Thu Aug 25 17:04:20 2022

Number of Points = 9925

Depth (nm)	Load (N)	Time (s)
2.293105	97.598916	0.000000
2.136464	97.933536	0.005005
2.589706	99.333709	0.010010
2.429504	102.070209	0.015014
2.302602	86.052834	0.020019
2.118546	78.352549	0.025024
1.570552	70.108169	0.030029
1.561225	58.172672	0.035034
1.520375	48.349205	0.040038
0.985703	40.498225	0.045043
0.343682	30.218463	0.050048
-0.104280	31.111260	0.055053
-0.307418	18.026065	0.060058
-0.626210	24.482699	0.065062
-0.624409	14.965783	0.070067
-0.948431	15.791702	0.075072
-1.589117	15.942732	0.080077
-1.766832	11.446394	0.085082
-2.494926	5.979589	0.090086
-2.171847	7.431787	0.095091
-2.445939	7.313404	0.100096
-3.058113	3.445130	0.105101
-3.431512	-2.526504	0.110106
-3.987780	6.238926	0.115110
-3.791623	-0.220585	0.120115
-3.850682	1.487642	0.125120
-3.901605	-5.350773	0.130125
-3.668477	-1.435717	0.135130
-4.579626	0.924879	0.140134
-5.261863	0.743895	0.145139
-5.172153	-0.295202	0.150144
-5.453479	9.341483	0.155149
-5.560237	-2.325605	0.160154
-5.738694	0.030922	0.165158
-6.296244	-1.071275	0.170163
-6.667629	-0.756795	0.175168
-6.958885	6.859789	0.180173
-6.873019	-0.866936	0.185178
-7.288729	1.207223	0.190182
-6.970151	11.860400	0.195187
-7.074935	8.475777	0.200192
-7.853115	-1.690881	0.205197
-7.839308	-0.465474	0.210202
-8.270370	0.779016	0.215206
-8.543739	-4.417345	0.220211
-9.295816	-5.846569	0.225216
-9.707261	6.158024	0.230221
-9.844384	-4.419127	0.235226
-9.824674	4.955250	0.240230
-9.663251	4.445923	0.245235
-9.667303	-3.235074	0.250240
-9.983318	5.207971	0.255245
-10.356323	-0.235373	0.260250
-10.863421	0.979902	0.265254
-11.171420	3.907225	0.270259
-10.995048	-5.475680	0.275264
-11.679510	1.411566	0.280269
-12.027528	0.064565	0.285274
-12.568219	-3.612425	0.290278
-12.518585	-7.530607	0.295283
-12.467011	0.759926	0.300288
-12.891549	10.858815	0.305293
-13.245365	-1.414973	0.310298
-13.814311	2.726998	0.315302
-13.766717	2.241834	0.320307
-14.224770	13.298273	0.325312
-14.370472	1.865078	0.330317
-14.337672	-7.004944	0.335322
-14.247606	-1.039491	0.340326
-14.384430	2.383033	0.345331
-14.844521	4.644482	0.350336
-15.644723	4.902765	0.355341
-15.488022	0.528040	0.360346
-15.496509	-3.216520	0.365350
-16.396420	-1.553716	0.370355
-16.880105	-1.436776	0.375360
-17.557200	10.925821	0.380365
-17.483110	6.146419	0.385370
-16.816320	7.285333	0.390374
-16.965915	5.144771	0.395379
-16.996864	-2.588960	0.400384
-17.788670	2.132100	0.405389
-18.197576	-4.849541	0.410394
-18.719215	-10.766306	0.415398
-18.516045	-4.037123	0.420403
-18.511319	-3.528471	0.425408
-19.070835	-5.130237	0.430413
-19.343625	-3.730210	0.435418
-19.961234	-5.417786	0.440422
-20.142755	-7.417301	0.445427
-19.974213	0.130399	0.450432
-20.344064	6.436838	0.455437
-20.615635	1.971028	0.460442
-21.310123	2.804374	0.465446
-21.468108	7.581149	0.470451
-21.484756	2.569191	0.475456
-21.887626	2.837985	0.480461
-21.646246	1.575805	0.485466
-21.777505	5.677671	0.490470
-22.392494	4.986274	0.495475
-22.773569	3.502083	0.500480
-23.108278	2.608582	0.505485
-22.804070	-0.099798	0.510490
-23.344244	10.697422	0.515494
-24.221269	9.781325	0.520499
-24.070017	-1.514896	0.525504
-24.502950	-0.962979	0.530509
-24.543399	1.295993	0.535514
-24.704832	12.116128	0.540518
-24.765332	4.491430	0.545523
-24.447689	4.941561	0.550528
-25.295309	3.362791	0.555533
-25.375319	0.221064	0.560538
-25.553582	-1.421455	0.565542
-25.883637	4.904057	0.570547
-26.459714	7.936660	0.575552
-27.008324	11.597716	0.580557
-27.133160	3.717342	0.585562
-26.794440	7.486138	0.590566
-27.214161	3.508617	0.595571
-27.893103	-0.529528	0.600576
-28.651384	-2.059020	0.605581
-28.541194	-2.031968	0.610586
-28.906295	5.748047	0.615590
-28.892088	-7.342706	0.620595
-28.988675	1.648090	0.625600
-29.332234	4.745500	0.630605
-28.994499	-6.469204	0.635610
-28.993766	-3.982566	0.640614
-29.810893	-1.506985	0.645619
-29.956646	-0.800748	0.650624
-30.759989	3.289365	0.655629
-30.407256	-5.105599	0.660634
-30.808344	-2.786957	0.665638
-31.513129	1.553470	0.670643
-31.777547	-2.815382	0.675648
-32.289755	8.303323	0.680653
-32.072381	4.830259	0.685658
-31.851608	8.718777	0.690662
-32.171797	6.487885	0.695667
-32.282216	-3.188607	0.700672
-33.264407	8.737735	0.705677
-33.244600	-6.758368	0.710682
-33.617923	3.111027	0.715686
-33.697530	2.171227	0.720691
-33.656429	4.151664	0.725696
-34.323454	-2.438352	0.730701
-34.510698	1.672284	0.735706
-34.723943	-1.423256	0.740710
-35.101495	5.112181	0.745715
-34.896040	-0.485074	0.750720
-35.362761	8.269489	0.755725
-35.974191	-8.247683	0.760730
-36.344321	-0.033446	0.765734
-36.627795	3.905607	0.770739
-36.388225	1.723051	0.775744
-36.153141	2.935933	0.780749
-36.568109	-5.572861	0.785754
-37.435834	-3.946736	0.790758
-37.699798	-1.269925	0.795763
-37.715222	4.999961	0.800768
-38.077374	3.057222	0.805773
-37.764090	4.887443	0.810778
-38.268608	8.810511	0.815782
-38.563021	-0.118975	0.820787
-38.849849	-1.905836	0.825792
-39.122187	5.511628	0.830797
-39.369449	-9.338344	0.835802
-39.833967	-3.251195	0.840806
-40.579625	0.314183	0.845811
-40.668832	-0.510217	0.850816
-41.024055	2.146093	0.855821
-41.129770	-1.700292	0.860826
-40.893266	5.026832	0.865830
-40.985729	13.289318	0.870835
-41.207786	0.162814	0.875840
-41.260414	3.189329	0.880845
-41.501236	2.065980	0.885850
-42.129286	-2.195274	0.890854
-42.319208	7.284715	0.895859
-42.496427	-0.274234	0.900864
-43.283462	3.908237	0.905869
-43.783883	-0.335049	0.910874
-43.755665	-0.048379	0.915878
-43.853015	4.475283	0.920883
-43.979294	4.007871	0.925888
-44.368417	3.904350	0.930893
-44.168331	3.449077	0.935898
-44.612488	-9.712222	0.940902
-45.235010	4.163595	0.945907
-45.582153	3.332154	0.950912
-45.888878	8.540363	0.955917
-45.845153	5.483652	0.960922
-46.023081	7.713546	0.965926
-45.957475	10.658260	0.970931
-45.860928	6.849785	0.975936
-46.562432	7.310906	0.980941
-47.154377	11.095812	0.985946
-47.131469	1.838193	0.990950
-46.944112	1.093846	0.995955
-47.863553	3.284902	1.000960
-48.487851	12.583017	1.005965
-48.627702	3.230676	1.010970
-48.641077	10.980891	1.015974
-48.501973	10.000493	1.020979
-48.416167	4.504243	1.025984
-48.999685	9.895028	1.030989
-49.793771	4.637889	1.035994
-49.813749	6.504509	1.040998
-49.944926	8.334769	1.046003
-50.118200	1.692697	1.051008
-50.259832	11.348621	1.056013
-50.821687	6.456893	1.061018
-51.213358	8.903777	1.066022
-51.625423	10.524947	1.071027
-51.772100	6.033241	1.076032
-51.975240	6.362490	1.081037
-51.586610	7.605096	1.086042
-51.956125	3.066049	1.091046
-52.382921	6.268252	1.096051
-52.794848	-3.104729	1.101056
-52.965056	4.075267	1.106061
-53.385556	-1.876327	1.111066
-53.474673	2.494183	1.116070
-53.763107	4.390212	1.121075
-53.864183	4.795219	1.126080
-54.579939	3.787417	1.131085
-54.738011	0.857240	1.136090
-54.755888	3.884637	1.141094
-54.572369	6.940590	1.146099
-55.129145	7.575189	1.151104
-56.098240	11.128124	1.156109
-56.065713	4.507589	1.161114
-55.876148	-1.526941	1.166118
-56.166284	6.570360	1.171123
-55.789912	-0.717823	1.176128
-56.857819	16.644671	1.181133
-57.366687	7.701330	1.186138
-57.722718	-2.335312	1.191142
-57.689861	-0.606686	1.196147
-57.364418	1.724669	1.201152
-57.581631	8.975307	1.206157
-58.047488	-2.119811	1.211162
-58.441371	6.066513	1.216166
-58.934820	3.185723	1.221171
-58.983096	-3.770163	1.226176
-59.543292	0.727944	1.231181
-59.444479	-0.334726	1.236186
-59.878950	6.883515	1.241190
-60.373544	-3.995126	1.246195
-60.161150	5.431313	1.251200
-60.594527	6.818539	1.256205
-60.400990	-1.377473	1.261210
-60.480928	4.159032	1.266214
-61.456208	2.761622	1.271219
-61.442872	-1.296406	1.276224
-61.732330	7.392415	1.281229
-61.654368	3.416009	1.286234
-62.002028	0.246618	1.291238
-62.944968	4.535778	1.296243
-62.976853	-3.884342	1.301248
-62.828126	3.536746	1.306253
-62.905872	2.976309	1.311258
-63.301157	4.332256	1.316262
-64.252691	3.731561	1.321267
-64.449747	-5.080296	1.326272
-64.578487	9.483788	1.331277
-64.700522	-2.019546	1.336282
-64.773376	-2.925602	1.341286
-64.671947	6.002528	1.346291
-64.621071	0.432659	1.351296
-65.349708	1.030912	1.356301
-65.567203	-2.503725	1.361306
-65.608272	2.083884	1.366310
-66.774488	-0.239068	1.371315
-67.034986	-2.912747	1.376320
-67.672456	4.754919	1.381325
-67.016679	3.339220	1.386330
-67.262772	6.171421	1.391334
-67.620295	5.161273	1.396339
-67.483785	-6.958377	1.401344
-67.701284	7.107080	1.406349
-67.894436	-0.711964	1.411354
-68.651504	1.868105	1.416358
-69.237279	-1.403180	1.421363
-69.097184	3.538859	1.426368
-69.313296	0.250779	1.431373
-69.284474	0.606958	1.436378
-69.604975	7.490962	1.441382
-70.346713	-2.561171	1.446387
-70.661791	-1.587954	1.451392
-70.947529	-0.742722	1.456397
-70.805757	-9.022369	1.461402
-71.058269	-4.708516	1.466406
-71.037069	3.172318	1.471411
-70.994842	-8.053027	1.476416
-71.617116	-2.441035	1.481421
-71.982754	0.568085	1.486426
-72.212117	6.200772	1.491430
-72.942203	5.464138	1.496435
-73.148046	12.102386	1.501440
-73.407061	9.051983	1.506445
-73.379483	-0.756862	1.511450
-73.345713	0.854561	1.516454
-73.502318	-1.332356	1.521459
-73.390197	-8.436760	1.526464
-74.338013	2.927368	1.531469
-74.958541	-9.513422	1.536474
-74.947768	-6.303854	1.541478
-75.238249	1.682766	1.546483
-75.036612	-1.939692	1.551488
-75.745899	3.575203	1.556493
-75.389664	4.098379	1.561498
-76.415025	-0.790319	1.566502
-76.864274	2.602065	1.571507
-76.910697	4.605707	1.576512
-77.381115	0.152076	1.581517
-76.966637	-1.073951	1.586522
-76.725395	5.525877	1.591526
-76.963362	-0.362567	1.596531
-77.628513	-11.473904	1.601536
-78.036433	-5.161506	1.606541
-78.240452	-3.876658	1.611546
-78.290022	-2.442003	1.616550
-78.854667	-8.238127	1.621555
-79.225713	-3.178033	1.626560
-79.771915	4.114661	1.631565
-79.958895	6.067561	1.636570
-79.744192	-2.248827	1.641574
-79.688078	-2.861877	1.646579
-79.989002	2.003732	1.651584
-80.718004	0.659485	1.656589
-81.036922	2.484360	1.661594
-80.755380	2.892689	1.666598
-81.192407	-2.698806	1.671603
-81.393179	-7.688235	1.676608
-82.259937	0.556363	1.681613
-82.310793	11.855880	1.686618
-82.611057	1.468813	1.691622
-82.695592	3.994123	1.696627
-82.707281	-4.277299	1.701632
-82.977543	4.256651	1.706637
-82.888614	-3.011800	1.711642
-83.405684	2.014228	1.716646
-83.898372	5.245740	1.721651
-83.967422	4.465639	1.726656
-84.429402	8.692093	1.731661
-84.458408	5.244980	1.736666
-84.804177	-0.123531	1.741670
-85.364688	12.015152	1.746675
-85.324478	7.820032	1.751680
-85.885008	9.062667	1.756685
-85.896390	0.177423	1.761690
-85.671022	3.116084	1.766694
-86.328320	2.523071	1.771699
-86.811488	9.891313	1.776704
-87.001009	14.366143	1.781709
-86.959587	2.599913	1.786714
-87.116855	-0.599309	1.791718
-87.576090	3.512817	1.796723
-88.102430	-12.141306	1.801728
-88.656295	11.170790	1.806733
-88.631884	-0.029621	1.811738
-88.736987	9.108043	1.816742
-88.927877	9.890958	1.821747
-88.717636	4.046178	1.826752
-89.261756	2.296471	1.831757
-89.231916	8.331471	1.836762
-89.612467	12.497710	1.841766
-90.337783	13.933847	1.846771
-90.165270	7.838711	1.851776
-90.608790	0.694820	1.856781
-90.521478	3.300770	1.861786
-91.323504	3.543527	1.866790
-91.755561	6.502944	1.871795
-91.678359	7.670960	1.876800
-92.203051	7.183720	1.881805
-92.255711	7.729838	1.886810
-92.192657	7.811732	1.891814
-92.298951	7.540508	1.896819
-92.684931	2.845855	1.901824
-93.538833	6.921747	1.906829
-93.720093	-6.612937	1.911834
-93.671339	4.269166	1.916838
-93.689265	-0.103504	1.921843
-93.573893	1.710268	1.926848
-94.352543	2.616919	1.931853
-94.851602	9.854772	1.936858
-94.727165	7.690256	1.941862
-95.144858	3.168253	1.946867
-95.014349	3.442058	1.951872
-95.761934	8.709855	1.956877
-95.978967	5.178309	1.961882
-96.050309	1.915003	1.966886
-96.393740	1.133603	1.971891
-96.240833	-0.715831	1.976896
-96.767397	9.000404	1.981901
-97.297660	0.813404	1.986906
-97.796361	1.559129	1.991910
-97.685413	8.783654	1.996915
-97.644940	5.601839	2.006912
-97.794399	7.313759	2.016909
-97.607394	5.811464	2.026906
-96.802357	10.199523	2.036902
-95.794132	8.676253	2.046899
-95.205209	7.053958	2.056896
-95.382363	5.317284	2.066893
-94.995421	10.635674	2.076890
-94.209634	5.659479	2.086886
-93.770201	6.062677	2.096883
-92.874816	3.283622	2.106880
-92.551964	1.728362	2.116877
-92.381379	0.653130	2.126874
-91.332989	6.884746	2.136870
-91.289607	-2.394236	2.146867
-90.771108	3.511760	2.156864
-90.076745	4.267823	2.166861
-89.740148	8.944696	2.176858
-88.888571	8.355140	2.186854
-88.706782	9.574827	2.196851
-88.245325	9.543749	2.206848
-87.159338	8.480302	2.216845
-86.817634	2.094317	2.226842
-87.066420	6.178666	2.236838
-86.176687	-1.338574	2.246835
-85.555376	4.256705	2.256832
-85.555548	0.274820	2.266829
-84.737265	0.602816	2.276826
-84.002998	2.762309	2.286822
-83.349548	3.363224	2.296819
-83.212819	8.388199	2.306816
-82.850843	-1.808691	2.316813
-81.943491	-1.149359	2.326810
-81.707117	-0.429238	2.336806
-81.343564	5.336312	2.346803
-80.543849	3.753849	2.356800
-80.211816	2.989108	2.366797
-79.106239	2.993318	2.376794
-78.977522	3.432532	2.386790
-78.472131	5.127373	2.396787
-78.533646	5.292284	2.406784
-77.638439	3.010607	2.416781
-77.362459	-2.243666	2.426778
-76.091439	2.768299	2.436774
-75.668644	3.671454	2.446771
-75.549653	-3.059771	2.456768
-75.460229	-1.984002	2.466765
-74.969682	15.029619	2.476762
-74.038581	8.639978	2.486758
-73.610091	-0.335050	2.496755
-73.017677	5.369297	2.506752
-72.654372	2.860519	2.516749
-71.774590	-0.730221	2.526746
-71.299472	1.634607	2.536742
-71.142160	5.452582	2.546739
-70.921843	8.462392	2.556736
-69.963534	7.609023	2.566733
-69.700935	-0.281956	2.576730
-68.644445	2.451111	2.586726
-68.310258	6.222365	2.596723
-68.283396	1.216202	2.606720
-67.955069	4.684261	2.616717
-67.229771	0.857966	2.626714
-66.587809	7.580928	2.636710
-65.590849	8.498655	2.646707
-65.371840	3.183614	2.656704
-65.169326	2.727441	2.666701
-65.035516	5.668442	2.676698
-64.273739	5.789882	2.686694
-63.347770	9.550773	2.696691
-62.745438	1.064861	2.706688
-62.692547	2.631032	2.716685
-62.355581	6.449368	2.726682
-61.761344	3.638306	2.736678
-60.866146	4.749377	2.746675
-60.267438	3.743279	2.756672
-60.657954	0.430779	2.766669
-59.484495	8.999669	2.776666
-58.736680	3.155106	2.786662
-58.666783	9.153574	2.796659
-58.176203	5.142309	2.806656
-57.336838	4.985493	2.816653
-57.360262	5.841358	2.826650
-56.519250	1.756176	2.836646
-55.732893	5.187314	2.846643
-55.833611	0.413386	2.856640
-54.617921	1.895561	2.866637
-54.254754	1.449061	2.876634
-54.277130	9.229637	2.886630
-53.922240	3.646214	2.896627
-53.040255	2.478520	2.906624
-52.676389	-0.863485	2.916621
-51.886106	-5.038919	2.926618
-51.643018	-2.425488	2.936614
-50.946820	4.390347	2.946611
-50.325013	6.000425	2.956608
-49.977046	-7.200539	2.966605
-49.873112	-2.474538	2.976602
-49.154779	-0.398076	2.986598
-48.452799	0.885824	2.996595
-47.475476	3.894229	3.006592
-47.426941	3.870833	3.016589
-47.227572	1.150155	3.026586
-46.838603	1.101927	3.036582
-46.141176	5.709594	3.046579
-45.238793	8.061331	3.056576
-44.533274	5.514770	3.066573
-44.398703	0.520240	3.076570
-44.202340	3.388084	3.086566
-43.768694	-0.088400	3.096563
-42.726248	-1.417453	3.106560
-42.722811	0.698167	3.116557
-41.990464	1.647855	3.126554
-41.280419	-0.690337	3.136550
-41.110228	-1.531088	3.146547
-40.622412	0.717711	3.156544
-39.806295	1.030211	3.166541
-39.676794	1.672044	3.176538
-39.038725	1.759016	3.186534
-38.419721	5.615525	3.196531
-38.089527	3.517417	3.206528
-37.212214	3.459197	3.216525
-36.890233	5.119422	3.226522
-36.853126	0.894107	3.236518
-36.000895	4.403625	3.246515
-35.249608	4.897346	3.256512
-35.193505	8.430238	3.266509
-34.300657	7.184814	3.276506
-33.787569	4.674742	3.286502
-33.855238	4.875463	3.296499
-33.188484	4.552458	3.306496
-32.517139	2.996449	3.316493
-31.330081	11.129223	3.326490
-31.132640	6.498644	3.336486
-30.814540	3.911417	3.346483
-30.696060	9.208521	3.356480
-30.385376	1.477900	3.366477
-29.415444	3.771536	3.376474
-29.150117	5.995010	3.386470
-28.216636	4.518304	3.396467
-27.981177	10.421142	3.406464
-27.767411	9.446849	3.416461
-27.220464	8.848009	3.426458
-26.318877	9.315014	3.436454
-25.497129	13.307654	3.446451
-25.170283	7.639924	3.456448
-25.156000	5.676847	3.466445
-24.921326	6.926264	3.476442
-24.111352	1.829074	3.486438
-23.316729	7.679144	3.496435
-22.308816	3.675519	3.506432
-22.317781	5.679040	3.516429
-22.002063	11.106800	3.526426
-21.957815	9.145363	3.536422
-21.028340	-0.576577	3.546419
-20.530819	4.059248	3.556416
-19.221948	-4.021011	3.566413
-19.425766	3.610596	3.576410
-19.077420	3.293133	3.586406
-18.539257	6.348178	3.596403
-17.654285	3.393362	3.606400
-17.416120	2.405744	3.616397
-17.231262	0.843598	3.626394
-16.190749	2.806226	3.636390
-15.984689	2.447701	3.646387
-15.724752	10.117521	3.656384
-14.430763	2.007914	3.666381
-14.763061	1.296581	3.676378
-14.071137	9.620980	3.686374
-13.225506	4.619574	3.696371
-12.752351	4.966807	3.706368
-12.578282	4.797028	3.716365
-11.947463	0.228428	3.726362
-11.662306	-1.713734	3.736358
-10.521717	0.797088	3.746355
-10.305110	-3.244108	3.756352
-10.130812	3.007269	3.766349
-9.709479	3.901153	3.776346
-8.807684	2.609981	3.786342
-8.482053	3.078532	3.796339
-7.678077	5.173258	3.806336
-7.306564	2.175349	3.816333
-7.062305	-4.531156	3.826330
-6.612539	3.311660	3.836326
-5.929686	3.198379	3.846323
-5.627846	4.643182	3.856320
-5.007195	8.854234	3.866317
-4.527313	14.262609	3.876314
-3.708283	22.373863	3.886310
-3.868156	21.353575	3.896307
-2.819204	40.737982	3.906304
-2.702846	44.299455	3.916301
-2.266468	51.010304	3.926298
-1.787336	63.948768	3.936294
-1.450939	78.784969	3.946291
-1.156828	88.182280	3.956288
-0.317525	120.223493	3.966285
0.000000	118.374269	3.971290
0.151340	115.949256	3.976294
0.192597	125.355123	3.981299
0.325919	128.928336	3.986304
0.395978	140.806955	3.991309
0.424304	141.748518	3.996314
0.535570	136.007787	4.001318
0.631211	149.932549	4.006323
0.984960	149.703137	4.011328
0.943368	167.968010	4.016333
1.080644	162.561723	4.021338
1.228097	159.972795	4.026342
0.796435	157.012690	4.031347
0.843798	151.633150	4.036352
0.673888	162.631879	4.041357
1.048709	165.313032	4.046362
1.367784	165.130183	4.051366
1.003670	169.967773	4.056371
1.143952	168.632836	4.061376
1.216688	165.074834	4.066381
1.102186	151.722549	4.071386
1.454509	144.260901	4.076390
0.680788	150.425023	4.081395
0.712079	147.582210	4.086400
0.654321	158.914547	4.091405
1.053950	154.248616	4.096410
1.232710	164.354307	4.101414
1.306763	171.464462	4.106419
1.434125	161.427912	4.111424
1.384897	169.645732	4.116429
1.176891	161.787809	4.121434
1.166877	163.456729	4.126438
1.159443	161.894997	4.131443
1.417019	161.554101	4.136448
1.133410	167.372512	4.141453
1.313785	159.229106	4.146458
1.522102	157.424758	4.151462
0.833239	147.709098	4.156467
1.245306	151.637280	4.161472
1.139237	169.909094	4.166477
1.472800	173.792633	4.171482
1.294225	161.567205	4.176486
1.173295	164.718347	4.181491
1.330831	162.346142	4.186496
1.146292	168.487558	4.191501
1.802787	168.675791	4.196506
1.434243	162.630573	4.201510
1.515219	172.201086	4.206515
1.579459	167.182735	4.211520
1.523854	157.260278	4.216525
1.110157	155.917228	4.221530
1.336912	160.146535	4.226534
1.377515	166.357080	4.231539
1.495289	153.395514	4.236544
1.516630	167.233853	4.241549
1.540955	172.314307	4.246554
1.664791	169.972692	4.251558
1.245003	169.652505	4.256563
1.586385	172.702737	4.261568
1.405932	174.961521	4.266573
1.373674	170.483481	4.271578
1.899998	164.962451	4.276582
1.423473	177.059615	4.281587
1.712097	167.190787	4.286592
1.473083	167.278882	4.291597
1.651534	169.851596	4.296602
1.832379	165.488867	4.301606
1.360300	169.552421	4.306611
1.512721	157.458635	4.311616
1.337533	171.716918	4.316621
1.488230	159.851195	4.321626
1.487086	155.365119	4.326630
1.673097	166.845931	4.331635
1.731831	154.817447	4.336640
1.322756	159.247620	4.341645
1.379667	167.600672	4.346650
1.639416	162.485249	4.351654
1.539416	168.189469	4.356659
1.986460	175.760049	4.361664
1.685026	190.405130	4.366669
1.656605	193.915112	4.371674
1.694291	198.879583	4.376678
1.827026	190.326004	4.381683
2.030886	190.569338	4.386688
1.957860	194.247664	4.391693
1.903761	192.898888	4.396698
2.070744	190.300569	4.401702
1.812871	187.126563	4.406707
1.676882	173.192324	4.411712
1.671220	188.256140	4.416717
2.153802	188.044508	4.421722
2.320337	191.707444	4.426726
1.838083	189.084297	4.431731
2.195370	179.850122	4.436736
1.844613	186.507979	4.441741
1.594902	186.961587	4.446746
1.707536	183.852919	4.451750
1.563652	189.785489	4.456755
1.819045	191.881071	4.461760
1.917028	194.042446	4.466765
2.023155	200.084546	4.471770
1.885172	192.927495	4.476774
1.793411	200.604655	4.481779
2.056860	186.803975	4.486784
1.510610	199.747326	4.491789
2.222279	202.445310	4.496794
2.449116	211.879094	4.501798
2.075528	199.184312	4.506803
1.825456	195.426941	4.511808
2.098195	210.247835	4.516813
2.354119	213.643665	4.521818
2.568789	206.216215	4.526822
1.869338	202.649478	4.531827
1.974457	202.984215	4.536832
2.372308	215.823945	4.541837
2.208159	220.661856	4.546842
2.253258	210.372407	4.551846
2.249179	213.043331	4.556851
2.269301	212.584613	4.561856
2.330673	214.590372	4.566861
2.100786	220.881284	4.571866
2.017394	208.602944	4.576870
2.164234	218.827564	4.581875
2.101828	211.994029	4.586880
2.345517	220.333660	4.591885
2.347279	218.833758	4.596890
2.724346	216.386019	4.601894
2.632771	228.410247	4.606899
2.485951	216.613249	4.611904
2.294324	225.555774	4.616909
2.600562	224.232797	4.621914
2.455881	218.025931	4.626918
2.543113	224.953705	4.631923
2.372562	225.002599	4.636928
2.212013	226.286978	4.641933
2.584165	226.374228	4.646938
2.432232	223.730958	4.651942
2.503278	225.697237	4.656947
2.450849	211.354397	4.661952
2.435558	220.142738	4.666957
2.388777	219.605915	4.671962
2.261335	219.474044	4.676966
2.268425	219.976004	4.681971
2.359535	222.151115	4.686976
2.291877	213.806097	4.691981
2.470601	215.619460	4.696986
2.602373	232.164593	4.701990
2.576926	243.672259	4.706995
2.447429	249.365307	4.712000
2.638918	247.319973	4.717005
2.312437	240.610062	4.722010
2.803663	243.282481	4.727014
2.278722	246.645638	4.732019
2.755196	238.699417	4.737024
2.810791	241.531842	4.742029
2.837410	240.309624	4.747034
2.681143	247.190135	4.752038
2.390329	253.253318	4.757043
3.092537	251.922081	4.762048
3.236215	247.875210	4.767053
2.841398	253.176387	4.772058
3.075860	246.286833	4.777062
3.143807	255.312091	4.782067
3.303778	239.490082	4.787072
3.172671	237.460492	4.792077
2.778813	230.330862	4.797082
3.002957	216.400275	4.802086
2.601225	222.446024	4.807091
2.712085	214.515969	4.812096
2.635918	225.120390	4.817101
2.811538	233.356795	4.822106
3.052940	243.269214	4.827110
2.539814	250.892190	4.832115
2.888753	245.054072	4.837120
2.861625	248.981487	4.842125
2.532769	248.093382	4.847130
2.844016	247.693455	4.852134
2.623639	248.696138	4.857139
2.685340	244.896235	4.862144
2.813807	241.016267	4.867149
2.559508	254.078431	4.872154
2.943617	259.004459	4.877158
2.733908	265.061265	4.882163
2.846625	263.502845	4.887168
2.919362	274.748368	4.892173
3.188785	275.607869	4.897178
3.404704	268.044153	4.902182
2.874432	270.693126	4.907187
3.187551	272.343064	4.912192
2.988633	274.196620	4.917197
3.194630	271.886412	4.922202
3.251958	263.958396	4.927206
3.126268	269.331307	4.932211
3.213218	270.602222	4.937216
3.158397	274.989573	4.942221
2.979285	273.919812	4.947226
2.971016	271.883627	4.952230
3.165120	273.833794	4.957235
3.322054	270.310036	4.962240
3.271392	257.150154	4.967245
3.073064	269.839720	4.972250
3.409967	283.141476	4.977254
3.203424	292.950098	4.982259
3.519400	288.673736	4.987264
3.674088	288.997544	4.992269
3.380862	282.715852	4.997274
3.331657	277.800668	5.002278
3.457032	279.249064	5.007283
3.714673	264.408335	5.012288
3.369507	281.547110	5.017293
3.194560	278.584727	5.022298
3.678271	266.470598	5.027302
3.536336	277.512472	5.032307
3.691501	270.018387	5.037312
3.564327	274.281029	5.042317
3.218979	271.187155	5.047322
3.299726	276.926366	5.052326
3.156498	275.752905	5.057331
3.563851	272.598044	5.062336
3.568503	284.841355	5.067341
3.602072	290.315874	5.072346
3.368749	290.175281	5.077350
3.528358	302.112745	5.082355
3.788712	299.227690	5.087360
3.886648	297.193844	5.092365
3.830143	292.716408	5.097370
3.624375	285.525648	5.102374
3.190505	276.671654	5.107379
3.565766	277.625306	5.112384
3.508062	300.436097	5.117389
3.458586	293.274631	5.122394
4.025861	290.613578	5.127398
3.667776	298.617252	5.132403
3.575352	296.461369	5.137408
3.793356	301.033775	5.142413
3.829472	299.699330	5.147418
4.080879	305.696556	5.152422
3.870208	304.448236	5.157427
3.864443	295.473371	5.162432
3.667998	298.386426	5.167437
3.602393	303.313325	5.172442
3.863187	297.188437	5.177446
3.744090	292.163974	5.182451
3.912792	307.801699	5.187456
3.548447	302.578372	5.192461
3.785835	301.424369	5.197466
3.978684	291.083249	5.202470
3.926425	294.850092	5.207475
4.132290	286.797550	5.212480
3.879031	297.132361	5.217485
3.601268	297.043025	5.222490
4.152113	295.703864	5.227494
4.099505	297.164329	5.232499
4.019985	293.873772	5.237504
4.022806	297.549727	5.242509
4.033153	307.416124	5.247514
4.350730	297.150373	5.252518
4.078841	287.242749	5.257523
4.424504	289.678548	5.262528
3.967563	275.898922	5.267533
3.784252	267.135392	5.272538
4.157036	274.546803	5.277542
3.730792	292.919530	5.282547
4.037121	287.771462	5.287552
3.906110	299.495025	5.292557
3.816043	298.847920	5.297562
3.934469	293.381271	5.302566
3.884859	291.851446	5.307571
4.024322	289.798439	5.312576
3.721583	293.743737	5.317581
3.782516	295.126299	5.322586
4.305405	290.912432	5.327590
3.956460	292.862264	5.332595
4.191181	306.914057	5.337600
4.303468	314.799746	5.342605
4.479538	311.627331	5.347610
4.422216	294.194125	5.352614
3.983323	294.737491	5.357619
4.107305	296.828365	5.362624
4.024166	308.715280	5.367629
3.987113	325.625483	5.372634
4.360717	325.604935	5.377638
4.262761	327.002904	5.382643
4.260658	327.655008	5.387648
4.468079	324.215080	5.392653
4.288301	327.479878	5.397658
4.227192	321.911632	5.402662
4.221786	329.597463	5.407667
4.671595	321.136514	5.412672
4.668473	321.466066	5.417677
4.304414	324.892618	5.422682
4.782354	322.394258	5.427686
4.205671	324.095032	5.432691
4.781941	321.258554	5.437696
4.742215	323.988865	5.442701
4.472901	322.876286	5.447706
4.685289	315.512425	5.452710
4.449538	320.437513	5.457715
4.778233	319.478015	5.462720
4.645776	325.510082	5.467725
4.430043	315.505056	5.472730
4.233270	315.640318	5.477734
4.424725	321.175531	5.482739
4.794420	319.105430	5.487744
4.734139	323.038056	5.492749
4.497598	321.819099	5.497754
4.552697	320.067216	5.502758
4.698784	323.432819	5.507763
4.745725	320.616002	5.512768
4.767303	331.192516	5.517773
4.717198	331.080165	5.522778
4.597219	310.654279	5.527782
4.386296	317.419991	5.532787
4.989680	323.865124	5.537792
4.494818	329.064937	5.542797
4.422034	326.893317	5.547802
4.936818	316.577673	5.552806
4.558074	327.273857	5.557811
4.849687	319.375548	5.562816
4.991124	326.677693	5.567821
4.602504	321.939067	5.572826
4.803355	318.981073	5.577830
4.496450	326.536967	5.582835
4.506195	320.441915	5.587840
4.295126	324.923364	5.592845
4.714019	321.867929	5.597850
5.103557	335.253228	5.602854
5.133414	336.137613	5.607859
5.086379	315.510462	5.612864
5.114629	318.964132	5.617869
5.122754	319.541865	5.622874
5.009657	313.029453	5.627878
4.793858	325.898971	5.632883
4.790772	315.427181	5.637888
4.910273	317.468138	5.642893
4.853819	327.908176	5.647898
4.994631	324.874165	5.652902
4.866515	320.936303	5.657907
4.928171	324.093667	5.662912
4.586526	329.680772	5.667917
4.769354	341.741177	5.672922
4.694709	341.145440	5.677926
4.616749	348.896432	5.682931
4.523565	347.186763	5.687936
4.841732	344.969705	5.692941
4.902454	357.289705	5.697946
5.091790	365.131705	5.702950
5.094531	375.619446	5.707955
5.165728	368.919946	5.712960
5.280673	373.850213	5.717965
5.110933	374.202709	5.722970
5.333959	368.950608	5.727974
5.225317	372.194776	5.732979
5.309564	372.007588	5.737984
5.244583	384.268206	5.742989
5.234846	383.665461	5.747994
5.509638	368.429642	5.752998
5.198831	368.124014	5.758003
5.447128	367.471348	5.763008
5.025365	364.003441	5.768013
5.195020	370.013498	5.773018
5.417452	374.746586	5.778022
5.521067	382.383719	5.783027
5.478658	379.751740	5.788032
5.175102	365.802474	5.793037
5.382392	374.429463	5.798042
5.229497	372.846209	5.803046
5.090632	378.604043	5.808051
5.352132	382.872254	5.813056
5.236099	378.154180	5.818061
5.290465	381.515182	5.823066
5.150685	380.521513	5.828070
5.208740	382.296850	5.833075
5.139174	373.689457	5.838080
5.393885	378.661104	5.843085
5.122528	377.770310	5.848090
5.373470	372.257563	5.853094
5.222529	388.435838	5.858099
5.485311	395.503856	5.863104
5.323731	402.492830	5.868109
5.167368	405.700188	5.873114
5.440466	403.936287	5.878118
5.561200	404.800109	5.883123
5.652547	396.635742	5.888128
5.388020	406.330120	5.893133
5.510687	411.050374	5.898138
5.879484	401.124562	5.903142
5.779873	410.552650	5.908147
5.338469	405.385661	5.913152
5.574522	399.182355	5.918157
5.662989	406.647860	5.923162
5.818195	401.861971	5.928166
5.685220	407.856180	5.933171
6.021955	407.771805	5.938176
5.681789	408.894509	5.943181
5.610184	400.072281	5.948186
6.082833	395.502418	5.953190
6.026088	410.172617	5.958195
5.857756	404.488264	5.963200
5.605820	403.376120	5.968205
5.850373	412.357968	5.973210
6.046550	404.803615	5.978214
5.775712	397.724248	5.983219
6.008738	395.001652	5.988224
5.603844	400.063999	5.993229
5.560412	410.634926	5.998234
5.803338	396.910070	6.003238
5.809444	412.038672	6.008243
6.135235	401.442533	6.013248
6.140139	406.102141	6.018253
5.826839	405.417241	6.023258
5.860983	405.880165	6.028262
5.711802	399.442980	6.033267
5.870347	400.639409	6.038272
5.737685	407.509956	6.043277
5.677300	414.869070	6.048282
6.082792	401.286422	6.053286
5.724967	404.683538	6.058291
5.852907	397.573327	6.063296
5.839789	403.947401	6.068301
5.383247	407.170153	6.073306
5.895362	403.268005	6.078310
5.147169	411.766301	6.083315
5.645140	401.823413	6.088320
5.660264	401.492027	6.093325
5.918570	403.565031	6.098330
5.867791	404.800585	6.103334
5.732810	398.070102	6.108339
5.766397	402.652446	6.113344
5.776968	403.058950	6.118349
5.646516	402.933877	6.123354
5.789109	401.060707	6.128358
5.277004	400.618933	6.133363
5.817354	399.895196	6.138368
5.841603	401.697979	6.143373
5.545355	395.660337	6.148378
5.876226	407.517252	6.153382
5.681041	416.273762	6.158387
5.859439	421.320655	6.163392
6.050361	421.917208	6.168397
5.892260	417.012720	6.173402
5.957768	396.159028	6.178406
5.874163	401.038153	6.183411
5.723204	402.017312	6.188416
5.645361	395.803076	6.193421
5.838100	407.140616	6.198426
5.873295	403.569465	6.203430
5.658392	402.843836	6.208435
5.543150	394.828902	6.213440
5.721212	414.062551	6.218445
5.679265	420.593012	6.223450
5.922581	428.616414	6.228454
5.823170	435.282439	6.233459
6.324966	423.700062	6.238464
6.344286	403.176312	6.243469
6.222896	409.387012	6.248474
6.324069	400.452288	6.253478
5.815106	408.530273	6.258483
5.872017	396.071629	6.263488
5.561913	396.075947	6.268493
5.860717	405.767484	6.273498
5.913695	401.820213	6.278502
6.001162	397.769460	6.283507
6.245826	398.376575	6.288512
6.144222	405.137848	6.293517
5.897215	400.174526	6.298522
6.259478	379.717295	6.303526
5.925001	388.128611	6.308531
5.875045	378.920175	6.313536
5.974309	380.454931	6.318541
5.411431	378.784050	6.323546
5.927307	371.008772	6.328550
5.735097	372.959366	6.333555
5.760516	373.708403	6.338560
5.858390	374.161341	6.343565
5.896070	378.065974	6.348570
5.761495	372.240297	6.353574
5.782370	379.501240	6.358579
5.729193	369.011957	6.363584
5.847850	374.887633	6.368589
5.308474	375.133524	6.373594
5.961573	375.489976	6.378598
5.519344	374.546859	6.383603
5.770917	381.933013	6.388608
6.156537	392.430377	6.393613
5.982443	394.409774	6.398618
5.838257	383.346265	6.403622
5.879607	385.918346	6.408627
5.777522	374.332540	6.413632
5.734472	365.901335	6.418637
5.760653	374.139072	6.423642
5.842128	366.621691	6.428646
5.889880	380.851537	6.433651
5.883507	377.812103	6.438656
6.106516	368.731752	6.443661
5.676938	368.447897	6.448666
5.849980	372.404088	6.453670
5.932664	367.835221	6.458675
6.171718	363.570893	6.463680
6.018154	371.906398	6.468685
5.842712	375.936175	6.473690
6.090964	367.652322	6.478694
6.152596	368.281786	6.483699
5.834112	367.879281	6.488704
5.751729	366.667805	6.493709
5.847365	360.654197	6.498714
6.201538	364.743363	6.503718
6.100290	371.222985	6.508723
5.911908	354.142460	6.513728
5.866166	357.534962	6.518733
5.582415	348.388485	6.523738
5.999637	349.107770	6.528742
5.791370	353.348335	6.533747
5.234970	349.021978	6.538752
5.729511	356.237171	6.543757
5.993614	359.375477	6.548762
6.016023	365.930637	6.553766
5.660152	355.552065	6.558771
6.101870	361.348644	6.563776
5.801411	350.429868	6.568781
5.509733	345.337515	6.573786
5.534491	355.347218	6.578790
6.095178	361.583913	6.583795
5.842032	368.039876	6.588800
5.676416	368.081669	6.593805
5.433189	370.578110	6.598810
5.875021	366.490823	6.603814
5.750559	377.773637	6.608819
5.931804	378.197693	6.613824
5.557328	366.622932	6.618829
5.781325	377.452504	6.623834
5.740712	374.446910	6.628838
5.841506	379.145272	6.633843
5.741612	371.115288	6.638848
6.086953	379.350479	6.643853
5.662497	369.466714	6.648858
5.911143	372.623263	6.653862
5.745274	377.676626	6.658867
5.974788	369.104634	6.663872
5.924338	378.477546	6.668877
5.545354	383.643399	6.673882
6.144456	375.488073	6.678886
5.868085	368.744951	6.683891
5.942344	376.519564	6.688896
6.229523	376.420806	6.693901
5.583378	361.481153	6.698906
5.926056	346.291665	6.703910
5.551752	351.535872	6.708915
5.769122	360.816190	6.713920
5.804002	368.818437	6.718925
5.802608	380.923553	6.723930
6.029123	363.331909	6.728934
5.543250	358.915404	6.733939
5.715155	366.649401	6.738944
6.008564	364.173621	6.743949
5.888138	366.309125	6.748954
5.887793	353.574735	6.753958
5.759280	350.000771	6.758963
5.236353	352.107587	6.763968
6.094548	360.021962	6.768973
5.886346	372.928289	6.773978
5.722564	363.937018	6.778982
6.016741	372.800336	6.783987
6.043995	372.881513	6.788992
5.957195	359.262133	6.793997
5.870056	354.257956	6.799002
5.739315	351.279143	6.804006
5.466535	346.152191	6.809011
5.487269	355.627835	6.814016
5.728816	361.395665	6.819021
5.968665	374.206480	6.824026
5.948929	368.283715	6.829030
5.750110	382.593326	6.834035
6.032708	376.635843	6.839040
5.983576	359.985924	6.844045
5.758058	361.179249	6.849050
5.989432	349.101438	6.854054
5.683619	363.481583	6.859059
5.728005	356.979283	6.864064
5.866744	349.725027	6.869069
5.931426	350.477402	6.874074
6.234955	349.002976	6.879078
5.849664	354.979752	6.884083
5.939128	351.226097	6.889088
5.864356	350.883487	6.894093
5.720468	355.101310	6.899098
6.118739	357.677576	6.904102
5.916022	355.966085	6.909107
5.789512	351.176891	6.914112
5.992345	350.692706	6.919117
5.698045	347.625622	6.924122
5.817528	342.408735	6.929126
5.679087	353.757001	6.934131
6.015272	356.273390	6.939136
6.089432	350.728235	6.944141
5.770902	356.855908	6.949146
5.836102	354.640518	6.954150
5.823293	356.319385	6.959155
5.917799	350.634997	6.964160
6.147871	352.962363	6.969165
6.078544	353.745226	6.974170
6.090439	342.277627	6.979174
5.701679	348.112572	6.984179
5.457971	331.401415	6.989184
5.934555	344.494665	6.994189
5.811609	353.388527	6.999194
5.959108	344.921148	7.004198
5.846723	351.146237	7.009203
6.080076	340.045748	7.014208
6.062089	327.405892	7.019213
5.757862	322.090880	7.024218
5.950576	315.884902	7.029222
5.756764	327.045668	7.034227
5.580844	321.947841	7.039232
5.741864	317.980496	7.044237
5.280174	324.633638	7.049242
5.664702	327.873295	7.054246
5.574787	349.664113	7.059251
5.987477	353.010097	7.064256
5.977201	352.628906	7.069261
5.685483	364.779500	7.074266
6.155665	346.690936	7.079270
5.785108	360.533879	7.084275
5.948331	347.226521	7.089280
5.854574	340.223837	7.094285
5.503178	328.835315	7.099290
5.510043	334.507025	7.104294
5.716205	347.750219	7.109299
5.938410	352.508646	7.114304
5.795997	352.274713	7.119309
5.436868	355.921967	7.124314
5.650128	359.688352	7.129318
5.743109	342.892792	7.134323
5.621190	343.509884	7.139328
5.702125	353.165925	7.144333
5.769975	361.957128	7.149338
6.025372	344.746966	7.154342
5.760823	352.552506	7.159347
5.772975	350.010062	7.164352
5.775991	352.009161	7.169357
5.774877	355.831281	7.174362
5.815225	356.761480	7.179366
5.789568	367.829485	7.184371
5.841673	355.757610	7.189376
5.973519	360.144209	7.194381
5.464229	364.586970	7.199386
5.672905	362.716105	7.204390
5.482133	362.863082	7.209395
5.379066	359.677445	7.214400
5.774076	354.183260	7.219405
5.370266	363.728592	7.224410
5.792549	374.710597	7.229414
5.662341	379.460972	7.234419
5.439134	378.822069	7.239424
5.966996	380.976226	7.244429
5.724399	382.640478	7.249434
5.848975	376.248996	7.254438
5.986507	389.218227	7.259443
5.775738	381.939623	7.264448
5.948721	383.870965	7.269453
5.817966	389.285837	7.274458
5.877897	377.010235	7.279462
5.611505	394.940393	7.284467
5.883021	383.897175	7.289472
6.092259	386.696058	7.294477
6.062720	385.789522	7.299482
5.763430	364.164097	7.304486
5.725903	367.647066	7.309491
5.746738	368.982131	7.314496
5.853801	371.439507	7.319501
5.937746	373.789771	7.324506
5.997589	358.685718	7.329510
5.764363	368.428957	7.334515
5.517974	363.304192	7.339520
5.729134	362.043560	7.344525
5.849982	384.779025	7.349530
5.886781	377.142085	7.354534
5.361267	376.914391	7.359539
5.723458	379.341285	7.364544
5.541344	375.905432	7.369549
5.700302	379.063379	7.374554
5.467037	373.866951	7.379558
5.574766	387.435653	7.384563
5.491561	386.581820	7.389568
6.059853	380.611210	7.394573
5.628621	382.776431	7.399578
5.646932	368.131308	7.404582
5.533790	387.027729	7.409587
5.604962	380.163709	7.414592
5.886173	379.983626	7.419597
5.937270	388.593964	7.424602
5.720550	383.992908	7.429606
5.935540	389.448522	7.434611
5.708615	389.164553	7.439616
5.764433	381.682824	7.444621
5.888022	385.634112	7.449626
5.832288	382.187947	7.454630
6.146827	378.648965	7.459635
5.829636	380.166712	7.464640
5.908312	383.827635	7.469645
5.850064	389.487418	7.474650
5.936149	384.339029	7.479654
5.789733	381.811933	7.484659
5.781158	376.953633	7.489664
5.978034	384.952653	7.494669
5.813879	380.998277	7.499674
5.694958	381.627556	7.504678
5.935673	387.987164	7.509683
5.946866	387.792439	7.514688
6.074847	377.809457	7.519693
5.870958	388.956022	7.524698
5.889776	377.588558	7.529702
5.769161	384.609074	7.534707
5.869772	381.306097	7.539712
5.649818	380.381938	7.544717
5.749808	388.617609	7.549722
5.668267	379.929829	7.554726
5.539133	386.394843	7.559731
5.696854	392.027115	7.564736
5.677662	381.583121	7.569741
5.633191	389.942670	7.574746
5.881245	382.911725	7.579750
5.677292	385.174217	7.584755
5.893622	386.019896	7.589760
5.849708	385.969851	7.594765
5.932003	385.181838	7.599770
6.064232	374.641355	7.604774
5.853729	384.425336	7.609779
5.842889	385.170562	7.614784
5.984995	380.408878	7.619789
5.757548	385.674378	7.624794
5.719410	380.295510	7.629798
5.685943	394.538093	7.634803
5.434363	382.200562	7.639808
5.657484	380.406528	7.644813
5.765139	387.688680	7.649818
6.073708	381.069045	7.654822
5.957789	385.564076	7.659827
5.579638	387.559624	7.664832
5.916327	390.999783	7.669837
5.833132	393.771719	7.674842
5.960423	388.601053	7.679846
5.828481	384.591008	7.684851
5.825537	395.291628	7.689856
6.183611	385.785133	7.694861
6.024479	382.943645	7.699866
5.796029	382.704208	7.704870
6.015447	385.957090	7.709875
5.713278	384.036546	7.714880
5.856726	385.602345	7.719885
5.760558	387.715068	7.724890
6.134173	382.100837	7.729894
5.912706	383.344151	7.734899
5.849153	385.239786	7.739904
5.824203	382.019759	7.744909
5.586489	387.008450	7.749914
6.011448	379.332837	7.754918
5.808782	381.383150	7.759923
6.037352	385.855843	7.764928
6.010889	381.370514	7.769933
5.820514	380.723304	7.774938
5.586647	367.503458	7.779942
5.806124	375.571701	7.784947
5.581903	383.826530	7.789952
5.890515	375.618639	7.794957
5.767960	388.021162	7.799962
5.942320	379.258485	7.804966
5.923432	389.233915	7.809971
5.902701	378.862932	7.814976
5.957706	368.287094	7.819981
5.797119	365.781204	7.824986
5.783077	355.121277	7.829990
5.474800	351.255930	7.834995
5.610601	365.326432	7.840000
6.220672	378.360825	7.845005
5.983599	369.621487	7.850010
6.059598	351.816150	7.855014
5.953730	357.878864	7.860019
5.564150	358.060154	7.865024
5.412120	355.603546	7.870029
5.264958	359.505499	7.875034
6.182957	373.330060	7.880038
6.460539	374.830548	7.885043
5.481198	366.292937	7.890048
5.762029	358.719012	7.895053
5.824313	351.821592	7.900058
5.685438	347.945523	7.905062
5.857914	358.612309	7.910067
5.725232	369.599004	7.915072
6.040261	376.880298	7.920077
5.700131	365.271682	7.925082
5.876446	350.453116	7.930086
5.778476	353.809507	7.935091
5.124259	357.161302	7.940096
5.733739	356.999390	7.945101
5.565303	379.631474	7.950106
6.091512	377.365996	7.955110
6.009648	375.974099	7.960115
5.790064	380.747970	7.965120
6.162505	374.906128	7.970125
5.981771	379.282377	7.975142
5.841374	362.903842	7.980160
