Thu Aug 25 17:10:23 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
1.514420	96.466156	0.000000
1.497997	107.276356	0.005005
1.141174	100.334029	0.010010
1.523856	94.304071	0.015014
1.236709	93.681589	0.020019
1.265650	76.197171	0.025024
0.759481	75.738723	0.030029
0.214762	57.126146	0.035034
0.003618	43.741685	0.040038
-0.240591	41.135110	0.045043
-0.663617	28.869038	0.050048
-0.803925	21.418250	0.055053
-1.188794	13.936181	0.060058
-1.088889	4.916491	0.065062
-1.482345	14.181672	0.070067
-1.853811	-1.009466	0.075072
-2.269269	-5.664642	0.080077
-2.749490	-3.722680	0.085082
-2.435797	2.704518	0.090086
-3.171743	-14.672621	0.095091
-3.703764	-14.462621	0.100096
-3.835262	-14.214137	0.105101
-4.192545	-9.061219	0.110106
-3.940550	-14.187970	0.115110
-4.944049	-18.415645	0.120115
-5.207861	-10.335060	0.125120
-5.216772	-6.394670	0.130125
-5.404961	-15.476778	0.135130
-5.050264	-17.908261	0.140134
-5.441809	-6.014291	0.145139
-6.246253	-0.933678	0.150144
-6.941488	-13.030518	0.155149
-7.006084	-4.987473	0.160154
-7.234476	-13.465328	0.165158
-6.861344	-7.294222	0.170163
-7.297631	-6.311442	0.175168
-7.192811	-9.719348	0.180173
-7.427745	-14.981777	0.185178
-8.216938	-16.787939	0.190182
-8.541179	-3.474485	0.195187
-8.597928	-10.482767	0.200192
-8.836464	-10.467449	0.205197
-8.913704	-11.031066	0.210202
-9.112006	-12.107228	0.215206
-9.844560	-11.973377	0.220211
-9.935225	-12.503252	0.225216
-10.315577	-6.242561	0.230221
-10.399592	-9.130493	0.235226
-10.100593	-8.737488	0.240230
-11.059598	-7.495633	0.245235
-11.503017	-16.471310	0.250240
-11.480073	-12.526421	0.255245
-11.812729	-2.751916	0.260250
-11.545441	-7.162887	0.265254
-11.832014	4.838030	0.270259
-12.174172	-12.078786	0.275264
-12.881777	-13.979988	0.280269
-13.048769	-1.725728	0.285274
-12.918878	-16.454399	0.290278
-13.130951	-7.999103	0.295283
-13.193241	-7.138198	0.300288
-13.562562	-13.917167	0.305293
-14.441340	-4.904987	0.310298
-14.045361	-12.920682	0.315302
-14.161894	-3.113602	0.320307
-14.815725	-5.500962	0.325312
-15.414574	-5.650653	0.330317
-15.650831	-8.460947	0.335322
-15.711330	-1.956139	0.340326
-16.023076	0.978164	0.345331
-15.905669	-2.944248	0.350336
-15.878725	-0.778028	0.355341
-17.071168	-3.052521	0.360346
-17.111505	0.456193	0.365350
-17.574954	-0.610063	0.370355
-17.299631	-4.373719	0.375360
-17.056387	3.462907	0.380365
-17.353518	-0.945051	0.385370
-18.248433	3.260716	0.390374
-18.676792	2.169979	0.395379
-18.754354	-10.400131	0.400384
-18.743310	-1.533699	0.405389
-18.761425	-3.210738	0.410394
-19.012095	0.074666	0.415398
-19.945757	-5.090940	0.420403
-20.141865	2.555095	0.425408
-20.029237	-2.755468	0.430413
-20.231885	2.094811	0.435418
-20.203526	-12.513550	0.440422
-21.187943	3.184433	0.445427
-21.462202	0.022584	0.450432
-21.657483	-5.138492	0.455437
-21.949444	6.296953	0.460442
-21.857831	-4.391908	0.465446
-22.070670	-0.394254	0.470451
-21.754675	-11.719386	0.475456
-22.636999	0.166064	0.480461
-23.004304	3.336865	0.485466
-23.085058	-2.414801	0.490470
-23.194305	-1.163721	0.495475
-23.281877	-10.226793	0.500480
-24.081579	-3.754861	0.505485
-24.848415	3.490214	0.510490
-24.757416	-15.414881	0.515494
-24.653727	0.365710	0.520499
-25.027146	-3.963854	0.525504
-25.093400	-7.822686	0.530509
-25.118342	6.943509	0.535514
-25.274205	-6.256582	0.540518
-25.958924	-1.707260	0.545523
-26.112727	-0.578913	0.550528
-26.448235	-3.069933	0.555533
-26.463165	-2.535990	0.560538
-26.879827	0.686837	0.565542
-27.280865	-3.097393	0.570547
-27.476540	-8.745628	0.575552
-27.674232	-10.359728	0.580557
-27.723160	-3.606796	0.585562
-27.571765	-6.661329	0.590566
-28.161014	-6.840998	0.595571
-28.934200	-9.817100	0.600576
-28.939282	-10.958338	0.605581
-29.150927	-7.400638	0.610586
-28.950114	-16.410816	0.615590
-29.832943	-6.236895	0.620595
-30.331266	-4.421810	0.625600
-30.801960	1.558808	0.630605
-30.854369	-0.169807	0.635610
-30.717260	-8.119632	0.640614
-30.727769	9.099395	0.645619
-30.987101	-1.578771	0.650624
-30.778042	-1.342518	0.655629
-31.359254	-4.921344	0.660634
-32.087096	-5.892388	0.665638
-32.068425	-3.487589	0.670643
-32.355634	-7.745237	0.675648
-32.467183	-11.103421	0.680653
-32.995050	-10.675770	0.685658
-33.151773	-6.911538	0.690662
-33.527097	-10.187263	0.695667
-33.520128	-3.683537	0.700672
-33.797577	-1.931534	0.705677
-33.972692	4.081865	0.710682
-34.343536	-1.500959	0.715686
-35.078770	-3.325065	0.720691
-35.122747	0.393028	0.725696
-35.199486	2.923510	0.730701
-35.229816	-5.208890	0.735706
-35.075622	-9.795130	0.740710
-35.921550	9.642891	0.745715
-36.071440	-1.112535	0.750720
-36.330442	-5.143648	0.755725
-36.578881	-1.342898	0.760730
-37.067440	-0.358253	0.765734
-37.669063	5.177806	0.770739
-37.425023	5.579422	0.775744
-37.546446	2.241765	0.780749
-38.221981	7.814716	0.785754
-37.892761	-2.772169	0.790758
-38.537856	-3.379687	0.795763
-38.531560	4.253616	0.800768
-39.082808	2.356389	0.805773
-39.799669	-0.141317	0.810778
-39.448585	-8.558107	0.815782
-39.705221	-2.082680	0.820787
-39.914740	-3.397531	0.825792
-39.735688	-2.153659	0.830797
-40.244781	1.305116	0.835802
-40.523761	-11.878841	0.840806
-40.687511	2.089679	0.845811
-40.784225	-0.255258	0.850816
-41.195351	-1.608123	0.855821
-42.058916	-1.539163	0.860826
-42.275868	-6.000810	0.865830
-42.712141	5.409788	0.870835
-42.395996	-13.359740	0.875840
-42.190600	-7.538845	0.880845
-42.440398	0.925528	0.885850
-42.946257	1.792661	0.890854
-43.371702	-1.801081	0.895859
-44.043841	-4.694938	0.900864
-43.599632	1.173963	0.905869
-43.964539	2.202509	0.910874
-44.741569	-3.468530	0.915878
-45.078445	0.700420	0.920883
-45.018361	2.428010	0.925888
-45.060386	-4.832518	0.930893
-45.433967	4.325138	0.935898
-45.212425	0.155453	0.940902
-45.979737	-0.489863	0.945907
-46.443451	-4.963466	0.950912
-46.128274	5.215738	0.955917
-46.685240	-7.295073	0.960922
-46.725288	-11.430094	0.965926
-47.168464	0.079660	0.970931
-47.907670	-4.211570	0.975936
-48.346134	-10.701291	0.980941
-48.601966	0.839220	0.985946
-48.390157	-10.254450	0.990950
-48.472240	-6.033675	0.995955
-48.768286	-3.506796	1.000960
-48.072732	0.696538	1.005965
-48.888464	-1.105462	1.010970
-49.304532	-5.409358	1.015974
-49.788068	-4.112285	1.020979
-50.053301	-0.577825	1.025984
-49.897865	3.052074	1.030989
-50.528577	0.784482	1.035994
-51.085369	-8.831495	1.040998
-51.570739	-3.642688	1.046003
-51.781009	-1.284274	1.051008
-51.181886	-4.355177	1.056013
-51.507301	1.365393	1.061018
-51.404249	1.017138	1.066022
-51.832735	3.542623	1.071027
-52.309908	0.064556	1.076032
-52.781615	2.599977	1.081037
-53.273498	4.951897	1.086042
-52.830037	-5.526334	1.091046
-52.961983	1.692027	1.096051
-53.590962	1.553387	1.101056
-53.993093	-8.725907	1.106061
-54.567461	-7.620247	1.111066
-54.454040	-0.614341	1.116070
-54.928551	0.890127	1.121075
-54.797466	-0.835601	1.126080
-55.153434	3.804582	1.131085
-56.082974	3.184686	1.136090
-55.809389	2.360453	1.141094
-56.073166	-0.002599	1.146099
-56.225309	-4.290902	1.151104
-56.480384	-4.538749	1.156109
-56.785923	5.845283	1.161114
-56.472301	-4.492381	1.166118
-57.548740	0.010753	1.171123
-57.737104	1.894332	1.176128
-57.552596	0.985979	1.181133
-57.723436	6.214092	1.186138
-57.786732	-7.829409	1.191142
-58.842086	-1.513570	1.196147
-59.141757	-0.713546	1.201152
-59.274510	-2.382114	1.206157
-59.281665	0.839823	1.211162
-59.305888	-1.054560	1.216166
-59.801826	-3.425527	1.221171
-59.262219	0.742130	1.226176
-60.081312	-1.964183	1.231181
-60.832675	-1.789415	1.236186
-60.792844	-3.105371	1.241190
-61.031082	4.591557	1.246195
-61.020188	-6.622494	1.251200
-61.002248	-5.764668	1.256205
-61.590844	1.961847	1.261210
-61.574304	-6.605005	1.266214
-61.829822	-2.521570	1.271219
-62.732166	1.511357	1.276224
-63.440179	-1.990651	1.281229
-63.571107	1.060854	1.286234
-63.568574	-3.941388	1.291238
-63.601161	10.250195	1.296243
-63.639911	3.526995	1.301248
-63.574720	-1.111740	1.306253
-63.946986	-6.738631	1.311258
-64.199795	-1.203445	1.316262
-64.899000	4.711738	1.321267
-64.682783	-4.509667	1.326272
-64.898164	0.807681	1.331277
-65.390480	-5.135759	1.336282
-65.859256	1.252685	1.341286
-66.660374	5.329863	1.346291
-66.303873	6.144131	1.351296
-66.315454	-5.803559	1.356301
-66.636412	5.209316	1.361306
-66.857502	-4.003679	1.366310
-67.721362	-4.830019	1.371315
-67.754519	3.426401	1.376320
-68.068033	-11.381488	1.381325
-68.049020	1.055597	1.386330
-67.828899	0.533973	1.391334
-68.222900	4.294257	1.396339
-68.284359	-2.048892	1.401344
-68.801648	-4.995485	1.406349
-69.541718	2.473189	1.411354
-69.627537	3.888280	1.416358
-69.730327	3.645045	1.421363
-69.728728	1.797236	1.426368
-70.210861	-0.465161	1.431373
-70.909455	-0.877632	1.436378
-70.630016	2.204485	1.441382
-70.817238	2.901468	1.446387
-70.964678	0.169008	1.451392
-71.580561	-0.737317	1.456397
-72.441804	-2.680881	1.461402
-72.304369	-11.554577	1.466406
-72.856885	-6.219206	1.471411
-72.615123	-8.212214	1.476416
-72.368490	-10.297734	1.481421
-72.721746	-4.797431	1.486426
-72.603436	-17.885443	1.491430
-73.140366	-2.972598	1.496435
-73.456238	-4.470102	1.501440
-73.711579	1.435642	1.506445
-74.893780	-5.383633	1.511450
-74.723782	-7.542567	1.516454
-75.248165	-3.771346	1.521459
-75.472022	-6.143816	1.526464
-75.218931	-6.139091	1.531469
-75.982090	-1.985604	1.536474
-75.427637	-6.365640	1.541478
-75.521813	-5.173869	1.546483
-75.941415	2.640062	1.551488
-76.267284	-10.593492	1.556493
-76.871073	-4.772357	1.561498
-77.116074	-6.027863	1.566502
-77.479318	-4.768621	1.571507
-77.354439	-7.407707	1.576512
-77.707573	-1.920078	1.581517
-78.200792	0.656680	1.586522
-78.232222	1.174226	1.591526
-78.730223	1.309296	1.596531
-78.719600	-1.644085	1.601536
-78.583831	-11.912745	1.606541
-79.195990	-3.704810	1.611546
-79.616300	-8.185210	1.616550
-80.075710	-1.159151	1.621555
-80.362547	1.059399	1.626560
-79.827919	-6.373741	1.631565
-80.145187	1.591835	1.636570
-80.574286	-5.035394	1.641574
-81.309679	0.243212	1.646579
-81.635360	0.164618	1.651584
-81.477142	-2.679011	1.656589
-82.102568	-0.730112	1.661594
-81.794270	-1.572440	1.666598
-81.979860	2.101403	1.671603
-82.725683	-2.628551	1.676608
-82.946039	-0.404599	1.681613
-83.133903	-9.122919	1.686618
-83.213229	-9.528018	1.691622
-83.584387	-0.997175	1.696627
-83.650680	-8.168474	1.701632
-84.092659	-5.533306	1.706637
-84.798489	1.980623	1.711642
-84.497077	-8.902457	1.716646
-84.858894	-8.969061	1.721651
-84.984140	-3.099522	1.726656
-84.951705	-1.854823	1.731661
-85.574943	1.960363	1.736666
-85.946581	-3.122454	1.741670
-86.051591	2.164944	1.746675
-86.146998	-7.893486	1.751680
-86.295659	-6.873513	1.756685
-86.775812	-0.363063	1.761690
-87.106250	-7.635342	1.766694
-87.626596	-6.297699	1.771699
-87.588508	-8.211335	1.776704
-87.666609	-6.133062	1.781709
-87.755081	-4.540385	1.786714
-88.094320	-9.435287	1.791718
-88.997325	-4.263297	1.796723
-89.451298	3.511728	1.801728
-89.076089	0.922001	1.806733
-89.473362	1.234278	1.811738
-89.085391	-4.578174	1.816742
-89.046169	-0.398553	1.821747
-89.981234	-3.365102	1.826752
-90.202674	-8.392359	1.831757
-90.410157	-3.376809	1.836762
-90.580358	-6.017115	1.841766
-91.133452	-5.427319	1.846771
-91.588528	-3.153932	1.851776
-91.863384	-8.995401	1.856781
-92.475561	4.265093	1.861786
-92.435522	-14.204897	1.866790
-92.660889	-16.305043	1.871795
-92.450047	-4.328296	1.876800
-92.199521	-10.388131	1.881805
-92.344458	-6.084741	1.886810
-92.914258	-14.746373	1.891814
-93.433418	-3.095003	1.896819
-93.814235	-4.370356	1.901824
-93.962617	-2.394966	1.906829
-94.873006	3.230604	1.911834
-95.063579	-16.342208	1.916838
-95.202583	-10.176285	1.921843
-95.287961	-4.901457	1.926848
-94.875048	-15.590031	1.931853
-95.461211	-4.374254	1.936858
-95.219785	-6.395684	1.941862
-95.774264	-4.296549	1.946867
-96.313852	-1.095588	1.951872
-96.611130	-7.752961	1.956877
-96.959368	0.021312	1.961882
-96.932313	-9.850660	1.966886
-97.368849	-2.388421	1.971891
-97.617253	-8.794022	1.976896
-97.874138	-5.311491	1.981901
-97.882513	-1.149722	1.986906
-97.976671	-2.757897	1.991910
-98.469252	-1.782110	1.996915
-99.192409	-4.446321	2.006912
-98.854115	0.781618	2.016909
-98.247152	-2.500148	2.026906
-97.601385	-2.442768	2.036902
-97.199964	-8.594056	2.046899
-96.363152	-0.060992	2.056896
-96.044982	0.551406	2.066893
-95.945726	-2.238987	2.076890
-94.990687	4.530080	2.086886
-94.460197	2.844211	2.096883
-94.038469	3.329509	2.106880
-93.235355	-2.089600	2.116877
-92.934620	-0.308709	2.126874
-92.811929	-6.162896	2.136870
-92.332358	-4.552580	2.146867
-91.740091	-2.665314	2.156864
-90.887902	0.495872	2.166861
-90.328170	6.911898	2.176858
-89.843918	-2.759160	2.186854
-89.785874	-4.066887	2.196851
-89.057903	1.052476	2.206848
-88.500652	2.134265	2.216845
-88.418607	1.136391	2.226842
-87.368624	-4.549483	2.236838
-87.347776	-6.614828	2.246835
-86.347257	-4.832715	2.256832
-85.750126	-2.116240	2.266829
-85.902047	-7.781677	2.276826
-85.359792	-1.169677	2.286822
-84.613047	-6.510260	2.296819
-84.062005	-9.732576	2.306816
-83.396262	-4.869561	2.316813
-83.207565	-8.092122	2.326810
-82.567394	-9.411869	2.336806
-81.826536	-5.963972	2.346803
-81.389096	-6.786281	2.356800
-81.481993	-4.246788	2.366797
-80.629839	-6.936575	2.376794
-80.381355	-3.683959	2.386790
-79.242575	1.656139	2.396787
-78.719069	-5.946140	2.406784
-78.729567	-7.803832	2.416781
-77.891863	-4.117683	2.426778
-77.567610	-1.009988	2.436774
-77.394803	-0.140392	2.446771
-76.201832	-6.520250	2.456768
-76.074047	-4.934006	2.466765
-75.990045	-1.890036	2.476762
-74.884360	-0.526713	2.486758
-74.312979	-3.359407	2.496755
-74.138340	-8.081316	2.506752
-73.051699	-13.490994	2.516749
-73.273935	-12.540491	2.526746
-72.885803	-8.118654	2.536742
-72.147697	-2.313460	2.546739
-71.300391	-7.682469	2.556736
-70.601017	-8.362087	2.566733
-70.811532	-7.239190	2.576730
-69.920258	-8.192800	2.586726
-69.369714	-5.614744	2.596723
-68.594636	-3.075038	2.606720
-68.392257	-3.784487	2.616717
-68.424204	-4.406534	2.626714
-67.630932	-4.749235	2.636710
-67.317094	-6.762287	2.646707
-66.433461	-2.278705	2.656704
-66.030795	0.804034	2.666701
-65.637571	-2.352373	2.676698
-64.798655	-6.345230	2.686694
-64.160604	-4.161025	2.696691
-64.029436	-3.741071	2.706688
-63.821295	0.354175	2.716685
-63.347245	-2.954281	2.726682
-63.081585	-0.078159	2.736678
-61.931041	-8.187338	2.746675
-61.096937	-4.240861	2.756672
-60.492949	1.452303	2.766669
-60.368787	2.145787	2.776666
-60.386656	1.711604	2.786662
-59.529960	2.147755	2.796659
-58.771432	2.859050	2.806656
-58.799698	4.751684	2.816653
-57.815931	8.332588	2.826650
-57.600786	5.308622	2.836646
-57.196302	-1.650946	2.846643
-56.225990	-5.287420	2.856640
-55.974969	0.685967	2.866637
-55.713169	3.784443	2.876634
-54.641723	7.281917	2.886630
-54.291989	1.382646	2.896627
-54.314691	-3.558602	2.906624
-53.168742	-2.588061	2.916621
-53.026356	-0.107608	2.926618
-52.923352	-2.404407	2.936614
-51.808742	3.275273	2.946611
-51.696964	0.828210	2.956608
-50.767696	-1.417491	2.966605
-50.350615	-1.542854	2.976602
-50.034519	-1.142373	2.986598
-49.377703	-2.458391	2.996595
-48.941725	-3.863350	3.006592
-48.719375	0.841062	3.016589
-47.574470	-5.052921	3.026586
-47.093845	-1.247460	3.036582
-46.939084	-2.031811	3.046579
-46.711457	-8.520169	3.056576
-45.601263	-1.024631	3.066573
-45.607806	-1.346546	3.076570
-45.393676	0.261016	3.086566
-44.498695	-3.363654	3.096563
-44.255848	-3.132262	3.106560
-43.177593	-2.819525	3.116557
-43.029460	-1.724313	3.126554
-42.508840	-0.351677	3.136550
-41.324683	-6.286655	3.146547
-41.063150	-1.540865	3.156544
-41.139669	-2.586753	3.166541
-40.804575	-4.070940	3.176538
-39.975834	-4.251302	3.186534
-39.666728	-6.589898	3.196531
-38.889862	-7.820187	3.206528
-38.647749	-6.321548	3.216525
-37.928062	0.500244	3.226522
-37.145099	-7.326422	3.236518
-36.970360	-6.599681	3.246515
-36.786557	-9.824643	3.256512
-35.814743	-13.686264	3.266509
-35.524111	-3.977878	3.276506
-35.083273	-1.078517	3.286502
-34.221512	-7.542692	3.296499
-33.802196	1.464450	3.306496
-33.704757	2.371200	3.316493
-32.897368	0.496227	3.326490
-32.465434	-6.062159	3.336486
-31.518278	-7.173409	3.346483
-31.202659	-7.476111	3.356480
-31.113415	-14.446470	3.366477
-30.541435	-5.333370	3.376474
-29.900985	-3.212893	3.386470
-29.565642	-4.082560	3.396467
-28.377773	-6.973833	3.406464
-28.065248	-9.240105	3.416461
-28.185049	0.447063	3.426458
-27.812020	-1.043068	3.436454
-26.839244	-7.597497	3.446451
-26.590957	0.913752	3.456448
-25.564330	-8.300589	3.466445
-25.088999	7.492777	3.476442
-25.193789	-1.461925	3.486438
-24.389681	7.804880	3.496435
-23.651407	-0.961968	3.506432
-23.411317	-1.607633	3.516429
-23.210890	-8.199436	3.526426
-22.361914	-9.393504	3.536422
-22.154343	-4.712119	3.546419
-21.108124	-1.727046	3.556416
-20.781144	-9.038769	3.566413
-20.713517	-4.984861	3.576410
-19.776428	-2.815828	3.586406
-19.202983	-4.727004	3.596403
-19.160980	-9.782928	3.606400
-17.963350	-9.301990	3.616397
-17.840217	-7.572464	3.626394
-17.403054	-9.915285	3.636390
-17.105640	-12.210867	3.646387
-16.551763	-8.480239	3.656384
-15.987160	-8.368953	3.666381
-15.011403	-6.161629	3.676378
-15.029248	1.510664	3.686374
-14.557509	-4.673820	3.696371
-13.458854	-12.825549	3.706368
-13.397632	-1.972474	3.716365
-13.361901	-5.437166	3.726362
-12.285167	-11.833651	3.736358
-11.825453	-4.480109	3.746355
-11.191722	-4.050200	3.756352
-10.775174	-1.650717	3.766349
-10.695332	-8.917381	3.776346
-9.720920	-4.824986	3.786342
-9.086207	-7.205097	3.796339
-8.769956	-3.972598	3.806336
-8.662761	-1.717881	3.816333
-7.644013	-9.590994	3.826330
-7.365260	-12.770644	3.836326
-6.961132	-7.210888	3.846323
-5.857516	-8.444853	3.856320
-5.902147	-1.335406	3.866317
-5.499061	-5.285314	3.876314
-4.989770	-1.246754	3.886310
-4.678680	-2.717676	3.896307
-4.263137	4.297497	3.906304
-3.816087	8.447183	3.916301
-3.041650	24.390108	3.926298
-2.698967	29.769433	3.936294
-2.104243	50.273715	3.946291
-1.890487	59.385959	3.956288
-1.192033	65.124538	3.966285
-0.891205	87.198645	3.976282
-0.182762	102.394866	3.986278
0.000000	102.361669	3.991283
0.077145	117.194222	3.996288
0.540929	123.376480	4.001293
0.527606	126.915788	4.006298
0.434076	134.251575	4.011302
0.831493	124.277197	4.016307
0.675294	131.230490	4.021312
0.966243	135.740871	4.026317
0.979491	132.692140	4.031322
0.848100	140.875433	4.036326
1.000181	145.932766	4.041331
1.059849	148.090714	4.046336
1.305432	147.862496	4.051341
0.897503	130.927373	4.056346
0.840636	129.300685	4.061350
1.140951	141.038893	4.066355
1.235632	150.407998	4.071360
1.402182	130.389902	4.076365
1.012422	132.896681	4.081370
0.935800	136.882514	4.086374
0.974972	135.835574	4.091379
0.671887	135.557279	4.096384
1.369210	144.942690	4.101389
1.317556	149.838954	4.106394
1.473152	145.293584	4.111398
1.161432	136.107365	4.116403
1.069938	139.586156	4.121408
1.168294	122.723577	4.126413
1.017970	129.296292	4.131418
1.120594	137.797264	4.136422
1.385014	143.447609	4.141427
0.977734	146.023575	4.146432
1.388233	140.568219	4.151437
1.320807	145.254978	4.156442
1.411088	148.189590	4.161446
1.621773	137.735090	4.166451
1.285061	134.766503	4.171456
1.453680	133.566400	4.176461
1.103090	137.329400	4.181466
1.239986	130.062927	4.186470
1.251765	135.316250	4.191475
1.370708	145.719279	4.196480
1.522608	149.852810	4.201485
1.586581	150.266826	4.206490
1.119530	137.222953	4.211494
1.654696	135.380114	4.216499
1.371777	147.545073	4.221504
1.470574	138.167979	4.226509
1.512759	137.104748	4.231514
1.100253	135.973551	4.236518
1.146946	141.553605	4.241523
1.332205	155.989593	4.246528
1.507248	156.316603	4.251533
1.696038	156.824959	4.256538
1.956980	163.640137	4.261542
2.022196	155.562294	4.266547
1.539612	154.486370	4.271552
1.172957	138.032000	4.276557
1.353723	153.300771	4.281562
1.551906	153.902570	4.286566
1.660645	154.249459	4.291571
1.801523	166.911187	4.296576
1.786973	160.889661	4.301581
1.789020	170.159394	4.306586
1.651543	158.759669	4.311590
1.690863	153.343484	4.316595
1.265897	151.385321	4.321600
1.774005	160.322653	4.326605
1.499247	163.887112	4.331610
1.647999	159.298516	4.336614
1.714265	149.119743	4.341619
1.280702	156.632204	4.346624
1.667541	150.225083	4.351629
1.832256	153.185998	4.356634
1.651171	156.058724	4.361638
1.717898	156.114798	4.366643
1.725858	156.132623	4.371648
1.801676	151.523819	4.376653
1.347462	154.211545	4.381658
1.974533	153.711579	4.386662
2.045331	150.774052	4.391667
1.560243	160.284624	4.396672
1.923367	150.676279	4.401677
1.837616	148.889597	4.406682
1.582188	161.423587	4.411686
1.890557	152.551497	4.416691
1.669762	156.319475	4.421696
1.886065	173.031720	4.426701
2.220914	175.349038	4.431706
2.021961	176.626842	4.436710
2.015194	170.914147	4.441715
1.560699	161.076394	4.446720
1.875738	168.471567	4.451725
2.023561	173.678274	4.456730
1.865576	183.985508	4.461734
1.860401	184.100305	4.466739
1.939997	182.876182	4.471744
2.112232	184.314130	4.476749
2.244159	179.478225	4.481754
2.055065	181.634024	4.486758
2.517349	173.876780	4.491763
2.268039	186.188362	4.496768
2.612219	175.852132	4.501773
2.282692	164.302157	4.506778
1.994572	157.260456	4.511782
2.195034	155.451076	4.516787
2.045875	163.339765	4.521792
2.346664	175.849891	4.526797
2.146724	166.228519	4.531802
2.528584	177.719853	4.536806
2.306019	162.071803	4.541811
1.911806	155.673160	4.546816
2.239534	164.724179	4.551821
2.352361	165.048281	4.556826
2.271721	168.272273	4.561830
2.283011	166.780438	4.566835
1.972267	174.950719	4.571840
2.422462	178.926786	4.576845
2.409940	174.426732	4.581850
2.472250	185.246789	4.586854
2.766702	173.532601	4.591859
2.132526	165.621285	4.596864
2.702311	163.630649	4.601869
2.330247	157.772710	4.606874
2.064233	149.642363	4.611878
2.500949	163.842803	4.616883
2.174450	169.408570	4.621888
2.549352	166.926439	4.626893
2.537685	172.730786	4.631898
2.059990	183.973980	4.636902
2.324632	178.025765	4.641907
1.777291	178.595677	4.646912
1.863396	174.222541	4.651917
2.417585	178.748636	4.656922
2.106924	186.966367	4.661926
2.744689	186.322352	4.666931
2.378735	188.841228	4.671936
2.423906	193.390132	4.676941
2.759043	196.849546	4.681946
2.825299	204.498854	4.686950
2.381208	193.802058	4.691955
2.388048	206.788541	4.696960
2.671322	207.560511	4.701965
2.799220	198.982435	4.706970
2.711208	207.510146	4.711974
2.853616	199.948546	4.716979
2.687343	202.588000	4.721984
2.464200	194.960289	4.726989
2.747702	204.072042	4.731994
2.655591	203.418998	4.736998
3.082341	209.448898	4.742003
2.714691	199.698759	4.747008
3.011960	191.144771	4.752013
2.723340	186.387411	4.757018
2.753289	182.548266	4.762022
2.605315	185.706879	4.767027
2.918615	203.663153	4.772032
3.160919	197.123634	4.777037
2.909406	188.522752	4.782042
2.688950	177.022119	4.787046
2.711405	181.305656	4.792051
2.599312	191.010906	4.797056
3.122078	197.240898	4.802061
3.182610	198.101552	4.807066
2.749508	195.676414	4.812070
2.494967	191.843875	4.817075
2.838294	194.371844	4.822080
3.156914	204.262721	4.827085
3.118339	209.818190	4.832090
2.943810	209.443820	4.837094
3.147177	203.758303	4.842099
3.011187	197.107210	4.847104
3.058984	188.038644	4.852109
2.958781	195.631770	4.857114
3.435359	197.265648	4.862118
3.019672	191.332274	4.867123
2.698993	179.249382	4.872128
2.848436	195.592466	4.877133
3.148846	207.789457	4.882138
2.715698	204.598681	4.887142
3.058865	201.438133	4.892147
2.827932	206.814929	4.897152
3.060401	205.142900	4.902157
3.163678	203.114619	4.907162
2.798140	206.946416	4.912166
3.248440	208.571757	4.917171
2.876961	207.763164	4.922176
3.192002	206.362942	4.927181
2.843162	222.281076	4.932186
3.093099	221.286530	4.937190
3.444071	201.660247	4.942195
3.109963	213.431466	4.947200
3.120206	206.523335	4.952205
3.153562	205.955038	4.957210
2.966006	211.682550	4.962214
2.912451	216.519018	4.967219
3.239588	236.836530	4.972224
3.489647	236.674050	4.977229
3.417827	230.623508	4.982234
3.308321	244.808355	4.987238
3.689256	235.627454	4.992243
3.516963	232.927324	4.997248
3.209820	232.602206	5.002253
3.362982	223.273499	5.007258
3.422955	237.052126	5.012262
3.469475	232.466875	5.017267
3.472797	237.471610	5.022272
3.459530	230.171676	5.027277
3.345132	229.680314	5.032282
3.315568	237.809731	5.037286
3.920563	234.487928	5.042291
3.361971	231.376915	5.047296
3.413791	235.931116	5.052301
3.503513	233.120328	5.057306
3.497480	237.740544	5.062310
3.889738	228.228835	5.067315
3.673816	238.551506	5.072320
3.358460	231.482405	5.077325
3.546861	240.283204	5.082330
3.591459	236.324690	5.087334
3.673483	230.889136	5.092339
3.161770	239.147883	5.097344
3.500690	239.977576	5.102349
3.372607	230.170900	5.107354
3.252024	236.473233	5.112358
3.432171	228.095770	5.117363
3.255644	240.301070	5.122368
3.693802	226.735641	5.127373
3.356016	228.911580	5.132378
3.489804	245.671623	5.137382
3.901618	253.472457	5.142387
3.718030	266.280009	5.147392
3.833867	263.161397	5.152397
3.850017	262.678053	5.157402
3.975888	259.013692	5.162406
3.869721	246.995222	5.167411
3.546963	248.292429	5.172416
3.957799	246.250756	5.177421
4.095633	252.129783	5.182426
3.840188	241.735602	5.187430
4.204057	239.011575	5.192435
3.905037	243.465722	5.197440
4.095303	228.154736	5.202445
3.812679	227.278435	5.207450
3.529018	233.840442	5.212454
3.753042	220.096593	5.217459
3.679184	235.285105	5.222464
4.348476	245.617781	5.227469
3.885735	235.525009	5.232474
3.570493	233.805914	5.237478
3.817953	242.917007	5.242483
3.937408	249.295632	5.247488
4.185350	253.796962	5.252493
4.247988	255.166665	5.257498
4.281179	257.072505	5.262502
4.330141	250.395577	5.267507
3.842211	241.765272	5.272512
4.000936	227.101484	5.277517
4.330737	241.024503	5.282522
3.862299	230.097377	5.287526
4.266187	236.159343	5.292531
4.016297	231.174436	5.297536
4.180549	237.210673	5.302541
4.454372	249.595359	5.307546
3.980280	241.608306	5.312550
4.029743	235.643166	5.317555
3.824816	252.940352	5.322560
3.947562	257.888416	5.327565
3.956555	253.910166	5.332570
3.865976	259.847131	5.337574
4.256208	250.525558	5.342579
4.451252	259.771425	5.347584
4.266661	255.276164	5.352589
4.712806	259.211754	5.357594
3.727120	259.821875	5.362598
4.092321	254.648835	5.367603
4.265083	259.756746	5.372608
4.038079	259.203931	5.377613
3.961223	255.074613	5.382618
4.247897	265.568493	5.387622
4.470358	247.442966	5.392627
4.229447	267.409746	5.397632
3.830600	258.044121	5.402637
4.326832	278.515525	5.407642
4.409164	286.839409	5.412646
4.716946	282.153096	5.417651
4.372053	282.662816	5.422656
4.723637	293.785636	5.427661
4.589040	285.846612	5.432666
4.590836	275.238096	5.437670
4.308672	270.650549	5.442675
4.473409	275.933732	5.447680
4.589770	275.627681	5.452685
4.236520	277.619382	5.457690
4.389603	285.612633	5.462694
4.787893	287.211328	5.467699
4.733680	287.998214	5.472704
4.689730	286.065760	5.477709
4.566604	269.130175	5.482714
4.300345	287.443102	5.487718
4.609984	289.555573	5.492723
4.281363	293.137989	5.497728
4.600717	288.263196	5.502733
4.619809	280.179868	5.507738
4.559562	291.531733	5.512742
4.668088	283.510323	5.517747
4.445410	285.247443	5.522752
4.384186	286.753618	5.527757
4.887392	291.351007	5.532762
4.639023	290.402895	5.537766
4.591033	287.752884	5.542771
4.458401	301.631344	5.547776
4.709068	293.603477	5.552781
4.975342	285.471926	5.557786
4.697625	293.659233	5.562790
5.021659	290.153646	5.567795
4.933508	293.809118	5.572800
4.844492	290.181583	5.577805
5.162610	290.356461	5.582810
4.665882	293.740584	5.587814
4.797486	294.273723	5.592819
4.836566	292.125774	5.597824
5.048570	292.127448	5.602829
5.103573	289.458136	5.607834
4.905065	293.485248	5.612838
5.005467	289.056059	5.617843
4.540028	289.505571	5.622848
4.631654	293.616941	5.627853
4.865421	290.426062	5.632858
4.849440	298.635638	5.637862
4.860710	295.682104	5.642867
4.998656	291.256524	5.647872
5.054235	290.653104	5.652877
4.833967	288.855847	5.657882
4.989117	294.861891	5.662886
5.048604	297.598867	5.667891
5.306466	314.228801	5.672896
4.882940	298.434943	5.677901
4.334082	309.534338	5.682906
4.277530	318.003386	5.687910
5.292815	320.543151	5.692915
5.394725	324.039132	5.697920
5.143393	323.224364	5.702925
5.370472	325.042883	5.707930
5.290419	327.947264	5.712934
5.244436	321.070045	5.717939
5.310356	329.393356	5.722944
4.955371	326.484548	5.727949
5.023436	328.157135	5.732954
4.760258	322.927504	5.737958
4.814510	328.196376	5.742963
4.841865	331.906526	5.747968
4.784273	332.371232	5.752973
5.325916	336.475379	5.757978
5.139774	352.671865	5.762982
5.334873	351.942176	5.767987
5.606672	347.350073	5.772992
5.784235	346.721211	5.777997
5.391290	343.995523	5.783002
4.953311	337.154406	5.788006
5.456245	334.573096	5.793011
5.199217	347.294133	5.798016
5.498913	351.059695	5.803021
5.381769	348.335087	5.808026
5.124078	353.156119	5.813030
5.210761	357.499239	5.818035
5.497374	356.748883	5.823040
5.452909	354.345090	5.828045
5.390793	362.141133	5.833050
5.262791	360.535061	5.838054
5.241946	346.076487	5.843059
5.472694	369.737616	5.848064
5.263447	355.337029	5.853069
5.654163	352.776463	5.858074
5.571737	355.921672	5.863078
5.489714	351.824780	5.868083
5.553449	367.950490	5.873088
5.060225	351.237336	5.878093
5.518510	343.553414	5.883098
5.163124	363.759706	5.888102
5.470106	359.817003	5.893107
5.574752	373.718454	5.898112
5.594347	380.289948	5.903117
5.927625	377.608660	5.908122
5.678643	378.742452	5.913126
5.889430	369.594470	5.918131
5.643455	359.777720	5.923136
5.371539	357.219734	5.928141
5.547987	368.689590	5.933146
5.553768	379.502803	5.938150
5.853539	370.030822	5.943155
5.443049	379.010949	5.948160
5.547347	379.447127	5.953165
6.009401	383.108161	5.958170
5.559074	388.085938	5.963174
5.649229	386.986701	5.968179
5.613821	388.567935	5.973184
5.610439	372.008972	5.978189
5.923177	382.087537	5.983194
5.752088	386.629245	5.988198
6.052398	377.796273	5.993203
5.704543	382.938333	5.998208
5.588710	382.956571	6.003213
5.758503	386.065431	6.008218
5.717140	384.537534	6.013222
5.802882	382.179776	6.018227
5.677970	382.977744	6.023232
5.533896	380.475656	6.028237
5.649735	386.794784	6.033242
5.608646	405.958429	6.038246
5.822880	399.568772	6.043251
6.110770	409.568986	6.048256
6.029575	413.685315	6.053261
6.038689	407.321466	6.058266
5.986933	414.350256	6.063270
5.970194	395.325558	6.068275
5.794895	391.338187	6.073280
5.923978	378.036212	6.078285
5.595388	386.484640	6.083290
5.906911	402.426021	6.088294
6.083943	401.142322	6.093299
5.885590	400.138910	6.098304
5.820228	390.183110	6.103309
5.906869	387.958093	6.108314
5.415833	388.965291	6.113318
6.226224	390.660783	6.118323
5.919691	395.973548	6.123328
5.762017	384.627464	6.128333
6.173134	384.819410	6.133338
6.196005	387.628577	6.138342
5.886975	385.921150	6.143347
5.853332	387.619170	6.148352
5.978306	390.042169	6.153357
5.855441	385.458108	6.158362
5.740638	390.924334	6.163366
5.755455	378.946932	6.168371
5.775055	396.449530	6.173376
5.758198	382.597762	6.178381
6.036964	381.238012	6.183386
6.181128	386.688971	6.188390
5.696779	388.910039	6.193395
5.673485	384.927328	6.198400
5.705794	384.523710	6.203405
6.047056	385.612478	6.208410
5.691801	390.322252	6.213414
5.913941	381.637572	6.218419
6.088616	393.006478	6.223424
5.933444	388.671094	6.228429
5.827294	390.775956	6.233434
5.789700	395.227146	6.238438
6.111282	387.833552	6.243443
5.967346	394.924235	6.248448
5.928545	384.837721	6.253453
5.848428	394.737395	6.258458
5.854188	393.578612	6.263462
5.946091	381.475232	6.268467
5.821976	391.619086	6.273472
5.314700	392.065663	6.278477
5.853924	384.274127	6.283482
5.799998	385.130576	6.288486
5.618082	382.792610	6.293491
5.430801	392.041500	6.298496
5.626589	394.867869	6.303501
5.955248	405.931075	6.308506
5.660897	414.557654	6.313510
5.991584	405.688270	6.318515
6.184963	414.190973	6.323520
6.043191	405.797425	6.328525
6.354772	391.802437	6.333530
5.568341	394.232193	6.338534
5.701277	381.590857	6.343539
5.787718	388.563181	6.348544
5.984134	388.203455	6.353549
5.859619	380.696256	6.358554
5.926616	384.719755	6.363558
6.050794	386.804347	6.368563
5.778518	390.972757	6.373568
5.664576	385.276787	6.378573
5.819970	379.209577	6.383578
5.706556	385.115358	6.388582
6.055715	384.358366	6.393587
5.769623	390.411431	6.398592
5.866318	377.949787	6.403597
5.929333	380.496392	6.408602
5.621900	392.545131	6.413606
6.128260	396.417532	6.418611
5.422423	394.497021	6.423616
6.150261	400.815180	6.428621
6.302453	402.654932	6.433626
5.782599	402.081556	6.438630
5.729931	392.481281	6.443635
5.802161	385.180543	6.448640
5.738954	396.232372	6.453645
5.921874	394.542779	6.458650
5.762867	396.589482	6.463654
5.828183	387.885076	6.468659
5.892702	393.861061	6.473664
5.844571	391.492639	6.478669
6.376449	384.236945	6.483674
6.081246	391.563305	6.488678
6.037593	393.756455	6.493683
6.226011	383.431855	6.498688
6.056520	377.054871	6.503693
6.157918	389.514129	6.508698
5.920974	393.173951	6.513702
5.886726	391.790476	6.518707
5.939110	390.497834	6.523712
6.018258	385.882121	6.528717
5.837980	386.274299	6.533722
5.637670	391.329966	6.538726
6.046500	383.223493	6.543731
5.978395	379.611646	6.548736
5.802633	380.841537	6.553741
5.649042	384.070669	6.558746
5.724594	384.501860	6.563750
6.157543	382.652866	6.568755
5.828528	383.153772	6.573760
5.636356	388.239803	6.578765
6.063702	378.716189	6.583770
5.691617	385.118094	6.588774
5.742536	382.034944	6.593779
5.911177	386.162743	6.598784
5.976240	379.037143	6.603789
5.938424	380.283385	6.608794
5.485248	387.526925	6.613798
5.860663	383.817110	6.618803
5.699326	380.226199	6.623808
5.670641	383.163670	6.628813
5.924688	375.673092	6.633818
5.952290	387.042891	6.638822
5.936703	381.590947	6.643827
5.883635	382.662404	6.648832
5.680118	387.266142	6.653837
5.859314	381.011700	6.658842
5.962640	380.388140	6.663846
6.304968	387.070427	6.668851
5.955377	387.960547	6.673856
5.820058	391.335519	6.678861
5.828865	392.663045	6.683866
5.663893	382.396980	6.688870
5.507899	387.429884	6.693875
5.520106	387.538795	6.698880
5.289600	386.262003	6.703885
6.062712	387.422317	6.708890
5.957520	390.615393	6.713894
5.991450	388.898523	6.718899
5.748175	386.557514	6.723904
5.702350	385.156870	6.728909
5.908151	382.331035	6.733914
5.885622	386.472968	6.738918
6.048709	386.260837	6.743923
6.074676	396.824118	6.748928
5.746991	395.954869	6.753933
5.761124	389.849676	6.758938
5.652008	389.733979	6.763942
6.269621	384.363162	6.768947
5.933513	384.675349	6.773952
5.800247	385.446151	6.778957
5.776484	386.478214	6.783962
5.713758	385.194117	6.788966
6.253247	383.097469	6.793971
6.148410	394.592431	6.798976
6.130559	388.520725	6.803981
6.267840	384.566639	6.808986
5.782755	383.968833	6.813990
5.825816	380.295274	6.818995
6.085885	387.366947	6.824000
5.949737	388.536846	6.829005
6.281211	391.395740	6.834010
5.842797	382.415912	6.839014
6.142699	366.461187	6.844019
5.639054	367.369117	6.849024
5.739281	358.140385	6.854029
5.931179	362.308828	6.859034
5.788604	365.605836	6.864038
5.991225	369.785257	6.869043
5.820531	363.883044	6.874048
5.960485	372.175792	6.879053
5.759562	356.574802	6.884058
5.687610	367.950696	6.889062
6.173266	370.965769	6.894067
5.677902	367.325953	6.899072
5.832513	364.970063	6.904077
6.146661	368.581500	6.909082
5.511394	363.261457	6.914086
6.074222	363.831440	6.919091
5.869019	364.727411	6.924096
5.586417	357.365218	6.929101
6.027230	361.456694	6.934106
5.824051	373.109424	6.939110
5.859372	366.251088	6.944115
5.559105	376.413042	6.949120
5.786140	375.744788	6.954125
6.194570	374.446983	6.959130
5.973457	382.274274	6.964134
6.047031	365.848796	6.969139
6.048957	357.125863	6.974144
5.905876	356.284640	6.979149
5.935500	354.600087	6.984154
5.731204	360.118291	6.989158
6.073036	352.129900	6.994163
5.827166	351.545236	6.999168
5.875504	357.270636	7.004173
5.842499	348.252615	7.009178
5.921701	364.983357	7.014182
5.852397	362.051929	7.019187
5.774026	353.439657	7.024192
5.738734	351.784258	7.029197
5.778121	354.173206	7.034202
5.749361	357.689668	7.039206
5.318546	352.609684	7.044211
5.730737	372.322386	7.049216
5.874604	380.513281	7.054221
6.136870	380.614651	7.059226
5.725087	388.101649	7.064230
6.154729	386.645491	7.069235
6.107478	375.437140	7.074240
5.951782	358.848269	7.079245
5.782966	359.488594	7.084250
5.891505	350.369298	7.089254
5.834565	352.748028	7.094259
5.958457	365.488490	7.099264
5.945928	363.576415	7.104269
6.012407	360.269362	7.109274
5.616162	366.073915	7.114278
5.837221	349.897434	7.119283
5.571701	355.785908	7.124288
5.990000	366.287698	7.129293
5.644311	357.872338	7.134298
5.793852	375.740545	7.139302
6.119379	370.754028	7.144307
5.972296	359.251272	7.149312
5.984124	358.401598	7.154317
5.874494	356.738863	7.159322
5.624898	364.035919	7.164326
5.869717	356.765100	7.169331
5.708904	358.777280	7.174336
5.603020	368.934084	7.179341
6.198195	372.821038	7.184346
5.951211	376.824126	7.189350
5.890871	358.325169	7.194355
5.839895	362.291215	7.199360
5.877478	354.986426	7.204365
6.262342	353.619546	7.209370
6.045933	364.698524	7.214374
6.004628	367.343732	7.219379
6.158405	358.074971	7.224384
5.681254	358.988241	7.229389
6.225086	354.856564	7.234394
6.071400	365.141081	7.239398
6.143597	358.121941	7.244403
5.831538	355.177928	7.249408
6.183205	356.483370	7.254413
6.001307	359.258176	7.259418
5.963661	365.528577	7.264422
5.910488	360.585579	7.269427
5.882927	365.996998	7.274432
5.902922	361.684797	7.279437
6.060219	351.811193	7.284442
5.681986	354.847722	7.289446
6.104611	344.682606	7.294451
5.935448	344.943324	7.299456
5.756036	339.956835	7.304461
5.967168	328.401138	7.309466
5.545728	330.745223	7.314470
5.897285	342.782428	7.319475
6.051847	355.328247	7.324480
6.079097	342.728808	7.329485
6.008867	337.788490	7.334490
5.653876	338.752222	7.339494
5.810950	335.975159	7.344499
5.538761	326.883890	7.349504
5.555453	343.981921	7.354509
5.695280	354.030613	7.359514
6.008907	370.484178	7.364518
5.962515	362.063050	7.369523
5.994028	357.027689	7.374528
6.108250	357.569882	7.379533
6.101562	350.199263	7.384538
5.172578	349.601405	7.389542
5.803473	351.132022	7.394547
5.794616	363.330119	7.399552
5.879617	371.036673	7.404557
6.004835	359.026168	7.409562
5.769396	356.032184	7.414566
5.968764	359.851434	7.419571
5.923566	368.138388	7.424576
5.921972	364.522451	7.429581
6.153602	354.880815	7.434586
5.689941	356.276038	7.439590
5.941711	352.481197	7.444595
5.837818	363.805144	7.449600
5.704735	360.991279	7.454605
5.721782	358.283610	7.459610
5.884664	368.135703	7.464614
6.114829	364.426504	7.469619
5.989582	360.744519	7.474624
5.860399	350.131169	7.479629
5.793186	343.662240	7.484634
5.790775	363.778424	7.489638
5.704036	367.398888	7.494643
5.886429	363.115026	7.499648
5.959021	366.248604	7.504653
6.195918	361.304451	7.509658
5.608925	356.840576	7.514662
5.608684	351.807027	7.519667
5.411355	355.837133	7.524672
5.497888	362.410788	7.529677
6.013346	354.952028	7.534682
5.938178	357.741749	7.539686
6.215743	361.143775	7.544691
5.916644	358.884285	7.549696
5.933857	357.132071	7.554701
6.246114	364.312620	7.559706
5.495799	358.877723	7.564710
5.927863	360.942546	7.569715
6.099667	371.615843	7.574720
5.899249	362.728452	7.579725
6.181729	367.243383	7.584730
5.652988	351.832970	7.589734
5.646063	346.006345	7.594739
5.700140	350.553895	7.599744
5.611962	364.131200	7.604749
5.811434	364.093707	7.609754
5.380045	365.097886	7.614758
5.905658	360.497649	7.619763
5.759142	363.738325	7.624768
5.571707	370.721916	7.629773
6.028665	366.553226	7.634778
6.062705	363.330351	7.639782
5.962622	365.102055	7.644787
5.846513	363.525758	7.649792
5.790012	369.745330	7.654797
5.856289	362.334799	7.659802
5.981066	358.072621	7.664806
5.967291	357.581309	7.669811
5.987556	360.023875	7.674816
6.155553	357.928487	7.679821
6.345689	359.616752	7.684826
5.881653	354.681183	7.689830
5.888434	340.537833	7.694835
5.550684	342.849825	7.699840
5.969286	350.383875	7.704845
6.400247	349.294518	7.709850
5.967352	349.229553	7.714854
5.957679	343.321100	7.719859
5.401334	332.701922	7.724864
5.712410	339.237223	7.729869
5.501293	337.160108	7.734874
5.893579	354.629582	7.739878
6.199812	356.049713	7.744883
5.749583	356.971420	7.749888
5.685274	357.782037	7.754893
5.760578	365.357228	7.759898
5.819105	362.507013	7.764902
5.911823	362.717208	7.769907
5.948528	373.044667	7.774912
5.701587	368.593949	7.779917
6.274481	363.407320	7.784922
6.062133	370.227130	7.789926
6.067215	350.256234	7.794931
5.945401	342.710663	7.799936
5.421868	342.631424	7.804941
5.412075	342.329319	7.809946
5.516857	361.963621	7.814950
5.968190	362.608023	7.819955
6.286764	368.094927	7.824960
6.088557	358.216908	7.829965
6.153404	347.231464	7.834970
5.731636	341.650179	7.839974
5.522661	338.291373	7.844979
5.364714	353.452030	7.849984
5.942121	361.764820	7.854989
6.304197	351.264328	7.859994
6.313126	362.646530	7.864998
5.769678	345.112323	7.870003
5.746773	340.136114	7.875008
5.689610	345.106063	7.880013
5.924414	343.920887	7.885018
5.747800	350.716108	7.890022
5.706308	354.164959	7.895027
5.773567	359.596322	7.900032
5.675897	360.832958	7.905037
5.960685	363.518824	7.910042
5.651590	362.801692	7.915046
5.774213	364.133530	7.920051
5.749923	359.568833	7.925056
5.556121	358.476123	7.930061
5.963812	363.373242	7.935066
5.883064	364.237057	7.940070
6.010125	362.486615	7.945075
5.670749	366.118187	7.950080
