.100378
3516.205674	820826.143147	41.105383
3516.337175	820607.143706	41.110388
3516.042834	820388.300399	41.115392
3515.887996	820174.586156	41.120397
3515.847654	819957.439871	41.125402
3515.697967	819749.160928	41.130407
3515.911624	819531.960005	41.135412
3515.430632	819316.612279	41.140416
3515.154176	819111.836161	41.145421
3515.364194	818901.038727	41.150426
3514.933577	818692.476098	41.155431
3514.780619	818476.755831	41.160436
3515.021962	818278.491663	41.165440
3514.762720	818074.262758	41.170445
3514.528785	817871.873182	41.175450
3514.447080	817671.887510	41.180455
3514.381950	817464.979186	41.185460
3514.224656	817277.164497	41.190464
3514.185810	817071.017979	41.195469
3513.979962	816873.655330	41.200474
3513.279394	816683.959968	41.205479
3513.588025	816495.367136	41.210484
3513.495648	816301.864230	41.215488
3513.210916	816116.274476	41.220493
3513.233510	815928.877972	41.225498
3512.824903	815758.491167	41.230503
3513.253961	815568.585258	41.235508
3513.111077	815379.931873	41.240512
3512.711277	815205.047825	41.245517
3512.747913	815023.661386	41.250522
3512.543037	814850.587792	41.255527
3512.312907	814677.318514	41.260532
3512.270670	814495.441983	41.265536
3511.822059	814328.139886	41.270541
3511.914760	814146.524388	41.275546
3511.590488	813986.695587	41.280551
3511.669136	813819.200031	41.285556
3511.563838	813655.041526	41.290560
3511.357413	813492.940706	41.295565
3511.624955	813331.443678	41.300570
3511.265665	813176.958862	41.305575
3510.881342	813006.103481	41.310580
3511.018661	812848.901949	41.315584
3511.052453	812705.550473	41.320589
3511.172746	812536.942219	41.325594
3510.884233	812385.155494	41.330599
3510.571318	812216.606360	41.335604
3510.742391	812067.956204	41.340608
3510.399136	811920.747393	41.345613
3510.421638	811767.630134	41.350618
3510.339457	811622.810132	41.355623
3510.356606	811477.776333	41.360628
3509.994760	811328.412262	41.365632
3509.916270	811186.700706	41.370637
3510.238562	811035.468230	41.375642
3509.846234	810905.106503	41.380647
3509.750704	810761.633460	41.385652
3509.646243	810615.039136	41.390656
3509.531460	810483.845454	41.395661
3509.524715	810344.638323	41.400666
3509.160705	810218.839805	41.405671
3508.892688	810085.517061	41.410676
3508.967474	809959.839766	41.415680
3508.710776	809827.484719	41.420685
3508.576796	809706.709709	41.425690
3508.750968	809578.084412	41.430695
3508.854027	809452.685101	41.435700
3508.769169	809325.460150	41.440704
3508.552002	809199.715874	41.445709
3508.367225	809078.254270	41.450714
3508.166155	808969.273793	41.455719
3508.324113	808839.855960	41.460724
3508.217886	808727.394920	41.465728
3507.968592	808603.837812	41.470733
3508.243780	808486.485990	41.475738
3507.935662	808379.169832	41.480743
3507.580644	808262.497472	41.485748
3507.478636	808168.700504	41.490752
3507.676593	808054.570895	41.495757
3507.552575	807940.977179	41.500762
3507.336574	807835.636631	41.505767
3507.581576	807720.957281	41.510772
3507.299169	807620.792435	41.515776
3506.889526	807536.445627	41.520781
3507.254497	807434.469880	41.525786
3506.925420	807333.234951	41.530791
3506.935083	807227.653966	41.535796
3507.024454	807132.251213	41.540800
3506.776790	807039.533205	41.545805
3506.769145	806931.852969	41.550810
3506.096950	806841.100424	41.555815
3506.490366	806749.545985	41.560820
3506.701443	806661.627808	41.565824
3506.461768	806559.927633	41.570829
3507.023389	806466.782127	41.575834
3506.528977	806381.506543	41.580839
3506.599432	806288.093788	41.585844
3506.521710	806201.677624	41.590848
3506.402631	806103.560633	41.595853
3506.295004	806010.513070	41.600858
3506.570993	805925.647482	41.605863
3506.238187	805825.754873	41.610868
3506.542075	805743.662827	41.615872
3505.871836	805662.990252	41.620877
3505.829925	805571.389366	41.625882
3505.646878	805487.565293	41.630887
3505.914113	805408.840500	41.635892
3505.784013	805323.152314	41.640896
3505.718859	805244.818928	41.645901
3505.604324	805160.345673	41.650906
3505.247299	805088.788011	41.655911
3505.220482	805026.446853	41.660916
3505.433407	804952.310591	41.665920
3505.015365	804876.906125	41.670925
3505.013206	804800.216117	41.675930
3505.179637	804732.524255	41.680935
3505.669534	804658.682790	41.685940
3505.193687	804586.991713	41.690944
3504.767011	804518.365766	41.695949
3505.314159	804439.292534	41.700954
3504.703911	804382.890883	41.705959
3504.738960	804316.581235	41.710964
3504.903671	804247.957513	41.715968
3504.565721	804185.461620	41.720973
3504.655842	804111.286004	41.725978
3504.384902	804056.389730	41.730983
3504.682940	803997.354334	41.735988
3504.602870	803925.252414	41.740992
3504.738690	803864.582217	41.745997
3504.521348	803798.648199	41.751002
3504.452300	803749.084970	41.756007
3504.859304	803690.664029	41.761012
3504.584795	803625.420277	41.766016
3504.434990	803559.912390	41.771021
3504.681275	803492.487686	41.776026
3504.327452	803438.135809	41.781031
3504.722952	803366.880375	41.786036
3504.366511	803310.771152	41.791040
3504.053566	803264.706874	41.796045
3503.948283	803196.699650	41.801050
3503.645835	803147.997811	41.806055
3503.868767	803097.554325	41.811060
3504.031710	803049.950155	41.816064
3504.137847	803004.062484	41.821069
3504.165392	802940.521302	41.826074
3503.816967	802884.992688	41.831079
3503.820820	802827.749304	41.836084
3503.822462	802781.046761	41.841088
3503.938143	802735.302078	41.846093
3503.905631	802672.987663	41.851098
3503.728564	802635.779529	41.856103
3503.707981	802581.075467	41.861108
3503.795952	802526.061152	41.866112
3503.621090	802491.438386	41.871117
3503.649800	802429.063227	41.876122
3503.528946	802394.821925	41.881127
3503.655348	802345.119669	41.886132
3503.665750	802301.877368	41.891136
3503.467635	802252.566756	41.896141
3503.721173	802200.354452	41.901146
3503.557155	802151.037730	41.906151
3503.458825	802111.959630	41.911156
3503.197792	802061.730071	41.916160
3503.349489	802026.126423	41.921165
3503.326413	801969.416462	41.926170
3503.509246	801942.348718	41.931175
3503.337580	801892.591938	41.936180
3503.070473	801853.636264	41.941184
3502.877582	801813.985435	41.946189
3503.070892	801772.956158	41.951194
3503.009640	801736.652065	41.956199
3502.910613	801695.472756	41.961204
3502.805061	801661.225147	41.966208
3503.031222	801632.294565	41.971213
3503.224182	801585.846275	41.976218
3503.079482	801552.092304	41.981223
3502.900080	801508.190983	41.986228
3502.793455	801476.090221	41.991232
3502.798091	801428.645206	41.996237
3502.779618	801396.823134	42.001242
3502.955304	801372.682795	42.006247
3503.026297	801330.644773	42.011252
3502.857427	801290.157151	42.016256
3502.627055	801255.536393	42.021261
3502.720740	801228.430768	42.026266
3502.596515	801213.171809	42.031271
3502.756705	801180.686172	42.036276
3502.714111	801132.416532	42.041280
3502.497201	801104.089785	42.046285
3502.734195	801074.471612	42.051290
3502.326409	801037.143832	42.056295
3502.634412	801016.740165	42.061300
3502.226137	800980.388418	42.066304
3502.153478	800942.421924	42.071309
3502.541387	800927.423934	42.076314
3502.104526	800911.529721	42.081319
3502.255803	800879.385662	42.086324
3502.297943	800848.722972	42.091328
3502.008807	800831.975604	42.096333
3502.378249	800792.718724	42.101338
3502.408542	800760.397720	42.106343
3502.549203	800748.611022	42.111348
3502.657241	800712.030597	42.116352
3501.990368	800683.235351	42.121357
3502.410909	800651.926769	42.126362
3502.117311	800642.355712	42.131367
3502.074237	800611.656397	42.136372
3502.430625	800577.526072	42.141376
3502.093999	800556.977632	42.146381
3502.370670	800538.920606	42.151386
3502.040321	800513.684520	42.156391
3501.767418	800483.703976	42.161396
3502.076592	800470.572331	42.166400
3501.984879	800439.245156	42.171405
3502.089635	800413.598931	42.176410
3502.080609	800391.729459	42.181415
3502.118814	800380.299838	42.186420
3502.079385	800358.044451	42.191424
3502.200657	800331.711848	42.196429
3501.947463	800296.406019	42.201434
3501.932975	800274.097624	42.206439
3502.153751	800262.053414	42.211444
3502.303489	800233.860799	42.216448
3501.807085	800218.169456	42.221453
3502.148598	800189.312002	42.226458
3502.199780	800165.040140	42.231463
3502.083996	800145.139351	42.236468
3502.088331	800121.899889	42.241472
3501.665075	800095.407336	42.246477
3501.645421	800079.934056	42.251482
3501.539363	800055.442253	42.256487
3501.600969	800038.296236	42.261492