5.740125	353.193642	7.985178
5.901717	351.338000	7.990195
5.912659	349.663752	7.995213
5.400671	358.024739	8.000230
5.658080	351.795964	8.005248
5.609817	367.304702	8.010266
5.767055	373.727335	8.015283
6.011222	369.157411	8.020301
5.532780	375.272550	8.025318
5.954920	373.871540	8.030336
6.107305	381.440482	8.035354
5.882772	381.813355	8.040371
6.154857	381.332095	8.045389
5.841831	380.415498	8.050406
5.693888	380.628048	8.055424
5.739015	379.282953	8.060442
5.947066	381.885452	8.065459
5.831220	373.761727	8.070477
5.583769	385.300168	8.075494
5.677657	378.459539	8.080512
5.828567	376.993728	8.085530
5.481926	382.315054	8.090547
5.708203	374.787814	8.095565
5.778239	381.621741	8.100582
5.748402	365.415227	8.105600
6.004574	377.070412	8.110618
6.208403	382.551639	8.115635
6.207568	374.684446	8.120653
5.824688	384.640973	8.125670
5.720400	382.293661	8.130688
5.553126	378.151115	8.135706
5.692649	394.536160	8.140723
6.249934	395.714334	8.145741
5.883488	407.258811	8.150758
6.386236	396.807016	8.155776
6.289047	392.031797	8.160794
5.843417	382.599600	8.165811
5.620601	379.109534	8.170829
5.734863	390.802741	8.175846
5.999599	394.747033	8.180864
5.947045	390.157323	8.185882
5.659978	406.666024	8.190899
6.334259	399.636619	8.195917
6.234477	402.186368	8.200934
5.975874	395.366247	8.205952
6.331921	397.958183	8.210970
5.997899	405.432936	8.215987
5.705354	398.226816	8.221005
6.067685	404.942371	8.226022
5.814341	397.449245	8.231040
6.115803	404.985372	8.236058
5.978339	404.142251	8.241075
5.924951	397.157433	8.246093
5.984083	406.110606	8.251110
6.136897	401.264655	8.256128
6.306817	399.874759	8.261146
6.106355	397.047056	8.266163
6.343241	399.335773	8.271181
6.112687	401.262233	8.276198
5.997092	402.908751	8.281216
6.433791	406.207569	8.286234
6.386567	407.010249	8.291251
6.505550	403.911589	8.296269
6.157201	405.155923	8.301286
5.889722	404.743424	8.306304
6.418857	401.656239	8.311322
6.173446	406.974335	8.316339
6.256816	401.479706	8.321357
6.403571	403.829883	8.326374
6.359129	390.295424	8.331392
6.008574	382.255807	8.336410
5.722273	389.098233	8.341427
6.291655	389.409828	8.346445
6.236759	392.716241	8.351462
6.153858	402.808811	8.356480
6.436901	398.816607	8.361498
6.536398	405.371375	8.366515
6.548014	380.306391	8.371533
6.240736	377.309237	8.376550
6.149551	377.219408	8.381568
6.227752	372.003307	8.386586
6.272406	382.306252	8.391603
6.079806	370.388689	8.396621
5.833849	378.938375	8.401638
6.058909	396.105275	8.406656
6.369932	400.143301	8.411674
6.196135	401.126757	8.416691
6.452742	403.567018	8.421709
6.444086	399.784619	8.426726
6.428051	394.494914	8.431744
6.390427	389.580976	8.436762
6.227474	392.632923	8.441779
6.236418	375.479902	8.446797
5.710840	388.762885	8.451814
5.935560	394.837285	8.456832
6.181646	404.193506	8.461850
6.118369	401.574680	8.466867
6.334764	400.117542	8.471885
6.342195	416.381294	8.476902
6.432673	410.582595	8.481920
6.371865	404.952767	8.486938
6.040226	411.941159	8.491955
6.146309	405.537262	8.496973
5.777786	409.678607	8.501990
5.793587	407.489199	8.507008
6.351244	418.623806	8.512026
6.323507	424.968144	8.517043
6.288905	433.058709	8.522061
6.429442	426.229686	8.527078
6.072684	430.167223	8.532096
6.393811	423.628640	8.537114
5.931006	426.503514	8.542131
6.349576	434.598813	8.547149
6.444090	433.567866	8.552166
6.301260	433.826953	8.557184
6.393032	434.213382	8.562202
6.258192	434.543801	8.567219
6.738675	431.599933	8.572237
6.263064	430.121831	8.577255
6.560231	432.981772	8.582272
6.455478	438.624974	8.587290
6.351996	431.666927	8.592307
6.609172	429.973024	8.597325
6.774756	433.831875	8.602343
6.441093	435.023417	8.607360
6.859759	429.018657	8.612378
6.576446	436.731628	8.617395
6.519256	426.219227	8.622413
6.927669	430.447126	8.627431
6.705470	431.072097	8.632448
6.819195	429.072469	8.637466
6.456230	425.733740	8.642483
6.548444	417.104029	8.647501
6.396361	415.322775	8.652519
6.393190	424.326743	8.657536
6.715466	432.399260	8.662554
6.613426	434.113084	8.667571
6.684302	421.292677	8.672589
6.512492	413.594266	8.677607
6.407004	425.202007	8.682624
6.604554	427.405373	8.687642
6.403512	437.080975	8.692659
6.824910	435.241422	8.697677
6.864927	428.065233	8.702695
6.166466	432.488652	8.707712
6.379580	420.898804	8.712730
6.585941	432.233628	8.717747
6.752596	429.026509	8.722765
6.871217	422.800521	8.727783
6.351584	434.245941	8.732800
6.487422	430.182122	8.737818
6.695916	429.117537	8.742835
6.689684	429.049110	8.747853
6.651499	433.817196	8.752871
6.804563	437.674854	8.757888
6.867050	429.431644	8.762906
6.864690	430.179959	8.767923
6.695155	416.646146	8.772941
6.477544	413.445590	8.777959
6.887953	427.591799	8.782976
6.685470	415.751494	8.787994
6.601350	419.292862	8.793011
6.890164	419.383333	8.798029
6.630008	411.386343	8.803047
6.462879	419.150530	8.808064
6.775077	421.484254	8.813082
6.801067	428.665924	8.818099
6.695148	435.142435	8.823117
6.446839	429.775506	8.828135
6.178387	430.881091	8.833152
6.748366	434.922732	8.838170
6.695292	433.728717	8.843187
6.858938	435.899527	8.848205
6.841946	431.881744	8.853223
6.913580	437.876003	8.858240
7.071081	438.211109	8.863258
7.006279	437.785788	8.868275
7.085651	440.717724	8.873293
7.232277	435.408833	8.878311
6.829460	419.746701	8.883328
6.886984	412.656137	8.888346
6.683857	409.806760	8.893363
6.669472	409.777480	8.898381
6.727018	410.560588	8.903399
6.605620	415.464783	8.908416
7.109256	421.646968	8.913434
6.906609	422.546584	8.918451
6.575847	415.153942	8.923469
6.929786	428.384356	8.928487
6.421895	435.394061	8.933504
6.780614	433.501213	8.938522
6.749373	435.510055	8.943539
6.888112	437.627964	8.948557
7.240310	428.875462	8.953575
6.721625	435.855300	8.958592
7.162039	428.944577	8.963610
6.804384	435.315365	8.968627
6.717720	438.809800	8.973645
6.601287	432.926748	8.978663
6.722780	438.720693	8.983680
6.781001	432.374778	8.988698
6.953983	435.348850	8.993715
6.666494	436.002985	8.998733
6.831132	429.984378	9.003751
6.611588	438.353229	9.008768
6.540776	431.115510	9.013786
6.878128	439.425507	9.018803
6.674757	453.544831	9.023821
7.045154	454.619748	9.028839
7.143294	460.035508	9.033856
7.018349	461.973829	9.038874
7.193807	457.641865	9.043891
7.035817	451.408715	9.048909
6.725331	445.196304	9.053927
6.685602	459.687621	9.058944
6.884574	458.406777	9.063962
7.035932	469.743931	9.068979
7.207740	472.068100	9.073997
6.940685	469.307625	9.079015
7.010991	473.891466	9.084032
7.066438	460.252941	9.089050
6.744062	461.341731	9.094067
6.589111	457.806303	9.099085
6.998631	451.045579	9.104103
7.210754	461.985045	9.109120
7.160437	454.848246	9.114138
7.080611	456.650109	9.119155
6.862803	460.692113	9.124173
6.990017	469.382187	9.129191
6.785731	462.215860	9.134208
6.948994	471.787064	9.139226
6.781589	458.915601	9.144243
7.131036	469.789375	9.149261
7.076040	474.149853	9.154279
7.102439	489.716426	9.159296
7.300082	489.382526	9.164314
7.106631	486.869290	9.169331
7.445578	491.777117	9.174349
7.003423	473.249327	9.179367
6.985589	479.263930	9.184384
6.930068	483.820152	9.189402
7.544889	491.064222	9.194419
7.133941	482.888855	9.199437
7.600773	476.646159	9.204455
7.135296	478.439023	9.209472
7.393849	468.429389	9.214490
7.227455	465.091411	9.219507
7.411297	466.463801	9.224525
7.304703	460.806416	9.229543
7.091239	460.224507	9.234560
7.257287	463.370083	9.239578
7.041211	461.807133	9.244595
7.327181	460.310687	9.249613
7.383390	460.772117	9.254631
7.017071	467.349400	9.259648
7.270539	470.077339	9.264666
7.276726	464.859871	9.269683
7.114569	480.228762	9.274701
7.511425	479.750041	9.279719
7.479356	483.415810	9.284736
7.223563	474.395631	9.289754
7.424611	460.188341	9.294771
7.114851	468.145310	9.299789
7.499650	469.524084	9.304807
6.932571	467.997194	9.309824
7.192428	483.198980	9.314842
7.214419	476.764052	9.319859
7.228376	486.822559	9.324877
7.496954	475.810964	9.329895
7.323518	488.698021	9.334912
7.427821	497.625227	9.339930
7.324745	487.072643	9.344947
7.566185	489.887676	9.349965
7.636691	483.369405	9.354983
7.603066	486.508401	9.360000
7.549908	482.912837	9.365018
7.440802	474.147384	9.370035
7.148004	472.366082	9.375053
7.403000	481.881892	9.380071
7.670140	487.656188	9.385088
7.452433	476.727097	9.390106
7.820589	478.648119	9.395123
7.541869	478.243691	9.400141
7.474619	464.308809	9.405159
7.138269	456.746613	9.410176
7.367671	478.072242	9.415194
7.509398	476.569993	9.420211
7.503213	491.387439	9.425229
7.708973	487.019162	9.430247
7.701463	467.889947	9.435264
7.494349	461.670801	9.440282
7.407740	465.480811	9.445299
7.313560	468.383140	9.450317
7.445730	477.435357	9.455335
7.358677	484.060408	9.460352
7.356580	484.067072	9.465370
7.682312	478.594407	9.470387
7.498965	487.333149	9.475405
7.986514	479.894315	9.480423
7.892400	480.309871	9.485440
7.520685	473.065632	9.490458
7.341448	469.732822	9.495475
7.546571	476.697097	9.500493
7.714296	477.557620	9.505511
7.544918	474.838643	9.510528
7.651225	483.396300	9.515546
7.736087	480.697447	9.520563
7.673822	479.479624	9.525581
7.493585	467.231857	9.530599
7.447893	482.733980	9.535616
7.377191	484.692207	9.540634
7.742089	479.005122	9.545651
7.487009	495.950704	9.550669
7.593842	489.332065	9.555687
7.435797	493.266882	9.560704
7.446110	492.208099	9.565722
7.673346	484.481848	9.570739
7.484771	485.057371	9.575757
7.596269	483.231655	9.580775
7.826645	486.559659	9.585792
7.290824	489.499632	9.590810
7.793195	486.445028	9.595827
7.416893	490.300433	9.600845
7.778580	477.980372	9.605863
7.621967	485.686136	9.610880
7.468496	488.604070	9.615898
7.494740	490.998386	9.620915
8.044381	503.620682	9.625933
8.062155	500.269621	9.630951
7.943412	500.932033	9.635968
7.624723	491.647145	9.640986
7.789437	492.754292	9.646003
7.527149	490.302334	9.651021
7.458856	497.716555	9.656039
8.046368	503.939275	9.661056
7.993909	513.926153	9.666074
7.951063	499.981108	9.671091
7.765397	501.158932	9.676109
7.897064	485.962106	9.681127
7.785223	492.297554	9.686144
7.495029	491.724511	9.691162
8.071115	506.034172	9.696179
7.789289	518.259737	9.701197
8.167378	512.728364	9.706215
8.124208	504.353352	9.711232
7.708186	497.333796	9.716250
7.621803	488.492193	9.721267
7.696689	493.548691	9.726285
7.848766	500.666454	9.731303
8.070741	505.387484	9.736320
8.077432	517.993876	9.741338
8.584264	518.006007	9.746355
7.680892	502.280219	9.751373
7.819680	488.464513	9.756391
7.964270	492.153098	9.761408
7.924438	494.008659	9.766426
7.260620	491.843675	9.771443
7.483371	503.999639	9.776461
8.017449	512.222042	9.781479
7.786410	512.974633	9.786496
7.950634	512.065302	9.791514
8.195712	514.239142	9.796531
7.882625	513.653906	9.801549
7.845820	522.937748	9.806567
8.246392	521.666338	9.811584
7.707711	522.192576	9.816602
7.897376	516.198421	9.821619
8.361402	515.144286	9.826637
7.721181	510.299485	9.831655
8.072978	512.623861	9.836672
8.046649	522.357341	9.841690
8.049793	509.313953	9.846707
8.026081	509.961475	9.851725
8.018409	519.834042	9.856743
8.073349	512.989996	9.861760
7.992970	510.332808	9.866778
8.156591	509.559271	9.871795
7.945560	515.023490	9.876813
8.064051	509.914645	9.881831
7.662585	510.592953	9.886848
8.108596	534.226313	9.891866
8.348734	544.568150	9.896883
7.999816	537.528596	9.901901
8.046235	540.875966	9.906919
7.990262	546.978619	9.911936
7.827865	549.127944	9.916954
8.204569	550.435409	9.921971
8.034702	557.038749	9.926989
8.081892	542.580946	9.932007
8.701533	539.552141	9.937024
8.166362	543.328308	9.942042
8.397391	544.923684	9.947059
8.320679	540.924701	9.952077
8.658586	541.067440	9.957095
8.730198	543.896468	9.962112
8.133044	539.161675	9.967130
8.272418	534.021149	9.972147
8.211552	542.204241	9.977165
8.219364	541.224742	9.982183
8.443065	540.782617	9.987200
8.179907	535.361178	9.992218
8.150799	525.614334	9.997235
8.475890	537.050542	10.002253
8.102792	543.912937	10.007271
8.076935	540.931622	10.012288
8.173256	539.499598	10.017306
8.268824	539.573011	10.022323
8.427548	539.390375	10.027341
8.415426	536.119731	10.032359
8.414265	531.045406	10.037376
8.217082	547.764215	10.042394
8.154464	543.614700	10.047411
8.415808	545.359961	10.052429
8.628653	531.958652	10.057447
8.918112	538.256487	10.062464
8.375217	544.211369	10.067482
8.459363	541.875537	10.072499
8.318867	537.034481	10.077517
8.299881	542.355009	10.082535
8.902071	538.489494	10.087552
8.340720	539.622043	10.092570
8.253576	539.793512	10.097587
8.514436	545.931728	10.102605
8.316355	547.540691	10.107623
8.725361	546.308983	10.112640
8.300362	545.684475	10.117658
8.607147	541.085762	10.122675
8.715175	548.983618	10.127693
8.103018	548.360033	10.132711
8.637783	536.378887	10.137728
8.528748	545.020807	10.142746
8.522974	539.540103	10.147763
8.312398	540.242152	10.152781
8.416911	545.540175	10.157799
8.657569	538.578657	10.162816
8.611164	540.952805	10.167834
8.483502	538.479747	10.172851
8.295294	542.599182	10.177869
7.961503	544.043215	10.182887
7.972424	534.492066	10.187904
8.398583	538.546797	10.192922
8.528918	545.920449	10.197939
8.703869	563.578200	10.202957
8.513420	569.184378	10.207975
8.670933	564.788927	10.212992
8.650669	567.742807	10.218010
9.010135	563.293624	10.223027
8.485579	548.833880	10.228045
8.485641	550.301344	10.233063
8.955518	551.887700	10.238080
8.595292	557.829745	10.243098
8.411046	553.812893	10.248115
8.873411	563.573967	10.253133
8.920317	565.305492	10.258151
9.175908	544.531822	10.263168
8.534577	550.246508	10.268186
8.196242	543.227385	10.273203
8.612684	553.876118	10.278221
8.495424	568.906691	10.283239
9.047169	571.764636	10.288256
8.852673	573.051147	10.293274
8.897549	570.068211	10.298291
9.013080	566.815430	10.303309
8.577595	561.692383	10.308327
8.705727	561.486138	10.313344
8.938307	576.887938	10.318362
8.964160	564.225961	10.323379
8.947689	558.737460	10.328397
8.416119	550.388458	10.333415
8.966423	559.337332	10.338432
8.645266	569.965945	10.343450
8.808347	571.130157	10.348467
8.850027	570.473554	10.353485
8.569350	574.834703	10.358503
8.975915	573.350911	10.363520
9.149977	581.443562	10.368538
8.906630	580.058444	10.373555
8.861808	567.281306	10.378573
8.583329	576.877598	10.383591
8.714657	572.631415	10.388608
8.637197	575.266054	10.393626
8.845368	572.497374	10.398643
8.589271	565.578966	10.403661
8.420987	571.585615	10.408679
8.658286	569.844321	10.413696
8.636919	579.712755	10.418714
8.486947	584.192282	10.423731
8.611447	588.038669	10.428749
8.584447	593.549816	10.433767
8.838521	592.074137	10.438784
8.749736	599.166562	10.443802
8.876173	598.925868	10.448819
9.045095	600.177530	10.453837
8.923924	606.552351	10.458855
9.064179	601.146579	10.463872
8.776839	605.565583	10.468890
8.802246	596.362427	10.473907
8.924233	600.742543	10.478925
9.122490	602.178957	10.483943
9.232101	599.207965	10.488960
9.061053	588.912124	10.493978
9.237629	599.039889	10.498995
9.399674	594.785733	10.504013
8.833776	597.733591	10.509031
9.163517	600.941906	10.514048
9.378318	599.254628	10.519066
9.054410	598.904614	10.524083
9.316288	589.740150	10.529101
9.275584	601.044364	10.534119
9.532565	596.750086	10.539136
8.903484	601.292063	10.544154
8.928247	602.152900	10.549171
9.096307	596.354608	10.554189
8.853599	603.963459	10.559207
9.004568	597.675537	10.564224
9.136418	611.007156	10.569242
9.104879	620.460638	10.574259
9.401751	619.211781	10.579277
9.484475	619.504958	10.584295
9.296327	602.745519	10.589312
9.483207	606.604226	10.594330
9.442017	595.338135	10.599347
9.560246	599.529490	10.604365
8.948794	602.626498	10.609383
9.212994	600.161461	10.614400
9.212994	596.188315	10.619418
9.192802	594.503142	10.624435
8.976596	599.188712	10.629453
9.289828	621.504927	10.634471
9.383938	621.285077	10.639488
9.316403	619.048741	10.644506
9.050566	629.255308	10.649523
9.255642	623.047263	10.654541
9.398437	622.194933	10.659559
9.630668	620.104133	10.664576
9.495114	623.568394	10.669594
9.105403	617.639736	10.674611
9.566551	621.919379	10.679629
9.321055	621.620196	10.684647
9.889669	617.924028	10.689664
9.530475	619.873822	10.694682
9.413085	622.322219	10.699699
9.722498	614.396843	10.704717
9.337242	608.331791	10.709735
9.446448	603.173881	10.714752
9.445623	600.636759	10.719770
9.416647	600.896944	10.724787
9.466265	593.782301	10.729805
8.919107	599.699999	10.734823
9.146505	610.911720	10.739840
9.338047	618.717626	10.744858
9.653320	623.682847	10.749875
9.492931	616.250804	10.754893
9.542809	622.100210	10.759911
9.389879	623.291849	10.764928
9.898368	622.350663	10.769946
9.832379	626.223748	10.774963
9.709623	614.793699	10.779981
9.598822	617.976368	10.784999
9.481146	619.285559	10.790016
9.555931	621.120019	10.795034
9.609715	626.432326	10.800051
9.832660	624.510239	10.805069
9.937934	623.363985	10.810087
9.830913	612.780387	10.815104
9.331743	612.820752	10.820122
9.691735	624.870088	10.825139
9.988209	625.274942	10.830157
9.643678	612.450057	10.835175
9.629382	608.390785	10.840192
9.606672	614.096928	10.845210
9.690172	616.905169	10.850227
9.682211	616.227940	10.855245
9.353399	631.036090	10.860263
9.484659	632.707068	10.865280
9.319064	626.055323	10.870298
9.470156	634.505050	10.875315
9.792682	627.319231	10.880333
9.516476	626.589356	10.885351
9.555896	632.591884	10.890368
9.920271	618.541916	10.895386
9.940970	625.178539	10.900403
9.933069	622.453174	10.905421
9.845599	619.210099	10.910439
9.874268	622.317267	10.915456
10.107840	619.901208	10.920474
10.115800	622.052253	10.925491
10.179696	619.126290	10.930509
10.002877	617.159541	10.935527
10.005230	620.677933	10.940544
10.122984	620.684754	10.945562
9.890627	617.218227	10.950579
10.100104	606.919559	10.955597
9.481452	599.158536	10.960615
9.171593	605.168443	10.965632
9.425498	614.302642	10.970650
9.581249	616.215934	10.975667
9.759493	608.670875	10.980685
9.606646	615.902733	10.985703
9.549046	614.343341	10.990720
9.837810	632.734412	10.995738
9.570240	647.476176	11.000755
9.862291	653.729464	11.005773
10.016167	657.467121	11.010791
10.090446	651.538337	11.015808
10.258981	649.287099	11.020826
10.092745	649.909620	11.025843
10.345191	653.833804	11.030861
10.157977	651.467891	11.035879
9.618260	649.131963	11.040896
10.066699	648.654623	11.045914
10.078939	644.815250	11.050931
10.003212	643.981378	11.055949
10.200283	647.150529	11.060967
10.476092	658.708146	11.065984
10.430812	642.781513	11.071002
9.736705	637.399162	11.076019
10.120707	629.683000	11.081037
10.232538	635.327043	11.086055
9.994055	629.131689	11.091072
10.152849	635.876067	11.096090
9.934430	642.629057	11.101107
9.994268	642.897418	11.106125
10.133581	645.371869	11.111143
10.013086	647.823912	11.116160
10.134796	650.190668	11.121178
9.942544	650.410164	11.126195
10.309798	650.721877	11.131213
10.593934	656.326307	11.136231
10.372348	654.218245	11.141248
10.356096	652.788072	11.146266
10.275609	659.333263	11.151283
10.222787	649.072512	11.156301
10.483043	654.712241	11.161319
10.392570	654.691726	11.166336
10.538025	645.094193	11.171354
10.115619	636.065323	11.176371
10.165198	628.600376	11.181389
10.492068	649.112516	11.186407
10.184854	650.684938	11.191424
10.515163	651.905005	11.196442
10.203861	641.962470	11.201459
10.276206	650.389829	11.206477
10.422336	655.280574	11.211495
10.273696	654.312959	11.216512
10.373471	658.172702	11.221530
10.426215	655.507258	11.226547
10.397242	648.057767	11.231565
10.314412	657.790705	11.236583
10.179468	660.677362	11.241600
10.231661	659.754019	11.246618
10.116942	656.862347	11.251635
10.384970	662.579756	11.256653
10.342570	653.734336	11.261671
10.449208	657.993793	11.266688
10.426952	654.017810	11.271706
10.516019	662.814941	11.276723
10.215310	657.796982	11.281741
10.453720	666.037381	11.286759
10.299618	667.001986	11.291776
10.282004	662.302590	11.296794
10.162439	668.674025	11.301811
10.143626	675.146442	11.306829
10.193603	679.298017	11.311847
10.303435	687.656403	11.316864
10.400168	693.536361	11.321882
10.368593	689.148417	11.326899
10.494937	692.735759	11.331917
10.558344	689.289149	11.336935
10.367273	695.065878	11.341952
10.633778	680.930209	11.346970
10.420250	686.035107	11.351987
10.824465	683.478692	11.357005
10.662071	687.332182	11.362023
10.227939	691.909908	11.367040
10.645863	690.399080	11.372058
10.634304	688.355938	11.377075
10.725552	694.505002	11.382093
10.471207	691.139736	11.387111
10.791421	703.135397	11.392128
11.188572	707.005362	11.397146
10.950746	703.561765	11.402163
10.570730	687.652826	11.407181
10.748441	688.666429	11.412199
10.536931	690.589936	11.417216
10.973512	685.582681	11.422234
10.548884	688.057135	11.427251
10.787455	685.703400	11.432269
10.908541	691.459621	11.437287
10.577475	682.735155	11.442304
10.883789	690.854472	11.447322
10.852879	697.338260	11.452339
10.830687	702.220677	11.457357
10.711852	707.345458	11.462375
11.129888	717.384964	11.467392
11.093384	700.383921	11.472410
10.764305	702.881276	11.477427
10.575607	689.141974	11.482445
10.940953	697.337252	11.487463
10.885782	699.908456	11.492480
11.013438	712.855797	11.497498
10.840618	717.228483	11.502515
11.237407	715.828263	11.507533
10.920492	696.349648	11.512551
10.739580	705.135451	11.517568
11.059933	704.226895	11.522586
11.048234	710.597224	11.527603
10.867118	703.525001	11.532621
11.378981	699.910293	11.537639
10.904447	702.461996	11.542656
11.009860	686.915660	11.547674
11.033666	701.889528	11.552691
10.740874	707.145707	11.557709
10.900060	703.475802	11.562727
11.188063	708.199165	11.567744
11.295653	707.986670	11.572762
11.102830	711.488323	11.577779
11.106611	714.719329	11.582797
11.116522	703.552461	11.587815
11.150681	717.297101	11.592832
11.297056	705.862695	11.597850
11.131967	708.255460	11.602867
11.302888	708.294976	11.607885
11.066148	690.694149	11.612903
11.017119	691.894759	11.617920
10.876112	694.706631	11.622938
10.969134	708.006536	11.627955
11.077476	710.785654	11.632973
11.141597	706.341685	11.637991
11.047839	713.103572	11.643008
10.867171	717.120878	11.648026
10.946330	711.705711	11.653043
10.766661	711.156368	11.658061
10.771318	708.356438	11.663079
10.769178	724.928086	11.668096
11.205712	726.437632	11.673114
11.394261	725.893712	11.678131
11.241042	734.081894	11.683149
11.548740	727.879824	11.688167
11.492193	733.629176	11.693184
11.470892	734.588757	11.698202
11.327382	733.418359	11.703219
11.504901	732.462753	11.708237
11.313949	741.849757	11.713255
11.578708	733.350651	11.718272
11.640887	724.015434	11.723290
11.462410	726.858428	11.728307
11.302908	721.288146	11.733325
11.363304	720.439255	11.738343
11.375535	731.384960	11.743360
11.700682	727.524943	11.748378
11.400455	716.829542	11.753395
11.458110	722.321154	11.758413
11.595533	720.014821	11.763431
11.181513	719.249730	11.768448
11.377668	725.537004	11.773466
11.636912	728.068416	11.778483
11.290915	732.723862	11.783501
11.589090	728.659787	11.788519
11.468563	738.023131	11.793536
11.766818	736.796140	11.798554
11.884201	728.556815	11.803571
11.453689	731.025885	11.808589
11.422850	720.458689	11.813607
11.670873	725.311398	11.818624
11.666402	729.853372	11.823642
11.716662	739.003763	11.828659
12.014367	735.454161	11.833677
11.826403	712.540706	11.838695
11.521088	703.461898	11.843712
11.312332	708.222068	11.848730
11.797448	704.384330	11.853747
11.730316	719.318812	11.858765
11.819034	708.912772	11.863783
11.842937	704.430924	11.868800
12.001483	701.827792	11.873818
11.507373	700.724953	11.878835
11.495526	709.746203	11.883853
11.515082	706.682005	11.888871
11.755342	717.860219	11.893888
11.943454	720.544788	11.898906
11.588095	711.820958	11.903923
11.289558	731.774770	11.908941
11.919094	722.461113	11.913959
11.991507	726.258886	11.918976
11.928576	726.369757	11.923994
12.170584	737.049087	11.929011
11.691391	722.162368	11.934029
12.002677	717.774345	11.939047
11.587320	721.392919	11.944064
12.010216	733.060084	11.949082
12.057252	733.677594	11.954099
11.294415	728.343854	11.959117
11.843802	729.728419	11.964135
11.885453	733.625688	11.969152
11.777832	736.009453	11.974170
11.740100	732.379864	11.979187
11.821467	747.161712	11.984205
11.934242	735.511643	11.989223
11.710599	739.226416	11.994240
11.763550	739.357000	11.999258
11.787124	733.609705	12.004275
11.523077	736.163148	12.009293
11.934991	739.402795	12.014311
11.956710	751.489439	12.019328
12.057796	765.570772	12.024346
11.945112	762.457855	12.029363
12.196969	772.059521	12.034381
12.476025	765.571588	12.039399
12.114007	751.758407	12.044416
11.790701	747.198404	12.049434
12.139558	760.767536	12.054451
12.181805	770.108549	12.059469
12.322647	762.465144	12.064487
12.257777	757.893048	12.069504
12.084906	746.527571	12.074522
12.201790	743.138845	12.079539
12.086177	759.579980	12.084557
12.187886	755.723408	12.089575
12.143038	760.331677	12.094592
12.097261	763.160197	12.099610
12.134223	765.735910	12.104627
11.929743	773.285193	12.109645
12.271603	760.399993	12.114663
12.244256	767.460767	12.119680
12.052596	760.715226	12.124698
12.412124	757.865998	12.129715
12.497345	768.579380	12.134733
12.420800	759.104932	12.139751
12.501806	758.344330	12.144768
12.413136	757.925896	12.149786
12.531196	769.094887	12.154803
12.472511	761.997146	12.159821
12.417743	760.121713	12.164839
12.396494	754.128967	12.169856
12.248355	753.868176	12.174874
12.464899	755.977088	12.179891
12.522014	773.464158	12.184909
12.364609	759.202341	12.189927
12.232656	756.745703	12.194944
12.391930	765.957924	12.199962
12.455580	759.030367	12.204979
12.296128	770.908723	12.209997
12.168018	771.465313	12.215015
12.541323	771.239587	12.220032
12.521142	767.821838	12.225050
12.662077	763.201716	12.230067
12.353092	774.942555	12.235085
12.448446	761.537393	12.240103
12.729010	760.811795	12.245120
12.533631	762.571834	12.250138
12.564451	764.375327	12.255155
12.141934	765.189487	12.260173
12.399680	767.721139	12.265191
12.414922	769.006360	12.270208
12.282765	764.602597	12.275226
12.575165	768.025080	12.280243
12.388367	769.531307	12.285261
12.521763	773.783444	12.290279
12.847050	782.489973	12.295296
12.668713	782.483225	12.300314
13.078111	786.906718	12.305331
12.544413	776.156343	12.310349
12.561827	772.025793	12.315367
12.482419	770.204713	12.320384
12.907856	794.343421	12.325402
13.065584	791.238624	12.330419
12.511521	781.838983	12.335437
12.521007	786.287265	12.340455
12.749984	791.783613	12.345472
12.801069	788.585071	12.350490
12.524194	790.679778	12.355507
12.524881	800.314500	12.360525
12.661527	790.790854	12.365543
12.812349	797.858438	12.370560
12.474478	796.103099	12.375578
12.553759	797.293080	12.380595
12.558055	797.570146	12.385613
12.328412	786.958319	12.390631
12.403090	805.701852	12.395648
12.432998	820.031070	12.400666
12.954032	815.203054	12.405683
12.635856	821.356350	12.410701
13.025923	824.204955	12.415719
12.844879	826.830613	12.420736
12.821303	822.068992	12.425754
12.861663	818.275668	12.430771
13.076024	821.328530	12.435789
13.115450	819.403618	12.440807
13.184833	815.564722	12.445824
12.750293	827.795490	12.450842
13.274257	815.610720	12.455859
12.875398	811.911463	12.460877
12.870430	817.873670	12.465895
12.907516	819.559420	12.470912
12.667498	843.180756	12.475930
12.808946	838.819315	12.480947
12.778537	854.571834	12.485965
13.053679	848.851358	12.490983
13.206869	847.760700	12.496000
12.874905	856.447167	12.501018
13.013101	845.963867	12.506035
13.020015	854.701379	12.511053
13.160624	847.525041	12.516071
13.325998	845.394197	12.521088
13.444784	850.828932	12.526106
13.519636	846.111844	12.531123
13.432357	846.548428	12.536141
13.168985	840.899707	12.541159
13.253506	851.086220	12.546176
13.169581	860.226139	12.551194
13.398886	855.008313	12.556211
13.399327	859.142445	12.561229
13.261113	860.644223	12.566247
13.644399	856.727732	12.571264
13.710695	857.777737	12.576282
13.517676	852.461978	12.581299
13.510088	844.403130	12.586317
13.653863	846.946339	12.591335
13.752682	846.088266	12.596352
13.756883	857.470814	12.601370
13.649638	841.765155	12.606387
13.456782	833.555456	12.611405
13.213297	828.152936	12.616423
13.401020	822.203165	12.621440
13.410974	843.266964	12.626458
13.503789	833.655486	12.631475
13.512940	851.402617	12.636493
13.526878	844.807869	12.641511
13.291098	844.756472	12.646528
13.614496	854.460583	12.651546
13.304278	847.263362	12.656563
13.585129	849.387456	12.661581
13.502050	842.710079	12.666599
13.707465	841.825837	12.671616
13.300946	847.664774	12.676634
13.455323	847.410233	12.681651
13.543815	848.800748	12.686669
13.477692	853.153594	12.691687
13.593015	840.688846	12.696704
13.050433	853.697121	12.701722
13.664329	848.706222	12.706739
13.548031	842.545298	12.711757
13.373873	855.795656	12.716775
13.912484	863.976487	12.721792
13.773966	873.576255	12.726810
14.157522	867.194991	12.731827
13.751456	868.915465	12.736845
13.500733	855.731718	12.741863
13.761902	860.838028	12.746880
13.938696	870.754471	12.751898
14.034377	857.551160	12.756915
13.515331	853.018644	12.761933
13.614422	863.815118	12.766951
14.013054	868.587463	12.771968
13.814131	881.286288	12.776986
14.057860	889.598542	12.782003
14.280623	881.200621	12.787021
14.038274	864.963834	12.792039
14.086471	856.413393	12.797056
13.702282	860.607789	12.802074
13.891978	841.081197	12.807091
14.082675	853.583254	12.812109
14.016615	858.239054	12.817127
14.034190	854.430358	12.822144
14.093942	853.158676	12.827162
13.723619	854.450664	12.832179
13.919088	854.410594	12.837197
13.829053	863.355809	12.842215
14.104704	867.749784	12.847232
14.400769	877.546555	12.852250
13.864905	861.917503	12.857267
14.344330	860.485390	12.862285
13.884464	862.151176	12.867303
14.368584	871.662854	12.872320
13.756893	866.002427	12.877338
14.039284	866.977549	12.882355
14.092415	886.226325	12.887373
13.913913	886.973854	12.892391
14.161570	879.297883	12.897408
14.027306	883.386853	12.902426
14.223800	881.298467	12.907443
14.201438	875.391062	12.912461
14.007498	879.621927	12.917479
14.223800	873.017554	12.922496
13.953019	882.183605	12.927514
14.026765	880.534181	12.932531
13.929081	882.733368	12.937549
13.831983	886.112757	12.942567
14.187282	901.789105	12.947584
14.199135	904.286719	12.952602
14.311083	905.421095	12.957619
14.352322	909.075465	12.962637
14.141745	907.625224	12.967655
14.033058	900.582601	12.972672
13.937909	906.486383	12.977690
14.344645	912.601870	12.982707
14.396465	907.721113	12.987725
14.232144	908.144523	12.992743
14.186423	907.220729	12.997760
14.486300	907.252665	13.002778
14.378465	908.137448	13.007795
14.589936	909.054255	13.012813
14.490798	917.158306	13.017831
14.742231	907.922732	13.022848
14.511544	907.526546	13.027866
14.872673	913.898493	13.032883
14.873190	910.389109	13.037901
15.022377	914.739794	13.042919
14.724915	909.847489	13.047936
14.640440	912.808331	13.052954
14.797421	912.483951	13.057971
14.968890	902.232095	13.062989
14.587783	917.168598	13.068007
14.697256	902.066416	13.073024
14.926170	907.266159	13.078042
14.605774	908.218961	13.083059
14.613096	907.794952	13.088077
15.098910	908.570942	13.093095
14.690492	908.997883	13.098112
14.767406	907.862367	13.103130
14.676559	914.150493	13.108147
14.926048	906.448976	13.113165
14.963141	911.117030	13.118183
14.704859	901.061900	13.123200
14.535916	897.888345	13.128218
14.791321	903.181767	13.133235
14.913716	903.115276	13.138253
14.492030	903.326541	13.143271
14.537022	904.395666	13.148288
14.720952	908.816646	13.153306
14.999001	904.992375	13.158323
14.813570	907.612420	13.163341
14.711130	909.907032	13.168359
15.124474	905.162140	13.173376
14.892645	902.342427	13.178394
14.867291	910.980879	13.183411
14.694423	903.455995	13.188429
14.807108	907.613577	13.193447
15.266535	916.646301	13.198464
15.032014	914.713807	13.203482
15.029898	910.693585	13.208499
15.087394	905.802472	13.213517
14.794254	905.321395	13.218535
15.241637	921.964808	13.223552
14.789409	925.472432	13.228570
14.992042	930.155580	13.233587
15.060628	924.915578	13.238605
15.210810	931.768717	13.243623
15.366550	929.219641	13.248640
15.289042	923.595422	13.253658
15.235454	925.137596	13.258675
15.300318	909.149286	13.263693
15.206488	927.395475	13.268711
15.046526	923.381047	13.273728
14.732880	929.025574	13.278746
15.093045	924.699272	13.283763
15.277045	920.204909	13.288781
15.221748	927.734039	13.293799
14.945562	926.518143	13.298816
14.889152	917.438097	13.303834
14.801364	928.737272	13.308851
15.247330	926.382570	13.313869
15.143527	932.470756	13.318887
15.114576	937.815054	13.323904
15.343442	946.107572	13.328922
15.240602	952.195614	13.333939
14.980536	947.205920	13.338957
15.012723	956.977806	13.343975
15.210075	944.613744	13.348992
15.459679	957.018280	13.354010
15.384828	953.356591	13.359027
15.541177	945.309881	13.364045
15.502568	950.065547	13.369063
15.961194	950.003181	13.374080
16.012556	942.613565	13.379098
15.596039	945.752672	13.384115
15.609196	944.788093	13.389133
15.584020	949.645798	13.394151
15.079383	943.681388	13.399168
15.227678	949.386091	13.404186
15.648472	956.285204	13.409203
15.886380	949.276620	13.414221
15.865848	952.337906	13.419239
15.423893	950.276959	13.424256
15.707411	950.500811	13.429274
15.556809	959.439784	13.434291
15.746174	958.128851	13.439309
15.847594	965.339946	13.444327
15.599893	962.585828	13.449344
15.746687	960.593584	13.454362
15.991983	976.476585	13.459379
15.644240	954.859675	13.464397
15.937252	969.053111	13.469415
15.565061	962.515664	13.474432
16.033444	964.556740	13.479450
15.496319	980.546557	13.484467
15.987063	975.533892	13.489485
15.783839	977.566586	13.494503
16.066155	978.910964	13.499520
16.179802	978.577594	13.504538
15.945901	988.457462	13.509555
16.123830	973.634835	13.514573
16.106083	965.561744	13.519591
15.694791	951.614114	13.524608
15.877707	959.348936	13.529626
15.992238	970.089405	13.534643
16.028489	971.090475	13.539661
16.197890	971.398480	13.544679
16.071470	973.065681	13.549696
16.012293	968.663058	13.554714
16.342886	976.185396	13.559731
16.071891	974.643628	13.564749
16.182268	967.793878	13.569767
15.899997	962.908646	13.574784
16.270097	968.250391	13.579802
16.121132	979.480286	13.584819
16.027267	974.467699	13.589837
16.286456	980.972410	13.594855
16.131031	985.645400	13.599872
16.526228	978.249235	13.604890
16.274666	983.644205	13.609907
16.177380	973.058868	13.614925
15.993999	972.005157	13.619943
16.239590	979.809065	13.624960
16.218935	986.326066	13.629978
16.278062	993.155624	13.634995
16.434313	983.594089	13.640013
16.602788	977.833479	13.645031
16.085317	988.114392	13.650048
16.434701	985.878959	13.655066
15.912272	987.671326	13.660083
16.422863	978.707542	13.665101
16.304860	989.011075	13.670119
16.016254	986.307545	13.675136
16.369432	983.973685	13.680154
16.235959	985.834501	13.685171
16.231796	978.630300	13.690189
16.083308	983.769273	13.695207
16.430423	996.559355	13.700224
16.742282	1007.092199	13.705242
16.712257	1014.156646	13.710259
16.714711	1011.268649	13.715277
16.879542	1007.875516	13.720295
17.037348	992.207094	13.725312
16.666693	987.300989	13.730330
16.180559	989.056111	13.735347
16.460649	973.879798	13.740365
16.448550	987.682387	13.745383
16.824563	1002.604478	13.750400
16.878239	1001.074955	13.755418
16.693829	999.936195	13.760435
16.867756	993.120662	13.765453
16.527373	982.033752	13.770471
16.622312	993.219128	13.775488
16.664814	1000.553080	13.780506
16.578697	1014.073789	13.785523
16.431039	1008.776123	13.790541
16.778747	1011.176948	13.795559
16.609452	1008.489435	13.800576
16.882589	1005.079333	13.805594
16.687660	1018.771733	13.810611
16.643265	1006.849460	13.815629
16.825893	1002.535177	13.820647
16.800698	1015.134291	13.825664
16.687999	1004.983707	13.830682
16.859447	1015.538556	13.835699
16.666752	1008.925629	13.840717
17.065992	1005.003451	13.845735
16.930270	1011.576360	13.850752
17.397647	1013.494520	13.855770
16.833948	1017.562439	13.860787
16.853245	1014.589750	13.865805
17.112803	1019.074649	13.870823
16.792886	1032.975997	13.875840
17.200373	1027.540850	13.880858
17.075974	1027.733939	13.885875
17.009924	1033.866739	13.890893
17.135450	1032.461659	13.895911
17.189722	1037.445800	13.900928
17.437637	1028.832425	13.905946
17.462202	1039.296690	13.910963
17.025537	1033.498330	13.915981
16.966140	1026.110254	13.920999
17.150470	1037.224846	13.926016
17.557021	1033.238398	13.931034
17.496055	1033.481510	13.936051
16.997476	1030.801405	13.941069
17.534290	1022.048091	13.946087
17.410915	1039.882447	13.951104
17.486186	1031.119391	13.956122
17.489514	1033.545773	13.961139
17.300539	1030.621493	13.966157
17.278992	1034.427741	13.971175
17.375332	1033.822519	13.976192
17.526963	1029.863390	13.981210
17.627391	1032.426041	13.986227
17.489747	1040.059641	13.991245
17.308006	1028.660660	13.996263
17.263414	1031.899302	14.001280
17.588389	1021.983098	14.006298
17.500815	1020.652435	14.011315
17.520388	1024.404900	14.016333
17.550609	1028.262997	14.021351
17.586082	1032.748295	14.026368
17.629249	1029.976996	14.031386
17.571502	1033.842566	14.036403
17.370648	1023.642665	14.041421
17.562270	1027.024182	14.046439
17.343357	1037.318306	14.051456
17.444199	1033.916258	14.056474
17.442850	1036.280256	14.061491
17.391874	1018.470114	14.066509
17.756715	1021.922322	14.071527
17.199956	1028.160409	14.076544
17.694307	1040.340457	14.081562
17.365458	1050.058505	14.086579
17.563716	1053.009786	14.091597
17.677516	1051.085819	14.096615
17.484365	1053.303141	14.101632
17.887075	1053.789194	14.106650
17.763349	1055.844155	14.111667
17.263755	1062.256338	14.116685
17.971384	1058.812864	14.121703
17.921565	1059.663318	14.126720
18.112166	1058.667774	14.131738
17.867413	1058.999645	14.136755
17.372745	1061.336796	14.141773
17.901244	1073.495737	14.146791
17.855223	1080.449104	14.151808
18.346718	1079.725160	14.156826
18.184310	1084.661210	14.161843
18.276742	1084.596257	14.166861
18.235554	1075.463252	14.171879
17.975477	1069.630900	14.176896
18.065770	1070.632975	14.181914
18.012043	1082.510751	14.186931
17.855506	1090.901593	14.191949
18.343531	1084.062058	14.196967
18.168341	1082.246486	14.201984
18.714358	1079.920271	14.207002
18.203771	1074.711009	14.212019
18.129292	1070.304445	14.217037
18.112602	1068.034839	14.222055
18.337193	1075.466527	14.227072
18.275293	1071.585028	14.232090
18.381674	1077.867556	14.237107
18.247064	1082.426854	14.242125
18.664431	1077.144783	14.247143
18.438310	1074.456696	14.252160
18.277885	1063.442528	14.257178
18.426172	1061.036617	14.262195
18.318443	1073.260529	14.267213
18.579144	1071.398753	14.272231
18.153236	1072.974028	14.277248
18.697199	1070.263116	14.282266
18.688247	1079.486077	14.287283
18.349307	1071.927180	14.292301
18.839070	1066.750538	14.297319
18.329035	1063.216974	14.302336
18.424212	1061.087635	14.307354
18.562275	1076.132279	14.312371
18.499829	1075.697106	14.317389
18.841097	1073.434531	14.322407
18.304574	1077.719119	14.327424
18.644082	1085.612502	14.332442
18.381284	1079.228291	14.337459
18.319838	1078.291173	14.342477
18.165526	1073.243846	14.347495
18.797503	1074.287286	14.352512
18.645251	1071.540287	14.357530
18.530123	1075.875618	14.362547
18.473458	1079.289735	14.367565
18.968660	1074.790756	14.372583
18.505819	1079.603458	14.377600
18.896638	1079.475975	14.382618
18.909566	1079.824278	14.387635
18.969753	1069.125845	14.392653
18.911341	1070.896012	14.397671
18.800449	1073.393946	14.402688
18.914758	1068.743203	14.407706
18.971566	1072.294178	14.412723
18.856828	1079.914739	14.417741
18.692078	1074.982660	14.422759
18.554068	1084.844400	14.427776
18.932216	1094.435919	14.432794
19.340144	1098.187514	14.437811
18.963157	1098.445427	14.442829
19.076428	1096.086024	14.447847
19.207681	1101.850252	14.452864
19.234369	1105.926677	14.457882
19.220840	1091.771444	14.462899
19.130766	1096.080763	14.467917
19.267389	1097.526875	14.472935
19.059799	1099.083725	14.477952
19.415584	1087.265960	14.482970
19.274890	1095.218807	14.487987
18.944005	1099.584793	14.493005
19.428706	1091.265658	14.498023
19.451386	1100.789796	14.503040
19.235846	1098.983700	14.508058
19.043172	1101.099964	14.513075
19.160734	1105.566107	14.518093
19.376433	1092.902414	14.523111
19.184221	1096.233627	14.528128
19.355600	1103.506401	14.533146
19.695941	1102.458991	14.538163
19.239138	1099.257917	14.543181
19.254116	1093.795884	14.548199
18.946544	1104.615193	14.553216
19.121126	1110.189593	14.558234
19.411922	1105.927767	14.563251
19.247054	1102.513688	14.568269
19.164752	1087.640220	14.573287
19.421212	1102.609529	14.578304
19.285417	1103.331440	14.583322
19.458492	1115.773324	14.588339
19.765048	1121.513248	14.593357
19.771877	1124.642861	14.598375
19.513528	1129.047983	14.603392
19.478831	1123.196080	14.608410
19.984799	1121.144387	14.613427
19.813385	1131.677283	14.618445
19.593342	1119.612036	14.623463
19.819731	1126.235552	14.628480
19.888948	1123.374947	14.633498
19.798956	1123.881393	14.638515
19.840212	1121.081976	14.643533
19.869338	1119.426898	14.648551
19.955038	1109.926844	14.653568
19.482681	1100.804575	14.658586
19.972835	1106.837629	14.663603
19.753846	1119.845889	14.668621
20.073594	1120.177680	14.673639
19.726851	1128.005030	14.678656
19.661728	1130.997590	14.683674
19.494761	1121.294114	14.688691
19.599587	1131.114676	14.693709
19.903960	1119.175553	14.698727
19.606664	1120.358284	14.703744
19.802514	1125.134068	14.708762
20.031108	1117.287407	14.713779