5.733014	365.016994	7.955085
5.857074	366.263183	7.960090
5.486347	363.515028	7.965094
5.879181	364.870969	7.970099
5.860689	361.368415	7.975104
5.801248	372.182351	7.980109
6.029283	360.073475	7.985114
5.874110	361.749404	7.990118
5.986773	368.234932	7.995136
6.002810	362.337521	8.000154
5.538142	365.976441	8.005171
5.690026	363.803650	8.010189
5.895769	369.259395	8.015206
5.863857	366.812447	8.020224
6.132797	350.306728	8.025242
5.415281	361.874696	8.030259
5.825395	353.419326	8.035277
5.729520	361.197639	8.040294
5.777546	364.939264	8.045312
6.081170	364.023942	8.050330
5.968751	368.295630	8.055347
5.883481	356.790504	8.060365
5.952639	359.140276	8.065382
5.759975	363.402445	8.070400
5.772878	360.134286	8.075418
5.798299	366.927930	8.080435
5.902567	374.387715	8.085453
5.916021	384.569389	8.090470
5.844272	386.682468	8.095488
5.770527	386.151318	8.100506
6.334673	396.413971	8.105523
6.301056	386.033658	8.110541
5.902303	385.171582	8.115558
5.814161	383.475050	8.120576
6.191981	376.479543	8.125594
5.741302	384.452312	8.130611
5.931577	387.887633	8.135629
5.859049	395.839027	8.140646
5.807640	396.219553	8.145664
6.174358	396.660797	8.150682
6.205388	389.025349	8.155699
5.841288	393.756196	8.160717
5.874715	401.230247	8.165734
5.637435	401.418991	8.170752
6.214791	395.960636	8.175770
5.924282	403.523313	8.180787
6.184432	396.467340	8.185805
5.738328	392.936582	8.190822
5.664391	399.853102	8.195840
5.992672	388.784928	8.200858
5.716013	393.688265	8.205875
6.066135	394.151044	8.210893
6.055956	400.025635	8.215910
5.889950	392.487330	8.220928
6.340464	392.899665	8.225946
6.165912	391.753154	8.230963
6.044591	394.353680	8.235981
6.223430	395.196743	8.240998
6.005569	392.712655	8.246016
6.286851	396.250483	8.251034
5.930486	391.932498	8.256051
5.995532	387.526395	8.261069
6.291076	399.349065	8.266086
6.225011	396.512991	8.271104
6.333415	395.271652	8.276122
6.005368	396.591765	8.281139
6.506934	394.196924	8.286157
6.332928	396.881444	8.291174
6.562450	399.720487	8.296192
6.525023	389.684749	8.301210
6.263361	401.613660	8.306227
6.241572	391.117882	8.311245
6.064136	390.817572	8.316262
5.819028	394.892307	8.321280
6.345714	392.761773	8.326298
5.857004	393.763078	8.331315
6.192132	393.398236	8.336333
6.065820	391.429975	8.341350
6.161233	394.772864	8.346368
6.116272	390.601746	8.351386
5.964839	395.861000	8.356403
6.293241	394.610438	8.361421
5.915800	393.069686	8.366438
6.006555	398.663376	8.371456
6.373163	402.108941	8.376474
6.102353	406.440169	8.381491
6.060000	406.898171	8.386509
6.342598	419.574943	8.391526
5.975746	427.241109	8.396544
6.392939	423.461472	8.401562
6.396590	424.360388	8.406579
6.608377	417.087924	8.411597
6.589921	415.762320	8.416614
6.321215	404.115493	8.421632
6.050780	390.364039	8.426650
6.159257	396.895374	8.431667
6.393980	409.661691	8.436685
6.148252	422.894613	8.441702
5.794541	418.405794	8.446720
6.217990	419.447216	8.451738
6.239218	423.069975	8.456755
6.109631	420.161800	8.461773
6.039321	416.613182	8.466790
6.448923	422.238972	8.471808
6.293588	413.045355	8.476826
6.326601	429.264159	8.481843
6.362140	423.524618	8.486861
6.256785	430.146274	8.491878
6.138358	428.886825	8.496896
6.491974	427.925798	8.501914
6.336981	424.254747	8.506931
6.579075	418.214603	8.511949
6.312926	422.639777	8.516966
6.271604	427.455757	8.521984
6.614453	419.569470	8.527002
6.089911	420.115646	8.532019
6.420092	426.650125	8.537037
6.339853	427.338124	8.542054
6.408316	435.788149	8.547072
6.754737	435.522523	8.552090
6.257521	426.357219	8.557107
6.736864	415.123350	8.562125
6.447412	418.861058	8.567143
6.084477	419.763764	8.572160
6.721203	431.886445	8.577178
6.277403	437.655421	8.582195
6.747473	433.198470	8.587213
6.498488	423.410454	8.592231
6.289403	426.700074	8.597248
6.449878	435.167240	8.602266
6.221688	445.210086	8.607283
6.712353	451.350201	8.612301
6.685169	448.435444	8.617319
6.524073	446.911282	8.622336
6.644801	445.633295	8.627354
6.768223	450.524455	8.632371
6.526250	423.075550	8.637389
6.548156	426.625621	8.642407
6.606169	420.879404	8.647424
6.704301	419.210486	8.652442
6.410985	423.614672	8.657459
6.842696	420.975154	8.662477
6.460215	421.379152	8.667495
6.400719	423.594457	8.672512
6.708112	425.414608	8.677530
6.458462	437.288011	8.682547
6.526980	435.140897	8.687565
6.685591	429.574574	8.692583
6.772124	440.189795	8.697600
6.809624	431.600268	8.702618
6.287989	427.188249	8.707635
6.317609	439.705859	8.712653
6.612892	442.420996	8.717671
6.609987	461.782312	8.722688
6.797324	453.118805	8.727706
6.587388	457.683503	8.732723
6.869158	461.315940	8.737741
7.012197	448.799843	8.742759
6.692480	449.294993	8.747776
6.700109	429.182052	8.752794
6.435859	425.316682	8.757811
6.676871	434.708498	8.762829
6.481260	435.016945	8.767847
6.496654	441.319885	8.772864
6.698476	448.199530	8.777882
6.974521	449.800533	8.782899
6.515212	456.840573	8.787917
6.571878	459.993886	8.792935
6.770204	474.293355	8.797952
7.153275	457.226859	8.802970
7.022880	458.714822	8.807987
6.754319	451.271455	8.813005
6.810700	429.528799	8.818023
6.325249	430.646360	8.823040
6.698675	436.719633	8.828058
6.874333	456.977611	8.833075
6.655343	454.184424	8.838093
7.054666	456.400427	8.843111
6.834289	460.660650	8.848128
6.726427	453.463501	8.853146
6.895723	457.555371	8.858163
6.502978	452.807572	8.863181
7.029397	452.497964	8.868199
7.161396	456.712442	8.873216
6.986144	439.629301	8.878234
6.661561	440.866823	8.883251
6.561765	439.153177	8.888269
6.893079	444.706034	8.893287
6.767455	450.134829	8.898304
6.930213	452.110187	8.903322
6.842227	456.949266	8.908339
6.682329	454.528671	8.913357
6.956281	446.618453	8.918375
6.833139	456.714273	8.923392
7.102368	448.407165	8.928410
6.863139	453.989460	8.933427
6.919536	454.899048	8.938445
7.222356	457.736083	8.943463
6.918697	452.005498	8.948480
7.077226	441.039628	8.953498
6.962212	431.240084	8.958515
6.912711	432.084213	8.963533
6.896924	428.202003	8.968551
6.908134	434.742281	8.973568
6.735527	430.774189	8.978586
7.165417	443.118633	8.983603
7.448656	445.955578	8.988621
7.077837	427.527167	8.993639
6.882243	430.798895	8.998656
6.791253	427.736349	9.003674
6.681748	428.318481	9.008691
6.756236	435.846073	9.013709
7.101758	452.789102	9.018727
7.225005	451.823144	9.023744
6.879315	437.493312	9.028762
6.639042	443.880493	9.033779
6.545755	452.261196	9.038797
7.100519	447.263955	9.043815
7.055361	454.829236	9.048832
6.932570	452.238726	9.053850
7.337387	446.892596	9.058867
7.127530	458.573587	9.063885
6.969691	451.390581	9.068903
7.019137	458.070043	9.073920
6.999135	460.692573	9.078938
7.206195	449.394048	9.083955
6.881689	461.389648	9.088973
7.181201	453.936168	9.093991
7.021023	462.346291	9.099008
6.702865	459.294087	9.104026
6.931106	461.486404	9.109043
6.831971	449.033497	9.114061
6.833084	451.583290	9.119079
6.746261	449.387930	9.124096
6.747509	449.744428	9.129114
7.172305	465.643105	9.134131
6.871838	481.993103	9.139149
7.187560	491.767717	9.144167
7.245161	493.693285	9.149184
7.227996	482.937954	9.154202
7.416005	484.915671	9.159219
6.838804	482.491029	9.164237
7.319070	475.621443	9.169255
7.207715	483.541089	9.174272
7.095006	484.325696	9.179290
7.332427	489.987954	9.184307
7.165229	488.897088	9.189325
7.467150	483.686989	9.194343
7.370200	489.335365	9.199360
7.044920	484.261407	9.204378
6.912998	476.818711	9.209395
7.181698	485.833831	9.214413
7.352837	479.179936	9.219431
7.227287	478.041520	9.224448
7.104012	486.688869	9.229466
7.115053	475.162265	9.234483
6.976594	485.288903	9.239501
7.053434	475.913709	9.244519
7.095363	489.066895	9.249536
6.796295	482.502451	9.254554
6.754414	485.440836	9.259571
6.717537	493.351974	9.264589
7.602787	501.276423	9.269607
7.134381	508.532502	9.274624
7.346187	512.993265	9.279642
7.528121	512.570373	9.284659
7.473060	519.610214	9.289677
7.606370	509.648643	9.294695
7.336092	508.419293	9.299712
7.161359	512.341017	9.304730
7.286234	507.477387	9.309747
7.376871	516.520423	9.314765
7.510042	499.559313	9.319783
7.349163	515.149013	9.324800
7.817959	508.107643	9.329818
7.633918	493.623051	9.334835
7.334620	497.788350	9.339853
7.248138	492.557054	9.344871
7.217312	487.080355	9.349888
7.372267	496.959056	9.354906
7.739988	498.823411	9.359923
7.376670	506.053556	9.364941
7.329646	485.892311	9.369959
7.540667	492.350810	9.374976
7.242696	494.291064	9.379994
7.606531	499.434902	9.385011
7.406938	504.496607	9.390029
7.318187	501.664071	9.395047
6.996746	512.879744	9.400064
7.301228	502.976563	9.405082
7.652372	511.887261	9.410099
7.400426	517.222260	9.415117
7.641922	515.161642	9.420135
7.980990	508.636058	9.425152
7.940997	520.423019	9.430170
7.881609	495.886602	9.435187
7.056681	490.502766	9.440205
7.481198	493.478529	9.445223
7.760774	510.917938	9.450240
7.561460	494.021552	9.455258
7.460325	484.926702	9.460275
7.361809	490.922461	9.465293
7.636317	496.670428	9.470311
7.287105	504.791453	9.475328
7.657262	505.636104	9.480346
8.137200	508.199244	9.485363
7.714720	505.349569	9.490381
7.497177	492.811044	9.495399
7.140691	490.654775	9.500416
7.516149	518.133539	9.505434
7.692967	510.181708	9.510451
7.325957	514.092534	9.515469
7.454619	507.221222	9.520487
7.394485	514.564813	9.525504
7.217363	516.842740	9.530522
7.594846	507.101688	9.535539
7.880098	512.548176	9.540557
7.984854	509.830486	9.545575
7.634590	519.627413	9.550592
7.399644	513.646202	9.555610
7.689137	507.614379	9.560627
7.487576	516.611679	9.565645
7.602322	518.739734	9.570663
7.458515	515.164742	9.575680
7.480262	514.754325	9.580698
7.906338	506.053386	9.585715
7.522240	516.963299	9.590733
7.570041	520.941676	9.595751
7.572450	527.963049	9.600768
7.783781	535.728018	9.605786
7.843802	530.031944	9.610803
8.039851	534.763423	9.615821
7.679299	539.026693	9.620839
7.777520	536.325803	9.625856
7.946689	535.538837	9.630874
8.115035	536.399330	9.635891
7.793630	533.202455	9.640909
7.805543	511.586588	9.645927
7.728644	513.511141	9.650944
7.867732	520.668886	9.655962
7.787214	526.620811	9.660979
7.901539	525.952892	9.665997
7.957053	516.003507	9.671015
7.817392	518.259786	9.676032
7.818019	517.502384	9.681050
7.673202	515.306636	9.686067
7.895829	527.872961	9.691085
7.732287	531.666704	9.696103
8.035734	532.395576	9.701120
7.815022	550.377314	9.706138
7.799642	539.687941	9.711155
7.770763	545.941051	9.716173
7.930063	539.639283	9.721191
7.826858	540.460273	9.726208
7.604590	535.445899	9.731226
7.782444	536.977089	9.736243
7.876375	540.288680	9.741261
7.625847	543.856213	9.746279
7.970503	533.858359	9.751296
8.221288	538.259371	9.756314
7.887205	537.948888	9.761331
7.896086	543.369260	9.766349
8.101363	538.846474	9.771367
7.947224	536.674274	9.776384
8.159044	534.476293	9.781402
8.042218	542.851259	9.786419
8.102067	540.708646	9.791437
7.885191	548.449195	9.796455
7.857852	534.501750	9.801472
7.606005	543.491164	9.806490
8.005988	537.543005	9.811507
7.966911	539.366961	9.816525
7.944451	543.908617	9.821543
8.024030	549.387341	9.826560
8.121414	544.723669	9.831578
8.493927	544.924168	9.836595
8.121682	547.321034	9.841613
8.088811	547.004381	9.846631
8.455552	534.995973	9.851648
8.091568	542.055824	9.856666
8.307597	542.994053	9.861683
8.313342	549.121818	9.866701
7.860614	539.996823	9.871719
8.132368	540.124746	9.876736
8.106289	543.773877	9.881754
7.926888	534.344127	9.886771
8.149775	538.260362	9.891789
7.975150	541.749730	9.896807
7.885951	526.328756	9.901824
7.809996	544.770645	9.906842
8.021119	556.805462	9.911859
8.512560	571.459870	9.916877
8.339169	563.708055	9.921895
8.611646	566.243748	9.926912
8.141120	546.275022	9.931930
8.214946	537.793361	9.936947
8.035677	540.298846	9.941965
7.605295	562.668460	9.946983
8.295785	561.648332	9.952000
8.218352	575.555587	9.957018
8.390876	567.629650	9.962035
8.565221	582.172804	9.967053
8.287584	569.122932	9.972071
8.441770	571.980118	9.977088
8.070556	571.457701	9.982106
8.423693	565.898726	9.987123
8.356463	564.962606	9.992141
8.408871	566.576570	9.997159
8.576549	568.557483	10.002176
8.278863	568.212894	10.007194
8.115601	565.240544	10.012211
8.804029	569.203763	10.017229
8.376846	556.710663	10.022247
8.176394	544.014789	10.027264
7.904958	560.294037	10.032282
8.384731	563.188571	10.037299
8.241568	572.448148	10.042317
8.431271	573.608255	10.047335
8.474508	564.244591	10.052352
8.526580	579.583231	10.057370
8.438504	573.045655	10.062387
8.572655	577.237733	10.067405
8.413488	576.132980	10.072423
8.616378	567.826744	10.077440
8.322051	570.179846	10.082458
8.468170	569.910888	10.087475
8.330241	575.338493	10.092493
8.414633	578.894583	10.097511
8.676682	576.177485	10.102528
8.546028	583.961344	10.107546
8.820840	578.831205	10.112563
8.748948	565.603930	10.117581
8.312377	560.973423	10.122599
8.371293	554.062527	10.127616
8.544929	568.312291	10.132634
8.477772	574.079102	10.137651
8.272921	577.671044	10.142669
8.131260	585.210474	10.147687
8.528884	571.786554	10.152704
8.412542	578.122807	10.157722
8.184968	577.085577	10.162739
8.194388	570.510635	10.167757
8.489741	573.304677	10.172775
8.492443	576.744178	10.177792
8.457326	582.203013	10.182810
8.749247	577.310035	10.187827
8.465873	579.585684	10.192845
8.342160	577.979913	10.197863
8.772532	579.096000	10.202880
8.489832	579.809416	10.207898
8.610399	585.490012	10.212915
8.916820	590.759637	10.217933
8.701520	587.643958	10.222951
8.684212	580.811267	10.227968
8.341239	591.430758	10.232986
8.696153	597.727894	10.238003
8.891755	601.001475	10.243021
8.607632	606.912745	10.248039
8.857814	602.464959	10.253056
8.783536	608.990292	10.258074
8.730892	595.362347	10.263091
9.010558	590.796335	10.268109
8.880971	595.373725	10.273127
8.759176	575.807919	10.278144
8.500284	576.842653	10.283162
8.386062	583.005005	10.288179
8.597103	586.430800	10.293197
8.112564	599.196339	10.298215
8.511050	599.026694	10.303232
8.661575	605.141262	10.308250
8.412214	602.308628	10.313267
8.743912	595.115135	10.318285
8.863696	597.012036	10.323303
8.675669	600.983200	10.328320
8.342972	612.235412	10.333338
8.690862	618.883952	10.338355
8.757499	617.718570	10.343373
8.872993	624.343564	10.348391
8.950108	613.137879	10.353408
8.928475	622.659309	10.358426
9.183806	619.469884	10.363443
9.095620	622.567026	10.368461
8.850134	613.693545	10.373479
8.991863	610.436715	10.378496
8.792198	609.647575	10.383514
8.848047	616.789998	10.388531
8.874198	621.267253	10.393549
9.019156	622.465932	10.398567
8.969511	623.382676	10.403584
8.952079	629.211142	10.408602
9.084984	633.971477	10.413619
9.118962	619.155976	10.418637
8.682177	612.597282	10.423655
8.927229	616.910850	10.428672
9.039520	618.386047	10.433690
8.999077	621.014959	10.438707
9.144258	620.055023	10.443725
8.969796	626.854837	10.448743
9.092187	622.468094	10.453760
9.001577	626.348260	10.458778
9.075731	627.696890	10.463795
9.326639	624.366145	10.468813
9.007281	616.214297	10.473831
9.075905	615.783910	10.478848
9.347481	624.618769	10.483866
9.155838	620.410619	10.488883
9.054589	605.335449	10.493901
8.780487	610.894854	10.498919
9.083360	611.276680	10.503936
9.221677	620.192376	10.508954
8.989444	623.119583	10.513971
9.264505	624.982690	10.518989
9.120225	639.686268	10.524007
9.199596	624.396588	10.529024
9.271109	626.319991	10.534042
9.008983	622.050300	10.539059
9.281873	616.699544	10.544077
9.107422	636.103705	10.549095
9.274846	619.976564	10.554112
9.639534	621.494267	10.559130
9.006513	615.348173	10.564147
9.247017	620.198943	10.569165
9.359443	625.685167	10.574183
8.917661	610.284651	10.579200
9.104429	622.452716	10.584218
9.012936	621.678186	10.589235
9.208974	629.859004	10.594253
9.038625	628.219511	10.599271
9.168140	621.354333	10.604288
9.156007	618.509774	10.609306
9.117448	623.792435	10.614323
9.311202	626.697080	10.619341
9.135978	623.464661	10.624359
8.805112	624.848347	10.629376
8.797177	628.374731	10.634394
9.124775	638.586224	10.639411
9.726880	638.646609	10.644429
9.082774	649.963417	10.649447
9.153830	648.734224	10.654464
9.217462	648.658071	10.659482
9.423601	645.410077	10.664499
9.481654	647.932041	10.669517
9.638658	652.859020	10.674535
9.433695	654.961445	10.679552
9.747191	649.935678	10.684570
9.881276	645.701733	10.689587
9.593544	631.438404	10.694605
9.437066	628.805809	10.699623
9.354772	622.901629	10.704640
9.273344	620.613884	10.709658
9.432198	631.044317	10.714675
9.590135	632.607039	10.719693
9.605491	634.277307	10.724711
9.196739	631.999821	10.729728
9.697236	633.471000	10.734746
9.491832	638.382173	10.739763
9.354191	627.822358	10.744781
9.476011	643.623497	10.749799
9.889078	654.102476	10.754816
10.041476	639.353611	10.759834
9.596282	637.410040	10.764851
9.952296	633.163416	10.769869
9.718511	628.065613	10.774887
9.529023	636.025972	10.779904
9.771687	628.852727	10.784922
9.640689	636.251653	10.789939
9.678865	619.463105	10.794957
9.306010	625.855345	10.799975
9.516286	624.178305	10.804992
10.071637	622.945817	10.810010
9.310120	627.899940	10.815027
9.726997	622.198417	10.820045
9.671989	621.642233	10.825063
9.722002	628.687745	10.830080
9.472413	627.805440	10.835098
9.254013	628.319434	10.840115
9.515581	626.779525	10.845133
9.323431	628.081517	10.850151
9.457646	641.135147	10.855168
9.314842	647.535531	10.860186
9.426323	654.483059	10.865203
9.876605	652.165649	10.870221
9.568853	656.540595	10.875239
9.621929	654.676742	10.880256
9.663462	662.417878	10.885274
9.653910	655.053765	10.890291
9.901639	652.304185	10.895309
9.528281	650.071644	10.900327
9.653276	652.034007	10.905344
9.942652	646.241999	10.910362
9.559639	662.463083	10.915379
9.963702	652.216011	10.920397
9.800498	658.969892	10.925415
9.653916	649.172019	10.930432
10.016774	649.642278	10.935450
9.783850	652.238236	10.940467
9.787418	658.868156	10.945485
9.844025	653.579679	10.950503
9.721812	666.522027	10.955520
9.759515	667.797475	10.960538
9.871641	682.015941	10.965555
10.018708	676.643856	10.970573
9.957753	678.351332	10.975591
10.034588	679.904674	10.980608
10.105219	678.883831	10.985626
10.036078	685.193791	10.990643
9.825615	680.104943	10.995661
10.231105	678.987452	11.000679
9.856590	680.352735	11.005696
10.300729	679.409070	11.010714
9.772988	684.194035	11.015731
9.649244	674.944840	11.020749
9.744205	679.193576	11.025767
9.679738	672.731160	11.030784
10.222229	680.955549	11.035802
9.588653	685.334215	11.040819
9.930410	679.641288	11.045837
9.957103	680.467178	11.050855
9.737835	682.502419	11.055872
9.710791	680.161964	11.060890
10.099003	680.858626	11.065907
10.026013	682.239782	11.070925
10.115188	684.791590	11.075943
10.174081	692.482680	11.080960
10.427922	684.357757	11.085978
10.312735	693.303741	11.090995
10.004320	691.086266	11.096013
10.263547	692.090320	11.101031
10.614881	686.720940	11.106048
10.073330	680.390077	11.111066
10.100155	694.435725	11.116083
10.079493	689.175123	11.121101
10.308008	678.841932	11.126119
9.816409	686.672922	11.131136
10.087586	688.173724	11.136154
9.640293	700.273930	11.141171
10.225159	702.501919	11.146189
10.349411	711.299943	11.151207
10.388457	718.451351	11.156224
10.356705	717.607495	11.161242
10.139907	717.269164	11.166259
10.268364	703.533865	11.171277
10.453014	706.458884	11.176295
9.889433	715.083811	11.181312
10.283117	710.187477	11.186330
10.241179	712.381131	11.191347
10.566962	707.609046	11.196365
10.625109	712.295907	11.201383
10.332185	712.266153	11.206400
10.567513	713.775730	11.211418
10.086543	712.759259	11.216435
11.080471	708.163357	11.221453
10.725564	711.611577	11.226471
10.607666	703.295578	11.231488
9.977702	684.396260	11.236506
9.779165	700.395968	11.241523
9.773633	704.253353	11.246541
9.849989	703.124313	11.251559
10.685265	715.579000	11.256576
10.404412	713.448723	11.261594
10.258490	717.952964	11.266611
10.086540	712.021775	11.271629
10.240910	712.802416	11.276647
10.264104	730.042366	11.281664
10.455098	732.691837	11.286682
10.636813	743.626844	11.291699
10.111930	736.274013	11.296717
10.304340	732.665233	11.301735
10.316787	742.294996	11.306752
10.675668	744.302775	11.311770
11.035625	742.233039	11.316787
10.559546	736.570403	11.321805
11.103693	732.284811	11.326823
10.718692	741.778030	11.331840
10.776539	739.575746	11.336858
10.841417	737.650075	11.341875
10.867465	728.210123	11.346893
10.600522	717.733630	11.351911
10.571962	712.859271	11.356928
10.520263	707.398398	11.361946
10.616318	723.156307	11.366963
10.926949	724.291165	11.371981
10.778906	719.126253	11.376999
11.037458	721.055074	11.382016
10.726416	709.963796	11.387034
10.363813	710.187958	11.392051
10.284199	717.111802	11.397069
10.526597	724.382831	11.402087
10.792588	734.761824	11.407104
10.813544	735.932602	11.412122
10.859594	735.496282	11.417139
10.666648	738.385793	11.422157
10.596035	740.148438	11.427175
10.628081	740.970336	11.432192
10.690835	734.945561	11.437210
11.156764	744.996584	11.442227
10.834050	744.195160	11.447245
11.125291	731.037101	11.452263
10.717945	746.700333	11.457280
10.675405	737.258500	11.462298
10.757816	733.436578	11.467315
10.867687	739.967821	11.472333
10.868468	740.185540	11.477351
10.493227	737.650322	11.482368
10.711084	743.713362	11.487386
11.107859	749.117201	11.492403
11.031511	733.886541	11.497421
11.103692	734.689527	11.502439
10.625793	733.091900	11.507456
10.869338	730.794249	11.512474
10.833784	727.069708	11.517491
10.989854	740.501843	11.522509
10.999273	733.715400	11.527527
10.823176	732.013681	11.532544
10.843880	730.050750	11.537562
11.047365	726.765287	11.542579
10.979881	733.611497	11.547597
11.100816	733.636820	11.552615
11.248385	739.032365	11.557632
11.213598	733.130172	11.562650
11.076410	730.008540	11.567667
10.753936	740.498674	11.572685
11.279733	736.746137	11.577703
10.855233	740.063254	11.582720
11.134464	744.292601	11.587738
11.110848	742.585925	11.592755
11.080029	753.573173	11.597773
11.444992	747.270667	11.602791
11.352919	735.668531	11.607808
11.109001	737.780225	11.612826
10.924866	739.096748	11.617843
10.811478	752.577424	11.622861
11.151477	748.052413	11.627879
11.204498	761.494398	11.632896
11.258589	763.594117	11.637914
11.348715	768.739892	11.642931
11.176620	774.441157	11.647949
11.478396	761.401346	11.652967
11.249309	773.012971	11.657984
11.493816	766.009798	11.663002
11.704946	761.773222	11.668019
11.302216	747.442611	11.673037
11.350719	734.395166	11.678055
11.215140	731.052373	11.683072
11.235262	730.254038	11.688090
11.157538	739.389838	11.693107
11.317020	745.783920	11.698125
11.317132	742.419865	11.703143
11.244487	762.584549	11.708160
11.391238	759.557281	11.713178
11.358474	761.380270	11.718195
11.481823	773.056596	11.723213
11.691418	757.979931	11.728231
11.464860	757.043518	11.733248
11.357553	746.803931	11.738266
11.187063	760.637547	11.743283
10.960241	762.367864	11.748301
11.185881	763.351937	11.753319
11.330453	770.890780	11.758336
11.250172	769.088836	11.763354
11.585204	762.087261	11.768371
11.317684	764.319422	11.773389
11.475331	765.181603	11.778407
11.507672	765.198716	11.783424
11.690557	769.941789	11.788442
11.357482	770.385390	11.793459
11.506025	761.421695	11.798477
11.622050	759.497476	11.803495
11.482003	759.525819	11.808512
11.707765	758.553250	11.813530
11.679864	762.635062	11.818547
11.138804	768.798083	11.823565
11.407577	756.707045	11.828583
11.406268	764.101483	11.833600
11.590178	772.574605	11.838618
11.831628	775.538073	11.843635
11.661636	780.241763	11.848653
11.691961	765.458272	11.853671
11.488611	767.326924	11.858688
11.359543	774.072344	11.863706
11.504655	786.310166	11.868723
11.521187	789.267851	11.873741
11.667647	785.966065	11.878759
12.228071	789.794754	11.883776
12.091391	794.644709	11.888794
12.196183	783.942674	11.893811
11.827994	777.783431	11.898829
12.205679	764.873738	11.903847
11.958792	760.721548	11.908864
11.782106	757.625035	11.913882
12.179425	749.745848	11.918899
11.792708	752.823515	11.923917
11.775850	756.218777	11.928935
11.797943	754.902574	11.933952
11.888945	744.174320	11.938970
12.038743	747.893767	11.943987
11.645942	759.073436	11.949005
11.798321	752.709560	11.954023
11.749861	758.744903	11.959040
11.804333	756.659913	11.964058
12.091730	754.831920	11.969075
11.903952	754.659457	11.974093
12.001223	752.151190	11.979111
11.922099	759.163337	11.984128
11.720816	762.246665	11.989146
11.790506	769.958188	11.994163
11.969001	780.486618	11.999181
12.364246	780.181779	12.004199
12.020623	775.609236	12.009216
11.735423	780.671808	12.014234
12.016316	784.146657	12.019251
12.073334	790.238069	12.024269
12.418681	786.362315	12.029287
11.912773	783.210082	12.034304
12.190081	777.804937	12.039322
12.319902	780.606013	12.044339
11.910446	784.432028	12.049357
12.258932	791.399280	12.054375
12.192799	782.702743	12.059392
11.641755	773.735045	12.064410
12.309830	781.617908	12.069427
12.048934	792.215190	12.074445
12.057444	790.030098	12.079463
12.355394	796.844322	12.084480
12.305304	789.660077	12.089498
12.509801	788.634032	12.094515
12.202735	796.978963	12.099533
12.318085	789.557355	12.104551
12.322791	788.774056	12.109568
12.129064	770.753050	12.114586
12.019879	783.103297	12.119603
12.251731	783.221696	12.124621
12.280572	775.684258	12.129639
12.235468	786.137271	12.134656
12.208166	784.311245	12.139674
12.548410	794.066404	12.144691
12.232609	794.201182	12.149709
12.504150	791.343707	12.154727
12.225632	793.097906	12.159744
12.190084	791.285795	12.164762
12.201596	778.603881	12.169779
12.282346	787.307771	12.174797
12.199916	782.956237	12.179815
12.355393	789.657079	12.184832
12.132433	797.786858	12.189850
12.400778	798.110981	12.194867
12.245072	784.300222	12.199885
12.152461	776.769189	12.204903
12.242526	782.252653	12.209920
12.300028	783.310410	12.214938
12.352638	802.496136	12.219955
12.597813	814.920273	12.224973
12.507373	813.747931	12.229991
12.822381	819.830489	12.235008
12.502656	808.551159	12.240026
12.734929	799.912002	12.245043
12.510176	799.426591	12.250061
12.608218	789.599780	12.255079
12.616884	795.020262	12.260096
12.042353	796.214917	12.265114
12.763707	800.908344	12.270131
12.538842	820.765579	12.275149
12.858669	821.277299	12.280167
12.696948	821.422650	12.285184
12.589029	822.679899	12.290202
13.018851	822.773592	12.295219
12.664022	821.992975	12.300237
12.794450	819.514217	12.305255
13.004246	815.167382	12.310272
12.815323	799.092757	12.315290
12.519557	794.679970	12.320307
12.816432	805.571725	12.325325
12.977051	799.635738	12.330343
13.161883	785.080490	12.335360
12.905307	790.031281	12.340378
12.963843	789.662432	12.345395
12.947802	791.852038	12.350413
13.056797	786.012508	12.355431
13.136874	782.796864	12.360448
13.121217	784.645578	12.365466
13.119486	784.324042	12.370483
13.157445	788.086267	12.375501
12.652998	788.641927	12.380519
12.828435	785.171498	12.385536
12.662729	789.861895	12.390554
12.911025	787.269998	12.395571
12.413879	794.839969	12.400589
12.748907	793.411614	12.405607
12.770461	785.042170	12.410624
12.404168	793.923406	12.415642
12.571936	788.241926	12.420659
12.704689	805.079769	12.425677
12.421744	812.691926	12.430695
12.115593	811.502889	12.435712
12.100261	807.566876	12.440730
12.293618	830.104186	12.445747
12.504763	850.237127	12.450765
12.466850	843.738930	12.455783
12.961087	838.271374	12.460800
12.774507	838.483737	12.465818
13.019483	854.944276	12.470835
12.868432	863.495171	12.475853
13.246334	875.835437	12.480871
13.310696	872.802124	12.485888
13.259899	866.820343	12.490906
13.056568	857.946448	12.495923
13.131663	867.689541	12.500941
13.322705	871.102744	12.505959
12.898932	865.466586	12.510976
12.860035	879.125038	12.515994
12.999289	867.982043	12.521011
13.179394	870.585903	12.526029
13.200969	871.803931	12.531047
13.530670	879.963921	12.536064
13.228596	877.038515	12.541082
13.360914	871.633968	12.546099
13.227716	879.790746	12.551117
13.648556	877.092905	12.556135
13.890911	875.470778	12.561152
13.447924	870.380438	12.566170
13.551972	854.105222	12.571187
13.531739	852.480057	12.576205
12.977175	851.399369	12.581223
13.468320	861.964068	12.586240
13.277341	877.180096	12.591258
13.608721	872.779482	12.596275
13.363114	863.710232	12.601293
13.508829	864.255546	12.606311
13.407513	867.929155	12.611328
13.063943	872.022581	12.616346
13.340665	865.651806	12.621363
13.724209	861.574388	12.626381
13.582594	869.656739	12.631399
13.587432	861.548659	12.636416
13.273105	872.854961	12.641434
13.366060	869.990741	12.646451
13.389092	861.447457	12.651469
13.646835	867.570562	12.656487
13.520882	860.808437	12.661504
12.953424	867.111330	12.666522
13.359992	866.419701	12.671539
13.511708	866.307654	12.676557
13.497259	869.592105	12.681575
13.749040	867.308926	12.686592
13.267716	863.133483	12.691610
13.330921	861.987559	12.696627
13.427048	881.456890	12.701645
13.848335	900.764840	12.706663
13.820707	901.302600	12.711680
13.567143	901.512835	12.716698
13.529067	901.973336	12.721715
13.547859	896.772765	12.726733
13.633006	896.043131	12.731751
13.741141	901.555359	12.736768
13.578639	900.050313	12.741786
13.349828	898.691359	12.746803
13.574824	897.116131	12.751821
13.054033	905.106427	12.756839
13.978242	915.208821	12.761856
13.591397	921.745371	12.766874
13.690020	924.879569	12.771891
13.889751	933.173560	12.776909
13.865657	931.353329	12.781927
13.728557	931.261287	12.786944
14.221803	936.343949	12.791962
14.239150	935.959459	12.796979
14.371443	942.165364	12.801997
13.971345	920.632493	12.807015
14.192474	908.602467	12.812032
13.913980	912.016662	12.817050
13.794581	914.402362	12.822067
14.119736	905.546626	12.827085
13.952170	904.111802	12.832103
14.210505	895.354905	12.837120
14.010009	898.785279	12.842138
13.924381	897.618490	12.847155
14.056283	898.184904	12.852173
13.918452	908.116018	12.857191
13.921088	898.846906	12.862208
14.156446	919.777722	12.867226
14.363590	919.025817	12.872243
13.947597	916.014110	12.877261
14.193988	929.220792	12.882279
14.354280	923.512038	12.887296
14.082537	915.993235	12.892314
14.407238	904.407742	12.897331
14.577196	906.549284	12.902349
13.958273	906.630568	12.907367
14.536860	903.036988	12.912384
14.147627	898.083387	12.917402
14.159734	899.618487	12.922419
14.351208	900.030398	12.927437
14.211597	907.314017	12.932455
14.017118	900.423756	12.937472
13.940769	905.737668	12.942490
13.659021	920.582938	12.947507
14.381781	921.407078	12.952525
14.358927	933.797552	12.957543
14.208533	922.201278	12.962560
14.232547	931.595796	12.967578
13.921737	931.373179	12.972595
14.347741	920.276743	12.977613
14.023289	927.863893	12.982631
14.161366	928.707058	12.987648
14.262276	944.174060	12.992666
14.472116	962.426429	12.997683
14.578040	946.466424	13.002701
14.499403	964.489434	13.007719
14.484805	953.518818	13.012736
14.432914	965.131206	13.017754
14.490169	964.330198	13.022771
14.638181	950.440165	13.027789
14.410937	957.500844	13.032807
14.891549	959.606343	13.037824
14.612418	964.933109	13.042842
14.480964	957.616375	13.047859
14.775654	959.400701	13.052877
14.667043	960.112101	13.057895
14.776784	964.125055	13.062912
14.906666	962.312254	13.067930
14.309551	943.603178	13.072947
14.378502	941.878823	13.077965
14.503169	953.921142	13.082983
14.698121	955.295052	13.088000
14.641192	962.859236	13.093018
14.464314	964.849996	13.098035
15.029643	962.309389	13.103053
14.486713	961.280521	13.108071
14.612962	956.246137	13.113088
14.574800	963.728484	13.118106
14.907804	962.931609	13.123123
14.770589	958.361393	13.128141
14.597644	962.974072	13.133159
14.638097	957.467125	13.138176
15.056223	962.773009	13.143194
14.643282	966.710063	13.148211
15.079469	958.149337	13.153229
14.769331	959.147939	13.158247
14.704827	964.955486	13.163264
14.496042	957.783415	13.168282
14.864182	980.025278	13.173299
15.159160	973.957726	13.178317
15.160957	971.716858	13.183335
15.187284	966.641321	13.188352
14.976730	965.576154	13.193370
14.801517	965.521643	13.198387
15.096312	954.256392	13.203405
14.868454	962.544806	13.208423
14.904201	964.738943	13.213440
15.024536	983.090566	13.218458
15.154969	982.101363	13.223475
15.497168	981.536582	13.228493
15.305398	979.711059	13.233511
15.639512	961.932213	13.238528
15.444871	968.201975	13.243546
15.332400	953.948798	13.248563
15.282106	957.658613	13.253581
15.393617	953.424977	13.258599
15.447704	957.888472	13.263616
15.025561	957.115239	13.268634
14.987509	963.947458	13.273651
15.323612	957.384306	13.278669
15.030151	955.846125	13.283687
15.419842	956.813973	13.288704
15.469958	952.741438	13.293722
15.214963	953.027639	13.298739
15.654314	956.117924	13.303757
15.296764	953.494694	13.308775
14.988341	962.404816	13.313792
15.208931	941.610977	13.318810
15.211001	962.792996	13.323827
15.214912	955.467676	13.328845
15.105667	963.866898	13.333863
15.114058	959.993408	13.338880
15.231538	967.148405	13.343898
15.226924	977.516288	13.348915
15.735991	974.504801	13.353933
15.263945	986.861549	13.358951
15.352207	979.046465	13.363968
15.666883	976.172735	13.368986
15.331029	989.224530	13.374003
15.707265	976.655748	13.379021
15.526433	989.979908	13.384039
15.282745	987.124232	13.389056
15.388218	986.833234	13.394074
15.341704	989.617789	13.399091
15.640601	978.067851	13.404109
15.265747	988.651545	13.409127
15.384829	983.400520	13.414144
15.599600	987.299190	13.419162
15.622305	987.112680	13.424179
15.788160	985.262682	13.429197
15.435264	988.739042	13.434215
15.794093	985.091513	13.439232
15.858654	984.443998	13.444250
15.596874	989.525051	13.449267
15.820468	980.271770	13.454285
15.762759	974.628716	13.459303
15.704521	985.879185	13.464320
15.781399	997.408300	13.469338
15.520415	1009.883476	13.474355
15.746687	1005.335193	13.479373
15.717666	1013.794454	13.484391
15.908282	1012.287721	13.489408
15.871589	1015.332680	13.494426
15.756489	1013.611909	13.499443
15.982593	1012.822314	13.504461
15.721732	1017.562395	13.509479
15.847288	1019.265927	13.514496
16.186012	1012.598200	13.519514
15.922151	1017.130462	13.524531
16.183985	1016.575117	13.529549
16.104162	1016.638207	13.534567
15.772136	1018.179899	13.539584
16.321830	1012.672043	13.544602
15.862401	1014.773353	13.549619
16.074923	1008.832320	13.554637
15.934224	1018.075962	13.559655
16.036617	1019.666356	13.564672
15.978188	1012.252948	13.569690
15.853529	1009.962459	13.574707
16.027321	1016.849870	13.579725
15.953222	1019.588258	13.584743
15.439823	1016.847423	13.589760
16.125991	1017.033499	13.594778
15.718413	1028.004206	13.599795
16.080628	1032.993814	13.604813
15.901773	1035.297325	13.609831
16.397375	1041.670408	13.614848
16.014639	1041.477993	13.619866
16.037904	1037.390711	13.624883
16.388426	1025.532844	13.629901
16.549275	1043.755102	13.634919
16.393234	1037.884430	13.639936
16.432325	1031.251020	13.644954
16.019255	1041.219022	13.649971
16.225396	1038.195026	13.654989
16.420694	1029.037674	13.660007
16.366560	1035.717801	13.665024
16.703624	1027.235691	13.670042
16.462267	1028.491771	13.675059
16.695341	1036.020015	13.680077
16.481586	1032.578958	13.685095
16.222921	1040.629232	13.690112
16.692110	1034.341854	13.695130
16.168355	1039.896325	13.700147
16.399929	1037.799332	13.705165
16.167852	1041.253616	13.710183
16.560626	1040.983876	13.715200
16.874420	1036.453430	13.720218
16.495123	1040.082264	13.725235
16.457911	1035.603659	13.730253
16.391881	1039.110824	13.735271
16.618639	1037.658388	13.740288
16.792804	1029.889785	13.745306
16.479926	1033.366195	13.750323
16.662805	1037.276184	13.755341
16.875293	1051.094200	13.760359
16.753588	1041.396359	13.765376
16.679828	1038.106941	13.770394
16.629409	1048.914399	13.775411
16.518503	1054.855481	13.780429
17.124284	1058.525640	13.785447
16.850069	1062.362082	13.790464
17.234686	1055.936465	13.795482
16.817842	1046.698286	13.800499
16.636757	1036.769903	13.805517
16.922349	1033.641938	13.810535
16.595322	1032.673913	13.815552
16.742090	1039.464579	13.820570
17.103298	1044.760470	13.825587
17.153700	1046.964944	13.830605
17.155493	1042.164637	13.835623
16.645439	1042.784300	13.840640
17.174358	1030.680721	13.845658
17.023806	1030.309913	13.850675
16.884673	1035.349670	13.855693
17.031062	1022.996754	13.860711
17.245799	1030.392166	13.865728
17.343814	1030.465263	13.870746
17.196728	1033.436001	13.875763
17.069757	1032.341954	13.880781
17.178449	1030.109577	13.885799
16.994182	1027.828425	13.890816
17.270708	1024.430476	13.895834
17.143183	1023.588987	13.900851
16.942759	1025.371999	13.905869
17.040571	1027.136685	13.910887
17.241639	1034.903480	13.915904
17.135021	1025.206439	13.920922
17.311770	1034.100541	13.925939
17.062453	1043.784104	13.930957
17.431624	1037.648099	13.935975
17.268936	1046.781588	13.940992
17.598121	1041.219909	13.946010
17.234328	1034.595972	13.951027
17.255135	1028.148470	13.956045
17.394201	1021.240616	13.961063
17.069295	1034.218143	13.966080
17.554170	1038.295416	13.971098
17.516999	1048.930381	13.976115
17.013028	1053.648600	13.981133
17.323504	1043.557985	13.986151
17.410312	1051.279571	13.991168
17.920862	1040.819929	13.996186
17.366659	1043.914419	14.001203
17.404514	1047.458958	14.006221
17.684106	1047.131210	14.011239
17.718463	1053.604969	14.016256
17.459749	1046.768898	14.021274
17.766755	1052.395185	14.026291
17.653425	1046.489415	14.031309
17.638160	1038.567447	14.036327
17.563664	1048.731720	14.041344
17.734943	1037.536263	14.046362
17.735808	1043.579753	14.051379
17.800790	1045.302247	14.056397
17.753599	1031.032469	14.061415
17.579491	1042.247479	14.066432
17.701401	1043.541319	14.071450
17.913387	1046.165456	14.076467
17.819024	1032.931890	14.081485
17.564065	1028.430598	14.086503
17.633676	1042.296241	14.091520
17.513061	1036.195951	14.096538
17.427212	1050.448885	14.101555
17.628262	1054.400214	14.106573
17.871291	1048.230320	14.111591
17.467220	1045.115734	14.116608
17.819757	1048.708801	14.121626
17.938049	1046.323435	14.126643
17.445434	1042.452684	14.131661
18.173047	1039.804587	14.136679
17.740557	1049.441111	14.141696
18.117289	1044.023464	14.146714
18.039298	1039.134670	14.151731
18.090949	1048.685870	14.156749
18.055737	1036.569688	14.161767
17.707734	1047.158676	14.166784
18.064524	1046.099288	14.171802
18.103130	1042.363062	14.176819
18.029515	1047.556664	14.181837
18.265093	1034.457598	14.186855
18.091056	1042.317883	14.191872
18.049369	1041.226252	14.196890
18.292832	1044.246257	14.201907
17.809004	1049.766072	14.206925
18.365689	1056.397841	14.211943
18.275342	1065.734606	14.216960
18.065492	1067.320277	14.221978
18.266124	1069.542242	14.226995
18.404543	1073.771640	14.232013
18.595145	1061.383367	14.237031
18.475197	1051.164522	14.242048
18.289812	1044.910271	14.247066
18.440591	1040.045594	14.252083
17.894649	1035.176470	14.257101
18.115452	1049.274057	14.262119
18.219584	1056.377531	14.267136
18.320179	1063.276429	14.272154
18.693913	1063.429407	14.277171
18.292449	1064.300308	14.282189
18.701766	1063.055959	14.287207
18.831027	1069.767326	14.292224
18.394320	1068.999526	14.297242
18.497316	1073.881433	14.302259
18.710776	1072.061838	14.307277
18.595739	1063.577961	14.312295
18.339228	1069.242051	14.317312
18.336245	1064.575034	14.322330
18.388450	1061.676142	14.327347
18.496997	1066.156378	14.332365
18.606846	1068.458841	14.337383
18.249454	1070.430557	14.342400
18.124547	1062.853970	14.347418
18.765288	1061.674350	14.352435
18.521339	1072.603667	14.357453
18.503630	1061.434651	14.362471
18.296937	1075.324675	14.367488
18.168352	1081.953367	14.372506
18.641405	1087.850303	14.377523
18.495866	1092.004272	14.382541
18.893904	1098.550457	14.387559
18.470385	1100.299001	14.392576
18.416224	1105.107707	14.397594
18.751737	1096.524818	14.402611
18.398341	1099.278576	14.407629
18.880260	1111.413353	14.412647
18.952186	1129.640164	14.417664
18.877792	1125.262040	14.422682
19.103334	1118.327976	14.427699
18.927660	1130.101881	14.432717
18.861456	1113.196677	14.437735
19.571217	1122.079895	14.442752
18.933682	1126.396168	14.447770
19.332672	1126.974392	14.452787
19.201478	1124.053730	14.457805
19.185738	1092.680272	14.462823
18.971191	1099.164644	14.467840
19.090095	1114.818329	14.472858
18.894657	1112.403212	14.477875
19.075236	1118.992944	14.482893
18.864623	1116.965225	14.487911
19.061520	1125.587964	14.492928
19.134169	1120.751286	14.497946
19.180729	1122.937437	14.502963
19.124311	1127.121632	14.507981
19.265907	1124.786255	14.512999
19.137241	1118.949139	14.518016
19.269363	1119.509214	14.523034
19.518989	1115.986070	14.528051
19.115400	1127.309673	14.533069
19.485129	1116.856272	14.538087
19.115974	1116.668040	14.543104
19.211271	1126.461760	14.548122
19.346223	1117.724087	14.553139
19.510475	1115.233677	14.558157
19.542383	1116.547936	14.563175
19.515183	1126.499709	14.568192
19.280603	1126.394536	14.573210
19.735454	1110.060968	14.578227
19.615660	1120.506943	14.583245
19.526904	1121.095314	14.588263
19.609673	1121.060343	14.593280
19.550773	1126.785011	14.598298
19.593619	1114.997384	14.603315
19.495485	1117.221983	14.608333
19.705657	1114.490842	14.613351
20.022791	1122.337322	14.618368
19.473427	1122.379304	14.623386
19.777082	1120.801201	14.628403
19.582156	1120.358445	14.633421
19.937322	1119.554936	14.638439
19.747542	1113.099372	14.643456
19.383319	1125.732819	14.648474
19.714201	1115.714709	14.653491
19.775567	1131.090236	14.658509
20.097578	1136.676327	14.663527
19.769269	1129.270441	14.668544
19.648593	1124.145307	14.673562
20.189119	1134.857071	14.678579
19.868718	1128.330446	14.683597
19.761651	1129.587583	14.688615
