Thu Aug 25 17:13:19 2022

Number of Points = 9925

Depth (nm)	Load (N)	Time (s)
2.046770	107.108678	0.000000
2.413706	109.316529	0.005005
2.030389	93.785438	0.010010
2.325450	88.860690	0.015014
2.029580	99.537475	0.020019
1.904105	84.276046	0.025024
1.991483	72.983481	0.030029
1.451149	66.294516	0.035034
1.192047	53.445879	0.040038
0.877265	49.796788	0.045043
0.682815	39.421607	0.050048
0.313589	29.624317	0.055053
0.041463	34.884102	0.060058
-0.014963	20.817312	0.065062
-0.312754	13.666419	0.070067
-1.127527	10.304485	0.075072
-1.157970	2.219520	0.080077
-1.266938	9.750641	0.085082
-1.608591	-1.101329	0.090086
-2.455328	-2.977602	0.095091
-2.362989	-1.875193	0.100096
-2.394813	-4.407499	0.105101
-2.770967	1.165971	0.110106
-3.104003	-4.378518	0.115110
-3.118728	-9.131314	0.120115
-3.829179	-5.637856	0.125120
-3.815827	-9.670544	0.130125
-3.942001	-7.860014	0.135130
-4.776709	-7.374825	0.140134
-5.308673	-3.937806	0.145139
-5.721023	-8.802309	0.150144
-5.363764	-10.449606	0.155149
-5.460081	-7.185251	0.160154
-5.276014	-12.054614	0.165158
-5.508303	-5.329924	0.170163
-6.243596	-0.636663	0.175168
-6.560012	-12.153811	0.180173
-7.164322	-4.586214	0.185178
-6.744876	-10.859211	0.190182
-6.987141	-6.069192	0.195187
-7.046142	-8.113181	0.200192
-7.926563	-13.825004	0.205197
-8.404072	-8.757680	0.210202
-8.195052	-12.675491	0.215206
-8.590413	-4.934987	0.220211
-8.541207	2.378357	0.225216
-8.444339	-5.799318	0.230221
-8.942396	-1.481753	0.235226
-9.008940	-9.257332	0.240230
-9.573194	-2.809661	0.245235
-10.233504	0.027367	0.250240
-10.540248	-11.076841	0.255245
-11.574062	-3.767817	0.260250
-10.941025	-10.599468	0.265254
-10.751199	-6.396011	0.270259
-11.077135	5.433881	0.275264
-11.369449	-10.060755	0.280269
-11.573129	-1.521372	0.285274
-11.473190	-7.902499	0.290278
-11.957496	-11.971108	0.295283
-13.174421	-3.257149	0.300288
-12.775417	-11.377756	0.305293
-13.101949	-8.434837	0.310298
-12.972157	-13.789246	0.315302
-13.501086	-4.575640	0.320307
-14.082958	-2.140047	0.325312
-14.060833	-6.123490	0.330317
-14.466981	2.185024	0.335322
-14.573479	-8.086847	0.340326
-14.528751	-1.693464	0.345331
-14.670568	-5.923305	0.350336
-15.337942	-14.246990	0.355341
-15.719209	-7.195235	0.360346
-15.780894	-7.944817	0.365350
-15.702370	-3.904255	0.370355
-15.688295	-5.092817	0.375360
-16.260081	-4.791194	0.380365
-16.991535	-6.407114	0.385370
-16.865823	-9.400704	0.390374
-16.887116	-1.016450	0.395379
-17.648862	-8.784343	0.400384
-18.382378	-4.334972	0.405389
-18.275190	-7.623055	0.410394
-18.426851	-17.482881	0.415398
-18.771317	-12.559790	0.420403
-18.941539	-15.339331	0.425408
-18.491701	-18.067327	0.430413
-19.013966	-4.982298	0.435418
-19.109903	-10.832855	0.440422
-19.757480	-8.288891	0.445427
-20.230805	-4.234630	0.450432
-20.163522	-5.184755	0.455437
-20.203849	-0.578236	0.460442
-20.390996	-14.785867	0.465446
-20.897828	-5.088500	0.470451
-21.662428	1.251357	0.475456
-21.363388	-2.044641	0.480461
-21.788642	2.014744	0.485466
-21.786387	-4.506104	0.490470
-22.209206	3.055206	0.495475
-22.999308	-6.116128	0.500480
-23.180971	-3.388897	0.505485
-23.638609	-3.652492	0.510490
-23.509754	-8.434111	0.515494
-23.363132	-0.680449	0.520499
-23.738094	-1.273376	0.525504
-23.378526	-3.098208	0.530509
-23.956284	-3.681507	0.535514
-24.678570	-1.043577	0.540518
-24.655303	-4.309020	0.545523
-24.713863	2.859855	0.550528
-24.946614	0.684900	0.555533
-25.898126	7.490648	0.560538
-26.061024	-1.984607	0.565542
-26.281043	-2.152554	0.570547
-26.043061	-1.158388	0.575552
-26.091559	-4.026606	0.580557
-27.066769	-2.174794	0.585562
-27.617739	3.128673	0.590566
-27.750207	-7.762394	0.595571
-27.973846	-2.402648	0.600576
-27.818373	-8.710216	0.605581
-27.728459	5.373568	0.610586
-28.105573	5.881975	0.615590
-27.628078	-2.415451	0.620595
-28.554413	-2.162679	0.625600
-28.815599	-7.114141	0.630605
-29.074018	-4.295789	0.635610
-29.497095	-9.921080	0.640614
-30.155153	-5.872677	0.645619
-30.388386	-12.650855	0.650624
-30.469668	-16.899669	0.655629
-30.602569	-0.740340	0.660634
-30.718964	-7.508352	0.665638
-30.867636	-6.801620	0.670643
-31.286948	-3.641681	0.675648
-31.403024	-7.612961	0.680653
-31.964748	-4.164950	0.685658
-32.222675	-10.904458	0.690662
-32.271858	-7.679126	0.695667
-32.432393	-0.412016	0.700672
-32.355698	-2.382353	0.705677
-33.012022	0.147165	0.710682
-33.132527	-4.620694	0.715686
-33.249840	-2.466699	0.720691
-33.407653	-0.426582	0.725696
-34.136411	-1.941683	0.730701
-34.497044	0.607944	0.735706
-34.826911	1.494929	0.740710
-34.606292	4.364775	0.745715
-34.893664	-6.780433	0.750720
-34.769321	-9.204328	0.755725
-35.577690	-4.268660	0.760730
-35.996753	-2.874150	0.765734
-36.160620	3.982192	0.770739
-36.258289	3.329998	0.775744
-36.330845	-2.701396	0.780749
-37.088422	3.017261	0.785754
-37.301490	-1.587398	0.790758
-37.532753	-0.484906	0.795763
-37.739829	-4.840564	0.800768
-37.580249	-7.361730	0.805773
-38.232753	0.010938	0.810778
-38.109390	-2.817768	0.815782
-38.483960	-5.426085	0.820787
-39.334255	-8.447083	0.825792
-39.396798	-2.957554	0.830797
-39.438020	0.228566	0.835802
-39.729504	3.330512	0.840806
-39.592250	6.406411	0.845811
-39.898002	-3.369164	0.850816
-39.749602	-4.990065	0.855821
-40.771518	-4.216110	0.860826
-41.095285	-4.563956	0.865830
-40.870690	5.572473	0.870835
-41.620564	6.006407	0.875840
-41.079389	-0.972208	0.880845
-41.481161	4.703355	0.885850
-42.529757	-0.583480	0.890854
-42.721565	2.300366	0.895859
-42.653063	6.836049	0.900864
-42.431727	-5.265234	0.905869
-42.860284	-2.018424	0.910874
-43.369619	7.866004	0.915878
-43.720088	-5.158095	0.920883
-43.939469	0.947636	0.925888
-44.353314	0.740456	0.930893
-44.545711	-1.630647	0.935898
-44.248167	-1.145692	0.940902
-44.353549	-0.097726	0.945907
-45.000168	3.702113	0.950912
-45.188883	-10.109799	0.955917
-45.542995	2.183251	0.960922
-45.342059	-0.236827	0.965926
-46.305134	1.356820	0.970931
-46.937696	-2.346871	0.975936
-46.957310	0.111358	0.980941
-46.940310	3.582588	0.985946
-47.375827	-9.269993	0.990950
-47.429477	1.824363	0.995955
-47.150650	2.185699	1.000960
-47.110445	-1.487362	1.005965
-48.120691	-4.666798	1.010970
-48.229823	-4.697094	1.015974
-48.487911	-8.709396	1.020979
-49.015055	-5.877413	1.025984
-48.834639	-9.534477	1.030989
-49.593791	-0.139261	1.035994
-50.054983	-1.968370	1.040998
-49.853173	-8.292690	1.046003
-49.928836	0.698037	1.051008
-49.978285	-2.185850	1.056013
-50.326616	3.497157	1.061018
-51.589100	-3.258958	1.066022
-51.474717	-5.738241	1.071027
-51.711395	-3.429501	1.076032
-51.593356	-3.995269	1.081037
-51.695272	-1.717135	1.086042
-51.554055	0.067318	1.091046
-51.603583	3.564791	1.096051
-52.553399	0.157585	1.101056
-52.591315	7.250459	1.106061
-52.755932	4.691504	1.111066
-53.668962	6.682274	1.116070
-54.163971	-1.086282	1.121075
-54.204193	-0.108638	1.126080
-54.077266	-9.012360	1.131085
-54.715633	0.661325	1.136090
-54.468484	6.425037	1.141094
-54.454590	-0.629149	1.146099
-54.721295	5.528292	1.151104
-55.176212	-2.604053	1.156109
-55.744193	-1.524732	1.161114
-55.733648	2.624558	1.166118
-56.158439	0.758108	1.171123
-56.368959	10.624190	1.176128
-56.246674	-4.660156	1.181133
-57.186061	11.884977	1.186138
-57.064066	2.542256	1.191142
-56.873458	0.800845	1.196147
-57.537242	5.973292	1.201152
-57.361573	-2.580564	1.206157
-58.672394	1.820061	1.211162
-59.127091	10.860691	1.216166
-58.802960	14.125610	1.221171
-59.339900	12.789264	1.226176
-58.990721	6.723425	1.231181
-58.858055	7.575903	1.236186
-59.393824	7.330880	1.241190
-59.738735	6.423195	1.246195
-60.457853	5.134377	1.251200
-60.070070	-0.260458	1.256205
-60.439477	-1.736949	1.261210
-60.721360	-0.822681	1.266214
-60.851051	2.089398	1.271219
-61.613703	2.914481	1.276224
-62.033570	-8.130867	1.281229
-62.379022	1.920869	1.286234
-62.048978	-6.650846	1.291238
-61.973610	2.591465	1.296243
-62.240477	4.800531	1.301248
-62.408772	7.468721	1.306253
-63.557631	7.696252	1.311258
-63.467369	3.240220	1.316262
-63.860806	3.064645	1.321267
-64.169258	6.061681	1.326272
-63.814801	-1.137616	1.331277
-64.020776	3.947278	1.336282
-64.832472	-6.748771	1.341286
-65.100417	0.199807	1.346291
-65.509008	1.589514	1.351296
-65.308256	8.293811	1.356301
-65.290948	4.064347	1.361306
-65.767680	8.932237	1.366310
-66.063804	3.799586	1.371315
-66.572218	7.242410	1.376320
-66.693415	-5.108923	1.381325
-66.914894	3.955272	1.386330
-67.027272	5.504212	1.391334
-66.933350	1.234271	1.396339
-67.901738	-0.493218	1.401344
-68.015032	-0.545009	1.406349
-68.202842	3.189268	1.411354
-68.249673	1.943810	1.416358
-68.059507	-2.796796	1.421363
-68.860347	-5.993221	1.426368
-69.495609	0.788284	1.431373
-69.560997	8.764993	1.436378
-69.787977	2.235772	1.441382
-69.844401	-1.061477	1.446387
-70.042777	5.142205	1.451392
-70.362580	8.979423	1.456397
-70.819029	4.628037	1.461402
-71.228002	6.805587	1.466406
-71.366893	-3.834532	1.471411
-71.414876	3.446580	1.476416
-71.106329	-2.280692	1.481421
-71.729585	6.890751	1.486426
-72.397472	0.845072	1.491430
-72.552003	-5.331663	1.496435
-73.017796	3.868891	1.501440
-72.445535	1.479215	1.506445
-72.919446	-1.189465	1.511450
-73.238715	-0.987516	1.516454
-73.684683	-8.263873	1.521459
-74.223974	11.059642	1.526464
-73.821372	5.792197	1.531469
-74.046724	1.167319	1.536474
-74.595431	-5.513970	1.541478
-75.373773	1.486109	1.546483
-75.921182	8.307635	1.551488
-75.581943	6.615701	1.556493
-75.738155	2.732969	1.561498
-75.481754	0.880008	1.566502
-75.679525	-5.913216	1.571507
-75.649650	0.979205	1.576512
-76.180922	-0.658586	1.581517
-77.149855	5.662671	1.586522
-77.078830	5.126415	1.591526
-77.082004	-1.260700	1.596531
-77.890966	3.709866	1.601536
-77.861833	-1.429454	1.606541
-78.572471	-4.526116	1.611546
-78.431902	6.667523	1.616550
-78.537674	0.381905	1.621555
-78.727516	-3.599961	1.626560
-79.069726	-3.834183	1.631565
-79.462016	9.420314	1.636570
-79.932304	0.825303	1.641574
-80.071844	-5.072204	1.646579
-80.127604	4.038791	1.651584
-79.709735	-5.185769	1.656589
-80.405446	-3.153118	1.661594
-81.003493	0.927015	1.666598
-81.007541	-1.568513	1.671603
-81.301214	14.404042	1.676608
-81.976991	-3.254643	1.681613
-82.754395	-6.438919	1.686618
-82.832931	-8.840516	1.691622
-81.745615	-0.281959	1.696627
-82.437160	2.873182	1.701632
-82.496575	-1.730240	1.706637
-82.876422	-8.842948	1.711642
-83.445485	3.787504	1.716646
-83.976365	8.059597	1.721651
-84.324904	-0.522852	1.726656
-84.114341	-0.824706	1.731661
-84.456174	8.074850	1.736666
-84.482719	7.667778	1.741670
-84.669784	0.290739	1.746675
-85.515615	13.632124	1.751680
-85.416674	-1.980762	1.756685
-85.602018	3.932973	1.761690
-86.341193	-5.315933	1.766694
-85.493738	-2.762612	1.771699
-86.385948	-6.492052	1.776704
-86.773547	-0.015111	1.781709
-87.556091	-3.821847	1.786714
-87.335747	4.195509	1.791718
-87.302156	2.579942	1.796723
-87.252729	17.343958	1.801728
-87.571868	3.606262	1.806733
-88.307546	3.465331	1.811738
-88.714091	-1.283016	1.816742
-88.816087	2.051833	1.821747
-88.969436	-0.670239	1.826752
-88.983462	-3.588149	1.831757
-89.338156	3.162049	1.836762
-89.879061	3.490477	1.841766
-90.333487	2.049455	1.846771
-90.789083	7.458204	1.851776
-90.495381	-4.679725	1.856781
-90.720478	0.518895	1.861786
-90.782373	2.812905	1.866790
-90.280897	-1.410164	1.871795
-91.496655	4.661865	1.876800
-91.439576	0.903902	1.881805
-92.171189	7.893497	1.886810
-92.075225	1.231417	1.891814
-92.036994	6.638717	1.896819
-92.611729	8.139881	1.901824
-93.215086	-4.974300	1.906829
-93.636567	6.655421	1.911834
-93.508804	-0.109718	1.916838
-93.509259	1.579873	1.921843
-94.080035	9.332049	1.926848
-93.933056	-4.545116	1.931853
-94.935306	3.157606	1.936858
-95.156909	-8.488285	1.941862
-94.788595	-4.901262	1.946867
-95.073891	-4.783730	1.951872
-95.029198	-5.654384	1.956877
-95.219954	-5.200487	1.961882
-96.033033	5.152315	1.966886
-96.451945	-0.356564	1.971891
-96.732379	6.771144	1.976896
-96.830157	6.612518	1.981901
-96.566303	2.455156	1.986906
-97.096485	-1.891000	1.991910
-97.527277	-5.945841	1.996915
-98.010649	2.654501	2.006912
-97.631826	-1.893553	2.016909
-96.720657	-2.562065	2.026906
-96.631757	-5.255857	2.036902
-95.602850	-2.759148	2.046899
-95.240194	-5.679570	2.056896
-95.414027	2.672850	2.066893
-94.810578	-2.420421	2.076890
-93.876375	-0.586788	2.086886
-93.243117	-4.072303	2.096883
-92.744025	-2.129309	2.106880
-92.701871	-5.404994	2.116877
-92.008629	2.171661	2.126874
-91.127330	-7.222712	2.136870
-91.288577	-6.652457	2.146867
-90.670758	1.211617	2.156864
-90.052285	-2.325436	2.166861
-89.715043	-2.942031	2.176858
-88.630002	-5.883777	2.186854
-88.452944	0.053627	2.196851
-88.200942	1.737562	2.206848
-87.641538	-0.925417	2.216845
-87.289175	-2.561255	2.226842
-85.938035	-4.112837	2.236838
-85.946281	-3.677430	2.246835
-85.487726	-9.549457	2.256832
-84.639579	-5.636913	2.266829
-84.476572	-3.166083	2.276826
-84.244346	-2.087272	2.286822
-83.082759	-3.618656	2.296819
-82.848164	-4.054440	2.306816
-82.816471	0.062064	2.316813
-82.489170	-4.275174	2.326810
-81.353166	0.057938	2.336806
-80.395254	-1.362337	2.346803
-80.354600	-1.634683	2.356800
-80.379279	-1.842938	2.366797
-79.602236	-2.607642	2.376794
-78.910540	5.149824	2.386790
-78.280033	-2.618169	2.396787
-77.281070	-5.555931	2.406784
-77.327530	1.493560	2.416781
-77.356932	1.064296	2.426778
-76.650242	0.114211	2.436774
-75.806051	-4.310355	2.446771
-75.468118	-1.746555	2.456768
-74.530487	-7.012565	2.466765
-74.327763	1.537447	2.476762
-74.497274	2.926297	2.486758
-73.196109	-3.755676	2.496755
-73.181275	1.000204	2.506752
-72.493234	1.719321	2.516749
-71.792285	3.266388	2.526746
-71.415247	1.100824	2.536742
-70.663868	-2.827689	2.546739
-70.063566	1.963168	2.556736
-70.156290	7.233254	2.566733
-69.866799	3.801602	2.576730
-68.907019	5.203575	2.586726
-68.155468	-0.768218	2.596723
-67.639393	1.926062	2.606720
-66.993933	2.132327	2.616717
-67.525141	-2.843344	2.626714
-66.528979	4.441928	2.636710
-66.094548	-1.210909	2.646707
-65.167738	1.076887	2.656704
-64.778244	-5.566775	2.666701
-64.727997	-3.106785	2.676698
-63.802736	-7.160745	2.686694
-63.166580	-0.566674	2.696691
-62.971573	-2.120835	2.706688
-62.382102	-5.266866	2.716685
-61.540277	-6.554906	2.726682
-61.224926	-4.535602	2.736678
-61.351173	-4.411161	2.746675
-60.243837	-1.359693	2.756672
-59.948839	-0.521969	2.766669
-59.447749	-1.759788	2.776666
-58.502753	-5.918211	2.786662
-58.392622	-5.067359	2.796659
-58.090226	-4.195948	2.806656
-57.430455	-2.471365	2.816653
-57.086428	-7.736231	2.826650
-56.084424	-2.789735	2.836646
-55.493963	-1.858921	2.846643
-55.647916	-1.970893	2.856640
-55.125145	-2.936508	2.866637
-54.408810	-1.100411	2.876634
-54.002309	-1.756367	2.886630
-53.012326	0.838315	2.896627
-52.678017	1.277069	2.906624
-52.610517	-3.694210	2.916621
-51.900808	-1.907759	2.926618
-51.335048	3.978247	2.936614
-51.031515	0.233949	2.946611
-49.728001	4.205030	2.956608
-49.856040	-0.051360	2.966605
-49.765231	-2.222760	2.976602
-48.990812	-6.303770	2.986598
-48.080406	-6.709227	2.996595
-48.100143	-1.127460	3.006592
-47.307414	-6.364429	3.016589
-47.031798	0.618759	3.026586
-46.413291	-1.635325	3.036582
-45.580650	-1.819520	3.046579
-45.344949	-2.011553	3.056576
-44.996986	0.791432	3.066573
-44.246238	3.056133	3.076570
-43.933918	-1.269256	3.086566
-42.838306	-5.077473	3.096563
-42.566238	-7.958357	3.106560
-42.553212	-7.960276	3.116557
-42.185546	-7.384196	3.126554
-41.346261	-4.705712	3.136550
-40.891504	-2.559362	3.146547
-40.185785	-1.301313	3.156544
-39.543269	-1.899214	3.166541
-39.519324	-2.254473	3.176538
-38.946636	-2.201531	3.186534
-38.505650	-4.085673	3.196531
-37.879339	-1.912349	3.206528
-37.057136	-0.697894	3.216525
-36.531429	1.158571	3.226522
-36.514068	-7.514384	3.236518
-35.826945	-8.350525	3.246515
-35.215496	-8.664789	3.256512
-35.136891	-8.331690	3.266509
-34.100292	-4.455002	3.276506
-33.981326	-10.286492	3.286502
-33.355434	-14.122478	3.296499
-32.524023	-8.512516	3.306496
-32.427760	-3.528639	3.316493
-32.064754	-10.998120	3.326490
-30.919513	-4.569344	3.336486
-30.724185	-7.561750	3.346483
-30.626584	-5.682557	3.356480
-29.481247	-10.816381	3.366477
-29.344959	-9.174502	3.376474
-29.066242	-8.771386	3.386470
-28.307840	-6.007367	3.396467
-27.512550	-9.115953	3.406464
-27.513960	-4.953079	3.416461
-26.355044	-2.185289	3.426458
-26.186070	-7.467076	3.436454
-26.180989	-3.609331	3.446451
-25.179656	-9.465032	3.456448
-24.749067	-0.589586	3.466445
-24.457115	-1.934020	3.476442
-23.660081	2.673962	3.486438
-23.592266	-4.841138	3.496435
-22.568543	-2.590696	3.506432
-22.019098	-5.587902	3.516429
-21.950745	-1.930139	3.526426
-21.168101	-4.190932	3.536422
-20.239922	-6.148241	3.546419
-20.229460	-2.522590	3.556416
-20.233321	4.393517	3.566413
-19.518938	0.290237	3.576410
-18.835738	2.045998	3.586406
-18.186144	3.762676	3.596403
-17.485993	1.923459	3.606400
-17.283266	0.703879	3.616397
-17.079684	6.155624	3.626394
-16.045220	2.892353	3.636390
-15.925129	6.003479	3.646387
-15.228444	4.237664	3.656384
-14.601097	2.124749	3.666381
-14.402842	4.697768	3.676378
-13.659339	-0.015132	3.686374
-12.818018	4.424354	3.696371
-12.512930	-0.378245	3.706368
-12.591767	1.987930	3.716365
-12.124015	-0.660685	3.726362
-11.618834	-2.529543	3.736358
-10.756553	2.983722	3.746355
-10.144288	4.202564	3.756352
-9.681189	3.778497	3.766349
-8.910805	15.606988	3.776346
-8.720509	11.547806	3.786342
-8.432459	8.385646	3.796339
-7.824087	16.545827	3.806336
-7.396870	11.828628	3.816333
-6.981609	16.195488	3.826330
-6.063085	15.633540	3.836326
-5.711922	17.121377	3.846323
-5.539038	24.038311	3.856320
-4.868782	24.918613	3.866317
-4.283361	25.926250	3.876314
-3.719595	41.021495	3.886310
-3.556926	48.817531	3.896307
-2.464729	58.093034	3.906304
-2.744244	51.364102	3.916301
-1.985009	64.056027	3.926298
-1.777913	74.331871	3.936294
-1.460574	86.535508	3.946291
-0.719354	96.372879	3.956288
-0.409610	110.446755	3.966285
0.000000	122.303416	3.971290
0.687879	138.925905	3.976294
1.041780	143.372615	3.981299
0.978611	148.156761	3.986304
1.339111	143.914619	3.991309
0.620476	150.010040	3.996314
0.941041	154.167741	4.001318
1.019296	145.451901	4.006323
1.080657	148.634632	4.011328
1.141515	148.099965	4.016333
0.947147	153.015402	4.021338
0.907469	146.013842	4.026342
1.389998	142.167040	4.031347
1.148185	146.893753	4.036352
0.986571	139.310177	4.041357
1.160250	140.633972	4.046362
1.417326	141.495439	4.051366
1.508782	146.941904	4.056371
1.589029	146.476967	4.061376
1.445284	139.428439	4.066381
1.361940	148.075592	4.071386
1.083808	137.014264	4.076390
1.320261	150.363351	4.081395
1.163227	151.004959	4.086400
1.405677	141.412330	4.091405
1.411756	145.916702	4.096410
1.408134	137.628153	4.101414
1.363305	132.560492	4.106419
1.196608	143.941576	4.111424
1.038520	135.316557	4.116429
1.149176	146.575091	4.121434
1.021199	140.397304	4.126438
1.252555	146.555852	4.131443
0.682157	148.704924	4.136448
1.479398	141.271674	4.141453
1.208663	150.185474	4.146458
1.252906	145.752434	4.151462
1.361910	142.717143	4.156467
0.808235	143.398751	4.161472
1.164062	157.516927	4.166477
1.294309	169.297599	4.171482
1.603338	163.263308	4.176486
1.644581	163.971928	4.181491
1.471538	177.100452	4.186496
1.937377	160.063161	4.191501
1.805298	166.595041	4.196506
1.394758	150.141169	4.201510
1.367664	160.038710	4.206515
1.411562	169.387286	4.211520
1.692757	171.159317	4.216525
1.886900	177.485062	4.221530
1.517412	165.849561	4.226534
1.737738	164.878612	4.231539
1.669831	162.826508	4.236544
1.754579	160.870710	4.241549
1.552468	158.520089	4.246554
1.542673	165.368172	4.251558
2.092113	166.563491	4.256563
1.771569	158.125268	4.261568
1.769037	142.936276	4.266573
1.458560	144.411861	4.271578
1.303288	150.757541	4.276582
1.565497	163.675487	4.281587
1.349708	169.793370	4.286592
1.763057	162.872685	4.291597
1.811877	166.240885	4.296602
2.056685	164.168258	4.301606
1.956417	174.254445	4.306611
1.844836	173.487363	4.311616
1.789193	159.784180	4.316621
1.920940	162.987522	4.321626
1.794415	163.991353	4.326630
2.126203	164.164060	4.331635
1.826158	161.300425	4.336640
2.006151	160.728109	4.341645
1.588226	171.705640	4.346650
1.556215	162.247754	4.351654
1.872243	163.033545	4.356659
1.928501	171.915105	4.361664
1.962009	158.261231	4.366669
1.832755	166.656153	4.371674
1.818741	164.987917	4.376678
1.728451	160.699341	4.381683
1.585339	163.971059	4.386688
1.653969	167.855020	4.391693
2.111455	177.825346	4.396698
2.052364	174.667688	4.401702
1.721388	176.361626	4.406707
1.785048	184.175827	4.411712
2.178674	195.026217	4.416717
2.101287	194.978290	4.421722
2.371686	186.150066	4.426726
2.348075	188.222962	4.431731
2.290858	188.184531	4.436736
2.303349	178.362152	4.441741
1.863864	174.938221	4.446746
1.745550	180.983887	4.451750
2.313988	180.670253	4.456755
2.248467	183.932982	4.461760
2.459793	181.005042	4.466765
2.397534	187.187462	4.471770
2.187513	186.489587	4.476774
2.244968	183.962249	4.481779
2.117337	189.110853	4.486784
2.023304	191.447889	4.491789
2.134841	195.581402	4.496794
2.383083	189.860353	4.501798
2.793542	181.642950	4.506803
2.337956	193.464806	4.511808
2.836730	185.249382	4.516813
2.303524	182.330526	4.521818
2.045833	170.949593	4.526822
2.335890	173.672544	4.531827
2.412048	182.028962	4.536832
2.713011	189.125764	4.541837
1.934640	185.479676	4.546842
2.241053	183.821346	4.551846
2.542091	189.048321	4.556851
2.654112	199.297418	4.561856
3.048006	187.507493	4.566861
2.107443	177.938846	4.571866
2.292670	176.343797	4.576870
2.205916	181.723281	4.581875
2.698650	193.529433	4.586880
2.886077	187.963448	4.591885
2.838248	178.163176	4.596890
2.262568	167.259183	4.601894
2.182868	177.202942	4.606899
2.511614	187.753440	4.611904
2.896918	186.275741	4.616909
2.822865	184.281546	4.621914
2.347670	177.158382	4.626918
2.694597	178.176619	4.631923
2.868933	198.578127	4.636928
2.548607	177.895889	4.641933
2.714828	185.124535	4.646938
2.679586	181.697378	4.651942
2.709274	176.757236	4.656947
2.356502	177.401040	4.661952
2.737529	172.886751	4.666957
3.005447	185.335574	4.671962
2.818418	185.010592	4.676966
2.636400	179.173459	4.681971
2.498764	186.301014	4.686976
2.965963	181.143622	4.691981
2.722633	189.758913	4.696986
2.833609	193.082577	4.701990
2.852358	188.128327	4.706995
2.852695	194.243993	4.712000
2.968255	184.965457	4.717005
2.681301	194.334246	4.722010
2.834011	183.727414	4.727014
2.712416	191.611774	4.732019
2.696075	186.441556	4.737024
3.176041	182.364188	4.742029
2.705244	189.838180	4.747034
3.010235	189.736670	4.752038
2.779329	185.951019	4.757043
2.561525	192.018604	4.762048
2.960201	186.549238	4.767053
2.706672	192.381970	4.772058
2.591564	189.008455	4.777062
2.953697	189.233356	4.782067
3.001703	185.859595	4.787072
3.255390	195.434747	4.792077
3.012067	189.012418	4.797082
3.053410	196.602326	4.802086
2.872920	192.429118	4.807091
2.674141	196.503682	4.812096
2.755279	182.668316	4.817101
2.810363	198.621202	4.822106
2.882796	211.853661	4.827110
3.429893	203.361734	4.832115
3.180166	215.540500	4.837120
3.237953	214.712077	4.842125
3.495043	205.892256	4.847130
2.912568	199.561028	4.852134
3.289395	202.162818	4.857139
2.976831	216.176954	4.862144
3.413133	222.379349	4.867149
3.443462	219.805635	4.872154
3.194191	208.106977	4.877158
3.220848	197.209833	4.882163
2.929262	209.404645	4.887168
3.415342	205.547782	4.892173
3.307495	215.983200	4.897178
3.181771	211.950106	4.902182
3.274448	211.094070	4.907187
3.073187	221.847855	4.912192
3.352602	212.375949	4.917197
3.435288	214.976371	4.922202
3.513680	221.228516	4.927206
3.241497	216.721648	4.932211
3.259111	220.689545	4.937216
3.781811	216.782648	4.942221
3.378291	219.332697	4.947226
3.380667	215.788906	4.952230
3.466797	211.716290	4.957235
3.292730	222.810671	4.962240
3.687351	210.859262	4.967245
3.527980	209.732663	4.972250
3.507619	214.532266	4.977254
4.019950	211.190156	4.982259
3.494926	199.841599	4.987264
3.493749	189.667008	4.992269
3.178175	192.317171	4.997274
3.471769	206.856433	5.002278
3.677124	204.498912	5.007283
3.379954	211.977347	5.012288
3.756778	208.147093	5.017293
3.859608	214.028404	5.022298
3.515191	213.838814	5.027302
3.767214	211.505618	5.032307
3.402662	211.452064	5.037312
3.923233	208.583236	5.042317
3.820222	223.940806	5.047322
3.325037	213.653773	5.052326
3.548174	208.781392	5.057331
3.377454	210.178135	5.062336
3.631449	210.125745	5.067341
3.685617	212.670522	5.072346
4.036689	209.480231	5.077350
4.241557	207.882102	5.082355
3.518400	213.772604	5.087360
3.545230	208.538666	5.092365
3.404334	213.815909	5.097370
3.469024	205.833007	5.102374
3.749141	205.475961	5.107379
3.517611	217.531652	5.112384
3.683201	215.291094	5.117389
3.769737	211.692987	5.122394
3.631167	198.581746	5.127398
3.517760	205.971274	5.132403
3.714671	218.997570	5.137408
3.836461	223.445865	5.142413
3.690657	236.392991	5.147418
3.541286	229.645872	5.152422
3.910888	236.396573	5.157427
3.873728	243.030670	5.162432
3.936473	236.579352	5.167437
3.900859	238.834473	5.172442
3.900372	232.861309	5.177446
3.945092	225.973047	5.182451
3.940099	233.089330	5.187456
4.122458	231.437777	5.192461
3.798801	230.077483	5.197466
3.960058	233.712823	5.202470
3.884096	217.722170	5.207475
3.461185	229.649664	5.212480
4.011954	227.124122	5.217485
4.080600	241.708149	5.222490
4.111492	245.949225	5.227494
4.172755	244.392576	5.232499
4.080580	254.819234	5.237504
4.376823	245.388968	5.242509
4.489287	252.391940	5.247514
3.937858	232.682341	5.252518
3.673445	233.454675	5.257523
3.930427	248.246486	5.262528
4.407635	247.330199	5.267533
4.294400	255.447400	5.272538
4.119273	256.427213	5.277542
4.631876	252.328897	5.282547
4.381083	255.905412	5.287552
4.292646	247.908519	5.292557
4.106017	247.855561	5.297562
4.156296	249.594177	5.302566
4.231241	249.433796	5.307571
4.067581	253.233945	5.312576
3.985116	264.200102	5.317581
4.424508	261.650877	5.322586
4.649685	255.920765	5.327590
4.673504	248.554867	5.332595
4.238185	256.320727	5.337600
4.282229	256.149368	5.342605
4.324607	254.804490	5.347610
4.272150	251.253464	5.352614
4.393721	258.928907	5.357619
4.417909	264.344818	5.362624
4.786537	255.877665	5.367629
4.367112	247.951613	5.372634
4.287880	256.528570	5.377638
4.191583	252.876842	5.382643
4.088620	258.265216	5.387648
4.353128	253.069958	5.392653
4.447117	255.814150	5.397658
4.382875	248.575948	5.402662
4.487983	255.266855	5.407667
4.501352	256.780295	5.412672
4.677181	267.974910	5.417677
4.627439	272.731675	5.422682
4.633830	270.601476	5.427686
4.548775	262.278171	5.432691
4.671883	270.744336	5.437696
4.698231	269.050783	5.442701
4.546363	277.167720	5.447706
4.677929	270.006400	5.452710
5.068575	263.434091	5.457715
4.645593	265.411379	5.462720
4.582249	255.518580	5.467725
4.168857	258.490970	5.472730
4.327070	274.870701	5.477734
4.822641	279.940670	5.482739
4.652524	282.704101	5.487744
4.739802	282.345629	5.492749
4.348404	282.967013	5.497754
4.541025	282.041530	5.502758
4.612403	285.795369	5.507763
4.886286	292.972387	5.512768
5.081520	278.663478	5.517773
4.744198	288.533765	5.522778
5.101857	277.537253	5.527782
4.906712	280.564039	5.532787
4.615129	281.587410	5.537792
4.947344	277.052269	5.542797
4.659708	280.052416	5.547802
4.969895	274.501973	5.552806
5.213948	279.529091	5.557811
4.670555	275.292497	5.562816
4.942561	277.208351	5.567821
4.699105	286.070487	5.572826
4.451458	281.638854	5.577830
5.196408	303.912654	5.582835
5.157852	300.245542	5.587840
5.317241	300.967295	5.592845
4.836941	298.460920	5.597850
4.897897	299.236061	5.602854
5.387539	309.084361	5.607859
5.206578	305.205436	5.612864
4.957434	284.233504	5.617869
4.566091	302.129418	5.622874
4.977298	309.379842	5.627878
5.439437	298.901636	5.632883
5.450711	306.107150	5.637888
5.458674	304.267774	5.642893
5.066762	295.397731	5.647898
5.052343	295.612028	5.652902
5.223489	297.072277	5.657907
5.443761	304.589903	5.662912