19.390844	1125.290138	14.718797
20.036373	1138.191361	14.723815
20.100104	1152.938437	14.728832
20.299783	1153.052347	14.733850
20.172236	1152.901936	14.738867
20.291932	1152.674916	14.743885
20.237073	1149.265683	14.748903
20.114731	1148.334947	14.753920
20.147453	1154.685850	14.758938
20.447889	1152.761033	14.763955
20.070074	1155.742628	14.768973
20.068726	1154.679321	14.773991
20.368695	1148.124856	14.779008
20.222418	1147.551332	14.784026
20.583725	1150.164647	14.789043
20.153707	1161.022111	14.794061
20.491588	1151.842296	14.799079
20.582611	1149.246523	14.804096
20.380638	1160.541643	14.809114
20.251223	1151.927368	14.814131
20.152329	1152.473080	14.819149
20.136203	1154.211382	14.824167
20.225546	1156.902025	14.829184
20.538464	1159.336724	14.834202
20.703117	1150.313444	14.839219
20.233306	1149.367720	14.844237
20.372733	1148.203458	14.849255
20.430663	1147.370713	14.854272
20.292514	1148.304441	14.859290
20.594134	1167.984817	14.864307
20.437976	1178.398581	14.869325
20.892308	1175.818467	14.874343
20.912387	1172.353306	14.879360
20.582416	1180.023411	14.884378
20.880076	1177.445752	14.889395
20.776774	1183.811666	14.894413
20.861566	1179.124492	14.899431
20.996548	1166.946781	14.904448
20.885091	1179.774129	14.909466
20.945716	1174.623667	14.914483
20.545746	1173.755364	14.919501
20.608952	1173.499323	14.924519
20.875286	1172.362515	14.929536
20.812701	1171.775877	14.934554
21.283378	1169.682370	14.939571
21.106395	1170.590624	14.944589
20.717824	1169.824680	14.949607
20.708253	1177.286788	14.954624
20.862843	1179.828350	14.959642
20.738552	1173.807425	14.964659
20.453771	1178.210389	14.969677
20.409117	1177.504172	14.974695
20.873587	1177.977396	14.979712
21.187687	1201.165232	14.984730
21.355834	1197.569566	14.989747
21.461044	1204.698109	14.994765
21.407180	1201.222436	14.999783
21.680568	1192.829062	15.004800
20.826223	1172.670400	15.009818
21.237283	1162.888958	15.014835
21.414082	1169.599157	15.019853
21.305944	1157.169201	15.024871
21.450751	1166.648992	15.029888
21.389854	1166.967837	15.034906
21.399317	1160.121202	15.039923
21.408595	1165.415395	15.044941
21.257978	1168.383486	15.049959
21.697051	1165.932000	15.054976
20.779682	1162.238168	15.059994
21.381745	1178.179063	15.065011
21.207578	1187.153401	15.070029
21.275854	1195.594277	15.075047
21.723567	1199.620536	15.080064
21.233593	1196.402550	15.085082
21.367572	1202.712358	15.090099
21.564357	1202.624743	15.095117
21.651721	1201.355022	15.100135
21.401271	1204.297734	15.105152
21.506678	1209.961901	15.110170
21.507640	1200.853786	15.115187
21.744662	1203.764303	15.120205
21.421636	1202.893411	15.125223
21.564938	1195.265215	15.130240
21.221862	1204.531123	15.135258
21.399477	1215.814142	15.140275
21.511744	1219.103984	15.145293
21.715642	1234.113198	15.150311
21.784111	1222.476066	15.155328
21.641228	1235.873288	15.160346
21.533335	1221.455016	15.165363
21.584726	1232.202380	15.170381
21.605603	1239.555597	15.175399
21.719615	1229.722827	15.180416
21.475836	1240.084082	15.185434
21.800324	1254.698864	15.190451
22.146498	1259.116602	15.195469
22.445902	1255.411992	15.200487
22.439158	1254.867097	15.205504
22.088385	1246.132818	15.210522
21.803491	1236.201593	15.215539
21.996273	1236.417575	15.220557
22.233258	1247.751274	15.225575
22.441340	1247.115913	15.230592
22.234490	1239.694046	15.235610
22.247506	1228.737811	15.240627
22.035724	1225.829695	15.245645
22.277265	1230.191234	15.250663
22.384408	1225.749864	15.255680
22.163981	1227.075198	15.260698
22.175304	1222.929719	15.265715
22.067334	1243.766303	15.270733
22.533226	1251.674674	15.275751
22.521963	1246.043130	15.280768
23.122796	1249.688790	15.285786
22.926876	1226.182609	15.290803
22.662682	1220.653822	15.295821
22.511860	1221.460146	15.300839
22.713515	1213.775460	15.305856
22.306218	1223.486958	15.310874
22.460656	1225.479420	15.315891
22.629209	1225.140599	15.320909
22.283316	1217.560638	15.325927
22.590449	1217.875471	15.330944
22.462814	1222.178082	15.335962
22.517061	1218.653907	15.340979
22.567723	1212.454073	15.345997
22.581519	1223.267284	15.351015
22.621970	1221.007641	15.356032
21.992204	1232.398236	15.361050
22.395463	1237.368780	15.366067
22.914375	1246.256646	15.371085
22.162254	1253.863532	15.376103
22.621654	1245.649280	15.381120
22.301728	1252.273230	15.386138
22.439195	1255.246693	15.391155
22.686953	1259.588329	15.396173
22.746596	1272.881260	15.401191
22.848889	1264.656678	15.406208
22.891439	1276.178656	15.411226
23.431041	1276.008925	15.416243
23.226764	1270.716896	15.421261
23.080268	1260.088604	15.426279
23.062725	1244.756716	15.431296
22.786353	1253.949080	15.436314
22.740927	1264.632735	15.441331
22.832485	1272.741783	15.446349
22.655413	1271.043255	15.451367
22.941945	1270.395602	15.456384
22.892763	1277.245395	15.461402
22.965723	1285.310024	15.466419
22.827729	1279.723573	15.471437
22.761355	1282.861528	15.476455
23.060174	1277.329719	15.481472
23.258920	1295.798696	15.486490
23.037466	1304.954077	15.491507
23.492171	1299.713431	15.496525
23.258849	1296.433122	15.501543
23.410325	1298.785834	15.506560
23.361130	1304.379576	15.511578
23.686474	1304.874602	15.516595
23.200475	1300.545083	15.521613
23.471675	1298.886776	15.526631
23.677132	1291.091004	15.531648
23.176143	1292.128928	15.536666
23.484171	1294.722209	15.541683
23.518687	1295.770908	15.546701
23.461669	1311.445943	15.551719
23.513700	1299.511523	15.556736
23.549239	1298.300411	15.561754
23.600969	1299.169680	15.566771
23.406949	1294.122201	15.571789
23.121094	1299.380621	15.576807
23.432820	1295.005014	15.581824
23.372426	1302.875940	15.586842
23.685537	1302.154691	15.591859
23.816518	1315.105103	15.596877
23.946387	1325.142764	15.601895
23.954124	1321.319730	15.606912
23.677013	1325.140835	15.611930
23.682719	1321.741015	15.616947
23.932278	1313.281888	15.621965
23.689073	1313.499907	15.626983
24.054030	1309.895473	15.632000
24.176063	1316.342897	15.637018
23.710026	1324.312106	15.642035
23.961983	1316.408047	15.647053
23.905597	1313.907933	15.652071
24.213438	1311.312881	15.657088
24.138149	1308.093020	15.662106
24.494903	1310.195810	15.667123
24.183512	1312.371726	15.672141
24.078787	1305.312543	15.677159
24.372924	1308.293026	15.682176
24.359840	1317.646151	15.687194
24.213252	1316.618214	15.692211
24.475183	1311.669712	15.697229
24.137863	1317.116089	15.702247
24.338618	1310.807494	15.707264
24.574934	1308.501371	15.712282
24.258905	1309.036926	15.717299
24.459539	1308.749883	15.722317
24.367776	1310.010881	15.727335
24.696568	1297.834274	15.732352
24.282419	1291.918687	15.737370
24.072493	1307.554558	15.742387
24.469453	1302.657488	15.747405
24.070021	1312.257344	15.752423
24.411155	1304.718031	15.757440
24.265258	1297.384423	15.762458
24.344856	1305.656313	15.767475
24.622574	1299.954226	15.772493
24.417407	1309.924447	15.777511
24.851800	1301.650969	15.782528
24.884783	1293.995833	15.787546
24.520714	1303.069413	15.792563
24.607413	1303.775407	15.797581
24.668273	1308.001166	15.802599
24.695232	1294.843016	15.807616
24.611289	1301.439478	15.812634
24.636167	1296.509186	15.817651
24.609346	1307.010062	15.822669
24.786239	1314.607120	15.827687
24.954251	1317.708357	15.832704
25.185337	1328.004727	15.837722
24.687826	1322.506152	15.842739
24.722383	1321.762272	15.847757
24.822527	1326.613067	15.852775
25.270240	1326.375679	15.857792
25.091249	1333.005980	15.862810
25.166268	1331.387875	15.867827
25.080744	1330.230444	15.872845
25.304401	1335.693079	15.877863
25.168998	1331.557940	15.882880
24.819017	1312.027026	15.887898
24.551670	1324.355016	15.892915
24.957173	1315.644227	15.897933
25.114922	1327.713103	15.902951
25.217653	1330.174446	15.907968
25.162219	1326.626408	15.912986
24.743974	1333.609790	15.918003
25.100603	1319.696194	15.923021
25.116099	1324.970525	15.928039
25.361787	1336.242954	15.933056
25.555827	1347.217356	15.938074
25.192766	1349.350878	15.943091
25.593958	1349.265951	15.948109
25.240824	1361.294969	15.953127
25.610057	1351.071834	15.958144
25.698907	1354.324342	15.963162
25.535706	1359.339490	15.968179
25.510847	1358.636476	15.973197
25.591996	1359.955596	15.978215
25.409153	1352.242729	15.983232
25.689533	1352.350308	15.988250
25.678520	1357.988580	15.993267
25.666909	1350.697029	15.998285
25.580857	1354.661782	16.003303
25.786110	1351.773514	16.008320
25.833809	1348.932025	16.013338
25.809681	1349.551239	16.018355
25.887530	1342.914735	16.023373
25.931031	1350.182399	16.028391
25.957719	1350.623230	16.033408
26.215499	1353.338006	16.038426
26.030801	1355.326812	16.043443
25.960364	1352.888857	16.048461
26.157678	1347.044713	16.053479
26.090371	1346.266296	16.058496
25.891997	1340.291638	16.063514
25.576637	1358.105894	16.068531
25.812614	1347.064158	16.073549
26.167269	1351.016667	16.078567
25.751092	1352.148608	16.083584
26.115414	1347.468088	16.088602
25.558983	1348.719838	16.093619
26.011913	1347.253969	16.098637
25.802629	1350.256529	16.103655
25.749076	1363.280072	16.108672
26.340758	1373.690392	16.113690
26.052339	1387.063190	16.118707
26.431396	1373.676239	16.123725
26.643653	1374.760213	16.128743
26.518025	1375.900283	16.133760
26.393761	1378.592867	16.138778
26.255955	1379.476058	16.143795
26.536677	1372.479538	16.148813
26.269520	1375.434363	16.153831
26.532676	1368.254396	16.158848
26.541900	1375.369643	16.163866
26.416701	1379.933853	16.168883
26.477954	1379.949527	16.173901
26.159090	1388.930857	16.178919
26.141850	1383.265491	16.183936
26.428914	1378.139455	16.188954
26.372030	1373.853143	16.193971
26.511488	1383.337042	16.198989
26.735953	1395.108319	16.204007
26.867073	1389.164073	16.209024
26.962802	1396.212123	16.214042
26.910373	1398.852428	16.219059
27.259322	1390.248299	16.224077
26.931881	1389.412803	16.229095
26.968185	1380.895535	16.234112
27.179710	1384.087800	16.239130
26.776215	1380.184012	16.244147
27.223768	1380.060262	16.249165
26.898493	1380.243801	16.254183
26.555950	1376.652371	16.259200
26.921038	1374.723714	16.264218
26.785576	1398.099013	16.269235
27.211167	1395.668545	16.274253
26.953148	1388.693311	16.279271
26.948710	1389.956411	16.284288
27.080806	1388.480844	16.289306
26.990639	1383.123564	16.294323
27.399848	1390.343412	16.299341
27.747020	1396.424216	16.304359
27.334161	1391.553015	16.309376
27.588309	1377.993118	16.314394
27.593088	1386.292547	16.319411
27.502617	1380.259942	16.324429
27.473288	1380.577000	16.329447
27.338857	1389.904991	16.334464
27.611425	1378.030644	16.339482
27.641169	1382.848302	16.344499
27.544160	1373.408295	16.349517
27.495917	1374.312167	16.354535
27.313035	1378.446738	16.359552
27.592531	1383.323100	16.364570
27.277363	1395.825897	16.369587
27.537803	1393.866295	16.374605
27.625401	1379.934841	16.379623
27.680101	1379.143619	16.384640
27.528345	1381.597503	16.389658
27.379375	1391.107662	16.394675
27.460162	1383.735346	16.399693
27.560274	1384.799020	16.404711
27.511532	1394.407092	16.409728
27.618240	1388.914817	16.414746
27.439989	1403.264491	16.419763
27.292985	1412.266245	16.424781
27.328993	1415.044182	16.429799
27.415893	1414.279472	16.434816
27.907602	1417.241643	16.439834
27.561025	1433.271437	16.444851
27.785909	1446.134644	16.449869
27.858096	1446.757706	16.454887
27.893020	1448.491194	16.459904
28.434783	1440.816243	16.464922
27.952830	1454.484516	16.469939
27.879046	1449.964135	16.474957
28.128948	1439.974253	16.479975
27.856694	1443.485336	16.484992
28.134543	1439.029791	16.490010
28.222345	1440.742370	16.495027
28.094887	1442.116272	16.500045
28.451442	1449.767293	16.505063
28.516454	1464.956261	16.510080
28.593164	1451.824917	16.515098
28.369246	1440.211364	16.520115
28.106493	1449.120813	16.525133
28.334807	1462.829292	16.530151
28.348999	1470.070037	16.535168
28.450239	1467.166489	16.540186
28.611041	1475.918065	16.545203
28.566538	1466.132094	16.550221
28.778757	1466.868923	16.555239
28.499511	1467.026314	16.560256
28.656818	1463.290275	16.565274
28.842396	1465.511426	16.570291
28.676005	1477.328217	16.575309
28.503379	1468.010466	16.580327
28.523146	1474.802192	16.585344
28.829341	1462.884648	16.590362
28.403634	1465.084805	16.595379
28.372714	1473.080584	16.600397
29.118036	1466.891749	16.605415
28.677876	1479.376316	16.610432
29.158260	1473.102751	16.615450
28.883913	1470.737756	16.620467
28.546760	1474.337913	16.625485
28.944909	1483.134361	16.630503
28.897298	1497.757147	16.635520
29.158572	1504.836110	16.640538
29.084338	1507.637646	16.645555
28.915664	1497.691222	16.650573
28.991934	1492.932714	16.655591
28.769345	1501.135270	16.660608
29.415052	1486.990050	16.665626
29.467746	1492.567887	16.670643
29.233812	1495.634297	16.675661
29.414482	1490.120935	16.680679
29.178021	1498.669664	16.685696
29.499465	1499.064316	16.690714
29.163125	1498.040851	16.695731
29.313076	1495.533631	16.700749
29.169061	1491.705934	16.705767
29.143050	1492.451686	16.710784
29.745041	1512.445160	16.715802
29.590569	1518.399465	16.720819
29.561136	1522.352228	16.725837
29.894690	1530.205714	16.730855
29.527772	1519.703327	16.735872
29.233032	1518.739618	16.740890
29.486521	1520.628227	16.745907
29.751371	1516.275691	16.750925
30.010624	1525.687245	16.755943
29.804655	1530.399856	16.760960
29.643129	1517.286855	16.765978
29.819036	1513.595230	16.770995
29.637722	1524.221431	16.776013
29.846484	1514.323164	16.781031
29.986461	1516.352641	16.786048
29.981359	1522.583362	16.791066
29.582032	1525.741966	16.796083
30.056951	1520.558053	16.801101
29.807260	1519.606222	16.806119
29.893575	1521.300106	16.811136
30.069069	1520.575162	16.816154
30.112019	1521.455286	16.821171
30.045634	1529.532390	16.826189
30.255168	1542.278144	16.831207
30.288462	1547.701238	16.836224
30.434563	1543.263154	16.841242
30.316534	1536.906591	16.846259
30.012788	1528.909617	16.851277
30.270909	1541.442619	16.856295
30.467833	1548.585333	16.861312
30.370175	1547.290926	16.866330
30.549382	1548.559980	16.871347
30.159798	1551.707595	16.876365
30.528421	1549.573227	16.881383
30.276933	1555.637424	16.886400
30.122537	1555.876246	16.891418
30.114400	1559.828835	16.896435
29.937908	1554.387194	16.901453
29.835410	1557.423553	16.906471
30.168787	1579.759900	16.911488
30.184150	1580.161483	16.916506
30.616195	1575.754333	16.921523
30.218223	1590.113335	16.926541
30.696315	1568.527245	16.931559
30.713695	1581.164270	16.936576
30.940531	1601.472258	16.941594
31.077725	1600.295694	16.946611
30.906832	1591.788697	16.951629
30.981042	1581.731584	16.956647
30.884428	1600.610091	16.961664
31.250701	1600.180321	16.966682
31.093961	1593.974979	16.971699
30.896825	1603.278189	16.976717
31.024545	1607.777582	16.981735
30.937137	1612.310682	16.986752
31.074981	1608.549257	16.991770
31.318178	1617.755080	16.996787
31.100971	1611.978953	17.001805
31.525982	1610.085067	17.006823
31.438240	1610.575393	17.011840
31.293696	1608.231070	17.016858
31.353279	1600.887235	17.021875
31.396627	1610.818685	17.026893
31.445930	1599.635619	17.031911
31.213196	1605.005732	17.036928
31.432101	1610.355580	17.041946
31.536688	1608.896929	17.046963
31.113341	1605.507472	17.051981
31.230561	1600.613124	17.056999
30.913060	1607.924830	17.062016
30.959061	1603.559222	17.067034
31.484922	1611.865481	17.072051
31.231186	1631.201009	17.077069
31.664708	1632.834190	17.082087
32.016104	1634.764279	17.087104
31.241688	1623.318915	17.092122
31.964657	1625.686277	17.097139
32.102020	1634.873974	17.102157
31.951642	1638.845712	17.107175
32.132717	1632.101404	17.112192
31.506358	1630.192353	17.117210
31.615243	1629.342134	17.122227
31.733558	1634.458426	17.127245
31.661522	1629.435923	17.132263
31.656395	1642.780304	17.137280
31.633404	1646.902508	17.142298
31.942242	1645.976776	17.147315
32.027428	1659.133440	17.152333
32.279432	1651.371248	17.157351
32.305728	1653.024051	17.162368
32.532985	1655.800465	17.167386
32.117090	1649.490532	17.172403
32.307379	1652.143341	17.177421
32.556344	1647.891098	17.182439
32.245911	1653.046168	17.187456
32.381975	1649.849938	17.192474
32.055417	1644.662169	17.197491
32.255667	1649.011344	17.202509
32.181878	1655.628437	17.207527
31.976496	1658.305369	17.212544
32.048445	1664.972218	17.217562
32.345356	1676.129532	17.222579
32.279115	1685.630041	17.227597
32.870701	1671.442661	17.232615
32.686166	1681.656022	17.237632
32.453542	1687.016675	17.242650
32.907458	1682.757560	17.247667
32.566035	1689.104153	17.252685
32.700801	1672.450918	17.257703
32.673326	1678.906118	17.262720
32.599793	1667.458216	17.267738
32.649888	1663.467516	17.272755
32.611892	1686.682744	17.277773
33.234907	1693.118087	17.282791
33.149002	1707.270487	17.287808
32.991125	1706.118056	17.292826
33.275579	1703.236260	17.297843
32.862158	1700.965612	17.302861
33.117902	1704.346680	17.307879
33.298856	1708.547404	17.312896
32.981848	1710.370774	17.317914
33.451379	1702.707030	17.322931
33.114930	1709.377920	17.327949
33.157551	1703.639954	17.332967
33.423788	1699.949918	17.337984
33.257115	1701.191120	17.343002
33.689268	1698.721712	17.348019
33.496403	1713.178072	17.353037
33.536040	1696.713299	17.358055
33.521702	1698.511338	17.363072
33.560554	1711.870973	17.368090
33.715281	1703.884142	17.373107
33.397706	1700.203522	17.378125
33.620932	1699.057656	17.383143
33.550942	1698.932938	17.388160
33.511072	1701.710184	17.393178
34.148585	1701.629259	17.398195
33.508113	1709.739583	17.403213
33.906990	1705.542738	17.408231
33.913555	1695.076411	17.413248
33.689328	1705.687350	17.418266
33.967241	1702.831827	17.423283
33.873543	1701.748241	17.428301
33.774942	1703.834055	17.433319
33.563470	1712.694571	17.438336
33.511168	1711.440386	17.443354
33.659206	1714.049328	17.448371
33.899779	1727.655098	17.453389
33.914637	1733.134789	17.458407
34.060882	1725.417539	17.463424
33.841424	1731.413656	17.468442
34.186368	1731.700484	17.473459
34.150609	1735.673220	17.478477
34.038133	1733.402757	17.483495
34.042128	1739.206066	17.488512
33.941203	1735.450465	17.493530
34.114683	1738.333154	17.498547
33.933900	1748.530185	17.503565
34.347244	1753.717059	17.508583
34.608273	1750.599068	17.513600
34.295174	1758.083726	17.518618
34.491397	1749.301370	17.523635
34.508007	1743.999840	17.528653
34.438028	1747.917976	17.533671
34.662772	1752.086602	17.538688
34.647036	1750.687820	17.543706
34.974164	1741.231662	17.548723
34.817072	1750.708567	17.553741
34.845387	1755.602294	17.558759
34.988191	1741.712407	17.563776
34.792116	1752.738712	17.568794
34.711631	1751.555216	17.573811
34.790691	1751.280904	17.578829
34.649461	1756.216975	17.583847
35.213913	1754.787253	17.588864
34.842796	1762.079018	17.593882
35.215683	1764.062563	17.598899
34.783575	1775.397281	17.603917
34.782002	1779.064849	17.608935
35.042070	1781.507915	17.613952
35.085117	1778.771235	17.618970
35.413674	1778.230598	17.623987
35.378085	1775.013900	17.629005
35.174108	1765.243284	17.634023
35.214519	1775.269965	17.639040
35.011387	1778.577766	17.644058
35.114963	1777.217097	17.649075
35.049326	1778.871692	17.654093
35.233617	1782.611132	17.659111
35.163966	1779.450267	17.664128
35.576184	1803.589253	17.669146
35.904374	1794.795666	17.674163
35.827135	1799.532362	17.679181
36.130997	1803.436121	17.684199
36.054240	1783.877664	17.689216
35.409639	1781.400213	17.694234
35.948377	1782.171110	17.699251
35.932979	1780.096884	17.704269
35.858284	1778.249714	17.709287
35.764472	1768.187262	17.714304
35.817253	1785.152100	17.719322
36.149582	1789.486928	17.724339
36.046630	1791.923752	17.729357
35.870639	1795.315673	17.734375
36.186929	1794.912666	17.739392
36.207918	1800.116843	17.744410
36.260676	1797.864667	17.749427
36.056523	1793.153172	17.754445
36.228484	1795.225010	17.759463
36.168629	1790.238426	17.764480
35.803169	1791.564431	17.769498
36.126499	1790.563833	17.774515
36.114983	1790.571973	17.779533
36.313086	1789.805605	17.784551
36.584777	1795.977273	17.789568
36.537407	1791.064477	17.794586
36.394357	1791.503509	17.799603
36.650420	1795.111777	17.804621
36.304485	1795.487917	17.809639
36.497691	1797.878341	17.814656
36.427378	1798.182892	17.819674
36.455901	1794.741536	17.824691
36.453304	1793.394344	17.829709
36.472581	1798.813399	17.834727
36.492617	1808.278362	17.839744
36.555603	1822.173978	17.844762
36.707602	1826.069976	17.849779
36.716674	1826.213756	17.854797
36.825404	1825.035325	17.859815
36.729270	1821.329453	17.864832
36.804507	1823.350172	17.869850
36.949548	1813.979313	17.874867
36.867567	1817.498530	17.879885
36.753868	1818.097077	17.884903
36.784789	1827.841232	17.889920
36.906360	1848.285922	17.894938
37.024365	1847.393235	17.899955
37.007997	1831.634598	17.904973
37.182526	1854.043516	17.909991
37.156971	1843.815681	17.915008
37.410325	1849.204388	17.920026
37.396598	1844.646094	17.925043
37.576914	1849.916847	17.930061
37.293577	1844.744340	17.935079
37.643100	1844.875807	17.940096
37.510550	1852.139697	17.945114
37.664745	1850.790028	17.950131
37.484753	1842.915544	17.955149
37.362905	1849.111017	17.960167
37.587215	1849.659763	17.965184
37.134478	1850.440829	17.970202
37.247235	1859.190652	17.975219
37.772516	1863.984452	17.980237
37.648415	1874.469341	17.985255
37.874503	1873.389293	17.990272
37.732779	1874.812804	17.995290
37.927938	1868.807870	18.000307
38.153790	1866.272926	18.005325
37.951071	1874.100126	18.010343
37.891146	1870.107682	18.015360
38.070283	1873.456600	18.020378
38.029397	1868.845746	18.025395
38.358894	1872.644512	18.030413
37.983340	1869.960780	18.035431
38.320112	1868.841298	18.040448
38.258805	1875.106196	18.045466
38.022181	1873.041372	18.050483
38.272261	1871.711394	18.055501
38.078116	1875.232415	18.060519
38.571571	1878.825599	18.065536
38.786197	1886.972451	18.070554
38.054882	1878.527876	18.075571
37.968155	1878.696135	18.080589
38.098707	1890.384614	18.085607
38.483489	1892.135919	18.090624
38.577146	1896.489231	18.095642
38.066927	1897.929450	18.100659
38.511703	1894.422857	18.105677
38.421145	1915.737211	18.110695
38.743564	1917.422543	18.115712
38.714183	1928.331314	18.120730
38.831948	1926.851636	18.125747
39.090315	1923.503642	18.130765
38.970010	1932.391010	18.135783
39.168118	1916.636567	18.140800
39.057645	1922.126484	18.145818
38.802653	1918.909420	18.150835
39.101957	1910.104523	18.155853
38.951596	1917.241832	18.160871
39.137382	1919.068502	18.165888
38.875611	1919.134789	18.170906
38.897858	1920.112858	18.175923
38.795616	1930.117791	18.180941
39.386443	1942.961892	18.185959
39.528023	1946.723839	18.190976
39.746360	1946.380361	18.195994
39.369445	1947.269481	18.201011
39.481331	1952.626732	18.206029
39.728998	1946.279004	18.211047
39.610626	1941.879103	18.216064
39.589724	1947.815778	18.221082
39.783087	1942.836818	18.226099
39.675591	1944.728379	18.231117
39.471433	1948.364600	18.236135
39.937179	1940.171133	18.241152
40.054645	1940.575663	18.246170
39.596042	1941.947834	18.251187
40.096562	1937.624549	18.256205
39.686507	1944.218689	18.261223
39.922704	1942.616304	18.266240
40.285783	1944.115375	18.271258
39.888185	1943.344496	18.276275
40.140832	1930.677581	18.281293
39.928361	1946.017737	18.286311
40.059002	1943.403019	18.291328
39.860930	1945.785334	18.296346
40.036725	1944.261847	18.301363
40.136225	1940.358027	18.306381
39.740686	1943.175256	18.311399
40.362680	1937.570519	18.316416
40.377659	1941.740494	18.321434
40.088743	1958.421335	18.326451
40.748467	1959.769779	18.331469
40.469355	1970.540964	18.336487
40.551764	1962.502228	18.341504
40.481092	1962.450204	18.346522
40.486902	1966.549033	18.351539
40.451918	1969.612756	18.356557
40.588384	1972.472877	18.361575
40.601827	1970.081661	18.366592
40.550030	1962.461616	18.371610
40.401943	1962.052463	18.376627
40.473920	1958.825191	18.381645
40.816217	1977.057767	18.386663
40.530456	1985.286221	18.391680
40.997777	1999.847673	18.396698
40.808050	1998.381450	18.401715
41.106456	1987.310605	18.406733
40.948318	1989.664577	18.411751
40.696876	1994.113012	18.416768
41.002450	1992.679649	18.421786
41.126105	1992.909627	18.426803
41.207116	1988.951885	18.431821
41.169340	1994.600861	18.436839
41.395724	2009.632451	18.441856
41.409681	2015.847733	18.446874
41.195827	2018.538669	18.451891
41.789332	2020.045828	18.456909
41.338515	2027.242880	18.461927
41.294316	2025.832755	18.466944
41.379238	2018.762514	18.471962
41.277061	2017.503497	18.476979
41.795496	2016.961508	18.481997
41.532196	2027.998515	18.487015
41.431191	2021.828477	18.492032
41.788584	2022.716168	18.497050
41.506336	2035.902272	18.502067
41.600212	2039.823204	18.507085
41.518362	2048.426871	18.512103
41.801149	2041.625445	18.517120
41.969890	2052.503249	18.522138
41.759290	2055.749149	18.527155
42.033604	2050.697511	18.532173
42.009547	2054.595895	18.537191
42.118693	2046.811730	18.542208
41.830591	2051.799299	18.547226
41.908072	2068.173505	18.552243
42.154816	2073.096216	18.557261
42.181083	2083.374615	18.562279
42.199685	2082.866753	18.567296
42.584371	2076.263962	18.572314
42.008243	2076.357409	18.577331
41.767502	2077.168390	18.582349
41.990639	2081.570894	18.587367
43.009192	2099.053800	18.592384
42.807968	2090.182058	18.597402
42.357887	2085.414336	18.602419
42.977668	2093.242161	18.607437
42.670410	2101.647620	18.612455
42.776295	2103.597291	18.617472
43.189035	2094.831340	18.622490
42.968866	2097.520121	18.627507
43.056950	2082.843213	18.632525
42.888328	2071.911767	18.637543
42.906184	2086.382751	18.642560
43.118758	2088.580815	18.647578
43.079366	2093.182259	18.652595
43.467324	2088.601996	18.657613
43.130716	2100.906652	18.662631
43.390918	2085.767235	18.667648
43.473301	2089.342810	18.672666
43.185494	2090.524115	18.677683
43.435471	2084.488428	18.682701
43.277259	2089.556650	18.687719
43.286567	2097.574808	18.692736
43.484812	2088.832998	18.697754
43.375805	2091.387587	18.702771
43.613533	2083.094069	18.707789
43.772200	2088.863789	18.712807
43.824285	2096.095693	18.717824
43.584340	2087.602435	18.722842
43.384282	2086.030518	18.727859
43.803977	2078.554320	18.732877
43.405589	2091.550361	18.737895
43.327237	2087.806930	18.742912
43.297595	2090.459547	18.747930
43.473206	2103.652866	18.752947
43.456546	2112.662951	18.757965
43.553473	2113.051767	18.762983
43.510082	2122.653077	18.768000
44.084137	2131.823107	18.773018
43.797805	2139.471000	18.778035
44.085041	2143.686736	18.783053
44.218662	2137.258971	18.788071
44.156269	2150.401245	18.793088
44.120472	2144.385064	18.798106
44.071026	2151.112144	18.803123
44.103710	2148.342315	18.808141
44.300997	2152.862506	18.813159
44.352049	2164.301664	18.818176
44.262672	2157.347047	18.823194
44.422634	2172.730038	18.828211
44.883330	2163.101240	18.833229
44.874300	2166.482851	18.838247
44.362863	2160.907294	18.843264
44.855921	2166.823480	18.848282
44.541071	2164.934996	18.853299
44.282581	2165.275348	18.858317
44.324248	2172.366891	18.863335
44.624959	2181.955348	18.868352
44.699648	2182.082538	18.873370
44.806343	2185.840532	18.878387
45.016529	2185.327899	18.883405
45.341990	2190.370865	18.888423
44.775802	2200.751624	18.893440
44.819643	2183.159022	18.898458
45.383658	2201.928341	18.903475
45.035114	2211.984646	18.908493
45.471244	2208.892796	18.913511
45.469764	2211.304311	18.918528
45.800830	2205.994406	18.923546
45.124542	2218.661659	18.928563
45.338698	2220.698531	18.933581
45.585192	2214.786435	18.938599
45.610823	2210.496462	18.943616
45.516103	2211.656990	18.948634
45.515118	2211.581422	18.953651
45.601775	2206.180411	18.958669
45.508025	2209.256538	18.963687
45.432486	2212.727480	18.968704
45.836728	2215.618276	18.973722
45.763691	2219.650613	18.978739
45.848455	2233.663067	18.983757
46.194051	2244.033550	18.988775
46.205999	2241.210146	18.993792
46.090101	2246.196036	18.998810
46.381577	2243.865373	19.003827
45.956692	2238.563436	19.008845
46.215579	2240.189320	19.013863
46.125774	2240.083483	19.018880
46.621255	2242.448700	19.023898
46.518055	2238.734379	19.028915
46.335641	2239.327926	19.033933
46.374142	2235.840737	19.038951
46.269642	2227.023207	19.043968
46.434758	2231.886161	19.048986
46.575864	2238.532920	19.054003
46.559649	2234.451488	19.059021
46.552712	2230.438038	19.064039
46.404999	2240.188312	19.069056
46.844041	2248.830393	19.074074
47.081828	2259.694349	19.079091
46.795607	2264.757427	19.084109
46.974457	2262.917824	19.089127
46.936527	2272.512046	19.094144
47.183108	2261.505963	19.099162
46.802562	2258.927105	19.104179
47.001310	2261.815388	19.109197
46.882544	2257.980414	19.114215
46.992700	2266.806590	19.119232
47.108628	2257.023457	19.124250
47.175023	2268.816918	19.129267
47.198061	2271.211975	19.134285
47.438610	2281.046619	19.139303
47.191353	2288.666361	19.144320
47.390597	2288.638324	19.149338
47.430774	2287.792527	19.154355
47.646712	2290.125802	19.159373
47.622210	2288.917718	19.164391
47.599881	2283.792561	19.169408
47.835080	2286.346901	19.174426
47.791515	2294.796349	19.179443
47.854706	2287.098185	19.184461
47.655874	2282.849676	19.189479
47.337792	2293.194771	19.194496
47.741171	2294.820114	19.199514
47.986250	2311.010477	19.204531
47.770124	2323.795073	19.209549
48.447014	2311.844138	19.214567
48.608208	2317.490447	19.219584
48.625709	2316.831257	19.224602
48.483713	2321.780227	19.229619
48.461641	2309.291802	19.234637
48.491927	2291.410855	19.239655
48.511170	2295.188886	19.244672
48.609854	2284.360611	19.249690
48.666384	2278.853834	19.254707
48.297704	2287.856039	19.259725
48.536642	2287.001194	19.264743
48.225376	2293.343273	19.269760
48.439767	2302.197321	19.274778
49.168238	2308.458560	19.279795
48.582271	2306.786124	19.284813
48.884458	2299.309310	19.289831
48.742975	2302.803226	19.294848
48.921978	2302.159762	19.299866
48.575051	2300.620305	19.304883
48.849574	2306.087892	19.309901
48.954734	2311.421055	19.314919
48.984841	2309.525849	19.319936
48.956309	2307.387341	19.324954
48.995112	2312.289045	19.329971
48.968662	2328.676615	19.334989
49.221103	2326.292092	19.340007
49.328806	2332.319208	19.345024
49.297054	2329.556291	19.350042
49.448359	2326.941436	19.355059
49.334181	2337.475537	19.360077
49.166840	2324.186115	19.365095
49.144592	2330.457675	19.370112
49.526038	2342.135544	19.375130
49.640428	2350.844322	19.380147
49.599837	2362.335838	19.385165
49.699216	2358.681281	19.390183
49.712254	2362.453986	19.395200
49.606099	2358.225656	19.400218
49.749835	2356.192709	19.405235
49.832503	2363.697668	19.410253
49.801510	2363.270159	19.415271
49.769677	2372.443714	19.420288
49.846109	2388.354425	19.425306
50.068921	2387.432667	19.430323
49.976362	2391.332388	19.435341
50.238923	2386.263562	19.440359
49.865441	2384.100188	19.445376
50.076995	2388.782322	19.450394
50.186102	2390.933512	19.455411
50.035359	2410.591445	19.460429
50.444818	2413.768664	19.465447
50.450202	2421.932763	19.470464
50.772396	2417.902421	19.475482
50.563926	2413.229313	19.480499
50.335763	2418.617887	19.485517
50.203863	2420.068306	19.490535
50.740395	2430.046026	19.495552
51.198557	2443.924393	19.500570
51.048521	2449.963526	19.505587
50.597242	2451.192558	19.510605
50.623407	2443.266574	19.515623
50.651140	2452.755920	19.520640
50.392322	2447.954977	19.525658
50.873563	2453.989887	19.530675
50.609943	2471.210094	19.535693
50.705470	2466.912265	19.540711
50.847408	2471.472770	19.545728
51.204109	2486.411750	19.550746
51.280831	2487.614870	19.555763
50.951896	2498.034374	19.560781
51.629806	2501.188485	19.565799
51.434413	2499.044537	19.570816
51.324878	2505.427675	19.575834
51.465851	2498.862915	19.580851
51.216406	2502.714649	19.585869
51.611357	2508.797816	19.590887
51.595990	2522.071862	19.595904
51.555472	2530.205328	19.600922
51.911382	2528.959719	19.605939
51.417435	2531.177006	19.610957
52.060170	2531.262541	19.615975
52.083093	2536.027922	19.620992
52.186959	2534.105356	19.626010
52.498790	2532.825623	19.631027
52.081460	2535.292866	19.636045
52.403314	2542.864578	19.641063
52.621444	2548.315825	19.646080
52.621873	2542.199151	19.651098
52.273362	2530.970526	19.656115
52.101832	2541.466390	19.661133
52.996254	2545.946891	19.666151
52.905888	2549.738993	19.671168
52.460173	2547.536417	19.676186
52.729192	2543.899430	19.681203
52.685669	2561.467134	19.686221
52.702672	2554.312639	19.691239
52.727715	2559.762581	19.696256
52.852452	2553.989385	19.701274
52.733230	2544.637458	19.706291
52.404945	2550.755050	19.711309
52.493398	2551.830090	19.716327
52.708895	2569.827487	19.721344
52.710518	2577.162175	19.726362
53.110262	2569.600529	19.731379
53.158552	2587.425303	19.736397
52.874009	2577.767864	19.741415
53.188426	2593.366883	19.746432
53.220797	2596.363348	19.751450
53.581135	2600.182687	19.756467
53.295089	2602.951299	19.761485
53.510242	2595.304942	19.766503
53.294066	2604.968298	19.771520
53.058505	2612.302288	19.776538
53.820068	2622.629911	19.781555
53.502387	2631.510673	19.786573
53.663345	2628.648081	19.791591
53.427067	2634.845971	19.796608
53.716022	2634.794410	19.801626
54.172422	2634.445183	19.806643
54.179071	2657.417955	19.811661
53.934156	2660.978644	19.816679
54.408644	2665.767995	19.821696
54.371169	2654.541059	19.826714
54.586089	2647.794227	19.831731
54.132572	2659.473719	19.836749
54.362381	2652.487838	19.841767
54.721056	2654.072877	19.846784
54.315777	2657.901717	19.851802
54.564391	2649.912383	19.856819
54.560564	2654.663050	19.861837
54.443934	2646.973969	19.866855
54.502683	2644.095826	19.871872
54.300251	2655.167865	19.876890
54.345752	2664.443075	19.881907
54.320159	2676.762515	19.886925
54.567821	2683.092907	19.891943
54.915055	2675.877156	19.896960
54.549505	2684.162614	19.901978
54.906809	2688.702056	19.906995
54.708061	2705.249523	19.912013
54.895480	2708.335337	19.917031
55.296133	2708.168434	19.922048
55.084049	2718.206795	19.927066
55.294719	2710.327534	19.932083
55.309531	2717.401406	19.937101
55.458080	2725.874611	19.942119
55.633680	2738.471878	19.947136
55.356563	2742.211219	19.952154
55.876045	2739.008379	19.957171
55.433509	2744.563198	19.962189
55.713259	2743.020201	19.967207
56.103625	2737.741881	19.972224
55.761982	2740.594973	19.977242
55.963900	2742.513887	19.982259
55.898539	2742.959706	19.987277
55.955498	2735.527447	19.992295
55.994571	2736.038964	19.997312
55.875233	2738.689948	20.002330
56.029040	2734.291395	20.007347
55.905055	2754.583060	20.012365
55.776882	2765.485722	20.017383
56.078646	2767.868736	20.022400
55.954617	2767.269579	20.027418
56.599963	2764.731909	20.032435
56.122535	2766.640485	20.037453
56.293887	2784.951163	20.042471
56.514427	2787.946584	20.047488
56.508213	2798.754409	20.052506
56.575479	2789.975971	20.057523
56.501387	2793.326863	20.062541
56.375334	2792.494462	20.067559
57.111032	2805.985600	20.072576
56.995211	2816.586518	20.077594
56.585989	2825.506967	20.082611
56.730723	2824.272332	20.087629
57.302083	2817.718931	20.092647
57.307430	2821.461375	20.097664
56.886930	2819.756651	20.102682
57.467202	2812.507491	20.107699
57.193151	2824.026410	20.112717
57.080279	2840.929822	20.117735
57.540571	2845.440543	20.122752
57.373614	2852.132640	20.127770
57.207044	2853.127718	20.132787
57.641607	2851.083868	20.137805
57.380183	2855.758168	20.142823
57.330951	2853.916366	20.147840
57.577169	2872.562587	20.152858
57.571117	2878.336275	20.157875
57.536331	2889.988184	20.162893
57.590294	2879.987175	20.167911
57.810882	2877.964222	20.172928
57.735586	2896.354689	20.177946
58.093343	2913.702052	20.182963
58.117825	2910.213774	20.187981
57.950616	2913.127937	20.192999
58.283767	2915.679646	20.198016
57.807249	2926.678013	20.203034
58.296041	2920.860286	20.208051
58.282227	2931.028668	20.213069
58.680562	2931.657495	20.218087
58.786268	2940.835040	20.223104
58.451859	2938.412977	20.228122
58.280993	2932.584976	20.233139
58.553352	2934.271938	20.238157
58.529638	2957.388722	20.243175
58.864380	2956.761866	20.248192
58.972545	2969.799107	20.253210
58.848126	2956.275246	20.258227
58.934768	2963.334803	20.263245
58.917615	2972.045553	20.268263
59.441980	2961.450020	20.273280
59.103956	2968.610833	20.278298
59.078172	2968.466554	20.283315
59.182670	2974.494388	20.288333
59.263781	2987.049820	20.293351
59.533652	2995.428394	20.298368
59.414312	2998.934756	20.303386
59.704546	2996.345381	20.308403
59.890200	3000.403643	20.313421
59.631271	2999.437396	20.318439
60.099599	2989.816434	20.323456
59.608493	2999.797667	20.328474
59.781295	2998.088344	20.333491
59.978199	2996.772930	20.338509
59.948386	3006.827080	20.343527
59.845555	2997.008384	20.348544
59.658894	3017.628943	20.353562
59.864070	3016.466887	20.358579
59.991707	3018.817249	20.363597
59.966151	3024.638226	20.368615
60.308424	3017.088556	20.373632
59.920300	3034.107868	20.378650
60.169361	3036.158302	20.383667
60.519153	3034.765275	20.388685
60.285025	3036.645227	20.393703
60.268066	3043.039299	20.398720
60.253584	3053.687603	20.403738
60.543476	3070.408189	20.408755
60.604063	3061.289792	20.413773
60.826749	3065.995608	20.418791
61.035231	3059.508444	20.423808
60.734621	3068.689745	20.428826
60.991305	3070.050926	20.433843
61.388904	3083.939277	20.438861
60.967154	3085.570879	20.443879
61.321788	3087.128185	20.448896
61.298328	3095.821045	20.453914
61.402770	3086.121326	20.458931
61.435935	3088.817905	20.463949
61.337004	3097.528903	20.468967
61.530169	3091.063064	20.473984
61.552532	3099.736122	20.479002
61.647497	3107.277339	20.484019
61.561434	3115.942142	20.489037
61.704424	3117.131765	20.494055
62.001554	3113.815355	20.499072
61.811794	3115.154956	20.504090
61.711466	3118.955050	20.509107
62.063740	3119.881477	20.514125
61.780524	3127.238922	20.519143
62.307842	3137.085917	20.524160
62.409520	3145.544570	20.529178
62.108054	3152.579790	20.534195
62.555325	3143.766893	20.539213
62.366368	3150.992798	20.544231
62.611963	3152.059034	20.549248
62.618201	3153.162773	20.554266
62.409838	3155.101825	20.559283
62.313875	3149.956396	20.564301
62.071071	3158.693121	20.569319
62.312638	3164.175602	20.574336
62.477460	3182.929585	20.579354
62.440801	3177.130977	20.584371
62.496114	3189.049870	20.589389
62.560493	3210.025849	20.594407
62.881025	3209.360180	20.599424
62.863380	3214.772820	20.604442
63.246472	3226.640382	20.609459
63.421512	3235.021301	20.614477
63.180898	3243.015998	20.619495
63.310917	3242.960932	20.624512
63.215252	3242.142688	20.629530
63.169478	3240.874747	20.634547
63.732681	3240.612935	20.639565
63.567196	3242.636811	20.644583
63.887889	3250.644569	20.649600
63.543526	3244.565897	20.654618
63.406475	3254.801113	20.659635
63.785648	3260.167376	20.664653
63.794312	3268.192467	20.669671
63.921801	3259.499054	20.674688
64.008613	3269.434077	20.679706
64.006492	3270.128816	20.684723
64.357691	3278.782001	20.689741
63.970776	3294.223225	20.694759
64.456849	3297.085596	20.699776
64.531669	3304.244984	20.704794
64.267787	3302.256859	20.709811
64.204219	3285.623742	20.714829
64.092038	3297.284883	20.719847
64.907823	3311.650770	20.724864
64.947438	3325.424955	20.729882
64.999864	3330.274299	20.734899
65.094633	3327.721816	20.739917
64.907318	3333.157918	20.744935
65.353534	3325.610772	20.749952
64.956049	3329.006118	20.754970
64.815911	3335.138683	20.759987
64.913059	3327.400036	20.765005
65.048713	3329.351489	20.770023
65.321627	3338.297879	20.775040
65.541805	3357.024431	20.780058
65.311251	3362.019122	20.785075
65.629693	3359.548373	20.790093
65.400275	3346.858151	20.795111
66.182625	3354.676842	20.800128
65.930646	3354.138743	20.805146
65.478921	3361.753094	20.810163
65.919468	3359.768222	20.815181
65.631862	3351.275522	20.820199
65.884909	3366.774355	20.825216
65.699495	3386.602907	20.830234
66.096794	3392.547129	20.835251
66.320322	3382.096332	20.840269
65.926573	3385.721512	20.845287
66.177149	3390.965929	20.850304
66.049912	3387.779084	20.855322
66.051967	3406.240012	20.860339
66.105399	3417.000986	20.865357
66.362962	3413.621282	20.870375
66.008954	3421.043594	20.875392
66.372097	3435.786661	20.880410
66.310914	3450.990761	20.885427
66.339897	3449.206083	20.890445
66.060352	3456.916593	20.895463
66.565368	3472.855800	20.900480
66.588820	3487.058743	20.905498
66.285152	3488.207900	20.910515
66.945612	3496.402415	20.915533
66.717682	3501.926995	20.920551
67.160680	3507.889346	20.925568
67.356339	3506.296335	20.930586
67.399254	3529.311875	20.935603
67.519847	3533.986465	20.940621
67.686264	3534.572744	20.945639
67.152211	3532.358634	20.950656
67.281891	3536.413160	20.955674
67.658256	3538.418457	20.960691
68.132930	3522.994887	20.965709
67.762985	3532.739642	20.970727
68.064883	3541.100827	20.975744
68.151676	3544.442432	20.980762
67.988337	3549.230950	20.985779
68.073461	3558.478316	20.990797
68.183880	3550.961594	20.995815
68.326996	3555.976702	21.000832
68.445022	3555.295404	21.005850
68.140850	3567.081488	21.010867
68.320474	3559.238287	21.015885
68.145139	3559.332065	21.020903
68.303127	3582.342269	21.025920
68.231735	3579.001449	21.030938
68.167509	3588.515267	21.035955
69.074294	3600.749226	21.040973
69.065821	3616.503879	21.045991
68.821563	3618.284473	21.051008
69.230911	3610.847146	21.056026
69.105117	3624.252931	21.061043
69.087993	3614.063805	21.066061
69.360377	3612.736521	21.071079
69.316772	3620.186034	21.076096
69.138790	3617.865624	21.081114
69.193575	3619.283732	21.086131
69.202468	3628.779802	21.091149
69.392897	3650.067958	21.096167
69.537306	3645.433932	21.101184
69.426886	3634.511357	21.106202
