Thu Aug 25 17:07:17 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
1.087857	86.586061	0.000000
0.890094	94.700612	0.005005
0.965796	95.337389	0.010010
0.732102	100.426653	0.015014
0.665615	92.755425	0.020019
0.737497	89.444380	0.025024
0.761810	78.275590	0.030029
0.581899	68.280934	0.035034
0.167201	53.643823	0.040038
0.176571	47.681831	0.045043
-0.294163	39.760749	0.050048
-0.751354	26.212334	0.055053
-0.492031	23.530000	0.060058
-1.046420	19.842526	0.065062
-1.258481	-2.666149	0.070067
-1.779645	-5.422344	0.075072
-2.327546	-0.619238	0.080077
-2.391652	-12.191738	0.085082
-3.262022	-6.604112	0.090086
-3.303068	-13.225741	0.095091
-3.538410	-12.771188	0.100096
-3.841196	-5.956360	0.105101
-3.441441	-16.358170	0.110106
-4.058229	-14.103772	0.115110
-5.014281	-16.519740	0.120115
-4.610874	-16.848645	0.125120
-5.136444	-14.852151	0.130125
-4.896409	-11.583550	0.135130
-5.206417	-5.985646	0.140134
-5.816835	-14.099954	0.145139
-6.198771	-21.924189	0.150144
-6.883326	-7.282467	0.155149
-6.610577	-21.384980	0.160154
-6.860619	-12.762409	0.165158
-6.668172	-11.954101	0.170163
-6.825709	-10.249391	0.175168
-7.697220	-16.285314	0.180173
-7.661102	-15.449348	0.185178
-8.050920	-7.716043	0.190182
-7.809117	-7.133769	0.195187
-7.827318	-10.307293	0.200192
-9.238654	-5.666299	0.205197
-9.221342	-16.137900	0.210202
-9.526845	-8.164704	0.215206
-9.257818	-11.395887	0.220211
-9.591315	-7.297099	0.225216
-10.023932	-7.080557	0.230221
-10.424236	-18.919916	0.235226
-10.654014	-20.348683	0.240230
-11.183402	-13.257906	0.245235
-10.772161	-12.759128	0.250240
-11.122232	-1.684769	0.255245
-11.127982	-17.100911	0.260250
-11.818204	-4.394532	0.265254
-12.021172	-11.376772	0.270259
-12.514380	-12.482688	0.275264
-13.000263	-5.923912	0.280269
-12.436251	-6.078663	0.285274
-12.179258	1.018621	0.290278
-13.460543	-2.694160	0.295283
-13.743176	-2.254344	0.300288
-14.082923	-6.668310	0.305293
-14.007308	-6.512418	0.310298
-14.042024	-7.123856	0.315302
-14.462090	-17.827485	0.320307
-14.919621	-16.037805	0.325312
-15.477317	-11.527399	0.330317
-15.492260	-27.223668	0.335322
-15.623138	-11.020374	0.340326
-15.631166	-13.727252	0.345331
-15.662890	-21.179248	0.350336
-15.905979	-18.717646	0.355341
-16.401732	-23.296991	0.360346
-16.967793	-11.274464	0.365350
-17.174677	-16.636233	0.370355
-17.005372	-17.409352	0.375360
-17.452991	-6.680383	0.380365
-17.795043	-12.694860	0.385370
-18.252539	-8.598789	0.390374
-18.424117	-15.911815	0.395379
-18.488831	-12.952973	0.400384
-18.656168	-13.300020	0.405389
-18.506508	-19.413684	0.410394
-19.523605	-13.097547	0.415398
-19.856482	-11.491915	0.420403
-20.067613	-8.782216	0.425408
-20.122281	-2.958561	0.430413
-20.274346	-10.673283	0.435418
-20.008884	-12.812403	0.440422
-20.613605	-9.269072	0.445427
-20.979449	-14.245264	0.450432
-21.393223	-7.466831	0.455437
-20.863700	-15.288345	0.460442
-21.757286	-5.153892	0.465446
-22.059886	-13.889073	0.470451
-22.226006	-9.797528	0.475456
-22.442040	-9.077079	0.480461
-22.210316	-15.621221	0.485466
-22.953731	-6.946655	0.490470
-23.283262	-19.100824	0.495475
-23.263913	-13.696898	0.500480
-23.662902	-14.592948	0.505485
-23.786372	-12.336750	0.510490
-24.557570	-8.156725	0.515494
-25.010084	-2.837050	0.520499
-25.280528	-7.647856	0.525504
-25.507772	-6.169506	0.530509
-25.329890	-6.520024	0.535514
-25.279831	-8.040094	0.540518
-25.249846	-3.096580	0.545523
-25.456931	-4.177724	0.550528
-26.141529	-0.258041	0.555533
-26.209298	-12.424754	0.560538
-26.847792	-6.092005	0.565542
-27.343516	-1.876046	0.570547
-27.829129	-12.730759	0.575552
-28.126586	-6.631781	0.580557
-27.864635	-10.994489	0.585562
-27.964669	-3.471105	0.590566
-28.164981	-9.080680	0.595571
-28.022169	-12.241466	0.600576
-28.443898	-6.040758	0.605581
-28.867967	-14.899275	0.610586
-29.473917	-7.771189	0.615590
-29.356045	-8.681784	0.620595
-29.641950	-7.444182	0.625600
-30.537971	-7.379659	0.630605
-30.562231	-8.299622	0.635610
-30.924557	-5.256182	0.640614
-31.058687	-8.060362	0.645619
-31.159413	-11.594281	0.650624
-31.520223	-0.423326	0.655629
-31.562861	-10.499554	0.660634
-31.369527	-1.645892	0.665638
-31.480427	-3.064812	0.670643
-32.033550	-11.896782	0.675648
-32.832464	-4.352479	0.680653
-32.845621	0.626270	0.685658
-32.831256	-5.671845	0.690662
-33.087562	0.309955	0.695667
-33.668128	-5.543763	0.700672
-34.267043	1.488311	0.705677
-34.205077	2.538528	0.710682
-34.210020	-0.115051	0.715686
-34.255884	-2.664140	0.720691
-34.777341	-6.587721	0.725696
-35.243744	-10.557893	0.730701
-35.543034	1.590523	0.735706
-35.751429	5.941798	0.740710
-35.878014	5.645314	0.745715
-35.785934	-8.909793	0.750720
-36.031958	-1.812790	0.755725
-36.286736	-2.095515	0.760730
-36.751245	-10.704086	0.765734
-37.321834	-2.379303	0.770739
-37.252596	-4.076387	0.775744
-37.533867	1.646732	0.780749
-38.338657	-15.912640	0.785754
-38.764731	-4.411920	0.790758
-38.891216	4.536149	0.795763
-38.175874	-9.449055	0.800768
-38.606180	-1.712568	0.805773
-38.617002	-6.551397	0.810778
-38.775274	-2.682545	0.815782
-39.450455	-4.414850	0.820787
-39.741563	-7.330475	0.825792
-40.425796	-4.040442	0.830797
-40.375832	-7.952316	0.835802
-40.319709	-5.303475	0.840806
-41.180910	5.240365	0.845811
-41.569012	-12.207127	0.850816
-41.767407	0.475976	0.855821
-41.681579	-14.024361	0.860826
-41.715955	-2.218016	0.865830
-41.922601	-2.853136	0.870835
-41.503192	-12.384822	0.875840
-42.333473	1.976017	0.880845
-42.865827	-7.140785	0.885850
-43.228070	0.717917	0.890854
-43.371942	-2.537157	0.895859
-43.406629	-4.910825	0.900864
-44.534301	2.280029	0.905869
-44.450725	-10.720325	0.910874
-44.638124	-3.936232	0.915878
-44.522224	3.369821	0.920883
-44.726909	-2.254889	0.925888
-44.775845	5.203544	0.930893
-44.773672	-1.810840	0.935898
-45.307364	2.917273	0.940902
-45.626640	1.866364	0.945907
-45.832193	1.841683	0.950912
-46.464195	3.899151	0.955917
-47.021972	0.386224	0.960922
-47.312201	-7.265719	0.965926
-47.785173	2.606679	0.970931
-47.414324	-2.291954	0.975936
-47.780993	0.919848	0.980941
-47.293914	-3.032043	0.985946
-47.406964	0.937293	0.990950
-47.519225	-3.534463	0.995955
-48.349728	-7.555153	1.000960
-49.112593	-5.258880	1.005965
-48.971534	-12.453211	1.010970
-49.696518	-5.252689	1.015974
-50.492321	-2.498834	1.020979
-49.734150	-5.692766	1.025984
-50.370179	-9.927426	1.030989
-50.494364	-9.854123	1.035994
-50.800751	-11.568281	1.040998
-50.993667	-1.673328	1.046003
-50.621135	-10.593388	1.051008
-50.713185	0.291844	1.056013
-51.247334	-10.552098	1.061018
-51.745136	-5.272784	1.066022
-51.667626	-5.933445	1.071027
-52.413549	-15.614731	1.076032
-53.118146	-9.262133	1.081037
-53.109511	-9.681045	1.086042
-53.228217	2.176480	1.091046
-53.649519	-6.742584	1.096051
-53.388028	-8.966504	1.101056
-53.897154	2.667456	1.106061
-53.759108	3.209038	1.111066
-54.312726	-5.790534	1.116070
-55.044463	-3.065701	1.121075
-54.943268	-7.336781	1.126080
-55.383393	0.375934	1.131085
-55.150647	-3.140633	1.136090
-55.149752	2.481325	1.141094
-56.051959	-8.225853	1.146099
-56.477076	-3.280633	1.151104
-56.701551	-1.691984	1.156109
-56.690545	-2.348552	1.161114
-56.924752	0.687470	1.166118
-56.965720	-3.279760	1.171123
-56.755611	1.363446	1.176128
-57.731879	-3.431676	1.181133
-58.090953	-1.641602	1.186138
-58.183095	-0.219222	1.191142
-58.339405	4.047961	1.196147
-58.320315	-9.128952	1.201152
-59.250480	3.931406	1.206157
-59.135369	-11.443560	1.211162
-59.583322	-6.719391	1.216166
-59.600488	-1.227483	1.221171
-59.600803	-7.342961	1.226176
-59.864287	-2.163638	1.231181
-60.450968	-5.279724	1.236186
-60.956675	5.129319	1.241190
-61.053910	4.299885	1.246195
-61.068181	-5.651073	1.251200
-61.302383	5.749984	1.256205
-61.188715	-2.237331	1.261210
-61.680054	-1.897690	1.266214
-62.457720	2.862325	1.271219
-62.693910	-9.214721	1.276224
-62.535506	-8.214417	1.281229
-62.773872	-1.567872	1.286234
-62.578389	-5.654408	1.291238
-63.412651	-2.457925	1.296243
-63.794262	-9.842444	1.301248
-64.224200	-2.729280	1.306253
-64.307191	-12.954207	1.311258
-64.213415	-2.395490	1.316262
-64.531086	-3.377047	1.321267
-64.623905	-7.244401	1.326272
-65.409186	-8.038792	1.331277
-65.447703	-12.610684	1.336282
-65.403566	-15.607311	1.341286
-65.940877	-15.969152	1.346291
-65.812977	-10.167781	1.351296
-66.846252	-2.102696	1.356301
-66.984530	-1.280533	1.361306
-67.022505	-6.507415	1.366310
-67.660359	-9.982480	1.371315
-67.169808	-11.539933	1.376320
-67.341110	-9.019974	1.381325
-67.514405	-14.311073	1.386330
-68.352212	-8.915209	1.391334
-68.916954	-2.875590	1.396339
-68.812701	-10.488100	1.401344
-69.325863	-8.721339	1.406349
-68.892151	-9.868086	1.411354
-68.852491	-4.983038	1.416358
-69.319865	-5.988594	1.421363
-70.046690	-9.968578	1.426368
-70.358182	-0.982033	1.431373
-70.067247	-10.230995	1.436378
-70.176672	-3.402172	1.441382
-71.020780	-0.181999	1.446387
-70.993604	-3.362633	1.451392
-71.520864	-3.846273	1.456397
-71.405217	-4.864088	1.461402
-71.710352	-0.434381	1.466406
-72.258205	-0.484520	1.471411
-72.464438	-14.749264	1.476416
-72.660381	-5.837775	1.481421
-72.762497	-2.901546	1.486426
-72.855820	2.399814	1.491430
-73.961577	-3.010936	1.496435
-74.046712	-6.148661	1.501440
-74.519207	-3.322077	1.506445
-73.973687	-8.890325	1.511450
-74.427347	-8.556587	1.516454
-74.798337	-9.469677	1.521459
-74.365426	-11.828026	1.526464
-74.853478	1.523726	1.531469
-75.693630	-10.632690	1.536474
-75.791412	-5.207246	1.541478
-75.938989	-4.434247	1.546483
-75.735082	-10.167267	1.551488
-76.152056	-1.474245	1.556493
-76.773457	-6.691967	1.561498
-77.099138	-0.620203	1.566502
-77.560541	-0.658577	1.571507
-77.303304	-2.160491	1.576512
-77.479865	-3.904482	1.581517
-77.680392	-5.119531	1.586522
-78.308234	-9.886985	1.591526
-79.156686	-0.265806	1.596531
-78.796679	-6.978749	1.601536
-79.152407	-2.794217	1.606541
-79.134301	-3.496190	1.611546
-79.168592	-3.430645	1.616550
-79.384953	1.715986	1.621555
-79.775657	-8.226606	1.626560
-80.529889	-3.859409	1.631565
-80.427477	-4.156973	1.636570
-80.421395	-6.119409	1.641574
-80.768495	8.697238	1.646579
-81.094961	-8.098677	1.651584
-81.616452	-1.619742	1.656589
-81.879259	-1.167211	1.661594
-82.021435	-0.034387	1.666598
-82.307500	0.820425	1.671603
-81.635453	-4.536694	1.676608
-82.619546	-8.444727	1.681613
-82.983817	-9.039328	1.686618
-83.255535	-12.423064	1.691622
-83.403889	-4.294157	1.696627
-83.411696	-14.942152	1.701632
-84.278150	-1.018578	1.706637
-84.784034	-4.501666	1.711642
-84.922423	-4.074958	1.716646
-84.624560	-9.420901	1.721651
-84.758390	-9.532750	1.726656
-85.358934	-2.358051	1.731661
-85.044073	-9.313858	1.736666
-85.306111	-12.749731	1.741670
-86.272976	-6.463604	1.746675
-86.344686	-6.199206	1.751680
-86.912691	-6.182911	1.756685
-86.731384	-6.416906	1.761690
-86.569157	-9.242210	1.766694
-87.135497	-1.402150	1.771699
-86.983596	-7.598426	1.776704
-87.837728	-8.204854	1.781709
-88.291425	0.633130	1.786714
-88.331790	-10.101516	1.791718
-88.769674	-1.142624	1.796723
-88.527082	-7.916262	1.801728
-88.338137	-2.839470	1.806733
-88.619797	-12.277120	1.811738
-89.439627	-7.693999	1.816742
-89.915469	-9.248724	1.821747
-89.411931	-12.659024	1.826752
-90.691669	-10.079277	1.831757
-90.976940	-0.919670	1.836762
-91.127806	-4.698833	1.841766
-91.304301	-4.620498	1.846771
-91.354354	-12.490403	1.851776
-91.495835	-3.726654	1.856781
-91.274213	-10.389438	1.861786
-91.317982	-3.805024	1.866790
-92.272525	3.849093	1.871795
-92.515778	-14.402538	1.876800
-92.769569	-7.930750	1.881805
-92.535280	0.391303	1.886810
-93.262238	-7.869252	1.891814
-93.531824	-7.766838	1.896819
-93.852410	-7.969646	1.901824
-94.019461	-10.259297	1.906829
-94.356315	-15.243188	1.911834
-94.279158	-4.077590	1.916838
-94.514981	4.852807	1.921843
-94.858994	-2.325630	1.926848
-95.460532	-1.250541	1.931853
-95.351859	-2.289410	1.936858
-95.781857	5.083195	1.941862
-95.788093	1.588255	1.946867
-96.252980	-11.765918	1.951872
-97.177227	-4.388637	1.956877
-96.866026	-4.706262	1.961882
-96.844544	1.133932	1.966886
-97.337023	8.010125	1.971891
-97.089648	0.871899	1.976896
-97.395126	0.704688	1.981901
-97.985505	-9.371129	1.986906
-98.315207	-3.336701	1.991910
-98.952448	-7.830596	1.996915
-98.757929	0.749732	2.006912
-98.547224	-1.031808	2.016909
-97.688986	1.326914	2.026906
-97.323692	-10.058366	2.036902
-97.440023	-7.369538	2.046899
-96.597775	3.357928	2.056896
-95.997457	-0.046402	2.066893
-95.714241	-5.539329	2.076890
-95.307208	-6.337925	2.086886
-94.117976	-7.518849	2.096883
-93.555103	-7.315488	2.106880
-93.327801	-8.991921	2.116877
-93.509779	-6.223114	2.126874
-92.643867	-3.922617	2.136870
-92.166435	-2.479917	2.146867
-91.310011	-8.892632	2.156864
-90.561339	-8.319238	2.166861
-90.390945	-2.475829	2.176858
-90.469343	-1.785510	2.186854
-89.707131	-2.943872	2.196851
-89.061817	-7.387964	2.206848
-87.845403	-13.679687	2.216845
-87.834354	-10.199855	2.226842
-87.736679	-4.088458	2.236838
-87.236284	-7.961807	2.246835
-86.532145	0.531806	2.256832
-86.166288	-3.348973	2.266829
-85.316308	-0.041775	2.276826
-85.001105	-1.399360	2.286822
-84.519728	2.928617	2.296819
-83.870063	3.558708	2.306816
-83.215023	-0.326203	2.316813
-83.110362	-2.170322	2.326810
-82.309908	-2.869005	2.336806
-81.825873	-2.342842	2.346803
-81.581759	-7.978530	2.356800
-80.391605	-12.124684	2.366797
-80.587595	2.535185	2.376794
-80.564706	4.454592	2.386790
-79.551783	-0.009089	2.396787
-79.029707	-1.025284	2.406784
-77.996047	-0.772145	2.416781
-77.588891	1.695274	2.426778
-77.406494	-3.772353	2.436774
-77.648338	-12.740479	2.446771
-76.277082	-0.192036	2.456768
-76.139805	-9.270254	2.466765
-75.234320	-1.124972	2.476762
-74.920172	-0.125525	2.486758
-74.665147	0.138746	2.496755
-73.481078	-1.202926	2.506752
-73.020693	-4.445944	2.516749
-73.111119	-4.412648	2.526746
-72.886676	10.843427	2.536742
-72.299128	5.204608	2.546739
-71.563820	-2.354893	2.556736
-71.108891	-0.047016	2.566733
-70.005786	-2.646301	2.576730
-69.667441	0.018802	2.586726
-69.289753	-2.546014	2.596723
-69.138500	-0.478826	2.606720
-68.479801	-1.060261	2.616717
-67.911840	3.076752	2.626714
-67.630829	0.786847	2.636710
-66.627425	1.104917	2.646707
-66.096764	-7.562935	2.656704
-66.448534	-6.117019	2.666701
-65.558382	-4.371519	2.676698
-65.039668	-3.100013	2.686694
-63.862078	-4.896836	2.696691
-63.935603	2.134718	2.706688
-63.426185	-1.404255	2.716685
-63.283634	-2.113892	2.726682
-62.574023	-6.751791	2.736678
-62.006238	-1.154382	2.746675
-60.913107	-5.611620	2.756672
-60.760144	-0.506750	2.766669
-60.653641	-5.151520	2.776666
-59.975558	-4.278789	2.786662
-59.419900	-6.842979	2.796659
-58.982171	-10.244005	2.806656
-58.153622	0.292376	2.816653
-57.730061	3.539680	2.826650
-57.910211	5.161447	2.836646
-56.848553	3.557020	2.846643
-56.582046	0.664332	2.856640
-55.567518	-0.530395	2.866637
-55.062416	-2.697021	2.876634
-54.987162	1.466509	2.886630
-55.007577	2.793981	2.896627
-53.809300	-1.378789	2.906624
-53.444149	0.357108	2.916621
-52.243887	2.972692	2.926618
-52.377559	-2.882572	2.936614
-52.040549	-2.425238	2.946611
-51.659446	5.216167	2.956608
-50.619649	-3.936945	2.966605
-50.345581	-6.681929	2.976602
-50.148672	-5.683118	2.986598
-49.237445	-1.904002	2.996595
-49.233788	-11.132347	3.006592
-48.275399	-10.379565	3.016589
-47.599181	-9.984883	3.026586
-47.540741	-7.846132	3.036582
-46.622017	-4.860148	3.046579
-46.159200	-4.679120	3.056576
-46.278495	-10.729873	3.066573
-45.401447	-12.878748	3.076570
-44.707085	-6.220941	3.086566
-44.553689	-6.469773	3.096563
-43.639596	-8.371027	3.106560
-43.293769	-5.754613	3.116557
-43.023577	-7.387080	3.126554
-42.154305	-6.845250	3.136550
-41.845071	-4.501871	3.146547
-41.333870	-8.700030	3.156544
-40.399680	-11.453411	3.166541
-40.192511	-7.326391	3.176538
-40.165707	-3.129927	3.186534
-39.647539	-7.291165	3.196531
-38.972708	-8.359804	3.206528
-38.353422	-5.738719	3.216525
-37.518414	-7.082714	3.226522
-37.424083	-2.608558	3.236518
-37.021066	-7.375816	3.246515
-36.286527	-4.753783	3.256512
-35.917967	-11.704612	3.266509
-35.610096	-10.913257	3.276506
-34.844007	-2.426176	3.286502
-34.173619	-11.974402	3.296499
-33.300966	-4.581082	3.306496
-33.367274	-9.857683	3.316493
-33.242859	-11.413456	3.326490
-32.220795	-10.252494	3.336486
-32.030021	-9.835603	3.346483
-31.336624	-5.233564	3.356480
-30.068433	-9.740403	3.366477
-30.661665	-10.347423	3.376474
-30.200088	-6.966691	3.386470
-28.951639	-4.197096	3.396467
-28.270664	-16.835614	3.406464
-28.123302	-9.930539	3.416461
-28.372486	-7.135363	3.426458
-27.366194	-4.669951	3.436454
-26.638977	-10.961047	3.446451
-26.491555	-12.552103	3.456448
-25.648440	-12.823472	3.466445
-25.295738	-9.070883	3.476442
-25.099753	-8.749843	3.486438
-24.269039	-9.557800	3.496435
-23.966115	-10.004291	3.506432
-23.115461	-12.012813	3.516429
-22.631664	-9.639764	3.526426
-22.583415	-9.875288	3.536422
-21.850030	-3.334465	3.546419
-21.239080	-3.696171	3.556416
-20.798717	-8.111315	3.566413
-20.059387	-5.068709	3.576410
-19.731280	-1.302761	3.586406
-19.597970	-6.883075	3.596403
-19.086994	-8.794024	3.606400
-18.197836	-3.338832	3.616397
-17.585909	-8.639340	3.626394
-16.868831	-2.960779	3.636390
-16.682387	-8.676130	3.646387
-16.672832	-3.060942	3.656384
-15.997040	-7.826590	3.666381
-15.301986	-5.565837	3.676378
-14.888458	2.251057	3.686374
-14.101518	-3.944860	3.696371
-13.856599	-4.363256	3.706368
-13.276822	-10.004020	3.716365
-12.696020	-9.955518	3.726362
-12.199036	-6.406101	3.736358
-11.714555	-9.858800	3.746355
-11.071016	-6.373528	3.756352
-10.802086	-10.118741	3.766349
-10.645034	-5.378810	3.776346
-9.445874	-10.128257	3.786342
-9.340379	-8.190115	3.796339
-8.795443	-7.283847	3.806336
-7.979231	-6.448594	3.816333
-7.676257	-11.456770	3.826330
-7.668880	-8.359667	3.836326
-6.734833	-6.640045	3.846323
-6.476871	-5.625455	3.856320
-5.413079	-9.650434	3.866317
-4.865338	-7.458465	3.876314
-5.048646	-4.344156	3.886310
-4.704427	-7.828732	3.896307
-3.836034	-2.177046	3.906304
-3.381773	3.501516	3.916301
-2.698525	10.129399	3.926298
-3.010441	16.932216	3.936294
-2.365347	29.828897	3.946291
-1.895637	46.082469	3.956288
-1.509997	59.672399	3.966285
-1.001956	97.242782	3.976282
-0.526428	110.676114	3.986278
0.000000	125.715757	3.991283
0.389680	141.059332	3.996288
0.517188	150.951625	4.001293
0.354431	143.988333	4.006298
0.595346	154.520931	4.011302
0.766028	160.464358	4.016307
0.981594	172.557533	4.021312
1.154245	179.927538	4.026317
1.143324	177.211593	4.031322
1.243691	176.800450	4.036326
1.388688	179.397429	4.041331
1.014882	166.228155	4.046336
1.045977	156.943885	4.051341
0.642970	155.830152	4.056346
0.915212	167.439872	4.061350
0.942216	181.786758	4.066355
1.019003	184.761428	4.071360
1.275315	175.445025	4.076365
1.033936	181.525789	4.081370
1.015200	177.488594	4.086374
1.328066	176.946078	4.091379
0.955804	175.710465	4.096384
1.564860	167.730874	4.101389
1.172727	192.289789	4.106394
1.377211	180.842763	4.111398
1.168852	185.472492	4.116403
1.199888	184.673572	4.121408
1.490088	183.542973	4.126413
1.161521	185.255517	4.131418
1.232543	178.730154	4.136422
1.649886	184.672908	4.141427
1.550626	176.671414	4.146432
1.459794	180.352566	4.151437
1.254752	186.503570	4.156442
1.503301	186.274858	4.161446
1.595199	190.142521	4.166451
1.439280	181.517139	4.171456
1.268577	178.212449	4.176461
1.454002	186.858636	4.181466
1.520060	177.600515	4.186470
1.651659	185.321810	4.191475
1.402438	187.344630	4.196480
1.542991	189.603779	4.201485
1.271103	188.036057	4.206490
1.442857	187.332149	4.211494
1.433830	198.422800	4.216499
1.769618	197.098393	4.221504
1.934323	184.528115	4.226509
1.355663	195.252427	4.231514
1.782837	186.038963	4.236518
1.458556	189.263139	4.241523
1.275947	185.738846	4.246528
1.268967	193.165475	4.251533
1.390125	193.013671	4.256538
1.134002	186.096630	4.261542
1.378268	189.500649	4.266547
1.155402	194.819201	4.271552
1.454859	181.826007	4.276557
1.235445	191.399349	4.281562
1.600910	199.172594	4.286566
1.682826	221.284410	4.291571
1.610364	219.555721	4.296576
1.717553	215.584210	4.301581
1.807739	214.076816	4.306586
1.808453	211.909547	4.311590
1.747086	215.671513	4.316595
1.562415	217.342530	4.321600
1.887487	213.846256	4.326605
1.990998	218.734020	4.331610
1.993073	208.910092	4.336614
1.930239	217.750219	4.341619
1.849076	223.122510	4.346624
1.994859	211.703645	4.351629
1.747632	222.398189	4.356634
2.023618	216.865777	4.361638
2.052460	212.517392	4.366643
2.180053	202.072676	4.371648
1.989547	186.229716	4.376653
1.609028	192.063360	4.381658
1.234508	199.636166	4.386662
1.754557	215.389659	4.391667
1.644215	216.248583	4.396672
1.524564	212.765041	4.401677
1.701074	218.641134	4.406682
1.661690	217.919686	4.411686
1.697490	222.400435	4.416691
1.669801	230.260605	4.421696
2.039043	236.274188	4.426701
1.573749	240.637298	4.431706
2.221182	232.942738	4.436710
2.212179	239.910949	4.441715
2.105765	238.491306	4.446720
2.161234	242.687398	4.451725
2.034297	245.406090	4.456730
2.060118	237.872200	4.461734
2.187007	246.859789	4.466739
2.241024	242.159432	4.471744
2.385191	248.347493	4.476749
2.109900	252.513153	4.481754
2.302968	241.153301	4.486758
2.093050	248.469378	4.491763
2.276230	244.226520	4.496768
2.005830	241.399357	4.501773
2.157605	244.602738	4.506778
2.725851	245.722345	4.511782
2.423152	238.182980	4.516787
2.515553	246.837444	4.521792
2.402267	226.758641	4.526797
2.212178	230.252870	4.531802
2.127081	230.617447	4.536806
2.377205	241.404924	4.541811
2.277459	248.324080	4.546816
2.071931	250.722885	4.551821
2.065826	252.967054	4.556826
2.068012	246.781490	4.561830
2.095654	248.052241	4.566835
2.336066	247.793165	4.571840
2.288838	237.008816	4.576845
2.187723	246.019474	4.581850
2.347214	249.243794	4.586854
2.449694	247.395941	4.591859
2.281454	246.887674	4.596864
2.414156	235.236721	4.601869
1.968413	245.345437	4.606874
2.288420	258.849193	4.611878
2.388674	271.324343	4.616883
2.306708	273.580401	4.621888
2.439121	279.675401	4.626893
2.376165	283.608476	4.631898
2.359988	268.016547	4.636902
2.511251	270.957415	4.641907
2.546496	275.261090	4.646912
2.669737	270.945358	4.651917
2.414083	270.811463	4.656922
2.824553	270.763029	4.661926
2.801840	276.395102	4.666931
2.763174	270.374123	4.671936
2.722085	264.907195	4.676941
2.505072	278.045843	4.681946
2.357387	276.983848	4.686950
2.456417	277.743530	4.691955
2.835312	272.394298	4.696960
3.026316	274.177306	4.701965
2.518722	274.086050	4.706970
2.666970	271.256564	4.711974
2.520404	273.105118	4.716979
2.412198	278.918271	4.721984
2.637718	273.466516	4.726989
2.479926	286.396570	4.731994
2.947960	282.801951	4.736998
2.632777	295.079612	4.742003
2.990661	302.354204	4.747008
2.961362	295.195931	4.752013
2.952396	296.080105	4.757018
3.004031	288.203619	4.762022
2.907122	285.153108	4.767027
2.900196	294.405303	4.772032
3.441884	281.051373	4.777037
2.891902	281.833648	4.782042
2.817453	273.562462	4.787046
2.714183	275.938920	4.792051
2.882461	277.896336	4.797056
2.737488	281.067123	4.802061
3.008923	296.226874	4.807066
2.769328	297.020631	4.812070
2.724075	299.881560	4.817075
2.503209	302.054979	4.822080
3.067985	298.315482	4.827085
2.864653	303.403209	4.832090
3.103710	300.062769	4.837094
3.408861	298.002817	4.842099
2.767334	303.557846	4.847104
2.943032	290.675715	4.852109
2.998161	297.054919	4.857114
3.114877	307.505824	4.862118
2.712050	304.307084	4.867123
2.639810	307.067837	4.872128
2.957848	313.782350	4.877133
3.415986	330.412536	4.882138
3.068718	333.469492	4.887142
3.003181	328.189878	4.892147
3.302476	337.413099	4.897152
3.260515	326.393747	4.902157
3.471522	331.732947	4.907162
3.383838	331.047536	4.912166
3.297536	334.680553	4.917171
2.976439	326.166405	4.922176
3.453468	330.764715	4.927181
3.090683	334.814385	4.932186
3.093153	334.285696	4.937190
3.140488	330.288736	4.942195
3.004645	332.793695	4.947200
3.228990	328.620300	4.952205
3.050541	344.024591	4.957210
2.898140	332.652369	4.962214
3.098339	334.712361	4.967219
3.205607	333.376292	4.972224
3.718366	346.552512	4.977229
3.223809	346.563619	4.982234
3.838945	342.746618	4.987238
3.636919	338.997540	4.992243
3.756217	324.972582	4.997248
3.790438	329.608634	5.002253
3.372236	331.835122	5.007258
3.288136	329.133783	5.012262
3.450009	332.958875	5.017267
3.318768	332.482775	5.022272
3.397215	320.549193	5.027277
3.186752	331.529116	5.032282
3.440063	336.374458	5.037286
3.562751	346.470100	5.042291
3.361990	358.429310	5.047296
3.809178	352.329015	5.052301
3.909558	359.188383	5.057306
3.890193	363.060861	5.062310
3.763143	346.476967	5.067315
3.223888	347.475869	5.072320
3.451813	349.876377	5.077325
3.384726	368.939630	5.082330
3.638743	347.480653	5.087334
3.741734	359.847865	5.092339
3.551552	354.942124	5.097344
3.984535	362.660568	5.102349
3.472438	359.981990	5.107354
3.386756	357.654229	5.112358
3.905187	358.629784	5.117363
3.884329	358.193337	5.122368
4.062344	361.278730	5.127373
4.051598	361.859457	5.132378
3.666794	364.884333	5.137382
3.664649	356.418276	5.142387
3.585250	356.759817	5.147392
4.081411	355.925978	5.152397
3.824271	362.407917	5.157402
3.932684	357.066238	5.162406
3.662518	355.052128	5.167411
4.080892	359.802009	5.172416
4.221664	360.982274	5.177421
3.843416	365.913923	5.182426
4.032884	356.392757	5.187430
3.942816	362.193603	5.192435
3.892504	357.791144	5.197440
3.977605	362.162961	5.202445
3.793916	365.728982	5.207450
3.658112	363.219243	5.212454
3.748170	367.118871	5.217459
3.747869	362.047331	5.222464
3.448186	361.989939	5.227469
3.853504	370.747299	5.232474
4.025854	373.789287	5.237478
3.762666	387.216832	5.242483
3.875204	395.083578	5.247488
4.610252	390.276476	5.252493
4.451527	393.911360	5.257498
4.453641	386.583609	5.262502
4.163756	372.078544	5.267507
3.995854	365.096988	5.272512
3.805425	373.773681	5.277517
4.214927	385.324071	5.282522
4.093773	385.915771	5.287526
4.123470	401.100831	5.292531
4.032392	395.401243	5.297536
3.893748	397.713655	5.302541
4.169454	394.250392	5.307546
4.343324	395.327394	5.312550
4.314046	387.267383	5.317555
4.288937	395.975133	5.322560
4.182158	398.931142	5.327565
4.052291	393.345203	5.332570
4.260446	394.087793	5.337574
4.348601	400.294175	5.342579
4.173737	388.783063	5.347584
4.363470	388.389552	5.352589
4.056104	400.906513	5.357594
3.929152	394.639888	5.362598
4.257035	390.896359	5.367603
4.154789	411.180084	5.372608
4.956758	408.795497	5.377613
4.356958	407.706253	5.382618
4.582278	394.721357	5.387622
4.490836	391.464321	5.392627
4.496160	397.459047	5.397632
4.246991	386.282292	5.402637
4.060310	391.753426	5.407642
4.234104	414.224419	5.412646
4.653414	417.319473	5.417651
4.722402	417.868726	5.422656
4.570150	419.284738	5.427661
4.317982	421.830082	5.432666
4.473724	425.687793	5.437670
5.033086	417.981643	5.442675
4.555706	420.109843	5.447680
4.796742	419.037555	5.452685
4.894536	424.204690	5.457690
4.158258	411.319826	5.462694
4.752668	409.692282	5.467699
4.629440	419.367738	5.472704
5.088028	399.699027	5.477709
4.667253	408.139736	5.482714
4.692782	411.704625	5.487718
4.733737	406.949321	5.492723
4.987096	404.407076	5.497728
4.534005	394.008937	5.502733
4.366663	403.289486	5.507738
4.520528	413.475197	5.512742
4.753296	408.338652	5.517747
5.083699	416.294661	5.522752
4.859412	416.079918	5.527757
4.594276	432.541941	5.532762
4.626628	418.600138	5.537766
4.581193	425.472887	5.542771
4.483758	425.833073	5.547776
4.676345	424.240012	5.552781
4.799289	436.398501	5.557786
4.543256	428.864398	5.562790
4.827928	419.486475	5.567795
4.847394	424.662719	5.572800
4.899158	417.387289	5.577805
4.787174	420.024568	5.582810
5.041762	421.462259	5.587814
4.817992	418.925164	5.592819
4.944198	423.701857	5.597824
4.932673	417.689230	5.602829
4.892549	422.950743	5.607834
4.917851	427.613529	5.612838
5.071054	436.549633	5.617843
5.175531	433.072061	5.622848
4.818835	426.869896	5.627853
4.833300	431.104096	5.632858
5.376823	427.611520	5.637862
5.235718	444.069939	5.642867
4.864584	434.984592	5.647872
5.213353	437.967312	5.652877
5.180545	445.980243	5.657882
4.835272	438.817635	5.662886
5.183907	451.510266	5.667891
5.184865	452.288486	5.672896
5.595670	438.277880	5.677901
4.996602	434.647940	5.682906
5.156455	436.720592	5.687910
5.458991	437.325005	5.692915
5.074574	440.213787	5.697920
4.985554	433.830470	5.702925
5.656435	448.573413	5.707930
5.867766	441.465967	5.712934
5.753779	424.288312	5.717939
5.407188	432.850292	5.722944
5.555891	422.462253	5.727949
5.314934	427.903935	5.732954
5.279066	425.084290	5.737958
5.606255	422.302676	5.742963
5.242453	424.087203	5.747968
5.206622	419.261667	5.752973
5.325100	431.556898	5.757978
5.217109	426.207974	5.762982
5.653966	418.030620	5.767987
5.537506	424.683535	5.772992
5.574684	426.623543	5.777997
5.295399	424.389384	5.783002
5.545468	430.788713	5.788006
5.822186	422.946506	5.793011
5.626280	430.984986	5.798016
5.749908	420.534436	5.803021
5.573521	423.226100	5.808026
5.243181	423.534191	5.813030
5.354294	421.162931	5.818035
5.039644	420.133416	5.823040
4.947010	414.111352	5.828045
5.293961	427.383216	5.833050
5.688542	422.645270	5.838054
5.688411	424.958131	5.843059
5.295909	426.848398	5.848064
5.648758	416.950413	5.853069
5.405384	421.003539	5.858074
5.461164	422.434414	5.863078
5.752497	424.628838	5.868083
5.612037	425.634866	5.873088
5.644801	421.383895	5.878093
5.554171	431.095380	5.883098
5.534778	438.669593	5.888102
5.913531	438.123075	5.893107
5.854208	442.084091	5.898112
6.008019	444.012154	5.903117
5.446423	434.317550	5.908122
5.680092	430.386287	5.913126
5.973706	437.677333	5.918131
5.663431	437.767137	5.923136
5.774831	442.761298	5.928141
5.568607	442.037506	5.933146
5.885754	439.814302	5.938150
5.906275	440.950137	5.943155
5.703234	440.298615	5.948160
6.076663	429.799429	5.953165
5.784920	441.535661	5.958170
5.784393	438.631380	5.963174
5.730215	443.034530	5.968179
5.698478	449.547626	5.973184
5.690699	439.044885	5.978189
5.999419	438.654877	5.983194
5.555784	445.602680	5.988198
6.128009	448.869940	5.993203
5.492101	445.530517	5.998208
5.436716	445.694284	6.003213
5.488232	448.998835	6.008218
5.796726	457.214569	6.013222
5.952896	464.081055	6.018227
5.978947	473.040264	6.023232
5.892824	466.871624	6.028237
5.979391	475.394231	6.033242
6.077478	478.688327	6.038246
6.056394	470.547898	6.043251
5.892875	470.677985	6.048256
6.032333	475.348208	6.053261
6.101549	470.506199	6.058266
5.893764	461.746435	6.063270
5.528564	457.529335	6.068275
5.697017	475.878729	6.073280
6.272717	470.694762	6.078285
6.055078	470.270162	6.083290
6.185214	462.254745	6.088294
6.315093	468.701395	6.093299
5.961008	458.774940	6.098304
6.031862	454.090873	6.103309
5.847115	450.111265	6.108314
5.656174	448.220777	6.113318
5.536669	453.023321	6.118323
5.605708	469.350758	6.123328
5.792450	471.938076	6.128333
5.795969	472.744370	6.133338
5.754408	477.876405	6.138342
6.083010	472.484372	6.143347
5.741967	473.597763	6.148352
5.851257	469.935925	6.153357
5.969261	472.451752	6.158362
6.184119	472.022664	6.163366
5.975159	466.471242	6.168371
6.208564	472.512517	6.173376
6.233548	471.372834	6.178381
6.090660	477.878044	6.183386
6.136933	479.440132	6.188390
6.298834	467.335184	6.193395
5.944001	464.698390	6.198400
6.077872	461.444005	6.203405
5.870347	456.670671	6.208410
5.710120	455.151871	6.213414
5.616187	462.456190	6.218419
5.783648	471.203409	6.223424
6.253141	469.858034	6.228429
6.084285	473.149660	6.233434
6.329501	477.240145	6.238438
6.175270	466.304738	6.243443
5.855789	454.550478	6.248448
5.825293	440.343250	6.253453
5.716986	450.215707	6.258458
5.711862	467.019849	6.263462
5.868478	463.553085	6.268467
5.994536	473.777990	6.273472
6.462806	469.300579	6.278477
6.024902	462.424567	6.283482
5.785280	462.405222	6.288486
6.049261	456.861961	6.293491
5.801053	466.503238	6.298496
6.141321	461.384637	6.303501
5.472245	463.653612	6.308506
5.855720	467.823676	6.313510
5.796199	467.674868	6.318515
5.780181	471.075429	6.323520
6.297089	469.102507	6.328525
6.336203	475.110948	6.333530
6.372714	462.721918	6.338534
6.054318	459.310597	6.343539
5.908981	456.122107	6.348544
6.039683	448.691922	6.353549
6.229337	448.459779	6.358554
5.944276	455.629521	6.363558
6.072385	449.737380	6.368563
5.696915	460.692613	6.373568
5.619106	442.832205	6.378573
6.052790	450.443006	6.383578
5.620442	451.770024	6.388582
5.705084	455.559785	6.393587
5.913041	467.432883	6.398592
6.304898	456.557458	6.403597
5.913615	459.871276	6.408602
6.129480	462.150298	6.413606
5.971684	452.765752	6.418611
5.821910	453.301824	6.423616
6.189086	454.234643	6.428621
5.813004	452.037794	6.433626
5.897356	451.043840	6.438630
5.973042	448.282645	6.443635
5.682283	446.464747	6.448640
6.000844	457.292253	6.453645
6.052931	471.258942	6.458650
5.671855	478.193792	6.463654
6.158058	476.257318	6.468659
5.902737	483.387609	6.473664
6.156812	472.549582	6.478669
5.695624	469.113174	6.483674
6.024647	474.465565	6.488678
5.635838	473.260997	6.493683
5.944888	475.000219	6.498688
5.842469	477.604369	6.503693
6.150875	482.991631	6.508698
5.981137	471.096836	6.513702
6.443378	475.887333	6.518707
6.015101	463.276887	6.523712
5.821879	456.720056	6.528717
6.083830	461.244528	6.533722
5.922001	456.922795	6.538726
6.281680	455.898357	6.543731
5.997606	460.666575	6.548736
6.193942	450.932304	6.553741
6.127835	459.450349	6.558746
5.684697	458.966164	6.563750
5.837927	454.974731	6.568755
5.845555	453.356862	6.573760
5.865130	452.952044	6.578765
6.145615	459.033396	6.583770
5.799008	455.395534	6.588774
5.993606	452.356270	6.593779
5.931825	458.874077	6.598784
5.864987	442.672978	6.603789
5.900761	454.718583	6.608794
5.598910	461.565080	6.613798
6.007532	465.870413	6.618803
5.735742	476.970769	6.623808
6.171975	480.987031	6.628813
5.892009	473.032701	6.633818
6.004172	482.721931	6.638822
6.281393	465.505089	6.643827
5.775392	458.133529	6.648832
6.044023	459.812641	6.653837
5.995635	459.715875	6.658842
5.644140	449.545403	6.663846
6.084780	472.430256	6.668851
5.884643	467.257115	6.673856
6.040147	463.869621	6.678861
5.993984	464.256578	6.683866
6.034681	449.718637	6.688870
6.336490	447.485180	6.693875
6.001454	452.679010	6.698880
5.879218	443.415451	6.703885
5.997301	448.990716	6.708890
5.956024	456.774018	6.713894
5.725235	445.955026	6.718899
5.730059	460.675784	6.723904
6.191263	454.661845	6.728909
5.956156	448.187513	6.733914
5.603452	447.303168	6.738918
6.036058	446.770359	6.743923
6.095424	451.329734	6.748928
5.872136	448.469845	6.753933
6.224398	448.117309	6.758938
5.891095	452.418658	6.763942
5.938434	441.119479	6.768947
5.613828	452.275552	6.773952
6.058362	459.432225	6.778957
5.853200	459.802963	6.783962
5.775732	460.786467	6.788966
6.205578	473.501193	6.793971
5.694718	468.765891	6.798976
6.108439	475.104793	6.803981
6.143063	477.646341	6.808986
6.060553	464.681151	6.813990
6.213619	446.211906	6.818995
5.828031	461.525363	6.824000
6.282020	446.552497	6.829005
6.074227	451.542886	6.834010
5.964338	456.426184	6.839014
6.101768	455.066397	6.844019
5.854443	452.855702	6.849024
5.789744	451.692106	6.854029
5.880515	447.087180	6.859034
5.967260	452.034584	6.864038
6.120004	443.221503	6.869043
6.085500	452.908386	6.874048
6.038855	454.905824	6.879053
5.949316	452.562835	6.884058
5.881220	454.329508	6.889062
6.117584	448.872838	6.894067
6.072232	457.080735	6.899072
6.080163	458.718434	6.904077
6.201086	454.966188	6.909082
6.004691	458.189358	6.914086
5.884503	452.769568	6.919091
5.961734	453.570640	6.924096
5.906177	450.001076	6.929101
5.919368	452.922478	6.934106
5.967373	455.740346	6.939110
6.234492	454.436171	6.944115
5.777524	455.646820	6.949120
5.928447	441.034666	6.954125
6.247690	454.361514	6.959130
6.107394	459.116695	6.964134
6.135562	447.532604	6.969139
5.932676	456.657393	6.974144
5.905551	452.229131	6.979149
6.193650	454.885989	6.984154
5.816929	463.623553	6.989158
6.013522	463.459928	6.994163
5.940946	454.875141	6.999168
5.984291	457.570348	7.004173
5.921509	465.018490	7.009178
5.954239	459.546264	7.014182
5.827822	455.212655	7.019187
5.946357	460.098131	7.024192
5.928099	451.669356	7.029197
5.759732	455.058982	7.034202
5.503310	451.302583	7.039206
5.904320	448.727705	7.044211
5.742168	459.643187	7.049216
5.730186	450.251615	7.054221
5.702522	450.765391	7.059226
5.214089	456.328117	7.064230
5.528670	458.376529	7.069235
5.710390	475.727228	7.074240
5.642879	479.543998	7.079245
6.067625	479.496490	7.084250
5.974987	492.150719	7.089254
6.343294	476.659723	7.094259
6.438027	483.013805	7.099264
6.300876	475.900833	7.104269
6.144580	461.583579	7.109274
6.072214	456.010758	7.114278
6.135535	457.380341	7.119283
5.937836	456.560297	7.124288
6.071459	443.070860	7.129293
6.071498	455.128391	7.134298
5.966215	454.018612	7.139302
5.946048	444.473296	7.144307
5.886962	456.546420	7.149312
5.656871	454.203306	7.154317
6.280392	455.089633	7.159322
5.806134	450.968718	7.164326
6.043030	448.093676	7.169331
6.002380	456.553946	7.174336
6.290436	446.849600	7.179341
6.030202	446.425347	7.184346
6.108279	457.122847	7.189350
5.993902	445.016908	7.194355
6.015224	454.207810	7.199360
5.467478	452.648483	7.204365
5.600575	448.796252	7.209370
5.632221	450.642212	7.214374
5.932390	450.829367	7.219379
5.795066	457.580479	7.224384
5.610050	452.639099	7.229389
5.794885	460.542003	7.234394
5.811731	470.742888	7.239398
5.921218	467.330965	7.244403
6.154831	474.242271	7.249408
6.150446	471.329097	7.254413
6.158259	460.327175	7.259418
5.701190	455.089886	7.264422
5.910149	464.956936	7.269427
5.801426	478.452099	7.274432
6.105617	481.970176	7.279437
6.246400	478.626117	7.284442
6.258402	466.971777	7.289446
5.624673	459.487348	7.294451
5.623264	456.845802	7.299456
5.609800	469.516085	7.304461
5.896425	472.758492	7.309466
6.007442	475.942991	7.314470
6.137461	484.898571	7.319475
5.964430	473.795256	7.324480
5.865163	474.171550	7.329485
5.837866	479.317171	7.334490
5.624866	482.489160	7.339494
5.691823	479.805261	7.344499
5.559255	479.405297	7.349504
6.107993	478.360728	7.354509
5.649540	476.964585	7.359514
5.909630	476.196204	7.364518
6.197422	480.969741	7.369523
5.759989	483.667513	7.374528
5.780081	477.292396	7.379533
6.391060	479.015950	7.384538
6.111635	476.629940	7.389542
5.960221	469.503386	7.394547
5.684283	481.389033	7.399552
5.917926	475.793571	7.404557
5.757847	480.200668	7.409562
5.768513	477.443328	7.414566
5.786798	472.536530	7.419571
5.698793	487.297164	7.424576
5.931929	480.999401	7.429581
6.098635	475.591603	7.434586
6.149111	482.265842	7.439590
5.715526	480.270994	7.444595
5.952953	476.978234	7.449600
5.978174	471.288874	7.454605
5.810676	469.935733	7.459610
5.888982	477.171941	7.464614
5.869963	483.569157	7.469619
5.799632	487.446483	7.474624
6.244548	486.971858	7.479629
6.149396	473.325246	7.484634
5.894961	479.971325	7.489638
6.395629	473.568370	7.494643
6.052818	480.149199	7.499648
6.117323	473.786107	7.504653
6.085216	475.031433	7.509658
6.049133	480.795385	7.514662
5.942628	475.262709	7.519667
5.896862	481.078799	7.524672
5.927556	474.100887	7.529677
6.047307	481.919083	7.534682
6.028971	480.083808	7.539686
5.896042	469.891735	7.544691
5.650935	480.842374	7.549696
5.842994	476.443041	7.554701
6.153310	482.731706	7.559706
5.859557	482.179821	7.564710
6.242464	472.897214	7.569715
5.870064	481.146873	7.574720
5.995448	490.144313	7.579725
5.824651	489.380166	7.584730
5.900705	485.669747	7.589734
6.078315	483.775296	7.594739
5.722218	486.457160	7.599744
6.041025	484.347591	7.604749
6.126511	479.366984	7.609754
5.546425	480.473534	7.614758
5.714799	479.453758	7.619763
5.427944	493.862726	7.624768
5.730397	483.472710	7.629773
5.895590	486.455725	7.634778
5.752303	503.417596	7.639782
6.179650	506.106430	7.644787
6.085442	510.528525	7.649792
6.195036	503.468634	7.654797
6.340101	494.349836	7.659802
5.701883	497.129691	7.664806
5.830381	489.386612	7.669811
5.830202	489.003871	7.674816
5.915436	488.177462	7.679821
6.146743	487.897662	7.684826
5.861425	484.639348	7.689830
6.231066	485.362967	7.694835
6.005848	484.003048	7.699840
5.923297	480.345955	7.704845
6.254137	478.418005	7.709850
6.034859	479.341469	7.714854
6.085604	474.103706	7.719859
5.900382	478.157225	7.724864
6.180714	476.604197	7.729869
6.117874	480.733458	7.734874
5.819032	491.433086	7.739878
5.798163	478.141841	7.744883
5.832458	477.693586	7.749888
5.799766	475.174002	7.754893
5.892519	482.699025	7.759898
5.604079	487.401492	7.764902
5.740107	472.535373	7.769907
5.683403	483.491297	7.774912
6.231894	500.107485	7.779917
5.974651	495.417864	7.784922
6.036334	495.772104	7.789926
5.918267	480.746467	7.794931
6.029614	493.571223	7.799936
5.895775	491.848961	7.804941
5.881772	478.344661	7.809946
5.858999	493.753164	7.814950
6.065024	495.970455	7.819955
5.868827	496.653013	7.824960
5.943112	496.695219	7.829965
6.364938	494.977646	7.834970
6.127430	491.373305	7.839974
6.105147	484.128433	7.844979
5.967353	484.953705	7.849984
6.202301	479.323234	7.854989
6.401995	480.684107	7.859994
5.592475	492.390763	7.864998
6.103328	481.066393	7.870003
5.947200	476.285000	7.875008
6.282275	482.196450	7.880013
6.042446	478.298235	7.885018
5.687422	482.482768	7.890022
6.047551	480.986842	7.895027
6.142162	489.302544	7.900032
6.198461	481.969427	7.905037
6.417913	475.787708	7.910042
6.026995	483.736539	7.915046