5.485209	291.152987	5.667917
5.294322	280.941627	5.672922
5.305104	274.751543	5.677926
4.903281	281.841434	5.682931
5.250330	283.267793	5.687936
5.285583	279.430929	5.692941
5.270489	280.135726	5.697946
4.734136	290.366237	5.702950
5.361299	302.467783	5.707955
5.273095	303.446634	5.712960
5.777521	308.841099	5.717965
5.259885	306.530403	5.722970
5.119135	313.658496	5.727974
5.291388	311.831345	5.732979
5.247520	314.068785	5.737984
5.535209	307.800502	5.742989
5.328587	302.014640	5.747994
5.689150	300.667363	5.752998
5.688684	309.890082	5.758003
5.033954	314.558145	5.763008
5.272376	305.734872	5.768013
5.322116	313.060916	5.773018
5.288606	312.822612	5.778022
5.327550	315.556455	5.783027
5.162886	310.846050	5.788032
5.153331	304.551572	5.793037
5.128804	314.894898	5.798042
5.364297	312.573770	5.803046
5.527956	325.358575	5.808051
5.517905	338.300323	5.813056
5.601693	331.399571	5.818061
5.640723	342.115780	5.823066
5.569678	341.829571	5.828070
6.063419	337.689898	5.833075
5.833115	332.907511	5.838080
5.652646	317.739922	5.843085
5.512670	319.242592	5.848090
5.416309	313.572332	5.853094
5.734268	317.160990	5.858099
5.738736	337.336164	5.863104
5.950581	335.736931	5.868109
5.762771	331.175684	5.873114
5.915811	328.712444	5.878118
5.993042	321.834871	5.883123
5.635006	321.834080	5.888128
5.667808	309.164155	5.893133
5.415408	317.882171	5.898138
5.823912	325.177319	5.903142
5.865671	330.435469	5.908147
5.544417	334.564056	5.913152
5.758328	334.628681	5.918157
5.774547	335.809478	5.923162
6.068859	341.407721	5.928166
5.844439	345.461026	5.933171
5.924068	343.445898	5.938176
5.969591	336.456225	5.943181
5.893469	343.317933	5.948186
6.277841	335.348163	5.953190
6.119634	342.406235	5.958195
6.061705	336.277517	5.963200
6.080998	320.790716	5.968205
5.789770	312.515511	5.973210
5.888083	319.061970	5.978214
5.754437	317.991446	5.983219
5.975889	325.296919	5.988224
5.828994	339.133328	5.993229
6.333049	339.263227	5.998234
6.099907	336.721285	6.003238
6.311840	327.652209	6.008243
5.833382	323.174468	6.013248
5.684925	313.092487	6.018253
6.032343	321.726017	6.023258
5.981474	322.939471	6.028262
5.513832	328.381840	6.033267
5.511506	333.384299	6.038272
6.478357	332.318523	6.043277
6.141878	340.926334	6.048282
6.411349	335.682816	6.053286
6.341049	318.023841	6.058291
6.086486	316.687517	6.063296
5.928424	310.577661	6.068301
6.019171	323.671289	6.073306
5.966170	315.842824	6.078310
6.107085	317.026229	6.083315
5.627979	316.421131	6.088320
5.860139	314.543463	6.093325
5.718596	316.603214	6.098330
5.587492	321.610027	6.103334
6.340899	328.480967	6.108339
6.118709	332.796519	6.113344
5.803657	326.024701	6.118349
5.866786	326.960859	6.123354
6.097133	335.147653	6.128358
5.869189	333.800830	6.133363
6.072962	336.113371	6.138368
6.048125	334.842295	6.143373
5.608063	338.138425	6.148378
5.700897	337.399420	6.153382
6.140841	336.542754	6.158387
5.732024	345.813653	6.163392
5.841196	338.367904	6.168397
5.806578	337.987401	6.173402
6.064581	338.079919	6.178406
5.911124	346.583124	6.183411
5.450215	352.081395	6.188416
6.108593	350.478638	6.193421
5.893850	352.135398	6.198426
5.887109	345.577865	6.203430
6.105436	343.249932	6.208435
6.057909	346.364334	6.213440
6.429022	335.938334	6.218445
6.201779	335.980328	6.223450
5.735807	351.388548	6.228454
6.215655	347.991389	6.233459
5.895492	344.786018	6.238464
6.267008	341.494422	6.243469
6.009120	342.515680	6.248474
5.656060	339.859645	6.253478
5.970641	344.840929	6.258483
5.953586	345.175866	6.263488
5.860843	343.213055	6.268493
6.060362	344.804908	6.273498
5.836777	346.115029	6.278502
5.739115	343.045644	6.283507
5.905758	345.572818	6.288512
6.319178	346.469912	6.293517
6.208475	343.083022	6.298522
5.818837	333.526050	6.303526
6.167463	336.521432	6.308531
5.923089	340.777184	6.313536
6.122625	336.326094	6.318541
6.086924	337.037285	6.323546
6.274088	339.944067	6.328550
6.056371	343.040841	6.333555
5.951028	336.875258	6.338560
5.801536	338.521793	6.343565
5.815566	340.430617	6.348570
6.159259	339.772534	6.353574
6.301521	336.330191	6.358579
6.140200	327.509427	6.363584
5.738554	321.149822	6.368589
5.727293	325.134922	6.373594
6.006407	331.510685	6.378598
6.480951	324.558204	6.383603
6.088051	323.885814	6.388608
5.778400	314.895302	6.393613
5.922633	311.588700	6.398618
5.868251	316.823943	6.403622
6.045954	304.099680	6.408627
5.554330	315.652009	6.413632
6.186577	326.392324	6.418637
5.849960	337.208516	6.423642
6.044677	335.526543	6.428646
6.122740	331.062847	6.433651
5.836057	344.174496	6.438656
6.132503	339.496243	6.443661
5.966484	325.690000	6.448666
5.963889	318.568664	6.453670
6.037056	316.598845	6.458675
5.722684	318.983075	6.463680
5.846224	325.728070	6.468685
6.056790	330.551635	6.473690
6.281346	336.799903	6.478694
5.888841	323.747339	6.483699
5.898974	342.893384	6.488704
6.224717	336.710879	6.493709
6.077330	311.828282	6.498714
5.607952	323.317017	6.503718
6.035873	325.043929	6.508723
6.001838	333.370225	6.513728
5.880365	332.206042	6.518733
6.083477	331.762980	6.523738
6.243496	331.225426	6.528742
5.937169	320.522753	6.533747
6.108286	316.677249	6.538752
6.152555	312.623824	6.543757
5.813967	310.212306	6.548762
5.512001	315.900803	6.553766
6.218897	324.576090	6.558771
5.810756	317.470838	6.563776
6.023872	319.769257	6.568781
5.996438	325.623557	6.573786
5.753631	319.878161	6.578790
6.173094	328.433966	6.583795
6.092640	338.381096	6.588800
5.690368	321.255036	6.593805
5.879821	328.812302	6.598810
6.161070	336.070444	6.603814
6.275357	340.931244	6.608819
5.928553	319.537962	6.613824
6.021328	316.770947	6.618829
5.741785	321.184069	6.623834
5.752105	335.448273	6.628838
6.245307	334.317499	6.633843
6.212972	325.720141	6.638848
6.303974	321.564478	6.643853
6.042246	310.519455	6.648858
5.840080	303.119338	6.653862
6.007397	298.502457	6.658867
5.800757	310.351825	6.663872
5.784541	307.076691	6.668877
5.663802	312.600748	6.673882
5.693279	316.237768	6.678886
6.267001	325.984316	6.683891
6.027059	336.399372	6.688896
6.003087	330.822172	6.693901
5.770010	325.148018	6.698906
5.606540	338.439680	6.703910
6.078510	337.062290	6.708915
5.793877	328.472823	6.713920
6.099788	338.346762	6.718925
5.878688	334.901238	6.723930
5.789077	339.338392	6.728934
6.433906	328.992900	6.733939
6.387746	336.027086	6.738944
5.700574	330.455717	6.743949
5.899539	329.722232	6.748954
5.814439	325.780825	6.753958
6.111324	334.175499	6.758963
5.788158	345.562243	6.763968
5.904404	339.637195	6.768973
6.034360	338.914521	6.773978
5.891612	335.874349	6.778982
6.286151	336.973723	6.783987
6.213519	355.313314	6.788992
6.211725	343.585283	6.793997
6.015616	333.298779	6.799002
6.266680	323.875551	6.804006
6.130329	311.687720	6.809011
5.825773	312.896628	6.814016
5.676242	310.759216	6.819021
6.191572	308.726447	6.824026
6.114936	302.451971	6.829030
6.279418	303.720270	6.834035
5.841854	318.760171	6.839040
5.515936	318.051976	6.844045
5.672898	309.678074	6.849050
5.869775	314.190560	6.854054
5.968590	332.610835	6.859059
5.776898	337.529067	6.864064
5.881660	332.251244	6.869069
5.813816	334.793009	6.874074
5.793521	336.884386	6.879078
6.308836	335.098396	6.884083
6.002756	346.007887	6.889088
6.282298	336.077139	6.894093
6.442766	338.504036	6.899098
5.966669	327.587506	6.904102
6.127259	315.821396	6.909107
5.486230	326.137932	6.914112
6.242567	323.497909	6.919117
5.961813	318.096991	6.924122
5.706321	311.967597	6.929126
6.232957	316.940958	6.934131
5.935519	318.509429	6.939136
6.031796	310.670232	6.944141
5.750650	309.059656	6.949146
5.991941	314.887668	6.954150
6.383038	320.296729	6.959155
5.783733	319.922442	6.964160
5.791823	309.028139	6.969165
6.101155	310.343348	6.974170
6.297935	313.549184	6.979174
6.189329	310.044909	6.984179
5.861860	314.155483	6.989184
6.025939	314.297519	6.994189
5.586949	310.727948	6.999194
5.872942	304.633942	7.004198
5.989681	308.453447	7.009203
6.054336	311.490154	7.014208
5.964068	313.377350	7.019213
5.813429	314.527340	7.024218
5.878826	311.786762	7.029222
5.955479	313.147919	7.034227
5.828888	330.591081	7.039232
6.139053	336.677235	7.044237
6.257649	330.989109	7.049242
5.782353	322.334603	7.054246
6.031754	311.301247	7.059251
5.659075	316.118113	7.064256
6.406797	315.472660	7.069261
6.217229	316.141518	7.074266
6.076871	317.334191	7.079270
6.068651	305.363576	7.084275
5.780643	314.258017	7.089280
5.543879	312.953707	7.094285
5.908462	317.300708	7.099290
6.213837	333.182860	7.104294
6.472555	323.046568	7.109299
5.767606	321.480246	7.114304
5.901771	315.343585	7.119309
5.993933	310.583448	7.124314
6.184925	317.210301	7.129318
5.973461	319.391741	7.134323
5.785516	317.029387	7.139328
6.125238	313.581421	7.144333
6.082125	317.527217	7.149338
5.957147	316.075674	7.154342
5.765232	314.571343	7.159347
5.780737	318.681965	7.164352
5.735511	315.692957	7.169357
6.003407	317.675901	7.174362
5.819965	316.825156	7.179366
6.224057	317.919869	7.184371
6.129790	321.152325	7.189376
5.987988	309.566479	7.194381
5.608311	317.219241	7.199386
6.010713	329.204156	7.204390
6.433081	320.791829	7.209395
6.082378	320.717121	7.214400
6.228164	316.881914	7.219405
5.953359	324.265140	7.224410
5.805083	314.894993	7.229414
5.981856	314.759787	7.234419
5.943153	319.113027	7.239424
5.984482	318.793392	7.244429
6.137018	317.339499	7.249434
6.091958	319.599274	7.254438
5.925307	314.784772	7.259443
5.701414	307.698113	7.264448
5.894178	313.998812	7.269453
5.967966	306.710484	7.274458
5.860877	321.850473	7.279462
5.959366	313.020646	7.284467
5.854733	321.962292	7.289472
5.933963	307.437411	7.294477
6.239499	309.904852	7.299482
6.179182	314.131759	7.304486
6.156506	317.552319	7.309491
5.617522	315.441125	7.314496
6.049704	309.074269	7.319501
5.862663	314.564421	7.324506
5.503021	315.199813	7.329510
5.983166	319.576166	7.334515
5.996394	338.329405	7.339520
6.110189	333.442484	7.344525
5.979712	335.478355	7.349530
5.786704	333.585041	7.354534
6.143591	332.722405	7.359539
6.185985	328.125090	7.364544
6.294597	324.805084	7.369549
5.964896	323.720984	7.374554
5.905607	313.659834	7.379558
5.891783	316.117200	7.384563
5.621725	311.002517	7.389568
5.847073	315.880712	7.394573
6.162508	320.225923	7.399578
5.832351	316.620315	7.404582
6.341165	323.542231	7.409587
5.921403	319.289420	7.414592
5.962936	311.908065	7.419597
6.015345	314.753697	7.424602
5.996474	312.067452	7.429606
6.022768	303.612784	7.434611
5.903063	315.654184	7.439616
5.777756	308.852643	7.444621
6.163174	317.461233	7.449626
5.699848	312.984289	7.454630
6.194598	311.546381	7.459635
5.954736	317.725035	7.464640
5.930631	312.843906	7.469645
5.832487	315.244879	7.474650
5.844865	317.239383	7.479654
6.164829	333.774164	7.484659
6.051548	328.460901	7.489664
5.978516	326.998055	7.494669
6.017615	320.835157	7.499674
5.721677	317.901249	7.504678
5.918696	320.844450	7.509683
5.977679	341.662838	7.514688
6.196509	336.183639	7.519693
5.867674	326.069800	7.524698
5.782524	326.950094	7.529702
6.046682	337.697467	7.534707
5.983969	338.346451	7.539712
5.996969	342.530239	7.544717
5.884600	338.827227	7.549722
6.150195	347.128730	7.554726
6.426087	329.687592	7.559731
5.949436	326.104935	7.564736
6.035841	325.559933	7.569741
6.295974	320.105906	7.574746
5.898005	330.216679	7.579750
5.738019	322.803617	7.584755
5.652924	332.374974	7.589760
5.841401	326.002003	7.594765
6.081176	320.696702	7.599770
6.026672	322.957957	7.604774
6.284301	316.716527	7.609779
6.168512	322.641618	7.614784
6.186438	321.050623	7.619789
5.934550	318.014898	7.624794
5.743165	321.889010	7.629798
5.691699	314.209006	7.634803
5.494286	319.409711	7.639808
5.984749	332.554616	7.644813
6.241460	338.022705	7.649818
6.241272	337.032512	7.654822
6.486443	319.219701	7.659827
6.048860	329.789109	7.664832
5.750608	317.746867	7.669837
5.707708	324.701442	7.674842
5.996381	320.543281	7.679846
5.944555	308.218820	7.684851
5.919678	326.772367	7.689856
5.911131	316.959536	7.694861
6.282927	320.833996	7.699866
5.765139	326.980267	7.704870
6.043660	325.743921	7.709875
6.094556	327.966515	7.714880
6.194563	317.174868	7.719885
5.986670	316.720271	7.724890
5.512686	317.462166	7.729894
5.888644	316.659820	7.734899
5.690940	322.657859	7.739904
5.810902	327.112794	7.744909
5.943404	333.748817	7.749914
5.642212	334.669290	7.754918
6.203523	341.763327	7.759923
6.475955	343.046354	7.764928
6.015852	327.615677	7.769933
5.851295	316.681979	7.774938
5.979510	322.660591	7.779942
6.369213	318.622647	7.784947
6.063513	324.267438	7.789952
5.629551	317.507926	7.794957
5.892017	316.830933	7.799962
5.815015	322.234241	7.804966
6.139375	317.744614	7.809971
5.860659	314.706765	7.814976
6.273779	303.970474	7.819981
6.172767	315.540697	7.824986
5.964248	320.202126	7.829990
6.372912	314.085733	7.834995
5.923453	317.715534	7.840000
5.886961	318.721086	7.845005
5.756707	320.310820	7.850010
6.006705	320.316005	7.855014
6.001732	314.729505	7.860019
6.396124	324.494658	7.865024
5.647778	318.290619	7.870029
5.910500	319.246126	7.875034
5.847752	313.526306	7.880038
5.770014	312.674819	7.885043
5.792309	319.087652	7.890048
5.606444	316.430736	7.895053
6.041013	332.333774	7.900058
5.777950	335.978668	7.905062
6.116626	337.412671	7.910067
6.230153	347.443312	7.915072
6.314393	334.702032	7.920077
6.247313	314.682330	7.925082
5.954344	319.331680	7.930086
5.998606	319.153958	7.935091
5.869833	315.206741	7.940096
5.639082	310.032115	7.945101
6.003608	311.060258	7.950106
5.992454	321.056634	7.955110
6.179775	309.912780	7.960115
5.904911	315.267991	7.965120
6.290587	316.280166	7.970125
5.901702	314.010708	7.975142
5.932832	315.899352	7.980160
6.218698	307.122617	7.985178
5.941683	315.390010	7.990195
5.952806	310.623119	7.995213
6.411118	312.324913	8.000230
5.883589	321.101769	8.005248
5.971625	324.568850	8.010266
5.795884	331.308769	8.015283
6.009102	323.322883	8.020301
6.128397	317.361941	8.025318
5.650607	319.144133	8.030336
5.793020	316.187017	8.035354
5.887525	317.204207	8.040371
5.801601	332.270751	8.045389
6.197532	330.501505	8.050406
6.258725	340.126548	8.055424
6.403088	328.345588	8.060442
5.946301	314.023757	8.065459
5.912010	319.163626	8.070477
5.960886	317.887410	8.075494
5.958298	325.770987	8.080512
6.084380	324.861367	8.085530
6.225051	335.663680	8.090547
6.062860	335.212632	8.095565
6.016377	334.550953	8.100582
5.828097	336.398238	8.105600
5.978581	335.708854	8.110618
6.240965	342.853497	8.115635
6.245509	342.253250	8.120653
6.401112	337.107113	8.125670
5.831068	350.633770	8.130688
6.126682	335.846900	8.135706
6.259743	353.305939	8.140723
5.900660	341.815287	8.145741
6.049657	340.674860	8.150758
6.238883	347.275551	8.155776
6.330836	340.766625	8.160794
6.011110	339.191558	8.165811
6.000470	345.839344	8.170829
6.598941	342.744496	8.175846
6.165582	346.646720	8.180864
6.084530	344.904871	8.185882
5.844073	348.562279	8.190899
6.296175	351.338013	8.195917
6.048048	336.080920	8.200934
6.100090	342.172935	8.205952
5.951173	341.505214	8.210970
5.877441	354.881529	8.215987
6.013217	351.281668	8.221005
6.215024	340.214372	8.226022
5.799072	342.059460	8.231040
6.141805	339.645304	8.236058
6.285074	349.317452	8.241075
6.479298	345.067813	8.246093
5.869684	342.256923	8.251110
6.109465	357.357662	8.256128
6.371000	356.780264	8.261146
6.604983	367.208217	8.266163
6.193202	363.277584	8.271181
6.297304	344.673822	8.276198
6.138123	343.767871	8.281216
6.461479	348.211089	8.286234
6.228667	345.997561	8.291251
6.252091	348.098853	8.296269
6.295817	350.913325	8.301286
6.104662	359.580693	8.306304
6.489018	359.552090	8.311322
6.327860	364.314222	8.316339
6.329846	367.760080	8.321357
6.489477	363.762007	8.326374
6.592541	361.792495	8.331392
6.622026	345.134914	8.336410
6.536850	342.222920	8.341427
6.471202	333.864160	8.346445
6.586002	335.395718	8.351462
6.264163	342.111195	8.356480
6.259802	334.702188	8.361498
6.197921	334.222800	8.366515
6.018180	344.680850	8.371533
5.834607	338.612721	8.376550
6.271660	349.008847	8.381568
6.581629	351.967795	8.386586
6.729049	362.759599	8.391603
6.668600	354.276940	8.396621
6.050958	356.601751	8.401638
6.406440	354.166661	8.406656
6.445971	361.945826	8.411674
6.275276	365.443986	8.416691
6.328484	373.271505	8.421709
6.778554	360.846183	8.426726
6.243333	376.229310	8.431744
6.068264	367.281770	8.436762
6.240975	359.387421	8.441779
6.156629	370.442759	8.446797
6.390834	364.369124	8.451814
6.267150	361.188607	8.456832
6.075845	368.871400	8.461850
6.533289	358.824380	8.466867
6.483437	367.040425	8.471885
6.432790	358.865494	8.476902
6.658221	358.994335	8.481920
6.668761	364.600559	8.486938
6.849588	370.233752	8.491955
6.380258	369.007168	8.496973
6.594109	357.186899	8.501990
6.538887	369.080265	8.507008
6.606210	361.095131	8.512026
6.250045	362.176624	8.517043
6.079889	371.020586	8.522061
6.580853	366.413615	8.527078
6.213893	372.388254	8.532096
6.541686	383.158122	8.537114
6.832638	385.618286	8.542131
6.359419	385.960733	8.547149
6.898641	374.417674	8.552166
6.499511	375.155608	8.557184
6.494342	371.502088	8.562202
6.796158	374.926216	8.567219
6.510862	360.577479	8.572237
6.904543	374.871488	8.577255
6.835972	371.287861	8.582272
6.701197	372.520858	8.587290
6.627523	368.439419	8.592307
6.698802	378.444752	8.597325
6.871834	365.415898	8.602343
6.600500	370.024881	8.607360
6.485023	372.053266	8.612378
6.630943	371.074264	8.617395
6.584043	376.812566	8.622413
6.581253	363.050719	8.627431
6.754420	369.016469	8.632448
6.497613	368.977872	8.637466
6.760009	373.746226	8.642483
6.317076	376.886259	8.647501
6.715456	369.578235	8.652519
6.610559	388.551496	8.657536
6.834425	389.027718	8.662554
6.810142	392.777496	8.667571
6.519516	384.378224	8.672589
6.894098	386.560199	8.677607
6.870968	375.158898	8.682624
6.773170	373.725780	8.687642
6.817703	367.647148	8.692659
6.451200	373.564912	8.697677
7.044808	379.341715	8.702695
6.866471	379.710542	8.707712
6.950052	376.888865	8.712730
6.902148	378.426984	8.717747
6.570053	371.400668	8.722765
6.829315	373.657514	8.727783
6.576879	372.157107	8.732800
6.774327	374.518312	8.737818
6.689118	369.529816	8.742835
6.395788	383.880981	8.747853
6.978332	385.238271	8.752871
6.915862	404.776098	8.757888
6.878734	398.893286	8.762906
7.137481	393.831957	8.767923
6.771791	386.987622	8.772941
6.840841	371.481989	8.777959
6.744855	375.631159	8.782976
6.851039	381.550603	8.787994
7.015016	395.407251	8.793011
6.712963	386.741527	8.798029
6.806572	387.197133	8.803047
7.378849	402.883282	8.808064
6.662119	379.024328	8.813082
6.840060	369.235688	8.818099
6.876106	379.060350	8.823117
6.969309	383.754231	8.828135
7.083612	379.643337	8.833152
6.650759	375.466696	8.838170
7.010754	372.784745	8.843187
7.064533	383.966773	8.848205
6.956773	370.133005	8.853223
6.477815	380.669515	8.858240
6.670382	379.733696	8.863258
7.095160	393.274928	8.868275
7.116593	395.505924	8.873293
7.064149	395.634122	8.878311
7.186577	394.112849	8.883328
7.095761	392.202113	8.888346
6.872416	376.190027	8.893363
6.854159	393.148955	8.898381
7.258682	396.676915	8.903399
6.895351	384.044507	8.908416
6.947878	386.384239	8.913434
6.988324	382.486887	8.918451
7.155286	397.438124	8.923469
7.316144	385.850200	8.928487
6.807190	387.230186	8.933504
6.958991	384.763889	8.938522
7.185961	386.097997	8.943539
7.042207	377.672560	8.948557
6.746327	371.647262	8.953575
7.021261	387.944871	8.958592
6.805297	394.208282	8.963610
7.144009	394.915817	8.968627
6.768966	391.579019	8.973645
6.881603	395.723908	8.978663
7.036736	399.010078	8.983680
7.427543	401.069594	8.988698
7.105240	397.579366	8.993715
6.906094	401.460684	8.998733
7.100562	400.792808	9.003751
7.145478	392.877441	9.008768
7.305700	395.193989	9.013786
7.054831	394.624291	9.018803
7.295060	401.766117	9.023821
7.104415	397.207541	9.028839
7.666518	397.065883	9.033856
7.150328	401.997260	9.038874
7.176771	400.415286	9.043891
6.909413	402.426446	9.048909
7.037673	390.524892	9.053927
7.410139	396.513072	9.058944
7.023116	404.075068	9.063962
7.120232	391.736583	9.068979
7.274309	403.559310	9.073997
7.446331	400.256716	9.079015
7.499926	397.035793	9.084032
7.017386	392.254711	9.089050
7.464191	401.349158	9.094067
6.991426	400.568075	9.099085
7.168175	389.952795	9.104103
7.244584	399.547084	9.109120
7.449942	400.433303	9.114138
7.334658	394.152485	9.119155
7.183028	402.977781	9.124173
7.166083	399.114664	9.129191
7.210124	401.727124	9.134208
7.729430	400.904211	9.139226
7.689382	391.869232	9.144243
7.274613	381.920988	9.149261
7.186055	370.785559	9.154279
7.367901	380.375941	9.159296
7.104364	380.095404	9.164314
7.562612	385.997557	9.169331
7.385049	388.243953	9.174349
7.127951	377.652475	9.179367
7.164920	392.270628	9.184384
6.876147	396.648823	9.189402
7.206554	398.339108	9.194419
7.273376	402.273428	9.199437
7.308103	396.540302	9.204455
7.432244	397.372974	9.209472
7.353510	401.913920	9.214490
7.515663	391.802695	9.219507
7.538061	401.096181	9.224525
7.413977	405.136152	9.229543
7.410213	404.025967	9.234560
7.390997	402.564755	9.239578
7.484666	396.478415	9.244595
7.364536	402.887758	9.249613
7.518380	409.396187	9.254631
7.275891	407.051625	9.259648
7.383753	401.480607	9.264666
7.383724	398.466900	9.269683
7.201862	400.104905	9.274701
7.387310	399.280653	9.279719
7.543488	395.339918	9.284736
7.098524	390.549793	9.289754
7.112757	388.127141	9.294771
7.187579	404.105826	9.299789
7.358268	405.824292	9.304807
7.424112	407.862141	9.309824
7.195511	422.058028	9.314842
7.272371	418.546280	9.319859
7.852373	419.856635	9.324877
7.727468	421.258501	9.329895
7.657162	429.493559	9.334912
7.491245	433.281316	9.339930
7.549165	425.692100	9.344947
7.604076	426.046473	9.349965
7.498998	426.328084	9.354983
7.590227	419.128125	9.360000
7.554809	430.160055	9.365018
7.642618	427.230411	9.370035
7.831084	435.570093	9.375053
7.611255	417.449353	9.380071
7.658639	419.584769	9.385088
7.664219	412.417167	9.390106
7.562424	400.138243	9.395123
7.384698	405.707706	9.400141
7.391902	417.130579	9.405159
7.845117	414.045855	9.410176
7.661814	425.845719	9.415194
7.716870	424.625332	9.420211
7.667906	426.356125	9.425229
7.975143	428.362466	9.430247
8.054481	417.326933	9.435264
7.228434	410.860829	9.440282
7.483793	405.298258	9.445299
7.623315	416.902370	9.450317
7.696948	420.273896	9.455335
7.912300	421.082811	9.460352
7.977102	413.003375	9.465370
7.402456	399.760286	9.470387
7.596692	408.761766	9.475405
7.439388	416.303554	9.480423
7.779195	420.816796	9.485440
7.388062	428.035465	9.490458
7.658812	419.522973	9.495475
7.699439	425.537910	9.500493
7.795808	426.469608	9.505511
8.050496	425.890125	9.510528
7.717220	424.648531	9.515546
7.917808	422.016796	9.520563
8.050376	421.838297	9.525581
7.300654	417.717604	9.530599
7.895893	420.237394	9.535616
7.731993	428.124200	9.540634
7.946292	425.045350	9.545651
7.611197	419.521640	9.550669
7.475106	424.027396	9.555687
7.932934	425.205416	9.560704
7.805735	436.974406	9.565722
7.737541	419.577828	9.570739
7.993623	425.416996	9.575757
7.860279	425.283316	9.580775
7.872295	418.518644	9.585792
7.683027	427.046894	9.590810
7.854384	418.654116	9.595827
8.025354	429.016240	9.600845
8.159522	417.075873	9.605863
8.109811	424.367278	9.610880
7.961245	429.632380	9.615898
7.878476	427.897103	9.620915
8.299765	428.083619	9.625933
8.100559	429.942093	9.630951
8.067165	416.159754	9.635968
8.258942	424.943879	9.640986
8.346271	425.757074	9.646003
7.984182	420.057712	9.651021
7.605540	424.557291	9.656039
8.171753	409.346113	9.661056
7.947431	420.761083	9.666074
7.837866	421.882836	9.671091
7.684817	414.490780	9.676109
7.790272	418.015110	9.681127
7.648119	414.307306	9.686144
7.681077	424.100919	9.691162
7.571144	419.321409	9.696179
7.735155	412.346733	9.701197
7.399878	426.026010	9.706215
7.915349	429.877418	9.711232
8.073445	441.797370	9.716250
8.126652	442.562264	9.721267
8.218165	442.074618	9.726285
8.450843	447.409379	9.731303
8.334777	440.121970	9.736320
7.938739	434.670919	9.741338
8.157428	423.881791	9.746355
7.803280	427.774778	9.751373
7.652075	438.105335	9.756391
8.030522	448.403405	9.761408
8.037809	447.240993	9.766426
8.270695	454.942567	9.771443
8.251375	451.976055	9.776461
8.076085	459.523834	9.781479
8.343966	446.688343	9.786496
8.407093	445.810671	9.791514
8.344992	451.336785	9.796531
8.309016	447.429302	9.801549
8.113702	450.066649	9.806567
8.352700	438.479070	9.811584
8.638463	437.834758	9.816602
8.277101	426.612650	9.821619
8.046788	425.389638	9.826637
8.335142	424.700739	9.831655
8.222853	418.851786	9.836672
7.846212	422.773542	9.841690
7.984457	434.791274	9.846707
8.423101	442.227075	9.851725
8.365178	452.243225	9.856743
8.466639	446.414422	9.861760
8.224555	437.906533	9.866778
8.021320	438.831526	9.871795
8.107359	446.294174	9.876813
8.200622	448.084735	9.881831
8.591224	456.124514	9.886848
8.838620	455.359981	9.891866
8.270419	446.776952	9.896883
8.498479	429.450711	9.901901
8.041470	427.338571	9.906919
8.578978	428.008649	9.911936
8.174356	426.020844	9.916954
8.235059	429.135624	9.921971
8.481119	422.050260	9.926989
7.751815	435.106475	9.932007
8.538001	442.153310	9.937024
8.399361	447.688259	9.942042
8.293265	448.291921	9.947059
8.304910	452.973352	9.952077
8.354032	449.920378	9.957095
8.230574	453.136600	9.962112
8.596312	450.106601	9.967130
8.164816	445.992846	9.972147
8.676110	450.065819	9.977165
8.322475	451.434097	9.982183
8.120305	442.307729	9.987200
8.116522	450.226262	9.992218
8.008458	453.269659	9.997235
8.195276	457.197813	10.002253
8.256041	455.692508	10.007271
8.257524	458.646159	10.012288
8.543886	476.927052	10.017306
8.314090	477.026234	10.022323
8.740066	480.683393	10.027341
8.816309	477.124393	10.032359
8.860461	465.602040	10.037376
8.615594	453.667387	10.042394
8.468420	461.927127	10.047411
8.678837	453.982648	10.052429
8.078999	453.868409	10.057447
8.202932	451.479053	10.062464
8.582269	464.068097	10.067482
8.709072	474.992588	10.072499
8.916207	477.465897	10.077517
8.657775	468.682845	10.082535
8.497233	456.580345	10.087552
8.195639	458.552694	10.092570
8.140808	473.302061	10.097587
8.580050	473.763476	10.102605
8.770540	479.341541	10.107623
8.984668	473.179496	10.112640
9.008626	477.212066	10.117658
8.800928	478.497521	10.122675
9.129112	469.868709	10.127693
8.430179	469.489132	10.132711
8.298573	456.889793	10.137728
8.596058	463.628200	10.142746
8.470681	477.318810	10.147763
8.809166	472.705712	10.152781
8.801278	475.133816	10.157799
8.894864	466.431310	10.162816
8.863316	471.009061	10.167834
8.911766	475.081975	10.172851
8.577008	457.105433	10.177869
8.531296	473.525942	10.182887
8.618143	478.943521	10.187904
8.923347	475.168767	10.192922
8.811653	477.335426	10.197939
8.930994	475.139290	10.202957
8.515136	476.570967	10.207975
8.776780	469.360067	10.212992
8.956329	479.051847	10.218010
8.753237	482.043866	10.223027
8.954407	485.742561	10.228045
8.612680	482.346877	10.233063
8.971067	478.819410	10.238080
9.006170	481.969768	10.243098
8.713393	489.425515	10.248115
8.867421	479.725767	10.253133
8.470238	481.700472	10.258151
8.446910	478.185475	10.263168
8.523756	481.127322	10.268186
8.347387	493.399513	10.273203
8.571803	479.507304	10.278221
8.724286	487.669613	10.283239
8.963149	489.841308	10.288256
9.194787	492.976654	10.293274
8.745713	491.260894	10.298291
8.810748	482.714332	10.303309
8.787831	486.729002	10.308327
8.952349	498.436548	10.313344
9.080154	504.788146	10.318362
8.908351	500.864062	10.323379
8.926815	501.968917	10.328397
9.041094	506.899369	10.333415
9.134814	506.493427	10.338432
9.456721	492.008421	10.343450
8.999818	483.685647	10.348467
8.852707	482.184507	10.353485
9.030337	489.077402	10.358503
9.054064	486.719520	10.363520
9.074578	490.361315	10.368538
9.013321	484.349711	10.373555
9.206061	482.217812	10.378573
8.813757	477.214286	10.383591
8.765244	492.600150	10.388608
9.025107	486.383599	10.393626
9.228106	500.556106	10.398643
9.439039	501.214238	10.403661
9.412853	498.491791	10.408679