19.849114	1144.346786	14.693632
20.131435	1151.624357	14.698650
20.164627	1146.730737	14.703667
19.832789	1151.949048	14.708685
20.024661	1150.934430	14.713703
20.150960	1152.012988	14.718720
19.682896	1156.384769	14.723738
20.032911	1150.905002	14.728755
19.924026	1153.658328	14.733773
19.910221	1149.876640	14.738791
19.787568	1151.486527	14.743808
19.762096	1157.556274	14.748826
20.139633	1140.048168	14.753843
19.889466	1145.004364	14.758861
20.186891	1150.752108	14.763879
20.197825	1152.066500	14.768896
20.072934	1160.935340	14.773914
20.042671	1156.468240	14.778931
20.016111	1167.281500	14.783949
19.930665	1167.885133	14.788967
20.204330	1172.999111	14.793984
20.327603	1180.560400	14.799002
20.443771	1178.787598	14.804019
20.298597	1180.495693	14.809037
20.590845	1165.352086	14.814055
20.871609	1170.395521	14.819072
20.184121	1170.598005	14.824090
20.692135	1179.563356	14.829107
20.218454	1178.687731	14.834125
20.520122	1176.377762	14.839143
20.437183	1173.250708	14.844160
20.216755	1175.014777	14.849178
20.450771	1169.325953	14.854195
20.412027	1174.545688	14.859213
20.633466	1175.606185	14.864231
20.262468	1173.963363	14.869248
20.465032	1174.465064	14.874266
21.010974	1183.336109	14.879283
20.312173	1181.981342	14.884301
20.774019	1187.618126	14.889319
20.790479	1194.145235	14.894336
20.836450	1197.937850	14.899354
20.337987	1197.186032	14.904371
20.863075	1196.188632	14.909389
21.280822	1195.428966	14.914407
21.070317	1188.900879	14.919424
20.735538	1182.234470	14.924442
20.685515	1174.485150	14.929459
20.893138	1190.980255	14.934477
20.934533	1201.782888	14.939495
20.839293	1194.794910	14.944512
20.661644	1196.391326	14.949530
20.816427	1195.720200	14.954547
20.972235	1204.769152	14.959565
21.001556	1193.494851	14.964583
20.914508	1201.796029	14.969600
21.139739	1209.827367	14.974618
20.807347	1196.460554	14.979635
21.155374	1195.601354	14.984653
20.826265	1200.279589	14.989671
21.165052	1188.795852	14.994688
20.747248	1188.949769	14.999706
21.151845	1193.516200	15.004723
20.895489	1195.651987	15.009741
21.059067	1198.580389	15.014759
21.144863	1205.973985	15.019776
21.063095	1223.833637	15.024794
21.447844	1220.156753	15.029811
21.466737	1229.309223	15.034829
21.178892	1221.871712	15.039847
21.541656	1221.717129	15.044864
21.408338	1224.966619	15.049882
21.591847	1223.344213	15.054899
21.577625	1208.838745	15.059917
21.244565	1201.086422	15.064935
21.361896	1202.983772	15.069952
21.148155	1225.613768	15.074970
21.462109	1226.770230	15.079987
21.590767	1229.341177	15.085005
21.429583	1232.891692	15.090023
21.513128	1225.525381	15.095040
21.321430	1236.172045	15.100058
21.224899	1223.847584	15.105075
21.259546	1234.449315	15.110093
21.096900	1228.084135	15.115111
21.554375	1220.207942	15.120128
21.223376	1229.093329	15.125146
21.828884	1237.831988	15.130163
21.363966	1258.588887	15.135181
21.734283	1256.384921	15.140199
21.991954	1254.968652	15.145216
21.551670	1261.128674	15.150234
21.814153	1258.218895	15.155251
21.651128	1252.396586	15.160269
22.098685	1253.872958	15.165287
22.015593	1243.774465	15.170304
21.632552	1256.581373	15.175322
21.971315	1261.413767	15.180339
21.780676	1261.166004	15.185357
21.526727	1262.338862	15.190375
21.749866	1255.720715	15.195392
22.199919	1258.197126	15.200410
22.353319	1251.305874	15.205427
22.028142	1255.393348	15.210445
21.624989	1257.489024	15.215463
21.945210	1255.958809	15.220480
21.711519	1267.123331	15.225498
22.102920	1254.854948	15.230515
22.140521	1251.844700	15.235533
21.931540	1258.533392	15.240551
22.149881	1250.811422	15.245568
21.500615	1254.391075	15.250586
21.977831	1262.679614	15.255603
22.208593	1268.425216	15.260621
22.073271	1278.248841	15.265639
22.242169	1274.176558	15.270656
22.176150	1280.012848	15.275674
22.623568	1280.911707	15.280691
22.428805	1275.428893	15.285709
22.553668	1279.382741	15.290727
22.574465	1275.311571	15.295744
22.380718	1278.709400	15.300762
22.151226	1271.202762	15.305779
22.557648	1283.254808	15.310797
22.533246	1273.913995	15.315815
22.333614	1269.179902	15.320832
22.424976	1262.661298	15.325850
22.861370	1274.266811	15.330867
22.788174	1278.191729	15.335885
22.999181	1264.379948	15.340903
22.863991	1266.020213	15.345920
22.611279	1276.916311	15.350938
22.670802	1268.799478	15.355955
22.800900	1270.417113	15.360973
22.749635	1263.867205	15.365991
22.916928	1254.016666	15.371008
22.593926	1256.320699	15.376026
22.542324	1267.563993	15.381043
22.601042	1259.346301	15.386061
22.557421	1265.545164	15.391079
22.838779	1267.050733	15.396096
22.343168	1264.865671	15.401114
22.835752	1265.965745	15.406131
22.605538	1260.756744	15.411149
22.559685	1269.919380	15.416167
22.595529	1259.723345	15.421184
22.714170	1283.399600	15.426202
22.894870	1287.612956	15.431219
23.115379	1293.748354	15.436237
23.069346	1296.422423	15.441255
23.042585	1301.002817	15.446272
23.047089	1304.262286	15.451290
23.344029	1296.865668	15.456307
23.396755	1295.923338	15.461325
23.217896	1303.573044	15.466343
23.173131	1289.372111	15.471360
23.182290	1284.179249	15.476378
23.224143	1291.712315	15.481395
23.420032	1290.375154	15.486413
23.088592	1286.867276	15.491431
23.416851	1293.449714	15.496448
23.426605	1291.346420	15.501466
23.119906	1284.584051	15.506483
23.512652	1292.103165	15.511501
23.424393	1279.496492	15.516519
23.286890	1271.852359	15.521536
23.102106	1282.791469	15.526554
23.383044	1276.577686	15.531571
23.701433	1286.850957	15.536589
23.439292	1288.779369	15.541607
23.443939	1291.110968	15.546624
23.509947	1293.354054	15.551642
23.347419	1288.888709	15.556659
23.522858	1292.923002	15.561677
23.610371	1300.310056	15.566695
23.592199	1291.564731	15.571712
23.708966	1299.300666	15.576730
23.369525	1291.890144	15.581747
23.808762	1292.891276	15.586765
23.653392	1290.160575	15.591783
23.738648	1290.933135	15.596800
23.832664	1290.022207	15.601818
23.825164	1286.258439	15.606835
24.111487	1276.553346	15.611853
23.634682	1282.337229	15.616871
23.795210	1281.737786	15.621888
24.184228	1289.866580	15.626906
23.824970	1280.139554	15.631923
23.909916	1286.668590	15.636941
23.581056	1297.475642	15.641959
23.558049	1284.274893	15.646976
23.821925	1280.083581	15.651994
23.955966	1291.152631	15.657011
23.841977	1290.624603	15.662029
23.593251	1290.764653	15.667047
23.780233	1291.830556	15.672064
23.635857	1310.558520	15.677082
23.607593	1311.295215	15.682099
23.796977	1318.688407	15.687117
23.915217	1318.127148	15.692135
24.083937	1311.631121	15.697152
23.953083	1317.225106	15.702170
23.921941	1316.655693	15.707187
24.144394	1334.101701	15.712205
24.340880	1346.552772	15.717223
24.326193	1343.680095	15.722240
24.168567	1344.389722	15.727258
24.075987	1346.203206	15.732275
24.552993	1338.873036	15.737293
24.264349	1340.086051	15.742311
24.438183	1339.841143	15.747328
24.505974	1340.446020	15.752346
24.272856	1338.472297	15.757363
24.209854	1344.478556	15.762381
24.302853	1344.533505	15.767399
24.862993	1340.226330	15.772416
24.678973	1334.441999	15.777434
24.315369	1340.466952	15.782451
24.500236	1340.415984	15.787469
24.706561	1344.533816	15.792487
24.668304	1335.722185	15.797504
24.579674	1339.479113	15.802522
24.909033	1344.508672	15.807539
24.846099	1337.966877	15.812557
24.546020	1345.569319	15.817575
24.971854	1336.997412	15.822592
24.936265	1341.683346	15.827610
24.439107	1341.941219	15.832627
25.018590	1334.049016	15.837645
24.940853	1335.068031	15.842663
24.864964	1338.169682	15.847680
25.168744	1342.136538	15.852698
24.816811	1333.809576	15.857715
24.744952	1335.058055	15.862733
24.838374	1336.621480	15.867751
24.857085	1349.135122	15.872768
25.035450	1350.530598	15.877786
25.016958	1357.192636	15.882803
25.007794	1360.820347	15.887821
24.746681	1371.818810	15.892839
25.148993	1357.216400	15.897856
25.403290	1364.268065	15.902874
25.215830	1368.785288	15.907891
25.706741	1351.628460	15.912909
25.292901	1359.030972	15.917927
25.180663	1356.713244	15.922944
25.555893	1361.177017	15.927962
25.282686	1365.755014	15.932979
25.260791	1346.478840	15.937997
25.371077	1357.974550	15.943015
25.374167	1359.353305	15.948032
25.381914	1352.917200	15.953050
25.488368	1358.379337	15.958067
25.468474	1364.419876	15.963085
25.106807	1360.149824	15.968103
25.343899	1357.310282	15.973120
25.464712	1346.681143	15.978138
25.416518	1347.471458	15.983155
25.655060	1357.997133	15.988173
25.472482	1357.457757	15.993191
25.567469	1355.678788	15.998208
25.630596	1360.046289	16.003226
25.675796	1356.394174	16.008243
25.806764	1356.275909	16.013261
25.719678	1360.796339	16.018279
25.667765	1353.826758	16.023296
25.691830	1356.060644	16.028314
25.600246	1357.163885	16.033331
25.773737	1354.826637	16.038349
25.714927	1360.368320	16.043367
25.807649	1369.537698	16.048384
26.082847	1386.369550	16.053402
25.676084	1390.103747	16.058419
25.958029	1378.032319	16.063437
26.186609	1385.583507	16.068455
26.043259	1387.060952	16.073472
26.560065	1378.257011	16.078490
25.866849	1372.113772	16.083507
26.152229	1363.873142	16.088525
25.999511	1373.169344	16.093543
26.046827	1383.904884	16.098560
26.462164	1386.490900	16.103578
25.970986	1388.691905	16.108595
26.372214	1379.685155	16.113613
26.060114	1384.572222	16.118631
25.985704	1384.072705	16.123648
26.425282	1374.987362	16.128666
26.194223	1383.446893	16.133683
26.438418	1381.171150	16.138701
26.196837	1379.425977	16.143719
26.167646	1384.584312	16.148736
26.232411	1383.750550	16.153754
26.010321	1387.541022	16.158771
26.555359	1387.550393	16.163789
26.144410	1384.458915	16.168807
25.954760	1390.358795	16.173824
26.412798	1399.142731	16.178842
26.359203	1401.530809	16.183859
26.332443	1404.823599	16.188877
26.172222	1418.854938	16.193895
26.356317	1412.002998	16.198912
26.983588	1408.067160	16.203930
26.627014	1408.157833	16.208947
26.593343	1403.871095	16.213965
26.800300	1407.155670	16.218983
26.646430	1408.483278	16.224000
26.558074	1398.849449	16.229018
26.493562	1409.801351	16.234035
26.744647	1405.517336	16.239053
27.081826	1416.103333	16.244071
26.836666	1421.087224	16.249088
27.033884	1421.378321	16.254106
27.055765	1424.341585	16.259123
27.216921	1414.359369	16.264141
27.213124	1410.036389	16.269159
26.952786	1406.637274	16.274176
26.893300	1403.042580	16.279194
26.914926	1408.227675	16.284211
27.507108	1408.554723	16.289229
27.030125	1409.541619	16.294247
27.086616	1421.617026	16.299264
27.267026	1417.643898	16.304282
27.242361	1428.946193	16.309299
27.433185	1421.266333	16.314317
27.438258	1420.391426	16.319335
27.230626	1422.229257	16.324352
27.328617	1418.938106	16.329370
27.203560	1421.709787	16.334387
27.291282	1419.051437	16.339405
27.391891	1419.512312	16.344423
27.460077	1425.747365	16.349440
27.260906	1420.937416	16.354458
27.359966	1423.853872	16.359475
27.427771	1425.288768	16.364493
27.519639	1422.257364	16.369511
27.150090	1423.041225	16.374528
27.505701	1422.019873	16.379546
26.844641	1435.239716	16.384563
27.410691	1430.041612	16.389581
27.846800	1447.163906	16.394599
27.498079	1451.662233	16.399616
27.797919	1456.027384	16.404634
27.538387	1455.724136	16.409651
27.767631	1458.740127	16.414669
27.620225	1449.705688	16.419687
27.581092	1453.132976	16.424704
27.818266	1451.205481	16.429722
27.601995	1460.262365	16.434739
27.787270	1451.481929	16.439757
27.840262	1452.363698	16.444775
27.413608	1449.643918	16.449792
28.217573	1454.027917	16.454810
27.879046	1464.249573	16.459827
28.173398	1473.598863	16.464845
28.338362	1468.842307	16.469863
27.780307	1457.325338	16.474880
28.091711	1469.382930	16.479898
27.891746	1479.857455	16.484915
28.118137	1480.876167	16.489933
28.144818	1488.364353	16.494951
27.983075	1482.750063	16.499968
28.281230	1481.283250	16.504986
28.264695	1482.532538	16.510003
28.372214	1486.937298	16.515021
28.149002	1480.982326	16.520039
28.061283	1486.339219	16.525056
28.348343	1484.160894	16.530074
28.209727	1483.658811	16.535091
28.325362	1485.101997	16.540109
28.703400	1481.606002	16.545127
28.425689	1481.274042	16.550144
28.313881	1476.166353	16.555162
28.517571	1485.346808	16.560179
28.625278	1503.716723	16.565197
28.456932	1500.391544	16.570215
28.721064	1508.543160	16.575232
28.399054	1497.285844	16.580250
28.565022	1507.217030	16.585267
28.984794	1498.159976	16.590285
28.703518	1507.952943	16.595303
28.493048	1506.048240	16.600320
28.813405	1502.984179	16.605338
28.682261	1504.443940	16.610355
29.015875	1510.179818	16.615373
28.930865	1500.273996	16.620391
28.828462	1502.893809	16.625408
29.056566	1498.562877	16.630426
29.199686	1487.627187	16.635443
29.082041	1499.758335	16.640461
29.209695	1493.858843	16.645479
29.143941	1494.879146	16.650496
28.932227	1498.456566	16.655514
29.069013	1499.120070	16.660531
29.067838	1501.111763	16.665549
29.428818	1495.778505	16.670567
28.985044	1505.032011	16.675584
29.213245	1503.718175	16.680602
29.280990	1505.702227	16.685619
29.216713	1513.185738	16.690637
29.512325	1507.177872	16.695655
29.311479	1504.429015	16.700672
29.790135	1492.752747	16.705690
29.220851	1498.977245	16.710707
29.363128	1501.713364	16.715725
29.467181	1502.138986	16.720743
29.538579	1497.886259	16.725760
29.590799	1495.391259	16.730778
29.179766	1509.149524	16.735795
29.091375	1514.777945	16.740813
29.684982	1515.906391	16.745831
29.685174	1525.863561	16.750848
29.750696	1529.296558	16.755866
29.366865	1535.949628	16.760883
29.513569	1531.546231	16.765901
29.685459	1525.781818	16.770919
29.525753	1524.222628	16.775936
29.542832	1535.935039	16.780954
29.728515	1528.483170	16.785971
29.400895	1533.151789	16.790989
29.705302	1541.871499	16.796007
29.903152	1559.097506	16.801024
29.839454	1553.650879	16.806042
29.685040	1557.560178	16.811059
29.578591	1566.773487	16.816077
29.841372	1559.009707	16.821095
29.793500	1554.658883	16.826112
30.196452	1550.139588	16.831130
29.975945	1558.458684	16.836147
29.867473	1571.718286	16.841165
30.557527	1576.861821	16.846183
30.008587	1582.843305	16.851200
30.215085	1579.563527	16.856218
30.208036	1580.246414	16.861235
30.011720	1586.201054	16.866253
30.340954	1575.447601	16.871271
30.517162	1587.160360	16.876288
30.350981	1581.856021	16.881306
30.668240	1581.784310	16.886323
30.192961	1589.619444	16.891341
30.450678	1566.944406	16.896359
30.156297	1571.052374	16.901376
30.623650	1569.574824	16.906394
30.656727	1568.338896	16.911411
30.203777	1577.319306	16.916429
30.803524	1574.949959	16.921447
30.783332	1578.803517	16.926464
30.577219	1577.595597	16.931482
30.820943	1572.848766	16.936499
30.786627	1572.204098	16.941517
30.635434	1569.882978	16.946535
30.483291	1581.662960	16.951552
31.236352	1586.859745	16.956570
31.115567	1576.801686	16.961587
30.622571	1569.131069	16.966605
30.835549	1583.498562	16.971623
31.126111	1596.370594	16.976640
30.986385	1604.503476	16.981658
30.981661	1603.103044	16.986675
31.079019	1599.370121	16.991693
31.296438	1593.298733	16.996711
31.154674	1603.366556	17.001728
31.078080	1594.390381	17.006746
31.391388	1599.867522	17.011763
31.253446	1604.219246	17.016781
31.462799	1598.228020	17.021799
31.440297	1600.709088	17.026816
31.316062	1604.184455	17.031834
31.382046	1593.424897	17.036851
31.341823	1600.099898	17.041869
31.655035	1602.345320	17.046887
31.286494	1600.455905	17.051904
31.335053	1594.796005	17.056922
31.523891	1600.942783	17.061939
31.229289	1599.925461	17.066957
31.543158	1604.708197	17.071975
31.755476	1599.638057	17.076992
31.257926	1597.219713	17.082010
31.384628	1600.075059	17.087027
31.377940	1605.602339	17.092045
31.624876	1596.786923	17.097063
31.456175	1590.312103	17.102080
31.478944	1604.772535	17.107098
31.571149	1616.479539	17.112115
31.566126	1626.380774	17.117133
31.746903	1622.536939	17.122151
31.930904	1613.744000	17.127168
31.942188	1627.843311	17.132186
32.349244	1623.686295	17.137203
31.987518	1628.495990	17.142221
32.214448	1620.955564	17.147239
32.011211	1624.695792	17.152256
32.033358	1623.275369	17.157274
32.035812	1620.362089	17.162291
31.887967	1624.185162	17.167309
31.947571	1616.128124	17.172327
32.108945	1627.761178	17.177344
32.145723	1607.995819	17.182362
32.291574	1615.361238	17.187379
32.057238	1619.658637	17.192397
32.177087	1616.531293	17.197415
32.125360	1634.869515	17.202432
32.297262	1652.415277	17.207450
32.605728	1644.679018	17.212467
32.393404	1645.832754	17.217485
32.483589	1641.463434	17.222503
32.360320	1639.153709	17.227520
32.520213	1644.973657	17.232538
32.493484	1637.075312	17.237555
32.670695	1647.213110	17.242573
32.669814	1630.208816	17.247591
32.389188	1631.414280	17.252608
32.210058	1632.098883	17.257626
32.551829	1634.163098	17.262643
32.653580	1643.902438	17.267661
32.664202	1654.404033	17.272679
32.873957	1667.730618	17.277696
32.767737	1667.065653	17.282714
33.137107	1655.668351	17.287731
32.916516	1663.507797	17.292749
33.150861	1668.748007	17.297767
32.759617	1671.807601	17.302784
33.063652	1669.724431	17.307802
33.200640	1661.857231	17.312819
33.123288	1667.023194	17.317837
33.150530	1671.251216	17.322855
32.928694	1664.885687	17.327872
32.953525	1662.593783	17.332890
33.418013	1663.647789	17.337907
33.097236	1669.814473	17.342925
32.933045	1662.237475	17.347943
33.024530	1658.050995	17.352960
32.598963	1659.768351	17.357978
32.899396	1673.023924	17.362995
33.263569	1684.647333	17.368013
33.475923	1686.570875	17.373031
33.659198	1687.795183	17.378048
33.370534	1681.957703	17.383066
33.481007	1686.882791	17.388083
33.349448	1696.870166	17.393101
33.733146	1684.858335	17.398119
33.793570	1689.071695	17.403136
33.760465	1693.924600	17.408154
34.179447	1690.535766	17.413171
33.609335	1693.039527	17.418189
33.835440	1686.509126	17.423207
34.136640	1693.525169	17.428224
33.583452	1688.079449	17.433242
33.922896	1686.025446	17.438259
33.537155	1690.488603	17.443277
33.511308	1693.023861	17.448295
33.647833	1705.560321	17.453312
33.743315	1716.067593	17.458330
33.989860	1714.889733	17.463347
34.152284	1723.357205	17.468365
33.954342	1720.355378	17.473383
34.210960	1720.435189	17.478400
33.550400	1728.542426	17.483418
34.502455	1707.547883	17.488435
34.003886	1722.348885	17.493453
34.292906	1718.838388	17.498471
34.072433	1712.740889	17.503488
34.377191	1719.276671	17.508506
34.323803	1728.522777	17.513523
34.561649	1741.747179	17.518541
34.652638	1735.130626	17.523559
34.691229	1732.498864	17.528576
34.578381	1727.965660	17.533594
34.807603	1710.710628	17.538611
34.710520	1714.670943	17.543629
34.388398	1711.322477	17.548647
34.860354	1706.650312	17.553664
34.446579	1716.240075	17.558682
35.002302	1720.183322	17.563699
34.757254	1717.002672	17.568717
35.162220	1718.536254	17.573735
35.131422	1699.295811	17.578752
34.780977	1711.927511	17.583770
34.641581	1703.983669	17.588787
34.856828	1693.276409	17.593805
34.937240	1705.244112	17.598823
35.166653	1715.645187	17.603840
34.894616	1721.924180	17.608858
35.283012	1729.201148	17.613875
35.385001	1709.573793	17.618893
35.247155	1710.731644	17.623911
35.216843	1700.365831	17.628928
35.030372	1705.668830	17.633946
34.900397	1706.494066	17.638963
34.793743	1720.605616	17.643981
35.060616	1725.433620	17.648999
35.319959	1721.135613	17.654016
35.250600	1725.296728	17.659034
35.226952	1724.075989	17.664051
35.585687	1730.319276	17.669069
35.494037	1724.053256	17.674087
35.788219	1728.201596	17.679104
35.184482	1723.675874	17.684122
35.602682	1726.567625	17.689139
35.310903	1721.390227	17.694157
35.854226	1725.310170	17.699175
36.045827	1723.796912	17.704192
35.568968	1731.556611	17.709210
35.948222	1718.595493	17.714227
35.499701	1718.479652	17.719245
35.610386	1730.259579	17.724263
35.959307	1750.353011	17.729280
35.736710	1762.197802	17.734298
36.057163	1747.409072	17.739315
36.010833	1745.106215	17.744333
35.977937	1748.254852	17.749351
36.414071	1759.800759	17.754368
36.120112	1747.850877	17.759386
36.026570	1743.870104	17.764403
36.372913	1744.081033	17.769421
36.325929	1746.723759	17.774439
36.099377	1747.643029	17.779456
36.119746	1751.278816	17.784474
36.513333	1740.259545	17.789491
36.507700	1741.106329	17.794509
36.136571	1748.442343	17.799527
36.344790	1743.445393	17.804544
36.346258	1743.145430	17.809562
36.533726	1739.840201	17.814579
36.599101	1748.496472	17.819597
36.544219	1746.387471	17.824615
36.552656	1750.558495	17.829632
36.174658	1743.592513	17.834650
36.344881	1748.236838	17.839667
36.529790	1751.761632	17.844685
36.396234	1755.680330	17.849703
37.091749	1765.572875	17.854720
36.855282	1768.128519	17.859738
36.968589	1768.672627	17.864755
36.880710	1773.272186	17.869773
36.831604	1775.451312	17.874791
37.021853	1771.937344	17.879808
36.749548	1784.954511	17.884826
37.234845	1775.871272	17.889843
37.229052	1778.750562	17.894861
36.937575	1781.097061	17.899879
37.316518	1766.835675	17.904896
37.069953	1766.255816	17.909914
37.106905	1767.118021	17.914931
37.055465	1763.477810	17.919949
37.080343	1768.798209	17.924967
37.495315	1761.029433	17.929984
37.086897	1772.306857	17.935002
37.221087	1766.829160	17.940019
37.101418	1770.584728	17.945037
37.125405	1766.983194	17.950055
37.267137	1765.471435	17.955072
37.233012	1773.647812	17.960090
37.366686	1784.613075	17.965107
37.562814	1792.242108	17.970125
37.231106	1787.509635	17.975143
37.736793	1786.878189	17.980160
37.415641	1793.780327	17.985178
37.261449	1798.516523	17.990195
37.382229	1793.747869	17.995213
37.306697	1786.923841	18.000231
37.647285	1807.422613	18.005248
37.441164	1825.908306	18.010266
37.517486	1821.231822	18.015283
37.966075	1825.851489	18.020301
38.042827	1820.957173	18.025319
38.217336	1817.461442	18.030336
38.105858	1822.383470	18.035354
38.099072	1820.828699	18.040371
38.212337	1824.241648	18.045389
38.276095	1821.148305	18.050407
38.083860	1815.926878	18.055424
38.276604	1822.622270	18.060442
38.327967	1820.774345	18.065459
38.284627	1815.488562	18.070477
38.290018	1822.538379	18.075495
38.594723	1834.972835	18.080512
38.211279	1839.533506	18.085530
38.582902	1848.905602	18.090547
38.178394	1846.365340	18.095565
38.032961	1854.344583	18.100583
38.073307	1849.276068	18.105600
38.172146	1851.147981	18.110618
38.153449	1847.515246	18.115635
38.485890	1865.048688	18.120653
38.418089	1879.574028	18.125671
38.624851	1874.286914	18.130688
38.709027	1877.874857	18.135706
38.419678	1874.890482	18.140723
38.560375	1870.740426	18.145741
38.634308	1889.892415	18.150759
38.912814	1897.363408	18.155776
39.052519	1903.761004	18.160794
38.922683	1896.169055	18.165811
38.872891	1902.287048	18.170829
38.840995	1900.010314	18.175847
39.121876	1892.672777	18.180864
39.260038	1898.089083	18.185882
39.368451	1903.289129	18.190899
39.471624	1893.924849	18.195917
39.220469	1907.869823	18.200935
39.307194	1896.087432	18.205952
39.563809	1902.394120	18.210970
39.239060	1896.792615	18.215987
39.493745	1901.180731	18.221005
39.438280	1909.654025	18.226023
39.270654	1899.306456	18.231040
39.442424	1920.980609	18.236058
39.450613	1918.583974	18.241075
39.701132	1914.609221	18.246093
39.856794	1922.484509	18.251111
39.731872	1921.330121	18.256128
39.938170	1921.039092	18.261146
39.744208	1918.841401	18.266163
39.849386	1917.240674	18.271181
39.476807	1922.967402	18.276199
39.576751	1918.350313	18.281216
39.660983	1915.619848	18.286234
39.882821	1918.280445	18.291251
39.998443	1919.764697	18.296269
40.091717	1934.479456	18.301287
40.137850	1940.525623	18.306304
40.121471	1938.034998	18.311322
40.100377	1941.980301	18.316339
40.157155	1943.644202	18.321357
39.921317	1949.428414	18.326375
40.179825	1946.171982	18.331392
40.419082	1946.743703	18.336410
40.149760	1945.438355	18.341427
40.633544	1947.745465	18.346445
40.061504	1940.582573	18.351463
40.267623	1946.644705	18.356480
40.371924	1959.211640	18.361498
40.639888	1962.729775	18.366515
40.859050	1970.958082	18.371533
40.446497	1976.151404	18.376551
40.714887	1979.458020	18.381568
40.664026	1981.078824	18.386586
40.756283	1975.355148	18.391603
40.818219	1977.406439	18.396621
40.750955	1982.296335	18.401639
40.775543	1971.502008	18.406656
41.490740	1970.528437	18.411674
41.222031	1976.128445	18.416691
41.113580	1975.419633	18.421709
40.946026	1972.842226	18.426727
41.158245	1972.698603	18.431744
41.116194	1973.822526	18.436762
40.841114	1980.177831	18.441779
41.250103	1968.767812	18.446797
41.486873	1973.887802	18.451815
41.453367	1966.053495	18.456832
41.151186	1971.816548	18.461850
40.627165	1978.842069	18.466867
40.935005	1986.725103	18.471885
41.279382	1995.378807	18.476903
41.274603	1996.657850	18.481920
41.202819	1994.961757	18.486938
41.164886	2001.762791	18.491955
41.800476	2023.020385	18.496973
41.888357	2027.977510	18.501991
41.781903	2021.991440	18.507008
41.833466	2022.314837	18.512026
41.863539	2023.452710	18.517043
41.861892	2015.042143	18.522061
41.509141	2020.702673	18.527079
41.975331	2023.104076	18.532096
42.017095	2014.557308	18.537114
42.047377	2023.411729	18.542131
42.168081	2016.231793	18.547149
41.949069	2023.462027	18.552167
41.902951	2020.733032	18.557184
42.102631	2012.278298	18.562202
42.096947	2030.776981	18.567219
42.304949	2030.507775	18.572237
42.513222	2042.540884	18.577255
42.286134	2046.657351	18.582272
42.373743	2044.453401	18.587290
42.619651	2052.917417	18.592307
42.296626	2041.290656	18.597325
42.608705	2057.609233	18.602343
42.603616	2044.739661	18.607360
42.683539	2041.640592	18.612378
42.654137	2047.215751	18.617395
42.863198	2041.833546	18.622413
42.716559	2050.078174	18.627431
42.888121	2042.423161	18.632448
42.790354	2052.452780	18.637466
42.555818	2032.297082	18.642483
43.029270	2033.876771	18.647501
42.742307	2040.448571	18.652519
42.724195	2033.075765	18.657536
42.955501	2039.282318	18.662554
42.801633	2033.944354	18.667571
43.168041	2034.502468	18.672589
42.765606	2043.636153	18.677607
42.979809	2060.503444	18.682624
43.220660	2066.241412	18.687642
43.264557	2072.265881	18.692659
43.181220	2064.136356	18.697677
43.269214	2066.514963	18.702695
43.252071	2074.755093	18.707712
43.755151	2061.174674	18.712730
43.676514	2071.043503	18.717747
43.795978	2065.489120	18.722765
43.463518	2066.519682	18.727783
43.369177	2069.053100	18.732800
43.352391	2061.598016	18.737818
43.299139	2078.059066	18.742835
43.503151	2077.638993	18.747853
43.988152	2094.653253	18.752871
43.712725	2098.698404	18.757888
44.115811	2099.105594	18.762906
44.084392	2101.865864	18.767923
43.944133	2087.287907	18.772941
44.227977	2090.734147	18.777959
43.723364	2094.029342	18.782976
44.247429	2086.426387	18.787994
44.165717	2089.816282	18.793011
44.168407	2098.845492	18.798029
44.015957	2090.669973	18.803047
44.130308	2097.911128	18.808064
44.538518	2094.706960	18.813082
44.244555	2097.937591	18.818099
44.187673	2086.127078	18.823117
44.108356	2108.055410	18.828135
44.182735	2116.259127	18.833152
44.068066	2113.001169	18.838170
44.413903	2123.456830	18.843187
44.284938	2112.617043	18.848205
44.557715	2116.150235	18.853223
44.515670	2123.040330	18.858240
44.884937	2133.725876	18.863258
44.521363	2145.823401	18.868275
44.840725	2134.313701	18.873293
44.954943	2152.525456	18.878311
44.753816	2149.448310	18.883328
44.926724	2149.594893	18.888346
45.288320	2145.015654	18.893363
45.093680	2148.016118	18.898381
45.283821	2145.161717	18.903399
44.786880	2136.532022	18.908416
45.196744	2145.648952	18.913434
45.046518	2148.434155	18.918451
45.333067	2140.050965	18.923469
45.366328	2141.235687	18.928487
44.983107	2139.758805	18.933504
45.230308	2146.928667	18.938522
45.302250	2161.504929	18.943539
45.328974	2161.421929	18.948557
45.458289	2166.991195	18.953575
45.446518	2173.049669	18.958592
45.478823	2179.142269	18.963610
45.667165	2168.757708	18.968627
45.360608	2162.282188	18.973645
45.560782	2167.187041	18.978663
45.535356	2182.577067	18.983680
45.687290	2183.575926	18.988698
45.404114	2195.408400	18.993715
45.722065	2191.861718	18.998733
45.958639	2194.387491	19.003751
45.998848	2199.655118	19.008768
46.277547	2193.062641	19.013786
45.971266	2193.953395	19.018803
45.969352	2186.934628	19.023821
46.170557	2190.422239	19.028839
45.738245	2198.721161	19.033856
46.560957	2210.285693	19.038874
46.405246	2221.899379	19.043891
46.433755	2216.321328	19.048909
46.329375	2215.384628	19.053927
45.876230	2213.123358	19.058944
46.205030	2212.494365	19.063962
46.114714	2221.317281	19.068979
46.226440	2235.524419	19.073997
46.472562	2244.427189	19.079015
46.760275	2244.637845	19.084032
46.682380	2245.527536	19.089050
46.490714	2251.352265	19.094067
46.538000	2246.105810	19.099085
46.408733	2238.863955	19.104103
46.912122	2264.494817	19.109120
46.883880	2276.953341	19.114138
46.669346	2272.862006	19.119155
47.109466	2268.563951	19.124173
47.560813	2273.921833	19.129191
47.343488	2275.410939	19.134208
47.196218	2274.635606	19.139226
47.080634	2275.559609	19.144243
47.362522	2278.431779	19.149261
47.643854	2279.419838	19.154279
47.475123	2269.981188	19.159296
47.359368	2266.537162	19.164314
47.483870	2274.029285	19.169331
47.534569	2266.879155	19.174349
47.641863	2261.695883	19.179367
47.487716	2274.675953	19.184384
48.024688	2284.088649	19.189402
48.133365	2297.545159	19.194419
47.776742	2279.248327	19.199437
48.025889	2268.620630	19.204455
48.042931	2288.116503	19.209472
48.267115	2285.035819	19.214490
48.241959	2267.990539	19.219507
47.898514	2258.655016	19.224525
48.439144	2259.899121	19.229543
48.598666	2264.349579	19.234560
48.326501	2258.645037	19.239578
48.226196	2257.477301	19.244595
48.029008	2264.925140	19.249613
48.357515	2261.465162	19.254631
48.447997	2270.215589	19.259648
48.573688	2288.602427	19.264666
48.552146	2281.880216	19.269683
48.411755	2279.118611	19.274701
48.709982	2282.493199	19.279719
48.665406	2283.526009	19.284736
48.632426	2278.920186	19.289754
48.511586	2283.502946	19.294771
48.806995	2278.388036	19.299789
48.744535	2279.227968	19.304807
48.632775	2290.910559	19.309824
48.510847	2282.900601	19.314842
48.457824	2275.571039	19.319859
48.501538	2275.756802	19.324877
48.483718	2284.921875	19.329895
48.490761	2306.650707	19.334912
49.132700	2303.488786	19.339930
49.004184	2313.362406	19.344947
49.149345	2314.213996	19.349965
49.171305	2305.038970	19.354983
49.184751	2329.373778	19.360000
49.065771	2332.163583	19.365018
49.123803	2332.394444	19.370035
48.944381	2343.907772	19.375053
49.521498	2338.111171	19.380071
49.252773	2334.943588	19.385088
49.521896	2335.097191	19.390106
49.536155	2347.744784	19.395123
49.558495	2358.143958	19.400141
49.827164	2356.422894	19.405159
49.851957	2364.271539	19.410176
49.649077	2357.413593	19.415194
49.914984	2366.139738	19.420211
49.876911	2361.872397	19.425229
50.034437	2358.972575	19.430247
49.779400	2364.387505	19.435264
49.588106	2355.548854	19.440282
49.920587	2379.035243	19.445299
49.699577	2393.026367	19.450317
50.156547	2388.649897	19.455335
50.231556	2395.812119	19.460352
50.593452	2391.936588	19.465370
50.024107	2405.650904	19.470387
49.791376	2400.489306	19.475405
50.676264	2409.102711	19.480423
50.384632	2425.203753	19.485440
50.451641	2420.967277	19.490458
50.558911	2424.611677	19.495475
50.557272	2421.323329	19.500493
50.969922	2413.333709	19.505511
51.014470	2423.839907	19.510528
51.061837	2419.502355	19.515546
50.893027	2423.486688	19.520563
50.672073	2422.808109	19.525581
51.089708	2422.401902	19.530599
50.778661	2427.030279	19.535616
50.859474	2437.354059	19.540634
50.898372	2439.895058	19.545651
51.021493	2445.017209	19.550669
51.617654	2444.381037	19.555687
51.089401	2436.696632	19.560704
51.308697	2447.465829	19.565722
51.475769	2452.874617	19.570739
51.144917	2455.157936	19.575757
51.501911	2437.329864	19.580775
51.299626	2441.480409	19.585792
51.782739	2455.888336	19.590810
52.064324	2469.867052	19.595827
51.830070	2474.382414	19.600845
52.314472	2455.391838	19.605863
51.617346	2452.386040	19.610880
51.630138	2441.211387	19.615898
51.774431	2461.997309	19.620915
51.527481	2467.287913	19.625933
51.848530	2459.918604	19.630951
51.791659	2468.203012	19.635968
51.879681	2468.391304	19.640986
52.198657	2474.587427	19.646003
52.136609	2469.036111	19.651021
51.900211	2470.989018	19.656039
52.199807	2489.831704	19.661056
52.077972	2494.045403	19.666074
52.351531	2490.900138	19.671091
52.142036	2493.628401	19.676109
52.554883	2499.165971	19.681127
52.466716	2500.259278	19.686144
52.459146	2507.333486	19.691162
52.635176	2494.829734	19.696179
52.443687	2508.851040	19.701197
52.729996	2512.956610	19.706215
52.464865	2518.644597	19.711232
52.420625	2526.923897	19.716250
52.758803	2515.909679	19.721267
52.746581	2531.859730	19.726285
52.903745	2532.258120	19.731303
53.041237	2548.023764	19.736320
53.128779	2550.459317	19.741338
52.956077	2558.370551	19.746355
52.933101	2559.867104	19.751373
53.318209	2556.028932	19.756391
53.077980	2547.873270	19.761408
53.294060	2553.946672	19.766426
53.458251	2563.623073	19.771443
53.332285	2584.230548	19.776461
53.269073	2585.717627	19.781479
53.371000	2581.857538	19.786496
53.189042	2585.591473	19.791514
53.515494	2586.686102	19.796531
53.627058	2593.306128	19.801549
54.037118	2602.710471	19.806567
53.817575	2604.768062	19.811584
54.154215	2601.328839	19.816602
54.303063	2597.597110	19.821619
53.947613	2602.188303	19.826637
54.182661	2601.365680	19.831655
54.021518	2606.065301	19.836672
54.177541	2601.896896	19.841690
54.412057	2594.219162	19.846707
54.296641	2602.717955	19.851725
54.686055	2601.830116	19.856743
54.149102	2593.547335	19.861760
54.271442	2595.311490	19.866778
54.884316	2591.024167	19.871795
54.686015	2602.183970	19.876813
54.875477	2605.200077	19.881831
54.871877	2598.983079	19.886848
54.753718	2599.910658	19.891866
55.018806	2604.938019	19.896883
54.636145	2602.302695	19.901901
55.248493	2612.982003	19.906919
54.822278	2625.316907	19.911936
54.909317	2627.045566	19.916954
55.202508	2625.743562	19.921971
54.894716	2627.486740	19.926989
54.796866	2624.614263	19.932007
55.198636	2625.987462	19.937024
54.678841	2623.200031	19.942042
55.184492	2639.214222	19.947059
54.972873	2649.609190	19.952077
55.265141	2642.660931	19.957095
55.648264	2644.084396	19.962112
55.648358	2654.667129	19.967130
55.968154	2642.326964	19.972147
55.947910	2657.195815	19.977165
55.844019	2650.562117	19.982183
55.601613	2648.895850	19.987200
55.945419	2648.040404	19.992218
56.322411	2641.394490	19.997235
56.135621	2650.933401	20.002253
56.240298	2645.857740	20.007271
56.121223	2656.534893	20.012288
56.202549	2656.847327	20.017306
56.165240	2641.201785	20.022323
56.137242	2646.107801	20.027341
56.144663	2651.882529	20.032359
56.017419	2649.358676	20.037376
55.553296	2651.454592	20.042394
56.094356	2660.443919	20.047411
56.222325	2674.071277	20.052429
56.771039	2678.457704	20.057447
56.520448	2676.675938	20.062464
56.825814	2676.501936	20.067482
56.836456	2672.409948	20.072499
56.785589	2671.894081	20.077517
56.347459	2674.872814	20.082535
56.545443	2690.174615	20.087552
56.273843	2688.885348	20.092570
56.439302	2696.885689	20.097587
56.595387	2711.862674	20.102605
57.104191	2720.509904	20.107623
56.740707	2716.757424	20.112640
56.692014	2734.581831	20.117658
57.221989	2733.211159	20.122675
57.407277	2730.881355	20.127693
57.468364	2746.627582	20.132711
57.299072	2759.272660	20.137728
57.202714	2763.043719	20.142746
57.343890	2753.897129	20.147763
57.657648	2758.560258	20.152781
57.589521	2757.886127	20.157799
57.816754	2748.299971	20.162816
57.416395	2759.213783	20.167834
57.796425	2774.966875	20.172851
57.672994	2779.584884	20.177869
57.512393	2788.330716	20.182887
57.731666	2786.958221	20.187904
58.140384	2790.716432	20.192922
58.207750	2787.057399	20.197939
58.131862	2789.916270	20.202957
58.082922	2800.743486	20.207975
58.525129	2804.739481	20.212992
58.173585	2813.489991	20.218010
58.554082	2807.976544	20.223027
58.651898	2826.257831	20.228045
58.904291	2811.519926	20.233063
58.729183	2806.895206	20.238080
58.297941	2810.216907	20.243098
58.816497	2809.217295	20.248115
58.944711	2806.943766	20.253133
58.912574	2810.922551	20.258151
59.010563	2813.874120	20.263168
58.845725	2816.964711	20.268186
59.045403	2808.976723	20.273203
58.507370	2815.244114	20.278221
58.663078	2825.199731	20.283239
59.231855	2836.567740	20.288256
58.712685	2833.152092	20.293274
59.323779	2830.739780	20.298291
59.234009	2832.464599	20.303309
59.225956	2844.573168	20.308327
59.301884	2850.974781	20.313344
59.076881	2866.936373	20.318362
59.062943	2863.842400	20.323379
59.143707	2865.281693	20.328397
58.967195	2866.246833	20.333415
59.481997	2880.893165	20.338432
59.798625	2899.515832	20.343450
59.975097	2892.989617	20.348467
59.776396	2897.445857	20.353485
59.903966	2893.894150	20.358503
60.016385	2881.687313	20.363520
59.888035	2898.066190	20.368538
59.932119	2914.856780	20.373555
60.410339	2911.695158	20.378573
60.159801	2919.429372	20.383591
60.225390	2914.400790	20.388608
60.286914	2918.573235	20.393626
60.420938	2925.234051	20.398643
60.479520	2928.441155	20.403661
60.417233	2926.573049	20.408679
60.729883	2927.897111	20.413696
60.447886	2945.890842	20.418714
60.520230	2949.187323	20.423731
60.542947	2946.633621	20.428749
60.685599	2950.594520	20.433767
60.841877	2949.137196	20.438784
61.025927	2961.919585	20.443802
61.306802	2967.929319	20.448819
61.330563	2971.422790	20.453837
61.297426	2983.393352	20.458855
61.389407	2976.956094	20.463872
61.323878	2980.286808	20.468890
61.058818	2976.392602	20.473907
61.519187	2971.478902	20.478925
61.187200	2974.712488	20.483943
61.428456	2964.060370	20.488960
61.334406	2984.619114	20.493978
61.574601	2985.720971	20.498995
61.667554	2994.679674	20.504013
61.604184	3007.608172	20.509031
61.667512	2999.824525	20.514048
61.805601	3009.274850	20.519066
61.904284	3003.133219	20.524083
62.032527	3001.664502	20.529101
61.702117	3018.012021	20.534119
61.954717	3027.700069	20.539136
62.006241	3031.321764	20.544154
62.114245	3026.876724	20.549171
61.869821	3020.025034	20.554189
61.854490	3032.987054	20.559207
61.981967	3049.319673	20.564224
61.901168	3062.853784	20.569242
62.238643	3053.278600	20.574259
62.645919	3079.847307	20.579277
62.568312	3079.935306	20.584295
62.437883	3077.348767	20.589312
63.095148	3079.590972	20.594330
62.879904	3078.381222	20.599347
62.855793	3076.153620	20.604365
62.632105	3089.691201	20.609383
62.790811	3098.150434	20.614400
63.201427	3106.270359	20.619418
62.760084	3106.225971	20.624435
63.243641	3109.316023	20.629453
63.166842	3105.218700	20.634471
63.627315	3106.740552	20.639488
63.328196	3105.026316	20.644506
63.617354	3114.383589	20.649523
63.998334	3123.338260	20.654541
63.552369	3126.542387	20.659559
63.918167	3123.474093	20.664576
63.718060	3134.801788	20.669594
63.648992	3138.360336	20.674611
63.895263	3131.599005	20.679629
63.893632	3131.504662	20.684647
63.708196	3127.616886	20.689664
63.904533	3135.098113	20.694682
64.173537	3130.179633	20.699699
64.179879	3142.181990	20.704717
64.109660	3155.105353	20.709735
64.455974	3159.113296	20.714752
64.278400	3167.543186	20.719770
64.403001	3161.801443	20.724787
64.419772	3158.724702	20.729805
64.335094	3166.530878	20.734823
64.769723	3165.803212	20.739840
64.346205	3172.273722	20.744858
64.943939	3186.986216	20.749875
65.227057	3187.664733	20.754893
64.675366	3192.529853	20.759911
64.947719	3192.045393	20.764928
64.839714	3195.130299	20.769946
64.820590	3196.840928	20.774963
65.046490	3196.145963	20.779981
65.281245	3211.777010	20.784999
65.486139	3216.488878	20.790016
65.469529	3221.734143	20.795034
65.712273	3213.041694	20.800051
65.663170	3216.268876	20.805069
65.573640	3221.361440	20.810087
65.878876	3213.770208	20.815104
65.698902	3218.864316	20.820122
66.037328	3214.891288	20.825139
66.045409	3219.776025	20.830157
65.661458	3229.522883	20.835175
65.924881	3224.210718	20.840192
65.633330	3224.692052	20.845210
65.883131	3230.997120	20.850227
66.077061	3247.363695	20.855245
66.022006	3246.441307	20.860263
66.285540	3249.685795	20.865280
66.293915	3243.921204	20.870298
66.290529	3244.126982	20.875315
66.165576	3255.629198	20.880333
66.305315	3269.921137	20.885351
66.714382	3269.806635	20.890368
66.435400	3275.329744	20.895386
66.277427	3274.524481	20.900403
66.899915	3273.991474	20.905421
66.645902	3301.503687	20.910439
66.659398	3296.842979	20.915456
66.921549	3303.711113	20.920474
66.699879	3298.648525	20.925491
67.288889	3305.348666	20.930509
67.126339	3305.775072	20.935527
67.289891	3322.320069	20.940544
67.526240	3329.630981	20.945562
67.090009	3332.401206	20.950579
67.575157	3325.482437	20.955597
67.621791	3331.396429	20.960615
67.541230	3322.830332	20.965632
67.822476	3329.828049	20.970650
67.592891	3338.452389	20.975667
67.708027	3330.022911	20.980685
67.719331	3344.732725	20.985703
67.919446	3351.301280	20.990720
67.667446	3354.020550	20.995738
67.789404	3355.923717	21.000755
68.011467	3360.554025	21.005773
67.932440	3359.622762	21.010791
68.080187	3370.744602	21.015808
68.183595	3378.066893	21.020826
68.235303	3395.882534	21.025843
68.356255	3389.308025	21.030861
68.238329	3389.323435	21.035879
68.122836	3383.189981	21.040896
69.154450	3399.718985	21.045914
68.729000	3416.454196	21.050931
69.078180	3420.098773	21.055949
68.596385	3425.581109	21.060967
68.767870	3421.122870	21.065984
68.879735	3420.950773	21.071002
68.699759	3419.192588	21.076019
68.846641	3416.846621	21.081037
68.950760	3436.661503	21.086055
69.069496	3436.018039	21.091072
69.191870	3443.084880	21.096090