3501.812451	800032.599874	42.266496
3501.610826	800011.296258	42.271501
3501.926732	799996.063254	42.276506
3501.669230	799965.003799	42.281511
3501.545101	799960.043350	42.286516
3501.723653	799945.905790	42.291520
3501.745970	799936.528408	42.296525
3501.888479	799914.926565	42.301530
3501.710244	799901.039971	42.306535
3501.987692	799873.558159	42.311540
3501.712407	799854.462574	42.316544
3501.686740	799853.636615	42.321549
3501.788469	799825.303250	42.326554
3501.510388	799807.428546	42.331559
3501.678603	799780.744590	42.336564
3501.658975	799773.961184	42.341568
3501.419505	799756.666188	42.346573
3501.820365	799738.489863	42.351578
3501.655097	799716.154283	42.356583
3501.591817	799704.885802	42.361588
3502.005522	799696.862793	42.366592
3501.633287	799680.223061	42.371597
3501.517856	799664.861406	42.376602
3501.988491	799635.639523	42.381607
3501.777995	799617.216653	42.386612
3501.947332	799597.904327	42.391616
3501.820767	799577.710521	42.396621
3501.873589	799558.025688	42.401626
3502.156237	799548.118792	42.406631
3501.757587	799529.236828	42.411636
3501.827849	799499.149229	42.416640
3501.466595	799490.270591	42.421645
3501.564933	799467.844117	42.426650
3501.859778	799455.396218	42.431655
3501.872502	799437.230895	42.436660
3501.359810	799420.026532	42.441664
3501.698249	799406.058103	42.446669
3501.443294	799385.639632	42.451674
3501.584134	799370.871963	42.456679
3501.599436	799360.664785	42.461684
3501.632717	799338.101550	42.466688
3501.382839	799335.503973	42.471693
3501.649065	799318.226403	42.476698
3501.686384	799311.189472	42.481703
3501.305753	799292.987579	42.486708
3501.635622	799269.059400	42.491712
3501.284981	799259.934647	42.496717
3501.370780	799259.091187	42.501722
3501.578110	799244.215180	42.506727
3501.548332	799228.009023	42.511732
3501.566298	799211.600050	42.516736
3501.225020	799197.737426	42.521741
3501.823737	799192.956357	42.526746
3501.654448	799167.299190	42.531751
3501.483929	799156.339483	42.536756
3501.490282	799132.559029	42.541760
3501.250785	799125.809312	42.546765
3501.267774	799111.353382	42.551770
3501.545224	799101.348959	42.556775
3501.418595	799087.403715	42.561780
3501.621167	799081.170793	42.566784
3501.395949	799056.352020	42.571789
3501.551602	799041.678942	42.576794
3501.523615	799036.751580	42.581799
3501.350774	799022.569273	42.586804
3501.506234	799007.407853	42.591808
3501.299349	798992.254210	42.596813
3501.551223	798966.090939	42.601818
3501.324757	798971.741794	42.606823
3501.713201	798956.543835	42.611828
3501.650073	798934.482561	42.616832
3501.351992	798931.257563	42.621837
3501.519657	798910.918014	42.626842
3501.575685	798909.297879	42.631847
3501.712210	798891.795294	42.636852
3501.291401	798869.154914	42.641856
3501.581076	798855.681229	42.646861
3501.527258	798839.477855	42.651866
3501.644824	798837.164451	42.656871
3501.438583	798817.224873	42.661876
3501.457441	798803.402765	42.666880
3501.084236	798796.575941	42.671885
3501.205041	798781.663565	42.676890
3501.467337	798780.987779	42.681895
3501.122458	798769.957009	42.686900
3501.403307	798760.146854	42.691904
3501.244369	798750.503096	42.696909
3501.370281	798733.245898	42.701914
3501.456932	798731.572100	42.706919
3501.403638	798709.948006	42.711924
3501.386283	798689.001870	42.716928
3501.279456	798698.394319	42.721933
3501.626164	798661.764963	42.726938
3501.381642	798654.576047	42.731943
3501.428971	798645.876532	42.736948
3501.382850	798630.013255	42.741952
3500.994375	798630.122837	42.746957
3501.220272	798619.197914	42.751962
3501.405784	798608.621114	42.756967
3500.964476	798587.643256	42.761972
3501.354834	798582.601319	42.766976
3501.199327	798579.207357	42.771981
3501.492227	798558.407628	42.776986
3501.037858	798553.937214	42.781991
3500.767429	798545.238403	42.786996
3501.290237	798547.158854	42.792001
3500.875362	798539.752274	42.797005
3501.081271	798520.724014	42.802010
3500.770425	798515.059139	42.807015
3500.809919	798521.157143	42.812020
3500.954019	798512.979487	42.817025
3501.086310	798516.181826	42.822029
3501.012864	798502.520004	42.827034
3500.664619	798497.349293	42.832039
3500.924161	798482.072706	42.837044
3501.230292	798480.266867	42.842049
3500.801410	798488.635627	42.847053
3501.332700	798488.454931	42.852058
3501.062659	798462.371211	42.857063
3501.043964	798460.713811	42.862068
3500.946203	798458.092097	42.867073
3500.749339	798455.241706	42.872077
3500.785265	798451.866585	42.877082
3501.066866	798451.041248	42.882087
3500.892624	798434.416179	42.887092
3501.139434	798421.876136	42.892097
3501.026279	798418.573137	42.897101
3500.856494	798423.629600	42.902106
3501.047276	798421.744109	42.907111
3501.177542	798410.638448	42.912116
3501.445822	798388.377001	42.917121
3501.397409	798393.707519	42.922125
3501.309025	798381.073294	42.927130
3501.201747	798368.637334	42.932135
3501.262635	798366.039617	42.937140
3501.158610	798362.832830	42.942145
3501.248796	798355.835430	42.947149
3501.252067	798332.101348	42.952154
3501.237768	798339.135791	42.957159
3501.480232	798326.547409	42.962164
3501.272103	798305.141504	42.967169
3501.170029	798298.906619	42.972173
3501.316411	798291.412016	42.977178
3501.212127	798267.743346	42.982183
3501.007466	798265.626615	42.987188
3501.171637	798261.889502	42.992193
3501.348777	798266.305834	42.997197
3501.539945	798239.172413	43.002202
3501.447304	798237.673021	43.007207
3501.381739	798228.355733	43.012212
3501.224044	798208.357851	43.017217
3501.329424	798195.448795	43.022221
3500.998280	798188.419406	43.027226
3500.973266	798180.170095	43.032231
3501.192448	798165.192086	43.037236
3501.027090	798167.513244	43.042241
3501.047270	798167.656620	43.047245
3501.161095	798157.090290	43.052250
3501.164735	798140.485494	43.057255
3500.804405	798132.386212	43.062260
3501.017354	798131.620404	43.067265
3500.978626	798138.561211	43.072269
3500.906684	798134.128393	43.077274
3501.191174	798116.161056	43.082279
3500.756305	798103.287432	43.087284
3500.907214	798100.724373	43.092289
3501.216260	798098.331938	43.097293
3501.079340	798100.599839	43.102298
3501.161560	798102.540464	43.107303
3501.165801	798088.230749	43.112308
3501.289035	798073.707056	43.117313
3500.827541	798072.997834	43.122317
3501.144355	798062.936821	43.127322
3501.320754	798046.109431	43.132327
3500.923486	798038.455336	43.137332
3501.141703	798029.777116	43.142337
3501.184170	798040.416942	43.147341
3501.202045	798013.700360	43.152346
3501.366431	798020.023499	43.157351
3501.069031	798017.188628	43.162356
3501.223935	798001.390059	43.167361
3501.191617	797982.397459	43.172365
3500.819617	797970.539325	43.177370
3501.022681	797979.054139	43.182375
3500.824840	797978.157180	43.187380
3501.489626	797967.113714	43.192385
3501.427342	797956.476912	43.197389
3501.527167	797941.565881	43.202394
3501.587132	797930.323875	43.207399
3501.197647	797918.468379	43.212404
3501.612558	797912.396494	43.217409
3501.320174	797896.032697	43.222413
3501.305294	797876.255652	43.227418
3501.172591	797872.711238	43.232423
3500.957352	797858.533002	43.237428
3501.467428	797836.964437	43.242433
3501.400573	797845.961167	43.247437
3500.927731	797830.357988	43.252442
3501.152038	797832.227645	43.257447
3501.189461	797814.493448	43.262452
3500.953970	797799.732186	43.267457
3500.730819	797810.120880	43.272461
3501.183827	797805.654614	43.277466
3501.093998	797788.917012	43.282471
3500.874278	797779.330142	43.287476
3501.024691	797771.638954	43.292481
3500.790807	797772.896509	43.297485
3500.995629	797769.152759	43.302490
3501.041811	797771.489829	43.307495
3500.597136	797757.249558	43.312500
3500.976919	797747.129375	43.317505
3500.492215	797744.763214	43.322509
3500.669414	797745.565801	43.327514
3500.795939	797734.947958	43.332519
3501.037987	797749.415355	43.337524
3501.062574	797736.371497	43.342529
3501.115969	797747.010096	43.347533
3500.933429	797728.626303	43.352538
3501.097971	797722.398023	43.357543
3501.119166	797724.006428	43.362548
3501.329935	797730.224921	43.367553
3501.115748	797713.067010	43.372557
3501.109731	797693.922934	43.377562
3501.340690	797696.475344	43.382567
3501.234392	797689.947495	43.387572
3500.969865	797672.943865	43.392577
3500.928443	797652.926089	43.397581
3500.766300	797661.058855	43.402586
3501.162832	797653.280213	43.407591
3501.087628	797651.875638	43.412596
3501.356192	797650.026607	43.417601
3501.400606	797633.169937	43.422605