8.931730	491.296273	10.413696
9.170673	484.745329	10.418714
8.938464	484.743903	10.423731
9.408653	478.977237	10.428749
9.124295	479.441572	10.433767
8.927438	478.954927	10.438784
8.972309	477.127063	10.443802
9.031359	501.960318	10.448819
9.089442	500.038864	10.453837
8.979005	502.258977	10.458855
8.955310	503.761756	10.463872
8.921167	490.834699	10.468890
9.076669	502.379558	10.473907
9.484726	500.561060	10.478925
9.024311	500.333458	10.483943
9.066378	506.894150	10.488960
8.942235	494.568170	10.493978
8.992401	505.056563	10.498995
9.207575	494.021791	10.504013
9.158263	498.801148	10.509031
9.277580	502.007743	10.514048
9.216620	499.470624	10.519066
9.329120	508.816321	10.524083
9.540616	495.718229	10.529101
9.665176	496.572931	10.534119
9.533285	505.306822	10.539136
9.702321	496.418911	10.544154
9.471713	506.916583	10.549171
9.880256	499.417567	10.554189
9.673374	506.563218	10.559207
9.343071	507.504967	10.564224
9.504050	500.388721	10.569242
9.397932	511.311858	10.574259
9.524265	507.120155	10.579277
9.000441	510.184522	10.584295
9.357966	507.313591	10.589312
9.435073	502.025072	10.594330
9.231342	503.941067	10.599347
9.440837	505.120132	10.604365
9.507060	501.477490	10.609383
9.502364	499.234513	10.614400
9.482156	496.116654	10.619418
9.158651	512.577568	10.624435
9.721225	505.938040	10.629453
9.430277	496.248043	10.634471
9.525380	511.059156	10.639488
9.547261	494.197501	10.644506
9.681136	501.255046	10.649523
9.624819	504.845765	10.654541
9.800546	502.060124	10.659559
9.529733	499.625312	10.664576
9.699233	506.936053	10.669594
9.451417	501.326059	10.674611
9.758128	503.531306	10.679629
9.485739	499.755527	10.684647
9.334106	504.727641	10.689664
9.523221	495.931258	10.694682
9.032668	503.528452	10.699699
8.942217	500.030279	10.704717
9.237138	506.333603	10.709735
9.140235	507.390262	10.714752
9.499878	515.482255	10.719770
9.342577	530.295062	10.724787
9.938643	525.821474	10.729805
10.063179	528.437120	10.734823
9.939695	532.129886	10.739840
9.746081	500.750573	10.744858
9.349835	505.129854	10.749875
9.931074	507.617137	10.754893
9.763921	501.240267	10.759911
9.365971	497.679820	10.764928
9.944654	507.634127	10.769946
9.739345	512.062389	10.774963
9.779537	505.249088	10.779981
9.615713	496.924569	10.784999
9.503434	501.972568	10.790016
10.006913	513.762714	10.795034
9.969479	520.048689	10.800051
9.887176	510.316526	10.805069
9.737496	497.682121	10.810087
9.553558	492.765864	10.815104
9.921047	499.083062	10.820122
9.811804	516.255178	10.825139
9.789898	511.610173	10.830157
10.297505	514.503469	10.835175
9.632981	510.164278	10.840192
10.020328	490.253665	10.845210
9.579305	490.843533	10.850227
9.757351	500.974217	10.855245
10.123078	513.170953	10.860263
9.811370	505.393464	10.865280
9.851092	512.364780	10.870298
9.775318	523.614530	10.875315
9.917169	522.213279	10.880333
9.736333	518.369502	10.885351
9.875689	527.524808	10.890368
10.179056	514.797317	10.895386
10.113587	516.568574	10.900403
10.239171	521.156432	10.905421
9.574978	511.875201	10.910439
9.842271	516.062158	10.915456
10.025711	518.400330	10.920474
10.077695	511.765060	10.925491
9.865088	518.157376	10.930509
10.373874	506.918803	10.935527
10.034963	519.506813	10.940544
10.451831	514.628959	10.945562
10.177992	510.537824	10.950579
9.860404	503.174667	10.955597
10.097391	490.047339	10.960615
9.757149	496.522761	10.965632
9.981304	513.128242	10.970650
10.186903	521.458969	10.975667
9.928134	516.557585	10.980685
10.162165	514.053140	10.985703
10.098069	527.636358	10.990720
10.295916	512.293459	10.995738
10.192675	514.679704	11.000755
10.142883	523.631115	11.005773
10.424773	526.884826	11.010791
10.418403	510.220086	11.015808
9.917736	502.289168	11.020826
10.526526	496.134707	11.025843
10.265725	493.370125	11.030861
10.505764	491.694717	11.035879
10.090089	500.460446	11.040896
10.192707	488.894203	11.045914
9.980582	495.608327	11.050931
9.957702	495.479429	11.055949
10.166451	499.864903	11.060967
9.819735	513.293575	11.065984
10.242331	511.087790	11.071002
10.280116	518.507535	11.076019
10.130185	509.798981	11.081037
10.619421	514.112110	11.086055
10.430513	526.626130	11.091072
10.350942	509.073456	11.096090
10.342864	509.740657	11.101107
10.261359	521.534102	11.106125
10.399934	506.134224	11.111143
10.108203	518.131018	11.116160
9.919411	510.504681	11.121178
9.927746	508.960249	11.126195
10.088850	510.585553	11.131213
10.494220	511.146950	11.136231
10.281125	520.442681	11.141248
10.518599	514.904969	11.146266
10.220261	511.215304	11.151283
10.385867	510.902240	11.156301
10.316616	514.242523	11.161319
10.240394	524.245801	11.166336
10.424258	515.033666	11.171354
10.242699	519.701205	11.176371
10.234759	520.949053	11.181389
10.658679	509.673281	11.186407
10.414366	514.824022	11.191424
10.652927	513.322413	11.196442
10.488954	512.145804	11.201459
10.400142	520.140807	11.206477
10.627311	527.934827	11.211495
10.422125	528.475121	11.216512
10.777561	529.145328	11.221530
10.547455	518.082477	11.226547
10.337764	521.211237	11.231565
10.809668	526.363372	11.236583
10.490559	531.244970	11.241600
10.987195	525.897023	11.246618
10.564479	517.272231	11.251635
10.479059	517.841097	11.256653
10.178540	514.230668	11.261671
10.619013	526.582960	11.266688
10.568247	532.773198	11.271706
10.582348	538.107519	11.276723
10.368633	548.640439	11.281741
10.632193	535.461577	11.286759
10.788843	543.642194	11.291776
10.549864	545.188175	11.296794
10.770794	539.984407	11.301811
10.460064	543.308882	11.306829
10.524370	536.649581	11.311847
10.506340	536.882842	11.316864
10.756368	537.067791	11.321882
10.711508	535.512756	11.326899
10.898005	536.663869	11.331917
10.741182	535.530320	11.336935
10.489364	543.273162	11.341952
10.713818	544.509846	11.346970
10.489455	547.009747	11.351987
10.685546	537.322313	11.357005
10.866236	527.820334	11.362023
10.545057	542.194923	11.367040
10.978134	543.222195	11.372058
10.982762	549.305930	11.377075
10.825216	547.478216	11.382093
11.016505	538.189165	11.387111
10.572085	543.642666	11.392128
10.674306	543.147029	11.397146
10.947797	560.417010	11.402163
11.067402	564.119033	11.407181
11.474144	553.164663	11.412199
10.897348	549.767928	11.417216
10.761427	537.443764	11.422234
11.016159	536.570781	11.427251
10.998554	531.672633	11.432269
10.795258	529.501794	11.437287
10.597510	532.720202	11.442304
10.811570	554.745823	11.447322
11.274440	555.916751	11.452339
11.316860	558.135012	11.457357
11.321815	546.009677	11.462375
11.038760	536.798103	11.467392
11.267117	548.000217	11.472410
11.079983	537.268294	11.477427
10.945367	540.104427	11.482445
11.030437	534.306565	11.487463
11.281398	541.831775	11.492480
10.849220	534.360327	11.497498
10.835007	529.957110	11.502515
10.935560	540.077867	11.507533
11.193773	542.517936	11.512551
11.313021	547.362414	11.517568
11.064969	547.357159	11.522586
11.430481	539.435678	11.527603
10.890266	547.441459	11.532621
11.251207	540.098206	11.537639
10.861430	543.734868	11.542656
11.172479	558.464850	11.547674
11.628192	560.678317	11.552691
11.398978	554.894977	11.557709
11.540511	545.569537	11.562727
10.909086	546.530066	11.567744
10.685186	539.111189	11.572762
11.135731	561.292270	11.577779
11.086153	568.318624	11.582797
11.463283	568.631983	11.587815
11.345001	564.917250	11.592832
11.412728	562.978499	11.597850
11.344356	567.984923	11.602867
11.464106	563.690097	11.607885
11.397649	559.301370	11.612903
11.153377	565.222136	11.617920
11.052688	566.143691	11.622938
11.214211	565.433634	11.627955
11.031665	565.007859	11.632973
11.381835	562.725053	11.637991
11.366729	563.532213	11.643008
11.018573	568.276360	11.648026
11.438333	568.750297	11.653043
11.329578	564.393442	11.658061
11.547370	556.476164	11.663079
11.437940	560.106774	11.668096
11.508852	568.067305	11.673114
11.731734	558.533452	11.678131
11.380607	560.655584	11.683149
11.673567	559.969115	11.688167
11.667295	565.587503	11.693184
11.365779	570.390615	11.698202
11.754851	565.018484	11.703219
11.262434	568.197861	11.708237
11.810569	566.256423	11.713255
11.337721	566.264298	11.718272
11.085568	562.258116	11.723290
11.614945	557.583529	11.728307
11.300951	560.154280	11.733325
11.505166	566.118387	11.738343
11.207673	572.296803	11.743360
11.233692	566.640727	11.748378
11.763892	571.881572	11.753395
11.734008	588.757300	11.758413
11.736655	579.321059	11.763431
11.658831	573.902158	11.768448
11.628890	573.979495	11.773466
11.582059	566.731680	11.778483
11.562686	575.646792	11.783501
11.774131	582.136792	11.788519
11.776226	583.651316	11.793536
11.732662	586.997056	11.798554
11.711382	583.027280	11.803571
12.089045	594.265990	11.808589
11.887984	579.701906	11.813607
11.669438	562.858921	11.818624
11.434458	561.756551	11.823642
11.667201	569.966283	11.828659
11.776617	588.480143	11.833677
11.789938	590.665097	11.838695
11.946490	590.479683	11.843712
12.231619	582.337248	11.848730
11.871439	563.597718	11.853747
11.624486	569.742969	11.858765
11.787377	560.518316	11.863783
11.693986	572.960598	11.868800
11.640480	580.132740	11.873818
12.148514	589.460688	11.878835
12.073620	591.454337	11.883853
11.997788	588.045374	11.888871
11.988077	584.272602	11.893888
12.022072	589.638535	11.898906
12.206647	578.150912	11.903923
12.050153	567.152237	11.908941
12.021400	565.711442	11.913959
11.660078	559.532231	11.918976
11.698292	565.452919	11.923994
12.249614	576.194193	11.929011
12.001819	581.452796	11.934029
12.044152	579.991394	11.939047
12.051482	588.163868	11.944064
11.717945	588.714807	11.949082
12.389046	575.910721	11.954099
12.167563	585.062632	11.959117
12.233915	580.949738	11.964135
12.023940	570.085673	11.969152
11.880679	571.585101	11.974170
12.260150	578.566327	11.979187
12.102936	577.786288	11.984205
11.987932	586.353470	11.989223
12.352816	581.619443	11.994240
11.994406	593.595177	11.999258
12.177762	582.404389	12.004275
12.359621	588.551887	12.009293
12.322342	586.178304	12.014311
12.480652	581.836406	12.019328
11.939433	576.000958	12.024346
12.163230	581.122555	12.029363
12.111091	575.500813	12.034381
12.066344	584.852252	12.039399
12.679447	581.859214	12.044416
12.467458	591.290509	12.049434
12.332371	567.021432	12.054451
12.148974	569.151999	12.059469
12.167253	575.123151	12.064487
12.301930	572.659511	12.069504
12.056354	588.893690	12.074522
12.319728	584.226060	12.079539
12.339053	588.748533	12.084557
12.233562	591.349736	12.089575
12.504317	582.411131	12.094592
12.291666	589.100125	12.099610
12.333651	576.987902	12.104627
12.115764	581.304542	12.109645
12.235992	581.834878	12.114663
12.663083	580.496229	12.119680
12.057830	583.696443	12.124698
12.148468	588.173029	12.129715
12.029069	580.911331	12.134733
12.157468	583.725197	12.139751
12.211301	574.463976	12.144768
12.052249	600.265661	12.149786
12.568332	613.193149	12.154803
12.609620	613.606465	12.159821
12.549753	618.087704	12.164839
13.033638	606.354351	12.169856
12.754758	602.917239	12.174874
12.537455	590.864566	12.179891
12.433295	585.667539	12.184909
12.321872	608.268088	12.189927
12.596699	610.667694	12.194944
12.706048	613.045890	12.199962
12.598992	605.075345	12.204979
12.661705	602.888065	12.209997
12.308436	609.719021	12.215015
12.652914	606.834339	12.220032
12.594688	618.094022	12.225050
12.784673	614.842223	12.230067
12.781800	617.515715	12.235085
12.504446	615.523727	12.240103
12.863663	611.850936	12.245120
12.475140	615.970257	12.250138
12.622083	608.029342	12.255155
12.663565	608.698249	12.260173
12.683384	610.090078	12.265191
12.794128	612.461743	12.270208
12.761623	622.161580	12.275226
12.597096	614.812265	12.280243
12.859964	604.735633	12.285261
12.831870	615.889607	12.290279
12.944866	612.473146	12.295296
12.565515	613.021796	12.300314
12.928731	611.838320	12.305331
12.545581	607.994665	12.310349
12.642698	610.431581	12.315367
13.093097	603.156339	12.320384
12.748978	606.243059	12.325402
12.638062	614.342553	12.330419
13.031318	617.092835	12.335437
13.273250	637.327996	12.340455
12.916169	624.375700	12.345472
12.823251	623.667637	12.350490
12.996106	617.638242	12.355507
12.902692	617.495149	12.360525
12.907194	621.903187	12.365543
13.287251	621.294588	12.370560
13.143494	630.421721	12.375578
13.093889	616.304095	12.380595
13.109704	612.003450	12.385613
12.955004	612.614733	12.390631
13.190413	600.295462	12.395648
12.971219	605.940912	12.400666
13.065917	616.425549	12.405683
13.096186	610.835065	12.410701
13.181470	619.809542	12.415719
13.164813	613.229170	12.420736
13.291055	618.003144	12.425754
13.232590	613.256543	12.430771
13.179444	612.217199	12.435789
12.817723	609.402139	12.440807
13.158166	619.513757	12.445824
13.514760	627.937642	12.450842
13.101566	623.164566	12.455859
13.514910	614.856859	12.460877
13.188364	619.405129	12.465895
12.920534	615.278314	12.470912
13.212843	623.390375	12.475930
13.318166	623.332908	12.480947
13.417401	627.741884	12.485965
13.368625	632.947229	12.490983
13.713484	624.808039	12.496000
13.051829	623.273897	12.501018
13.458675	620.467804	12.506035
13.331367	612.752894	12.511053
12.938510	621.685522	12.516071
13.321446	622.597578	12.521088
13.290008	628.664900	12.526106
13.545297	628.183147	12.531123
13.799788	628.654578	12.536141
13.667546	626.952279	12.541159
13.514189	621.024488	12.546176
13.207233	628.993757	12.551194
13.171215	632.234181	12.556211
13.601299	623.844951	12.561229
13.503203	630.493922	12.566247
13.624607	627.603162	12.571264
13.369609	639.130376	12.576282
13.514741	636.952269	12.581299
13.531173	628.634160	12.586317
13.299108	627.263084	12.591335
13.679867	629.747082	12.596352
13.695854	626.172246	12.601370
13.520312	628.434134	12.606387
13.940854	623.287431	12.611405
13.747568	631.491357	12.616423
13.864278	622.788308	12.621440
13.928581	635.619339	12.626458
13.505315	625.085306	12.631475
13.708468	633.176626	12.636493
13.955370	631.058315	12.641511
13.456260	620.207963	12.646528
13.627145	628.610452	12.651546
13.666460	637.254467	12.656563
13.824748	629.103481	12.661581
13.217278	632.449219	12.666599
13.660015	621.018950	12.671616
13.451166	625.239509	12.676634
13.765654	639.306296	12.681651
13.793514	629.326432	12.686669
13.734380	634.268311	12.691687
13.815802	633.627606	12.696704
13.480678	630.495949	12.701722
13.607848	630.845316	12.706739
13.798091	630.932336	12.711757
13.712234	634.726526	12.716775
13.824964	627.560984	12.721792
13.654646	638.213390	12.726810
13.551866	651.875346	12.731827
13.830420	644.469220	12.736845
13.848665	656.502747	12.741863
13.885088	659.368905	12.746880
14.091196	664.335506	12.751898
14.057473	651.424046	12.756915
14.380185	654.826020	12.761933
13.947193	663.528269	12.766951
14.117605	651.468457	12.771968
14.465879	651.915728	12.776986
14.258954	655.283919	12.782003
14.055291	635.001839	12.787021
13.811943	632.004125	12.792039
14.098233	648.091908	12.797056
14.129262	660.246512	12.802074
14.240095	657.089158	12.807091
14.451095	651.416696	12.812109
14.009610	638.354537	12.817127
14.042661	642.183748	12.822144
14.013292	640.474797	12.827162
13.858948	642.727054	12.832179
14.445338	650.139794	12.837197
14.080243	653.640066	12.842215
14.233630	649.298923	12.847232
14.448506	659.209330	12.852250
14.461892	662.120124	12.857267
14.190543	654.109027	12.862285
14.363179	665.218958	12.867303
14.397687	647.080225	12.872320
14.027090	641.890213	12.877338
13.948475	646.828836	12.882355
14.095339	663.023685	12.887373
14.104873	667.645543	12.892391
14.259343	656.642273	12.897408
14.069813	654.977350	12.902426
14.318768	662.026396	12.907443
14.511909	655.463631	12.912461
14.463348	663.234639	12.917479
14.156463	656.289466	12.922496
14.346315	654.375752	12.927514
14.442581	662.155627	12.932531
14.373839	656.340799	12.937549
14.190531	653.365233	12.942567
14.650995	663.432825	12.947584
14.507567	659.482170	12.952602
14.391348	665.553321	12.957619
14.325293	654.792888	12.962637
14.353589	672.628419	12.967655
14.412581	683.664649	12.972672
14.948292	684.322395	12.977690
14.668558	684.517766	12.982707
15.012420	680.945197	12.987725
14.292349	677.842286	12.992743
13.993820	672.811388	12.997760
14.716010	675.377597	13.002778
14.640430	687.305924	13.007795
15.140837	675.936013	13.012813
14.672323	683.315232	13.017831
14.802152	683.058264	13.022848
15.185049	675.490609	13.027866
14.531101	665.169422	13.032883
14.530359	653.518281	13.037901
14.739862	670.751058	13.042919
14.977777	679.969896	13.047936
15.002964	663.132810	13.052954
14.501612	666.184214	13.057971
14.947451	665.252880	13.062989
14.928185	674.379465	13.068007
14.742188	655.372705	13.073024
14.997323	659.697302	13.078042
14.670436	664.494947	13.083059
15.136692	658.911878	13.088077
14.813621	664.639894	13.093095
14.812746	661.604185	13.098112
15.008758	659.575895	13.103130
14.711089	659.673089	13.108147
15.242378	661.470782	13.113165
15.023812	656.433671	13.118183
14.887496	661.592779	13.123200
14.886877	658.904171	13.128218
15.011904	670.390798	13.133235
15.016813	676.982621	13.138253
15.319017	680.514046	13.143271
15.223817	659.747880	13.148288
15.270425	643.099962	13.153306
15.023994	650.333918	13.158323
15.004095	637.177304	13.163341
15.041730	644.470892	13.168359
14.957585	637.989449	13.173376
15.210035	647.256486	13.178394
14.869433	647.155277	13.183411
15.177758	656.211591	13.188429
15.223965	665.416277	13.193447
15.061229	672.889595	13.198464
15.170907	665.834970	13.203482
15.072400	669.880461	13.208499
15.321305	673.821026	13.213517
15.307915	671.838168	13.218535
15.156717	668.226402	13.223552
14.935794	669.403488	13.228570
15.136068	666.342573	13.233587
15.263535	663.103717	13.238605
15.429063	669.376879	13.243623
15.152736	672.175276	13.248640
15.203648	672.397736	13.253658
15.124755	673.394777	13.258675
15.233831	672.898062	13.263693
15.049619	673.441386	13.268711
15.091736	673.911379	13.273728
15.231657	671.667812	13.278746
14.845074	679.605398	13.283763
15.454089	690.157820	13.288781
15.476989	696.308170	13.293799
15.357733	704.598362	13.298816
15.488798	690.310357	13.303834
15.701901	705.481844	13.308851
15.981823	698.129131	13.313869
15.912452	698.922708	13.318887
15.659262	692.054317	13.323904
15.734833	681.066549	13.328922
15.487633	676.134906	13.333939
15.617762	658.151595	13.338957
15.401989	668.937374	13.343975
15.494295	680.141953	13.348992
15.983498	680.264183	13.354010
15.793097	687.618764	13.359027
15.840365	672.649619	13.364045
15.573938	675.556919	13.369063
15.535894	669.787770	13.374080
15.621221	668.404832	13.379098
15.611316	673.582008	13.384115
15.971274	685.991208	13.389133
15.694953	686.422730	13.394151
15.864780	683.884140	13.399168
16.084752	677.184618	13.404186
15.616627	676.074588	13.409203
15.909544	670.562856	13.414221
16.124211	672.331263	13.419239
15.674778	667.021050	13.424256
16.007613	670.093235	13.429274
15.773210	666.756440	13.434291
15.917404	655.110991	13.439309
15.791131	661.593973	13.444327
15.644826	671.958612	13.449344
15.812348	675.315477	13.454362
15.978316	691.201243	13.459379
16.023776	686.271081	13.464397
16.290409	689.653446	13.469415
15.961069	680.297569	13.474432
15.890317	665.656193	13.479450
15.821031	675.484899	13.484467
16.018541	673.030336	13.489485
16.142518	688.761732	13.494503
16.289960	690.745802	13.499520
16.346896	679.347541	13.504538
15.863674	679.956649	13.509555
15.636859	676.003276	13.514573
15.744562	678.678387	13.519591
15.753277	684.938254	13.524608
16.147348	697.417857	13.529626
15.912734	691.505929	13.534643
16.040919	694.323002	13.539661
16.289977	685.756977	13.544679
16.228250	699.093799	13.549696
16.143075	684.823899	13.554714
16.209084	686.965896	13.559731
16.063034	694.679608	13.564749
16.111153	692.993226	13.569767
15.928242	693.504789	13.574784
16.579327	702.990266	13.579802
16.109300	702.256077	13.584819
16.339499	714.067083	13.589837
16.625378	718.137566	13.594855
16.163121	708.928734	13.599872
16.802061	697.319352	13.604890
16.485651	709.414815	13.609907
16.360890	685.898204	13.614925
16.650713	682.722270	13.619943
16.310437	696.093264	13.624960
16.610968	685.846582	13.629978
16.482843	688.539709	13.634995
16.517729	683.989904	13.640013
16.305157	682.590523	13.645031
16.565837	696.381761	13.650048
16.495818	696.544273	13.655066
16.517717	696.345241	13.660083
16.733448	701.767942	13.665101
16.806143	704.240256	13.670119
16.337098	690.194600	13.675136
16.801595	695.202778	13.680154
16.542293	695.846231	13.685171
16.344400	703.198837	13.690189
16.726437	709.561168	13.695207
16.692721	713.975217	13.700224
16.785479	708.434874	13.705242
16.792796	714.707594	13.710259
16.647732	718.735143	13.715277
16.915163	714.101558	13.720295
17.020188	714.429150	13.725312
16.933842	707.424157	13.730330
16.784309	702.619217	13.735347
16.866048	693.426147	13.740365
16.892280	684.563672	13.745383
16.660391	690.539345	13.750400
17.026427	692.511257	13.755418
16.697753	700.875284	13.760435
17.056797	707.837671	13.765453
17.297213	700.500614	13.770471
16.704148	693.212098	13.775488
16.967569	694.029274	13.780506
17.065749	682.141706	13.785523
16.684575	683.536407	13.790541
17.212890	682.727850	13.795559
17.200369	694.422237	13.800576
17.260194	681.956850	13.805594
16.806850	689.816537	13.810611
16.648126	682.841829	13.815629
17.181261	686.737864	13.820647
16.832938	701.429262	13.825664
17.280838	700.668018	13.830682
17.009357	708.328804	13.835699
16.974210	712.821974	13.840717
17.290825	711.727845	13.845735
16.904814	712.731982	13.850752
17.322146	698.178210	13.855770
17.756586	702.503126	13.860787
17.028847	696.302382	13.865805
17.175525	702.386004	13.870823
17.002476	705.221873	13.875840
17.117997	707.892607	13.880858
17.132414	701.891164	13.885875
16.967502	698.729670	13.890893
16.942254	701.835874	13.895911
17.429457	707.250756	13.900928
17.409871	703.315401	13.905946
17.301804	705.926492	13.910963
16.896552	708.161264	13.915981
17.024196	706.067941	13.920999
16.959167	709.309768	13.926016
17.053677	718.891926	13.931034
17.168509	741.138453	13.936051
17.361903	737.712527	13.941069
18.043738	733.878709	13.946087
17.557619	731.067340	13.951104
17.540099	729.422798	13.956122
17.577633	729.211848	13.961139
17.542524	723.353859	13.966157
17.637487	719.611995	13.971175
17.575759	726.955900	13.976192
17.645652	730.750954	13.981210
17.516762	720.628339	13.986227
17.651585	729.225876	13.991245
17.675283	717.936941	13.996263
17.531608	725.394671	14.001280
17.969761	728.074819	14.006298
17.474007	729.332840	14.011315
17.592435	734.111224	14.016333
18.043640	720.536749	14.021351
17.498471	725.782025	14.026368
17.516142	719.268821	14.031386
17.651493	728.522689	14.036403
17.461279	724.582505	14.041421
17.752355	717.404764	14.046439
17.777684	726.404467	14.051456
17.741554	728.581407	14.056474
17.705879	728.135773	14.061491
17.645531	728.224185	14.066509
17.929046	718.614475	14.071527
17.864702	727.978527	14.076544
18.079878	728.733835	14.081562
17.991300	728.760398	14.086579
18.181665	735.247445	14.091597
18.134368	728.716013	14.096615
18.190447	732.308103	14.101632
18.196965	730.757625	14.106650
17.628991	732.156350	14.111667
17.879394	728.825636	14.116685
18.222224	726.045337	14.121703
18.297735	732.092781	14.126720
18.201353	725.461743	14.131738
18.153040	717.535593	14.136755
17.926177	730.156689	14.141773
18.390432	726.237041	14.146791
18.150376	733.129201	14.151808
18.303066	715.842893	14.156826
18.197945	713.631403	14.161843
18.074044	717.721909	14.166861
17.978921	718.207094	14.171879
18.054906	731.869505	14.176896
18.262351	753.438811	14.181914
18.495819	754.863449	14.186931
18.454384	750.095209	14.191949
18.584157	737.751368	14.196967
18.156692	734.309108	14.201984
18.046423	729.333905	14.207002
18.580053	731.390018	14.212019
18.458462	730.645416	14.217037
18.325719	725.872554	14.222055
18.626517	739.717500	14.227072
18.279035	736.022864	14.232090
18.796002	743.361314	14.237107
17.722042	743.217214	14.242125
18.473695	743.620221	14.247143
18.968195	750.078557	14.252160
18.340474	753.645243	14.257178
18.965451	751.347759	14.262195
18.583147	745.361122	14.267213
18.831543	741.551031	14.272231
18.608627	727.864418	14.277248
18.368192	723.739598	14.282266
18.168152	735.595937	14.287283
18.336915	753.387449	14.292301
18.680390	744.822383	14.297319
19.069356	750.397839	14.302336
18.693479	751.252065	14.307354
18.812529	749.008603	14.312371
18.776027	753.855450	14.317389
18.624541	750.814920	14.322407
18.930776	760.423888	14.327424
18.815311	752.350452	14.332442
18.697292	751.740991	14.337459
19.064771	746.552073	14.342477
18.943330	742.724188	14.347495
19.162966	750.617317	14.352512
18.901612	749.579028	14.357530
19.106065	747.590432	14.362547
18.929650	749.874563	14.367565
19.001949	748.215946	14.372583
18.842137	749.194111	14.377600
19.357219	744.676353	14.382618
19.118225	741.949341	14.387635
19.040614	747.446418	14.392653
19.291245	734.670228	14.397671
19.172676	734.303854	14.402688
18.887349	723.407320	14.407706
19.031268	722.807313	14.412723
18.560857	734.390430	14.417741
18.886863	744.920953	14.422759
18.744033	740.197005	14.427776
18.949409	748.777185	14.432794
18.839120	753.689242	14.437811
18.900056	747.781482	14.442829
19.384823	756.150631	14.447847
18.991913	747.394822	14.452864
18.960139	747.497693	14.457882
19.289680	752.886798	14.462899
19.226448	763.879111	14.467917
18.964541	765.873677	14.472935
19.088349	768.243317	14.477952
18.893788	776.419107	14.482970
19.427356	770.254248	14.487987
19.206908	776.038805	14.493005
19.727971	773.047534	14.498023
19.469798	772.923942	14.503040
19.279087	774.897886	14.508058
19.606330	767.329445	14.513075
19.383853	772.672500	14.518093
19.617962	768.107239	14.523111
19.916404	770.399024	14.528128
19.824965	768.867046	14.533146
19.866999	769.718912	14.538163
19.598398	779.746164	14.543181
19.399411	767.015150	14.548199
19.448051	766.215472	14.553216
19.459567	766.018067	14.558234
19.353162	768.512140	14.563251
19.454872	777.613512	14.568269
19.258590	766.321142	14.573287
19.527916	769.466412	14.578304
19.705039	770.754710	14.583322
19.685114	760.431961	14.588339
19.477156	773.349931	14.593357
19.690825	768.342897	14.598375
19.248570	778.204849	14.603392
19.541418	795.964339	14.608410
19.689157	789.011002	14.613427
19.689619	799.359030	14.618445
19.794065	792.068487	14.623463
19.894222	789.502927	14.628480
19.767049	796.068151	14.633498
20.030234	790.728301	14.638515
19.647776	794.250255	14.643533
19.321811	791.407472	14.648551
19.727644	792.366444	14.653568
20.001054	814.319969	14.658586
19.942895	807.244248	14.663603
20.124059	820.148621	14.668621
20.363972	809.116091	14.673639
20.130848	808.991729	14.678656
20.185230	808.270047	14.683674
20.508946	791.057858	14.688691
20.282404	789.973086	14.693709
20.378375	791.283569	14.698727
20.242917	785.299268	14.703744
20.288288	783.547035	14.708762
20.339771	784.769812	14.713779
20.258966	785.521003	14.718797
20.391662	782.319176	14.723815
20.408922	783.692484	14.728832
20.237720	786.468115	14.733850
20.706289	784.207756	14.738867
20.177859	792.356968	14.743885
20.218069	781.870147	14.748903
20.325525	780.550006	14.753920
20.542606	788.847501	14.758938
20.411113	784.781337	14.763955
20.222582	785.177016	14.768973
20.403331	784.782679	14.773991
20.299031	778.569434	14.779008
20.273327	793.507009	14.784026
20.393705	787.110233	14.789043
20.471227	788.066995	14.794061
20.551496	793.378401	14.799079
20.605319	794.203175	14.804096
20.832147	795.423726	14.809114
20.869962	788.443429	14.814131
20.723079	789.896105	14.819149
20.430041	790.775224	14.824167
20.516056	780.953424	14.829184
20.464582	788.769125	14.834202
20.722065	797.618879	14.839219
20.736404	803.978895	14.844237
20.708582	813.302555	14.849255
21.005715	799.802653	14.854272
20.516434	794.309295	14.859290
20.934893	797.424891	14.864307
20.670227	813.495005	14.869325
21.191836	807.281514	14.874343
20.885872	796.972001	14.879360
20.796600	801.596751	14.884378