69.457866	3651.642339	21.111219
69.443664	3664.083764	21.116237
69.891191	3668.495691	21.121255
69.903334	3659.930631	21.126272
70.180216	3671.875098	21.131290
69.830622	3675.376632	21.136307
70.090542	3682.923808	21.141325
69.865866	3694.991060	21.146343
70.158701	3697.722799	21.151360
70.502296	3697.627957	21.156378
70.147923	3704.049876	21.161395
70.182565	3704.865126	21.166413
70.389610	3716.899473	21.171431
70.475420	3725.206220	21.176448
70.482959	3731.842893	21.181466
70.241882	3733.039074	21.186483
70.269041	3749.034455	21.191501
70.726475	3755.900504	21.196519
70.895494	3756.855677	21.201536
71.302189	3764.796532	21.206554
70.776597	3790.382380	21.211571
71.414536	3793.981725	21.216589
71.253103	3793.240043	21.221607
71.409935	3794.591674	21.226624
71.401379	3789.318738	21.231642
71.538245	3797.204035	21.236659
71.408299	3792.578236	21.241677
71.736279	3810.871726	21.246695
71.813254	3821.862823	21.251712
72.019083	3821.988417	21.256730
71.595382	3828.332863	21.261747
71.878714	3826.312603	21.266765
71.771421	3824.334605	21.271783
71.860572	3832.167422	21.276800
72.254699	3843.626488	21.281818
72.546005	3849.849448	21.286835
72.608323	3844.341289	21.291853
72.428554	3850.511800	21.296871
72.389471	3853.412352	21.301888
72.554224	3846.202634	21.306906
72.494835	3849.036926	21.311923
72.474973	3843.039778	21.316941
72.503938	3845.146884	21.321959
72.211568	3865.002184	21.326976
72.747441	3874.923997	21.331994
72.620665	3876.799840	21.337011
72.450865	3875.664916	21.342029
72.900026	3886.670337	21.347047
72.871583	3899.761215	21.352064
72.987656	3910.698893	21.357082
72.955208	3909.106866	21.362099
73.070321	3919.183005	21.367117
73.294439	3931.331606	21.372135
73.286966	3933.952611	21.377152
73.452180	3938.882296	21.382170
73.256415	3946.002265	21.387187
73.376948	3953.587175	21.392205
73.730642	3958.995515	21.397223
73.478712	3966.689288	21.402240
73.856987	3958.047786	21.407258
73.884015	3966.385949	21.412275
74.190404	3983.126889	21.417293
74.200161	3987.897872	21.422311
73.991446	3994.366512	21.427328
74.310302	3992.810973	21.432346
74.613927	4001.165787	21.437363
74.324481	3995.255016	21.442381
74.494569	4004.138935	21.447399
74.597251	4017.670190	21.452416
74.670504	4012.984091	21.457434
74.286219	4032.330009	21.462451
74.385684	4032.598527	21.467469
74.608912	4035.183402	21.472487
74.681529	4050.610084	21.477504
74.954488	4054.572838	21.482522
75.001762	4065.878064	21.487539
75.067240	4056.834155	21.492557
75.177315	4080.199704	21.497575
75.183737	4091.211486	21.502592
75.185075	4076.426610	21.507610
75.309402	4090.983522	21.512627
75.255126	4107.354966	21.517645
75.499118	4115.087891	21.522663
75.294036	4116.429964	21.527680
75.614381	4114.681639	21.532698
75.722052	4136.005426	21.537715
75.877075	4145.049597	21.542733
75.929041	4146.543942	21.547751
75.746845	4150.069842	21.552768
76.388497	4151.629621	21.557786
76.310789	4178.253750	21.562803
76.402189	4171.746657	21.567821
76.546111	4178.160113	21.572839
76.371764	4179.686762	21.577856
77.001871	4179.291359	21.582874
76.869369	4183.194565	21.587891
76.878081	4179.566474	21.592909
76.707383	4181.502889	21.597927
76.677210	4180.282941	21.602944
76.738630	4197.125588	21.607962
76.812610	4207.044196	21.612979
76.428430	4213.325766	21.617997
77.358551	4210.866389	21.623015
77.061122	4209.994487	21.628032
76.845484	4222.597268	21.633050
77.004215	4241.141817	21.638067
76.832087	4241.869542	21.643085
77.163347	4246.987934	21.648103
77.370169	4269.546298	21.653120
77.523610	4263.345098	21.658138
77.625510	4264.740092	21.663155
77.287170	4281.462375	21.668173
77.790737	4290.511983	21.673191
77.891469	4303.450341	21.678208
77.754991	4297.105165	21.683226
77.686697	4311.111643	21.688243
77.811595	4321.104403	21.693261
78.079386	4328.773718	21.698279
77.709572	4336.719694	21.703296
78.153580	4341.571087	21.708314
77.795242	4356.323779	21.713331
78.097786	4366.424460	21.718349
78.562450	4390.340895	21.723367
78.479525	4389.290178	21.728384
78.600402	4389.769987	21.733402
78.690695	4398.751827	21.738419
78.767043	4421.065677	21.743437
79.255374	4416.920486	21.748455
78.884574	4422.338312	21.753472
79.098178	4427.481502	21.758490
79.535578	4433.138859	21.763507
79.560250	4441.695406	21.768525
79.794326	4443.577900	21.773543
79.926793	4451.069610	21.778560
80.147122	4439.769612	21.783578
80.240546	4443.347081	21.788595
80.184813	4444.217557	21.793613
80.342799	4436.210076	21.798631
80.014564	4445.772019	21.803648
80.391354	4439.270621	21.808666
80.371829	4443.516021	21.813683
80.359348	4440.737136	21.818701
80.539883	4445.011166	21.823719
80.204151	4450.726529	21.828736
80.239110	4448.126443	21.833754
80.009577	4455.113016	21.838771
80.235220	4468.511707	21.843789
80.678464	4471.049548	21.848807
80.736427	4482.605878	21.853824
80.747245	4494.889283	21.858842
80.442693	4494.337289	21.863859
80.706892	4510.482435	21.868877
81.137824	4510.241335	21.873895
80.874738	4522.457195	21.878912
81.093932	4536.980662	21.883930
80.795437	4535.016760	21.888947
81.085301	4531.947441	21.893965
81.250525	4549.503302	21.898983
81.200554	4561.329114	21.904000
81.258368	4563.548574	21.909018
81.742276	4578.753440	21.914035
81.921532	4587.086976	21.919053
81.781463	4591.344984	21.924071
81.836929	4597.188492	21.929088
81.998271	4595.105192	21.934106
81.983016	4599.160569	21.939123
81.828420	4622.836584	21.944141
82.293984	4625.276255	21.949159
82.538878	4629.508680	21.954176
82.420805	4630.881349	21.959194
82.385852	4639.860835	21.964211
82.305817	4652.723598	21.969229
82.778703	4658.719527	21.974247
82.564892	4664.229619	21.979264
83.035963	4656.728538	21.984282
82.968237	4658.674122	21.989299
83.205523	4670.846407	21.994317
83.104845	4681.316621	21.999335
83.004118	4683.750327	22.004352
83.037828	4693.928032	22.009370
83.059234	4680.541021	22.014387
82.925399	4693.096588	22.019405
83.111116	4706.280753	22.024423
83.123159	4719.327999	22.029440
83.589268	4724.321233	22.034458
83.456728	4735.784466	22.039475
83.359881	4752.510379	22.044493
83.937912	4739.414901	22.049511
83.675260	4751.397261	22.054528
83.727044	4772.313886	22.059546
84.122183	4777.517117	22.064563
84.097371	4778.632132	22.069581
84.425528	4779.704473	22.074599
84.555916	4806.347421	22.079616
84.523531	4817.469889	22.084634
84.649464	4811.058167	22.089651
84.282131	4811.661826	22.094669
84.575232	4807.269360	22.099687
84.500125	4831.684451	22.104704
84.659547	4841.580549	22.109722
84.889449	4842.403136	22.114739
84.684346	4847.621516	22.119757
84.786489	4862.668630	22.124775
85.127347	4880.304616	22.129792
85.242562	4871.994302	22.134810
85.463433	4880.817033	22.139827
85.450391	4894.790050	22.144845
85.614451	4900.765000	22.149863
85.686234	4910.589639	22.154880
85.300282	4913.099628	22.159898
85.811826	4918.016354	22.164915
85.352975	4925.657721	22.169933
85.819802	4929.656581	22.174951
85.857952	4943.157598	22.179968
85.727855	4952.515150	22.184986
85.874714	4955.209976	22.190003
85.766167	4971.353955	22.195021
86.530717	4977.474750	22.200039
86.564238	4987.816790	22.205056
86.427645	4987.042757	22.210074
86.922872	5002.116784	22.215091
86.840263	5013.057845	22.220109
86.619641	5011.198484	22.225127
86.563504	5022.937176	22.230144
86.874908	5040.180201	22.235162
86.977364	5043.042983	22.240179
86.872655	5057.718623	22.245197
87.097131	5059.766829	22.250215
87.039600	5067.440076	22.255232
87.329474	5080.428267	22.260250
87.576150	5076.829003	22.265267
87.502889	5087.273058	22.270285
87.587704	5096.300292	22.275303
87.830842	5106.843147	22.280320
87.888515	5110.420034	22.285338
87.996766	5121.176583	22.290355
88.188275	5137.131651	22.295373
87.902319	5135.118369	22.300391
88.221146	5147.369740	22.305408
87.826686	5144.619028	22.310426
88.184895	5152.830087	22.315443
88.333373	5173.700456	22.320461
88.141773	5184.021059	22.325479
88.379858	5187.541287	22.330496
88.500816	5193.226364	22.335514
88.858038	5201.914250	22.340531
88.698875	5212.876894	22.345549
88.929676	5212.768155	22.350567
89.016292	5228.471424	22.355584
88.920505	5236.220181	22.360602
89.132617	5238.163019	22.365619
89.129631	5258.574252	22.370637
89.356639	5268.409487	22.375655
89.533526	5275.070695	22.380672
89.418727	5279.949917	22.385690
89.590446	5282.603017	22.390707
89.730336	5301.596682	22.395725
89.765107	5300.448557	22.400743
90.130615	5298.992926	22.405760
90.248761	5308.163405	22.410778
89.988952	5316.581848	22.415795
90.279392	5323.310513	22.420813
90.366234	5326.573522	22.425831
90.406091	5338.590944	22.430848
90.239327	5339.699823	22.435866
90.816452	5359.076445	22.440883
90.911077	5359.405718	22.445901
90.633924	5368.682353	22.450919
90.621504	5368.564370	22.455936
90.892643	5384.563998	22.460954
91.136064	5394.548248	22.465971
91.106152	5399.439454	22.470989
91.278634	5398.001432	22.476007
91.562304	5398.146412	22.481024
91.206105	5415.207132	22.486042
91.288745	5416.384267	22.491059
91.241506	5424.027641	22.496077
91.576928	5440.140356	22.501095
91.822573	5444.609603	22.506112
91.720221	5449.641595	22.511130
91.987651	5464.925313	22.516147
91.970787	5482.046570	22.521165
92.508860	5479.118137	22.526183
92.461891	5479.153930	22.531200
92.213989	5493.514590	22.536218
92.725144	5491.537372	22.541235
92.633001	5507.625591	22.546253
92.657568	5521.962525	22.551271
93.030870	5515.420258	22.556288
92.725727	5520.506138	22.561306
93.024820	5518.072858	22.566323
93.330969	5538.997859	22.571341
93.399399	5548.040510	22.576359
93.236668	5543.220530	22.581376
93.118462	5546.556741	22.586394
93.398303	5539.378833	22.591411
93.376164	5552.488849	22.596429
93.618254	5565.999411	22.601447
93.592759	5562.483731	22.606464
93.400879	5570.569666	22.611482
93.540337	5581.441551	22.616499
93.745496	5598.584952	22.621517
93.895011	5599.833696	22.626535
93.857417	5616.020791	22.631552
93.953853	5626.006099	22.636570
94.150482	5625.953220	22.641587
94.618194	5635.290064	22.646605
94.313934	5654.022228	22.651623
94.285120	5664.210269	22.656640
94.052012	5668.890317	22.661658
94.381677	5676.402142	22.666675
94.638293	5693.837458	22.671693
94.767034	5691.244599	22.676711
94.789741	5701.806550	22.681728
94.863818	5728.248165	22.686746
94.983570	5728.216800	22.691763
94.587177	5740.009260	22.696781
94.936346	5754.762713	22.701799
95.502686	5753.556531	22.706816
95.466322	5772.420463	22.711834
95.637741	5785.320387	22.716851
95.718226	5785.030010	22.721869
95.788532	5781.972786	22.726887
96.216767	5788.266504	22.731904
96.121017	5810.495373	22.736922
96.019411	5816.171320	22.741939
96.524660	5816.392074	22.746957
96.378846	5820.341907	22.751975
96.730412	5824.100174	22.756992
96.766995	5849.948061	22.762010
96.995965	5846.884909	22.767027
96.735389	5847.184609	22.772045
96.931263	5847.791605	22.777063
97.004892	5848.581902	22.782080
96.751442	5871.457427	22.787098
97.006356	5873.889235	22.792115
97.206718	5887.573880	22.797133
97.310267	5890.616558	22.802151
97.417668	5901.373699	22.807168
97.662088	5901.670043	22.812186
97.533736	5914.373955	22.817203
97.622970	5914.786158	22.822221
97.800614	5932.155155	22.827239
97.946174	5940.036861	22.832256
97.853118	5947.668691	22.837274
97.982773	5951.815307	22.842291
98.545267	5970.951802	22.847309
98.316688	5973.844497	22.852327
98.600123	5965.488393	22.857344
98.560591	5974.200926	22.862362
98.539761	5986.834378	22.867379
98.536187	6003.496310	22.872397
98.527242	6003.920741	22.877415
98.964896	6016.870662	22.882432
98.785153	6024.866506	22.887450
98.671122	6035.263823	22.892467
99.215628	6044.345775	22.897485
99.022718	6060.475519	22.902503
99.134421	6059.416310	22.907520
99.097668	6068.352583	22.912538
99.425316	6081.843809	22.917555
99.929063	6085.515152	22.922573
99.720219	6099.466099	22.927591
100.069584	6100.358419	22.932608
99.573956	6120.888833	22.937626
99.907241	6119.040436	22.942643
100.113110	6126.855951	22.947661
99.888574	6153.348120	22.952679
100.363509	6148.911064	22.957696
100.358756	6159.152432	22.962714
100.731449	6168.633864	22.967731
100.529198	6186.100502	22.972749
100.844095	6181.417028	22.977767
100.760216	6200.667658	22.982784
100.868439	6216.422054	22.987802
101.050723	6208.886669	22.992819
101.177951	6213.396756	22.997837
100.653350	6226.775382	23.002855
101.315017	6234.724724	23.007872
101.090147	6245.609888	23.012890
101.322522	6250.520208	23.017907
101.711404	6273.664942	23.022925
101.598924	6277.956899	23.027943
102.203980	6271.946281	23.032960
101.975595	6291.143883	23.037978
101.731687	6296.422418	23.042995
101.835756	6306.782562	23.048013
102.134805	6310.460767	23.053031
102.394482	6325.007724	23.058048
102.407041	6331.028977	23.063066
102.157482	6336.901889	23.068083
102.332377	6350.786592	23.073101
102.546242	6362.528034	23.078119
102.890217	6365.646769	23.083136
102.902914	6384.026963	23.088154
102.995463	6386.594767	23.093171
103.532211	6382.738297	23.098189
103.436361	6391.456695	23.103207
103.396418	6403.771431	23.108224
103.533733	6411.664102	23.113242
103.785371	6418.096196	23.118259
103.987242	6418.929563	23.123277
104.032475	6425.340331	23.128295
104.425247	6442.000545	23.133312
104.133132	6443.691044	23.138330
103.997822	6445.890481	23.143347
104.424966	6447.553528	23.148365
104.504506	6454.940706	23.153383
104.191252	6470.429886	23.158400
104.425706	6479.541690	23.163418
104.456057	6480.815478	23.168435
104.654829	6496.840044	23.173453
104.554381	6515.607446	23.178471
105.044593	6509.974624	23.183488
104.707435	6530.231275	23.188506
105.190242	6529.988345	23.193523
105.435530	6537.775762	23.198541
105.537620	6553.812368	23.203559
105.605800	6560.794134	23.208576
105.545135	6572.585036	23.213594
105.758800	6576.813337	23.218611
105.949856	6579.151069	23.223629
105.872318	6603.060645	23.228647
106.265061	6598.803673	23.233664
105.962947	6611.491093	23.238682
105.534872	6628.144335	23.243699
106.041949	6638.678290	23.248717
105.968744	6653.280818	23.253735
106.442304	6667.254713	23.258752
106.665686	6674.963542	23.263770
106.717041	6685.404766	23.268787
106.926665	6697.503814	23.273805
106.924129	6709.733973	23.278823
106.868577	6705.730310	23.283840
106.871003	6714.676543	23.288858
106.855051	6729.115474	23.293875
107.297996	6734.305465	23.298893
107.286710	6751.616444	23.303911
107.879261	6765.085611	23.308928
107.784284	6767.341905	23.313946
107.610021	6782.133996	23.318963
108.094306	6783.447178	23.323981
107.781674	6797.894762	23.328999
108.020950	6801.866551	23.334016
107.865834	6820.548122	23.339034
107.948577	6827.101528	23.344051
108.451403	6844.010044	23.349069
108.390930	6852.631567	23.354087
108.344409	6852.405269	23.359104
108.506727	6862.118906	23.364122
108.589504	6884.450534	23.369139
108.992192	6874.231702	23.374157
108.952625	6894.145379	23.379175
108.969871	6901.072117	23.384192
108.913737	6905.083897	23.389210
108.902870	6915.134072	23.394227
109.356730	6928.909211	23.399245
109.369145	6942.715639	23.404263
109.707810	6963.545620	23.409280
110.061466	6962.959874	23.414298
109.600954	6967.167613	23.419315
110.283324	6980.670221	23.424333
109.821202	6990.024003	23.429351
110.132020	6993.744699	23.434368
110.826681	7006.007886	23.439386
110.862579	7025.524736	23.444403
111.294027	7023.319923	23.449421
110.829966	7024.128217	23.454439
110.808589	7027.146459	23.459456
110.889634	7029.602506	23.464474
111.162583	7045.467552	23.469491
111.562357	7047.299104	23.474509
111.263435	7064.292394	23.479527
111.425231	7068.844629	23.484544
111.473247	7079.545469	23.489562
111.285501	7087.034758	23.494579
111.491996	7100.905606	23.499597
111.873513	7112.056169	23.504615
112.058442	7125.804137	23.509632
111.937421	7139.887330	23.514650
112.136812	7144.840941	23.519667
111.810833	7151.063877	23.524685
111.970402	7162.855378	23.529703
112.272293	7179.511559	23.534720
112.831492	7205.112152	23.539738
112.562083	7216.611002	23.544755
112.759905	7217.637616	23.549773
113.016995	7231.604815	23.554791
113.008421	7237.711756	23.559808
113.146409	7251.552410	23.564826
113.106321	7264.155028	23.569843
113.417909	7274.697879	23.574861
112.999540	7284.325924	23.579879
113.513423	7298.420262	23.584896
113.392231	7317.340108	23.589914
113.649645	7332.162875	23.594931
113.961994	7339.258218	23.599949
113.917908	7349.790538	23.604967
113.811501	7359.483399	23.609984
114.468212	7363.734023	23.615002
114.537510	7378.980923	23.620019
114.506689	7390.821340	23.625037
114.485719	7401.163806	23.630055
114.638222	7413.385926	23.635072
114.719281	7426.525305	23.640090
114.574860	7434.513067	23.645107
114.844001	7448.797400	23.650125
114.865643	7456.999087	23.655143
115.129739	7470.239259	23.660160
115.469823	7483.969499	23.665178
115.334061	7493.480766	23.670195
115.588971	7501.538588	23.675213
115.867832	7518.441772	23.680231
115.467854	7527.252552	23.685248
116.045452	7535.559750	23.690266
115.811078	7549.787295	23.695283
116.232511	7556.499418	23.700301
116.057911	7562.957651	23.705319
116.522710	7580.160092	23.710336
116.612827	7588.887803	23.715354
116.579472	7597.874798	23.720371
116.660656	7610.979562	23.725389
117.024717	7628.797666	23.730407
116.644534	7634.842991	23.735424
117.055416	7644.461271	23.740442
116.856228	7658.765470	23.745459
117.283147	7678.707934	23.750477
117.547230	7679.989385	23.755495
117.422270	7693.805268	23.760512
117.679976	7705.913231	23.765530
117.836095	7722.687452	23.770547
117.881685	7727.965236	23.775565
118.328590	7735.993080	23.780583
118.444305	7757.771277	23.785600
118.554908	7758.293830	23.790618
118.586447	7756.126330	23.795635
118.817728	7766.909352	23.800653
118.815128	7779.054988	23.805671
118.856140	7786.205642	23.810688
119.193794	7783.181972	23.815706
119.530962	7811.110219	23.820723
119.306495	7810.012024	23.825741
119.454877	7824.703887	23.830759
118.974795	7832.457115	23.835776
119.860252	7836.659384	23.840794
119.700266	7851.143857	23.845811
119.604987	7847.995423	23.850829
120.025827	7869.618607	23.855847
119.980694	7875.605204	23.860864
120.134634	7875.540068	23.865882
119.866658	7894.859192	23.870899
120.203438	7908.148275	23.875917
120.317283	7917.608025	23.880935
120.163908	7935.359109	23.885952
120.542825	7951.745038	23.890970
120.758678	7968.333326	23.895987
120.940531	7963.626050	23.901005
120.897240	7975.351982	23.906023
120.940066	7995.579117	23.911040
121.058124	8007.320834	23.916058
121.162975	8031.557278	23.921075
121.391115	8030.855410	23.926093
121.822081	8042.298715	23.931111
121.700690	8067.173657	23.936128
122.011226	8074.282197	23.941146
122.514038	8090.866680	23.946163
122.220313	8094.006692	23.951181
122.617260	8099.396862	23.956199
122.470030	8117.702810	23.961216
122.633492	8127.293807	23.966234
122.671066	8132.544548	23.971251
122.584170	8137.467508	23.976269
122.818408	8146.416002	23.981287
123.042213	8158.456959	23.986304
123.419760	8175.667311	23.991322
123.422712	8186.773649	23.996339
123.380601	8187.787395	24.001357
123.715323	8203.277532	24.006375
123.647039	8209.523591	24.011392
124.064256	8217.209013	24.016410
124.080199	8223.318752	24.021427
124.219147	8238.899577	24.026445
124.394183	8238.408079	24.031463
124.341108	8261.135196	24.036480
124.572843	8247.681067	24.041498
124.707724	8261.330378	24.046515
124.650463	8276.152689	24.051533
124.656362	8277.083146	24.056551
124.899369	8284.988476	24.061568
125.201773	8296.805680	24.066586
125.161387	8319.423538	24.071603
125.389404	8317.477762	24.076621
125.299150	8320.121833	24.081639
125.300527	8339.730722	24.086656
125.587810	8342.817636	24.091674
125.826486	8364.312081	24.096691
126.103325	8369.658004	24.101709
126.017741	8370.883786	24.106727
125.881044	8389.961857	24.111744
126.074788	8391.248064	24.116762
126.201980	8410.426885	24.121779
126.075412	8421.882001	24.126797
126.549615	8431.032983	24.131815
126.761152	8453.485249	24.136832
126.988227	8458.138102	24.141850
127.070730	8476.752543	24.146867
127.290926	8481.245464	24.151885
127.358981	8492.992165	24.156903
127.598319	8499.246955	24.161920
127.869773	8514.084257	24.166938
127.503793	8525.731648	24.171955
127.640644	8542.298098	24.176973
127.882548	8545.992022	24.181991
127.795932	8565.769637	24.187008
127.956443	8570.565549	24.192026
128.401134	8594.206449	24.197043
128.202865	8592.728394	24.202061
128.925089	8609.537858	24.207079
128.451485	8625.274962	24.212096
128.990583	8626.071386	24.217114
128.838412	8652.966231	24.222131
129.196128	8665.103355	24.227149
129.121804	8665.866440	24.232167
129.556244	8678.105211	24.237184
129.967591	8683.209148	24.242202
130.033631	8682.712615	24.247219
130.063396	8695.232646	24.252237
130.454268	8719.658812	24.257255
130.251569	8726.608062	24.262272
130.326225	8728.367591	24.267290
130.313543	8729.196794	24.272307
130.369921	8746.098071	24.277325
130.427507	8745.164006	24.282343
130.420359	8764.263208	24.287360
130.843692	8778.164487	24.292378
130.514083	8782.377380	24.297395
130.929933	8808.245761	24.302413
131.292937	8813.458340	24.307431
131.620979	8832.271462	24.312448
131.295319	8845.071441	24.317466
131.416293	8849.068524	24.322483
131.161077	8852.044767	24.327501
131.528263	8864.313142	24.332519
131.740870	8878.639010	24.337536
132.244216	8902.132194	24.342554
131.988527	8906.481924	24.347571
132.370159	8927.979883	24.352589
132.484205	8927.415835	24.357607
132.553863	8947.311449	24.362624
132.777835	8957.329097	24.367642
132.981208	8961.430112	24.372659
132.768399	8970.818443	24.377677
133.428792	8977.474704	24.382695
133.318087	8990.174803	24.387712
133.425483	8996.914551	24.392730
133.231790	9004.048772	24.397747
133.460678	9024.153160	24.402765
133.710876	9039.328883	24.407783
134.114054	9047.938775	24.412800
134.029163	9055.696897	24.417818
134.316518	9063.377760	24.422835
134.228054	9080.636703	24.427853
135.005288	9079.987694	24.432871
135.435422	9083.519630	24.437888
135.496721	9086.942016	24.442906
135.062009	9091.465071	24.447923
135.006693	9105.176373	24.452941
134.875181	9114.943543	24.457959
134.849286	9127.633606	24.462976
135.216561	9142.308006	24.467994
135.939887	9143.047177	24.473011
135.307871	9169.538036	24.478029
136.068918	9177.286811	24.483047
135.998827	9188.635674	24.488064
136.116211	9200.245645	24.493082
135.884259	9200.585109	24.498099
136.192143	9227.822315	24.503117
136.295637	9238.301013	24.508135
136.485223	9250.922670	24.513152
137.027815	9263.624797	24.518170
136.738395	9272.460122	24.523187
136.997798	9292.364266	24.528205
137.161121	9297.762973	24.533223
137.404412	9314.341852	24.538240
137.184729	9314.123707	24.543258
137.097903	9336.671144	24.548275
137.640024	9357.172001	24.553293
137.910302	9367.750935	24.558311
138.051815	9387.215836	24.563328
138.048963	9400.508683	24.568346
138.424762	9403.073577	24.573363
138.232512	9432.583786	24.578381
138.254832	9425.943584	24.583399
138.675800	9454.034830	24.588416
138.885653	9471.316861	24.593434
139.095943	9469.307440	24.598451
138.823292	9491.284280	24.603469
139.130180	9489.468109	24.608487
139.561420	9516.080199	24.613504
139.215216	9523.895241	24.618522
139.875866	9528.584630	24.623539
140.146738	9550.403768	24.628557
140.347688	9554.227448	24.633575
140.573654	9558.347158	24.638592
140.234232	9568.658629	24.643610
140.777620	9579.362237	24.648627
140.618738	9585.821864	24.653645
140.776530	9591.152061	24.658663
140.797756	9610.471858	24.663680
140.964605	9617.821362	24.668698
141.308225	9620.504993	24.673715
141.361132	9637.287642	24.678733
141.315513	9642.523427	24.683751
141.876829	9652.501229	24.688768
141.928428	9664.405959	24.693786
142.170031	9670.023000	24.698803
141.673395	9681.429516	24.703821
142.113426	9694.968925	24.708839
142.388031	9710.826525	24.713856
142.236080	9718.841704	24.718874
142.843084	9727.827283	24.723891
142.458689	9737.482841	24.728909
142.822860	9737.836273	24.733927
142.839275	9750.715890	24.738944
142.735467	9767.602142	24.743962
142.956902	9777.150178	24.748979
142.895068	9805.604916	24.753997
143.351443	9806.164922	24.759015
143.645056	9823.203666	24.764032
143.593318	9842.389893	24.769050
143.947761	9846.997882	24.774067
143.809992	9855.130880	24.779085
143.907496	9868.174688	24.784103
144.495982	9885.937702	24.789120
144.132853	9891.820052	24.794138
144.628912	9901.040958	24.799155
144.998730	9924.376381	24.804173
144.848160	9937.976921	24.809191
144.950226	9950.464366	24.814208
145.265659	9971.415037	24.819226
145.433279	9976.800640	24.824243
145.327609	9989.055431	24.829261
145.516949	10002.615395	24.834279
145.598369	10010.991975	24.839296
146.026757	10029.203304	24.844314
146.462091	10037.379207	24.849331
146.268891	10058.491755	24.854349
146.837609	10053.268673	24.859367
146.989387	10073.850419	24.864384
146.746843	10083.566025	24.869402
147.023747	10084.773018	24.874419
146.810285	10102.077747	24.879437
146.738443	10107.497745	24.884455
147.027782	10127.956961	24.889472
147.217428	10141.766417	24.894490
147.876115	10161.788910	24.899507
147.504196	10187.378470	24.904525
147.909233	10184.621718	24.909543
147.997511	10197.916642	24.914560
148.115562	10200.926185	24.919578
148.706636	10211.183799	24.924595
148.850216	10233.816204	24.929613
148.795800	10226.442576	24.934631
149.128883	10231.382385	24.939648
148.913921	10258.106246	24.944666
149.240048	10258.112011	24.949683
149.264933	10279.326414	24.954701
149.596256	10294.856718	24.959719
149.528561	10299.262569	24.964736
149.374892	10316.056088	24.969754
149.985543	10325.934956	24.974771
149.986234	10338.567999	24.979789
150.440136	10363.169583	24.984807
150.199830	10366.686817	24.989824
150.194905	10384.555904	24.994842
150.436213	10388.000847	24.999859
150.670408	10398.175544	25.004877
150.617746	10415.351173	25.009895
150.755937	10419.421676	25.014912
150.838342	10447.892684	25.019930
151.099963	10457.832618	25.024947
151.230030	10473.868229	25.029965
151.484056	10493.430327	25.034983
151.715563	10499.990141	25.040000
151.633363	10525.051671	25.045018
152.317812	10527.208411	25.050035
152.316144	10550.770164	25.055053
151.971085	10551.323137	25.060071
152.360485	10565.508933	25.065088
152.572622	10579.968798	25.070106
152.601331	10585.398442	25.075123
152.815481	10600.972618	25.080141
153.010365	10618.668535	25.085159
153.212254	10635.419266	25.090176
153.434388	10644.879225	25.095194
153.811234	10654.835946	25.100211
153.854599	10680.001155	25.105229
153.724109	10683.842260	25.110247
153.850991	10687.403070	25.115264
153.716037	10705.526492	25.120282
154.315954	10718.482710	25.125299
154.385347	10746.637296	25.130317
154.529751	10751.565755	25.135335
154.716173	10759.844123	25.140352
154.665027	10790.477402	25.145370
155.013285	10800.214491	25.150387
155.258505	10816.838608	25.155405
155.741707	10835.556821	25.160423
156.098043	10832.352915	25.165440
155.921144	10850.404109	25.170458
156.101315	10852.769352	25.175475
156.530057	10858.325858	25.180493
156.262471	10868.838345	25.185511
156.203836	10870.113746	25.190528
156.245446	10894.079636	25.195546
156.404078	10903.325485	25.200563
156.894431	10917.385217	25.205581
156.944228	10931.829738	25.210599
157.807870	10941.467214	25.215616
157.684922	10949.497319	25.220634
157.582535	10962.882651	25.225651
157.984896	10971.730385	25.230669
157.761729	10983.145365	25.235687
157.800240	10985.251792	25.240704
158.113089	11002.847493	25.245722
158.129969	11019.728595	25.250739
158.693653	11041.563595	25.255757
158.875024	11052.457387	25.260775
158.837882	11061.077201	25.265792
158.825178	11079.510223	25.270810
158.934165	11086.098911	25.275827
159.443028	11100.847400	25.280845
159.563280	11113.178047	25.285863
159.549544	11115.469501	25.290880
159.520471	11143.722206	25.295898
159.633197	11152.684869	25.300915
160.329702	11172.554113	25.305933
160.336839	11180.005036	25.310951
160.653774	11188.367349	25.315968
160.568756	11205.993996	25.320986
160.557811	11214.268752	25.326003
160.919555	11227.256321	25.331021
160.894266	11234.447104	25.336039
161.390088	11245.515937	25.341056
161.518553	11262.843950	25.346074
161.693175	11266.463702	25.351091
161.923842	11279.010826	25.356109
162.113853	11296.834453	25.361127
162.489931	11294.868335	25.366144
162.381896	11302.836260	25.371162
162.836858	11313.598927	25.376179
162.926742	11312.132347	25.381197
162.907810	11322.457721	25.386215
162.878577	11320.615094	25.391232
163.507683	11331.369436	25.396250
164.099590	11331.276729	25.401267
164.148280	11342.371462	25.406285
163.966048	11340.230722	25.411303
164.285165	11331.816107	25.416320
164.575751	11329.058176	25.421338
164.320508	11323.003905	25.426355
164.602768	11328.330888	25.431373
164.968673	11351.431880	25.436391
165.232657	11345.334149	25.441408
165.039746	11363.691479	25.446426
165.224569	11357.625091	25.451443
165.340207	11360.985701	25.456461
165.193061	11372.635305	25.461479
165.547924	11377.982504	25.466496
165.369573	11389.924356	25.471514
165.379607	11399.935783	25.476531
165.805097	11414.823888	25.481549
166.137202	11423.063938	25.486567
166.359474	11438.918571	25.491584
166.282524	11454.756942	25.496602
166.647954	11465.963168	25.501619
166.794190	11485.666338	25.506637
166.576465	11487.677183	25.511655
167.096715	11497.902395	25.516672
166.826179	11520.070738	25.521690
167.050365	11523.316482	25.526707
167.478399	11542.975565	25.531725
167.141630	11559.880979	25.536743
167.623978	11572.442551	25.541760
167.670935	11586.149118	25.546778
167.796246	11608.293442	25.551795
168.002704	11629.004109	25.556813
167.773222	11650.029396	25.561831
168.132813	11664.564886	25.566848
168.251395	11677.035105	25.571866
168.136972	11705.270447	25.576883
168.745627	11727.187617	25.581901
168.658473	11744.796156	25.586919
168.911398	11760.182072	25.591936
169.012689	11790.313121	25.596954
169.356740	11804.876416	25.601971
169.665028	11830.990034	25.606989
169.357623	11849.991007	25.612007
169.630070	11861.464656	25.617024
170.399354	11877.650785	25.622042
170.098332	11890.095306	25.627059
170.771018	11913.126822	25.632077
170.897362	11933.209350	25.637095
171.181012	11943.702388	25.642112
171.062042	11952.540684	25.647130
171.554332	11977.583617	25.652147
171.865465	11984.734612	25.657165
171.681082	11997.375658	25.662183
172.509759	12017.101939	25.667200
172.250891	12025.557991	25.672218
172.468032	12042.478107	25.677236
172.675368	12044.738198	25.682253
172.552977	12065.342974	25.687271
172.913104	12083.538575	25.692288
173.161251	12086.644879	25.697306
173.054877	12102.633661	25.702324
173.703332	12118.883137	25.707341
173.302512	12136.203297	25.712359
173.779893	12147.591332	25.717376
173.864169	12155.636853	25.722394
173.955565	12172.576786	25.727412
174.258924	12175.791294	25.732429
174.288942	12194.461864	25.737447
174.539632	12203.624459	25.742464
174.526252	12222.766054	25.747482
174.832699	12242.940692	25.752500
175.057431	12249.183242	25.757517
175.405398	12268.359849	25.762535
175.605240	12279.403034	25.767552
175.687757	12278.114371	25.772570
175.562613	12310.220625	25.777588
176.107191	12314.679443	25.782605
176.132217	12323.413250	25.787623
176.606688	12333.567145	25.792640
176.657151	12347.122140	25.797658
176.712485	12364.213154	25.802676
177.069244	12370.311905	25.807693
177.004555	12379.612414	25.812711
177.435165	12398.665682	25.817728
177.593052	12404.296662	25.822746
177.744534	12424.022095	25.827764
177.875593	12432.114088	25.832781
178.038508	12435.830635	25.837799
178.544539	12450.779574	25.842816
178.538623	12457.563583	25.847834
178.610867	12470.398422	25.852852
178.794590	12473.413833	25.857869
178.959888	12490.787730	25.862887
179.417998	12507.544198	25.867904
179.407491	12506.159569	25.872922
179.048563	12527.711368	25.877940
179.284660	12546.365790	25.882957
179.424161	12560.068039	25.887975
179.616043	12571.400007	25.892992
179.938828	12589.333528	25.898010
180.047086	12615.826936	25.903028
180.638581	12628.656324	25.908045
180.529122	12641.810270	25.913063
180.635091	12665.383068	25.918080
180.863004	12674.704197	25.923098
181.049408	12693.783390	25.928116
181.527562	12707.735850	25.933133
181.389778	12719.059553	25.938151
181.316399	12725.816332	25.943168
182.033870	12746.542906	25.948186
182.062992	12767.222604	25.953204
182.664140	12768.470558	25.958221
183.032198	12783.267692	25.963239
183.157403	12794.079712	25.968256
183.445997	12788.722929	25.973274
183.052448	12806.026770	25.978292
183.547101	12810.127212	25.983309
184.104237	12820.363157	25.988327
183.772122	12823.832069	25.993344
183.953866	12838.740540	25.998362
184.266010	12848.838038	26.003380
185.003607	12852.685691	26.008397
184.660598	12861.231086	26.013415
184.760139	12878.385113	26.018432
184.959104	12878.562390	26.023450
185.068457	12905.870775	26.028468
185.517503	12903.940433	26.033485
185.453235	12914.750626	26.038503
185.470720	12931.927031	26.043520
185.831739	12936.822128	26.048538
185.725366	12959.007489	26.053556
186.146339	12962.456342	26.058573
186.453321	12973.461042	26.063591
186.499385	12986.391913	26.068608
187.040575	12990.835635	26.073626
186.695394	13000.076179	26.078644
186.979700	13011.873938	26.083661
186.864834	13033.264915	26.088679
187.292583	13033.450563	26.093696
187.444555	13049.428092	26.098714
187.303442	13057.117720	26.103732
187.627109	13077.385291	26.108749
187.547122	13093.282351	26.113767
187.670011	13120.298392	26.118784
188.047303	13132.927993	26.123802
188.194217	13151.312767	26.128820
188.215496	13180.397489	26.133837
188.378809	13186.548917	26.138855
188.554669	13212.805194	26.143872
189.191749	13233.061727	26.148890
189.194324	13262.923210	26.153908
189.414728	13281.713451	26.158925
189.698570	13294.019895	26.163943
189.939380	13314.629130	26.168960
189.978533	13319.963185	26.173978
190.208279	13344.063768	26.178996
190.209192	13353.471322	26.184013
190.404845	13377.848876	26.189031
190.288070	13401.340637	26.194048
191.194093	13418.637239	26.199066
191.165954	13448.873313	26.204084
191.112887	13465.555970	26.209101
191.630619	13480.952331	26.214119
191.739494	13506.868969	26.219136
192.051433	13519.543804	26.224154
192.077277	13538.857431	26.229172
192.650614	13542.664644	26.234189
192.806476	13567.152889	26.239207
192.702694	13574.937936	26.244224
193.509418	13593.125029	26.249242
193.376413	13601.299945	26.254260
193.661769	13624.087901	26.259277
193.851810	13634.204947	26.264295
194.072539	13658.354712	26.269312
194.335092	13666.767702	26.274330
194.106194	13674.780821	26.279348
194.123731	13693.142175	26.284365
194.705048	13710.136210	26.289383
194.793733	13725.448398	26.294400
195.190397	13750.136010	26.299418
195.057084	13770.065363	26.304436
195.322933	13789.240586	26.309453
195.679447	13791.613315	26.314471
195.789907	13812.865651	26.319488
195.980401	13824.438600	26.324506
196.152041	13851.438569	26.329524
196.561641	13862.042424	26.334541
196.687196	13874.528788	26.339559
197.252967	13890.495886	26.344576
196.956401	13907.226551	26.349594
197.370770	13928.219814	26.354612
197.760080	13935.277192	26.359629
197.662031	13947.015426	26.364647
197.782933	13964.309202	26.369664
198.317407	13975.395695	26.374682
198.416343	13993.990918	26.379700
198.570940	14002.379914	26.384717
198.504072	14021.594863	26.389735
198.796221	14037.882864	26.394752
199.158593	14041.622169	26.399770
198.812115	14071.406962	26.404788
199.002358	14087.559381	26.409805
199.798540	14105.890735	26.414823
199.541742	14122.773264	26.419840
200.189852	14137.540216	26.424858
200.154641	14149.998258	26.429876
200.623233	14156.822230	26.434893
200.518566	14176.438022	26.439911
200.437877	14187.731546	26.444928
200.805622	14208.795586	26.449946
200.824851	14229.131028	26.454964
201.170348	14245.417165	26.459981
201.420672	14268.025050	26.464999
201.404048	14283.584729	26.470016
201.600682	14294.885401	26.475034
201.699799	14316.121127	26.480052
201.957610	14324.614105	26.485069
202.133494	14355.350225	26.490087
202.203981	14379.644451	26.495104
202.797399	14397.338320	26.500122
203.237006	14423.798129	26.505140
203.005342	14435.393370	26.510157
203.463647	14455.736064	26.515175
203.480774	14477.919636	26.520192
203.868433	14492.373949	26.525210
204.185287	14514.756947	26.530228
204.662939	14526.190591	26.535245
204.840406	14546.267875	26.540263
204.787823	14563.046161	26.545280
205.029138	14577.757172	26.550298
205.082274	14589.623710	26.555316
205.085806	14610.505228	26.560333
205.727106	14620.719490	26.565351
206.130236	14642.163766	26.570368
206.104496	14656.888251	26.575386
206.195010	14683.551545	26.580404
206.336556	14696.418087	26.585421
206.761140	14711.378414	26.590439
206.911157	14736.225956	26.595456
207.062456	14733.659905	26.600474
207.285586	14760.109878	26.605492
207.517822	14774.133969	26.610509
207.782673	14795.770625	26.615527
207.784555	14805.595631	26.620544
208.156563	14816.878614	26.625562
208.364107	14838.082142	26.630580
208.448604	14849.359653	26.635597
208.986062	14875.962672	26.640615
209.307723	14888.321073	26.645632
209.749612	14909.175301	26.650650
209.905805	14915.249448	26.655668
209.862975	14927.946060	26.660685
210.267938	14935.456148	26.665703
210.130407	14952.447054	26.670720
210.108305	14972.319180	26.675738
210.759172	14981.003537	26.680756
211.297446	14998.488684	26.685773
211.387829	15012.566755	26.690791
211.431678	15020.515600	26.695808
211.653522	15028.123894	26.700826
211.777266	15037.181416	26.705844
211.663405	15045.180244	26.710861
211.931758	15070.107588	26.715879
212.381506	15077.613875	26.720896
212.795277	15094.300619	26.725914
212.877850	15105.360661	26.730932
213.209442	15123.579441	26.735949
213.551679	15119.224259	26.740967
213.160494	15140.032384	26.745984
213.918215	15156.990604	26.751002
213.945018	15164.111547	26.756020
213.864589	15181.728528	26.761037
214.231953	15201.252473	26.766055
214.371317	15204.783756	26.771072
214.325948	15223.627022	26.776090
214.691495	15249.142610	26.781108
214.796627	15263.935492	26.786125
215.108117	15271.586689	26.791143
215.229429	15300.725295	26.796160
215.662493	15308.193229	26.801178
216.127828	15320.965250	26.806196
215.646657	15337.909265	26.811213
216.186139	15351.291881	26.816231
216.018130	15367.738380	26.821248
216.587543	15388.538413	26.826266
216.810460	15407.295613	26.831284
216.924132	15427.292224	26.836301
216.991788	15441.408912	26.841319
217.060859	15465.335212	26.846336
217.462889	15490.526413	26.851354
217.884656	15510.528536	26.856372
217.719791	15526.684110	26.861389
218.192505	15547.420505	26.866407
218.661859	15578.305274	26.871424
218.302354	15596.797006	26.876442
218.963929	15613.688577	26.881460
219.206873	15646.605016	26.886477
219.329068	15663.056839	26.891495
218.997380	15680.761015	26.896512
219.419398	15697.696506	26.901530
219.935431	15716.218586	26.906548
220.052480	15749.606574	26.911565
220.589186	15759.139829	26.916583
220.693839	15776.396729	26.921600
220.739548	15803.769764	26.926618
221.235200	15827.711807	26.931636
221.229871	15840.175741	26.936653
221.706021	15859.414850	26.941671
222.122703	15880.605719	26.946688
222.470279	15895.171602	26.951706
222.863331	15894.636289	26.956724
222.669040	15925.069700	26.961741
223.150217	15935.331863	26.966759
223.242846	15955.427073	26.971776
223.642119	15968.806820	26.976794
224.084635	15982.476694	26.981812
224.488433	15995.378827	26.986829
224.643008	15994.858762	26.991847
224.104523	16015.400330	26.996864
224.485268	16036.698072	27.001882
224.845295	16046.726599	27.006900
224.942596	16070.121769	27.011917
225.160423	16086.224177	27.016935
225.441183	16098.378151	27.021952
225.570463	16111.594995	27.026970
225.763164	16130.600836	27.031988
225.707753	16158.381865	27.037005
226.168228	16180.924344	27.042023
226.456372	16193.525724	27.047040
226.333666	16214.052904	27.052058
226.684555	16227.579383	27.057076
226.823183	16257.029415	27.062093
227.221056	16286.508366	27.067111
227.078169	16315.257185	27.072128
227.537121	16333.567711	27.077146
227.803820	16344.710168	27.082164
227.954706	16363.571183	27.087181
228.229109	16386.304135	27.092199
228.385818	16404.876855	27.097216
228.762606	16419.966029	27.102234
228.928003	16443.019341	27.107252
229.372507	16460.880584	27.112269
229.472668	16478.988457	27.117287
229.321053	16502.050441	27.122304
229.926573	16517.782941	27.127322
229.984949	16542.113387	27.132340
229.953026	16562.127668	27.137357
230.294867	16583.264708	27.142375
230.495228	16599.600854	27.147392
230.700270	16622.003829	27.152410
230.959373	16645.990265	27.157428
231.248324	16676.276510	27.162445
231.817225	16691.765364	27.167463
231.923684	16727.064467	27.172480
231.795585	16738.016316	27.177498
232.396055	16756.794651	27.182516
232.300270	16790.754738	27.187533
232.819391	16806.387301	27.192551
233.147053	16837.252070	27.197568
233.153361	16853.012385	27.202586
233.627794	16877.676055	27.207604
233.667088	16889.817819	27.212621
233.760177	16918.217869	27.217639
234.027080	16936.470613	27.222656
234.227883	16963.072411	27.227674
234.786621	16983.477863	27.232692
234.739762	17011.508307	27.237709
235.006147	17031.656383	27.242727
235.458492	17051.649003	27.247744
235.346143	17070.308733	27.252762
235.903885	17093.569840	27.257780
236.587438	17133.912028	27.262797
236.616798	17134.640253	27.267815
236.562126	17159.437709	27.272832
236.908471	17178.663728	27.277850
237.431603	17194.229646	27.282868
237.545974	17216.284272	27.287885