3501.084713	797626.235229	43.427610
3501.117022	797630.967677	43.432615
3500.831103	797604.296896	43.437620
3501.090553	797596.197734	43.442625
3501.079236	797596.394887	43.447629
3501.001116	797595.576838	43.452634
3501.085434	797585.453751	43.457639
3500.998790	797567.591752	43.462644
3501.287957	797553.382837	43.467649
3500.590131	797569.902338	43.472653
3500.994624	797572.427671	43.477658
3501.433034	797560.442098	43.482663
3501.401194	797536.124501	43.487668
3501.188345	797526.780386	43.492673
3501.121533	797537.438120	43.497677
3501.118923	797515.850953	43.502682
3501.252946	797498.979927	43.507687
3501.166336	797495.037373	43.512692
3500.968869	797499.512789	43.517697
3501.153499	797491.571716	43.522701
3501.296648	797467.812600	43.527706
3501.030799	797454.325164	43.532711
3500.912392	797453.659919	43.537716
3501.550683	797451.020417	43.542721
3501.158542	797433.987266	43.547725
3501.080574	797422.375209	43.552730
3501.149574	797428.030058	43.557735
3501.289787	797411.890459	43.562740
3501.277487	797390.450914	43.567745
3501.301188	797390.544915	43.572749
3501.192214	797394.615837	43.577754
3501.376109	797380.276475	43.582759
3501.309622	797362.313076	43.587764
3501.572134	797353.333978	43.592769
3501.031809	797345.945631	43.597773
3501.174328	797330.440417	43.602778
3501.320919	797326.021725	43.607783
3501.381800	797317.318308	43.612788
3501.304643	797302.335789	43.617793
3500.896752	797290.579701	43.622797
3500.890536	797281.447141	43.627802
3501.195761	797282.327460	43.632807
3500.973574	797277.673328	43.637812
3501.010387	797261.158777	43.642817
3501.003090	797256.812937	43.647821
3500.942894	797255.112873	43.652826
3500.889209	797252.630307	43.657831
3500.762744	797267.205232	43.662836
3501.139521	797238.622172	43.667841
3500.978074	797232.249011	43.672845
3500.609997	797224.784755	43.677850
3500.530348	797232.270203	43.682855
3500.621445	797220.826727	43.687860
3500.749561	797214.896714	43.692865
3500.739788	797226.864805	43.697869
3500.953480	797229.859688	43.702874
3501.061443	797231.015064	43.707879
3500.404610	797221.495696	43.712884
3500.473804	797210.153312	43.717889
3500.721736	797212.849791	43.722893
3500.543356	797208.872564	43.727898
3501.044031	797213.971689	43.732903
3500.745261	797214.751062	43.737908
3501.186985	797207.502099	43.742913
3500.831233	797220.843049	43.747917
3500.990550	797216.324607	43.752922
3500.796010	797199.211105	43.757927
3500.759002	797181.731029	43.762932
3501.086309	797179.530780	43.767937
3500.784516	797184.608841	43.772941
3501.039546	797176.607535	43.777946
3500.824743	797188.656591	43.782951
3501.171505	797185.134534	43.787956
3501.407906	797169.809634	43.792961
3501.140046	797155.100803	43.797965
3500.947529	797152.297996	43.802970
3501.157880	797151.483639	43.807975
3501.089363	797138.453133	43.812980
3501.049134	797126.541585	43.817985
3500.866405	797123.395328	43.822989
3500.958035	797121.378433	43.827994
3500.950365	797102.916683	43.832999
3500.443330	797105.877756	43.838004
3500.651850	797091.240843	43.843009
3501.009007	797095.776369	43.848013
3500.921377	797083.383711	43.853018
3500.908250	797088.074814	43.858023
3501.016398	797092.356203	43.863028
3501.029741	797079.947755	43.868033
3501.193114	797075.184361	43.873037
3501.007575	797061.048577	43.878042
3500.978074	797051.284359	43.883047
3501.295849	797062.029288	43.888052
3500.802564	797054.095965	43.893057
3500.827246	797059.220777	43.898061
3500.981694	797041.710394	43.903066
3500.996296	797022.414579	43.908071
3500.982831	797034.774358	43.913076
3500.928648	797028.042316	43.918081
3500.632748	797027.453616	43.923085
3500.860532	797027.613409	43.928090
3500.978514	797015.725770	43.933095
3500.895827	796998.691942	43.938100
3501.071141	796987.527959	43.943105
3500.778060	797003.155263	43.948109
3501.173873	796992.445266	43.953114
3501.406302	796990.308631	43.958119
3501.258730	796980.660453	43.963124
3501.308416	796963.752375	43.968129
3501.515703	796955.953642	43.973133
3501.410310	796938.874361	43.978138
3501.141819	796932.419947	43.983143
3500.946576	796923.707195	43.988148
3501.075836	796916.360218	43.993153
3500.921365	796899.532732	43.998157
3500.657210	796888.779197	44.003162
3501.042701	796886.472064	44.008167
3501.261645	796895.571971	44.013172
3501.157450	796883.963049	44.018177
3500.967372	796869.290255	44.023181
3501.134052	796854.415121	44.028186
3501.263994	796855.322901	44.033191
3500.862961	796865.692065	44.038196
3501.124104	796851.583689	44.043201
3500.710402	796833.966177	44.048205
3500.840054	796825.837502	44.053210
3500.656329	796822.935485	44.058215
3500.480725	796833.513690	44.063220
3500.895218	796820.407039	44.068225
3500.807581	796827.259203	44.073229
3500.942626	796826.700810	44.078234
3500.970713	796830.262198	44.083239
3500.520833	796819.439888	44.088244
3500.778679	796803.182696	44.093249
3500.947189	796802.130608	44.098253
3500.824287	796793.845988	44.103258
3500.753641	796803.430909	44.108263
3500.644570	796798.954134	44.113268
3500.694822	796804.514765	44.118273
3500.796443	796806.990056	44.123277
3500.954248	796804.620795	44.128282
3501.218357	796797.692220	44.133287
3501.064400	796787.702830	44.138292
3501.362659	796770.169235	44.143297
3500.813843	796777.142390	44.148301
3500.918799	796768.577887	44.153306
3500.984738	796748.882462	44.158311
3500.974364	796750.691429	44.163316
3501.184276	796742.012791	44.168321
3500.851454	796736.594016	44.173325
3500.842400	796743.629371	44.178330
3500.825070	796748.858688	44.183335
3500.518014	796734.741188	44.188340
3501.005892	796722.599803	44.193345
3500.983427	796723.238346	44.198349
3500.307005	796719.680599	44.203354
3500.896695	796727.697004	44.208359
3500.673578	796734.521597	44.213364
3501.036774	796733.097137	44.218369
3500.896912	796728.136659	44.223373
3501.008238	796725.188474	44.228378
3501.137158	796709.781598	44.233383
3501.181700	796699.663348	44.238388
3501.212086	796689.009978	44.243393
3501.006035	796697.541588	44.248397
3500.827189	796678.763460	44.253402
3500.861120	796668.011807	44.258407
3500.862734	796664.201496	44.263412
3501.016956	796657.631881	44.268417
3500.991143	796665.842274	44.273421
3500.655142	796659.788918	44.278426
3500.888261	796662.390250	44.283431
3500.861587	796657.460870	44.288436
3501.170217	796639.290287	44.293441
3500.709888	796631.009359	44.298445
3501.071216	796628.950152	44.303450
3500.993143	796628.913531	44.308455
3501.315459	796639.316521	44.313460
3500.852448	796618.042574	44.318465
3500.977089	796604.199238	44.323469
3501.007899	796597.941940	44.328474
3501.330654	796582.992941	44.333479
3500.953825	796595.654596	44.338484
3501.002064	796566.778006	44.343489
3501.072436	796567.939379	44.348493
3500.901506	796565.670268	44.353498
3501.021833	796549.092004	44.358503
3500.753732	796559.343177	44.363508
3501.258530	796549.201593	44.368513
3500.836674	796538.276734	44.373517
3500.741970	796528.668466	44.378522
3500.956982	796528.146395	44.383527
3500.742096	796535.116455	44.388532
3501.074139	796524.317963	44.393537
3500.818540	796535.788426	44.398541
3500.832843	796510.971290	44.403546
3500.921348	796514.328014	44.408551
3500.348733	796505.087509	44.413556
3500.552247	796500.463966	44.418561
3500.741442	796500.874049	44.423565
3500.884616	796502.414841	44.428570
3500.900887	796510.374609	44.433575
3500.676210	796510.702844	44.438580
3500.445549	796506.391418	44.443585
3500.919090	796505.438145	44.448589
3500.426133	796510.839702	44.453594
3500.625342	796516.572689	44.458599
3500.751024	796520.754019	44.463604
3500.581350	796495.867888	44.468609
3500.888919	796492.058498	44.473613
3500.729843	796488.810536	44.478618
3500.788445	796470.678568	44.483623
3500.699446	796486.372907	44.488628
3500.902893	796488.001977	44.493633
3500.746071	796486.365664	44.498637
3500.564779	796482.095352	44.503642
3500.760318	796489.050152	44.508647
3500.467103	796483.966913	44.513652
3500.956473	796484.574316	44.518657
3501.063346	796493.154974	44.523661
3500.883312	796465.388284	44.528666
3500.998972	796450.275958	44.533671
3500.817136	796457.582876	44.538676
3501.260870	796443.689318	44.543681
3501.017374	796451.934010	44.548685
3501.085204	796433.702798	44.553690
3501.035716	796415.831817	44.558695
3500.792169	796425.053533	44.563700
3500.703520	796420.817548	44.568705
3501.115572	796420.460063	44.573709
3500.829942	796412.444639	44.578714
3501.298230	796389.656584	44.583719