6.194943	480.350257	7.920051
6.263296	477.450996	7.925056
5.742231	467.591830	7.930061
5.997188	451.125162	7.935066
5.621592	455.898227	7.940070
5.975014	465.454730	7.945075
6.104983	477.729209	7.950080
6.199473	480.707483	7.955085
5.957247	472.592210	7.960090
5.607077	460.630776	7.965094
5.657963	473.566235	7.970099
6.088411	477.349277	7.975104
5.913201	484.552440	7.980109
5.967630	489.758028	7.985114
5.776064	485.899708	7.990118
5.883935	477.448503	7.995136
5.419019	480.623555	8.000154
5.701216	480.554153	8.005171
6.127033	479.625963	8.010189
6.023435	492.170770	8.015206
6.170096	485.353418	8.020224
6.090501	488.417605	8.025242
6.020760	482.691353	8.030259
6.190403	485.773293	8.035277
6.133487	489.499800	8.040294
5.976593	483.209692	8.045312
5.956251	483.777827	8.050330
5.798687	487.176121	8.055347
5.814171	483.298436	8.060365
6.007201	488.835078	8.065382
6.030694	486.278417	8.070400
5.769995	490.257760	8.075418
5.747434	487.986024	8.080435
5.969388	483.618398	8.085453
5.687918	488.257400	8.090470
6.075331	484.087911	8.095488
5.907266	487.727692	8.100506
5.667852	483.381861	8.105523
6.190492	475.233818	8.110541
5.966301	493.096102	8.115558
6.239264	506.358245	8.120576
6.061129	501.242261	8.125594
6.027660	499.382487	8.130611
6.229886	504.292845	8.135629
6.143388	496.764096	8.140646
6.103164	487.224168	8.145664
6.055243	481.093711	8.150682
5.862892	488.142401	8.155699
6.318819	496.556968	8.160717
6.169113	503.075120	8.165734
5.972963	508.732706	8.170752
6.062680	515.633071	8.175770
6.129631	502.355652	8.180787
6.216768	501.360605	8.185805
6.137870	510.524850	8.190822
6.720867	498.529884	8.195840
5.944707	486.571158	8.200858
5.976862	489.592589	8.205875
6.522712	497.526009	8.210893
6.091097	500.661133	8.215910
6.281637	480.569929	8.220928
6.122034	489.544837	8.225946
6.046789	485.195374	8.230963
6.079057	486.490567	8.235981
6.054863	507.603559	8.240998
6.270677	509.097213	8.246016
6.319888	508.183847	8.251034
6.267506	516.968400	8.256051
6.432905	503.924863	8.261069
6.091992	503.735341	8.266086
6.202099	506.242790	8.271104
6.450033	505.351936	8.276122
5.974699	506.887608	8.281139
6.012691	506.367320	8.286157
6.132925	510.880272	8.291174
6.464827	514.138765	8.296192
6.279294	509.478373	8.301210
6.543856	508.935209	8.306227
6.372822	499.033918	8.311245
6.163862	513.188927	8.316262
6.342302	514.514868	8.321280
6.584694	505.445045	8.326298
5.927130	500.940665	8.331315
6.318977	505.669835	8.336333
6.251462	512.828363	8.341350
6.331627	509.723177	8.346368
6.400813	510.384583	8.351386
6.268651	519.699188	8.356403
6.662682	510.214284	8.361421
6.455149	512.951383	8.366438
6.188597	494.604357	8.371456
6.216876	498.954989	8.376474
6.001681	501.608080	8.381491
6.499404	501.773153	8.386509
6.340727	511.035104	8.391526
6.797306	508.943913	8.396544
6.446433	510.052986	8.401562
6.481915	503.423460	8.406579
6.251577	486.916912	8.411597
6.299322	496.856567	8.416614
6.369363	503.513858	8.421632
6.100188	505.607364	8.426650
6.245553	512.726226	8.431667
6.077076	503.705001	8.436685
6.334898	509.793231	8.441702
6.070597	510.913986	8.446720
6.493392	511.109733	8.451738
6.164383	515.794060	8.456755
6.365278	513.733463	8.461773
6.513733	513.388370	8.466790
6.376176	515.300309	8.471808
6.299425	520.595208	8.476826
6.365985	520.515412	8.481843
6.570781	517.718900	8.486861
6.647236	514.970900	8.491878
6.239727	518.910135	8.496896
6.422820	511.358074	8.501914
6.260571	511.926354	8.506931
6.377228	509.039512	8.511949
6.283147	514.321346	8.516966
6.084586	525.871199	8.521984
6.717701	527.722349	8.527002
6.271756	538.114921	8.532019
6.601325	534.266908	8.537037
6.409831	531.469370	8.542054
6.526735	541.357189	8.547072
6.545239	536.365019	8.552090
6.712169	542.947184	8.557107
6.873351	541.549213	8.562125
6.383515	537.624458	8.567143
6.402592	542.828610	8.572160
6.564279	535.283050	8.577178
5.941208	539.060404	8.582195
6.177744	530.572154	8.587213
6.657934	537.979393	8.592231
6.455170	542.094836	8.597248
6.839631	539.765633	8.602266
6.913677	543.121337	8.607283
6.616180	541.713183	8.612301
6.239851	542.150903	8.617319
6.302829	548.165533	8.622336
6.625610	540.130825	8.627354
6.557538	541.981387	8.632371
6.685563	539.474611	8.637389
6.555735	547.545478	8.642407
6.211076	546.072129	8.647424
6.541190	547.128154	8.652442
6.801047	563.059051	8.657459
6.721088	557.649957	8.662477
6.521122	541.615126	8.667495
6.439939	556.845215	8.672512
6.640442	558.994524	8.677530
6.677377	562.943028	8.682547
7.159994	561.216981	8.687565
6.441757	556.482252	8.692583
6.808972	566.169919	8.697600
7.130066	553.591102	8.702618
6.629729	554.187108	8.707635
6.545709	550.905668	8.712653
6.631701	544.710026	8.717671
6.314521	564.048089	8.722688
6.998865	557.619836	8.727706
6.357568	570.876953	8.732723
6.663052	562.762894	8.737741
6.891238	573.971359	8.742759
6.524258	571.122415	8.747776
6.690819	562.389494	8.752794
6.595578	570.634833	8.757811
6.793634	563.765217	8.762829
6.612980	558.548625	8.767847
6.403627	575.629181	8.772864
6.977182	563.471550	8.777882
6.474352	564.345658	8.782899
6.802184	569.110121	8.787917
6.633219	566.201750	8.792935
6.594809	577.647649	8.797952
6.808285	566.265959	8.802970
6.653345	561.632318	8.807987
6.637658	567.873875	8.813005
6.761081	584.416304	8.818023
6.735086	594.149817	8.823040
7.110982	589.259426	8.828058
6.933027	595.980854	8.833075
6.990625	595.419622	8.838093
7.116590	584.190488	8.843111
6.746948	574.036251	8.848128
7.327710	565.443558	8.853146
7.287703	573.449870	8.858163
6.759745	565.289670	8.863181
7.173551	564.417006	8.868199
6.855362	566.934765	8.873216
6.779441	566.504907	8.878234
6.836121	568.206536	8.883251
7.154661	559.878994	8.888269
7.010412	565.541089	8.893287
6.521836	569.369960	8.898304
7.123214	567.918796	8.903322
6.755351	568.118505	8.908339
6.919655	576.528308	8.913357
7.273151	579.411044	8.918375
6.977785	573.953644	8.923392
7.276943	567.576272	8.928410
6.981958	573.344038	8.933427
6.948992	574.759912	8.938445
7.196043	572.212392	8.943463
6.635981	576.677316	8.948480
6.840394	568.011045	8.953498
7.365246	574.710711	8.958515
7.018817	573.777281	8.963533
6.899538	571.451261	8.968551
6.382939	582.527116	8.973568
7.040450	571.975258	8.978586
6.897391	582.105803	8.983603
6.640689	588.148443	8.988621
7.496736	593.193070	8.993639
7.257171	599.419222	8.998656
7.071235	587.216471	9.003674
6.896320	587.430130	9.008691
7.130878	596.384359	9.013709
7.245715	583.440204	9.018727
7.078196	585.770256	9.023744
7.213401	577.679715	9.028762
6.805731	581.937726	9.033779
6.721782	591.784459	9.038797
7.137624	591.760390	9.043815
6.674893	595.484231	9.048832
7.261669	601.618781	9.053850
7.342856	603.748921	9.058867
7.075223	601.685983	9.063885
7.536764	596.097360	9.068903
7.519127	597.889531	9.073920
7.570518	591.762411	9.078938
7.145749	583.769072	9.083955
7.056681	579.238714	9.088973
7.464006	570.995086	9.093991
6.773294	580.340433	9.099008
7.181492	577.414213	9.104026
7.397939	581.280946	9.109043
6.997918	577.944870	9.114061
6.975312	583.897182	9.119079
7.277864	598.985131	9.124096
7.397861	594.769152	9.129114
7.436323	583.036176	9.134131
7.066576	581.008175	9.139149
7.270084	575.652491	9.144167
7.276018	594.084736	9.149184
7.009010	581.998832	9.154202
7.286821	590.062653	9.159219
7.212068	602.277969	9.164237
7.737063	596.919245	9.169255
7.815986	590.522723	9.174272
7.418335	576.664789	9.179290
7.291615	569.315881	9.184307
7.209617	581.895237	9.189325
7.588904	574.719509	9.194343
7.079439	572.808075	9.199360
7.401345	569.093800	9.204378
7.377789	577.372092	9.209395
7.418085	567.750077	9.214413
7.254423	563.221944	9.219431
6.883525	579.766081	9.224448
7.444642	571.937014	9.229466
7.443819	574.133649	9.234483
6.981130	583.765164	9.239501
7.456288	570.632019	9.244519
7.136101	585.707075	9.249536
7.289697	592.846770	9.254554
7.748957	597.170925	9.259571
7.222680	593.993484	9.264589
7.600802	592.359547	9.269607
7.535111	591.372662	9.274624
7.374322	581.100490	9.279642
7.444497	586.205130	9.284659
7.099374	580.948029	9.289677
7.236733	589.526162	9.294695
7.519067	602.029513	9.299712
7.841941	601.089044	9.304730
7.715403	594.443844	9.309747
7.504960	591.655577	9.314765
7.377007	580.564060	9.319783
7.280641	578.430110	9.324800
7.643919	586.789807	9.329818
7.505137	578.950478	9.334835
7.417071	582.902792	9.339853
7.662789	568.896723	9.344871
7.393267	577.674302	9.349888
7.336169	582.619001	9.354906
7.753995	584.623810	9.359923
7.515485	593.020995	9.364941
7.266629	587.436383	9.369959
7.513458	594.110190	9.374976
7.579146	600.269580	9.379994
7.868840	600.407287	9.385011
7.630408	599.873502	9.390029
7.285970	586.609984	9.395047
7.396427	597.622315	9.400064
7.339202	594.475524	9.405082
7.445634	600.480207	9.410099
7.523480	606.082270	9.415117
7.537209	606.787082	9.420135
7.279281	605.432683	9.425152
7.476861	604.868452	9.430170
7.887365	603.538711	9.435187
7.849801	598.952942	9.440205
7.621671	604.997422	9.445223
7.609058	604.876382	9.450240
7.373872	604.913291	9.455258
7.658019	595.382443	9.460275
7.468122	594.951507	9.465293
7.577603	595.931651	9.470311
7.474538	597.989673	9.475328
7.461996	600.936076	9.480346
7.402602	605.123745	9.485363
7.543021	601.160187	9.490381
7.959944	601.331609	9.495399
7.652400	599.896621	9.500416
7.616706	600.132648	9.505434
7.674890	589.835629	9.510451
7.903174	598.282756	9.515469
8.025273	591.791105	9.520487
7.488614	604.454337	9.525504
7.793267	593.295031	9.530522
7.935913	587.661700	9.535539
7.714846	600.556349	9.540557
7.719103	593.019651	9.545575
7.625442	597.676593	9.550592
7.514665	603.816295	9.555610
7.820040	600.417030	9.560627
7.977939	612.220358	9.565645
7.524141	607.491519	9.570663
7.651875	623.332717	9.575680
7.637226	618.935858	9.580698
8.464763	619.150242	9.585715
7.863402	622.946303	9.590733
7.639487	615.637851	9.595751
8.092727	628.578348	9.600768
7.774771	624.206919	9.605786
8.198047	609.320926	9.610803
7.449386	611.274975	9.615821
7.949253	615.933600	9.620839
7.845631	619.964100	9.625856
7.795367	617.232783	9.630874
7.806587	613.750215	9.635891
8.009218	630.482249	9.640909
8.282348	620.514455	9.645927
7.792546	607.740759	9.650944
7.679148	609.061939	9.655962
8.189493	615.454623	9.660979
8.143069	619.813834	9.665997
8.008404	599.243273	9.671015
7.621424	606.208895	9.676032
7.566048	615.628285	9.681050
8.096311	613.863210	9.686067
7.911940	618.218788	9.691085
8.018334	622.588769	9.696103
7.970594	632.148983	9.701120
8.142180	634.558454	9.706138
8.219197	626.836771	9.711155
8.318799	626.382566	9.716173
7.731162	604.658513	9.721191
7.999482	610.943949	9.726208
8.109732	626.222998	9.731226
8.179256	619.360876	9.736243
7.796639	619.098991	9.741261
7.879318	612.039150	9.746279
7.888896	623.184068	9.751296
7.956671	622.602305	9.756314
7.875707	621.340099	9.761331
7.803401	636.152295	9.766349
7.956583	636.415534	9.771367
8.127138	626.760455	9.776384
8.229152	630.260118	9.781402
8.481578	622.744484	9.786419
8.300472	632.341374	9.791437
8.338394	618.263682	9.796455
8.629360	617.359770	9.801472
7.843037	618.436090	9.806490
8.196954	614.057223	9.811507
8.220881	620.904821	9.816525
8.373759	609.362184	9.821543
8.175472	602.381083	9.826560
7.826707	600.125730	9.831578
8.268815	606.649023	9.836595
8.609162	622.135015	9.841613
8.050448	601.637204	9.846631
8.343196	598.451357	9.851648
7.885250	601.587467	9.856666
8.098802	608.676750	9.861683
8.457824	616.992947	9.866701
8.037995	613.028804	9.871719
8.198784	619.697167	9.876736
8.244018	631.234136	9.881754
8.281081	620.586957	9.886771
7.920650	617.689641	9.891789
8.114971	630.493982	9.896807
8.496268	627.862304	9.901824
8.265187	630.817706	9.906842
8.172787	629.740329	9.911859
8.338389	627.852506	9.916877
8.450056	625.957356	9.921895
8.346909	627.324269	9.926912
8.009001	630.750847	9.931930
8.162864	626.655789	9.936947
8.134837	632.318630	9.941965
8.255212	630.346375	9.946983
8.462706	630.074082	9.952000
8.125950	632.695745	9.957018
8.371592	622.694386	9.962035
8.310454	619.238934	9.967053
8.162102	621.332456	9.972071
8.449452	625.090259	9.977088
8.173177	626.395934	9.982106
8.428062	630.016813	9.987123
8.389527	632.295103	9.992141
8.240032	634.748570	9.997159
8.093725	632.751826	10.002176
7.945958	636.887077	10.007194
8.366919	647.178597	10.012211
8.258462	652.958189	10.017229
8.531551	661.694973	10.022247
8.550512	661.565829	10.027264
8.338121	666.525416	10.032282
8.894543	657.179094	10.037299
8.369275	665.463452	10.042317
8.834178	658.933845	10.047335
8.499340	652.580038	10.052352
8.235741	642.876209	10.057370
8.513930	650.400352	10.062387
8.716262	662.594385	10.067405
8.464021	665.704588	10.072423
8.641098	661.627975	10.077440
8.537456	666.766184	10.082458
8.825854	654.302873	10.087475
8.913548	646.203966	10.092493
8.278849	634.267157	10.097511
8.468405	623.640265	10.102528
8.626945	625.600496	10.107546
8.392800	633.400566	10.112563
8.082468	636.469372	10.117581
8.202013	644.289770	10.122599
8.459464	654.120916	10.127616
8.005156	657.471063	10.132634
8.510904	662.144558	10.137651
8.433636	658.199316	10.142669
8.362460	667.542313	10.147687
8.584289	660.646845	10.152704
8.613953	665.439116	10.157722
8.371711	673.593925	10.162739
8.736343	682.676141	10.167757
8.587171	690.690142	10.172775
8.786131	684.158013	10.177792
8.565696	690.864042	10.182810
9.107533	682.864377	10.187827
8.739991	681.558705	10.192845
8.841919	677.310824	10.197863
8.805415	664.182039	10.202880
8.604620	664.570169	10.207898
8.865918	661.572277	10.212915
8.599983	660.604139	10.217933
9.018511	669.987175	10.222951
9.262455	663.384889	10.227968
8.562222	663.507285	10.232986
8.791724	654.751834	10.238003
8.935891	657.421226	10.243021
8.572382	665.172151	10.248039
8.946574	661.986156	10.253056
8.934660	657.254340	10.258074
8.786865	655.664929	10.263091
9.078194	666.450146	10.268109
8.893460	659.971831	10.273127
8.942968	649.048128	10.278144
8.864627	656.880602	10.283162
8.996401	652.015820	10.288179
9.154505	651.211619	10.293197
8.556982	663.808689	10.298215
9.020730	663.657192	10.303232
9.198406	662.878326	10.308250
8.520031	662.949961	10.313267
8.555126	657.952002	10.318285
8.590743	664.965044	10.323303
8.932167	655.822824	10.328320
8.646987	663.166996	10.333338
8.759553	679.809046	10.338355
9.058825	684.338172	10.343373
9.102276	688.954719	10.348391
8.797079	688.813248	10.353408
8.825981	685.927504	10.358426
9.095485	691.344929	10.363443
9.314780	689.521271	10.368461
8.796554	694.206889	10.373479
9.304209	683.940379	10.378496
8.872807	679.574088	10.383514
8.799419	675.789182	10.388531
8.946670	691.125605	10.393549
8.586295	685.116618	10.398567
9.209278	679.209182	10.403584
8.835723	684.149843	10.408602
9.292695	683.425046	10.413619
9.323438	681.779257	10.418637
9.063815	691.303272	10.423655
9.413680	683.046505	10.428672
8.948830	682.434583	10.433690
8.941794	682.931211	10.438707
8.985781	685.404863	10.443725
8.803288	687.929780	10.448743
9.033468	684.239321	10.453760
9.140235	688.508273	10.458778
9.087157	688.194754	10.463795
9.259499	685.668392	10.468813
8.787918	686.534454	10.473831
9.144574	679.463217	10.478848
8.925780	682.457728	10.483866
8.844928	687.608152	10.488883
9.322473	681.480502	10.493901
9.070704	694.774509	10.498919
9.107292	681.653194	10.503936
8.985543	694.324064	10.508954
8.994114	692.501865	10.513971
9.216250	697.409157	10.518989
9.230627	716.509241	10.524007
9.370927	712.785521	10.529024
9.027172	713.562128	10.534042
9.287695	718.750592	10.539059
9.120654	713.273043	10.544077
9.208979	714.398521	10.549095
9.382525	712.676705	10.554112
9.235324	713.965319	10.559130
9.069340	716.434004	10.564147
9.183676	716.908461	10.569165
9.008451	719.021984	10.574183
9.247972	711.634569	10.579200
9.191456	708.137349	10.584218
9.052969	720.252278	10.589235
9.161028	709.735934	10.594253
9.245941	722.607976	10.599271
9.476302	712.564780	10.604288
9.317166	705.403933	10.609306
9.358470	715.811784	10.614323
9.165393	711.035755	10.619341
9.173544	717.759628	10.624359
9.630824	729.475100	10.629376
9.916493	730.178335	10.634394
9.376701	722.341812	10.639411
9.452512	714.465645	10.644429
9.074601	718.911531	10.649447
9.380939	720.441513	10.654464
9.856197	727.025930	10.659482
9.670897	723.391093	10.664499
9.461170	716.597934	10.669517
9.338520	723.364394	10.674535
9.385252	714.997316	10.679552
9.505210	718.140730	10.684570
9.576825	709.451016	10.689587
9.997163	713.718181	10.694605
9.127654	716.344433	10.699623
9.394459	711.537375	10.704640
9.875749	720.825397	10.709658
9.700353	721.354717	10.714675
9.871038	717.222287	10.719693
9.569706	708.707774	10.724711
9.532972	708.240214	10.729728
9.601426	710.580646	10.734746
9.610433	711.311449	10.739763
9.745567	703.580628	10.744781
9.743052	713.228474	10.749799
9.375578	716.492442	10.754816
9.636518	710.146254	10.759834
9.398213	712.348556	10.764851
9.727187	707.348720	10.769869
9.511121	717.301430	10.774887
9.341093	713.301281	10.779904
9.997995	722.394529	10.784922
9.943230	720.317160	10.789939
9.814935	714.615787	10.794957
9.426281	715.718168	10.799975
9.557778	718.471606	10.804992
9.658697	726.089829	10.810010
9.818877	735.046314	10.815027
9.921397	737.106854	10.820045
9.879192	741.588511	10.825063
9.743264	730.390852	10.830080
9.829272	711.107884	10.835098
9.761029	719.077659	10.840115
9.660437	712.766025	10.845133
9.625224	730.658898	10.850151
9.665526	733.868445	10.855168
10.019775	743.602422	10.860186
9.524934	745.605079	10.865203
9.962742	739.975947	10.870221
9.572252	747.961511	10.875239
9.826509	745.564319	10.880256
10.189462	740.028968	10.885274
9.846103	741.723864	10.890291
10.158294	738.184648	10.895309
9.909482	741.067106	10.900327
10.111133	744.137764	10.905344
10.038556	725.245706	10.910362
9.616976	732.481889	10.915379
10.023539	735.403673	10.920397
9.925480	738.152056	10.925415
9.864371	739.130534	10.930432
9.791477	739.921508	10.935450
9.679783	739.973783	10.940467
10.072079	729.690607	10.945485
9.883337	743.000021	10.950503
10.256932	736.516251	10.955520
10.319100	736.232012	10.960538
9.895668	742.035737	10.965555
10.014171	739.741867	10.970573
10.147074	733.904887	10.975591
10.065842	735.104271	10.980608
10.142423	738.529044	10.985626
10.125786	740.674527	10.990643
9.945958	743.861761	10.995661
9.656234	745.949046	11.000679
10.132491	735.980919	11.005696
10.261349	729.885796	11.010714
10.015407	738.157980	11.015731
10.064162	733.665950	11.020749
9.687287	738.392549	11.025767
9.732250	738.701148	11.030784
9.778178	738.791843	11.035802
9.725856	743.600137	11.040819
9.940575	735.089963	11.045837
9.958655	739.079329	11.050855
10.148802	756.596087	11.055872
10.185547	754.933571	11.060890
10.086177	761.800541	11.065907
10.540197	766.128714	11.070925
10.596915	760.051195	11.075943
10.263422	749.288427	11.080960
10.286036	739.287233	11.085978
10.059314	734.589054	11.090995
10.341215	732.556765	11.096013
10.416288	738.354967	11.101031
10.002394	742.632925	11.106048
10.518103	737.026304	11.111066
10.153660	742.360033	11.116083
10.094232	729.701857	11.121101
10.210693	742.408022	11.126119
10.268939	760.885891	11.131136
10.498278	758.240134	11.136154
10.613888	765.799266	11.141171
10.371438	740.972414	11.146189
10.054697	741.441829	11.151207
10.211099	759.026993	11.156224
10.374675	748.779643	11.161242
10.335598	764.984778	11.166259
10.400104	761.096196	11.171277
10.927949	759.899539	11.176295
10.456216	759.134056	11.181312
10.191012	748.139680	11.186330
10.098670	749.940416	11.191347
10.293007	754.369235	11.196365
10.651318	757.693064	11.201383
10.635132	767.926913	11.206400
10.652629	763.878436	11.211418
10.035129	757.130217	11.216435
10.502985	756.687739	11.221453
10.865809	751.414340	11.226471
10.702661	768.970685	11.231488
10.729533	753.234643	11.236506
10.215854	745.179421	11.241523
9.926931	757.008672	11.246541
10.656340	756.152824	11.251559
10.665286	765.779968	11.256576
10.571742	760.139408	11.261594
10.364569	766.000776	11.266611
10.154683	764.660928	11.271629
10.163245	763.072255	11.276647
10.252504	768.536880	11.281664
10.555251	756.276380	11.286682
10.543190	768.321039	11.291699
10.640535	763.180752	11.296717
11.040106	766.605416	11.301735
10.737467	768.192948	11.306752
10.814985	755.402841	11.311770
10.451905	768.711187	11.316787
10.415999	766.801273	11.321805
10.608206	768.213440	11.326823
10.256843	772.001920	11.331840
10.649572	763.211373	11.336858
10.670092	788.003719	11.341875
10.750784	789.414425	11.346893
10.728317	782.244757	11.351911
10.758101	791.079688	11.356928
11.123720	786.638985	11.361946
10.583872	782.974479	11.366963
10.570756	769.946096	11.371981
11.099422	778.453542	11.376999
10.600372	784.587869	11.382016
10.896074	779.782577	11.387034
10.428618	791.867044	11.392051
10.610549	787.291018	11.397069
10.798921	788.669073	11.402087
10.833769	789.086557	11.407104
11.005512	790.546113	11.412122
11.016544	784.014990	11.417139
10.960754	783.345284	11.422157
10.583788	788.680989	11.427175
10.595169	798.361418	11.432192
10.620269	786.384245	11.437210
10.851834	793.199376	11.442227
10.772091	792.489240	11.447245
11.084359	785.374423	11.452263
10.715895	788.259856	11.457280
10.793402	787.692343	11.462298
10.944158	784.891634	11.467315
11.099042	792.031207	11.472333
11.136664	792.037996	11.477351
10.917527	790.576517	11.482368
11.038209	780.073934	11.487386
11.258858	785.391744	11.492403
10.864640	785.415700	11.497421
11.055184	784.590631	11.502439
11.117902	785.347735	11.507456
11.239381	782.882978	11.512474
11.163777	789.307572	11.517491
11.089975	783.351482	11.522509
11.280611	783.839232	11.527527
11.206008	789.758733	11.532544
11.493456	778.560981	11.537562
11.139981	786.354568	11.542579
11.004113	797.509759	11.547597
11.134040	789.707132	11.552615
11.201127	788.790951	11.557632
10.990571	794.996846	11.562650
11.091180	787.823672	11.567667
11.170741	793.851565	11.572685
11.182723	791.628029	11.577703
11.220718	794.528675	11.582720
11.299727	793.954614	11.587738
11.210874	794.770182	11.592755
11.022289	794.705114	11.597773
11.033195	790.566143	11.602791
11.030490	799.952131	11.607808
10.871539	787.495702	11.612826
11.070619	793.356544	11.617843
10.872011	793.002708	11.622861
11.221229	804.883486	11.627879
11.157387	818.176542	11.632896
11.231933	824.602869	11.637914
11.329875	813.131826	11.642931
11.229431	815.511359	11.647949
11.618439	813.951437	11.652967
11.189501	820.273610	11.657984
11.417202	816.409940	11.663002
11.646569	816.064789	11.668019
11.319397	819.199381	11.673037
11.556613	816.211549	11.678055
11.366131	812.662714	11.683072
11.351095	816.745651	11.688090
11.520731	818.779905	11.693107
11.570393	819.750500	11.698125
11.645825	812.631754	11.703143
11.270050	819.649352	11.708160
11.307547	816.695968	11.713178
11.763287	815.236045	11.718195
11.558479	823.643837	11.723213
11.513938	812.034170	11.728231
11.641592	826.543791	11.733248
11.260971	820.563177	11.738266
11.370943	825.273480	11.743283
11.246820	814.007646	11.748301
11.137163	822.182774	11.753319
11.237642	817.196617	11.758336
11.469034	818.580558	11.763354
11.629995	825.981129	11.768371
11.395677	822.988279	11.773389
11.628422	818.669375	11.778407
11.562555	819.102640	11.783424
11.475326	819.239445	11.788442
11.720987	816.272380	11.793459
11.340658	821.693830	11.798477
11.605076	816.315908	11.803495
11.381940	810.436857	11.808512
11.336843	832.045820	11.813530
11.701891	833.459314	11.818547
11.546125	853.372012	11.823565
11.715347	844.676406	11.828583
11.970916	849.720516	11.833600
11.756289	840.949352	11.838618
12.053934	842.108315	11.843635
11.861007	841.308612	11.848653
11.908319	840.985673	11.853671
11.667157	823.426452	11.858688
11.597286	826.302978	11.863706
11.828386	831.268863	11.868723
11.818282	841.325073	11.873741
11.686399	838.088950	11.878759
11.606956	850.049545	11.883776
11.612364	843.421449	11.888794
11.872916	839.997603	11.893811
11.877624	845.046302	11.898829
12.056670	844.314552	11.903847
11.864458	846.364479	11.908864
11.738095	852.850698	11.913882
11.792308	839.581336	11.918899
11.444065	849.968247	11.923917
11.907767	840.718410	11.928935
12.075552	842.175435	11.933952
11.918035	843.329973	11.938970
11.687310	849.419125	11.943987
11.833487	838.439134	11.949005
11.972269	843.750853	11.954023
12.167432	840.750670	11.959040
12.142457	849.941353	11.964058
12.426038	843.484272	11.969075
12.423235	843.005080	11.974093
12.183364	841.483728	11.979111
12.255436	840.658284	11.984128
12.381988	842.390018	11.989146
12.391715	839.968009	11.994163
12.247841	848.082238	11.999181
12.334673	836.786493	12.004199
12.096039	833.219951	12.009216
12.000175	835.213754	12.014234
12.190753	840.744579	12.019251
12.054526	845.979464	12.024269
11.910668	846.144078	12.029287
12.028710	844.560336	12.034304
11.981262	843.901943	12.039322
12.235043	843.745474	12.044339
12.051834	851.976322	12.049357
12.129244	848.180375	12.054375
12.344241	838.262595	12.059392
11.993909	840.839077	12.064410
12.454548	838.573641	12.069427
12.471777	847.688282	12.074445
12.100766	847.743316	12.079463
12.064829	840.758776	12.084480
12.183083	841.532428	12.089498
12.408512	838.148800	12.094515
12.203594	839.711559	12.099533
12.372457	833.019987	12.104551
12.012617	846.264765	12.109568
12.064274	846.670149	12.114586
12.596130	841.742631	12.119603
12.127043	845.095127	12.124621
12.507010	842.356328	12.129639
12.377355	842.581833	12.134656
12.207211	847.799942	12.139674
12.407549	837.019753	12.144691
12.220386	844.168758	12.149709
12.160470	852.822109	12.154727
12.587732	857.807761	12.159744
12.282173	864.587153	12.164762
12.907386	865.158297	12.169779
12.412862	852.388321	12.174797
12.368560	848.646159	12.179815
12.501745	862.583731	12.184832
12.377160	874.286323	12.189850
12.635330	865.996501	12.194867
12.220829	867.412215	12.199885
12.711289	870.361904	12.204903
12.550125	872.388034	12.209920
12.353817	870.856698	12.214938
12.500905	866.191435	12.219955
12.650240	871.586717	12.224973
12.627501	868.813178	12.229991
12.550218	871.529923	12.235008
12.683608	869.432524	12.240026
12.513498	869.872655	12.245043
12.578737	870.083404	12.250061
12.733625	865.871363	12.255079
12.511651	868.582376	12.260096
12.459775	880.633348	12.265114
12.775202	863.138362	12.270131
12.632190	867.175089	12.275149
12.499479	870.301313	12.280167
12.638788	869.635749	12.285184
12.729526	873.430722	12.290202
13.006581	863.544230	12.295219
12.751701	876.842014	12.300237
12.918605	871.501445	12.305255
12.971851	881.572999	12.310272
12.585397	876.338065	12.315290
12.815488	868.554424	12.320307
12.943805	875.530933	12.325325
12.767865	857.664808	12.330343
12.851105	867.251963	12.335360
12.465141	864.248152	12.340378
12.599025	864.157806	12.345395
12.855886	880.105235	12.350413
13.147263	892.945050	12.355431
12.924667	876.137121	12.360448
12.692290	876.751114	12.365466
12.939945	879.218129	12.370483
12.996737	895.039125	12.375501
12.751338	893.228295	12.380519
12.816088	889.068242	12.385536
12.924058	903.347475	12.390554
12.911968	886.983090	12.395571
12.930339	898.950483	12.400589
12.801640	888.060868	12.405607
13.395003	885.339121	12.410624
13.180401	897.276742	12.415642
13.259734	894.130593	12.420659
13.309122	888.587521	12.425677
13.370797	893.999700	12.430695
13.363760	888.717938	12.435712
13.058273	891.498845	12.440730
13.142368	874.548188	12.445747
13.162327	868.571068	12.450765
12.924626	868.488448	12.455783
13.050293	875.844076	12.460800
12.951732	885.156763	12.465818
12.735038	887.153724	12.470835
13.201018	891.975526	12.475853
13.216045	892.011102	12.480871
13.557455	891.474821	12.485888
13.302695	894.471847	12.490906
13.251947	900.627492	12.495923
13.263548	897.668684	12.500941
13.538658	888.249552	12.505959
13.741674	886.671428	12.510976
13.411590	890.055803	12.515994
13.215908	881.493094	12.521011
13.303686	882.432473	12.526029
13.377767	883.367686	12.531047
13.538973	888.354006	12.536064
13.156124	882.755580	12.541082
13.312540	887.689001	12.546099
13.708086	893.825213	12.551117
13.372070	877.394822	12.556135
13.329829	868.890131	12.561152
13.276151	876.838759	12.566170
13.476525	885.252524	12.571187
13.156580	877.993725	12.576205
12.795170	894.161117	12.581223
13.087196	897.356500	12.586240
12.891867	895.578851	12.591258
12.749129	894.143263	12.596275
13.497116	907.735229	12.601293
13.233378	912.207456	12.606311
13.564612	917.684708	12.611328
13.429585	924.371130	12.616346
13.653539	918.374654	12.621363
13.394398	921.145148	12.626381
13.621145	918.979465	12.631399
13.766169	914.377631	12.636416
13.794129	920.868098	12.641434
14.022654	919.642587	12.646451
14.070500	908.621154	12.651469
13.556026	911.343288	12.656487
13.816762	900.279036	12.661504
13.242278	899.090980	12.666522
13.555504	910.829142	12.671539
13.295692	916.225426	12.676557
13.497102	916.146590	12.681575
14.043790	913.028201	12.686592
13.631490	914.102739	12.691610
13.656509	909.563890	12.696627
13.763432	921.230240	12.701645
13.673586	922.531974	12.706663
13.625655	911.493987	12.711680
13.551656	920.698699	12.716698
13.804877	917.171844	12.721715
14.068092	918.702288	12.726733
13.780872	919.621527	12.731751
13.880415	921.004042	12.736768
13.745823	921.470169	12.741786
14.010206	918.736844	12.746803
14.244690	920.792509	12.751821
13.854672	921.611088	12.756839
14.272725	914.198773	12.761856
13.801990	923.194243	12.766874
13.942707	923.566739	12.771891
14.106700	909.708912	12.776909
13.990951	916.152464	12.781927
14.265344	916.731239	12.786944
13.903425	921.496568	12.791962
13.780818	912.546846	12.796979
13.934984	920.055821	12.801997
13.535123	916.587109	12.807015
13.733075	914.220807	12.812032
13.630016	922.041490	12.817050
13.795634	937.040724	12.822067
13.912085	942.065631	12.827085
13.860935	950.307392	12.832103
13.934460	942.081180	12.837120
13.730564	950.586720	12.842138
13.755792	947.130296	12.847155
14.201166	951.216867	12.852173
13.881321	946.536378	12.857191
14.202676	951.437662	12.862208
14.284894	954.508134	12.867226
14.139530	942.911023	12.872243
13.974033	942.043900	12.877261
14.063474	940.941168	12.882279
14.296437	951.391712	12.887296
14.710665	951.844434	12.892314
14.398212	955.068265	12.897331
14.558706	940.074845	12.902349
14.449253	944.415607	12.907367
14.691848	937.100203	12.912384
14.354432	944.872406	12.917402
14.306098	934.853817	12.922419
14.559691	939.361762	12.927437
14.454876	938.491443	12.932455
14.590461	936.715592	12.937472
14.229335	946.101008	12.942490
14.416477	940.312269	12.947507
14.502589	936.666422	12.952525
14.451718	943.279704	12.957543
14.658415	939.908460	12.962560
14.553936	930.447792	12.967578
14.546472	939.717831	12.972595
14.547104	947.781060	12.977613
14.255939	945.459831	12.982631
14.307262	940.541304	12.987648
14.557139	941.991787	12.992666
14.060361	945.064611	12.997683
14.678524	942.622999	13.002701
14.275303	950.153044	13.007719
14.641444	945.109449	13.012736
14.553860	946.379271	13.017754
14.114183	942.916792	13.022771
14.692950	950.343473	13.027789
14.633234	955.383361	13.032807
14.983627	965.569355	13.037824
14.977918	968.120263	13.042842
14.619110	960.668698	13.047859
14.703574	945.548328	13.052877
14.620580	941.919508	13.057895
14.661385	937.703234	13.062912
14.625168	944.762355	13.067930
14.793215	961.111945	13.072947
15.024409	964.824968	13.077965
14.617998	953.262440	13.082983
14.841467	960.653274	13.088000
15.002838	964.241534	13.093018
14.558009	960.805106	13.098035
14.892216	962.053025	13.103053
14.854435	973.950369	13.108071
14.620050	967.659608	13.113088
14.957276	964.580340	13.118106
14.834537	971.946525	13.123123
14.827666	969.116834	13.128141
14.950521	963.903063	13.133159
14.754936	968.200520	13.138176
14.527892	960.497932	13.143194
14.961446	967.249922	13.148211
15.432405	959.128694	13.153229
14.773814	971.602999	13.158247
14.790151	953.605664	13.163264
15.197486	971.915444	13.168282
15.011608	982.482124	13.173299
15.267365	965.539200	13.178317
15.330618	975.290495	13.183335
15.048436	960.565238	13.188352
15.355474	966.279831	13.193370
14.697154	963.441755	13.198387
15.142279	961.822534	13.203405
15.083595	964.583718	13.208423
15.230293	967.337969	13.213440
15.545179	961.851108	13.218458
15.079675	976.431696	13.223475
15.355430	969.152110	13.228493
15.003219	971.407005	13.233511
15.042858	961.175796	13.238528
15.046194	961.904342	13.243546
14.861873	973.209249	13.248563
15.183215	967.866545	13.253581
15.185159	972.234042	13.258599
14.993212	962.190600	13.263616
15.110561	967.133320	13.268634
15.145594	973.818362	13.273651
15.421711	964.746180	13.278669
15.222881	963.758043	13.283687
15.328893	977.034071	13.288704
15.882695	979.390015	13.293722
15.131288	977.358649	13.298739
14.962518	975.756716	13.303757
15.225651	987.726845	13.308775
15.608935	986.928375	13.313792
15.788651	988.718067	13.318810
15.717277	995.239904	13.323827
15.817752	979.564716	13.328845
15.546978	970.919053	13.333863
15.522557	960.805182	13.338880
15.557112	954.535405	13.343898
15.063772	964.638995	13.348915
15.516095	970.245617	13.353933
15.506434	973.422009	13.358951
15.760746	981.417104	13.363968
15.814379	985.792285	13.368986
15.463639	982.322175	13.374003
15.553953	978.192811	13.379021
15.912921	977.224577	13.384039
15.586558	981.507813	13.389056
15.615760	976.097268	13.394074
15.502250	984.055318	13.399091
16.496379	979.929513	13.404109
15.848336	971.942579	13.409127
15.802795	964.684933	13.414144
15.887492	956.163467	13.419162
16.276031	960.697613	13.424179
15.878916	954.511250	13.429197
15.805935	951.619335	13.434215
15.762622	960.882378	13.439232
15.969611	953.932317	13.444250
15.993639	960.581208	13.449267
15.528241	956.324318	13.454285
15.860788	964.960415	13.459303
15.564003	961.888965	13.464320
15.566610	951.445808	13.469338
15.459033	957.812354	13.474355
16.115098	971.188392	13.479373
15.685698	970.495163	13.484391
15.786281	980.073349	13.489408
15.976759	981.315387	13.494426
16.072560	983.765183	13.499443
15.920433	982.693986	13.504461
16.068846	985.015615	13.509479
16.125059	986.799410	13.514496
16.145663	979.749151	13.519514
15.998969	979.371397	13.524531
15.931477	980.268835	13.529549
16.225756	987.957862	13.534567
15.917925	991.565993	13.539584
16.196728	980.331599	13.544602
15.928755	987.701611	13.549619
16.210614	989.194426	13.554637
16.043529	982.508096	13.559655
15.893636	980.180507	13.564672
16.105064	982.975113	13.569690
15.635773	982.651060	13.574707
16.030919	981.247957	13.579725
16.054249	985.012489	13.584743
15.638051	979.747469	13.589760
16.052309	1001.552915	13.594778
16.183008	1010.618302	13.599795
16.080623	1010.025317	13.604813
16.653283	1018.977278	13.609831
16.141118	1021.134161	13.614848
16.449017	1016.352142	13.619866
16.242096	1015.706106	13.624883
16.172104	1013.470139	13.629901
16.350384	1018.131919	13.634919
16.735386	1016.257019	13.639936
16.824490	1014.333804	13.644954
16.529450	1019.113928	13.649971
16.746674	1015.668435	13.654989
16.564518	1018.360607	13.660007
16.602852	1017.373179	13.665024
16.957530	1010.649271	13.670042
16.640349	998.277448	13.675059
16.252550	985.872517	13.680077
16.247000	1002.445009	13.685095
16.527254	1008.646663	13.690112
16.772374	1008.699838	13.695130
16.649225	1017.741883	13.700147
16.631649	1008.065581	13.705165
16.571190	1020.796509	13.710183
16.617692	1023.594871	13.715200
16.513779	1010.646812	13.720218
16.645521	1015.915502	13.725235
16.512098	1015.324224	13.730253
16.521396	1017.184803	13.735271
16.241605	1019.292653	13.740288
16.547860	1012.876141	13.745306
16.387985	1016.599954	13.750323
16.301025	1017.049152	13.755341
16.710352	1024.530815	13.760359
16.775323	1031.274307	13.765376
16.884369	1035.915380	13.770394
16.773430	1038.517500	13.775411
17.197350	1038.646805	13.780429
17.047215	1028.454760	13.785447
16.602645	1029.199836	13.790464
16.971885	1021.391172	13.795482
16.876636	1020.866498	13.800499
17.013550	1026.068108	13.805517
16.731835	1027.740747	13.810535
16.832010	1034.071614	13.815552
16.955305	1029.264865	13.820570
17.192101	1036.978699	13.825587
16.737258	1033.010479	13.830605
17.155888	1032.591488	13.835623
17.034280	1041.759540	13.840640
17.195930	1031.521798	13.845658
17.128932	1030.576119	13.850675
17.109818	1035.107881	13.855693
17.072932	1025.093759	13.860711
17.063728	1033.136477	13.865728
17.186655	1027.354615	13.870746
17.232629	1025.428689	13.875763
17.434302	1026.545896	13.880781
17.457653	1028.770358	13.885799
17.149880	1022.838223	13.890816
17.327691	1009.817621	13.895834
17.471926	1004.016649	13.900851
17.099944	1008.133464	13.905869
17.273690	998.534491	13.910887
17.178263	1009.923326	13.915904
17.171237	1012.111518	13.920922
17.219222	1019.220594	13.925939
16.721078	1026.083871	13.930957
17.560592	1020.401181	13.935975
17.102751	1024.354723	13.940992
17.480625	1027.748124	13.946010
17.248856	1029.703280	13.951027
16.892014	1025.590316	13.956045
16.732465	1017.100778	13.961063
16.934249	1033.192677	13.966080
17.493204	1040.234325	13.971098
17.582577	1049.760655	13.976115
17.343962	1044.429922	13.981133
17.248554	1049.147216	13.986151
17.472334	1058.276940	13.991168
17.664671	1053.449900	13.996186
17.754093	1059.239645	14.001203
17.440175	1059.175278	14.006221
17.675526	1054.795947	14.011239
17.497143	1058.074531	14.016256
17.809401	1049.716188	14.021274
18.001027	1048.237667	14.026291
17.738816	1063.985714	14.031309
18.240752	1043.583151	14.036327
18.120924	1050.046326	14.041344
17.734801	1032.998775	14.046362
17.883431	1019.048593	14.051379
18.018494	1017.250724	14.056397
18.046794	1024.132506	14.061415
18.010228	1021.184380	14.066432
17.621500	1021.119110	14.071450
18.044092	1009.997873	14.076467
17.679338	1017.424087	14.081485
18.101847	1019.737490	14.086503
17.803381	1018.736558	14.091520
18.009799	1018.710588	14.096538
18.070254	1016.507831	14.101555
17.532561	1018.769702	14.106573
17.859259	1012.782344	14.111591
17.774323	1011.110467	14.116608
17.960219	1011.460107	14.121626
18.029001	1013.365015	14.126643
18.073826	1015.235807	14.131661
17.744592	1014.552129	14.136679
18.040466	1023.124571	14.141696
18.034675	1035.042190	14.146714
18.500650	1025.987568	14.151731
17.463557	1027.005368	14.156749
17.862268	1033.677634	14.161767
18.047029	1042.289585	14.166784
18.074729	1045.447512	14.171802
18.272482	1043.702937	14.176819
18.061251	1049.959520	14.181837
18.539700	1038.646471	14.186855
18.339843	1045.699712	14.191872
18.267776	1040.977220	14.196890
18.584402	1041.864972	14.201907
18.419402	1048.770737	14.206925
18.298535	1033.338471	14.211943
18.025323	1024.210313	14.216960
18.067689	1034.854875	14.221978
18.409736	1034.772939	14.226995
18.286787	1045.339264	14.232013
18.308556	1039.809940	14.237031
18.323874	1042.474332	14.242048
18.240600	1042.613675	14.247066
18.577079	1036.545879	14.252083
18.079944	1045.450870	14.257101
18.704077	1051.642842	14.262119
18.271577	1050.501957	14.267136
18.303110	1039.145319	14.272154
18.409775	1044.269620	14.277171
18.252241	1041.596072	14.282189
18.441351	1044.293196	14.287207
18.322242	1051.674624	14.292224
18.180553	1039.997977	14.297242
18.615743	1054.626861	14.302259
18.363927	1072.699184	14.307277
18.515446	1066.672981	14.312295
18.464942	1069.126777	14.317312
18.208202	1070.505164	14.322330
18.513765	1067.620194	14.327347
18.595539	1066.872117	14.332365
18.871267	1065.222623	14.337383
18.568581	1072.017422	14.342400
18.764712	1071.163062	14.347418
18.513530	1067.418553	14.352435
18.593864	1071.691739	14.357453
18.773647	1061.151328	14.362471
18.741147	1074.045175	14.367488
18.689377	1077.105103	14.372506
18.925883	1077.481530	14.377523
18.788063	1086.109330	14.382541
18.945733	1082.335474	14.387559
19.021288	1088.461927	14.392576
19.143775	1092.980986	14.397594
19.140251	1086.452033	14.402611
19.262578	1091.075260	14.407629
18.982518	1074.664324	14.412647
19.075351	1066.996780	14.417664
18.760978	1066.127729	14.422682
19.299892	1061.675587	14.427699
18.659672	1073.127729	14.432717
19.034516	1080.447556	14.437735
19.258602	1087.257659	14.442752
19.194185	1087.782224	14.447770
19.230713	1089.767936	14.452787
19.041271	1093.755182	14.457805
19.528340	1093.031967	14.462823
19.130285	1075.440274	14.467840
18.759875	1090.321644	14.472858
19.199483	1092.692340	14.477875
19.226355	1095.578998	14.482893
19.081099	1091.679028	14.487911
19.112629	1090.389695	14.492928
19.518624	1098.553587	14.497946
19.432605	1081.279083	14.502963
19.166336	1090.154234	14.507981
19.416884	1097.553505	14.512999
19.385593	1093.260126	14.518016
19.279880	1095.252345	14.523034
19.522851	1085.270083	14.528051
19.106585	1093.824745	14.533069
19.351131	1096.746728	14.538087
19.207791	1092.224743	14.543104
19.180657	1102.305860	14.548122
19.337605	1087.991392	14.553139
19.251466	1093.859150	14.558157
19.346659	1080.403303	14.563175
19.378998	1094.833399	14.568192
19.716664	1112.081231	14.573210
19.959442	1120.466372	14.578227
19.757344	1112.305358	14.583245
19.433082	1093.966758	14.588263
19.620797	1108.233660	14.593280
19.948769	1119.183829	14.598298
20.013032	1104.442043	14.603315
19.765771	1103.985366	14.608333
19.942257	1103.680055	14.613351
19.673043	1088.905321	14.618368
19.253570	1093.386214	14.623386
19.610492	1098.878432	14.628403
19.416277	1115.408003	14.633421
19.670236	1114.487774	14.638439
20.074469	1122.752942	14.643456