20.887931	795.059354	14.889395
21.276734	805.892504	14.894413
20.760684	794.631283	14.899431
20.931572	793.619943	14.904448
21.070003	804.214606	14.909466
21.083052	804.802767	14.914483
21.086173	796.559250	14.919501
20.824955	792.459760	14.924519
21.277204	791.369623	14.929536
20.894403	802.639251	14.934554
21.127338	800.425277	14.939571
21.107529	795.435882	14.944589
21.272134	804.423271	14.949607
21.304238	800.514511	14.954624
21.135083	810.112781	14.959642
21.133367	798.269191	14.964659
21.186714	807.968300	14.969677
21.047151	801.631182	14.974695
21.152123	805.922537	14.979712
21.198495	803.879807	14.984730
21.313645	812.007087	14.989747
21.411665	802.369590	14.994765
21.183341	801.635397	14.999783
21.342948	799.849484	15.004800
21.540437	800.446618	15.009818
21.316306	797.105033	15.014835
21.147938	795.282144	15.019853
21.390245	801.514921	15.024871
21.506840	797.760184	15.029888
21.411207	804.828562	15.034906
21.286346	788.570297	15.039923
21.185905	803.327084	15.044941
21.223255	804.343790	15.049959
21.434218	813.103009	15.054976
21.627016	825.222912	15.059994
21.459631	828.496577	15.065011
21.622146	819.398085	15.070029
21.672579	822.079034	15.075047
21.935209	825.563040	15.080064
21.798426	832.076133	15.085082
21.816039	822.681601	15.090099
21.855671	825.768193	15.095117
21.740313	826.256551	15.100135
22.018305	822.994082	15.105152
22.093247	832.752939	15.110170
22.041072	799.577346	15.115187
21.777793	798.741330	15.120205
21.520225	797.831835	15.125223
21.990426	803.230476	15.130240
21.808887	822.181491	15.135258
22.275961	821.420395	15.140275
22.142183	799.871145	15.145293
21.792820	800.566582	15.150311
21.465867	802.262070	15.155328
21.741544	818.616762	15.160346
21.843130	815.978390	15.165363
22.363051	822.350718	15.170381
22.143388	827.841674	15.175399
22.048967	824.779568	15.180416
22.090989	828.225554	15.185434
22.002331	820.274121	15.190451
22.113606	826.732567	15.195469
21.746702	832.536933	15.200487
22.134065	821.203578	15.205504
21.898968	824.165953	15.210522
22.235733	825.820570	15.215539
22.180564	821.969661	15.220557
22.065546	825.203562	15.225575
22.053927	817.751309	15.230592
22.137603	831.235863	15.235610
22.493294	843.639531	15.240627
22.561336	834.227623	15.245645
22.159954	843.044929	15.250663
22.429471	842.390526	15.255680
22.499641	842.209176	15.260698
22.229891	846.177393	15.265715
22.776815	849.288651	15.270733
22.492891	849.917031	15.275751
22.732732	840.746452	15.280768
21.985795	850.855000	15.285786
22.524132	844.162340	15.290803
22.444875	849.735448	15.295821
22.425770	849.760593	15.300839
22.610302	842.018817	15.305856
22.696916	851.340346	15.310874
22.739795	845.580553	15.315891
22.498745	839.249854	15.320909
22.049620	847.209936	15.325927
22.359816	844.841838	15.330944
22.401586	851.576276	15.335962
23.090149	870.075429	15.340979
22.932796	860.133923	15.345997
22.767512	862.630922	15.351015
22.978029	866.075763	15.356032
23.065698	860.870691	15.361050
22.929813	854.239482	15.366067
22.965558	844.977799	15.371085
23.012629	847.533045	15.376103
23.153244	846.267665	15.381120
22.933041	851.338983	15.386138
22.704044	845.523956	15.391155
23.055641	854.128615	15.396173
23.064246	861.250112	15.401191
23.176978	862.870404	15.406208
23.200498	862.213516	15.411226
23.295650	854.675090	15.416243
23.142170	843.196081	15.421261
22.939916	840.845156	15.426279
23.446437	851.757722	15.431296
23.168611	850.251785	15.436314
23.154551	857.102271	15.441331
23.360843	858.294486	15.446349
23.288902	862.724029	15.451367
23.229931	854.272459	15.456384
23.147201	868.505806	15.461402
23.289390	858.312238	15.466419
23.464800	866.673104	15.471437
23.321905	869.564235	15.476455
23.261243	856.574795	15.481472
23.006726	857.694039	15.486490
23.160368	864.631864	15.491507
23.229526	865.832942	15.496525
23.329788	856.422286	15.501543
23.269961	857.605702	15.506560
23.264614	861.160104	15.511578
23.237350	863.158943	15.516595
23.318920	875.504594	15.521613
23.955105	887.220548	15.526631
23.800825	874.772792	15.531648
24.079133	877.307592	15.536666
23.862319	874.741189	15.541683
23.604670	870.776824	15.546701
23.641686	857.046230	15.551719
23.628850	862.302816	15.556736
23.582092	861.114130	15.561754
23.649043	875.292473	15.566771
23.810326	880.436575	15.571789
23.938198	888.814367	15.576807
24.131346	883.753711	15.581824
23.873398	871.180187	15.586842
23.843980	874.918247	15.591859
24.354669	877.927888	15.596877
23.784093	873.577042	15.601895
23.936161	866.534632	15.606912
23.877560	880.038359	15.611930
24.086280	884.083099	15.616947
24.164326	887.848507	15.621965
24.181604	882.550314	15.626983
24.189531	882.249326	15.632000
23.728634	878.206349	15.637018
24.327913	881.309409	15.642035
24.526754	873.000477	15.647053
23.977696	870.785938	15.652071
23.932635	882.902121	15.657088
23.981695	884.904783	15.662106
23.985833	887.473073	15.667123
24.220916	881.613725	15.672141
23.662600	888.069805	15.677159
24.030771	886.437403	15.682176
24.367247	879.687993	15.687194
24.063963	885.204692	15.692211
24.379202	888.598415	15.697229
24.550932	906.036158	15.702247
24.774002	901.721906	15.707264
24.575022	892.175076	15.712282
24.240349	893.029165	15.717299
24.487899	876.794523	15.722317
24.527494	885.523823	15.727335
24.755136	896.688398	15.732352
24.892357	894.934387	15.737370
24.577396	890.619228	15.742387
24.562030	882.523738	15.747405
24.655982	882.524858	15.752423
24.453992	890.774449	15.757440
24.872914	901.116935	15.762458
24.734560	907.772316	15.767475
25.053688	909.170922	15.772493
24.254103	895.454609	15.777511
24.364623	897.217265	15.782528
24.932644	911.670587	15.787546
24.816476	911.420600	15.792563
25.344946	908.633278	15.797581
25.065504	905.000530	15.802599
25.390884	912.952905	15.807616
25.042654	894.886510	15.812634
24.884969	888.602694	15.817651
24.571647	889.358761	15.822669
24.986338	905.167878	15.827687
24.949575	906.682206	15.832704
25.159604	904.042610	15.837722
25.275871	910.156315	15.842739
25.436753	906.041158	15.847757
25.015531	907.426371	15.852775
25.375800	905.975090	15.857792
24.864270	893.144629	15.862810
25.015175	902.134213	15.867827
25.109741	903.047284	15.872845
25.108247	910.457567	15.877863
25.085799	902.394736	15.882880
25.111027	909.456842	15.887898
25.082610	910.550132	15.892915
25.536940	911.312160	15.897933
25.283849	921.564284	15.902951
25.416052	913.789648	15.907968
25.309153	912.342133	15.912986
25.314667	919.224291	15.918003
25.448665	902.720233	15.923021
25.599075	907.774526	15.928039
25.409340	911.638701	15.933056
25.665451	900.549926	15.938074
25.267653	912.465770	15.943091
25.694869	913.503451	15.948109
25.472590	915.226731	15.953127
25.562875	904.577355	15.958144
25.415793	905.563002	15.963162
25.409489	925.162027	15.968179
26.033636	921.144701	15.973197
25.589666	933.124599	15.978215
25.644931	927.643711	15.983232
25.950140	920.485766	15.988250
26.111518	928.012552	15.993267
26.063514	927.815003	15.998285
25.821402	931.308682	16.003303
25.734527	919.573030	16.008320
26.247117	929.708348	16.013338
25.923144	930.352474	16.018355
25.835901	918.496957	16.023373
26.250465	926.214453	16.028391
26.415008	921.846249	16.033408
26.722237	902.301189	16.038426
26.473931	904.905878	16.043443
26.227425	889.780603	16.048461
26.132141	892.506485	16.053479
25.874112	892.294505	16.058496
26.443996	886.329049	16.063514
25.884514	895.534076	16.068531
26.006273	885.738176	16.073549
26.149218	892.021268	16.078567
26.176737	894.929885	16.083584
26.201310	905.015417	16.088602
26.037415	912.864565	16.093619
26.140015	916.124348	16.098637
26.420879	916.121430	16.103655
26.506726	922.271464	16.108672
26.540739	914.761527	16.113690
26.237210	922.903962	16.118707
26.320717	912.751116	16.123725
26.455386	914.175467	16.128743
26.372857	928.860122	16.133760
26.542022	906.682597	16.138778
26.664060	920.524134	16.143795
26.610272	911.983360	16.148813
26.553885	917.202603	16.153831
26.320247	919.590397	16.158848
26.759028	909.921543	16.163866
26.443692	911.059787	16.168883
26.789855	908.493537	16.173901
26.465529	909.200835	16.178919
26.468974	920.006068	16.183936
26.657947	925.013297	16.188954
26.852202	934.015041	16.193971
27.012974	929.694765	16.198989
27.029014	931.582683	16.204007
27.141562	930.148121	16.209024
27.392153	927.107682	16.214042
26.795685	922.281187	16.219059
26.773632	915.998202	16.224077
27.181830	927.674162	16.229095
26.839846	924.515123	16.234112
26.994086	922.767911	16.239130
26.857125	930.272012	16.244147
26.574464	917.872744	16.249165
27.102349	928.684178	16.254183
26.820723	924.919222	16.259200
27.197481	929.035477	16.264218
26.740874	929.671981	16.269235
27.034034	931.200892	16.274253
26.577281	937.054084	16.279271
26.788388	942.540700	16.284288
27.176894	946.711924	16.289306
27.352129	951.576144	16.294323
27.323256	957.864087	16.299341
27.194374	951.992312	16.304359
27.245375	951.615145	16.309376
27.609585	947.641695	16.314394
27.253764	957.168303	16.319411
27.199081	948.488793	16.324429
27.727730	970.620277	16.329447
27.350636	971.307442	16.334464
27.762344	966.329287	16.339482
27.633864	976.568229	16.344499
27.934998	977.354263	16.349517
27.795317	977.022750	16.354535
27.766859	958.499081	16.359552
28.014237	947.970236	16.364570
27.384964	959.079758	16.369587
27.666606	968.657978	16.374605
28.009555	970.598825	16.379623
27.827042	983.992654	16.384640
28.246207	975.879533	16.389658
28.135178	970.699250	16.394675
27.875684	952.000341	16.399693
27.872505	959.139503	16.404711
27.869728	967.402099	16.409728
28.035194	969.752615	16.414746
27.894976	976.490367	16.419763
27.857007	969.496626	16.424781
28.282858	967.280809	16.429799
27.860748	963.364282	16.434816
28.294054	967.219216	16.439834
28.303060	971.399412	16.444851
28.045506	967.447634	16.449869
28.634229	974.560337	16.454887
27.797628	969.118185	16.459904
28.368713	962.047957	16.464922
28.120860	960.745601	16.469939
28.469591	960.757297	16.474957
28.562005	954.629937	16.479975
28.147347	969.423468	16.484992
28.537309	970.258702	16.490010
28.281390	959.180686	16.495027
28.536666	956.836957	16.500045
28.534154	964.140123	16.505063
28.197828	967.216214	16.510080
28.587341	958.031592	16.515098
28.461985	955.813774	16.520115
28.223880	954.711868	16.525133
28.434316	963.042045	16.530151
28.448426	971.788003	16.535168
28.813095	972.254805	16.540186
28.973552	973.277480	16.545203
28.650264	974.470623	16.550221
28.800306	981.121873	16.555239
28.634948	985.682850	16.560256
29.095040	979.220156	16.565274
29.173235	997.035570	16.570291
28.751413	978.194805	16.575309
29.100019	972.677411	16.580327
28.317792	973.456454	16.585344
28.742922	970.543300	16.590362
28.874566	986.586190	16.595379
28.607802	986.921545	16.600397
29.026134	981.333262	16.605415
28.946157	989.412299	16.610432
29.433724	981.313706	16.615450
29.171999	981.203291	16.620467
29.172302	990.585755	16.625485
29.375112	988.262867	16.630503
28.958697	996.075875	16.635520
29.608646	987.579443	16.640538
29.574554	990.172672	16.645555
29.025221	988.482038	16.650573
29.583157	986.734686	16.655591
29.029128	993.578306	16.660608
29.388256	983.290715	16.665626
29.258142	986.946743	16.670643
29.358245	986.211578	16.675661
29.620448	990.355264	16.680679
29.115389	991.324417	16.685696
29.381135	976.390216	16.690714
29.542863	984.721722	16.695731
29.889537	996.132805	16.700749
29.691376	1001.210180	16.705767
29.527666	1007.184742	16.710784
29.624754	998.134281	16.715802
29.697321	1003.226045	16.720819
29.364865	1009.905564	16.725837
29.739516	1003.686628	16.730855
29.803439	1006.797849	16.735872
30.047899	1002.537028	16.740890
30.040481	1003.595475	16.745907
29.974571	997.028990	16.750925
30.016736	999.764912	16.755943
29.980618	1003.197928	16.760960
30.003974	1002.872429	16.765978
29.909590	1004.866021	16.770995
30.038447	1009.570260	16.776013
30.171237	1003.840512	16.781031
29.970683	1008.350203	16.786048
30.152831	1003.676256	16.791066
30.374304	999.999721	16.796083
29.964867	1004.128717	16.801101
30.234389	995.347894	16.806119
30.007151	1002.055107	16.811136
29.988128	1005.984075	16.816154
30.020084	1000.876057	16.821171
30.096377	993.378397	16.826189
30.133650	997.762459	16.831207
29.828026	1010.298260	16.836224
30.126149	1019.037613	16.841242
30.327584	1026.747519	16.846259
30.230884	1025.449879	16.851277
30.450980	1015.963558	16.856295
30.500698	1023.078679	16.861312
30.670089	1018.226841	16.866330
30.805996	1020.392641	16.871347
30.467423	1016.393584	16.876365
30.729408	1016.693434	16.881383
30.385093	1022.465919	16.886400
30.628429	1019.811620	16.891418
30.907400	1021.039797	16.896435
30.539720	1025.581990	16.901453
30.789594	1015.848000	16.906471
30.589104	1016.374948	16.911488
30.759889	1024.578818	16.916506
30.819899	1020.100733	16.921523
30.956387	1023.462527	16.926541
30.927872	1021.109604	16.931559
30.989599	1033.966572	16.936576
31.238650	1044.291574	16.941594
31.121311	1036.742181	16.946611
31.251885	1032.445547	16.951629
30.994180	1022.150433	16.956647
31.019409	1027.713537	16.961664
31.072931	1032.571601	16.966682
30.915551	1034.448831	16.971699
30.997699	1047.570861	16.976717
31.299515	1038.437808	16.981735
31.358429	1049.856140	16.986752
31.286477	1039.099556	16.991770
31.465308	1043.417267	16.996787
31.322065	1054.059366	17.001805
31.055697	1035.825363	17.006823
31.171298	1045.846217	17.011840
31.043494	1044.023259	17.016858
31.387054	1045.395957	17.021875
31.333751	1042.945927	17.026893
31.460874	1049.193682	17.031911
31.427670	1057.931316	17.036928
31.963704	1059.535798	17.041946
31.768802	1059.803089	17.046963
31.666241	1053.526357	17.051981
31.550417	1065.211925	17.056999
31.833163	1064.246163	17.062016
32.009925	1057.288174	17.067034
32.068843	1060.346538	17.072051
31.923731	1052.672098	17.077069
31.704992	1039.808280	17.082087
31.985170	1052.971873	17.087104
32.301649	1058.192699	17.092122
32.196901	1043.657327	17.097139
32.178462	1042.135980	17.102157
32.027851	1036.466402	17.107175
32.101966	1033.327360	17.112192
32.168441	1030.694457	17.117210
31.968992	1029.349798	17.122227
32.036917	1032.166898	17.127245
31.942149	1044.133184	17.132263
32.398064	1056.316164	17.137280
32.143438	1058.271750	17.142298
32.626901	1057.968839	17.147315
32.234257	1061.688106	17.152333
32.367184	1056.542160	17.157351
32.652952	1064.308299	17.162368
32.183758	1059.689049	17.167386
32.591684	1051.378835	17.172403
32.472261	1059.341004	17.177421
32.743054	1056.590876	17.182439
32.528308	1055.434810	17.187456
32.779368	1057.251204	17.192474
32.751299	1025.958640	17.197491
32.412480	1032.721218	17.202509
32.596188	1030.284549	17.207527
32.303489	1037.301841	17.212544
32.215475	1040.042386	17.217562
32.776080	1053.957328	17.222579
32.801469	1042.286059	17.227597
32.740012	1052.505077	17.232615
32.637959	1057.845128	17.237632
32.625249	1058.352125	17.242650
32.996037	1058.587590	17.247667
32.937079	1060.809174	17.252685
32.736557	1058.827189	17.257703
32.966117	1054.827475	17.262720
32.904489	1056.607651	17.267738
33.161833	1056.135034	17.272755
33.080321	1056.788513	17.277773
32.921674	1048.134711	17.282791
33.263133	1050.505003	17.287808
33.111270	1050.762394	17.292826
33.385701	1047.803409	17.297843
33.079384	1058.502619	17.302861
33.442305	1068.693027	17.307879
33.257351	1072.613292	17.312896
33.197204	1079.568918	17.317914
33.088464	1069.805876	17.322931
33.230250	1076.704615	17.327949
33.159744	1076.756750	17.332967
33.420650	1073.228661	17.337984
33.210095	1074.823883	17.343002
33.454938	1068.306517	17.348019
33.204375	1077.977648	17.353037
33.089447	1073.738404	17.358055
33.379340	1091.883673	17.363072
33.553791	1097.685359	17.368090
33.968721	1098.709197	17.373107
33.704489	1110.667364	17.378125
33.608103	1099.103503	17.383143
34.054773	1096.597221	17.388160
33.780460	1096.173187	17.393178
33.629705	1096.569265	17.398195
33.978614	1098.386112	17.403213
33.859854	1092.389625	17.408231
34.307244	1093.155905	17.413248
33.814073	1095.802142	17.418266
34.339955	1088.177196	17.423283
34.275571	1090.544805	17.428301
34.130583	1094.824899	17.433319
33.698014	1098.095979	17.438336
33.709283	1099.249336	17.443354
34.059168	1092.264209	17.448371
34.173517	1093.871646	17.453389
34.360205	1109.031836	17.458407
34.234776	1112.516737	17.463424
34.601202	1120.412279	17.468442
34.592463	1106.982161	17.473459
34.158451	1104.146787	17.478477
34.728493	1108.620978	17.483495
34.410127	1115.579204	17.488512
34.895912	1111.927509	17.493530
34.420650	1097.380715	17.498547
34.736326	1110.854379	17.503565
34.680244	1099.830174	17.508583
34.755171	1096.567913	17.513600
34.606398	1095.568770	17.518618
34.671464	1102.820377	17.523635
34.603525	1112.298807	17.528653
34.931759	1114.787948	17.533671
34.765630	1111.888510	17.538688
34.556711	1117.273726	17.543706
34.799296	1112.492448	17.548723
34.901119	1111.321493	17.553741
34.659142	1115.165493	17.558759
34.626526	1120.157002	17.563776
34.749345	1126.238195	17.568794
34.748517	1126.535042	17.573811
34.815253	1124.236611	17.578829
35.035246	1124.173801	17.583847
35.338987	1134.755384	17.588864
35.194389	1133.970187	17.593882
35.366971	1128.739109	17.598899
34.948650	1128.776309	17.603917
35.206474	1142.120201	17.608935
35.554760	1138.979210	17.613952
35.248899	1147.690177	17.618970
35.439786	1139.893625	17.623987
35.635734	1146.383104	17.629005
35.260353	1147.467652	17.634023
35.399904	1138.284230	17.639040
35.145366	1143.269488	17.644058
35.433313	1142.615343	17.649075
35.447056	1139.463649	17.654093
35.611572	1137.089935	17.659111
35.634119	1134.744777	17.664128
35.329536	1143.038961	17.669146
35.670179	1128.635715	17.674163
35.700674	1133.516350	17.679181
35.688960	1133.745473	17.684199
35.577530	1142.419662	17.689216
35.501799	1158.703489	17.694234
35.688242	1152.513990	17.699251
35.824519	1155.661239	17.704269
35.786602	1172.967983	17.709287
35.749599	1162.111170	17.714304
35.852475	1171.894239	17.719322
36.030203	1157.014705	17.724339
35.808311	1165.649407	17.729357
36.275041	1176.776698	17.734375
36.459948	1180.512802	17.739392
36.516409	1179.282676	17.744410
36.467445	1161.516273	17.749427
36.656920	1165.324244	17.754445
36.722595	1157.013953	17.759463
36.794696	1154.051936	17.764480
36.461571	1155.192981	17.769498
36.432589	1142.640197	17.774515
36.506255	1150.250251	17.779533
36.416476	1149.450152	17.784551
36.762797	1149.601087	17.789568
36.400410	1154.884123	17.794586
36.821075	1149.374321	17.799603
36.679700	1144.066192	17.804621
36.573054	1147.668081	17.809639
37.049296	1141.916036	17.814656
36.454998	1147.251184	17.819674
36.796149	1144.253327	17.824691
36.467554	1153.677939	17.829709
36.821736	1164.229545	17.834727
36.855112	1166.988961	17.839744
36.808449	1187.869589	17.844762
36.495755	1174.913092	17.849779
37.000214	1172.464021	17.854797
36.848096	1181.791568	17.859815
37.033008	1173.958067	17.864832
37.087337	1178.705587	17.869850
37.391456	1168.410730	17.874867
37.420631	1179.786466	17.879885
37.036361	1169.949769	17.884903
37.208707	1176.969996	17.889920
36.743786	1177.702487	17.894938
37.138565	1176.861183	17.899955
37.229206	1181.997505	17.904973
37.331930	1201.507165	17.909991
37.558111	1197.422738	17.915008
37.365358	1204.730561	17.920026
37.869782	1208.564938	17.925043
37.989081	1206.488644	17.930061
37.781307	1199.300503	17.935079
37.476312	1178.008005	17.940096
38.063112	1186.241448	17.945114
38.147121	1185.373092	17.950131
38.107952	1179.061136	17.955149
37.836123	1182.647886	17.960167
37.827761	1176.387911	17.965184
37.493065	1171.674973	17.970202
37.745500	1171.395633	17.975219
37.876069	1178.895794	17.980237
38.032011	1187.679599	17.985255
38.206024	1179.806776	17.990272
38.032293	1185.252773	17.995290
37.693840	1186.555608	18.000307
37.969593	1192.313050	18.005325
38.095750	1199.428888	18.010343
37.868848	1194.954684	18.015360
38.108961	1203.690594	18.020378
38.302703	1201.965569	18.025395
38.290098	1203.548723	18.030413
38.216365	1204.914229	18.035431
38.328166	1194.280245	18.040448
37.982379	1204.253552	18.045466
38.266593	1202.725799	18.050483
38.372803	1215.692698	18.055501
38.565328	1224.111013	18.060519
38.962820	1219.135016	18.065536
38.838210	1229.114711	18.070554
39.085667	1205.179321	18.075571
39.283422	1197.571024	18.080589
38.685609	1198.573655	18.085607
38.960542	1182.208210	18.090624
38.817170	1184.316798	18.095642
38.819910	1183.259196	18.100659
38.926761	1184.025185	18.105677
38.794774	1186.062559	18.110695
38.817651	1176.846903	18.115712
38.854233	1186.684550	18.120730
38.884574	1188.021125	18.125747
38.822073	1191.972725	18.130765
39.204668	1207.159112	18.135783
39.229662	1208.269299	18.140800
39.422148	1210.129601	18.145818
38.992900	1207.378674	18.150835
39.216165	1209.773818	18.155853
39.104164	1212.947353	18.160871
39.272611	1208.499570	18.165888
39.369625	1208.812648	18.170906
39.303330	1204.938152	18.175923
39.571095	1207.190618	18.180941
39.251486	1211.053113	18.185959
39.760796	1208.978832	18.190976
39.352322	1207.502800	18.195994
39.292283	1210.813366	18.201011
39.630171	1203.858479	18.206029
39.491270	1206.660673	18.211047
39.692070	1207.310954	18.216064
39.824073	1225.433757	18.221082
39.838537	1219.555214	18.226099
40.162993	1214.417086	18.231117
39.874449	1207.320495	18.236135
39.876824	1202.709378	18.241152
39.751236	1213.143670	18.246170
39.949288	1222.286981	18.251187
39.801933	1221.227646	18.256205
39.558659	1227.868026	18.261223
40.081459	1218.943265	18.266240
40.075357	1225.076250	18.271258
40.198705	1227.537546	18.276275
39.914933	1217.107542	18.281293
39.901744	1226.280797	18.286311
40.018692	1229.551013	18.291328
40.127971	1225.462804	18.296346
40.415348	1244.164066	18.301363
40.503580	1245.983900	18.306381
40.147659	1248.169980	18.311399
40.460672	1250.071366	18.316416
40.229271	1252.449385	18.321434
40.133866	1247.481176	18.326451
40.472545	1243.659991	18.331469
40.405473	1253.113111	18.336487
40.584135	1248.793111	18.341504
40.581535	1250.706075	18.346522
40.527029	1262.006608	18.351539
41.041145	1265.100990	18.356557
41.238715	1274.780913	18.361575
41.173257	1261.094468	18.366592
41.024674	1257.349622	18.371610
40.984311	1264.772455	18.376627
41.022620	1261.736816	18.381645
40.816267	1267.973777	18.386663
40.835260	1270.808049	18.391680
40.933432	1262.599920	18.396698
41.454946	1264.604345	18.401715
41.775714	1253.356894	18.406733
41.125512	1261.698971	18.411751
41.301407	1262.700308	18.416768
41.297216	1266.295637	18.421786
41.492107	1257.996613	18.426803
41.497123	1253.457655	18.431821
41.639163	1259.217133	18.436839
41.522171	1251.601320	18.441856
41.571496	1255.440737	18.446874
41.462501	1253.027806	18.451891
41.359612	1252.535882	18.456909
41.105597	1245.967218	18.461927
41.318838	1251.712383	18.466944
41.692258	1266.628847	18.471962
41.467956	1278.571401	18.476979
42.016594	1268.083535	18.481997
41.901988	1275.180319	18.487015
42.134474	1285.905705	18.492032
41.756805	1275.266307	18.497050
42.118316	1272.678666	18.502067
42.409786	1270.995129	18.507085
42.068359	1286.153004	18.512103
41.906009	1274.826591	18.517120
42.026836	1273.980866	18.522138
42.077309	1272.309840	18.527155
42.091599	1275.772882	18.532173
41.813110	1276.611872	18.537191
42.037576	1281.534743	18.542208
42.260796	1283.598530	18.547226
42.509721	1293.563920	18.552243
42.596974	1301.840969	18.557261
42.435045	1298.237068	18.562279
42.337897	1298.037746	18.567296
42.664751	1300.956337	18.572314
42.199744	1303.547696	18.577331
42.349413	1294.479379	18.582349
42.589812	1295.161330	18.587367
42.454707	1290.366594	18.592384
42.791235	1294.066342	18.597402
42.929059	1297.554216	18.602419
42.808207	1288.663992	18.607437
42.731018	1291.585923	18.612455
42.810447	1292.813825	18.617472
43.110712	1284.463564	18.622490
42.917452	1290.632207	18.627507
43.220360	1299.907459	18.632525
43.276557	1313.983689	18.637543
43.418373	1309.060350	18.642560
43.204209	1291.729974	18.647578
43.274244	1287.764670	18.652595
43.292778	1282.311520	18.657613
42.987842	1299.426682	18.662631
43.217297	1315.145261	18.667648
43.694280	1309.440386	18.672666
43.216387	1308.249789	18.677683
43.513168	1310.081138	18.682701
43.712827	1311.520587	18.687719
43.428072	1313.323123	18.692736
43.783517	1309.382528	18.697754
43.902241	1309.105200	18.702771
44.025518	1300.151473	18.707789
44.048587	1309.180228	18.712807
43.719428	1306.861747	18.717824
43.656280	1299.900226	18.722842
43.707906	1311.771167	18.727859
43.913055	1298.591429	18.732877
43.621387	1311.008483	18.737895
43.851593	1315.375018	18.742912
44.143785	1314.824349	18.747930
43.859041	1309.964686	18.752947
43.803721	1309.402189	18.757965
44.003127	1329.335517	18.762983
44.291082	1336.400812	18.768000
44.399633	1329.491277	18.773018
44.388369	1337.812181	18.778035
44.768002	1335.818166	18.783053
44.173275	1345.603326	18.788071
44.265861	1332.510630	18.793088
44.496746	1329.097654	18.798106
44.637318	1337.158073	18.803123
44.801535	1327.260601	18.808141
44.618595	1337.625053	18.813159
44.321600	1333.284878	18.818176
44.763961	1326.171558	18.823194
44.309539	1330.064668	18.828211
44.229456	1327.852334	18.833229
44.616601	1341.239233	18.838247
44.889757	1351.781553	18.843264
44.922563	1356.112752	18.848282
45.322168	1358.713827	18.853299
45.113708	1346.671881	18.858317
45.470254	1361.521638	18.863335
45.384693	1360.200136	18.868352
45.470076	1356.589035	18.873370
44.994347	1372.686406	18.878387
45.368980	1359.925058	18.883405
45.362942	1354.583039	18.888423
45.298621	1359.172464	18.893440
45.270094	1353.843436	18.898458
45.157130	1354.653340	18.903475
45.229592	1353.543777	18.908493
44.923000	1357.476850	18.913511
45.171485	1361.262994	18.918528
45.276031	1344.378117	18.923546
45.497951	1368.319173	18.928563
46.022509	1371.541333	18.933581
45.752550	1373.079613	18.938599
45.695624	1376.370786	18.943616
45.964484	1374.523517	18.948634
45.637782	1378.418718	18.953651
45.992633	1374.819045	18.958669
45.900959	1371.163094	18.963687
46.051792	1378.615981	18.968704
46.059424	1372.482825	18.973722
45.882313	1376.540790	18.978739
45.931369	1373.209945	18.983757
46.209189	1385.563073	18.988775
46.229525	1383.786300	18.993792
46.060229	1375.638960	18.998810
46.073698	1379.673378	19.003827
46.237239	1370.703840	19.008845
46.430248	1376.669975	19.013863
45.867820	1385.869401	19.018880
46.406712	1393.185751	19.023898
46.358570	1408.029521	19.028915
46.378758	1401.837581	19.033933
46.556480	1400.692588	19.038951
46.500804	1404.479056	19.043968
46.473949	1403.514445	19.048986
46.640857	1396.589428	19.054003
46.759900	1405.098241	19.059021
47.077442	1425.372947	19.064039
46.962100	1421.944767	19.069056
47.376724	1412.503502	19.074074
47.434647	1408.997683	19.079091
47.111860	1400.347335	19.084109
46.999656	1388.072518	19.089127
47.008148	1397.993581	19.094144
47.364208	1407.825479	19.099162
47.215109	1416.452052	19.104179
47.588428	1411.037955	19.109197
47.579857	1407.548867	19.114215
47.348402	1398.454999	19.119232
47.159442	1399.655527	19.124250
47.346889	1413.749143	19.129267
47.393872	1413.066468	19.134285
47.625094	1412.200284	19.139303
47.268767	1428.875474	19.144320
47.613008	1415.238335	19.149338
47.607098	1418.846587	19.154355
47.618187	1415.865683	19.159373
47.566297	1412.295013	19.164391
47.466977	1410.439150	19.169408
48.139632	1421.319727	19.174426
48.342241	1433.571057	19.179443
48.490816	1416.208975	19.184461
49.050380	1397.611657	19.189479
48.561170	1397.615778	19.194496
48.624825	1395.494530	19.199514
48.388713	1390.144364	19.204531
48.586120	1389.674818	19.209549
48.324324	1389.655933	19.214567
48.557212	1394.665883	19.219584
48.876659	1378.589945	19.224602
48.489294	1370.401030	19.229619
48.649200	1366.778250	19.234637
48.479026	1365.091291	19.239655
48.423766	1376.183722	19.244672
48.698821	1379.725854	19.249690
48.551403	1369.359608	19.254707
48.506215	1386.642450	19.259725
48.766450	1404.196209	19.264743