3500.615169	796397.628113	44.588724
3501.170208	796379.662532	44.593729
3500.866225	796386.500131	44.598733
3500.562564	796390.944058	44.603738
3500.923819	796389.031336	44.608743
3500.762567	796391.010537	44.613748
3500.989754	796362.642408	44.618753
3500.581834	796361.436111	44.623757
3500.680723	796359.759792	44.628762
3500.892822	796358.945067	44.633767
3500.861129	796359.682787	44.638772
3500.942510	796358.058054	44.643777
3500.571779	796369.888753	44.648781
3500.549446	796358.901137	44.653786
3500.928741	796357.620629	44.658791
3500.764238	796350.367785	44.663796
3500.548756	796328.809945	44.668801
3500.326855	796334.950870	44.673805
3500.695858	796332.401875	44.678810
3500.835893	796335.848335	44.683815
3500.797375	796337.124471	44.688820
3500.923028	796334.369269	44.693825
3501.004975	796338.606404	44.698829
3500.769596	796344.602877	44.703834
3500.602277	796336.861962	44.708839
3500.647051	796347.259958	44.713844
3500.746373	796338.598070	44.718849
3500.738961	796323.993186	44.723853
3500.616180	796307.598858	44.728858
3500.858274	796305.362791	44.733863
3500.718679	796308.608729	44.738868
3500.837213	796299.113337	44.743873
3500.990897	796318.971238	44.748877
3500.895018	796329.195851	44.753882
3501.098479	796317.684371	44.758887
3500.730970	796307.336824	44.763892
3500.952199	796290.009377	44.768897
3500.977102	796285.950954	44.773901
3500.865671	796274.830573	44.778906
3500.945085	796272.766475	44.783911
3500.781270	796287.740236	44.788916
3500.841012	796286.558519	44.793921
3500.809538	796278.991699	44.798925
3501.068108	796272.649635	44.803930
3501.223424	796257.774913	44.808935
3501.086208	796261.509005	44.813940
3501.067100	796251.937361	44.818945
3500.720707	796236.945618	44.823949
3500.800252	796231.999311	44.828954
3500.860652	796221.633586	44.833959
3500.732774	796229.420830	44.838964
3500.768544	796221.110674	44.843969
3501.127537	796220.224119	44.848973
3500.612282	796227.388013	44.853978
3501.067566	796233.227773	44.858983
3500.601401	796211.269075	44.863988
3500.740020	796200.939940	44.868993
3500.750492	796207.386615	44.873997
3500.410397	796198.158172	44.879002
3500.905486	796194.319295	44.884007
3500.599824	796194.025144	44.889012
3500.475476	796190.380798	44.894017
3500.216457	796200.826518	44.899021
3500.462075	796205.526661	44.904026
3501.118591	796197.901050	44.909031
3501.130319	796214.948118	44.914036
3501.092942	796207.821793	44.919041
3500.981166	796198.264556	44.924045
3500.903809	796177.563934	44.929050
3500.801030	796180.608777	44.934055
3500.602457	796173.312209	44.939060
3501.076236	796165.763978	44.944065
3500.889604	796168.675381	44.949069
3500.756985	796170.210514	44.954074
3501.022296	796159.128744	44.959079
3500.786722	796148.906871	44.964084
3500.830859	796136.100997	44.969089
3500.951549	796145.021914	44.974093
3500.677285	796144.869406	44.979098
3500.783008	796140.016639	44.984103
3500.860225	796150.214474	44.989108
3500.780947	796155.209698	44.994113
3500.800796	796127.166060	44.999117
3500.715820	796112.963637	45.004122
3501.175151	796113.331519	45.009127
3500.738704	796126.345363	45.014132
3500.849127	796108.595094	45.019137
3501.002556	796115.849986	45.024141
3500.981959	796117.123363	45.029146
3500.802943	796098.685542	45.034151
3500.660450	796088.497875	45.039156
3500.453061	796081.349137	45.044161
3500.654183	796080.633797	45.049165
3500.624708	796095.293892	45.054170
3501.077193	796086.625313	45.059175
3500.661292	796090.891582	45.064180
3500.880566	796086.216432	45.069185
3500.450317	796089.459062	45.074189
3500.462572	796092.339409	45.079194
3500.692680	796086.099316	45.084199
3500.406734	796095.328125	45.089204
3500.862032	796095.892044	45.094209
3501.039841	796095.473459	45.099213
3500.800839	796070.254574	45.104218
3501.029365	796065.431407	45.109223
3500.430413	796069.530899	45.114228
3500.570244	796068.141216	45.119233
3500.581310	796078.642614	45.124237
3500.546199	796077.475687	45.129242
3500.821064	796070.886621	45.134247
3500.641549	796073.552696	45.139252
3500.860850	796067.949346	45.144257
3500.500055	796070.399502	45.149261
3500.529973	796070.297144	45.154266
3500.519524	796064.387744	45.159271
3500.719653	796070.902610	45.164276
3500.989668	796070.518462	45.169281
3500.743533	796059.565325	45.174285
3500.555369	796047.186403	45.179290
3500.809690	796040.600518	45.184295
3500.780636	796043.927011	45.189300
3500.781857	796041.777360	45.194305
3501.004233	796047.507142	45.199309
3500.923990	796050.060004	45.204314
3501.267877	796041.799157	45.209319
3500.765211	796036.894862	45.214324
3500.699980	796013.798078	45.219329
3500.853609	796018.903554	45.224333
3500.983251	796014.291215	45.229338
3500.900375	796012.496666	45.234343
3500.637871	796018.546530	45.239348
3500.602055	796009.172548	45.244353
3500.782303	796021.357417	45.249357
3500.958235	796015.076873	45.254362
3501.159498	795991.352126	45.259367
3500.861830	795997.798325	45.264372
3501.051699	795983.748064	45.269377
3501.333178	795974.422136	45.274381
3501.070683	795969.089426	45.279386
3501.074292	795956.045271	45.284391
3501.185578	795958.421671	45.289396
3501.082092	795954.138848	45.294401
3500.488712	795954.085071	45.299405
3500.566987	795951.679082	45.304410
3500.865730	795942.790084	45.309415
3500.582563	795931.598256	45.314420
3500.782823	795918.620990	45.319425
3500.862577	795916.752138	45.324429
3500.876588	795916.994234	45.329434
3500.944635	795915.811152	45.334439
3500.868602	795923.932626	45.339444
3501.025966	795922.442466	45.344449
3500.757888	795924.780476	45.349453
3500.622820	795908.484767	45.354458
3500.956406	795884.983211	45.359463
3500.942058	795899.983352	45.364468
3500.898217	795894.420988	45.369473
3501.035979	795886.680698	45.374477
3500.992183	795890.644663	45.379482
3501.058842	795882.622364	45.384487
3500.885336	795873.269710	45.389492
3500.827170	795858.769421	45.394497
3500.823009	795861.261610	45.399501
3500.214487	795866.144375	45.404506
3500.792400	795848.759997	45.409511
3500.444320	795854.627977	45.414516
3500.618950	795861.440160	45.419521
3500.659956	795864.511526	45.424525
3500.572832	795870.338700	45.429530
3500.806184	795868.103851	45.434535
3500.451978	795867.866124	45.439540
3500.693846	795867.828338	45.444545
3501.191779	795871.414512	45.449549
3500.761650	795858.682230	45.454554
3500.708398	795849.213036	45.459559
3500.441202	795841.047461	45.464564
3500.468501	795831.321382	45.469569
3500.554541	795838.733679	45.474573
3500.829892	795848.656748	45.479578
3500.769838	795848.421891	45.484583
3500.696026	795852.976812	45.489588
3500.524943	795837.028526	45.494593
3500.630673	795846.147607	45.499597
3500.662577	795856.059867	45.504602
3500.671408	795858.794293	45.509607
3500.876608	795858.664532	45.514612
3501.008856	795851.462447	45.519617
3500.795206	795842.848824	45.524621
3500.910569	795837.945473	45.529626
3501.078070	795824.924288	45.534631
3500.702327	795831.920243	45.539636
3500.375660	795831.678211	45.544641
3500.676624	795827.087812	45.549645
3500.462741	795832.055471	45.554650
3500.750503	795832.889873	45.559655
3500.539748	795847.334597	45.564660
3500.690907	795850.388750	45.569665
3500.870973	795841.957847	45.574669
3500.885970	795845.472968	45.579674
3500.803916	795820.179724	45.584679
3500.671597	795810.625127	45.589684
3500.631543	795805.355217	45.594689
3501.164216	795804.148337	45.599693
3500.698232	795803.683813	45.604698
3500.841944	795812.015344	45.609703
3500.923844	795823.336594	45.614708
3500.513584	795809.330916	45.619713
3500.307657	795808.874594	45.624717
3500.443642	795818.672934	45.629722
3500.686835	795814.238118	45.634727
3500.411598	795823.025955	45.639732
3500.821258	795826.577099	45.644737
3500.583685	795802.871411	45.649741
3500.392090	795792.984078	45.654746
3500.769095	795785.792514	45.659751
3500.643915	795792.553928	45.664756
3500.376622	795792.449173	45.669761
3500.734526	795798.109136	45.674765
3500.065881	795801.731149	45.679770
3500.390278	795797.479042	45.684775
3500.208335	795816.365019	45.689780
3500.407644	795821.023828	45.694785
3500.644017	795823.234163	45.699789
3500.144641	795831.861612	45.704794
3500.542530	795832.727652	45.709799
3500.550339	795844.500128	45.714804
3500.605959	795841.071719	45.719809
3500.599069	795847.277198	45.724813
3500.551838	795846.747217	45.729818
3500.737872	795840.367219	45.734823
3500.543683	795812.062560	45.739828
3500.615038	795751.814638	45.744833