237.816043	17230.999129	27.292903
238.360075	17256.625241	27.297920
238.208474	17277.502367	27.302938
238.827603	17293.716643	27.307956
238.956607	17313.292708	27.312973
239.381592	17341.312886	27.317991
239.798589	17355.739494	27.323008
239.667035	17367.162880	27.328026
240.320834	17378.760156	27.333044
240.473201	17386.323413	27.338061
240.950141	17382.439377	27.343079
241.162468	17408.509328	27.348096
241.021157	17408.588345	27.353114
241.370738	17415.785901	27.358132
241.491819	17439.854959	27.363149
241.758523	17448.240536	27.368167
242.297070	17460.645584	27.373184
241.859246	17484.189470	27.378202
242.213795	17497.526748	27.383220
242.626399	17515.182335	27.388237
242.781849	17541.867842	27.393255
242.843778	17560.387029	27.398272
242.814922	17573.834961	27.403290
243.059148	17593.968142	27.408308
243.185644	17615.351679	27.413325
243.623682	17641.070714	27.418343
243.966971	17664.934671	27.423360
243.835689	17688.664527	27.428378
244.621565	17700.348703	27.433396
244.430908	17724.972344	27.438413
244.212607	17754.527951	27.443431
244.700902	17771.451726	27.448448
244.803737	17805.872079	27.453466
245.276980	17827.618482	27.458484
245.183378	17847.343674	27.463501
245.906525	17881.426922	27.468519
246.303880	17899.167375	27.473536
246.341579	17924.576769	27.478554
246.894719	17943.821693	27.483572
246.900415	17963.594622	27.488589
247.104551	17986.988009	27.493607
247.281002	18013.039122	27.498624
247.515247	18035.145392	27.503642
248.060808	18065.700013	27.508660
248.324938	18086.967745	27.513677
248.456074	18110.435892	27.518695
248.601142	18131.324318	27.523712
248.496724	18152.536141	27.528730
249.294462	18170.751114	27.533748
249.549610	18198.413765	27.538765
249.940076	18225.663566	27.543783
250.505274	18237.957540	27.548800
250.669260	18261.515487	27.553818
250.744910	18274.884357	27.558836
251.354594	18299.143278	27.563853
251.096727	18314.813494	27.568871
251.663052	18317.574049	27.573888
251.870088	18355.965474	27.578906
251.915572	18363.880692	27.583924
252.369473	18397.773273	27.588941
252.493789	18407.028136	27.593959
252.962567	18430.456412	27.598976
253.171979	18457.671725	27.603994
253.345509	18463.861153	27.609012
253.540668	18486.795358	27.614029
253.673958	18508.747405	27.619047
254.037472	18526.272614	27.624064
253.946735	18553.762517	27.629082
254.346597	18574.023958	27.634100
254.525922	18600.340751	27.639117
254.707205	18626.385611	27.644135
255.301260	18648.069784	27.649152
255.324131	18679.781267	27.654170
255.333879	18690.166135	27.659188
255.729197	18720.164088	27.664205
256.037082	18747.377015	27.669223
256.047356	18777.068944	27.674240
256.464333	18804.896639	27.679258
256.902406	18822.467295	27.684276
257.380341	18854.177269	27.689293
257.248314	18877.024196	27.694311
257.649034	18896.654057	27.699328
257.754994	18923.342894	27.704346
257.791019	18951.034623	27.709364
258.378213	18967.387979	27.714381
258.711406	18995.854537	27.719399
258.707602	19011.270704	27.724416
259.305411	19041.117392	27.729434
259.556509	19056.550524	27.734452
259.939865	19079.203229	27.739469
260.283102	19108.590787	27.744487
260.513751	19125.492926	27.749504
261.026658	19154.569670	27.754522
261.188390	19178.583966	27.759540
261.490190	19193.769184	27.764557
261.542156	19209.726429	27.769575
261.570943	19218.465938	27.774592
261.772246	19244.988649	27.779610
262.510967	19267.339504	27.784628
262.599944	19277.636458	27.789645
262.659847	19306.866526	27.794663
263.241847	19321.850001	27.799680
263.217316	19348.717809	27.804698
263.448787	19361.412263	27.809716
263.737194	19380.674811	27.814733
263.958783	19408.849874	27.819751
264.344948	19425.045568	27.824768
264.758222	19450.031671	27.829786
265.289110	19464.599957	27.834804
265.521511	19476.940533	27.839821
265.489201	19492.576357	27.844839
265.908208	19514.029879	27.849856
265.997584	19546.465238	27.854874
266.106419	19562.912986	27.859892
266.441338	19580.885885	27.864909
266.367386	19601.582746	27.869927
266.758103	19629.687406	27.874944
267.048551	19656.879060	27.879962
267.080977	19678.273278	27.884980
267.655251	19702.950170	27.889997
267.845951	19735.477377	27.895015
268.522883	19748.582474	27.900032
268.375482	19771.944618	27.905050
268.620805	19806.453585	27.910068
269.149886	19830.872358	27.915085
269.298839	19851.743062	27.920103
269.715144	19873.045767	27.925120
269.783154	19895.281276	27.930138
269.884421	19924.941738	27.935156
270.202195	19949.785485	27.940173
270.231840	19966.669294	27.945191
270.957459	19993.003473	27.950208
271.272788	20018.239417	27.955226
271.912740	20050.248179	27.960244
272.004064	20061.221223	27.965261
271.910527	20089.579312	27.970279
272.556614	20109.753230	27.975296
272.859490	20131.396213	27.980314
272.775140	20152.739741	27.985332
273.735939	20169.086127	27.990349
273.579061	20202.180332	27.995367
274.109843	20220.439048	28.000384
274.033346	20245.363888	28.005402
274.251930	20263.500958	28.010420
274.605395	20282.773157	28.015437
274.782648	20308.347017	28.020455
275.565298	20320.096466	28.025472
275.553248	20349.004489	28.030490
275.932791	20374.850024	28.035508
276.292797	20393.476842	28.040525
276.380198	20417.870762	28.045543
276.943673	20438.272783	28.050560
276.838761	20464.301738	28.055578
277.042141	20491.849377	28.060596
277.778346	20495.992626	28.065613
277.649641	20522.884678	28.070631
277.888360	20546.838044	28.075648
278.341872	20562.777715	28.080666
278.399255	20586.772172	28.085684
278.689987	20616.220764	28.090701
278.947008	20648.151485	28.095719
279.022498	20662.507676	28.100736
279.445602	20684.189300	28.105754
279.752681	20714.595874	28.110772
280.000188	20737.909937	28.115789
280.064026	20767.640717	28.120807
280.526134	20794.263671	28.125824
280.462806	20816.849355	28.130842
280.721391	20842.872414	28.135860
281.035352	20866.163583	28.140877
281.062346	20901.214149	28.145895
281.418093	20929.022862	28.150912
281.949806	20960.039108	28.155930
281.901244	20986.742320	28.160948
282.445937	21022.666095	28.165965
282.457838	21055.539419	28.170983
282.444231	21075.343785	28.176000
283.233513	21107.330877	28.181018
283.052877	21146.989016	28.186036
283.675982	21180.411292	28.191053
284.081282	21209.002456	28.196071
284.573448	21225.252538	28.201088
285.229309	21258.113781	28.206106
285.663846	21286.321363	28.211124
285.970641	21298.885219	28.216141
286.152961	21331.921863	28.221159
286.521102	21346.321169	28.226176
287.004291	21368.322701	28.231194
287.122317	21393.205882	28.236212
287.415960	21416.216545	28.241229
287.707531	21435.442702	28.246247
288.095481	21450.312878	28.251264
288.405676	21467.229847	28.256282
288.755871	21493.953420	28.261300
288.829390	21517.617912	28.266317
288.910563	21546.336163	28.271335
289.636075	21564.028538	28.276352
289.692965	21575.728148	28.281370
289.529171	21610.196947	28.286388
289.888733	21640.912661	28.291405
290.196376	21664.009881	28.296423
290.473363	21694.195205	28.301440
290.481847	21727.474578	28.306458
290.763180	21759.043120	28.311476
290.895139	21788.215033	28.316493
291.094976	21828.667966	28.321511
291.101998	21861.442292	28.326528
292.111830	21896.511267	28.331546
291.891097	21932.329125	28.336564
292.378624	21956.182038	28.341581
292.452149	21998.057875	28.346599
293.064628	22031.148360	28.351616
293.478144	22062.424969	28.356634
293.881924	22089.595909	28.361652
294.559180	22113.602537	28.366669
294.537944	22141.377228	28.371687
294.686418	22181.036431	28.376704
295.580321	22199.366479	28.381722
295.563207	22225.541968	28.386740
295.959475	22254.673164	28.391757
296.540331	22274.082299	28.396775
296.725049	22293.130141	28.401792
297.162455	22321.225010	28.406810
297.526136	22346.304705	28.411828
297.484496	22372.876003	28.416845
297.743858	22401.251632	28.421863
298.040879	22415.827151	28.426880
298.948464	22449.693570	28.431898
299.227399	22474.508669	28.436916
299.439867	22490.790969	28.441933
299.615740	22516.172014	28.446951
299.564425	22540.659791	28.451968
299.667634	22559.398389	28.456986
300.652855	22579.692329	28.462004
300.961188	22591.372107	28.467021
301.051372	22610.011689	28.472039
301.078839	22636.837912	28.477056
301.879387	22654.810186	28.482074
301.590937	22672.137912	28.487092
301.931828	22685.796819	28.492109
302.270682	22720.251994	28.497127
302.395330	22743.271715	28.502144
302.508764	22775.645417	28.507162
302.840896	22798.038708	28.512180
303.199106	22833.009210	28.517197
303.397788	22858.652520	28.522215
303.199002	22902.424410	28.527232
303.804197	22934.291639	28.532250
303.885712	22954.196722	28.537268
304.317758	22987.260195	28.542285
304.746553	23024.469583	28.547303
305.006116	23059.108382	28.552320
305.528945	23077.162459	28.557338
305.527782	23125.453669	28.562356
306.023779	23159.878669	28.567373
306.565394	23188.381825	28.572391
306.541508	23217.169501	28.577408
307.206141	23247.435484	28.582426
307.395015	23281.984635	28.587444
308.021325	23313.021346	28.592461
308.263791	23338.348773	28.597479
308.507155	23373.887987	28.602496
309.327120	23399.605291	28.607514
309.301472	23433.202505	28.612532
309.492979	23442.341783	28.617549
309.724471	23475.260542	28.622567
309.893933	23511.342397	28.627584
310.367364	23533.259392	28.632602
310.722958	23569.849335	28.637620
311.099505	23592.615720	28.642637
311.414225	23627.139436	28.647655
311.819071	23650.331169	28.652672
312.201000	23676.913684	28.657690
312.702491	23704.886720	28.662708
312.930076	23726.122032	28.667725
313.231133	23744.249371	28.672743
313.669459	23768.655633	28.677760
314.105568	23777.775706	28.682778
314.247867	23816.958860	28.687796
315.002303	23838.522522	28.692813
315.406450	23856.267289	28.697831
315.323132	23879.156593	28.702848
315.832236	23893.851639	28.707866
315.875611	23919.735501	28.712884
316.361387	23942.074413	28.717901
316.473878	23968.206607	28.722919
316.903720	23994.162735	28.727936
317.348319	24009.253456	28.732954
317.594885	24030.909522	28.737972
318.406485	24059.719201	28.742989
318.711749	24070.736785	28.748007
318.773738	24093.906907	28.753024
318.932981	24102.640775	28.758042
319.095392	24127.975424	28.763060
319.515883	24141.774528	28.768077
319.877345	24170.737034	28.773095
319.831052	24203.820577	28.778112
320.616714	24221.714450	28.783130
320.823233	24242.012003	28.788148
320.885134	24249.712144	28.793165
321.338063	24256.738041	28.798183
321.463098	24286.729915	28.803200
322.163169	24301.104648	28.808218
321.691985	24327.341380	28.813236
322.219109	24344.188901	28.818253
322.622507	24371.179747	28.823271
322.836152	24392.664413	28.828288
323.288850	24418.168822	28.833306
323.641164	24443.790101	28.838324
323.662746	24469.532736	28.843341
323.879276	24497.469365	28.848359
323.709625	24531.811413	28.853376
324.404383	24564.975376	28.858394
324.757367	24605.125567	28.863412
325.138100	24630.293939	28.868429
325.338170	24664.357110	28.873447
325.657673	24693.225829	28.878464
326.134332	24733.634969	28.883482
326.400717	24764.768234	28.888500
326.377377	24799.536517	28.893517
326.777125	24836.848623	28.898535
326.946096	24873.944160	28.903552
327.744020	24911.965038	28.908570
328.101568	24941.927787	28.913588
328.633709	24965.284376	28.918605
329.277513	24994.703103	28.923623
329.114096	25037.791579	28.928640
329.231100	25064.133045	28.933658
329.479241	25109.470244	28.938676
329.667652	25146.923466	28.943693
330.345325	25185.361846	28.948711
330.424222	25221.890711	28.953728
331.512235	25238.442569	28.958746
331.791181	25266.338889	28.963764
331.984572	25288.048880	28.968781
332.496175	25320.775114	28.973799
332.967906	25354.569384	28.978816
333.136463	25370.424837	28.983834
333.690128	25399.213650	28.988852
333.792456	25427.257937	28.993869
334.508047	25456.135224	28.998887
334.674235	25485.736924	29.003904
335.133106	25511.601989	29.008922
335.434863	25533.762943	29.013940
335.774036	25567.274979	29.018957
335.833960	25595.875977	29.023975
336.018039	25625.715237	29.028992
336.434612	25643.996837	29.034010
336.567766	25688.645514	29.039028
337.228724	25713.613347	29.044045
337.302802	25747.565366	29.049063
337.450352	25774.143133	29.054080
338.030499	25802.947334	29.059098
338.221282	25839.750510	29.064116
338.843281	25868.895851	29.069133
339.183316	25901.984865	29.074151
339.349346	25934.696707	29.079168
339.650406	25968.126897	29.084186
340.214736	25998.994195	29.089204
340.262530	26034.278026	29.094221
340.719402	26061.597728	29.099239
340.848282	26098.505873	29.104256
340.999881	26124.710580	29.109274
341.726134	26159.976836	29.114292
342.164663	26197.190583	29.119309
342.914396	26223.023638	29.124327
343.007743	26248.245369	29.129344
343.189336	26274.281248	29.134362
343.861420	26290.336636	29.139380
344.042623	26318.654211	29.144397
344.581363	26335.337259	29.149415
344.986310	26361.900759	29.154432
345.511454	26372.120422	29.159450
345.923061	26399.732080	29.164468
346.135505	26414.026710	29.169485
346.392078	26439.760328	29.174503
346.768825	26450.907066	29.179520
346.789677	26478.548439	29.184538
347.301716	26501.265296	29.189556
347.031155	26529.205195	29.194573
348.094816	26560.349067	29.199591
348.011967	26586.350927	29.204608
348.414046	26618.236866	29.209626
348.450680	26650.761564	29.214644
348.907025	26685.179857	29.219661
349.338621	26705.419352	29.224679
349.569300	26753.360610	29.229696
350.115873	26774.776702	29.234714
350.634144	26801.771770	29.239732
350.901222	26831.593486	29.244749
351.428063	26857.961574	29.249767
351.661984	26891.062506	29.254784
352.202848	26922.194023	29.259802
352.326817	26940.212932	29.264820
352.623457	26971.806245	29.269837
352.800411	26998.134517	29.274855
353.238212	27035.141344	29.279872
353.423903	27065.007753	29.284890
353.818530	27097.458128	29.289908
353.991354	27140.409917	29.294925
354.653031	27168.994718	29.299943
354.653621	27209.932133	29.304960
355.375354	27242.552717	29.309978
355.930768	27276.551984	29.314996
356.049783	27316.276495	29.320013
356.083541	27336.117543	29.325031
356.460329	27387.962430	29.330048
356.510823	27429.221135	29.335066
356.672878	27461.127032	29.340084
356.730997	27499.786950	29.345101
357.467233	27544.155623	29.350119
357.809197	27596.398369	29.355136
358.189051	27633.326872	29.360154
358.654591	27679.849316	29.365172
358.938780	27718.354144	29.370189
360.004710	27755.175400	29.375207
360.343365	27795.391049	29.380224
360.963132	27825.076806	29.385242
361.742339	27857.082591	29.390260
361.806584	27892.499801	29.395277
361.988346	27913.948957	29.400295
362.407217	27949.835332	29.405312
362.783444	27987.605694	29.410330
363.415997	28016.607094	29.415348
363.433006	28053.011689	29.420365
363.820647	28073.961030	29.425383
364.212544	28109.984648	29.430400
364.171521	28145.595766	29.435418
364.490306	28175.177481	29.440436
365.234447	28203.156668	29.445453
365.452984	28241.331444	29.450471
366.001508	28282.956313	29.455488
365.960792	28305.300354	29.460506
366.647668	28348.970582	29.465524
367.217713	28385.940183	29.470541
367.486069	28396.744682	29.475559
367.842876	28440.353033	29.480576
368.091777	28471.842372	29.485594
368.832579	28497.736610	29.490612
368.833200	28525.320716	29.495629
368.889724	28555.816340	29.500647
369.242991	28580.993921	29.505664
369.446286	28618.571306	29.510682
370.225472	28655.622410	29.515700
370.226524	28687.277320	29.520717
370.632478	28731.238883	29.525735
371.071013	28758.501870	29.530752
371.322603	28803.062970	29.535770
371.787197	28836.320550	29.540788
371.915049	28878.764716	29.545805
372.062316	28909.613267	29.550823
372.832881	28958.353746	29.555840
372.976187	28997.767986	29.560858
373.558993	29022.334944	29.565876
373.884523	29073.199732	29.570893
374.613752	29111.991446	29.575911
375.186683	29142.596682	29.580928
375.486128	29179.591138	29.585946
375.942029	29206.453774	29.590964
376.473330	29247.419588	29.595981
376.731797	29288.105845	29.600999
376.746448	29325.157815	29.606016
377.182111	29361.410656	29.611034
377.485211	29397.962454	29.616052
377.843187	29437.343910	29.621069
378.145792	29475.533097	29.626087
378.822374	29517.582893	29.631104
379.339031	29546.895387	29.636122
379.861200	29584.057960	29.641140
380.250334	29625.249073	29.646157
380.555329	29652.660588	29.651175
380.816311	29681.039858	29.656192
381.005174	29721.990723	29.661210
381.791934	29746.779449	29.666228
382.365230	29780.343912	29.671245
383.080201	29814.910279	29.676263
383.329399	29838.986843	29.681280
383.777704	29869.713823	29.686298
384.346749	29899.998410	29.691316
384.280006	29926.570898	29.696333
384.389253	29954.563429	29.701351
384.755239	29986.529807	29.706368
385.141394	30022.121508	29.711386
385.827934	30056.313455	29.716404
386.022376	30088.262612	29.721421
386.248627	30131.863392	29.726439
386.860572	30150.560928	29.731456
387.181227	30187.206196	29.736474
387.896447	30222.171454	29.741492
388.371810	30247.698591	29.746509
388.523873	30279.920181	29.751527
388.997856	30314.430313	29.756544
389.350019	30347.897588	29.761562
389.408603	30380.936796	29.766580
389.629041	30409.582597	29.771597
389.854634	30439.068380	29.776615
390.112519	30486.963532	29.781632
390.405771	30524.384907	29.786650
391.117955	30571.020657	29.791668
391.462665	30614.471147	29.796685
391.985452	30652.823988	29.801703
391.828755	30692.029273	29.806720
392.076845	30741.077061	29.811738
392.807613	30781.439417	29.816756
393.023281	30828.210414	29.821773
393.257795	30856.804054	29.826791
393.995248	30888.738927	29.831808
394.240985	30937.781228	29.836826
394.730354	30979.079447	29.841844
394.793672	31022.170285	29.846861
394.996217	31064.525060	29.851879
395.477668	31109.440751	29.856896
395.895960	31155.004919	29.861914
396.108363	31191.156864	29.866932
396.820209	31244.090562	29.871949
397.321404	31300.780873	29.876967
397.894109	31338.197873	29.881984
398.157700	31386.928672	29.887002
398.814523	31427.253294	29.892020
399.082975	31457.258514	29.897037
399.281358	31496.795322	29.902055
399.545386	31540.582797	29.907072
400.223010	31593.573320	29.912090
400.790001	31635.360106	29.917108
401.587305	31679.974683	29.922125
401.206711	31720.019842	29.927143
401.826170	31761.963032	29.932160
402.675704	31804.426590	29.937178
403.400148	31830.928159	29.942196
403.675882	31875.548989	29.947213
404.033104	31911.824904	29.952231
404.762923	31934.235503	29.957248
404.942983	31974.401954	29.962266
405.719724	32004.846743	29.967284
406.322897	32047.008002	29.972301
406.478625	32074.502998	29.977319
407.061216	32105.073174	29.982336
407.554454	32149.426609	29.987354
407.922559	32179.177026	29.992372
408.250872	32211.734353	29.997389
408.042701	32238.692298	30.002407
409.024236	32269.642766	30.007424
408.680799	32315.986274	30.012442
409.203983	32353.216872	30.017460
409.607890	32402.092436	30.022477
409.750052	32437.637985	30.027495
410.073116	32473.623090	30.032512
410.514977	32530.882379	30.037530
411.204523	32572.980595	30.042548
411.697391	32621.741585	30.047565
411.793948	32653.488739	30.052583
412.376994	32697.766049	30.057600
412.515825	32743.838976	30.062618
412.690377	32791.392115	30.067636
413.416072	32839.491249	30.072653
413.817069	32878.550060	30.077671
414.537121	32930.007363	30.082688
414.877159	32978.173545	30.087706
415.105439	33024.871621	30.092724
415.897456	33064.741998	30.097741
415.679905	33108.728310	30.102759
416.244339	33154.008415	30.107776
416.777472	33195.405322	30.112794
417.556037	33241.606738	30.117812
417.734789	33274.549514	30.122829
418.039546	33318.865403	30.127847
418.888527	33373.736614	30.132864
418.871811	33413.481436	30.137882
419.849543	33455.156944	30.142900
420.066259	33491.963393	30.147917
420.417419	33535.709781	30.152935
421.429642	33549.169655	30.157952
422.051953	33582.327944	30.162970
422.510793	33606.976653	30.167988
422.734712	33631.099493	30.173005
423.255337	33661.302304	30.178023
423.798278	33677.333121	30.183040
423.803814	33719.117176	30.188058
424.464628	33748.855584	30.193076
424.575189	33773.413625	30.198093
424.844309	33814.600207	30.203111
425.142096	33845.211212	30.208128
425.423634	33885.156783	30.213146
426.028141	33921.346863	30.218164
426.471770	33960.135462	30.223181
426.472579	34003.438220	30.228199
426.803967	34046.430064	30.233216
427.057020	34085.438420	30.238234
427.541080	34134.741716	30.243252
428.413858	34183.933659	30.248269
428.251238	34228.710346	30.253287
428.719456	34270.669601	30.258304
428.965174	34326.927598	30.263322
429.553471	34382.904470	30.268340
430.156754	34432.082300	30.273357
430.443589	34480.753418	30.278375
431.054522	34522.785659	30.283392
431.188388	34584.183223	30.288410
431.872282	34627.658463	30.293428
432.558904	34677.051427	30.298445
433.061484	34734.604367	30.303463
433.547100	34766.458155	30.308480
433.801786	34809.084199	30.313498
434.378612	34851.786326	30.318516
435.062257	34882.268844	30.323533
435.140558	34934.255189	30.328551
436.272765	34971.312832	30.333568
436.544236	35017.913711	30.338586
436.845003	35058.048170	30.343604
437.457530	35098.222393	30.348621
437.483223	35145.171867	30.353639
438.353158	35179.337150	30.358656
438.911354	35218.571682	30.363674
439.104895	35256.301649	30.368692
439.777588	35304.218702	30.373709
440.094596	35334.405216	30.378727
440.712089	35383.545093	30.383744
440.737022	35413.783790	30.388762
441.554617	35455.273355	30.393780
441.987046	35501.306310	30.398797
441.994162	35544.655487	30.403815
442.637138	35575.663857	30.408832
442.764620	35620.246286	30.413850
443.204079	35674.106385	30.418868
444.150702	35716.904084	30.423885
444.316564	35767.746929	30.428903
444.633353	35805.464889	30.433920
445.071123	35852.629593	30.438938
445.439074	35904.079739	30.443956
446.351616	35927.540905	30.448973
446.279713	35985.421170	30.453991
447.059540	36031.704367	30.459008
447.718431	36064.810233	30.464026
447.987993	36115.479587	30.469044
448.190072	36158.464348	30.474061
448.719668	36205.191797	30.479079
449.174066	36239.929728	30.484096
449.493722	36286.304525	30.489114
449.846798	36335.987548	30.494132
450.489512	36379.156664	30.499149
450.620748	36423.107860	30.504167
450.885418	36459.760190	30.509184
451.720020	36501.862486	30.514202
451.990079	36547.904163	30.519220
452.635311	36583.264059	30.524237
453.142254	36618.259953	30.529255
453.672973	36646.467277	30.534272
454.636452	36680.974429	30.539290
455.165911	36731.016466	30.544308
455.627594	36764.729731	30.549325
455.807430	36800.731982	30.554343
456.417295	36827.479103	30.559360
456.995988	36861.654768	30.564378
457.524322	36901.516767	30.569396
458.075213	36933.597541	30.574413
458.122955	36981.723749	30.579431
458.418481	37010.961167	30.584448
458.869516	37046.036076	30.589466
459.480195	37090.052660	30.594484
459.850696	37119.727447	30.599501
460.301334	37175.126175	30.604519
460.589606	37216.088700	30.609536
461.025901	37261.562054	30.614554
460.962379	37307.392025	30.619572
461.547517	37355.523427	30.624589
461.970581	37416.523403	30.629607
462.287949	37466.018610	30.634624
462.923716	37515.445090	30.639642
463.020084	37580.670249	30.644660
463.443258	37629.871024	30.649677
463.858336	37682.608074	30.654695
464.229161	37739.329743	30.659712
465.060683	37795.650573	30.664730
465.276892	37853.535015	30.669748
465.853103	37908.821109	30.674765
466.473738	37963.866411	30.679783
466.793866	38024.593342	30.684800
467.239629	38083.770425	30.689818
467.467791	38134.918986	30.694836
468.633817	38180.678380	30.699853
469.527790	38226.916824	30.704871
470.473837	38271.136249	30.709888
471.676513	38311.426439	30.714906
471.737255	38342.574283	30.719924
472.612837	38369.414508	30.724941
472.914910	38407.487158	30.729959
473.446122	38445.119260	30.734976
473.938392	38479.968715	30.739994
474.224786	38509.070475	30.745012
474.731076	38542.058622	30.750029
475.086766	38582.323885	30.755047
475.090872	38623.763618	30.760064
475.664694	38657.715242	30.765082
476.067387	38698.378088	30.770100
476.615376	38729.507088	30.775117
477.275519	38771.046714	30.780135
477.453424	38814.173372	30.785152
477.894926	38860.041367	30.790170
477.817309	38904.447721	30.795188
478.622935	38951.966349	30.800205
478.686257	39000.271690	30.805223
479.252505	39045.962441	30.810240
479.770782	39094.481313	30.815258
479.875567	39154.264922	30.820276
480.464780	39206.383958	30.825293
481.023783	39261.853283	30.830311
480.808612	39316.179190	30.835328
481.535557	39360.599589	30.840346
482.231037	39413.461370	30.845364
482.736351	39447.159350	30.850381
482.875985	39508.051519	30.855399
483.576773	39555.885126	30.860416
484.178477	39605.359668	30.865434
484.380525	39657.287461	30.870452
484.795111	39717.542678	30.875469
485.452848	39766.528171	30.880487
485.682086	39829.304468	30.885504
486.452235	39884.337559	30.890522
486.818307	39940.787471	30.895540
487.838765	39983.550485	30.900557
488.119535	40050.120237	30.905575
488.820910	40095.532734	30.910592
489.436319	40136.512792	30.915610
489.588014	40201.617008	30.920628
490.009111	40251.880228	30.925645
490.521723	40308.358734	30.930663
491.008023	40357.815115	30.935680
491.566467	40417.044155	30.940698
491.838706	40481.377719	30.945716
492.629511	40534.201994	30.950733
492.713433	40583.804127	30.955751
493.243614	40637.776250	30.960768
494.341938	40699.963567	30.965786
494.399278	40758.532054	30.970804
494.905879	40820.192590	30.975821
495.015914	40879.796693	30.980839
495.827792	40945.002103	30.985856
496.459991	40999.654841	30.990874
496.856447	41062.326268	30.995892
497.156010	41108.505834	31.000909
497.965001	41176.071460	31.005927
498.078947	41239.875477	31.010944
498.607257	41300.623216	31.015962
499.356024	41364.625425	31.020980
499.575797	41429.634079	31.025997
500.038474	41492.056022	31.031015
500.758756	41556.822218	31.036032
501.442104	41609.204210	31.041050
501.797184	41673.110860	31.046068
502.748525	41722.092698	31.051085
502.973471	41787.493735	31.056103
503.331713	41848.516292	31.061120
504.306095	41895.205325	31.066138
504.467119	41957.561988	31.071156
505.389825	42017.921044	31.076173
505.519628	42089.934713	31.081191
506.137872	42145.098476	31.086208
507.002227	42200.723499	31.091226
507.528990	42259.469130	31.096244
508.158112	42306.624232	31.101261
508.549793	42359.584987	31.106279
508.760780	42405.281475	31.111296
509.390624	42456.579642	31.116314
509.982242	42523.392828	31.121332
510.428582	42570.475922	31.126349
511.379178	42622.325114	31.131367
511.544831	42689.597671	31.136384
512.246984	42729.772029	31.141402
512.626272	42785.221496	31.146420
513.159862	42845.795565	31.151437
513.592418	42891.705033	31.156455
514.088643	42956.630609	31.161472
514.910089	42997.292780	31.166490
515.062578	43062.576111	31.171508
515.730327	43108.923579	31.176525
516.328692	43156.705179	31.181543
516.746868	43207.785234	31.186560
516.968721	43261.812079	31.191578
517.334444	43314.368045	31.196596
517.745563	43368.409783	31.201613
518.462060	43426.293860	31.206631
518.496205	43478.914798	31.211648
519.479427	43525.251678	31.216666
519.982382	43597.350957	31.221684
520.427829	43654.424164	31.226701
520.791452	43699.606037	31.231719
520.840591	43772.883897	31.236736
521.493286	43832.214882	31.241754
521.779453	43906.556673	31.246772
522.495785	43968.667556	31.251789
523.019855	44029.885212	31.256807
523.347797	44101.374664	31.261824
524.436643	44157.127575	31.266842
524.948126	44218.208559	31.271860
525.175894	44289.613095	31.276877
525.789710	44343.467315	31.281895
526.676951	44403.294428	31.286912
527.810352	44457.105497	31.291930
528.330445	44524.163621	31.296948
528.871303	44567.719122	31.301965
529.844263	44619.240546	31.306983
529.966827	44670.578998	31.312000
530.636297	44720.889392	31.317018
531.105369	44774.115780	31.322036
531.122034	44838.527341	31.327053
532.282979	44887.951449	31.332071
531.900945	44959.137346	31.337088
532.698562	45011.560083	31.342106
533.083207	45071.834595	31.347124
533.470841	45138.149890	31.352141
534.412233	45201.778761	31.357159
534.603215	45266.088337	31.362176
535.273672	45332.916580	31.367194
535.864969	45397.537057	31.372212
536.334638	45451.315305	31.377229
536.851796	45518.281975	31.382247
537.421005	45588.030403	31.387264
537.778605	45638.031125	31.392282
538.922520	45698.422459	31.397300
539.232885	45765.207171	31.402317
540.692685	45821.823393	31.407335
541.084715	45871.654768	31.412352
541.503444	45920.887430	31.417370
542.134271	45967.012553	31.422388
542.769390	46025.592986	31.427405
543.599320	46067.138739	31.432423
543.792259	46119.399401	31.437440
544.219049	46174.843512	31.442458
544.689156	46222.208930	31.447476
545.197434	46273.933455	31.452493
546.320802	46329.148652	31.457511
546.798939	46375.918484	31.462528
547.490736	46416.037839	31.467546
547.849120	46459.359892	31.472564
548.257510	46509.557029	31.477581
548.944454	46562.399263	31.482599
549.140080	46615.736097	31.487616
549.658338	46661.690487	31.492634
550.127413	46712.435273	31.497652
550.315665	46777.091199	31.502669
551.321403	46834.110046	31.507687
551.572415	46889.577114	31.512704
551.982526	46946.651574	31.517722
552.828291	46986.229074	31.522740
553.271321	47044.437353	31.527757
554.156588	47096.028799	31.532775
554.389952	47139.580502	31.537792
555.136274	47183.178477	31.542810
555.278234	47242.984366	31.547828
555.684043	47294.942369	31.552845
556.190724	47349.491156	31.557863
556.490846	47413.644244	31.562880
557.014827	47475.668413	31.567898
557.330606	47537.700054	31.572916
557.691422	47609.252426	31.577933
558.919618	47666.599133	31.582951
559.572180	47722.176158	31.587968
560.398252	47781.465098	31.592986
561.006993	47849.569420	31.598004
561.170146	47911.214759	31.603021
561.768507	47965.314134	31.608039
561.735154	48030.609353	31.613056
562.269553	48105.742235	31.618074
563.204790	48172.531071	31.623092
563.487652	48245.470520	31.628109
564.370861	48309.433581	31.633127
564.590602	48372.532755	31.638144
564.923622	48454.202122	31.643162
565.539670	48516.309602	31.648180
566.271491	48601.877545	31.653197
566.930313	48667.312915	31.658215
567.290179	48755.831006	31.663232
567.620694	48825.348391	31.668250
568.433283	48901.370353	31.673268
568.998270	48975.900257	31.678285
569.789179	49051.078318	31.683303
570.250324	49121.651705	31.688320
571.013928	49190.058434	31.693338
571.726864	49270.083159	31.698356
572.474490	49335.683682	31.703373
572.990370	49398.549491	31.708391
573.677435	49467.222111	31.713408
574.433491	49536.156191	31.718426
575.075202	49604.532630	31.723444
575.199698	49668.820777	31.728461
576.148321	49727.431231	31.733479
576.610723	49797.240924	31.738496
577.561736	49869.119179	31.743514
577.921775	49935.440129	31.748532
578.240044	50010.170202	31.753549
578.949920	50059.878701	31.758567
579.673249	50135.064563	31.763584
580.031427	50201.253699	31.768602
580.901696	50260.345990	31.773620
581.364845	50327.398524	31.778637
581.853365	50401.672950	31.783655
582.552390	50479.122552	31.788672
583.196681	50539.389850	31.793690
583.984158	50611.681992	31.798708
584.496138	50683.701143	31.803725
585.267453	50739.811024	31.808743
585.422508	50810.405881	31.813760
585.770435	50868.354033	31.818778
586.496022	50931.779616	31.823796
586.840061	51013.393053	31.828813
587.365238	51083.937101	31.833831
587.777421	51159.788779	31.838848
588.047510	51236.460215	31.843866
588.462858	51321.442417	31.848884
589.069577	51411.387342	31.853901
590.073816	51477.839605	31.858919
590.505278	51555.075275	31.863936
590.732459	51633.418877	31.868954
591.526329	51705.441339	31.873972
591.969683	51791.104245	31.878989
592.351965	51862.805672	31.884007
593.281308	51941.692084	31.889024
593.603677	52021.161053	31.894042
594.178340	52099.685922	31.899060
594.667071	52181.768021	31.904077
595.479681	52261.857076	31.909095
596.310509	52336.862380	31.914112
596.909076	52429.425861	31.919130
597.658583	52494.908477	31.924148
598.209657	52570.831579	31.929165
599.119723	52647.970595	31.934183
599.472491	52728.924243	31.939200
600.042431	52802.763282	31.944218
600.935242	52882.658393	31.949236
601.635566	52959.375675	31.954253
602.100899	53034.193667	31.959271
603.378886	53102.474419	31.964288
604.206443	53160.049401	31.969306
605.067574	53222.618365	31.974324
605.388792	53291.125444	31.979341
606.268833	53347.230900	31.984359
606.820729	53409.969025	31.989376
607.020719	53473.180082	31.994394
608.104703	53542.220221	31.999412
608.673866	53619.814489	32.004429
609.196311	53686.936997	32.009447
609.941151	53751.120260	32.014464
610.005308	53822.782577	32.019482
610.905382	53886.530569	32.024500
611.182656	53961.361975	32.029517
611.946341	54029.523465	32.034535
612.430447	54099.912169	32.039552
613.107365	54165.993004	32.044570
613.944263	54238.896131	32.049588
614.270642	54308.278653	32.054605
614.861857	54377.449038	32.059623
615.716754	54448.293300	32.064640
615.684855	54525.282233	32.069658
616.605811	54599.280762	32.074676
616.888784	54670.462063	32.079693
618.121836	54749.803948	32.084711
619.003428	54820.107229	32.089728
619.256215	54895.413721	32.094746
619.968452	54967.345052	32.099764
620.409630	55031.737558	32.104781
621.196521	55111.966900	32.109799
622.026869	55175.286290	32.114816
622.422594	55259.741542	32.119834
623.146771	55324.134819	32.124852
623.653369	55398.985472	32.129869
624.467347	55472.307335	32.134887
625.106134	55546.030248	32.139904
625.411588	55619.514477	32.144922
626.207096	55683.840597	32.149940
626.437274	55770.032313	32.154957
627.042372	55848.881319	32.159975
627.575986	55915.672962	32.164992
627.976937	56002.585557	32.170010
628.917189	56078.484280	32.175028
629.342966	56169.000971	32.180045
630.138028	56241.986408	32.185063
630.696034	56311.116984	32.190080
631.321544	56402.419691	32.195098
631.732329	56478.700058	32.200116
632.228015	56565.549229	32.205133
632.728161	56634.461959	32.210151
633.548134	56713.052319	32.215168
633.799692	56792.149665	32.220186
634.257749	56870.955445	32.225204
635.238373	56961.084439	32.230221
636.161063	57048.564669	32.235239
636.821984	57121.478855	32.240256
637.267727	57198.300327	32.245274
638.046823	57277.088804	32.250292
638.610120	57355.873361	32.255309
639.636352	57436.003392	32.260327
640.208192	57509.736499	32.265344
640.992206	57575.708737	32.270362
641.906199	57658.306457	32.275380
642.647971	57732.760473	32.280397
643.291630	57800.305952	32.285415
644.318951	57863.278813	32.290432
645.038405	57933.857143	32.295450
646.020808	57987.046056	32.300468
646.601587	58066.133997	32.305485
647.013384	58124.570920	32.310503
647.643205	58187.182816	32.315520
648.378799	58259.006437	32.320538
649.416986	58322.206647	32.325556
649.250842	58400.975932	32.330573
649.884653	58468.936228	32.335591
650.819739	58537.786280	32.340608
651.216121	58610.752719	32.345626
651.890305	58687.315287	32.350644
652.408027	58760.269502	32.355661
653.087351	58836.869713	32.360679
653.780670	58909.537369	32.365696
654.177768	58998.265260	32.370714
654.520757	59064.215678	32.375732
655.276065	59156.369281	32.380749
656.133856	59235.980978	32.385767
656.558904	59306.615736	32.390784
657.066490	59402.018159	32.395802
657.863415	59483.975822	32.400820
658.351980	59571.469856	32.405837
658.940100	59649.270547	32.410855
659.797225	59737.549303	32.415872
661.017806	59826.948784	32.420890
661.313200	59906.081067	32.425908
662.045781	59995.639876	32.430925
662.672832	60072.055928	32.435943
663.858529	60145.359088	32.440960
664.173659	60229.698748	32.445978
664.829951	60307.351599	32.450996
665.485703	60387.378477	32.456013
666.229109	60470.784704	32.461031
666.709430	60558.922873	32.466048
667.114824	60635.413371	32.471066
667.658150	60721.250823	32.476084
668.763706	60819.166723	32.481101
669.549759	60900.206650	32.486119
670.000651	60984.078206	32.491136
670.403294	61064.798917	32.496154
670.758810	61146.995846	32.501172
671.306342	61247.210026	32.506189
672.027198	61340.972414	32.511207
672.876920	61437.310329	32.516224
673.382400	61531.866785	32.521242
674.250021	61613.896446	32.526260
674.650533	61716.939821	32.531277
675.123061	61806.963736	32.536295
675.843118	61905.792568	32.541312
676.738684	61992.522481	32.546330
677.888311	62071.996379	32.551348
678.354454	62163.212682	32.556365
678.808844	62254.310884	32.561383
679.603240	62337.652127	32.566400
680.449803	62424.486179	32.571418
681.278205	62504.695450	32.576436
681.810648	62581.456935	32.581453
682.713545	62671.625491	32.586471
683.382412	62763.356665	32.591488
684.308159	62844.355755	32.596506
684.405775	62916.191615	32.601524
685.493146	63011.593161	32.606541
686.067760	63101.979278	32.611559
687.696682	63155.584597	32.616576
688.789215	63220.510813	32.621594
689.547505	63286.799976	32.626612
690.149324	63362.324865	32.631629
690.618355	63438.807711	32.636647
691.521126	63505.688900	32.641664
691.925992	63579.915852	32.646682
692.697833	63653.927288	32.651700
693.319037	63728.506973	32.656717
693.693561	63806.721365	32.661735
694.384445	63878.555710	32.666752
694.522934	63966.607564	32.671770
695.268777	64055.260999	32.676788
696.007626	64140.725113	32.681805
696.567802	64236.429137	32.686823
697.298550	64313.190204	32.691840
697.650552	64409.402301	32.696858
698.379894	64496.287229	32.701876
698.802157	64593.318373	32.706893
699.620715	64704.981972	32.711911
700.317628	64794.019198	32.716928
701.090147	64886.507956	32.721946
701.968583	64976.815255	32.726964
702.927176	65050.307734	32.731981
703.658151	65157.169127	32.736999
704.477982	65243.561295	32.742016
705.182341	65343.950940	32.747034
705.729990	65430.829549	32.752052
706.563719	65518.657648	32.757069
707.409634	65610.479118	32.762087
708.364169	65681.403606	32.767104
708.890499	65776.998472	32.772122
709.741343	65865.426557	32.777140
710.709072	65946.935566	32.782157
711.317864	66038.732406	32.787175
712.271562	66113.520319	32.792192
712.955180	66196.594134	32.797210
713.822490	66281.342587	32.802228
714.426254	66366.031292	32.807245
715.072495	66464.155171	32.812263
715.538764	66531.258355	32.817280
716.042724	66620.940024	32.822298
717.095457	66708.231421	32.827316
717.670390	66791.742071	32.832333
718.216519	66880.449331	32.837351
719.040371	66974.400227	32.842368
719.408799	67070.075319	32.847386
719.968271	67162.181506	32.852404
720.958113	67254.568864	32.857421
721.182339	67352.508976	32.862439
721.664969	67447.933324	32.867456
722.716539	67546.637374	32.872474
723.192081	67644.216326	32.877492
723.823500	67730.804720	32.882509
724.632999	67832.029804	32.887527
725.133367	67928.947448	32.892544
726.044146	68013.238939	32.897562
726.967779	68110.502549	32.902580
727.560723	68197.155522	32.907597
728.535064	68303.010532	32.912615
728.739719	68398.437610	32.917632
729.642141	68496.472152	32.922650
730.133787	68592.386882	32.927668
731.001530	68683.741062	32.932685
731.305481	68791.121407	32.937703
732.365967	68885.428471	32.942720
732.904593	68992.241013	32.947738
733.205383	69107.240578	32.952756
734.469133	69211.401320	32.957773
735.201323	69309.218646	32.962791
736.364582	69408.570861	32.967808
737.171572	69504.186296	32.972826
738.082957	69608.441803	32.977844
739.026171	69704.049304	32.982861
739.691910	69798.592471	32.987879
740.161675	69899.657211	32.992896
740.964741	70004.013583	32.997914
741.348294	70107.777508	33.002932
742.276167	70204.453070	33.007949
742.931787	70308.517132	33.012967
743.410428	70413.331212	33.017984
743.997046	70525.639012	33.023002
744.565863	70632.732173	33.028020
745.555440	70745.256438	33.033037
746.309635	70854.588488	33.038055
747.331285	70970.021630	33.043072
747.999543	71087.093751	33.048090
748.669540	71193.388120	33.053108
749.701398	71300.892768	33.058125
749.997231	71416.416200	33.063143
751.107656	71521.072437	33.068160
751.772737	71630.776295	33.073178
752.426238	71743.876739	33.078196
753.883627	71846.491474	33.083213
754.679041	71957.683465	33.088231
755.030824	72057.153800	33.093248
756.208461	72161.092782	33.098266
756.721289	72272.381009	33.103284
758.183391	72366.067768	33.108301
758.440781	72473.850457	33.113319
759.296152	72587.214204	33.118336
760.323068	72683.668041	33.123354
760.998109	72782.976486	33.128372
762.311836	72884.262494	33.133389
762.804224	72981.459745	33.138407
763.533489	73081.064794	33.143424
764.589931	73172.234060	33.148442
765.430091	73261.930242	33.153460
766.194725	73353.133157	33.158477
766.595097	73451.309155	33.163495
767.600751	73543.956922	33.168512
768.357311	73646.169048	33.173530
769.233946	73734.290490	33.178548
769.932133	73839.375081	33.183565
770.557130	73933.553105	33.188583
771.187029	74032.113283	33.193600
772.200605	74115.844612	33.198618
772.706280	74223.912149	33.203636
773.615045	74323.886383	33.208653
774.065576	74421.057419	33.213671
774.819460	74519.219971	33.218688
776.068416	74612.720003	33.223706
776.592738	74712.743217	33.228724
777.153566	74797.776247	33.233741
777.946675	74891.867970	33.238759
778.456689	74982.698292	33.243776
779.532033	75078.355166	33.248794
779.923184	75172.688150	33.253812
780.965146	75265.500843	33.258829
781.376297	75374.423821	33.263847
781.738867	75470.915724	33.268864
782.910363	75580.176481	33.273882
783.158114	75684.540775	33.278900
784.091270	75790.850239	33.283917
785.123362	75903.022266	33.288935
785.233436	76014.553761	33.293952
786.004826	76123.790690	33.298970
786.692458	76244.961275	33.303988