68.883592	3453.463889	21.101107
69.324096	3447.214896	21.106125
69.208977	3469.873285	21.111143
69.433333	3461.786454	21.116160
69.467818	3467.380449	21.121178
69.326511	3478.408764	21.126195
69.510258	3487.533397	21.131213
69.687399	3494.670585	21.136231
69.939500	3491.891488	21.141248
70.122117	3497.711633	21.146266
69.852435	3499.824523	21.151283
70.190487	3522.304662	21.156301
70.028215	3528.592331	21.161319
69.996921	3531.523241	21.166336
70.150375	3532.304152	21.171354
70.328711	3535.126466	21.176371
70.229723	3527.446932	21.181389
70.938573	3551.163107	21.186407
70.736920	3550.797092	21.191424
70.933038	3553.806003	21.196442
70.663137	3557.424506	21.201459
70.954532	3556.551981	21.206477
70.830620	3553.550873	21.211495
70.735497	3556.551757	21.216512
70.967880	3560.031595	21.221530
71.133440	3572.564805	21.226547
71.280452	3579.596276	21.231565
71.125255	3580.936874	21.236583
71.518251	3580.446128	21.241600
71.506525	3576.565759	21.246618
71.141340	3581.512231	21.251635
71.763524	3588.254626	21.256653
71.701726	3591.180856	21.261671
71.646302	3604.051720	21.266688
71.607105	3595.172848	21.271706
71.667634	3604.338940	21.276723
71.708037	3600.238923	21.281741
71.859422	3615.009074	21.286759
72.170680	3622.150551	21.291776
72.361820	3628.269255	21.296794
72.236304	3637.253037	21.301811
72.389413	3632.090603	21.306829
72.582472	3631.801624	21.311847
72.296535	3635.593098	21.316864
72.656949	3634.978045	21.321882
72.550522	3635.537701	21.326899
72.467881	3630.484800	21.331917
72.468849	3642.317886	21.336935
72.670410	3660.990931	21.341952
72.679321	3653.512227	21.346970
72.252061	3658.013931	21.351987
72.559778	3663.890282	21.357005
72.819508	3678.400470	21.362023
73.030516	3689.310587	21.367040
73.003147	3694.238883	21.372058
73.291640	3699.603771	21.377075
73.035894	3692.889322	21.382093
73.305599	3703.076914	21.387111
73.373745	3719.703506	21.392128
73.964088	3723.136761	21.397146
73.315956	3729.664753	21.402163
73.678773	3721.464579	21.407181
73.592910	3723.712826	21.412199
73.537511	3744.667234	21.417216
73.935958	3745.914789	21.422234
73.906235	3748.911771	21.427251
73.772042	3753.626405	21.432269
73.785390	3756.540887	21.437287
73.885965	3768.891877	21.442304
74.099188	3773.877190	21.447322
74.055606	3785.325960	21.452339
74.355440	3793.918070	21.457357
74.515029	3795.278805	21.462375
74.534409	3808.608393	21.467392
74.949939	3806.734775	21.472410
74.839380	3816.413861	21.477427
74.978346	3812.995913	21.482445
74.738859	3814.220323	21.487463
74.875868	3811.932666	21.492480
75.070624	3809.326637	21.497498
75.493957	3828.672137	21.502515
75.224565	3832.972392	21.507533
75.628959	3832.609267	21.512551
75.432982	3837.579800	21.517568
75.496247	3831.642290	21.522586
75.684341	3838.935718	21.527603
75.801258	3840.227388	21.532621
75.818138	3839.075909	21.537639
75.956027	3833.319247	21.542656
75.928539	3836.985047	21.547674
75.658988	3841.174855	21.552691
75.782839	3852.575340	21.557709
76.067366	3851.751224	21.562727
75.719342	3857.679874	21.567744
76.056272	3856.093171	21.572762
76.038851	3859.107183	21.577779
76.003208	3879.509439	21.582797
76.381306	3888.925776	21.587815
76.526521	3886.071831	21.592832
76.705029	3887.278101	21.597850
76.564170	3898.682212	21.602867
76.561394	3890.602370	21.607885
76.707861	3898.303205	21.612903
76.590789	3917.152691	21.617920
76.898702	3916.656329	21.622938
76.586812	3919.890089	21.627955
76.759078	3915.169626	21.632973
76.633968	3926.975305	21.637991
77.199305	3945.544302	21.643008
77.319774	3932.884132	21.648026
77.436267	3941.662857	21.653043
77.563356	3939.310455	21.658061
77.525902	3939.572080	21.663079
77.730592	3945.575139	21.668096
77.869789	3953.261355	21.673114
77.804394	3960.594547	21.678131
77.785566	3960.212504	21.683149
77.924230	3962.113119	21.688167
77.709488	3964.362649	21.693184
78.092956	3950.199846	21.698202
77.902369	3964.509366	21.703219
78.040588	3985.711481	21.708237
78.272762	3985.558407	21.713255
78.478551	3982.300405	21.718272
78.518206	3992.972414	21.723290
78.536431	3985.277477	21.728307
78.549757	3988.880098	21.733325
78.635652	3999.339699	21.738343
78.300822	4018.690556	21.743360
78.795022	4015.131692	21.748378
78.437169	4015.446673	21.753395
78.684770	4034.321212	21.758413
78.957868	4041.165818	21.763431
78.761284	4048.626917	21.768448
79.127847	4052.010073	21.773466
79.388790	4060.687314	21.778483
79.489461	4076.706261	21.783501
79.665660	4079.753102	21.788519
79.465696	4083.269215	21.793536
79.519547	4079.892961	21.798554
79.331812	4086.140622	21.803571
79.652312	4095.588186	21.808589
79.670489	4101.263842	21.813607
79.593270	4115.760887	21.818624
79.842400	4109.958301	21.823642
79.664229	4123.407453	21.828659
80.285741	4134.761708	21.833677
80.352853	4138.046601	21.838695
80.143661	4140.964447	21.843712
80.154464	4142.976650	21.848730
80.363108	4154.992171	21.853747
80.201230	4165.184512	21.858765
80.553068	4165.268361	21.863783
80.492311	4168.248179	21.868800
80.802211	4189.268968	21.873818
80.953628	4203.345175	21.878835
80.907114	4208.453370	21.883853
80.615243	4199.039318	21.888871
80.859474	4201.324286	21.893888
81.418126	4216.163690	21.898906
81.292785	4221.359993	21.903923
80.848998	4229.759485	21.908941
81.366549	4232.604518	21.913959
81.257409	4240.080404	21.918976
81.475712	4254.831122	21.923994
81.211151	4279.852867	21.929011
81.253197	4266.049488	21.934029
81.743232	4277.901058	21.939047
81.927571	4298.711224	21.944064
81.957266	4288.413437	21.949082
82.226732	4296.322436	21.954099
82.374404	4300.980423	21.959117
82.141797	4295.489989	21.964135
82.229024	4320.204157	21.969152
82.479047	4322.254655	21.974170
82.533744	4328.107735	21.979187
82.345739	4325.896187	21.984205
82.379400	4326.935794	21.989223
82.664412	4341.433083	21.994240
82.820596	4360.966204	21.999258
82.941726	4352.128129	22.004275
83.001914	4357.702589	22.009293
82.925156	4358.001943	22.014311
82.990644	4355.974786	22.019328
83.357442	4367.466946	22.024346
83.330290	4371.527360	22.029363
83.502221	4382.260941	22.034381
83.394101	4374.636139	22.039399
83.397713	4376.258091	22.044416
83.530469	4374.996886	22.049434
83.385095	4394.350023	22.054451
83.450839	4404.869831	22.059469
83.682382	4403.422696	22.064487
83.618029	4412.094254	22.069504
83.977808	4424.995342	22.074522
84.218438	4430.639405	22.079539
83.991493	4435.870627	22.084557
84.342366	4431.046292	22.089575
84.308601	4448.548082	22.094592
84.716652	4458.465062	22.099610
84.736720	4463.998493	22.104627
84.517284	4472.407136	22.109645
85.064375	4466.289453	22.114663
84.459315	4473.944140	22.119680
84.508547	4481.950854	22.124698
84.791385	4487.957632	22.129715
84.850715	4491.395319	22.134733
85.115318	4488.913980	22.139751
84.816898	4512.495675	22.144768
85.039921	4518.458173	22.149786
85.375654	4521.009775	22.154803
85.436628	4531.650351	22.159821
85.784726	4541.374753	22.164839
85.807689	4550.752380	22.169856
85.970157	4555.367080	22.174874
85.623603	4549.114765	22.179891
85.572248	4554.268006	22.184909
85.749094	4555.603999	22.189927
86.010308	4571.251013	22.194944
86.019654	4587.736099	22.199962
86.156321	4576.730113	22.204979
85.885819	4603.132628	22.209997
85.993634	4610.865073	22.215015
86.448115	4614.635439	22.220032
86.355406	4615.363426	22.225050
86.542661	4631.419800	22.230067
86.357577	4643.270061	22.235085
86.442648	4639.330108	22.240103
86.661412	4661.950296	22.245120
86.366284	4671.447265	22.250138
86.865781	4673.392431	22.255155
87.104746	4688.152890	22.260173
87.286349	4691.325249	22.265191
87.353577	4703.161270	22.270208
87.108004	4716.097433	22.275226
87.838899	4716.617474	22.280243
87.739414	4724.470829	22.285261
87.919614	4725.740023	22.290279
87.820244	4720.948275	22.295296
87.946516	4721.528323	22.300314
88.230841	4717.506630	22.305331
88.280430	4726.725506	22.310349
88.542401	4739.367523	22.315367
88.452933	4752.235062	22.320384
88.304635	4754.095493	22.325402
88.613614	4750.650735	22.330419
88.716634	4756.843601	22.335437
88.759086	4752.935553	22.340455
88.529996	4754.524553	22.345472
88.614603	4760.934951	22.350490
88.847276	4760.879647	22.355507
88.815816	4766.490687	22.360525
89.151395	4777.072600	22.365543
88.981141	4784.305760	22.370560
89.305593	4782.244295	22.375578
89.881774	4786.696384	22.380595
89.516481	4787.934253	22.385613
89.700588	4788.243249	22.390631
89.759355	4806.084418	22.395648
89.704331	4809.369628	22.400666
90.182574	4808.022699	22.405683
89.876136	4814.866855	22.410701
90.100798	4809.427729	22.415719
90.104798	4806.848289	22.420736
90.208234	4817.993740	22.425754
90.296068	4818.377794	22.430771
90.019289	4831.416781	22.435789
90.553731	4826.008029	22.440807
90.223941	4823.676589	22.445824
90.157105	4823.178945	22.450842
90.574725	4846.311134	22.455859
90.649798	4864.083517	22.460877
90.419369	4859.353302	22.465895
90.584858	4873.992848	22.470912
90.384730	4890.874031	22.475930
90.814125	4888.316316	22.480947
90.565566	4910.211418	22.485965
90.872147	4918.635707	22.490983
91.216844	4923.619679	22.496000
91.437850	4944.121807	22.501018
91.393521	4954.918017	22.506035
91.052313	4959.147716	22.511053
91.442112	4977.123426	22.516071
91.851376	4985.500093	22.521088
91.580606	4995.081798	22.526106
91.415366	4994.422797	22.531123
91.494320	5014.925164	22.536141
91.821568	5019.697248	22.541159
91.717217	5034.069854	22.546176
92.137141	5057.953219	22.551194
92.262194	5065.045524	22.556211
92.572271	5070.120188	22.561229
92.615660	5079.968377	22.566247
92.415472	5092.042256	22.571264
91.964518	5093.741804	22.576282
92.417454	5106.840273	22.581299
92.601732	5124.368524	22.586317
93.020718	5145.209183	22.591335
93.078389	5150.042476	22.596352
92.855375	5153.600283	22.601370
93.014159	5155.961893	22.606387
93.107740	5188.103749	22.611405
93.193248	5193.144186	22.616423
93.358255	5193.550880	22.621440
93.423274	5215.804422	22.626458
93.773750	5220.159402	22.631475
93.644976	5231.991752	22.636493
93.695928	5244.054794	22.641511
94.062980	5245.020123	22.646528
93.954037	5251.230584	22.651546
94.110168	5262.538509	22.656563
94.259761	5277.076700	22.661581
94.164068	5283.761747	22.666599
94.454950	5290.196832	22.671616
94.457010	5307.554940	22.676634
94.832208	5304.860454	22.681651
94.530173	5314.873370	22.686669
94.729557	5310.331385	22.691687
95.050004	5321.866134	22.696704
94.860535	5336.687929	22.701722
95.008034	5332.078308	22.706739
94.974003	5346.897855	22.711757
95.279756	5358.488592	22.716775
95.557181	5362.722473	22.721792
95.380546	5367.292651	22.726810
95.711944	5372.341963	22.731827
95.314707	5386.274608	22.736845
95.357051	5400.570855	22.741863
96.077100	5401.007390	22.746880
96.064031	5418.008115	22.751898
96.388158	5420.687930	22.756915
96.332805	5434.475505	22.761933
96.233091	5428.648241	22.766951
96.358615	5440.156784	22.771968
96.329321	5452.352490	22.776986
96.551392	5455.108276	22.782003
96.595860	5463.655957	22.787021
96.459794	5485.357348	22.792039
97.198034	5491.813960	22.797056
96.854430	5501.457847	22.802074
97.050513	5500.309753	22.807091
97.062138	5510.100017	22.812109
97.082579	5522.382677	22.817127
97.314338	5521.607794	22.822144
97.107317	5531.706955	22.827162
97.522372	5538.163711	22.832179
97.393570	5553.257120	22.837197
97.337316	5558.139937	22.842215
97.864330	5575.333979	22.847232
97.607975	5579.190663	22.852250
98.056777	5593.518081	22.857267
98.288181	5613.154398	22.862285
97.906949	5615.404959	22.867303
98.201189	5615.134824	22.872320
97.992779	5642.356161	22.877338
98.392028	5651.950032	22.882355
98.632356	5652.026110	22.887373
98.804431	5669.351611	22.892391
99.074319	5679.676021	22.897408
98.517927	5683.898561	22.902426
98.979988	5686.058047	22.907443
98.869017	5702.528265	22.912461
98.851440	5706.278118	22.917479
99.381600	5722.969890	22.922496
99.569875	5738.941847	22.927514
99.640332	5744.328876	22.932531
99.565717	5746.323071	22.937549
99.732274	5749.207555	22.942567
99.688678	5770.310804	22.947584
99.874586	5773.460581	22.952602
99.787959	5769.288435	22.957619
99.915182	5783.827377	22.962637
100.284328	5799.897318	22.967655
100.372609	5806.676844	22.972672
100.131976	5813.125941	22.977690
100.476339	5823.950154	22.982707
100.891468	5831.985366	22.987725
100.719788	5828.776707	22.992743
100.675891	5842.130322	22.997760
100.622336	5850.605152	23.002778
101.237725	5855.502776	23.007795
100.838310	5844.864124	23.012813
100.943968	5872.772116	23.017831
101.418699	5876.154453	23.022848
101.321872	5891.738738	23.027866
101.358483	5892.023511	23.032883
101.379445	5906.263525	23.037901
101.547437	5920.199563	23.042919
101.585587	5920.831338	23.047936
101.810798	5938.944268	23.052954
101.981388	5941.045278	23.057971
101.905867	5961.336150	23.062989
101.840681	5964.597905	23.068007
102.169234	5973.862093	23.073024
102.420789	5991.102841	23.078042
102.407883	5985.722685	23.083059
102.677146	6006.515179	23.088077
102.740341	6008.443616	23.093095
102.404999	6008.609888	23.098112
102.494792	6035.276849	23.103130
102.726689	6050.083711	23.108147
102.787179	6059.563562	23.113165
102.667069	6072.683057	23.118183
103.241366	6078.417410	23.123200
103.244841	6095.728691	23.128218
103.372791	6112.243920	23.133235
103.597752	6114.374313	23.138253
103.961219	6132.396324	23.143271
103.895952	6137.744754	23.148288
104.108937	6152.052734	23.153306
104.149076	6146.995682	23.158323
104.448182	6150.929612	23.163341
104.321651	6167.895143	23.168359
104.299860	6174.076477	23.173376
104.357929	6187.543795	23.178394
104.120921	6194.866887	23.183411
104.352727	6203.650733	23.188429
104.601447	6210.935613	23.193447
105.157088	6224.018795	23.198464
105.150566	6236.489251	23.203482
104.826063	6240.445139	23.208499
105.191867	6253.583338	23.213517
105.277616	6269.502371	23.218535
105.671809	6278.320791	23.223552
105.368895	6279.138598	23.228570
105.157687	6290.100639	23.233587
105.733542	6292.090844	23.238605
105.705753	6304.700421	23.243623
106.204029	6308.334853	23.248640
106.401480	6325.451805	23.253658
106.305023	6323.591860	23.258675
106.710382	6325.286786	23.263693
106.808901	6337.933420	23.268711
106.993303	6328.478372	23.273728
106.585973	6338.997646	23.278746
106.568152	6358.222384	23.283763
107.216498	6354.626298	23.288781
106.941552	6359.025873	23.293799
106.944925	6371.832650	23.298816
107.227366	6378.487264	23.303834
107.406142	6386.922785	23.308851
107.053592	6392.796135	23.313869
106.835092	6409.346969	23.318887
107.034864	6414.972794	23.323904
107.200837	6447.301239	23.328922
107.475971	6453.369854	23.333939
107.432116	6456.571530	23.338957
107.307648	6469.837205	23.343975
107.668712	6487.111772	23.348992
107.847341	6504.623289	23.354010
107.887846	6517.247567	23.359027
108.242822	6531.928202	23.364045
107.897166	6538.570789	23.369063
108.412603	6551.357446	23.374080
108.723352	6568.848325	23.379098
108.597747	6579.033167	23.384115
109.053167	6580.177294	23.389133
109.018427	6598.123250	23.394151
108.966236	6612.002761	23.399168
108.924129	6614.279231	23.404186
109.097576	6631.876917	23.409203
109.281358	6634.373705	23.414221
109.330533	6650.002052	23.419239
109.390954	6666.048514	23.424256
109.092100	6676.503632	23.429274
109.598246	6698.459408	23.434291
110.140987	6700.757908	23.439309
109.647709	6717.219479	23.444327
110.165483	6725.987184	23.449344
110.254171	6738.386240	23.454362
110.188472	6742.667886	23.459379
110.954891	6756.251939	23.464397
110.399119	6770.084191	23.469415
110.596509	6776.414487	23.474432
110.694546	6784.891253	23.479450
110.593602	6803.561238	23.484467
110.637361	6804.757248	23.489485
110.808581	6827.027674	23.494503
111.142829	6832.856699	23.499520
110.948442	6849.561995	23.504538
111.310573	6863.004268	23.509555
111.590741	6875.502850	23.514573
111.533405	6890.463040	23.519591
111.735562	6891.972029	23.524608
111.594352	6915.377487	23.529626
111.801410	6936.846888	23.534643
111.958853	6935.070222	23.539661
112.034649	6954.198834	23.544679
112.205144	6959.936750	23.549696
112.346308	6983.010774	23.554714
112.054930	6998.203447	23.559731
112.670936	7008.581716	23.564749
112.757854	7026.022861	23.569767
113.014044	7039.374526	23.574784
113.059417	7045.264662	23.579802
113.045491	7057.553732	23.584819
113.256824	7057.416532	23.589837
113.466388	7087.153739	23.594855
113.362692	7087.343706	23.599872
113.894869	7091.307621	23.604890
113.595356	7117.626740	23.609907
114.036780	7129.232070	23.614925
113.753616	7134.630711	23.619943
114.108567	7148.740436	23.624960
114.321707	7150.342434	23.629978
113.848319	7160.619968	23.634995
114.390672	7176.351441	23.640013
114.621188	7192.879983	23.645031
114.646664	7206.874052	23.650048
114.887062	7214.132223	23.655066
114.937721	7230.007072	23.660083
114.846143	7229.513237	23.665101
114.900474	7249.179046	23.670119
114.925493	7251.883897	23.675136
115.342471	7270.416385	23.680154
115.254159	7282.663591	23.685171
115.305681	7287.605748	23.690189
115.544143	7312.224487	23.695207
115.645394	7318.560561	23.700224
115.775008	7328.768971	23.705242
115.873218	7342.470776	23.710259
116.072788	7336.959070	23.715277
116.109120	7349.369896	23.720295
116.309915	7366.888232	23.725312
116.762859	7371.524432	23.730330
116.547530	7389.846719	23.735347
116.754004	7394.723588	23.740365
116.747242	7397.180879	23.745383
117.071007	7404.511302	23.750400
117.346716	7416.524773	23.755418
117.214649	7438.764529	23.760435
117.383558	7428.411600	23.765453
117.435319	7444.226478	23.770471
117.260029	7467.262291	23.775488
118.210911	7467.643783	23.780506
118.139554	7471.244570	23.785523
118.011720	7479.236136	23.790541
118.181808	7486.868486	23.795559
118.177225	7498.673363	23.800576
118.226270	7499.148791	23.805594
118.080565	7527.894239	23.810611
118.461060	7525.192292	23.815629
118.213270	7545.695005	23.820647
118.420398	7559.973427	23.825664
118.302927	7570.365904	23.830682
117.905018	7601.607145	23.835699
118.783376	7612.358225	23.840717
118.634499	7629.031838	23.845735
119.162451	7651.752496	23.850752
119.348635	7656.531587	23.855770
119.437381	7683.169527	23.860787
119.601404	7690.515620	23.865805
119.729215	7700.481425	23.870823
119.462166	7729.091501	23.875840
119.545993	7724.027173	23.880858
120.017422	7750.595784	23.885875
119.840454	7765.206048	23.890893
119.698804	7785.196738	23.895911
120.067325	7804.523464	23.900928
120.108537	7811.244804	23.905946
119.937173	7832.206262	23.910963
120.575277	7851.970677	23.915981
121.004049	7873.924193	23.920999
120.770416	7894.156720	23.926016
121.018909	7893.161283	23.931034
121.344382	7912.936858	23.936051
121.524191	7925.117224	23.941069
121.655164	7939.038492	23.946087
121.562575	7951.908756	23.951104
121.657794	7964.534923	23.956122
121.978904	7981.476185	23.961139
122.154363	7988.009231	23.966157
122.579273	7992.211146	23.971175
122.268286	8009.333549	23.976192
122.382210	8024.163639	23.981210
122.620462	8021.171353	23.986227
122.842128	8041.929403	23.991245
122.560768	8060.609979	23.996263
122.564553	8063.173048	24.001280
122.844034	8081.576352	24.006298
122.892808	8096.729262	24.011315
122.423901	8113.418720	24.016333
123.268018	8128.882732	24.021351
122.964331	8158.383204	24.026368
123.363653	8164.729698	24.031386
123.417126	8187.187538	24.036403
123.648363	8191.375641	24.041421
124.083421	8212.119393	24.046439
123.734561	8222.542172	24.051456
124.018309	8235.413657	24.056474
123.796788	8248.758955	24.061491
124.205381	8257.336127	24.066509
124.555404	8274.276286	24.071527
124.648191	8291.127317	24.076544
124.725221	8311.011698	24.081562
124.722066	8322.100202	24.086579
124.757517	8331.351514	24.091597
124.903582	8354.281253	24.096615
125.562584	8366.974067	24.101632
125.595686	8374.287271	24.106650
125.627086	8392.284591	24.111667
125.910568	8399.697494	24.116685
125.673630	8410.254387	24.121703
125.544310	8423.777952	24.126720
125.907841	8443.042984	24.131738
126.329947	8451.157182	24.136755
126.600306	8453.770099	24.141773
126.277518	8477.992115	24.146791
126.461294	8489.313479	24.151808
126.528062	8492.463447	24.156826
127.027566	8512.597574	24.161843
126.759918	8519.901125	24.166861
126.864681	8540.425473	24.171879
127.147231	8559.128703	24.176896
127.524777	8569.002178	24.181914
127.364645	8590.613114	24.186931
127.586842	8595.759357	24.191949
127.900207	8609.368404	24.196967
127.469930	8624.363164	24.201984
128.127019	8637.902596	24.207002
128.255059	8651.275503	24.212019
128.507108	8656.038221	24.217037
128.727448	8676.891906	24.222055
128.547300	8677.933684	24.227072
128.656251	8697.150463	24.232090
128.537504	8707.297512	24.237107
128.369182	8712.738604	24.242125
128.777618	8738.352392	24.247143
129.034252	8758.142812	24.252160
129.134274	8766.951684	24.257178
129.292015	8789.876974	24.262195
129.569648	8813.711736	24.267213
129.750259	8816.809194	24.272231
129.807375	8830.057581	24.277248
129.805315	8841.954477	24.282266
129.910555	8855.533167	24.287283
129.943993	8872.024626	24.292301
130.157341	8891.878801	24.297319
129.946892	8916.472128	24.302336
130.341570	8914.576019	24.307354
130.561036	8937.826489	24.312371
130.771274	8954.479758	24.317389
130.906379	8970.428114	24.322407
130.653778	8985.745783	24.327424
131.085952	9000.084776	24.332442
131.274518	9016.826742	24.337459
131.056662	9037.386397	24.342477
131.583954	9051.435844	24.347495
131.452865	9068.060601	24.352512
132.064663	9074.348862	24.357530
131.989028	9104.695985	24.362547
132.143333	9112.871374	24.367565
132.226535	9113.136270	24.372583
132.054343	9141.086411	24.377600
132.013468	9149.453417	24.382618
132.694725	9169.297727	24.387635
132.538908	9174.774881	24.392653
133.044387	9187.274459	24.397671
132.858005	9212.123304	24.402688
133.056429	9218.574254	24.407706
133.355102	9238.885869	24.412723
133.233913	9246.845579	24.417741
133.745115	9267.174446	24.422759
133.616243	9281.292138	24.427776
133.753936	9279.006859	24.432794
133.996042	9294.247276	24.437811
133.973734	9303.381828	24.442829
134.367076	9321.522253	24.447847
134.156192	9339.053274	24.452864
134.564744	9346.686919	24.457882
134.563321	9360.737344	24.462899
134.810285	9380.182634	24.467917
135.214433	9394.273736	24.472935
134.983480	9414.892690	24.477952
135.385830	9404.956747	24.482970
135.173926	9423.024754	24.487987
135.542288	9432.240244	24.493005
135.723599	9453.650292	24.498023
135.676179	9467.824825	24.503040
135.648786	9473.424027	24.508058
136.002690	9488.214531	24.513075
135.858321	9505.268000	24.518093
136.484581	9525.705418	24.523111
136.347801	9536.360920	24.528128
136.596751	9555.907118	24.533146
136.743290	9561.204406	24.538163
136.729073	9584.353371	24.543181
137.113397	9587.775826	24.548199
136.894537	9603.906474	24.553216
137.262491	9628.504842	24.558234
137.165637	9642.611476	24.563251
137.306016	9661.514903	24.568269
137.543300	9673.772661	24.573287
137.701856	9700.437286	24.578304
137.973104	9704.729972	24.583322
137.844428	9726.586729	24.588339
137.827474	9739.790533	24.593357
138.496019	9756.618994	24.598375
138.018012	9772.585156	24.603392
138.377141	9789.569474	24.608410
138.520751	9806.723341	24.613427
138.617177	9828.945941	24.618445
139.000499	9839.305429	24.623463
138.760116	9864.643527	24.628480
138.842217	9878.466552	24.633498
139.143512	9900.833956	24.638515
139.181873	9920.549298	24.643533
139.264758	9933.661820	24.648551
139.720622	9963.194545	24.653568
140.067386	9963.797054	24.658586
139.921922	9976.395987	24.663603
139.927912	10000.890526	24.668621
140.071190	10012.500173	24.673639
140.922805	10030.048514	24.678656
141.131066	10055.818616	24.683674
141.154759	10063.323405	24.688691
140.991551	10081.428622	24.693709
141.312830	10093.174620	24.698727
141.318556	10106.630884	24.703744
141.236384	10101.434045	24.708762
141.380896	10131.994628	24.713779
141.534420	10139.605405	24.718797
141.758381	10156.248125	24.723815
141.900486	10169.351534	24.728832
141.933215	10191.549812	24.733850
142.110496	10200.902973	24.738867
142.213186	10226.876142	24.743885
142.371148	10243.601902	24.748903
142.482499	10252.040276	24.753920
142.557356	10268.576999	24.758938
142.740965	10286.476520	24.763955
142.752165	10300.765643	24.768973
142.883348	10319.008102	24.773991
142.847657	10340.775227	24.779008
143.284834	10356.086991	24.784026
143.445279	10375.985765	24.789043
143.445631	10392.269040	24.794061
143.826060	10402.010423	24.799079
143.619813	10439.585603	24.804096
143.853419	10458.787824	24.809114
144.128753	10466.278610	24.814131
144.185455	10484.435016	24.819149
144.425874	10507.788358	24.824167
144.245986	10525.410358	24.829184
144.489558	10540.102153	24.834202
144.996484	10548.488161	24.839219
145.177917	10570.316262	24.844237
145.603075	10585.049110	24.849255
145.942830	10590.913195	24.854272
145.915959	10608.530246	24.859290
146.014457	10621.261898	24.864307
145.733188	10634.981374	24.869325
146.519762	10647.100038	24.874343
146.782266	10654.987604	24.879360
146.702971	10666.304141	24.884378
147.386961	10678.862010	24.889395
147.313483	10686.896952	24.894413
147.708832	10688.657012	24.899431
147.812001	10688.410437	24.904448
147.416082	10703.985621	24.909466
147.573257	10710.516174	24.914483
147.650672	10716.159322	24.919501
147.824326	10730.849591	24.924519
148.140896	10753.963965	24.929536
148.141569	10752.899849	24.934554
148.300097	10767.005209	24.939571
148.096918	10783.873285	24.944589
148.264136	10798.586718	24.949607
148.458379	10819.001667	24.954624
148.515633	10834.771199	24.959642
148.765643	10849.020168	24.964659
149.011611	10878.205154	24.969677
149.275939	10885.022110	24.974695
149.256807	10898.511254	24.979712
149.333834	10914.997686	24.984730
149.124055	10928.358840	24.989747
149.431630	10954.048310	24.994765
149.677250	10971.083061	24.999783
149.701705	10996.769580	25.004800
149.693747	11018.321586	25.009818
150.119119	11026.651118	25.014835
150.475990	11053.766556	25.019853
150.344726	11056.155422	25.024871
150.455046	11084.869393	25.029888
150.453314	11094.611015	25.034906
150.939228	11116.142597	25.039923
150.568632	11136.955831	25.044941
151.158866	11164.009607	25.049959
151.434491	11184.431149	25.054976
151.467427	11194.227387	25.059994
151.764546	11214.923467	25.065011
151.409272	11228.648654	25.070029
151.991305	11240.414517	25.075047
151.870616	11261.056114	25.080064
151.812121	11278.741900	25.085082
152.147697	11297.483774	25.090099
152.126157	11325.211478	25.095117
152.717620	11339.966231	25.100135
152.704885	11360.578394	25.105152
152.685184	11379.915972	25.110170
152.968326	11396.016875	25.115187
152.687932	11422.743244	25.120205
153.194863	11435.660917	25.125223
153.233684	11462.173132	25.130240
153.554829	11495.003897	25.135258
153.907482	11506.581667	25.140275
154.148140	11521.988327	25.145293
154.324800	11546.957059	25.150311
154.363870	11557.977711	25.155328
154.120154	11577.950550	25.160346
154.716525	11589.755437	25.165363
154.732366	11621.320647	25.170381
154.555108	11636.019234	25.175399
154.927920	11649.475931	25.180416
155.088985	11677.579733	25.185434
155.410581	11694.950586	25.190451
155.580198	11717.088169	25.195469
155.676081	11731.207225	25.200487
156.199333	11755.190404	25.205504
155.927680	11782.844286	25.210522
156.340206	11794.406538	25.215539
156.379892	11806.125099	25.220557
156.595660	11823.556859	25.225575
156.374951	11845.269451	25.230592
156.466386	11874.495982	25.235610
156.922533	11896.052068	25.240627
157.147492	11918.020172	25.245645
157.015522	11938.730590	25.250663
157.662399	11951.702480	25.255680
157.675742	11977.341552	25.260698
157.637719	11999.913034	25.265715
157.858023	12018.342120	25.270733
157.850232	12042.560434	25.275751
158.232668	12055.842237	25.280768
158.185769	12082.671900	25.285786
158.668353	12087.130968	25.290803
158.412376	12109.553575	25.295821
158.785553	12126.793592	25.300839
158.743196	12157.389899	25.305856
159.083213	12178.197157	25.310874
159.509361	12189.302795	25.315891
159.614898	12215.600358	25.320909
159.599563	12230.703501	25.325927
160.106480	12255.896161	25.330944
159.839383	12276.782851	25.335962
160.450837	12285.873247	25.340979
160.462962	12295.745946	25.345997
160.528803	12320.050972	25.351015
160.898303	12337.585436	25.356032
161.023793	12357.390732	25.361050
161.299058	12374.706313	25.366067
161.402261	12396.466685	25.371085
161.677182	12406.547740	25.376103
161.899497	12414.540235	25.381120
161.988802	12440.108034	25.386138
162.201588	12454.095633	25.391155
162.337617	12471.243646	25.396173
162.601271	12478.803382	25.401191
163.122115	12480.013435	25.406208
162.717478	12507.392370	25.411226
163.020055	12509.713450	25.416243
163.057011	12526.466513	25.421261
163.080286	12540.597548	25.426279
163.250623	12549.100344	25.431296
163.444178	12566.855215	25.436314
163.250422	12583.691840	25.441331
163.416447	12602.319472	25.446349
163.513829	12620.730508	25.451367
164.161462	12634.378538	25.456384
164.150023	12659.466630	25.461402
164.189693	12685.355167	25.466419
164.547902	12704.069632	25.471437
164.170443	12717.565686	25.476455
164.635581	12737.457116	25.481472
164.401749	12751.985431	25.486490
164.531505	12779.328406	25.491507
164.517551	12798.950746	25.496525
164.796808	12833.138826	25.501543
165.022553	12844.345720	25.506560
165.352931	12881.671161	25.511578
165.479481	12911.143267	25.516595
166.038265	12932.870776	25.521613
166.138317	12954.727020	25.526631
166.480706	12971.246306	25.531648
166.529847	13002.612811	25.536666
166.442479	13009.068788	25.541683
166.603408	13038.109383	25.546701
167.007630	13061.187591	25.551719
167.037115	13078.962330	25.556736
167.379649	13114.044177	25.561754
167.400121	13132.281440	25.566771
167.577318	13153.418443	25.571789
167.436785	13166.394528	25.576807
167.962708	13194.743430	25.581824
168.085942	13219.498523	25.586842
168.262794	13219.695123	25.591859
168.773191	13241.616887	25.596877
169.068284	13259.138599	25.601895
169.804237	13263.893002	25.606912
169.502830	13279.051270	25.611930
169.855492	13311.662351	25.616947
169.914477	13320.343995	25.621965
169.928883	13334.650701	25.626983
170.312256	13343.755236	25.632000
170.113690	13357.346878	25.637018
170.373767	13388.147272	25.642035
170.677174	13395.473770	25.647053
170.522089	13413.132469	25.652071
170.772002	13415.212430	25.657088
170.909489	13453.876631	25.662106
171.215807	13454.097163	25.667123
171.478256	13473.945329	25.672141
171.460615	13494.086879	25.677159
171.797661	13508.248429	25.682176
171.980451	13529.988157	25.687194
172.204082	13549.722479	25.692212
172.013623	13557.379053	25.697229
171.813008	13585.990790	25.702247
172.404701	13593.985918	25.707264
172.391855	13623.600972	25.712282
172.670276	13642.565718	25.717300
173.058868	13668.230396	25.722317
172.826835	13696.490360	25.727335
173.545202	13707.958502	25.732352
173.282789	13731.006166	25.737370
173.370623	13746.675435	25.742388
173.675430	13762.563370	25.747405
173.922489	13780.857340	25.752423
174.452677	13788.931665	25.757440
174.412719	13806.585323	25.762458
174.575543	13819.425902	25.767476
174.925318	13836.841680	25.772493
175.036012	13851.989529	25.777511
174.840528	13864.977857	25.782528
174.989716	13888.169661	25.787546
175.354192	13915.382756	25.792564
175.840515	13931.087649	25.797581
175.718690	13949.474311	25.802599
175.992282	13967.397965	25.807616
175.606754	13982.421539	25.812634
175.599772	14005.236873	25.817652
176.336775	14025.292341	25.822669
176.188233	14048.275176	25.827687
176.562905	14066.454685	25.832704
176.604290	14097.915795	25.837722
177.064857	14113.091151	25.842740
177.468626	14127.912233	25.847757
177.019558	14158.414413	25.852775
177.549598	14177.299216	25.857792
177.899624	14205.790876	25.862810
177.790720	14224.251574	25.867828
177.886132	14229.697146	25.872845
178.045487	14254.836378	25.877863
178.562341	14283.819956	25.882880
178.507253	14299.818411	25.887898
179.046950	14327.241505	25.892916
179.306022	14337.373444	25.897933
179.108406	14357.828336	25.902951
179.563493	14382.261349	25.907968
179.825787	14397.303769	25.912986
179.688211	14428.338683	25.918004
179.984693	14440.763969	25.923021
180.041085	14458.065211	25.928039
180.621329	14464.593948	25.933056
180.913329	14485.986049	25.938074
180.675516	14505.651533	25.943092
180.895473	14530.829008	25.948109
181.076104	14550.694272	25.953127
181.350748	14569.313130	25.958144
181.444678	14596.790656	25.963162
181.711082	14612.615837	25.968180
181.817284	14627.329173	25.973197
181.695427	14649.844293	25.978215
182.098103	14659.802312	25.983232
182.612754	14684.646425	25.988250
182.497756	14704.365511	25.993268
182.830062	14722.476486	25.998285
183.048959	14748.924021	26.003303
183.226123	14762.659926	26.008320
183.451973	14789.766498	26.013338
182.982674	14804.156401	26.018356
183.609349	14820.443264	26.023373
183.878042	14847.761125	26.028391
184.259459	14868.116374	26.033408
184.171911	14880.058891	26.038426
184.612112	14900.872387	26.043444
184.815238	14925.664553	26.048461
184.700798	14941.694950	26.053479
184.697371	14957.398459	26.058496
185.053948	14973.459315	26.063514
185.155583	15001.381530	26.068532
185.733999	15015.452697	26.073549
185.835603	15048.579822	26.078567
185.971832	15063.651991	26.083584
185.770129	15077.059007	26.088602
185.201519	15098.346589	26.093620
186.312948	15121.269128	26.098637
185.710236	15156.777591	26.103655
186.347216	15173.893773	26.108672
187.039857	15197.077827	26.113690
187.320021	15206.603688	26.118708
187.423310	15230.151725	26.123725
187.344653	15246.584192	26.128743
187.420909	15268.933195	26.133760
187.922922	15290.593335	26.138778
188.346652	15310.522370	26.143796
188.444610	15321.599144	26.148813
188.234735	15342.991870	26.153831
189.092893	15353.895877	26.158848
189.537450	15366.450168	26.163866
189.375171	15374.905269	26.168884
189.794462	15382.084888	26.173901
189.959479	15394.638774	26.178919
190.054951	15416.899664	26.183936
190.375632	15434.940494	26.188954
190.297337	15442.722373	26.193972
190.399411	15465.917156	26.198989
190.233091	15494.021034	26.204007
190.683781	15502.026426	26.209024
190.587011	15518.910450	26.214042
190.379641	15543.215011	26.219060
190.972865	15567.760551	26.224077
191.177602	15603.269675	26.229095
191.141319	15621.707707	26.234112
191.675376	15636.493758	26.239130
191.609407	15674.461580	26.244148
191.969545	15684.925823	26.249165
192.322434	15704.749506	26.254183
192.804003	15734.764129	26.259200
192.367136	15745.934409	26.264218
192.604448	15773.062685	26.269236
193.131995	15795.306858	26.274253
193.417039	15819.512517	26.279271
193.552928	15842.986713	26.284288
193.728960	15866.078798	26.289306
193.921812	15875.236502	26.294324
193.758671	15890.763656	26.299341
193.871173	15919.882544	26.304359
193.935587	15938.930472	26.309376
194.158942	15966.127533	26.314394
194.580924	16002.648801	26.319412
195.232303	16017.164092	26.324429
194.697401	16051.523382	26.329447
195.263400	16065.853102	26.334464
195.292251	16090.048702	26.339482
195.535393	16121.162520	26.344500
195.850802	16142.268542	26.349517
196.184346	16163.738128	26.354535
196.303056	16183.444227	26.359552
196.609982	16203.739920	26.364570
196.808626	16233.452213	26.369588
197.299129	16245.194472	26.374605
197.442090	16265.670683	26.379623
197.379136	16288.393270	26.384640
197.674491	16303.773124	26.389658
197.691857	16326.732694	26.394676
198.489554	16347.466488	26.399693
198.239780	16359.735393	26.404711
198.495703	16390.572855	26.409728
198.874854	16394.527999	26.414746
199.101916	16422.249435	26.419764
199.153954	16426.208454	26.424781
198.988023	16450.090743	26.429799
199.283425	16469.450445	26.434816
199.549653	16485.463551	26.439834
199.393410	16510.535157	26.444852
199.847740	16520.517639	26.449869
200.012707	16556.325335	26.454887
199.945017	16568.167872	26.459904
200.126876	16598.252905	26.464922
200.242542	16618.484242	26.469940
200.732290	16642.251415	26.474957
200.936243	16666.496111	26.479975
200.859554	16702.120836	26.484992
201.213743	16723.234054	26.490010
201.194535	16753.148680	26.495028
201.718003	16770.107194	26.500045
201.936832	16799.949857	26.505063
202.287102	16822.478835	26.510080
202.832783	16829.721321	26.515098
202.549770	16861.326216	26.520116
203.244204	16873.763385	26.525133
203.493981	16893.983476	26.530151
203.198696	16925.710425	26.535168
203.544502	16939.819448	26.540186
203.415472	16971.299325	26.545204
203.728766	16984.023693	26.550221
203.967378	17004.510971	26.555239
204.238072	17035.599837	26.560256
205.006111	17047.583382	26.565274
204.825104	17082.969304	26.570292
205.090615	17096.149754	26.575309
205.244016	17114.824820	26.580327
205.522725	17140.170232	26.585344
205.932579	17158.369273	26.590362
206.038167	17181.840369	26.595380
206.130948	17189.791986	26.600397
206.287393	17218.447947	26.605415
206.283363	17239.857905	26.610432
206.787869	17257.922184	26.615450
206.845279	17284.559593	26.620468
207.049198	17306.960449	26.625485
207.376620	17328.501780	26.630503
207.208320	17357.752110	26.635520
207.410779	17376.217588	26.640538
207.642444	17409.536865	26.645556
207.701997	17428.890255	26.650573
208.081992	17456.260714	26.655591
208.325700	17487.133425	26.660608
208.898611	17511.289793	26.665626
208.798855	17534.130161	26.670644
209.067402	17556.672797	26.675661
209.530993	17577.529749	26.680679
209.199872	17602.074233	26.685696
209.483228	17615.353320	26.690714
209.398393	17647.768662	26.695732
209.928012	17677.535561	26.700749
210.019132	17707.453328	26.705767
209.940182	17742.022148	26.710784
210.341658	17766.502611	26.715802
210.671375	17796.964342	26.720820
210.784878	17828.388660	26.725837
211.077215	17861.629717	26.730855
211.206069	17896.204162	26.735872
211.914170	17914.363509	26.740890
211.944237	17937.847350	26.745908
212.305668	17952.447431	26.750925
212.718134	17970.811083	26.755943
212.631513	17996.726565	26.760960
213.196292	18014.036641	26.765978
213.422495	18042.228028	26.770996
213.497716	18056.171778	26.776013
213.823084	18069.848918	26.781031
213.725628	18080.370356	26.786048
214.349523	18097.500671	26.791066
214.436840	18118.960463	26.796084
214.643169	18130.558864	26.801101
214.754350	18152.065493	26.806119
214.820892	18175.228028	26.811136
215.086590	18195.775498	26.816154
215.512041	18220.315953	26.821172
215.473377	18239.439151	26.826189
215.892696	18263.178285	26.831207
215.690624	18286.901077	26.836224
215.734353	18304.274086	26.841242
216.224159	18325.866899	26.846260
216.574919	18357.968797	26.851277
216.859664	18387.345547	26.856295
216.593598	18406.226556	26.861312
216.828527	18434.328697	26.866330
217.310707	18463.680950	26.871348
217.652674	18476.951446	26.876365
218.356198	18500.671618	26.881383
218.053817	18512.267810	26.886400
218.520585	18537.528727	26.891418
218.770532	18559.595297	26.896436
219.145327	18587.985316	26.901453
219.334686	18600.755433	26.906471
219.335428	18620.119221	26.911488
219.498319	18624.124501	26.916506
219.911117	18648.711703	26.921524
219.994802	18676.155572	26.926541
220.631296	18695.337708	26.931559
220.362024	18716.335965	26.936576
220.546599	18735.892191	26.941594
220.961145	18760.416082	26.946612
221.211279	18779.115500	26.951629
221.377893	18808.884141	26.956647
221.593801	18821.264858	26.961664
222.037668	18838.998951	26.966682
221.690890	18868.677529	26.971700
221.748928	18893.213213	26.976717
222.873163	18902.747663	26.981735
222.897826	18927.402339	26.986752
223.059542	18943.620225	26.991770
223.274523	18967.284827	26.996788
223.270667	18985.348223	27.001805
223.645405	19011.300181	27.006823
223.717130	19044.028164	27.011840
224.180263	19060.306333	27.016858
224.136444	19082.665911	27.021876
224.313450	19102.369001	27.026893
224.833903	19128.273016	27.031911
224.654653	19155.398629	27.036928
224.917572	19174.462861	27.041946
225.264193	19191.309048	27.046964
225.301178	19215.532539	27.051981
225.734052	19244.129225	27.056999
226.104314	19272.186100	27.062016
226.151733	19293.969331	27.067034
226.223000	19315.830983	27.072052
226.584189	19339.327818	27.077069
226.798219	19363.618526	27.082087
226.831246	19393.187855	27.087104
226.869061	19413.822852	27.092122
227.027156	19439.645051	27.097140
227.330023	19475.875620	27.102157
227.760982	19500.814859	27.107175
227.703989	19531.737918	27.112192
228.137908	19555.899647	27.117210
228.028307	19585.984417	27.122228
228.246905	19607.570592	27.127245
229.040632	19631.151651	27.132263
228.736888	19674.149479	27.137280
229.067258	19690.088841	27.142298
229.345225	19715.279771	27.147316
229.816999	19755.439514	27.152333
229.960114	19766.018943	27.157351
229.975570	19796.880524	27.162368
230.365564	19823.842068	27.167386
230.734831	19854.123909	27.172404
230.501262	19879.534185	27.177421
230.955771	19912.879693	27.182439
231.128173	19945.448092	27.187456
231.264193	19975.147482	27.192474
231.311888	20005.593660	27.197492
231.624710	20043.997171	27.202509
232.285565	20070.032075	27.207527
232.533153	20102.639502	27.212544
232.909360	20129.976400	27.217562
233.278447	20147.129484	27.222580
233.343873	20177.680561	27.227597
233.903098	20183.942863	27.232615
234.190651	20214.187516	27.237632
234.445809	20228.660631	27.242650
235.098394	20241.043340	27.247668
234.991426	20268.639353	27.252685
235.292474	20289.252988	27.257703
235.649035	20307.684464	27.262720
235.981033	20321.463238	27.267738
236.400191	20341.976288	27.272756
236.756826	20351.480067	27.277773
236.964627	20362.112866	27.282791