3500.711809	795653.846383	45.749837
3500.508120	795505.553364	45.754842
3500.000985	795307.665464	45.759847
3499.889021	795054.596710	45.764852
3499.656253	794752.919931	45.769857
3499.392091	794412.631559	45.774861
3498.882741	794026.868738	45.779866
3498.912115	793578.542880	45.784871
3498.327270	793085.904804	45.789876
3497.764540	792549.040550	45.794881
3497.475428	791970.197445	45.799885
3497.010502	791326.897757	45.804890
3496.296998	790647.540424	45.809895
3495.988092	789925.606670	45.814900
3495.477335	789134.476205	45.819905
3494.772292	788315.843032	45.824909
3493.845074	787435.460329	45.829914
3492.937440	786503.686451	45.834919
3491.955440	785543.218231	45.839924
3490.991083	784530.000897	45.844929
3490.314685	783477.575218	45.849933
3489.083437	782381.942735	45.854938
3488.420209	781229.785380	45.859943
3487.257806	780036.716017	45.864948
3485.981662	778793.200122	45.869953
3485.012481	777502.181926	45.874957
3483.432141	776181.858844	45.879962
3482.426351	774800.663918	45.884967
3480.968806	773392.151987	45.889972
3479.816064	771929.958359	45.894977
3478.522445	770428.782175	45.899981
3476.760479	768868.833688	45.904986
3475.498473	767288.779917	45.909991
3474.033262	765669.432533	45.914996
3472.769868	764002.210329	45.920001
3471.382949	762289.291562	45.925005
3469.540544	760559.228718	45.930010
3468.262071	758759.733235	45.935015
3466.305574	756928.486931	45.940020
3465.062215	755058.860383	45.945025
3463.234594	753151.765696	45.950029
3460.900989	751200.130818	45.955034
3459.461560	749225.542158	45.960039
3457.090727	747202.585644	45.965044
3455.565910	745141.969591	45.970049
3453.845433	743059.384261	45.975053
3451.547035	740920.648952	45.980058
3449.649136	738770.980969	45.985063
3447.357608	736576.746165	45.990068
3445.381653	734354.407331	45.995073
3443.275078	732084.932393	46.000077
3441.098655	729804.077412	46.005082
3439.222130	727472.262311	46.010087
3436.976982	725108.843699	46.015092
3434.491478	722719.452988	46.020097
3432.872404	720293.280447	46.025101
3430.286551	717841.795144	46.030106
3428.283529	715351.888322	46.035111
3425.616541	712825.255088	46.040116
3423.566068	710281.046324	46.045121
3421.161854	707698.282764	46.050125
3418.373967	705091.432970	46.055130
3416.151468	702448.650243	46.060135
3413.579726	699788.068850	46.065140
3411.016107	697090.405441	46.070145
3408.800655	694365.731887	46.075149
3405.794918	691623.918777	46.080154
3403.483174	688840.481110	46.085159
3400.629961	686040.273275	46.090164
3397.817441	683213.867646	46.095169
3395.118566	680363.863339	46.100173
3392.073813	677489.471444	46.105178
3389.986929	674592.407248	46.110183
3386.888564	671667.449150	46.115188
3384.257044	668707.785638	46.120193
3381.475783	665742.913489	46.125197
3378.700748	662739.544033	46.130202
3375.911631	659714.711163	46.135207
3372.992571	656671.305444	46.140212
3370.096502	653610.039087	46.145217
3366.912863	650517.954775	46.150221
3363.788142	647412.160425	46.155226
3361.518506	644281.066130	46.160231
3358.013277	641142.776788	46.165236
3354.895179	637967.522402	46.170241
3351.591419	634769.928989	46.175245
3348.676527	631578.134298	46.180250
3345.880406	628355.061714	46.185255
3342.501640	625122.068789	46.190260
3339.668053	621856.403953	46.195265
3336.666936	618574.943274	46.200269
3333.393046	615284.744601	46.205274
3330.358909	611964.931737	46.210279
3326.880334	608633.096767	46.215284
3323.467787	605287.307629	46.220289
3320.445621	601931.063792	46.225293
3316.817251	598556.362082	46.230298
3313.901485	595156.229116	46.235303
3310.499978	591755.183504	46.240308
3307.286611	588332.535958	46.245313
3303.822087	584900.826645	46.250317
3299.925406	581457.178599	46.255322
3296.752465	577993.637367	46.260327
3293.485226	574539.071440	46.265332
3290.488353	571056.406881	46.270337
3286.977562	567559.507261	46.275341
3283.837376	564056.619150	46.280346
3280.050532	560520.482107	46.285351
3276.765963	556989.085506	46.290356
3273.046893	553457.566212	46.295361
3270.121325	549887.685767	46.300365
3266.221821	546322.144114	46.305370
3263.040482	542745.802653	46.310375
3259.589345	539171.650421	46.315380
3255.721679	535575.514506	46.320385
3252.200423	531966.684495	46.325389
3248.265161	528368.397111	46.330394
3244.943837	524749.431743	46.335399
3241.152549	521122.046968	46.340404
3237.447454	517492.714032	46.345409
3234.198831	513854.731530	46.350413
3230.312543	510212.210048	46.355418
3226.939945	506564.373561	46.360423
3223.312941	502896.820201	46.365428
3220.212377	499234.154741	46.370433
3216.495664	495560.671541	46.375437
3212.581013	491883.732531	46.380442
3209.148613	488191.827921	46.385447
3205.314615	484497.222297	46.390452
3201.562272	480789.644598	46.395457
3197.870305	477092.452035	46.400461
3194.268130	473381.698840	46.405466
3190.459826	469660.367967	46.410471
3186.719791	465958.059708	46.415476
3182.743099	462234.732922	46.420481
3179.616557	458504.536166	46.425485
3175.913083	454777.013544	46.430490
3172.019023	451044.526926	46.435495
3168.079608	447312.329347	46.440500
3164.021402	443575.533854	46.445505
3160.464569	439823.620253	46.450509
3156.305397	436099.218544	46.455514
3152.997280	432357.136386	46.460519
3149.183749	428619.685256	46.465524
3145.326357	424872.565440	46.470529
3141.626084	421124.574986	46.475533
3137.360306	417394.246522	46.480538
3133.867651	413648.428045	46.485543
3130.412133	409902.710933	46.490548
3126.264876	406152.504359	46.495553
3122.443056	402410.954654	46.500557
3118.511850	398661.755167	46.505562
3114.776124	394923.851319	46.510567
3110.765563	391174.389057	46.515572
3106.601735	387434.453681	46.520577
3102.832725	383690.748515	46.525581
3099.005170	379961.538246	46.530586
3095.377237	376229.175748	46.535591
3091.450559	372493.903085	46.540596
3087.219064	368764.421432	46.545601
3083.608803	365031.556042	46.550605
3079.429570	361304.525704	46.555610
3075.549385	357578.584397	46.560615
3071.769761	353879.320876	46.565620
3067.660225	350155.907846	46.570625
3063.832416	346441.151606	46.575629
3059.558058	342746.419952	46.580634
3055.785077	339042.010285	46.585639
3051.969673	335345.157808	46.590644
3047.957337	331650.255243	46.595649
3044.003849	327966.076525	46.600653
3039.572912	324289.770089	46.605658
3035.855540	320594.120753	46.610663
3032.119375	316924.131451	46.615668
3027.713230	313262.823795	46.620673
3023.876110	309594.902840	46.625677
3019.251637	305950.900694	46.630682
3015.435951	302302.589458	46.635687
3011.539430	298673.331693	46.640692
3007.525131	295042.047576	46.645697
3003.675756	291432.352284	46.650701
2999.119192	287824.108611	46.655706
2995.150227	284218.958837	46.660711
2991.245939	280636.345920	46.665716
2986.915493	277056.909383	46.670721
2982.763511	273483.290772	46.675725
2978.399422	269932.597723	46.680730
2974.504898	266379.579226	46.685735
2970.543021	262836.985890	46.690740
2966.240889	259310.551133	46.695745
2962.057321	255797.312308	46.700749
2957.602736	252288.988968	46.705754
2953.672243	248796.342239	46.710759
2949.513528	245316.215881	46.715764
2945.466640	241842.684577	46.720769
2941.158406	238383.508738	46.725773
2936.854674	234943.521990	46.730778
2932.861244	231510.309128	46.735783
2928.143274	228095.604961	46.740788
2923.772861	224693.292025	46.745793
2919.769010	221301.008399	46.750797
2915.522367	217942.646828	46.755802
2910.918365	214577.433144	46.760807
2906.869395	211242.341689	46.765812
2902.595463	207917.739333	46.770817
2898.646660	204605.815273	46.775821
2894.348462	201322.523969	46.780826
2890.037819	198031.351413	46.785831
2885.810880	194764.633857	46.790836
2881.890384	191510.450899	46.795841
2877.566514	188261.459822	46.800845
2872.807500	185047.313755	46.805850
2868.807902	181831.214697	46.810855
2864.383090	178644.038389	46.815860
2859.895665	175460.538959	46.820865
2856.052474	172310.312925	46.825869
2851.943699	169082.185328	46.830874
2847.835891	165938.594053	46.835879
2843.275567	162832.510929	46.840884
2839.065183	159731.038298	46.845889
2834.850361	156662.238191	46.850893
2830.800143	153601.358582	46.855898
2825.996620	150548.650635	46.860903
2821.894647	147517.902918	46.865908
2817.865594	144506.951910	46.870913
2813.410569	141505.801748	46.875917
2808.868312	138526.274799	46.880922
2804.823422	135566.144822	46.885927
2800.658242	132621.491176	46.890932
2796.662396	129698.708333	46.895937
2792.048060	126784.514900	46.900941