48.797707	1389.143761	19.269760
48.616441	1395.509386	19.274778
49.111187	1397.988259	19.279795
48.693271	1388.803684	19.284813
48.848645	1389.962886	19.289831
48.813158	1393.197052	19.294848
49.059837	1377.479671	19.299866
48.593743	1398.915433	19.304883
48.702891	1390.601378	19.309901
48.925097	1405.200808	19.314919
48.775001	1419.031717	19.319936
49.129798	1408.271168	19.324954
49.037810	1426.438738	19.329971
49.092779	1419.206186	19.334989
49.095694	1419.723369	19.340007
49.035037	1438.611914	19.345024
49.473416	1443.337205	19.350042
49.279697	1444.844610	19.355059
49.887886	1440.776020	19.360077
49.738915	1432.227818	19.365095
49.926234	1432.236402	19.370112
50.329299	1435.004214	19.375130
50.580300	1441.482020	19.380147
50.049629	1444.957889	19.385165
50.240150	1436.422770	19.390183
50.065349	1440.777048	19.395200
50.094229	1435.404286	19.400218
49.985556	1439.404203	19.405235
49.846185	1436.708814	19.410253
50.418793	1427.362715	19.415271
49.904029	1435.642625	19.420288
50.151797	1431.453772	19.425306
50.223478	1438.120626	19.430323
50.153650	1429.525310	19.435341
50.203270	1429.350331	19.440359
50.382333	1445.872223	19.445376
50.768091	1456.062431	19.450394
50.245323	1452.297271	19.455411
50.749357	1450.555167	19.460429
50.822724	1459.203713	19.465447
50.647381	1460.357927	19.470464
51.117850	1441.809238	19.475482
50.835021	1454.512199	19.480499
50.718036	1451.582914	19.485517
50.856537	1455.228512	19.490535
50.721077	1455.843118	19.495552
50.667168	1454.166338	19.500570
50.751364	1466.209014	19.505587
50.863480	1476.587281	19.510605
51.179844	1477.604495	19.515623
51.202499	1481.255624	19.520640
51.322038	1481.069689	19.525658
51.056908	1483.427775	19.530675
51.365881	1488.949723	19.535693
51.374999	1479.846525	19.540711
51.110742	1489.879804	19.545728
51.167486	1491.518394	19.550746
51.260389	1503.919512	19.555763
51.732897	1509.775626	19.560781
51.995684	1505.959965	19.565799
51.371081	1507.361305	19.570816
51.650240	1501.633713	19.575834
51.657873	1502.352141	19.580851
51.959275	1502.462779	19.585869
51.903723	1502.143322	19.590887
52.014886	1493.658481	19.595904
52.479479	1491.149338	19.600922
52.181481	1497.785767	19.605939
51.968328	1498.971156	19.610957
52.372037	1494.249744	19.615975
52.100036	1495.999804	19.620992
52.265589	1494.364380	19.626010
52.347515	1501.528296	19.631027
52.382463	1509.927252	19.636045
52.607672	1509.535402	19.641063
52.582117	1512.392473	19.646080
52.680347	1511.786976	19.651098
52.453012	1519.277079	19.656115
52.674967	1520.470042	19.661133
52.673673	1511.848168	19.666151
52.615604	1513.564712	19.671168
52.821783	1519.970670	19.676186
53.027080	1513.793873	19.681203
52.755362	1513.050667	19.686221
52.952545	1506.613197	19.691239
53.195111	1513.051323	19.696256
53.016500	1507.887783	19.701274
53.317653	1510.854620	19.706291
52.761055	1518.206952	19.711309
53.115431	1515.153310	19.716327
53.553497	1525.234371	19.721344
53.324046	1530.746010	19.726362
53.650813	1531.307136	19.731379
53.544249	1546.289569	19.736397
53.698643	1532.713645	19.741415
53.990003	1531.926401	19.746432
54.137116	1528.416053	19.751450
54.046996	1516.506937	19.756467
53.635453	1506.759538	19.761485
53.748114	1499.562098	19.766503
53.579949	1509.697105	19.771520
53.836843	1518.099162	19.776538
53.701417	1526.565846	19.781555
54.113939	1526.280357	19.786573
54.066790	1525.643985	19.791591
53.929705	1530.790839	19.796608
54.248064	1534.250474	19.801626
54.291088	1526.928227	19.806643
53.868879	1528.020132	19.811661
53.995751	1524.522424	19.816679
54.081671	1529.694302	19.821696
54.276276	1536.124170	19.826714
54.396631	1555.937586	19.831731
54.389159	1554.319797	19.836749
54.447477	1553.881507	19.841767
54.079071	1547.153918	19.846784
54.176555	1552.538598	19.851802
54.396846	1555.776903	19.856819
54.689164	1572.562051	19.861837
54.738111	1569.240655	19.866855
54.704851	1580.225617	19.871872
54.940290	1578.222608	19.876890
54.636583	1583.635438	19.881907
54.819555	1588.706916	19.886925
55.072155	1579.578144	19.891943
55.218389	1585.965113	19.896960
55.385389	1596.214923	19.901978
55.670194	1598.051335	19.906995
54.924864	1605.123984	19.912013
55.587175	1592.632999	19.917031
55.811098	1602.529891	19.922048
55.616065	1604.725522	19.927066
55.406995	1599.235348	19.932083
55.378049	1602.020376	19.937101
55.409770	1601.030797	19.942119
55.126042	1612.736716	19.947136
55.289670	1604.249915	19.952154
55.574161	1599.218931	19.957171
55.476457	1626.028714	19.962189
55.394349	1619.934782	19.967207
55.596314	1625.779670	19.972224
55.509448	1630.057096	19.977242
55.800622	1634.145898	19.982259
55.915758	1640.417831	19.987277
56.116330	1656.330596	19.992295
56.209807	1662.236677	19.997312
56.444792	1649.582216	20.002330
56.580269	1647.721101	20.007347
56.679651	1656.163682	20.012365
56.687990	1649.689473	20.017383
56.548707	1648.306935	20.022400
56.938250	1649.451557	20.027418
56.897136	1644.452640	20.032435
56.929090	1645.994136	20.037453
56.788874	1645.621665	20.042471
56.616318	1643.546864	20.047488
56.393253	1646.128768	20.052506
56.829945	1635.418372	20.057523
56.623153	1640.358414	20.062541
57.108650	1644.031741	20.067559
57.206206	1643.921838	20.072576
57.200048	1663.871966	20.077594
57.612115	1661.942267	20.082611
57.382191	1660.466625	20.087629
57.158733	1647.773532	20.092647
57.410184	1663.646771	20.097664
57.460999	1661.085663	20.102682
57.927224	1670.973034	20.107699
57.708173	1667.024534	20.112717
57.760853	1669.512743	20.117735
57.711192	1661.479081	20.122752
57.636570	1662.466040	20.127770
57.991826	1661.523604	20.132787
57.904919	1669.307368	20.137805
58.008990	1652.314971	20.142823
58.041451	1658.410503	20.147840
57.812072	1667.194950	20.152858
58.147703	1656.680268	20.157875
58.079241	1666.547261	20.162893
57.875337	1661.854728	20.167911
58.244155	1658.202314	20.172928
58.220407	1650.376050	20.177946
58.385809	1660.831288	20.182963
58.130976	1670.841099	20.187981
58.591815	1683.579196	20.192999
58.480818	1686.437056	20.198016
58.542438	1681.753413	20.203034
58.758401	1681.880595	20.208051
58.500356	1679.472022	20.213069
58.873259	1672.363137	20.218087
58.893381	1669.945700	20.223104
58.860911	1679.349440	20.228122
58.887256	1676.050501	20.233139
58.463172	1679.588614	20.238157
58.663616	1694.478886	20.243175
58.812786	1702.279330	20.248192
58.901185	1711.275960	20.253210
58.895912	1703.973832	20.258227
58.498790	1715.258898	20.263245
59.322258	1717.317061	20.268263
59.291492	1726.310276	20.273280
59.415524	1741.133658	20.278298
59.915029	1730.293436	20.283315
60.080979	1724.665567	20.288333
59.965696	1717.462726	20.293351
59.933508	1699.749968	20.298368
59.941214	1690.258696	20.303386
60.115701	1690.682729	20.308403
59.879235	1693.721205	20.313421
59.953401	1696.711013	20.318439
60.188664	1692.716576	20.323456
60.003934	1694.853795	20.328474
60.078886	1684.922772	20.333491
60.107218	1697.349921	20.338509
60.087401	1709.926643	20.343527
60.484514	1710.937531	20.348544
60.361320	1717.414100	20.353562
60.632367	1708.023580	20.358579
60.715129	1710.093644	20.363597
60.451918	1710.302212	20.368615
60.635219	1717.084235	20.373632
60.584995	1712.957785	20.378650
60.862371	1714.034774	20.383667
60.594342	1709.102950	20.388685
60.721993	1708.338192	20.393703
60.659723	1713.097811	20.398720
60.402692	1719.791022	20.403738
61.072157	1714.444054	20.408755
61.514782	1727.863580	20.413773
61.098657	1738.384725	20.418791
61.364163	1728.726801	20.423808
61.232041	1735.927503	20.428826
61.398623	1732.249952	20.433843
61.457999	1734.841270	20.438861
61.358844	1736.709449	20.443879
61.429539	1730.367462	20.448896
61.334255	1733.487973	20.453914
61.822366	1731.956635	20.458931
61.547042	1730.690085	20.463949
61.465267	1730.775547	20.468967
61.436547	1729.681814	20.473984
61.628722	1744.412466	20.479002
61.966487	1749.346121	20.484019
61.833069	1753.570906	20.489037
62.093076	1755.127178	20.494055
61.954920	1748.271914	20.499072
61.592041	1752.087650	20.504090
61.952564	1749.834636	20.509107
62.084626	1766.802876	20.514125
62.374967	1775.789991	20.519143
62.550739	1778.359923	20.524160
62.572882	1783.251512	20.529178
62.292886	1776.551013	20.534195
62.501067	1783.256574	20.539213
62.435046	1782.885100	20.544231
62.882672	1781.382193	20.549248
62.781825	1780.637452	20.554266
62.894415	1776.163565	20.559283
62.702552	1779.927265	20.564301
62.731730	1769.892905	20.569319
62.937751	1793.982201	20.574336
62.906401	1807.996791	20.579354
63.298330	1799.041753	20.584371
63.275102	1803.236662	20.589389
63.415973	1797.877805	20.594407
63.440118	1792.341565	20.599424
63.085446	1801.581239	20.604442
63.163452	1802.673690	20.609459
63.348763	1808.009970	20.614477
63.185913	1804.712245	20.619495
63.699940	1810.460961	20.624512
63.573487	1817.670276	20.629530
63.866778	1823.759715	20.634547
63.884002	1824.356724	20.639565
63.608599	1825.384617	20.644583
63.914007	1828.224600	20.649600
63.787241	1828.781048	20.654618
63.792270	1817.361791	20.659635
63.892682	1825.681205	20.664653
63.711096	1823.449995	20.669671
64.283749	1825.446475	20.674688
64.417758	1843.661117	20.679706
64.486801	1838.269317	20.684723
64.694571	1840.019987	20.689741
64.729894	1835.255211	20.694759
64.696310	1838.962565	20.699776
64.641851	1841.376059	20.704794
64.648738	1836.521056	20.709811
64.907234	1835.540119	20.714829
64.851010	1835.059804	20.719847
65.087127	1837.721283	20.724864
64.765598	1843.840778	20.729882
64.801144	1831.349990	20.734899
64.646888	1844.055174	20.739917
64.870143	1854.450964	20.744935
65.464233	1849.983677	20.749952
65.296992	1864.887513	20.754970
65.664467	1852.600345	20.759987
65.438967	1853.393185	20.765005
65.431186	1858.172710	20.770023
65.765411	1847.285724	20.775040
65.632879	1848.019814	20.780058
65.436310	1843.632219	20.785075
65.741090	1853.731193	20.790093
65.361468	1857.398085	20.795111
65.731820	1863.554365	20.800128
65.929314	1877.937130	20.805146
65.641604	1881.943103	20.810163
66.140633	1880.012381	20.815181
65.944878	1875.706708	20.820199
66.284010	1872.996248	20.825216
65.993166	1895.689654	20.830234
66.218602	1894.019563	20.835251
66.402414	1900.432318	20.840269
66.348211	1910.041571	20.845287
66.705919	1908.940936	20.850304
66.766938	1910.818755	20.855322
66.586467	1907.422778	20.860339
66.442090	1904.223134	20.865357
66.551328	1900.459851	20.870375
66.916893	1906.342320	20.875392
66.657205	1904.842916	20.880410
66.962427	1930.122463	20.885427
67.264806	1934.105429	20.890445
67.179070	1933.115298	20.895463
66.947252	1928.982533	20.900480
67.170610	1925.043563	20.905498
67.234090	1927.353377	20.910515
67.703639	1924.000734	20.915533
67.501786	1923.751532	20.920551
67.553260	1922.234936	20.925568
67.199396	1919.778222	20.930586
67.652118	1928.449617	20.935603
67.524081	1941.819845	20.940621
67.325049	1955.845042	20.945639
67.795854	1959.189350	20.950656
67.593628	1952.618623	20.955674
67.765561	1948.955970	20.960691
68.076897	1957.943044	20.965709
67.668994	1954.134531	20.970727
68.275906	1968.368009	20.975744
68.037644	1975.620153	20.980762
68.329194	1971.500062	20.985779
68.399180	1971.504939	20.990797
68.273416	1968.337084	20.995815
68.528395	1963.692506	21.000832
68.299831	1970.393974	21.005850
68.269405	1973.993555	21.010867
68.316564	1977.678819	21.015885
68.485028	1994.019827	21.020903
68.895862	1991.392797	21.025920
68.652285	1990.856617	21.030938
68.718819	1992.626274	21.035955
69.080595	1994.747339	21.040973
69.042807	2012.641900	21.045991
69.363035	2016.912447	21.051008
69.659403	2024.147126	21.056026
69.259188	2016.733163	21.061043
69.425667	2016.700830	21.066061
69.756169	2017.554901	21.071079
69.904216	2011.986557	21.076096
69.764322	2014.804811	21.081114
69.658931	2015.859731	21.086131
70.060256	2020.477364	21.091149
69.926953	2017.181283	21.096167
70.347185	2017.178626	21.101184
70.090948	2010.906698	21.106202
70.137351	2023.388050	21.111219
70.072565	2002.337825	21.116237
70.258220	2017.278023	21.121255
69.988670	2013.435197	21.126272
70.233018	2008.855394	21.131290
69.913573	2022.568122	21.136307
70.412129	2012.396967	21.141325
70.291388	2027.019074	21.146343
70.674439	2034.350638	21.151360
70.526572	2042.406069	21.156378
70.583425	2050.047544	21.161395
70.702769	2036.571413	21.166413
70.790856	2042.778292	21.171431
70.802334	2031.954385	21.176448
71.234441	2048.036367	21.181466
71.047649	2057.489732	21.186483
71.098689	2058.984088	21.191501
71.274144	2064.558695	21.196519
71.194950	2048.983310	21.201536
71.327484	2061.163991	21.206554
71.212758	2057.331615	21.211571
71.316179	2051.931209	21.216589
71.513381	2063.909240	21.221607
71.351388	2075.375462	21.226624
71.424650	2088.531208	21.231642
71.276968	2091.934570	21.236659
71.533708	2082.703901	21.241677
71.613746	2094.088029	21.246695
72.225846	2104.394638	21.251712
72.278416	2110.326213	21.256730
72.133800	2111.447249	21.261747
72.422397	2113.030635	21.266765
72.182245	2117.628865	21.271783
72.191037	2115.389884	21.276800
72.363606	2120.529420	21.281818
72.224833	2109.965714	21.286835
72.117331	2106.031200	21.291853
72.276163	2115.730273	21.296871
72.387093	2123.581077	21.301888
72.602189	2132.753746	21.306906
72.971119	2133.002146	21.311923
72.934400	2126.058255	21.316941
72.907161	2132.062307	21.321959
73.270732	2125.683763	21.326976
73.356971	2127.235732	21.331994
73.011001	2126.317922	21.337011
73.322409	2121.042715	21.342029
73.473011	2133.283736	21.347047
73.713533	2139.362614	21.352064
73.973201	2149.339423	21.357082
74.088836	2146.282052	21.362099
73.841597	2127.144452	21.367117
73.689879	2123.409384	21.372135
73.811223	2127.780551	21.377152
73.998047	2132.251923	21.382170
73.916295	2148.985756	21.387187
73.656550	2147.366408	21.392205
73.981290	2155.477245	21.397223
74.498526	2154.222203	21.402240
74.218439	2150.024358	21.407258
74.226025	2152.980489	21.412275
74.393076	2146.459142	21.417293
74.263545	2152.958953	21.422311
74.057556	2154.544084	21.427328
74.343419	2160.530652	21.432346
74.219774	2166.606628	21.437363
74.676975	2177.489865	21.442381
74.768631	2175.493538	21.447399
74.978410	2176.031986	21.452416
74.771144	2182.095821	21.457434
74.720647	2190.284399	21.462451
74.982407	2184.944361	21.467469
74.844845	2191.871517	21.472487
75.329416	2186.136775	21.477504
75.513672	2182.042915	21.482522
75.122961	2193.074786	21.487539
75.309294	2208.810375	21.492557
75.261533	2217.096376	21.497575
75.265489	2215.748161	21.502592
75.956508	2215.579993	21.507610
75.783209	2202.534632	21.512627
76.177369	2210.372660	21.517645
75.814830	2214.740758	21.522663
76.057855	2228.027814	21.527680
76.451753	2243.027102	21.532698
76.295461	2245.866898	21.537715
76.303240	2240.083751	21.542733
76.422601	2236.217818	21.547751
76.637487	2239.823203	21.552768
76.516385	2227.748039	21.557786
76.405799	2232.546926	21.562803
76.713579	2229.828701	21.567821
76.815269	2226.394768	21.572839
76.893596	2237.779256	21.577856
76.855648	2241.215951	21.582874
76.515179	2236.134369	21.587891
76.902692	2236.282020	21.592909
77.277043	2260.825298	21.597927
77.253682	2257.360454	21.602944
77.141378	2262.595161	21.607962
77.253650	2259.629825	21.612979
77.338250	2258.897038	21.617997
77.758501	2252.891458	21.623015
77.453939	2252.661499	21.628032
77.466009	2256.500654	21.633050
77.336011	2257.935020	21.638067
77.599874	2268.097449	21.643085
77.642363	2278.130448	21.648103
77.853210	2282.749588	21.653120
77.719199	2277.215884	21.658138
77.955400	2284.024551	21.663155
78.216467	2274.938287	21.668173
77.842481	2285.276406	21.673191
78.440875	2295.193915	21.678208
78.528640	2302.265710	21.683226
78.499955	2299.597033	21.688243
78.674688	2293.996016	21.693261
78.640823	2298.688217	21.698279
78.783589	2301.124526	21.703296
78.779415	2300.831722	21.708314
78.666156	2294.698255	21.713331
78.866760	2300.745569	21.718349
79.038088	2291.887973	21.723367
79.068919	2298.681479	21.728384
79.116320	2307.672207	21.733402
79.273910	2316.011296	21.738419
79.319491	2320.504844	21.743437
79.500693	2323.594764	21.748455
79.762098	2309.127243	21.753472
80.146837	2310.335787	21.758490
80.010130	2317.474317	21.763507
80.323846	2311.245544	21.768525
80.187927	2308.884030	21.773543
80.332033	2309.928282	21.778560
80.367822	2283.891081	21.783578
80.295315	2281.273459	21.788595
80.225259	2280.605931	21.793613
80.575522	2283.738792	21.798631
80.603080	2286.584508	21.803648
80.541309	2274.916623	21.808666
80.496099	2278.739509	21.813683
80.615186	2294.271093	21.818701
80.573687	2300.952844	21.823719
80.569193	2309.866489	21.828736
80.739382	2290.868462	21.833754
80.496624	2302.372731	21.838771
80.711827	2300.855700	21.843789
81.219527	2300.504792	21.848807
80.668900	2305.391578	21.853824
80.724437	2312.888189	21.858842
80.780701	2321.928034	21.863859
81.275750	2315.614040	21.868877
81.120327	2323.774932	21.873895
81.196241	2341.273272	21.878912
81.520855	2343.021467	21.883930
81.136585	2351.641146	21.888947
81.677629	2357.420526	21.893965
81.703122	2360.970393	21.898983
81.738772	2376.117448	21.904000
82.042268	2370.417330	21.909018
81.781039	2376.454966	21.914035
81.944892	2379.768543	21.919053
82.533292	2372.650871	21.924071
81.975247	2374.376394	21.929088
82.283447	2365.266920	21.934106
82.335872	2378.132623	21.939123
82.358938	2393.603589	21.944141
82.209197	2401.321768	21.949159
82.327921	2393.166713	21.954176
82.717472	2395.684304	21.959194
82.625549	2408.553707	21.964211
82.896881	2411.503276	21.969229
83.085821	2422.040486	21.974247
82.992288	2427.206021	21.979264
83.042841	2420.043194	21.984282
83.200944	2426.722125	21.989299
83.148385	2428.109654	21.994317
83.364421	2424.932353	21.999335
83.302913	2425.800521	22.004352
83.805199	2433.293469	22.009370
83.756454	2446.970420	22.014387
83.782493	2442.146971	22.019405
83.647285	2448.423691	22.024423
83.761177	2460.427664	22.029440
84.232581	2451.945899	22.034458
84.002300	2450.265096	22.039475
84.197617	2451.692696	22.044493
83.990502	2443.942156	22.049511
84.075483	2461.085704	22.054528
84.148556	2466.064184	22.059546
84.054907	2478.315303	22.064563
84.186444	2478.802896	22.069581
84.474598	2477.239704	22.074599
84.500051	2496.074839	22.079616
85.082448	2497.981500	22.084634
84.833675	2491.733482	22.089651
85.044983	2499.729688	22.094669
85.269134	2496.604758	22.099687
84.921411	2491.009786	22.104704
85.520415	2496.540263	22.109722
85.272297	2509.756137	22.114739
85.423544	2509.805094	22.119757
85.883218	2513.867700	22.124775
85.657137	2519.202367	22.129792
85.951154	2512.127606	22.134810
85.729858	2513.248055	22.139827
85.682512	2519.413194	22.144845
85.810854	2512.373858	22.149863
85.857745	2517.460607	22.154880
86.043830	2522.149968	22.159898
85.929313	2532.229801	22.164915
86.223262	2542.210926	22.169933
86.366013	2533.767989	22.174951
86.431122	2539.041260	22.179968
86.229141	2537.296048	22.184986
86.505211	2547.485129	22.190003
86.326085	2551.000812	22.195021
86.701982	2552.144479	22.200039
86.966013	2552.358823	22.205056
87.284393	2550.961322	22.210074
86.893049	2551.432997	22.215091
86.843292	2558.349693	22.220109
87.306528	2572.644038	22.225127
87.124110	2569.892097	22.230144
87.477238	2581.240061	22.235162
87.544939	2574.049237	22.240179
87.307244	2585.047905	22.245197
87.576411	2585.700152	22.250215
87.898902	2599.640986	22.255232
87.926177	2608.196309	22.260250
87.797936	2614.238439	22.265267
87.753415	2616.252801	22.270285
88.217466	2607.933080	22.275303
87.979502	2615.826137	22.280320
88.224469	2617.978203	22.285338
88.187338	2628.771885	22.290355
88.174563	2632.829634	22.295373
88.391101	2636.583181	22.300391
88.692681	2631.523986	22.305408
88.695967	2630.447276	22.310426
88.509999	2630.937275	22.315443
88.840280	2647.291399	22.320461
89.124599	2652.981693	22.325479
88.853634	2648.703398	22.330496
89.030721	2653.189051	22.335514
89.176280	2664.405466	22.340531
89.081157	2659.679846	22.345549
89.140068	2663.003605	22.350567
89.539489	2684.788188	22.355584
89.746737	2677.143063	22.360602
89.599339	2679.735351	22.365619
89.674866	2692.446162	22.370637
89.954533	2676.176461	22.375655
89.877558	2680.345276	22.380672
89.842290	2687.196628	22.385690
90.031355	2690.430564	22.390707
89.648062	2694.278100	22.395725
90.280426	2710.433457	22.400743
90.275439	2716.049162	22.405760
90.071043	2703.705827	22.410778
90.582814	2701.258567	22.415795
90.462617	2723.336071	22.420813
90.856660	2725.471107	22.425831
90.788456	2736.512749	22.430848
91.270441	2732.602521	22.435866
90.995083	2725.537977	22.440883
91.295747	2736.240927	22.445901
91.255552	2722.748248	22.450919
91.116129	2729.306627	22.455936
91.343390	2739.891675	22.460954
91.540168	2750.191136	22.465971
91.429859	2760.844865	22.470989
91.591476	2744.659877	22.476007
91.889258	2751.490635	22.481024
91.919947	2745.293432	22.486042
92.087084	2738.844450	22.491059
92.192614	2743.382367	22.496077
92.257814	2742.482166	22.501095
92.481002	2757.363445	22.506112
92.589109	2764.028241	22.511130
92.730833	2759.574796	22.516147
92.731107	2770.517357	22.521165
93.008920	2759.247292	22.526183
93.127251	2757.461344	22.531200
92.995493	2757.251645	22.536218
93.258541	2763.519735	22.541235
93.022659	2762.739296	22.546253
93.449449	2760.002348	22.551271
93.261778	2755.322765	22.556288
93.295605	2759.556300	22.561306
93.365173	2755.489748	22.566323
93.440652	2755.664199	22.571341
93.528431	2743.874739	22.576359
93.542122	2753.256027	22.581376
93.772515	2758.011100	22.586394
93.758273	2763.290556	22.591411
93.726541	2782.557881	22.596429
93.856851	2779.517041	22.601447
93.810979	2776.948829	22.606464
93.764557	2780.191269	22.611482
94.243996	2789.313391	22.616499
93.989893	2795.630953	22.621517
94.266460	2804.418746	22.626535
93.858443	2808.008214	22.631552
94.472265	2821.439614	22.636570
94.610165	2832.988737	22.641587
94.639999	2837.926751	22.646605
95.131317	2825.865705	22.651623
95.091219	2835.309118	22.656640
94.925148	2823.407878	22.661658
95.224161	2823.288500	22.666675
95.103292	2838.779243	22.671693
95.089636	2846.741412	22.676711
95.573535	2858.728712	22.681728
95.376652	2856.834328	22.686746
95.603223	2859.601612	22.691763
95.526827	2861.750400	22.696781
95.469357	2849.608037	22.701799
95.506156	2871.673751	22.706816
95.641156	2872.747869	22.711834
96.078027	2879.844102	22.716851
95.949326	2881.013191	22.721869
96.248029	2895.011636	22.726887
96.472292	2900.039142	22.731904
96.477989	2912.773674	22.736922
96.681057	2888.227538	22.741939
96.731827	2899.913447	22.746957
96.767894	2902.025683	22.751975
96.797742	2901.367730	22.756992
96.714447	2908.747467	22.762010
97.223029	2917.211749	22.767027
97.169063	2930.829916	22.772045
97.211446	2924.592944	22.777063
97.361735	2927.646781	22.782080
97.520812	2922.975953	22.787098
97.444373	2925.639221	22.792115
97.557310	2931.861450	22.797133
97.884708	2939.233669	22.802151
97.879651	2945.417577	22.807168
98.029885	2948.367270	22.812186
98.251117	2943.399483	22.817203
98.019329	2945.127598	22.822221
98.213273	2947.401322	22.827239
98.434378	2958.751272	22.832256
98.205779	2979.801359	22.837274
98.865544	2973.552863	22.842291
98.556295	2968.709210	22.847309
98.839331	2969.072082	22.852327
98.561216	2968.140439	22.857344
98.727465	2982.326985	22.862362
99.295088	2989.020871	22.867379
99.073537	2990.406513	22.872397
99.672567	2995.116520	22.877415
99.358674	2990.990054	22.882432
99.504567	2996.841020	22.887450
99.360132	2993.278222	22.892467
99.636208	2991.284474	22.897485
99.721596	3005.701487	22.902503
99.757655	3011.897914	22.907520
99.779710	3022.758309	22.912538
100.137425	3015.768060	22.917555
100.057815	3022.200393	22.922573
100.270713	3024.909876	22.927591
100.249980	3024.749061	22.932608
100.606710	3042.863742	22.937626
100.626626	3041.509809	22.942643
100.675690	3045.898837	22.947661
100.948125	3036.841973	22.952679
100.761557	3047.075412	22.957696
100.781240	3047.258608	22.962714
100.784070	3042.807916	22.967731
101.198348	3062.558007	22.972749
101.210377	3065.412591	22.977767
101.342070	3069.466741	22.982784
101.036899	3069.309457	22.987802
101.399673	3068.056463	22.992819
101.350068	3080.446277	22.997837
101.663590	3082.814910	23.002855
101.733413	3094.523209	23.007872
101.688297	3102.004356	23.012890
101.809724	3089.966367	23.017907
101.712669	3092.948515	23.022925
102.139913	3106.046390	23.027943
102.363603	3116.733220	23.032960
102.192729	3122.779042	23.037978
101.952977	3119.007058	23.042995
102.547280	3131.261307	23.048013
102.520743	3145.920062	23.053031
102.527083	3143.018522	23.058048
102.439204	3144.354826	23.063066
102.923223	3160.637987	23.068083
102.820491	3174.115633	23.073101
103.167177	3169.276473	23.078119
103.744702	3162.617857	23.083136
103.423780	3171.679347	23.088154
103.928826	3152.126106	23.093171
104.289882	3158.388448	23.098189
104.507710	3149.961867	23.103207
104.682882	3137.959614	23.108224
104.452083	3150.545146	23.113242
104.641529	3143.407615	23.118259
104.298662	3134.456571	23.123277
104.907974	3135.768865	23.128295
104.932428	3136.263785	23.133312
104.539696	3142.865155	23.138330
104.747017	3140.888477	23.143347
104.808809	3140.386479	23.148365
104.804350	3128.668032	23.153383
105.022703	3124.331898	23.158400
105.033147	3140.424110	23.163418
105.208313	3139.143691	23.168435
105.755210	3147.273829	23.173453
105.570054	3154.246685	23.178471
105.670645	3150.471873	23.183488
105.590404	3154.735997	23.188506
105.873757	3152.769499	23.193523
106.105725	3157.404494	23.198541
106.092920	3151.239215	23.203559
106.188656	3148.393106	23.208576
105.837868	3149.066753	23.213594
105.828983	3150.911466	23.218611
106.108421	3166.630151	23.223629
106.401876	3175.519637	23.228647
106.272034	3179.172909	23.233664
106.447836	3180.692001	23.238682
106.630470	3193.178071	23.243699
106.756211	3206.146505	23.248717
106.536137	3201.989510	23.253735
106.754468	3218.693103	23.258752
106.247644	3233.070515	23.263770
106.753879	3231.286873	23.268787
107.092578	3245.219356	23.273805
107.320114	3251.010268	23.278823
107.590484	3258.094862	23.283840
107.510251	3268.551644	23.288858
107.545705	3265.039516	23.293875
107.572395	3270.486304	23.298893
107.546336	3280.761010	23.303911
108.067190	3275.878754	23.308928
108.000697	3290.341883	23.313946
108.157187	3284.008003	23.318963
108.587955	3298.440577	23.323981
108.731839	3316.036529	23.328999
108.837541	3304.183926	23.334016
108.572080	3313.473519	23.339034
108.835034	3309.048290	23.344051
108.939084	3318.920722	23.349069
108.934039	3301.517766	23.354087
108.750775	3310.485163	23.359104
109.101977	3335.617449	23.364122
109.231313	3330.259947	23.369139
109.602381	3333.654864	23.374157
109.396194	3334.488928	23.379175
109.666115	3336.479357	23.384192
109.518196	3342.439592	23.389210
109.848219	3345.673658	23.394227
110.015443	3351.290987	23.399245
109.846627	3363.273571	23.404263
110.532022	3352.324352	23.409280
110.178139	3359.386847	23.414298
110.230683	3367.316780	23.419315
110.677358	3384.859048	23.424333
111.095304	3376.969146	23.429351
111.331061	3372.538694	23.434368
111.159806	3376.331058	23.439386
111.093961	3369.362844	23.444403
111.156150	3380.709550	23.449421
111.092341	3378.235595	23.454439
111.487657	3386.260181	23.459456
111.543860	3398.870360	23.464474
111.502652	3406.884437	23.469491
111.486295	3407.180598	23.474509
111.728003	3402.629266	23.479527
111.588497	3400.542768	23.484544
111.561756	3418.822064	23.489562
111.917358	3425.097979	23.494579
112.351017	3425.197384	23.499597
112.187001	3422.650746	23.504615
112.680069	3441.233697	23.509632
112.589699	3461.893399	23.514650
112.549378	3458.923367	23.519667
113.044044	3461.888623	23.524685
113.131394	3456.329344	23.529703
113.153113	3451.159108	23.534720
112.883245	3455.756018	23.539738
112.841779	3466.857043	23.544755
113.359342	3470.509947	23.549773
113.441427	3473.767099	23.554791
113.527968	3480.536541	23.559808
113.680425	3495.558921	23.564826