237.154091	20378.352867	27.287808
237.100925	20391.547563	27.292826
237.587867	20406.982790	27.297844
237.423487	20427.271430	27.302861
238.494321	20444.163202	27.307879
238.435898	20455.659138	27.312896
238.545348	20471.444195	27.317914
238.928674	20486.497663	27.322932
238.704605	20495.675473	27.327949
239.415125	20506.419147	27.332967
239.406582	20520.358820	27.337984
239.543202	20534.515859	27.343002
240.157735	20548.901321	27.348020
240.103796	20562.355304	27.353037
240.036919	20577.902699	27.358055
239.957303	20601.571196	27.363072
240.168285	20616.563305	27.368090
240.879585	20643.330318	27.373108
240.878037	20671.775999	27.378125
241.414426	20694.185523	27.383143
241.351719	20720.675835	27.388160
241.642490	20741.721207	27.393178
241.799606	20759.457734	27.398196
241.701449	20782.282685	27.403213
242.151838	20803.138837	27.408231
242.007513	20822.521206	27.413248
242.320305	20847.095245	27.418266
242.492749	20874.458781	27.423284
242.846407	20908.794821	27.428301
242.691502	20940.765341	27.433319
243.270598	20983.191749	27.438336
243.588639	21008.201142	27.443354
243.682566	21029.113376	27.448372
243.572725	21064.804952	27.453389
244.214008	21095.140871	27.458407
244.335194	21118.746938	27.463424
244.416895	21146.327259	27.468442
245.033567	21166.538531	27.473460
244.995703	21200.121320	27.478477
245.689590	21223.182859	27.483495
245.595816	21253.950101	27.488512
245.870102	21278.195825	27.493530
246.646740	21298.824474	27.498548
246.685652	21332.060574	27.503565
247.147389	21355.101769	27.508583
247.098415	21380.263907	27.513600
247.440048	21404.170667	27.518618
247.831424	21422.016420	27.523636
247.610687	21441.221806	27.528653
248.416827	21470.786880	27.533671
248.451884	21502.734868	27.538688
248.850002	21515.884893	27.543706
249.182119	21536.975185	27.548724
249.573970	21572.949249	27.553741
249.691994	21585.315452	27.558759
250.213988	21611.494208	27.563776
249.998631	21633.220093	27.568794
250.309009	21643.578449	27.573812
250.704808	21677.233123	27.578829
250.957411	21700.933035	27.583847
250.956239	21717.058672	27.588864
251.341534	21758.866280	27.593882
251.523532	21769.712400	27.598900
251.574265	21805.879337	27.603917
251.837210	21829.040688	27.608935
251.992144	21859.302321	27.613952
251.861878	21881.836587	27.618970
252.390070	21906.991122	27.623988
252.463114	21942.466066	27.629005
253.052435	21970.290273	27.634023
252.930573	21995.085482	27.639040
253.242343	22037.385425	27.644058
253.803369	22068.449439	27.649076
254.467582	22086.423660	27.654093
254.923474	22114.123638	27.659111
254.730923	22139.511434	27.664128
255.472830	22172.247048	27.669146
255.922759	22184.662733	27.674164
255.642033	22199.758348	27.679181
255.809491	22227.263552	27.684199
256.678139	22251.025588	27.689216
256.525094	22278.612666	27.694234
256.777742	22295.811137	27.699252
256.947595	22328.598710	27.704269
257.379625	22345.535324	27.709287
257.614518	22365.460092	27.714304
257.562979	22390.604956	27.719322
258.143059	22411.872180	27.724340
258.250124	22431.595875	27.729357
258.517357	22451.130207	27.734375
259.031742	22475.434569	27.739392
259.062068	22502.708878	27.744410
259.302571	22525.988301	27.749428
259.572533	22553.996056	27.754445
259.900731	22583.176379	27.759463
260.240085	22601.189321	27.764480
260.383357	22627.359239	27.769498
260.762787	22645.365943	27.774516
261.157144	22670.378120	27.779533
261.069913	22687.617536	27.784551
261.338864	22719.366546	27.789568
261.741790	22735.385474	27.794586
261.982066	22744.984465	27.799604
262.314832	22776.394980	27.804621
262.469811	22797.583873	27.809639
262.905452	22824.896235	27.814656
262.918079	22839.567235	27.819674
263.301441	22862.578229	27.824692
263.268911	22887.847124	27.829709
263.338534	22920.531311	27.834727
263.733056	22943.294205	27.839744
263.736089	22973.726670	27.844762
264.193553	22991.683549	27.849780
264.206362	23026.563227	27.854797
264.433544	23054.641579	27.859815
264.757762	23095.229335	27.864832
264.809108	23123.967246	27.869850
265.012342	23151.297505	27.874868
265.421462	23192.232351	27.879885
265.460622	23229.913975	27.884903
265.601002	23256.091491	27.889920
266.011319	23298.922131	27.894938
266.505305	23332.779083	27.899956
266.531804	23378.640059	27.904973
267.062832	23406.134171	27.909991
267.821188	23447.217048	27.915008
267.338694	23478.364587	27.920026
267.899215	23513.096120	27.925044
268.317864	23545.486521	27.930061
268.415970	23593.428461	27.935079
268.701509	23601.023872	27.940096
269.309420	23635.918817	27.945114
269.378049	23675.738918	27.950132
269.481357	23705.777628	27.955149
269.903927	23738.477376	27.960167
270.553242	23762.149195	27.965184
270.540174	23805.281061	27.970202
270.910061	23839.417407	27.975220
271.302807	23858.693320	27.980237
271.213562	23892.383490	27.985255
271.976978	23921.238498	27.990272
272.227636	23952.316158	27.995290
272.576904	23984.193626	28.000308
273.045260	24021.771591	28.005325
273.182083	24044.361249	28.010343
273.637471	24060.518372	28.015360
273.375850	24091.569066	28.020378
273.815526	24110.863149	28.025396
274.383084	24139.490055	28.030413
273.930244	24167.657539	28.035431
274.614750	24196.411555	28.040448
274.670371	24228.822015	28.045466
275.320532	24249.549386	28.050484
275.405548	24288.104232	28.055501
275.523759	24317.490613	28.060519
276.032344	24344.060559	28.065536
276.098719	24384.324789	28.070554
276.545106	24400.281370	28.075572
277.032648	24433.370208	28.080589
277.520220	24458.686003	28.085607
277.531358	24480.196232	28.090624
277.848799	24513.381364	28.095642
278.158692	24535.521051	28.100660
278.527639	24558.706887	28.105677
278.318152	24581.060697	28.110695
279.031668	24609.690689	28.115712
278.776231	24650.220731	28.120730
279.172180	24680.057067	28.125748
279.187495	24715.501741	28.130765
279.405619	24739.659362	28.135783
279.985460	24766.901232	28.140800
280.474869	24805.918256	28.145818
280.634231	24832.518278	28.150836
280.616370	24862.735694	28.155853
280.933168	24883.503304	28.160871
281.253818	24919.286009	28.165888
281.193740	24956.784192	28.170906
281.613509	24984.639169	28.175924
282.341685	25022.766044	28.180941
282.077120	25064.183114	28.185959
282.505235	25084.352075	28.190976
282.756671	25124.835267	28.195994
283.100649	25145.257621	28.201012
284.045904	25172.942064	28.206029
284.415364	25196.198073	28.211047
284.549490	25217.127360	28.216064
284.654445	25254.176815	28.221082
285.196251	25274.366075	28.226100
285.518951	25300.062669	28.231117
285.988410	25336.145117	28.236135
286.257929	25346.688758	28.241152
286.470956	25382.343788	28.246170
286.343859	25412.427462	28.251188
286.916495	25436.549345	28.256205
287.090471	25464.152774	28.261223
287.532883	25482.967436	28.266240
287.992626	25505.274314	28.271258
287.803723	25532.732444	28.276276
288.598564	25558.241648	28.281293
288.621384	25579.536343	28.286311
289.042438	25607.000144	28.291328
289.200172	25637.728409	28.296346
289.482364	25659.582954	28.301364
289.766687	25686.821804	28.306381
289.800492	25712.937058	28.311399
290.687386	25735.031917	28.316416
290.584563	25772.500390	28.321434
290.677344	25795.971074	28.326452
291.028890	25830.221114	28.331469
291.366373	25866.451584	28.336487
291.548072	25886.975952	28.341504
292.001541	25917.563515	28.346522
292.610598	25946.034814	28.351540
292.961935	25971.708817	28.356557
293.209096	25994.409780	28.361575
293.666521	26023.094543	28.366592
293.471911	26054.668645	28.371610
293.986794	26085.461725	28.376628
294.232150	26108.346382	28.381645
294.041839	26145.039236	28.386663
294.331953	26164.997052	28.391680
294.735772	26200.806922	28.396698
295.141682	26234.796326	28.401716
295.352941	26263.077581	28.406733
295.855108	26291.237463	28.411751
296.365206	26309.966452	28.416768
296.561141	26340.392751	28.421786
296.861215	26364.229792	28.426804
297.296726	26390.036505	28.431821
297.333381	26433.817184	28.436839
297.425437	26452.744515	28.441856
297.773600	26490.358555	28.446874
297.998108	26508.867016	28.451892
298.381237	26548.137906	28.456909
298.371696	26590.649471	28.461927
298.829867	26620.011230	28.466944
298.844791	26646.813233	28.471962
299.242350	26690.879225	28.476980
299.598464	26712.596921	28.481997
299.450054	26750.782214	28.487015
300.246218	26793.035263	28.492032
300.447497	26826.501526	28.497050
300.480993	26861.599494	28.502068
300.930053	26896.335368	28.507085
301.185128	26928.093198	28.512103
301.386890	26966.382050	28.517120
301.915816	26999.354847	28.522138
301.710635	27045.197246	28.527156
302.383359	27073.717042	28.532173
302.867763	27113.004761	28.537191
303.561689	27141.995363	28.542208
303.873889	27165.180441	28.547226
304.428725	27198.004132	28.552244
304.640502	27229.560641	28.557261
304.815313	27257.457121	28.562279
305.013027	27282.847147	28.567296
305.128767	27321.074296	28.572314
305.655366	27352.290936	28.577332
305.848115	27382.896269	28.582349
306.350101	27408.902441	28.587367
306.768030	27445.698295	28.592384
306.682537	27482.787974	28.597402
307.100902	27514.426332	28.602420
307.349421	27541.951385	28.607437
307.458232	27581.178753	28.612455
307.677232	27617.374023	28.617472
308.195853	27646.557140	28.622490
308.505421	27687.453501	28.627508
308.633426	27721.090727	28.632525
309.132388	27765.806825	28.637543
309.569587	27794.939703	28.642560
310.103796	27832.185766	28.647578
310.273853	27871.315608	28.652596
310.450514	27897.240631	28.657613
310.934210	27939.703027	28.662631
311.400339	27954.926129	28.667648
311.634634	27989.691189	28.672666
311.768493	28027.272112	28.677684
312.276637	28054.712942	28.682701
312.362389	28093.553022	28.687719
312.590763	28124.299261	28.692736
312.929328	28158.447806	28.697754
313.148828	28190.225816	28.702772
313.726975	28223.426751	28.707789
313.851989	28266.268370	28.712807
314.219221	28290.457430	28.717824
315.086320	28329.441035	28.722842
315.011660	28360.291986	28.727860
315.435526	28388.896853	28.732877
315.356946	28430.373807	28.737895
315.790849	28467.200603	28.742912
316.504010	28498.332886	28.747930
316.853177	28529.724502	28.752948
317.098862	28559.944053	28.757965
317.202901	28588.795246	28.762983
317.491996	28621.795593	28.768000
317.982592	28650.068007	28.773018
318.252416	28688.602260	28.778036
318.563043	28718.628567	28.783053
318.784815	28754.022657	28.788071
319.590417	28779.281392	28.793088
320.511232	28791.696931	28.798106
320.899498	28816.287858	28.803124
321.763825	28816.076703	28.808141
321.549057	28830.250386	28.813159
321.921116	28851.462188	28.818176
321.954524	28870.242924	28.823194
322.496792	28883.937763	28.828212
322.649024	28891.435952	28.833229
323.174561	28916.732408	28.838247
323.147031	28936.274945	28.843264
323.313244	28952.253722	28.848282
323.871347	28974.372014	28.853300
323.981666	28993.671778	28.858317
324.053092	29024.519806	28.863335
324.207413	29045.848090	28.868352
324.464677	29060.004879	28.873370
324.849913	29093.243765	28.878388
325.289551	29115.861165	28.883405
325.391238	29147.924597	28.888423
326.058465	29172.390080	28.893440
326.644062	29184.125128	28.898458
326.629364	29212.945229	28.903476
326.955613	29231.048316	28.908493
327.608114	29263.537652	28.913511
327.757302	29294.923838	28.918528
328.270467	29317.555227	28.923546
328.227467	29341.885643	28.928564
328.494370	29368.285115	28.933581
328.980121	29406.306487	28.938599
328.781397	29436.394667	28.943616
329.173670	29457.509112	28.948634
329.348939	29498.259452	28.953652
329.955950	29522.279662	28.958669
330.207805	29571.064986	28.963687
330.528423	29598.726895	28.968704
330.825660	29624.489825	28.973722
330.596651	29668.628776	28.978740
331.082853	29692.465830	28.983757
331.714328	29747.317359	28.988775
332.290824	29789.294954	28.993792
332.478875	29819.493779	28.998810
332.416112	29855.907807	29.003828
332.664440	29889.030357	29.008845
332.853934	29940.354830	29.013863
332.843352	29976.590222	29.018880
333.469134	30025.261153	29.023898
333.945609	30068.354892	29.028916
334.529240	30108.726403	29.033933
334.827619	30158.586775	29.038951
335.245123	30197.220824	29.043968
335.486063	30236.982523	29.048986
335.793473	30282.290387	29.054004
336.297282	30315.531635	29.059021
336.841438	30359.620482	29.064039
336.971498	30391.763580	29.069056
337.287194	30434.010910	29.074074
337.483082	30483.274939	29.079092
337.719684	30514.996966	29.084109
337.946892	30559.932392	29.089127
338.398093	30604.719041	29.094144
338.711692	30641.947861	29.099162
338.983107	30700.088606	29.104180
339.434530	30736.075953	29.109197
339.557080	30773.809052	29.114215
339.823283	30815.578153	29.119232
340.403847	30855.047618	29.124250
340.807483	30904.507682	29.129268
341.644009	30932.640539	29.134285
342.020201	30967.318860	29.139303
342.475089	31009.039830	29.144320
342.751452	31041.432846	29.149338
343.004442	31083.482707	29.154356
343.387073	31103.361305	29.159373
343.759123	31136.042919	29.164391
343.918624	31174.700240	29.169408
343.986717	31204.730224	29.174426
344.074112	31241.388672	29.179444
344.733659	31285.208546	29.184461
344.928737	31330.751233	29.189479
345.401691	31366.154703	29.194496
345.483538	31395.259836	29.199514
345.741933	31445.376111	29.204532
346.347169	31473.912595	29.209549
346.766453	31511.828134	29.214567
346.601576	31562.731675	29.219584
347.281500	31603.976063	29.224602
347.664284	31648.864186	29.229620
348.185429	31689.735343	29.234637
347.928915	31733.958850	29.239655
348.337077	31778.691553	29.244672
348.950232	31825.067534	29.249690
349.120023	31865.665336	29.254708
349.699474	31917.711200	29.259725
350.428807	31948.062243	29.264743
350.817258	32001.996875	29.269760
351.111682	32020.802798	29.274778
351.806691	32072.217721	29.279796
351.731195	32099.786966	29.284813
352.074121	32146.155415	29.289831
352.289518	32184.736311	29.294848
352.744013	32225.366078	29.299866
353.079381	32266.488735	29.304884
353.451381	32315.603073	29.309901
353.976588	32351.385673	29.314919
354.211390	32396.184787	29.319936
354.768973	32436.470071	29.324954
355.227701	32477.864634	29.329972
355.695328	32505.109099	29.334989
355.749964	32544.695760	29.340007
356.258795	32582.156672	29.345024
356.671973	32608.316079	29.350042
356.885912	32654.756436	29.355060
357.114630	32698.868040	29.360077
358.181396	32724.628074	29.365095
358.301492	32772.657603	29.370112
358.677684	32809.336786	29.375130
358.980141	32841.905529	29.380148
359.323388	32887.447367	29.385165
359.621801	32912.240573	29.390183
359.851903	32951.446474	29.395200
360.225538	32987.671171	29.400218
360.289789	33035.691083	29.405236
360.725051	33074.732311	29.410253
361.208793	33108.796731	29.415271
361.681623	33152.466427	29.420288
362.654700	33190.487932	29.425306
362.489194	33228.472898	29.430324
362.703322	33270.906263	29.435341
363.344624	33304.181322	29.440359
363.102272	33354.134035	29.445376
363.278807	33391.351294	29.450394
363.946491	33434.902542	29.455412
364.061144	33480.961971	29.460429
364.921142	33524.110260	29.465447
364.700703	33569.899932	29.470464
365.492259	33600.496523	29.475482
365.739052	33652.649385	29.480500
366.386497	33691.026281	29.485517
366.544819	33732.084705	29.490535
366.756631	33776.586887	29.495552
367.282858	33813.193741	29.500570
367.544801	33853.275157	29.505588
367.660620	33894.865321	29.510605
368.344830	33928.551932	29.515623
368.313718	33974.761721	29.520640
368.993707	34014.752671	29.525658
368.867447	34051.639175	29.530676
369.477131	34098.020729	29.535693
370.376688	34132.217672	29.540711
370.838486	34169.910072	29.545728
371.498439	34209.253305	29.550746
371.880111	34239.744322	29.555764
372.138959	34267.377841	29.560781
373.156115	34287.678527	29.565799
373.180647	34322.518652	29.570816
373.686174	34354.033664	29.575834
373.864062	34385.992047	29.580852
374.008363	34430.449278	29.585869
374.372231	34452.603827	29.590887
374.487493	34491.672516	29.595904
375.113469	34534.024942	29.600922
375.435050	34568.711456	29.605940
375.819670	34606.404079	29.610957
376.173031	34638.645170	29.615975
376.587148	34680.386158	29.620992
377.127635	34718.547737	29.626010
377.714758	34759.288081	29.631028
377.905811	34792.585437	29.636045
378.570225	34822.413377	29.641063
378.850801	34854.425932	29.646080
379.106040	34887.795580	29.651098
379.170815	34927.922563	29.656116
379.521945	34967.638045	29.661133
380.018338	35003.948142	29.666151
380.362911	35043.487754	29.671168
381.013985	35087.576133	29.676186
381.648321	35117.327003	29.681204
381.734074	35157.741985	29.686221
382.178230	35171.595443	29.691239
382.435649	35219.697549	29.696256
382.861580	35254.564850	29.701274
382.984488	35294.006870	29.706292
383.181343	35337.155252	29.711309
383.764218	35380.641600	29.716327
384.000183	35425.339475	29.721344
384.480545	35454.280308	29.726362
384.803399	35504.680685	29.731380
384.687221	35546.689808	29.736397
385.252507	35584.621434	29.741415
385.734444	35638.721449	29.746432
386.110933	35688.430975	29.751450
386.390817	35733.002479	29.756468
386.624878	35779.800642	29.761485
387.021606	35829.349251	29.766503
387.326977	35882.560698	29.771520
387.578744	35927.617567	29.776538
388.054870	35985.848350	29.781556
388.193354	36041.963348	29.786573
388.763083	36078.750674	29.791591
388.947652	36135.977896	29.796608
389.748367	36191.350919	29.801626
389.993514	36241.075983	29.806644
389.750034	36296.227124	29.811661
390.062802	36356.741888	29.816679
390.692679	36414.987697	29.821696
391.043352	36464.886448	29.826714
391.865681	36516.722235	29.831732
391.907457	36568.547622	29.836749
392.637035	36609.680210	29.841767
392.688111	36659.417675	29.846784
393.120053	36720.268904	29.851802
394.274298	36766.412903	29.856820
394.637076	36827.496588	29.861837
395.119779	36864.678301	29.866855
395.113652	36909.809251	29.871872
395.284524	36956.917086	29.876890
396.236326	37004.389605	29.881908
396.635014	37046.415875	29.886925
397.448610	37085.531694	29.891943
397.960781	37128.982093	29.896960
398.246888	37161.787676	29.901978
398.910994	37203.102394	29.906996
398.731026	37246.579240	29.912013
399.687615	37283.440836	29.917031
399.959189	37321.516406	29.922048
400.542745	37350.879968	29.927066
400.953632	37391.260892	29.932084
400.963425	37441.436634	29.937101
401.225388	37473.430740	29.942119
401.577219	37518.696606	29.947136
402.126155	37564.342725	29.952154
402.676891	37608.749237	29.957172
402.863229	37652.605853	29.962189
403.437491	37699.291685	29.967207
403.592429	37734.749311	29.972224
403.962557	37782.890114	29.977242
404.345405	37823.605070	29.982260
404.578067	37874.537368	29.987277
405.043732	37916.466317	29.992295
405.747222	37963.986178	29.997312
405.869493	38011.812189	30.002330
406.383131	38058.811835	30.007348
406.505770	38105.474432	30.012365
407.259326	38157.527316	30.017383
407.441040	38210.213739	30.022400
407.838570	38268.545237	30.027418
408.487717	38311.110211	30.032436
408.532413	38356.678897	30.037453
409.367652	38396.362855	30.042471
409.725936	38452.987245	30.047488
409.721016	38508.359638	30.052506
410.294640	38546.712576	30.057524
410.595822	38613.104045	30.062541
410.976877	38660.435637	30.067559
411.651468	38716.473641	30.072576
411.815096	38769.309708	30.077594
412.543062	38809.536115	30.082612
413.037965	38870.023093	30.087629
413.132479	38912.682451	30.092647
413.453080	38965.766340	30.097664
413.967617	39023.234131	30.102682
414.533791	39070.082295	30.107700
414.880427	39131.579772	30.112717
415.373002	39175.290324	30.117735
415.658809	39233.844292	30.122752
415.880016	39285.844147	30.127770
416.517615	39332.903032	30.132788
416.926675	39395.453925	30.137805
417.602331	39439.111036	30.142823
418.228812	39487.398877	30.147840
418.468708	39521.758372	30.152858
419.157188	39574.950556	30.157876
419.723604	39622.419641	30.162893
419.750408	39663.029397	30.167911
420.468102	39711.208586	30.172928
420.704850	39752.727931	30.177946
421.404044	39793.947248	30.182964
421.610081	39836.192523	30.187981
422.176846	39875.042177	30.192999
422.467001	39911.411848	30.198016
422.757627	39955.206196	30.203034
423.625360	39978.931844	30.208052
423.918671	40025.508594	30.213069
424.691603	40061.474034	30.218087
425.482183	40092.820024	30.223104
425.777425	40117.097170	30.228122
426.341919	40150.002815	30.233140
426.303753	40187.366698	30.238157
426.846512	40223.855433	30.243175
427.000991	40248.692343	30.248192
427.153784	40297.922615	30.253210
427.708530	40328.028361	30.258228
428.165941	40364.922813	30.263245
429.090423	40411.825258	30.268263
429.814570	40448.671747	30.273280
429.370186	40478.504139	30.278298
429.807016	40510.241334	30.283316
430.159077	40559.447307	30.288333
430.971426	40611.648657	30.293351
431.283961	40651.975168	30.298368
431.392851	40700.220281	30.303386
431.951509	40739.901253	30.308404
432.037485	40781.857263	30.313421
432.536747	40826.442865	30.318439
432.920995	40879.066081	30.323456
433.021799	40934.263640	30.328474
433.717983	40979.666199	30.333492
433.914009	41046.682388	30.338509
434.199544	41099.195102	30.343527
434.729176	41148.899528	30.348544
434.860929	41212.555273	30.353562
435.530541	41262.212731	30.358580
435.672920	41321.775083	30.363597
436.293724	41382.186062	30.368615
436.785573	41443.123381	30.373632
436.965452	41511.338884	30.378650
437.440483	41554.437127	30.383668
437.853844	41625.215877	30.388685
438.366374	41686.194903	30.393703
438.979638	41739.612854	30.398720
439.967750	41792.137349	30.403738
440.523421	41828.620411	30.408756
441.691010	41878.485880	30.413773
442.292227	41912.261249	30.418791
442.445346	41962.583075	30.423808
442.797535	42002.146873	30.428826
443.631096	42029.624421	30.433844
443.832423	42079.413999	30.438861
444.078454	42124.737636	30.443879
444.742181	42164.139081	30.448896
444.649813	42210.161038	30.453914
445.110275	42251.763924	30.458932
445.575162	42304.466469	30.463949
445.717504	42353.184337	30.468967
446.642775	42400.185788	30.473984
446.861256	42460.719668	30.479002
447.504949	42494.735951	30.484020
447.916643	42533.930858	30.489037
448.301541	42588.752839	30.494055
448.948293	42639.397364	30.499072
448.640573	42686.466049	30.504090
449.158856	42739.648298	30.509108
449.640118	42787.295700	30.514125
449.597493	42838.934171	30.519143
450.858703	42877.351466	30.524160
450.752641	42937.671828	30.529178
451.128918	42984.007822	30.534196
451.339143	43035.752625	30.539213
451.521671	43101.708219	30.544231
452.411087	43145.617538	30.549248
452.429872	43207.430797	30.554266
453.291688	43262.571907	30.559284
453.574647	43319.226998	30.564301
453.570135	43388.381682	30.569319
454.316321	43442.478707	30.574336
454.317276	43513.783515	30.579354
454.957339	43576.778198	30.584372
455.529447	43630.890298	30.589389
456.162466	43701.116280	30.594407
456.674820	43756.332329	30.599424
456.687423	43824.935380	30.604442
457.175501	43888.808677	30.609460
457.833756	43955.767606	30.614477
458.014975	44026.286769	30.619495
458.568771	44088.942188	30.624512
459.400854	44167.570290	30.629530
459.852336	44228.281229	30.634548
460.704362	44294.065910	30.639565
460.710156	44357.838976	30.644583
461.595062	44424.801766	30.649600
461.968388	44480.730868	30.654618
462.844454	44542.002388	30.659636
463.229606	44607.108374	30.664653
463.233887	44658.035245	30.669671
464.369683	44719.431036	30.674688
464.520989	44785.649525	30.679706
465.377853	44839.226554	30.684724
465.770700	44896.032904	30.689741
466.069895	44949.646940	30.694759
466.736857	44995.397575	30.699776
466.967446	45055.152220	30.704794
467.528118	45112.691920	30.709812
468.041963	45176.362436	30.714829
468.519738	45242.025077	30.719847
468.842891	45285.489617	30.724864
469.482474	45350.406091	30.729882
469.878214	45404.018741	30.734900
470.403029	45462.709929	30.739917
470.316093	45518.871857	30.744935
471.044168	45579.511506	30.749952
471.828203	45646.228061	30.754970
472.204743	45704.354795	30.759988
473.173282	45759.270276	30.765005
473.663581	45809.566950	30.770023
474.845705	45843.440757	30.775040
475.343764	45898.822478	30.780058
475.667643	45938.929081	30.785076
476.124043	45986.239276	30.790093
476.786817	46026.065219	30.795111
477.242615	46055.492064	30.800128
477.880476	46097.738571	30.805146
478.359606	46134.999803	30.810164
479.231371	46168.985972	30.815181
479.466120	46218.096335	30.820199
479.721709	46247.409290	30.825216
479.916592	46300.732907	30.830234
480.060326	46341.361876	30.835252
481.172424	46370.553490	30.840269
481.445729	46421.935651	30.845287
482.116346	46459.629234	30.850304
482.522703	46507.511385	30.855322
483.097463	46551.558920	30.860340
483.494896	46572.240199	30.865357
483.645201	46621.617711	30.870375
484.510902	46652.334933	30.875392
484.739207	46697.183505	30.880410
485.263268	46741.378528	30.885428
485.567896	46775.182415	30.890445
485.415285	46813.359795	30.895463
485.525656	46869.234802	30.900480
485.875406	46922.643173	30.905498
486.311090	46978.828093	30.910516
486.896634	47035.230078	30.915533
487.017515	47102.269898	30.920551
487.431410	47160.843696	30.925568
487.963227	47226.016519	30.930586
489.010622	47297.599612	30.935604
488.954361	47360.625400	30.940621
489.572847	47424.969117	30.945639
490.114898	47476.121782	30.950656
490.254621	47543.672391	30.955674
490.398910	47610.672085	30.960692
491.072750	47682.321226	30.965709
491.755600	47762.560541	30.970727
492.470592	47821.430511	30.975744
492.886591	47889.982747	30.980762
493.147904	47961.096357	30.985780
494.032882	48026.728609	30.990797
494.070739	48093.759045	30.995815
495.030753	48159.519110	31.000832
495.510077	48229.738995	31.005850
495.692756	48304.934004	31.010868
496.175273	48374.780563	31.015885
496.732591	48438.782430	31.020903
496.968365	48512.065476	31.025920
497.684916	48596.610921	31.030938
498.034260	48667.187823	31.035956
498.768399	48728.581500	31.040973
498.962496	48813.133653	31.045991
499.561641	48881.040151	31.051008
500.056612	48961.186566	31.056026
500.540951	49041.575346	31.061044
501.463895	49123.610290	31.066061
501.638093	49190.034180	31.071079
502.625476	49256.065167	31.076096
502.992545	49326.400898	31.081114
503.550431	49403.900682	31.086132
504.051128	49459.315963	31.091149
504.579143	49540.775230	31.096167
505.278535	49609.920923	31.101184
505.962619	49670.635318	31.106202
506.408815	49743.231326	31.111220
507.357135	49795.173366	31.116237
508.036048	49858.951357	31.121255
508.342549	49915.264959	31.126272
508.981208	49961.713359	31.131290
509.416793	50028.079745	31.136308
510.313284	50073.848950	31.141325
510.720097	50133.393185	31.146343
511.031928	50193.648437	31.151360
511.661082	50259.124677	31.156378
512.011458	50315.679144	31.161396
512.423934	50369.914594	31.166413
512.845787	50443.161990	31.171431
513.337721	50485.686241	31.176448
513.517486	50558.168359	31.181466
514.323759	50638.499632	31.186484
514.641392	50694.889317	31.191501
514.792809	50760.125435	31.196519
515.677319	50822.184493	31.201536
516.147526	50873.843188	31.206554
516.952105	50938.275173	31.211572
517.584000	50988.440854	31.216589
518.035832	51042.526185	31.221607
518.550815	51101.638361	31.226624
518.895345	51154.032361	31.231642
519.115462	51215.778922	31.236660
519.912013	51271.398981	31.241677
520.294532	51332.367450	31.246695
520.206348	51401.724111	31.251712
521.046775	51464.880119	31.256730
521.726744	51535.660777	31.261748
522.570498	51584.022858	31.266765
523.049230	51649.140603	31.271783
523.485213	51711.348219	31.276800
524.299904	51764.631745	31.281818
524.795460	51826.583562	31.286836
525.477570	51882.811474	31.291853
525.759357	51946.125888	31.296871
525.611810	52016.607336	31.301888
526.855119	52079.632308	31.306906
527.320744	52148.240043	31.311924
528.044495	52199.317790	31.316941
528.452032	52268.226049	31.321959
529.023162	52331.844215	31.326976
529.523755	52391.044177	31.331994
530.022220	52457.078609	31.337012
530.574806	52511.012357	31.342029
531.093637	52581.815099	31.347047
531.457416	52648.124276	31.352064
531.701746	52715.983686	31.357082
531.954492	52780.747653	31.362100
532.816341	52856.964768	31.367117
533.478694	52935.598992	31.372135
534.186899	52996.356269	31.377152
534.510303	53060.160753	31.382170
534.941243	53135.946357	31.387188
535.417387	53212.743929	31.392205
535.924714	53283.835348	31.397223
536.292278	53349.462490	31.402240
537.103914	53426.999217	31.407258
537.523798	53501.300643	31.412276
537.856184	53582.779381	31.417293
538.729323	53660.509742	31.422311
539.454209	53714.558487	31.427328
539.884564	53784.669961	31.432346
540.624291	53871.711602	31.437364
541.021112	53932.494752	31.442381
541.886436	54007.000117	31.447399
541.924617	54075.136201	31.452416
542.358004	54140.913440	31.457434
542.746711	54226.517905	31.462452
543.538419	54292.891255	31.467469
543.827478	54375.202185	31.472487
544.410344	54448.069856	31.477504
545.476693	54526.177817	31.482522
545.747552	54594.247310	31.487540
546.363307	54667.021907	31.492557
546.781615	54748.383620	31.497575
547.421029	54824.926711	31.502592
548.163655	54881.766172	31.507610
548.731549	54968.724847	31.512628
549.025926	55030.976073	31.517645
549.488395	55097.428555	31.522663
550.319094	55166.576445	31.527680
551.624380	55231.751845	31.532698
551.982035	55302.239920	31.537716
552.793368	55361.208810	31.542733
553.478798	55405.426712	31.547751
553.722055	55469.060387	31.552768
554.568853	55519.353971	31.557786
554.797477	55581.351134	31.562804
555.394165	55631.367697	31.567821
555.640421	55691.153697	31.572839
555.594253	55752.865254	31.577856
556.429366	55817.103312	31.582874
556.657099	55891.619523	31.587892
557.255776	55962.995789	31.592909
557.691219	56035.467388	31.597927
558.366066	56113.768456	31.602944
559.310709	56183.047011	31.607962
559.712105	56254.512005	31.612980
560.001967	56330.551416	31.617997
560.709625	56393.899639	31.623015
561.146958	56466.043147	31.628032
561.773661	56535.916799	31.633050
562.601477	56608.366652	31.638068
563.354046	56673.347759	31.643085
564.331680	56742.375939	31.648103
565.033657	56810.251324	31.653120
565.368046	56862.077312	31.658138
565.956482	56946.267891	31.663156
566.386960	56996.515866	31.668173
566.911585	57061.951437	31.673191
567.393131	57130.697677	31.678208
568.309607	57200.597499	31.683226
568.988462	57272.249911	31.688244
569.447880	57338.898967	31.693261
569.422603	57398.320359	31.698279
570.017490	57461.049822	31.703296
570.520272	57540.572361	31.708314
571.060315	57617.266531	31.713332
571.752241	57684.690257	31.718349
572.164957	57760.620009	31.723367
572.406057	57843.646589	31.728384
573.232237	57916.891788	31.733402
573.463045	58003.762364	31.738420
574.255248	58081.007132	31.743437
574.940619	58153.838382	31.748455
575.579915	58234.683631	31.753472
575.997960	58321.007018	31.758490
576.496540	58413.261355	31.763508
577.407375	58482.944244	31.768525
577.873715	58564.988614	31.773543
578.280069	58654.099947	31.778560
578.600496	58723.167100	31.783578
579.341995	58799.687884	31.788596
580.110559	58879.185850	31.793613
581.488498	58954.031407	31.798631
581.672057	59028.095839	31.803648
582.475329	59106.886539	31.808666
583.015557	59177.275075	31.813684
583.995177	59243.828909	31.818701
585.077486	59306.796959	31.823719
585.253485	59381.395333	31.828736
586.140968	59436.906320	31.833754
586.802465	59504.770283	31.838772
586.957518	59568.884315	31.843789
587.536228	59641.331628	31.848807
587.898655	59709.293636	31.853824
588.123405	59770.973013	31.858842
588.812061	59850.220813	31.863860
589.477883	59925.339126	31.868877
590.188674	59980.935989	31.873895
590.556765	60049.600657	31.878912
591.085148	60122.690254	31.883930
591.769537	60197.616601	31.888948
592.211971	60250.268435	31.893965
593.162210	60323.305222	31.898983
593.287710	60388.147627	31.904000
594.294578	60456.131044	31.909018
594.839188	60531.137269	31.914036
594.957590	60600.304664	31.919053
595.564692	60669.686893	31.924071
595.698188	60752.461706	31.929088
596.547827	60825.800591	31.934106
596.868547	60907.660407	31.939124
597.287342	61000.316800	31.944141
597.992679	61075.470422	31.949159
598.262597	61170.492883	31.954176
598.872594	61256.435750	31.959194
599.289862	61343.997957	31.964212
599.857796	61431.638160	31.969229
600.602586	61533.955914	31.974247
600.833708	61629.296391	31.979264
601.544991	61719.206686	31.984282
602.080212	61814.323003	31.989300
602.722515	61912.106940	31.994317
603.484839	62002.567332	31.999335
604.043270	62104.087361	32.004352
604.791916	62194.867111	32.009370
605.059305	62289.818296	32.014388
605.574850	62397.689248	32.019405
606.393071	62497.891464	32.024423
606.890319	62603.290987	32.029440
607.582224	62701.950193	32.034458
608.662780	62790.603748	32.039476
609.453403	62885.918394	32.044493
610.005646	62968.938887	32.049511
610.677302	63072.483560	32.054528
611.647297	63157.300434	32.059546
612.286276	63242.479637	32.064564
612.913547	63327.464714	32.069581
613.836738	63418.747027	32.074599
614.076411	63511.193940	32.079616
614.773057	63596.992053	32.084634
615.474179	63683.720372	32.089652
615.784685	63772.770233	32.094669
616.564390	63866.368370	32.099687
617.092786	63956.764861	32.104704
617.690751	64045.004645	32.109722
618.299194	64133.331730	32.114740
618.922793	64229.139797	32.119757
619.808154	64322.716756	32.124775
620.298199	64419.844292	32.129792
621.319258	64497.535462	32.134810
622.424618	64585.267176	32.139828
622.867278	64666.392179	32.144845
623.797249	64741.641962	32.149863
624.315216	64827.174702	32.154880
625.002413	64909.623352	32.159898
625.435560	64989.174462	32.164916
625.952624	65061.495289	32.169933
626.537584	65145.315563	32.174951
627.078154	65234.613125	32.179968
627.216288	65312.464073	32.184986
627.690744	65396.581054	32.190004
628.128060	65487.991283	32.195021
628.613768	65577.520235	32.200039
629.754456	65683.578982	32.205056
630.062952	65774.985094	32.210074
630.507647	65866.249911	32.215092
631.091662	65966.591269	32.220109
632.194681	66048.820222	32.225127
632.411749	66144.021759	32.230144
633.373156	66231.648766	32.235162
634.199210	66309.572310	32.240180
634.636999	66397.921360	32.245197
635.389211	66477.104262	32.250215
635.841975	66575.448858	32.255232
636.774485	66653.913948	32.260250
637.282694	66737.998419	32.265268
637.706483	66833.322107	32.270285
638.405700	66923.613788	32.275303
639.163176	67016.777509	32.280320
639.365881	67112.808004	32.285338
640.209109	67203.679617	32.290356
640.155692	67295.762014	32.295373
641.298308	67385.656640	32.300391
641.578186	67494.833589	32.305408
642.205863	67600.689390	32.310426
642.783683	67706.198859	32.315444
643.345538	67810.147324	32.320461
643.792226	67908.232050	32.325479
643.931261	68021.675563	32.330496
644.701160	68132.988266	32.335514
645.486499	68261.097387	32.340532
646.031664	68370.958330	32.345549
646.790716	68480.362008	32.350567
647.206090	68603.300624	32.355584
647.906104	68717.843407	32.360602
648.528553	68828.188081	32.365620
649.266144	68942.314393	32.370637
650.220205	69055.552482	32.375655
650.956250	69176.221054	32.380672
651.449904	69289.931189	32.385690
652.479778	69401.455584	32.390708
653.172298	69515.566145	32.395725
654.645116	69617.789838	32.400743
655.409180	69722.398187	32.405760
656.309555	69833.127860	32.410778
656.873528	69919.613869	32.415796
657.169291	70032.725015	32.420813
657.946419	70122.395107	32.425831
658.717235	70235.863330	32.430848
659.211390	70334.013111	32.435866
660.193327	70429.401948	32.440884
660.303435	70544.900021	32.445901
661.287420	70639.643399	32.450919
661.953425	70748.013666	32.455936
662.488692	70845.133068	32.460954
663.414003	70942.141085	32.465972
664.032374	71051.735903	32.470989
664.732482	71143.891233	32.476007
665.364702	71249.849833	32.481024
665.995958	71350.438977	32.486042
666.700523	71455.171217	32.491060
667.636388	71554.307597	32.496077
668.573309	71642.324039	32.501095
669.312487	71742.707800	32.506112
669.788968	71842.335161	32.511130
670.228662	71936.079223	32.516148
670.932611	72036.494947	32.521165
671.577605	72128.117732	32.526183
672.455684	72215.740002	32.531200
673.138293	72308.598748	32.536218
673.947886	72403.920405	32.541236
674.592750	72506.994292	32.546253
675.338443	72594.397899	32.551271
675.960054	72695.449637	32.556288
676.539224	72780.448098	32.561306
677.533765	72867.572981	32.566324
677.533458	72968.976472	32.571341
678.252820	73057.095016	32.576359
678.743129	73140.715286	32.581376
679.540596	73228.125533	32.586394
680.483238	73324.151619	32.591412
680.833995	73410.264480	32.596429
681.774097	73497.209956	32.601447
682.411205	73594.804808	32.606464
682.958888	73681.825006	32.611482
683.958569	73781.504360	32.616500
684.311657	73882.729312	32.621517
684.446159	73977.402337	32.626535
685.159927	74083.207472	32.631552
685.574477	74190.807863	32.636570
686.073983	74294.734742	32.641588
686.543279	74404.962064	32.646605
687.666225	74521.471479	32.651623
688.274964	74627.738540	32.656640
689.067640	74738.562589	32.661658
689.816125	74846.708647	32.666676
690.175757	74961.502813	32.671693
690.791379	75071.203271	32.676711
691.978267	75191.758991	32.681728
692.431662	75303.322510	32.686746
693.436911	75416.459456	32.691764
693.847743	75535.833532	32.696781
694.480733	75644.760900	32.701799
695.258447	75762.368446	32.706816
696.210272	75877.998469	32.711834
697.073430	75990.121344	32.716852
697.549739	76097.124289	32.721869
698.607931	76207.532751	32.726887
699.524802	76319.648573	32.731904
699.916186	76430.694401	32.736922
700.893117	76546.424676	32.741940
701.448324	76651.162605	32.746957
702.349423	76756.619500	32.751975
703.070833	76863.612406	32.756992
703.651594	76979.976610	32.762010
704.152388	77088.309730	32.767028
704.800015	77200.686689	32.772045
705.386211	77325.095642	32.777063
706.241342	77428.446772	32.782080
707.099374	77538.461248	32.787098
707.563073	77663.866362	32.792116
707.992351	77774.772356	32.797133
709.222827	77878.408441	32.802151
710.012620	77986.167780	32.807168
710.887486	78108.520816	32.812186
711.822411	78216.017628	32.817204
712.415582	78323.517705	32.822221
713.091529	78442.900954	32.827239
713.912674	78538.685814	32.832256
714.325552	78644.188405	32.837274
715.361459	78760.273496	32.842292
716.229792	78862.234386	32.847309
716.813545	78973.564408	32.852327
717.414706	79081.015501	32.857344
718.120425	79210.063682	32.862362
719.028625	79304.494660	32.867380
719.456142	79419.841638	32.872397
719.753158	79528.963717	32.877415
720.431206	79646.780863	32.882432
720.593359	79770.000318	32.887450
721.841196	79885.917565	32.892468
722.525774	80012.172890	32.897485
723.199858	80125.051684	32.902503
723.873538	80239.172589	32.907520
724.331899	80356.444344	32.912538
725.164832	80467.424576	32.917556
725.667724	80575.986386	32.922573
725.885764	80699.581266	32.927591
727.045309	80822.877215	32.932608
727.567204	80942.421993	32.937626
728.236029	81065.859203	32.942644
728.419767	81194.048054	32.947661
729.577584	81326.418021	32.952679
730.217946	81447.074002	32.957696
731.602565	81582.589790	32.962714
732.398835	81694.784249	32.967732
733.308897	81815.285538	32.972749
734.461507	81922.901903	32.977767
735.591676	82036.743220	32.982784
736.403414	82148.544283	32.987802
737.335815	82244.172361	32.992820
738.218656	82352.567477	32.997837
738.759625	82455.517627	33.002855
739.980233	82557.398774	33.007872
740.463299	82673.041808	33.012890
741.101150	82765.714882	33.017908
742.112167	82872.165999	33.022925
742.376615	82988.072616	33.027943
743.121291	83084.100362	33.032960
743.674800	83200.672129	33.037978
744.309638	83315.293019	33.042996
744.744192	83442.907905	33.048013
745.482219	83556.981433	33.053031
746.461669	83672.474757	33.058048
746.948176	83799.322843	33.063066
748.209932	83907.107008	33.068084
749.556308	84001.218990	33.073101
750.428899	84119.062310	33.078119
751.252801	84223.000874	33.083136
752.046262	84328.959291	33.088154
753.071753	84416.039717	33.093172
753.939117	84522.456108	33.098189
754.736915	84625.779324	33.103207
755.539013	84729.963886	33.108224
755.833270	84832.707786	33.113242
756.874997	84930.329797	33.118260
757.721608	85030.162180	33.123277
758.568523	85137.559741	33.128295
759.328468	85223.809854	33.133312
759.659324	85331.149559	33.138330
760.592381	85429.145073	33.143348
760.822187	85537.907915	33.148365
761.958394	85655.044620	33.153383
762.618089	85754.034417	33.158400
763.050785	85866.555573	33.163418
763.341816	85984.370842	33.168436
763.938299	86086.032757	33.173453
764.712831	86214.493677	33.178471
765.403650	86332.475841	33.183488
766.193413	86455.841288	33.188506
766.455853	86586.588973	33.193524
767.135294	86701.558442	33.198541
767.564769	86839.022693	33.203559
768.547904	86971.027836	33.208576
769.186540	87112.186266	33.213594
769.849001	87237.501133	33.218612
770.586652	87385.627865	33.223629
771.040013	87518.314030	33.228647
772.298583	87649.138558	33.233664
773.163681	87783.484912	33.238682
773.939463	87917.693791	33.243700
774.294978	88051.411489	33.248717
775.085753	88183.578913	33.253735
775.840275	88303.599328	33.258752
776.545795	88443.410324	33.263770
777.045401	88569.592754	33.268788
777.809688	88710.067471	33.273805
778.574822	88842.837478	33.278823
779.774263	88978.138063	33.283840
780.453606	89127.790740	33.288858
781.313690	89249.040415	33.293876
782.253133	89375.753028	33.298893
783.097918	89529.335885	33.303911
784.017604	89656.471003	33.308928
784.693829	89795.203010	33.313946