2787.916719	123900.962356	46.905946
2783.862544	121012.147985	46.910951
2779.510523	118156.351341	46.915956
2775.440767	115314.050434	46.920961
2771.025594	112497.272544	46.925965
2766.715671	109681.714334	46.930970
2762.514803	106884.110477	46.935975
2758.228548	104107.060273	46.940980
2754.078530	101350.999655	46.945985
2750.018112	98606.530778	46.950989
2745.533356	95886.330398	46.955994
2741.300758	93179.706221	46.960999
2737.009220	90494.687873	46.966004
2733.128281	87817.720837	46.971009
2728.833676	85156.787741	46.976013
2724.739691	82530.669349	46.981018
2720.336739	79899.988853	46.986023
2716.154860	77303.215221	46.991028
2711.371767	74709.777691	46.996033
2707.250563	72145.297354	47.001037
2702.802427	69604.420672	47.006042
2698.521118	67071.096618	47.011047
2694.724247	64568.400183	47.016052
2690.194073	62082.871628	47.021057
2685.849352	59602.410323	47.026061
2681.556298	57158.029878	47.031066
2677.242542	54729.241210	47.036071
2672.670683	52319.563191	47.041076
2668.249905	49934.093015	47.046081
2663.963892	47559.357337	47.051085
2659.414878	45213.556664	47.056090
2655.167245	42899.120900	47.061095
2650.590095	40600.607346	47.066100
2646.023319	38309.465284	47.071105
2642.266705	36047.517328	47.076109
2637.815473	33814.466451	47.081114
2633.663124	31589.862885	47.086119
2629.336266	29393.749904	47.091124
2624.692809	27231.288843	47.096129
2620.227875	25060.658629	47.101133
2615.907510	22935.834500	47.106138
2611.139795	20819.357461	47.111143
2606.638046	18739.720221	47.116148
2602.097139	16691.742428	47.121153
2597.168210	14671.740913	47.126157
2592.375297	12678.145354	47.131162
2587.096455	10703.290851	47.136167
2582.008463	8775.559143	47.141172
2576.858658	6896.176611	47.146177
2570.951944	5078.784098	47.151181
2562.977282	3330.746855	47.156186
2552.990871	1716.560927	47.161191
2538.075709	326.467956	47.166196
2480.177202	198.300587	47.171201
2434.573540	220.782595	47.176205
2413.436695	234.466758	47.181210
2412.398552	226.010758	47.186215
2421.517094	221.641881	47.191220
2433.135462	224.285440	47.196225
2443.937490	221.073807	47.201229
2449.798005	232.531000	47.206234
2452.123657	220.460827	47.211239
2451.490205	221.300293	47.216244
2448.317377	223.365945	47.221249
2444.615807	219.059984	47.226253
2441.003968	224.753687	47.231258
2437.784908	221.447968	47.236263
2434.543779	226.767292	47.241268
2431.717434	225.931248	47.246273
2429.247565	216.541243	47.251277
2426.452115	222.660915	47.256282
2423.444761	222.780209	47.261287
2420.550512	213.880557	47.266292
2417.071939	215.234714	47.271297
2414.455717	206.231461	47.276301
2411.111079	226.481531	47.281306
2408.177007	210.719320	47.286311
2405.293770	211.464635	47.291316
2401.774186	216.308648	47.296321
2398.392694	211.664720	47.301325
2394.896348	223.225190	47.306330
2391.454107	220.466949	47.311335
2388.314550	215.918058	47.316340
2385.184223	218.182730	47.321345
2382.043475	213.592897	47.326349
2378.772998	214.152016	47.331354
2375.377025	213.139335	47.336359
2372.450873	207.683834	47.341364
2368.725833	212.968138	47.346369
2365.665626	201.446305	47.351373
2362.235758	209.598366	47.356378
2358.600547	210.078503	47.361383
2355.264256	211.011771	47.366388
2351.668811	207.723834	47.371393
2348.463177	211.471501	47.376397
2344.634932	206.087531	47.381402
2341.560230	206.008567	47.386407
2338.548511	196.377490	47.391412
2334.748031	213.076228	47.396417
2331.952446	199.326768	47.401421
2328.594481	211.441421	47.406426
2324.955165	195.220092	47.411431
2321.539595	203.841341	47.416436
2317.708937	208.579012	47.421441
2314.456482	207.151576	47.426445
2310.914348	210.569067	47.431450
2307.410089	205.188211	47.436455
2303.946706	197.152798	47.441460
2300.450877	199.439869	47.446465
2297.271995	200.671242	47.451469
2293.681891	201.650564	47.456474
2290.052313	196.640514	47.461479
2287.118145	193.904069	47.466484
2283.649242	200.597377	47.471489
2280.236861	196.768279	47.476493
2276.475334	202.260804	47.481498
2273.314121	200.104070	47.486503
2270.085512	200.485820	47.491508
2266.436863	202.736697	47.496513
2263.184874	192.377581	47.501517
2259.522504	201.910686	47.506522
2255.892442	195.113134	47.511527
2252.720128	188.427475	47.516532
2248.900271	192.657253	47.521537
2245.599342	189.595373	47.526541
2242.236659	197.774913	47.531546
2238.765772	189.487592	47.536551
2235.034903	189.340469	47.541556
2231.393739	196.462552	47.546561
2227.822880	190.209429	47.551565
2224.851351	197.948110	47.556570
2221.150556	189.326593	47.561575
2217.866628	193.456712	47.566580
2213.785603	201.131694	47.571585
2211.113289	180.402481	47.576589
2207.584990	187.304421	47.581594
2203.683581	186.196862	47.586599
2200.466742	192.455268	47.591604
2197.028082	186.127688	47.596609
2193.438568	186.227392	47.601613
2190.192523	191.778498	47.606618
2186.660320	193.296145	47.611623
2183.064768	187.600581	47.616628
2179.766320	192.008239	47.621633
2176.058743	192.863603	47.626637
2172.300840	192.141741	47.631642
2168.965797	193.302667	47.636647
2165.853536	191.812213	47.641652
2161.633122	192.263748	47.646657
2158.768570	181.736488	47.651661
2155.412832	187.842623	47.656666
2151.973564	192.414695	47.661671
2148.657729	186.580463	47.666676
2144.668880	183.825575	47.671681
2141.267063	176.720270	47.676685
2137.965092	182.083977	47.681690
2134.287196	183.564321	47.686695
2130.768434	183.887102	47.691700
2126.808102	183.737952	47.696705
2123.976819	179.583865	47.701709
2120.150254	181.422845	47.706714
2117.292178	176.830010	47.711719
2113.843336	179.660297	47.716724
2110.034608	178.705957	47.721729
2106.284374	171.898801	47.726733
2103.019038	172.273690	47.731738
2099.287199	168.811033	47.736743
2095.876069	177.437956	47.741748
2092.315961	179.773112	47.746753
2089.134217	177.271625	47.751757
2085.576294	179.796273	47.756762
2081.946099	186.084579	47.761767
2078.498904	179.821659	47.766772
2075.181847	193.015157	47.771777
2071.828651	176.277779	47.776781
2067.893528	182.946007	47.781786
2064.547530	180.653732	47.786791
2061.099464	183.629451	47.791796
2057.300997	184.407324	47.796801
2054.364022	178.906168	47.801805
2050.108940	191.968023	47.806810
2047.115506	179.945477	47.811815
2043.907928	180.178465	47.816820
2040.148553	181.836110	47.821825
2036.875066	185.796957	47.826829
2033.013485	190.568024	47.831834
2029.350219	185.031817	47.836839
2026.049602	185.070552	47.841844
2022.596882	185.161564	47.846849
2019.141695	180.763434	47.851853
2015.787803	175.852730	47.856858
2012.464433	182.377793	47.861863
2008.951403	182.614292	47.866868
2004.990094	180.696738	47.871873
2001.702983	179.179909	47.876877
1998.104129	181.973589	47.881882
1994.409893	168.940721	47.886887
1991.398088	168.795065	47.891892
1987.761496	180.678110	47.896897
1984.176814	174.231089	47.901901
1980.870089	176.618382	47.906906
1976.897981	180.011496	47.911911
1973.866266	182.048864	47.916916
1970.103168	181.922694	47.921921
1967.108724	171.574028	47.926925
1963.347400	181.138502	47.931930
1960.178972	176.651229	47.936935
1956.409302	171.957473	47.941940
1953.107423	176.780191	47.946945
1949.630073	174.771111	47.951949
1945.730960	176.314607	47.956954
1942.185929	179.068244	47.961959
1938.810257	167.285902	47.966964
1935.024120	180.255417	47.971969
1931.626052	166.704819	47.976973
1927.864179	176.456053	47.981978
1924.631097	170.637433	47.986983
1921.717885	168.492628	47.991988
1918.021830	178.651196	47.996993
1914.455411	171.388233	48.001997
1910.963638	166.568751	48.007002
1907.232462	174.568735	48.012007
1903.847664	172.190835	48.017012
1900.334643	171.664877	48.022017
1897.067368	170.097521	48.027021
1893.404099	165.788953	48.032026
1889.710107	165.009735	48.037031
1886.432263	165.851735	48.042036
1882.741013	169.792570	48.047041
1879.753815	170.807397	48.052045
1876.018886	160.558828	48.057050
1872.508319	165.142130	48.062055
1869.127311	169.287530	48.067060
1864.887328	163.879610	48.072065
1861.383541	166.531900	48.077069
1858.200915	172.266156	48.082074
1854.656452	165.980581	48.087079
1851.269772	159.085004	48.092084
1847.968672	168.653415	48.097089
1844.516910	161.787007	48.102093
1841.097029	160.559938	48.107098
1837.647635	167.803974	48.112103
1834.272704	158.742486	48.117108
1830.212022	165.930320	48.122113
1826.896836	164.057263	48.127117
1823.183971	154.415893	48.132122
1820.227172	158.232319	48.137127
1816.342138	155.863130	48.142132
1812.809883	168.131691	48.147137
1809.301947	160.024364	48.152141