19.633875	1118.529998	14.648474
20.237756	1122.427667	14.653491
19.961203	1124.042700	14.658509
19.929722	1115.204835	14.663527
19.876305	1114.708319	14.668544
19.936723	1120.070269	14.673562
20.060921	1108.967320	14.678579
20.014795	1116.362588	14.683597
20.073366	1118.357473	14.688615
20.371177	1104.652103	14.693632
20.195633	1111.452244	14.698650
20.116370	1105.922950	14.703667
20.115510	1117.398025	14.708685
19.976615	1113.402375	14.713703
20.066275	1106.303375	14.718720
19.806551	1116.430410	14.723738
20.263411	1105.278497	14.728755
20.155398	1111.654634	14.733773
19.956004	1106.434505	14.738791
20.326855	1102.693517	14.743808
20.273086	1113.387903	14.748826
20.060538	1103.224529	14.753843
19.915648	1110.363860	14.758861
20.191471	1108.954196	14.763879
20.124435	1101.447390	14.768896
19.635687	1112.405594	14.773914
19.940783	1123.943192	14.778931
20.090114	1131.285750	14.783949
20.255946	1125.102646	14.788967
20.802230	1125.398979	14.793984
20.441876	1136.214000	14.799002
20.418167	1137.091963	14.804019
20.576130	1129.095440	14.809037
20.390621	1135.704641	14.814055
20.573222	1133.230259	14.819072
20.488315	1135.777820	14.824090
20.791102	1132.457758	14.829107
20.904891	1129.116815	14.834125
20.405184	1131.593662	14.839143
21.136325	1129.705545	14.844160
20.786325	1141.860209	14.849178
20.686816	1127.803649	14.854195
20.590092	1129.153814	14.859213
20.724926	1126.961482	14.864231
20.949573	1133.294972	14.869248
20.809106	1131.587601	14.874266
20.588820	1126.623213	14.879283
20.881667	1121.991852	14.884301
20.804237	1132.061931	14.889319
21.058347	1126.988498	14.894336
21.144220	1125.109961	14.899354
20.834022	1122.091078	14.904371
20.795278	1126.067343	14.909389
20.877625	1135.093030	14.914407
20.935786	1124.208709	14.919424
21.010462	1123.960375	14.924442
21.074631	1127.387167	14.929459
20.845255	1128.186896	14.934477
20.831466	1129.558782	14.939495
21.073018	1118.352230	14.944512
20.948152	1120.760877	14.949530
20.907839	1123.165745	14.954547
20.770431	1128.183140	14.959565
20.806851	1122.891343	14.964583
20.961244	1114.330479	14.969600
20.672460	1127.135127	14.974618
21.022689	1118.619319	14.979635
21.208487	1124.737980	14.984653
20.886963	1129.171976	14.989671
21.511134	1140.015787	14.994688
21.129926	1144.377084	14.999706
21.341767	1148.067931	15.004723
21.160162	1141.301763	15.009741
21.188052	1152.857566	15.014759
21.360288	1150.993898	15.019776
21.315218	1144.717594	15.024794
21.502773	1145.180590	15.029811
21.694333	1149.407965	15.034829
21.468634	1149.916774	15.039847
21.661134	1137.708003	15.044864
21.036416	1139.544852	15.049882
21.308664	1139.297122	15.054899
21.307465	1154.660359	15.059917
21.158655	1146.733985	15.064935
21.305536	1149.986871	15.069952
21.179990	1146.478289	15.074970
21.541216	1151.931978	15.079987
20.909862	1152.273965	15.085005
21.246416	1161.477594	15.090023
21.489283	1166.905649	15.095040
21.710729	1180.498270	15.100058
22.200780	1177.035247	15.105075
21.880201	1190.280438	15.110093
21.779552	1172.509503	15.115111
21.864718	1161.983858	15.120128
21.630694	1152.385574	15.125146
22.044912	1150.323040	15.130163
21.926588	1146.923784	15.135181
21.804722	1150.180905	15.140199
21.508172	1147.049423	15.145216
22.071722	1156.700339	15.150234
21.991829	1161.632990	15.155251
21.725391	1143.654521	15.160269
21.895510	1162.080562	15.165287
22.147146	1169.880494	15.170304
21.887445	1166.468670	15.175322
21.984355	1170.130190	15.180339
22.505439	1162.824711	15.185357
21.955038	1157.943596	15.190375
21.849546	1144.077316	15.195392
21.861501	1143.195003	15.200410
22.215234	1160.853790	15.205427
22.611058	1164.115012	15.210445
22.055065	1153.292183	15.215463
22.387881	1140.648001	15.220480
21.934945	1136.269190	15.225498
21.760989	1143.100653	15.230515
22.255289	1159.181549	15.235533
22.160489	1167.386067	15.240551
22.345817	1162.029902	15.245568
22.539776	1172.161626	15.250586
22.469124	1172.955424	15.255603
22.318350	1162.318417	15.260621
22.306577	1171.646058	15.265639
22.262729	1167.635504	15.270656
22.127366	1170.273029	15.275674
22.241123	1167.424407	15.280691
22.439907	1175.614489	15.285709
22.166953	1175.376438	15.290727
22.384998	1168.803272	15.295744
22.301533	1165.038776	15.300762
21.953715	1178.177769	15.305779
22.165242	1168.800012	15.310797
22.160992	1188.553638	15.315815
22.394438	1186.282730	15.320832
22.752105	1193.292858	15.325850
22.416563	1198.574855	15.330867
22.486673	1196.755586	15.335885
22.510215	1203.736016	15.340903
22.455409	1193.601526	15.345920
22.643509	1195.329963	15.350938
22.680762	1200.361039	15.355955
22.482345	1188.686871	15.360973
22.505333	1200.413893	15.365991
22.425563	1201.461594	15.371008
22.673853	1205.465490	15.376026
22.650413	1222.072548	15.381043
23.108189	1223.228539	15.386061
22.934907	1226.998679	15.391079
22.959548	1217.438731	15.396096
23.278096	1220.705759	15.401114
23.208443	1216.718173	15.406131
23.064697	1208.506946	15.411149
22.849544	1198.195597	15.416167
22.807185	1199.767632	15.421184
22.949350	1208.174890	15.426202
23.202451	1220.323480	15.431219
23.492367	1208.932562	15.436237
23.356226	1215.265804	15.441255
23.444235	1194.347233	15.446272
23.562039	1191.112951	15.451290
22.886741	1190.925315	15.456307
23.259200	1189.544687	15.461325
22.848222	1192.645136	15.466343
23.325970	1194.530170	15.471360
23.490798	1190.789884	15.476378
23.346135	1188.051179	15.481395
23.345433	1184.655578	15.486413
23.006287	1189.007139	15.491431
23.520537	1200.085968	15.496448
23.208898	1192.020979	15.501466
23.474942	1204.401068	15.506483
23.413776	1206.768186	15.511501
23.056662	1215.805962	15.516519
23.082207	1214.927828	15.521536
23.337507	1212.189571	15.526554
23.302802	1216.007427	15.531571
23.038607	1212.804589	15.536589
23.332210	1217.587214	15.541607
23.268986	1218.291484	15.546624
23.526624	1219.440962	15.551642
23.460874	1227.981795	15.556659
23.743197	1229.638666	15.561677
23.770180	1234.873340	15.566695
23.613309	1235.787951	15.571712
23.513284	1226.613618	15.576730
23.458576	1237.257730	15.581747
24.013104	1229.003362	15.586765
23.858708	1231.388247	15.591783
23.479850	1237.674315	15.596800
23.805759	1230.718139	15.601818
23.866981	1231.049446	15.606835
23.979717	1227.891694	15.611853
23.874090	1236.555549	15.616871
23.797690	1234.929652	15.621888
23.866495	1228.231518	15.626906
23.872143	1231.828452	15.631923
24.131202	1227.568446	15.636941
23.959727	1235.213785	15.641959
23.633842	1234.662122	15.646976
23.771402	1237.723972	15.651994
23.603743	1240.521207	15.657011
24.078125	1248.926928	15.662029
24.118797	1261.033086	15.667047
23.905296	1258.974213	15.672064
24.159424	1254.516150	15.677082
24.283198	1253.471139	15.682099
24.308855	1252.583518	15.687117
24.068432	1256.632438	15.692135
24.361101	1253.651625	15.697152
24.305419	1250.618090	15.702170
24.393214	1259.668234	15.707187
24.455345	1252.832275	15.712205
24.864830	1250.186625	15.717223
24.714850	1250.159688	15.722240
24.767859	1248.724962	15.727258
24.751396	1235.535810	15.732275
24.669398	1218.134307	15.737293
24.306044	1217.597983	15.742311
24.253801	1226.736325	15.747328
24.553019	1220.933092	15.752346
24.547370	1230.427068	15.757363
24.593221	1231.963193	15.762381
24.447802	1240.153583	15.767399
24.580225	1241.931776	15.772416
24.758717	1242.118473	15.777434
24.513009	1241.967674	15.782451
24.978458	1242.983604	15.787469
24.914127	1250.397559	15.792487
24.809442	1241.552165	15.797504
24.909599	1236.367119	15.802522
24.702973	1244.958436	15.807539
24.946915	1240.325240	15.812557
25.220692	1235.744177	15.817575
24.725353	1232.675385	15.822592
24.575834	1229.587126	15.827610
24.754220	1244.325832	15.832627
24.959786	1234.674408	15.837645
24.996628	1246.951578	15.842663
24.694687	1249.239657	15.847680
25.008368	1249.831224	15.852698
24.886099	1245.757197	15.857715
25.108065	1245.261714	15.862733
24.770168	1245.825976	15.867751
24.420116	1246.941275	15.872768
24.468801	1243.234955	15.877786
24.724781	1255.411521	15.882803
24.717690	1266.291197	15.887821
25.050165	1269.966324	15.892839
25.064322	1274.309890	15.897856
24.776644	1268.409240	15.902874
24.801464	1281.395246	15.907891
25.322307	1274.588398	15.912909
25.513959	1289.555446	15.917927
25.703388	1285.208502	15.922944
25.456786	1271.645111	15.927962
25.455051	1271.812707	15.932979
25.164417	1272.675691	15.937997
25.292964	1270.433831	15.943015
25.444098	1284.024923	15.948032
25.892591	1287.277917	15.953050
25.494432	1284.209669	15.958067
25.417226	1274.561502	15.963085
25.762016	1270.733040	15.968103
25.245573	1276.475766	15.973120
25.982378	1282.132593	15.978138
25.790311	1292.214410	15.983155
25.594121	1271.368681	15.988173
26.022234	1273.214162	15.993191
25.976355	1274.761507	15.998208
25.922349	1264.093499	16.003226
25.775827	1268.493797	16.008243
25.507718	1272.471316	16.013261
25.698998	1263.992968	16.018279
25.728946	1275.930396	16.023296
25.956199	1282.415016	16.028314
25.943827	1290.584583	16.033331
26.117005	1295.193585	16.038349
26.231954	1288.040056	16.043367
25.927906	1273.775577	16.048384
26.012643	1269.463976	16.053402
26.034438	1271.161670	16.058419
26.110755	1272.986527	16.063437
25.994336	1267.914303	16.068455
26.018738	1297.150304	16.073472
26.186478	1291.443391	16.078490
26.054827	1290.504672	16.083507
26.033169	1291.133002	16.088525
26.169980	1286.276727	16.093543
25.677553	1297.926771	16.098560
26.130518	1294.592618	16.103578
26.289514	1291.175131	16.108595
26.047562	1294.425847	16.113613
26.170272	1290.158786	16.118631
25.913016	1298.758062	16.123648
25.995331	1293.509520	16.128666
26.045537	1305.601591	16.133683
26.291404	1313.389866	16.138701
26.348377	1316.656869	16.143719
26.079306	1322.556519	16.148736
26.656813	1317.378713	16.153754
26.327254	1317.957451	16.158771
26.703425	1321.581560	16.163789
26.713952	1322.271122	16.168807
26.578267	1325.331616	16.173824
26.564599	1314.688817	16.178842
26.672003	1312.993087	16.183859
26.634218	1317.830817	16.188877
27.037849	1315.129267	16.193895
26.447379	1317.150123	16.198912
26.453682	1313.870170	16.203930
26.418334	1320.686295	16.208947
26.778456	1318.092552	16.213965
26.760933	1324.148459	16.218983
26.827057	1335.228154	16.224000
27.046236	1326.612855	16.229018
27.008926	1334.353985	16.234035
27.134281	1324.797135	16.239053
27.252474	1308.803288	16.244071
27.357425	1307.089007	16.249088
27.670304	1300.731318	16.254106
27.574429	1298.022823	16.259123
27.409549	1308.955650	16.264141
27.465669	1308.148464	16.269159
27.587255	1313.623970	16.274176
27.218049	1292.243567	16.279194
27.241442	1279.401604	16.284211
26.927547	1277.336367	16.289229
27.445628	1288.051718	16.294247
27.464158	1299.063104	16.299264
27.473348	1285.727879	16.304282
27.452050	1282.423853	16.309299
27.009823	1276.509543	16.314317
27.388016	1268.172328	16.319335
27.121476	1276.072430	16.324352
27.256897	1282.132763	16.329370
27.982398	1291.360731	16.334387
27.555764	1296.641248	16.339405
27.534853	1289.995019	16.344423
27.398234	1294.923971	16.349440
27.720325	1288.123011	16.354458
27.705917	1302.077739	16.359475
27.644542	1301.437292	16.364493
27.919895	1289.215436	16.369511
27.509866	1277.984637	16.374528
27.532713	1272.227845	16.379546
27.813724	1286.152055	16.384563
27.486261	1294.522477	16.389581
27.577324	1296.184074	16.394599
27.626787	1300.556829	16.399616
27.576515	1291.838591	16.404634
27.601106	1296.937953	16.409651
27.678409	1298.289267	16.414669
27.808725	1291.228007	16.419687
27.878070	1300.363117	16.424704
27.389643	1290.091376	16.429722
27.539312	1302.975781	16.434739
27.753495	1327.044225	16.439757
28.263183	1322.653405	16.444775
27.975772	1325.412610	16.449792
28.104835	1320.857355	16.454810
28.234101	1326.170709	16.459827
27.974083	1321.452343	16.464845
28.120177	1324.575990	16.469863
28.182708	1321.009503	16.474880
28.258405	1327.716710	16.479898
28.209349	1317.634900	16.484915
27.945770	1318.967038	16.489933
28.381038	1311.649698	16.494951
28.095848	1318.101007	16.499968
28.268920	1316.716894	16.504986
28.108599	1312.964408	16.510003
28.134259	1331.552119	16.515021
28.772514	1344.457838	16.520039
28.730832	1344.887326	16.525056
28.510764	1324.698557	16.530074
28.548846	1321.438871	16.535091
28.440077	1326.537044	16.540109
28.724765	1319.622007	16.545127
28.308246	1328.432451	16.550144
28.644345	1346.491834	16.555162
29.084299	1348.641595	16.560179
28.590393	1340.330528	16.565197
28.552837	1342.141674	16.570215
28.636923	1346.199733	16.575232
28.957386	1340.945424	16.580250
29.233091	1347.719136	16.585267
28.828664	1340.047331	16.590285
28.854151	1328.369550	16.595303
28.604052	1336.989814	16.600320
28.897218	1341.378048	16.605338
29.112346	1340.224040	16.610355
28.841077	1347.730421	16.615373
28.644807	1347.802260	16.620391
28.786465	1339.893409	16.625408
29.005144	1350.261214	16.630426
29.261100	1347.084157	16.635443
28.840631	1347.093288	16.640461
28.998408	1345.263425	16.645479
28.705798	1350.497712	16.650496
28.660657	1341.791269	16.655514
29.108283	1356.853974	16.660531
28.835705	1372.329348	16.665549
29.320231	1371.174156	16.670567
29.286101	1368.702140	16.675584
29.080838	1370.063017	16.680602
29.781895	1372.323357	16.685619
29.292501	1371.039879	16.690637
29.408217	1367.278848	16.695655
29.539976	1374.460150	16.700672
29.218551	1367.109859	16.705690
29.332078	1371.794502	16.710707
29.265398	1372.130073	16.715725
29.603373	1367.816642	16.720743
29.860653	1376.120733	16.725760
29.177482	1375.580861	16.730778
29.115820	1372.087473	16.735795
29.704924	1388.687079	16.740813
29.826642	1387.907483	16.745831
29.821519	1392.923161	16.750848
29.770997	1397.548303	16.755866
29.895995	1394.489591	16.760883
29.601650	1403.404011	16.765901
29.898640	1395.224634	16.770919
30.296509	1393.783203	16.775936
30.016712	1392.867690	16.780954
30.464670	1387.151558	16.785971
30.023282	1383.398911	16.790989
30.075105	1382.197900	16.796007
29.931450	1376.148411	16.801024
29.726969	1377.657495	16.806042
29.881845	1380.773464	16.811059
30.133919	1382.151053	16.816077
29.625240	1390.111235	16.821095
30.119410	1383.586250	16.826112
29.901175	1389.055060	16.831130
29.922931	1385.696929	16.836147
29.623864	1392.923648	16.841165
30.055272	1402.753200	16.846183
30.253916	1402.460192	16.851200
30.333261	1407.866603	16.856218
30.512567	1405.364297	16.861235
30.430331	1415.832938	16.866253
30.598569	1406.998353	16.871271
30.635898	1407.813114	16.876288
30.365004	1414.776638	16.881306
30.282847	1409.247704	16.886323
29.903216	1416.199862	16.891341
30.144353	1407.341231	16.896359
30.414090	1413.424748	16.901376
30.490874	1402.972862	16.906394
30.787018	1410.829045	16.911411
31.153165	1430.237712	16.916429
31.039241	1419.954558	16.921447
31.403885	1404.480618	16.926464
30.945954	1408.121817	16.931482
30.818261	1401.829965	16.936499
30.814790	1404.399519	16.941517
31.278952	1405.664981	16.946535
30.841993	1412.316836	16.951552
30.972193	1410.200939	16.956570
31.217775	1406.583662	16.961587
30.804640	1407.544745	16.966605
31.071184	1410.381278	16.971623
31.026234	1411.568710	16.976640
31.058829	1416.070375	16.981658
31.178561	1405.779024	16.986675
31.149990	1418.517862	16.991693
31.100901	1411.071233	16.996711
31.069613	1413.831349	17.001728
31.028633	1407.077762	17.006746
31.297539	1404.763399	17.011763
31.268321	1415.372064	17.016781
31.214435	1430.576527	17.021799
31.450112	1434.140616	17.026816
31.690972	1440.395933	17.031834
31.549031	1436.911954	17.036851
31.542667	1421.934807	17.041869
31.228172	1418.698785	17.046887
31.334862	1428.067962	17.051904
31.256173	1431.656058	17.056922
31.609642	1434.680958	17.061939
31.717963	1432.013036	17.066957
31.496764	1432.274983	17.071975
31.800498	1431.160738	17.076992
31.593778	1435.002436	17.082010
31.888650	1430.850386	17.087027
31.603777	1432.589832	17.092045
31.630215	1428.000134	17.097063
31.941117	1431.602932	17.102080
31.702911	1431.842296	17.107098
32.024390	1427.136940	17.112115
31.719196	1426.275900	17.117133
31.719709	1432.650926	17.122151
31.568768	1429.184139	17.127168
31.927002	1446.227091	17.132186
32.176174	1445.493798	17.137203
32.295159	1452.323665	17.142221
32.101611	1454.866200	17.147239
32.257122	1455.432061	17.152256
32.348785	1459.321692	17.157274
32.532163	1451.033851	17.162291
32.472382	1459.832650	17.167309
32.295628	1447.839321	17.172327
32.373846	1441.799230	17.177344
32.244569	1450.018746	17.182362
32.674729	1453.577616	17.187379
32.488844	1436.940141	17.192397
31.981877	1437.609797	17.197415
32.400634	1445.778162	17.202432
32.625667	1455.005728	17.207450
32.635168	1445.760471	17.212467
32.858067	1448.553353	17.217485
32.408394	1454.509747	17.222503
32.697427	1443.841536	17.227520
32.491877	1451.119901	17.232538
32.428728	1446.746217	17.237555
32.443139	1455.722747	17.242573
32.626613	1456.877548	17.247591
32.401329	1447.754287	17.252608
32.582427	1451.304840	17.257626
32.648746	1450.013186	17.262643
32.806509	1445.005256	17.267661
32.626537	1455.072646	17.272679
32.976043	1460.891204	17.277696
32.723982	1482.628058	17.282714
32.850787	1472.963599	17.287731
33.123417	1477.121542	17.292749
32.769772	1481.538565	17.297767
33.261611	1480.764094	17.302784
33.033539	1482.138020	17.307802
33.226780	1482.811586	17.312819
33.247439	1476.509087	17.317837
33.215221	1473.421343	17.322855
33.383397	1481.840435	17.327872
33.023907	1477.396402	17.332890
33.280929	1479.590621	17.337907
33.351924	1483.502432	17.342925
32.896607	1476.125735	17.347943
33.283386	1466.909722	17.352960
33.159402	1473.531499	17.357978
33.547997	1485.943078	17.362995
33.732206	1509.391580	17.368013
33.559680	1499.856061	17.373031
33.607171	1492.122852	17.378048
33.470864	1500.700118	17.383066
33.383893	1498.801283	17.388083
33.704365	1508.316897	17.393101
33.490961	1511.392756	17.398119
33.721353	1498.988444	17.403136
33.695532	1510.937923	17.408154
33.943777	1504.356746	17.413171
33.963700	1508.945632	17.418189
33.807134	1506.877809	17.423207
33.840824	1499.345586	17.428224
33.910053	1502.295105	17.433242
33.654025	1501.139164	17.438259
33.942898	1499.143570	17.443277
33.803999	1500.702353	17.448295
34.194600	1504.822883	17.453312
33.980470	1523.694530	17.458330
34.206563	1527.809280	17.463347
34.458499	1532.257673	17.468365
34.303761	1523.322146	17.473383
34.318177	1511.737504	17.478400
34.005905	1515.608380	17.483418
33.765510	1527.926023	17.488435
34.560131	1531.257382	17.493453
34.091172	1531.037412	17.498471
34.165246	1524.082708	17.503488
34.172580	1518.101037	17.508506
34.215688	1519.132660	17.513523
34.366538	1524.101845	17.518541
34.715049	1522.494558	17.523559
34.742014	1520.492658	17.528576
34.709335	1527.747125	17.533594
34.488874	1527.810130	17.538611
34.697825	1516.974532	17.543629
34.335231	1528.153077	17.548647
34.680924	1542.244087	17.553664
35.184700	1552.497909	17.558682
35.313717	1544.833960	17.563699
35.467535	1525.242829	17.568717
35.024701	1525.429043	17.573735
35.112669	1511.024054	17.578752
34.887252	1511.365562	17.583770
34.923107	1518.770242	17.588787
34.885796	1511.526865	17.593805
34.823275	1516.169697	17.598823
35.083941	1506.799844	17.603840
35.180868	1514.078183	17.608858
35.034487	1511.118778	17.613875
35.096726	1517.989120	17.618893
35.151677	1530.014324	17.623911
35.402136	1541.699617	17.628928
35.583754	1543.788887	17.633946
35.035272	1532.639583	17.638963
35.440288	1532.124880	17.643981
35.615849	1532.842245	17.648999
35.560936	1535.754412	17.654016
35.388599	1536.756672	17.659034
35.513064	1541.193479	17.664051
35.507936	1537.656485	17.669069
35.448196	1536.523439	17.674087
35.647233	1533.317396	17.679104
35.457666	1539.450828	17.684122
35.404966	1539.222446	17.689139
35.694367	1539.814671	17.694157
35.591708	1541.033245	17.699175
35.452836	1538.041100	17.704192
35.617712	1541.931902	17.709210
35.441590	1535.518195	17.714227
35.844489	1541.378910	17.719245
35.569479	1557.845803	17.724263
35.903516	1563.572139	17.729280
35.985266	1563.316379	17.734298
36.114549	1565.824129	17.739315
35.805506	1554.239642	17.744333
35.847545	1570.896728	17.749351
35.617524	1564.175857	17.754368
36.031973	1568.131710	17.759386
35.769205	1565.250495	17.764403
36.246059	1570.698822	17.769421
36.200846	1594.028736	17.774439
36.230690	1584.770752	17.779456
36.762523	1585.157728	17.784474
36.486718	1579.236178	17.789491
36.791530	1583.688923	17.794509
37.112583	1569.360984	17.799527
37.052312	1560.085571	17.804544
37.030593	1549.914136	17.809562
36.688305	1553.224801	17.814579
36.745629	1545.947647	17.819597
36.703128	1548.655888	17.824615
36.467715	1549.077863	17.829632
36.379331	1546.791057	17.834650
36.224986	1547.127742	17.839667
36.266927	1543.002672	17.844685
36.392027	1573.356345	17.849703
36.652178	1568.445954	17.854720
36.492442	1569.073835	17.859738
36.547442	1572.653636	17.864755
36.868681	1572.297234	17.869773
36.807036	1577.542739	17.874791
37.032455	1595.641807	17.879808
36.907532	1595.361621	17.884826
37.026745	1592.322718	17.889843
37.236672	1587.461219	17.894861
37.106900	1606.083035	17.899879
37.225456	1600.077599	17.904896
37.248661	1597.246253	17.909914
37.086225	1598.351112	17.914931
37.200530	1594.422988	17.919949
37.187214	1598.272289	17.924967
36.991833	1600.190246	17.929984
37.137710	1593.700820	17.935002
37.047224	1593.263750	17.940019
37.194693	1591.082006	17.945037
37.486160	1616.233858	17.950055
37.931911	1615.179408	17.955072
37.817896	1611.062977	17.960090
37.615385	1612.896839	17.965107
37.705436	1610.597849	17.970125
37.923924	1611.949159	17.975143
37.912568	1608.024940	17.980160
37.924722	1599.037979	17.985178
37.860916	1606.250015	17.990195
38.091657	1601.719786	17.995213
38.141880	1595.374743	18.000231
37.485727	1590.191320	18.005248
37.860927	1598.155128	18.010266
37.987066	1608.666978	18.015283
37.886309	1604.150815	18.020301
38.015535	1616.622059	18.025319
37.955184	1613.926886	18.030336
38.300604	1610.382294	18.035354
38.296435	1610.493467	18.040371
38.244412	1607.411958	18.045389
38.194037	1616.020000	18.050407
38.010518	1612.621401	18.055424
38.419768	1602.152025	18.060442
38.195440	1608.442413	18.065459
38.424705	1611.575172	18.070477
38.396269	1611.412419	18.075495
38.151499	1614.490054	18.080512
38.276894	1622.635031	18.085530
38.283797	1636.353137	18.090547
38.422959	1632.806142	18.095565
38.907852	1639.957470	18.100583
38.720771	1637.260057	18.105600
38.770807	1631.502045	18.110618
38.729848	1631.338099	18.115635
38.620860	1626.586520	18.120653
38.929810	1629.192369	18.125671
38.673620	1618.287568	18.130688
39.151191	1623.600090	18.135706
39.122585	1622.919781	18.140723
39.171583	1619.238583	18.145741
39.255436	1618.846785	18.150759
39.155119	1624.155170	18.155776
39.384340	1616.674318	18.160794
38.865902	1622.695193	18.165811
39.278861	1624.293762	18.170829
39.358362	1616.334565	18.175847
39.425115	1612.893598	18.180864
39.475989	1614.880276	18.185882
39.207269	1621.969780	18.190899
39.280299	1614.750101	18.195917
39.403171	1618.524417	18.200935
39.228384	1623.348979	18.205952
39.669392	1620.657308	18.210970
39.415569	1614.647091	18.215987
39.803239	1625.938534	18.221005
39.679212	1619.579754	18.226023
39.194635	1629.164759	18.231040
39.905574	1644.915488	18.236058
39.551348	1648.329034	18.241075
39.926929	1648.689997	18.246093
39.973237	1634.761680	18.251111
39.981336	1652.080607	18.256128
40.143413	1645.522348	18.261146
39.974913	1642.695783	18.266163
40.053412	1636.955402	18.271181
40.125426	1627.918020	18.276199
40.419200	1634.120931	18.281216
40.516319	1615.759956	18.286234
40.312625	1620.809966	18.291251
40.138947	1611.426055	18.296269
40.251985	1615.602724	18.301287
40.062777	1618.226658	18.306304
40.116736	1608.904919	18.311322
40.264162	1616.235351	18.316339
40.161518	1622.127960	18.321357
40.639462	1633.553596	18.326375
40.275056	1642.125639	18.331392
40.554938	1635.867683	18.336410
40.307037	1640.489096	18.341427
40.285424	1638.882982	18.346445
40.723607	1639.918988	18.351463
40.373343	1644.184033	18.356480
40.452185	1630.907070	18.361498
40.550554	1638.734377	18.366515
40.644660	1638.173705	18.371533
40.786317	1637.776006	18.376551
40.784909	1634.506670	18.381568
40.853281	1641.101527	18.386586
40.760866	1650.726092	18.391603
40.850777	1638.861278	18.396621
41.204210	1660.187881	18.401639
41.033166	1666.728734	18.406656
40.967089	1670.131853	18.411674
41.482528	1670.363599	18.416691
41.433490	1670.516519	18.421709
41.648653	1666.752468	18.426727
40.739511	1651.815582	18.431744
40.950172	1651.059912	18.436762
40.874191	1673.627842	18.441779
41.366659	1667.781564	18.446797
41.294677	1671.864150	18.451815
41.156818	1665.766314	18.456832
41.141375	1667.659240	18.461850
41.229335	1666.976446	18.466867
41.332986	1679.653725	18.471885
41.834343	1691.568067	18.476903
41.529439	1694.592016	18.481920
41.688226	1697.827357	18.486938
41.389114	1696.974818	18.491955
41.381047	1696.960362	18.496973
41.846674	1692.137672	18.501991
41.527060	1695.896121	18.507008
41.546418	1689.199250	18.512026
41.689776	1687.327428	18.517043
41.940997	1713.347314	18.522061
42.216267	1709.895750	18.527079
42.257013	1705.379484	18.532096
42.104678	1711.320936	18.537114
42.018270	1718.564962	18.542131
42.166104	1708.811869	18.547149
42.069669	1709.776998	18.552167
41.880636	1713.546551	18.557184
42.548291	1709.702128	18.562202
42.246379	1715.944746	18.567219
41.702064	1715.048568	18.572237
42.110843	1704.894807	18.577255
42.113764	1717.373286	18.582272
42.240209	1718.499168	18.587290
42.411255	1716.698749	18.592307
43.069879	1725.997386	18.597325
43.126687	1719.755415	18.602343
42.777510	1726.333667	18.607360
43.136246	1718.223370	18.612378
43.510195	1698.313519	18.617395
42.701664	1697.711219	18.622413
43.070384	1697.249540	18.627431
43.028628	1696.321962	18.632448
43.248459	1691.361048	18.637466
43.187334	1701.129070	18.642483
42.921519	1697.686540	18.647501
43.215494	1682.302334	18.652519
43.068388	1688.274519	18.657536
42.913256	1693.386372	18.662554
42.896487	1687.013920	18.667571
42.958950	1689.159748	18.672589
43.197136	1685.379462	18.677607
43.258225	1700.547204	18.682624
43.211645	1711.411245	18.687642
43.563843	1719.160946	18.692659
43.216688	1724.047257	18.697677
43.464268	1717.535539	18.702695
43.469197	1725.140824	18.707712
43.524396	1714.625862	18.712730
43.705230	1725.148147	18.717747
43.310174	1717.941800	18.722765
43.521834	1714.979916	18.727783
43.733746	1720.933734	18.732800
43.481992	1716.554817	18.737818
43.310734	1721.378852	18.742835
43.363877	1742.591644	18.747853
44.127219	1740.483814	18.752871
43.715321	1751.973200	18.757888
43.768864	1744.128473	18.762906
43.751042	1744.999231	18.767923
43.973390	1744.853993	18.772941
43.975579	1746.163458	18.777959
44.111773	1742.781019	18.782976
44.167340	1741.592022	18.787994
44.342970	1746.039800	18.793011
44.422809	1768.450883	18.798029
44.538870	1769.799317	18.803047
44.522982	1767.229707	18.808064
44.048396	1757.665632	18.813082
44.660464	1758.611281	18.818099
44.596095	1760.309898	18.823117
44.544279	1767.299199	18.828135
44.609946	1775.668214	18.833152
44.866882	1775.495465	18.838170
44.844071	1766.864217	18.843187
44.590257	1767.888723	18.848205
44.950192	1754.602344	18.853223
44.749516	1765.168647	18.858240
44.604072	1759.677923	18.863258
44.516133	1756.709321	18.868275
44.643978	1774.735490	18.873293
44.733573	1759.651501	18.878311
44.687855	1763.010420	18.883328
45.130108	1777.547267	18.888346
45.349759	1787.722656	18.893363
45.159832	1791.558642	18.898381
45.756585	1781.612089	18.903399
45.794298	1780.807766	18.908416
45.364588	1769.043215	18.913434
45.653121	1751.491614	18.918451
45.559897	1751.597805	18.923469
45.752757	1754.771009	18.928487
45.576344	1746.993870	18.933504
45.794981	1748.922719	18.938522
45.416318	1747.883812	18.943539
45.609481	1753.446076	18.948557
45.734463	1750.226349	18.953575
45.782495	1753.403308	18.958592
45.455794	1747.773718	18.963610
45.488431	1744.492716	18.968627
45.485395	1756.467193	18.973645
45.699740	1773.185839	18.978663
45.989164	1778.045015	18.983680
45.759319	1780.795268	18.988698
45.943896	1776.130208	18.993715
45.838646	1780.805052	18.998733
46.196610	1774.465381	19.003751
45.905919	1780.305447	19.008768
45.652896	1784.454296	19.013786
46.021921	1771.832402	19.018803
45.918578	1792.391226	19.023821
46.453021	1795.103791	19.028839
46.374820	1798.773941	19.033856
46.026984	1799.017860	19.038874
46.445479	1804.560616	19.043891
46.362363	1803.289194	19.048909
46.488875	1803.859610	19.053927
46.690772	1798.380730	19.058944
46.302527	1795.522293	19.063962
46.732795	1795.502280	19.068979
46.386159	1816.039285	19.073997
46.584232	1825.271267	19.079015
47.035452	1825.307937	19.084032
46.558658	1831.922002	19.089050
46.979915	1825.947965	19.094067
47.052020	1830.004855	19.099085
46.663574	1828.831766	19.104103
46.626561	1832.975186	19.109120
46.589015	1835.187197	19.114138
46.926223	1839.104717	19.119155
46.762910	1851.580930	19.124173
47.160316	1850.922235	19.129191
47.177137	1859.362062	19.134208
47.172313	1863.781334	19.139226
47.733487	1855.642414	19.144243
47.024939	1859.701692	19.149261
47.318540	1850.001429	19.154279
47.445440	1851.938350	19.159296
48.038511	1868.850231	19.164314
48.419336	1847.623069	19.169331
48.375689	1843.198892	19.174349
48.470469	1831.235351	19.179367
48.692465	1835.871561	19.184384
48.331865	1832.093536	19.189402
48.132860	1808.268325	19.194419
48.155886	1804.297647	19.199437
47.885298	1800.969462	19.204455
48.191634	1801.981952	19.209472
47.659803	1803.485551	19.214490
48.042810	1803.583404	19.219507
48.246921	1820.654018	19.224525
48.437017	1827.861078	19.229543
48.304082	1836.097124	19.234560
48.367481	1839.369528	19.239578
49.029425	1827.938867	19.244595
48.222337	1824.192926	19.249613
48.039180	1809.987978	19.254631
48.149192	1822.367695	19.259648
48.298312	1836.597041	19.264666
48.182172	1829.227020	19.269683
47.698301	1832.219068	19.274701
48.463144	1835.062811	19.279719
48.722168	1832.437495	19.284736
47.932580	1851.279717	19.289754
48.571758	1844.703444	19.294771
48.137797	1859.409200	19.299789
48.459815	1859.030579	19.304807
48.741256	1864.664260	19.309824
48.393992	1880.454752	19.314842
48.797079	1876.576002	19.319859
48.588143	1880.746370	19.324877
48.719879	1883.288497	19.329895
49.094753	1890.665463	19.334912
48.939488	1900.101178	19.339930
49.479765	1902.935932	19.344947
49.430522	1897.714138	19.349965
49.369938	1907.466407	19.354983
49.152952	1902.902103	19.360000
49.203437	1904.387063	19.365018
49.412136	1899.866526	19.370035
49.241491	1906.022365	19.375053
49.071050	1906.203776	19.380071
49.755451	1917.729801	19.385088
50.074595	1929.953740	19.390106
50.037868	1926.459493	19.395123
49.892606	1927.877287	19.400141
49.865603	1931.053410	19.405159
49.865487	1926.698137	19.410176
50.078123	1936.997796	19.415194
50.110044	1927.013418	19.420211
50.101092	1932.623184	19.425229
49.968328	1928.740009	19.430247
50.328200	1932.941199	19.435264
49.797224	1935.508265	19.440282
50.308369	1923.823437	19.445299
50.549968	1935.500909	19.450317
50.500672	1925.459823	19.455335
50.802088	1932.895656	19.460352
50.610053	1927.450053	19.465370
50.511475	1919.420785	19.470387
50.429116	1928.191790	19.475405
50.399009	1921.947585	19.480423
50.534807	1928.143790	19.485440
50.586239	1943.149135	19.490458
50.720822	1940.215071	19.495475
50.537919	1952.473500	19.500493
50.199023	1954.092060	19.505511
50.328872	1957.199428	19.510528
50.599840	1964.943027	19.515546
50.672785	1974.816434	19.520563
50.994704	1981.924002	19.525581
51.027333	1979.087963	19.530599
51.166183	1977.040078	19.535616
51.262276	1976.797846	19.540634
51.205544	1978.630997	19.545651
51.223652	1969.939588	19.550669
51.219943	1977.694667	19.555687
51.580967	1969.748014	19.560704
51.720586	1977.938266	19.565722
51.566435	1975.080995	19.570739
51.263303	1974.958121	19.575757
51.644987	1983.495489	19.580775
51.985754	1989.946802	19.585792
51.932537	2005.088525	19.590810
51.952048	1984.173454	19.595827
52.030110	1971.824243	19.600845
51.757090	1975.916303	19.605863
52.001581	1973.678284	19.610880
52.006182	1974.018477	19.615898
51.834269	1981.206572	19.620915
52.071360	1998.051263	19.625933
52.263267	1995.007215	19.630951
52.723629	1990.702867	19.635968
52.489239	1999.529286	19.640986
52.739581	1984.091693	19.646003
52.532753	1964.127364	19.651021
52.284437	1966.766921	19.656039
52.483122	1960.657285	19.661056
52.313116	1958.465272	19.666074
52.459189	1966.165319	19.671091
52.514764	1982.306229	19.676109
52.395102	1983.044619	19.681127
52.884168	1988.128215	19.686144
52.689908	1989.269644	19.691162
52.633378	1985.775332	19.696179
52.920784	1981.845251	19.701197
52.713776	1988.786363	19.706215
52.569232	1978.488749	19.711232
52.225921	1987.430066	19.716250
52.729862	2002.796944	19.721267
52.529779	2005.952857	19.726285
52.852910	2018.990497	19.731303
52.927028	2010.249264	19.736320
52.809896	2026.906463	19.741338
53.169777	2028.532323	19.746355
53.565604	2025.920262	19.751373
53.214666	2039.407539	19.756391
53.176852	2043.437515	19.761408
53.111795	2050.359566	19.766426
53.409534	2037.325742	19.771443
53.252462	2046.515643	19.776461
53.263000	2059.816901	19.781479
53.684273	2054.909540	19.786496
53.595190	2065.565841	19.791514
53.696880	2068.904877	19.796531
54.014632	2054.810619	19.801549
53.831949	2070.263040	19.806567
53.833737	2067.665369	19.811584
54.258607	2081.258364	19.816602
54.286303	2084.220799	19.821619
54.403779	2091.742327	19.826637
54.365183	2094.339576	19.831655
54.580386	2081.959335	19.836672
54.423562	2083.158027	19.841690
54.576557	2075.303887	19.846707
54.648570	2069.488638	19.851725
54.610189	2077.650015	19.856743
54.660872	2080.883426	19.861760
54.576847	2083.778151	19.866778
54.489999	2079.045076	19.871795
54.534204	2082.816035	19.876813
54.626543	2082.164100	19.881831
54.886209	2073.990264	19.886848
54.704549	2075.404303	19.891866
54.553858	2087.029717	19.896883
55.148795	2079.058992	19.901901
54.421572	2075.884358	19.906919
55.401003	2085.710484	19.911936
55.032090	2106.238685	19.916954
55.139268	2114.446706	19.921971
54.990249	2103.458539	19.926989
55.320408	2115.510451	19.932007
55.291929	2104.509710	19.937024
55.412984	2109.155494	19.942042
55.288553	2105.725450	19.947059
55.727743	2097.321487	19.952077
55.736544	2092.046357	19.957095
55.918989	2094.874085	19.962112
55.769246	2091.757306	19.967130
55.563046	2085.944613	19.972147
56.210877	2084.590210	19.977165
56.070964	2087.503159	19.982183
56.148176	2094.197792	19.987200
56.123312	2089.884230	19.992218
55.995047	2091.981086	19.997235
56.090474	2083.656238	20.002253
56.155676	2087.824731	20.007271
55.956984	2081.124004	20.012288
56.328135	2095.760621	20.017306
56.331488	2093.459373	20.022323
56.216720	2092.540058	20.027341
56.408550	2093.939767	20.032359
56.249863	2104.641714	20.037376
56.640381	2109.661882	20.042394
56.753218	2111.477948	20.047411
56.768852	2112.659090	20.052429
56.437027	2112.531242	20.057447
56.895176	2113.529434	20.062464
56.631096	2116.212511	20.067482
57.003771	2124.378940	20.072499
57.188571	2113.079667	20.077517
56.744615	2109.844864	20.082535
56.627290	2116.822471	20.087552
57.045473	2108.690061	20.092570
56.991045	2109.765405	20.097587
56.879875	2112.355091	20.102605
56.979507	2127.520311	20.107623
57.259445	2136.184156	20.112640
57.068159	2126.231482	20.117658
57.080355	2144.351888	20.122675
57.241192	2140.943421	20.127693
57.041381	2147.612043	20.132711
57.213672	2145.915537	20.137728
57.693768	2157.189680	20.142746
57.726057	2160.173500	20.147763
58.148359	2156.440017	20.152781
57.935379	2159.471733	20.157799
57.629529	2161.340777	20.162816
58.113310	2150.045135	20.167834
57.817213	2156.814060	20.172851
57.856035	2160.434388	20.177869
57.807292	2147.997616	20.182887
58.151931	2159.359262	20.187904
58.104439	2174.392923	20.192922
58.344006	2182.233063	20.197939
58.671994	2173.373073	20.202957
58.925809	2177.767680	20.207975
59.131662	2161.831930	20.212992
58.616485	2155.231258	20.218010
58.554445	2153.760832	20.223027
58.834029	2144.725386	20.228045
58.704926	2144.426908	20.233063
58.581643	2151.115102	20.238080
58.921908	2150.244423	20.243098
58.369146	2170.643698	20.248115
58.819345	2159.290190	20.253133
59.039123	2168.601007	20.258151
58.800649	2177.658548	20.263168
58.916628	2174.904103	20.268186
58.980247	2180.742440	20.273203
59.146974	2172.620993	20.278221
59.226014	2185.299330	20.283239
59.188126	2185.835550	20.288256
59.475986	2188.296451	20.293274
59.309092	2195.496469	20.298291
59.613101	2193.062888	20.303309
59.714291	2201.262419	20.308327
59.638876	2198.279157	20.313344
59.612246	2194.069997	20.318362
59.755772	2206.233269	20.323379
59.881860	2195.252441	20.328397
60.130637	2190.242669	20.333415
59.771972	2191.757040	20.338432
59.786376	2187.263717	20.343450
59.688325	2193.370407	20.348467
59.679833	2193.564320	20.353485
59.833888	2196.229239	20.358503
59.957230	2209.367754	20.363520
59.982475	2220.444933	20.368538
59.883706	2221.779718	20.373555
60.014892	2214.304511	20.378573
60.339519	2217.952661	20.383591
59.973940	2227.727640	20.388608
60.350033	2240.845515	20.393626
60.572033	2254.707135	20.398643
60.764390	2243.930510	20.403661
60.797224	2239.402725	20.408679
60.697967	2242.138900	20.413696
60.962782	2234.601718	20.418714
60.831616	2248.916335	20.423731
60.648985	2253.975845	20.428749
60.950897	2249.961375	20.433767
61.036966	2256.288572	20.438784
61.345568	2260.731425	20.443802
61.133329	2277.690964	20.448819
61.270027	2274.822793	20.453837
61.241792	2277.248015	20.458855
61.495734	2262.769078	20.463872
61.686165	2265.264190	20.468890
61.622578	2263.459449	20.473907
61.643934	2266.688020	20.478925
61.656426	2265.590953	20.483943
61.708294	2266.671744	20.488960
62.085444	2264.621208	20.493978
61.935793	2260.453400	20.498995
62.005417	2269.484809	20.504013
62.079564	2255.125575	20.509031
61.878665	2272.095955	20.514048
62.055031	2262.044574	20.519066
62.067644	2264.987309	20.524083
62.130456	2263.235355	20.529101
62.132836	2284.289467	20.534119
61.877703	2287.050070	20.539136
62.751381	2285.792826	20.544154
62.135558	2290.345804	20.549171
62.306516	2283.830107	20.554189
62.217491	2286.870829	20.559207
62.311173	2289.321137	20.564224
62.717219	2296.494552	20.569242
62.230950	2312.988923	20.574259
62.850550	2314.615148	20.579277
62.828720	2316.862629	20.584295
62.792909	2310.032145	20.589312
62.921121	2311.508118	20.594330
62.930034	2319.924152	20.599347
62.876476	2316.044263	20.604365
63.061195	2325.256503	20.609383
63.412645	2336.288957	20.614400
63.615945	2331.463014	20.619418
63.409272	2337.713017	20.624435
63.438192	2327.526894	20.629453
63.623729	2336.388682	20.634471
63.418903	2334.019024	20.639488
63.813856	2329.128337	20.644506
63.279853	2332.964691	20.649523
63.403199	2330.467870	20.654541
63.505663	2328.416177	20.659559
63.400358	2329.543691	20.664576
63.913714	2347.551065	20.669594
63.498817	2355.534849	20.674611
64.073779	2356.953455	20.679629
63.904580	2350.557307	20.684647
63.892460	2361.858200	20.689664
64.054688	2359.746642	20.694682
63.803491	2364.264604	20.699699
64.394384	2379.211042	20.704717
64.880606	2381.694545	20.709735
64.762376	2381.053497	20.714752
65.092800	2379.761429	20.719770
64.799673	2380.782659	20.724787
65.116622	2377.965134	20.729805
64.978967	2362.647973	20.734823
64.965091	2350.697955	20.739840
65.050045	2348.768936	20.744858
64.664689	2349.264917	20.749875
64.367400	2361.181747	20.754893
65.145997	2373.046796	20.759911
65.540936	2377.826483	20.764928
65.387383	2371.822392	20.769946
65.107303	2369.871660	20.774963
65.318066	2368.109140	20.779981
65.386404	2365.797675	20.784999
65.379733	2372.196254	20.790016
65.750136	2365.242139	20.795034
65.485561	2366.965868	20.800051
65.502735	2371.706899	20.805069
65.819612	2383.808414	20.810087
65.522389	2389.166812	20.815104
65.844954	2391.391906	20.820122
65.696847	2387.984454	20.825139
65.648776	2397.536192	20.830157
66.053594	2395.405559	20.835175
66.006781	2394.949002	20.840192
65.777115	2397.721413	20.845210
66.261128	2417.475641	20.850227
66.081468	2417.866805	20.855245
66.660739	2419.672946	20.860263
66.199344	2426.650926	20.865280
66.647582	2425.037406	20.870298
66.274590	2428.630781	20.875315
66.461525	2421.001570	20.880333
66.645072	2430.851588	20.885351
66.843450	2443.798618	20.890368
66.926297	2442.444338	20.895386
66.931080	2442.850791	20.900403
67.151961	2439.268741	20.905421
66.836680	2443.269687	20.910439
66.789429	2454.393085	20.915456
67.107393	2442.059620	20.920474
66.974519	2439.871199	20.925491
67.130724	2449.810727	20.930509
67.743992	2455.354731	20.935527
67.457112	2471.922160	20.940544
68.030533	2471.949157	20.945562
67.681876	2463.053012	20.950579
67.579916	2461.768715	20.955597
68.089362	2468.348425	20.960615
67.672096	2470.133960	20.965632
68.007934	2458.665623	20.970650
67.912149	2460.448131	20.975667
68.017576	2468.744961	20.980685
68.143883	2461.191512	20.985703
67.866983	2462.936118	20.990720
68.036138	2467.959509	20.995738
68.011640	2459.268226	21.000755
67.975793	2465.141176	21.005773
68.373225	2459.805049	21.010791
68.246577	2470.000366	21.015808
68.480541	2470.658122	21.020826
68.754745	2475.835488	21.025843
68.463553	2478.330342	21.030861
68.649847	2474.340248	21.035879