785.396189	89931.954491	33.318964
786.380553	90070.297332	33.323981
787.124190	90200.580033	33.328999
788.163417	90319.474034	33.334016
789.256080	90462.161478	33.339034
790.390975	90579.710780	33.344052
791.497409	90705.629756	33.349069
792.196651	90819.015136	33.354087
793.572067	90932.637256	33.359104
794.158340	91060.514913	33.364122
794.782513	91186.955004	33.369140
795.871978	91300.876767	33.374157
796.127170	91427.743191	33.379175
797.345951	91545.232416	33.384192
797.866845	91666.354828	33.389210
798.287136	91790.117062	33.394228
799.079426	91924.201867	33.399245
799.678488	92059.635663	33.404263
800.723158	92182.832766	33.409280
801.637263	92318.307098	33.414298
802.351493	92456.817212	33.419316
803.409281	92575.298890	33.424333
804.241631	92706.250218	33.429351
805.104043	92832.102142	33.434368
806.070132	92957.355306	33.439386
806.566701	93078.182927	33.444404
807.419505	93207.371384	33.449421
807.962188	93337.420144	33.454439
808.887396	93468.816480	33.459456
809.524607	93611.412545	33.464474
810.106565	93742.014564	33.469492
811.405882	93877.866410	33.474509
811.791610	94006.776449	33.479527
812.932100	94137.064522	33.484544
813.995304	94264.183733	33.489562
814.786425	94405.479147	33.494580
815.411371	94525.367020	33.499597
816.380227	94669.272298	33.504615
817.288935	94798.078379	33.509632
817.870533	94937.621765	33.514650
818.174972	95063.646199	33.519668
819.274118	95203.198460	33.524685
819.452793	95361.528895	33.529703
820.359317	95500.326745	33.534720
820.897830	95642.668712	33.539738
821.748648	95798.322895	33.544756
823.026929	95940.309530	33.549773
823.762575	96085.601504	33.554791
824.532889	96235.071849	33.559808
825.216755	96386.356462	33.564826
825.706136	96526.403052	33.569844
826.402095	96681.452037	33.574861
827.298567	96826.240539	33.579879
828.207161	96987.202952	33.584896
829.346547	97134.959148	33.589914
829.695251	97292.436006	33.594932
830.780773	97415.533343	33.599949
831.453526	97564.163233	33.604967
832.508386	97693.579435	33.609984
833.150738	97838.539113	33.615002
834.645911	97987.549269	33.620020
835.846879	98120.557229	33.625037
836.025532	98264.361790	33.630055
836.765626	98397.430391	33.635072
837.841826	98545.279083	33.640090
839.020102	98688.890990	33.645108
840.130837	98826.162848	33.650125
840.788439	98977.223017	33.655143
841.280919	99104.717306	33.660160
842.472264	99251.473647	33.665178
843.995626	99367.905039	33.670196
844.886495	99500.865856	33.675213
845.670140	99632.893197	33.680231
846.522361	99763.629907	33.685248
847.184673	99903.600820	33.690266
848.204064	100031.485330	33.695284
849.208892	100164.862069	33.700301
850.143240	100295.613419	33.705319
851.051420	100422.819607	33.710336
852.076635	100547.700597	33.715354
852.781908	100690.786924	33.720372
853.417412	100812.192813	33.725389
853.867288	100954.889239	33.730407
854.686647	101091.240111	33.735424
855.745877	101244.010191	33.740442
856.186229	101376.960470	33.745460
857.304483	101524.347069	33.750477
857.917495	101671.851476	33.755495
858.853587	101813.397847	33.760512
859.697813	101953.805477	33.765530
860.654381	102105.581365	33.770548
860.948197	102241.841802	33.775565
861.934869	102400.067691	33.780583
862.609926	102545.626468	33.785600
863.646179	102706.609998	33.790618
864.724033	102858.788746	33.795636
866.278301	102986.448873	33.800653
867.239578	103137.049623	33.805671
868.106979	103268.596683	33.810688
869.013638	103417.089875	33.815706
869.459932	103551.987841	33.820724
870.644984	103696.229253	33.825741
871.474081	103845.941007	33.830759
872.246727	103982.577364	33.835776
873.882684	104115.972689	33.840794
874.858438	104241.572737	33.845812
876.368521	104371.349838	33.850829
877.357596	104489.683481	33.855847
877.892301	104633.130521	33.860864
879.102801	104749.807442	33.865882
879.368247	104880.529483	33.870900
880.137120	104996.401520	33.875917
881.216156	105134.376649	33.880935
881.788588	105263.885579	33.885952
882.675508	105401.689005	33.890970
882.976383	105539.825670	33.895988
884.018771	105675.450305	33.901005
884.862702	105809.813211	33.906023
885.637819	105942.057198	33.911040
886.666781	106098.544071	33.916058
886.973767	106245.545936	33.921076
887.628840	106382.679554	33.926093
888.446040	106527.535889	33.931111
888.935748	106661.716689	33.936128
889.765967	106808.930686	33.941146
890.504418	106965.099283	33.946164
891.825420	107104.769015	33.951181
893.043139	107245.469919	33.956199
893.603557	107396.938567	33.961216
894.633087	107544.213265	33.966234
895.109703	107696.013359	33.971252
896.166297	107834.763728	33.976269
896.962461	107985.221634	33.981287
897.988305	108136.468475	33.986304
898.881197	108289.157039	33.991322
899.677468	108448.886580	33.996340
900.759996	108590.869521	34.001357
901.644677	108759.577386	34.006375
902.022862	108909.597498	34.011392
903.290929	109060.696296	34.016410
904.159084	109234.101027	34.021428
904.745345	109392.016320	34.026445
905.698928	109556.278827	34.031463
906.449312	109723.985184	34.036480
907.425869	109884.897768	34.041498
908.347470	110067.137137	34.046516
909.658599	110226.388353	34.051533
910.523407	110394.079979	34.056551
911.098350	110569.515510	34.061568
912.001253	110742.744676	34.066586
912.658711	110913.578228	34.071604
913.299946	111081.168606	34.076621
914.270263	111267.109589	34.081639
915.080451	111443.019864	34.086656
916.528559	111624.740916	34.091674
916.969282	111808.028331	34.096692
918.169888	111986.746285	34.101709
918.906138	112171.219444	34.106727
919.879168	112356.531547	34.111744
920.708792	112537.922865	34.116762
921.359483	112721.930311	34.121780
922.579839	112915.830560	34.126797
923.435134	113100.530792	34.131815
924.331774	113286.848857	34.136832
925.408577	113477.147375	34.141850
926.026028	113678.210313	34.146868
927.487438	113853.725982	34.151885
928.549341	114041.176158	34.156903
929.227546	114219.251314	34.161920
930.169304	114410.019737	34.166938
931.110468	114614.030304	34.171956
931.985065	114788.171102	34.176973
933.328619	114965.511542	34.181991
934.586115	115145.948326	34.187008
935.817077	115326.136481	34.192026
936.683072	115511.937951	34.197044
937.842807	115680.191297	34.202061
939.319818	115853.088599	34.207079
940.033888	116011.139644	34.212096
941.708102	116177.653151	34.217114
942.571983	116346.234870	34.222132
943.682826	116506.103061	34.227149
944.603540	116658.251958	34.232167
945.224924	116836.970090	34.237184
946.949712	116979.430833	34.242202
947.918766	117128.276276	34.247220
949.238056	117273.515973	34.252237
949.999713	117416.915579	34.257255
950.565807	117573.766036	34.262272
951.771029	117715.752820	34.267290
952.715461	117859.265011	34.272308
953.764859	117994.174137	34.277325
954.468133	118133.070038	34.282343
955.115377	118281.653304	34.287360
956.261930	118418.869944	34.292378
956.802529	118579.432364	34.297396
957.643158	118720.249607	34.302413
958.468262	118862.870992	34.307431
959.438227	119019.917867	34.312448
959.952886	119178.609558	34.317466
960.873510	119334.980483	34.322484
961.834626	119495.125731	34.327501
962.606772	119659.816990	34.332519
963.333981	119825.771779	34.337536
964.117408	119995.016531	34.342554
965.027661	120179.489389	34.347572
965.556333	120346.327383	34.352589
966.693702	120522.698696	34.357607
967.234733	120706.128271	34.362624
968.462383	120875.332680	34.367642
969.564169	121070.422582	34.372660
970.290979	121247.559142	34.377677
971.483933	121431.131070	34.382695
972.618838	121628.857108	34.387712
973.288963	121805.814785	34.392730
974.018733	122000.295232	34.397748
974.907120	122187.305397	34.402765
976.021468	122381.879738	34.407783
976.842488	122576.729303	34.412800
977.730547	122768.727729	34.417818
978.915561	122979.899544	34.422836
979.856694	123179.782201	34.427853
980.402840	123372.001985	34.432871
981.737251	123581.707402	34.437888
983.062616	123772.094499	34.442906
983.977314	123973.266550	34.447924
984.862722	124177.095600	34.452941
985.909349	124381.179536	34.457959
986.877298	124579.999326	34.462976
988.155883	124779.697562	34.467994
989.334579	124975.682615	34.473012
990.395931	125168.870591	34.478029
991.992462	125362.622704	34.483047
992.873525	125550.702674	34.488064
993.967176	125739.574857	34.493082
994.563896	125929.274232	34.498100
995.457189	126123.038562	34.503117
996.940225	126313.679320	34.508135
997.593745	126521.463953	34.513152
998.529043	126707.409334	34.518170
999.620936	126902.021632	34.523188
1000.617193	127096.015465	34.528205
1001.623507	127297.443287	34.533223
1002.808223	127490.610168	34.538240
1003.615852	127695.724935	34.543258
1004.853941	127877.695101	34.548276
1005.593681	128084.788939	34.553293
1006.972111	128279.134436	34.558311
1007.355043	128480.843187	34.563328
1008.454489	128674.231879	34.568346
1009.484527	128876.069582	34.573364
1009.864438	129079.532557	34.578381
1011.797403	129275.914667	34.583399
1012.578794	129478.085987	34.588416
1013.415603	129677.864276	34.593434
1014.747322	129878.834805	34.598452
1015.782809	130073.292983	34.603469
1016.765374	130259.145166	34.608487
1018.079315	130448.816134	34.613504
1019.558972	130627.233002	34.618522
1020.401382	130807.704361	34.623540
1021.560860	130973.713003	34.628557
1022.755745	131138.638238	34.633575
1023.622074	131328.535417	34.638592
1024.955053	131500.888461	34.643610
1026.480160	131671.575302	34.648628
1027.184539	131858.784831	34.653645
1028.027007	132025.012079	34.658663
1029.182925	132192.218659	34.663680
1030.198646	132360.539051	34.668698
1031.282990	132536.221469	34.673716
1032.170671	132710.615752	34.678733
1033.495932	132888.634652	34.683751
1033.927847	133074.711971	34.688768
1034.711572	133247.030992	34.693786
1035.505258	133428.269447	34.698804
1036.393169	133631.940719	34.703821
1037.580308	133822.458284	34.708839
1038.378485	134021.425061	34.713856
1039.339632	134211.637064	34.718874
1040.494932	134414.229533	34.723892
1041.106224	134613.862663	34.728909
1042.312561	134817.692511	34.733927
1042.894425	135034.450025	34.738944
1043.935124	135233.028895	34.743962
1044.863586	135446.498310	34.748980
1045.831685	135673.235814	34.753997
1046.616137	135883.379782	34.759015
1047.724584	136107.902170	34.764032
1048.735848	136334.420478	34.769050
1049.649161	136548.976054	34.774068
1050.424165	136785.799641	34.779085
1051.648226	136998.646288	34.784103
1052.393971	137238.052835	34.789120
1053.704094	137466.027337	34.794138
1054.688713	137696.845749	34.799156
1055.538350	137932.508712	34.804173
1057.064235	138161.138110	34.809191
1058.041862	138398.661543	34.814208
1059.251568	138626.124440	34.819226
1060.572588	138860.385779	34.824244
1061.417020	139095.332040	34.829261
1062.569735	139315.015212	34.834279
1063.912664	139543.388081	34.839296
1064.688398	139776.305279	34.844314
1066.363172	140009.907759	34.849332
1067.917201	140229.354649	34.854349
1069.326680	140444.802171	34.859367
1070.165897	140665.302090	34.864384
1071.088601	140887.998178	34.869402
1072.428841	141104.233639	34.874420
1073.177713	141321.654084	34.879437
1074.644333	141538.696617	34.884455
1075.409538	141763.502732	34.889472
1076.724976	141973.451101	34.894490
1078.168612	142185.728194	34.899508
1078.786400	142416.994889	34.904525
1080.153232	142625.364271	34.909543
1081.079513	142848.766771	34.914560
1082.277051	143056.123772	34.919578
1083.354068	143279.403083	34.924596
1083.852327	143505.693088	34.929613
1084.769151	143727.819165	34.934631
1086.032474	143950.018898	34.939648
1086.806883	144179.340125	34.944666
1088.604863	144395.112209	34.949684
1089.398878	144613.656936	34.954701
1090.826587	144812.367351	34.959719
1092.111972	145024.541698	34.964736
1093.062860	145221.678401	34.969754
1094.610274	145428.140045	34.974772
1095.355852	145634.702673	34.979789
1096.203182	145831.921405	34.984807
1097.760454	146050.581263	34.989824
1098.473157	146238.113024	34.994842
1099.577829	146457.949703	34.999860
1099.955123	146677.012719	35.004877
1101.164285	146888.077074	35.009895
1102.268614	147117.677135	35.014912
1103.146778	147338.111471	35.019930
1103.962190	147566.096002	35.024948
1104.988614	147794.835436	35.029965
1106.060022	148019.722910	35.034983
1107.192466	148256.012642	35.040000
1108.231370	148494.272777	35.045018
1109.620993	148715.648230	35.050036
1110.567073	148954.889623	35.055053
1111.596091	149200.478324	35.060071
1112.620309	149446.208525	35.065088
1113.648085	149670.195891	35.070106
1115.140979	149914.166662	35.075124
1116.195161	150159.857342	35.080141
1117.922425	150377.302633	35.085159
1118.928670	150612.556251	35.090176
1120.178249	150856.290088	35.095194
1121.898120	151081.710825	35.100212
1122.815407	151311.510473	35.105229
1123.813404	151550.831340	35.110247
1125.275933	151774.759272	35.115264
1126.053186	152013.837436	35.120282
1127.381841	152242.903778	35.125300
1128.136944	152484.107283	35.130317
1129.455851	152717.201034	35.135335
1130.696396	152950.739612	35.140352
1131.909753	153199.059202	35.145370
1133.088768	153427.379465	35.150388
1134.183361	153669.118812	35.155405
1135.210785	153898.810272	35.160423
1136.127454	154141.188791	35.165440
1137.066303	154384.859674	35.170458
1138.119952	154616.822172	35.175476
1139.381432	154875.360415	35.180493
1140.685786	155108.885126	35.185511
1141.312838	155366.039630	35.190528
1142.272564	155618.827051	35.195546
1143.855989	155867.823803	35.200564
1144.560562	156124.550579	35.205581
1145.829036	156370.920200	35.210599
1147.025068	156623.535297	35.215616
1148.116882	156888.240521	35.220634
1149.496850	157141.197167	35.225652
1150.604408	157414.065035	35.230669
1151.265232	157661.030211	35.235687
1152.613372	157920.850392	35.240704
1153.262175	158185.846496	35.245722
1154.597007	158443.893690	35.250740
1155.610532	158718.432515	35.255757
1156.532364	158979.568074	35.260775
1157.852551	159249.732194	35.265792
1158.958933	159516.452445	35.270810
1160.435446	159773.734010	35.275828
1161.719029	160048.261854	35.280845
1163.021149	160294.781745	35.285863
1164.409820	160547.801866	35.290880
1165.588480	160802.696741	35.295898
1166.850883	161049.035365	35.300916
1168.084377	161288.181015	35.305933
1169.258253	161521.255637	35.310951
1170.826297	161768.349024	35.315968
1171.728340	162006.355841	35.320986
1173.216736	162237.504841	35.326004
1174.310159	162493.308502	35.331021
1175.248253	162726.868750	35.336039
1176.674030	162972.630536	35.341056
1177.208366	163230.314748	35.346074
1178.795451	163476.510226	35.351092
1179.981057	163716.853062	35.356109
1180.934182	163971.237081	35.361127
1182.353380	164220.775317	35.366144
1183.332355	164470.002511	35.371162
1184.914517	164714.959103	35.376180
1186.067935	164965.062263	35.381197
1187.274516	165218.255958	35.386215
1188.386283	165472.874749	35.391232
1189.425431	165728.026417	35.396250
1190.548162	165978.836413	35.401268
1191.736876	166244.999920	35.406285
1192.872318	166505.306924	35.411303
1194.146656	166759.194007	35.416320
1195.326134	167019.330981	35.421338
1196.476332	167280.755884	35.426356
1197.638560	167543.551136	35.431373
1198.764909	167810.923872	35.436391
1200.198353	168069.742573	35.441408
1201.178794	168348.123043	35.446426
1202.640599	168602.381003	35.451444
1203.935989	168867.293389	35.456461
1205.820260	169118.350846	35.461479
1207.269825	169377.781188	35.466496
1208.606556	169641.064681	35.471514
1210.230718	169892.940054	35.476532
1211.634660	170147.199767	35.481549
1212.266848	170387.334718	35.486567
1213.657259	170631.211760	35.491584
1215.022970	170888.755925	35.496602
1216.260784	171136.328065	35.501620
1217.147818	171396.234450	35.506637
1218.216304	171639.593767	35.511655
1219.211073	171897.288319	35.516672
1220.324487	172160.666417	35.521690
1221.459801	172409.985627	35.526708
1222.637989	172671.793514	35.531725
1223.663617	172936.749824	35.536743
1224.883610	173203.720958	35.541760
1226.050247	173481.786603	35.546778
1227.015827	173751.427884	35.551796
1228.020214	174014.118220	35.556813
1229.052277	174293.845817	35.561831
1230.060681	174567.051295	35.566848
1231.218784	174864.411445	35.571866
1232.468003	175148.006331	35.576884
1234.028057	175430.753559	35.581901
1235.433481	175713.462478	35.586919
1236.572308	175991.718911	35.591936
1237.809527	176273.973544	35.596954
1238.410253	176554.843062	35.601972
1240.039658	176844.619150	35.606989
1241.285349	177137.554723	35.612007
1242.512182	177415.662421	35.617024
1243.587256	177704.766313	35.622042
1244.434730	177997.132246	35.627060
1245.855254	178286.006232	35.632077
1247.176824	178576.344315	35.637095
1248.555113	178846.331165	35.642112
1249.481718	179137.748830	35.647130
1250.447589	179417.427632	35.652148
1251.998561	179691.098070	35.657165
1253.315549	179983.803467	35.662183
1254.816704	180266.677433	35.667200
1255.791696	180542.828013	35.672218
1257.305453	180828.978079	35.677236
1258.498477	181112.893420	35.682253
1259.653714	181411.216280	35.687271
1260.988092	181698.133660	35.692288
1261.632848	181997.554229	35.697306
1263.234609	182276.710441	35.702324
1264.334971	182589.624282	35.707341
1265.365712	182886.244197	35.712359
1267.095996	183191.949809	35.717376
1267.945965	183501.553191	35.722394
1269.341224	183795.248771	35.727412
1270.749187	184096.308898	35.732429
1272.144138	184403.162926	35.737447
1273.304530	184707.311523	35.742464
1274.447005	185014.562528	35.747482
1275.440624	185330.829058	35.752500
1276.852108	185645.634199	35.757517
1278.187119	185988.442296	35.762535
1279.604148	186331.848269	35.767552
1281.054215	186655.311615	35.772570
1282.817269	186959.143914	35.777588
1284.068949	187260.999758	35.782605
1285.477822	187582.465796	35.787623
1286.607683	187883.224864	35.792640
1288.054209	188193.206124	35.797658
1289.582899	188504.369190	35.802676
1290.784050	188806.542012	35.807693
1291.830660	189125.199061	35.812711
1293.144272	189432.181964	35.817728
1294.619016	189745.744516	35.822746
1296.003453	190058.941055	35.827764
1297.171399	190361.250195	35.832781
1298.339030	190683.169254	35.837799
1300.175697	190983.216283	35.842816
1301.501138	191302.013464	35.847834
1302.840050	191622.765226	35.852852
1304.086890	191928.139459	35.857869
1305.492106	192240.449454	35.862887
1306.506426	192548.884306	35.867904
1308.076007	192862.211566	35.872922
1309.124608	193185.730711	35.877940
1310.315218	193505.824719	35.882957
1311.689742	193817.559200	35.887975
1313.090214	194131.728872	35.892992
1314.111558	194461.554942	35.898010
1315.050095	194781.158108	35.903028
1316.431899	195104.706051	35.908045
1317.888699	195431.723007	35.913063
1319.382151	195744.510231	35.918080
1320.345035	196077.118135	35.923098
1321.807667	196399.869022	35.928116
1323.407647	196716.477370	35.933133
1324.662502	197057.856216	35.938151
1326.252822	197374.442120	35.943168
1327.626606	197692.231084	35.948186
1329.353081	198010.270342	35.953204
1330.954683	198320.328244	35.958221
1332.357511	198627.090246	35.963239
1334.057394	198931.164562	35.968256
1335.502846	199240.664522	35.973274
1336.439412	199532.996765	35.978292
1338.045808	199814.632030	35.983309
1339.386726	200110.839360	35.988327
1340.753736	200393.249766	35.993344
1341.909297	200680.443971	35.998362
1342.949180	200979.164001	36.003380
1344.671619	201257.303465	36.008397
1345.853373	201549.931145	36.013415
1347.387309	201836.128196	36.018432
1348.438010	202142.596289	36.023450
1349.677266	202437.959919	36.028468
1350.980296	202735.549475	36.033485
1352.538968	203034.445840	36.038503
1354.220514	203332.917016	36.043520
1355.610717	203632.120144	36.048538
1356.112170	203932.707592	36.053556
1357.525328	204231.298405	36.058573
1358.561037	204541.583220	36.063591
1359.866865	204850.962547	36.068608
1361.288468	205172.390576	36.073626
1361.882200	205493.669266	36.078644
1364.014525	205813.361268	36.083661
1365.680041	206125.150298	36.088679
1366.889221	206443.412765	36.093696
1368.440699	206767.337801	36.098714
1369.464348	207082.480262	36.103732
1371.055870	207408.279787	36.108749
1372.289692	207741.578885	36.113767
1373.464779	208062.160663	36.118784
1374.798704	208394.479695	36.123802
1375.988224	208719.429442	36.128820
1377.868699	209047.777116	36.133837
1379.046102	209375.879620	36.138855
1380.468551	209711.895431	36.143872
1381.920092	210046.662353	36.148890
1383.091881	210374.843192	36.153908
1384.800834	210709.214990	36.158925
1386.039426	211057.327873	36.163943
1387.752941	211386.085588	36.168960
1389.164829	211712.756987	36.173978
1390.372217	212058.233969	36.178996
1391.334920	212392.927713	36.184013
1392.620263	212735.598845	36.189031
1394.470334	213087.174828	36.194048
1395.565367	213427.183680	36.199066
1396.760861	213781.022146	36.204084
1398.507503	214120.497814	36.209101
1399.527682	214475.736201	36.214119
1401.009691	214824.500887	36.219136
1402.609450	215162.882714	36.224154
1403.702836	215523.978862	36.229172
1405.387465	215875.939019	36.234189
1406.488710	216234.290924	36.239207
1407.967291	216584.861279	36.244224
1409.433238	216936.577046	36.249242
1410.908237	217295.658776	36.254260
1412.552907	217646.610353	36.259277
1413.869083	218009.883670	36.264295
1415.191268	218357.710685	36.269312
1416.651136	218713.518600	36.274330
1417.820340	219080.575362	36.279348
1419.392859	219437.966494	36.284365
1420.735032	219799.382289	36.289383
1421.997657	220160.353437	36.294400
1423.639952	220524.034358	36.299418
1424.576017	220889.985314	36.304436
1425.968737	221246.135190	36.309453
1427.169491	221616.643119	36.314471
1429.209603	221980.059082	36.319488
1430.350432	222328.144834	36.324506
1431.450110	222687.389498	36.329524
1433.088273	223035.804037	36.334541
1434.004712	223394.112174	36.339559
1435.523294	223746.686417	36.344576
1437.024886	224125.505782	36.349594
1438.185832	224487.383171	36.354612
1439.866369	224854.260075	36.359629
1440.839456	225230.037536	36.364647
1442.054576	225588.857993	36.369664
1444.227458	225964.422247	36.374682
1445.434409	226341.788929	36.379700
1447.216029	226712.816222	36.384717
1448.755882	227084.338579	36.389735
1450.306881	227466.376416	36.394752
1451.823849	227838.867571	36.399770
1453.308554	228214.234346	36.404788
1454.821195	228591.552758	36.409805
1455.876646	228975.750894	36.414823
1457.299649	229355.115410	36.419840
1459.619778	229723.415634	36.424858
1461.037316	230107.302621	36.429876
1463.058723	230474.429892	36.434893
1464.164327	230849.448545	36.439911
1465.698688	231228.388322	36.444928
1467.728668	231589.696178	36.449946
1469.316134	231949.193200	36.454964
1470.585641	232319.155388	36.459981
1472.269725	232689.941587	36.464999
1473.985814	233058.436176	36.470016
1475.409005	233426.950945	36.475034
1476.409510	233794.490039	36.480052
1478.210491	234165.841159	36.485069
1479.262730	234541.678624	36.490087
1480.994838	234918.400106	36.495104
1482.260970	235294.863935	36.500122
1483.433959	235675.584419	36.505140
1485.261259	236044.059144	36.510157
1486.719686	236413.912236	36.515175
1489.007227	236791.230884	36.520192
1491.042353	237138.917178	36.525210
1492.198200	237516.945643	36.530228
1494.012057	237879.704748	36.535245
1495.729163	238236.686576	36.540263
1497.318022	238604.713204	36.545280
1498.774470	238956.298645	36.550298
1500.152766	239317.955676	36.555316
1501.681266	239675.625812	36.560333
1503.146808	240039.300553	36.565351
1504.705971	240397.828681	36.570368
1506.191036	240754.005419	36.575386
1507.734175	241110.553635	36.580404
1509.141696	241476.470986	36.585421
1511.246667	241835.521386	36.590439
1512.563798	242192.433684	36.595456
1514.122900	242544.785821	36.600474
1515.087243	242916.105034	36.605492
1516.827259	243269.545499	36.610509
1518.361104	243630.206740	36.615527
1519.723146	243987.591895	36.620544
1521.129176	244345.909489	36.625562
1522.366298	244714.134649	36.630580
1523.675253	245084.989819	36.635597
1525.066222	245455.806081	36.640615
1526.440266	245839.782946	36.645632
1527.926390	246202.428644	36.650650
1529.349034	246582.027185	36.655668
1530.885652	246941.259635	36.660685
1532.370951	247310.381033	36.665703
1533.619813	247682.485391	36.670720
1535.268817	248031.054480	36.675738
1536.753545	248408.734373	36.680756
1537.686541	248784.340607	36.685773
1539.553770	249156.116478	36.690791
1541.185084	249516.878482	36.695808
1542.258950	249896.041942	36.700826
1543.955834	250275.030821	36.705844
1545.532568	250650.100302	36.710861
1547.068784	251036.326735	36.715879
1548.421072	251420.167827	36.720896
1549.946706	251797.833586	36.725914
1551.630164	252215.913427	36.730932
1553.060563	252586.454227	36.735949
1555.149586	252975.027840	36.740967
1556.529271	253366.785041	36.745984
1558.473492	253766.251109	36.751002
1559.865383	254147.894458	36.756020
1561.788472	254537.480488	36.761037
1562.990936	254928.600687	36.766055
1564.053650	255333.813951	36.771072
1565.965033	255725.760766	36.776090
1567.249940	256135.051842	36.781108
1568.455337	256549.739115	36.786125
1569.752172	256967.154064	36.791143
1571.141897	257384.832531	36.796160
1572.756681	257805.598699	36.801178
1574.090634	258237.329710	36.806196
1575.354734	258674.556680	36.811213
1577.048704	259108.819149	36.816231
1578.423587	259544.654018	36.821248
1579.904035	259980.013565	36.826266
1581.350000	260431.709251	36.831284
1582.867713	260873.308094	36.836301
1585.033470	261332.736243	36.841319
1586.230919	261779.131504	36.846336
1587.833477	262229.830352	36.851354
1589.494240	262679.400664	36.856372
1591.069102	263138.507425	36.861389
1592.972837	263589.966307	36.866407
1594.336764	264054.461452	36.871424
1595.983059	264507.633070	36.876442
1597.560731	264966.426672	36.881460
1599.151560	265432.607296	36.886477
1601.034621	265882.865703	36.891495
1602.753437	266340.919840	36.896512
1604.411770	266797.812991	36.901530
1605.915350	267266.386192	36.906548
1607.852494	267726.914161	36.911565
1609.707101	268178.588814	36.916583
1611.425658	268639.502172	36.921600
1613.300066	269085.759570	36.926618
1614.725768	269539.729847	36.931636
1616.458287	269990.957699	36.936653
1618.087727	270450.656896	36.941671
1619.874645	270903.674936	36.946688
1621.874299	271334.053632	36.951706
1623.787422	271785.142623	36.956724
1625.269621	272227.763266	36.961741
1627.530775	272661.980297	36.966759
1628.703177	273115.083088	36.971776
1630.567212	273548.799040	36.976794
1632.386974	273972.234030	36.981812
1633.747761	274410.875065	36.986829
1635.810781	274838.762779	36.991847
1637.057886	275263.042699	36.996864
1639.291430	275673.782253	37.001882
1641.164580	276075.687505	37.006900
1642.681083	276484.554251	37.011917
1644.480459	276883.394082	37.016935
1645.955173	277290.841049	37.021952
1647.758268	277684.038405	37.026970
1649.426403	278089.851017	37.031988
1650.974713	278497.432522	37.037005
1652.591940	278901.928264	37.042023
1653.928269	279317.715799	37.047040
1654.947888	279730.477829	37.052058
1656.721166	280152.414108	37.057076
1658.352833	280570.891097	37.062093
1659.776601	280998.870368	37.067111
1660.973729	281437.979902	37.072128
1662.589212	281871.206059	37.077146
1663.781245	282302.845271	37.082164
1665.353309	282749.125423	37.087181
1666.777034	283199.336604	37.092199
1668.283109	283661.924038	37.097216
1669.986521	284107.717942	37.102234
1671.956201	284572.461385	37.107252
1673.136204	285045.577982	37.112269
1674.886838	285514.056691	37.117287
1676.345772	285987.732509	37.122304
1678.042739	286459.107810	37.127322
1679.728127	286929.059624	37.132340
1681.267215	287409.213218	37.137357
1682.984895	287891.087391	37.142375
1685.229209	288378.233233	37.147392
1687.292124	288846.030072	37.152410
1689.566538	289324.048495	37.157428
1691.476294	289793.360456	37.162445
1693.279349	290254.560527	37.167463
1695.095603	290729.567716	37.172480
1696.786693	291193.215899	37.177498
1698.245690	291654.205548	37.182516
1699.892406	292125.902410	37.187533
1701.879532	292593.606906	37.192551
1703.550554	293069.456600	37.197568
1705.797910	293535.513519	37.202586
1707.523041	293996.951486	37.207604
1708.764101	294466.408435	37.212621
1710.872341	294935.268939	37.217639
1712.609617	295409.667716	37.222656
1713.816482	295876.325945	37.227674
1716.072731	296349.924931	37.232692
1717.592518	296823.584479	37.237709
1719.374897	297286.104465	37.242727
1721.517854	297757.500731	37.247744
1723.744318	298206.640503	37.252762
1725.124278	298670.684558	37.257780
1726.568449	299149.312275	37.262797
1728.823844	299606.382363	37.267815
1730.020202	300070.544931	37.272832
1731.280017	300542.588806	37.277850
1733.337664	301010.822715	37.282868
1734.590600	301489.764444	37.287885
1736.257242	301964.245407	37.292903
1737.653943	302441.683717	37.297920
1739.909669	302928.629710	37.302938
1741.767516	303397.076948	37.307956
1743.652265	303870.948131	37.312973
1745.687692	304346.339869	37.317991
1747.417016	304818.805149	37.323008
1749.428434	305287.439690	37.328026
1751.246387	305762.446176	37.333044
1752.350090	306227.355732	37.338061
1754.077878	306674.521831	37.343079
1755.728065	307142.561100	37.348096
1757.580023	307591.603297	37.353114
1759.490876	308035.225676	37.358132
1760.814685	308491.652574	37.363149
1762.952267	308953.252777	37.368167
1764.155331	309413.167335	37.373184
1765.882409	309887.057051	37.378202
1767.224008	310342.575412	37.383220
1769.026667	310823.068656	37.388237
1770.606896	311303.871053	37.393255
1772.265249	311782.702024	37.398272
1773.751197	312276.275818	37.403290
1775.730012	312758.041604	37.408308
1776.874869	313268.460027	37.413325
1778.588337	313759.038429	37.418343
1780.094584	314264.414870	37.423360
1782.370924	314776.086157	37.428378
1784.074729	315291.292811	37.433396
1786.032391	315802.647090	37.438413
1787.697764	316313.559109	37.443431
1789.331109	316833.682524	37.448448
1790.800693	317355.551170	37.453466
1792.494118	317873.546649	37.458484
1794.225698	318409.903078	37.463501
1795.862045	318944.466083	37.468519
1797.585499	319485.479888	37.473536
1799.494512	320023.590385	37.478554
1801.388481	320554.236006	37.483572
1803.435798	321102.334776	37.488589
1805.426739	321644.396007	37.493607
1807.065301	322201.552716	37.498624
1809.110081	322735.852156	37.503642
1811.324422	323281.993358	37.508660
1812.733481	323836.296905	37.513677
1814.652497	324372.041299	37.518695
1816.752279	324922.720607	37.523712
1818.807072	325468.350338	37.528730
1820.865805	326008.314061	37.533748
1822.341714	326555.719699	37.538765
1824.385663	327095.950263	37.543783
1826.404856	327652.897205	37.548800
1827.983932	328191.155961	37.553818
1830.412905	328729.934048	37.558836
1832.096701	329286.606028	37.563853
1834.271973	329823.759721	37.568871
1836.461727	330368.742981	37.573888
1837.855516	330913.411845	37.578906
1839.772659	331446.143799	37.583924
1841.596249	331995.727772	37.588941
1843.330433	332531.821894	37.593959
1844.772330	333074.194690	37.598976
1846.809981	333626.714969	37.603994
1849.530653	334158.826502	37.609012
1851.439350	334703.969224	37.614029
1853.279233	335235.061713	37.619047
1855.282352	335783.369978	37.624064
1857.112237	336321.576271	37.629082
1858.892109	336855.673304	37.634100
1860.469176	337399.458302	37.639117
1862.476679	337943.497542	37.644135
1864.004303	338487.679770	37.649152
1865.501878	339044.007726	37.654170
1867.706552	339583.755537	37.659188
1869.411465	340115.406465	37.664205
1871.607942	340661.277037	37.669223
1873.992575	341202.240165	37.674240
1876.386261	341723.867790	37.679258
1878.567196	342219.728261	37.684276
1880.484416	342727.314419	37.689293
1882.474698	343229.327697	37.694311
1883.736805	343736.418246	37.699328
1884.969308	344233.995930	37.704346
1887.009783	344743.815468	37.709364
1888.950991	345269.340296	37.714381
1890.657687	345794.842954	37.719399
1891.769850	346305.798612	37.724416
1893.168432	346846.193151	37.729434
1895.506859	347375.984545	37.734452
1897.175167	347923.926740	37.739469
1898.649185	348471.357790	37.744487
1900.750346	349013.204648	37.749504
1901.881075	349574.515688	37.754522
1903.759199	350130.578335	37.759540
1905.439672	350701.926198	37.764557
1907.190697	351269.272273	37.769575
1909.028665	351846.533626	37.774592
1910.988886	352433.577382	37.779610
1913.010990	353007.163435	37.784628
1914.875052	353593.338887	37.789645
1916.858265	354179.510205	37.794663
1919.159913	354766.229249	37.799680
1920.845935	355353.616737	37.804698
1923.071772	355943.317062	37.809716
1925.311649	356540.457043	37.814733
1927.355977	357109.731143	37.819751
1929.490414	357699.488379	37.824768
1931.549637	358298.751927	37.829786
1933.470971	358883.678043	37.834804
1935.112472	359485.163603	37.839821
1936.695997	360075.062478	37.844839
1939.361189	360680.368981	37.849856
1940.632252	361282.915866	37.854874
1942.557845	361888.516441	37.859892
1944.190912	362490.627437	37.864909
1946.103746	363113.617339	37.869927
1948.437007	363707.990493	37.874944
1950.188524	364330.650383	37.879962
1952.306431	364956.661028	37.884980
1954.077365	365565.225959	37.889997
1956.093743	366191.124491	37.895015
1958.118818	366817.413542	37.900032
1959.449817	367437.943716	37.905050
1961.892654	368062.670381	37.910068
1964.287630	368691.495898	37.915085
1966.129249	369321.154214	37.920103
1968.291136	369942.234486	37.925120
1969.635755	370585.878661	37.930138
1971.955297	371206.196765	37.935156
1974.263926	371845.809691	37.940173
1976.138421	372470.071115	37.945191
1977.908343	373103.253059	37.950208
1979.894188	373741.073682	37.955226
1981.857859	374370.953088	37.960244
1983.925733	374997.508165	37.965261
1985.799736	375630.767188	37.970279
1988.598924	376254.721359	37.975296
1990.465209	376887.952039	37.980314
1993.004438	377507.687208	37.985332
1994.901549	378142.960534	37.990349
1996.883880	378767.895730	37.995367
1999.327118	379374.759658	38.000384
2000.988574	380008.226602	38.005402
2002.905475	380613.193905	38.010420
2004.658433	381233.749775	38.015437
2006.865797	381853.586556	38.020455
2009.094417	382465.148540	38.025472
2010.806040	383062.518082	38.030490
2012.538445	383655.134542	38.035508
2014.623601	384263.915655	38.040525
2016.617777	384856.995129	38.045543
2018.472600	385465.353035	38.050560
2019.778400	386075.478900	38.055578
2021.733057	386683.260074	38.060596
2024.303143	387301.514985	38.065613
2026.012625	387935.512739	38.070631
2028.337434	388551.648057	38.075648
2029.749346	389177.304785	38.080666
2031.443864	389809.332695	38.085684
2033.311371	390438.532230	38.090701
2035.617134	391082.584953	38.095719
2037.386013	391728.274408	38.100736
2039.168274	392393.540077	38.105754
2041.485980	393036.374669	38.110772
2043.168765	393692.556931	38.115789
2045.227239	394356.358290	38.120807
2047.351983	395028.737763	38.125824
2049.723395	395692.908728	38.130842
2051.294308	396347.567478	38.135860
2053.489157	397026.157099	38.140877
2055.577965	397707.882409	38.145895
2057.498037	398387.437616	38.150912
2059.620552	399071.092255	38.155930
2062.214913	399738.910675	38.160948
2064.866017	400415.356513	38.165965
2067.067816	401080.413744	38.170983
2069.536201	401744.650854	38.176000
2071.781064	402411.991075	38.181018
2073.752532	403082.188810	38.186036
2076.428144	403741.578022	38.191053
2078.453474	404408.033730	38.196071
2080.872094	405053.558295	38.201088
2083.091284	405718.021916	38.206106
2085.502273	406371.151214	38.211124
2087.379581	407031.783451	38.216141
2089.198461	407704.144604	38.221159
2091.424616	408356.637372	38.226176
2093.633066	409025.557908	38.231194
2095.942554	409683.766524	38.236212
2097.634457	410341.495472	38.241229
2099.727068	411003.341178	38.246247
2101.717014	411665.840527	38.251264
2103.656388	412344.263426	38.256282
2105.404851	413019.760782	38.261300
2107.406864	413700.255979	38.266317
2108.872062	414389.615414	38.271335
2111.456775	415066.586847	38.276352
2113.626271	415753.364048	38.281370
2115.405595	416435.324361	38.286388
2117.321197	417134.792174	38.291405
2119.418983	417832.690962	38.296423
2121.699895	418520.220539	38.301440
2123.908267	419228.221191	38.306458
2125.647042	419930.910637	38.311476
2127.673753	420628.322530	38.316493
2130.380210	421340.320001	38.321511
2132.293874	422050.090832	38.326528
2134.318455	422765.786449	38.331546
2136.491497	423466.871604	38.336564
2138.260961	424166.478942	38.341581
2140.438449	424884.756010	38.346599
2142.643525	425592.942246	38.351616
2145.069935	426306.175155	38.356634
2146.984917	427011.070731	38.361652
2149.717209	427698.878509	38.366669
2151.412829	428384.549959	38.371687
2153.922232	429060.213373	38.376704
2156.021762	429741.730818	38.381722
2158.408555	430421.157973	38.386740
2160.474030	431094.698297	38.391757
2162.294582	431773.206942	38.396775
2164.987525	432448.422053	38.401792
2166.756370	433140.385545	38.406810
2168.854070	433826.764416	38.411828
2171.150942	434529.663275	38.416845
2173.457387	435207.420011	38.421863
2175.432624	435897.281673	38.426880
2178.044685	436595.255189	38.431898
2179.898102	437301.103134	38.436916
2182.050382	437986.920426	38.441933
2184.097839	438706.630923	38.446951
2186.354287	439404.203172	38.451968
2188.145291	440122.485158	38.456986
2190.168451	440845.047909	38.462004
2192.410853	441558.758619	38.467021
2194.173098	442293.126963	38.472039
2195.821404	443016.371397	38.477056
2198.485194	443757.915503	38.482074
2200.520824	444494.780287	38.487092
2202.452027	445251.733356	38.492109
2204.350968	446009.165242	38.497127
2206.709197	446754.070356	38.502144
2208.859569	447519.783464	38.507162
2211.287421	448286.683266	38.512180
2213.336672	449048.610668	38.517197
2215.205806	449826.944381	38.522215
2218.024812	450601.712815	38.527232
2220.329921	451388.292002	38.532250
2222.383863	452154.933437	38.537268
2225.164198	452926.729015	38.542285
2227.406376	453713.770309	38.547303
2229.473552	454484.448248	38.552320
2231.795089	455259.292730	38.557338
2234.129062	456039.653291	38.562356
2236.475473	456815.131534	38.567373
2238.611401	457605.345694	38.572391
2240.864032	458400.451493	38.577408
2243.174316	459182.541738	38.582426
2245.124209	459966.419044	38.587444
2248.119099	460750.853959	38.592461
2249.861737	461540.444236	38.597479
2252.674304	462328.417717	38.602496
2255.110561	463120.550758	38.607514
2256.932863	463908.656065	38.612532
2259.256680	464684.941604	38.617549
2261.260911	465489.643394	38.622567
2264.067925	466276.121448	38.627584
2266.275953	467069.314585	38.632602
2268.340392	467862.088805	38.637620
2271.131323	468653.248729	38.642637
2273.045424	469447.029682	38.647655
2275.207959	470240.481312	38.652672
2277.808232	471029.337722	38.657690
2280.145626	471830.199149	38.662708
2282.264605	472632.971551	38.667725
2284.505686	473424.692836	38.672743
2286.844087	474208.141526	38.677760
2289.295749	475007.769220	38.682778
2291.644462	475801.928301	38.687796
2294.076831	476590.892744	38.692813
2296.341998	477385.036699	38.697831
2298.921674	478168.102765	38.702848
2301.070898	478931.690341	38.707866
2303.760392	479691.124240	38.712884
2305.951920	480443.896073	38.717901
2308.221671	481195.410045	38.722919
2310.419726	481949.116635	38.727936
2312.823973	482696.959292	38.732954
2314.819172	483465.641760	38.737972
2317.209174	484223.038041	38.742989
2318.789425	484996.647648	38.748007
2321.411722	485772.322764	38.753024
2323.600749	486540.116639	38.758042
2325.940501	487322.005001	38.763060
2328.316670	488092.664118	38.768077
2330.371909	488886.405691	38.773095
2332.654094	489679.616968	38.778112
2335.193934	490468.968765	38.783130
2336.550897	491263.954214	38.788148
2339.537148	492067.254944	38.793165
2341.734063	492876.981559	38.798183
2343.975891	493684.491939	38.803200
2346.652028	494496.321902	38.808218
2349.232141	495305.252467	38.813236
2351.948344	496114.268635	38.818253
2354.205944	496927.793090	38.823271
2356.152674	497744.190843	38.828288
2359.128592	498547.192830	38.833306
2361.173382	499369.576006	38.838324
2363.844871	500179.130248	38.843341
2366.289778	501002.415709	38.848359
2368.521726	501818.238917	38.853376
2371.496569	502642.908417	38.858394
2373.568531	503467.621621	38.863412
2376.080569	504294.785032	38.868429
2377.993873	505119.629362	38.873447
2380.152879	505944.689508	38.878464
2382.534285	506792.307645	38.883482
2384.757374	507645.383637	38.888500
2386.811665	508467.647073	38.893517
2389.125901	509323.223398	38.898535
2391.555752	510197.340676	38.903552
2393.996752	511051.836088	38.908570
2396.016091	511916.504588	38.913588
2398.124691	512776.981580	38.918605
2400.174503	513657.982142	38.923623
2402.852204	514538.778117	38.928640
2405.706406	515410.892116	38.933658
2407.335654	516299.080566	38.938676
2409.451954	517185.224840	38.943693
2412.134838	518085.449872	38.948711
2414.523076	518988.878638	38.953728
2417.402697	519884.278827	38.958746
2419.492903	520787.332720	38.963764
2422.139345	521690.540696	38.968781
2424.542886	522581.011511	38.973799
2427.047561	523475.678712	38.978816
2429.743121	524385.833037	38.983834
2432.402234	525290.052228	38.988852
2434.938347	526184.532502	38.993869
2437.844357	527075.578751	38.998887
2440.313941	527974.067760	39.003904
2443.365049	528861.303365	39.008922
2445.830524	529747.365045	39.013940
2448.345226	530623.515000	39.018957
2451.274945	531495.372788	39.023975
2453.691694	532370.717292	39.028992
2456.948049	533240.849896	39.034010
2458.769019	534104.068642	39.039028
2461.432265	534954.144264	39.044045
2464.017696	535795.139012	39.049063