1805.676037	164.135338	48.157146
1802.295616	161.880180	48.162151
1798.966404	154.732015	48.167156
1795.454693	167.190359	48.172161
1792.111320	153.511047	48.177165
1788.355563	165.937979	48.182170
1784.688002	160.557578	48.187175
1781.289708	158.355846	48.192180
1777.793375	157.096468	48.197185
1774.614945	156.087908	48.202189
1770.558644	156.374704	48.207194
1767.214258	160.229653	48.212199
1764.253789	164.296613	48.217204
1760.031626	163.388121	48.222209
1756.917057	158.130004	48.227213
1753.270649	161.750641	48.232218
1749.834718	163.547596	48.237223
1746.569228	160.467688	48.242228
1742.863126	160.041606	48.247233
1739.543571	160.561138	48.252237
1735.930005	159.696620	48.257242
1732.185499	162.006960	48.262247
1728.831744	152.059488	48.267252
1725.214039	160.706169	48.272257
1722.247882	154.390259	48.277261
1718.318295	162.506767	48.282266
1715.081376	166.015873	48.287271
1711.901466	159.473980	48.292276
1708.125413	158.223601	48.297281
1703.942066	153.775033	48.302285
1700.596797	150.258361	48.307290
1697.115923	151.919993	48.312295
1693.929617	149.194719	48.317300
1690.258732	157.216961	48.322305
1687.260372	149.222934	48.327309
1683.572782	158.000789	48.332314
1679.733483	158.772530	48.337319
1676.609334	154.284758	48.342324
1672.711751	159.377955	48.347329
1669.401371	157.175159	48.352333
1665.659584	151.227441	48.357338
1662.389085	157.320355	48.362343
1659.192337	155.764187	48.367348
1655.170775	157.652828	48.372353
1651.675790	153.564800	48.377357
1648.256929	148.771976	48.382362
1644.700933	159.642700	48.387367
1641.785286	151.059922	48.392372
1638.271343	145.965600	48.397377
1634.724320	149.611847	48.402381
1630.851820	145.462687	48.407386
1626.861752	158.128814	48.412391
1623.877960	153.960789	48.417396
1620.142244	153.934869	48.422401
1616.983426	141.397384	48.427405
1613.389677	146.212083	48.432410
1609.822106	147.241887	48.437415
1606.596381	143.820438	48.442420
1602.684634	144.375749	48.447425
1598.809720	140.619299	48.452429
1595.570288	148.083640	48.457434
1592.079434	150.699186	48.462439
1589.093728	143.997232	48.467444
1585.315211	151.666177	48.472449
1582.525590	148.736480	48.477453
1578.785392	141.418606	48.482458
1574.387422	147.102695	48.487463
1571.513677	142.313171	48.492468
1567.903702	145.678218	48.497473
1564.449189	149.623229	48.502477
1560.431309	145.626571	48.507482
1557.125901	150.440453	48.512487
1553.817791	147.354629	48.517492
1550.380900	146.361283	48.522497
1546.918383	135.760183	48.527501
1543.222821	146.393335	48.532506
1539.663301	145.390712	48.537511
1536.363893	149.238687	48.542516
1532.755841	152.135196	48.547521
1529.668247	148.543452	48.552525
1526.209816	141.270086	48.557530
1522.558015	143.376156	48.562535
1518.826693	138.616471	48.567540
1514.916004	136.453907	48.572545
1511.449303	142.318132	48.577549
1508.311404	145.713715	48.582554
1504.543114	147.091356	48.587559
1501.358236	143.052928	48.592564
1497.925813	144.365346	48.597569
1494.383502	145.511461	48.602573
1490.817129	152.103161	48.607578
1486.891187	150.370113	48.612583
1483.988254	140.225631	48.617588
1480.362081	140.109848	48.622593
1476.837878	148.001618	48.627597
1473.300198	144.062716	48.632602
1469.565232	148.358547	48.637607
1466.153343	139.046733	48.642612
1462.700099	145.124008	48.647617
1459.532276	130.733993	48.652621
1455.726603	139.052648	48.657626
1452.314114	141.769871	48.662631
1448.809725	136.054016	48.667636
1445.057766	143.231612	48.672641
1441.560415	140.109010	48.677645
1438.402894	145.526217	48.682650
1434.708511	141.656153	48.687655
1431.581853	144.334970	48.692660
1427.600708	145.470703	48.697665
1424.248032	139.259697	48.702669
1420.905886	137.163205	48.707674
1417.082360	130.741161	48.712679
1414.033458	136.609619	48.717684
1410.210238	140.634537	48.722689
1406.927967	137.649129	48.727693
1403.175602	137.644879	48.732698
1399.430171	141.192540	48.737703
1396.317598	135.779217	48.742708
1392.765027	142.327652	48.747713
1389.205473	138.335259	48.752717
1385.436827	138.263960	48.757722
1381.618316	148.182391	48.762727
1378.660914	143.633822	48.767732
1375.295392	150.871178	48.772737
1371.917727	136.707039	48.777741
1368.497348	142.405863	48.782746
1364.476613	145.211998	48.787751
1361.361139	138.875299	48.792756
1357.395296	140.619285	48.797761
1354.129188	143.272495	48.802765
1350.820845	134.589947	48.807770
1346.905747	147.573450	48.812775
1344.026445	143.341707	48.817780
1340.348419	144.686296	48.822785
1336.966307	139.694847	48.827789
1333.344505	131.656178	48.832794
1329.480512	150.655639	48.837799
1326.396628	134.031524	48.842804
1322.660972	142.405701	48.847809
1319.144525	140.573818	48.852813
1315.802813	132.798204	48.857818
1312.175067	145.597524	48.862823
1308.555421	136.710617	48.867828
1304.956851	135.470578	48.872833
1301.569454	144.369228	48.877837
1298.356915	138.398933	48.882842
1294.746967	136.084974	48.887847
1291.292596	124.210855	48.892852
1287.407437	132.693867	48.897857
1284.018758	124.865508	48.902861
1280.414983	134.892720	48.907866
1277.053672	126.541210	48.912871
1273.730942	123.625463	48.917876
1270.340350	129.572755	48.922881
1266.949777	123.503795	48.927885
1263.350579	139.655485	48.932890
1259.167371	139.851617	48.937895
1255.502852	126.706910	48.942900
1252.612168	127.928273	48.947905
1249.441868	132.281315	48.952909
1245.569247	139.718314	48.957914
1242.132535	130.451616	48.962919
1239.165685	125.910906	48.967924
1234.824494	132.168380	48.972929
1231.460370	130.072234	48.977933
1227.870835	128.998494	48.982938
1224.624922	141.994329	48.987943
1221.126650	128.747679	48.992948
1217.613770	126.269855	48.997953
1214.191298	130.042273	49.002957
1210.387673	130.334030	49.007962
1206.847844	132.473301	49.012967
1203.263770	124.362346	49.017972
1200.342774	138.458953	49.022977
1196.482301	131.220194	49.027981
1193.515266	137.003124	49.032986
1189.900540	133.244081	49.037991
1186.075956	131.890770	49.042996
1182.193942	134.169044	49.048001
1178.801662	131.400264	49.053005
1175.179250	128.423898	49.058010
1171.797105	135.834755	49.063015
1168.912903	132.919995	49.068020
1165.119703	128.284048	49.073025
1161.665714	130.368766	49.078029
1158.167840	134.013798	49.083034
1154.307059	129.840863	49.088039
1150.840836	133.019023	49.093044
1147.431339	133.353508	49.098049
1144.239307	127.013061	49.103053
1140.868624	126.329044	49.108058
1137.391887	136.747707	49.113063
1133.971979	126.845660	49.118068
1129.879173	132.763724	49.123073
1126.025326	129.602143	49.128077
1122.986482	131.723122	49.133082
1119.454592	139.989527	49.138087
1116.068877	127.032198	49.143092
1112.523511	137.028167	49.148097
1108.849543	129.902622	49.153101
1105.392285	124.888231	49.158106
1101.633176	124.761763	49.163111
1098.699224	125.806443	49.168116
1094.762901	126.960600	49.173121
1091.311306	121.885216	49.178125
1088.021105	126.804419	49.183130
1084.390333	138.155232	49.188135
1081.195643	126.155128	49.193140
1077.355686	122.504165	49.198145
1074.071996	126.071397	49.203149
1070.768356	129.518364	49.208154
1066.951600	129.903984	49.213159
1063.538358	126.717740	49.218164
1059.755222	133.042939	49.223169
1056.011288	127.541927	49.228173
1053.011406	126.296838	49.233178
1049.703296	134.189695	49.238183
1046.497973	134.191684	49.243188
1042.095554	133.884380	49.248193
1038.684150	129.581025	49.253197
1035.410557	134.038889	49.258202
1032.038123	136.566475	49.263207
1028.802548	121.709531	49.268212
1024.975645	126.706456	49.273217
1021.118742	126.282112	49.278221
1017.941119	133.895113	49.283226
1014.209386	137.447093	49.288231
1011.158785	130.179696	49.293236
1007.487844	135.750175	49.298241
1003.807160	126.002914	49.303245
1000.738331	129.625115	49.308250
996.775821	124.829085	49.313255
993.369662	121.474078	49.318260
989.602105	125.553705	49.323265
986.190441	126.980107	49.328269
982.850512	122.621291	49.333274
979.327178	125.520540	49.338279
976.163817	133.080698	49.343284
972.440456	129.183727	49.348289
968.463435	129.502729	49.353293
965.181639	131.494112	49.358298
962.072607	140.795367	49.363303
958.321515	137.250764	49.368308
954.768436	137.535030	49.373313
951.441214	133.373555	49.378317
948.429165	128.931774	49.383322
944.609398	132.165360	49.388327
941.035193	121.718072	49.393332
937.119564	128.968912	49.398337
933.366346	118.094068	49.403341
929.925261	121.186105	49.408346
926.607960	126.021012	49.413351
923.204083	127.784746	49.418356
919.838397	124.417101	49.423361