68.820930	2489.425144	21.040896
68.831404	2485.087013	21.045914
69.044682	2484.296182	21.050931
68.823689	2472.713085	21.055949
68.894491	2483.032124	21.060967
68.895950	2472.957531	21.065984
69.161727	2486.427422	21.071002
69.327682	2486.291015	21.076019
69.108062	2506.004087	21.081037
69.322424	2498.765066	21.086055
69.337141	2505.636920	21.091072
69.501418	2505.002104	21.096090
69.475502	2505.785794	21.101107
69.326915	2500.977065	21.106125
69.713392	2507.493995	21.111143
69.535538	2519.897202	21.116160
69.347424	2523.916115	21.121178
69.793262	2522.833197	21.126195
69.763415	2525.482793	21.131213
70.161351	2523.858209	21.136231
70.073789	2527.176483	21.141248
70.233379	2533.776313	21.146266
70.445232	2537.767283	21.151283
70.432362	2539.006574	21.156301
70.802915	2544.831658	21.161319
70.468289	2548.971373	21.166336
70.641552	2549.638642	21.171354
70.840070	2538.119178	21.176371
70.818389	2540.281448	21.181389
70.609944	2540.639250	21.186407
70.735078	2546.565909	21.191424
70.529784	2538.480491	21.196442
70.709515	2534.990086	21.201459
70.987977	2557.352098	21.206477
71.315987	2559.409084	21.211495
71.325739	2575.141092	21.216512
71.311840	2574.158606	21.221530
71.485187	2563.738259	21.226547
71.047878	2565.340729	21.231565
71.355940	2567.258814	21.236583
71.292270	2567.111041	21.241600
71.431448	2571.930851	21.246618
71.682629	2579.485290	21.251635
71.638329	2585.346980	21.256653
71.745947	2588.625217	21.261671
71.796556	2595.226364	21.266688
71.561693	2595.960734	21.271706
71.857823	2594.765552	21.276723
71.852059	2605.986698	21.281741
71.990510	2612.047008	21.286759
72.074934	2623.601213	21.291776
71.977481	2614.583575	21.296794
72.272823	2620.530934	21.301811
71.934652	2617.197403	21.306829
72.553459	2635.889216	21.311847
72.348444	2637.733041	21.316864
72.668884	2637.594524	21.321882
72.911038	2630.445781	21.326899
72.808493	2630.755431	21.331917
72.951064	2626.219825	21.336935
73.091456	2626.472476	21.341952
72.973456	2630.499365	21.346970
73.048188	2628.464608	21.351987
73.310086	2622.941361	21.357005
73.488310	2619.255493	21.362023
73.283035	2614.338836	21.367040
73.399938	2624.313024	21.372058
74.082283	2624.278770	21.377075
73.607990	2631.965832	21.382093
73.905401	2628.428566	21.387111
73.766667	2623.820255	21.392128
73.753674	2637.296060	21.397146
74.110851	2636.271214	21.402163
74.114231	2643.122803	21.407181
74.267163	2632.213251	21.412199
74.269525	2636.817801	21.417216
74.271801	2639.026828	21.422234
74.551867	2631.212504	21.427251
73.920179	2639.157786	21.432269
74.508855	2633.763240	21.437287
74.436189	2638.546823	21.442304
74.482808	2638.782604	21.447322
74.508109	2634.123341	21.452339
74.516518	2631.988509	21.457357
74.452751	2628.179588	21.462375
74.715789	2647.141773	21.467392
75.064648	2662.328364	21.472410
75.073694	2653.565452	21.477427
74.834466	2652.744512	21.482445
74.969798	2656.053138	21.487463
74.980269	2652.791224	21.492480
74.958070	2657.273380	21.497498
74.993635	2663.346671	21.502515
75.635603	2673.418524	21.507533
75.464352	2668.752172	21.512551
75.403008	2685.574830	21.517568
75.392241	2681.110576	21.522586
75.768222	2680.808703	21.527603
75.880275	2682.931100	21.532621
75.905052	2681.459652	21.537639
75.521400	2688.996822	21.542656
75.663141	2698.973471	21.547674
75.743740	2704.477919	21.552691
75.600544	2711.573432	21.557709
75.981467	2708.884706	21.562727
76.315478	2725.721208	21.567744
76.787921	2737.195756	21.572762
76.859970	2735.606431	21.577779
76.791174	2740.140095	21.582797
76.964414	2726.945376	21.587815
77.283300	2720.081259	21.592832
77.070414	2728.020931	21.597850
77.297745	2697.644927	21.602867
77.356722	2702.928672	21.607885
76.992874	2701.041526	21.612903
77.253785	2702.212684	21.617920
76.910273	2714.253767	21.622938
76.943340	2713.118731	21.627955
77.013495	2726.237551	21.632973
77.067050	2732.730976	21.637991
77.435282	2727.380410	21.643008
77.147970	2726.582780	21.648026
77.594771	2738.812521	21.653043
77.549195	2756.431292	21.658061
77.830206	2749.948684	21.663079
77.587313	2764.801988	21.668096
77.566460	2759.524996	21.673114
77.750661	2760.594553	21.678131
77.936020	2761.490338	21.683149
77.894827	2763.491569	21.688167
78.071321	2774.409675	21.693184
78.155262	2769.592848	21.698202
78.134230	2778.591373	21.703219
78.422936	2783.056411	21.708237
78.092211	2782.366580	21.713255
78.148558	2778.352593	21.718272
78.169492	2799.985141	21.723290
78.570184	2810.653522	21.728307
78.626501	2806.914123	21.733325
78.712384	2809.561408	21.738343
79.112592	2808.996930	21.743360
78.997237	2832.134287	21.748378
79.532512	2828.228313	21.753395
79.480585	2831.354844	21.758413
79.124742	2828.437505	21.763431
79.300074	2825.623163	21.768448
79.470591	2825.801661	21.773466
79.584721	2825.913244	21.778483
79.525792	2829.555333	21.783501
79.832010	2825.123442	21.788519
80.028764	2828.712848	21.793536
79.772098	2830.637378	21.798554
79.929432	2822.709640	21.803571
80.150753	2837.761707	21.808589
80.181350	2847.348702	21.813607
80.468851	2853.802361	21.818624
80.335432	2862.963722	21.823642
80.563034	2854.535748	21.828659
80.761693	2853.030731	21.833677
80.454330	2852.501359	21.838695
80.764859	2852.298113	21.843712
80.627861	2858.553160	21.848730
80.988710	2852.992247	21.853747
80.941649	2848.956571	21.858765
80.700778	2846.482023	21.863783
80.936123	2847.833944	21.868800
80.712223	2854.670724	21.873818
81.228832	2865.620816	21.878835
80.985893	2871.993464	21.883853
81.111891	2879.633924	21.888871
80.970172	2876.058099	21.893888
81.267763	2867.259345	21.898906
81.676646	2876.761838	21.903923
81.782829	2891.914051	21.908941
81.969730	2893.589188	21.913959
82.038511	2895.112395	21.918976
81.667027	2899.273744	21.923994
81.703512	2889.376491	21.929011
81.701996	2892.103763	21.934029
81.920825	2886.448311	21.939047
82.134200	2899.197634	21.944064
82.270029	2912.656642	21.949082
82.425361	2920.513459	21.954099
81.959629	2924.954703	21.959117
82.034262	2926.981992	21.964135
82.375320	2916.042795	21.969152
82.381076	2937.412764	21.974170
82.605523	2944.933671	21.979187
82.980869	2941.434634	21.984205
82.764671	2946.780501	21.989223
82.875071	2943.651222	21.994240
83.113864	2943.680150	21.999258
83.294238	2941.922337	22.004275
83.117359	2936.934861	22.009293
83.193267	2941.550060	22.014311
83.414934	2947.351259	22.019328
83.296981	2966.689095	22.024346
83.307858	2962.615910	22.029363
83.588052	2954.785646	22.034381
83.694381	2957.656999	22.039399
84.176369	2954.359032	22.044416
84.201180	2964.171087	22.049434
84.230301	2963.437495	22.054451
84.103744	2955.229085	22.059469
84.050415	2956.660960	22.064487
84.212091	2958.254837	22.069504
84.238756	2977.850932	22.074522
84.272978	2980.831429	22.079539
84.444198	2980.255478	22.084557
84.220455	2973.921309	22.089575
84.885445	2978.267475	22.094592
84.460514	2975.184187	22.099610
85.050788	2979.718809	22.104627
85.200810	3000.554939	22.109645
84.834374	3004.456710	22.114663
84.941560	2996.195879	22.119680
85.136065	3005.791996	22.124698
85.296061	3001.114691	22.129715
85.768387	2997.448950	22.134733
85.610264	2991.558993	22.139751
85.774076	2994.238284	22.144768
85.602950	2993.583407	22.149786
85.470125	2999.623225	22.154803
85.849296	2988.056233	22.159821
85.539759	2993.571393	22.164839
86.039441	3000.717798	22.169856
86.013622	3019.501538	22.174874
86.050795	3016.582562	22.179891
86.266730	3012.227896	22.184909
86.129772	3016.469309	22.189927
86.362663	3008.823182	22.194944
86.424096	3018.623217	22.199962
86.824951	3035.853536	22.204979
86.527359	3040.814496	22.209997
86.398790	3036.627423	22.215015
86.584539	3036.118631	22.220032
86.470701	3041.224395	22.225050
86.635668	3045.664699	22.230067
86.969976	3052.095315	22.235085
87.019990	3061.180694	22.240103
87.108926	3062.012695	22.245120
87.183298	3064.993229	22.250138
87.060127	3072.278277	22.255155
87.248772	3082.250947	22.260173
87.154704	3097.280050	22.265191
87.607508	3091.341688	22.270208
87.631208	3096.953014	22.275226
87.580946	3095.461727	22.280243
88.181428	3107.437236	22.285261
87.679505	3118.067307	22.290279
88.063721	3116.334353	22.295296
88.061082	3117.666768	22.300314
88.251512	3115.291892	22.305331
88.250694	3115.765519	22.310349
88.312675	3123.614957	22.315367
88.318845	3129.169070	22.320384
88.684597	3143.166667	22.325402
88.533738	3144.800057	22.330419
88.903802	3145.035671	22.335437
88.957267	3144.007881	22.340455
89.186436	3133.748898	22.345472
89.515091	3142.074190	22.350490
89.600159	3141.865234	22.355507
89.962279	3131.654860	22.360525
89.573357	3140.468172	22.365543
89.419115	3133.662243	22.370560
89.899451	3140.549765	22.375578
89.886675	3139.671229	22.380595
90.078701	3129.825225	22.385613
89.696863	3137.318108	22.390631
89.983119	3127.233248	22.395648
89.805480	3126.749824	22.400666
89.801482	3127.801546	22.405683
89.812804	3126.480515	22.410701
89.842935	3146.638064	22.415719
90.208285	3149.882337	22.420736
90.296014	3150.348405	22.425754
90.383345	3163.600572	22.430771
90.672849	3161.582607	22.435789
90.354610	3160.717209	22.440807
90.292830	3172.408298	22.445824
90.608410	3179.050208	22.450842
90.779076	3183.233995	22.455859
91.001030	3183.126686	22.460877
90.725476	3193.462522	22.465895
90.981281	3204.239056	22.470912
91.077602	3202.939421	22.475930
91.174339	3210.227947	22.480947
91.368191	3204.229118	22.485965
91.301138	3209.763166	22.490983
91.624316	3217.486502	22.496000
91.552432	3229.687372	22.501018
91.704123	3236.061446	22.506035
92.202886	3226.018988	22.511053
91.917882	3222.490793	22.516071
91.916663	3231.473814	22.521088
92.511450	3234.524343	22.526106
92.600869	3243.389012	22.531123
92.909261	3241.289173	22.536141
92.689224	3244.868211	22.541159
92.967921	3248.195516	22.546176
92.934703	3241.948185	22.551194
92.893903	3242.942554	22.556211
93.453854	3232.802130	22.561229
93.127311	3240.826115	22.566247
92.902710	3242.827728	22.571264
93.218093	3235.095987	22.576282
92.992537	3238.363417	22.581299
93.342791	3241.834168	22.586317
93.142067	3232.911307	22.591335
93.261245	3246.925522	22.596352
93.408068	3251.476033	22.601370
93.337572	3255.116864	22.606387
93.596200	3256.828142	22.611405
93.768505	3261.592447	22.616423
93.757218	3283.647253	22.621440
93.695574	3277.719992	22.626458
93.552965	3291.967790	22.631475
94.105728	3290.637669	22.636493
94.572578	3296.040751	22.641511
94.399295	3302.898175	22.646528
94.584552	3324.373043	22.651546
94.563631	3320.939175	22.656563
94.839850	3318.737053	22.661581
94.430241	3317.298891	22.666599
94.627345	3317.220725	22.671616
94.624700	3319.206509	22.676634
94.936504	3335.983936	22.681651
95.137752	3330.189066	22.686669
95.119297	3342.810898	22.691687
95.238343	3346.813432	22.696704
95.535720	3338.484772	22.701722
95.660194	3349.619693	22.706739
95.576837	3338.080757	22.711757
95.642363	3354.476998	22.716775
95.689735	3362.212045	22.721792
95.918161	3360.737043	22.726810
95.682053	3357.693543	22.731827
96.126073	3350.730676	22.736845
96.126958	3360.433068	22.741863
96.136558	3371.977382	22.746880
96.053950	3381.209951	22.751898
96.273112	3392.052309	22.756915
96.460578	3381.275773	22.761933
96.738550	3380.067605	22.766951
96.408535	3381.321922	22.771968
96.926678	3397.855606	22.776986
96.886813	3410.897472	22.782003
97.286350	3406.608636	22.787021
97.045431	3419.394783	22.792039
97.216885	3411.092131	22.797056
97.605138	3404.961778	22.802074
97.222653	3427.210636	22.807091
97.452082	3440.434431	22.812109
97.866824	3439.144862	22.817127
98.072045	3434.403547	22.822144
98.462253	3429.292368	22.827162
98.768709	3425.513652	22.832179
98.994181	3419.033196	22.837197
98.885396	3402.883673	22.842215
99.072510	3401.595050	22.847232
98.978711	3382.457328	22.852250
98.640485	3388.131761	22.857267
99.364003	3375.311178	22.862285
99.195698	3381.198866	22.867303
99.063667	3378.565158	22.872320
99.211251	3376.676719	22.877338
98.923850	3370.424978	22.882355
99.270226	3368.824182	22.887373
99.183404	3374.490786	22.892391
98.957152	3381.277630	22.897408
99.440286	3381.116777	22.902426
99.352740	3400.866945	22.907443
99.405576	3405.170247	22.912461
99.480461	3394.285089	22.917479
99.441690	3401.497076	22.922496
99.377984	3405.900701	22.927514
99.402208	3420.103524	22.932531
99.390481	3426.335984	22.937549
99.558550	3433.799647	22.942567
99.785440	3455.962538	22.947584
100.224450	3454.972173	22.952602
100.170463	3454.712404	22.957619
100.019362	3467.304603	22.962637
100.409470	3477.176489	22.967655
100.546884	3481.283491	22.972672
100.934015	3490.044825	22.977690
100.584817	3492.817190	22.982707
100.618613	3501.154126	22.987725
101.165077	3518.886045	22.992743
101.183543	3514.199219	22.997760
100.926334	3505.161975	23.002778
101.122289	3518.959211	23.007795
101.588308	3528.626697	23.012813
101.641473	3533.558087	23.017831
101.466681	3540.851411	23.022848
101.550582	3538.704644	23.027866
101.623794	3534.593157	23.032883
101.835858	3548.722464	23.037901
101.911517	3553.423079	23.042919
101.841355	3569.237913	23.047936
102.136533	3569.396889	23.052954
101.993617	3569.255210	23.057971
102.330250	3581.370220	23.062989
102.729193	3585.575150	23.068007
102.845193	3587.757007	23.073024
103.160960	3597.277627	23.078042
103.010540	3591.799747	23.083059
102.988019	3592.851241	23.088077
103.343454	3586.422959	23.093095
103.393437	3586.371000	23.098112
103.590663	3573.859988	23.103130
103.814405	3578.344874	23.108147
103.836176	3575.825919	23.113165
103.980911	3584.783093	23.118183
103.971581	3599.710960	23.123200
104.114125	3596.560751	23.128218
104.110173	3598.805590	23.133235
104.069890	3595.333671	23.138253
104.443852	3591.045642	23.143271
104.166681	3595.369128	23.148288
104.195131	3589.986322	23.153306
104.296286	3592.735490	23.158323
104.481923	3601.907208	23.163341
104.711998	3610.216599	23.168359
104.511182	3616.444029	23.173376
104.716330	3611.219758	23.178394
104.513243	3620.061000	23.183411
104.865810	3626.870881	23.188429
105.220326	3639.633336	23.193447
105.364631	3642.814484	23.198464
105.072648	3643.138048	23.203482
105.329572	3658.570298	23.208499
105.008920	3661.410812	23.213517
105.563984	3664.540236	23.218535
105.112732	3677.599401	23.223552
105.599439	3691.739449	23.228570
105.490512	3698.138736	23.233587
105.532439	3706.061008	23.238605
106.393243	3718.741043	23.243623
106.066297	3727.099879	23.248640
106.246849	3723.530210	23.253658
106.380379	3737.340549	23.258675
106.138030	3753.820107	23.263693
106.190933	3750.712322	23.268711
106.600593	3755.341724	23.273728
107.050133	3769.298273	23.278746
107.505818	3778.462493	23.283763
107.424832	3771.808977	23.288781
107.136120	3776.506766	23.293799
107.201770	3782.383180	23.298816
107.565698	3778.901556	23.303834
107.992924	3797.444681	23.308851
108.167148	3811.460179	23.313869
108.158808	3808.346197	23.318887
108.005637	3803.651467	23.323904
107.852313	3807.185442	23.328922
107.971010	3806.977523	23.333939
108.045057	3798.418506	23.338957
108.251412	3817.769569	23.343975
108.285571	3837.804158	23.348992
108.530080	3828.391448	23.354010
108.694544	3823.167178	23.359027
108.536572	3831.070321	23.364045
108.636027	3829.729118	23.369063
108.723672	3847.081880	23.374080
109.161945	3862.811000	23.379098
109.244880	3859.818435	23.384115
109.280459	3853.241319	23.389133
109.585752	3850.324392	23.394151
109.608547	3848.973103	23.399168
109.371159	3871.796331	23.404186
109.634059	3877.856508	23.409203
109.597897	3889.698709	23.414221
109.767064	3876.355442	23.419239
110.022040	3886.485453	23.424256
110.407176	3898.419475	23.429274
110.377953	3906.447674	23.434291
110.227936	3904.649996	23.439309
110.113122	3901.615808	23.444327
110.259859	3907.650005	23.449344
110.445120	3931.290882	23.454362
110.593179	3930.181943	23.459379
110.647565	3935.034342	23.464397
111.077641	3938.896743	23.469415
110.979942	3953.456821	23.474432
110.997328	3957.140839	23.479450
111.075965	3957.605196	23.484467
111.545786	3981.990659	23.489485
111.602192	3984.301844	23.494503
111.850463	3985.361438	23.499520
111.876998	3988.093950	23.504538
111.910173	3986.968286	23.509555
111.940069	3997.326164	23.514573
112.341708	3997.250674	23.519591
112.724982	3997.070742	23.524608
112.775422	3997.179687	23.529626
112.877226	4003.565005	23.534643
112.780900	4006.383052	23.539661
112.554697	4000.834854	23.544679
112.480127	3998.690766	23.549696
113.047110	4019.784701	23.554714
113.167254	4020.971689	23.559731
112.960639	4021.218756	23.564749
113.264307	4023.061934	23.569767
113.124802	4027.648031	23.574784
113.487378	4042.738945	23.579802
113.408007	4044.840991	23.584819
113.299794	4054.942775	23.589837
113.810098	4059.193499	23.594855
113.584508	4073.404408	23.599872
114.328277	4076.087692	23.604890
114.434899	4067.270931	23.609907
114.485027	4075.286773	23.614925
114.482215	4081.890520	23.619943
114.596017	4096.834225	23.624960
114.736463	4094.681691	23.629978
114.784070	4088.680232	23.634995
114.743009	4099.396493	23.640013
114.602481	4113.092233	23.645031
114.533130	4120.852204	23.650048
114.821695	4128.707613	23.655066
115.167076	4138.148124	23.660083
115.132830	4150.438409	23.665101
115.599108	4147.022748	23.670119
115.379077	4158.890775	23.675136
115.756552	4178.458459	23.680154
116.195343	4179.904868	23.685171
116.131250	4189.355898	23.690189
116.299255	4175.990498	23.695207
116.459722	4179.844689	23.700224
116.627566	4168.729865	23.705242
116.705273	4166.561900	23.710259
116.540958	4176.858770	23.715277
116.826794	4190.178439	23.720295
117.022713	4193.159055	23.725312
117.148176	4190.566955	23.730330
117.352087	4183.988598	23.735347
117.363617	4187.821934	23.740365
117.404865	4191.754777	23.745383
117.441485	4190.808478	23.750400
117.349315	4190.235879	23.755418
117.644217	4205.129206	23.760435
117.652738	4215.834611	23.765453
117.628147	4216.952751	23.770471
117.959012	4221.386292	23.775488
117.975045	4233.558281	23.780506
118.315049	4234.489886	23.785523
118.061348	4244.305236	23.790541
117.676723	4241.199629	23.795559
118.424932	4262.233889	23.800576
118.268841	4274.069879	23.805594
118.534287	4272.920433	23.810611
118.740789	4285.791759	23.815629
119.072254	4301.664253	23.820647
119.208077	4299.127331	23.825664
118.899221	4303.815784	23.830682
119.593534	4313.148060	23.835699
119.515005	4328.339885	23.840717
119.618382	4324.520202	23.845735
119.885740	4334.755845	23.850752
119.938592	4328.330518	23.855770
120.056373	4336.181209	23.860787
120.134397	4349.015891	23.865805
120.276985	4354.580572	23.870823
120.668847	4347.537118	23.875840
120.429986	4358.076192	23.880858
120.586929	4362.344472	23.885875
120.552235	4376.386824	23.890893
120.994810	4379.710762	23.895911
121.045444	4382.862525	23.900928
120.955794	4376.819346	23.905946
121.625118	4373.608569	23.910963
121.726807	4384.091148	23.915981
121.763526	4382.305200	23.920999
122.211574	4382.184562	23.926016
122.345227	4395.985914	23.931034
122.659104	4387.294352	23.936051
122.226312	4388.627966	23.941069
122.113493	4378.163030	23.946087
122.668768	4379.682744	23.951104
122.312262	4388.854573	23.956122
122.760025	4382.452582	23.961139
122.357221	4391.915749	23.966157
122.420869	4392.811748	23.971175
122.526259	4404.243860	23.976192
122.377087	4401.808390	23.981210
122.861942	4422.524257	23.986227
123.024358	4443.906180	23.991245
123.136256	4444.892473	23.996263
123.316076	4453.314289	24.001280
123.235679	4467.954137	24.006298
123.574654	4470.962891	24.011315
123.530861	4460.581788	24.016333
123.530282	4484.135710	24.021351
124.103017	4493.149382	24.026368
123.922073	4498.142965	24.031386
124.366987	4496.589765	24.036403
124.135359	4503.791371	24.041421
124.160765	4518.209510	24.046439
124.798110	4521.796515	24.051456
124.565488	4526.485707	24.056474
124.877665	4526.982934	24.061491
124.686504	4535.702804	24.066509
124.943898	4549.819477	24.071527
125.337916	4544.906253	24.076544
125.395078	4542.501568	24.081562
125.690950	4541.773468	24.086579
126.229409	4551.887848	24.091597
126.591220	4558.494617	24.096615
126.706325	4520.516485	24.101632
126.631232	4524.546539	24.106650
126.930449	4518.631780	24.111667
126.800214	4512.153003	24.116685
126.911763	4517.482703	24.121703
126.907850	4515.150720	24.126720
126.916543	4516.519341	24.131738
126.894508	4517.021580	24.136755
126.961636	4527.452840	24.141773
127.019942	4539.037614	24.146791
127.395140	4529.367330	24.151808
127.359601	4539.742082	24.156826
127.501292	4534.476985	24.161843
127.669390	4540.435447	24.166861
127.576435	4558.770449	24.171879
127.837465	4556.842021	24.176896
127.655317	4570.232131	24.181914
128.024666	4554.701107	24.186931
127.770155	4577.032329	24.191949
127.621253	4588.397075	24.196967
127.993708	4603.919353	24.201984
128.170403	4614.743844	24.207002
128.356628	4626.854711	24.212019
128.282490	4634.328407	24.217037
128.739186	4646.497921	24.222055
128.707311	4650.615928	24.227072
128.698949	4668.104465	24.232090
128.838220	4677.533358	24.237107
129.102284	4665.468823	24.242125
129.351082	4701.288113	24.247143
129.565444	4701.674408	24.252160
129.652867	4708.785074	24.257178
129.908646	4729.357258	24.262195
130.044894	4738.837161	24.267213
129.879442	4737.035505	24.272231
130.325732	4735.971335	24.277248
130.733555	4760.014025	24.282266
130.536727	4755.426896	24.287283
131.033121	4760.816324	24.292301
130.684308	4759.283289	24.297319
131.042722	4759.634391	24.302336
131.030948	4775.381152	24.307354
131.743519	4772.059366	24.312371
131.886289	4772.567358	24.317389
131.730201	4774.309034	24.322407
131.797641	4774.696253	24.327424
131.780696	4774.440131	24.332442
131.839111	4794.377278	24.337459
132.245112	4793.155277	24.342477
132.335627	4797.724469	24.347495
132.413199	4802.693416	24.352512
132.225562	4807.135734	24.357530
132.348902	4827.012240	24.362547
132.545653	4822.578079	24.367565
132.713076	4830.967291	24.372583
132.685493	4839.563825	24.377600
132.947070	4856.688282	24.382618
133.224520	4849.346904	24.387635
133.391158	4845.813918	24.392653
133.472899	4855.510755	24.397671
133.755189	4869.333372	24.402688
133.480737	4880.771631	24.407706
133.643500	4886.273341	24.412723
134.185085	4884.184132	24.417741
134.016024	4896.448693	24.422759
134.078051	4909.163170	24.427776
134.064633	4911.277079	24.432794
133.979250	4911.893421	24.437811
134.294764	4930.590940	24.442829
134.470627	4938.379130	24.447847
134.500239	4949.100601	24.452864
134.731891	4967.179981	24.457882
134.822775	4968.014923	24.462899
134.916411	4984.764926	24.467917
135.009725	4993.162666	24.472935
135.504472	5005.509542	24.477952
135.519465	5015.055935	24.482970
135.593584	5023.077906	24.487987
135.830602	5037.924166	24.493005
135.864092	5053.739834	24.498023
135.865495	5045.914473	24.503040
136.181938	5061.262834	24.508058
136.544888	5076.124119	24.513075
137.138938	5074.285511	24.518093
136.950777	5067.771419	24.523111
137.284901	5074.534231	24.528128
137.041747	5086.122388	24.533146
137.505895	5089.427296	24.538163
138.081093	5088.245057	24.543181
137.864630	5083.073793	24.548199
138.142649	5074.396993	24.553216
138.171494	5088.366808	24.558234
138.292244	5092.227415	24.563251
138.272421	5093.442716	24.568269
138.161495	5113.656114	24.573287
138.203337	5103.987248	24.578304
138.794895	5110.570851	24.583322
138.872162	5110.798708	24.588339
139.138424	5126.281250	24.593357
138.986016	5133.716907	24.598375
139.365449	5145.608453	24.603392
139.318669	5142.907469	24.608410
139.151892	5143.312450	24.613427
139.464235	5149.093840	24.618445
139.809089	5164.390488	24.623463
139.494581	5168.751758	24.628480
139.979211	5172.441736	24.633498
139.824691	5175.534237	24.638515
140.682622	5181.204908	24.643533
140.357274	5193.320539	24.648551
140.855909	5186.354735	24.653568
140.680923	5184.112600	24.658586
140.593207	5198.384856	24.663603
140.779305	5210.559263	24.668621
140.915415	5226.756738	24.673639
140.998107	5217.422328	24.678656
141.011589	5232.133310	24.683674
140.942111	5242.270718	24.688691
141.466920	5241.004822	24.693709
141.533406	5265.796115	24.698727
141.735844	5269.069455	24.703744
141.922915	5276.518274	24.708762
142.174519	5291.122552	24.713779
142.520991	5309.190596	24.718797
142.725946	5305.932460	24.723815
142.629936	5298.665194	24.728832
142.499544	5306.829812	24.733850
142.575566	5310.836366	24.738867
142.892024	5316.323596	24.743885
143.119152	5324.195462	24.748903
142.973559	5325.064312	24.753920
143.248222	5346.887423	24.758938
143.399635	5351.330418	24.763955
143.689799	5349.864528	24.768973
143.700933	5358.562567	24.773991
143.804223	5365.437411	24.779008
144.208506	5379.695862	24.784026
144.212782	5391.614776	24.789043
144.379749	5387.655487	24.794061
144.342199	5409.758022	24.799079
144.730244	5403.803809	24.804096
144.628794	5404.631024	24.809114
144.516676	5418.654742	24.814131
145.194959	5428.962360	24.819149
144.876629	5434.094517	24.824167
145.213842	5450.128105	24.829184
145.486203	5462.854209	24.834202
145.720037	5471.028128	24.839219
146.156133	5464.292984	24.844237
146.361570	5482.569539	24.849255
146.302625	5484.703273	24.854272
146.593434	5479.171480	24.859290
146.546481	5483.667681	24.864307
147.166163	5481.389399	24.869325
146.905841	5481.023032	24.874343
146.732912	5491.148375	24.879360
146.853300	5499.387430	24.884378
146.908064	5513.142012	24.889395
147.265893	5518.367132	24.894413
147.146169	5545.457628	24.899431
147.220679	5541.354956	24.904448
147.606991	5554.943987	24.909466
147.837413	5570.801853	24.914483
147.904298	5563.957211	24.919501
147.901770	5591.840684	24.924519
148.078778	5595.222237	24.929536
148.244896	5603.678300	24.934554
148.110428	5611.846849	24.939571
148.510045	5610.610013	24.944589
148.792055	5629.537624	24.949607
149.156418	5638.193084	24.954624
149.172846	5642.515246	24.959642
149.279750	5656.520616	24.964659
149.673389	5665.531366	24.969677
149.800981	5673.930363	24.974695
149.739364	5675.407944	24.979712
150.110757	5688.216549	24.984730
149.973226	5695.867915	24.989747
150.364374	5698.511994	24.994765
150.613022	5701.487755	24.999783
150.566716	5724.608503	25.004800
150.552211	5723.752209	25.009818
150.507362	5736.461910	25.014835
150.760212	5743.884831	25.019853
150.697863	5750.255442	25.024871
151.024262	5779.369295	25.029888
151.729631	5776.035836	25.034906
151.398593	5791.997639	25.039923
151.731332	5798.366348	25.044941
151.960773	5806.774704	25.049959
152.123935	5810.439416	25.054976
152.092441	5802.221137	25.059994
152.083943	5819.123645	25.065011
152.382407	5819.076946	25.070029
152.693431	5824.969244	25.075047
152.990745	5832.151637	25.080064
153.255663	5843.291338	25.085082
153.362560	5855.816354	25.090099
153.526797	5857.760487	25.095117
153.706198	5855.510099	25.100135
153.579755	5851.906037	25.105152
153.586841	5860.775412	25.110170
153.606867	5878.465847	25.115187
154.006289	5871.644755	25.120205
153.968080	5888.422556	25.125223
154.001697	5915.129707	25.130240
154.457444	5911.971071	25.135258
154.439267	5916.532318	25.140275
154.505691	5924.107632	25.145293
154.813184	5940.282047	25.150311
154.511875	5955.039770	25.155328
154.963104	5962.419074	25.160346
154.870012	5980.360929	25.165363
155.274879	5994.572418	25.170381
155.206723	6008.267710	25.175399
155.391786	6024.685510	25.180416
155.831074	6022.107121	25.185434
156.328429	6038.343424	25.190451
156.708859	6037.602023	25.195469
157.076292	6037.364583	25.200487
156.883033	6053.216639	25.205504
157.369564	6043.982693	25.210522
156.980150	6056.080517	25.215539
157.088966	6061.985630	25.220557
157.430165	6071.591956	25.225575
157.326996	6071.772331	25.230592
157.582933	6075.611968	25.235610
157.772759	6098.787740	25.240627
158.183777	6096.636779	25.245645
158.039197	6113.235729	25.250663
158.127592	6125.069337	25.255680
158.464273	6125.935274	25.260698
158.632857	6138.043595	25.265715
158.891514	6142.874050	25.270733
159.131991	6146.362564	25.275751
158.850651	6146.444581	25.280768
159.031375	6159.766377	25.285786
159.420089	6183.378301	25.290803
159.503904	6177.812435	25.295821
159.699316	6188.963236	25.300839
159.741958	6206.833538	25.305856
159.896925	6206.338958	25.310874
159.932460	6224.071492	25.315891
160.040111	6233.383028	25.320909
160.200026	6237.771242	25.325927
160.667065	6252.970741	25.330944
160.913574	6258.324002	25.335962
160.981153	6267.237763	25.340979
161.100024	6273.172936	25.345997
161.294358	6286.268558	25.351015
161.363704	6291.005595	25.356032
161.862537	6298.532262	25.361050
161.851867	6318.494521	25.366067
162.189183	6320.673603	25.371085
162.903436	6303.723323	25.376103
162.879878	6300.194601	25.381120
162.862527	6301.172834	25.386138
163.013107	6311.169026	25.391155
163.504547	6317.639327	25.396173
163.767458	6316.543822	25.401191
164.057500	6319.238558	25.406208
164.160635	6295.170705	25.411226
164.485813	6292.288163	25.416243
164.383995	6280.333554	25.421261
164.634876	6278.880060	25.426279
164.402433	6289.542353	25.431296
164.575961	6273.996358	25.436314
164.546879	6277.871220	25.441331
164.307639	6284.563312	25.446349
164.407019	6292.427199	25.451367
164.553897	6317.112617	25.456384
164.732387	6304.710006	25.461402
164.872183	6323.853182	25.466419
164.946058	6334.527492	25.471437
164.995772	6334.617625	25.476455
164.973863	6360.134532	25.481472
165.282089	6366.093737	25.486490
165.514135	6389.888314	25.491507
165.409295	6396.616214	25.496525
165.798347	6403.086802	25.501543
166.042861	6423.795247	25.506560
165.784989	6433.688184	25.511578
166.243928	6455.262771	25.516595
166.045271	6463.470165	25.521613
166.590321	6473.912898	25.526631
166.307243	6494.157944	25.531648
166.980350	6510.689132	25.536666
167.181733	6525.122323	25.541683
167.111606	6542.110917	25.546701
167.629622	6553.501830	25.551719
167.958789	6569.215661	25.556736
167.802267	6570.910220	25.561754
167.786548	6592.830820	25.566771
168.315921	6599.077455	25.571789
168.299771	6613.292247	25.576807
168.338354	6626.005276	25.581824
168.661553	6640.375278	25.586842
169.352099	6654.605663	25.591859
169.052623	6653.225734	25.596877
169.463206	6669.561428	25.601895
169.428467	6688.176716	25.606912
169.787473	6698.415115	25.611930
170.067551	6716.343422	25.616947
169.972053	6713.807682	25.621965
170.446071	6733.735498	25.626983
170.346911	6741.094011	25.632000
170.955408	6745.917172	25.637018
170.793371	6762.494188	25.642035
170.941320	6776.907537	25.647053
171.526645	6774.094656	25.652071
171.438361	6801.257844	25.657088
171.582470	6792.721178	25.662106
171.649995	6798.964471	25.667123
171.512808	6811.253728	25.672141
172.085898	6814.706048	25.677159
171.744202	6842.060527	25.682176
172.821299	6844.770943	25.687194
173.287504	6849.919487	25.692212
172.948266	6854.786975	25.697229
173.299182	6859.154886	25.702247
173.354335	6879.217933	25.707264
173.598697	6865.977515	25.712282
173.690647	6878.211978	25.717300
173.879071	6873.807042	25.722317
174.041211	6882.980938	25.727335
173.995970	6898.605333	25.732352
174.149889	6895.730586	25.737370
174.482940	6902.412167	25.742388
174.366567	6919.556729	25.747405
174.702911	6922.440030	25.752423
174.768365	6923.187496	25.757440
174.864379	6938.006879	25.762458
175.301318	6945.571924	25.767476
175.563892	6950.752398	25.772493
175.557600	6952.104607	25.777511
175.433405	6962.826096	25.782528
175.753279	6968.875224	25.787546
176.043429	6967.320818	25.792564
176.179264	6992.261427	25.797581
176.412717	6996.559379	25.802599
176.356357	7013.214773	25.807616
176.739317	7029.984459	25.812634
177.056766	7038.960470	25.817652
176.905409	7038.450719	25.822669
177.514584	7050.528502	25.827687
177.356934	7060.462897	25.832704
177.896703	7050.898102	25.837722
178.338862	7061.745595	25.842740
178.376623	7070.752811	25.847757
178.479290	7068.842620	25.852775
178.681579	7075.705755	25.857792
178.991331	7074.587084	25.862810
179.009356	7069.937299	25.867828
179.142862	7092.684334	25.872845
179.352859	7090.987784	25.877863
179.258573	7098.658213	25.882880
179.442903	7108.021319	25.887898
179.841929	7115.166185	25.892916
179.862029	7124.573970	25.897933
179.954886	7123.006262	25.902951
180.016369	7145.196394	25.907968
179.904197	7153.718869	25.912986
180.440788	7162.092358	25.918004
180.399338	7177.631157	25.923021
180.840432	7193.621587	25.928039
181.077639	7204.990602	25.933056
181.202039	7201.609004	25.938074
181.510903	7216.628882	25.943092
181.767215	7236.278811	25.948109
181.794453	7230.983519	25.953127
181.641134	7249.387493	25.958144
182.280466	7260.952417	25.963162
182.840557	7255.115880	25.968180
182.550399	7275.334479	25.973197
182.677980	7289.157908	25.978215
183.157169	7288.953461	25.983232
182.856821	7304.270897	25.988250
183.302832	7307.225475	25.993268
183.186164	7325.162862	25.998285
183.357270	7327.990033	26.003303
183.563053	7350.798675	26.008320
183.493789	7369.476886	26.013338
183.730043	7366.263997	26.018356
183.980345	7384.443867	26.023373
184.302218	7395.948115	26.028391
184.497553	7421.659763	26.033408
184.483155	7426.154495	26.038426
184.797178	7435.579533	26.043444
185.183446	7453.482452	26.048461
185.588129	7452.550937	26.053479
186.242669	7466.288788	26.058496
185.922578	7465.167742	26.063514
186.038093	7464.565658	26.068532
186.382208	7482.367872	26.073549
186.676748	7490.274308	26.078567
186.796388	7502.845807	26.083584
186.904218	7501.117871	26.088602
187.283393	7496.149368	26.093620
186.936109	7521.346329	26.098637
187.271224	7524.160464	26.103655
187.493193	7523.816362	26.108672
187.605832	7544.392036	26.113690
187.830705	7545.313446	26.118708
187.954830	7559.626958	26.123725
188.487028	7566.978444	26.128743
188.302353	7579.098859	26.133760
188.352943	7585.373485	26.138778
188.664832	7604.437363	26.143796
188.508292	7616.202963	26.148813
188.765102	7625.880153	26.153831
189.131260	7640.954542	26.158848
188.759938	7658.303896	26.163866
189.483552	7668.245782	26.168884
189.639918	7684.066565	26.173901
189.808850	7703.250810	26.178919
189.923772	7713.477501	26.183936
190.202741	7728.114162	26.188954
190.601780	7734.422649	26.193972
190.910693	7754.731029	26.198989
190.883887	7752.332765	26.204007
191.561262	7770.572393	26.209024
191.725673	7773.735330	26.214042
191.970903	7776.585686	26.219060
191.639406	7786.901297	26.224077
192.120538	7801.708398	26.229095
192.442150	7808.407887	26.234112
192.434275	7812.497587	26.239130
192.835804	7826.259559	26.244148
192.825898	7838.052842	26.249165
193.012061	7843.775928	26.254183
193.100148	7860.115848	26.259200
193.111841	7865.989400	26.264218
193.655018	7879.261974	26.269236
193.492606	7898.694069	26.274253
194.080249	7904.452148	26.279271
193.962722	7922.810142	26.284288
194.012963	7929.788971	26.289306
194.609110	7947.249069	26.294324
194.604970	7962.293334	26.299341
194.572373	7972.975802	26.304359
194.778252	7978.263319	26.309376
195.008270	7994.833691	26.314394
195.472264	8001.728786	26.319412
195.849243	8024.110487	26.324429
196.105573	8034.551987	26.329447
196.408641	8039.574885	26.334464
196.075438	8054.572905	26.339482
196.665189	8063.629886	26.344500
196.977506	8068.367203	26.349517
196.968228	8082.758847	26.354535
196.990864	8087.528922	26.359552
196.893412	8100.229550	26.364570
197.273590	8108.508006	26.369588
197.551243	8132.010391	26.374605
197.666680	8151.288724	26.379623
197.901221	8159.249048	26.384640
198.088304	8176.640848	26.389658
198.240338	8184.857208	26.394676
198.411416	8198.264076	26.399693
198.712866	8211.672630	26.404711
198.789082	8224.762879	26.409728
198.850451	8236.911477	26.414746
199.355725	8254.035660	26.419764
199.295148	8272.470320	26.424781
199.677684	8286.327169	26.429799
199.609590	8297.084842	26.434816
199.695267	8316.964711	26.439834
199.970829	8327.946395	26.444852
200.269924	8329.572893	26.449869
200.303169	8347.620385	26.454887
200.739254	8362.365536	26.459904
200.743637	8388.430474	26.464922
200.937715	8395.693191	26.469940
201.169992	8404.547454	26.474957
201.422990	8429.594779	26.479975
201.662213	8438.485857	26.484992
201.685171	8461.681271	26.490010
202.078667	8460.483101	26.495028
202.355360	8482.707423	26.500045
202.549582	8499.328055	26.505063
202.889726	8511.205843	26.510080
203.229486	8527.712142	26.515098
203.218200	8518.482343	26.520116
204.194621	8542.065211	26.525133
204.282716	8538.044991	26.530151
204.834352	8533.822708	26.535168
204.806188	8551.276996	26.540186
205.142580	8562.097744	26.545204
205.484774	8564.743600	26.550221
205.604121	8567.427525	26.555239
205.772215	8564.319826	26.560256
205.498298	8563.772401	26.565274
205.856453	8568.565810	26.570292
206.610466	8586.617438	26.575309
206.343507	8592.935838	26.580327
206.765949	8590.643891	26.585344
206.706333	8594.726082	26.590362
207.020873	8608.975847	26.595380
206.949800	8607.689430	26.600397
206.882814	8606.585490	26.605415
207.479940	8624.525972	26.610432
207.368696	8642.517457	26.615450
207.463461	8642.515300	26.620468
207.870538	8657.246288	26.625485
207.948781	8672.505542	26.630503
208.073893	8678.658362	26.635520
208.145110	8694.900630	26.640538
208.067122	8711.513581	26.645556
208.505548	8723.969667	26.650573
208.350317	8758.799333	26.655591
208.725740	8765.705433	26.660608
209.237364	8783.466873	26.665626
209.511113	8794.887974	26.670644
209.818366	8811.510122	26.675661
209.786134	8828.100223	26.680679
210.389651	8844.420252	26.685696
210.574583	8849.212456	26.690714
210.600235	8867.880464	26.695732
210.956429	8877.470125	26.700749
211.112293	8895.404223	26.705767
211.443823	8902.901344	26.710784
211.537049	8914.552863	26.715802
211.708304	8926.773102	26.720820
211.827006	8934.398295	26.725837
211.784563	8959.625224	26.730855
212.343077	8961.615269	26.735872
212.425802	8986.342721	26.740890
212.708741	8994.819930	26.745908
213.208781	9003.203145	26.750925
212.879397	9020.790307	26.755943
213.418918	9035.491376	26.760960
213.547603	9052.719497	26.765978
214.253279	9052.015438	26.770996
214.213948	9064.376105	26.776013
214.483941	9074.752906	26.781031
214.695587	9073.478997	26.786048
215.139215	9081.132280	26.791066
215.518163	9084.015566	26.796084
215.703365	9086.777654	26.801101
215.561013	9099.909075	26.806119
215.641886	9088.059792	26.811136
215.818593	9103.524984	26.816154
216.150919	9108.805647	26.821172
216.570833	9115.897504	26.826189
216.603055	9146.281477	26.831207
216.674510	9146.841814	26.836224
216.751422	9157.271010	26.841242
216.652287	9175.460023	26.846260
217.163169	9181.893565	26.851277
217.321579	9203.316382	26.856295
217.697810	9205.855967	26.861312
217.594550	9227.152467	26.866330
218.225404	9231.915958	26.871348
218.432892	9245.393656	26.876365
218.458558	9257.179109	26.881383
218.784433	9278.370553	26.886400
219.149053	9292.139400	26.891418
218.903313	9302.695000	26.896436
219.202706	9319.426183	26.901453
219.426478	9334.622138	26.906471
220.191674	9337.271302	26.911488
220.105149	9355.951059	26.916506
220.409324	9369.334766	26.921524
220.582165	9375.186708	26.926541
220.695296	9399.534223	26.931559
221.080569	9410.575139	26.936576
221.157654	9413.161615	26.941594
221.413105	9432.716135	26.946612
221.555013	9433.581178	26.951629
221.928550	9447.310855	26.956647
222.315212	9468.006761	26.961664
222.645229	9482.854670	26.966682
222.519562	9493.675729	26.971700
222.570138	9508.141192	26.976717
222.646160	9530.426622	26.981735
223.107854	9547.628291	26.986752
223.401334	9547.055096	26.991770
223.496693	9563.881610	26.996788
223.872210	9578.586701	27.001805
224.126274	9594.494845	27.006823
224.264436	9606.070297	27.011840
224.696795	9621.306428	27.016858
224.992505	9639.206706	27.021876
225.240779	9644.197581	27.026893
225.060013	9668.572544	27.031911
225.417784	9681.922821	27.036928
225.746645	9693.522128	27.041946
225.781116	9714.914432	27.046964
226.059042	9729.814902	27.051981
226.443101	9754.019401	27.056999
226.163620	9755.326203	27.062016
227.001015	9767.060594	27.067034
226.901248	9774.931902	27.072052
227.612064	9792.975688	27.077069
227.986430	9807.213844	27.082087
228.121185	9810.823815	27.087104
228.042644	9818.243463	27.092122
228.177069	9835.585076	27.097140
228.406599	9843.572169	27.102157
228.838934	9863.588830	27.107175
228.952890	9867.442034	27.112192
229.028582	9880.321984	27.117210
229.033480	9890.576584	27.122228
229.743494	9901.023842	27.127245
229.325058	9916.447174	27.132263
229.647601	9934.053049	27.137280
229.860250	9953.305392	27.142298
230.082895	9972.496198	27.147316
230.169705	9979.425863	27.152333
230.461384	10002.192735	27.157351
230.683408	10019.839698	27.162368
230.971460	10032.288646	27.167386
231.049789	10055.540521	27.172404
231.649073	10073.390502	27.177421
231.739483	10090.695043	27.182439
232.197643	10111.364675	27.187456
232.142073	10121.054217	27.192474
232.042216	10143.030082	27.197492
232.574389	10162.677788	27.202509
233.156124	10183.492331	27.207527
233.043909	10184.968722	27.212544
233.271720	10209.690855	27.217562
233.434418	10239.923555	27.222580
233.952003	10254.467995	27.227597
233.938613	10274.728585	27.232615
234.475883	10304.978490	27.237632
234.559834	10310.131058	27.242650
234.792418	10339.241532	27.247668
234.936506	10352.265810	27.252685
235.452210	10374.009742	27.257703
235.673889	10388.717470	27.262720
235.613118	10404.306197	27.267738
236.195285	10428.988896	27.272756
236.700542	10423.848311	27.277773
237.003923	10444.874099	27.282791
237.174043	10450.411054	27.287808