2466.474840	536626.510200	39.054080
2469.119021	537443.843035	39.059098
2471.409467	538281.758415	39.064116
2473.858410	539109.806431	39.069133
2476.025938	539943.013632	39.074151
2478.053812	540779.750774	39.079168
2480.342503	541607.559623	39.084186
2482.642633	542465.468929	39.089204
2484.920599	543307.919386	39.094221
2487.206312	544174.845333	39.099239
2489.840731	545028.863671	39.104256
2492.370565	545875.264830	39.109274
2494.935792	546746.381838	39.114292
2497.125598	547610.223312	39.119309
2499.551926	548487.759325	39.124327
2501.995010	549362.220965	39.129344
2504.394928	550241.541174	39.134362
2506.181341	551139.446679	39.139380
2508.605767	552036.684735	39.144397
2511.492137	552937.544287	39.149415
2513.630978	553843.917943	39.154432
2516.430406	554753.127797	39.159450
2519.221158	555661.568502	39.164468
2521.428664	556580.055545	39.169485
2524.352389	557500.364621	39.174503
2526.955249	558417.846513	39.179520
2529.815004	559329.204380	39.184538
2532.062648	560253.615000	39.189556
2534.434446	561166.661257	39.194573
2537.271445	562094.292358	39.199591
2539.821401	563038.175136	39.204608
2542.521413	563952.756744	39.209626
2545.373090	564888.629098	39.214644
2547.958219	565823.165789	39.219661
2550.830571	566746.515392	39.224679
2553.422290	567674.992670	39.229696
2556.202861	568607.671584	39.234714
2558.635005	569536.123965	39.239732
2561.129528	570461.387704	39.244749
2563.643514	571395.533634	39.249767
2566.141680	572327.553390	39.254784
2568.943260	573272.461808	39.259802
2571.058812	574209.641978	39.264820
2573.544155	575155.393557	39.269837
2576.141476	576102.049001	39.274855
2578.529656	577056.562375	39.279872
2580.983420	578013.635644	39.284890
2583.279878	578972.952605	39.289908
2585.831631	579942.500859	39.294925
2588.274770	580902.828946	39.299943
2590.799364	581873.913142	39.304960
2593.960097	582837.411713	39.309978
2596.469644	583810.127983	39.314996
2598.924976	584778.516890	39.320013
2601.257801	585745.489541	39.325031
2604.016802	586741.202672	39.330048
2606.820337	587712.176204	39.335066
2609.001121	588689.207669	39.340084
2611.588964	589675.082592	39.345101
2614.386921	590660.085056	39.350119
2616.690093	591657.316090	39.355136
2619.458099	592651.184306	39.360154
2622.268594	593636.561031	39.365172
2624.692994	594630.298845	39.370189
2627.239186	595620.128867	39.375207
2629.530123	596619.645009	39.380224
2632.346327	597600.907440	39.385242
2635.132966	598583.231612	39.390260
2637.387192	599553.964095	39.395277
2639.955976	600526.804047	39.400295
2642.325674	601502.879219	39.405312
2645.038968	602464.683744	39.410330
2647.531171	603445.948258	39.415348
2649.694993	604429.416949	39.420365
2652.284678	605409.482038	39.425383
2654.788515	606411.121646	39.430400
2657.673978	607400.630452	39.435418
2660.165559	608414.798348	39.440436
2662.735868	609413.989114	39.445453
2665.469812	610424.627344	39.450471
2668.148695	611442.155492	39.455488
2670.864659	612457.680816	39.460506
2673.217767	613484.379323	39.465524
2675.782405	614517.919825	39.470541
2678.933027	615554.452755	39.475559
2681.287303	616600.772484	39.480576
2683.886075	617635.780412	39.485594
2686.880062	618678.492769	39.490612
2690.298126	619712.907232	39.495629
2693.538502	620745.049179	39.500647
2696.283612	621778.705057	39.505664
2699.650873	622801.345669	39.510682
2702.458671	623832.285189	39.515700
2705.410898	624850.642881	39.520717
2708.411561	625882.531316	39.525735
2711.205845	626910.409070	39.530752
2714.318637	627933.647366	39.535770
2717.159062	628941.537096	39.540788
2719.574546	629963.873061	39.545805
2722.573116	630985.710678	39.550823
2725.252454	632012.067940	39.555840
2727.906314	633022.594816	39.560858
2731.233181	634054.354076	39.565876
2733.626987	635070.973717	39.570893
2736.351247	636095.590989	39.575911
2739.266347	637124.295406	39.580928
2741.917923	638143.330363	39.585946
2744.676785	639164.177710	39.590964
2747.391712	640193.075565	39.595981
2750.133226	641221.011063	39.600999
2752.666142	642251.003701	39.606016
2756.018848	643272.055633	39.611034
2759.165579	644286.467007	39.616052
2761.226719	645312.516189	39.621069
2764.103012	646336.336403	39.626087
2766.894559	647378.588486	39.631104
2769.784522	648406.548513	39.636122
2772.429140	649448.340172	39.641140
2775.163566	650486.969353	39.646157
2777.875149	651525.334810	39.651175
2780.281598	652559.805877	39.656192
2783.258115	653599.332776	39.661210
2785.847486	654646.942495	39.666228
2788.197251	655700.325431	39.671245
2790.852370	656745.198887	39.676263
2793.731613	657812.843487	39.681280
2796.642180	658877.031141	39.686298
2799.100499	659936.945260	39.691316
2801.761535	661007.714776	39.696333
2804.184749	662074.572802	39.701351
2807.184074	663150.189305	39.706368
2809.676126	664229.870132	39.711386
2812.712293	665298.920486	39.716404
2815.496165	666373.879188	39.721421
2818.365377	667457.268718	39.726439
2820.760299	668519.531908	39.731456
2823.525213	669550.136233	39.736474
2826.371350	670606.969010	39.741492
2828.773169	671667.854887	39.746509
2831.442408	672718.015958	39.751527
2834.363654	673785.694359	39.756544
2837.073142	674851.143360	39.761562
2839.717579	675932.070344	39.766580
2842.052154	677027.913130	39.771597
2845.031261	678106.284070	39.776615
2847.916719	679209.533204	39.781632
2850.434304	680305.518892	39.786650
2853.193649	681410.876797	39.791668
2856.024840	682523.006615	39.796685
2858.651879	683633.289462	39.801703
2861.306529	684768.404850	39.806720
2863.837717	685897.597906	39.811738
2866.599817	687037.037907	39.816756
2869.272988	688186.671287	39.821773
2872.360383	689338.948365	39.826791
2875.477299	690506.188520	39.831808
2878.072557	691663.310343	39.836826
2881.427003	692837.301026	39.841844
2883.813682	694004.949452	39.846861
2886.699976	695194.884234	39.851879
2889.916545	696362.460978	39.856896
2892.713881	697554.930072	39.861914
2895.729032	698746.547632	39.866932
2898.294213	699934.948835	39.871949
2901.695635	701114.946667	39.876967
2904.266535	702331.235233	39.881984
2907.222737	703532.520490	39.887002
2910.581913	704739.138927	39.892020
2913.593123	705937.585868	39.897037
2916.507822	707137.889952	39.902055
2919.593274	708346.322201	39.907072
2922.981454	709564.140060	39.912090
2926.095781	710773.330378	39.917108
2929.219551	711988.101970	39.922125
2931.997851	713189.625595	39.927143
2934.701226	714395.018023	39.932160
2937.832414	715610.950196	39.937178
2941.577156	716817.282851	39.942196
2944.276864	718032.951991	39.947213
2947.249660	719241.687616	39.952231
2950.267789	720449.438381	39.957248
2953.165726	721655.934595	39.962266
2956.581917	722856.546613	39.967284
2959.141350	724068.918964	39.972301
2962.761989	725278.323626	39.977319
2965.655566	726473.131176	39.982336
2968.575096	727672.666802	39.987354
2972.003370	728867.160099	39.992372
2974.784922	730070.665336	39.997389
2978.076213	731267.159986	40.002407
2981.197760	732466.686407	40.007424
2984.181384	733656.896684	40.012442
2986.998265	734844.976503	40.017460
2990.225538	736036.930881	40.022477
2993.336350	737227.089969	40.027495
2996.199861	738417.046889	40.032512
2998.923772	739622.750823	40.037530
3002.288648	740812.242034	40.042548
3004.658261	742016.085481	40.047565
3007.790650	743208.023026	40.052583
3010.570533	744417.887890	40.057600
3013.521813	745613.878402	40.062618
3016.743289	746801.973053	40.067636
3019.636659	747969.608344	40.072653
3022.559595	749129.543305	40.077671
3025.553367	750282.755795	40.082688
3028.136031	751442.272450	40.087706
3031.650422	752606.261460	40.092724
3034.363447	753772.343331	40.097741
3037.620656	754941.139584	40.102759
3040.299571	756112.137603	40.107776
3042.985064	757289.213945	40.112794
3045.532320	758471.407699	40.117812
3048.450193	759675.488984	40.122829
3051.471398	760866.171595	40.127847
3054.743213	762072.578261	40.132864
3057.792200	763285.372932	40.137882
3060.953035	764488.637351	40.142900
3063.974714	765718.000574	40.147917
3066.574805	766926.608217	40.152935
3069.730290	768155.713574	40.157952
3072.699457	769399.941727	40.162970
3075.487425	770626.413303	40.167988
3078.431096	771876.604580	40.173005
3081.566940	773133.285003	40.178023
3084.470310	774388.597089	40.183040
3087.467230	775663.165122	40.188058
3090.745950	776923.375710	40.193076
3093.561575	778201.355362	40.198093
3096.734475	779470.683907	40.203111
3100.078477	780760.845474	40.208128
3103.022238	782043.985313	40.213146
3106.426324	783331.738261	40.218164
3109.595320	784626.796658	40.223181
3112.583161	785912.651767	40.228199
3116.186773	787209.091289	40.233216
3119.209055	788511.612150	40.238234
3122.509328	789812.710823	40.243252
3125.611447	791114.217324	40.248269
3129.109476	792407.408198	40.253287
3131.833896	793713.382083	40.258304
3135.145570	795024.412631	40.263322
3138.455237	796323.923988	40.268340
3141.772194	797628.143187	40.273357
3144.680390	798936.108842	40.278375
3148.635359	800228.550223	40.283392
3151.248681	801546.745701	40.288410
3154.460538	802848.416648	40.293428
3157.630010	804171.437563	40.298445
3160.378109	805483.302751	40.303463
3163.817280	806794.741154	40.308480
3166.839693	808119.738019	40.313498
3170.148438	809437.216433	40.318516
3173.056310	810765.178277	40.323533
3176.180679	812081.647196	40.328551
3179.546696	813412.089559	40.333568
3182.639068	814746.664891	40.338586
3186.089828	816074.195944	40.343604
3189.483041	817402.035991	40.348621
3192.712614	818729.909268	40.353639
3195.999341	820055.061986	40.358656
3199.439211	821374.471002	40.363674
3203.096517	822694.534084	40.368692
3206.069757	824013.159350	40.373709
3209.120075	825330.130964	40.378727
3212.296430	826652.036317	40.383744
3215.407772	827974.344042	40.388762
3219.090444	829289.683035	40.393780
3222.256591	830610.632693	40.398797
3225.461366	831926.733674	40.403815
3228.686049	833233.631769	40.408832
3231.674915	834524.592185	40.413850
3234.880567	835794.905548	40.418868
3238.246048	837077.510323	40.423885
3241.170572	838363.393093	40.428903
3244.232282	839630.202734	40.433920
3246.869368	840925.060383	40.438938
3249.708144	842220.764311	40.443956
3252.924043	843520.960694	40.448973
3256.149592	844833.341552	40.453991
3259.098302	846150.789357	40.459008
3262.188729	847476.713658	40.464026
3265.782482	848798.683561	40.469044
3269.198765	850133.422634	40.474061
3272.186677	851475.745224	40.479079
3275.652149	852816.041090	40.484096
3278.752016	854164.675078	40.489114
3281.115237	855524.979848	40.494132
3283.967589	856910.648872	40.499149
3287.017287	858288.524715	40.504167
3290.430116	859685.975325	40.509184
3293.904383	861089.630485	40.514202
3296.991018	862504.663599	40.519220
3299.965633	863915.603024	40.524237
3302.941471	865354.708572	40.529255
3306.400810	866783.546929	40.534272
3309.690856	868237.470939	40.539290
3313.130226	869680.405159	40.544308
3316.492793	871140.303451	40.549325
3319.622472	872595.622476	40.554343
3323.070346	874060.322964	40.559360
3326.538887	875530.018979	40.564378
3329.934199	877009.527174	40.569396
3333.643696	878476.863025	40.574413
3337.233172	879957.855581	40.579431
3340.624283	881426.182722	40.584448
3344.198698	882911.470224	40.589466
3347.610829	884388.601357	40.594484
3351.060035	885865.805319	40.599501
3354.719945	887353.993266	40.604519
3358.234493	888840.259261	40.609536
3361.643181	890324.885169	40.614554
3364.951422	891806.623755	40.619572
3368.629483	893305.340570	40.624589
3371.614303	894797.995706	40.629607
3375.035353	896291.601578	40.634624
3378.426292	897795.902138	40.639642
3381.785397	899305.621119	40.644660
3384.838511	900817.349466	40.649677
3388.355462	902339.384669	40.654695
3391.650254	903840.445637	40.659712
3394.979344	905374.161357	40.664730
3398.049686	906907.753859	40.669748
3401.533170	908438.918451	40.674765
3404.530117	909974.867263	40.679783
3408.109714	911526.794788	40.684800
3411.646246	913080.458696	40.689818
3415.106291	914635.574722	40.694836
3418.619257	916178.281466	40.699853
3421.394469	917751.264142	40.704871
3424.769555	919306.739971	40.709888
3428.249815	920927.505792	40.714906
3431.997570	922536.526686	40.719924
3435.621947	924150.985242	40.724941
3438.874523	925775.118801	40.729959
3441.964620	927392.174472	40.734976
3445.758349	929015.407444	40.739994
3449.069481	930637.085810	40.745012
3452.826858	932248.624514	40.750016
3456.206166	933824.395946	40.755021
3459.704886	935338.075289	40.760026
3462.756150	936800.951164	40.765031
3466.546710	938191.948624	40.770036
3469.562155	939515.169445	40.775040
3472.098632	940781.464413	40.780045
3475.285835	941964.209712	40.785050
3478.248930	943106.586485	40.790055
3480.445508	944158.587461	40.795060
3482.985510	945150.661526	40.800064
3485.276034	946077.854131	40.805069
3488.015599	946949.852111	40.810074
3490.061031	947757.974933	40.815079
3491.999489	948502.938881	40.820084
3493.963750	949191.970793	40.825088
3495.950626	949834.070198	40.830093
3497.577115	950408.331912	40.835098
3498.923539	950940.329003	40.840103
3501.028514	951425.910653	40.845108
3502.603561	951850.460857	40.850112
3503.447401	952258.021759	40.855117
3504.923457	952605.170281	40.860122
3505.941795	952911.206250	40.865127
3507.179302	953189.003071	40.870132
3508.501138	953428.442431	40.875136
3509.128418	953644.865659	40.880141
3510.110618	953822.116907	40.885146
3510.803696	953958.545061	40.890151
3511.621827	954069.594487	40.895156
3512.466798	954170.690392	40.900160
3513.054927	954242.471211	40.905165
3513.864706	954279.304664	40.910170
3514.223806	954307.236598	40.915175
3514.884656	954307.035866	40.920180
3515.575271	954290.154734	40.925184
3515.758717	954256.676984	40.930189
3516.625429	954197.151779	40.935194
3516.763713	954127.207459	40.940199
3517.262951	954040.139286	40.945204
3517.573716	953939.153164	40.950208
3517.684875	953827.273433	40.955213
3518.331810	953688.779808	40.960218
3518.625171	953544.778771	40.965223
3518.557470	953398.002034	40.970228
3519.273497	953234.127551	40.975232
3518.973513	953068.358835	40.980237
3519.537141	952879.625205	40.985242
3519.359839	952687.099282	40.990247
3519.574000	952505.626331	40.995252
3519.692359	952299.774319	41.000256
3519.625172	952099.504602	41.005261
3519.693710	951884.865274	41.010266
3519.986955	951667.646068	41.015271
3519.983531	951438.659243	41.020276
3520.133327	951217.152294	41.025280
3519.673821	950985.681686	41.030285
3519.642868	950754.915317	41.035290
3519.849734	950524.200011	41.040295
3519.654511	950302.809034	41.045300
3519.766344	950056.670825	41.050304
3519.579103	949811.447101	41.055309
3519.912719	949568.571410	41.060314
3519.690380	949337.582372	41.065319
3519.672060	949078.928978	41.070324
3519.642660	948824.072483	41.075328
3519.135434	948578.748142	41.080333
3519.353676	948321.780535	41.085338
3519.435538	948070.875467	41.090343
3519.216279	947824.985561	41.095348
3519.283972	947571.815277	41.100352
3519.036753	947320.635758	41.105357
3518.826034	947066.412549	41.110362
3518.870563	946815.848707	41.115367
3518.772609	946564.319627	41.120372
3518.648576	946310.732770	41.125376
3518.296878	946063.029840	41.130381
3518.563610	945807.015690	41.135386
3518.397053	945565.903427	41.140391
3518.223278	945319.117099	41.145396
3518.439699	945061.416965	41.150400
3517.958942	944815.633641	41.155405
3518.354059	944558.175924	41.160410
3517.943201	944302.884093	41.165415
3517.442668	944065.179842	41.170420
3517.346266	943819.293570	41.175424
3517.027310	943576.069479	41.180429
3517.082979	943347.823281	41.185434
3517.103922	943100.715283	41.190439
3517.015569	942867.586897	41.195444
3516.955773	942622.816020	41.200448
3516.795244	942388.018147	41.205453
3516.606148	942155.267364	41.210458
3516.617613	941918.371065	41.215463
3516.149136	941685.644844	41.220468
3516.105793	941455.188426	41.225472
3515.840175	941231.208486	41.230477
3515.668643	940998.310142	41.235482
3515.613636	940773.692893	41.240487
3515.593873	940559.032241	41.245492
3515.144900	940329.278170	41.250496
3514.996370	940126.450125	41.255501
3515.211566	939893.055314	41.260506
3515.284415	939678.542706	41.265511
3514.694991	939456.010448	41.270516
3515.072139	939247.593821	41.275520
3514.507218	939037.263497	41.280525
3514.565551	938824.676780	41.285530
3514.652909	938621.367423	41.290535
3514.523010	938405.763189	41.295540
3514.307330	938202.584134	41.300544
3514.124788	937998.708111	41.305549
3513.670020	937790.172928	41.310554
3513.782252	937592.202241	41.315559
3513.356235	937389.125028	41.320564
3513.291982	937190.874645	41.325568
3513.388520	937011.177074	41.330573
3513.328441	936815.945329	41.335578
3513.354790	936620.986890	41.340583
3513.392234	936421.324510	41.345588
3513.157354	936232.067513	41.350592
3512.700013	936047.926259	41.355597
3512.740014	935856.265947	41.360602
3512.359676	935672.883287	41.365607
3512.330923	935500.691455	41.370612
3512.727557	935309.250646	41.375616
3512.184659	935131.844559	41.380621
3512.218664	934950.428816	41.385626
3512.078967	934778.036944	41.390631
3512.000423	934595.257631	41.395636
3512.061747	934424.780842	41.400640
3511.664372	934257.991572	41.405645
3511.719253	934070.673069	41.410650
3511.498753	933905.998945	41.415655
3511.623461	933741.657617	41.420660
3511.633194	933574.686985	41.425664
3511.196010	933404.453575	41.430669
3510.979815	933247.785732	41.435674
3511.147122	933087.432054	41.440679
3510.901997	932925.670109	41.445684
3511.060747	932755.324300	41.450688
3510.516205	932601.333102	41.455693
3510.600590	932442.442732	41.460698
3510.346582	932307.193553	41.465703
3510.294976	932141.365583	41.470708
3510.571867	931987.425317	41.475712
3509.975014	931847.128087	41.480717
3510.045245	931695.561972	41.485722
3509.891697	931563.118824	41.490727
3509.880963	931408.228935	41.495732
3510.175577	931271.303054	41.500736
3509.199227	931133.691355	41.505741
3509.129617	930992.507518	41.510746
3509.572526	930860.640368	41.515751
3509.603935	930726.386480	41.520756
3509.574609	930583.325789	41.525760
3509.343542	930451.162912	41.530765
3509.222822	930313.397813	41.535770
3508.848086	930175.669122	41.540775
3509.172229	930055.749669	41.545780
3509.504297	929922.605221	41.550784
3508.746586	929793.643487	41.555789
3508.568855	929664.979955	41.560794
3508.615808	929534.613409	41.565799
3508.586964	929408.075581	41.570804
3508.764581	929281.306805	41.575808
3508.548259	929159.004495	41.580813
3508.574558	929043.714088	41.585818
3508.249662	928922.599128	41.590823
3508.030202	928808.321945	41.595828
3508.204422	928682.226186	41.600832
3507.798058	928574.536656	41.605837
3507.566786	928451.535936	41.610842
3507.668568	928351.403705	41.615847
3507.589352	928239.052536	41.620852
3507.981210	928135.834327	41.625856
3507.485733	928022.760280	41.630861
3507.631050	927909.877750	41.635866
3507.512445	927796.740350	41.640871
3507.111361	927695.107768	41.645876
3507.503595	927595.504831	41.650880
3507.235957	927493.651882	41.655885
3507.360580	927381.937962	41.660890
3507.252504	927284.465406	41.665895
3506.892729	927179.779879	41.670900
3506.742021	927089.757321	41.675904
3506.560596	926992.095315	41.680909
3506.477124	926878.640427	41.685914
3506.683238	926784.931802	41.690919
3506.729943	926697.027999	41.695924
3506.888980	926604.793658	41.700928
3506.395998	926514.717625	41.705933
3506.810719	926418.226614	41.710938
3506.564767	926336.830731	41.715943
3506.608404	926251.566515	41.720948
3506.497493	926149.273296	41.725952
3506.313721	926057.181778	41.730957
3506.276012	925967.614025	41.735962
3506.185342	925880.797275	41.740967
3506.211610	925802.291409	41.745972
3506.269412	925711.430674	41.750976
3506.277082	925631.651300	41.755981
3506.369958	925551.955513	41.760986
3506.039877	925459.583285	41.765991
3506.143120	925364.397478	41.770996
3506.336539	925276.841133	41.776000
3505.666089	925204.218879	41.781005
3506.065077	925119.078394	41.786010
3505.948164	925047.151768	41.791015
3505.627385	924961.533361	41.796020
3505.651176	924884.485680	41.801024
3505.105718	924801.448562	41.806029
3505.433982	924726.605694	41.811034
3505.597491	924658.649358	41.816039
3505.264769	924582.927700	41.821044
3505.463111	924514.376062	41.826048
3505.577834	924439.072709	41.831053
3505.206273	924358.844859	41.836058
3505.386958	924295.881094	41.841063
3505.052940	924217.507998	41.846068
3505.229657	924151.112138	41.851072
3504.970811	924089.391227	41.856077
3505.435594	924011.674744	41.861082
3505.041651	923940.365830	41.866087
3504.835343	923873.242348	41.871092
3505.310510	923808.854700	41.876096
3505.103974	923749.180798	41.881101
3504.872452	923672.156831	41.886106
3504.976162	923616.256680	41.891111
3504.696930	923551.591919	41.896116
3504.755041	923481.971456	41.901120
3504.493335	923419.851645	41.906125
3504.819874	923351.952481	41.911130
3504.975121	923297.021654	41.916135
3505.138964	923231.891856	41.921140
3505.229654	923155.693068	41.926144
3504.928982	923095.438813	41.931149
3504.985085	923029.833320	41.936154
3504.756384	922974.273071	41.941159
3504.894120	922903.652650	41.946164
3504.512414	922834.975627	41.951168
3504.549016	922784.765153	41.956173
3504.411400	922718.401947	41.961178
3504.714330	922661.873065	41.966183
3504.352819	922607.016450	41.971188
3504.584513	922534.709813	41.976192
3504.255603	922488.966645	41.981197
3504.378886	922424.520512	41.986202
3504.376135	922365.584941	41.991207
3504.102652	922309.534970	41.996212
3504.321810	922269.294080	42.001216
3503.837284	922208.667037	42.006221
3504.343848	922152.297470	42.011226
3504.237598	922100.142021	42.016231
3503.996694	922048.007150	42.021236
3504.153576	921987.179446	42.026240
3504.382967	921940.462023	42.031245
3504.154060	921878.320483	42.036250
3504.439240	921826.689810	42.041255
3504.225581	921776.019318	42.046260
3504.180234	921716.593412	42.051264
3503.951719	921674.653012	42.056269
3504.106491	921618.921690	42.061274
3503.746885	921573.372212	42.066279
3503.764039	921527.959635	42.071284
3504.331612	921472.848923	42.076288
3503.700536	921432.538955	42.081293
3503.866611	921369.937879	42.086298
3504.186240	921327.222704	42.091303
3504.095982	921273.684148	42.096308
3503.813604	921210.072535	42.101312
3503.646023	921174.788651	42.106317
3503.675004	921124.957271	42.111322
3503.773276	921080.803603	42.116327
3503.689310	921042.661355	42.121332
3503.552773	920986.380950	42.126336
3503.284075	920957.487215	42.131341
3503.147789	920919.940861	42.136346
3503.531077	920872.307951	42.141351
3503.534777	920837.191407	42.146356
3503.220897	920789.372524	42.151360
3503.180794	920751.810042	42.156365
3503.207921	920703.937145	42.161370
3503.394839	920671.341347	42.166375
3503.380682	920632.596922	42.171380
3503.624311	920585.375853	42.176384
3503.380233	920548.334404	42.181389
3503.620973	920506.017873	42.186394
3503.593408	920457.366720	42.191399
3503.703747	920419.680466	42.196404
3503.743627	920376.903904	42.201408
3503.167198	920338.343497	42.206413
3503.111065	920290.872586	42.211418
3503.354804	920251.300498	42.216423
3503.017871	920219.863140	42.221428
3503.270286	920174.305046	42.226432
3503.090794	920141.861642	42.231437
3502.833955	920102.366783	42.236442
3503.243989	920079.052482	42.241447
3502.877255	920042.517473	42.246452
3502.706698	920000.948263	42.251456
3502.897527	919973.645537	42.256461
3503.208986	919933.275851	42.261466
3503.359918	919899.209749	42.266471
3502.731337	919857.416786	42.271476
3503.111084	919829.102781	42.276480
3502.976016	919791.745116	42.281485
3502.635289	919761.777468	42.286490
3502.774486	919733.696816	42.291495
3502.848487	919696.992616	42.296500
3502.660181	919659.446198	42.301504
3502.428210	919650.652657	42.306509
3502.734299	919615.775752	42.311514
3503.119389	919577.648618	42.316519
3502.803222	919561.509756	42.321524
3502.514021	919524.665014	42.326528
3502.640206	919505.121034	42.331533
3502.598002	919470.886374	42.336538
3502.990890	919437.270294	42.341543
3502.761693	919417.683458	42.346548
3502.751015	919383.345238	42.351552
3502.892198	919356.537933	42.356557
3502.871549	919315.038469	42.361562
3502.716212	919280.624136	42.366567
3502.793968	919260.890668	42.371572
3503.377670	919224.220702	42.376576
3502.747515	919192.572159	42.381581
3502.660830	919160.742839	42.386586
3502.884697	919129.438528	42.391591
3502.815957	919100.187909	42.396596
3502.742648	919070.459703	42.401600
3502.477926	919044.108191	42.406605
3502.463220	919016.952440	42.411610
3502.543991	918980.696950	42.416615
3502.397085	918956.526015	42.421620
3502.618035	918931.054284	42.426624
3502.554419	918923.031465	42.431629
3502.605038	918888.501358	42.436634
3502.714103	918867.350142	42.441639
3502.397692	918834.215865	42.446644
3502.530851	918806.844617	42.451648
3502.876419	918783.934720	42.456653
3502.799032	918766.733138	42.461658
3502.982228	918733.711373	42.466663
3502.442581	918702.906323	42.471668
3502.716465	918663.366850	42.476672
3502.555351	918648.377541	42.481677
3502.671644	918619.764677	42.486682
3502.822946	918583.208428	42.491687
3502.640000	918559.423782	42.496692
3502.753705	918522.872977	42.501696
3502.666680	918503.089817	42.506701
3502.698058	918467.699131	42.511706
3502.675348	918429.447499	42.516711
3502.357148	918415.629721	42.521716
3502.249447	918385.615975	42.526720
3502.438531	918372.292618	42.531725
3502.281926	918343.912144	42.536730
3502.718443	918328.828473	42.541735
3502.479463	918307.824981	42.546740
3502.767310	918277.079279	42.551744
3502.230738	918254.113615	42.556749
3502.226526	918233.073116	42.561754
3502.286909	918198.249878	42.566759
3501.658939	918190.218479	42.571764
3501.976357	918170.275161	42.576768
3502.342609	918158.453846	42.581773
3502.243398	918139.436327	42.586778
3501.945489	918111.267932	42.591783
3501.913651	918104.386588	42.596788
3502.255259	918071.909642	42.601792
3501.844793	918067.765501	42.606797
3501.933258	918045.848935	42.611802
3502.046381	918027.945556	42.616807
3502.060210	918009.292465	42.621812
3502.197502	917988.515777	42.626816
3502.081295	917982.508278	42.631821
3501.831948	917952.514122	42.636826
3501.941949	917945.227801	42.641831
3501.992911	917929.246745	42.646836
3502.058512	917909.341772	42.651840
3502.302600	917891.800038	42.656845
3501.943574	917868.709229	42.661850
3502.105048	917846.780395	42.666855
3501.920553	917835.713973	42.671860
3501.961282	917815.716873	42.676864
3502.006097	917796.292959	42.681869
3501.863679	917792.871894	42.686874
3501.958055	917756.509918	42.691879
3501.813090	917750.315338	42.696884
3501.989864	917734.505308	42.701888
3501.559858	917722.233547	42.706893
3501.633293	917710.265666	42.711898
3501.572554	917703.483951	42.716903
3501.293089	917685.640740	42.721908
3501.611769	917678.034461	42.726912
3501.724275	917686.721345	42.731917
3501.487907	917663.993044	42.736922
3501.711698	917653.818932	42.741927
3501.708879	917649.228112	42.746932
3501.957153	917639.050144	42.751936
3501.956261	917626.232805	42.756941
3501.645966	917616.716029	42.761946
3501.956543	917578.979839	42.766951
3501.736663	917571.361934	42.771956
3502.166184	917550.155163	42.776960
3501.858016	917532.889834	42.781965
3501.784872	917523.814090	42.786970
3501.824536	917504.198558	42.791975
3501.529722	917492.574699	42.796980
3501.774873	917486.892753	42.801985
3501.731890	917464.707270	42.806989
3501.394280	917452.994354	42.811994
3502.162942	917448.569726	42.816999
3501.835401	917432.454968	42.822004
3501.373297	917415.308961	42.827009
3501.687752	917426.643131	42.832013
3501.512085	917407.539175	42.837018
3501.603707	917379.305840	42.842023
3501.683761	917375.084451	42.847028
3501.799138	917365.787640	42.852033
3501.640485	917354.620474	42.857037
3501.611025	917347.355101	42.862042
3501.555239	917340.285152	42.867047
3501.418473	917326.436051	42.872052
3501.935395	917313.154345	42.877057
3501.396823	917313.429942	42.882061
3501.468205	917287.208110	42.887066
3501.737616	917265.355568	42.892071
3501.760261	917268.413248	42.897076
3501.710172	917263.064186	42.902081
3502.081925	917240.238934	42.907085
3501.951396	917222.657803	42.912090
3501.373658	917208.590330	42.917095
3501.440876	917202.935884	42.922100
3501.445543	917199.108780	42.927105
3501.186427	917193.027027	42.932109
3501.380720	917193.762038	42.937114
3501.550398	917177.281762	42.942119
3501.332547	917174.350381	42.947124
3501.455960	917155.103065	42.952129
3501.501216	917154.904755	42.957133
3501.176025	917141.084604	42.962138
3501.620239	917122.839309	42.967143
3501.376431	917117.616040	42.972148
3501.013915	917113.750607	42.977153
3501.353207	917120.872394	42.982157
3501.225022	917104.725435	42.987162
3501.562103	917102.281246	42.992167
3500.982778	917102.754548	42.997172
3501.281055	917088.741133	43.002177
3501.206549	917098.127900	43.007181
3501.260461	917092.858066	43.012186
3501.141317	917090.102534	43.017191
3501.622359	917091.749372	43.022196
3501.864596	917073.535475	43.027201
3501.616956	917068.982402	43.032205
3501.447325	917064.034475	43.037210
3501.528442	917034.078920	43.042215
3501.182204	917030.880531	43.047220
3501.553357	917031.109596	43.052225
3501.310136	917026.460129	43.057229
3501.090763	917021.328606	43.062234
3501.532476	917006.335894	43.067239
3501.480876	917006.631045	43.072244
3501.220491	916993.470020	43.077249
3501.406710	916992.867006	43.082253
3501.361955	916992.587095	43.087258
3501.566068	916975.431127	43.092263
3501.405408	916962.158767	43.097268
3501.259048	916963.999389	43.102273
3501.579922	916951.130057	43.107277
3501.418447	916945.606742	43.112282
3501.482567	916928.663834	43.117287
3501.234454	916932.051040	43.122292
3501.397347	916923.893997	43.127297
3501.272288	916922.478633	43.132301
3501.404728	916914.900337	43.137306
3501.813033	916895.033507	43.142311
3501.608746	916899.944560	43.147316
3501.619645	916891.524223	43.152321
3501.505437	916867.529598	43.157325
3501.550724	916852.407070	43.162330
3501.494162	916864.374499	43.167335
3501.579030	916867.135689	43.172340
3501.453047	916840.464078	43.177345
3501.566403	916827.339870	43.182349
3501.308398	916833.024732	43.187354
3501.672660	916827.801780	43.192359
3501.261498	916808.445386	43.197364
3501.172387	916788.464560	43.202369
3501.487739	916784.014564	43.207373
3501.277523	916788.543972	43.212378
3501.614660	916780.742141	43.217383
3501.509871	916768.512907	43.222388
3501.257957	916751.523144	43.227393
3501.374897	916749.591553	43.232397
3501.005441	916746.492283	43.237402
3501.318683	916739.268145	43.242407
3501.369403	916742.130411	43.247412
3501.542910	916711.871515	43.252417
3501.567555	916722.295850	43.257421
3501.490934	916715.802316	43.262426
3501.871782	916713.255433	43.267431
3501.790519	916696.812837	43.272436
3501.629369	916676.651493	43.277441
3501.567883	916680.105362	43.282445
3501.105894	916652.241564	43.287450
3501.396931	916637.845361	43.292455
3501.306418	916650.392630	43.297460
3501.463886	916650.463776	43.302465
3501.204353	916646.964574	43.307469
3500.966798	916633.607706	43.312474
3501.396120	916618.041764	43.317479
3501.386920	916617.469256	43.322484
3501.525630	916616.586609	43.327489
3501.542463	916615.531669	43.332493
3501.195047	916623.431207	43.337498
3501.063888	916593.123561	43.342503
3501.011819	916582.990446	43.347508
3501.260982	916568.409247	43.352513
3501.376545	916583.220630	43.357517
3501.369102	916577.385817	43.362522
3501.341471	916580.451768	43.367527
3501.293965	916569.935221	43.372532
3501.375690	916549.257040	43.377537
3501.371815	916559.016451	43.382541
3501.372977	916560.451462	43.387546
3501.513432	916546.461235	43.392551
3501.381760	916544.281408	43.397556
3501.353322	916524.481413	43.402561
3501.358970	916534.430730	43.407565
3501.321411	916522.381745	43.412570
3501.357350	916517.209802	43.417575
3501.393729	916505.914615	43.422580
3501.401560	916496.633036	43.427585
3501.500358	916491.642591	43.432589
3501.357833	916486.689864	43.437594
3501.799892	916484.994377	43.442599
3501.368846	916463.439255	43.447604
3501.760241	916455.532774	43.452609
3501.753835	916451.993869	43.457613
3501.019890	916439.096789	43.462618
3501.336085	916424.217674	43.467623
3501.275161	916424.801343	43.472628
3501.184112	916424.432960	43.477633
3501.026147	916426.753968	43.482637
3501.343357	916423.834188	43.487642
3501.283430	916421.547417	43.492647
3501.253742	916403.373643	43.497652
3501.564069	916389.739140	43.502657
3501.732983	916400.141581	43.507661
3501.070445	916400.053883	43.512666
3501.148123	916390.091457	43.517671
3501.316120	916376.096459	43.522676
3501.443180	916363.542981	43.527681
3501.534287	916356.448707	43.532685
3501.251567	916363.477434	43.537690
3501.332727	916364.038900	43.542695
3501.462978	916343.352302	43.547700
3501.479483	916318.473567	43.552705
3501.070376	916332.602267	43.557709
3501.054618	916332.030752	43.562714
3501.308730	916329.407816	43.567719
3501.295709	916337.351199	43.572724
3501.463047	916313.309960	43.577729
3501.340416	916299.168827	43.582733
3501.427097	916291.309726	43.587738
3501.282480	916292.289207	43.592743
3501.401827	916306.526729	43.597748
3501.626901	916279.797315	43.602753
3501.425591	916267.390611	43.607757
3501.350809	916259.843739	43.612762
3501.681007	916272.039133	43.617767
3501.369331	916253.047794	43.622772
3501.275732	916236.797004	43.627777
3501.313097	916240.140038	43.632781
3501.626120	916235.976972	43.637786
3501.359951	916222.145102	43.642791
3500.991345	916209.477369	43.647796
3501.355117	916197.364883	43.652801
3501.452506	916198.689272	43.657805
3501.438140	916202.327458	43.662810
3501.849911	916197.383484	43.667815
3501.604370	916187.758230	43.672820
3501.667208	916168.133948	43.677825
3501.702865	916170.520485	43.682829
3501.417566	916145.113999	43.687834
3501.785773	916128.503633	43.692839
3501.459261	916132.190663	43.697844
3501.385505	916119.093888	43.702849
3501.312291	916100.543114	43.707853
3501.215185	916095.678589	43.712858
3501.834253	916094.050990	43.717863
3501.261450	916102.464971	43.722868
3501.460051	916088.464404	43.727873
3501.596983	916071.028862	43.732877
3501.522973	916062.811800	43.737882
3501.382352	916065.417307	43.742887
3501.421283	916063.880385	43.747892
3501.697153	916035.228096	43.752897
3501.394089	916024.367642	43.757901
3501.385938	916033.937355	43.762906
3501.650285	916023.083884	43.767911
3501.439845	916004.458529	43.772916
3501.383226	915996.430009	43.777921
3501.493822	915990.576076	43.782925
3501.309195	915993.762603	43.787930
3501.542436	915980.426116	43.792935
3501.279538	915968.793789	43.797940
3501.490931	915963.306806	43.802945
3501.764795	915971.014542	43.807949
3501.445390	915944.751230	43.812954
3501.694479	915926.819240	43.817959
3501.429625	915926.095247	43.822964
3501.469758	915923.027128	43.827969
3501.614253	915903.580438	43.832973
3501.566446	915898.038218	43.837978
3501.890442	915886.792391	43.842983
3501.502011	915879.676732	43.847988
3501.739404	915869.401268	43.852993
3501.547264	915868.378840	43.857997
3501.391509	915861.035410	43.863002
3501.592141	915839.474595	43.868007
3501.454092	915829.066365	43.873012
3501.417130	915831.560099	43.878017
3501.420075	915831.176978	43.883021
3501.360088	915808.030089	43.888026
3501.381625	915793.195206	43.893031
3501.229045	915788.243371	43.898036
3501.038627	915789.899922	43.903041
3501.399919	915796.733064	43.908045
3501.273070	915796.274542	43.913050
3501.541716	915782.070814	43.918055
3500.717066	915766.985377	43.923060
3500.875433	915770.501180	43.928065
3501.108591	915759.077897	43.933069
3501.206745	915758.871265	43.938074
3501.273577	915766.228920	43.943079
3501.080303	915769.225561	43.948084
3501.265822	915759.532116	43.953089
3501.294510	915765.364718	43.958093
3501.150459	915751.225417	43.963098
3501.171498	915734.763735	43.968103
3501.625677	915742.922075	43.973108
3501.334553	915737.034959	43.978113
3501.692350	915737.744629	43.983117
3501.763167	915719.648405	43.988122
3501.363639	915703.252363	43.993127
3501.739252	915702.428220	43.998132
3501.623961	915682.351474	44.003137
3501.723664	915668.556601	44.008141
3501.235378	915663.561432	44.013146
3501.605271	915651.446703	44.018151
3501.624052	915644.745512	44.023156
3501.446645	915632.620602	44.028161
3501.486752	915626.107434	44.033165
3501.262645	915624.324425	44.038170
3501.479692	915621.515544	44.043175
3501.474627	915596.062523	44.048180
3501.585542	915593.940058	44.053185
3501.604391	915589.726767	44.058189
3501.501650	915584.766944	44.063194
3501.364465	915566.511310	44.068199
3501.299403	915559.631729	44.073204
3501.420526	915551.957496	44.078209
3501.933018	915550.155009	44.083213
3501.437809	915535.400157	44.088218
3501.687876	915518.136435	44.093223
3501.348401	915516.275728	44.098228
3501.588558	915511.836392	44.103233
3501.747659	915490.280602	44.108237
3501.340073	915487.377902	44.113242
3501.195098	915479.458076	44.118247
3501.246666	915478.875941	44.123252
3501.410484	915464.496334	44.128257
3501.609374	915463.029922	44.133261
3501.427563	915446.599023	44.138266
3501.722556	915447.892720	44.143271
3501.251735	915452.559734	44.148276
3501.556612	915418.349194	44.153281
3501.776167	915413.147434	44.158285
3501.158153	915416.689149	44.163290
3501.625271	915401.592090	44.168295
3501.527944	915386.678915	44.173300
3501.137130	915379.084449	44.178305
3501.387914	915379.619509	44.183309
3501.598696	915383.223082	44.188314
3501.720176	915352.103026	44.193319
3501.650847	915359.004071	44.198324
3501.450160	915345.350981	44.203329
3501.500998	915325.246865	44.208333
3501.170445	915321.279364	44.213338
3501.239940	915314.569814	44.218343
3501.210003	915308.258586	44.223348
3501.166546	915306.255831	44.228353
3501.279419	915312.458577	44.233357
3501.324392	915300.585207	44.238362
3501.331281	915275.702909	44.243367
3501.348140	915278.092801	44.248372
3501.353711	915271.584583	44.253377
3501.643602	915272.592030	44.258381
3501.727915	915259.851138	44.263386
3501.219046	915243.566409	44.268391
3501.172931	915243.382310	44.273396
3501.174025	915242.329548	44.278401
3501.191313	915249.982785	44.283405
3501.114907	915239.563718	44.288410
3501.683553	915225.120159	44.293415
3501.628145	915216.420336	44.298420
3501.586535	915208.101136	44.303425
3501.575062	915202.456784	44.308429
3501.259339	915181.069617	44.313434
3501.389939	915167.555665	44.318439
3501.413633	915174.633815	44.323444
3501.446481	915165.154513	44.328449
3501.576950	915153.650237	44.333453
3501.494345	915152.132041	44.338458
3501.847054	915135.042386	44.343463
3501.540961	915134.611822	44.348468
3501.283062	915115.607847	44.353473
3501.291143	915100.581662	44.358477
3501.485681	915101.699750	44.363482
3501.488957	915093.660451	44.368487
3501.380615	915086.787001	44.373492
3501.307075	915069.763760	44.378497
3501.383781	915066.115203	44.383501
3501.062238	915065.112838	44.388506
3501.272828	915069.099470	44.393511
3501.180281	915076.100225	44.398516
3501.200883	915059.636442	44.403521
3501.254092	915038.286709	44.408525
3501.108945	915033.332980	44.413530
3500.976735	915030.482672	44.418535
3501.166024	915037.726530	44.423540
3501.308964	915031.005129	44.428545
3501.352293	915032.912487	44.433549
3501.211704	915039.825100	44.438554
3501.235023	915029.294315	44.443559
3501.286059	915009.667441	44.448564
3501.197171	915005.853321	44.453569
3501.375255	915002.284574	44.458573
3500.912057	915006.567986	44.463578
3500.980384	914999.571099	44.468583
3500.900713	915007.048450	44.473588
3500.846538	915007.248412	44.478593
3501.196650	915006.715259	44.483597
3501.184211	915008.248534	44.488602
3501.182968	914993.510599	44.493607
3501.113283	914985.386832	44.498612
3501.051529	914978.888766	44.503617
3501.288214	914977.894826	44.508621
3501.032765	914981.093048	44.513626
3501.184695	914974.752981	44.518631
3501.488477	914982.074724	44.523636
3501.098839	914975.627908	44.528641
3501.138340	914965.955791	44.533645
3500.791465	914955.291315	44.538650
3501.137221	914950.356472	44.543655
3501.207294	914949.484274	44.548660
3501.075049	914948.452295	44.553665
3501.207037	914964.509946	44.558669
3501.379214	914957.018250	44.563674
3501.434262	914947.726483	44.568679
3501.492350	914955.086672	44.573684
3501.402652	914927.538081	44.578689
3501.315856	914917.789913	44.583693
3501.174658	914927.669603	44.588698
3501.374001	914921.800578	44.593703
3501.188701	914919.341324	44.598708
3501.273128	914895.880624	44.603713
3501.390029	914888.780289	44.608717
3501.048782	914896.585804	44.613722
3501.367031	914889.836814	44.618727
3501.446888	914898.246434	44.623732
3501.070776	914875.240449	44.628737
3501.197252	914855.984015	44.633741
3501.132777	914868.914397	44.638746
3501.602168	914858.887764	44.643751
3501.251156	914859.995481	44.648756
3501.138983	914866.903884	44.653761
3501.211755	914863.255798	44.658765
3501.371730	914860.933953	44.663770
3501.587637	914842.046309	44.668775
3501.094037	914840.687971	44.673780
3501.364145	914827.055609	44.678785
3501.384686	914828.200959	44.683789
3501.149093	914817.040268	44.688794
3501.209147	914795.114217	44.693799
3500.902412	914799.469047	44.698804
3501.197799	914788.608119	44.703809
3500.980754	914789.312082	44.708813
3501.109062	914800.489781	44.713818
3501.221263	914794.921353	44.718823
3501.114561	914805.752951	44.723828
3501.397089	914803.124803	44.728833
3501.250968	914791.375833	44.733837