787.633799	76363.736508	33.309005
788.646939	76482.906379	33.314023
789.079909	76603.675072	33.319040
790.041494	76718.091007	33.324058
790.549019	76850.503408	33.329076
791.385462	76967.220181	33.334093
791.799241	77092.858483	33.339111
792.633209	77223.562079	33.344128
793.949108	77345.031869	33.349146
794.250602	77475.617359	33.354164
795.119043	77596.284235	33.359181
796.187150	77727.675650	33.364199
797.292282	77852.943140	33.369216
798.707836	77972.031142	33.374234
799.431123	78093.774398	33.379252
800.241614	78207.890832	33.384269
801.230536	78325.780331	33.389287
801.812732	78444.316775	33.394304
802.609931	78554.091426	33.399322
803.408469	78685.263579	33.404340
804.278183	78790.150397	33.409357
805.372525	78904.427958	33.414375
806.052229	79027.854423	33.419392
806.632544	79139.438984	33.424410
807.159421	79266.349028	33.429428
807.651089	79384.586946	33.434445
808.573017	79517.479355	33.439463
809.534308	79639.572205	33.444480
810.323784	79765.290521	33.449498
811.209576	79887.522971	33.454516
812.263006	80019.662372	33.459533
812.909270	80144.682676	33.464551
814.260111	80262.333684	33.469568
815.470296	80374.166628	33.474586
815.970176	80495.803361	33.479604
816.992620	80600.128294	33.484621
818.067839	80717.127552	33.489639
819.095957	80829.472267	33.494656
820.909628	80923.006717	33.499674
821.824035	81024.220748	33.504692
822.365492	81123.352361	33.509709
823.138998	81216.214466	33.514727
823.889577	81314.528481	33.519744
824.492679	81411.180843	33.524762
825.399137	81525.751942	33.529780
826.316742	81618.896887	33.534797
826.829614	81719.770854	33.539815
827.708152	81833.029894	33.544832
827.872373	81931.349183	33.549850
828.593743	82040.832642	33.554868
829.483395	82150.366193	33.559885
830.677550	82260.498669	33.564903
831.109705	82364.200360	33.569920
832.047394	82463.236615	33.574938
832.515587	82576.119417	33.579956
833.599691	82674.246556	33.584973
834.180626	82782.196403	33.589991
834.393936	82886.390402	33.595008
835.201918	83009.712896	33.600026
835.711113	83131.752294	33.605044
836.486960	83251.862530	33.610061
837.332237	83374.129091	33.615079
837.842281	83500.072511	33.620096
838.967191	83623.272000	33.625114
839.722879	83757.502823	33.630132
840.447448	83886.911516	33.635149
841.531897	84007.230015	33.640167
842.188209	84144.189801	33.645184
843.499178	84268.072504	33.650202
844.407736	84396.263595	33.655220
845.187454	84519.457626	33.660237
845.966236	84657.857868	33.665255
846.850415	84776.791759	33.670272
847.487286	84904.520797	33.675290
848.350709	85040.476711	33.680308
849.451760	85158.643270	33.685325
850.527106	85289.967415	33.690343
851.598449	85414.690869	33.695360
852.489654	85540.697561	33.700378
853.228604	85672.836414	33.705396
854.027249	85805.118582	33.710413
855.026405	85925.496438	33.715431
855.928129	86051.567055	33.720448
857.187450	86168.445750	33.725466
858.198074	86307.197713	33.730484
859.194240	86422.420583	33.735501
859.854717	86536.137802	33.740519
860.742264	86659.653501	33.745536
862.065195	86769.339528	33.750554
862.686992	86891.212412	33.755572
863.572443	87012.068750	33.760589
865.015077	87127.477931	33.765607
865.555937	87246.133510	33.770624
866.821703	87356.274218	33.775642
867.105001	87481.826877	33.780660
867.761385	87586.158475	33.785677
868.993559	87705.468009	33.790695
869.369499	87822.897145	33.795712
870.356278	87936.809469	33.800730
871.380184	88075.377612	33.805748
872.305338	88185.714153	33.810765
873.187591	88299.732952	33.815783
873.992367	88419.074271	33.820800
874.802516	88532.408245	33.825818
876.051915	88659.931011	33.830836
876.871309	88788.763618	33.835853
878.257104	88896.369329	33.840871
878.703119	89016.884459	33.845888
879.784651	89125.438435	33.850906
881.267432	89230.470179	33.855924
881.491152	89344.076494	33.860941
882.473629	89459.845636	33.865959
882.898022	89571.165535	33.870976
884.011678	89693.353130	33.875994
884.817034	89804.322754	33.881012
885.476958	89927.938417	33.886029
886.898632	90035.301818	33.891047
887.749240	90157.279021	33.896064
888.482677	90256.449739	33.901082
889.253473	90383.256360	33.906100
889.810967	90489.438629	33.911117
890.767629	90602.313925	33.916135
891.306695	90723.860599	33.921152
892.001565	90835.687805	33.926170
892.958799	90956.903788	33.931188
893.358325	91077.586556	33.936205
894.386975	91195.750545	33.941223
895.077828	91325.957621	33.946240
895.865335	91453.805397	33.951258
896.440096	91591.294104	33.956276
897.108211	91729.579970	33.961293
897.988712	91864.550549	33.966311
898.567460	92012.142002	33.971328
899.294477	92153.056848	33.976346
900.241317	92306.751891	33.981364
901.154963	92448.145858	33.986381
902.345353	92596.861128	33.991399
902.947842	92747.316889	33.996416
903.984689	92905.107456	34.001434
904.882229	93059.827981	34.006452
905.445548	93217.681624	34.011469
906.593995	93370.349112	34.016487
907.356939	93534.954242	34.021504
907.603827	93698.208765	34.026522
908.726451	93854.381026	34.031540
909.406008	94036.113387	34.036557
910.617641	94202.236223	34.041575
911.569595	94371.201872	34.046592
912.650702	94536.054042	34.051610
913.576503	94701.007459	34.056628
914.317986	94855.267055	34.061645
915.627906	95030.898304	34.066663
916.810260	95186.421453	34.071680
917.928569	95347.900352	34.076698
918.877568	95492.319542	34.081716
919.915662	95660.708279	34.086733
921.071438	95815.249994	34.091751
921.792408	95991.676032	34.096768
922.788634	96143.189415	34.101786
923.888420	96297.919736	34.106804
924.625384	96463.888072	34.111821
925.793454	96618.850126	34.116839
926.936915	96770.140648	34.121856
927.512346	96933.170472	34.126874
928.528891	97095.726418	34.131892
929.043533	97261.201334	34.136909
929.979503	97415.024706	34.141927
930.995117	97585.924527	34.146944
931.819527	97751.695764	34.151962
932.756486	97911.745669	34.156980
933.750371	98089.573139	34.161997
934.834460	98241.425066	34.167015
935.853122	98407.574953	34.172032
936.533534	98579.217134	34.177050
937.696241	98737.752606	34.182068
938.222862	98917.179087	34.187085
939.370341	99092.427271	34.192103
940.428340	99258.676819	34.197120
941.432410	99420.523927	34.202138
942.693929	99588.835085	34.207156
942.880582	99762.563920	34.212173
943.845286	99916.711725	34.217191
944.980505	100093.754801	34.222208
945.811670	100265.940161	34.227226
947.241230	100422.147443	34.232244
947.969085	100602.667403	34.237261
948.823912	100767.561932	34.242279
949.842264	100928.045099	34.247296
950.657032	101089.625889	34.252314
952.045277	101246.376064	34.257332
952.910119	101405.478336	34.262349
953.784752	101552.751041	34.267367
955.050308	101708.432305	34.272384
955.894890	101864.636641	34.277402
956.826245	102022.818644	34.282420
957.656606	102179.090088	34.287437
958.809817	102352.592584	34.292455
959.770163	102499.285563	34.297472
960.672893	102647.649118	34.302490
961.763182	102804.212462	34.307508
962.550330	102981.135428	34.312525
963.216653	103129.119749	34.317543
964.607584	103292.738477	34.322560
965.259851	103451.642976	34.327578
966.316183	103626.701450	34.332596
967.050630	103794.634868	34.337613
968.093184	103946.076014	34.342631
969.694941	104092.954526	34.347648
970.603475	104268.102891	34.352666
971.804554	104412.725229	34.357684
972.741921	104586.159026	34.362701
974.019317	104748.116281	34.367719
975.109071	104902.470621	34.372736
975.649388	105065.939554	34.377754
976.707165	105227.477028	34.382772
977.609366	105398.156337	34.387789
978.321810	105555.552462	34.392807
979.292680	105712.388982	34.397824
980.274278	105883.920528	34.402842
980.926376	106051.459625	34.407860
981.471562	106239.646664	34.412877
982.904014	106408.282613	34.417895
983.839502	106580.002397	34.422912
984.614922	106763.806981	34.427930
985.668910	106938.198210	34.432948
986.493127	107131.989182	34.437965
987.213952	107301.958255	34.442983
988.432048	107481.614273	34.448000
989.378669	107665.980169	34.453018
990.951071	107848.714717	34.458036
991.956891	108032.172972	34.463053
992.595467	108207.485256	34.468071
993.678136	108385.708883	34.473088
994.945042	108574.974977	34.478106
995.907412	108743.404274	34.483124
997.075292	108931.533843	34.488141
998.076685	109114.453209	34.493159
999.053688	109277.315797	34.498176
1000.201613	109450.322694	34.503194
1001.631035	109627.040022	34.508212
1002.344862	109809.412014	34.513229
1003.528634	109973.589676	34.518247
1004.522373	110149.084336	34.523264
1005.561925	110328.922452	34.528282
1006.140147	110499.398624	34.533300
1007.752402	110668.990865	34.538317
1008.518433	110836.940973	34.543335
1010.151462	111010.209282	34.548352
1011.093604	111183.548561	34.553370
1012.401046	111338.036956	34.558388
1013.077666	111505.408166	34.563405
1014.246749	111680.603932	34.568423
1015.409264	111836.677058	34.573440
1015.988788	112008.060662	34.578458
1017.511361	112157.090970	34.583476
1018.510684	112330.185885	34.588493
1019.022299	112486.794939	34.593511
1020.366260	112632.050497	34.598528
1021.022525	112798.454375	34.603546
1021.948935	112948.291506	34.608564
1022.493245	113114.841190	34.613581
1023.568463	113272.189763	34.618599
1024.434152	113429.457680	34.623616
1025.291362	113600.678528	34.628634
1026.528817	113771.409435	34.633652
1027.265833	113948.928684	34.638669
1028.351876	114126.000981	34.643687
1029.688334	114290.707147	34.648704
1030.540471	114463.518193	34.653722
1031.776431	114639.466081	34.658740
1032.707663	114818.506460	34.663757
1033.588473	114986.077359	34.668775
1034.883481	115154.573460	34.673792
1035.401275	115336.369919	34.678810
1036.563227	115516.658569	34.683828
1037.563869	115706.270272	34.688845
1038.473264	115889.885273	34.693863
1039.287082	116070.992126	34.698880
1040.181163	116265.887021	34.703898
1041.420392	116445.330955	34.708916
1042.121603	116642.515698	34.713933
1043.353016	116833.314633	34.718951
1044.404849	117031.664169	34.723968
1045.031361	117229.789610	34.728986
1046.331659	117429.624410	34.734004
1047.716172	117630.195441	34.739021
1048.376886	117830.094442	34.744039
1049.525517	118025.148860	34.749056
1050.382558	118227.517999	34.754074
1051.719603	118425.817508	34.759092
1052.780967	118628.879796	34.764109
1053.874883	118842.174410	34.769127
1054.621100	119031.233819	34.774144
1055.611558	119253.476813	34.779162
1056.663729	119443.124579	34.784180
1057.903185	119664.100553	34.789197
1058.648123	119875.121554	34.794215
1060.119656	120074.879967	34.799232
1060.950952	120294.845240	34.804250
1062.191358	120492.891476	34.809268
1063.267606	120711.082914	34.814285
1064.272620	120927.130255	34.819303
1065.523079	121128.362116	34.824320
1066.646993	121349.403828	34.829338
1067.702404	121552.507770	34.834356
1069.266082	121763.119053	34.839373
1070.950622	121950.701120	34.844391
1072.044226	122139.886174	34.849408
1073.115431	122342.458927	34.854426
1074.405556	122536.372206	34.859444
1075.339036	122732.473468	34.864461
1076.077803	122931.029164	34.869479
1077.074051	123125.156242	34.874496
1078.041534	123329.475542	34.879514
1079.008045	123528.429877	34.884532
1080.429692	123735.318826	34.889549
1081.263248	123938.913728	34.894567
1082.057245	124137.263787	34.899584
1083.229964	124345.717188	34.904602
1084.374474	124552.488808	34.909620
1085.430820	124757.385022	34.914637
1086.552696	124965.545107	34.919655
1087.825542	125165.804322	34.924672
1088.543670	125375.184184	34.929690
1089.600256	125565.444172	34.934708
1090.805171	125763.420685	34.939725
1091.432236	125965.104338	34.944743
1092.645806	126149.240150	34.949760
1093.946473	126358.089799	34.954778
1094.877787	126553.575589	34.959796
1095.943383	126754.737728	34.964813
1096.879345	126959.029463	34.969831
1098.217529	127164.375697	34.974848
1098.946858	127369.095101	34.979866
1100.179155	127573.571834	34.984884
1101.476674	127773.332380	34.989901
1102.744443	127985.684378	34.994919
1103.879953	128183.163150	34.999936
1104.771516	128404.013285	35.004954
1105.736683	128599.072000	35.009972
1107.312411	128806.495238	35.014989
1108.793780	129015.812041	35.020007
1109.885332	129213.454775	35.025024
1110.773772	129419.948229	35.030042
1112.123969	129616.118628	35.035060
1113.320196	129827.907451	35.040077
1114.331117	130039.193443	35.045095
1115.218497	130236.657194	35.050112
1116.332201	130452.509506	35.055130
1117.172159	130654.423430	35.060148
1118.158631	130867.290653	35.065165
1119.523502	131084.604019	35.070183
1120.887134	131296.665704	35.075200
1122.279604	131511.781813	35.080218
1123.068782	131715.852978	35.085236
1123.877329	131925.974485	35.090253
1124.861181	132154.493362	35.095271
1125.796662	132373.847120	35.100288
1127.227112	132596.613877	35.105306
1127.787833	132833.526323	35.110324
1129.127741	133058.720460	35.115341
1130.215851	133299.245291	35.120359
1131.249012	133534.717130	35.125376
1132.232598	133759.551876	35.130394
1133.346154	134012.093099	35.135412
1134.348463	134230.938033	35.140429
1135.168311	134469.379398	35.145447
1136.643820	134715.434481	35.150464
1137.611318	134958.728021	35.155482
1138.909598	135193.697571	35.160500
1140.438035	135427.832870	35.165517
1141.391510	135674.672826	35.170535
1142.554032	135913.372713	35.175552
1143.722002	136159.280750	35.180570
1144.646886	136400.469499	35.185588
1146.102661	136639.216092	35.190605
1146.806253	136891.101528	35.195623
1148.027356	137121.232841	35.200640
1149.453117	137375.279365	35.205658
1150.517016	137615.830893	35.210676
1151.954735	137856.337833	35.215693
1153.377546	138102.140178	35.220711
1154.738602	138329.362185	35.225728
1155.926766	138566.916938	35.230746
1157.301187	138805.776227	35.235764
1158.763691	139027.833415	35.240781
1159.823715	139263.761976	35.245799
1160.950634	139500.709179	35.250816
1162.234261	139719.688411	35.255834
1163.253091	139956.223320	35.260852
1164.523522	140182.250101	35.265869
1165.468447	140406.844077	35.270887
1166.996147	140622.679973	35.275904
1168.347750	140845.765568	35.280922
1169.124886	141061.441728	35.285940
1170.509622	141266.959697	35.290957
1171.347647	141492.235392	35.295975
1172.368144	141707.889016	35.300992
1173.391891	141929.114546	35.306010
1174.580237	142155.797956	35.311028
1175.825587	142360.657023	35.316045
1176.545441	142591.908532	35.321063
1178.017160	142829.452622	35.326080
1179.290805	143054.007334	35.331098
1180.363491	143282.097405	35.336116
1181.200268	143508.677071	35.341133
1182.479704	143754.429118	35.346151
1183.734419	143980.729738	35.351168
1185.097261	144211.748508	35.356186
1186.317765	144448.362365	35.361204
1187.321794	144683.780101	35.366221
1188.124798	144928.013278	35.371239
1189.661293	145158.958427	35.376256
1190.674366	145409.062845	35.381274
1191.779444	145658.659089	35.386292
1193.031865	145893.561229	35.391309
1193.453904	146155.045233	35.396327
1195.202605	146411.360153	35.401344
1196.254698	146657.580669	35.406362
1197.057865	146933.452948	35.411380
1198.631475	147171.306043	35.416397
1199.265723	147441.305406	35.421415
1200.401016	147703.383632	35.426432
1201.920973	147967.624181	35.431450
1203.146987	148230.934720	35.436468
1204.481372	148495.054642	35.441485
1205.681904	148766.723754	35.446503
1206.861217	149027.862366	35.451520
1208.195615	149287.708666	35.456538
1209.350912	149558.144956	35.461556
1210.992939	149814.036154	35.466573
1212.115995	150090.407884	35.471591
1213.176819	150353.843566	35.476608
1214.560237	150619.134030	35.481626
1215.426149	150876.103731	35.486644
1217.137214	151150.840182	35.491661
1218.326363	151414.438588	35.496679
1219.783824	151676.904596	35.501696
1221.564095	151939.537106	35.506714
1222.901702	152202.671741	35.511732
1224.506916	152441.114343	35.516749
1225.699148	152697.787530	35.521767
1226.998068	152944.442376	35.526784
1228.433604	153181.112143	35.531802
1229.507527	153434.925673	35.536820
1231.228761	153680.552871	35.541837
1232.123447	153926.678649	35.546855
1233.377872	154171.517834	35.551872
1234.960662	154420.102242	35.556890
1236.130518	154650.586817	35.561908
1237.924671	154886.648958	35.566925
1238.918522	155125.376224	35.571943
1240.174818	155364.418830	35.576960
1241.142321	155604.167738	35.581978
1241.950668	155841.263989	35.586996
1243.356221	156087.737890	35.592013
1244.493352	156339.840493	35.597031
1245.529875	156582.489658	35.602048
1246.769810	156836.685604	35.607066
1247.576819	157082.114804	35.612084
1249.007669	157319.449582	35.617101
1250.543572	157550.929188	35.622119
1251.426312	157786.256947	35.627136
1252.724319	158020.047993	35.632154
1253.581001	158254.086756	35.637172
1255.206881	158500.447227	35.642189
1255.992199	158738.929619	35.647207
1257.755022	158987.212974	35.652224
1259.393001	159224.103823	35.657242
1260.023000	159466.904350	35.662260
1261.033803	159714.648193	35.667277
1262.386102	159967.113043	35.672295
1263.817062	160218.690612	35.677312
1264.650664	160470.134181	35.682330
1265.518806	160730.929986	35.687348
1266.949109	160987.322352	35.692365
1267.852586	161248.140145	35.697383
1268.855789	161527.555342	35.702400
1270.118486	161794.311520	35.707418
1271.423346	162078.023852	35.712436
1272.493541	162352.341111	35.717453
1274.181557	162630.777873	35.722471
1275.124967	162905.320446	35.727488
1276.533352	163187.180492	35.732506
1277.611697	163474.997103	35.737524
1278.790551	163756.590807	35.742541
1279.844975	164050.050762	35.747559
1281.085166	164333.110066	35.752576
1282.848981	164617.840694	35.757594
1283.661815	164914.465551	35.762612
1285.159130	165204.776000	35.767629
1286.570357	165508.699116	35.772647
1287.799780	165802.190080	35.777664
1289.493602	166092.156126	35.782682
1290.531348	166395.836914	35.787700
1292.215620	166684.702330	35.792717
1293.659830	166980.526262	35.797735
1295.152877	167289.027928	35.802752
1296.767644	167575.635167	35.807770
1297.993569	167860.755410	35.812788
1299.325539	168144.984104	35.817805
1300.750356	168430.151672	35.822823
1302.026927	168724.802904	35.827840
1303.532442	169002.913228	35.832858
1304.912230	169282.098165	35.837876
1306.206582	169558.059751	35.842893
1307.766036	169858.956423	35.847911
1309.457818	170135.289673	35.852928
1310.694594	170421.738803	35.857946
1311.728432	170703.764005	35.862964
1312.997494	170982.134670	35.867981
1314.428270	171253.027609	35.872999
1315.630876	171546.685875	35.878016
1317.260880	171826.907785	35.883034
1318.491129	172106.266370	35.888052
1319.696505	172386.683773	35.893069
1320.883048	172668.578082	35.898087
1322.237297	172956.453221	35.903104
1323.509825	173235.377535	35.908122
1324.407478	173524.418249	35.913140
1325.869867	173815.035051	35.918157
1327.269345	174104.773906	35.923175
1328.036620	174406.764786	35.928192
1329.666523	174693.028535	35.933210
1330.565830	174991.331197	35.938228
1331.980215	175292.284433	35.943245
1333.556638	175567.474135	35.948263
1334.800429	175861.370563	35.953280
1336.679495	176133.086252	35.958298
1337.225477	176425.138370	35.963316
1338.565953	176697.714805	35.968333
1340.059142	176981.722199	35.973351
1341.619031	177275.472531	35.978368
1342.971831	177542.005286	35.983386
1343.921089	177832.805477	35.988404
1344.949581	178116.457636	35.993421
1346.497568	178410.391495	35.998439
1347.932219	178707.721934	36.003456
1349.277301	178997.981514	36.008474
1350.174129	179297.582312	36.013492
1351.862236	179597.187249	36.018509
1352.991247	179891.572585	36.023527
1354.117851	180190.784839	36.028544
1355.859709	180492.898725	36.033562
1357.245497	180795.424917	36.038580
1358.566351	181105.835661	36.043597
1360.298439	181405.160293	36.048615
1361.359786	181718.153517	36.053632
1362.884327	182014.007633	36.058650
1363.539313	182325.796570	36.063668
1365.083479	182637.193361	36.068685
1366.812368	182941.755444	36.073703
1368.103848	183269.677483	36.078720
1369.713384	183571.136196	36.083738
1371.081644	183886.526733	36.088756
1371.997506	184205.214745	36.093773
1373.573519	184526.797521	36.098791
1374.578884	184854.490217	36.103808
1376.262064	185167.016211	36.108826
1377.767543	185502.125451	36.113844
1379.003656	185815.485380	36.118861
1380.656496	186140.921911	36.123879
1381.913832	186457.150576	36.128896
1383.294440	186805.821451	36.133914
1384.762526	187178.761781	36.138932
1386.515621	187492.655365	36.143949
1388.364759	187817.583712	36.148967
1389.839256	188133.808733	36.153984
1391.461693	188443.077339	36.159002
1392.959505	188755.846106	36.164020
1394.254843	189068.266440	36.169037
1395.629094	189379.405282	36.174055
1396.922444	189697.999885	36.179072
1398.496952	190006.670672	36.184090
1399.656428	190317.515469	36.189108
1400.913860	190639.013914	36.194125
1402.950553	190942.306151	36.199143
1403.957777	191251.983420	36.204160
1405.857453	191574.526888	36.209178
1407.318199	191886.217643	36.214196
1408.705512	192185.245739	36.219213
1410.140746	192500.142531	36.224231
1411.591456	192811.278374	36.229248
1413.024458	193103.951316	36.234266
1414.541667	193424.019368	36.239284
1415.645647	193725.762569	36.244301
1417.081688	194039.164389	36.249319
1418.766333	194358.217898	36.254336
1419.827564	194666.167833	36.259354
1421.133286	194982.818237	36.264372
1422.578645	195294.494273	36.269389
1424.472042	195591.190296	36.274407
1425.929646	195901.722736	36.279424
1427.649424	196204.162566	36.284442
1428.602810	196506.672201	36.289460
1429.658042	196808.633105	36.294477
1431.706192	197103.479184	36.299495
1432.580885	197407.730344	36.304512
1433.823438	197705.142293	36.309530
1435.157902	197995.148534	36.314548
1436.247605	198295.532191	36.319565
1437.840338	198605.566631	36.324583
1439.038596	198915.307814	36.329600
1440.555350	199227.692374	36.334618
1442.021985	199533.379264	36.339636
1443.179531	199849.555376	36.344653
1444.788720	200157.862964	36.349671
1445.666031	200484.626065	36.354688
1447.250778	200800.889572	36.359706
1448.501597	201136.765701	36.364724
1450.052221	201466.549815	36.369741
1451.322936	201789.849961	36.374759
1452.683471	202115.981720	36.379776
1454.108172	202449.242133	36.384794
1455.428878	202797.710152	36.389812
1456.701274	203135.415709	36.394829
1459.007025	203478.167680	36.399847
1459.985884	203833.194226	36.404864
1461.261910	204161.121034	36.409882
1463.093673	204510.325128	36.414900
1464.186229	204861.880987	36.419917
1466.009931	205206.997717	36.424935
1467.546884	205555.817928	36.429952
1468.749875	205898.365667	36.434970
1470.534733	206245.344617	36.439988
1471.939117	206597.972340	36.445005
1473.566759	206945.408868	36.450023
1474.739789	207301.808171	36.455040
1475.967313	207658.377324	36.460058
1477.578006	208024.260822	36.465076
1479.062019	208381.680039	36.470093
1480.834107	208746.218410	36.475111
1482.034592	209112.955255	36.480128
1483.466319	209483.568547	36.485146
1485.433588	209827.552047	36.490164
1486.999771	210207.569962	36.495181
1488.627287	210558.999961	36.500199
1489.760219	210923.336556	36.505216
1490.971262	211291.522720	36.510234
1492.677144	211656.710493	36.515252
1493.534574	212033.259871	36.520269
1495.084771	212406.144779	36.525287
1497.001652	212777.397708	36.530304
1498.658077	213141.527998	36.535322
1499.900194	213522.769382	36.540340
1501.906503	213903.815366	36.545357
1503.529592	214256.621993	36.550375
1505.378366	214627.938361	36.555392
1507.168973	214997.409717	36.560410
1508.949581	215348.516043	36.565428
1510.163978	215712.006729	36.570445
1511.917101	216065.505913	36.575463
1513.296749	216425.160754	36.580480
1515.477018	216783.496585	36.585498
1517.663220	217129.587082	36.590516
1518.712962	217479.920310	36.595533
1520.903487	217813.562680	36.600551
1522.180347	218158.017902	36.605568
1523.372230	218506.322625	36.610586
1525.043580	218843.705015	36.615604
1525.926050	219192.541224	36.620621
1527.522206	219544.009544	36.625639
1528.791234	219889.127426	36.630656
1529.973281	220231.744081	36.635674
1531.470906	220581.424615	36.640692
1532.532790	220944.332772	36.645709
1533.991258	221287.363848	36.650727
1535.253709	221637.970718	36.655744
1536.721818	221994.134402	36.660762
1538.297958	222343.549201	36.665780
1539.769276	222707.155962	36.670797
1540.904091	223057.224291	36.675815
1542.659355	223418.729031	36.680832
1543.854818	223792.540806	36.685850
1545.414225	224160.452731	36.690868
1546.642822	224543.557300	36.695885
1548.261861	224920.427594	36.700903
1550.111040	225299.243398	36.705920
1551.505930	225665.733106	36.710938
1553.186235	226053.949431	36.715956
1554.428752	226439.109541	36.720973
1555.784448	226823.642196	36.725991
1557.791302	227221.740274	36.731008
1559.222110	227613.628221	36.736026
1561.155841	227987.578312	36.741044
1562.479889	228385.884601	36.746061
1564.645790	228768.587947	36.751079
1566.224672	229145.413090	36.756096
1567.600991	229533.777825	36.761114
1569.443127	229927.531361	36.766132
1571.278111	230318.796246	36.771149
1572.819335	230705.026117	36.776167
1574.461007	231087.632702	36.781184
1575.644474	231479.430813	36.786202
1577.720309	231875.128257	36.791220
1578.851163	232272.497576	36.796237
1580.428640	232661.464241	36.801255
1581.752390	233057.227776	36.806272
1583.397181	233457.513465	36.811290
1585.513902	233859.681069	36.816308
1586.406758	234258.788181	36.821325
1588.205564	234656.305138	36.826343
1589.787496	235056.396052	36.831360
1591.496810	235472.394804	36.836378
1593.216596	235874.394025	36.841396
1594.459480	236288.356397	36.846413
1596.438213	236681.016474	36.851431
1598.225457	237088.491013	36.856448
1599.599161	237497.299971	36.861466
1601.540014	237896.772760	36.866484
1602.944637	238316.321575	36.871501
1604.476239	238716.771909	36.876519
1605.994966	239123.142742	36.881536
1607.879436	239540.557081	36.886554
1609.719869	239942.049762	36.891572
1611.584992	240349.025128	36.896589
1613.301697	240751.552121	36.901607
1615.470402	241136.835130	36.906624
1616.761183	241540.392884	36.911642
1618.339085	241943.473200	36.916660
1620.046122	242336.981046	36.921677
1621.543685	242742.790740	36.926695
1623.250907	243143.765734	36.931712
1624.445457	243546.928708	36.936730
1626.434295	243949.865036	36.941748
1627.883853	244347.321770	36.946765
1629.277192	244755.354171	36.951783
1630.843229	245155.636282	36.956800
1632.196273	245570.913196	36.961818
1633.899440	245982.374850	36.966836
1635.845822	246387.116672	36.971853
1637.197170	246792.484224	36.976871
1638.720968	247188.882209	36.981888
1640.314985	247591.237956	36.986906
1642.117135	247968.106961	36.991924
1643.426298	248356.915260	36.996941
1645.079468	248762.815464	37.001959
1646.934172	249146.075126	37.006976
1648.458620	249554.737057	37.011994
1649.838589	249951.430773	37.017012
1651.517061	250351.328294	37.022029
1653.422766	250755.787043	37.027047
1654.806982	251167.388136	37.032064
1655.841694	251581.100406	37.037082
1657.932339	251988.422867	37.042100
1659.200595	252412.663526	37.047117
1660.471276	252841.144694	37.052135
1662.242820	253264.973944	37.057152
1663.623279	253708.854197	37.062170
1665.316908	254139.170475	37.067188
1666.661742	254579.649790	37.072205
1668.243552	255027.253799	37.077223
1670.151550	255469.394835	37.082240
1671.917219	255921.590156	37.087258
1673.111591	256361.680830	37.092276
1675.182618	256823.782498	37.097293
1676.724172	257278.649915	37.102311
1678.387864	257743.199702	37.107328
1679.794853	258192.166508	37.112346
1682.188196	258660.180194	37.117364
1683.447577	259127.607530	37.122381
1685.382955	259602.572789	37.127399
1686.978815	260052.239767	37.132416
1688.658953	260519.087780	37.137434
1690.593072	260973.803709	37.142452
1692.399889	261443.041158	37.147469
1694.416920	261916.434741	37.152487
1696.238974	262375.582139	37.157504
1698.253131	262847.041805	37.162522
1699.792730	263302.800550	37.167540
1701.567497	263761.619293	37.172557
1702.990901	264225.240715	37.177575
1704.594998	264692.895688	37.182592
1706.620010	265162.717802	37.187610
1708.868757	265614.875828	37.192628
1710.881266	266067.906964	37.197645
1712.802098	266532.430647	37.202663
1714.897351	266981.177677	37.207680
1716.448169	267431.226979	37.212698
1718.667598	267875.759689	37.217716
1720.538332	268318.846402	37.222733
1722.221340	268760.334936	37.227751
1723.944895	269192.036787	37.232768
1725.690239	269651.036026	37.237786
1727.651162	270076.321714	37.242804
1729.253159	270527.922818	37.247821
1730.862338	270974.263236	37.252839
1732.863084	271410.304972	37.257856
1734.056159	271858.661667	37.262874
1735.591181	272294.873489	37.267892
1737.715573	272742.495762	37.272909
1739.188090	273179.804969	37.277927
1741.461728	273617.164342	37.282944
1743.046488	274075.429125	37.287962
1744.962999	274512.179409	37.292980
1746.579940	274955.831298	37.297997
1748.300751	275390.931391	37.303015
1750.197513	275825.823851	37.308032
1751.763235	276270.492434	37.313050
1753.586334	276702.877471	37.318068
1755.412650	277118.066747	37.323085
1756.806723	277543.657474	37.328103
1758.699324	277961.574630	37.333120
1760.359824	278384.046215	37.338138
1761.942810	278808.635404	37.343156
1763.796749	279224.926445	37.348173
1765.570893	279655.245655	37.353191
1767.264927	280076.889933	37.358208
1768.902518	280506.032058	37.363226
1770.763177	280937.117550	37.368244
1772.407658	281373.287798	37.373261
1773.736469	281814.329712	37.378279
1775.481616	282258.351058	37.383296
1776.394071	282710.346643	37.388314
1778.528578	283168.572715	37.393332
1779.955421	283635.311787	37.398349
1781.589780	284089.750298	37.403367
1783.173487	284551.760917	37.408384
1784.275860	285044.010604	37.413402
1786.142113	285510.922171	37.418420
1788.685725	285979.527398	37.423437
1790.537485	286464.285637	37.428455
1792.475237	286946.056001	37.433472
1794.295773	287425.505128	37.438490
1795.947122	287916.251218	37.443508
1798.002130	288390.933685	37.448525
1799.858859	288877.628477	37.453543
1801.861911	289362.544678	37.458560
1803.207659	289853.171474	37.463578
1804.933129	290352.291775	37.468596
1806.789728	290839.834812	37.473613
1808.238776	291349.527537	37.478631
1810.293545	291851.351843	37.483648
1812.132753	292352.190164	37.488666
1813.810037	292852.795799	37.493684
1815.662735	293349.205928	37.498701
1817.434864	293867.205581	37.503719
1819.390590	294368.110432	37.508736
1821.216104	294887.895440	37.513754
1822.751969	295390.609121	37.518772
1824.778741	295915.507408	37.523789
1826.162874	296442.989536	37.528807
1827.993000	296962.780594	37.533824
1829.783532	297494.810044	37.538842
1831.208968	298018.869124	37.543860
1833.251893	298550.569832	37.548877
1835.392176	299079.939995	37.553895
1837.568399	299602.749644	37.558912
1839.358418	300140.770569	37.563930
1841.400793	300673.770958	37.568948
1843.241100	301189.535133	37.573965
1845.351391	301718.198918	37.578983
1847.688541	302231.489031	37.584000
1850.375048	302748.095763	37.589018
1852.200446	303262.319034	37.594036
1854.035976	303761.507793	37.599053
1856.091872	304277.766537	37.604071
1858.287154	304771.634639	37.609088
1860.124596	305279.236042	37.614106
1862.052233	305784.152965	37.619124
1863.980495	306277.921326	37.624141
1865.809229	306780.153092	37.629159
1867.858983	307259.271937	37.634176
1869.876168	307759.915973	37.639194
1871.469902	308248.107546	37.644212
1873.748306	308738.243109	37.649229
1875.175651	309246.299803	37.654247
1877.326234	309718.525703	37.659264
1878.886368	310208.352702	37.664282
1880.673462	310683.088030	37.669300
1881.951154	311159.852690	37.674317
1883.500669	311635.123318	37.679335
1884.704481	312124.377209	37.684352
1886.075019	312627.356058	37.689370
1887.598577	313127.386834	37.694388
1889.769491	313644.873739	37.699405
1891.212929	314164.270610	37.704423
1893.160966	314680.131069	37.709440
1894.752673	315201.371017	37.714458
1896.488264	315728.444919	37.719476
1898.736603	316255.178640	37.724493
1900.243030	316801.817107	37.729511
1902.282013	317337.047077	37.734528
1905.253963	317858.243153	37.739546
1906.888446	318397.507804	37.744564
1909.246893	318918.330490	37.749581
1910.683182	319467.509875	37.754599
1912.795121	320001.934530	37.759616
1914.446426	320536.678376	37.764634
1916.452592	321085.138918	37.769652
1918.421582	321632.760821	37.774669
1919.909170	322174.208738	37.779687
1922.006779	322727.150394	37.784704
1923.459010	323288.787565	37.789722
1925.196121	323852.783089	37.794740
1927.489021	324421.758650	37.799757
1929.777147	324990.828568	37.804775
1931.904506	325549.386005	37.809792
1933.868490	326112.579106	37.814810
1935.700780	326669.797148	37.819828
1938.042082	327223.553375	37.824845
1940.453613	327788.276742	37.829863
1942.972015	328339.985397	37.834880
1945.258371	328881.878832	37.839898
1947.496163	329429.277752	37.844916
1949.652760	329963.540067	37.849933
1951.678045	330526.077337	37.854951
1953.655815	331058.272244	37.859968
1955.548011	331589.534532	37.864986
1957.357147	332128.235431	37.870004
1959.179744	332669.463425	37.875021
1961.014850	333214.258598	37.880039
1963.024795	333770.991982	37.885056
1964.942177	334308.757016	37.890074
1966.856697	334872.185857	37.895092
1968.891144	335423.310090	37.900109
1970.455553	335971.658662	37.905127
1971.920192	336530.566742	37.910144
1973.608029	337091.206924	37.915162
1975.330256	337662.689213	37.920180
1977.646435	338237.950301	37.925197
1979.392719	338815.041483	37.930215
1980.850325	339389.048826	37.935232
1983.022361	339969.428113	37.940250
1984.563819	340567.422203	37.945268
1986.763138	341145.241667	37.950285
1988.151330	341746.181744	37.955303
1990.084254	342349.486316	37.960320
1992.168673	342955.242088	37.965338
1993.843984	343558.236237	37.970356
1996.043317	344160.503826	37.975373
1998.115202	344763.795140	37.980391
1999.839955	345370.122461	37.985408
2002.171746	345973.250188	37.990426
2004.243267	346583.913892	37.995444
2006.144859	347181.483071	38.000461
2008.542588	347774.906744	38.005479
2010.867759	348353.877718	38.010496
2013.066284	348923.603244	38.015514
2014.998265	349502.995900	38.020532
2017.438721	350076.111983	38.025549
2019.483881	350655.086159	38.030567
2021.445070	351228.130139	38.035584
2024.074465	351790.435971	38.040602
2025.695450	352363.436918	38.045620
2027.937460	352939.170015	38.050637
2029.861748	353518.288994	38.055655
2031.751655	354085.740659	38.060672
2033.841115	354672.088817	38.065690
2035.320852	355248.710403	38.070708
2037.491825	355837.838017	38.075725
2039.239365	356424.967340	38.080743
2041.012503	357026.708512	38.085760
2042.902121	357616.632186	38.090778
2044.544279	358241.134001	38.095796
2047.117261	358836.073134	38.100813
2048.985890	359456.002602	38.105831
2050.876069	360063.597121	38.110848
2052.946546	360673.254989	38.115866
2054.767640	361295.790156	38.120884
2057.269639	361917.470788	38.125901
2059.176753	362536.392807	38.130919
2061.178432	363161.395208	38.135936
2063.572637	363790.707512	38.140954
2065.193240	364424.131664	38.145972
2067.280513	365060.712999	38.150989
2069.329569	365697.184999	38.156007
2071.329638	366344.699824	38.161024
2073.385035	366991.963358	38.166042
2075.775275	367633.888966	38.171060
2077.727797	368286.207495	38.176077
2079.831619	368938.918147	38.181095
2081.711671	369585.668680	38.186112
2084.063331	370235.751284	38.191130
2086.058916	370890.435358	38.196148
2088.185337	371544.475494	38.201165
2090.167022	372203.691583	38.206183
2092.230404	372867.059647	38.211200
2094.765737	373521.014362	38.216218
2096.965317	374186.508090	38.221236
2099.079491	374828.969952	38.226253
2101.373572	375499.483656	38.231271
2103.362336	376166.076512	38.236288
2105.650490	376818.698442	38.241306
2107.444655	377489.367422	38.246324
2109.813053	378151.291727	38.251341
2112.351455	378814.363469	38.256359
2114.663446	379461.116127	38.261376
2117.248422	380114.294510	38.266394
2118.944161	380775.599619	38.271412
2121.487709	381413.073527	38.276429
2123.730497	382061.697625	38.281447
2125.962492	382712.054705	38.286464
2128.253097	383343.087603	38.291482
2130.883999	383994.008330	38.296500
2133.355929	384633.085260	38.301517
2135.573317	385260.967277	38.306535
2137.665753	385890.322065	38.311552
2140.092940	386509.125035	38.316570
2141.916584	387128.969454	38.321588
2143.803212	387761.424282	38.326605
2145.897339	388391.070609	38.331623
2147.950223	389027.062896	38.336640
2150.288279	389650.384923	38.341658
2152.111985	390259.947339	38.346676
2154.033532	390873.023937	38.351693
2155.974255	391474.638437	38.356711
2157.543727	392091.435976	38.361728
2159.536526	392712.809913	38.366746
2161.111710	393339.904034	38.371764
2163.035040	393979.939505	38.376781
2164.889312	394607.463249	38.381799
2166.938729	395269.924038	38.386816
2169.362480	395905.981970	38.391834
2171.386408	396555.450505	38.396852
2174.006047	397199.948113	38.401869
2176.083495	397850.739486	38.406887
2178.439452	398510.935399	38.411904
2180.330435	399169.312482	38.416922
2182.789762	399828.138845	38.421940
2184.664668	400495.389703	38.426957
2187.152105	401163.942703	38.431975
2189.052244	401837.123414	38.436992
2190.974100	402511.951178	38.442010
2192.972061	403187.911155	38.447028
2195.643179	403869.565823	38.452045
2197.645108	404550.697383	38.457063
2199.780520	405248.993654	38.462080
2202.039684	405939.759391	38.467098
2203.817641	406637.663548	38.472116
2206.181479	407340.058970	38.477133
2208.324327	408035.838175	38.482151
2210.259047	408755.561087	38.487168
2212.637241	409461.479442	38.492186
2214.934992	410173.307316	38.497204
2217.368457	410899.611101	38.502221
2219.945651	411599.256963	38.507239
2221.986810	412323.803855	38.512256
2224.816552	413018.305379	38.517274
2226.819174	413736.892021	38.522292
2229.017370	414456.789805	38.527309
2231.000748	415173.257285	38.532327
2233.417811	415896.461335	38.537344
2235.538723	416622.974748	38.542362
2237.851218	417357.070508	38.547380
2240.149606	418088.260019	38.552397
2242.488044	418812.185599	38.557415
2244.898784	419553.572972	38.562432
2247.289768	420286.896225	38.567450
2249.198100	421017.032602	38.572468
2251.287924	421745.496612	38.577485
2254.142143	422471.742054	38.582503
2256.263779	423199.087627	38.587520
2258.920768	423926.626911	38.592538
2261.379547	424660.794561	38.597556
2263.796974	425385.032626	38.602573
2266.173829	426096.915237	38.607591
2268.238575	426830.054495	38.612608
2271.418456	427546.714435	38.617626
2273.298239	428260.013436	38.622644
2275.675624	428980.639775	38.627661
2277.968809	429703.376080	38.632679
2279.944570	430430.229786	38.637696
2281.643044	431138.095562	38.642714
2284.380821	431872.105562	38.647732
2286.754009	432600.585611	38.652749
2288.593595	433326.190658	38.657767
2291.064154	434059.351369	38.662784
2293.273026	434775.242464	38.667802
2295.288414	435504.679911	38.672820
2298.018623	436232.613492	38.677837
2300.566305	436936.597347	38.682855
2303.425509	437654.552901	38.687872
2305.632656	438336.963269	38.692890
2307.911450	439019.994628	38.697908
2310.073815	439718.428451	38.702925
2312.293572	440399.196094	38.707943
2314.379211	441102.137186	38.712960
2316.467859	441796.514218	38.717978
2318.813699	442488.754060	38.722996
2320.761886	443198.103281	38.728013
2323.120818	443907.613597	38.733031
2325.056770	444616.405151	38.738048
2327.051135	445346.221205	38.743066
2329.734291	446065.294606	38.748084
2331.790076	446783.326764	38.753101
2334.359635	447502.664208	38.758119
2336.719313	448229.277636	38.763136
2339.213773	448970.686538	38.768154
2341.776408	449696.300187	38.773172
2343.968174	450433.909048	38.778189
2346.661230	451156.262179	38.783207
2348.960827	451901.972850	38.788224
2351.121836	452634.547679	38.793242
2354.123157	453368.172358	38.798260
2356.750463	454098.392309	38.803277
2359.379861	454822.776507	38.808295
2361.376699	455577.970262	38.813312
2363.895115	456313.818867	38.818330
2366.470587	457047.457125	38.823348
2368.182607	457790.788859	38.828365
2370.780698	458540.006277	38.833383
2372.935697	459284.314761	38.838400
2375.081869	460028.996109	38.843418
2377.502965	460786.520319	38.848436
2379.581905	461544.417660	38.853453
2382.184674	462313.249467	38.858471
2384.057457	463084.784269	38.863488
2386.409767	463850.104082	38.868506
2389.035034	464627.908586	38.873524
2391.113975	465407.780440	38.878541
2393.893341	466191.390715	38.883559
2396.137702	466969.145991	38.888576
2398.636624	467759.788386	38.893594
2401.432085	468547.875180	38.898612
2403.393935	469335.953879	38.903629
2405.803228	470122.260549	38.908647
2407.983969	470919.206271	38.913664
2410.129293	471713.345106	38.918682
2412.646797	472520.144880	38.923700
2414.621865	473329.762723	38.928717
2417.241217	474135.911493	38.933735
2419.792545	474953.324401	38.938752
2422.144722	475768.508586	38.943770
2424.680146	476571.926680	38.948788
2427.116954	477394.022269	38.953805
2429.522624	478198.689354	38.958823
2432.107482	479015.334595	38.963840
2434.635607	479833.660232	38.968858
2437.245805	480652.686539	38.973876
2439.942895	481454.974794	38.978893
2442.662239	482264.878549	38.983911
2444.970668	483073.695888	38.988928
2447.401716	483889.708167	38.993946
2450.063265	484695.765477	38.998964
2452.537871	485515.010810	39.003981
2454.850626	486310.255937	39.008999
2457.519894	487129.737454	39.014016
2459.733108	487939.473295	39.019034
2462.296320	488738.784686	39.024052
2464.707127	489532.486640	39.029069
2467.528010	490309.259637	39.034087
2469.804444	491084.768325	39.039104
2471.970586	491859.750701	39.044122
2474.709653	492636.466843	39.049140