237.408142	10465.568422	27.292826
237.848101	10479.594735	27.297844
238.228722	10479.222574	27.302861
238.512760	10499.938860	27.307879
238.836684	10512.028867	27.312896
238.791205	10508.603819	27.317914
239.142253	10532.236671	27.322932
239.372210	10527.609657	27.327949
239.405945	10548.766215	27.332967
239.638032	10562.594655	27.337984
240.448383	10572.388752	27.343002
239.748090	10584.879227	27.348020
240.156409	10592.762853	27.353037
240.127114	10615.258684	27.358055
240.084979	10636.004114	27.363072
240.618861	10652.494521	27.368090
240.950913	10665.694812	27.373108
241.380803	10690.445917	27.378125
241.530999	10693.409499	27.383143
241.628202	10717.495991	27.388160
242.032778	10729.017773	27.393178
241.839916	10750.983660	27.398196
242.330912	10764.749587	27.403213
242.519768	10792.184630	27.408231
242.904326	10809.459543	27.413248
243.171609	10817.838994	27.418266
243.079775	10836.830503	27.423284
243.470433	10853.694015	27.428301
243.757248	10869.942292	27.433319
244.017535	10890.388021	27.438336
244.108855	10906.098588	27.443354
244.101348	10929.592340	27.448372
244.612533	10950.137764	27.453389
244.975800	10957.927558	27.458407
244.839265	10983.812951	27.463424
245.238016	10990.068918	27.468442
245.222045	11019.989844	27.473460
245.859556	11036.268583	27.478477
246.041736	11057.348780	27.483495
246.522774	11080.766188	27.488512
246.550055	11083.758559	27.493530
246.807094	11097.422447	27.498548
247.324803	11103.006188	27.503565
247.805780	11131.693751	27.508583
247.526096	11150.705531	27.513600
248.326888	11147.324622	27.518618
248.495520	11173.860308	27.523636
248.623076	11195.969135	27.528653
248.993974	11204.155700	27.533671
248.752639	11226.186572	27.538688
249.698109	11224.061833	27.543706
249.723716	11254.406058	27.548724
249.860436	11259.689558	27.553741
250.171251	11286.891498	27.558759
250.182544	11290.145335	27.563776
250.233912	11304.972035	27.568794
250.655570	11332.301930	27.573812
250.828690	11343.222500	27.578829
251.166816	11370.669740	27.583847
251.416646	11388.263113	27.588864
251.720477	11399.649523	27.593882
252.009476	11419.914500	27.598900
252.346110	11428.491768	27.603917
252.745609	11446.355415	27.608935
252.812877	11458.530447	27.613952
253.175673	11475.222053	27.618970
253.381647	11491.805618	27.623988
253.350890	11513.794365	27.629005
253.504275	11539.758255	27.634023
253.783717	11553.210557	27.639040
254.474465	11568.729887	27.644058
254.728285	11595.925415	27.649076
254.877244	11605.668940	27.654093
255.256494	11622.036012	27.659111
255.466445	11633.241492	27.664128
255.741960	11642.980999	27.669146
255.862832	11657.465528	27.674164
256.115204	11684.130914	27.679181
256.428573	11699.390540	27.684199
256.760204	11721.417491	27.689216
257.253058	11733.901803	27.694234
257.206444	11759.742598	27.699252
257.098941	11778.128066	27.704269
257.236676	11791.463797	27.709287
257.712117	11820.131174	27.714304
258.023112	11839.928970	27.719322
258.614441	11858.858698	27.724340
258.578707	11873.870009	27.729357
259.148498	11889.800116	27.734375
259.129955	11908.790696	27.739392
259.266778	11924.596035	27.744410
259.296170	11939.445623	27.749428
259.604924	11960.731205	27.754445
260.066672	11981.863376	27.759463
260.188855	12005.303418	27.764480
261.013804	12011.581382	27.769498
260.969270	12030.045649	27.774516
261.459002	12047.510482	27.779533
262.033970	12070.892307	27.784551
261.961828	12075.776138	27.789568
262.265360	12084.794667	27.794586
262.304781	12107.663610	27.799604
262.661203	12119.566412	27.804621
262.932743	12139.847531	27.809639
262.930605	12159.034735	27.814656
263.446924	12171.986175	27.819674
263.626847	12196.544747	27.824692
263.349145	12214.976249	27.829709
264.017601	12230.783823	27.834727
264.033388	12259.770186	27.839744
264.331537	12270.775917	27.844762
264.597369	12285.332955	27.849780
265.279890	12304.953042	27.854797
265.315436	12321.428248	27.859815
265.621392	12344.685189	27.864832
266.003527	12351.683150	27.869850
266.347403	12379.260430	27.874868
266.278405	12400.141482	27.879885
266.982248	12418.924677	27.884903
267.213484	12439.240852	27.889920
267.431886	12446.646598	27.894938
267.605213	12455.256234	27.899956
267.811529	12476.116346	27.904973
268.697853	12485.094298	27.909991
268.370719	12498.424404	27.915008
269.215787	12519.402395	27.920026
269.491396	12532.638105	27.925044
269.589788	12534.659576	27.930061
269.777918	12558.462602	27.935079
270.011279	12580.322795	27.940096
270.292429	12586.335617	27.945114
270.128131	12614.990737	27.950132
270.260581	12633.557341	27.955149
270.529428	12652.604701	27.960167
271.064532	12681.396674	27.965184
271.751740	12691.905916	27.970202
272.061014	12714.120687	27.975220
272.197159	12728.944699	27.980237
272.692290	12742.743011	27.985255
272.857820	12761.383507	27.990272
272.828656	12781.895580	27.995290
272.986947	12791.009832	28.000308
273.247305	12809.038675	28.005325
273.296229	12829.409092	28.010343
273.432549	12858.459595	28.015360
273.622829	12872.826815	28.020378
274.276006	12895.474247	28.025396
274.088107	12933.815752	28.030413
274.663056	12956.671304	28.035431
274.568671	12980.737015	28.040448
274.734497	12993.216549	28.045466
275.289849	13029.764949	28.050484
275.607361	13065.308552	28.055501
275.792362	13081.022045	28.060519
275.824488	13110.341893	28.065536
276.643833	13129.464553	28.070554
276.855281	13168.375566	28.075572
276.845190	13188.035595	28.080589
277.335754	13206.278234	28.085607
277.801217	13236.572527	28.090624
277.946595	13258.658871	28.095642
278.231630	13276.431654	28.100660
278.854525	13306.088746	28.105677
279.456874	13320.900192	28.110695
279.660307	13337.053129	28.115712
279.903949	13350.379686	28.120730
280.143643	13361.313102	28.125748
280.238345	13373.298748	28.130765
280.904000	13381.967477	28.135783
280.955413	13406.797232	28.140800
281.233560	13415.634052	28.145818
281.792289	13431.106127	28.150836
281.505665	13451.681360	28.155853
281.884835	13461.244511	28.160871
281.850474	13474.144159	28.165888
282.279419	13493.044121	28.170906
282.434409	13516.708273	28.175924
282.795457	13539.152754	28.180941
283.104332	13564.776105	28.185959
282.998081	13576.985999	28.190976
283.591950	13599.997267	28.195994
283.896001	13625.409867	28.201012
284.122055	13657.204511	28.206029
284.444788	13661.117373	28.211047
284.714168	13693.928502	28.216064
285.181171	13719.893626	28.221082
285.356940	13740.156724	28.226100
285.309412	13768.672125	28.231117
285.726587	13788.407958	28.236135
286.146583	13812.577311	28.241152
286.245463	13826.501649	28.246170
286.800251	13859.959975	28.251188
287.062649	13877.162095	28.256205
287.745236	13889.311780	28.261223
288.097756	13914.044499	28.266240
288.486497	13927.857185	28.271258
289.451284	13936.577212	28.276276
289.682068	13951.636844	28.281293
289.825194	13955.956875	28.286311
290.119022	13970.539246	28.291328
290.471040	13987.711637	28.296346
291.030137	13988.138887	28.301364
290.717912	13999.443359	28.306381
290.975859	14013.984013	28.311399
290.971942	14026.869791	28.316416
291.447607	14046.473563	28.321434
291.673096	14066.555524	28.326452
291.917976	14081.938337	28.331469
291.899001	14106.934780	28.336487
291.967366	14121.018862	28.341504
292.368963	14151.362517	28.346522
292.624046	14170.991497	28.351540
292.532964	14187.364990	28.356557
292.935641	14217.051687	28.361575
292.989917	14248.596312	28.366592
293.434463	14284.577069	28.371610
293.796193	14297.557343	28.376628
293.986457	14332.147377	28.381645
294.356703	14365.180724	28.386663
294.973124	14391.818158	28.391680
295.215179	14412.216863	28.396698
295.620924	14443.924668	28.401716
295.580333	14478.712197	28.406733
295.911337	14498.275932	28.411751
296.311471	14516.985619	28.416768
296.619379	14555.306407	28.421786
297.043502	14585.634591	28.426804
296.865510	14613.123165	28.431821
297.192093	14631.673943	28.436839
297.636833	14665.356208	28.441856
298.057781	14691.320397	28.446874
298.422896	14716.841742	28.451892
298.701751	14742.534545	28.456909
299.152848	14766.513902	28.461927
299.577298	14795.342206	28.466944
299.763602	14815.355295	28.471962
300.076176	14825.276974	28.476980
300.238236	14852.194670	28.481997
300.323317	14869.295973	28.487015
300.777292	14896.742807	28.492032
300.910351	14917.996065	28.497050
301.499544	14936.537585	28.502068
301.615907	14964.817493	28.507085
301.527498	14989.127987	28.512103
302.390351	15011.707202	28.517120
302.851131	15042.488320	28.522138
303.187636	15062.010713	28.527156
303.420027	15091.254860	28.532173
303.546295	15109.158448	28.537191
303.630297	15135.709776	28.542208
303.768063	15163.844502	28.547226
304.495651	15191.154148	28.552244
304.413421	15211.895070	28.557261
304.658927	15242.779715	28.562279
305.233007	15269.920863	28.567296
305.505914	15300.457052	28.572314
306.059503	15326.995092	28.577332
306.177648	15357.290315	28.582349
306.429397	15377.840133	28.587367
306.911835	15395.981921	28.592384
307.246528	15421.499496	28.597402
307.774760	15444.311667	28.602420
307.875055	15478.368312	28.607437
307.684904	15498.857989	28.612455
308.429768	15527.232934	28.617472
308.747979	15559.780633	28.622490
309.211135	15583.057968	28.627508
309.411630	15618.871013	28.632525
309.637036	15643.022633	28.637543
310.254494	15664.042920	28.642560
310.352256	15684.730889	28.647578
310.934769	15707.260090	28.652596
311.073937	15746.538261	28.657613
311.299452	15763.829976	28.662631
311.749035	15784.895643	28.667648
311.980137	15811.380644	28.672666
312.641093	15830.312908	28.677684
312.866542	15851.814877	28.682701
313.092617	15876.137240	28.687719
313.737112	15894.342551	28.692736
313.841578	15916.419426	28.697754
314.459335	15918.002999	28.702772
314.747447	15951.171970	28.707789
314.860834	15977.918840	28.712807
314.825733	15992.718520	28.717824
315.432265	16021.261154	28.722842
315.664467	16044.268858	28.727860
315.892839	16072.150680	28.732877
315.713337	16086.764594	28.737895
316.742342	16116.750933	28.742912
316.791782	16145.981127	28.747930
317.031083	16163.583730	28.752948
317.379877	16194.166305	28.757965
317.714410	16218.326822	28.762983
318.129908	16235.131223	28.768000
318.704367	16267.169366	28.773018
318.587154	16296.978629	28.778036
318.875736	16312.713299	28.783053
318.953533	16328.749473	28.788071
319.500158	16357.504135	28.793088
319.747031	16395.560212	28.798106
319.976086	16422.728612	28.803124
320.299825	16446.834254	28.808141
320.571242	16470.534355	28.813159
321.171200	16490.181176	28.818176
321.049538	16519.451372	28.823194
322.039896	16548.111542	28.828212
322.336916	16560.702357	28.833229
322.803633	16584.855262	28.838247
323.220532	16597.165164	28.843264
323.310049	16635.859120	28.848282
323.559211	16645.978031	28.853300
324.240018	16666.882103	28.858317
324.257512	16680.041102	28.863335
324.536959	16696.481874	28.868352
324.850910	16733.318384	28.873370
325.172847	16740.463215	28.878388
325.070051	16771.445936	28.883405
325.283275	16807.565579	28.888423
326.240528	16827.655830	28.893440
326.316167	16853.588598	28.898458
326.766760	16870.991345	28.903476
327.111885	16898.871867	28.908493
327.256681	16926.278435	28.913511
327.548018	16943.605120	28.918528
327.826005	16978.413596	28.923546
328.174242	16998.144587	28.928564
328.512143	17035.976041	28.933581
328.499691	17061.430143	28.938599
329.465356	17086.383614	28.943616
329.268104	17118.676720	28.948634
329.270338	17145.632136	28.953652
330.263303	17178.168474	28.958669
330.185683	17212.824606	28.963687
331.049448	17237.914263	28.968704
331.423389	17251.273665	28.973722
332.212792	17272.875239	28.978740
332.614974	17298.150990	28.983757
332.710290	17315.395003	28.988775
333.417803	17330.123602	28.993792
333.412799	17358.906153	28.998810
333.470560	17376.648854	29.003828
333.898541	17388.711151	29.008845
334.365168	17415.031955	29.013863
335.191659	17433.020697	29.018880
335.427952	17461.620304	29.023898
335.294233	17475.539502	29.028916
336.079895	17494.362272	29.033933
336.064842	17512.369198	29.038951
336.602368	17534.124232	29.043968
336.902691	17567.812094	29.048986
337.041648	17588.258749	29.054004
337.054919	17611.795372	29.059021
337.476473	17629.866681	29.064039
338.299605	17642.378949	29.069056
338.695912	17678.357824	29.074074
338.615228	17683.329705	29.079092
339.303157	17696.103249	29.084109
339.515189	17728.851288	29.089127
340.121922	17735.711815	29.094144
340.140719	17768.995587	29.099162
340.644162	17790.326662	29.104180
340.872336	17804.303121	29.109197
341.417220	17835.596724	29.114215
341.924472	17847.173079	29.119232
341.992809	17876.576658	29.124250
342.080126	17893.961423	29.129268
342.298821	17913.391448	29.134285
342.257631	17950.222730	29.139303
342.892645	17965.291682	29.144320
342.948700	18000.174664	29.149338
343.261516	18029.268524	29.154356
343.604140	18052.349768	29.159373
343.622497	18083.941044	29.164391
343.916020	18107.453322	29.169408
343.970358	18148.344845	29.174426
344.084443	18179.523274	29.179444
344.989086	18215.827845	29.184461
345.259644	18261.474480	29.189479
345.695055	18281.028866	29.194496
345.916742	18318.925251	29.199514
346.399652	18356.483862	29.204532
347.035479	18376.600810	29.209549
347.145801	18411.235957	29.214567
347.522821	18433.939523	29.219584
348.108554	18472.985859	29.224602
348.517486	18499.626740	29.229620
348.891854	18532.142220	29.234637
348.996916	18563.790187	29.239655
349.291252	18586.765911	29.244672
349.771427	18617.375960	29.249690
349.899170	18655.553060	29.254708
350.383349	18663.576628	29.259725
351.121767	18718.261242	29.264743
351.636965	18739.515706	29.269760
352.004600	18768.570496	29.274778
352.145814	18795.891815	29.279796
352.667845	18827.285361	29.284813
353.063712	18857.131904	29.289831
353.461806	18880.382340	29.294848
353.579475	18909.767115	29.299866
353.974799	18931.482815	29.304884
354.162512	18960.370221	29.309901
354.194370	18982.117639	29.314919
354.713724	19012.658993	29.319936
355.254429	19047.031999	29.324954
355.616665	19084.756228	29.329972
356.074232	19114.940984	29.334989
355.960091	19139.421823	29.340007
356.702106	19168.734461	29.345024
357.180876	19199.187696	29.350042
357.323530	19236.289549	29.355060
358.019254	19262.128398	29.360077
357.974682	19293.497725	29.365095
358.432810	19330.076493	29.370112
358.933768	19356.476684	29.375130
359.157700	19392.062424	29.380148
359.510875	19424.121497	29.385165
359.697406	19455.815010	29.390183
359.710315	19490.802184	29.395200
360.376533	19527.209729	29.400218
360.687878	19557.373847	29.405236
361.240385	19592.624171	29.410253
361.512372	19632.675999	29.415271
361.448794	19668.174597	29.420288
362.356400	19692.717212	29.425306
362.592900	19738.985490	29.430324
362.534224	19777.762610	29.435341
363.072464	19814.967865	29.440359
364.054095	19836.434778	29.445376
364.878137	19863.656947	29.450394
364.886971	19903.365143	29.455412
365.509546	19915.158440	29.460429
365.858751	19945.532042	29.465447
366.176371	19962.737256	29.470464
366.765018	20001.223876	29.475482
366.693144	20025.863473	29.480500
367.607161	20043.853567	29.485517
367.918572	20070.265457	29.490535
367.859446	20087.637204	29.495552
368.459583	20109.587496	29.500570
368.435680	20135.211675	29.505588
369.233574	20154.723798	29.510605
369.005288	20178.244487	29.515623
369.639381	20208.201095	29.520640
369.316666	20228.223691	29.525658
369.917901	20260.851829	29.530676
370.417038	20292.030175	29.535693
370.442409	20326.757837	29.540711
370.923069	20364.440707	29.545728
370.938951	20391.556425	29.550746
371.638350	20434.165035	29.555764
372.052723	20466.753285	29.560781
372.141963	20505.199071	29.565799
372.545094	20541.618120	29.570816
373.352436	20578.081334	29.575834
373.323467	20601.830360	29.580852
373.718101	20630.801546	29.585869
373.764517	20681.341451	29.590887
374.389522	20713.638062	29.595904
374.964165	20749.733666	29.600922
375.621090	20790.681640	29.605940
376.033316	20822.007127	29.610957
376.300600	20850.922764	29.615975
376.687752	20891.224493	29.620992
377.263117	20931.035574	29.626010
377.681641	20963.282798	29.631028
377.707616	20993.588598	29.636045
378.350574	21026.679042	29.641063
378.886000	21054.162904	29.646080
379.442616	21082.591264	29.651098
379.803161	21119.719409	29.656116
380.105225	21142.349400	29.661133
380.482002	21171.463187	29.666151
381.009714	21198.089134	29.671168
381.372516	21235.855320	29.676186
381.556686	21269.315008	29.681204
382.091069	21284.534984	29.686221
382.521204	21317.172720	29.691239
382.677400	21348.033660	29.696256
383.186636	21385.246431	29.701274
383.572777	21414.517075	29.706292
383.767162	21440.633204	29.711309
384.379442	21472.497067	29.716327
384.869484	21506.288364	29.721344
385.161499	21538.524751	29.726362
385.531153	21568.821831	29.731380
385.787041	21595.680454	29.736397
386.091639	21638.138675	29.741415
386.483906	21670.827159	29.746432
386.958180	21692.628329	29.751450
387.259266	21735.896106	29.756468
387.545199	21755.426828	29.761485
387.921302	21804.148716	29.766503
387.859327	21836.643237	29.771520
388.763566	21867.533146	29.776538
389.006114	21903.708156	29.781556
389.549185	21933.763793	29.786573
389.917271	21979.871386	29.791591
389.883837	22019.836893	29.796608
390.603081	22038.554400	29.801626
390.694325	22086.955110	29.806644
390.989748	22123.545601	29.811661
391.540085	22162.244646	29.816679
391.635485	22209.197982	29.821696
392.467434	22244.011194	29.826714
392.321386	22287.015310	29.831732
392.979745	22319.859071	29.836749
393.876792	22345.019593	29.841767
394.533562	22372.043957	29.846784
395.695011	22384.651624	29.851802
395.760912	22412.539506	29.856820
396.295454	22424.518717	29.861837
396.795383	22433.236455	29.866855
397.249789	22455.363845	29.871872
397.568753	22478.138053	29.876890
397.735952	22504.177696	29.881908
398.002535	22521.690131	29.886925
398.600366	22544.370183	29.891943
398.632119	22572.781796	29.896960
399.162077	22591.801194	29.901978
399.272728	22624.345792	29.906996
399.861452	22656.240527	29.912013
399.689949	22681.082287	29.917031
399.986540	22731.025841	29.922048
400.364639	22761.007468	29.927066
400.522867	22790.625479	29.932084
401.098471	22828.178115	29.937101
401.699129	22860.880152	29.942119
401.645129	22906.803248	29.947136
402.240507	22945.351426	29.952154
402.685789	22994.115950	29.957172
402.689218	23031.132997	29.962189
402.977609	23080.541584	29.967207
403.638797	23120.242518	29.972224
404.265021	23159.095918	29.977242
403.914322	23214.810384	29.982260
404.708166	23250.016802	29.987277
405.268538	23289.746503	29.992295
405.394298	23345.487811	29.997312
406.121291	23390.221734	30.002330
406.148749	23440.310328	30.007348
406.325818	23479.443241	30.012365
407.132683	23538.389708	30.017383
407.621193	23579.439340	30.022400
408.127327	23626.426468	30.027418
408.244355	23670.036929	30.032436
409.099620	23712.204785	30.037453
409.407489	23747.342857	30.042471
409.719282	23799.087724	30.047488
410.372750	23834.114941	30.052506
410.898102	23873.996637	30.057524
411.263116	23915.394911	30.062541
411.473293	23965.753212	30.067559
411.876596	24006.292553	30.072576
412.568137	24052.486987	30.077594
413.223685	24090.667744	30.082612
413.952809	24127.983917	30.087629
414.418780	24156.879564	30.092647
414.780112	24196.648565	30.097664
415.341918	24228.638506	30.102682
415.582053	24256.842927	30.107700
415.918418	24285.847534	30.112717
416.426688	24310.376294	30.117735
416.416051	24362.444860	30.122752
416.831398	24396.935280	30.127770
417.101883	24441.660907	30.132788
417.800915	24478.704385	30.137805
418.512425	24505.811546	30.142823
418.723155	24551.008109	30.147840
419.031805	24591.481303	30.152858
419.567602	24623.178925	30.157876
419.770963	24661.235688	30.162893
420.698708	24691.753446	30.167911
421.001584	24733.915185	30.172928
421.209936	24754.699656	30.177946
421.736257	24785.198278	30.182964
422.300330	24820.418175	30.187981
422.441494	24850.313654	30.192999
422.691593	24886.707756	30.198016
423.263071	24914.633691	30.203034
423.907682	24954.385101	30.208052
423.887346	24984.881174	30.213069
424.331051	25020.606898	30.218087
424.619705	25062.480842	30.223104
425.308257	25087.291984	30.228122
425.911502	25121.627822	30.233140
426.009444	25160.321382	30.238157
426.651023	25199.934717	30.243175
427.177344	25236.684336	30.248192
427.827596	25269.685898	30.253210
428.090281	25305.592157	30.258228
428.120025	25339.323012	30.263245
428.902179	25365.510208	30.268263
429.082701	25412.798997	30.273280
429.574661	25445.566526	30.278298
429.744391	25486.126478	30.283316
430.014202	25525.160372	30.288333
431.055008	25554.037511	30.293351
431.509913	25601.504963	30.298368
432.183385	25643.869677	30.303386
432.569499	25674.258888	30.308404
433.368337	25705.942296	30.313421
433.808647	25742.067990	30.318439
433.924336	25776.595073	30.323456
434.444355	25813.548971	30.328474
434.910259	25831.311163	30.333492
435.265253	25872.253674	30.338509
435.368037	25899.559184	30.343527
435.602524	25946.619568	30.348544
435.477900	25982.543456	30.353562
436.269489	26027.677627	30.358580
436.527137	26073.040893	30.363597
436.950206	26119.421170	30.368615
437.237056	26169.665530	30.373632
437.963882	26213.268147	30.378650
438.353108	26256.121077	30.383668
439.003287	26308.653652	30.388685
439.404874	26344.167109	30.393703
440.205515	26385.173579	30.398720
440.848969	26420.706169	30.403738
441.201061	26452.675612	30.408756
441.628453	26491.933178	30.413773
442.046511	26528.411374	30.418791
442.566325	26579.119558	30.423808
442.770526	26608.900321	30.428826
443.538991	26641.993056	30.433844
443.811205	26684.201589	30.438861
444.710350	26721.957323	30.443879
445.040657	26760.611226	30.448896
445.665129	26780.725855	30.453914
446.092112	26819.750268	30.458932
445.907761	26857.340986	30.463949
447.029882	26896.888702	30.468967
447.241331	26931.276344	30.473984
447.958527	26960.749738	30.479002
448.368115	26993.387308	30.484020
448.267096	27028.854280	30.489037
448.841183	27065.018264	30.494055
449.143078	27097.653907	30.499072
449.203131	27145.218424	30.504090
449.580116	27188.359659	30.509108
449.859523	27234.866115	30.514125
450.587786	27278.053647	30.519143
450.741838	27323.195754	30.524160
450.651347	27368.926148	30.529178
451.358702	27422.830520	30.534196
451.813242	27455.683008	30.539213
452.261046	27496.430963	30.544231
452.747341	27537.861911	30.549248
453.216855	27590.546189	30.554266
453.872534	27636.261439	30.559284
454.061605	27696.113219	30.564301
454.677782	27739.312964	30.569319
455.215270	27784.566691	30.574336
455.533792	27827.522496	30.579354
456.288049	27876.048171	30.584372
456.494502	27928.603867	30.589389
456.945619	27967.253778	30.594407
457.407309	28016.514568	30.599424
457.872848	28070.521734	30.604442
458.542630	28102.222783	30.609460
458.618134	28165.664939	30.614477
459.366732	28209.660316	30.619495
460.216746	28262.798712	30.624512
460.369397	28306.255561	30.629530
460.712119	28345.024297	30.634548
461.095165	28408.273655	30.639565
461.832050	28445.678754	30.644583
462.697609	28499.074484	30.649600
462.999958	28538.785396	30.654618
463.759774	28575.397033	30.659636
463.961860	28618.252638	30.664653
464.452885	28658.224991	30.669671
464.841291	28702.619173	30.674688
465.348838	28751.602749	30.679706
465.833667	28786.810341	30.684724
465.983203	28847.234240	30.689741
466.598335	28884.450619	30.694759
466.898241	28944.080092	30.699776
467.395064	28995.644895	30.704794
468.074411	29036.606170	30.709812
468.417123	29092.588462	30.714829
468.877845	29139.981077	30.719847
469.441059	29186.649788	30.724864
469.746450	29231.456342	30.729882
470.576206	29273.285803	30.734900
470.550696	29327.215163	30.739917
471.260136	29380.106666	30.744935
471.697147	29432.023272	30.749952
471.997902	29478.815929	30.754970
472.856691	29533.403787	30.759988
472.851850	29590.194088	30.765005
473.410319	29630.499113	30.770023
474.441009	29672.152526	30.775040
475.387070	29719.148074	30.780058
476.097544	29752.842812	30.785076
476.514580	29795.812590	30.790093
476.739997	29830.658041	30.795111
477.262548	29859.142060	30.800128
477.751322	29907.549772	30.805146
478.081949	29945.684970	30.810164
478.062386	29997.162486	30.815181
478.407400	30039.568813	30.820199
478.920164	30082.056415	30.825216
479.252654	30125.052763	30.830234
479.760667	30185.203188	30.835252
480.262812	30233.059609	30.840269
480.701604	30290.041524	30.845287
481.078215	30330.629256	30.850304
481.607098	30375.226290	30.855322
482.462902	30421.712897	30.860340
482.994483	30455.341980	30.865357
483.981447	30487.136104	30.870375
484.744082	30521.715254	30.875392
484.868379	30569.138559	30.880410
485.445005	30589.081109	30.885428
485.496129	30633.936853	30.890445
485.957863	30676.389419	30.895463
486.336634	30712.249065	30.900480
486.589291	30757.870024	30.905498
487.094413	30811.397743	30.910516
487.092071	30858.474893	30.915533
487.668319	30911.372215	30.920551
488.076656	30957.632997	30.925568
488.582952	31000.237286	30.930586
489.029011	31059.034482	30.935604
489.389227	31116.568315	30.940621
489.677102	31180.169800	30.945639
490.174851	31236.443376	30.950656
490.725262	31301.123050	30.955674
491.520292	31349.935005	30.960692
491.955444	31412.964145	30.965709
492.205564	31459.813460	30.970727
493.032076	31527.643082	30.975744
493.194008	31587.788560	30.980762
494.038288	31645.412405	30.985780
494.214961	31713.843838	30.990797
494.635470	31776.990165	30.995815
495.387360	31840.015239	31.000832
495.788341	31893.726422	31.005850
496.202399	31960.338710	31.010868
496.691527	32018.012889	31.015885
497.072312	32076.500761	31.020903
497.676236	32138.487825	31.025920
497.972520	32202.894001	31.030938
499.469291	32244.833623	31.035956
500.070530	32307.485419	31.040973
500.620093	32357.185331	31.045991
502.003478	32389.887555	31.051008
502.909921	32427.127899	31.056026
503.409024	32465.747098	31.061044
503.774367	32501.928032	31.066061
504.306898	32532.494121	31.071079
505.251361	32561.529010	31.076096
505.418084	32593.233560	31.081114
505.820948	32627.341507	31.086132
505.932829	32680.316050	31.091149
506.128137	32723.522595	31.096167
506.805801	32754.401350	31.101184
506.975289	32812.766321	31.106202
507.308748	32850.925368	31.111220
507.721843	32899.775483	31.116237
507.818402	32949.060943	31.121255
508.418714	33008.041778	31.126272
508.729309	33073.478912	31.131290
509.165074	33134.508993	31.136308
509.494507	33191.029152	31.141325
509.945560	33257.538614	31.146343
510.478467	33309.279174	31.151360
511.005264	33368.949025	31.156378
511.842172	33425.598968	31.161396
512.211792	33488.884873	31.166413
512.901720	33543.781570	31.171431
513.728213	33595.527431	31.176448
513.810832	33670.125355	31.181466
514.413175	33727.660056	31.186484
514.956935	33775.745692	31.191501
515.012337	33839.967008	31.196519
516.032357	33882.389227	31.201536
516.251445	33937.291147	31.206554
516.815054	33984.748223	31.211572
517.417548	34047.152112	31.216589
517.850110	34097.892398	31.221607
518.267502	34153.219043	31.226624
519.349369	34206.759954	31.231642
519.770538	34256.686792	31.236660
520.234320	34312.385945	31.241677
520.372868	34360.978964	31.246695
521.147269	34413.101704	31.251712
521.114542	34473.741163	31.256730
522.298221	34534.443186	31.261748
522.916831	34599.419514	31.266765
522.993190	34653.068461	31.271783
523.560261	34707.380446	31.276800
524.007012	34764.967633	31.281818
524.393348	34826.636302	31.286836
525.132505	34895.198637	31.291853
525.415475	34942.973699	31.296871
526.101026	35005.007005	31.301888
526.655649	35058.480905	31.306906
527.447029	35115.332200	31.311924
528.068502	35184.489282	31.316941
528.350301	35246.637115	31.321959
529.012178	35298.520420	31.326976
529.562973	35364.388598	31.331994
529.930299	35427.187471	31.337012
530.633646	35489.718919	31.342029
531.234219	35550.477243	31.347047
531.819137	35603.486192	31.352064
532.461372	35677.080372	31.357082
532.978304	35724.415873	31.362100
533.740748	35779.098352	31.367117
533.907806	35839.805262	31.372135
534.727669	35889.117066	31.377152
535.045727	35956.035221	31.382170
535.482555	36011.205588	31.387188
536.727134	36065.332732	31.392205
536.862499	36126.759937	31.397223
537.489063	36185.372451	31.402240
537.703372	36234.432123	31.407258
538.591605	36292.561326	31.412276
539.123896	36352.997502	31.417293
539.143771	36426.053095	31.422311
540.005405	36469.567609	31.427328
540.241813	36531.960256	31.432346
541.237514	36589.384198	31.437364
541.898987	36647.322244	31.442381
542.038770	36709.793776	31.447399
542.821560	36761.206424	31.452416
543.114385	36823.673289	31.457434
543.490921	36876.692743	31.462452
544.567509	36933.358782	31.467469
545.037561	36996.392791	31.472487
545.906742	37043.758251	31.477504
546.143740	37106.702617	31.482522
546.684269	37165.305997	31.487540
547.325097	37225.936313	31.492557
547.593850	37275.173221	31.497575
548.623202	37318.606283	31.502592
549.818817	37369.095738	31.507610
550.564959	37413.591436	31.512628
551.558556	37455.158609	31.517645
552.002082	37495.294360	31.522663
552.355813	37536.437051	31.527680
553.039836	37567.385063	31.532698
553.375852	37607.898307	31.537716
554.105008	37632.300751	31.542733
554.876020	37663.583077	31.547751
555.793414	37686.305639	31.552768
555.984121	37716.932742	31.557786
556.166615	37745.954973	31.562804
557.118534	37786.789452	31.567821
556.955260	37819.596886	31.572839
557.503898	37853.886435	31.577856
557.842193	37889.429452	31.582874
558.185593	37937.947935	31.587892
558.873576	37976.901711	31.592909
558.987973	38034.796387	31.597927
559.193953	38084.253661	31.602944
559.559722	38144.708316	31.607962
559.890184	38212.238643	31.612980
560.315809	38271.046421	31.617997
560.502592	38344.733740	31.623015
561.111627	38411.949138	31.628032
562.062256	38479.029035	31.633050
562.148993	38551.031610	31.638068
562.877391	38617.805255	31.643085
563.084188	38686.678124	31.648103
563.586373	38766.255631	31.653120
564.025923	38850.896080	31.658138
564.828973	38923.799539	31.663156
565.370138	38998.843826	31.668173
565.901961	39071.537301	31.673191
566.021611	39145.554057	31.678208
566.515842	39221.738470	31.683226
567.181090	39310.949283	31.688244
568.100888	39390.381460	31.693261
568.517783	39483.862712	31.698279
569.724436	39556.325637	31.703296
570.241921	39629.813745	31.708314
570.420785	39713.783750	31.713332
571.265500	39792.286847	31.718349
571.916751	39872.173918	31.723367
572.113743	39946.940195	31.728384
572.889915	40030.735657	31.733402
573.097140	40116.808763	31.738420
574.176790	40191.311153	31.743437
575.056094	40268.507733	31.748455
575.587896	40339.156348	31.753472
576.140201	40416.031525	31.758490
576.834648	40495.003395	31.763508
577.675030	40567.634564	31.768525
578.057829	40637.472652	31.773543
578.679247	40711.384513	31.778560
579.309161	40787.198972	31.783578
579.788035	40859.394415	31.788596
580.763969	40935.313309	31.793613
581.248381	41014.901809	31.798631
581.812238	41073.859949	31.803648
581.957475	41148.682709	31.808666
582.408119	41229.263916	31.813684
583.389870	41296.581635	31.818701
583.687455	41374.999014	31.823719
584.348963	41450.779195	31.828736
585.136135	41511.822314	31.833754
585.341647	41593.625972	31.838772
586.386715	41662.724801	31.843789
587.071529	41737.857195	31.848807
587.530422	41807.547941	31.853824
588.417306	41882.168495	31.858842
588.835623	41950.575783	31.863860
589.882628	42014.552284	31.868877
590.488462	42091.804437	31.873895
590.352377	42146.182003	31.878912
591.041832	42208.627514	31.883930
591.512379	42282.941459	31.888948
592.505874	42349.197968	31.893965
593.174750	42415.891341	31.898983
593.315780	42475.532980	31.904000
594.087300	42543.481988	31.909018
594.813087	42617.453482	31.914036
595.128576	42678.567380	31.919053
595.259877	42745.219437	31.924071
596.106673	42820.222621	31.929088
596.570273	42886.987513	31.934106
597.107472	42972.735480	31.939124
597.362628	43045.883942	31.944141
598.115720	43126.677715	31.949159
598.360563	43202.851749	31.954176
599.538450	43284.718106	31.959194
600.497652	43356.093791	31.964212
601.196339	43430.211397	31.969229
601.499844	43513.600774	31.974247
601.748464	43598.118640	31.979264
602.743015	43661.943664	31.984282
603.087077	43744.524235	31.989300
603.821018	43828.884740	31.994317
604.385228	43904.884652	31.999335
604.713516	43988.531267	32.004352
605.452980	44057.995385	32.009370
606.106100	44159.733173	32.014388
606.839493	44240.919931	32.019405
607.394061	44325.057384	32.024423
607.472785	44413.147241	32.029440
608.531779	44489.432211	32.034458
608.836028	44583.382854	32.039476
609.805945	44662.630096	32.044493
610.854092	44738.734172	32.049511
611.154665	44814.708886	32.054528
612.009249	44894.038267	32.059546
613.075563	44970.336383	32.064564
613.855134	45038.241142	32.069581
614.481273	45117.132660	32.074599
615.056747	45198.588004	32.079616
615.815629	45254.635834	32.084634
616.309947	45330.069562	32.089652
617.014871	45393.982850	32.094669
617.820475	45460.100925	32.099687
618.367003	45535.052726	32.104704
619.172644	45597.672995	32.109722
619.592312	45672.543906	32.114740
620.452561	45734.181814	32.119757
620.783905	45803.190209	32.124775
621.339538	45871.543745	32.129792
621.987742	45950.592882	32.134810
622.479427	46027.459031	32.139828
623.110495	46091.828689	32.144845
623.502822	46169.438376	32.149863
624.020288	46253.158693	32.154880
624.548985	46323.440942	32.159898
625.330236	46399.250833	32.164916
626.236148	46465.387781	32.169933
627.314333	46539.152583	32.174951
627.614061	46610.433158	32.179968
628.461382	46669.228870	32.184986
628.892040	46754.805559	32.190004
629.834508	46806.703812	32.195021
630.236672	46882.277359	32.200039
630.448467	46960.651878	32.205056
631.538794	47037.668105	32.210074
631.795532	47107.331119	32.215092
632.476229	47170.000623	32.220109
632.760834	47249.642653	32.225127
633.387545	47320.222636	32.230144
634.161355	47383.074263	32.235162
634.455915	47461.279386	32.240180
635.007711	47540.399783	32.245197
635.694208	47614.684931	32.250215
636.150032	47696.351481	32.255232
637.238668	47761.356461	32.260250
637.495517	47847.995705	32.265268
637.931684	47922.169224	32.270285
639.045314	48004.638554	32.275303
639.248310	48083.024641	32.280320
639.737789	48167.408036	32.285338
640.473434	48246.514744	32.290356
641.193873	48331.128292	32.295373
641.858255	48417.478113	32.300391
641.869274	48502.291968	32.305408
643.013358	48578.020671	32.310426
643.910856	48662.879766	32.315444
645.339482	48732.636266	32.320461
646.140262	48816.384914	32.325479
646.470343	48896.177409	32.330496
647.019941	48959.580964	32.335514
647.565798	49034.335632	32.340532
648.281347	49125.779546	32.345549
648.880078	49203.462151	32.350567
649.251403	49289.260098	32.355584
650.044688	49377.295287	32.360602
649.954363	49459.920449	32.365620
650.730231	49544.997991	32.370637
651.505178	49628.918150	32.375655
652.310075	49727.253226	32.380672
652.618636	49810.595402	32.385690
653.126393	49910.040738	32.390708
653.824546	49997.662955	32.395725
655.060633	50096.140872	32.400743
655.522348	50175.575520	32.405760
656.640633	50263.126622	32.410778
656.805482	50360.292869	32.415796
657.553650	50451.863481	32.420813
658.730978	50531.744079	32.425831
659.283244	50619.954628	32.430848
660.310814	50697.834525	32.435866
660.994383	50784.183893	32.440884
661.669422	50863.973463	32.445901
662.437056	50925.671532	32.450919
663.155457	51023.987706	32.455936
663.870519	51095.482929	32.460954
664.342343	51174.077873	32.465972
664.957049	51261.585067	32.470989
665.503027	51340.074047	32.476007
666.153934	51429.930024	32.481024
666.633684	51499.128494	32.486042
667.663566	51587.071766	32.491060
667.773228	51676.507254	32.496077
668.454198	51760.810526	32.501095
669.068878	51853.552863	32.506112
669.707945	51937.047073	32.511130
670.455945	52032.926733	32.516148
671.120554	52118.613291	32.521165
672.637127	52187.303408	32.526183
673.004616	52269.708679	32.531200
674.033886	52345.201947	32.536218
674.903295	52419.961163	32.541236
675.495281	52501.863840	32.546253
676.044380	52571.168527	32.551271
676.720851	52649.495935	32.556288
677.575163	52716.671399	32.561306
677.928907	52792.651573	32.566324
678.288546	52867.580640	32.571341
679.345563	52933.604946	32.576359
679.853211	53015.383411	32.581376
680.217748	53085.250065	32.586394
680.475894	53159.120206	32.591412
680.923383	53247.382407	32.596429
681.975144	53325.665955	32.601447
682.409298	53418.695878	32.606464
683.100372	53499.225988	32.611482
683.740142	53587.427711	32.616500
684.220409	53685.330415	32.621517
684.760785	53771.276601	32.626535
685.333156	53866.697663	32.631552
686.108478	53966.061424	32.636570
686.662000	54057.088121	32.641588
688.423694	54131.130850	32.646605
690.601862	54176.061966	32.651623
691.510075	54252.421977	32.656640
692.252560	54305.811238	32.661658
693.384216	54373.941540	32.666676
694.195858	54432.098116	32.671693
695.041766	54475.858871	32.676711
695.524246	54541.471395	32.681728
695.719795	54594.940632	32.686746
696.196287	54659.212810	32.691764
696.814778	54722.614922	32.696781
697.349728	54785.979658	32.701799
697.755522	54866.635045	32.706816
698.241703	54934.311141	32.711834
699.105983	55008.389575	32.716852
699.273484	55084.450587	32.721869
699.910472	55158.141073	32.726887
700.487645	55247.921926	32.731904
701.081004	55335.409648	32.736922
701.612232	55424.717393	32.741940
701.882797	55515.490225	32.746957
702.516138	55600.789296	32.751975
703.194757	55702.086713	32.756992
704.263055	55795.241826	32.762010
704.903701	55894.305657	32.767028
705.121053	55989.259233	32.772045
705.723042	56081.431590	32.777063
706.702917	56187.765870	32.782080
707.364572	56278.341120	32.787098
708.451715	56382.406416	32.792116
709.178844	56480.826249	32.797133
709.835521	56568.055413	32.802151
710.049513	56668.024670	32.807168
711.251201	56761.301890	32.812186
712.511780	56854.538606	32.817204
712.589922	56945.644451	32.822221
713.821273	57048.373626	32.827239
714.597180	57139.510173	32.832256
715.265831	57232.049922	32.837274
716.211379	57316.483430	32.842292
716.179039	57406.418454	32.847309
716.851978	57504.572482	32.852327
717.052267	57610.914890	32.857344
717.835020	57711.160167	32.862362
718.972573	57810.780670	32.867380
719.556339	57919.298589	32.872397
720.935625	58005.976754	32.877415
722.010043	58079.367200	32.882432
723.317362	58181.108267	32.887450
723.859586	58252.854685	32.892468
724.467911	58342.794129	32.897485
725.153740	58426.405068	32.902503
725.678766	58499.901813	32.907520
725.786203	58581.850626	32.912538
726.411777	58664.807235	32.917556
726.815951	58758.723418	32.922573
727.572603	58852.818957	32.927591
728.336560	58943.052724	32.932608
728.641456	59030.567398	32.937626
729.343500	59140.648302	32.942644
730.091221	59232.430092	32.947661
730.830999	59334.518049	32.952679
731.466615	59453.719057	32.957696
732.174711	59552.148033	32.962714
732.674528	59656.338379	32.967732
732.918575	59770.601805	32.972749
733.730070	59874.953153	32.977767
734.726708	59981.586316	32.982784
735.529125	60094.656106	32.987802
736.237317	60213.982375	32.992820
736.723627	60330.603145	32.997837
737.731530	60437.084608	33.002855
738.682465	60550.513033	33.007872
738.949637	60662.377953	33.012890
740.119882	60772.513141	33.017908
740.870385	60891.912035	33.022925
741.498594	61007.519982	33.027943
742.106268	61124.669890	33.032960
743.113043	61239.485356	33.037978
744.196427	61350.643213	33.042996
745.309480	61461.777934	33.048013
745.960327	61562.654700	33.053031
746.920083	61675.289316	33.058048
747.882042	61770.636261	33.063066
748.824403	61869.949376	33.068084
749.505519	61985.091502	33.073101
750.381942	62068.463449	33.078119
752.016463	62160.408490	33.083136
752.626181	62238.302735	33.088154
753.813956	62327.735577	33.093172
754.556642	62426.784663	33.098189
755.107350	62505.822128	33.103207
755.776699	62590.823519	33.108224
756.474090	62686.791484	33.113242
757.182581	62780.333507	33.118260
757.984165	62872.493915	33.123277
758.635747	62956.524439	33.128295
759.035843	63038.980340	33.133312
759.726846	63146.460003	33.138330
760.028553	63249.063225	33.143348
760.863853	63355.046161	33.148365
761.196052	63459.418044	33.153383
762.019126	63568.372872	33.158400
762.311001	63684.204203	33.163418
763.078363	63777.810377	33.168436
764.059261	63897.339563	33.173453
765.449851	64006.777194	33.178471
766.502779	64101.321128	33.183488
767.144309	64196.062790	33.188506
768.158193	64290.062766	33.193524
768.632441	64400.905449	33.198541
769.469113	64502.075209	33.203559
770.484435	64600.102579	33.208576
770.745559	64699.242393	33.213594
772.034708	64804.071447	33.218612
772.340564	64913.037122	33.223629
772.972703	65012.848135	33.228647
774.320523	65113.832677	33.233664
774.804542	65224.937021	33.238682
775.709350	65324.852182	33.243700
776.234313	65419.838279	33.248717
777.130394	65512.291131	33.253735
777.514293	65607.027779	33.258752
778.074612	65702.230988	33.263770
779.122343	65806.886739	33.268788
779.644723	65914.366626	33.273805
780.004281	66019.112021	33.278823
780.982878	66122.798549	33.283840
781.452961	66239.892608	33.288858
782.409864	66354.745643	33.293876
782.984470	66473.844117	33.298893
783.823839	66578.352057	33.303911
784.252253	66697.563107	33.308928