3501.211105	914789.180900	44.738842
3501.104339	914772.161864	44.743847
3501.344143	914778.919658	44.748852
3501.059846	914769.872029	44.753857
3501.089874	914773.025755	44.758861
3501.023414	914780.309956	44.763866
3501.404944	914772.019611	44.768871
3501.165207	914758.658181	44.773876
3501.340214	914746.380372	44.778881
3501.355431	914737.190158	44.783885
3501.285508	914729.544561	44.788890
3501.234377	914734.146614	44.793895
3501.327369	914745.138538	44.798900
3501.077466	914736.372596	44.803905
3501.324823	914714.034088	44.808909
3501.144833	914707.075619	44.813914
3501.164387	914699.703115	44.818919
3501.246395	914709.931166	44.823924
3501.284981	914701.215775	44.828929
3501.237619	914709.645591	44.833933
3500.901922	914712.473691	44.838938
3501.199899	914697.305299	44.843943
3501.134960	914680.566546	44.848948
3501.268802	914671.931924	44.853953
3501.413836	914672.387885	44.858957
3501.308017	914677.955625	44.863962
3501.334625	914678.334390	44.868967
3501.189995	914677.591417	44.873972
3501.107437	914662.865244	44.878977
3501.429422	914642.524648	44.883981
3501.268282	914642.454217	44.888986
3501.337687	914636.796599	44.893991
3501.240903	914648.775491	44.898996
3500.899926	914647.297532	44.904001
3501.647988	914642.969473	44.909005
3501.395109	914626.164212	44.914010
3501.486229	914607.678052	44.919015
3501.117758	914606.108668	44.924020
3500.849849	914612.371787	44.929025
3501.358194	914621.480560	44.934029
3501.161980	914614.620211	44.939034
3501.398265	914592.570037	44.944039
3501.475938	914581.742705	44.949044
3501.104665	914569.167026	44.954049
3501.275824	914561.962047	44.959053
3501.154050	914577.582024	44.964058
3501.232483	914564.361771	44.969063
3501.401937	914550.074434	44.974068
3501.150891	914544.466807	44.979073
3501.560977	914548.135528	44.984077
3501.039555	914548.217125	44.989082
3501.486567	914540.107594	44.994087
3501.563695	914540.861316	44.999092
3501.397422	914516.959518	45.004097
3501.300503	914523.961709	45.009101
3501.049406	914511.462813	45.014106
3501.222831	914508.468725	45.019111
3501.148319	914510.873258	45.024116
3501.497164	914503.257574	45.029121
3501.550086	914482.479846	45.034125
3501.289407	914481.276422	45.039130
3501.235946	914473.053595	45.044135
3501.241585	914482.145487	45.049140
3501.189577	914479.760895	45.054145
3501.257542	914456.875038	45.059149
3500.842000	914455.025826	45.064154
3501.398705	914441.730495	45.069159
3501.390500	914444.411834	45.074164
3501.213651	914454.776570	45.079169
3501.372825	914442.691938	45.084173
3501.061834	914430.202206	45.089178
3501.245241	914423.856540	45.094183
3501.184699	914410.561902	45.099188
3501.176929	914419.368861	45.104193
3501.233009	914424.624426	45.109197
3501.255315	914434.479505	45.114202
3501.280824	914430.934214	45.119207
3501.196860	914416.398979	45.124212
3500.807139	914398.752939	45.129217
3500.842196	914385.730436	45.134221
3501.082981	914394.020012	45.139226
3501.555825	914377.961919	45.144231
3501.350664	914382.875507	45.149236
3501.057207	914389.525746	45.154241
3501.270973	914389.779562	45.159245
3500.999863	914390.204887	45.164250
3501.300809	914382.213655	45.169255
3501.114287	914365.588595	45.174260
3500.933308	914356.236938	45.179265
3500.782558	914355.494874	45.184269
3500.949336	914353.554597	45.189274
3500.892809	914357.583541	45.194279
3501.148315	914353.045097	45.199284
3500.573684	914363.376484	45.204289
3501.354963	914358.181567	45.209293
3501.360726	914364.402207	45.214298
3501.147651	914363.287028	45.219303
3501.351791	914368.806650	45.224308
3501.341422	914354.834024	45.229313
3501.230503	914340.877077	45.234317
3501.061720	914338.606389	45.239322
3501.093864	914332.284255	45.244327
3500.943730	914329.436356	45.249332
3501.062629	914329.705005	45.254337
3501.357388	914332.339043	45.259341
3500.962819	914341.876604	45.264346
3501.291866	914337.135219	45.269351
3500.977484	914319.189983	45.274356
3501.227905	914303.836436	45.279361
3501.389868	914301.035450	45.284365
3500.917867	914303.693647	45.289370
3501.113126	914310.363308	45.294375
3501.329283	914311.956773	45.299380
3501.291660	914310.527009	45.304385
3501.588825	914310.097783	45.309389
3501.286077	914288.992007	45.314394
3501.230389	914268.613255	45.319399
3501.046689	914278.692269	45.324404
3500.665547	914277.986207	45.329409
3501.332921	914273.287594	45.334413
3501.191691	914278.861301	45.339418
3501.175776	914263.740699	45.344423
3501.147149	914276.666968	45.349428
3500.967064	914269.899352	45.354433
3501.337999	914247.826650	45.359437
3501.025309	914248.354202	45.364442
3501.193695	914240.574907	45.369447
3500.976980	914239.747420	45.374452
3500.894006	914240.717648	45.379457
3501.036305	914245.768485	45.384461
3501.253339	914241.235956	45.389466
3500.935397	914240.902878	45.394471
3500.966162	914245.205416	45.399476
3501.015741	914245.102037	45.404481
3501.520549	914222.816868	45.409485
3500.895114	914221.096097	45.414490
3501.088550	914211.302779	45.419495
3500.915575	914220.040186	45.424500
3500.846785	914214.499423	45.429505
3500.823783	914206.558559	45.434509
3501.333976	914222.463697	45.439514
3501.109305	914216.564434	45.444519
3501.239535	914218.649947	45.449524
3501.120406	914217.615767	45.454529
3501.287685	914224.289915	45.459533
3501.089142	914204.603260	45.464538
3501.227529	914192.999879	45.469543
3501.405032	914189.717815	45.474548
3501.286994	914191.746429	45.479553
3501.215147	914193.193516	45.484557
3501.157178	914186.119546	45.489562
3501.324687	914184.466246	45.494567
3501.281629	914164.180823	45.499572
3501.065146	914148.899799	45.504577
3501.337236	914147.038701	45.509581
3501.266994	914148.772705	45.514586
3501.034122	914150.532131	45.519591
3500.921615	914158.111568	45.524596
3501.319793	914161.112403	45.529601
3501.346528	914152.493652	45.534605
3500.949507	914132.837747	45.539610
3501.045334	914126.792562	45.544615
3501.327642	914127.227116	45.549620
3501.190623	914124.377052	45.554625
3501.339707	914127.225408	45.559629
3501.232190	914126.572270	45.564634
3501.180127	914123.421769	45.569639
3501.123003	914105.914167	45.574644
3501.371342	914091.230347	45.579649
3501.434352	914087.870396	45.584653
3501.185570	914092.599639	45.589658
3501.112028	914081.699172	45.594663
3501.452040	914088.250776	45.599668
3500.901806	914074.266058	45.604673
3501.591355	914066.309312	45.609677
3501.131327	914059.010856	45.614682
3501.198891	914047.418217	45.619687
3501.333615	914052.757591	45.624692
3501.256595	914057.555736	45.629697
3501.257208	914063.586105	45.634701
3501.418781	914047.575640	45.639706
3501.193985	914031.434081	45.644711
3501.203214	914033.347143	45.649716
3501.378110	914025.662226	45.654721
3501.588906	914024.863596	45.659725
3501.204917	914007.119590	45.664730
3501.172482	913984.821651	45.669735
3501.274734	914000.025477	45.674740
3501.090998	913998.809909	45.679745
3501.175411	913992.862073	45.684749
3501.292632	914002.607422	45.689754
3501.333682	913998.580797	45.694759
3501.236246	913988.258195	45.699764
3501.211482	913965.480366	45.704769
3501.414878	913955.876449	45.709773
3501.291894	913959.054594	45.714778
3501.438804	913963.626379	45.719783
3501.124768	913965.972886	45.724788
3501.259057	913952.072273	45.729793
3501.114329	913931.418934	45.734797
3501.123111	913938.596844	45.739802
3501.312488	913931.675304	45.744807
3501.292432	913934.454484	45.749812
3501.171883	913931.888906	45.754817
3501.594422	913905.403427	45.759821
3500.985935	913850.553261	45.764826
3500.736075	913735.913588	45.769831
3500.980462	913587.497579	45.774836
3500.897077	913381.210450	45.779841
3500.614906	913125.737205	45.784845
3500.204256	912822.974393	45.789850
3500.115822	912474.662471	45.794855
3499.934416	912070.994140	45.799860
3499.395457	911618.318313	45.804865
3498.899209	911109.951065	45.809869
3498.321664	910565.722953	45.814874
3497.988067	909969.861312	45.819879
3497.574212	909324.698478	45.824884
3496.957617	908646.141534	45.829889
3496.487626	907890.326642	45.834893
3495.614970	907112.802949	45.839898
3494.766245	906271.697477	45.844903
3494.434231	905388.571703	45.849908
3493.504137	904454.948081	45.854913
3492.692555	903467.906247	45.859917
3492.204517	902450.120851	45.864922
3491.377816	901364.831662	45.869927
3490.122556	900241.475720	45.874932
3489.426771	899076.226902	45.879937
3488.917871	897834.453862	45.884941
3487.296599	896564.615657	45.889946
3486.158861	895240.409707	45.894951
3485.485754	893876.020651	45.899956
3483.813962	892467.802837	45.904961
3483.323884	891005.767627	45.909965
3481.855158	889504.443004	45.914970
3480.406490	887955.175897	45.919975
3479.486348	886366.410913	45.924980
3478.071888	884733.943385	45.929985
3476.744012	883037.617831	45.934989
3475.135875	881311.817842	45.939994
3473.509679	879537.400217	45.944999
3472.255106	877719.077800	45.950004
3470.502310	875867.550385	45.955009
3469.151312	873966.829759	45.960013
3467.429494	872023.742061	45.965018
3466.036654	870042.479179	45.970023
3464.222338	868016.169573	45.975028
3462.303081	865968.186983	45.980033
3460.689265	863850.428782	45.985037
3459.188409	861719.198930	45.990042
3457.292352	859539.370499	45.995047
3455.424153	857317.886480	46.000052
3453.485665	855064.007267	46.005057
3451.610121	852758.607923	46.010061
3449.517272	850436.054272	46.015066
3447.590359	848064.880820	46.020071
3445.876134	845662.568712	46.025076
3443.427957	843226.808744	46.030081
3441.796136	840736.757724	46.035085
3439.462187	838224.808807	46.040090
3437.381057	835676.616249	46.045095
3435.544355	833101.076726	46.050100
3432.864227	830483.950444	46.055105
3430.715476	827823.127717	46.060109
3428.717353	825134.664460	46.065114
3425.942853	822420.913937	46.070119
3423.753583	819684.167616	46.075124
3421.101097	816912.782852	46.080129
3418.942799	814102.966249	46.085133
3416.280735	811268.865827	46.090138
3413.891477	808402.192702	46.095143
3411.665574	805507.757243	46.100148
3409.168796	802588.135689	46.105153
3406.395289	799629.729820	46.110157
3403.231120	796653.370754	46.115162
3400.605614	793640.424741	46.120167
3398.215465	790628.691946	46.125172
3394.884270	787573.659279	46.130177
3392.745710	784492.364485	46.135181
3390.219816	781391.735890	46.140186
3387.217199	778253.157057	46.145191
3384.617947	775101.244840	46.150196
3381.749179	771915.455385	46.155201
3379.245929	768700.263706	46.160205
3375.977940	765473.777890	46.165210
3373.297037	762215.013597	46.170215
3370.586174	758931.598290	46.175220
3367.638353	755632.239954	46.180225
3364.632850	752296.446786	46.185229
3361.249585	748950.349628	46.190234
3358.294247	745575.759363	46.195239
3355.648827	742199.894492	46.200244
3352.263410	738792.340692	46.205249
3349.366793	735356.767650	46.210253
3346.119268	731922.764669	46.215258
3343.237302	728449.540503	46.220263
3340.408291	724960.544221	46.225268
3336.930749	721450.100797	46.230273
3333.989355	717912.921459	46.235277
3330.887094	714367.574670	46.240282
3327.314978	710799.823525	46.245287
3324.017401	707233.376144	46.250292
3320.980282	703639.599291	46.255297
3317.883911	700032.679536	46.260301
3314.456182	696410.229449	46.265306
3311.282102	692760.952903	46.270311
3307.824472	689107.964631	46.275316
3304.529108	685436.276923	46.280321
3301.359470	681742.115120	46.285325
3297.715388	678041.046143	46.290330
3294.308379	674335.795750	46.295335
3290.945785	670605.686967	46.300340
3287.491207	666867.723078	46.305345
3284.379011	663108.714660	46.310349
3280.556527	659352.792652	46.315354
3277.385534	655571.297582	46.320359
3273.906518	651788.908493	46.325364
3270.407468	647993.591667	46.330369
3266.969416	644175.169590	46.335373
3263.093016	640364.315386	46.340378
3259.689770	636531.788597	46.345383
3256.252548	632689.781804	46.350388
3252.601657	628846.812827	46.355393
3249.386308	624984.871062	46.360397
3245.771181	621123.261667	46.365402
3242.123212	617239.458638	46.370407
3238.647381	613361.613856	46.375412
3234.632266	609473.460131	46.380417
3231.427426	605558.583053	46.385421
3227.727839	601654.306625	46.390426
3224.160650	597736.831680	46.395431
3220.476333	593807.802212	46.400436
3216.861596	589888.235527	46.405441
3213.052382	585943.418186	46.410445
3209.394447	582009.584725	46.415450
3205.573644	578064.093386	46.420455
3201.896527	574116.835054	46.425460
3198.232974	570173.265884	46.430465
3194.569588	566211.318079	46.435469
3190.889176	562256.656907	46.440474
3187.215671	558292.824355	46.445479
3183.463564	554326.827509	46.450484
3180.166080	550361.765262	46.455489
3176.313892	546366.181282	46.460493
3172.714201	542385.816046	46.465498
3168.400279	538403.592228	46.470503
3165.185039	534408.570159	46.475508
3161.242118	530413.327049	46.480513
3157.764950	526418.448808	46.485517
3153.730851	522412.524765	46.490522
3149.737261	518420.970439	46.495527
3145.965263	514409.556849	46.500532
3142.152100	510423.205681	46.505537
3138.766053	506407.959811	46.510541
3134.936803	502396.794980	46.515546
3130.876626	498400.398208	46.520551
3127.236519	494379.571943	46.525556
3123.505935	490380.396390	46.530561
3119.602369	486362.964876	46.535565
3115.599810	482371.173539	46.540570
3111.759404	478357.968717	46.545575
3107.836322	474339.514493	46.550580
3103.890222	470344.735847	46.555585
3100.231368	466331.186945	46.560589
3096.464782	462331.105456	46.565594
3092.300101	458340.211643	46.570599
3088.323462	454333.638184	46.575604
3085.135530	450346.276000	46.580609
3081.243691	446342.439270	46.585613
3077.661024	442353.475067	46.590618
3073.644578	438347.512476	46.595623
3069.708305	434348.896969	46.600628
3065.552691	430359.520711	46.605633
3061.795413	426367.043296	46.610637
3057.715655	422379.145429	46.615642
3054.167050	418392.670217	46.620647
3050.105189	414412.311559	46.625652
3045.875678	410425.911950	46.630657
3042.044624	406461.349309	46.635661
3038.225114	402494.913967	46.640666
3034.224619	398526.447850	46.645671
3030.784623	394555.443685	46.650676
3026.319618	390597.191037	46.655681
3022.559754	386639.915210	46.660685
3018.411992	382698.835032	46.665690
3014.412013	378764.899676	46.670695
3010.267097	374817.041414	46.675700
3006.571845	370888.606519	46.680705
3002.851437	366960.231600	46.685709
2998.499140	363048.187273	46.690714
2994.445444	359136.136061	46.695719
2990.697804	355231.767449	46.700724
2986.887373	351337.393790	46.705729
2983.264793	347435.274887	46.710733
2978.798953	343539.389935	46.715738
2974.731735	339641.144820	46.720743
2970.805875	335761.930194	46.725748
2966.538491	331897.035245	46.730753
2962.408602	328026.665445	46.735757
2958.490975	324184.197047	46.740762
2954.318105	320345.556459	46.745767
2950.579421	316509.047970	46.750772
2946.406643	312691.768335	46.755777
2942.408948	308877.405539	46.760781
2938.151580	305079.275490	46.765786
2933.944621	301277.342450	46.770791
2930.280243	297485.337519	46.775796
2926.058167	293709.048208	46.780801
2922.078049	289942.969101	46.785805
2918.057641	286187.235726	46.790810
2913.911945	282440.297736	46.795815
2909.675914	278710.642214	46.800820
2905.042139	274982.648437	46.805825
2901.181400	271277.203646	46.810829
2896.855148	267573.127697	46.815834
2892.939703	263892.373751	46.820839
2888.732133	260218.896118	46.825844
2884.470203	256561.303437	46.830849
2880.423678	252914.651856	46.835853
2876.147467	249282.792871	46.840858
2871.690020	245666.368344	46.845863
2867.903731	242059.985548	46.850868
2863.218356	238471.771795	46.855873
2859.191427	234884.151299	46.860877
2854.909836	231327.382458	46.865882
2850.267013	227790.057993	46.870887
2846.495173	224262.496284	46.875892
2842.230343	220750.651930	46.880897
2837.846783	217247.676698	46.885901
2833.864285	213777.618493	46.890906
2829.471406	210313.082312	46.895911
2825.137418	206859.913335	46.900916
2820.574442	203437.725306	46.905921
2816.254654	200013.396320	46.910925
2812.424628	196610.683513	46.915930
2807.826740	193245.402375	46.920935
2803.730056	189870.122999	46.925940
2799.643851	186534.231532	46.930945
2795.465569	183196.574880	46.935949
2791.252464	179875.792075	46.940954
2786.957821	176580.045370	46.945959
2783.097101	173197.258380	46.950964
2778.368330	169932.490106	46.955969
2773.916748	166689.690953	46.960973
2769.702180	163456.067593	46.965978
2765.351110	160247.799081	46.970983
2761.483374	157058.887326	46.975988
2757.339107	153873.484169	46.980993
2752.986289	150707.913731	46.985997
2748.635341	147575.458103	46.991002
2744.366065	144439.167579	46.996007
2740.252770	141326.127414	47.001012
2735.948805	138242.425495	47.006017
2731.721938	135168.366076	47.011021
2727.645225	132111.779157	47.016026
2723.034808	129066.962025	47.021031
2718.690667	126043.104564	47.026036
2714.464007	123053.344931	47.031041
2710.331617	120059.724454	47.036045
2705.938309	117094.237035	47.041050
2701.740197	114153.505268	47.046055
2697.969195	111225.020524	47.051060
2693.700254	108304.760770	47.056065
2689.404144	105413.046963	47.061069
2685.358152	102538.801272	47.066074
2680.911499	99687.020269	47.071079
2676.677647	96823.853026	47.076084
2672.513220	94004.724015	47.081089
2668.380630	91196.112755	47.086093
2663.919388	88399.933263	47.091098
2659.770198	85639.005788	47.096103
2656.116468	82875.111630	47.101108
2651.402456	80139.340210	47.106113
2646.968301	77422.334527	47.111117
2642.503721	74726.491993	47.116122
2638.642811	72045.909058	47.121127
2634.502486	69388.900789	47.126132
2629.999375	66744.045544	47.131137
2625.522776	64129.924739	47.136141
2621.271620	61524.188256	47.141146
2617.326213	58952.202029	47.146151
2612.893271	56380.283554	47.151156
2608.196983	53853.828016	47.156161
2604.010760	51325.354431	47.161165
2599.749573	48818.447304	47.166170
2595.127617	46328.499387	47.171175
2590.742076	43881.410124	47.176180
2585.899520	41455.230145	47.181185
2581.800328	39051.328189	47.186189
2577.287053	36675.472981	47.191194
2572.601453	34309.998803	47.196199
2568.301605	31984.094327	47.201204
2563.645733	29681.426250	47.206209
2558.945310	27405.603941	47.211213
2554.122701	25160.714089	47.216218
2549.179570	22936.492112	47.221223
2544.635806	20749.721911	47.226228
2539.213319	18609.936368	47.231233
2533.957885	16496.990194	47.236237
2528.348675	14435.155510	47.241242
2522.984086	12412.692763	47.246247
2515.768329	10463.361339	47.251252
2508.035072	8594.076154	47.256257
2499.578324	6820.827436	47.261261
2489.888496	5166.657602	47.266266
2478.752793	3637.980330	47.271271
2467.449391	2247.108225	47.276276
2454.239545	1051.532260	47.281281
2433.777420	208.244407	47.286285
2393.506171	122.096023	47.291290
2362.834330	178.199868	47.296295
2351.843992	196.773321	47.301300
2352.814347	228.557846	47.306305
2360.554510	261.874556	47.311309
2369.953713	267.861495	47.316314
2377.931444	268.296715	47.321319
2382.283638	271.045597	47.326324
2382.728617	264.293928	47.331329
2381.947103	251.846133	47.336333
2378.959907	242.204916	47.341338
2375.095747	245.932284	47.346343
2371.318251	231.865038	47.351348
2367.731020	225.449955	47.356353
2364.860760	219.324523	47.361357
2361.752636	217.627778	47.366362
2358.902551	211.242920	47.371367
2356.470683	205.321006	47.376372
2353.332329	194.880863	47.381377
2350.964748	192.454477	47.386381
2347.832756	185.942886	47.391386
2344.239412	193.402394	47.396391
2340.910933	191.189617	47.401396
2337.399307	196.889883	47.406401
2334.227883	191.517133	47.411405
2331.483645	184.214028	47.416410
2328.068028	199.568091	47.421415
2325.042559	195.925298	47.426420
2321.772165	196.174430	47.431425
2318.479528	194.139557	47.436429
2315.126644	192.927228	47.441434
2311.924682	204.587265	47.446439
2308.897966	193.911365	47.451444
2304.678937	189.983892	47.456449
2301.674580	197.711949	47.461453
2298.495792	191.628489	47.466458
2294.871637	199.864820	47.471463
2291.914981	198.378528	47.476468
2288.479736	210.413605	47.481473
2285.098774	212.053170	47.486477
2281.973894	202.775249	47.491482
2278.721006	204.461220	47.496487
2274.955271	207.129134	47.501492
2271.265105	204.567987	47.506497
2268.298202	206.867305	47.511501
2265.299245	208.712876	47.516506
2261.105028	203.291348	47.521511
2258.240539	200.607355	47.526516
2254.959149	194.071707	47.531521
2251.215528	195.856609	47.536525
2247.474658	195.306140	47.541530
2243.983868	203.151446	47.546535
2241.133510	205.198410	47.551540
2237.229503	200.285167	47.556545
2233.575459	203.555739	47.561549
2230.613603	208.511936	47.566554
2227.215299	210.647796	47.571559
2224.109387	197.649373	47.576564
2220.056388	204.187376	47.581569
2216.983225	200.938070	47.586573
2213.687109	203.858407	47.591578
2210.330826	210.537356	47.596583
2206.798125	203.651884	47.601588
2202.856487	205.850613	47.606593
2199.485646	205.985777	47.611597
2196.503742	206.003140	47.616602
2193.178674	208.905866	47.621607
2189.269820	200.250533	47.626612
2185.630411	214.045054	47.631617
2182.178250	209.089610	47.636621
2179.279411	204.787943	47.641626
2175.697991	209.625945	47.646631
2171.930162	212.281565	47.651636
2168.620367	210.986606	47.656641
2165.072692	206.799116	47.661645
2161.738752	201.967559	47.666650
2158.215075	202.484167	47.671655
2154.693272	196.767647	47.676660
2151.122422	202.100730	47.681665
2147.797176	203.298166	47.686669
2144.271110	203.413340	47.691674
2140.421491	209.887910	47.696679
2137.398434	200.195463	47.701684
2133.373814	208.747608	47.706689
2130.246471	207.946153	47.711693
2127.165496	209.453403	47.716698
2123.847638	207.890790	47.721703
2120.523949	191.645548	47.726708
2116.940982	205.010450	47.731713
2113.143156	206.427377	47.736717
2109.571444	196.229144	47.741722
2105.782840	201.140713	47.746727
2102.628195	188.121495	47.751732
2099.058420	201.712133	47.756737
2095.861539	209.201432	47.761741
2092.474207	203.201291	47.766746
2088.245379	200.066408	47.771751
2085.432007	198.602050	47.776756
2081.512517	194.349380	47.781761
2078.166790	191.421187	47.786765
2074.866777	204.238769	47.791770
2071.553660	206.952990	47.796775
2068.196584	198.429681	47.801780
2064.551265	202.145046	47.806785
2060.450406	203.808731	47.811789
2057.529559	197.843185	47.816794
2054.007094	196.334759	47.821799
2050.694722	205.575939	47.826804
2046.820825	206.330888	47.831809
2043.269197	209.326056	47.836813
2040.046462	198.684089	47.841818
2036.551740	201.641879	47.846823
2033.141907	198.321919	47.851828
2029.719488	196.446656	47.856833
2025.897579	202.761893	47.861837
2022.647563	193.472014	47.866842
2018.929664	185.729717	47.871847
2015.841715	183.163023	47.876852
2011.914908	200.435340	47.881857
2008.435195	205.931380	47.886861
2004.909483	195.640569	47.891866
2001.530421	203.291276	47.896871
1998.496447	187.307655	47.901876
1994.525720	196.863841	47.906881
1991.082674	195.023458	47.911885
1987.728167	197.329711	47.916890
1984.136985	193.879953	47.921895
1980.905337	197.223716	47.926900
1977.448551	192.974619	47.931905
1973.593260	196.441282	47.936909
1970.222096	194.921864	47.941914
1966.362635	205.691397	47.946919
1963.259216	195.733171	47.951924
1959.622040	200.184475	47.956929
1956.374964	193.972608	47.961933
1953.028850	195.318906	47.966938
1949.161081	199.936015	47.971943
1945.830069	195.566003	47.976948
1942.607640	201.129372	47.981953
1938.556217	203.921196	47.986957
1935.312522	200.255721	47.991962
1931.734438	204.871801	47.996967
1928.202777	198.631706	48.001972
1924.684899	200.463652	48.006977
1921.454955	190.512588	48.011981
1918.214630	195.790850	48.016986
1914.613632	193.535432	48.021991
1910.995288	194.908523	48.026996
1907.324877	190.525196	48.032001
1903.427483	195.419047	48.037005
1900.246971	189.902328	48.042010
1896.604727	199.720364	48.047015
1893.342226	191.641088	48.052020
1890.060802	192.926660	48.057025
1886.852687	201.873142	48.062029
1882.991134	186.509475	48.067034
1878.856970	192.927403	48.072039
1875.770487	191.072392	48.077044
1872.243661	197.816077	48.082049
1868.821264	187.661026	48.087053
1865.898195	187.947694	48.092058
1861.884345	193.441934	48.097063
1858.556642	188.229848	48.102068
1854.995361	196.041988	48.107073
1851.372858	198.678133	48.112077
1847.912471	189.402262	48.117082
1844.534681	189.544953	48.122087
1841.081764	182.441496	48.127092
1837.719826	196.562830	48.132097
1833.886420	199.877414	48.137101
1830.295108	185.882569	48.142106
1826.773908	191.119384	48.147111
1823.461270	186.325748	48.152116
1820.035285	187.526392	48.157121
1816.212872	185.947926	48.162125
1813.403558	190.503843	48.167130
1809.293983	181.636481	48.172135
1806.116493	186.329114	48.177140
1802.393661	196.922275	48.182145
1799.254147	194.271965	48.187149
1795.345998	182.667983	48.192154
1791.576422	199.251330	48.197159
1788.684641	189.750453	48.202164
1785.037736	196.281991	48.207169
1781.388558	192.768615	48.212173
1778.316086	183.055569	48.217178
1774.641053	189.930044	48.222183
1771.248254	186.512597	48.227188
1767.349102	189.986193	48.232193
1763.714230	180.547836	48.237197
1760.414835	180.684614	48.242202
1756.548908	188.228068	48.247207
1753.450000	190.130545	48.252212
1750.112489	181.990299	48.257217
1746.408534	172.819039	48.262221
1743.452827	177.290308	48.267226
1739.669134	180.685730	48.272231
1736.140362	178.558286	48.277236
1732.554261	176.522075	48.282241
1728.552676	186.361584	48.287245
1725.229646	177.314219	48.292250
1722.046770	171.082907	48.297255
1718.772962	181.504565	48.302260
1715.344064	178.523075	48.307265
1711.536401	175.047189	48.312269
1708.002377	173.550186	48.317274
1704.238199	181.596602	48.322279
1700.923852	178.454816	48.327284
1697.372421	180.111744	48.332289
1693.879724	173.024066	48.337293
1690.379829	173.094166	48.342298
1687.021837	185.424160	48.347303
1683.768499	181.956445	48.352308
1680.306259	180.172960	48.357313
1676.500980	180.990072	48.362317
1673.217568	181.320535	48.367322
1669.302879	181.433413	48.372327
1665.789947	172.922013	48.377332
1662.696997	179.430160	48.382337
1658.872484	181.284870	48.387341
1655.466795	171.481656	48.392346
1652.130440	174.965286	48.397351
1648.632135	167.625397	48.402356
1645.167250	170.562815	48.407361
1641.394749	171.555149	48.412365
1638.107843	167.861744	48.417370
1634.441441	174.491287	48.422375
1631.028195	167.188715	48.427380
1627.705958	160.517330	48.432385
1623.788500	176.522707	48.437389
1620.539216	179.454864	48.442394
1616.967791	176.679221	48.447399
1613.680153	172.622095	48.452404
1610.311015	180.290324	48.457409
1606.597854	175.012110	48.462413
1602.905435	175.526837	48.467418
1599.450603	175.010929	48.472423
1595.842390	173.873602	48.477428
1592.398498	178.525725	48.482433
1588.804802	178.006244	48.487437
1585.418095	173.607118	48.492442
1581.640633	180.190784	48.497447
1578.784822	172.873751	48.502452
1575.236358	179.658866	48.507457
1571.402438	177.145795	48.512461
1567.762384	169.742701	48.517466
1564.295553	168.874331	48.522471
1561.334730	171.849943	48.527476
1557.787585	173.129748	48.532481
1553.941354	166.046843	48.537485
1550.258120	166.917667	48.542490
1546.755374	172.306700	48.547495
1543.499494	171.373682	48.552500
1540.167299	163.194730	48.557505
1536.305851	176.818472	48.562509
1533.141325	171.201309	48.567514
1529.455380	176.068512	48.572519
1526.176302	166.299323	48.577524
1522.567389	172.556058	48.582529
1519.069308	173.005595	48.587533
1515.521292	164.066306	48.592538
1511.933536	175.932407	48.597543
1508.409901	163.866582	48.602548
1505.095697	166.220456	48.607553
1501.029409	173.232179	48.612557
1498.230787	165.279784	48.617562
1494.373247	169.183570	48.622567
1491.194165	172.342065	48.627572
1487.055612	169.243941	48.632577
1483.829284	176.345666	48.637581
1480.789477	164.947626	48.642586
1476.984631	169.143736	48.647591
1473.547030	162.980865	48.652596
1470.394674	167.353264	48.657601
1466.242729	168.528445	48.662605
1462.809133	174.593236	48.667610
1459.170008	193.769576	48.672615
1456.247384	170.444451	48.677620
1452.676866	170.623766	48.682625
1448.727514	185.242092	48.687629
1445.472609	169.869130	48.692634
1441.873352	180.360777	48.697639
1438.627038	175.680294	48.702644
1434.819324	165.550951	48.707649
1431.297231	167.282472	48.712653
1428.461445	168.128259	48.717658
1424.442857	171.756714	48.722663
1421.184547	174.329663	48.727668
1417.397869	167.278626	48.732673
1414.058076	177.049437	48.737677
1410.376871	168.880872	48.742682
1407.065163	181.472609	48.747687
1403.483529	176.196038	48.752692
1400.180148	171.919984	48.757697
1396.242951	169.410496	48.762701
1393.293882	164.465198	48.767706
1389.328668	175.909511	48.772711
1385.712704	173.371889	48.777716
1381.968689	166.975434	48.782721
1378.828054	168.833928	48.787725
1375.506179	163.019987	48.792730
1371.571279	174.136846	48.797735
1368.534095	173.751800	48.802740
1365.038442	171.084619	48.807745
1361.389417	172.446880	48.812749
1357.949327	170.349988	48.817754
1354.172619	174.617670	48.822759
1350.814571	163.323286	48.827764
1347.062449	168.789382	48.832769
1343.776628	170.075811	48.837773
1340.527080	149.026135	48.842778
1337.142206	165.913176	48.847783
1333.443750	163.458094	48.852788
1329.761013	166.844178	48.857793
1326.152420	165.039439	48.862797
1322.784845	157.299563	48.867802
1319.551991	166.155120	48.872807
1316.079182	166.967777	48.877812
1312.705032	161.478429	48.882817
1308.906448	164.509321	48.887821
1305.098229	159.742842	48.892826
1301.626029	166.734400	48.897831
1298.469102	167.345750	48.902836
1294.927175	163.296912	48.907841
1291.514042	166.074476	48.912845
1288.171658	159.612027	48.917850
1284.392924	162.282306	48.922855
1280.821533	153.732773	48.927860
1277.322222	166.537400	48.932865
1273.504484	167.296499	48.937869
1270.661309	162.204949	48.942874
1266.935186	163.497053	48.947879
1263.399353	152.230547	48.952884
1259.954136	159.771564	48.957889
1256.159359	158.432610	48.962893
1252.563313	160.020741	48.967898
1249.177100	166.492638	48.972903
1245.843777	162.714891	48.977908
1242.411517	154.858623	48.982913
1238.732425	161.980666	48.987917
1235.590359	155.955129	48.992922
1231.530198	150.076488	48.997927
1228.153883	150.829776	49.002932
1224.883523	151.753144	49.007937
1220.886577	164.490152	49.012941
1218.144125	157.560479	49.017946
1214.427746	165.874809	49.022951
1210.902316	161.513366	49.027956
1207.483756	158.078019	49.032961
1203.656310	151.061941	49.037965
1200.443464	146.948970	49.042970
1196.715505	148.848845	49.047975
1193.152057	155.522513	49.052980
1189.398103	151.405671	49.057985
1186.187643	160.665888	49.062989
1182.935975	159.640580	49.067994
1179.026995	163.388012	49.072999
1176.058280	167.272986	49.078004
1172.225018	160.979186	49.083009
1168.596999	156.083313	49.088013
1165.325174	157.089190	49.093018
1161.867785	154.716663	49.098023
1158.555599	155.523211	49.103028
1154.753228	161.902096	49.108033
1151.313113	156.410484	49.113037
1148.054117	153.456394	49.118042
1144.092937	160.657432	49.123047
1140.528599	152.385276	49.128052
1136.982907	161.318329	49.133057
1133.600747	159.183978	49.138061
1129.936955	155.141631	49.143066
1126.402524	156.160161	49.148071
1123.316450	153.356182	49.153076
1119.848973	157.477449	49.158081
1116.658856	168.357552	49.163085
1112.922619	158.365877	49.168090
1109.300253	162.821455	49.173095
1105.729537	158.596862	49.178100
1102.215057	158.087306	49.183105
1098.519840	168.837681	49.188109
1095.387367	160.874423	49.193114
1091.323916	164.981439	49.198119
1088.001628	156.785305	49.203124
1084.850985	158.306924	49.208129
1081.118664	157.610014	49.213133
1077.778021	157.984435	49.218138
1074.137930	155.567778	49.223143
1070.468820	161.277240	49.228148
1067.644714	161.219605	49.233153
1063.549100	161.307264	49.238157
1060.134479	139.391388	49.243162
1056.599631	154.014503	49.248167
1053.058785	148.402660	49.253172
1049.923177	155.873114	49.258177
1046.525088	156.993714	49.263181
1042.593475	153.857065	49.268186
1038.989483	161.587525	49.273191
1035.971148	158.364835	49.278196
1032.342248	150.586903	49.283201
1028.218958	154.829864	49.288205
1024.812141	156.448561	49.293210
1021.918577	159.856726	49.298215
1018.115367	153.159650	49.303220
1014.923853	155.348932	49.308225
1011.017615	162.630003	49.313229
1007.592151	158.993328	49.318234
1003.863695	160.298551	49.323239
1000.299615	146.932643	49.328244
997.063012	149.299837	49.333249
993.698017	151.114482	49.338253
990.570771	153.606929	49.343258
986.572375	158.991479	49.348263
982.836085	150.866543	49.353268
979.734610	152.598802	49.358273
976.027176	158.589548	49.363277
972.526614	154.986794	49.368282
968.886454	151.301493	49.373287
965.940872	148.665402	49.378292
962.347712	151.243465	49.383297
958.266140	155.084442	49.388301
955.143392	146.221195	49.393306
951.527877	153.798456	49.398311
948.049623	150.831313	49.403316
944.557179	145.752955	49.408321
940.744659	150.232034	49.413325
937.670697	145.217869	49.418330
933.778865	148.209713	49.423335
930.463705	148.586523	49.428340
927.454556	142.290353	49.433345
923.458167	150.458783	49.438349
920.401548	146.631510	49.443354
916.536075	147.141952	49.448359
913.300571	151.707865	49.453364
909.973117	133.375709	49.458369
906.052585	139.662439	49.463373
902.663428	141.958636	49.468378
898.856174	147.825827	49.473383
895.444127	152.178939	49.478388
892.086362	143.336700	49.483393
888.191337	146.711885	49.488397
884.973331	146.494517	49.493402
881.475337	146.937939	49.498407
878.164957	143.346575	49.503412
874.676710	152.545960	49.508417
870.866836	147.036434	49.513421
867.941766	139.414132	49.518426
864.105246	150.819458	49.523431
860.194402	142.522596	49.528436
857.056598	150.860332	49.533441
853.469635	152.665489	49.538445
850.067034	148.278634	49.543450
846.194211	147.217832	49.548455
842.733289	142.080796	49.553460
839.631179	154.117794	49.558465
836.266496	151.490424	49.563469
832.738001	143.526017	49.568474
829.003092	161.591130	49.573479
825.756241	151.152796	49.578484
822.010309	145.848421	49.583489
818.137784	147.856499	49.588493
814.753417	141.799467	49.593498
811.130148	146.634945	49.598503
807.892848	151.273939	49.603508
804.511967	145.051845	49.608513
800.844135	154.080053	49.613517
797.960908	145.796309	49.618522
793.877401	149.371893	49.623527
790.566102	147.909963	49.628532
787.410787	152.077370	49.633537
783.328480	152.817980	49.638541
780.097614	140.744633	49.643546
776.078072	143.326256	49.648551
773.006433	146.436500	49.653556
769.207871	155.317507	49.658561
765.411745	147.407694	49.663565
762.356739	143.422035	49.668570
758.899779	156.935180	49.673575
755.422860	146.738557	49.678580
751.853421	148.556826	49.683585
748.587759	146.360084	49.688589
745.513689	143.975150	49.693594
741.380413	150.589496	49.698599
737.234333	139.051808	49.703604
733.786317	141.138976	49.708609
730.022718	154.355291	49.713613
727.149672	154.014351	49.718618
724.639705	141.182713	49.723623
720.706452	145.231516	49.728628
717.746362	145.268052	49.733633
713.587819	151.883202	49.738637
709.655010	146.434133	49.743642
706.397880	151.370500	49.748647
702.670615	147.202233	49.753652
699.563799	138.083494	49.758657
695.686709	146.185864	49.763661
692.530486	134.050250	49.768666
688.644638	140.996032	49.773671
685.321249	146.948878	49.778676
681.951031	134.293113	49.783681
678.370494	141.978877	49.788685
675.518167	135.262768	49.793690
671.751230	140.978188	49.798695
667.627613	135.188858	49.803700
663.994838	136.786119	49.808705
660.050383	149.258801	49.813709
657.238365	139.508603	49.818714
653.738789	141.562745	49.823719
650.341768	135.795674	49.828724
646.936712	137.604056	49.833729
643.025390	147.331684	49.838733
639.736771	141.218600	49.843738
636.284341	138.269688	49.848743
632.820751	141.833673	49.853748
629.320066	136.199908	49.858753
625.852895	144.152678	49.863757
622.753651	134.760699	49.868762
619.112247	143.626629	49.873767
615.431473	136.673286	49.878772
612.201477	136.461055	49.883777
607.801470	128.541499	49.888781
604.861506	135.566963	49.893786
601.094064	136.777206	49.898791
597.331127	138.587871	49.903796
594.299047	139.499445	49.908801
590.772878	138.416100	49.913805
587.381809	136.659849	49.918810
583.482677	132.081949	49.923815
580.442976	136.177525	49.928820
577.115769	143.032690	49.933825
573.283823	140.038836	49.938829
569.825105	133.892313	49.943834
566.239626	135.251245	49.948839
562.459980	141.674229	49.953844
559.283618	136.597151	49.958849
555.406642	146.037848	49.963853
551.994437	135.691984	49.968858
548.604549	134.185506	49.973863
545.189342	132.660848	49.978868
542.037779	130.598179	49.983873
538.176388	141.808178	49.988877
534.705116	132.303660	49.993882
531.090922	141.159028	49.998887
527.950705	137.503185	50.003892
524.473662	133.014230	50.008897
520.617466	141.398130	50.013901
517.023236	137.939954	50.018906
513.639040	136.565479	50.023911
510.376932	139.348123	50.028916
507.152932	139.584254	50.033921
502.800615	136.213183	50.038925
499.490656	131.815130	50.043930
495.876521	140.325644	50.048935
492.583247	138.275697	50.053940
489.199402	132.946403	50.058945
485.710147	145.850889	50.063949
482.759772	137.941629	50.068954
478.639827	132.199277	50.073959
475.216002	133.542416	50.078964
471.556450	135.707104	50.083969
468.149851	147.570409	50.088973
464.539013	132.778895	50.093978
460.958628	142.369324	50.098983
457.813041	141.349809	50.103988
454.327908	140.016477	50.108993
450.225994	147.992794	50.113997
446.910555	132.870276	50.119002
443.573170	142.830781	50.124007
440.207273	134.885382	50.129012
436.933424	140.128177	50.134017
433.176970	144.861261	50.139021
429.961065	138.939361	50.144026
426.160268	136.731650	50.149031
422.240818	136.981829	50.154036
419.000350	136.682721	50.159041
415.652812	143.594906	50.164045
412.090733	129.947414	50.169050
408.549078	135.130923	50.174055
405.171284	133.040465	50.179060
401.473459	126.197467	50.184065
398.240468	134.414186	50.189069
394.828001	132.155153	50.194074
390.839273	132.476310	50.199079
387.197865	136.508004	50.204084
383.803742	131.908043	50.209089
380.414307	142.550612	50.214093
377.167551	129.761761	50.219098
373.233034	135.433936	50.224103
370.018623	138.579324	50.229108
366.642370	135.798927	50.234113
362.721739	134.106735	50.239117
359.396368	129.540308	50.244122
355.961886	135.042412	50.249127
352.399497	126.105924	50.254132
349.347373	134.825846	50.259137
345.548868	144.244832	50.264141
342.224998	137.684972	50.269146
338.407849	144.262612	50.274151
334.438216	140.262194	50.279156
331.920094	135.189667	50.284161
328.082423	140.875165	50.289165
324.544921	137.325927	50.294170
321.003493	141.756446	50.299175
317.285556	138.324062	50.304180
314.296687	130.781577	50.309185
310.345209	137.642864	50.314189
307.023934	132.022267	50.319194
303.317091	139.161617	50.324199
299.669476	130.260649	50.329204
296.685351	138.903495	50.334209
292.765683	133.987258	50.339213
289.601531	142.367239	50.344218
286.236778	137.389386	50.349223
282.531971	143.174314	50.354228
279.159680	137.830643	50.359233
275.284685	138.580132	50.364237
271.911986	133.442177	50.369242
268.573076	139.900631	50.374247
264.679872	130.009914	50.379252
261.578564	131.973336	50.384257
257.778723	133.267891	50.389261
254.531605	126.110744	50.394266
250.678878	128.837301	50.399271
247.525844	137.171256	50.404276
243.776117	130.289005	50.409281
240.053625	136.525979	50.414285
236.999199	131.635578	50.419290
233.952172	132.233231	50.424295
230.130198	130.750276	50.429300
226.818780	134.761973	50.434305
222.593787	138.461203	50.439309
219.076842	129.596753	50.444314
215.924661	138.098266	50.449319
212.293089	135.152283	50.454324
209.258938	135.678324	50.459329
205.448747	141.229848	50.464333
202.267838	136.539612	50.469338
198.215249	132.792708	50.474343
194.458514	141.812890	50.479348
191.333094	127.002430	50.484353
187.548665	137.131119	50.489357
184.491521	136.091521	50.494362
181.106155	135.362777	50.499367
177.008173	131.588194	50.504372
173.864542	134.004374	50.509377
169.944634	134.691342	50.514381
166.981634	133.364914	50.519386
163.580623	137.691231	50.524391
160.163359	132.342004	50.529396
156.649922	133.737267	50.534401
152.725880	129.426073	50.539405
149.269917	125.206067	50.544410
145.770345	130.822845	50.549415
142.116781	129.164846	50.554420
138.896745	132.652883	50.559425
135.467352	126.236202	50.564429
132.256591	121.911349	50.569434
128.335368	131.406580	50.574439
125.118557	125.893085	50.579444
121.720278	120.629490	50.584449
117.317725	129.785676	50.589453
114.485011	121.927742	50.594458
110.620300	128.370543	50.599463
106.653984	128.460523	50.604468
103.852677	121.205124	50.609473
100.059406	128.788361	50.614477
97.109944	131.053921	50.619482
93.498136	135.707524	50.624487
89.829037	135.738290	50.629492
86.073269	133.678705	50.634497
82.595698	135.761251	50.639501
79.088309	134.289188	50.644506
76.068445	129.905973	50.649511
71.974618	129.098443	50.654516
69.010435	134.615548	50.659521
64.943421	137.350447	50.664525
61.657223	128.060773	50.669530
58.320502	122.284516	50.674535
54.852864	134.676358	50.679540
51.422606	130.800385	50.684545
47.691835	136.450259	50.689549
44.342749	130.992323	50.694554
40.850534	131.020707	50.699559
36.951171	132.653657	50.704564
33.853817	126.203980	50.709569
29.923682	137.304696	50.714573
26.403128	129.946876	50.719578
23.537203	139.662789	50.724583
19.931828	131.388102	50.729588
16.572961	129.070206	50.734593
12.515044	140.260554	50.739597
9.063836	127.000873	50.744602
5.499762	128.486389	50.749607
1.618583	131.211181	50.754612