113.736177	3514.639721	23.569843
113.884850	3507.884039	23.574861
114.111017	3492.868737	23.579879
114.343007	3506.474100	23.584896
113.993327	3504.474175	23.589914
114.469675	3522.236027	23.594931
114.696042	3528.667948	23.599949
114.634961	3534.018095	23.604967
115.066398	3525.292743	23.609984
115.210479	3513.374020	23.615002
114.790428	3515.453628	23.620019
115.649684	3516.243876	23.625037
115.353217	3521.981249	23.630055
115.291575	3526.523460	23.635072
115.858787	3539.707038	23.640090
115.422976	3541.388264	23.645107
115.743626	3547.540289	23.650125
115.816202	3548.396972	23.655143
115.932615	3533.550335	23.660160
115.526071	3532.389431	23.665178
116.089575	3558.773395	23.670195
116.174504	3558.059444	23.675213
116.588643	3561.447656	23.680231
116.460728	3563.374186	23.685248
116.410345	3562.747717	23.690266
116.156189	3553.691031	23.695283
116.623085	3572.372908	23.700301
116.827527	3581.106098	23.705319
117.021423	3579.229322	23.710336
117.140538	3589.825501	23.715354
117.309505	3583.401184	23.720371
117.570569	3594.132944	23.725389
117.276421	3605.507210	23.730407
117.760687	3612.804628	23.735424
117.721240	3607.227292	23.740442
117.714253	3607.632461	23.745459
118.100320	3614.904231	23.750477
117.756372	3607.853241	23.755495
118.355217	3610.691728	23.760512
118.429644	3624.558592	23.765530
118.142225	3631.254112	23.770547
118.358414	3613.926667	23.775565
118.607174	3621.851222	23.780583
118.410712	3644.342654	23.785600
118.533197	3650.342692	23.790618
118.515033	3643.325869	23.795635
118.883398	3662.016963	23.800653
119.144956	3673.048546	23.805671
119.494926	3671.980588	23.810688
119.533937	3670.140693	23.815706
119.756823	3679.477063	23.820723
119.683493	3679.974691	23.825741
119.613348	3698.949156	23.830759
120.007113	3695.333464	23.835776
119.864806	3697.549491	23.840794
119.748642	3708.529800	23.845811
119.900317	3718.057258	23.850829
120.355382	3727.862296	23.855847
120.565798	3715.229178	23.860864
121.011379	3736.079831	23.865882
121.158881	3743.243836	23.870899
121.133304	3738.630136	23.875917
120.860881	3742.959227	23.880935
121.256494	3741.221276	23.885952
121.275832	3742.954311	23.890970
121.198640	3748.818376	23.895987
121.400311	3771.885179	23.901005
121.205284	3765.584108	23.906023
121.433431	3771.043673	23.911040
121.371666	3771.328016	23.916058
121.788799	3791.242589	23.921075
121.998047	3806.439399	23.926093
122.572668	3821.768364	23.931111
122.682122	3822.347833	23.936128
122.382335	3831.276927	23.941146
122.555879	3824.274190	23.946163
122.913795	3824.249741	23.951181
122.747949	3836.696160	23.956199
122.841735	3835.409505	23.961216
123.306392	3852.820000	23.966234
123.199398	3855.737545	23.971251
123.618858	3855.583512	23.976269
123.156497	3849.494739	23.981287
123.535121	3867.392184	23.986304
123.665260	3882.939186	23.991322
123.456601	3885.045689	23.996339
123.779231	3880.194329	24.001357
123.845364	3887.945603	24.006375
123.928585	3901.577727	24.011392
124.472778	3904.942474	24.016410
123.922154	3909.147900	24.021427
124.424691	3911.853174	24.026445
124.527842	3929.326691	24.031463
124.890021	3921.852467	24.036480
124.903777	3924.684822	24.041498
125.360564	3929.568870	24.046515
125.183417	3920.272675	24.051533
125.070186	3938.231466	24.056551
125.409706	3945.662171	24.061568
125.668812	3954.118683	24.066586
125.987660	3952.768352	24.071603
126.132459	3948.639243	24.076621
125.928349	3941.641968	24.081639
126.320883	3950.153329	24.086656
126.250945	3962.925700	24.091674
126.491717	3971.422970	24.096691
126.654784	3969.532046	24.101709
126.675794	3972.634723	24.106727
126.694229	3973.818706	24.111744
126.856421	3978.389091	24.116762
126.907338	3978.873575	24.121779
127.095461	3985.993436	24.126797
126.760124	3996.389599	24.131815
126.906195	4001.928378	24.136832
127.394434	3999.399414	24.141850
127.475254	4012.053509	24.146867
127.895592	4016.586617	24.151885
128.043508	4023.791702	24.156903
127.808802	4018.645695	24.161920
128.074718	4025.699725	24.166938
127.798358	4044.953059	24.171955
127.920379	4039.255600	24.176973
128.163886	4057.710995	24.181991
128.495466	4071.818834	24.187008
128.515386	4066.393034	24.192026
128.394420	4079.896304	24.197043
128.933980	4086.339329	24.202061
128.756134	4102.212536	24.207079
128.703676	4105.730769	24.212096
129.518418	4116.199336	24.217114
129.624609	4137.450830	24.222131
129.501974	4130.942591	24.227149
129.536542	4134.993259	24.232167
129.803954	4150.840941	24.237184
129.984350	4150.500253	24.242202
130.163744	4150.446957	24.247219
130.301710	4152.707511	24.252237
130.169248	4165.638173	24.257255
130.483332	4175.759091	24.262272
131.229514	4171.696695	24.267290
130.910552	4188.958826	24.272307
131.037007	4179.109901	24.277325
131.301827	4183.651634	24.282343
131.214697	4195.246351	24.287360
131.277784	4196.884195	24.292378
131.485133	4200.478532	24.297395
131.592809	4194.556008	24.302413
131.684471	4209.522219	24.307431
132.480491	4214.829823	24.312448
132.300898	4219.624264	24.317466
132.180963	4216.281493	24.322483
132.385728	4217.976054	24.327501
132.310311	4217.710163	24.332519
132.536158	4218.798538	24.337536
132.569314	4229.957781	24.342554
132.503800	4242.019454	24.347571
132.880381	4244.974934	24.352589
132.922582	4240.186352	24.357607
133.398137	4243.776556	24.362624
133.217031	4243.883901	24.367642
133.191298	4267.425709	24.372659
133.662450	4269.968663	24.377677
133.930198	4271.233552	24.382695
133.316333	4274.621975	24.387712
134.029706	4276.647200	24.392730
133.999188	4297.977116	24.397747
134.127775	4300.362260	24.402765
134.060382	4292.617442	24.407783
134.298225	4319.631170	24.412800
134.169562	4317.675438	24.417818
134.613107	4320.809828	24.422835
134.722343	4320.982164	24.427853
134.355805	4333.987495	24.432871
134.701210	4341.676272	24.437888
135.381160	4342.863962	24.442906
135.437086	4363.539649	24.447923
135.509831	4365.144430	24.452941
135.532853	4367.653441	24.457959
135.749115	4367.354477	24.462976
136.074805	4381.059452	24.467994
135.604877	4390.902445	24.473011
136.122037	4392.914233	24.478029
135.889361	4405.109523	24.483047
136.101814	4411.572347	24.488064
136.386525	4409.337202	24.493082
136.654421	4433.234096	24.498099
136.817220	4442.179399	24.503117
137.335387	4443.897481	24.508135
137.068924	4445.687984	24.513152
137.575101	4451.893322	24.518170
137.559826	4466.942784	24.523187
137.855532	4459.002125	24.528205
138.004323	4463.615766	24.533223
137.746327	4466.036244	24.538240
137.995214	4453.191415	24.543258
138.254334	4478.579609	24.548275
138.310218	4481.560118	24.553293
138.447815	4487.996819	24.558311
138.264209	4484.525088	24.563328
138.937186	4505.252620	24.568346
138.847326	4518.659804	24.573363
139.270379	4504.102080	24.578381
139.427832	4511.959261	24.583399
139.240903	4514.273916	24.588416
139.188588	4520.071203	24.593434
139.056554	4533.418717	24.598451
139.717040	4535.862605	24.603469
139.645353	4544.626895	24.608487
140.039225	4564.441798	24.613504
140.384628	4560.372663	24.618522
140.335733	4578.609250	24.623539
140.636011	4568.174180	24.628557
140.526132	4571.916141	24.633575
140.844989	4588.163337	24.638592
140.908792	4589.232931	24.643610
140.725796	4593.747073	24.648627
140.847413	4600.012708	24.653645
141.357543	4603.474464	24.658663
141.401153	4615.153132	24.663680
141.436949	4612.682342	24.668698
141.438552	4619.254030	24.673715
141.728758	4629.609369	24.678733
142.098720	4647.338490	24.683751
141.761353	4646.747474	24.688768
142.245075	4647.757598	24.693786
142.256049	4659.583450	24.698803
141.955448	4662.796604	24.703821
142.298804	4668.825507	24.708839
142.608565	4673.707541	24.713856
142.553194	4689.899821	24.718874
142.250104	4700.016713	24.723891
142.830326	4710.478177	24.728909
142.932456	4723.587127	24.733927
142.857360	4735.524365	24.738944
143.303539	4746.073137	24.743962
143.658754	4753.883658	24.748979
144.038027	4759.209367	24.753997
143.891424	4757.130136	24.759015
143.778168	4784.332134	24.764032
144.186642	4775.603473	24.769050
144.248281	4785.502288	24.774067
144.660140	4792.713676	24.779085
144.799685	4798.692482	24.784103
145.300995	4804.816633	24.789120
145.575235	4799.770593	24.794138
145.692200	4806.349528	24.799155
145.700405	4799.719540	24.804173
146.243552	4793.943245	24.809191
145.826096	4801.196178	24.814208
146.221915	4791.008007	24.819226
146.312091	4807.032388	24.824243
146.403910	4803.918328	24.829261
146.189362	4808.970923	24.834279
145.735604	4819.199868	24.839296
146.558137	4823.231410	24.844314
146.762845	4830.210116	24.849331
146.895235	4837.648386	24.854349
147.128841	4831.178781	24.859367
146.958421	4848.020538	24.864384
147.455942	4854.880779	24.869402
146.962888	4867.858962	24.874419
146.928833	4867.981151	24.879437
147.433481	4879.010108	24.884455
147.758409	4894.922031	24.889472
147.934129	4891.324483	24.894490
148.453016	4911.372705	24.899507
147.979631	4919.928642	24.904525
148.572363	4918.257556	24.909543
148.527182	4919.208511	24.914560
148.604394	4935.455996	24.919578
148.728550	4944.151917	24.924595
148.835187	4940.110635	24.929613
149.183477	4952.152141	24.934631
148.755182	4970.786312	24.939648
149.656314	4962.255003	24.944666
149.920945	4970.868954	24.949683
149.945775	4991.831161	24.954701
150.493502	4983.775034	24.959719
150.056017	5000.216848	24.964736
150.452631	4994.239329	24.969754
150.578008	4983.357936	24.974771
150.549844	4994.833443	24.979789
150.884605	4999.017200	24.984807
150.983885	5012.051046	24.989824
150.984252	5005.886230	24.994842
151.340109	5011.370356	24.999859
151.249046	5008.316478	25.004877
151.540176	5015.783615	25.009895
151.570383	5028.992437	25.014912
151.869358	5025.482877	25.019930
151.935244	5032.035173	25.024947
152.103285	5038.448361	25.029965
152.576310	5044.835866	25.034983
152.313742	5058.289443	25.040000
152.717329	5051.872046	25.045018
153.102271	5048.254316	25.050035
153.116542	5047.702894	25.055053
153.195933	5040.957499	25.060071
153.063037	5047.654580	25.065088
153.404566	5048.166166	25.070106
153.761164	5063.318849	25.075123
153.855121	5071.789131	25.080141
153.924473	5066.696201	25.085159
153.745596	5073.018547	25.090176
153.727133	5073.018344	25.095194
154.056897	5085.065997	25.100211
153.895274	5097.370568	25.105229
154.379939	5094.412719	25.110247
154.201508	5110.125908	25.115264
154.667597	5119.469111	25.120282
154.693411	5117.899451	25.125299
154.662436	5135.426706	25.130317
154.981863	5151.866870	25.135335
154.799728	5164.916504	25.140352
155.070739	5176.424171	25.145370
155.946556	5180.873591	25.150387
155.436986	5178.421875	25.155405
155.864238	5200.315612	25.160423
155.843827	5196.928658	25.165440
155.838580	5198.990816	25.170458
156.109140	5222.758909	25.175475
156.108467	5238.384383	25.180493
156.440937	5244.383618	25.185511
156.502989	5263.320062	25.190528
156.501189	5269.415866	25.195546
156.869414	5280.608489	25.200563
157.146902	5293.093772	25.205581
157.492668	5298.642699	25.210599
157.846756	5318.186873	25.215616
158.057703	5313.785094	25.220634
157.843911	5318.370527	25.225651
158.047486	5327.855977	25.230669
158.238810	5338.274561	25.235687
158.553398	5345.981220	25.240704
158.644030	5363.464390	25.245722
158.605323	5366.030559	25.250739
158.919571	5378.058741	25.255757
159.096048	5390.323167	25.260775
159.369254	5391.240050	25.265792
159.622884	5398.315480	25.270810
159.470926	5399.422080	25.275827
159.479907	5417.593618	25.280845
160.064389	5416.211039	25.285863
160.707590	5414.374171	25.290880
160.664994	5401.362846	25.295898
161.381997	5407.472352	25.300915
161.599599	5410.336136	25.305933
161.515002	5397.555516	25.310951
161.553601	5398.054595	25.315968
161.357502	5388.242924	25.320986
161.788606	5394.532952	25.326003
161.669523	5413.658919	25.331021
161.974135	5413.904829	25.336039
162.043834	5413.051142	25.341056
162.034001	5409.930808	25.346074
162.486227	5408.474249	25.351091
162.381572	5405.813860	25.356109
162.328371	5414.443091	25.361127
162.604949	5424.049734	25.366144
163.120589	5432.675088	25.371162
163.196300	5429.654988	25.376179
162.609353	5435.583672	25.381197
162.912891	5445.265019	25.386215
163.405972	5458.515277	25.391232
163.265491	5466.230146	25.396250
163.446198	5468.970296	25.401267
163.386278	5483.323655	25.406285
163.469985	5491.735761	25.411303
163.886828	5496.560205	25.416320
163.961161	5512.152067	25.421338
164.256017	5513.917867	25.426355
164.168542	5536.887001	25.431373
164.397117	5540.307819	25.436391
164.418982	5558.635313	25.441408
164.769817	5569.714041	25.446426
164.888234	5575.983671	25.451443
165.220793	5589.764243	25.456461
165.528978	5591.231234	25.461479
165.511681	5605.180268	25.466496
165.149015	5625.967157	25.471514
165.686167	5624.576194	25.476531
165.865666	5641.521697	25.481549
166.273292	5649.580086	25.486567
165.990454	5657.472016	25.491584
166.486284	5669.954919	25.496602
166.815929	5680.140530	25.501619
167.054446	5706.963651	25.506637
167.472145	5707.093991	25.511655
167.293856	5706.001351	25.516672
167.514666	5720.244625	25.521690
167.670752	5735.596585	25.526707
167.882367	5742.520896	25.531725
168.204873	5744.279231	25.536743
168.278356	5755.360486	25.541760
168.430747	5771.890512	25.546778
168.289880	5770.514214	25.551795
168.686589	5785.632804	25.556813
169.113853	5783.993881	25.561831
169.289325	5787.574588	25.566848
169.218587	5812.845854	25.571866
169.450331	5818.939977	25.576883
169.484037	5823.657225	25.581901
170.036244	5825.821526	25.586919
169.690600	5849.185050	25.591936
169.759928	5848.864890	25.596954
170.383390	5865.359082	25.601971
170.668340	5864.247526	25.606989
170.646522	5867.953858	25.612007
170.988548	5873.320457	25.617024
170.863881	5887.747410	25.622042
171.425954	5892.899607	25.627059
171.568596	5900.649222	25.632077
171.323921	5892.622137	25.637095
171.553633	5900.856877	25.642112
171.774166	5924.235971	25.647130
172.042671	5918.521293	25.652147
171.878571	5941.108344	25.657165
172.364716	5942.351767	25.662183
172.600295	5957.495742	25.667200
172.550035	5972.447753	25.672218
172.823340	5978.989992	25.677236
172.776786	5985.247726	25.682253
173.145896	5987.232385	25.687271
173.549673	6001.090499	25.692288
173.610489	6000.014048	25.697306
174.173294	6005.216671	25.702324
174.089181	6017.168785	25.707341
174.123266	6021.772382	25.712359
174.112052	6023.343112	25.717376
174.286476	6037.811717	25.722394
174.593623	6044.168741	25.727412
174.505119	6050.332053	25.732429
174.903122	6049.818345	25.737447
175.392853	6064.903653	25.742464
175.143653	6073.200871	25.747482
175.385125	6083.851940	25.752500
175.031388	6086.956863	25.757517
176.082501	6085.324355	25.762535
176.064516	6101.291053	25.767552
175.834522	6105.459368	25.772570
175.681659	6117.135051	25.777588
176.219640	6124.431387	25.782605
176.466015	6138.348989	25.787623
176.710727	6145.735472	25.792640
176.680349	6152.849375	25.797658
177.528242	6152.277811	25.802676
177.513563	6164.847344	25.807693
178.047615	6166.083278	25.812711
178.240918	6169.585504	25.817728
178.087466	6172.794806	25.822746
178.237984	6170.375283	25.827764
178.228569	6184.629732	25.832781
178.353422	6194.115338	25.837799
178.875314	6192.035388	25.842816
178.636443	6213.520140	25.847834
178.855657	6217.270859	25.852852
178.869717	6237.285985	25.857869
179.066048	6243.092215	25.862887
179.194899	6251.866944	25.867904
179.094652	6274.226582	25.872922
179.594516	6271.209346	25.877940
179.958864	6297.315966	25.882957
180.071419	6301.828419	25.887975
180.396790	6314.824619	25.892992
180.153310	6335.025410	25.898010
180.834732	6337.018004	25.903028
180.472364	6353.509239	25.908045
180.540608	6368.222030	25.913063
180.964854	6374.387200	25.918080
181.729062	6390.588332	25.923098
182.234813	6386.525246	25.928116
182.461120	6399.025618	25.933133
182.329656	6413.962299	25.938151
182.685617	6412.283983	25.943168
182.780418	6412.026117	25.948186
183.571291	6403.839734	25.953204
183.326991	6407.887242	25.958221
183.244489	6410.608789	25.963239
183.781241	6411.620183	25.968256
183.577535	6419.332729	25.973274
184.020003	6428.279390	25.978292
183.994731	6426.465074	25.983309
184.014780	6426.790305	25.988327
184.014696	6429.025418	25.993344
184.207749	6443.538777	25.998362
184.451870	6442.057920	26.003380
184.608285	6464.279718	26.008397
184.790243	6470.773308	26.013415
185.216097	6478.453545	26.018432
185.249932	6485.061893	26.023450
185.406326	6493.614601	26.028468
185.475518	6509.864741	26.033485
185.560856	6519.748155	26.038503
185.890418	6529.309198	26.043520
185.817858	6532.717399	26.048538
186.186575	6547.537947	26.053556
186.406177	6556.099723	26.058573
186.332677	6558.172726	26.063591
186.556380	6570.531565	26.068608
186.787480	6589.098800	26.073626
186.974540	6597.820380	26.078644
187.103529	6618.543995	26.083661
187.080931	6624.021604	26.088679
187.258074	6636.722410	26.093696
187.576508	6647.544849	26.098714
187.472228	6665.107149	26.103732
187.910592	6686.565279	26.108749
188.101250	6700.091113	26.113767
188.670975	6708.683346	26.118784
188.731747	6711.773945	26.123802
188.570327	6724.259516	26.128820
188.879401	6739.237937	26.133837
188.797049	6749.583395	26.138855
189.594031	6756.656311	26.143872
189.580606	6774.217109	26.148890
190.022639	6793.275550	26.153908
190.023370	6793.237614	26.158925
190.314908	6806.864528	26.163943
190.776100	6809.892415	26.168960
190.762416	6812.328589	26.173978
190.911274	6827.177493	26.178996
191.249290	6837.633933	26.184013
191.307139	6839.717960	26.189031
191.670472	6850.113616	26.194048
191.568712	6860.487433	26.199066
192.028460	6859.553634	26.204084
192.346576	6871.244405	26.209101
192.557867	6886.156185	26.214119
192.949106	6884.889015	26.219136
192.620775	6892.832795	26.224154
192.940762	6902.925895	26.229172
193.392002	6911.729357	26.234189
193.061343	6919.398862	26.239207
193.618317	6924.378523	26.244224
193.607924	6929.873253	26.249242
193.584964	6942.289926	26.254260
193.838562	6959.591242	26.259277
193.859218	6973.276501	26.264295
194.155293	6974.410871	26.269312
194.386220	6995.485144	26.274330
194.642103	7017.433160	26.279348
195.144262	7019.766453	26.284365
195.351479	7026.332048	26.289383
195.526741	7035.737583	26.294400
195.586695	7038.755756	26.299418
195.737965	7056.287866	26.304436
196.013371	7064.481246	26.309453
196.033386	7076.875492	26.314471
196.475160	7085.124899	26.319488
196.345215	7099.149539	26.324506
196.633940	7107.707058	26.329524
196.950519	7124.199953	26.334541
196.789650	7137.500211	26.339559
197.118731	7147.418388	26.344576
197.256430	7159.952102	26.349594
197.512911	7169.783799	26.354612
197.609862	7185.597683	26.359629
198.070689	7207.179182	26.364647
199.043092	7205.069587	26.369664
198.903708	7207.108787	26.374682
199.242053	7201.294378	26.379700
199.537756	7206.832790	26.384717
199.452292	7225.109307	26.389735
199.701072	7219.918219	26.394752
199.771708	7220.005081	26.399770
200.040883	7215.385368	26.404788
200.435901	7231.446195	26.409805
200.090212	7251.367247	26.414823
200.634195	7246.152004	26.419840
200.520660	7250.709581	26.424858
200.567476	7252.792226	26.429876
200.952321	7266.701621	26.434893
200.955002	7270.906357	26.439911
201.237325	7279.423919	26.444928
201.313332	7295.342202	26.449946
201.348923	7302.945018	26.454964
201.950705	7317.574985	26.459981
201.645999	7330.954741	26.464999
201.699801	7336.423750	26.470016
202.220557	7347.672671	26.475034
202.495651	7374.293609	26.480052
202.673019	7390.215037	26.485069
202.837615	7396.964234	26.490087
202.920370	7409.459371	26.495104
203.166228	7432.839575	26.500122
203.217469	7436.357986	26.505140
203.917889	7451.736603	26.510157
203.785846	7466.090180	26.515175
204.539041	7473.425954	26.520192
204.454148	7490.986003	26.525210
204.594062	7497.170841	26.530228
204.894067	7507.194792	26.535245
205.006428	7518.555152	26.540263
205.428557	7527.347686	26.545280
205.650585	7546.318251	26.550298
205.811874	7553.472123	26.555316
206.394200	7558.823674	26.560333
206.049363	7583.019565	26.565351
206.293979	7579.745348	26.570368
206.817732	7596.597684	26.575386
206.813083	7605.820173	26.580404
207.028436	7616.927681	26.585421
207.125157	7626.566814	26.590439
207.447789	7631.204537	26.595456
207.422286	7652.348148	26.600474
207.417583	7665.965281	26.605492
207.852824	7683.475601	26.610509
207.800815	7705.125395	26.615527
208.430725	7713.901253	26.620544
208.469797	7723.975671	26.625562
208.667920	7737.829433	26.630580
208.962313	7748.804670	26.635597
208.986367	7763.197164	26.640615
209.260792	7770.175544	26.645632
209.609286	7793.173907	26.650650
209.905451	7803.179679	26.655668
209.873267	7811.753071	26.660685
209.975391	7831.806646	26.665703
210.132520	7840.644002	26.670720
210.426440	7869.497915	26.675738
210.756040	7889.143381	26.680756
210.932075	7897.245358	26.685773
211.243304	7918.058697	26.690791
211.299887	7923.757913	26.695808
211.413818	7945.056811	26.700826
211.577424	7965.160884	26.705844
212.020598	7976.040335	26.710861
212.033115	7992.505872	26.715879
212.517764	8001.661378	26.720896
212.939455	8015.006759	26.725914
213.350713	8025.644985	26.730932
213.218032	8039.762322	26.735949
213.339093	8048.520186	26.740967
213.717929	8064.426420	26.745984
213.794801	8066.409735	26.751002
213.953927	8075.761500	26.756020
214.588913	8092.214854	26.761037
214.531707	8098.323432	26.766055
214.461403	8111.127161	26.771072
215.060244	8119.721812	26.776090
215.353166	8122.728924	26.781108
215.587053	8134.935677	26.786125
215.944736	8144.938311	26.791143
215.771306	8147.109231	26.796160
216.598796	8159.185123	26.801178
216.445759	8169.646634	26.806196
216.601479	8177.669832	26.811213
216.851533	8178.549447	26.816231
216.883811	8190.427907	26.821248
217.083836	8198.352616	26.826266
217.139494	8214.476935	26.831284
217.847633	8221.378071	26.836301
217.591982	8238.397293	26.841319
217.960327	8251.514417	26.846336
218.468221	8266.930193	26.851354
218.409382	8283.804968	26.856372
218.597521	8282.929439	26.861389
218.488436	8295.066897	26.866407
218.320505	8311.740944	26.871424
219.155098	8332.134945	26.876442
219.212476	8350.178667	26.881460
219.472247	8357.134307	26.886477
219.563508	8386.923725	26.891495
219.873951	8401.622296	26.896512
220.180275	8417.271833	26.901530
220.339041	8440.641699	26.906548
220.656432	8441.232946	26.911565
220.855987	8453.107469	26.916583
221.109227	8478.915713	26.921600
221.445940	8489.944748	26.926618
221.382267	8509.841913	26.931636
222.249440	8513.324266	26.936653
222.223365	8528.536606	26.941671
222.177206	8547.695442	26.946688
223.017155	8559.769646	26.951706
222.898723	8591.669678	26.956724
223.213263	8579.111627	26.961741
223.181292	8606.328639	26.966759
223.657946	8609.240747	26.971776
223.803739	8627.485577	26.976794
223.769168	8626.682808	26.981812
224.233922	8641.824664	26.986829
224.135748	8656.139125	26.991847
224.539423	8666.346371	26.996864
225.017836	8675.392688	27.001882
224.966902	8691.455189	27.006900
225.441544	8712.117534	27.011917
225.598184	8716.172191	27.016935
225.721286	8731.793867	27.021952
225.867459	8739.638842	27.026970
225.777087	8766.637917	27.031988
226.255794	8781.316745	27.037005
226.462835	8805.235181	27.042023
226.690872	8811.166704	27.047040
227.009770	8823.982571	27.052058
227.096609	8840.762413	27.057076
227.315742	8852.501521	27.062093
227.597552	8870.052788	27.067111
227.554267	8887.535024	27.072128
228.174692	8903.625141	27.077146
228.586174	8912.382120	27.082164
228.905870	8924.465447	27.087181
228.651554	8940.929424	27.092199
229.092751	8946.840227	27.097216
229.330044	8964.486961	27.102234
229.162228	8986.910978	27.107252
229.487410	8992.953632	27.112269
229.837766	9006.945517	27.117287
229.976399	9028.162858	27.122304
230.446115	9030.195240	27.127322
230.779330	9048.467955	27.132340
230.966487	9058.153655	27.137357
231.201145	9074.645340	27.142375
231.308329	9080.958970	27.147392
231.657082	9089.804791	27.152410
231.753953	9106.245472	27.157428
232.211605	9109.908916	27.162445
232.393217	9132.189965	27.167463
232.570791	9141.968771	27.172480
232.869152	9150.440483	27.177498
233.246821	9160.402650	27.182516
233.248088	9169.580787	27.187533
233.486101	9194.584142	27.192551
233.521636	9201.669947	27.197568
234.141143	9207.846531	27.202586
234.030557	9234.543192	27.207604
234.162344	9256.598554	27.212621
234.616062	9265.140700	27.217639
234.627603	9275.848580	27.222656
235.107458	9296.848593	27.227674
234.786385	9324.427677	27.232692
235.287772	9337.729955	27.237709
235.800199	9358.317639	27.242727
236.113177	9372.072541	27.247744
236.609718	9383.500154	27.252762
236.473291	9412.367052	27.257780
236.681406	9412.940721	27.262797
237.176325	9422.685748	27.267815
237.132982	9429.562983	27.272832
237.283257	9452.370286	27.277850
237.558882	9471.176558	27.282868
238.181953	9484.611433	27.287885
238.778160	9497.122263	27.292903
238.641595	9517.259253	27.297920
239.264566	9512.040485	27.302938
239.337978	9513.462487	27.307956
239.384680	9525.222718	27.312973
240.132892	9522.443913	27.317991
240.043449	9537.714364	27.323008
240.539956	9542.157992	27.328026
240.594906	9546.209817	27.333044
240.926723	9555.525805	27.338061
241.135007	9569.704554	27.343079
241.341753	9576.457416	27.348096
241.605858	9577.805348	27.353114
241.548914	9600.522157	27.358132
242.036795	9597.790438	27.363149
242.163585	9606.273449	27.368167
242.365549	9629.022353	27.373184
242.459360	9633.159674	27.378202
242.728399	9650.577912	27.383220
242.991429	9660.725648	27.388237
243.162819	9673.034768	27.393255
243.300390	9694.464580	27.398272
243.910613	9708.769913	27.403290
243.611496	9724.774305	27.408308
243.886556	9737.013552	27.413325
244.230985	9760.769612	27.418343
244.053166	9779.170461	27.423360
244.215497	9781.948868	27.428378
244.576094	9814.309553	27.433396
244.583754	9819.919135	27.438413
244.945783	9839.773135	27.443431
245.269329	9849.785197	27.448448
245.865696	9868.020651	27.453466
245.899421	9889.662715	27.458484
246.192517	9897.560942	27.463501
246.677944	9918.835481	27.468519
247.124298	9932.093132	27.473536
247.162510	9948.619523	27.478554
247.495526	9966.492177	27.483572
247.774007	9976.615563	27.488589
248.105315	9986.973802	27.493607
247.818427	10003.800608	27.498624
248.401059	10017.586366	27.503642
248.434244	10036.235426	27.508660
248.801097	10049.458252	27.513677
249.275742	10064.445006	27.518695
249.396164	10086.102133	27.523712
249.667114	10094.575413	27.528730
249.458725	10114.945320	27.533748
250.122913	10132.178966	27.538765
250.464809	10145.162645	27.543783
250.598856	10162.293076	27.548800
250.834586	10169.401566	27.553818
250.941129	10191.383051	27.558836
251.102463	10210.100619	27.563853
251.677724	10224.714945	27.568871
251.463145	10244.385001	27.573888
252.169678	10251.751305	27.578906
252.531192	10278.880700	27.583924
252.804397	10291.426879	27.588941
252.900397	10307.486698	27.593959
253.125963	10324.855542	27.598976
253.366997	10336.153263	27.603994
253.592004	10352.710742	27.609012
253.722534	10359.731587	27.614029
254.351690	10383.608026	27.619047
254.515599	10402.969515	27.624064
254.981376	10420.502899	27.629082
255.298504	10421.735232	27.634100
255.378475	10428.486161	27.639117
255.732679	10442.810063	27.644135
255.645533	10463.546573	27.649152
256.045996	10470.237839	27.654170
256.227864	10492.482582	27.659188
256.538728	10503.460029	27.664205
256.538267	10527.242674	27.669223
257.009376	10545.697339	27.674240
257.351953	10556.057287	27.679258
257.380675	10574.849671	27.684276
257.665441	10598.155142	27.689293
258.099776	10611.279385	27.694311
257.737023	10634.256910	27.699328
258.361355	10654.092789	27.704346
258.350408	10679.553930	27.709364
258.776398	10702.726893	27.714381
258.995537	10732.105330	27.719399
259.083714	10746.240636	27.724416
259.387014	10758.207736	27.729434
259.829408	10781.589785	27.734452
260.259160	10805.605359	27.739469
260.461696	10813.101360	27.744487