785.519983	66815.763204	33.313946
786.114814	66921.083281	33.318964
786.992651	67036.369641	33.323981
787.108405	67158.949527	33.328999
788.507904	67271.983530	33.334016
789.527185	67393.258037	33.339034
790.724411	67498.657110	33.344052
791.843517	67626.628644	33.349069
792.128523	67733.526509	33.354087
793.028171	67839.638409	33.359104
793.344829	67961.038283	33.364122
794.502024	68070.466643	33.369140
795.377670	68194.515420	33.374157
796.074762	68301.712025	33.379175
796.934253	68434.014889	33.384192
797.800836	68546.985979	33.389210
798.293580	68660.117414	33.394228
799.397333	68782.354017	33.399245
800.066292	68906.299271	33.404263
800.583772	69018.978826	33.409280
801.549774	69137.762392	33.414298
802.101718	69263.627293	33.419316
803.306530	69388.839676	33.424333
803.376672	69516.699878	33.429351
804.663051	69627.532993	33.434368
805.438715	69755.625827	33.439386
806.668860	69877.075261	33.444404
807.462117	69994.503028	33.449421
808.457922	70121.676671	33.454439
809.369470	70232.096129	33.459456
810.160379	70358.543130	33.464474
811.337268	70458.891549	33.469492
812.264650	70575.072441	33.474509
813.164649	70690.574232	33.479527
814.427380	70803.702051	33.484544
814.573728	70903.833598	33.489562
815.458402	71015.615719	33.494580
816.484835	71138.800021	33.499597
817.130014	71248.961510	33.504615
817.446237	71359.719573	33.509632
818.280993	71488.824842	33.514650
819.363671	71602.300923	33.519668
820.012359	71716.643368	33.524685
820.531651	71836.136065	33.529703
821.645673	71961.324296	33.534720
822.178252	72091.227090	33.539738
823.050361	72201.129037	33.544756
823.674706	72331.512597	33.549773
824.341462	72452.314876	33.554791
825.767864	72566.716532	33.559808
826.252237	72695.464583	33.564826
827.597894	72805.434206	33.569844
829.159441	72914.433199	33.574861
829.659487	73024.751463	33.579879
830.690418	73124.056265	33.584896
831.233439	73235.280625	33.589914
832.410940	73335.538552	33.594932
833.419107	73437.837295	33.599949
834.018319	73553.208689	33.604967
834.621296	73653.317115	33.609984
835.562862	73746.533079	33.615002
836.186517	73850.869560	33.620020
836.966271	73952.572720	33.625037
837.080161	74060.916433	33.630055
838.118391	74167.633859	33.635072
838.761801	74288.372106	33.640090
839.741705	74398.684228	33.645108
840.601323	74518.692989	33.650125
841.630063	74639.701809	33.655143
842.848379	74744.024645	33.660160
843.493183	74866.741289	33.665178
844.554479	74972.546286	33.670196
845.453937	75077.845027	33.675213
846.185183	75197.104226	33.680231
847.104245	75311.369053	33.685248
847.492895	75425.299402	33.690266
847.975063	75549.982684	33.695284
849.039017	75676.323518	33.700301
849.499574	75802.100725	33.705319
850.672599	75924.017416	33.710336
851.313602	76055.252503	33.715354
851.903071	76183.785454	33.720372
852.809852	76317.082987	33.725389
853.298087	76447.723177	33.730407
854.748944	76572.576156	33.735424
855.316437	76707.676862	33.740442
855.862806	76848.051339	33.745460
856.690586	76984.164080	33.750477
857.641801	77126.680799	33.755495
858.504676	77268.730708	33.760512
859.145423	77412.576993	33.765530
859.738706	77561.916754	33.770548
860.894790	77705.810562	33.775565
861.573640	77851.300040	33.780583
862.797459	78003.799206	33.785600
863.182109	78152.034689	33.790618
863.943731	78298.413020	33.795636
864.925498	78431.937123	33.800653
865.774103	78593.999686	33.805671
867.339463	78740.317849	33.810688
868.057224	78886.300763	33.815706
868.384958	79044.760927	33.820724
869.708152	79180.072150	33.825741
870.147471	79336.831550	33.830759
871.086988	79482.250778	33.835776
871.951705	79642.251893	33.840794
872.749663	79811.500179	33.845812
873.899504	79952.999506	33.850829
874.701058	80106.045111	33.855847
875.986976	80248.918249	33.860864
876.696225	80395.227135	33.865882
877.845415	80541.087814	33.870900
878.948706	80675.984626	33.875917
879.940051	80823.201788	33.880935
881.213661	80963.673275	33.885952
881.943289	81109.260521	33.890970
882.794248	81247.861139	33.895988
883.932140	81381.134184	33.901005
884.452641	81519.243076	33.906023
885.484189	81654.928678	33.911040
886.456718	81805.448110	33.916058
887.072232	81937.614593	33.921076
887.749086	82071.393866	33.926093
888.912554	82212.066195	33.931111
889.692068	82339.229475	33.936128
890.285379	82479.700989	33.941146
891.444092	82615.295256	33.946164
892.627481	82741.117385	33.951181
893.286957	82871.849570	33.956199
893.970606	83000.259854	33.961216
895.173969	83138.637146	33.966234
895.587205	83272.438001	33.971252
896.861256	83412.680814	33.976269
897.205130	83549.306731	33.981287
898.064317	83687.512495	33.986304
899.033761	83838.321912	33.991322
899.627156	83979.979185	33.996340
901.025845	84127.339752	34.001357
901.486139	84271.135367	34.006375
902.302389	84418.271844	34.011392
903.083628	84568.341614	34.016410
904.351709	84729.664101	34.021428
905.183253	84869.894612	34.026445
905.853230	85022.303026	34.031463
907.155294	85180.644916	34.036480
907.986544	85339.124749	34.041498
908.600742	85486.120892	34.046516
909.923802	85636.491510	34.051533
910.524877	85795.554757	34.056551
911.221045	85951.968236	34.061568
912.266015	86111.445233	34.066586
913.580419	86271.438483	34.071604
914.754744	86411.812840	34.076621
915.901855	86568.779946	34.081639
916.648791	86715.317975	34.086656
917.256730	86870.166156	34.091674
918.126584	87032.400128	34.096692
919.610486	87175.656981	34.101709
920.215436	87329.620984	34.106727
921.914603	87475.101287	34.111744
922.769576	87628.432096	34.116762
923.142964	87772.816179	34.121780
924.602866	87915.117266	34.126797
926.347769	88050.505773	34.131815
927.386223	88182.330396	34.136832
928.118707	88333.352240	34.141850
929.138759	88474.901151	34.146868
930.500545	88597.590492	34.151885
931.280985	88745.210558	34.156903
932.225349	88875.139358	34.161920
933.191636	89009.412191	34.166938
933.962534	89143.019195	34.171956
934.909027	89262.265816	34.176973
936.065438	89398.310237	34.181991
936.704622	89517.910157	34.187008
937.521310	89662.778961	34.192026
938.398554	89808.716234	34.197044
939.118455	89934.667283	34.202061
940.316072	90079.985402	34.207079
941.097547	90204.115612	34.212096
941.985885	90342.956483	34.217114
942.242984	90499.754216	34.222132
943.397382	90637.769012	34.227149
944.047923	90793.644846	34.232167
944.697451	90937.354612	34.237184
945.884920	91093.578839	34.242202
947.295143	91234.509360	34.247220
948.062964	91386.009987	34.252237
949.212965	91530.315936	34.257255
950.409620	91668.658347	34.262272
952.158845	91792.884366	34.267290
953.409669	91919.723810	34.272308
954.214436	92039.548606	34.277325
955.375591	92167.214285	34.282343
956.004376	92277.206808	34.287360
956.498462	92396.752113	34.292378
957.281389	92529.738486	34.297396
957.905408	92656.590410	34.302413
958.536230	92800.818890	34.307431
959.144249	92945.913506	34.312448
960.134898	93075.637643	34.317466
960.635500	93230.788925	34.322484
961.294452	93387.614647	34.327501
962.344784	93558.905520	34.332519
963.280535	93702.089149	34.337536
964.470741	93857.820070	34.342554
965.037254	94015.411290	34.347572
965.946500	94173.773545	34.352589
967.037490	94341.247112	34.357607
968.060894	94501.063511	34.362624
969.178342	94658.242173	34.367642
970.266369	94827.810288	34.372660
970.938816	94989.129160	34.377677
971.937483	95146.835912	34.382695
973.245538	95315.675064	34.387712
974.614916	95471.601505	34.392730
975.657737	95624.943261	34.397748
977.200469	95772.389223	34.402765
978.625080	95929.779711	34.407783
979.162791	96080.959122	34.412800
980.329906	96236.185819	34.417818
980.973353	96394.055870	34.422836
981.259339	96546.138908	34.427853
982.583048	96703.599767	34.432871
983.342261	96871.341631	34.437888
984.416765	97031.555894	34.442906
985.109660	97206.738336	34.447924
986.096793	97375.195097	34.452941
987.084356	97544.527375	34.457959
987.578988	97727.273679	34.462976
988.555439	97897.332147	34.467994
989.513545	98079.133198	34.473012
990.589495	98262.780348	34.478029
991.421485	98431.343038	34.483047
991.848237	98629.393635	34.488064
993.654461	98808.239038	34.493082
994.368531	98992.783720	34.498100
995.481724	99173.869444	34.503117
996.466230	99355.014366	34.508135
997.406408	99539.197160	34.513152
998.588520	99710.285254	34.518170
999.700698	99900.769270	34.523188
1001.332092	100069.253394	34.528205
1001.888796	100260.485730	34.533223
1002.740770	100430.500991	34.538240
1004.015178	100608.564848	34.543258
1004.834377	100794.662708	34.548276
1006.152191	100972.442840	34.553293
1007.249728	101149.700590	34.558311
1008.113233	101326.831125	34.563328
1009.935752	101490.196042	34.568346
1010.772125	101658.356427	34.573364
1012.267424	101820.797993	34.578381
1013.641535	101976.894767	34.583399
1014.860388	102142.284559	34.588416
1016.112869	102300.684036	34.593434
1016.942673	102454.928475	34.598452
1017.741147	102606.427268	34.603469
1018.913642	102752.264201	34.608487
1019.782008	102902.574283	34.613504
1020.452397	103049.898480	34.618522
1021.143353	103204.726010	34.623540
1022.097200	103364.850936	34.628557
1023.075203	103512.395274	34.633575
1023.829671	103668.901321	34.638592
1024.619737	103835.127416	34.643610
1025.423629	104011.584279	34.648628
1026.253776	104168.245639	34.653645
1026.952420	104335.718415	34.658663
1027.752368	104517.503865	34.663680
1028.857101	104695.273909	34.668698
1029.717435	104884.989222	34.673716
1030.814164	105067.174951	34.678733
1032.264398	105234.001970	34.683751
1033.496039	105404.629910	34.688768
1035.006714	105577.586142	34.693786
1036.203017	105752.646608	34.698804
1037.644997	105914.545806	34.703821
1038.909784	106079.643507	34.708839
1040.170472	106237.033192	34.713856
1041.370469	106393.152417	34.718874
1042.396921	106564.528378	34.723892
1043.432334	106722.729057	34.728909
1044.896370	106881.522733	34.733927
1045.502252	107040.552942	34.738944
1046.820560	107186.956811	34.743962
1047.332277	107348.818229	34.748980
1048.340859	107520.708972	34.753997
1049.674691	107688.618674	34.759015
1050.074922	107854.811307	34.764032
1051.107090	108015.288257	34.769050
1052.259056	108197.456625	34.774068
1052.912732	108371.144414	34.779085
1054.223762	108547.710157	34.784103
1054.945559	108725.066499	34.789120
1055.643269	108903.682931	34.794138
1056.586748	109098.696466	34.799156
1058.018035	109290.489790	34.804173
1059.015816	109472.054890	34.809191
1059.851616	109656.905376	34.814208
1060.983332	109848.697924	34.819226
1062.056876	110030.292086	34.824244
1063.325799	110208.559411	34.829261
1065.246612	110389.959366	34.834279
1066.171947	110565.834746	34.839296
1067.737694	110742.840857	34.844314
1068.223703	110917.505912	34.849332
1069.681039	111097.853376	34.854349
1070.880855	111273.676603	34.859367
1071.683790	111454.204414	34.864384
1072.761761	111631.380079	34.869402
1073.535844	111799.029256	34.874420
1074.254823	111976.161373	34.879437
1076.106382	112157.682626	34.884455
1076.683615	112347.115100	34.889472
1077.890404	112520.280079	34.894490
1078.979243	112714.973634	34.899508
1079.779488	112897.944126	34.904525
1081.188603	113080.642663	34.909543
1082.107023	113270.089967	34.914560
1083.147660	113448.015988	34.919578
1083.830862	113636.512782	34.924596
1085.174235	113819.884825	34.929613
1086.317377	114007.664708	34.934631
1087.252447	114191.419610	34.939648
1088.279182	114386.017679	34.944666
1089.032902	114571.718002	34.949684
1090.107481	114745.992316	34.954701
1091.348706	114934.421103	34.959719
1092.417846	115101.950527	34.964736
1093.112502	115285.266568	34.969754
1094.112511	115471.820689	34.974772
1095.122088	115673.264541	34.979789
1096.125951	115852.996315	34.984807
1097.201895	116064.667440	34.989824
1098.112000	116243.363044	34.994842
1099.050198	116444.670040	34.999860
1099.967994	116652.348538	35.004877
1100.986789	116847.480795	35.009895
1101.944366	117064.313038	35.014912
1103.114270	117281.455754	35.019930
1104.328430	117485.020912	35.024948
1106.141578	117681.123951	35.029965
1107.418546	117873.214977	35.034983
1108.646060	118080.700645	35.040000
1110.310136	118274.064937	35.045018
1111.387925	118468.016689	35.050036
1112.499781	118662.306571	35.055053
1113.881009	118851.354645	35.060071
1114.372504	119047.620906	35.065088
1115.596924	119254.073309	35.070106
1116.723538	119461.100260	35.075124
1117.348707	119661.306339	35.080141
1118.549373	119869.237189	35.085159
1119.875031	120082.109370	35.090176
1120.581503	120284.221361	35.095194
1121.603178	120487.185692	35.100212
1122.926929	120712.530977	35.105229
1124.275311	120922.220255	35.110247
1125.587610	121119.269166	35.115264
1126.927861	121320.716480	35.120282
1128.160483	121534.625987	35.125300
1129.482558	121735.431325	35.130317
1130.767958	121940.277407	35.135335
1131.576976	122138.919798	35.140352
1133.388139	122342.987957	35.145370
1134.996421	122532.995172	35.150388
1136.078178	122726.206412	35.155405
1137.226610	122922.160967	35.160423
1138.127725	123118.396236	35.165440
1139.239628	123311.643656	35.170458
1140.579456	123507.253976	35.175476
1142.437827	123695.895563	35.180493
1143.443616	123867.583366	35.185511
1144.598265	124067.995378	35.190528
1145.389378	124255.208221	35.195546
1146.847174	124436.760983	35.200564
1147.627104	124624.827271	35.205581
1148.926704	124811.442948	35.210599
1149.856979	125001.162047	35.215616
1150.518991	125200.717999	35.220634
1151.781043	125399.166067	35.225652
1152.528791	125604.267284	35.230669
1153.962451	125805.785998	35.235687
1154.845450	126011.730777	35.240704
1155.658908	126214.211290	35.245722
1156.878929	126416.261233	35.250740
1157.644990	126638.187538	35.255757
1159.154810	126850.267667	35.260775
1160.059998	127053.664090	35.265792
1161.228426	127269.377561	35.270810
1162.280679	127479.286917	35.275828
1163.178540	127699.954921	35.280845
1164.479744	127910.296901	35.285863
1165.867526	128131.410666	35.290880
1167.728426	128315.086982	35.295898
1169.309945	128501.522965	35.300916
1170.208425	128694.753048	35.305933
1171.618378	128879.365178	35.310951
1172.720335	129071.397870	35.315968
1174.030824	129255.126387	35.320986
1175.389490	129439.000410	35.326004
1176.204053	129633.009178	35.331021
1176.712095	129824.998686	35.336039
1177.915796	130027.246214	35.341056
1178.756892	130231.530794	35.346074
1179.723828	130439.565007	35.351092
1180.956072	130651.961479	35.356109
1181.660300	130863.388536	35.361127
1182.842596	131082.240555	35.366144
1183.588415	131308.711570	35.371162
1185.074171	131527.581774	35.376180
1186.506953	131754.645433	35.381197
1187.716075	131967.293053	35.386215
1189.032594	132190.875151	35.391232
1190.573261	132402.102615	35.396250
1192.458917	132594.066381	35.401268
1193.631521	132818.663927	35.406285
1194.838448	133037.521889	35.411303
1196.069341	133250.248446	35.416320
1197.747683	133460.647343	35.421338
1198.887858	133660.574225	35.426356
1199.932015	133882.824430	35.431373
1200.911082	134081.484136	35.436391
1202.333407	134290.087107	35.441408
1203.252234	134506.294597	35.446426
1204.914432	134711.207471	35.451444
1205.929804	134924.762483	35.456461
1206.974573	135136.829240	35.461479
1208.328279	135361.715774	35.466496
1209.025992	135573.052155	35.471514
1210.402736	135790.666094	35.476532
1210.992508	136018.873253	35.481549
1212.316362	136246.230629	35.486567
1213.452478	136477.730020	35.491584
1214.333679	136713.737318	35.496602
1216.112380	136935.722539	35.501620
1217.281918	137165.481636	35.506637
1218.612740	137394.505982	35.511655
1219.998753	137633.370354	35.516672
1220.837320	137866.395333	35.521690
1222.594886	138082.957956	35.526708
1223.399404	138322.932107	35.531725
1224.842013	138548.200979	35.536743
1225.907452	138776.461463	35.541760
1227.276531	139014.409128	35.546778
1228.325214	139239.590684	35.551796
1229.740542	139486.328037	35.556813
1230.806958	139715.709672	35.561831
1231.842830	139949.323209	35.566848
1233.178045	140190.035952	35.571866
1234.613987	140425.784697	35.576884
1235.545787	140670.687536	35.581901
1236.878135	140917.191436	35.586919
1238.170035	141151.976383	35.591936
1238.932243	141390.119696	35.596954
1240.310335	141628.345440	35.601972
1241.694024	141871.343381	35.606989
1243.023364	142115.340960	35.612007
1243.927748	142352.692539	35.617024
1245.534293	142589.960729	35.622042
1246.931998	142826.983540	35.627060
1247.774381	143072.470844	35.632077
1249.073251	143300.804986	35.637095
1250.863156	143526.931107	35.642112
1251.737537	143760.600850	35.647130
1253.178205	143979.879390	35.652148
1254.071205	144202.189128	35.657165
1255.235188	144436.679730	35.662183
1256.487638	144667.045377	35.667200
1257.681261	144904.769962	35.672218
1259.107953	145130.122475	35.677236
1260.041336	145382.041696	35.682253
1261.457586	145611.941760	35.687271
1262.511118	145851.114213	35.692288
1263.271123	146105.094892	35.697306
1264.747408	146343.822687	35.702324
1265.871005	146597.177713	35.707341
1266.753662	146853.668664	35.712359
1268.457419	147105.932647	35.717376
1269.279699	147358.665842	35.722394
1271.047973	147619.413570	35.727412
1272.088192	147887.917597	35.732429
1273.480401	148143.256214	35.737447
1275.298580	148398.224753	35.742464
1276.473964	148663.208324	35.747482
1278.369481	148894.570973	35.752500
1280.008505	149158.012038	35.757517
1281.061071	149401.072206	35.762535
1282.902110	149646.675613	35.767552
1284.011104	149886.809710	35.772570
1285.177995	150142.180445	35.777588
1286.445312	150395.391485	35.782605
1287.803165	150627.873896	35.787623
1289.608831	150866.354669	35.792640
1290.779265	151119.025715	35.797658
1292.282924	151357.771687	35.802676
1293.471027	151602.292911	35.807693
1294.625007	151843.101309	35.812711
1295.717722	152088.363147	35.817728
1296.892535	152333.651293	35.822746
1298.657691	152580.929896	35.827764
1299.950499	152829.476755	35.832781
1301.209363	153079.984894	35.837799
1302.501621	153322.770955	35.842816
1303.559492	153572.309906	35.847834
1304.896060	153820.041843	35.852852
1306.936055	154059.591246	35.857869
1309.046181	154280.470158	35.862887
1310.721006	154509.517008	35.867904
1311.753801	154740.772525	35.872922
1313.369975	154959.586020	35.877940
1314.626451	155194.807064	35.882957
1315.615846	155423.253932	35.887975
1317.504610	155637.482683	35.892992
1318.463111	155864.387376	35.898010
1320.777010	156065.932743	35.903028
1322.313353	156282.922967	35.908045
1323.275661	156495.801895	35.913063
1324.554333	156705.737661	35.918080
1325.686015	156938.966744	35.923098
1327.003817	157142.664776	35.928116
1328.050094	157363.963037	35.933133
1328.785112	157581.451572	35.938151
1330.714878	157801.889537	35.943168
1331.517727	158025.132575	35.948186
1332.436685	158261.446885	35.953204
1333.630358	158491.930131	35.958221
1334.490259	158725.678371	35.963239
1336.203724	158961.122004	35.968256
1336.908516	159196.457826	35.973274
1338.134827	159433.718771	35.978292
1339.492166	159658.112401	35.983309
1340.091103	159896.108083	35.988327
1341.944653	160124.805640	35.993344
1342.689744	160375.729641	35.998362
1344.236815	160621.654012	36.003380
1345.066596	160862.727635	36.008397
1346.362937	161104.033838	36.013415
1348.190278	161338.287898	36.018432
1349.538779	161600.776954	36.023450
1350.747297	161844.486505	36.028468
1352.084911	162095.591150	36.033485
1353.141579	162348.149992	36.038503
1354.989816	162603.696423	36.043520
1355.639599	162874.628567	36.048538
1357.396640	163135.422109	36.053556
1358.246265	163397.298235	36.058573
1359.221384	163678.517399	36.063591
1360.768744	163950.887796	36.068608
1361.755559	164228.577909	36.073626
1363.305245	164507.552272	36.078644
1365.568492	164780.499592	36.083661
1366.976572	165057.758997	36.088679
1368.460234	165326.589943	36.093696
1370.405163	165600.339482	36.098714
1371.641730	165861.974196	36.103732
1373.234446	166134.397072	36.108749
1374.193923	166400.508323	36.113767
1376.011723	166667.781310	36.118784
1376.673885	166943.019329	36.123802
1378.120305	167205.438854	36.128820
1379.821829	167483.284210	36.133837
1380.380355	167768.775355	36.138855
1382.163379	168042.775679	36.143872
1383.160313	168331.527063	36.148890
1384.785166	168617.502241	36.153908
1386.033460	168904.616749	36.158925
1387.670655	169189.246363	36.163943
1389.366054	169478.667528	36.168960
1390.122412	169762.256407	36.173978
1391.327266	170056.987908	36.178996
1392.412489	170350.380690	36.184013
1393.499451	170665.753592	36.189031
1395.181630	170957.150708	36.194048
1396.766980	171262.848821	36.199066
1398.610082	171564.508090	36.204084
1399.904531	171869.911349	36.209101
1401.164361	172176.870361	36.214119
1402.884662	172471.949639	36.219136
1403.965813	172768.895075	36.224154
1405.472562	173067.654305	36.229172
1407.343392	173369.240105	36.234189
1408.747111	173668.843111	36.239207
1410.430241	173952.162820	36.244224
1411.935622	174242.127023	36.249242
1413.460563	174532.673324	36.254260
1415.122323	174829.497516	36.259277
1416.471854	175116.848057	36.264295
1418.155647	175398.560088	36.269312
1419.466318	175690.363095	36.274330
1420.832468	175989.828213	36.279348
1422.222380	176259.906770	36.284365
1423.375324	176567.483472	36.289383
1424.925092	176848.688077	36.294400
1426.141424	177148.561744	36.299418
1427.688508	177439.927499	36.304436
1429.121201	177708.657955	36.309453
1430.778365	177996.427384	36.314471
1432.609777	178263.954292	36.319488
1434.069396	178523.336882	36.324506
1435.191049	178795.751210	36.329524
1436.913559	179050.852849	36.334541
1438.305734	179329.169490	36.339559
1439.890768	179591.862673	36.344576
1441.031518	179858.080254	36.349594
1442.822576	180119.828419	36.354612
1444.035721	180390.963408	36.359629
1445.214171	180671.120899	36.364647
1446.458165	180937.960433	36.369664
1447.821269	181221.951196	36.374682
1448.887398	181499.487382	36.379700
1450.298947	181786.697850	36.384717
1451.423608	182086.958033	36.389735
1452.440890	182380.708589	36.394752
1453.840926	182685.829453	36.399770
1455.417841	182992.650703	36.404788
1456.629116	183297.041091	36.409805
1457.756424	183611.935239	36.414823
1459.340023	183917.107438	36.419840
1461.002313	184230.141913	36.424858
1462.288745	184553.827563	36.429876
1464.173052	184858.142812	36.434893
1465.395658	185181.408684	36.439911
1467.540888	185488.504284	36.444928
1469.217910	185800.703140	36.449946
1470.501345	186121.447920	36.454964
1472.247591	186425.967217	36.459981
1473.493870	186746.008538	36.464999
1474.988608	187048.435436	36.470016
1476.650395	187361.047697	36.475034
1478.260221	187677.097959	36.480052
1480.160227	187979.260838	36.485069
1481.178700	188370.639843	36.490087
1482.697610	188679.214256	36.495104
1483.994555	189005.070873	36.500122
1485.452877	189325.289753	36.505140
1487.314072	189639.223439	36.510157
1488.781015	189953.905497	36.515175
1490.222704	190268.211358	36.520192
1491.930705	190597.411797	36.525210
1493.029551	190908.877391	36.530228
1494.823816	191226.966089	36.535245
1496.059051	191544.406508	36.540263
1497.482924	191876.779209	36.545280
1498.857152	192200.600543	36.550298
1500.457975	192525.581096	36.555316
1502.368185	192841.903188	36.560333
1503.829191	193178.642500	36.565351
1505.340838	193503.868138	36.570368
1506.951191	193819.833173	36.575386
1508.329670	194140.051848	36.580404
1509.874318	194461.058132	36.585421
1511.614353	194788.715131	36.590439
1512.863386	195114.620885	36.595456
1514.242365	195443.428238	36.600474
1515.601049	195771.426710	36.605492
1517.058414	196093.669783	36.610509
1518.772018	196420.394962	36.615527
1520.071232	196759.099089	36.620544
1521.829770	197090.086233	36.625562
1523.237494	197416.353520	36.630580
1525.259298	197737.394268	36.635597
1527.220111	198059.639141	36.640615
1528.766463	198370.239318	36.645632
1530.668348	198676.212142	36.650650
1532.086669	198990.491490	36.655668
1533.640813	199285.597104	36.660685
1534.863188	199596.098034	36.665703
1536.317142	199890.102764	36.670720
1538.057153	200190.286785	36.675738
1538.801839	200501.219849	36.680756
1540.460443	200808.911388	36.685773
1541.755945	201116.965149	36.690791
1543.381344	201423.799330	36.695808
1544.935555	201738.824767	36.700826
1545.997871	202062.767803	36.705844
1547.740260	202369.178903	36.710861
1548.998006	202698.909677	36.715879
1550.585435	203021.832372	36.720896
1551.944630	203352.412135	36.725914
1553.265635	203692.930895	36.730932
1554.798733	204012.815487	36.735949
1556.399067	204355.349327	36.740967
1557.841139	204694.631577	36.745984
1559.385988	205035.117655	36.751002
1561.343921	205374.675957	36.756020
1563.367843	205699.694029	36.761037
1564.688352	206039.658015	36.766055
1566.732889	206370.135526	36.771072
1568.173931	206703.451519	36.776090
1570.181832	207029.159991	36.781108
1572.080026	207354.200222	36.786125
1573.793666	207687.119367	36.791143
1575.736906	208012.356700	36.796160
1577.642525	208327.845536	36.801178
1578.973557	208653.458988	36.806196
1581.111604	208968.607436	36.811213
1582.896077	209292.118496	36.816231
1584.229642	209599.366189	36.821248
1585.908107	209914.384500	36.826266
1587.073217	210243.480795	36.831284
1588.780618	210567.157896	36.836301
1590.399691	210887.521344	36.841319
1591.501322	211212.411742	36.846336
1593.193034	211538.200889	36.851354
1594.033895	211869.255066	36.856372
1596.079531	212194.329037	36.861389
1598.273904	212511.200112	36.866407
1600.145288	212836.505240	36.871424
1601.603660	213167.235494	36.876442
1603.058094	213498.093705	36.881460
1604.657895	213824.458430	36.886477
1606.493665	214146.874351	36.891495
1607.664998	214481.943983	36.896512
1609.090190	214810.089762	36.901530
1610.688000	215146.592046	36.906548
1612.443424	215485.203860	36.911565
1613.918736	215822.843633	36.916583
1614.862676	216162.522923	36.921600
1616.783454	216501.211264	36.926618
1618.086402	216859.430503	36.931636
1619.663493	217205.159193	36.936653
1621.310898	217562.689930	36.941671
1622.717749	217908.750576	36.946688
1624.817711	218243.703059	36.951706
1626.019444	218600.694512	36.956724
1628.066486	218947.874969	36.961741
1629.587078	219300.574452	36.966759
1630.653302	219656.215874	36.971776
1632.690505	220008.072737	36.976794
1633.873118	220367.151221	36.981812
1635.282165	220738.388352	36.986829
1637.176292	221096.720682	36.991847
1639.115945	221439.600357	36.996864
1641.263703	221768.729385	37.001882
1642.828065	222108.822742	37.006900
1644.365504	222436.726449	37.011917
1646.176274	222772.411906	37.016935
1647.867828	223104.762749	37.021952
1649.606582	223427.808370	37.026970
1650.802653	223769.280712	37.031988
1652.349650	224097.640476	37.037005
1654.082758	224439.841774	37.042023
1655.274694	224783.169354	37.047040
1657.018970	225141.094068	37.052058
1658.691068	225491.840724	37.057076
1660.453733	225836.374600	37.062093
1661.759293	226187.026165	37.067111
1663.435680	226546.130034	37.072128
1665.103179	226900.586306	37.077146
1666.728167	227270.571067	37.082164
1668.165090	227635.402761	37.087181
1669.971661	228002.869357	37.092199
1671.261112	228370.772444	37.097216
1672.749075	228748.475727	37.102234
1674.040313	229132.281237	37.107252
1675.891419	229516.608686	37.112269
1677.560983	229909.068271	37.117287
1679.194627	230296.096842	37.122304
1680.707000	230685.582988	37.127322
1681.782197	231094.774622	37.132340
1683.669477	231491.568813	37.137357
1685.407222	231892.501603	37.142375
1687.016273	232297.341070	37.147392
1688.899699	232700.232021	37.152410
1690.420799	233114.331685	37.157428
1692.382416	233532.375890	37.162445
1694.271999	233936.458894	37.167463
1695.847128	234351.438193	37.172480
1697.813088	234743.644944	37.177498
1700.034478	235147.217660	37.182516
1702.281799	235544.765231	37.187533
1704.476310	235932.667249	37.192551
1705.889359	236338.981830	37.197568
1708.008994	236717.342960	37.202586
1709.475574	237125.502746	37.207604
1711.492623	237519.070437	37.212621
1713.412120	237909.096426	37.217639
1714.515771	238304.584360	37.222656
1716.268341	238695.067363	37.227674
1718.057880	239108.407214	37.232692
1719.628340	239496.021669	37.237709
1721.514438	239899.463338	37.242727
1723.263245	240298.912173	37.247744
1725.234373	240693.498992	37.252762
1726.774115	241092.572903	37.257780
1728.528237	241486.252557	37.262797
1730.428295	241872.338596	37.267815
1732.267894	242280.889899	37.272832
1734.005223	242666.365057	37.277850
1735.725304	243072.545800	37.282868
1737.258080	243478.399490	37.287885
1738.853374	243875.885072	37.292903
1740.501368	244278.594694	37.297920
1742.122476	244669.876456	37.302938
1744.431163	245069.763073	37.307956
1745.469806	245472.133909	37.312973
1748.006939	245856.309697	37.317991
1749.534305	246278.391178	37.323008
1751.288793	246676.989551	37.328026
1753.210352	247056.864630	37.333044
1755.160272	247439.681195	37.338061
1757.600630	247813.326120	37.343079
1759.276134	248175.633459	37.348096
1761.035617	248529.442519	37.353114
1763.033430	248894.416000	37.358132
1764.868910	249247.525841	37.363149
1766.625728	249592.950379	37.368167
1768.423888	249967.199212	37.373184
1770.302513	250335.236485	37.378202
1771.573512	250696.230029	37.383220
1772.986801	251064.744890	37.388237
1774.850621	251437.430514	37.393255
1775.967892	251821.205683	37.398272
1777.556118	252200.714895	37.403290
1779.086178	252590.291352	37.408308
1780.651269	252985.017851	37.413325
1782.151150	253383.157312	37.418343
1783.333745	253783.733074	37.423360
1784.936403	254192.853080	37.428378
1786.986983	254615.313743	37.433396
1788.375510	255026.700141	37.438413
1790.822465	255446.403691	37.443431
1792.497069	255879.867220	37.448448
1794.188704	256298.314635	37.453466
1795.968354	256718.372607	37.458484
1797.740652	257142.367510	37.463501
1800.263383	257562.027040	37.468519
1801.927723	257990.277944	37.473536
1804.181813	258413.202555	37.478554
1806.387146	258833.440880	37.483572
1807.967243	259257.433257	37.488589
1810.207854	259660.797260	37.493607
1811.751648	260090.913847	37.498624
1813.735154	260505.973924	37.503642
1815.871505	260919.205185	37.508660
1817.810317	261345.521477	37.513677
1819.944464	261747.701059	37.518695
1821.739974	262165.095887	37.523712
1823.604553	262571.886638	37.528730
1825.375360	262979.985929	37.533748
1827.153589	263396.616767	37.538765
1829.545038	263804.793605	37.543783
1831.193928	264213.516851	37.548800
1832.642738	264639.490503	37.553818
1834.429822	265039.426140	37.558836
1836.020254	265472.663741	37.563853
1838.078549	265889.113780	37.568871
1839.254707	266319.364697	37.573888
1840.811382	266751.916289	37.578906
1842.697573	267179.436288	37.583924
1844.372176	267630.354129	37.588941
1846.192208	268059.734679	37.593959
1848.123833	268500.677438	37.598976
1850.222541	268932.550253	37.603994
1852.250022	269360.825695	37.609012
1853.656234	269814.873646	37.614029
1855.800689	270255.673178	37.619047
1857.590179	270683.700294	37.624064
1859.487206	271130.553509	37.629082
1861.617804	271577.596506	37.634100
1863.047160	272020.962767	37.639117
1865.015278	272466.680595	37.644135
1866.477941	272907.040255	37.649152
1868.447021	273362.150183	37.654170
1870.152414	273813.387830	37.659188
1871.646591	274263.437065	37.664205
1873.535122	274725.434687	37.669223
1875.307811	275192.628695	37.674240
1876.974041	275648.840145	37.679258
1879.069615	276089.845806	37.684276
1880.794232	276533.979991	37.689293
1882.796333	276967.909974	37.694311
1884.526915	277410.133630	37.699328
1886.695070	277849.264254	37.704346
1889.091338	278282.287215	37.709364
1890.818377	278726.535541	37.714381
1892.941429	279164.802272	37.719399
1894.563923	279609.823640	37.724416
1896.164088	280051.112837	37.729434
1898.237374	280495.220369	37.734452
1899.722510	280955.212590	37.739469
1901.416583	281411.563242	37.744487
1903.561017	281871.319550	37.749504
1905.437013	282329.261168	37.754522
1907.662207	282786.713516	37.759540
1909.093957	283250.737039	37.764557
1911.298720	283718.445561	37.769575
1913.052706	284187.084851	37.774592
1914.991220	284653.813005	37.779610
1917.269901	285128.635887	37.784628
1919.222017	285601.982990	37.789645
1920.744580	286069.655269	37.794663
1922.718890	286551.447945	37.799680
1924.813035	287027.124252	37.804698
1926.521910	287515.350286	37.809716
1927.945137	288002.804836	37.814733
1930.203033	288482.786949	37.819751
1931.926495	288971.355243	37.824768
1933.822192	289460.146771	37.829786
1935.799736	289957.833988	37.834804
1938.170698	290453.195931	37.839821
1940.023519	290946.578379	37.844839
1941.830713	291445.194475	37.849856
1943.687954	291951.872798	37.854874
1945.897310	292454.962613	37.859892
1948.048387	292947.520603	37.864909
1950.476632	293428.986715	37.869927
1952.564958	293927.360699	37.874944
1954.499927	294420.676656	37.879962
1956.852744	294904.833851	37.884980
1958.390479	295416.813712	37.889997
1960.418142	295905.659614	37.895015
1962.355508	296407.336605	37.900032
1963.904017	296898.737090	37.905050
1966.532047	297392.401660	37.910068
1968.466521	297902.164655	37.915085
1970.515335	298382.252614	37.920103
1972.824225	298887.225983	37.925120
1974.562908	299380.834437	37.930138
1976.785146	299869.767800	37.935156
1979.023064	300370.651382	37.940173
1981.079589	300854.169117	37.945191
1983.190662	301339.374845	37.950208
1985.688396	301822.560971	37.955226
1988.220635	302295.633841	37.960244
1989.826530	302766.613503	37.965261
1991.432216	303240.203650	37.970279
1993.615968	303728.676159	37.975296
1995.395691	304208.982655	37.980314
1997.193130	304695.856477	37.985332
1998.749582	305183.702600	37.990349
2000.543220	305671.329257	37.995367
2002.761414	306176.374164	38.000384
2004.309946	306672.812261	38.005402
2006.792007	307161.129050	38.010420
2008.353017	307649.559770	38.015437
2010.499675	308140.406923	38.020455
2012.394897	308618.495762	38.025472
2013.954543	309097.647717	38.030490
2015.851065	309572.351164	38.035508
2017.975363	310060.948860	38.040525
2020.312383	310537.756699	38.045543
2021.910127	311019.167914	38.050560
2023.330613	311515.069109	38.055578
2025.190344	312006.886232	38.060596
2027.153381	312514.950866	38.065613
2028.863566	313017.795851	38.070631
2031.041450	313519.826199	38.075648
2033.016705	314037.770384	38.080666
2035.226246	314556.636478	38.085684
2037.398168	315071.619574	38.090701
2039.347236	315597.087702	38.095719
2041.323794	316113.916757	38.100736
2042.890620	316642.427123	38.105754
2045.151026	317163.234750	38.110772
2047.041691	317698.813043	38.115789
2049.251857	318236.263503	38.120807
2051.425922	318765.059509	38.125824
2053.610210	319309.377940	38.130842
2055.452040	319850.215813	38.135860
2057.650124	320396.472349	38.140877
2059.599429	320935.351168	38.145895
2061.831490	321478.238968	38.150912
2063.875506	322037.236925	38.155930
2066.190873	322586.288914	38.160948
2068.046477	323123.657347	38.165965
2070.378845	323669.546011	38.170983
2072.595024	324219.378556	38.176000
2074.454480	324780.779018	38.181018
2076.759996	325317.794749	38.186036
2079.014981	325868.081151	38.191053
2081.201957	326424.612275	38.196071
2083.722610	326978.165733	38.201088
2085.735236	327532.526789	38.206106
2088.138578	328071.545556	38.211124
2090.233118	328624.483133	38.216141
2092.208349	329182.378852	38.221159
2094.424480	329724.220405	38.226176
2096.803133	330270.012046	38.231194
2099.071138	330807.771214	38.236212
2101.015223	331366.705963	38.241229
2103.177021	331909.235722	38.246247
2105.547500	332450.405966	38.251264
2107.639392	332993.489309	38.256282
2110.203967	333532.685756	38.261300
2112.659123	334069.177292	38.266317
2115.122214	334594.194071	38.271335
2117.231571	335119.461716	38.276352
2119.170603	335646.067597	38.281370
2121.471691	336158.505939	38.286388
2123.840888	336688.022762	38.291405
2125.581438	337232.544903	38.296423
2127.828903	337764.956728	38.301440
2129.640149	338304.962154	38.306458
2131.564629	338832.386628	38.311476
2132.924954	339378.229432	38.316493
2135.130532	339926.214326	38.321511
2137.442786	340474.757409	38.326528
2138.861236	341025.663689	38.331546
2141.067247	341572.938173	38.336564
2143.505802	342122.729228	38.341581
2145.687699	342675.924784	38.346599
2148.050748	343218.406289	38.351616
2149.862229	343775.699910	38.356634
2152.438489	344316.152638	38.361652
2154.172753	344848.740285	38.366669
2156.009098	345383.281635	38.371687
2158.145039	345904.885431	38.376704
2160.464490	346435.327870	38.381722
2162.684305	346957.282595	38.386740
2165.042209	347488.006635	38.391757
2167.395194	348024.301549	38.396775
2169.473743	348562.253542	38.401792
2171.457745	349099.704423	38.406810
2173.329526	349639.091111	38.411828
2175.415306	350182.644430	38.416845
2177.624202	350733.750569	38.421863
2179.499286	351277.927036	38.426880
2181.182412	351840.607557	38.431898
2182.956582	352405.697936	38.436916
2185.208348	352976.915165	38.441933
2187.165377	353566.954688	38.446951
2189.503432	354135.450177	38.451968
2191.047091	354725.253872	38.456986
2193.211837	355311.374777	38.462004
2195.543919	355907.573528	38.467021
2197.399950	356498.055426	38.472039
2200.057235	357102.191088	38.477056
2202.375669	357712.882721	38.482074
2204.864576	358304.016844	38.487092
2207.025728	358907.205964	38.492109
2209.049627	359512.128249	38.497127
2211.229072	360129.941298	38.502144
2213.472600	360746.971243	38.507162
2215.880285	361357.955718	38.512180
2218.174875	361972.595182	38.517197
2220.175212	362604.122610	38.522215
2222.972786	363213.360487	38.527232
2225.003677	363834.135959	38.532250
2227.068503	364456.388256	38.537268
2229.428714	365083.016131	38.542285
2231.328225	365720.701259	38.547303
2234.229625	366343.542531	38.552320
2236.762563	366972.281856	38.557338
2239.508139	367585.566808	38.562356
2241.814285	368213.249997	38.567373
2244.063777	368827.827467	38.572391
2246.581587	369442.932410	38.577408
2248.416398	370064.870871	38.582426
2250.582807	370690.721759	38.587444
2252.796778	371313.333297	38.592461
2254.771991	371945.697667	38.597479
2257.278388	372578.749921	38.602496
2259.205498	373203.466734	38.607514
2261.890881	373836.487361	38.612532
2264.294384	374455.476640	38.617549
2266.257499	375091.519935	38.622567
2268.815168	375714.205840	38.627584
2270.929820	376354.857073	38.632602
2273.140596	376986.130349	38.637620
2275.609667	377614.663150	38.642637
2278.135313	378253.152740	38.647655
2280.360475	378870.573613	38.652672
2282.479353	379511.730845	38.657690
2285.085841	380142.107191	38.662708
2287.516807	380771.811943	38.667725
2289.294886	381409.354025	38.672743
2291.360151	382032.322886	38.677760
2293.729107	382678.783232	38.682778
2295.676234	383311.110652	38.687796
2298.666217	383939.181931	38.692813
2300.635903	384588.898287	38.697831
2302.728949	385214.647260	38.702848
2305.123446	385846.740532	38.707866
2306.595701	386451.587976	38.712884
2309.211142	387073.461344	38.717901
2311.383550	387707.087272	38.722919
2313.525484	388333.257444	38.727936
2315.589224	388967.678578	38.732954
2317.740514	389588.245087	38.737972
2319.924842	390213.854671	38.742989
2321.891110	390864.851694	38.748007
2324.092106	391513.566706	38.753024
2326.492685	392167.904298	38.758042
2328.789225	392823.253190	38.763060
2331.456009	393478.323878	38.768077
2333.691854	394146.861206	38.773095
2335.959765	394795.528331	38.778112
2338.872460	395468.631365	38.783130
2341.321691	396116.221647	38.788148
2343.724588	396776.812056	38.793165
2346.214082	397444.558952	38.798183
2348.834043	398101.939614	38.803200
2351.081572	398760.574978	38.808218
2353.382479	399419.993313	38.813236
2356.202108	400090.852618	38.818253
2358.382248	400756.174129	38.823271
2360.298319	401431.337006	38.828288
2362.878104	402106.224390	38.833306
2365.003468	402778.986654	38.838324
2367.742010	403458.971632	38.843341
2370.037625	404137.234231	38.848359
2372.093667	404826.596935	38.853376
2374.139220	405504.047886	38.858394
2376.504835	406212.397998	38.863412
2379.179008	406913.997891	38.868429
2381.225627	407618.102686	38.873447
2383.725977	408310.324551	38.878464
2385.868226	409014.875971	38.883482
2388.722791	409720.102958	38.888500
2392.084937	410395.124207	38.893517
2394.816782	411092.838177	38.898535
2397.802069	411772.732623	38.903552
2400.645336	412462.796472	38.908570
2402.697322	413132.423314	38.913588
2405.597978	413811.912692	38.918605
2408.201810	414496.434861	38.923623
2410.399399	415168.099922	38.928640
2412.979140	415856.730018	38.933658
2414.775699	416536.355868	38.938676
2417.431108	417221.186828	38.943693
2419.433975	417902.759520	38.948711
2421.592493	418586.966203	38.953728
2423.960089	419277.085447	38.958746
2426.360254	419974.105050	38.963764
2429.024895	420662.513545	38.968781
2430.958752	421353.187864	38.973799
2433.773972	422046.684601	38.978816
2436.168087	422746.544383	38.983834
2438.261287	423450.826280	38.988852
2441.137031	424142.321091	38.993869
2443.053137	424845.368939	38.998887
2445.036041	425550.151442	39.003904
2447.955174	426270.435262	39.008922
2450.115186	426974.078521	39.013940
2452.602341	427689.525716	39.018957
2454.451359	428416.016555	39.023975
2456.742284	429131.189881	39.028992
2459.066323	429859.120584	39.034010
2461.330406	430586.477811	39.039028
2463.242345	431309.617573	39.044045
2465.795154	432039.857815	39.049063
2468.088370	432755.101108	39.054080
2470.482186	433462.620636	39.059098