2476.785984	493417.728263	39.054157
2479.216770	494187.512902	39.059175
2481.324974	494989.282560	39.064192
2484.247315	495777.085490	39.069210
2486.597456	496560.052201	39.074228
2488.768883	497356.145407	39.079245
2491.590191	498150.231189	39.084263
2494.159844	498961.076444	39.089280
2496.360770	499759.098452	39.094298
2498.664587	500576.942656	39.099316
2500.734190	501393.972139	39.104333
2503.385322	502204.372190	39.109351
2505.807389	503038.365280	39.114368
2508.276542	503875.422672	39.119386
2510.758785	504703.723855	39.124404
2512.838857	505540.040332	39.129421
2515.348560	506380.366284	39.134439
2517.744809	507233.388925	39.139456
2520.616770	508093.731341	39.144474
2522.855810	508930.778938	39.149492
2525.417758	509789.255394	39.154509
2528.007382	510657.533521	39.159527
2530.838086	511525.267382	39.164544
2533.073009	512396.862634	39.169562
2536.040004	513260.292757	39.174580
2538.685203	514140.967490	39.179597
2541.357503	515011.776684	39.184615
2544.044468	515878.506132	39.189632
2546.491437	516748.084133	39.194650
2549.259530	517621.930409	39.199668
2551.329804	518507.492467	39.204685
2554.286372	519374.209282	39.209703
2556.679829	520260.008595	39.214720
2558.956091	521165.068049	39.219738
2561.740703	522042.748018	39.224756
2563.866771	522933.338494	39.229773
2566.654097	523832.660556	39.234791
2569.057615	524724.746492	39.239808
2571.413760	525643.961619	39.244826
2574.041883	526547.797578	39.249844
2576.327480	527472.875253	39.254861
2579.012112	528386.221783	39.259879
2581.314287	529301.724452	39.264896
2583.893319	530225.959522	39.269914
2586.744594	531145.616763	39.274932
2589.456874	532077.785358	39.279949
2592.171945	532998.387249	39.284967
2594.997125	533915.843434	39.289984
2597.755995	534843.637668	39.295002
2600.288584	535766.681059	39.300020
2602.664626	536696.509656	39.305037
2605.053672	537622.102126	39.310055
2607.792284	538562.981903	39.315072
2610.554884	539495.908361	39.320090
2613.589550	540410.807067	39.325108
2615.978010	541345.712914	39.330125
2618.612858	542278.352982	39.335143
2621.448638	543206.777843	39.340160
2623.624358	544148.130815	39.345178
2626.845151	545081.021738	39.350196
2628.775919	546030.648321	39.355213
2631.464291	546957.361273	39.360231
2634.066486	547881.159172	39.365248
2636.039400	548798.767215	39.370266
2639.653826	549697.545120	39.375284
2642.169828	550608.212668	39.380301
2644.327588	551505.330139	39.385319
2647.025723	552406.959611	39.390336
2649.975310	553321.467190	39.395354
2652.877677	554223.731395	39.400372
2655.291934	555136.881632	39.405389
2657.834076	556044.378871	39.410407
2660.874833	556953.182761	39.415424
2663.019981	557870.827527	39.420442
2665.879224	558782.527155	39.425460
2668.431489	559703.975534	39.430477
2670.807407	560625.680344	39.435495
2674.146974	561551.220436	39.440512
2676.957306	562482.982207	39.445530
2679.600903	563413.143202	39.450548
2682.522191	564348.946760	39.455565
2685.578868	565267.625857	39.460583
2688.917906	566181.781237	39.465600
2691.965729	567100.166419	39.470618
2694.983839	568016.430354	39.475636
2697.429395	568940.321157	39.480653
2700.171998	569857.232609	39.485671
2703.010011	570761.440906	39.490688
2705.410784	571691.774731	39.495706
2707.878798	572605.805601	39.500724
2710.847133	573557.069658	39.505741
2713.149421	574478.782835	39.510759
2716.273670	575409.349245	39.515776
2718.353314	576356.163226	39.520794
2721.041204	577291.145274	39.525812
2724.094669	578240.249484	39.530829
2726.295504	579184.604289	39.535847
2728.902761	580143.020398	39.540864
2731.634260	581105.785511	39.545882
2734.453050	582066.902983	39.550900
2736.839221	583032.604824	39.555917
2739.622646	584000.359820	39.560935
2742.570298	584962.004342	39.565952
2744.843907	585947.215549	39.570970
2747.809305	586921.332572	39.575988
2750.450704	587905.109554	39.581005
2752.951149	588892.917519	39.586023
2756.143064	589879.027957	39.591040
2758.581287	590882.005392	39.596058
2761.413271	591867.190556	39.601076
2764.144822	592867.438480	39.606093
2766.821125	593867.951138	39.611111
2769.662881	594858.204238	39.616128
2772.283541	595867.678396	39.621146
2775.536095	596867.918410	39.626164
2778.440887	597882.699248	39.631181
2780.744688	598881.548458	39.636199
2784.177765	599898.998072	39.641216
2786.822502	600902.494239	39.646234
2789.516230	601913.224003	39.651252
2792.340165	602922.537608	39.656269
2794.966559	603932.582492	39.661287
2797.434724	604944.649450	39.666304
2800.375362	605962.381218	39.671322
2802.768721	606990.425517	39.676340
2805.432354	608011.490108	39.681357
2808.417549	609038.587866	39.686375
2811.165726	610061.928420	39.691392
2813.796366	611096.255926	39.696410
2816.522679	612125.276896	39.701428
2819.566821	613152.198883	39.706445
2822.159510	614161.038871	39.711463
2825.276472	615145.069023	39.716480
2827.980835	616150.600889	39.721498
2831.053473	617140.074594	39.726516
2834.149140	618127.054363	39.731533
2836.978866	619123.744791	39.736551
2840.108506	620114.259132	39.741568
2842.531628	621108.322102	39.746586
2845.508667	622107.030508	39.751604
2848.369411	623110.736487	39.756621
2851.113672	624118.940183	39.761639
2853.958401	625114.026115	39.766656
2857.118358	626129.726298	39.771674
2859.973810	627125.302259	39.776692
2862.596888	628150.285665	39.781709
2865.220143	629171.526492	39.786727
2868.461510	630182.159537	39.791744
2870.847611	631205.063611	39.796762
2874.190834	632231.242290	39.801780
2876.785308	633256.532326	39.806797
2879.412306	634295.090959	39.811815
2882.274021	635328.474952	39.816832
2885.427556	636384.184661	39.821850
2888.395750	637431.698360	39.826868
2891.401925	638473.768515	39.831885
2894.194557	639528.387191	39.836903
2897.589022	640587.765323	39.841920
2900.789350	641633.929048	39.846938
2903.739751	642668.034523	39.851956
2907.064093	643720.257744	39.856973
2909.484702	644780.504419	39.861991
2912.372311	645836.183659	39.867008
2915.470974	646893.249439	39.872026
2918.133197	647947.827661	39.877044
2921.266957	649008.817842	39.882061
2924.069514	650080.266813	39.887079
2926.603181	651147.062969	39.892096
2929.556735	652229.708013	39.897114
2932.351824	653295.515907	39.902132
2935.230612	654390.526172	39.907149
2938.187958	655470.251037	39.912167
2941.092533	656559.980016	39.917184
2944.247689	657644.276908	39.922202
2947.107976	658743.672927	39.927220
2949.904837	659840.462639	39.932237
2953.025904	660943.714221	39.937255
2955.483890	662048.023614	39.942272
2958.596281	663162.756356	39.947290
2961.372057	664265.598206	39.952308
2964.548126	665367.991333	39.957325
2967.386438	666492.063838	39.962343
2970.729844	667601.784858	39.967360
2973.731184	668726.139328	39.972378
2976.366165	669844.111728	39.977396
2979.233430	670968.097920	39.982413
2981.832107	672102.335362	39.987431
2985.145349	673232.101060	39.992448
2987.799290	674371.678672	39.997466
2991.432766	675509.168783	40.002484
2994.235522	676645.300460	40.007501
2996.545609	677786.655842	40.012519
3000.013923	678915.646752	40.017536
3003.128074	680053.799368	40.022554
3005.930402	681197.291921	40.027572
3008.829966	682342.989639	40.032589
3012.059163	683504.511395	40.037607
3015.242594	684642.874248	40.042624
3018.340293	685771.894714	40.047642
3021.348019	686877.431160	40.052660
3024.562833	687967.309238	40.057677
3027.359262	689065.070553	40.062695
3030.244935	690167.121926	40.067712
3033.252983	691269.847354	40.072730
3036.066981	692370.181689	40.077748
3039.527110	693464.139291	40.082765
3042.594798	694574.071652	40.087783
3045.584396	695674.132036	40.092800
3048.614001	696783.028478	40.097818
3051.397699	697900.999220	40.102836
3054.451024	699010.525819	40.107853
3057.373888	700147.919037	40.112871
3060.264243	701270.394120	40.117888
3063.258230	702394.522721	40.122906
3066.307089	703533.440930	40.127924
3069.503293	704676.220648	40.132941
3072.404466	705827.962120	40.137959
3075.710594	706975.624987	40.142976
3078.569057	708142.529332	40.147994
3081.395960	709300.437417	40.153012
3084.596472	710457.821089	40.158029
3087.474887	711633.871414	40.163047
3090.564666	712815.431226	40.168064
3093.735312	714001.581311	40.173082
3096.722855	715204.238342	40.178100
3100.213835	716386.968347	40.183117
3102.939015	717582.004709	40.188135
3106.105457	718780.531385	40.193152
3109.236519	719983.802837	40.198170
3112.072368	721192.792629	40.203188
3115.331548	722394.188746	40.208205
3118.200315	723613.279295	40.213223
3121.514616	724828.265703	40.218240
3124.921669	726050.229055	40.223258
3127.764918	727262.389403	40.228276
3131.200885	728485.972542	40.233293
3134.728501	729719.624034	40.238311
3137.664524	730941.557905	40.243328
3141.320113	732156.295314	40.248346
3144.249143	733382.011875	40.253364
3148.072277	734609.255201	40.258381
3151.024653	735834.662514	40.263399
3154.146483	737062.494558	40.268416
3157.061567	738303.520029	40.273434
3160.323237	739533.081204	40.278452
3163.076785	740755.295530	40.283469
3166.204623	742005.535803	40.288487
3169.467282	743252.644080	40.293504
3172.566757	744495.440545	40.298522
3175.751926	745746.306697	40.303540
3179.189379	746988.966947	40.308557
3182.716584	748232.479042	40.313575
3185.614585	749469.546116	40.318592
3188.751635	750723.138852	40.323610
3191.577069	751973.226106	40.328628
3195.079499	753224.165767	40.333645
3198.228802	754479.745701	40.338663
3201.386183	755739.318143	40.343680
3204.541279	756994.011273	40.348698
3207.447773	758259.300672	40.353716
3210.688644	759514.218442	40.358733
3213.710877	760792.066260	40.363751
3216.744012	762056.064739	40.368768
3219.953796	763322.157392	40.373786
3223.046067	764601.354530	40.378804
3226.582366	765872.121677	40.383821
3229.591349	767137.893449	40.388839
3232.199810	768396.694958	40.393856
3235.670435	769633.753706	40.398874
3238.545845	770875.280626	40.403892
3241.479587	772110.852055	40.408909
3244.514449	773369.849067	40.413927
3247.621257	774626.158214	40.418944
3251.092273	775884.866554	40.423962
3254.180647	777144.329614	40.428980
3257.212106	778412.361445	40.433997
3260.108671	779693.365058	40.439015
3263.298606	780975.641778	40.444032
3267.267445	782274.104839	40.449050
3269.953571	783560.018534	40.454068
3273.348184	784860.997795	40.459085
3276.183669	786158.491650	40.464103
3279.509159	787468.194588	40.469120
3282.751077	788783.163692	40.474138
3286.072856	790103.174404	40.479156
3289.688396	791428.140693	40.484173
3292.469827	792755.066176	40.489191
3296.181525	794089.229695	40.494208
3299.713193	795432.553841	40.499226
3302.783914	796775.380376	40.504244
3306.043138	798118.532801	40.509261
3309.324778	799479.714733	40.514279
3312.196506	800833.223786	40.519296
3316.082083	802195.149565	40.524314
3319.105109	803562.566815	40.529332
3322.199189	804936.103818	40.534349
3325.555256	806311.152787	40.539367
3329.012888	807684.478054	40.544384
3332.453129	809064.851566	40.549402
3335.862548	810452.124033	40.554420
3339.332997	811838.595672	40.559437
3342.972628	813224.929501	40.564455
3345.792972	814614.485837	40.569472
3349.559264	816003.099709	40.574490
3352.912763	817402.735603	40.579508
3356.795475	818795.855904	40.584525
3360.411620	820186.374672	40.589543
3363.583161	821570.438052	40.594560
3367.204518	822958.681183	40.599578
3370.873457	824354.752799	40.604596
3374.383158	825734.817749	40.609613
3377.816821	827128.547221	40.614631
3381.133156	828514.801727	40.619648
3384.687758	829898.764076	40.624666
3387.968181	831302.222372	40.629684
3391.506354	832684.483938	40.634701
3395.171243	834086.265495	40.639719
3397.930156	835471.592316	40.644736
3401.198573	836870.848254	40.649754
3404.561074	838272.955960	40.654772
3408.311234	839686.963119	40.659789
3411.907006	841081.307855	40.664807
3415.554159	842468.932304	40.669824
3419.197300	843863.870970	40.674842
3422.591518	845266.929395	40.679860
3426.127722	846656.388288	40.684877
3429.586401	848059.831634	40.689895
3432.989775	849466.810830	40.694912
3436.027602	850864.041601	40.699930
3439.518524	852260.092890	40.704948
3443.041718	853662.367442	40.709965
3446.501920	855075.700495	40.714983
3449.473632	856487.991104	40.720000
3452.954213	857892.233699	40.725018
3456.103272	859289.285226	40.730023
3459.362956	860656.153650	40.735028
3462.796311	861969.510516	40.740032
3465.589458	863227.779939	40.745037
3469.052560	864425.962727	40.750042
3471.582552	865592.743421	40.755047
3474.643196	866669.488737	40.760052
3477.204037	867698.700084	40.765056
3479.341736	868681.742666	40.770061
3482.384992	869589.863482	40.775066
3484.600744	870456.277119	40.780071
3486.650009	871239.602131	40.785076
3489.052631	871985.039704	40.790080
3491.539346	872669.013160	40.795085
3493.390365	873296.480233	40.800090
3495.075662	873883.878395	40.805095
3496.618608	874409.808242	40.810100
3498.587351	874898.979900	40.815104
3499.740192	875337.038009	40.820109
3500.880843	875743.536972	40.825114
3502.321143	876116.410479	40.830119
3504.082706	876442.166085	40.835124
3505.146327	876733.502649	40.840128
3506.373641	876982.483391	40.845133
3507.571569	877191.457481	40.850138
3508.186652	877377.961263	40.855143
3508.862656	877540.547075	40.860148
3510.010924	877666.141774	40.865152
3510.641367	877778.225604	40.870157
3511.803433	877852.638195	40.875162
3512.452133	877912.481308	40.880167
3513.095416	877941.196304	40.885172
3513.496267	877961.661026	40.890176
3514.041031	877964.467065	40.895181
3514.709883	877935.932619	40.900186
3514.630309	877896.913942	40.905191
3515.378015	877834.828560	40.910196
3515.926216	877760.823068	40.915200
3515.972528	877690.364617	40.920205
3516.186665	877592.893022	40.925210
3516.510709	877488.945024	40.930215
3517.034507	877372.819637	40.935220
3517.125922	877246.253454	40.940224
3517.110654	877117.966075	40.945229
3517.332593	876964.673728	40.950234
3517.419315	876816.892630	40.955239
3517.597889	876654.151977	40.960244
3517.906160	876489.072701	40.965248
3517.948213	876320.463270	40.970253
3518.130731	876145.464069	40.975258
3518.041485	875964.910193	40.980263
3518.407705	875770.492517	40.985268
3518.250130	875580.584933	40.990272
3518.174732	875385.451449	40.995277
3518.754090	875182.687911	41.000282
3518.590349	874978.008202	41.005287
3518.133982	874761.409585	41.010292
3518.476253	874548.438501	41.015296
3518.562509	874344.757073	41.020301
3518.642205	874126.217565	41.025306
3518.348099	873907.727883	41.030311
3518.398287	873680.881343	41.035316
3518.708529	873457.650021	41.040320
3518.268290	873232.405043	41.045325
3518.372023	873005.136725	41.050330
3518.167493	872779.740099	41.055335
3518.173990	872554.590750	41.060340
3518.485527	872334.015190	41.065344
3517.905301	872091.477664	41.070349
3517.909801	871860.705043	41.075354
3517.597610	871638.173384	41.080359
3517.682726	871412.290199	41.085364
3517.741396	871178.972250	41.090368
3516.994521	870961.981504	41.095373
3517.750089	870728.535792	41.100378
3517.487361	870502.380668	41.105383
3517.477740	870280.616096	41.110388
3517.389179	870041.869334	41.115392
3516.867454	869816.112969	41.120397
3516.873575	869590.844083	41.125402
3516.748904	869356.996145	41.130407
3516.772434	869134.505313	41.135412
3516.587677	868914.161853	41.140416
3516.111209	868689.704401	41.145421
3516.319215	868472.467783	41.150426
3516.052039	868252.593894	41.155431
3515.825208	868039.463200	41.160436
3515.938702	867824.147157	41.165440
3515.583623	867606.096104	41.170445
3515.931201	867385.995634	41.175450
3515.386143	867182.441179	41.180455
3515.260139	866972.247577	41.185460
3515.073437	866768.042727	41.190464
3514.999281	866560.819209	41.195469
3515.103752	866356.553918	41.200474
3514.747497	866157.471815	41.205479
3514.909878	865952.796531	41.210484
3514.620967	865740.554239	41.215488
3514.787008	865539.050637	41.220493
3514.495861	865340.026079	41.225498
3514.375311	865139.035951	41.230503
3513.947593	864945.621297	41.235508
3514.490403	864744.223632	41.240512
3513.798268	864541.949194	41.245517
3513.994809	864348.513122	41.250522
3513.745582	864158.328282	41.255527
3513.438938	863966.696810	41.260532
3513.424717	863772.501080	41.265536
3513.283303	863587.014446	41.270541
3513.372677	863402.451899	41.275546
3512.721532	863222.250688	41.280551
3512.384474	863039.868783	41.285556
3512.686683	862861.536306	41.290560
3512.533714	862690.420448	41.295565
3512.265164	862510.909903	41.300570
3512.254611	862353.967563	41.305575
3512.340665	862173.424499	41.310580
3512.121343	861998.625656	41.315584
3511.527112	861839.247490	41.320589
3511.531413	861674.455359	41.325594
3511.817855	861515.413712	41.330599
3511.851269	861355.343928	41.335604
3511.462785	861184.896148	41.340608
3511.287136	861024.173097	41.345613
3511.200786	860870.198239	41.350618
3511.013672	860707.051354	41.355623
3510.831105	860554.919737	41.360628
3510.756090	860405.377468	41.365632
3510.468486	860263.985401	41.370637
3510.446609	860111.333438	41.375642
3510.273889	859970.109484	41.380647
3510.095713	859821.438166	41.385652
3510.848817	859675.034577	41.390656
3509.894959	859527.637106	41.395661
3510.012526	859385.483099	41.400666
3510.141578	859251.832873	41.405671
3509.993737	859109.810191	41.410676
3509.987872	858963.603718	41.415680
3509.672259	858821.406697	41.420685
3509.808953	858670.722172	41.425690
3509.675515	858557.598006	41.430695
3509.327806	858418.393868	41.435700
3509.595995	858288.857850	41.440704
3508.747575	858165.779783	41.445709
3509.045778	858033.041764	41.450714
3509.083063	857909.819739	41.455719
3509.003469	857781.680656	41.460724
3508.780640	857657.623394	41.465728
3508.622529	857540.517412	41.470733
3508.614240	857409.650610	41.475738
3508.491233	857307.139906	41.480743
3508.270989	857184.909826	41.485748
3508.241797	857067.000185	41.490752
3508.389520	856952.833062	41.495757
3508.120650	856827.314034	41.500762
3508.205046	856718.279117	41.505767
3508.048319	856608.022215	41.510772
3507.985615	856512.549834	41.515776
3507.469768	856394.025260	41.520781
3507.862067	856280.290251	41.525786
3507.457379	856171.127913	41.530791
3507.408669	856076.516816	41.535796
3507.595327	855971.031408	41.540800
3507.641542	855881.529998	41.545805
3507.112801	855772.185972	41.550810
3507.381249	855685.839630	41.555815
3507.320085	855579.418236	41.560820
3507.424705	855473.646267	41.565824
3507.162416	855375.186696	41.570829
3507.381011	855279.262827	41.575834
3507.078969	855169.388097	41.580839
3506.574078	855080.540960	41.585844
3506.914691	854984.496345	41.590848
3506.380124	854895.554225	41.595853
3506.702677	854804.154282	41.600858
3506.621453	854718.622259	41.605863
3506.855378	854635.749325	41.610868
3506.687085	854536.389772	41.615872
3505.954619	854464.697654	41.620877
3506.188995	854362.562457	41.625882
3506.160835	854287.177291	41.630887
3505.979077	854206.008390	41.635892
3505.672634	854125.922426	41.640896
3506.082595	854045.045886	41.645901
3506.128849	853968.580323	41.650906
3506.092282	853889.900647	41.655911
3505.929381	853812.981796	41.660916
3506.045162	853718.983771	41.665920
3505.686909	853646.351888	41.670925
3505.623867	853564.671467	41.675930
3505.486202	853501.101540	41.680935
3505.355015	853420.204058	41.685940
3505.656201	853353.176162	41.690944
3505.534380	853294.634756	41.695949
3505.671278	853218.725869	41.700954
3505.668882	853150.387936	41.705959
3505.581355	853064.348403	41.710964
3505.599635	852986.131841	41.715968
3505.628862	852918.367024	41.720973
3505.624690	852833.472638	41.725978
3505.648827	852770.643806	41.730983
3505.648361	852693.200642	41.735988
3505.684138	852620.203853	41.740992
3505.326677	852551.236706	41.745997
3505.203574	852478.650196	41.751002
3505.092867	852410.998121	41.756007
3505.139042	852339.061066	41.761012
3505.193479	852268.961250	41.766016
3505.110228	852208.466588	41.771021
3505.154471	852142.142530	41.776026
3505.216489	852073.491374	41.781031
3505.050573	852015.718443	41.786036
3505.074174	851949.589042	41.791040
3504.869875	851884.656330	41.796045
3504.998727	851814.345748	41.801050
3504.627913	851744.112421	41.806055
3504.875398	851684.819259	41.811060
3504.997792	851615.185024	41.816064
3505.026959	851565.026096	41.821069
3505.077749	851489.979429	41.826074
3504.781860	851434.254341	41.831079
3504.816747	851377.024610	41.836084
3504.735624	851307.031184	41.841088
3504.622714	851255.148885	41.846093
3504.292000	851199.136496	41.851098
3503.982849	851141.086750	41.856103
3504.032561	851089.177546	41.861108
3504.346016	851033.450186	41.866112
3504.062912	850982.754046	41.871117
3504.060890	850927.655987	41.876122
3504.092438	850876.231891	41.881127
3504.124000	850833.522563	41.886132
3504.004634	850782.314898	41.891136
3504.088366	850741.920820	41.896141
3503.885443	850682.106808	41.901146
3504.240686	850635.471894	41.906151
3504.269469	850586.079283	41.911156
3504.106234	850528.194280	41.916160
3503.817848	850483.692419	41.921165
3504.294210	850423.866405	41.926170
3504.081171	850386.034153	41.931175
3503.762082	850337.371711	41.936180
3504.029445	850282.031734	41.941184
3503.498889	850244.538730	41.946189
3503.643743	850182.437761	41.951194
3503.401178	850147.707664	41.956199
3503.142186	850106.491123	41.961204
3503.517347	850061.979154	41.966208
3503.210770	850031.132310	41.971213
3503.334226	849983.850466	41.976218
3503.079472	849950.767546	41.981223
3503.107950	849922.095308	41.986228
3503.129311	849877.056127	41.991232
3503.272015	849838.486740	41.996237
3503.284652	849805.651753	42.001242
3503.308460	849772.330567	42.006247
3502.795249	849735.122122	42.011252
3503.136508	849691.096891	42.016256
3502.878711	849668.473149	42.021261
3502.869047	849631.282180	42.026266
3503.019627	849597.068472	42.031271
3503.049027	849567.425780	42.036276
3503.141949	849531.380420	42.041280
3502.630746	849504.146491	42.046285
3502.939772	849473.006739	42.051290
3503.102663	849454.384453	42.056295
3502.704228	849415.800001	42.061300
3502.981386	849381.080942	42.066304
3502.973331	849346.793703	42.071309
3502.613810	849313.432954	42.076314
3502.650805	849296.573344	42.081319
3502.776702	849255.774916	42.086324
3502.950311	849225.333045	42.091328
3502.540053	849206.024661	42.096333
3502.915858	849168.964211	42.101338
3502.738005	849142.063930	42.106343
3502.734815	849112.908340	42.111348
3502.783878	849077.157620	42.116352
3502.564261	849055.106714	42.121357
3503.082923	849022.575673	42.126362
3502.917847	848996.350783	42.131367
3502.716816	848962.478915	42.136372
3502.856417	848925.744446	42.141376
3502.620234	848900.983254	42.146381
3502.870478	848861.518782	42.151386
3502.586742	848836.571013	42.156391
3502.646607	848813.313074	42.161396
3502.831829	848784.998217	42.166400
3502.484914	848769.262664	42.171405
3502.674606	848741.624989	42.176410
3502.619838	848715.962817	42.181415
3502.562110	848692.722780	42.186420
3502.754995	848656.075155	42.191424
3502.311166	848629.601573	42.196429
3502.596105	848601.173365	42.201434
3502.662533	848582.272758	42.206439
3502.297390	848554.914678	42.211444
3502.545119	848523.101327	42.216448
3502.251834	848511.134785	42.221453
3502.537638	848475.730870	42.226458
3502.565007	848451.023443	42.231463
3502.326354	848430.329403	42.236468
3502.215925	848405.837076	42.241472
3502.111136	848385.800085	42.246477
3502.353387	848361.446194	42.251482
3502.387272	848342.065513	42.256487
3502.205406	848326.690471	42.261492
3502.350212	848294.407577	42.266496
3502.027882	848282.832617	42.271501
3502.531976	848253.205920	42.276506
3502.495873	848236.548432	42.281511
3502.466585	848231.612206	42.286516
3502.320499	848203.249441	42.291520
3502.446710	848176.684691	42.296525
3502.309131	848153.164348	42.301530
3502.345963	848121.769302	42.306535
3502.453681	848105.088956	42.311540
3502.591793	848079.200072	42.316544
3502.185778	848070.641099	42.321549
3502.295266	848033.808845	42.326554
3502.506681	848014.302443	42.331559
3502.171124	847990.715510	42.336564
3502.211276	847971.913920	42.341568
3501.878587	847949.585856	42.346573
3501.950053	847919.734449	42.351578
3501.924936	847909.081127	42.356583
3501.905599	847899.105074	42.361588
3502.023657	847878.353313	42.366592
3502.259707	847866.399584	42.371597
3502.293921	847837.619318	42.376602
3502.184774	847827.172753	42.381607
3502.048160	847797.353249	42.386612
3502.169045	847784.060947	42.391616
3502.076980	847761.307002	42.396621
3502.428437	847749.334994	42.401626
3502.399012	847713.200645	42.406631
3501.972978	847697.474562	42.411636
3502.264328	847667.587496	42.416640
3502.133280	847659.856930	42.421645
3502.246670	847634.454384	42.426650
3501.692408	847619.910803	42.431655
3501.824947	847604.290931	42.436660
3501.790498	847588.697120	42.441664
3501.916327	847567.264814	42.446669
3501.909084	847556.704945	42.451674
3502.264415	847535.236646	42.456679
3501.773639	847523.105163	42.461684
3501.898346	847496.925124	42.466688
3501.834709	847484.629899	42.471693
3501.997620	847479.953667	42.476698
3501.959671	847462.616020	42.481703
3501.874123	847446.060900	42.486708
3502.397176	847428.344779	42.491712
3501.965761	847420.757742	42.496717
3501.878012	847391.994348	42.501722
3501.571068	847369.756933	42.506727
3501.691007	847375.842484	42.511732
3501.825713	847345.396901	42.516736
3501.724194	847335.432733	42.521741
3502.145149	847317.344662	42.526746
3502.104428	847296.809449	42.531751
3501.903187	847283.469471	42.536756
3502.330202	847256.756628	42.541760
3501.905674	847240.641496	42.546765
3501.827650	847219.530469	42.551770
3501.839541	847206.544582	42.556775
3502.150351	847200.682256	42.561780
3502.008993	847182.972361	42.566784
3501.700266	847171.296168	42.571789
3501.831631	847148.408014	42.576794
3501.828131	847139.978542	42.581799
3501.963774	847119.899623	42.586804
3502.104712	847099.722911	42.591808
3501.707101	847090.095303	42.596813
3501.591834	847078.776274	42.601818
3501.962034	847062.536418	42.606823
3501.693823	847057.248954	42.611828
3501.944863	847029.302903	42.616832
3501.626007	847036.135694	42.621837
3501.791220	847007.621563	42.626842
3501.865343	847003.927825	42.631847
3501.291226	846995.878042	42.636852
3501.434449	846978.123041	42.641856
3501.547866	846974.520042	42.646861
3501.464268	846962.808239	42.651866
3501.528522	846951.751602	42.656871
3501.709383	846929.533157	42.661876
3501.814195	846918.663919	42.666880
3501.840275	846910.520195	42.671885
3501.771528	846889.212724	42.676890
3501.784067	846888.920084	42.681895
3501.658491	846866.749304	42.686900
3501.952920	846851.683529	42.691904
3501.735616	846849.488778	42.696909
3501.527968	846838.474431	42.701914
3501.771356	846829.327603	42.706919
3501.767606	846815.277368	42.711924
3501.908347	846792.870872	42.716928
3501.554553	846786.530609	42.721933
3501.504133	846778.398659	42.726938
3501.579834	846754.064120	42.731943
3501.565013	846742.050413	42.736948
3501.673283	846739.126401	42.741952
3501.478745	846724.621254	42.746957
3501.318409	846716.894017	42.751962
3501.810397	846717.592366	42.756967
3501.990151	846703.706986	42.761972
3501.703316	846679.719523	42.766976
3501.519865	846676.259652	42.771981
3501.574730	846652.509377	42.776986
3501.605576	846648.822181	42.781991
3501.818809	846646.656956	42.786996
3501.861090	846619.226111	42.792001
3501.479603	846607.075634	42.797005
3501.436035	846600.977391	42.802010
3501.706238	846595.023905	42.807015
3501.531904	846578.577115	42.812020
3502.301020	846560.916824	42.817025
3501.717720	846551.123538	42.822029
3501.670159	846536.401135	42.827034
3501.870565	846530.167773	42.832039
3501.533555	846505.121457	42.837044
3501.704663	846491.043111	42.842049
3501.560699	846486.414061	42.847053
3501.383205	846467.544753	42.852058
3501.716696	846460.902881	42.857063
3501.439846	846460.655457	42.862068
3501.466170	846452.898692	42.867073
3501.136327	846450.236839	42.872077
3501.281638	846431.801498	42.877082
3501.333818	846437.898618	42.882087
3500.957204	846437.860606	42.887092
3501.337780	846448.073456	42.892097
3501.318733	846435.769056	42.897101
3501.276735	846402.051295	42.902106
3501.139144	846404.786288	42.907111
3501.016652	846402.673456	42.912116
3501.263738	846399.243028	42.917121
3501.279352	846412.904817	42.922125
3501.231553	846402.155387	42.927130
3501.302359	846385.863553	42.932135
3500.957509	846385.239117	42.937140
3501.116817	846373.778893	42.942145
3501.255587	846368.427183	42.947149
3501.478925	846367.907745	42.952154
3501.256679	846375.598388	42.957159
3501.519877	846360.923875	42.962164
3501.237224	846339.938574	42.967169
3501.389647	846338.751847	42.972173
3501.253313	846337.222616	42.977178
3501.535416	846331.073183	42.982183
3501.343893	846319.280053	42.987188
3501.283122	846305.625153	42.992193
3501.077438	846312.538001	42.997197
3501.078958	846318.546254	43.002202
3501.084348	846310.695663	43.007207
3500.981876	846315.751067	43.012212
3501.092900	846300.324905	43.017217
3501.172205	846283.643814	43.022221
3500.964560	846275.245009	43.027226
3501.099991	846280.941634	43.032231
3500.978234	846284.352587	43.037236
3501.343829	846276.445642	43.042241
3501.258012	846277.040549	43.047245
3501.294213	846284.497087	43.052250
3501.210762	846272.493146	43.057255
3500.827917	846260.439070	43.062260
3501.190252	846248.559218	43.067265
3501.132619	846260.100752	43.072269
3501.318023	846260.265617	43.077274
3501.405327	846272.172117	43.082279
3501.342714	846261.327833	43.087284
3501.355092	846248.242834	43.092289
3501.110578	846236.651645	43.097293
3501.265805	846223.738085	43.102298
3501.453544	846227.100690	43.107303
3501.266612	846236.724237	43.112308
3501.358005	846214.226333	43.117313
3501.278698	846216.661565	43.122317
3501.210786	846202.426066	43.127322
3501.245134	846202.226895	43.132327
3501.211821	846201.844476	43.137332
3501.370352	846190.190190	43.142337
3501.278593	846177.315137	43.147341
3501.503772	846172.240481	43.152346
3501.356845	846167.417814	43.157351
3501.376483	846173.907949	43.162356
3501.306466	846144.651089	43.167361
3501.569290	846142.090275	43.172365
3501.276646	846134.092209	43.177370
3501.325806	846132.243186	43.182375
3501.380798	846133.591407	43.187380
3501.558069	846115.053161	43.192385
3501.135066	846112.502629	43.197389
3501.568035	846109.721375	43.202394
3501.726424	846100.974358	43.207399
3501.221019	846076.146359	43.212404
3501.371871	846060.616426	43.217409
3501.434010	846068.650674	43.222413
3501.293014	846067.703590	43.227418
3501.528588	846063.693278	43.232423
3501.361004	846045.111805	43.237428
3501.323062	846032.131105	43.242433
3501.303361	846042.116491	43.247437
3501.710392	846037.885529	43.252442
3501.170110	846011.124398	43.257447
3501.227191	846012.666152	43.262452
3501.595397	845994.291509	43.267457
3501.301511	846004.513652	43.272461
3501.296692	845989.104781	43.277466
3501.214648	845976.033935	43.282471
3501.211844	845981.074046	43.287476
3501.063945	845974.700712	43.292481
3501.074153	845975.571387	43.297485
3500.969970	845970.935709	43.302490
3501.365205	845973.684526	43.307495
3501.084849	845963.842894	43.312500
3501.241867	845946.470281	43.317505
3501.546716	845953.400660	43.322509
3501.375614	845959.339349	43.327514
3501.372123	845958.758419	43.332519
3501.218142	845942.694327	43.337524
3501.130703	845926.425954	43.342529
3500.999137	845931.970822	43.347533
3500.869940	845927.532854	43.352538
3501.287023	845922.427984	43.357543
3501.097706	845928.078800	43.362548
3501.078289	845931.377042	43.367553
3501.191075	845928.161170	43.372557
3501.363802	845927.455773	43.377562
3501.112515	845896.190748	43.382567
3501.128553	845897.642030	43.387572
3501.032437	845896.978655	43.392577
3501.299485	845892.963308	43.397581
3501.154758	845900.351700	43.402586
3501.635717	845898.628940	43.407591
3501.391157	845888.878503	43.412596
3501.320424	845870.669008	43.417601
3501.433265	845872.589755	43.422605
3501.152720	845868.369237	43.427610
3501.722365	845862.368203	43.432615
3501.287942	845854.682672	43.437620
3501.650857	845839.022086	43.442625
3501.225963	845839.379285	43.447629
3501.170450	845836.189672	43.452634
3501.330279	845812.322668	43.457639
3501.476139	845805.903228	43.462644
3501.546237	845807.636840	43.467649
3501.485814	845800.280449	43.472653
3501.375159	845784.984506	43.477658
3501.237457	845776.574051	43.482663
3501.173204	845775.130324	43.487668
3501.282830	845769.491866	43.492673
3501.694628	845772.335110	43.497677
3501.462347	845753.762827	43.502682
3501.624812	845741.234756	43.507687
3501.331935	845741.571323	43.512692
3501.300071	845733.919624	43.517697
3501.584689	845718.367877	43.522701
3501.247265	845711.636200	43.527706
3501.600673	845707.994911	43.532711
3501.028124	845709.925931	43.537716
3501.294630	845699.126080	43.542721
3501.175918	845688.580269	43.547725
3501.167265	845674.721909	43.552730
3501.620635	845673.100321	43.557735
3501.208075	845670.644880	43.562740
3501.361324	845669.554812	43.567745
3501.536219	845654.020047	43.572749
3501.383845	845641.734823	43.577754
3501.741677	845641.485067	43.582759
3501.629721	845634.911900	43.587764
3501.519982	845613.412355	43.592769
3501.567538	845611.272652	43.597773
3501.160266	845601.741017	43.602778
3501.377123	845582.710291	43.607783
3501.212858	845578.471386	43.612788
3501.354399	845575.444672	43.617793
3501.489778	845578.621991	43.622797
3500.974687	845578.411766	43.627802
3501.372692	845582.614181	43.632807
3501.234921	845555.109583	43.637812
3501.623007	845549.427386	43.642817
3501.622967	845550.687421	43.647821
3501.124244	845549.214631	43.652826
3501.321813	845525.049790	43.657831
3501.228783	845503.353382	43.662836
3501.374990	845504.105944	43.667841
3501.368099	845502.459335	43.672845
3501.093834	845511.031554	43.677850
3501.427081	845504.000949	43.682855
3501.430423	845488.007942	43.687860
3501.447512	845474.242010	43.692865
3501.199661	845474.571552	43.697869
3501.311781	845483.180337	43.702874
3501.537140	845465.504846	43.707879
3501.172998	845456.257005	43.712884
3501.674883	845447.649172	43.717889
3501.430823	845450.013550	43.722893
3501.468107	845425.582581	43.727898
3501.699252	845413.818481	43.732903
3501.149579	845413.710579	43.737908
3501.256394	845413.693905	43.742913
3501.005676	845412.763865	43.747917
3501.131316	845392.583675	43.752922
3501.343507	845370.645212	43.757927
3501.291503	845377.922838	43.762932
3501.401912	845376.839414	43.767937
3501.471917	845383.128698	43.772941
3501.537179	845359.565417	43.777946
3501.528008	845360.729993	43.782951
3501.109907	845353.622808	43.787956
3501.315751	845346.127298	43.792961
3501.310266	845342.541888	43.797965
3501.095527	845329.974979	43.802970
3501.426045	845314.414990	43.807975
3501.165276	845316.975886	43.812980
3501.359526	845322.179614	43.817985
3501.229115	845318.419864	43.822989
3501.151982	845309.514634	43.827994
3501.173830	845294.099770	43.832999
3501.000731	845294.417636	43.838004
3501.334748	845281.474058	43.843009
3500.962658	845287.250987	43.848013
3501.048016	845296.930434	43.853018
3501.193969	845286.827165	43.858023
3501.096264	845298.958418	43.863028
3501.115443	845285.385572	43.868033
3501.121999	845277.824200	43.873037
3501.333768	845268.970675	43.878042
3501.305346	845254.435918	43.883047
3501.186757	845268.121352	43.888052
3501.408722	845256.358372	43.893057
3501.282637	845254.439540	43.898061
3501.484821	845230.660482	43.903066
3501.274950	845228.463953	43.908071
3501.231631	845227.113747	43.913076
3501.147516	845229.550137	43.918081
3501.184968	845226.636445	43.923085
3501.033808	845212.799273	43.928090
3501.423830	845201.494557	43.933095
3501.041874	845201.651218	43.938100
3501.393338	845197.525275	43.943105
3501.406902	845202.175779	43.948109
3501.374163	845193.651150	43.953114
3501.524374	845167.165940	43.958119
3501.261077	845167.788701	43.963124
3501.333650	845168.068169	43.968129
3501.244678	845170.602273	43.973133
3501.130334	845156.565353	43.978138
3501.244758	845139.584735	43.983143
3501.234750	845130.184089	43.988148
3501.447000	845117.743838	43.993153
3501.329569	845123.868840	43.998157
3501.662684	845129.341823	44.003162
3501.480183	845104.750017	44.008167
3501.575774	845100.082420	44.013172
3501.587038	845088.352042	44.018177
3501.409227	845089.349172	44.023181
3501.149653	845072.911479	44.028186
3501.542933	845064.707792	44.033191
3501.234619	845073.189039	44.038196
3501.292084	845071.338385	44.043201
3501.316836	845045.744621	44.048205
3501.079703	845029.884890	44.053210
3501.057030	845031.827098	44.058215
3501.107904	845044.032582	44.063220
3501.369792	845029.354955	44.068225
3501.442384	845047.954544	44.073229
3501.242303	845024.431399	44.078234
3501.178714	845008.544481	44.083239
3501.170853	845008.836531	44.088244
3501.172262	845001.954135	44.093249
3500.865063	845007.333463	44.098253
3500.942251	845007.999947	44.103258
3501.216095	845000.881098	44.108263
3500.981217	845005.861392	44.113268
3501.094880	845004.389662	44.118273
3501.253471	845003.104774	44.123277
3501.377218	844984.086667	44.128282
3501.185023	844978.009970	44.133287
3501.229285	844984.206773	44.138292
3501.167114	844976.849623	44.143297
3501.346939	844983.800698	44.148301
3501.091454	844975.795237	44.153306
3500.786134	844966.052760	44.158311
3500.991686	844958.266004	44.163316
3501.265391	844957.544710	44.168321
3501.390377	844962.274919	44.173325
3501.114398	844956.792895	44.178330
3501.320590	844957.342286	44.183335
3500.986198	844969.026553	44.188340
3501.127196	844958.341898	44.193345
3501.226996	844938.261122	44.198349
3501.471020	844933.085522	44.203354
3501.433762	844922.234799	44.208359
3501.193454	844936.327767	44.213364
3501.500029	844922.321422	44.218369
3501.213257	844907.826193	44.223373
3500.977643	844904.664226	44.228378
3501.619846	844893.416434	44.233383
3501.389819	844891.319863	44.238388
3501.445432	844883.556446	44.243393
3501.436440	844870.374784	44.248397
3501.414728	844862.526493	44.253402
3501.503526	844864.451330	44.258407
3501.161203	844863.147780	44.263412
3501.288981	844843.934722	44.268417
3501.231865	844840.454011	44.273421
3500.944034	844834.198244	44.278426
3501.053313	844820.513305	44.283431
3500.862831	844826.746970	44.288436
3501.099812	844822.541728	44.293441
3501.148830	844824.472797	44.298445
3501.363465	844816.005886	44.303450
3501.517674	844804.252595	44.308455
3501.223046	844801.972218	44.313460
3500.950860	844801.142369	44.318465
3501.402051	844807.372683	44.323469
3501.334351	844807.577161	44.328474
3501.260810	844795.859456	44.333479
3501.155013	844779.590774	44.338484
3501.218538	844766.494479	44.343489
3501.417643	844770.728575	44.348493
3501.429155	844763.747385	44.353498
3501.079975	844755.174650	44.358503
3501.147878	844748.184626	44.363508
3501.486417	844738.438059	44.368513
3501.287674	844741.086443	44.373517
3500.880520	844751.425399	44.378522
3501.085533	844738.597734	44.383527
3501.155673	844734.127700	44.388532
3501.167274	844719.100678	44.393537
3501.028844	844709.525560	44.398541
3501.475399	844694.430483	44.403546
3501.076741	844700.890698	44.408551
3501.315094	844707.929889	44.413556
3501.348135	844712.965484	44.418561
3501.131457	844703.402588	44.423565
3501.163554	844687.596783	44.428570
3501.270503	844675.075122	44.433575
3501.215096	844680.415385	44.438580
3501.174440	844671.115734	44.443585
3501.151816	844673.833555	44.448589
3501.248384	844674.206235	44.453594
3501.302734	844666.345792	44.458599
3501.343039	844649.860036	44.463604
3501.555426	844627.531021	44.468609
3501.346629	844631.053473	44.473613
3501.335328	844639.101158	44.478618
3501.563837	844613.376723	44.483623
3501.261679	844609.546425	44.488628
3501.442615	844609.905921	44.493633
3501.492217	844613.291052	44.498637
3501.297205	844606.729715	44.503642
3501.527172	844582.459001	44.508647
3501.388363	844582.383784	44.513652
3501.302015	844585.790183	44.518657
3501.456900	844570.061807	44.523661
3501.509537	844549.017680	44.528666
3501.442017	844534.875015	44.533671
3501.614985	844533.684719	44.538676
3501.275126	844519.584590	44.543681
3501.227717	844508.928572	44.548685
3501.189830	844499.337394	44.553690
3501.134319	844497.891984	44.558695
3500.928837	844512.271343	44.563700
3501.246345	844503.497081	44.568705
3501.344180	844509.201308	44.573709
3501.108655	844497.993033	44.578714
3500.945824	844469.033155	44.583719
3501.066105	844481.422841	44.588724
3501.354175	844468.581604	44.593729
3501.116828	844480.251667	44.598733
3501.284798	844484.684720	44.603738
3501.432786	844468.763270	44.608743
3500.979084	844462.048327	44.613748
3501.167206	844460.273999	44.618753
3501.437647	844449.471246	44.623757
3501.184945	844456.005852	44.628762
3501.291178	844456.280094	44.633767
3501.265205	844461.325131	44.638772
3501.301043	844445.905857	44.643777
3501.154397	844428.285406	44.648781
3500.978473	844422.011704	44.653786
3501.379818	844416.035524	44.658791
3500.886407	844431.041743	44.663796
3501.189344	844423.432942	44.668801
3501.389116	844414.095300	44.673805
3501.089924	844413.075731	44.678810
3501.233535	844391.047397	44.683815
3501.384019	844394.610768	44.688820
3501.210864	844388.045770	44.693825
3500.973017	844385.853295	44.698829
3500.716580	844396.363196	44.703834
3501.224285	844380.482219	44.708839
3501.248478	844377.861008	44.713844
3501.143702	844362.172668	44.718849
3501.164784	844356.158928	44.723853