260.536766	10837.163064	27.749504
260.886209	10853.524668	27.754522
260.690927	10880.669534	27.759540
261.242341	10908.524758	27.764557
261.519706	10924.351451	27.769575
261.912098	10946.781629	27.774592
261.968764	10952.560699	27.779610
262.093568	10979.832392	27.784628
262.609117	10993.038909	27.789645
262.873063	11006.338528	27.794663
263.037701	11033.474597	27.799680
263.614165	11063.763808	27.804698
264.241546	11068.319924	27.809716
264.057705	11090.370056	27.814733
264.063443	11103.470213	27.819751
264.345578	11120.698312	27.824768
264.513852	11144.209011	27.829786
264.534680	11164.642035	27.834804
264.565672	11193.472819	27.839821
265.168674	11215.283004	27.844839
265.538084	11242.320986	27.849856
266.189067	11271.714717	27.854874
266.505933	11286.155632	27.859892
266.707566	11301.902936	27.864909
267.101265	11312.953138	27.869927
267.564779	11338.505046	27.874944
267.916913	11352.940488	27.879962
267.926898	11377.483571	27.884980
268.484858	11384.144179	27.889997
268.515837	11393.495582	27.895015
268.834027	11418.587239	27.900032
269.426771	11426.855988	27.905050
269.553236	11434.525197	27.910068
269.708966	11446.048517	27.915085
270.208813	11469.261382	27.920103
270.245678	11477.130948	27.925120
270.985811	11491.180474	27.930138
271.508921	11493.384760	27.935156
271.556403	11513.248760	27.940173
271.974890	11522.975287	27.945191
271.625850	11538.199616	27.950208
272.127514	11543.211306	27.955226
272.265703	11556.591013	27.960244
272.435936	11572.125580	27.965261
272.781216	11588.927401	27.970279
272.880905	11602.347905	27.975296
273.218243	11629.890388	27.980314
273.674332	11636.020759	27.985332
273.687554	11664.810841	27.990349
274.031468	11663.983386	27.995367
274.285779	11699.158562	28.000384
274.437959	11714.787649	28.005402
274.717255	11729.149532	28.010420
274.668094	11748.075284	28.015437
275.192209	11768.228028	28.020455
274.959247	11785.382698	28.025472
275.680702	11812.814753	28.030490
276.150852	11831.997118	28.035508
275.997503	11862.499833	28.040525
276.372675	11884.488586	28.045543
276.795887	11895.291361	28.050560
276.825183	11930.306435	28.055578
277.180670	11947.504856	28.060596
277.214354	11974.602798	28.065613
277.376760	11988.007437	28.070631
277.946140	12020.547638	28.075648
278.155678	12048.164434	28.080666
278.778375	12077.620698	28.085684
278.497708	12105.497520	28.090701
278.766233	12121.048721	28.095719
279.359977	12151.175931	28.100736
279.429254	12180.191694	28.105754
280.470387	12185.299046	28.110772
281.166083	12195.260384	28.115789
281.568314	12203.669846	28.120807
281.876458	12217.383389	28.125824
281.918556	12209.646526	28.130842
282.142483	12217.929192	28.135860
282.393711	12238.497811	28.140877
282.423471	12244.290965	28.145895
282.770024	12260.082684	28.150912
283.146752	12274.483403	28.155930
283.391930	12284.215369	28.160948
283.425218	12309.965463	28.165965
283.926135	12316.104825	28.170983
283.897047	12341.188956	28.176000
284.282250	12354.078964	28.181018
284.408276	12372.081072	28.186036
284.542201	12392.077716	28.191053
284.741995	12407.254663	28.196071
285.215449	12419.660372	28.201088
285.021541	12451.730369	28.206106
285.776298	12482.312880	28.211124
286.094439	12499.628179	28.216141
286.364485	12518.589961	28.221159
286.873266	12542.248010	28.226176
286.904938	12561.581910	28.231194
287.063324	12583.472807	28.236212
287.515295	12610.341927	28.241229
287.811373	12626.552383	28.246247
287.786680	12656.568858	28.251264
287.965147	12684.819872	28.256282
288.683620	12704.595805	28.261300
288.429910	12728.913531	28.266317
289.032500	12750.842406	28.271335
289.508258	12785.675442	28.276352
289.488524	12799.769192	28.281370
289.791392	12826.848293	28.286388
290.233578	12851.862434	28.291405
290.476710	12880.498350	28.296423
290.656433	12905.601046	28.301440
290.820108	12926.995716	28.306458
291.450893	12945.291936	28.311476
291.597917	12981.124207	28.316493
291.747966	13001.687400	28.321511
292.638857	13038.129582	28.326528
292.414988	13058.069291	28.331546
293.116330	13072.047131	28.336564
293.119755	13101.140939	28.341581
293.588308	13122.961766	28.346599
293.878491	13153.554980	28.351616
294.111259	13170.555839	28.356634
294.299600	13196.011261	28.361652
294.832605	13226.149701	28.366669
295.474286	13234.686330	28.371687
295.972600	13257.674263	28.376704
296.129650	13275.391308	28.381722
296.617500	13305.802220	28.386740
296.661093	13315.449449	28.391757
297.040980	13330.662085	28.396775
297.056778	13338.226242	28.401792
297.522206	13361.172082	28.406810
297.680581	13377.742660	28.411828
297.660469	13399.450874	28.416845
298.172545	13417.867203	28.421863
298.494072	13432.956427	28.426880
298.579403	13459.255740	28.431898
298.851163	13482.544709	28.436916
298.976287	13518.021409	28.441933
299.004841	13539.952696	28.446951
299.781723	13564.991143	28.451968
299.843064	13583.740357	28.456986
300.445357	13599.262597	28.462004
300.594186	13626.569084	28.467021
300.823440	13638.176965	28.472039
301.533343	13672.618093	28.477056
301.610019	13684.069894	28.482074
301.799798	13697.872530	28.487092
302.130667	13729.025590	28.492109
302.248123	13752.828562	28.497127
303.021152	13774.021360	28.502144
302.812126	13797.269179	28.507162
303.441016	13820.079436	28.512180
303.849114	13841.291577	28.517197
304.248062	13856.792194	28.522215
304.622996	13880.441301	28.527232
304.458619	13901.654759	28.532250
304.805173	13913.882369	28.537268
305.322151	13942.259081	28.542285
305.880939	13966.564804	28.547303
306.176651	13988.498971	28.552320
306.288717	14010.651419	28.557338
306.570884	14022.368096	28.562356
306.841594	14054.213266	28.567373
306.974500	14067.920861	28.572391
307.506616	14086.615774	28.577408
307.589460	14113.396415	28.582426
307.912540	14136.990802	28.587444
307.765364	14167.537307	28.592461
308.300438	14195.545218	28.597479
308.784014	14219.130356	28.602496
308.824239	14250.528761	28.607514
309.347224	14276.776436	28.612532
309.934729	14311.212629	28.617549
310.136508	14333.196648	28.622567
310.651267	14348.458453	28.627584
310.437642	14375.529081	28.632602
310.386114	14400.676291	28.637620
310.806087	14430.332197	28.642637
311.138641	14463.722188	28.647655
312.015660	14492.498100	28.652672
312.024698	14528.594923	28.657690
312.771051	14551.545568	28.662708
312.847960	14582.266075	28.667725
313.403252	14608.250173	28.672743
313.794030	14635.198067	28.677760
313.817013	14663.346889	28.682778
314.157866	14682.722942	28.687796
314.333822	14714.978835	28.692813
314.551337	14737.661981	28.697831
315.260911	14756.355020	28.702848
316.031000	14786.752512	28.707866
316.320551	14808.603316	28.712884
316.069257	14835.952104	28.717901
316.350780	14855.204980	28.722919
317.000910	14876.582489	28.727936
317.195411	14904.774280	28.732954
317.425468	14925.968144	28.737972
318.119754	14955.960889	28.742989
318.073954	14970.935168	28.748007
318.517210	14993.084250	28.753024
318.715287	15022.276827	28.758042
319.394708	15033.120221	28.763060
319.489687	15071.879670	28.768077
319.545835	15089.664740	28.773095
319.880992	15111.233975	28.778112
320.277335	15141.662153	28.783130
321.106131	15141.099700	28.788148
321.305787	15172.499911	28.793165
321.796613	15180.366225	28.798183
322.120428	15202.970106	28.803200
322.295155	15215.399176	28.808218
323.002728	15231.932711	28.813236
323.206224	15231.212383	28.818253
323.120892	15255.987013	28.823271
323.908446	15266.955726	28.828288
324.007344	15292.522708	28.833306
324.210798	15296.176665	28.838324
324.362010	15325.620237	28.843341
324.628473	15340.280590	28.848359
324.969140	15345.915446	28.853376
325.469075	15379.325034	28.858394
325.520408	15394.521303	28.863412
325.680833	15424.197301	28.868429
326.076539	15448.631526	28.873447
326.433331	15462.121868	28.878464
326.684304	15495.760158	28.883482
326.816977	15516.395110	28.888500
327.037984	15550.780405	28.893517
327.317723	15580.283194	28.898535
327.882160	15610.148863	28.903552
327.561271	15643.921208	28.908570
327.854963	15674.896921	28.913588
328.607992	15715.500158	28.918605
329.155934	15747.699519	28.923623
329.429992	15771.414146	28.928640
329.702006	15805.223395	28.933658
329.934553	15839.910607	28.938676
330.338639	15864.116644	28.943693
330.629838	15898.586319	28.948711
331.151819	15919.887159	28.953728
332.006873	15935.096929	28.958746
332.611262	15955.209964	28.963764
332.820225	15975.312317	28.968781
333.114837	16009.825875	28.973799
333.484998	16022.553333	28.978816
333.867505	16042.969684	28.983834
334.242040	16056.599795	28.988852
334.165115	16081.064642	28.993869
334.188941	16118.684513	28.998887
334.787049	16141.508686	29.003904
334.952040	16167.000151	29.008922
335.168286	16189.697847	29.013940
335.567716	16228.601448	29.018957
335.463858	16253.531871	29.023975
336.088972	16277.037365	29.028992
336.548853	16324.781772	29.034010
336.972568	16355.005442	29.039028
337.328447	16368.003838	29.044045
337.335715	16395.424887	29.049063
337.899007	16426.138484	29.054080
337.881729	16460.834363	29.059098
338.561753	16497.199326	29.064116
339.050435	16522.094132	29.069133
339.385530	16562.085541	29.074151
339.750376	16583.108511	29.079168
340.125604	16616.606114	29.084186
340.449561	16642.850308	29.089204
340.855451	16675.073475	29.094221
340.954055	16705.967698	29.099239
341.195885	16725.977246	29.104256
341.477956	16754.290692	29.109274
341.671690	16788.575079	29.114292
342.438650	16820.514513	29.119309
342.664274	16850.637330	29.124327
343.412611	16865.573968	29.129344
343.165319	16891.285741	29.134362
343.645722	16919.467287	29.139380
343.994966	16945.117275	29.144397
344.264434	16973.553043	29.149415
344.448370	16993.341359	29.154432
344.968092	17036.823515	29.159450
345.524985	17048.214737	29.164468
345.820285	17079.249312	29.169485
345.816996	17105.693850	29.174503
346.265761	17143.337594	29.179520
346.607143	17166.279005	29.184538
346.912689	17192.694237	29.189556
347.143630	17226.777737	29.194573
347.291223	17269.933354	29.199591
347.784944	17288.441574	29.204608
348.230853	17333.951180	29.209626
348.521066	17356.723947	29.214644
348.611903	17402.087178	29.219661
348.705601	17439.155382	29.224679
349.537171	17474.042297	29.229696
350.235439	17499.739427	29.234714
350.475933	17533.171280	29.239732
351.140044	17556.631165	29.244749
351.212342	17598.327355	29.249767
351.684224	17623.434688	29.254784
351.929875	17657.706164	29.259802
352.098903	17681.376416	29.264820
352.498437	17710.494128	29.269837
352.876723	17745.863171	29.274855
353.608861	17783.413232	29.279872
353.776288	17810.501641	29.284890
354.375361	17844.819167	29.289908
354.729786	17861.435558	29.294925
355.121639	17893.915653	29.299943
355.638124	17922.699489	29.304960
355.833952	17944.249499	29.309978
356.329445	17980.276584	29.314996
356.792370	18003.591634	29.320013
356.745278	18052.446317	29.325031
357.470184	18067.602356	29.330048
357.447092	18095.479112	29.335066
358.233285	18122.540526	29.340084
358.761031	18146.407858	29.345101
359.252120	18152.440098	29.350119
359.692009	18173.156116	29.355136
360.016548	18196.802638	29.360154
360.230549	18217.187666	29.365172
361.175755	18234.229880	29.370189
361.066919	18251.936306	29.375207
361.677192	18271.406441	29.380224
361.802747	18289.385750	29.385242
362.029749	18318.303965	29.390260
361.864559	18333.972379	29.395277
362.360541	18370.985664	29.400295
362.919759	18398.632653	29.405312
363.169319	18418.683804	29.410330
363.419800	18448.906293	29.415348
363.702909	18477.569567	29.420365
364.160936	18507.715414	29.425383
364.757120	18529.645600	29.430400
365.131176	18564.732499	29.435418
365.098746	18586.407423	29.440436
365.435272	18613.552594	29.445453
365.861196	18645.712722	29.450471
366.022380	18671.369180	29.455488
366.673104	18704.555576	29.460506
366.615902	18734.163337	29.465524
367.172580	18767.130813	29.470541
367.337621	18807.595735	29.475559
367.798502	18833.338136	29.480576
367.617872	18858.429236	29.485594
368.074507	18897.168131	29.490612
368.750243	18925.385175	29.495629
369.148445	18960.885982	29.500647
369.640126	18983.161577	29.505664
370.239427	19023.558924	29.510682
370.197510	19044.900996	29.515700
370.804207	19072.225611	29.520717
370.718402	19116.142121	29.525735
371.198380	19151.535697	29.530752
371.750681	19176.127007	29.535770
371.948352	19221.048123	29.540788
372.050502	19251.105551	29.545805
372.161624	19280.593004	29.550823
372.974412	19326.226708	29.555840
373.543702	19362.750228	29.560858
373.490587	19407.774235	29.565876
374.094910	19443.085682	29.570893
374.388460	19486.937283	29.575911
375.013699	19516.028660	29.580928
375.521850	19553.655133	29.585946
375.510125	19591.401018	29.590964
375.990141	19622.240128	29.595981
376.313717	19659.238637	29.600999
376.638459	19702.915248	29.606016
376.991719	19741.893142	29.611034
377.437388	19787.598063	29.616052
377.890560	19823.660456	29.621069
378.279388	19869.582970	29.626087
378.886273	19907.523200	29.631104
379.655424	19943.751137	29.636122
379.780385	19976.030097	29.641140
380.180605	20004.323448	29.646157
381.137758	20036.067791	29.651175
381.279140	20054.810745	29.656192
381.981787	20088.503134	29.661210
382.169093	20118.359007	29.666228
382.811118	20139.241318	29.671245
383.295714	20169.752025	29.676263
383.586458	20196.938157	29.681280
383.879498	20228.325604	29.686298
384.015902	20250.595112	29.691316
384.603188	20278.221412	29.696333
385.034664	20305.373014	29.701351
385.454503	20340.569657	29.706368
385.521969	20370.084541	29.711386
385.447759	20405.598782	29.716404
385.856388	20432.760456	29.721421
386.047069	20471.961134	29.726439
386.454536	20509.598894	29.731456
387.013461	20535.618821	29.736474
387.372052	20580.062920	29.741492
387.871274	20608.802876	29.746509
387.999802	20656.695107	29.751527
389.048614	20667.796581	29.756544
389.736280	20705.125453	29.761562
390.044938	20731.254343	29.766580
390.430446	20765.635731	29.771597
390.718493	20794.377444	29.776615
390.773099	20827.521810	29.781632
391.288072	20848.589057	29.786650
391.341410	20890.276277	29.791668
392.201966	20911.971856	29.796685
392.420476	20959.667493	29.801703
392.864526	20990.021545	29.806720
393.243940	21026.735868	29.811738
393.413389	21056.077842	29.816756
393.992159	21086.423577	29.821773
394.262944	21111.516347	29.826791
394.486602	21141.841968	29.831808
394.638904	21176.734492	29.836826
395.137655	21206.239940	29.841844
395.476458	21235.378734	29.846861
395.980764	21281.665570	29.851879
396.358248	21309.597883	29.856896
396.688560	21338.561238	29.861914
397.201719	21380.019502	29.866932
397.709311	21414.382898	29.871949
397.953282	21448.067320	29.876967
398.604007	21487.482296	29.881984
398.564869	21526.424089	29.887002
398.905028	21568.522757	29.892020
399.329083	21605.648198	29.897037
399.598221	21650.569984	29.902055
399.726405	21679.647643	29.907072
400.346254	21725.481429	29.912090
400.261170	21779.090381	29.917108
401.115901	21818.309774	29.922125
401.549183	21873.032032	29.927143
402.064201	21901.790354	29.932160
402.481092	21943.606093	29.937178
402.924508	21994.156689	29.942196
403.333372	22030.792438	29.947213
403.749005	22074.700183	29.952231
403.924807	22112.806967	29.957248
403.951596	22158.690418	29.962266
404.716519	22214.094659	29.967284
405.329304	22256.499625	29.972301
405.582009	22288.825545	29.977319
405.946059	22341.733774	29.982336
406.821733	22385.886095	29.987354
407.319472	22425.206841	29.992372
407.917162	22471.431280	29.997389
408.250792	22499.593304	30.002407
408.605305	22545.198831	30.007424
409.006255	22579.239726	30.012442
409.379074	22634.359013	30.017460
409.633500	22660.037657	30.022477
410.348777	22708.588590	30.027495
410.541163	22745.291161	30.032512
411.447951	22774.886692	30.037530
411.417858	22816.331947	30.042548
411.962122	22854.230781	30.047565
412.691619	22884.441921	30.052583
412.966173	22930.800190	30.057600
413.456326	22959.368049	30.062618
413.984023	22992.227080	30.067636
413.983297	23021.920893	30.072653
414.505302	23069.599343	30.077671
414.763293	23099.960494	30.082688
415.531135	23132.023840	30.087706
415.593204	23165.493220	30.092724
416.010457	23210.079372	30.097741
416.394987	23256.395896	30.102759
416.657532	23294.390248	30.107776
417.166360	23323.600266	30.112794
417.608222	23366.388249	30.117812
417.979317	23403.752839	30.122829
418.924671	23447.252039	30.127847
419.638851	23478.547078	30.132864
419.838884	23503.622359	30.137882
420.565890	23552.179831	30.142900
420.994889	23569.863653	30.147917
421.317611	23604.013343	30.152935
421.635816	23627.888556	30.157952
422.214336	23638.743095	30.162970
422.509251	23678.736339	30.167988
422.794067	23708.032563	30.173005
423.067863	23728.047402	30.178023
423.108501	23769.414042	30.183040
423.894169	23798.935280	30.188058
424.142637	23837.855502	30.193076
424.224961	23861.072805	30.198093
424.645914	23904.307574	30.203111
424.924832	23943.690869	30.208128
425.375438	23980.829224	30.213146
425.355688	24032.696151	30.218164
425.901084	24074.635264	30.223181
426.637173	24117.947524	30.228199
426.815915	24168.886345	30.233216
427.121648	24213.005600	30.238234
427.490791	24262.037938	30.243252
428.101837	24297.559226	30.248269
429.076095	24335.703180	30.253287
429.501666	24377.876562	30.258304
429.730074	24406.727634	30.263322
430.085259	24460.944702	30.268340
430.750168	24494.745292	30.273357
431.537716	24534.302864	30.278375
431.524417	24578.416016	30.283392
432.480165	24615.855604	30.288410
432.637430	24653.976460	30.293428
432.952075	24691.447090	30.298445
433.691953	24733.673104	30.303463
433.798497	24774.115137	30.308480
434.435307	24816.509141	30.313498
434.728356	24857.269713	30.318516
434.891632	24895.390084	30.323533
435.759282	24936.124013	30.328551
435.996433	24982.265379	30.333568
436.368751	25028.417278	30.338586
436.789309	25060.910983	30.343604
437.299009	25106.510682	30.348621
437.811777	25151.983606	30.353639
438.009179	25194.807463	30.358656
438.987996	25235.094836	30.363674
438.728886	25281.630610	30.368692
439.306374	25325.121993	30.373709
439.750859	25378.436444	30.378727
440.094995	25428.613122	30.383744
440.551502	25468.616219	30.388762
441.036451	25516.533811	30.393780
441.321980	25559.483676	30.398797
441.658870	25611.286168	30.403815
441.934586	25662.276779	30.408832
442.465051	25708.000984	30.413850
443.076857	25758.838076	30.418868
443.551958	25814.879126	30.423885
443.791483	25859.296759	30.428903
444.499102	25910.340427	30.433920
445.102448	25956.224420	30.438938
445.904323	26002.867432	30.443956
446.321252	26046.094794	30.448973
446.885122	26089.406674	30.453991
447.185972	26126.193238	30.459008
448.129075	26155.181355	30.464026
448.462229	26200.747976	30.469044
448.643863	26239.512664	30.474061
449.216136	26266.460732	30.479079
449.337962	26312.408314	30.484096
450.095690	26345.672899	30.489114
450.185843	26392.737977	30.494132
450.849677	26432.268093	30.499149
451.603188	26470.545476	30.504167
451.501132	26514.506109	30.509184
452.353094	26531.841881	30.514202
452.924145	26561.685207	30.519220
453.368279	26602.033778	30.524237
453.784262	26628.735037	30.529255
453.895159	26665.647137	30.534272
454.703429	26690.991376	30.539290
455.114881	26739.207788	30.544308
455.338557	26773.725983	30.549325
456.095666	26814.714872	30.554343
456.219974	26855.278369	30.559360
456.661879	26895.381379	30.564378
457.013263	26925.120598	30.569396
457.226021	26974.613803	30.574413
457.768598	27021.950776	30.579431
458.121229	27077.098040	30.584448
458.569860	27117.491174	30.589466
458.908889	27155.638837	30.594484
459.073046	27212.642596	30.599501
459.739710	27265.029706	30.604519
460.085355	27316.986875	30.609536
460.686568	27356.939433	30.614554
461.076529	27415.975198	30.619572
461.524219	27467.708190	30.624589
461.949624	27520.664671	30.629607
462.192055	27572.626017	30.634624
463.261703	27621.632628	30.639642
463.729803	27654.015597	30.644660
464.553864	27695.931224	30.649677
465.449823	27728.822473	30.654695
465.585661	27781.534237	30.659712
466.138077	27820.401877	30.664730
467.189314	27859.065049	30.669748
467.151376	27900.528289	30.674765
467.757991	27933.155475	30.679783
467.725298	27976.147650	30.684800
468.711985	28015.598675	30.689818
469.327511	28059.172133	30.694836
469.702479	28087.714739	30.699853
470.402717	28122.388122	30.704871
470.920471	28158.076182	30.709888
471.421003	28197.736440	30.714906
471.938125	28225.681786	30.719924
472.037484	28262.946225	30.724941
472.728155	28292.305617	30.729959
473.032939	28332.470856	30.734976
473.427220	28352.875935	30.739994
474.079809	28390.167730	30.745012
474.309274	28434.617842	30.750029
475.389351	28469.769592	30.755047
475.474034	28509.350209	30.760064
475.801840	28550.694270	30.765082
476.107891	28591.340204	30.770100
476.716775	28633.221928	30.775117
476.820403	28685.131989	30.780135
477.340433	28726.604320	30.785152
477.893364	28760.650802	30.790170
478.271067	28806.507033	30.795188
478.778278	28860.320140	30.800205
478.908874	28899.072590	30.805223
479.433309	28963.079009	30.810240
479.845302	29004.315983	30.815258
480.330462	29048.158483	30.820276
480.215018	29102.132957	30.825293
480.859725	29154.806476	30.830311
481.063692	29217.220404	30.835328
481.632980	29260.639311	30.840346
482.241325	29321.662791	30.845364
482.169372	29372.780343	30.850381
483.232754	29416.090584	30.855399
483.436951	29478.479984	30.860416
484.139534	29535.608148	30.865434
484.516918	29581.700040	30.870452
484.950984	29636.759266	30.875469
485.689344	29692.738125	30.880487
486.076956	29754.865747	30.885504
486.319381	29800.897091	30.890522
486.971853	29856.112331	30.895540
487.410396	29917.252668	30.900557
487.904753	29963.346055	30.905575
488.035205	30017.853327	30.910592
488.747383	30077.288771	30.915610
489.552673	30134.219189	30.920628
489.848555	30195.679797	30.925645
490.406827	30249.595997	30.930663
490.644964	30311.084957	30.935680
491.122182	30376.879475	30.940698
492.115016	30425.746784	30.945716
492.284222	30494.181710	30.950733
492.938319	30544.044253	30.955751
493.337698	30604.560606	30.960768
493.790892	30653.601476	30.965786
494.453737	30708.728868	30.970804
494.753886	30776.265522	30.975821
495.338347	30842.651590	30.980839
495.792798	30901.636686	30.985856
496.363907	30963.397828	30.990874
496.800236	31013.131245	30.995892
497.571986	31080.550773	31.000909
498.056553	31138.981842	31.005927
498.398468	31199.837657	31.010944
499.214973	31254.171185	31.015962
500.341252	31300.231790	31.020980
500.713019	31359.344926	31.025997
501.794579	31398.275521	31.031015
502.280734	31436.382790	31.036032
502.912757	31485.821174	31.041050
503.529280	31516.467452	31.046068
503.723991	31568.686569	31.051085
504.286025	31606.150086	31.056103
505.076027	31636.699831	31.061120
505.161809	31689.138608	31.066138
506.057736	31713.040277	31.071156
506.331670	31762.219311	31.076173
506.997749	31808.820940	31.081191
507.423537	31859.082745	31.086208
507.812437	31898.552653	31.091226
508.108072	31930.950390	31.096244
508.286859	31988.413909	31.101261
508.869388	32032.563575	31.106279
509.441957	32090.629503	31.111296
509.722079	32140.320536	31.116314
509.803327	32188.955456	31.121332
510.161949	32251.215202	31.126349
510.679235	32297.936057	31.131367
511.687657	32353.614273	31.136384
512.020232	32416.890117	31.141402
512.447918	32485.702033	31.146420
512.759068	32533.018363	31.151437
513.415330	32585.566023	31.156455
514.203237	32645.711347	31.161472
514.237806	32700.992990	31.166490
514.727460	32754.060294	31.171508
515.358813	32813.939802	31.176525
516.125416	32869.486567	31.181543
516.371812	32918.394455	31.186560
517.052622	32960.937493	31.191578
517.416297	33017.413901	31.196596
518.059822	33072.714947	31.201613
518.293447	33135.148631	31.206631
519.077383	33187.393300	31.211648
519.133366	33241.490746	31.216666
519.754050	33301.702076	31.221684
520.374700	33355.117076	31.226701
520.807131	33405.463742	31.231719
522.045294	33466.286936	31.236736
522.430516	33526.485210	31.241754
523.033038	33562.080786	31.246772
523.461405	33626.578139	31.251789
523.711402	33676.460877	31.256807
524.718759	33724.107097	31.261824
524.947170	33786.682623	31.266842
525.460347	33827.110356	31.271860
526.151409	33892.149046	31.276877
526.683264	33944.169533	31.281895
527.136637	33995.595478	31.286912
527.766203	34054.840225	31.291930
528.529667	34102.171438	31.296948
528.838354	34156.617328	31.301965
529.562800	34206.863269	31.306983
530.143872	34261.791544	31.312000
530.346684	34316.760237	31.317018
530.896453	34367.324759	31.322036
531.177019	34428.218518	31.327053
531.887644	34479.934129	31.332071
532.243034	34538.015544	31.337088
532.569339	34603.176778	31.342106
533.316152	34656.802934	31.347124
534.066905	34732.608782	31.352141
534.245024	34786.741637	31.357159
534.682832	34841.428298	31.362176
535.261218	34921.510723	31.367194
536.150459	34979.680452	31.372212
536.424927	35044.199910	31.377229
536.912656	35107.680829	31.382247
537.066943	35158.391377	31.387264
537.439012	35239.809827	31.392282
538.677247	35298.564384	31.397300
538.943578	35374.214446	31.402317
539.166606	35443.731969	31.407335
540.134344	35512.393294	31.412352
540.059884	35586.099423	31.417370
541.241624	35648.821994	31.422388
541.563924	35711.723616	31.427405
542.090215	35772.816697	31.432423
542.763374	35843.731974	31.437440
543.402714	35916.600297	31.442458
543.706438	35976.729771	31.447476
544.228373	36048.693759	31.452493
545.132465	36120.187131	31.457511
545.805010	36177.755438	31.462528
546.041941	36247.823520	31.467546
546.585776	36309.920779	31.472564
547.238849	36379.822946	31.477581
547.826095	36438.404386	31.482599
548.541644	36499.722836	31.487616
548.784448	36565.352105	31.492634
549.659505	36639.570776	31.497652
550.202940	36687.890710	31.502669
551.217504	36745.887554	31.507687
552.329670	36799.765411	31.512704
552.551277	36850.260763	31.517722
552.879604	36896.426971	31.522740
553.388968	36939.915421	31.527757
554.501145	36981.772960	31.532775
555.336116	37040.032695	31.537792
555.755008	37083.276346	31.542810
556.402600	37117.403789	31.547828
556.593271	37164.085362	31.552845
556.625180	37214.408930	31.557863
556.999775	37260.372648	31.562880
557.864447	37323.662002	31.567898
558.672619	37373.718927	31.572916
558.951383	37423.707117	31.577933
559.099091	37485.901443	31.582951
559.754816	37532.125242	31.587968
559.981921	37603.849745	31.592986
560.864623	37651.290324	31.598004
561.517230	37717.933947	31.603021
561.735282	37779.428827	31.608039
562.397883	37837.256096	31.613056
562.574189	37907.528800	31.618074
563.372940	37970.027274	31.623092
563.606379	38039.399817	31.628109
564.251053	38111.623422	31.633127
564.939922	38173.184809	31.638144
565.226819	38247.292468	31.643162
565.796421	38324.960673	31.648180
566.412219	38387.963296	31.653197
566.899985	38467.421823	31.658215
567.769462	38534.938314	31.663232
568.006767	38609.902380	31.668250
568.374806	38676.757953	31.673268
569.038856	38748.481062	31.678285
569.452745	38830.564274	31.683303
570.597184	38892.258726	31.688320
570.686576	38973.198070	31.693338
571.382673	39049.982677	31.698356
572.231648	39121.184785	31.703373
572.498326	39205.695606	31.708391
573.378508	39269.462543	31.713408
573.931280	39357.223992	31.718426
574.533611	39425.316322	31.723444
575.431222	39495.468560	31.728461
575.636458	39568.031458	31.733479
576.554164	39635.366746	31.738496
577.095438	39710.502027	31.743514
577.872009	39777.549974	31.748532
578.506907	39846.669372	31.753549
578.740787	39917.350645	31.758567
579.953180	39983.249520	31.763584
580.186170	40050.990573	31.768602
580.930950	40118.948925	31.773620
581.436923	40189.986900	31.778637
581.807956	40256.922754	31.783655
582.597231	40317.070489	31.788672
582.785204	40398.410773	31.793690
583.275969	40462.084082	31.798708
583.974280	40537.115398	31.803725
584.773824	40606.805915	31.808743