2472.387104	434187.878329	39.064116
2474.763547	434903.383062	39.069133
2477.013305	435632.069855	39.074151
2479.747356	436360.198436	39.079168
2481.973700	437102.021265	39.084186
2484.557653	437853.813949	39.089204
2486.987321	438598.527595	39.094221
2489.270488	439353.541320	39.099239
2491.934752	440102.806922	39.104256
2494.619068	440860.627533	39.109274
2496.727077	441626.135479	39.114292
2499.407986	442390.057463	39.119309
2501.695133	443160.879197	39.124327
2504.065586	443931.706287	39.129344
2506.771206	444720.176856	39.134362
2509.378482	445496.356141	39.139380
2512.046626	446273.200017	39.144397
2514.305056	447070.578288	39.149415
2516.872366	447861.863881	39.154432
2519.841346	448646.285498	39.159450
2522.063781	449439.525277	39.164468
2524.743639	450234.122757	39.169485
2527.945824	451042.588960	39.174503
2530.646267	451835.243870	39.179520
2533.089312	452615.282328	39.184538
2535.558083	453418.555123	39.189556
2538.062189	454218.908410	39.194573
2540.396172	455017.737506	39.199591
2542.571745	455829.779709	39.204608
2545.326044	456643.611618	39.209626
2547.437241	457462.199862	39.214644
2550.464694	458280.858470	39.219661
2552.947592	459106.729681	39.224679
2555.734181	459922.269499	39.229696
2558.055105	460744.251986	39.234714
2560.629195	461570.192062	39.239732
2563.381854	462404.389502	39.244749
2565.893291	463228.240462	39.249767
2568.938420	464051.261441	39.254784
2571.775497	464874.829653	39.259802
2574.050982	465705.709626	39.264820
2577.005127	466534.827924	39.269837
2579.445284	467360.202177	39.274855
2582.240414	468189.918531	39.279872
2585.112727	469015.495784	39.284890
2587.468742	469839.296781	39.289908
2590.286079	470665.657187	39.294925
2592.855992	471495.746323	39.299943
2595.332047	472329.640312	39.304960
2598.216377	473142.047804	39.309978
2600.652604	473975.913813	39.314996
2603.496518	474799.034562	39.320013
2606.584378	475621.268361	39.325031
2608.980076	476443.568225	39.330048
2611.647321	477258.372832	39.335066
2614.380958	478093.238408	39.340084
2617.272388	478907.721747	39.345101
2619.390043	479718.755905	39.350119
2622.318390	480552.453112	39.355136
2625.182110	481374.020619	39.360154
2627.570223	482193.805151	39.365172
2630.091695	483016.902077	39.370189
2632.626404	483843.984580	39.375207
2635.186643	484653.937594	39.380224
2638.365386	485474.382615	39.385242
2640.307292	486264.193824	39.390260
2642.700624	487063.566691	39.395277
2645.512759	487852.706519	39.400295
2647.754072	488644.615009	39.405312
2650.629060	489439.304718	39.410330
2652.735754	490248.831066	39.415348
2655.507873	491041.941628	39.420365
2657.853177	491857.942318	39.425383
2659.811655	492673.254111	39.430400
2662.856452	493497.718230	39.435418
2665.041964	494327.910974	39.440436
2667.422580	495164.723756	39.445453
2669.958244	496004.939184	39.450471
2672.194475	496864.990299	39.455488
2675.171983	497716.820250	39.460506
2677.719037	498583.115919	39.465524
2680.255076	499453.288372	39.470541
2682.831477	500319.224795	39.475559
2685.178907	501192.544221	39.480576
2688.378391	502079.316848	39.485594
2690.589150	502975.197923	39.490612
2693.182656	503865.427894	39.495629
2695.851969	504780.398188	39.500647
2698.057683	505686.577097	39.505664
2701.226487	506598.736232	39.510682
2704.046507	507519.091765	39.515700
2706.253401	508432.691953	39.520717
2709.202577	509348.481113	39.525735
2712.129603	510282.623769	39.530752
2714.980808	511205.248386	39.535770
2717.576196	512148.069828	39.540788
2721.036239	513064.692386	39.545805
2724.509202	513993.823887	39.550823
2726.924585	514923.510828	39.555840
2730.060317	515845.580973	39.560858
2733.026348	516772.794142	39.565876
2735.705734	517688.024357	39.570893
2738.707886	518613.548416	39.575911
2741.039126	519542.582700	39.580928
2744.301354	520464.069337	39.585946
2746.892536	521398.866389	39.590964
2749.721133	522327.078396	39.595981
2752.485423	523248.502425	39.600999
2755.038945	524183.312268	39.606016
2757.941373	525106.596321	39.611034
2761.261261	526035.026253	39.616052
2764.245785	526953.295401	39.621069
2767.146888	527885.629586	39.626087
2770.103421	528797.545439	39.631104
2772.854179	529716.311199	39.636122
2776.019929	530638.262240	39.641140
2778.883148	531547.740656	39.646157
2782.186451	532455.429384	39.651175
2784.519210	533362.704090	39.656192
2787.839721	534260.521921	39.661210
2790.939473	535170.812990	39.666228
2793.362692	536072.911973	39.671245
2796.123449	536982.876208	39.676263
2798.762936	537891.338764	39.681280
2801.491384	538786.170589	39.686298
2804.124769	539700.929110	39.691316
2806.815663	540611.095741	39.696333
2809.963336	541516.608830	39.701351
2812.334324	542443.804593	39.706368
2814.854477	543359.468696	39.711386
2817.635924	544274.824053	39.716404
2820.231916	545197.114184	39.721421
2823.228073	546095.094675	39.726439
2825.551764	547003.447883	39.731456
2828.299659	547888.947380	39.736474
2830.731351	548781.303332	39.741492
2833.651922	549671.812814	39.746509
2836.589748	550564.410904	39.751527
2839.072893	551465.338077	39.756544
2842.106618	552364.457807	39.761562
2844.874159	553278.993489	39.766580
2847.507449	554190.122222	39.771597
2850.776580	555107.999928	39.776615
2853.337464	556032.033064	39.781632
2856.199406	556944.119929	39.786650
2859.024783	557874.685046	39.791668
2861.205923	558818.006116	39.796685
2864.094319	559758.285532	39.801703
2866.761601	560708.946021	39.806720
2869.361719	561655.833108	39.811738
2871.814553	562616.643206	39.816756
2874.382178	563582.616036	39.821773
2877.296851	564557.720605	39.826791
2879.765693	565549.340153	39.831808
2882.990168	566543.010344	39.836826
2885.885904	567543.256255	39.841844
2888.716362	568553.339232	39.846861
2891.410212	569554.243227	39.851879
2894.971521	570556.175715	39.856896
2898.113808	571555.733302	39.861914
2901.505899	572557.366397	39.866932
2904.481379	573561.328511	39.871949
2907.174283	574567.247506	39.876967
2910.437635	575579.842840	39.881984
2913.814715	576584.173908	39.887002
2916.940647	577592.806842	39.892020
2919.690281	578603.908885	39.897037
2923.144755	579610.307302	39.902055
2925.897820	580615.623969	39.907072
2928.516446	581625.621490	39.912090
2931.478120	582645.124205	39.917108
2934.232125	583665.365080	39.922125
2936.938000	584675.019450	39.927143
2940.033799	585710.015643	39.932160
2943.287705	586729.742888	39.937178
2946.064203	587752.348224	39.942196
2949.049997	588779.022601	39.947213
2952.158557	589795.036042	39.952231
2955.189282	590829.454206	39.957248
2958.141394	591866.433214	39.962266
2960.848172	592894.207852	39.967284
2963.881158	593937.468187	39.972301
2967.288358	594973.275324	39.977319
2970.074358	596008.129650	39.982336
2973.358577	597039.708732	39.987354
2975.869783	598088.685004	39.992372
2978.973356	599133.070367	39.997389
2982.318374	600158.193044	40.002407
2985.327552	601194.200146	40.007424
2988.744366	602229.042339	40.012442
2991.879405	603257.936309	40.017460
2994.750824	604285.421997	40.022477
2997.807967	605317.267511	40.027495
3000.614780	606357.630756	40.032512
3003.419284	607385.316927	40.037530
3006.694121	608423.052834	40.042548
3009.148325	609468.792370	40.047565
3012.535582	610489.790429	40.052583
3015.188952	611535.735254	40.057600
3018.165595	612575.388265	40.062618
3021.092424	613608.659821	40.067636
3023.999940	614630.212432	40.072653
3026.915933	615636.655290	40.077671
3029.476698	616658.653667	40.082688
3032.425783	617658.258647	40.087706
3035.201058	618676.777120	40.092724
3038.381026	619700.210362	40.097741
3041.361318	620721.227332	40.102759
3044.054230	621762.110943	40.107776
3047.286746	622790.396722	40.112794
3050.401009	623816.949621	40.117812
3053.267031	624872.070094	40.122829
3056.162557	625910.041325	40.127847
3059.257861	626967.886902	40.132864
3061.980377	628023.235944	40.137882
3065.041378	629078.566328	40.142900
3068.132732	630158.564647	40.147917
3071.124825	631219.694093	40.152935
3074.392622	632302.011897	40.157952
3077.369509	633392.910699	40.162970
3080.366169	634473.084306	40.167988
3083.841337	635568.233278	40.173005
3086.779478	636648.218359	40.178023
3090.094281	637746.771530	40.183040
3093.459561	638840.215810	40.188058
3096.452809	639935.629742	40.193076
3099.043550	641048.678251	40.198093
3101.989917	642164.968746	40.203111
3105.258221	643279.683398	40.208128
3107.804231	644407.647179	40.213146
3111.414049	645531.381454	40.218164
3113.844204	646670.218897	40.223181
3117.172146	647807.980228	40.228199
3120.065966	648954.311983	40.233216
3123.259758	650109.989797	40.238234
3126.559742	651265.752959	40.243252
3129.580046	652421.413019	40.248269
3132.450319	653580.474480	40.253287
3135.791806	654751.079348	40.258304
3139.198741	655919.735038	40.263322
3142.496954	657085.774225	40.268340
3145.274243	658262.412423	40.273357
3148.936542	659429.032177	40.278375
3151.801081	660614.178561	40.283392
3155.195275	661792.436944	40.288410
3158.174349	662982.011022	40.293428
3160.984607	664171.599977	40.298445
3164.145001	665350.411846	40.303463
3167.353211	666541.650722	40.308480
3170.732091	667738.996262	40.313498
3174.189778	668932.943407	40.318516
3177.393304	670135.686726	40.323533
3180.815828	671324.503365	40.328551
3184.357755	672514.921401	40.333568
3187.600569	673704.775911	40.338586
3191.124881	674882.831533	40.343604
3194.521706	676074.859272	40.348621
3197.916622	677252.559196	40.353639
3201.435947	678434.928756	40.358656
3204.593766	679622.189970	40.363674
3207.818766	680786.654547	40.368692
3211.200657	681962.217493	40.373709
3214.654318	683131.073385	40.378727
3217.952345	684305.727860	40.383744
3221.067748	685463.525698	40.388762
3224.845759	686621.455007	40.393780
3228.081236	687774.461432	40.398797
3231.585156	688927.957950	40.403815
3234.357377	690071.668189	40.408832
3237.410764	691197.379664	40.413850
3240.558274	692308.242466	40.418868
3243.482692	693430.010629	40.423885
3246.133616	694553.743206	40.428903
3249.254524	695685.053956	40.433920
3252.016776	696821.450585	40.438938
3254.875766	697944.731972	40.443956
3257.801715	699104.886878	40.448973
3260.622174	700269.730746	40.453991
3263.676182	701449.181188	40.459008
3266.281397	702628.429809	40.464026
3269.800334	703819.701254	40.469044
3272.725328	705011.924138	40.474061
3275.596382	706217.200717	40.479079
3278.668801	707428.331035	40.484096
3281.928870	708664.058347	40.489114
3285.104738	709903.698866	40.494132
3288.158175	711149.672400	40.499149
3291.433166	712401.231304	40.504167
3295.019314	713656.879381	40.509184
3298.241490	714922.880542	40.514202
3301.847115	716182.554263	40.519220
3305.064943	717458.392931	40.524237
3308.431144	718730.303101	40.529255
3311.681591	720009.114289	40.534272
3314.805509	721300.684498	40.539290
3317.922105	722585.243204	40.544308
3321.307137	723886.233130	40.549325
3324.333149	725188.435195	40.554343
3327.904490	726502.139991	40.559360
3331.150801	727815.274009	40.564378
3334.434777	729137.717816	40.569396
3337.475618	730461.295323	40.574413
3340.900334	731798.742889	40.579431
3344.819570	733123.974825	40.584448
3347.406650	734469.384823	40.589466
3350.764501	735812.907173	40.594484
3354.436014	737169.651410	40.599501
3358.051030	738518.441250	40.604519
3361.745148	739865.154118	40.609536
3364.882811	741220.940899	40.614554
3368.514520	742573.403868	40.619572
3372.154977	743925.958560	40.624589
3375.779009	745271.441048	40.629607
3378.920444	746620.234133	40.634624
3382.575207	747990.826373	40.639642
3385.993701	749344.367003	40.644660
3389.388458	750696.724534	40.649677
3392.546770	752055.877020	40.654695
3396.733246	753404.215181	40.659712
3399.859014	754758.150776	40.664730
3403.730883	756104.212410	40.669748
3407.216290	757458.164534	40.674765
3410.580365	758806.535431	40.679783
3414.262758	760155.529079	40.684800
3417.424539	761506.108038	40.689818
3420.903957	762854.320077	40.694836
3424.695732	764203.789467	40.699853
3427.632934	765560.277228	40.704871
3431.483193	766904.660519	40.709888
3434.784809	768250.825434	40.714906
3438.186540	769605.224056	40.719924
3441.446817	770944.558084	40.724941
3444.618663	772297.874517	40.729959
3448.361747	773657.776314	40.734976
3451.572469	775012.944001	40.739994
3455.048111	776367.555693	40.745012
3458.810257	777707.843995	40.750016
3461.700692	779008.070254	40.755021
3465.567791	780256.965823	40.760026
3468.228851	781443.687921	40.765031
3471.487532	782574.154995	40.770036
3474.531237	783654.835761	40.775040
3477.544888	784662.871830	40.780045
3480.162872	785617.973638	40.785050
3482.490522	786513.102378	40.790055
3485.170154	787346.812008	40.795060
3487.522203	788125.101017	40.800064
3489.676297	788841.317417	40.805069
3492.012641	789506.033278	40.810074
3493.500551	790117.616029	40.815079
3495.550131	790668.868461	40.820084
3497.652293	791195.426909	40.825088
3499.473928	791651.055783	40.830093
3501.007387	792060.651781	40.835098
3502.038763	792452.508857	40.840103
3503.865015	792766.114396	40.845108
3505.269186	793056.702330	40.850112
3506.185372	793303.955203	40.855117
3507.316635	793521.451821	40.860122
3508.024184	793727.034510	40.865127
3508.941234	793883.417033	40.870132
3510.019682	794019.490844	40.875136
3510.759692	794122.581299	40.880141
3511.563574	794202.839977	40.885146
3512.156481	794268.813208	40.890151
3512.618287	794304.998829	40.895156
3513.390483	794321.003528	40.900160
3513.968860	794319.007454	40.905165
3514.274726	794299.022892	40.910170
3514.416616	794253.800674	40.915175
3515.008690	794204.305337	40.920180
3515.131464	794143.985887	40.925184
3515.546586	794071.599031	40.930189
3516.250366	793979.668272	40.935194
3515.855097	793875.739913	40.940199
3516.368595	793767.465126	40.945204
3516.644338	793656.489015	40.950208
3516.573597	793525.968109	40.955213
3517.091745	793383.916586	40.960218
3517.013127	793249.041805	40.965223
3517.218854	793091.882240	40.970228
3517.011222	792936.152017	40.975232
3517.313944	792789.575894	40.980237
3517.589525	792616.851391	40.985242
3517.722660	792446.637413	40.990247
3517.890103	792264.633581	40.995252
3517.852793	792081.239143	41.000256
3517.357252	791896.346958	41.005261
3518.049777	791699.287214	41.010266
3517.901448	791512.374559	41.015271
3517.745766	791309.569435	41.020276
3518.005648	791108.795295	41.025280
3517.587383	790914.476741	41.030285
3517.743234	790704.075150	41.035290
3517.603847	790505.398441	41.040295
3517.272101	790289.290412	41.045300
3517.601367	790086.127255	41.050304
3517.388170	789869.840231	41.055309
3517.094802	789669.646528	41.060314
3517.111734	789458.199942	41.065319
3517.404576	789250.077711	41.070324
3517.079583	789039.698106	41.075328
3516.844086	788837.416114	41.080333
3516.894286	788624.128088	41.085338
3516.503313	788408.456707	41.090343
3516.692048	788202.225154	41.095348
3516.672950	787994.650128	41.100352
3516.332746	787792.841631	41.105357
3516.203972	787579.939191	41.110362
3516.104112	787378.276135	41.115367
3516.034079	787169.411358	41.120372
3515.540838	786967.699455	41.125376
3515.381788	786769.891749	41.130381
3515.461829	786567.735609	41.135386
3515.645287	786371.183371	41.140391
3515.450036	786160.104800	41.145396
3515.452853	785965.525798	41.150400
3515.103693	785765.026882	41.155405
3515.210898	785563.618770	41.160410
3514.967503	785371.898789	41.165415
3514.882323	785169.725920	41.170420
3514.801083	784973.663043	41.175424
3514.356522	784779.510731	41.180429
3514.301172	784591.115395	41.185434
3514.348763	784398.783581	41.190439
3514.194112	784204.422366	41.195444
3514.177079	784019.822179	41.200448
3513.898651	783837.851688	41.205453
3513.707854	783660.707954	41.210458
3513.379639	783474.281454	41.215463
3513.323176	783289.863014	41.220468
3513.296070	783107.050165	41.225472
3513.064648	782937.725226	41.230477
3513.116678	782765.365724	41.235482
3512.607481	782596.467162	41.240487
3512.591241	782413.780510	41.245492
3512.611349	782245.818359	41.250496
3512.451983	782079.250796	41.255501
3512.298796	781904.698219	41.260506
3512.244429	781748.435826	41.265511
3512.010247	781582.014465	41.270516
3512.600950	781414.578742	41.275520
3511.830553	781259.298159	41.280525
3511.671785	781092.412204	41.285530
3511.371809	780941.310447	41.290535
3511.561915	780777.789578	41.295540
3511.669313	780618.831486	41.300544
3511.192191	780471.468251	41.305549
3511.240144	780323.872797	41.310554
3511.015452	780175.190433	41.315559
3511.357043	780015.544866	41.320564
3511.274480	779864.972555	41.325568
3510.624812	779713.897855	41.330573
3510.695267	779565.008946	41.335578
3510.843013	779430.258318	41.340583
3510.236686	779288.668347	41.345588
3510.347822	779145.836779	41.350592
3510.222021	779011.806215	41.355597
3510.061305	778859.313505	41.360602
3509.941268	778724.247770	41.365607
3509.860645	778595.148803	41.370612
3510.275771	778473.757931	41.375616
3509.843616	778335.255512	41.380621
3509.916398	778196.573349	41.385626
3509.837318	778071.382801	41.390631
3509.366304	777940.666874	41.395636
3509.663624	777814.482004	41.400640
3509.485809	777688.320066	41.405645
3509.587426	777554.910839	41.410650
3509.205407	777433.282970	41.415655
3508.816302	777310.968161	41.420660
3509.110706	777186.241723	41.425664
3508.419852	777066.860127	41.430669
3508.984453	776947.231173	41.435674
3508.409039	776841.741425	41.440679
3508.636584	776718.731594	41.445684
3508.622120	776609.426977	41.450688
3507.919517	776496.063526	41.455693
3508.083496	776387.413373	41.460698
3508.470800	776284.067282	41.465703
3508.195574	776168.279664	41.470708
3508.627781	776065.168211	41.475712
3508.256240	775955.810877	41.480717
3508.232817	775836.450251	41.485722
3508.123011	775734.251510	41.490727
3507.371971	775620.733982	41.495732
3507.598087	775515.441301	41.500736
3507.050068	775429.477407	41.505741
3507.497505	775331.742822	41.510746
3507.335443	775245.765272	41.515751
3507.376924	775146.082280	41.520756
3507.265074	775046.225770	41.525760
3507.050342	774949.324295	41.530765
3507.509911	774854.423359	41.535770
3506.796462	774770.633322	41.540775
3507.008061	774676.013702	41.545780
3506.950884	774585.698620	41.550784
3506.666925	774503.994577	41.555789
3506.926045	774405.246910	41.560794
3506.690431	774324.758429	41.565799
3506.758229	774233.634955	41.570804
3506.666175	774139.643496	41.575808
3506.523123	774061.980181	41.580813
3506.442020	773979.306875	41.585818
3506.370391	773896.042910	41.590823
3506.130712	773807.951695	41.595828
3506.472632	773722.807404	41.600832
3506.087357	773642.677368	41.605837
3506.484119	773556.248000	41.610842
3505.959004	773494.421397	41.615847
3506.011213	773409.122410	41.620852
3506.159761	773333.954154	41.625856
3505.948030	773258.155123	41.630861
3505.825639	773177.635392	41.635866
3505.918061	773108.944032	41.640871
3505.720919	773034.561822	41.645876
3505.953269	772955.258553	41.650880
3505.232988	772893.015811	41.655885
3505.714042	772822.447013	41.660890
3505.500961	772760.712044	41.665895
3505.482892	772691.837671	41.670900
3505.268865	772619.757671	41.675904
3505.582892	772554.555802	41.680909
3505.373111	772473.109965	41.685914
3505.258367	772404.394882	41.690919
3504.997549	772347.222987	41.695924
3505.320393	772276.624265	41.700928
3505.316449	772215.341937	41.705933
3505.103801	772150.120492	41.710938
3504.873737	772096.128449	41.715943
3504.818374	772031.910866	41.720948
3504.977014	771965.403921	41.725952
3504.971131	771903.628820	41.730957
3505.131377	771841.778163	41.735962
3504.749121	771788.837100	41.740967
3504.846863	771731.358856	41.745972
3504.773122	771666.307204	41.750976
3504.534286	771614.126859	41.755981
3504.869847	771566.171077	41.760986
3504.933548	771507.715652	41.765991
3504.771608	771452.972409	41.770996
3504.684200	771387.282827	41.776000
3504.186658	771342.005402	41.781005
3504.698537	771280.585040	41.786010
3504.407633	771229.390568	41.791015
3504.336271	771175.317417	41.796020
3504.391018	771126.029502	41.801024
3504.239092	771074.861184	41.806029
3504.327629	771018.310060	41.811034
3504.115921	770966.071500	41.816039
3504.224012	770923.736839	41.821044
3504.085438	770868.592987	41.826048
3503.922673	770829.487442	41.831053
3504.264395	770783.192467	41.836058
3504.046493	770746.841134	41.841063
3503.972084	770680.505264	41.846068
3503.881923	770632.560471	41.851072
3504.122621	770596.872223	41.856077
3504.344155	770547.063694	41.861082
3503.790293	770493.796175	41.866087
3503.977904	770443.648926	41.871092
3503.756181	770399.204859	41.876096
3503.673519	770362.487070	41.881101
3503.621256	770321.792079	41.886106
3503.657051	770290.302683	41.891111
3503.636359	770244.158812	41.896116
3503.622724	770210.126657	41.901120
3503.597815	770172.418004	41.906125
3504.053129	770133.211871	41.911130
3503.856165	770081.209476	41.916135
3503.890468	770036.968250	41.921140
3503.725734	769993.934874	41.926144
3503.324896	769949.319723	41.931149
3503.089522	769905.953537	41.936154
3503.183253	769890.588426	41.941159
3503.317180	769849.027794	41.946164
3503.312466	769808.518505	41.951168
3503.356179	769776.927431	41.956173
3503.531384	769731.485156	41.961178
3503.507187	769707.211987	41.966183
3503.271829	769670.808638	41.971188
3503.313087	769639.756811	41.976192
3502.878172	769611.721995	41.981197
3503.085051	769559.750615	41.986202
3503.301962	769541.913188	41.991207
3503.132976	769504.762898	41.996212
3503.229545	769480.224820	42.001216
3503.074721	769447.093789	42.006221
3503.106074	769410.500230	42.011226
3503.369478	769380.099158	42.016231
3503.360168	769346.160145	42.021236
3503.293990	769306.197024	42.026240
3502.978334	769273.041250	42.031245
3503.218433	769241.171779	42.036250
3503.198132	769224.842050	42.041255
3502.702875	769176.754233	42.046260
3502.981301	769143.406868	42.051264
3503.117645	769114.495945	42.056269
3503.010809	769085.917208	42.061274
3503.075855	769057.115287	42.066279
3503.115112	769037.930951	42.071284
3502.797156	768998.888293	42.076288
3502.621949	768977.677231	42.081293
3503.020103	768942.642488	42.086298
3502.806812	768918.052745	42.091303
3502.620510	768896.303615	42.096308
3502.856436	768858.792238	42.101312
3502.795991	768843.203638	42.106317
3503.003354	768816.487645	42.111322
3502.741698	768785.479318	42.116327
3502.668375	768761.553851	42.121332
3502.924483	768733.505531	42.126336
3502.489656	768707.919586	42.131341
3502.495171	768676.672797	42.136346
3502.835347	768658.813819	42.141351
3502.819291	768633.996020	42.146356
3502.612056	768592.922610	42.151360
3502.547194	768581.797885	42.156365
3502.812934	768555.464176	42.161370
3502.694980	768526.394328	42.166375
3502.708421	768502.895876	42.171380
3502.688944	768482.296634	42.176384
3502.612853	768458.664868	42.181389
3502.801673	768425.328041	42.186394
3502.573506	768408.636442	42.191399
3502.401496	768384.528878	42.196404
3502.330291	768359.865876	42.201408
3502.387822	768328.609378	42.206413
3502.588523	768313.469301	42.211418
3502.480903	768301.320662	42.216423
3502.683550	768270.924201	42.221428
3502.498868	768245.935147	42.226432
3502.105514	768226.570906	42.231437
3502.474202	768212.876000	42.236442
3502.427687	768189.533020	42.241447
3502.557043	768169.351075	42.246452
3502.656382	768149.762433	42.251456
3502.357308	768118.413562	42.256461
3502.282664	768091.886016	42.261466
3502.269787	768067.703411	42.266471
3502.409136	768045.017674	42.271476
3502.649366	768016.380247	42.276480
3502.496918	768009.094702	42.281485
3502.478827	767988.346599	42.286490
3502.610991	767965.171155	42.291495
3502.240346	767954.583787	42.296500
3502.489111	767923.737076	42.301504
3501.946755	767908.663211	42.306509
3502.545506	767880.655980	42.311514
3502.206235	767860.644507	42.316519
3502.226582	767835.572857	42.321524
3502.230741	767818.401989	42.326528
3502.510626	767809.233502	42.331533
3502.218232	767787.252165	42.336538
3502.253160	767769.732958	42.341543
3502.099210	767761.956803	42.346548
3502.180911	767739.180956	42.351552
3502.274090	767727.539561	42.356557
3502.129655	767696.360832	42.361562
3502.292890	767685.346180	42.366567
3501.988740	767664.151231	42.371572
3502.044290	767655.213846	42.376576
3501.827845	767640.431860	42.381581
3502.056322	767621.312124	42.386586
3501.983713	767615.191107	42.391591
3502.220567	767601.172186	42.396596
3502.052290	767583.586154	42.401600
3501.868084	767561.145646	42.406605
3502.000621	767545.965485	42.411610
3501.688808	767541.844192	42.416615
3501.978420	767529.828338	42.421620
3501.896351	767512.032407	42.426624
3501.476989	767512.343323	42.431629
3501.844334	767495.212998	42.436634
3501.985936	767468.894555	42.441639
3501.920738	767471.554072	42.446644
3502.037123	767447.594392	42.451648
3502.034259	767440.971711	42.456653
3502.205998	767424.313334	42.461658
3501.922178	767407.039279	42.466663
3502.175245	767394.685477	42.471668
3502.415375	767371.491165	42.476672
3502.180460	767359.557011	42.481677
3502.148451	767339.545054	42.486682
3501.868287	767324.576105	42.491687
3501.964426	767308.763314	42.496692
3501.873078	767286.798015	42.501696
3502.017390	767286.530206	42.506701
3501.990680	767265.535970	42.511706
3501.906825	767260.054201	42.516711
3501.983750	767250.327960	42.521716
3502.295346	767231.930087	42.526720
3502.116310	767214.884481	42.531725
3502.167753	767192.307812	42.536730
3501.740489	767184.819043	42.541735
3501.760874	767162.296194	42.546740
3501.599223	767155.060246	42.551744
3501.779159	767149.978717	42.556749
3501.782913	767145.856919	42.561754
3502.168322	767129.311619	42.566759
3501.593665	767120.275807	42.571764
3502.154126	767110.277531	42.576768
3501.742342	767091.060166	42.581773
3501.773230	767085.118752	42.586778
3502.187263	767060.277128	42.591783
3501.847477	767056.159915	42.596788
3502.176662	767041.046033	42.601792
3502.126249	767015.884345	42.606797
3501.987934	767013.550968	42.611802
3501.727149	766993.917219	42.616807
3501.874623	766982.952978	42.621812
3502.143680	766968.338976	42.626816
3502.015346	766946.918083	42.631821
3502.040648	766936.414445	42.636826
3501.880434	766923.682831	42.641831
3501.655803	766909.538395	42.646836
3501.832933	766911.816793	42.651840
3501.862427	766898.172317	42.656845
3501.819976	766873.695770	42.661850
3501.811386	766866.288398	42.666855
3501.310377	766862.932243	42.671860
3501.678871	766834.760524	42.676864
3501.194038	766835.768609	42.681869
3501.671706	766832.259449	42.686874
3502.094592	766823.803282	42.691879
3501.884941	766810.294147	42.696884
3502.166886	766797.002529	42.701888
3501.890910	766789.391547	42.706893
3501.887373	766767.509002	42.711898
3502.165854	766762.019261	42.716903
3501.388479	766752.818392	42.721908
3501.956127	766738.059098	42.726912
3501.760452	766731.564010	42.731917
3501.868927	766711.184813	42.736922
3502.290045	766701.894656	42.741927
3502.319026	766693.647106	42.746932
3502.312038	766676.916739	42.751936
3502.399393	766664.685674	42.756941
3502.146041	766639.799673	42.761946
3502.104067	766616.990400	42.766951
3502.159405	766602.359970	42.771956
3502.171790	766581.848215	42.776960
3501.839496	766560.997744	42.781965
3502.070870	766559.685895	42.786970
3501.834129	766534.796919	42.791975
3501.717962	766527.504136	42.796980
3501.929026	766523.104223	42.801985
3501.546532	766508.247634	42.806989
3501.595532	766488.809359	42.811994
3502.013564	766489.185678	42.816999
3501.629156	766478.156582	42.822004
3501.879405	766456.576854	42.827009
3501.796603	766454.234610	42.832013
3501.771020	766436.230809	42.837018
3501.773310	766419.302098	42.842023
3501.476965	766415.717456	42.847028
3501.921077	766406.766787	42.852033
3501.819924	766398.293888	42.857037
3501.749794	766387.215518	42.862042
3501.986377	766392.968633	42.867047
3501.539680	766372.773363	42.872052
3501.821951	766352.709422	42.877057
3501.936201	766352.250006	42.882061
3501.560485	766327.332940	42.887066
3501.502368	766313.210322	42.892071
3501.473395	766302.861413	42.897076
3501.553323	766299.365096	42.902081
3501.516344	766287.545352	42.907085
3501.501731	766275.574885	42.912090
3502.072684	766269.940899	42.917095
3501.848337	766276.207787	42.922100
3502.008272	766241.196606	42.927105
3501.876172	766243.916121	42.932109
3501.908437	766229.975480	42.937114
3501.651442	766215.000504	42.942119
3502.032562	766206.157563	42.947124
3501.635671	766186.003031	42.952129
3501.744369	766169.547772	42.957133
3501.717874	766177.844746	42.962138
3502.302757	766164.455492	42.967143
3501.728391	766141.727878	42.972148
3501.960058	766125.842131	42.977153
3501.846943	766120.314961	42.982157
3501.831860	766100.542125	42.987162
3501.612416	766107.495381	42.992167
3501.540213	766093.570796	42.997172
3501.874967	766076.932769	43.002177
3501.468681	766079.940561	43.007181
3501.450863	766058.646852	43.012186
3501.835946	766048.870754	43.017191
3501.768373	766045.789931	43.022196
3501.906606	766037.573593	43.027201
3501.654554	766029.320113	43.032205
3501.935152	765999.490341	43.037210
3502.120774	766003.141700	43.042215
3501.880321	765991.794897	43.047220
3502.026842	765977.492391	43.052225
3501.960720	765966.265508	43.057229
3502.048267	765940.538563	43.062234
3502.043988	765940.244864	43.067239
3501.873626	765922.458645	43.072244
3501.669970	765900.457430	43.077249
3501.546657	765903.960849	43.082253
3501.608904	765886.874250	43.087258
3501.659595	765869.298698	43.092263
3501.552587	765870.787640	43.097268
3501.514286	765865.984649	43.102273
3501.212429	765857.689678	43.107277
3501.246374	765843.011918	43.112282
3501.237577	765833.395234	43.117287
3501.617556	765833.826615	43.122292
3501.459664	765827.815490	43.127297
3501.457546	765841.556057	43.132301
3501.673628	765834.112461	43.137306
3501.512147	765817.796747	43.142311
3501.554360	765810.184016	43.147316
3501.714198	765803.338045	43.152321
3501.376412	765797.845738	43.157325
3501.598533	765773.078582	43.162330
3501.445991	765770.354427	43.167335
3501.422215	765774.087713	43.172340
3501.415825	765764.028904	43.177345
3501.525453	765764.944205	43.182349
3501.582944	765742.509084	43.187354
3501.532020	765736.726522	43.192359
3501.168117	765747.628538	43.197364
3501.373512	765740.579094	43.202369
3501.357365	765734.300366	43.207373
3500.865892	765718.870241	43.212378
3501.042889	765723.161044	43.217383
3500.991330	765727.389427	43.222388
3501.341648	765711.091602	43.227393
3501.004238	765712.714740	43.232397
3500.985356	765709.282646	43.237402
3501.063718	765708.043632	43.242407
3501.179400	765716.956880	43.247412
3501.351225	765721.101274	43.252417
3501.137345	765727.416092	43.257421
3500.754745	765724.139008	43.262426
3500.754613	765729.537099	43.267431
3500.878308	765733.787155	43.272436
3500.768802	765725.412883	43.277441
3501.029642	765726.353624	43.282445
3500.840059	765734.774768	43.287450
3500.987307	765734.751810	43.292455
3500.695471	765742.256547	43.297460
3501.257102	765730.783931	43.302465
3500.860226	765731.582124	43.307469
3501.083717	765732.921285	43.312474
3501.365204	765732.779196	43.317479
3500.880754	765740.019608	43.322484
3501.389798	765735.817982	43.327489
3501.124028	765750.630473	43.332493
3501.238498	765749.729330	43.337498
3501.294721	765737.697788	43.342503
3501.090629	765729.681817	43.347508
3501.167638	765722.407060	43.352513
3501.294221	765727.000178	43.357517
3501.079227	765723.304311	43.362522
3500.756077	765714.767133	43.367527
3500.921100	765719.403320	43.372532
3501.144267	765708.278015	43.377537
3501.082985	765728.456609	43.382541
3501.129619	765725.112427	43.387546
3501.193214	765714.944461	43.392551
3501.171255	765729.031863	43.397556
3501.455434	765729.625446	43.402561
3501.097115	765726.737150	43.407565
3501.423619	765713.485567	43.412570
3501.069759	765707.799410	43.417575
3501.001227	765697.897438	43.422580
3501.469690	765694.438226	43.427585
3501.002654	765700.939861	43.432589
3501.300004	765699.666613	43.437594
3501.511280	765700.958616	43.442599
3501.106721	765708.382865	43.447604
3501.652919	765704.175412	43.452609
3501.276067	765692.898514	43.457613
3501.341785	765685.478263	43.462618
3501.209954	765683.290641	43.467623
3501.258830	765683.332133	43.472628
3501.793460	765685.653201	43.477633
3501.312905	765671.987897	43.482637
3501.355912	765661.037899	43.487642
3501.350840	765654.462927	43.492647
3500.937020	765654.184163	43.497652
3501.221024	765660.372137	43.502657
3501.204076	765667.932129	43.507661
3501.341893	765664.917177	43.512666
3501.194017	765661.603370	43.517671
3501.379721	765663.341038	43.522676
3501.058177	765644.596274	43.527681
3500.848851	765639.181906	43.532685
3501.232564	765635.637767	43.537690
3501.377949	765629.726281	43.542695
3501.225490	765639.074134	43.547700
3501.112449	765633.399343	43.552705
3500.813084	765641.101659	43.557709
3501.043919	765649.604405	43.562714
3501.273192	765641.128000	43.567719
3501.069925	765647.195864	43.572724
3501.450241	765643.455967	43.577729
3501.157277	765643.599970	43.582733
3501.030653	765630.124622	43.587738
3500.852570	765617.295250	43.592743
3501.064912	765619.077838	43.597748
3501.516912	765615.326720	43.602753
3501.277826	765616.983583	43.607757
3501.204878	765620.282977	43.612762
3501.337094	765610.987456	43.617767
3500.788785	765626.187894	43.622772
3501.316364	765620.756463	43.627777
3501.284743	765634.060392	43.632781
3501.104169	765633.205357	43.637786
3501.189259	765631.621763	43.642791
3501.343787	765623.157020	43.647796
3501.565260	765597.064351	43.652801
3501.213602	765597.462899	43.657805
3501.374139	765596.211019	43.662810
3501.537794	765593.093849	43.667815
3501.434216	765598.213770	43.672820
3500.980199	765576.054367	43.677825
3500.860269	765573.668553	43.682829
3500.866121	765572.342702	43.687834
3501.678533	765564.560228	43.692839
3501.268679	765572.083597	43.697844
3501.223068	765576.654659	43.702849
3501.290855	765572.963580	43.707853
3501.119733	765580.302399	43.712858
3501.209011	765576.460740	43.717863
3501.262008	765577.875658	43.722868
3501.497779	765571.262958	43.727873
3501.481529	765552.077628	43.732877
3500.917464	765538.474188	43.737882
3501.174791	765547.316438	43.742887
3501.177718	765538.728068	43.747892
3501.245876	765543.035997	43.752897
3501.133867	765539.667451	43.757901
3501.059760	765555.775397	43.762906
3501.495204	765551.045352	43.767911
3501.296506	765547.101472	43.772916
3501.354611	765523.438695	43.777921
3501.237088	765524.978428	43.782925
3501.277086	765518.298134	43.787930
3501.531082	765523.313139	43.792935
3501.238292	765527.481205	43.797940
3501.207389	765528.860174	43.802945
3501.203358	765536.810883	43.807949
3501.146544	765510.466946	43.812954
3501.158773	765501.631705	43.817959
3501.272396	765495.430624	43.822964
3501.235745	765490.823412	43.827969
3501.446333	765503.108239	43.832973
3501.540662	765504.025966	43.837978
3501.525090	765499.219167	43.842983
3501.494396	765479.201628	43.847988
3501.174592	765480.576693	43.852993
3501.247277	765478.455184	43.857997
3500.980008	765473.540490	43.863002
3501.492800	765472.331672	43.868007
3501.061745	765480.300125	43.873012
3501.265136	765475.508155	43.878017
3501.307217	765483.893388	43.883021
3501.170618	765469.388722	43.888026
3501.407195	765448.053371	43.893031
3501.319944	765460.728356	43.898036
3501.524558	765454.365790	43.903041
3501.125540	765451.581889	43.908045
3501.207153	765464.819366	43.913050
3501.469325	765452.607911	43.918055
3500.883246	765432.333532	43.923060
3501.408588	765422.632781	43.928065
3501.113509	765423.513243	43.933069
3501.037083	765423.279875	43.938074
3501.157011	765428.070532	43.943079
3501.270097	765431.684458	43.948084
3501.336297	765425.049053	43.953089
3501.427563	765431.218287	43.958093
3501.432943	765427.340587	43.963098
3501.389281	765402.662733	43.968103
3501.415802	765391.469511	43.973108
3501.291679	765382.606358	43.978113
3501.547565	765397.828805	43.983117
3501.150441	765404.368861	43.988122
3501.400933	765405.900166	43.993127
3501.586347	765393.357082	43.998132
3501.582798	765374.120198	44.003137
3501.554598	765378.835895	44.008141
3501.277585	765375.051385	44.013146
3501.072991	765365.415585	44.018151
3501.337322	765376.857952	44.023156
3501.445483	765351.861733	44.028161
3501.230062	765332.412477	44.033165
3501.394994	765345.097326	44.038170
3501.492302	765338.309748	44.043175
3501.360336	765343.385219	44.048180
3501.467449	765342.337948	44.053185
3501.367607	765315.509243	44.058189
3501.558919	765303.406755	44.063194
3501.737551	765306.176212	44.068199
3501.618995	765315.028442	44.073204
3501.328838	765293.824034	44.078209
3501.671779	765290.531475	44.083213
3501.420002	765276.486094	44.088218
3501.653951	765284.007283	44.093223
3501.288101	765290.935163	44.098228
3501.459832	765276.038362	44.103233
3501.914941	765258.201740	44.108237
3501.501440	765257.284916	44.113242
3501.505995	765253.309095	44.118247
3501.201894	765242.510850	44.123252
3501.407628	765235.657147	44.128257
3501.271064	765223.703929	44.133261
3501.187099	765221.066989	44.138266
3501.197136	765222.734077	44.143271
3501.016324	765230.222008	44.148276
3501.353127	765230.463876	44.153281
3501.376522	765227.270316	44.158285
3501.059076	765228.301527	44.163290
3501.472474	765227.451741	44.168295
3501.193404	765208.551928	44.173300
3501.559183	765207.660507	44.178305
3501.772347	765200.805609	44.183309
3501.556918	765201.477340	44.188314
3501.274757	765179.142571	44.193319
3501.385114	765170.733259	44.198324
3501.687033	765173.434420	44.203329
3501.329464	765166.423322	44.208333
3501.447859	765167.288256	44.213338
3501.421666	765154.875974	44.218343
3501.480233	765145.149652	44.223348
3501.324351	765140.364538	44.228353
3501.590834	765139.635863	44.233357
3501.427818	765138.630789	44.238362
3501.329456	765130.695750	44.243367
3501.059984	765119.695592	44.248372
3501.391717	765100.356461	44.253377
3501.585512	765110.387055	44.258381
3501.371152	765106.298140	44.263386
3501.641102	765102.133513	44.268391
3501.449713	765102.801496	44.273396
3501.497009	765079.776901	44.278401
3501.660600	765075.039956	44.283405
3500.931768	765076.282729	44.288410
3501.528864	765081.293499	44.293415
3501.426537	765083.910656	44.298420
3501.436335	765057.211045	44.303425
3501.631969	765045.205588	44.308429
3501.243723	765044.481097	44.313434
3501.528527	765036.829596	44.318439
3501.340770	765058.207773	44.323444
3500.948400	765033.386807	44.328449
3501.329818	765023.069990	44.333453
3501.495861	765023.044094	44.338458
3501.603638	765011.052312	44.343463
3501.568108	765010.321758	44.348468
3501.516628	765013.519927	44.353473
3501.606614	764995.150774	44.358477
3501.378698	764987.579369	44.363482
3501.579678	764979.744597	44.368487
3501.296798	764983.322500	44.373492
3501.260810	764977.389735	44.378497
3501.344311	764982.480864	44.383501
3501.454410	764967.593038	44.388506
3501.475253	764955.516594	44.393511
3501.277098	764959.228499	44.398516
3501.038532	764958.971383	44.403521
3501.345782	764954.506368	44.408525
3501.531753	764965.323648	44.413530
3501.536323	764944.710117	44.418535
3501.692355	764922.747728	44.423540
3501.357945	764921.867572	44.428545
3501.599099	764916.725766	44.433549
3501.216258	764927.043082	44.438554
3501.636265	764902.487282	44.443559
3501.565628	764895.921842	44.448564
3501.627521	764890.906198	44.453569
3501.684088	764892.173461	44.458573
3501.521509	764877.180831	44.463578
3501.500634	764860.251938	44.468583
3501.288789	764858.125640	44.473588
3501.511270	764848.373279	44.478593
3501.370614	764862.088363	44.483597
3501.800718	764852.303551	44.488602
3501.502852	764833.405653	44.493607
3501.512003	764828.103734	44.498612
3501.515545	764818.287398	44.503617
3501.361287	764823.366732	44.508621
3501.380806	764804.320982	44.513626
3501.665303	764799.908505	44.518631
3501.597655	764788.238239	44.523636
3501.694354	764781.793771	44.528641
3501.791571	764764.698946	44.533645
3501.250802	764754.329573	44.538650
3501.683982	764750.630019	44.543655
3501.412928	764768.144809	44.548660
3501.779774	764753.756265	44.553665
3501.681477	764733.452666	44.558669
3501.641231	764729.041829	44.563674
3501.667315	764736.203469	44.568679
3501.412700	764707.727896	44.573684
3501.552588	764698.822598	44.578689
3501.442204	764691.330656	44.583693
3501.469951	764691.669939	44.588698
3501.819433	764686.658271	44.593703
3501.653502	764676.622827	44.598708
3502.034542	764664.440491	44.603713
3501.739865	764667.136952	44.608717
3501.287034	764646.103234	44.613722
3501.333081	764629.948606	44.618727
3501.083210	764632.196352	44.623732
3501.072860	764631.805385	44.628737
3501.465236	764624.921906	44.633741
3501.435971	764633.515641	44.638746
3501.329475	764620.869556	44.643751
3501.433057	764607.650720	44.648756
3501.541683	764591.338977	44.653761
3501.648020	764590.095393	44.658765
3501.388209	764593.866211	44.663770
3501.400581	764585.618752	44.668775
3500.893222	764566.998281	44.673780
3501.045258	764566.140197	44.678785
3501.117669	764569.810013	44.683789
3500.889814	764569.109476	44.688794
3501.475188	764563.471873	44.693799
3501.434974	764566.864810	44.698804
3501.089201	764570.354592	44.703809
3501.539586	764568.959060	44.708813
3501.103768	764563.726497	44.713818
3501.125146	764551.452944	44.718823
3501.064096	764545.818215	44.723828
3501.081564	764529.127928	44.728833