3501.260239	844362.251442	44.728858
3500.949386	844355.707932	44.733863
3501.003701	844361.031333	44.738868
3500.930996	844359.006919	44.743873
3501.522021	844363.567817	44.748877
3501.044319	844350.652145	44.753882
3501.258857	844343.250946	44.758887
3501.215870	844334.241956	44.763892
3501.008043	844334.953071	44.768897
3501.224481	844332.495675	44.773901
3500.927429	844333.317682	44.778906
3501.260396	844339.082261	44.783911
3501.098078	844337.071848	44.788916
3501.350782	844318.031432	44.793921
3501.499546	844301.430803	44.798925
3501.149513	844312.924924	44.803930
3501.243059	844303.603712	44.808935
3500.970677	844300.544108	44.813940
3500.803359	844301.539727	44.818945
3501.030780	844305.963622	44.823949
3501.120342	844294.994974	44.828954
3501.130195	844280.839603	44.833959
3500.834549	844278.850011	44.838964
3500.755230	844268.198545	44.843969
3501.220941	844272.488271	44.848973
3500.723381	844266.943293	44.853978
3500.992763	844266.998151	44.858983
3500.836867	844276.620048	44.863988
3501.091394	844283.657221	44.868993
3501.295002	844273.640147	44.873997
3501.250957	844275.489000	44.879002
3500.911261	844277.674903	44.884007
3500.785764	844280.699819	44.889012
3501.228833	844276.946697	44.894017
3501.394546	844257.919685	44.899021
3500.722961	844256.861355	44.904026
3500.936428	844246.357971	44.909031
3500.957945	844239.471540	44.914036
3501.026438	844239.170022	44.919041
3500.940042	844243.546075	44.924045
3500.793181	844254.329935	44.929050
3501.132339	844232.852110	44.934055
3500.978292	844245.769901	44.939060
3501.082003	844250.213176	44.944065
3501.310538	844250.662200	44.949069
3501.103241	844247.689338	44.954074
3501.479510	844228.047647	44.959079
3501.308253	844225.553866	44.964084
3501.039997	844219.488271	44.969089
3501.049485	844228.793557	44.974093
3501.186562	844231.195782	44.979098
3501.597181	844222.406548	44.984103
3501.221132	844202.882376	44.989108
3501.065021	844191.951939	44.994113
3501.318676	844200.734372	44.999117
3500.751380	844207.027594	45.004122
3501.412923	844205.179185	45.009127
3501.366737	844202.568898	45.014132
3501.328781	844172.133854	45.019137
3501.467988	844166.780078	45.024141
3501.476693	844170.656588	45.029146
3501.437644	844165.136784	45.034151
3501.192410	844158.485849	45.039156
3501.286471	844128.902461	45.044161
3501.406203	844125.781470	45.049165
3501.037808	844134.661241	45.054170
3501.477380	844130.908573	45.059175
3501.173081	844121.746213	45.064180
3501.074470	844101.596653	45.069185
3501.073451	844095.198312	45.074189
3501.034655	844100.536504	45.079194
3501.208792	844102.254358	45.084199
3500.747524	844105.428800	45.089204
3501.101992	844094.418367	45.094209
3501.423547	844102.026965	45.099213
3500.866305	844108.318719	45.104218
3501.165843	844101.388666	45.109223
3501.285941	844073.933772	45.114228
3501.368176	844070.624717	45.119233
3501.455946	844064.988047	45.124237
3501.258570	844074.519809	45.129242
3501.652812	844057.395381	45.134247
3501.323933	844044.940510	45.139252
3501.359242	844034.949341	45.144257
3501.517246	844029.592502	45.149261
3501.504776	844034.732742	45.154266
3501.211739	844018.782070	45.159271
3501.154470	844006.866351	45.164276
3501.232816	843999.970757	45.169281
3501.363297	844012.068990	45.174285
3500.767484	844012.452998	45.179290
3501.354416	844005.090112	45.184295
3501.085288	844000.769506	45.189300
3501.293554	843986.679361	45.194305
3501.493859	843976.274503	45.199309
3501.015353	843985.074761	45.204314
3501.331558	843985.025356	45.209319
3501.223050	843976.801654	45.214324
3501.435641	843964.552818	45.219329
3501.371127	843944.397389	45.224333
3501.059363	843951.038736	45.229338
3501.340445	843944.305284	45.234343
3501.247678	843940.441813	45.239348
3501.493647	843937.494889	45.244353
3501.397474	843927.330190	45.249357
3501.246024	843914.071704	45.254362
3501.512437	843906.080147	45.259367
3501.680983	843903.242259	45.264372
3501.308243	843889.339655	45.269377
3501.475472	843880.394060	45.274381
3501.549155	843873.208194	45.279386
3501.557554	843861.088013	45.284391
3501.152712	843850.195823	45.289396
3501.055611	843834.892682	45.294401
3501.717216	843846.035666	45.299405
3501.489235	843850.337192	45.304410
3501.344272	843813.615178	45.309415
3501.612582	843809.695177	45.314420
3501.383240	843813.221326	45.319425
3501.461347	843810.300579	45.324429
3501.117985	843787.473544	45.329434
3501.118421	843779.038631	45.334439
3501.087530	843771.190320	45.339444
3500.738800	843773.086959	45.344449
3501.152782	843776.803422	45.349453
3500.672128	843773.291334	45.354458
3500.884490	843776.360646	45.359463
3500.882173	843783.050760	45.364468
3500.840555	843783.542052	45.369473
3500.944602	843783.816669	45.374477
3501.035009	843793.013042	45.379482
3501.453886	843786.063965	45.384487
3501.331822	843772.606662	45.389492
3501.371455	843763.583883	45.394497
3501.338908	843750.306441	45.399501
3501.861791	843758.271826	45.404506
3501.803785	843737.339049	45.409511
3501.572581	843723.607834	45.414516
3501.581808	843714.201919	45.419521
3501.742770	843702.930147	45.424525
3501.284733	843683.029248	45.429530
3501.192215	843684.788909	45.434535
3501.272659	843688.557568	45.439540
3501.269454	843680.413945	45.444545
3501.581410	843655.641830	45.449549
3501.691862	843648.352987	45.454554
3501.741756	843652.902082	45.459559
3501.441042	843633.945970	45.464564
3501.635853	843617.045353	45.469569
3501.768453	843610.043866	45.474573
3501.330141	843595.278218	45.479578
3501.225758	843582.302494	45.484583
3501.264913	843582.102485	45.489588
3501.294987	843582.582587	45.494593
3501.349244	843577.532425	45.499597
3501.457943	843566.753343	45.504602
3500.928462	843548.996191	45.509607
3501.203285	843550.407599	45.514612
3501.587772	843540.554921	45.519617
3501.669772	843545.583863	45.524621
3501.459443	843518.953689	45.529626
3501.313674	843503.075553	45.534631
3501.506804	843507.893241	45.539636
3501.013567	843500.698585	45.544641
3501.388789	843505.003025	45.549645
3501.478108	843493.645096	45.554650
3501.809401	843473.910972	45.559655
3501.862587	843465.758238	45.564660
3501.278522	843460.129054	45.569665
3501.687433	843442.515763	45.574669
3501.245587	843439.191322	45.579674
3501.613173	843431.668101	45.584679
3501.527820	843408.605347	45.589684
3501.191655	843394.114102	45.594689
3501.499308	843391.060306	45.599693
3501.479165	843397.559726	45.604698
3500.693957	843378.096772	45.609703
3500.840169	843384.958038	45.614708
3500.880821	843374.770996	45.619713
3501.022451	843363.695518	45.624717
3500.835217	843362.561297	45.629722
3501.035335	843360.396930	45.634727
3500.529873	843368.911436	45.639732
3501.075518	843360.196778	45.644737
3501.007972	843369.709381	45.649741
3500.699455	843368.109324	45.654746
3501.270170	843366.080947	45.659751
3500.977643	843375.337832	45.664756
3500.815023	843362.564645	45.669761
3501.042643	843372.709819	45.674765
3500.883784	843382.139718	45.679770
3501.042319	843373.970388	45.684775
3501.370238	843382.839396	45.689780
3501.232759	843349.506886	45.694785
3501.573831	843347.805279	45.699789
3501.010757	843350.026436	45.704794
3501.446492	843346.952596	45.709799
3501.395063	843346.960659	45.714804
3501.303647	843333.400601	45.719809
3501.317572	843307.607055	45.724813
3500.841776	843305.742249	45.729818
3500.871174	843311.070495	45.734823
3501.102896	843291.157405	45.739828
3501.244002	843236.546297	45.744833
3501.462916	843124.229609	45.749837
3501.058250	842980.106629	45.754842
3501.292326	842760.535594	45.759847
3500.651857	842503.176571	45.764852
3500.221084	842195.344892	45.769857
3500.060480	841839.350857	45.774861
3499.652733	841444.383813	45.779866
3499.236752	840992.453963	45.784871
3498.905659	840490.518220	45.789876
3498.220584	839945.617651	45.794881
3497.802012	839349.396337	45.799885
3497.168581	838716.081365	45.804890
3496.855138	838023.256644	45.809895
3496.128108	837297.416218	45.814900
3495.641913	836506.897719	45.819905
3495.108116	835667.351470	45.824909
3494.220554	834793.175611	45.829914
3493.276573	833862.263831	45.834919
3492.667016	832900.656905	45.839924
3491.494985	831873.410948	45.844929
3490.765510	830815.994694	45.849933
3489.941975	829709.817916	45.854938
3488.963838	828542.227878	45.859943
3487.969912	827337.181144	45.864948
3486.839967	826079.019411	45.869953
3485.685676	824768.179355	45.874957
3484.518210	823425.152533	45.879962
3483.565939	822042.487934	45.884967
3482.042623	820607.922343	45.889972
3480.693706	819121.790747	45.894977
3479.533943	817601.776766	45.899981
3478.013656	816045.897356	45.904986
3476.618673	814433.494872	45.909991
3475.153272	812785.411548	45.914996
3473.654063	811086.993943	45.920001
3472.378392	809363.708082	45.925005
3470.839046	807594.447994	45.930010
3468.972356	805772.845864	45.935015
3467.315450	803918.926045	45.940020
3465.757498	802023.601916	45.945025
3464.228632	800098.127779	45.950029
3462.114217	798133.345106	45.955034
3460.495812	796113.516780	45.960039
3458.714792	794063.277288	45.965044
3456.454839	791987.782965	45.970049
3454.787657	789865.574639	45.975053
3452.467197	787711.137044	45.980058
3450.704947	785526.650153	45.985063
3448.596645	783308.998828	45.990068
3446.410837	781054.194621	45.995073
3444.371843	778759.279025	46.000077
3442.243363	776453.796911	46.005082
3439.887701	774094.190434	46.010087
3437.628121	771719.042154	46.015092
3435.346660	769307.366502	46.020097
3432.970577	766851.732252	46.025101
3430.796494	764375.807067	46.030106
3428.563796	761877.405583	46.035111
3426.087444	759343.030378	46.040116
3423.904036	756765.488397	46.045121
3421.661847	754176.300678	46.050125
3419.093033	751542.360300	46.055130
3416.349883	748886.768447	46.060135
3413.885861	746200.775668	46.065140
3410.950545	743486.834647	46.070145
3408.811277	740748.317302	46.075149
3406.060964	737989.659507	46.080154
3403.467676	735201.903735	46.085159
3400.916360	732381.886889	46.090164
3398.364904	729543.938183	46.095169
3395.719394	726670.593549	46.100173
3392.963969	723795.336140	46.105178
3390.150004	720864.343761	46.110183
3387.247714	717924.095058	46.115188
3384.546740	714959.619312	46.120193
3381.895413	711963.258691	46.125197
3378.721956	708960.492528	46.130202
3375.976636	705924.459356	46.135207
3373.058793	702867.645556	46.140212
3369.987372	699785.379409	46.145217
3367.151866	696683.027876	46.150221
3364.149107	693570.351328	46.155226
3361.524270	690428.675098	46.160231
3358.478645	687258.844224	46.165236
3355.090885	684080.020268	46.170241
3352.476928	680869.053330	46.175245
3349.303065	677647.967434	46.180250
3346.194212	674393.124741	46.185255
3343.088634	671138.039978	46.190260
3339.859737	667862.566057	46.195265
3336.903508	664571.152790	46.200269
3333.647261	661264.330174	46.205274
3330.750686	657926.465595	46.210279
3327.432406	654572.091389	46.215284
3323.977818	651213.752619	46.220289
3321.114963	647823.001201	46.225293
3317.865168	644429.214314	46.230298
3314.557381	640999.700002	46.235303
3311.019330	637574.298731	46.240308
3307.484366	634135.980684	46.245313
3304.360678	630677.693973	46.250317
3301.406413	627222.129554	46.255322
3297.781201	623733.630162	46.260327
3294.373262	620238.608950	46.265332
3290.682490	616725.456422	46.270337
3287.553108	613207.180809	46.275341
3283.847385	609672.915992	46.280346
3280.781222	606132.522398	46.285351
3276.902038	602586.033448	46.290356
3273.317952	599021.368621	46.295361
3269.946702	595458.114174	46.300365
3266.739758	591878.960551	46.305370
3262.958065	588289.532173	46.310375
3259.777042	584679.071773	46.315380
3255.841795	581060.368975	46.320385
3252.528562	577438.129089	46.325389
3248.994218	573820.220577	46.330394
3245.434421	570176.667307	46.335399
3241.710820	566537.201224	46.340404
3237.967880	562892.174613	46.345409
3234.844084	559239.586876	46.350413
3230.967998	555565.538210	46.355418
3227.379752	551904.242470	46.360423
3223.871622	548224.330925	46.365428
3220.256168	544535.939486	46.370433
3216.821216	540832.337761	46.375437
3212.830974	537148.014428	46.380442
3209.063211	533431.731512	46.385447
3205.429932	529727.701372	46.390452
3201.589790	526013.637412	46.395457
3198.315854	522303.380454	46.400461
3194.158360	518591.176862	46.405466
3190.570975	514866.224969	46.410471
3187.222599	511130.244107	46.415476
3183.373487	507397.982194	46.420481
3180.043232	503653.303399	46.425485
3176.060711	499915.369888	46.430490
3172.474169	496162.129488	46.435495
3168.879367	492409.097812	46.440500
3164.755610	488651.825156	46.445505
3161.648361	484894.172405	46.450509
3157.827867	481136.272258	46.455514
3153.950819	477372.274217	46.460519
3150.158788	473610.355120	46.465524
3146.085734	469836.884996	46.470529
3142.669975	466060.826572	46.475533
3138.336545	462281.072628	46.480538
3134.671755	458511.756222	46.485543
3131.116456	454734.766715	46.490548
3127.067036	450958.255900	46.495553
3123.556822	447193.670589	46.500557
3119.494221	443414.464852	46.505562
3116.053853	439638.035506	46.510567
3112.344545	435866.969205	46.515572
3108.226698	432086.661022	46.520577
3104.351997	428310.396978	46.525581
3100.317958	424552.297138	46.530586
3096.641721	420768.551331	46.535591
3092.845625	416994.628105	46.540596
3088.638468	413232.316384	46.545601
3085.310148	409452.774087	46.550605
3080.978128	405700.185647	46.555610
3077.051886	401927.065414	46.560615
3073.007256	398173.084572	46.565620
3068.916324	394420.488852	46.570625
3065.371077	390662.092314	46.575629
3061.182928	386923.224982	46.580634
3057.399814	383184.371587	46.585639
3053.610139	379450.206106	46.590644
3049.499127	375716.627546	46.595649
3045.823391	371981.778155	46.600653
3042.048745	368249.793434	46.605658
3037.954582	364540.947096	46.610663
3033.452213	360820.892852	46.615668
3029.863919	357113.627307	46.620673
3026.111928	353394.147506	46.625677
3021.802082	349690.892958	46.630682
3018.200815	345990.361946	46.635687
3013.973948	342304.777812	46.640692
3010.121365	338624.694476	46.645697
3006.440316	334932.076010	46.650701
3001.976573	331254.141991	46.655706
2997.867077	327579.055955	46.660711
2993.705146	323912.440210	46.665716
2989.934177	320259.684239	46.670721
2985.951717	316611.992895	46.675725
2981.741280	312982.333483	46.680730
2977.506529	309347.609916	46.685735
2973.788831	305725.384210	46.690740
2969.264457	302125.192738	46.695745
2965.638184	298512.348094	46.700749
2960.932236	294929.269336	46.705754
2957.101684	291344.026612	46.710759
2953.378758	287774.647082	46.715764
2948.735366	284215.551831	46.720769
2945.076157	280663.909748	46.725773
2940.708553	277130.512884	46.730778
2936.987820	273599.707392	46.735783
2932.460527	270079.752472	46.740788
2928.480350	266574.598995	46.745793
2924.209547	263074.459004	46.750797
2919.929427	259598.500383	46.755802
2915.922247	256114.298699	46.760807
2911.690793	252653.978465	46.765812
2907.735451	249211.259338	46.770817
2903.462093	245772.671076	46.775821
2899.010411	242354.068650	46.780826
2894.754117	238942.084339	46.785831
2890.737625	235554.956771	46.790836
2886.109284	232178.948841	46.795841
2882.368015	228817.503321	46.800845
2877.568043	225465.025173	46.805850
2873.360079	222134.713151	46.810855
2869.732368	218816.899858	46.815860
2865.288745	215511.888837	46.820865
2861.246467	212212.392580	46.825869
2856.578189	208945.576737	46.830874
2852.923821	205676.963383	46.835879
2848.596155	202432.929151	46.840884
2844.253912	199214.014828	46.845889
2840.164098	195984.099434	46.850893
2835.710260	192782.709429	46.855898
2831.481123	189599.649053	46.860903
2827.645919	186422.802682	46.865908
2823.054839	183273.161237	46.870913
2818.610629	180113.845868	46.875917
2814.077860	177005.781433	46.880922
2809.784273	173903.559952	46.885927
2806.248664	170793.842328	46.890932
2801.715578	167659.497538	46.895937
2797.804873	164599.962506	46.900941
2793.310831	161563.071573	46.905946
2789.357328	158547.927250	46.910951
2784.917736	155536.761331	46.915956
2780.884180	152536.974408	46.920961
2777.077962	149553.511380	46.925965
2772.453410	146595.587116	46.930970
2767.976448	143649.946715	46.935975
2764.067829	140729.430129	46.940980
2759.861405	137811.439032	46.945985
2755.669915	134914.326025	46.950989
2751.191496	132038.064049	46.955994
2747.464938	129179.922991	46.960999
2743.012503	126329.706246	46.966004
2738.648626	123490.584646	46.971009
2734.590195	120677.623358	46.976013
2730.142369	117880.859396	46.981018
2726.227060	115096.221318	46.986023
2722.190862	112329.205005	46.991028
2717.809216	109585.351905	46.996033
2713.488892	106843.533127	47.001037
2709.111725	104133.936783	47.006042
2704.978752	101434.599738	47.011047
2701.535052	98757.211223	47.016052
2696.730751	96093.042657	47.021057
2692.983185	93436.837693	47.026061
2688.237696	90817.420875	47.031066
2684.342939	88195.225872	47.036071
2680.815018	85591.803697	47.041076
2675.958136	83006.491683	47.046081
2671.578031	80436.644343	47.051085
2667.376901	77888.252247	47.056090
2663.126024	75352.675587	47.061095
2658.783164	72842.226267	47.066100
2654.687427	70351.667721	47.071105
2650.559910	67866.676279	47.076109
2646.406628	65412.611120	47.081114
2641.967110	62976.604797	47.086119
2637.702704	60549.717974	47.091124
2633.481031	58148.045543	47.096129
2629.155338	55750.389121	47.101133
2624.947833	53398.290333	47.106138
2620.659680	51042.587661	47.111143
2616.455203	48707.566208	47.116148
2611.561358	46409.428112	47.121153
2607.300315	44127.252765	47.126157
2603.218146	41850.919180	47.131162
2598.630264	39604.958983	47.136167
2594.449702	37381.653238	47.141172
2590.009857	35189.583801	47.146177
2585.818204	32985.505643	47.151181
2581.195060	30842.492553	47.156186
2577.087753	28698.820709	47.161191
2572.779934	26594.892457	47.166196
2568.052163	24505.553493	47.171201
2563.621070	22432.336717	47.176205
2558.939485	20394.601071	47.181210
2554.040624	18391.122836	47.186215
2548.703969	16407.649722	47.191220
2542.469092	14492.729193	47.196225
2535.347771	12660.337797	47.201229
2526.278488	10926.767844	47.206234
2517.540749	9261.672862	47.211239
2508.513775	7706.755067	47.216244
2498.353059	6275.343085	47.221249
2486.437487	4984.298203	47.226253
2474.351291	3849.197874	47.231258
2462.897056	2849.164539	47.236263
2451.918782	1998.069227	47.241268
2441.774522	1288.310884	47.246273
2431.923980	711.196372	47.251277
2420.895752	315.069184	47.256282
2404.466792	212.939798	47.261287
2391.482808	219.868737	47.266292
2385.557766	222.801586	47.271297
2385.268041	223.435417	47.276301
2387.736132	228.801273	47.281306
2390.425792	233.904669	47.286311
2392.238562	231.982207	47.291316
2391.846126	229.632743	47.296321
2390.849649	231.940100	47.301325
2388.666916	219.901309	47.306330
2386.007364	218.621555	47.311335
2383.094167	202.014506	47.316340
2379.631219	210.121122	47.321345
2376.809693	203.956366	47.326349
2373.428704	210.699185	47.331354
2370.058516	206.363564	47.336359
2367.627716	202.963032	47.341364
2364.623920	215.253243	47.346369
2361.657072	207.554595	47.351373
2357.978891	207.532074	47.356378
2355.539204	208.287111	47.361383
2352.046092	215.965004	47.366388
2348.765352	210.492217	47.371393
2346.082119	199.392330	47.376397
2342.811814	209.689860	47.381402
2339.568963	215.525190	47.386407
2336.035105	212.328872	47.391412
2332.441276	217.212999	47.396417
2329.650844	206.512714	47.401421
2326.413907	208.727641	47.406426
2322.731851	209.841572	47.411431
2319.407179	196.776032	47.416436
2316.126792	207.211191	47.421441
2312.933258	204.613398	47.426445
2309.148808	213.083555	47.431450
2305.801960	208.336163	47.436455
2303.269922	198.383272	47.441460
2299.442751	210.615638	47.446465
2296.252913	201.553466	47.451469
2292.789793	201.497321	47.456474
2288.947800	209.030484	47.461479
2285.976529	194.900393	47.466484
2282.317822	201.028593	47.471489
2278.850377	201.824212	47.476493
2275.790948	198.104421	47.481498
2271.954668	195.683135	47.486503
2268.932818	196.836166	47.491508
2265.735428	214.193573	47.496513
2262.595067	198.289695	47.501517
2259.114921	208.202440	47.506522
2255.327304	201.461179	47.511527
2251.942714	196.207166	47.516532
2247.971009	203.441080	47.521537
2244.701168	194.951454	47.526541
2241.771804	194.542888	47.531546
2237.444492	202.753130	47.536551
2234.370394	201.781892	47.541556
2230.918392	199.262530	47.546561
2227.368146	202.902790	47.551565
2223.791499	192.221149	47.556570
2220.489337	193.585735	47.561575
2216.846629	189.457330	47.566580
2213.466749	197.683867	47.571585
2210.339706	193.977841	47.576589
2207.079772	192.412403	47.581594
2204.091152	194.423991	47.586599
2200.217293	194.242306	47.591604
2196.804961	195.893065	47.596609
2193.620295	191.240569	47.601613
2189.708026	197.123717	47.606618
2186.446454	195.558543	47.611623
2182.633715	194.345370	47.616628
2179.106170	198.415541	47.621633
2175.633015	196.174766	47.626637
2172.041790	196.856902	47.631642
2168.940967	187.888429	47.636647
2165.407678	189.583433	47.641652
2161.769240	194.395486	47.646657
2158.786327	191.457894	47.651661
2155.502556	193.164483	47.656666
2151.635930	195.012891	47.661671
2148.186113	192.951978	47.666676
2144.626134	191.471473	47.671681
2141.065585	191.680566	47.676685
2137.219276	190.276502	47.681690
2134.194671	193.787085	47.686695
2130.877942	193.651137	47.691700
2126.881011	198.569915	47.696705
2123.549419	201.068637	47.701709
2120.252180	192.633967	47.706714
2116.554540	191.643264	47.711719
2113.612179	185.168460	47.716724
2110.170547	192.243541	47.721729
2106.556856	193.660068	47.726733
2102.774655	192.309263	47.731738
2099.031496	190.613817	47.736743
2095.706861	194.807293	47.741748
2092.347468	197.952639	47.746753
2089.236075	194.225219	47.751757
2085.771677	190.388514	47.756762
2082.051777	198.693596	47.761767
2078.469559	190.135848	47.766772
2074.855989	198.449606	47.771777
2071.616874	193.612674	47.776781
2067.936586	196.444392	47.781786
2064.578641	195.834005	47.786791
2061.056628	193.157972	47.791796
2057.394158	193.661460	47.796801
2054.029402	187.062936	47.801805
2050.364349	185.605233	47.806810
2047.058042	194.532167	47.811815
2043.724736	181.708559	47.816820
2040.387186	178.775874	47.821825
2036.781387	180.637293	47.826829
2033.040710	179.324312	47.831834
2029.696397	182.451495	47.836839
2026.456325	180.901991	47.841844
2022.498342	179.002898	47.846849
2019.162248	172.523299	47.851853
2015.619464	177.352062	47.856858
2011.915036	183.158445	47.861863
2008.982185	179.618260	47.866868
2005.465936	184.585250	47.871873
2002.251564	181.339063	47.876877
1998.270692	180.183906	47.881882
1994.636932	186.089972	47.886887
1991.190938	172.787300	47.891892
1987.515851	183.591170	47.896897
1984.633668	181.650308	47.901901
1981.032000	187.535538	47.906906
1977.320012	186.698995	47.911911
1973.765826	186.692004	47.916916
1970.215072	183.406712	47.921921
1966.581485	185.592052	47.926925
1963.425334	185.794874	47.931930
1959.905907	180.426024	47.936935
1956.490179	170.105322	47.941940
1952.894131	179.134558	47.946945
1949.501017	176.669359	47.951949
1945.893369	171.874326	47.956954
1941.978853	181.348884	47.961959
1938.805952	178.526515	47.966964
1935.270721	182.620104	47.971969
1931.797898	176.383402	47.976973
1928.739860	178.934287	47.981978
1925.103694	176.000912	47.986983
1921.689990	164.053686	47.991988
1917.936844	180.030046	47.996993
1914.242912	173.875409	48.001997
1910.780469	177.888010	48.007002
1907.098183	167.751416	48.012007
1904.095824	175.741765	48.017012
1900.417172	176.326936	48.022017
1896.872450	174.258816	48.027021
1893.363335	175.595769	48.032026
1890.072192	172.927966	48.037031
1886.926110	173.891726	48.042036
1882.981413	182.235197	48.047041
1879.610604	168.145665	48.052045
1876.087841	175.695420	48.057050
1872.558324	185.609643	48.062055
1869.471184	170.985323	48.067060
1865.343272	179.161310	48.072065
1861.898991	175.296230	48.077069
1858.106862	177.379861	48.082074
1854.727304	178.551015	48.087079
1851.510448	169.683086	48.092084
1847.579442	170.583022	48.097089
1844.345650	176.752416	48.102093
1841.110353	181.697633	48.107098
1837.768108	174.171825	48.112103
1834.179513	167.988083	48.117108
1830.239349	176.590295	48.122113
1827.107510	174.229789	48.127117
1823.861239	168.312030	48.132122
1820.409162	171.433989	48.137127
1816.543197	166.372538	48.142132
1812.471924	175.473015	48.147137
1809.322615	167.882225	48.152141
1806.239928	171.746837	48.157146
1802.519641	174.148285	48.162151
1799.521827	171.684554	48.167156
1795.279671	176.863283	48.172161
1791.854530	174.668915	48.177165
1788.969716	175.085598	48.182170
1785.644260	177.194301	48.187175
1781.685449	168.189405	48.192180
1778.134490	168.726160	48.197185
1774.330737	159.836215	48.202189
1771.129503	163.732043	48.207194
1767.510362	169.828879	48.212199
1764.240125	170.824759	48.217204
1760.634150	165.975752	48.222209
1756.802055	163.756498	48.227213
1753.431770	170.402869	48.232218
1749.839070	178.327448	48.237223
1746.665121	161.726707	48.242228
1743.378827	166.917217	48.247233
1739.975797	160.277354	48.252237
1736.229021	159.566571	48.257242
1732.712484	162.470845	48.262247
1729.125011	159.352750	48.267252
1725.338624	160.780609	48.272257
1721.369543	158.139868	48.277261
1718.283120	158.202132	48.282266
1714.879984	155.615196	48.287271
1711.812333	157.702555	48.292276
1708.284713	160.222582	48.297281
1704.581316	164.326737	48.302285
1701.166285	163.472295	48.307290
1696.819119	163.671764	48.312295
1694.170273	151.279064	48.317300
1690.460420	157.541980	48.322305
1687.041275	154.989198	48.327309
1683.686663	160.649173	48.332314
1680.192320	153.808485	48.337319
1676.605501	150.310647	48.342324
1673.034137	154.099907	48.347329
1669.654938	157.460449	48.352333
1666.083606	151.903686	48.357338
1662.033856	155.356520	48.362343
1658.831613	160.363049	48.367348
1655.681883	167.303968	48.372353
1652.330818	161.677930	48.377357
1648.894354	161.263473	48.382362
1645.238390	161.282015	48.387367
1641.900535	154.663631	48.392372
1637.614569	165.566353	48.397377
1634.172446	156.619874	48.402381
1630.949169	152.201423	48.407386
1627.424317	159.258006	48.412391
1624.382330	158.427465	48.417396
1620.544596	161.647810	48.422401
1617.094137	161.283011	48.427405
1613.469934	157.718278	48.432410
1609.785976	169.545550	48.437415
1606.584058	155.170282	48.442420
1602.778639	149.343288	48.447425
1599.369659	161.763455	48.452429
1596.096239	151.439625	48.457434
1592.353228	163.908911	48.462439
1589.059277	161.130918	48.467444
1585.683324	162.871085	48.472449
1581.980432	168.133172	48.477453
1578.894767	151.319376	48.482458
1575.038777	158.987803	48.487463
1571.476882	153.790279	48.492468
1568.211728	157.648709	48.497473
1564.419430	155.954830	48.502477
1561.290782	160.329751	48.507482
1557.679068	155.345679	48.512487
1553.906411	162.751128	48.517492
1550.850749	169.791249	48.522497
1547.275910	165.361409	48.527501
1543.617414	159.729746	48.532506
1539.820548	164.604745	48.537511
1536.589228	155.837290	48.542516
1532.950332	161.968924	48.547521
1529.451830	158.976188	48.552525
1526.333934	155.000037	48.557530
1522.516609	159.052478	48.562535
1518.977439	151.706328	48.567540
1515.559229	156.351217	48.572545
1512.093374	159.984806	48.577549
1508.599398	153.827521	48.582554
1504.389551	150.680374	48.587559
1501.363216	147.208773	48.592564
1498.024221	156.118790	48.597569
1494.488964	153.884817	48.602573
1491.171733	151.910957	48.607578
1487.215158	156.057974	48.612583
1483.759771	149.208105	48.617588
1480.633152	154.107928	48.622593
1477.334034	150.498693	48.627597
1473.655478	149.407160	48.632602
1469.743855	153.360480	48.637607
1466.554441	145.950117	48.642612
1462.979867	146.481184	48.647617
1459.487206	149.720339	48.652621
1455.674001	152.307296	48.657626
1452.119861	158.159924	48.662631
1448.920936	158.211405	48.667636
1445.853926	159.042692	48.672641
1442.151281	157.540477	48.677645
1438.700913	154.255495	48.682650
1435.049342	157.177838	48.687655
1431.645272	153.588210	48.692660
1427.843161	153.591742	48.697665
1424.619987	151.894257	48.702669
1421.182471	160.221750	48.707674
1417.508409	156.452919	48.712679
1413.809142	156.120810	48.717684
1409.937630	154.705154	48.722689
1406.878174	155.842163	48.727693
1403.435607	161.895647	48.732698
1399.684652	153.092526	48.737703
1396.598010	151.433791	48.742708
1392.847456	150.287118	48.747713
1389.678577	150.840131	48.752717
1386.070516	151.430253	48.757722
1382.414804	151.524784	48.762727
1378.950166	151.981724	48.767732
1375.384853	156.886970	48.772737
1371.557120	151.870349	48.777741
1368.751232	156.387793	48.782746
1365.146145	156.942655	48.787751
1361.480098	157.709546	48.792756
1357.727877	149.074329	48.797761
1354.215372	151.047923	48.802765
1350.692669	148.049553	48.807770
1347.217758	153.266532	48.812775
1344.133521	143.612407	48.817780
1340.843472	151.268246	48.822785
1337.224435	154.777168	48.827789
1333.469323	150.214281	48.832794
1329.700563	149.323590	48.837799
1326.428659	154.841000	48.842804
1322.786261	157.632228	48.847809
1319.175259	153.910516	48.852813
1315.972712	151.925092	48.857818
1312.151089	159.784382	48.862823
1309.220376	150.362505	48.867828
1305.579847	162.546897	48.872833
1301.803136	156.551017	48.877837
1298.257767	147.117796	48.882842
1294.660020	154.024529	48.887847
1291.027775	149.724008	48.892852
1287.957268	150.998827	48.897857
1284.291912	146.216262	48.902861
1281.209707	148.201615	48.907866
1277.407666	144.095365	48.912871
1274.350004	146.861511	48.917876
1270.425549	151.190244	48.922881
1266.912360	147.570304	48.927885
1263.745844	145.534964	48.932890
1259.578180	156.501548	48.937895
1256.131145	148.761425	48.942900
1252.724911	155.828021	48.947905
1249.257754	144.949359	48.952909
1245.714711	139.584500	48.957914
1242.309473	145.002579	48.962919
1238.986967	137.916871	48.967924
1235.425104	149.389750	48.972929
1231.754878	152.334065	48.977933
1228.981493	137.955170	48.982938
1224.674585	140.844131	48.987943
1221.087309	144.490491	48.992948
1217.551194	141.351900	48.997953
1214.407883	142.347067	49.002957
1210.479990	152.383925	49.007962
1206.983905	150.710255	49.012967
1203.935614	138.554293	49.017972
1200.541945	142.939162	49.022977
1197.157159	144.348634	49.027981
1193.588759	142.714766	49.032986
1189.541819	144.294345	49.037991
1186.560712	145.919041	49.042996
1182.703543	143.773550	49.048001
1179.160155	145.280627	49.053005
1175.682345	138.339484	49.058010
1172.237053	147.630064	49.063015
1168.910861	143.711962	49.068020
1165.294402	152.425051	49.073025
1161.486275	149.677089	49.078029
1158.435909	144.320555	49.083034
1154.632603	145.564604	49.088039
1151.536626	140.569565	49.093044
1148.009854	153.081041	49.098049
1144.397559	146.866499	49.103053
1140.528762	149.278771	49.108058
1137.003122	164.653353	49.113063
1133.763031	145.899200	49.118068
1130.216123	142.762333	49.123073
1126.849598	145.788854	49.128077
1123.440227	146.585252	49.133082
1119.325206	155.914264	49.138087
1116.325865	153.761050	49.143092
1112.967117	154.634950	49.148097
1108.992226	152.087129	49.153101
1105.374804	152.757915	49.158106
1102.407174	152.314541	49.163111
1098.997463	146.409996	49.168116
1095.329717	140.647096	49.173121
1091.762478	143.262116	49.178125
1088.556859	149.765823	49.183130
1084.628448	154.440102	49.188135
1081.429840	151.030417	49.193140
1077.671830	144.360979	49.198145
1073.706941	144.753976	49.203149
1070.643955	146.983162	49.208154
1066.813073	156.169627	49.213159
1063.787184	140.061747	49.218164
1060.062034	145.112344	49.223169
1056.598168	147.986445	49.228173
1053.366597	146.673227	49.233178
1049.929767	149.625357	49.238183
1046.644109	153.601050	49.243188
1042.706827	156.925776	49.248193
1039.232843	153.881933	49.253197
1035.714053	139.632479	49.258202
1032.154100	148.738566	49.263207
1028.397383	139.145568	49.268212
1024.976861	150.004736	49.273217
1021.085871	147.845625	49.278221
1018.454009	151.592407	49.283226
1014.793391	150.862083	49.288231
1011.275641	137.536320	49.293236
1007.596701	145.243646	49.298241
1004.392373	156.986486	49.303245
1000.845126	148.243408	49.308250
996.876292	149.595695	49.313255
993.739550	142.942919	49.318260
990.014616	154.435072	49.323265
986.436131	150.452134	49.328269
983.101478	148.383105	49.333274
979.439860	153.082090	49.338279
975.514152	147.068557	49.343284
972.513448	151.012311	49.348289
969.227435	146.123024	49.353293
965.862689	149.611239	49.358298
961.698982	158.748609	49.363303
958.500153	149.296082	49.368308
955.287930	142.155254	49.373313
951.851759	139.339650	49.378317
948.077939	145.366039	49.383322
944.407776	151.170550	49.388327
941.320397	134.506034	49.393332
937.674598	140.544017	49.398337
934.150276	141.314187	49.403341
930.816707	140.520032	49.408346
926.878103	146.660818	49.413351
923.738999	150.778120	49.418356
919.901028	147.766007	49.423361
916.576518	144.410900	49.428365
913.135662	143.225417	49.433370
909.609035	148.596166	49.438375
906.316091	144.951375	49.443380
902.816335	139.061012	49.448385
898.644585	142.732561	49.453389
895.300018	143.550531	49.458394
891.597901	147.499731	49.463399
888.476820	140.800251	49.468404
884.803644	148.753494	49.473409
881.352697	138.660260	49.478413
878.403400	140.846391	49.483418
874.731265	148.375521	49.488423
871.434932	141.007448	49.493428
867.456618	139.232246	49.498433
864.165943	136.732423	49.503437
860.823646	143.630926	49.508442
856.979520	141.958106	49.513447
853.272737	143.712353	49.518452
849.805700	147.052104	49.523457
846.382881	144.386314	49.528461
843.129706	146.003094	49.533466
839.157774	154.987087	49.538471
836.368116	144.647946	49.543476
832.520568	142.994654	49.548481
828.922689	135.104332	49.553485
825.131484	137.390677	49.558490
821.643080	156.423207	49.563495
818.722352	144.146187	49.568500
815.133182	139.152571	49.573505
811.554363	141.158885	49.578509
808.072475	142.026863	49.583514
804.032916	146.323172	49.588519
800.838056	143.833679	49.593524
797.566637	144.200456	49.598529
794.116614	143.430914	49.603533
790.529213	140.082222	49.608538
787.119428	140.502308	49.613543
783.210953	140.231680	49.618548
779.824798	147.918542	49.623553
776.005698	142.790102	49.628557
772.976152	141.407381	49.633562
769.313448	141.231151	49.638567
766.103208	145.188793	49.643572
763.008540	141.240919	49.648577
758.817641	139.018154	49.653581
755.618600	130.388351	49.658586
752.013057	142.728758	49.663591
748.300169	136.862347	49.668596
744.616272	139.483104	49.673601
741.626376	140.289879	49.678605
737.785534	137.888916	49.683610
733.714519	146.325297	49.688615
730.668462	133.153603	49.693620
727.485587	143.048632	49.698625
723.986586	139.705106	49.703629
720.534982	135.145580	49.708634
716.865358	143.398882	49.713639
713.728261	136.249555	49.718644
709.920978	139.715405	49.723649
706.162553	133.460668	49.728653
703.114947	133.267233	49.733658
699.178069	144.840115	49.738663
696.263815	129.638770	49.743668
692.588158	131.897579	49.748673
688.854300	135.291825	49.753677
685.363168	134.781870	49.758682
681.484272	132.703274	49.763687
678.363399	144.591305	49.768692
674.697234	141.441661	49.773697
671.308965	139.786116	49.778701
668.042644	137.187639	49.783706
664.309242	136.709305	49.788711
660.990899	135.482585	49.793716
657.481050	142.378915	49.798721
653.785751	142.720376	49.803725
650.608129	134.644093	49.808730
646.782008	142.020238	49.813735
643.141280	139.951816	49.818740
639.666627	127.448416	49.823745
636.103311	143.012503	49.828749
632.915343	132.944641	49.833754
629.082585	134.038482	49.838759
625.775136	124.675890	49.843764
622.270690	126.303622	49.848769
618.722638	123.581606	49.853773
615.349085	129.257512	49.858778
611.479630	133.394374	49.863783
608.400530	124.606644	49.868788
604.845740	130.687432	49.873793
601.364461	131.049180	49.878797
598.119066	131.924490	49.883802
594.337906	130.150172	49.888807
591.028713	133.174219	49.893812
587.226399	130.934971	49.898817
583.593895	135.246710	49.903821
580.100032	131.393066	49.908826
576.753494	132.113378	49.913831
573.422245	131.201931	49.918836
569.760254	128.285804	49.923841
566.022841	127.020349	49.928845
562.945350	122.443428	49.933850
559.378545	135.236571	49.938855
555.946379	122.441819	49.943860
552.263988	127.833914	49.948865
548.704886	127.755445	49.953869
545.098216	128.272898	49.958874
541.680027	131.905666	49.963879
537.996251	127.686308	49.968884
535.051298	126.100592	49.973889
531.419538	126.954180	49.978893
527.673591	126.553800	49.983898
523.943173	136.971244	49.988903
520.632097	128.887447	49.993908
517.229484	131.033953	49.998913
513.496634	131.216834	50.003917
509.985097	133.332946	50.008922
506.071155	137.606535	50.013927
503.287840	128.601672	50.018932
499.564264	137.863260	50.023937
496.243526	134.428633	50.028941
492.882539	127.289156	50.033946
489.112873	130.825130	50.038951
486.173018	122.426938	50.043956
481.794826	126.346134	50.048961
478.447172	130.667079	50.053965
475.048184	126.577153	50.058970
471.660862	130.885330	50.063975
468.159180	128.962886	50.068980
464.357747	126.002206	50.073985
460.908461	127.074019	50.078989
457.800376	125.865064	50.083994
454.240539	124.400997	50.088999
450.589984	119.989812	50.094004
447.163512	123.652383	50.099009
443.631189	123.022421	50.104013
440.336714	123.984570	50.109018
436.699284	128.885601	50.114023
433.441115	128.639816	50.119028
430.010250	125.124389	50.124033
425.998889	130.859130	50.129037
422.427784	122.971136	50.134042
419.012616	133.595501	50.139047
415.556753	127.252381	50.144052
411.919383	123.914843	50.149057
408.407337	126.341127	50.154061
405.128770	128.692874	50.159066
401.712450	132.970816	50.164071
398.082800	119.431943	50.169076
394.422564	122.264264	50.174081
390.911114	127.344899	50.179085
387.903160	119.185210	50.184090
383.923833	116.945308	50.189095
380.904232	118.320010	50.194100
377.007044	123.840728	50.199105
373.425074	128.489482	50.204109
370.402149	123.505447	50.209114
366.575447	126.683400	50.214119
363.040254	112.958909	50.219124
359.592664	123.411191	50.224129
355.579235	126.678511	50.229133
352.660607	125.360821	50.234138
349.112576	122.765468	50.239143
345.236322	121.202312	50.244148
341.614803	119.055080	50.249153
338.459282	118.027609	50.254157
335.193179	118.188071	50.259162
331.444546	132.294266	50.264167
328.302542	127.126416	50.269172
324.730991	124.737240	50.274177
321.182200	133.047673	50.279181
317.701843	130.549301	50.284186
314.533617	122.819714	50.289191
310.661164	120.385930	50.294196
306.995803	130.046591	50.299201
303.099040	126.888942	50.304205
299.841369	133.489614	50.309210
296.241404	132.016078	50.314215
292.719715	123.032053	50.319220
289.744329	118.913815	50.324225
286.175983	130.634744	50.329229
282.814799	116.421117	50.334234
278.425143	122.183537	50.339239
275.344835	124.013881	50.344244
271.973356	122.381175	50.349249
268.435134	131.863743	50.354253
265.239009	123.939227	50.359258
261.396893	130.444801	50.364263
258.193595	120.983802	50.369268
254.584011	118.145027	50.374273
250.992652	119.593522	50.379277
247.627257	119.516466	50.384282
243.594710	123.473375	50.389287
239.902066	124.029728	50.394292
236.706498	120.648367	50.399297
233.179290	125.908699	50.404301
230.143330	125.093495	50.409306
226.021475	125.802517	50.414311
222.785784	121.924402	50.419316
219.254073	120.152301	50.424321
215.653728	119.169250	50.429325
212.652162	117.551386	50.434330
208.709067	124.670757	50.439335
205.212192	119.242172	50.444340
201.774075	123.352751	50.449345
198.634186	127.549491	50.454349
195.200018	115.615793	50.459354
191.446634	119.851696	50.464359
187.917465	122.929325	50.469364
184.553539	121.219539	50.474369
180.789281	126.134206	50.479373
177.521894	126.797973	50.484378
174.187120	123.403644	50.489383
170.214980	117.790099	50.494388
166.836103	117.171013	50.499393
163.109677	120.111872	50.504397
159.972323	124.985281	50.509402
156.284946	122.452970	50.514407
152.463538	120.362446	50.519412
149.408007	119.749657	50.524417
145.627252	120.145845	50.529421
142.345497	114.645621	50.534426
139.091151	119.065958	50.539431
135.303563	126.012296	50.544436
131.927136	124.918268	50.549441
127.953804	129.634755	50.554445
124.789055	119.361007	50.559450
121.402019	126.108552	50.564455
117.859452	116.858962	50.569460
114.320015	112.212220	50.574465
110.413116	117.661797	50.579469
107.426587	120.752517	50.584474
103.842587	123.392672	50.589479
100.100941	114.952578	50.594484
96.717226	120.636572	50.599489
93.697910	122.318214	50.604493
90.126234	109.400027	50.609498
86.254043	119.165928	50.614503
82.641189	121.478412	50.619508
79.454442	128.555266	50.624513
75.707818	123.925180	50.629517
72.135656	114.784656	50.634522
68.759999	117.126422	50.639527
65.167617	114.126847	50.644532
61.638095	112.810058	50.649537
58.051212	117.317324	50.654541
54.548998	113.579116	50.659546
50.912579	128.784634	50.664551
47.825717	118.685383	50.669556
44.426081	122.612817	50.674561
41.221907	119.438530	50.679565
37.522670	114.639686	50.684570
33.689343	131.597171	50.689575
29.986601	121.002792	50.694580
26.510267	120.588858	50.699585
22.919848	112.647137	50.704589
19.615018	125.029220	50.709594
16.305712	110.424786	50.714599
12.585258	115.535136	50.719604
9.217833	109.054961	50.724609
5.680683	115.582450	50.729613
2.335059	119.166073	50.734618