916.718703	112.455958	49.428365
913.260129	125.652833	49.433370
909.120958	129.698927	49.438375
906.415213	126.057105	49.443380
902.381940	125.075119	49.448385
898.652071	126.124260	49.453389
895.099121	123.500973	49.458394
891.499008	126.962781	49.463399
888.056854	124.559434	49.468404
884.345341	128.649308	49.473409
881.545498	122.484841	49.478413
877.992692	116.295908	49.483418
874.072916	117.033102	49.488423
871.057640	120.915879	49.493428
867.402819	127.325456	49.498433
863.438668	121.109188	49.503437
860.317216	115.697460	49.508442
856.856824	121.956368	49.513447
853.458704	125.326447	49.518452
849.871750	132.823252	49.523457
846.324037	120.577972	49.528461
842.495013	123.335307	49.533466
838.986540	125.523582	49.538471
836.026372	121.507163	49.543476
832.235978	121.081974	49.548481
828.692697	119.985327	49.553485
825.355473	113.686728	49.558490
821.880098	121.374877	49.563495
818.469618	114.875776	49.568500
814.625491	115.715047	49.573505
810.856867	120.813656	49.578509
807.404865	114.571003	49.583514
804.273025	121.759263	49.588519
800.805860	118.492981	49.593524
797.329880	122.634588	49.598529
793.595238	116.856989	49.603533
790.476168	121.768466	49.608538
786.718524	126.488870	49.613543
783.091470	112.297645	49.618548
779.730503	119.667328	49.623553
776.121677	113.645404	49.628557
772.774088	105.693775	49.633562
769.311246	122.868274	49.638567
765.791937	107.056132	49.643572
762.405759	116.745682	49.648577
758.790057	112.604153	49.653581
755.364762	118.057149	49.658586
751.473172	117.584565	49.663591
748.355971	112.308259	49.668596
744.814915	122.202408	49.673601
741.385460	113.621354	49.678605
737.469636	116.930171	49.683610
733.774252	117.989796	49.688615
730.167197	116.966450	49.693620
726.934132	117.956841	49.698625
723.675580	114.895208	49.703629
720.438301	118.923527	49.708634
716.590223	118.054994	49.713639
713.262046	113.748231	49.718644
709.995768	114.092082	49.723649
706.096153	127.551073	49.728653
702.477877	122.830989	49.733658
698.563785	131.945164	49.738663
695.757784	119.577475	49.743668
692.122776	120.273313	49.748673
688.775372	118.627178	49.753677
685.425242	114.795274	49.758682
681.369748	122.741999	49.763687
677.967358	113.441711	49.768692
674.150376	117.459589	49.773697
670.976149	117.115144	49.778701
667.793916	115.661455	49.783706
664.154770	120.050127	49.788711
661.063259	120.357134	49.793716
657.184937	122.837518	49.798721
653.169819	128.673994	49.803725
649.961489	121.425116	49.808730
646.428131	126.278129	49.813735
643.591442	117.765638	49.818740
640.032151	123.907224	49.823745
635.949579	126.283560	49.828749
632.279030	115.421233	49.833754
628.685592	115.354433	49.838759
625.343604	121.784700	49.843764
621.821326	122.997595	49.848769
618.435984	121.230876	49.853773
615.127381	125.374807	49.858778
611.551580	121.641550	49.863783
608.219567	113.431280	49.868788
604.685962	121.112796	49.873793
600.590893	115.920091	49.878797
597.720209	121.175546	49.883802
593.689640	123.711438	49.888807
590.491767	116.827952	49.893812
587.081552	126.701659	49.898817
583.437872	118.989472	49.903821
580.341445	116.130296	49.908826
576.346354	125.883632	49.913831
573.715597	121.094364	49.918836
569.548657	121.474920	49.923841
566.181392	121.907406	49.928845
562.849800	121.685724	49.933850
558.526476	125.007815	49.938855
555.678018	118.433456	49.943860
551.663872	118.223766	49.948865
548.313049	118.220241	49.953869
545.005299	120.829610	49.958874
541.291979	123.983401	49.963879
538.090883	122.213167	49.968884
534.404364	120.215236	49.973889
531.057967	127.000572	49.978893
527.685686	122.416046	49.983898
523.756654	124.353923	49.988903
520.418713	118.457367	49.993908
516.634361	119.594288	49.998913
513.407027	118.173028	50.003917
510.047504	116.636430	50.008922
506.379863	126.107546	50.013927
503.085064	120.125144	50.018932
499.351191	108.728629	50.023937
495.781425	116.007711	50.028941
492.320997	103.926120	50.033946
488.425250	120.706569	50.038951
485.528757	105.954981	50.043956
481.879224	110.225119	50.048961
478.542137	114.996825	50.053965
475.481769	113.615868	50.058970
471.682249	114.967158	50.063975
468.153989	120.667335	50.068980
464.290752	120.905455	50.073985
460.679156	115.678223	50.078989
457.058666	105.143513	50.083994
453.724257	119.801718	50.088999
450.404882	114.395840	50.094004
446.759845	117.200444	50.099009
443.148112	119.553735	50.104013
440.136672	116.456669	50.109018
435.957558	114.093004	50.114023
433.014360	120.527307	50.119028
429.426892	115.704441	50.124033
426.071089	117.739236	50.129037
422.579061	113.879043	50.134042
418.998678	115.047331	50.139047
415.423906	113.724823	50.144052
411.571144	120.222507	50.149057
407.982475	114.925268	50.154061
404.977757	114.934023	50.159066
401.060326	112.716051	50.164071
397.707019	112.437720	50.169076
394.549786	110.559428	50.174081
391.005425	112.291570	50.179085
387.606658	117.924033	50.184090
383.780125	120.557771	50.189095
380.294793	116.190336	50.194100
376.918803	112.539781	50.199105
373.356190	117.438599	50.204109
369.908723	115.744985	50.209114
366.207501	119.735358	50.214119
363.103518	118.339126	50.219124
359.237804	120.102636	50.224129
355.473816	115.892759	50.229133
352.278394	111.780487	50.234138
348.078979	111.169632	50.239143
345.088524	110.480136	50.244148
341.880951	112.735354	50.249153
338.330153	109.238751	50.254157
335.317267	119.319212	50.259162
331.372142	117.861759	50.264167
327.895348	113.958091	50.269172
324.103603	115.523363	50.274177
320.786154	115.774127	50.279181
317.026433	109.870964	50.284186
313.577240	115.957447	50.289191
310.133432	110.966597	50.294196
306.637940	115.766337	50.299201
303.391538	115.268812	50.304205
299.977718	122.216643	50.309210
295.963481	116.638100	50.314215
292.569674	117.337441	50.319220
289.559733	115.616452	50.324225
285.696664	114.326503	50.329229
282.591474	110.143177	50.334234
278.528005	119.293550	50.339239
275.076223	109.343115	50.344244
271.547917	119.564446	50.349249
268.130338	119.448095	50.354253
264.945795	116.390864	50.359258
261.176360	122.378834	50.364263
257.736186	117.109021	50.369268
254.061552	116.817805	50.374273
250.312517	112.070952	50.379277
247.648297	115.196554	50.384282
243.467785	114.535330	50.389287
240.280556	116.145145	50.394292
236.771403	108.639847	50.399297
233.165734	110.406965	50.404301
229.963622	108.820507	50.409306
225.926994	118.659568	50.414311
222.640079	114.422473	50.419316
219.254507	112.782501	50.424321
215.421289	115.556562	50.429325
212.121879	113.248186	50.434330
208.497224	116.948210	50.439335
204.980382	120.587052	50.444340
201.692042	110.452857	50.449345
197.996320	113.841309	50.454349
195.091786	104.804946	50.459354
190.979831	117.892391	50.464359
187.356250	112.062875	50.469364
183.979933	109.023066	50.474369
180.506465	119.571197	50.479373
177.367523	112.340127	50.484378
173.660005	121.121561	50.489383
170.403404	113.415372	50.494388
166.696449	113.176714	50.499393
162.823302	118.836114	50.504397
159.640905	114.259963	50.509402
155.969984	118.375385	50.514407
152.744214	114.660259	50.519412
149.194332	119.168016	50.524417
145.289312	121.412345	50.529421
142.006943	115.943851	50.534426
138.439915	116.698864	50.539431
135.509446	113.636682	50.544436
131.449004	114.225386	50.549441
128.030738	104.045144	50.554445
124.677764	107.035073	50.559450
120.714907	109.136610	50.564455
117.424911	107.937292	50.569460
114.023670	107.995615	50.574465
110.488466	116.326123	50.579469
106.917040	111.785633	50.584474
103.472879	117.760666	50.589479
100.238419	120.061311	50.594484
96.623517	118.697766	50.599489
93.143573	116.743594	50.604493
89.815468	115.199075	50.609498
85.576351	116.771263	50.614503
82.619770	111.492202	50.619508
79.321710	107.313863	50.624513
75.541083	111.696444	50.629517
71.756581	108.091038	50.634522
68.205245	117.803504	50.639527
64.917704	109.387193	50.644532
61.226104	112.914260	50.649537
57.832079	110.585969	50.654541
54.847267	104.232489	50.659546
51.141868	112.561206	50.664551
47.672459	95.023696	50.669556
43.925879	102.931751	50.674561
40.221399	105.758481	50.679565
37.011724	104.366275	50.684570
33.142810	106.484769	50.689575
29.968647	104.261250	50.694580
26.351196	106.093572	50.699585
23.086141	111.414138	50.704589
19.661089	99.722718	50.709594
15.926230	110.371962	50.714599
12.545272	105.374561	50.719604
8.947479	105.659877	50.724609
5.329955	106.704434	50.729613
2.071834	103.367768	50.734618