3501.230635	764533.325673	44.733837
3501.255530	764540.242295	44.738842
3501.259499	764532.192411	44.743847
3501.078436	764536.687169	44.748852
3501.104293	764540.806009	44.753857
3501.230309	764542.160642	44.758861
3501.042985	764550.435621	44.763866
3501.462854	764542.762465	44.768871
3501.307915	764552.701138	44.773876
3501.255393	764518.647029	44.778881
3501.488056	764516.500219	44.783885
3501.266827	764516.534862	44.788890
3501.303993	764512.897089	44.793895
3500.901383	764519.046177	44.798900
3501.100474	764519.358684	44.803905
3501.204533	764526.164781	44.808909
3501.247530	764526.599851	44.813914
3501.184460	764517.137072	44.818919
3501.020820	764496.401262	44.823924
3501.112518	764485.098230	44.828929
3501.349650	764482.754385	44.833933
3501.189128	764496.865946	44.838938
3501.311984	764489.680896	44.843943
3501.005157	764489.581675	44.848948
3501.097144	764492.561330	44.853953
3501.247562	764503.679377	44.858957
3501.169589	764502.170100	44.863962
3501.180798	764493.628225	44.868967
3500.834556	764503.302385	44.873972
3500.886357	764500.987517	44.878977
3501.037639	764509.504101	44.883981
3500.823264	764517.685184	44.888986
3501.197752	764508.988377	44.893991
3501.239682	764508.932800	44.898996
3501.324959	764490.366725	44.904001
3501.298134	764478.345986	44.909005
3501.124493	764470.618286	44.914010
3500.985867	764472.406957	44.919015
3500.922336	764481.349809	44.924020
3500.918178	764476.442354	44.929025
3500.920299	764478.209022	44.934029
3500.882457	764482.975915	44.939034
3501.007501	764484.527039	44.944039
3501.086815	764482.256946	44.949044
3500.962647	764482.227334	44.954049
3501.022619	764473.186995	44.959053
3501.159251	764483.031107	44.964058
3501.528639	764479.292301	44.969063
3501.332151	764493.654899	44.974068
3501.281298	764492.975767	44.979073
3501.561172	764467.213301	44.984077
3501.009575	764475.005414	44.989082
3501.317989	764452.477822	44.994087
3501.145505	764455.547917	44.999092
3501.638932	764456.354316	45.004097
3501.471675	764462.957479	45.009101
3501.381252	764446.136613	45.014106
3501.230364	764433.987946	45.019111
3501.385009	764440.148154	45.024116
3501.580285	764427.110969	45.029121
3501.502749	764425.601607	45.034125
3501.594650	764435.747270	45.039130
3501.551731	764408.709836	45.044135
3501.385670	764391.066264	45.049140
3501.417151	764397.049435	45.054145
3501.604971	764398.050861	45.059149
3501.102162	764386.938769	45.064154
3501.135615	764364.502957	45.069159
3501.192947	764363.365158	45.074164
3501.077740	764358.524063	45.079169
3501.452986	764353.557212	45.084173
3501.052475	764362.503812	45.089178
3501.374789	764365.496598	45.094183
3501.609054	764363.643986	45.099188
3501.396319	764355.431445	45.104193
3501.441018	764332.355699	45.109197
3501.102140	764331.672493	45.114202
3501.283282	764337.288742	45.119207
3501.318666	764339.835567	45.124212
3501.251050	764335.968668	45.129217
3501.391393	764337.517434	45.134221
3501.026448	764343.513539	45.139226
3501.291106	764334.195610	45.144231
3501.080767	764322.939530	45.149236
3501.254969	764309.218260	45.154241
3501.253463	764303.377695	45.159245
3500.943339	764315.991439	45.164250
3501.118332	764308.552638	45.169255
3501.474832	764321.847489	45.174260
3501.518662	764316.245261	45.179265
3501.778670	764309.234917	45.184269
3501.726680	764298.592120	45.189274
3501.328702	764287.610730	45.194279
3501.290702	764290.070878	45.199284
3501.286181	764285.016097	45.204289
3501.556143	764273.832104	45.209293
3501.496812	764269.129461	45.214298
3501.410713	764256.774023	45.219303
3501.615161	764254.238879	45.224308
3501.452636	764252.251932	45.229313
3501.589245	764252.525136	45.234317
3501.194923	764229.861263	45.239322
3501.203225	764224.509932	45.244327
3501.262778	764225.924102	45.249332
3501.594348	764219.147897	45.254337
3501.342807	764220.365282	45.259341
3501.113126	764220.695747	45.264346
3501.195260	764222.400888	45.269351
3501.306817	764202.848269	45.274356
3501.076177	764196.356263	45.279361
3501.390645	764186.195928	45.284365
3501.383386	764193.608758	45.289370
3501.626952	764191.509229	45.294375
3501.557314	764189.065991	45.299380
3501.339556	764166.423393	45.304385
3501.441007	764152.222349	45.309389
3501.180214	764153.588443	45.314394
3501.393829	764144.081904	45.319399
3501.473897	764150.793952	45.324404
3501.116916	764147.855694	45.329409
3501.334016	764149.736090	45.334413
3501.183014	764131.696834	45.339418
3501.180315	764126.494401	45.344423
3501.302084	764131.972845	45.349428
3500.964746	764120.343616	45.354433
3501.621265	764120.142878	45.359437
3501.308467	764128.487055	45.364442
3501.531111	764124.525580	45.369447
3501.465859	764105.442085	45.374452
3501.151481	764095.968934	45.379457
3501.348916	764092.600394	45.384461
3500.946739	764099.633299	45.389466
3501.185983	764097.436249	45.394471
3501.010774	764101.586780	45.399476
3501.440523	764089.886672	45.404481
3501.377237	764098.339133	45.409485
3501.180258	764090.958248	45.414490
3501.515991	764077.603947	45.419495
3501.533898	764069.649519	45.424500
3501.270014	764063.211669	45.429505
3501.605877	764061.833942	45.434509
3501.324631	764055.153376	45.439514
3501.377669	764048.616887	45.444519
3501.157366	764038.932613	45.449524
3501.250377	764031.997181	45.454529
3501.032349	764023.883243	45.459533
3501.091200	764029.322519	45.464538
3501.435540	764027.599867	45.469543
3500.989945	764025.313511	45.474548
3501.063790	764028.737965	45.479553
3501.309783	764031.399234	45.484557
3501.139953	764042.273573	45.489562
3501.173106	764035.298417	45.494567
3500.911201	764031.019957	45.499572
3501.102841	764030.499211	45.504577
3500.952015	764011.232495	45.509581
3500.632907	764014.718383	45.514586
3501.031047	764024.276841	45.519591
3501.128979	764041.588520	45.524596
3500.965445	764028.508511	45.529601
3501.021894	764010.780105	45.534605
3501.199462	764007.807310	45.539610
3501.148519	764001.188860	45.544615
3500.877218	764010.459306	45.549620
3501.032078	764012.693064	45.554625
3501.056512	764019.659360	45.559629
3500.805306	764021.956593	45.564634
3500.998031	764022.760968	45.569639
3501.108396	764026.572393	45.574644
3500.935674	764019.629404	45.579649
3501.357621	764018.287296	45.584653
3501.337715	764020.401117	45.589658
3501.090662	764017.887383	45.594663
3500.957469	764025.418248	45.599668
3500.804341	764028.240080	45.604673
3501.249729	764025.470850	45.609677
3501.149802	764042.518948	45.614682
3501.262502	764036.414882	45.619687
3500.907751	764034.261583	45.624692
3501.037857	764029.185571	45.629697
3501.234961	764019.485104	45.634701
3500.892264	764006.334890	45.639706
3501.133580	764002.615853	45.644711
3501.360444	764004.200253	45.649716
3501.223236	763999.656856	45.654721
3501.722856	764000.315089	45.659725
3501.365169	764006.653942	45.664730
3501.325169	764001.751756	45.669735
3501.566947	763997.983559	45.674740
3501.020570	763978.729502	45.679745
3501.242369	763973.835456	45.684749
3501.048968	763978.528841	45.689754
3501.113724	763969.536186	45.694759
3501.197924	763984.592233	45.699764
3501.274282	763981.242567	45.704769
3501.484993	763983.663945	45.709773
3501.417951	763976.900733	45.714778
3501.153635	763951.221431	45.719783
3501.357484	763951.631392	45.724788
3501.475857	763947.293435	45.729793
3501.409410	763942.837110	45.734797
3501.297177	763945.161728	45.739802
3501.435049	763945.532919	45.744807
3501.435727	763930.954494	45.749812
3501.201522	763928.095120	45.754817
3501.447872	763904.691921	45.759821
3501.272169	763855.633587	45.764826
3501.209371	763740.732113	45.769831
3501.141445	763595.002433	45.774836
3500.969194	763386.942838	45.779841
3500.870483	763132.327307	45.784845
3500.049189	762835.988149	45.789850
3500.072290	762488.101441	45.794855
3499.816135	762097.329197	45.799860
3499.328254	761645.538349	45.804865
3499.329628	761143.554837	45.809869
3498.420552	760607.596236	45.814874
3498.366778	760017.488017	45.819879
3497.700072	759382.287287	45.824884
3496.820165	758701.477294	45.829889
3496.395764	757957.549306	45.834893
3495.697633	757178.062769	45.839898
3494.910175	756347.351187	45.844903
3494.204740	755485.470049	45.849908
3492.885636	754562.534969	45.854913
3492.527181	753601.970231	45.859917
3491.436396	752603.533960	45.864922
3490.510540	751554.088970	45.869927
3489.947866	750444.336504	45.874932
3488.478055	749301.107042	45.879937
3487.687866	748111.493820	45.884941
3486.329961	746875.620246	45.889946
3485.582364	745590.375460	45.894951
3484.515074	744256.666846	45.899956
3482.744056	742890.922303	45.904961
3481.535098	741477.022162	45.909965
3480.072376	740034.914682	45.914970
3478.974159	738544.685110	45.919975
3477.696208	737002.300971	45.924980
3476.157651	735406.954893	45.929985
3474.416238	733783.004234	45.934989
3473.077731	732131.125753	45.939994
3471.506536	730423.786192	45.944999
3470.175038	728685.439254	45.950004
3468.410383	726890.564618	45.955009
3466.923942	725072.421625	45.960013
3465.170447	723227.378699	45.965018
3463.767955	721315.724717	45.970023
3461.842791	719378.933574	45.975028
3459.919821	717396.752105	45.980033
3458.136744	715370.806255	45.985037
3456.233923	713327.497343	45.990042
3454.610038	711241.094293	45.995047
3452.649115	709115.766228	46.000052
3450.606166	706957.083603	46.005057
3448.631500	704761.535327	46.010061
3446.583097	702531.788912	46.015066
3444.529963	700260.036064	46.020071
3442.271071	697974.353757	46.025076
3440.164326	695635.249241	46.030081
3438.206703	693269.734065	46.035085
3435.958225	690881.377120	46.040090
3433.499355	688449.079901	46.045095
3431.332256	685989.045176	46.050100
3429.214488	683504.713690	46.055105
3426.733472	680978.120506	46.060109
3424.178407	678435.494447	46.065114
3421.850283	675850.612877	46.070119
3419.348843	673249.033725	46.075124
3416.686905	670608.636899	46.080129
3414.344869	667938.362053	46.085133
3411.721961	665254.238941	46.090138
3409.304990	662522.668314	46.095143
3406.717738	659781.475601	46.100148
3403.903480	657014.843836	46.105153
3401.497177	654209.914383	46.110157
3398.656055	651394.223696	46.115162
3396.250500	648539.144024	46.120167
3393.463433	645661.064391	46.125172
3390.843101	642762.376312	46.130177
3388.026308	639820.890698	46.135181
3385.268720	636880.816743	46.140186
3382.533357	633900.816310	46.145191
3379.700318	630907.573977	46.150196
3376.436118	627895.546928	46.155201
3373.701085	624845.502249	46.160205
3370.701012	621780.711288	46.165210
3367.941752	618702.588285	46.170215
3364.960473	615600.556691	46.175220
3362.084979	612471.402058	46.180225
3359.378888	609319.748670	46.185229
3356.239359	606153.982639	46.190234
3353.090662	602956.970538	46.195239
3350.070698	599748.942920	46.200244
3346.857548	596516.180408	46.205249
3343.811833	593279.698937	46.210253
3340.662584	590012.092598	46.215258
3337.198234	586727.859064	46.220263
3334.325757	583437.127992	46.225268
3330.931905	580130.199162	46.230273
3327.797670	576799.321733	46.235277
3324.339705	573463.893100	46.240282
3321.027839	570093.180376	46.245287
3318.266938	566714.711979	46.250292
3314.603686	563335.649289	46.255297
3311.181548	559915.486264	46.260301
3307.945162	556501.188590	46.265306
3304.710773	553061.286715	46.270311
3301.480422	549610.902765	46.275316
3298.075221	546160.376635	46.280321
3294.702742	542679.554546	46.285325
3291.352426	539197.407763	46.290330
3288.476004	535696.461077	46.295335
3284.717151	532190.365182	46.300340
3281.384103	528668.246668	46.305345
3277.887364	525119.366355	46.310349
3274.500783	521573.853505	46.315354
3271.167413	518019.030973	46.320359
3267.265689	514428.130564	46.325364
3263.920645	510862.228087	46.330369
3260.702546	507263.468037	46.335373
3256.949177	503669.880850	46.340378
3253.124982	500048.911195	46.345383
3249.959814	496430.521137	46.350388
3246.447230	492807.309242	46.355393
3242.872724	489163.332025	46.360397
3239.155829	485519.916385	46.365402
3235.497956	481867.797872	46.370407
3231.763954	478208.520398	46.375412
3228.150477	474552.777355	46.380417
3224.633954	470863.931757	46.385421
3220.972641	467195.314083	46.390426
3217.148703	463509.320296	46.395431
3213.850531	459823.400192	46.400436
3209.942152	456124.486234	46.405441
3206.344404	452413.552699	46.410445
3202.882306	448716.856508	46.415450
3199.172894	445002.072685	46.420455
3195.314928	441288.939769	46.425460
3192.029097	437553.652333	46.430465
3188.187056	433820.554618	46.435469
3184.619557	430084.717151	46.440474
3180.339078	426341.947252	46.445479
3176.676856	422599.853128	46.450484
3172.962032	418866.412514	46.455489
3169.228647	415119.780998	46.460493
3165.310409	411378.554921	46.465498
3161.221472	407626.666810	46.470503
3157.605492	403883.304542	46.475508
3153.875447	400131.120647	46.480513
3149.973645	396379.116777	46.485517
3146.216282	392628.932083	46.490522
3142.140184	388886.872553	46.495527
3138.399296	385136.578455	46.500532
3134.293824	381391.957090	46.505537
3130.395353	377646.103108	46.510541
3126.612604	373899.297461	46.515546
3122.912577	370159.102901	46.520551
3119.081834	366416.422179	46.525556
3114.712737	362678.293482	46.530561
3111.224221	358940.545257	46.535565
3106.943178	355203.935251	46.540570
3103.278008	351468.688734	46.545575
3099.146340	347739.971176	46.550580
3095.087862	344016.009820	46.555585
3091.308409	340294.854391	46.560589
3087.004962	336576.745880	46.565594
3083.283745	332868.722459	46.570599
3079.277722	329158.751897	46.575604
3075.287530	325462.748632	46.580609
3071.444995	321750.663917	46.585613
3067.354170	318063.020905	46.590618
3062.944988	314366.542798	46.595623
3059.116850	310675.374529	46.600628
3054.954975	307006.137758	46.605633
3050.967837	303334.618098	46.610637
3046.687793	299684.468639	46.615642
3042.749662	296022.746191	46.620647
3038.693527	292373.358300	46.625652
3034.371846	288747.313979	46.630657
3030.530645	285114.854010	46.635661
3026.622015	281508.611548	46.640666
3022.375216	277890.606735	46.645671
3018.083342	274289.880669	46.650676
3013.946045	270698.369741	46.655681
3009.734994	267121.367653	46.660685
3005.530973	263548.052275	46.665690
3001.076224	259989.476465	46.670695
2997.025431	256449.268324	46.675700
2992.698655	252909.847319	46.680705
2988.462193	249376.566126	46.685709
2984.247323	245884.923212	46.690714
2979.690412	242377.277520	46.695719
2975.733137	238904.224725	46.700724
2971.295906	235442.743280	46.705729
2967.336735	231981.054574	46.710733
2962.878200	228548.025185	46.715738
2958.679344	225116.855109	46.720743
2954.254682	221704.719868	46.725748
2950.314714	218312.969717	46.730753
2945.998600	214919.539817	46.735757
2941.745037	211552.004472	46.740762
2937.409810	208200.054740	46.745767
2933.182886	204856.513090	46.750772
2928.657319	201534.924151	46.755777
2924.901176	198217.098174	46.760781
2920.494765	194931.278751	46.765786
2915.998061	191650.467660	46.770791
2912.082497	188376.299771	46.775796
2907.265889	185129.895480	46.780801
2903.169669	181901.560199	46.785805
2898.565288	178678.073837	46.790810
2894.365016	175475.609470	46.795815
2890.178234	172291.738743	46.800820
2885.547206	169129.504948	46.805825
2881.617209	165886.277467	46.810829
2877.615210	162764.694086	46.815834
2873.260112	159641.812417	46.820839
2868.917369	156542.413818	46.825844
2864.463273	153464.943283	46.830849
2860.157399	150385.579266	46.835853
2856.076070	147342.289135	46.840858
2851.515036	144313.374204	46.845863
2847.548697	141285.285511	46.850868
2843.183633	138296.786136	46.855873
2839.112531	135300.351997	46.860877
2834.455391	132350.015713	46.865882
2830.228273	129405.966418	46.870887
2826.364088	126463.933169	46.875892
2821.783703	123549.018852	46.880897
2817.767497	120659.192223	46.885901
2813.120448	117777.282448	46.890906
2808.905405	114914.978459	46.895911
2804.648835	112059.437524	46.900916
2800.241838	109246.596932	46.905921
2796.231730	106423.431081	46.910925
2791.907680	103634.104836	46.915930
2787.639872	100856.148713	46.920935
2783.475504	98098.695888	46.925940
2779.461295	95352.690699	46.930945
2775.099681	92627.464004	46.935949
2770.869189	89925.659656	46.940954
2766.490067	87238.642601	46.945959
2762.626800	84560.720093	46.950964
2757.965848	81906.377591	46.955969
2754.011102	79267.528561	46.960973
2749.597241	76642.437744	46.965978
2745.137374	74040.933681	46.970983
2741.232617	71458.615446	46.975988
2736.526232	68900.131408	46.980993
2732.208662	66335.884020	46.985997
2727.728150	63814.247160	46.991002
2723.674927	61310.730739	46.996007
2719.216165	58825.317553	47.001012
2714.973799	56356.195557	47.006017
2711.040626	53906.470504	47.011021
2706.268046	51468.574024	47.016026
2701.978143	49065.781577	47.021031
2697.534814	46667.475046	47.026036
2693.106457	44306.474304	47.031041
2688.769523	41962.923974	47.036045
2684.455247	39638.683981	47.041050
2679.606338	37334.409137	47.046055
2675.076174	35046.869259	47.051060
2670.655964	32799.705337	47.056065
2666.736482	30557.380170	47.061069
2661.655751	28355.389156	47.066074
2657.180798	26172.472299	47.071079
2652.446628	24030.081154	47.076084
2647.805457	21903.703265	47.081089
2643.126754	19807.475752	47.086093
2638.100326	17761.055475	47.091098
2632.625335	15711.456027	47.096103
2627.479430	13732.556224	47.101108
2620.753580	11813.126809	47.106113
2610.952454	10034.782122	47.111117
2597.617428	8421.251100	47.116122
2585.442335	6908.482210	47.121127
2573.650383	5529.594847	47.126132
2562.394188	4298.143550	47.131137
2551.682095	3178.121527	47.136141
2541.447316	2210.809157	47.141146
2532.166826	1391.820247	47.146151
2523.497657	697.812909	47.151156
2512.867425	181.970805	47.156161
2486.910405	205.106417	47.161165
2471.511368	204.952643	47.166170
2465.264584	213.168886	47.171175
2466.286925	214.920006	47.176180
2469.820702	221.612570	47.181185
2474.042556	215.228714	47.186189
2476.178549	212.730534	47.191194
2477.114134	212.619040	47.196199
2475.885793	199.503941	47.201204
2473.488581	210.841874	47.206209
2470.488070	206.616104	47.211213
2467.341353	197.803426	47.216218
2464.005988	201.546086	47.221223
2461.487912	194.286619	47.226228
2457.881439	194.933117	47.231233
2454.874570	190.822250	47.236237
2452.183985	196.118758	47.241242
2448.806898	196.045976	47.246247
2446.397162	186.124560	47.251252
2442.892602	192.769663	47.256257
2439.542720	199.371588	47.261261
2436.637238	196.231997	47.266266
2433.441300	196.513711	47.271271
2430.177470	191.107891	47.276276
2426.960048	197.205022	47.281281
2423.908031	202.608701	47.286285
2420.625307	197.933531	47.291290
2417.160730	200.127130	47.296295
2414.216804	192.839380	47.301300
2410.928508	200.469432	47.306305
2407.518435	190.359654	47.311309
2403.962787	197.091857	47.316314
2400.235523	198.079986	47.321319
2397.216862	196.571693	47.326324
2393.798092	197.340713	47.331329
2390.687249	190.205639	47.336333
2387.419092	193.871363	47.341338
2384.049263	192.582533	47.346343
2380.587387	191.409348	47.351348
2376.785055	202.672865	47.356353
2373.431938	186.523831	47.361357
2370.433975	189.514512	47.366362
2367.646249	189.748202	47.371367
2363.998780	184.335982	47.376372
2360.142362	197.560076	47.381377
2356.927869	190.321002	47.386381
2353.183863	187.341093	47.391386
2349.370398	201.861992	47.396391
2346.234049	192.320044	47.401396
2342.250384	193.278698	47.406401
2339.960218	187.932565	47.411405
2336.533327	189.386270	47.416410
2332.893965	193.983312	47.421415
2329.227091	178.202943	47.426420
2325.745878	187.941858	47.431425
2322.601887	189.161476	47.436429
2319.222186	185.327288	47.441434
2315.687797	191.496180	47.446439
2312.451800	184.317438	47.451444
2308.736793	190.846795	47.456449
2305.537085	180.738955	47.461453
2301.132060	183.962440	47.466458
2297.894530	180.286359	47.471463
2294.787087	182.129878	47.476468
2291.563363	187.484513	47.481473
2288.007930	176.758428	47.486477
2284.593722	191.811678	47.491482
2280.864986	195.511521	47.496487
2277.444607	187.548519	47.501492
2274.277000	184.899258	47.506497
2270.991070	183.363211	47.511501
2267.193936	175.490802	47.516506
2263.399718	187.088439	47.521511
2260.056620	184.365394	47.526516
2256.803527	194.821641	47.531521
2253.463136	186.453814	47.536525
2250.212981	185.158959	47.541530
2246.324392	191.715492	47.546535
2242.845887	182.217627	47.551540
2239.302417	179.978373	47.556545
2236.031328	184.100191	47.561549
2232.868707	186.578808	47.566554
2229.112092	182.313220	47.571559
2225.091682	176.045043	47.576564
2221.719755	181.843676	47.581569
2218.049905	181.437103	47.586573
2214.941990	179.148695	47.591578
2211.456221	181.291882	47.596583
2208.673397	175.820377	47.601588
2204.947949	182.076137	47.606593
2201.021535	183.494137	47.611597
2197.352019	181.391681	47.616602
2194.105025	175.034150	47.621607
2190.794321	168.667607	47.626612
2187.073922	174.552406	47.631617
2184.137537	174.505669	47.636621
2180.679710	172.942761	47.641626
2176.679204	175.090560	47.646631
2173.545558	161.701000	47.651636
2169.960439	179.549389	47.656641
2166.097872	176.426743	47.661645
2162.572631	175.386936	47.666650
2159.032118	175.516989	47.671655
2156.161103	169.534097	47.676660
2152.370737	178.204571	47.681665
2148.936845	161.021056	47.686669
2145.463454	160.061732	47.691674
2141.739300	171.556674	47.696679
2138.692488	172.865545	47.701684
2135.059022	174.516152	47.706689
2131.360078	161.537772	47.711693
2128.219523	163.291599	47.716698
2124.027202	175.059123	47.721703
2120.951584	174.641868	47.726708
2117.639976	172.341067	47.731713
2113.998246	169.117449	47.736717
2110.945925	162.720000	47.741722
2106.927575	166.297520	47.746727
2103.432382	163.041487	47.751732
2100.246414	176.660616	47.756737
2096.793427	171.591408	47.761741
2093.217302	166.206101	47.766746
2089.668106	165.613008	47.771751
2086.204463	161.387065	47.776756
2082.628760	175.022882	47.781761
2079.281978	168.383604	47.786765
2075.749920	168.227612	47.791770
2072.165770	169.623741	47.796775
2068.667104	161.445283	47.801780
2065.403748	173.937532	47.806785
2061.236856	156.811805	47.811789
2057.788397	163.887996	47.816794
2054.306125	167.609453	47.821799
2051.046484	160.105473	47.826804
2047.874413	161.791484	47.831809
2044.232120	164.671082	47.836813
2040.832734	159.542890	47.841818
2036.940793	163.043704	47.846823
2033.569044	167.459743	47.851828
2030.156764	164.621048	47.856833
2026.578717	174.846595	47.861837
2023.323388	169.101057	47.866842
2019.730145	165.303554	47.871847
2016.231628	160.279470	47.876852
2012.455954	158.383527	47.881857
2009.498456	164.177476	47.886861
2005.969157	164.277349	47.891866
2002.380438	171.954493	47.896871
1998.623496	161.687193	47.901876
1995.113445	163.957634	47.906881
1991.848044	165.449450	47.911885
1988.572670	164.452864	47.916890
1984.504051	158.765000	47.921895
1981.353392	162.507356	47.926900
1977.990816	158.132755	47.931905
1974.500976	165.294541	47.936909
1970.936140	159.629095	47.941914
1967.276120	153.791879	47.946919
1963.994481	154.814828	47.951924
1960.102408	165.715969	47.956929
1956.713432	156.321289	47.961933
1953.219229	160.772329	47.966938
1949.858548	159.997920	47.971943
1946.421764	157.289644	47.976948
1942.589014	153.305016	47.981953
1939.325765	156.005106	47.986957
1935.970373	150.291084	47.991962
1932.271822	163.797447	47.996967
1929.091823	158.014848	48.001972
1925.516925	158.400304	48.006977
1922.130836	155.165230	48.011981
1918.519279	162.820656	48.016986
1914.516188	162.621364	48.021991
1911.099945	155.929745	48.026996
1907.745880	158.419421	48.032001
1904.241129	163.049304	48.037005
1900.785840	154.209208	48.042010
1897.355744	162.238054	48.047015
1894.033418	152.364720	48.052020
1890.541332	154.641873	48.057025
1886.714165	153.639916	48.062029
1883.687758	156.071998	48.067034
1880.180918	156.146251	48.072039
1876.430988	149.608109	48.077044
1872.537907	151.872086	48.082049
1868.882746	152.703570	48.087053
1866.185284	152.189246	48.092058
1862.344768	165.338179	48.097063
1859.335178	150.423344	48.102068
1855.424982	151.165024	48.107073
1851.871186	152.107206	48.112077
1848.958771	159.248267	48.117082
1844.704207	147.967384	48.122087
1841.462302	152.995926	48.127092
1837.894053	162.960543	48.132097
1834.452905	153.988543	48.137101
1831.049836	146.484949	48.142106
1827.255183	156.652680	48.147111
1823.856796	158.636772	48.152116
1820.141800	161.739797	48.157121
1816.881745	154.890890	48.162125
1813.783536	152.237248	48.167130
1810.131932	147.983873	48.172135
1806.488064	150.468309	48.177140
1802.984104	156.433245	48.182145
1799.018639	152.893401	48.187149
1795.655659	148.617010	48.192154
1791.883015	150.242051	48.197159
1789.055201	151.757198	48.202164
1785.094032	146.207639	48.207169
1782.012296	148.341511	48.212173
1778.511407	147.244240	48.217178
1774.887532	146.767350	48.222183
1771.335364	139.369376	48.227188
1767.716583	143.669116	48.232193
1764.341465	145.187660	48.237197
1761.259036	142.819478	48.242202
1757.247232	151.277924	48.247207
1754.131459	149.139595	48.252212
1750.317396	148.512138	48.257217
1746.748564	147.134437	48.262221
1743.786247	144.864525	48.267226
1739.723084	153.251919	48.272231
1736.699120	138.557701	48.277236
1732.537599	143.097419	48.282241
1729.330776	146.329757	48.287245
1725.913939	145.950201	48.292250
1722.235570	149.797358	48.297255
1718.815641	140.682882	48.302260
1715.585196	140.508285	48.307265
1711.966353	144.681497	48.312269
1708.282327	141.287479	48.317274
1704.912844	148.588688	48.322279
1701.380531	137.599823	48.327284
1697.958267	143.789288	48.332289
1694.136911	147.234876	48.337293
1690.750808	139.326875	48.342298
1687.206803	153.065373	48.347303
1684.276030	143.909157	48.352308
1680.198542	142.566792	48.357313
1676.747731	139.898776	48.362317
1673.205231	139.848962	48.367322
1669.575120	142.056034	48.372327
1666.375998	144.787296	48.377332
1663.338902	137.270788	48.382337
1659.685696	142.306799	48.387341
1655.980584	131.860710	48.392346
1652.118684	149.559488	48.397351
1649.034167	138.649264	48.402356
1645.222151	136.442764	48.407361
1641.933924	146.363597	48.412365
1638.409216	139.160702	48.417370
1634.896626	132.933546	48.422375
1631.243986	133.935565	48.427380
1627.987622	129.886170	48.432385
1624.225005	142.561033	48.437389
1620.867923	128.621385	48.442394
1617.235095	144.563179	48.447399
1613.822776	136.634002	48.452404
1610.246855	141.528214	48.457409
1606.461740	144.465107	48.462413
1603.318858	136.999980	48.467418
1599.664576	136.762037	48.472423
1596.254880	139.731926	48.477428
1592.874478	137.429419	48.482433
1589.206203	137.427795	48.487437
1586.030803	137.991292	48.492442
1582.044333	143.557229	48.497447
1578.990527	135.578282	48.502452
1575.339232	134.109143	48.507457
1571.667042	133.902488	48.512461
1568.529607	136.484912	48.517466
1564.725641	138.412337	48.522471
1561.411336	131.654287	48.527476
1557.851142	129.807053	48.532481
1554.059203	135.314076	48.537485
1550.993166	136.613462	48.542490
1547.071138	135.721399	48.547495
1543.973230	136.532215	48.552500
1540.222491	140.577425	48.557505
1536.568050	134.217481	48.562509
1532.948480	129.592199	48.567514
1530.033769	136.312890	48.572519
1525.956524	132.278117	48.577524
1523.077633	138.898288	48.582529
1519.429149	129.009729	48.587533
1516.159950	134.226130	48.592538
1512.417813	137.634068	48.597543
1508.527591	133.383362	48.602548
1505.284745	138.554512	48.607553
1501.753897	138.733896	48.612557
1498.106660	137.906412	48.617562
1494.882292	142.761452	48.622567
1491.698145	129.965417	48.627572
1487.910629	126.435822	48.632577
1483.928134	130.827381	48.637581
1480.484437	121.276960	48.642586
1477.004422	133.898131	48.647591
1473.478630	127.518079	48.652596
1470.094931	128.440092	48.657601
1466.932901	136.148662	48.662605
1463.862822	128.643722	48.667610
1460.115188	133.685082	48.672615
1456.385085	126.277130	48.677620
1452.500371	128.236216	48.682625
1449.056361	131.160899	48.687629
1446.214932	130.251597	48.692634
1442.865615	121.651392	48.697639
1439.020658	130.615340	48.702644
1434.947239	135.030641	48.707649
1431.116355	127.379039	48.712653
1427.928167	128.944361	48.717658
1424.319674	135.770510	48.722663
1421.400181	125.271164	48.727668
1417.746645	127.326958	48.732673
1414.307100	124.635130	48.737677
1411.078981	124.466594	48.742682
1407.201638	128.936635	48.747687
1403.547385	122.554576	48.752692
1400.098726	121.708700	48.757697
1397.163751	126.866488	48.762701
1393.230770	124.296200	48.767706
1389.577068	128.107963	48.772711
1386.307487	118.726487	48.777716
1382.327577	124.433835	48.782721
1378.952889	123.269495	48.787725
1375.733120	120.030737	48.792730
1372.083599	132.086826	48.797735
1369.030422	125.560068	48.802740
1365.387988	125.405780	48.807745
1361.829137	125.425077	48.812749
1358.035604	114.907554	48.817754
1354.423096	124.417285	48.822759
1351.035081	121.005550	48.827764
1347.815007	123.999616	48.832769
1344.087804	129.091601	48.837773
1340.408574	115.705571	48.842778
1336.863703	120.595003	48.847783
1333.575311	120.261916	48.852788
1329.981674	123.554917	48.857793
1326.630726	133.210383	48.862797
1323.380861	132.178386	48.867802
1320.001888	137.617677	48.872807
1316.764896	124.440841	48.877812
1312.870010	123.898974	48.882817
1308.784020	139.842166	48.887821
1305.573230	128.606995	48.892826
1301.839111	136.528552	48.897831
1298.681646	127.278258	48.902836
1295.217049	132.000111	48.907841
1291.503349	130.126386	48.912845
1288.118967	125.397946	48.917850
1284.480993	134.725022	48.922855
1280.985218	122.809958	48.927860
1277.694719	125.448065	48.932865
1273.997966	124.429095	48.937869
1270.973277	123.861753	48.942874
1266.859724	128.349839	48.947879
1263.834110	125.953944	48.952884
1259.984647	134.165661	48.957889
1256.353446	130.507284	48.962893
1253.218659	124.366678	48.967898
1249.669881	137.039800	48.972903
1246.082050	127.755656	48.977908
1242.541366	122.760630	48.982913
1238.732232	126.675873	48.987917
1235.823603	126.473198	48.992922
1231.875160	121.244610	48.997927
1228.597275	129.585160	49.002932
1224.970670	130.795225	49.007937
1221.540552	127.760297	49.012941
1218.321894	124.622663	49.017946
1214.583885	130.962935	49.022951
1210.942951	121.171419	49.027956
1207.468868	125.366422	49.032961
1204.002335	133.141711	49.037965
1200.461077	121.246461	49.042970
1197.133756	121.526971	49.047975
1193.456399	126.487813	49.052980
1189.681007	123.883449	49.057985
1186.134303	123.372547	49.062989
1183.053330	113.195982	49.067994
1179.247120	119.512138	49.072999
1176.631152	119.307957	49.078004
1172.880777	119.088380	49.083009
1169.224367	122.305840	49.088013
1165.528167	118.901293	49.093018
1161.514616	130.479740	49.098023
1158.701017	121.536348	49.103028
1154.989558	122.266164	49.108033
1151.610480	132.577829	49.113037
1147.810249	119.036823	49.118042
1144.524782	118.893173	49.123047
1141.176305	115.393068	49.128052
1137.585682	127.142595	49.133057
1133.739410	119.885857	49.138061
1131.079077	115.487062	49.143066
1126.686969	120.768639	49.148071
1123.219953	121.447542	49.153076
1119.826808	132.887742	49.158081
1116.153500	132.953522	49.163085
1113.169030	117.013185	49.168090
1109.218522	121.070832	49.173095
1106.344726	112.266606	49.178100
1102.318153	115.526222	49.183105
1098.610498	112.417735	49.188109
1095.230879	112.725451	49.193114
1091.805176	115.125350	49.198119
1088.398062	120.160976	49.203124
1084.851671	115.628831	49.208129
1081.529982	115.304207	49.213133
1078.317448	109.065112	49.218138
1074.474537	123.204880	49.223143
1070.933890	124.496458	49.228148
1067.562275	116.611766	49.233153
1063.596556	118.770348	49.238157
1060.354337	110.337042	49.243162
1056.634366	125.188414	49.248167
1053.623044	115.943818	49.253172
1050.322936	115.321590	49.258177
1046.500503	119.327570	49.263181
1042.910704	112.040213	49.268186
1039.284889	118.676193	49.273191
1035.989265	110.842896	49.278196
1032.329110	113.931272	49.283201
1028.603250	114.837401	49.288205
1025.571845	115.960676	49.293210
1021.631122	118.071067	49.298215
1018.084536	117.974671	49.303220
1015.236897	117.227827	49.308225
1011.352628	117.250746	49.313229
1008.035520	115.334023	49.318234
1004.302291	119.787971	49.323239
1000.823105	121.361023	49.328244
997.413689	124.979644	49.333249
993.999217	127.178496	49.338253
990.528216	120.065553	49.343258
986.823620	124.394799	49.348263
983.348613	116.912318	49.353268
980.013374	121.550738	49.358273
975.866636	124.737469	49.363277
973.095537	126.047798	49.368282
969.348324	127.409722	49.373287
965.934349	119.639275	49.378292
962.403826	115.664693	49.383297
958.630641	116.321989	49.388301
955.151520	120.188824	49.393306
951.576747	121.435167	49.398311
948.569492	112.345006	49.403316
944.941894	112.966856	49.408321
941.416913	118.473412	49.413325
938.127476	107.908803	49.418330
934.224011	121.675268	49.423335
930.546919	110.557577	49.428340
927.137764	112.562626	49.433345
923.607323	115.811068	49.438349
920.380037	113.019752	49.443354
916.820980	121.568927	49.448359
913.470857	117.632558	49.453364
909.920316	116.287110	49.458369
906.133181	116.620737	49.463373
902.884095	110.994888	49.468378
899.253734	112.313231	49.473383
895.866752	117.579888	49.478388
892.286086	118.475991	49.483393
888.523462	120.881258	49.488397
885.599586	113.726984	49.493402
881.728028	121.306351	49.498407
878.257723	115.781590	49.503412
874.551076	117.962957	49.508417
870.989340	118.391020	49.513421
867.718621	118.368546	49.518426
864.206694	123.294103	49.523431
860.765182	113.370285	49.528436
857.260071	112.663165	49.533441
853.664687	119.364045	49.538445
850.163476	111.104262	49.543450
846.321666	122.602128	49.548455
843.254568	117.374919	49.553460
840.214766	108.935320	49.558465
835.977117	116.072143	49.563469
832.531673	112.818300	49.568474
828.685780	124.101671	49.573479
825.486303	118.711697	49.578484
822.336702	108.042982	49.583489
818.758730	116.066788	49.588493
815.513443	118.150621	49.593498
811.823789	115.362145	49.598503
808.190160	120.882594	49.603508
804.649822	115.324537	49.608513
801.484906	113.532759	49.613517
798.048572	109.609937	49.618522
794.073183	115.781871	49.623527
790.276408	117.759079	49.628532
787.184746	118.986779	49.633537
783.646224	123.460937	49.638541
780.577214	113.624359	49.643546
776.465568	112.955302	49.648551
773.038133	108.028165	49.653556
769.707974	123.217209	49.658561
766.000136	118.840194	49.663565
762.819573	106.474218	49.668570
758.862639	117.189688	49.673575
755.304246	116.304285	49.678580
752.097397	108.602741	49.683585
748.849583	114.872730	49.688589
745.177275	114.726522	49.693594
741.414769	111.607791	49.698599
738.369481	110.322496	49.703604
734.645355	108.662609	49.708609
730.903486	111.615190	49.713613
727.859580	104.008367	49.718618
724.073447	113.902980	49.723623
720.446265	115.290497	49.728628
717.095314	115.223691	49.733633
713.725786	108.920739	49.738637
710.363423	103.907507	49.743642
706.658988	106.971296	49.748647
703.260702	110.730641	49.753652
699.620176	105.106063	49.758657
695.953767	112.188282	49.763661
692.741283	107.316103	49.768666
688.678176	110.916971	49.773671
685.194552	112.411735	49.778676
682.247707	110.592176	49.783681
678.394949	110.765326	49.788685
675.402004	107.038877	49.793690
671.446883	123.164230	49.798695
667.684972	105.684853	49.803700
663.900606	110.438001	49.808705
660.902289	114.875056	49.813709
657.376288	108.653582	49.818714
654.520519	109.784268	49.823719
651.115567	114.863988	49.828724
646.834290	107.849622	49.833729
643.566561	112.142209	49.838733
640.150984	108.703429	49.843738
636.447313	111.112215	49.848743
633.156967	111.896507	49.853748
629.553975	103.494578	49.858753
625.761735	102.187097	49.863757
622.597841	96.237968	49.868762
618.461230	112.363276	49.873767
615.421113	107.483116	49.878772
612.178629	103.207302	49.883777
608.997848	109.507962	49.888781
605.060167	114.892597	49.893786
601.537780	112.021065	49.898791
598.185268	113.454198	49.903796
594.394236	112.643259	49.908801
590.896393	115.725359	49.913805
587.530990	114.888892	49.918810
583.651517	109.295461	49.923815
580.209487	107.009315	49.928820
576.805683	112.750116	49.933825
573.376677	112.198869	49.938829
569.692888	112.177918	49.943834
566.160950	101.249656	49.948839
562.983648	99.906003	49.953844
559.951045	108.799945	49.958849
556.165588	112.493426	49.963853
552.401863	106.432620	49.968858
549.012488	112.664726	49.973863
545.478393	108.507378	49.978868
541.993853	112.947852	49.983873
538.431832	116.264653	49.988877
535.043942	95.904656	49.993882
531.630618	112.328004	49.998887
527.594354	110.093820	50.003892
524.095859	107.784901	50.008897
520.635610	113.012533	50.013901
517.614403	109.439267	50.018906
514.190601	113.424140	50.023911
510.532449	110.782721	50.028916
507.300332	106.394591	50.033921
503.589567	115.869341	50.038925
500.116153	111.139348	50.043930
496.290704	113.193932	50.048935
492.608384	111.793359	50.053940
489.182889	104.964584	50.058945
485.857149	114.280955	50.063949
482.375376	105.379208	50.068954
478.897037	108.227333	50.073959
475.787263	101.516797	50.078964
471.898300	99.898659	50.083969
468.079918	105.036865	50.088973
464.493590	104.551431	50.093978
460.992014	112.560220	50.098983
457.589092	113.510907	50.103988
454.403113	106.530735	50.108993
450.689666	108.289378	50.113997
447.857264	102.797769	50.119002
444.163020	102.310264	50.124007
440.195547	101.745332	50.129012
436.899572	100.050147	50.134017
433.227623	110.863458	50.139021
429.402817	108.615181	50.144026
426.093149	111.870349	50.149031
422.903746	102.429280	50.154036
419.633087	102.501871	50.159041
416.031903	106.815123	50.164045
412.290151	101.681104	50.169050
408.998510	110.739050	50.174055
405.331877	109.155719	50.179060
401.859818	95.478300	50.184065
398.368994	103.330394	50.189069
394.549647	99.034294	50.194074
390.938436	102.814441	50.199079
387.760177	96.083032	50.204084
384.542443	97.672302	50.209089
380.466353	101.740411	50.214093
377.811206	92.886409	50.219098
373.726416	107.535666	50.224103
370.110939	98.249950	50.229108
367.005631	94.190035	50.234113
363.090889	113.574197	50.239117
359.729933	104.248614	50.244122
355.926092	99.668523	50.249127
352.529552	98.558610	50.254132
349.297608	95.749259	50.259137
345.604874	105.591398	50.264141
342.308813	102.918645	50.269146
338.888293	99.724378	50.274151
335.416115	96.576171	50.279156
331.968471	101.441215	50.284161
328.244340	104.653769	50.289165
324.905905	104.347864	50.294170
321.124164	101.615155	50.299175
317.510482	108.502579	50.304180
314.351837	101.015140	50.309185
310.529187	110.444201	50.314189
307.666574	104.916246	50.319194
304.029356	105.429122	50.324199
300.300383	104.981918	50.329204
296.478893	102.749002	50.334209
292.728895	104.238183	50.339213
289.452639	98.964862	50.344218
286.076714	102.749320	50.349223
282.897856	103.174583	50.354228
279.209656	101.917394	50.359233
275.555401	107.469733	50.364237
272.527859	112.012722	50.369242
268.844413	105.502869	50.374247
265.161820	116.118584	50.379252
261.796769	102.209329	50.384257
257.694822	111.062056	50.389261
254.506614	103.601419	50.394266
251.006510	112.442127	50.399271
247.468405	107.387014	50.404276
244.653460	98.162617	50.409281
240.418474	105.473269	50.414285
237.360373	106.904705	50.419290
233.585994	101.617690	50.424295
229.931635	111.650014	50.429300
226.826404	101.974380	50.434305
223.226370	112.950503	50.439309
219.695476	104.357136	50.444314
216.135179	100.564712	50.449319
212.335179	98.144967	50.454324
209.228698	94.961671	50.459329
205.769546	107.282489	50.464333
202.039948	98.707607	50.469338
198.279118	98.825432	50.474343
195.066398	100.436131	50.479348
191.873985	100.414289	50.484353
188.490816	103.779130	50.489357
184.221708	98.848060	50.494362
181.100697	111.226647	50.499367
176.971495	112.234273	50.504372
173.833789	98.314759	50.509377
170.270263	108.443604	50.514381
166.894240	103.628896	50.519386
163.858851	104.661323	50.524391
160.199554	102.896612	50.529396
156.952056	98.001663	50.534401
153.029083	113.403943	50.539405
149.675471	98.290709	50.544410
145.977267	101.859947	50.549415
142.685351	99.306849	50.554420
139.452261	95.165800	50.559425
135.259118	101.916274	50.564429
131.963142	89.593994	50.569434
128.377251	102.171972	50.574439
124.755218	101.496116	50.579444
121.725325	106.153414	50.584449
117.999616	106.531531	50.589453
114.452082	100.231419	50.594458
110.869005	104.817198	50.599463
107.301863	105.787418	50.604468
104.052563	104.322335	50.609473
100.380934	102.407721	50.614477
97.088874	98.029150	50.619482
93.544093	109.309872	50.624487
89.819476	114.373424	50.629492
86.431329	104.169527	50.634497
82.954682	111.589230	50.639501
79.294774	111.925416	50.644506
75.517513	101.969155	50.649511
72.719603	101.401486	50.654516
68.892085	106.351451	50.659521
65.413495	107.763402	50.664525
62.050319	102.984692	50.669530
58.526586	105.207325	50.674535
54.724542	106.128947	50.679540
51.476189	103.230534	50.684545
47.731597	108.642085	50.689549
44.593330	98.497139	50.694554
41.227124	106.722139	50.699559
37.433941	102.184822	50.704564
33.790495	102.856975	50.709569
30.291539	107.622597	50.714573
27.086402	98.082931	50.719578
23.264407	104.936656	50.724583
19.677181	106.789596	50.729588
16.514626	91.621192	50.734593
12.792874	104.410322	50.739597
9.455922	94.922957	50.744602
6.057414	93.433834	50.749607
2.663965	96.537757	50.754612