585.116144	40679.218222	31.813760
585.560728	40753.670217	31.818778
586.321303	40814.133717	31.823796
587.138005	40895.908641	31.828813
587.385950	40973.269849	31.833831
588.811376	41038.385922	31.838848
589.182443	41104.426270	31.843866
589.959213	41166.456709	31.848884
590.959848	41227.838773	31.853901
591.241413	41282.635807	31.858919
591.838653	41330.103837	31.863936
592.603810	41390.903419	31.868954
592.937017	41440.772150	31.873972
593.549241	41505.953725	31.878989
593.779479	41554.757312	31.884007
594.362225	41619.203845	31.889024
594.475865	41695.058037	31.894042
595.233580	41753.152780	31.899060
596.149695	41820.431800	31.904077
596.505012	41887.507910	31.909095
597.441892	41940.755566	31.914112
597.868602	42010.217988	31.919130
598.024229	42085.421810	31.924148
598.864631	42144.383796	31.929165
599.192685	42220.901956	31.934183
599.939782	42280.087640	31.939200
600.597408	42361.886605	31.944218
601.159266	42437.660502	31.949236
601.942516	42502.723365	31.954253
602.042222	42575.104006	31.959271
602.509490	42647.224917	31.964288
603.321974	42731.568968	31.969306
603.952073	42810.894474	31.974324
604.615204	42890.303643	31.979341
604.747574	42963.932812	31.984359
605.737624	43038.914316	31.989376
606.518792	43118.059133	31.994394
607.135865	43200.266033	31.999412
607.854973	43267.390557	32.004429
608.542707	43348.733034	32.009447
609.205188	43418.738548	32.014464
609.418365	43506.430594	32.019482
610.009295	43585.107171	32.024500
611.047776	43646.610218	32.029517
611.482833	43733.376537	32.034535
611.948413	43808.493380	32.039552
612.164597	43886.742658	32.044570
613.104840	43982.817733	32.049588
613.773481	44052.564933	32.054605
614.317026	44133.692493	32.059623
614.839483	44216.626417	32.064640
615.269114	44300.947825	32.069658
616.066715	44391.980258	32.074676
616.668518	44471.290814	32.079693
617.722930	44559.854693	32.084711
618.351952	44634.993000	32.089728
618.707320	44715.374090	32.094746
619.156362	44801.699573	32.099764
620.281047	44873.022586	32.104781
620.322166	44964.669225	32.109799
621.167151	45038.724996	32.114816
621.755901	45125.706700	32.119834
622.287137	45211.742555	32.124852
623.438082	45283.847160	32.129869
624.098017	45373.228804	32.134887
624.951686	45443.697809	32.139904
625.713465	45520.121414	32.144922
625.941111	45603.834116	32.149940
626.815882	45669.916686	32.154957
627.310155	45750.014037	32.159975
627.898901	45821.151983	32.164992
628.607757	45898.205103	32.170010
629.629734	45969.731140	32.175028
630.154322	46038.184946	32.180045
630.936428	46107.503252	32.185063
631.509222	46171.477410	32.190080
632.060141	46251.713171	32.195098
632.296707	46329.202315	32.200116
632.682778	46389.473938	32.205133
633.282034	46468.836223	32.210151
634.199546	46531.125272	32.215168
634.692760	46613.383070	32.220186
635.122343	46691.026683	32.225204
635.801396	46752.999421	32.230221
636.285186	46840.794955	32.235239
637.023396	46912.045779	32.240256
637.585738	46982.786636	32.245274
638.146644	47067.572317	32.250292
638.507202	47153.123545	32.255309
638.844733	47240.911900	32.260327
639.798194	47321.569212	32.265344
640.481616	47398.036744	32.270362
640.798656	47497.602716	32.275380
641.679503	47587.761973	32.280397
641.895556	47670.218839	32.285415
642.803864	47758.305717	32.290432
643.648933	47846.579982	32.295450
643.917437	47934.116107	32.300468
644.903470	48020.565906	32.305485
645.447435	48112.216127	32.310503
646.309435	48201.020546	32.315520
646.949192	48293.554871	32.320538
648.238351	48373.075153	32.325556
649.283423	48452.330257	32.330573
649.772930	48520.177023	32.335591
650.540122	48593.288620	32.340608
651.351430	48667.102138	32.345626
651.877399	48747.527760	32.350644
652.670873	48817.497884	32.355661
653.146113	48897.571350	32.360679
653.988676	48972.051598	32.365696
654.610783	49047.528293	32.370714
655.555119	49117.387130	32.375732
656.068511	49192.489062	32.380749
656.617952	49274.114962	32.385767
657.375880	49352.494422	32.390784
658.327843	49414.001421	32.395802
659.032383	49487.897571	32.400820
659.354727	49556.735280	32.405837
659.682798	49641.617589	32.410855
660.613716	49716.023142	32.415872
661.002912	49786.926335	32.420890
661.509702	49871.825793	32.425908
661.937321	49953.960366	32.430925
662.603965	50043.530127	32.435943
663.591075	50115.568154	32.440960
664.168106	50202.210445	32.445978
664.545964	50294.515449	32.450996
664.969028	50371.596797	32.456013
665.544730	50462.194776	32.461031
666.559728	50556.254924	32.466048
667.583207	50646.682265	32.471066
667.689980	50741.113180	32.476084
668.416121	50819.141942	32.481101
669.193278	50913.297733	32.486119
669.744993	50992.607212	32.491136
670.002797	51086.161680	32.496154
670.439830	51182.162482	32.501172
671.604588	51270.209998	32.506189
671.614984	51372.650147	32.511207
672.689086	51463.718147	32.516224
673.479164	51562.145612	32.521242
673.960485	51671.846940	32.526260
674.503208	51761.006137	32.531277
675.363414	51857.544573	32.536295
675.846164	51954.946130	32.541312
676.787448	52053.902495	32.546330
677.205002	52142.063994	32.551348
677.892095	52225.652972	32.556365
678.680659	52315.554095	32.561383
679.412744	52407.565225	32.566400
680.267944	52496.545411	32.571418
680.776334	52590.389382	32.576436
681.560367	52675.198708	32.581453
682.374504	52761.250214	32.586471
683.063285	52857.401985	32.591488
683.794132	52936.025585	32.596506
684.556102	53027.604172	32.601524
685.393049	53100.719067	32.606541
685.736651	53201.906400	32.611559
686.097566	53292.530021	32.616576
687.358255	53388.290657	32.621594
687.835430	53491.325084	32.626612
688.714051	53574.363644	32.631629
689.154900	53661.970332	32.636647
689.695515	53772.627743	32.641664
690.792463	53846.147206	32.646682
691.171104	53946.889278	32.651700
691.927547	54033.258224	32.656717
692.682493	54138.523800	32.661735
693.222929	54226.357458	32.666752
694.380037	54324.409959	32.671770
694.735621	54421.866961	32.676788
695.167774	54520.881798	32.681805
696.369685	54618.301995	32.686823
696.517600	54731.904791	32.691840
697.473490	54828.079715	32.696858
698.047329	54917.030829	32.701876
698.398327	55016.800870	32.706893
699.242376	55122.677050	32.711911
699.890644	55228.223635	32.716928
700.756868	55329.730587	32.721946
701.420485	55440.686617	32.726964
702.435734	55540.664929	32.731981
703.479714	55633.899175	32.736999
703.506607	55739.032711	32.742016
704.668958	55836.615983	32.747034
705.452394	55939.157411	32.752052
706.138735	56033.063107	32.757069
706.924039	56139.617517	32.762087
707.387879	56235.052437	32.767104
708.397906	56337.376552	32.772122
709.133210	56436.516419	32.777140
709.727775	56536.950838	32.782157
710.425969	56626.952097	32.787175
711.439736	56737.732731	32.792192
712.337135	56827.279508	32.797210
713.245080	56921.957758	32.802228
713.836529	57014.470798	32.807245
714.220181	57101.428215	32.812263
715.193646	57195.299825	32.817280
716.410487	57288.051419	32.822298
716.887115	57395.779986	32.827316
717.301247	57478.518817	32.832333
718.339806	57564.286739	32.837351
718.942765	57644.129471	32.842368
719.996713	57743.832424	32.847386
720.383654	57841.000963	32.852404
721.084349	57917.917859	32.857421
721.851337	58007.514761	32.862439
722.735320	58105.517937	32.867456
723.159701	58183.687840	32.872474
723.824757	58282.909596	32.877492
724.422036	58375.009199	32.882509
725.461986	58456.786252	32.887527
725.831296	58555.289582	32.892544
726.924320	58628.495237	32.897562
727.440013	58711.874307	32.902580
727.762874	58799.277746	32.907597
728.836828	58883.139632	32.912615
729.558534	58972.253488	32.917632
730.323751	59058.588525	32.922650
731.049712	59161.981818	32.927668
731.550579	59248.820983	32.932685
732.170794	59341.515633	32.937703
732.505355	59439.920378	32.942720
733.607453	59535.888675	32.947738
734.036727	59637.418889	32.952756
734.674130	59740.024629	32.957773
735.562491	59841.863582	32.962791
736.003306	59946.539144	32.967808
736.785452	60042.053151	32.972826
737.181684	60146.932773	32.977844
738.079892	60253.171108	32.982861
738.733969	60362.859928	32.987879
739.264194	60477.417327	32.992896
740.345385	60578.748071	32.997914
741.182282	60703.626905	33.002932
741.747761	60818.180370	33.007949
742.291605	60922.711027	33.012967
742.713053	61052.834633	33.017984
744.195359	61160.890761	33.023002
744.762784	61277.161501	33.028020
745.659460	61386.538364	33.033037
746.515030	61490.883349	33.038055
747.572938	61607.920747	33.043072
748.782354	61696.183178	33.048090
749.712369	61794.801616	33.053108
750.673778	61896.833866	33.058125
751.427606	61988.074268	33.063143
752.104791	62089.474480	33.068160
752.789976	62188.632918	33.073178
753.516136	62280.638367	33.078196
753.981220	62381.572887	33.083213
754.882844	62481.148055	33.088231
755.432926	62591.337827	33.093248
756.119790	62701.778876	33.098266
756.896611	62808.977780	33.103284
757.311887	62911.973326	33.108301
758.454736	63013.570264	33.113319
758.766287	63143.057327	33.118336
759.560068	63232.694400	33.123354
760.710987	63343.970896	33.128372
761.510800	63460.247107	33.133389
762.380397	63557.324647	33.138407
762.807819	63669.152702	33.143424
763.867330	63771.569770	33.148442
764.807614	63886.344570	33.153460
765.385533	63987.350205	33.158477
766.443845	64084.457212	33.163495
766.726625	64194.999780	33.168512
767.819116	64299.851211	33.173530
768.237602	64407.227022	33.178548
769.134237	64509.615626	33.183565
769.867782	64621.805158	33.188583
770.596420	64734.356823	33.193600
771.168038	64838.545006	33.198618
772.019229	64950.603619	33.203636
772.179426	65064.739891	33.208653
773.408572	65168.035086	33.213671
774.246134	65281.578772	33.218688
774.984028	65391.992000	33.223706
776.189450	65501.072596	33.228724
776.918951	65607.651394	33.233741
777.792549	65702.463673	33.238759
778.159235	65796.557949	33.243776
778.815893	65903.535601	33.248794
779.832739	66017.098823	33.253812
780.426988	66116.495926	33.258829
781.170858	66223.176355	33.263847
781.789884	66340.095611	33.268864
782.652365	66446.011298	33.273882
783.179671	66557.652866	33.278900
784.010761	66671.336731	33.283917
784.894354	66777.611380	33.288935
785.266107	66895.996484	33.293952
786.016996	67005.876495	33.298970
786.851523	67122.600965	33.303988
787.575861	67242.603991	33.309005
788.570174	67374.677702	33.314023
789.265720	67488.652348	33.319040
790.194572	67614.950414	33.324058
790.717051	67728.984885	33.329076
791.383299	67861.587348	33.334093
792.572728	67978.798332	33.339111
792.864271	68112.321882	33.344128
793.875572	68237.134777	33.349146
794.617355	68356.272803	33.354164
794.931881	68478.663227	33.359181
796.313478	68615.722846	33.364199
797.268002	68742.345341	33.369216
798.185147	68867.207682	33.374234
798.704979	68998.192587	33.379252
799.429280	69126.106747	33.384269
800.252726	69250.504369	33.389287
801.232141	69387.149807	33.394304
802.600411	69498.938376	33.399322
803.177742	69626.308119	33.404340
803.549807	69754.901081	33.409357
804.450130	69879.935558	33.414375
805.313262	70015.298059	33.419392
806.230393	70142.851408	33.424410
806.894845	70261.111089	33.429428
807.991343	70395.843779	33.434445
808.595151	70523.612689	33.439463
809.592047	70655.918010	33.444480
810.409040	70774.827360	33.449498
811.434292	70900.315753	33.454516
812.076717	71036.439995	33.459533
813.214015	71151.982658	33.464551
813.954023	71285.154605	33.469568
815.072698	71406.577936	33.474586
815.973209	71531.784909	33.479604
816.741315	71659.951567	33.484621
818.031165	71775.308428	33.489639
818.513032	71892.907443	33.494656
819.636446	72006.201576	33.499674
820.689096	72118.278716	33.504692
821.291220	72226.715855	33.509709
822.510696	72334.537476	33.514727
822.913882	72449.136855	33.519744
823.815264	72558.491084	33.524762
825.130342	72668.211623	33.529780
825.767194	72784.194430	33.534797
826.470540	72889.743274	33.539815
827.057301	73000.136528	33.544832
827.891356	73111.314809	33.549850
828.709202	73226.536571	33.554868
829.354831	73342.191115	33.559885
830.351032	73449.456912	33.564903
830.705904	73557.950858	33.569920
831.340739	73663.817483	33.574938
832.296992	73772.737450	33.579956
833.296805	73883.563665	33.584973
834.598081	73991.353853	33.589991
835.088303	74098.359487	33.595008
835.111504	74210.986624	33.600026
836.384679	74321.683180	33.605044
837.141951	74441.593633	33.610061
838.137022	74558.085373	33.615079
838.619154	74679.572642	33.620096
839.661337	74805.494820	33.625114
840.712013	74924.335468	33.630132
841.426180	75046.636738	33.635149
842.439342	75155.806739	33.640167
842.955408	75279.115440	33.645184
843.413874	75407.107885	33.650202
843.948790	75530.566785	33.655220
844.868957	75661.908273	33.660237
845.913526	75790.444115	33.665255
846.843300	75910.764766	33.670272
847.713769	76049.070284	33.675290
848.781691	76180.391145	33.680308
849.328837	76318.558648	33.685325
850.561400	76437.136766	33.690343
851.220940	76582.761888	33.695360
852.049975	76714.528095	33.700378
852.739915	76845.379301	33.705396
853.826883	76978.233824	33.710413
854.634421	77114.312390	33.715431
855.241035	77249.270308	33.720448
856.449790	77387.162263	33.725466
857.526654	77517.474710	33.730484
858.329671	77656.178967	33.735501
858.675989	77778.030703	33.740519
859.630882	77920.500305	33.745536
859.882277	78054.149623	33.750554
861.186651	78196.983988	33.755572
861.937586	78355.589318	33.760589
862.842956	78488.327553	33.765607
864.001623	78630.160823	33.770624
864.652395	78770.630120	33.775642
865.807991	78913.466147	33.780660
866.704103	79059.168682	33.785677
867.710433	79190.462901	33.790695
868.131562	79326.600216	33.795712
869.273721	79466.248624	33.800730
870.312557	79608.257685	33.805748
871.072537	79757.025763	33.810765
872.593976	79882.668182	33.815783
872.814109	80023.832027	33.820800
873.661461	80157.018072	33.825818
875.278025	80296.330299	33.830836
876.100412	80440.759325	33.835853
876.425993	80573.192867	33.840871
877.223257	80712.394730	33.845888
878.422144	80843.223136	33.850906
879.390227	80975.013176	33.855924
880.198967	81120.537426	33.860941
881.387853	81259.363934	33.865959
882.579540	81375.828406	33.870976
883.221134	81516.731042	33.875994
884.468724	81648.303088	33.881012
884.760829	81781.913190	33.886029
885.948862	81905.729035	33.891047
886.568129	82038.833000	33.896064
887.344519	82172.989954	33.901082
888.378881	82306.955106	33.906100
888.923934	82435.802676	33.911117
890.057792	82566.079080	33.916135
890.845252	82687.591700	33.921152
891.397422	82825.879392	33.926170
892.247414	82949.664027	33.931188
893.229031	83087.657677	33.936205
894.003832	83218.170672	33.941223
895.006608	83355.161318	33.946240
895.500017	83486.251767	33.951258
896.564602	83625.679492	33.956276
897.310937	83769.706582	33.961293
898.232229	83911.831697	33.966311
899.322772	84045.403409	33.971328
900.101683	84187.108693	33.976346
901.122463	84326.876130	33.981364
901.802426	84476.783899	33.986381
902.277972	84628.156309	33.991399
903.501770	84772.303724	33.996416
903.918534	84938.436417	34.001434
904.791729	85082.184102	34.006452
905.730264	85252.279100	34.011469
906.769362	85404.517696	34.016487
907.963684	85553.906999	34.021504
908.310207	85707.396076	34.026522
909.093791	85868.230546	34.031540
910.357271	86029.903139	34.036557
911.400998	86184.983598	34.041575
912.352093	86347.239085	34.046592
912.863588	86525.290389	34.051610
913.762369	86682.487081	34.056628
914.941576	86839.399936	34.061645
915.544723	87013.131288	34.066663
916.657907	87183.805794	34.071680
917.434292	87353.951091	34.076698
918.560753	87520.038034	34.081716
919.740152	87680.503658	34.086733
920.509821	87845.178275	34.091751
921.579112	88015.078759	34.096768
922.577578	88171.330007	34.101786
923.586838	88334.829279	34.106804
924.699043	88498.959656	34.111821
925.146519	88661.002586	34.116839
926.513803	88835.575478	34.121856
927.102796	89006.291879	34.126874
927.925708	89164.793642	34.131892
929.345450	89330.008366	34.136909
930.350199	89499.167037	34.141927
931.389693	89657.789584	34.146944
931.820722	89825.227624	34.151962
933.177809	89976.844370	34.156980
934.155545	90139.838851	34.161997
935.103741	90303.840064	34.167015
936.044962	90468.033370	34.172032
936.842167	90632.858466	34.177050
938.062359	90796.312817	34.182068
938.704966	90950.238924	34.187085
939.752946	91119.095759	34.192103
941.150417	91280.421075	34.197120
941.798634	91451.116731	34.202138
942.944490	91601.532642	34.207156
944.048852	91769.116840	34.212173
944.822011	91919.719422	34.217191
946.035764	92063.891185	34.222208
946.877137	92237.286014	34.227226
947.496534	92394.239605	34.232244
948.687705	92549.190603	34.237261
949.701911	92700.519773	34.242279
950.495267	92850.363295	34.247296
951.345613	93008.437276	34.252314
952.232915	93157.583146	34.257332
953.316885	93317.016376	34.262349
953.646495	93467.100288	34.267367
954.951060	93619.960227	34.272384
955.463990	93776.912198	34.277402
956.539217	93931.495384	34.282420
957.540370	94092.669418	34.287437
958.105807	94258.653096	34.292455
959.215540	94421.713144	34.297472
959.993911	94589.566565	34.302490
960.947085	94753.362694	34.307508
962.145131	94917.121344	34.312525
963.160830	95088.857067	34.317543
964.310064	95245.273178	34.322560
965.406379	95415.451632	34.327578
966.202241	95578.503495	34.332596
967.035588	95746.202416	34.337613
967.951224	95917.159765	34.342631
968.885433	96096.164463	34.347648
969.606327	96264.593618	34.352666
970.722758	96447.108433	34.357684
971.863565	96617.032903	34.362701
972.736645	96793.541220	34.367719
973.511182	96982.957910	34.372736
974.698764	97155.337181	34.377754
975.652341	97327.525848	34.382772
976.812624	97502.028268	34.387789
977.422482	97680.864534	34.392807
978.764643	97850.548580	34.397824
979.830651	98035.476344	34.402842
980.819077	98208.602405	34.407860
981.589812	98381.167667	34.412877
982.570126	98563.221538	34.417895
983.865348	98739.928083	34.422912
984.956040	98930.637933	34.427930
985.865207	99115.583805	34.432948
986.310904	99283.679004	34.437965
987.149293	99479.794136	34.442983
988.265192	99666.612413	34.448000
988.950552	99857.644752	34.453018
990.237793	100048.685402	34.458036
991.404582	100235.334179	34.463053
992.033895	100429.167758	34.468071
993.339718	100618.383239	34.473088
994.232660	100817.794160	34.478106
995.307836	101006.528206	34.483124
996.393282	101198.836962	34.488141
997.201862	101389.681489	34.493159
998.257568	101573.490031	34.498176
999.980727	101754.925678	34.503194
1001.567986	101926.278918	34.508212
1002.430425	102101.131682	34.513229
1003.560503	102282.168630	34.518247
1004.853416	102447.446929	34.523264
1005.678069	102627.747513	34.528282
1006.697697	102803.758496	34.533300
1008.068949	102975.962434	34.538317
1008.953019	103147.216552	34.543335
1009.923233	103314.058474	34.548352
1010.516940	103487.134850	34.553370
1011.633004	103664.453899	34.558388
1012.401882	103831.114382	34.563405
1013.556801	104007.364118	34.568423
1014.696935	104188.232345	34.573440
1015.673562	104360.391089	34.578458
1016.700322	104543.345708	34.583476
1018.099311	104708.441080	34.588493
1018.616821	104870.835059	34.593511
1019.754510	105027.388870	34.598528
1020.879313	105198.108579	34.603546
1021.806599	105353.226001	34.608564
1023.125938	105514.990343	34.613581
1023.743807	105688.048882	34.618599
1024.997600	105839.744575	34.623616
1025.536361	106003.155035	34.628634
1026.220307	106183.978551	34.633652
1027.780427	106352.391537	34.638669
1028.525880	106532.471823	34.643687
1029.391139	106699.803376	34.648704
1030.155126	106883.293575	34.653722
1031.313485	107058.062342	34.658740
1032.252699	107238.940216	34.663757
1033.084335	107428.357155	34.668775
1034.216117	107609.397029	34.673792
1034.998313	107800.852634	34.678810
1036.341188	107988.493398	34.683828
1037.489486	108172.272654	34.688845
1038.138041	108361.127362	34.693863
1039.329481	108549.910778	34.698880
1040.169258	108738.610784	34.703898
1041.251226	108925.955066	34.708916
1042.592326	109124.558624	34.713933
1043.469949	109320.686961	34.718951
1044.634342	109512.409154	34.723968
1045.987275	109701.604660	34.728986
1046.738122	109902.486212	34.734004
1048.229107	110088.986417	34.739021
1049.229043	110287.231467	34.744039
1050.635162	110461.395143	34.749056
1051.607726	110659.735335	34.754074
1052.686211	110842.563009	34.759092
1053.892798	111026.652426	34.764109
1055.264360	111219.632295	34.769127
1056.161411	111399.422230	34.774144
1057.169190	111588.529658	34.779162
1058.402768	111772.086051	34.784180
1059.128123	111946.566480	34.789197
1060.525632	112141.982221	34.794215
1061.781532	112318.397857	34.799232
1062.952096	112512.227814	34.804250
1063.990592	112692.078169	34.809268
1065.176728	112869.433233	34.814285
1066.074710	113069.421778	34.819303
1067.024195	113263.290372	34.824320
1068.124416	113448.042962	34.829338
1068.901897	113632.453855	34.834356
1070.319103	113810.157815	34.839373
1071.163267	113992.974747	34.844391
1072.653777	114168.348020	34.849408
1073.657802	114348.364151	34.854426
1074.658687	114550.171043	34.859444
1075.729294	114724.927835	34.864461
1076.709888	114919.117409	34.869479
1077.964717	115097.043271	34.874496
1079.193789	115281.721512	34.879514
1080.153538	115471.998132	34.884532
1081.156526	115644.271245	34.889549
1081.829658	115832.971115	34.894567
1083.486254	116021.251619	34.899584
1084.619912	116209.957402	34.904602
1085.415752	116399.998074	34.909620
1086.085091	116582.969330	34.914637
1086.966810	116774.368296	34.919655
1088.354262	116968.378031	34.924672
1089.492766	117151.760594	34.929690
1090.251246	117339.059466	34.934708
1091.248431	117519.612055	34.939725
1091.956439	117704.092105	34.944743
1093.283068	117888.920148	34.949760
1094.735888	118081.910644	34.954778
1095.365677	118273.864019	34.959796
1095.997551	118459.932509	34.964813
1097.512545	118653.499649	34.969831
1098.704744	118833.393732	34.974848
1100.470457	119017.777982	34.979866
1101.591542	119201.274644	34.984884
1102.938531	119385.142724	34.989901
1103.754624	119564.135086	34.994919
1104.949242	119746.164098	34.999936
1106.428413	119926.259383	35.004954
1107.324131	120108.818922	35.009972
1108.420531	120300.861599	35.014989
1109.934205	120486.941379	35.020007
1110.651392	120672.601287	35.025024
1111.939979	120859.720209	35.030042
1112.885334	121051.587278	35.035060
1114.038475	121240.898396	35.040077
1114.712953	121439.659803	35.045095
1116.043506	121624.302180	35.050112
1116.871774	121818.259046	35.055130
1117.269890	122018.944088	35.060148
1118.777331	122226.255937	35.065165
1119.692863	122434.777874	35.070183
1120.560775	122642.940479	35.075200
1121.619354	122863.848880	35.080218
1122.520813	123073.847924	35.085236
1123.751739	123288.604447	35.090253
1124.566428	123510.658286	35.095271
1125.580751	123726.237599	35.100288
1127.144010	123946.096151	35.105306
1128.131781	124172.604750	35.110324
1129.558855	124392.246023	35.115341
1130.772376	124616.501680	35.120359
1131.812503	124830.509759	35.125376
1133.158827	125053.211991	35.130394
1134.253420	125274.178741	35.135412
1135.526080	125494.788961	35.140429
1136.801896	125726.767122	35.145447
1137.924733	125935.655335	35.150464
1139.312600	126148.588266	35.155482
1139.813263	126360.519377	35.160500
1141.735206	126567.065499	35.165517
1142.920852	126789.523216	35.170535
1144.149564	127002.536221	35.175552
1145.806008	127218.553641	35.180570
1146.681290	127443.258324	35.185588
1147.844356	127634.272589	35.190605
1148.699958	127860.885689	35.195623
1149.642908	128071.322625	35.200640
1151.332712	128276.289599	35.205658
1152.318805	128495.666551	35.210676
1153.539040	128698.628345	35.215693
1154.705183	128924.932129	35.220711
1155.804421	129143.343163	35.225728
1156.945918	129340.572839	35.230746
1157.979130	129561.407034	35.235764
1159.418761	129771.926938	35.240781
1160.470727	129991.466261	35.245799
1161.339606	130204.577175	35.250816
1163.138447	130418.279471	35.255834
1163.687781	130629.082535	35.260852
1165.132164	130839.670382	35.265869
1166.734387	131044.334507	35.270887
1167.547894	131245.050123	35.275904
1168.811374	131438.844504	35.280922
1170.175374	131638.828656	35.285940
1171.117802	131829.008079	35.290957
1172.346302	132023.026242	35.295975
1173.302468	132217.202097	35.300992
1174.773230	132420.852812	35.306010
1175.908197	132618.897874	35.311028
1176.815466	132816.992162	35.316045
1177.640032	133021.533523	35.321063
1179.258844	133232.448207	35.326080
1180.296193	133431.920665	35.331098
1181.500468	133634.019891	35.336116
1182.677048	133848.014026	35.341133
1183.810126	134052.093100	35.346151
1184.979122	134267.067494	35.351168
1186.216602	134471.753909	35.356186
1187.419171	134686.395137	35.361204
1188.677495	134898.972984	35.366221
1190.208119	135100.342513	35.371239
1191.908790	135311.482597	35.376256
1192.955585	135497.385024	35.381274
1195.064283	135693.895434	35.386292
1196.294473	135871.509762	35.391309
1197.667674	136066.436508	35.396327
1198.454965	136264.729763	35.401344
1199.915751	136456.433955	35.406362
1201.102469	136655.567347	35.411380
1202.139942	136835.233269	35.416397
1203.300285	137039.752971	35.421415
1204.208489	137244.021179	35.426432
1205.446796	137444.304689	35.431450
1206.382431	137657.504234	35.436468
1207.211277	137858.513515	35.441485
1208.414500	138073.855787	35.446503
1209.712246	138291.481198	35.451520
1210.909825	138499.618222	35.456538
1211.760835	138717.099804	35.461556
1212.565649	138937.356145	35.466573
1214.124516	139149.436983	35.471591
1215.014613	139379.263383	35.476608
1216.039782	139602.660971	35.481626
1216.984174	139830.349022	35.486644
1217.980859	140076.698104	35.491661
1219.531171	140299.090317	35.496679
1220.380466	140534.741070	35.501696
1221.553147	140768.692527	35.506714
1222.819904	141017.034704	35.511732
1224.396592	141253.552307	35.516749
1225.281173	141495.382778	35.521767
1226.590177	141732.541100	35.526784
1228.119172	141963.675855	35.531802
1228.980952	142211.503723	35.536820
1230.433372	142449.315707	35.541837
1231.617148	142687.500871	35.546855
1233.027898	142935.868329	35.551872
1234.037736	143178.080914	35.556890
1235.585728	143421.339993	35.561908
1236.424381	143665.079360	35.566925
1238.048429	143898.480094	35.571943
1239.152776	144146.952320	35.576960
1240.454429	144379.200034	35.581978
1241.824536	144639.614234	35.586996
1242.366359	144878.912997	35.592013
1243.963894	145126.665545	35.597031
1245.439012	145377.941493	35.602048
1246.984433	145617.492772	35.607066
1248.399586	145856.012108	35.612084
1249.750057	146081.698054	35.617101
1250.702208	146302.002316	35.622119
1251.805471	146532.552033	35.627136
1253.224365	146756.770589	35.632154
1254.359590	146985.489598	35.637172
1255.279471	147206.602382	35.642189
1257.221296	147449.120929	35.647207
1258.345336	147673.110341	35.652224
1259.559515	147900.005930	35.657242
1260.420575	148138.825551	35.662260
1261.883212	148368.794001	35.667277
1262.638477	148607.606910	35.672295
1263.736727	148849.197734	35.677312
1265.457382	149085.564234	35.682330
1266.845920	149324.166979	35.687348
1267.930077	149569.431563	35.692365
1269.744927	149799.376418	35.697383
1271.405749	150031.389979	35.702400
1272.836163	150270.815417	35.707418
1274.192686	150500.720753	35.712436
1274.993454	150740.449912	35.717453
1276.529478	150973.883299	35.722471
1276.923185	151212.675456	35.727488
1278.886742	151450.994423	35.732506
1280.220248	151689.958871	35.737524
1281.221778	151939.004338	35.742541
1282.562799	152189.698740	35.747559
1283.284103	152438.003288	35.752576
1284.955434	152674.253373	35.757594
1286.341525	152925.388298	35.762612
1287.623219	153177.568895	35.767629
1288.931752	153428.680114	35.772647
1290.207467	153682.514118	35.777664
1291.375681	153926.781996	35.782682
1293.175197	154177.096091	35.787700
1294.195593	154421.325745	35.792717
1295.754994	154664.811958	35.797735
1297.183639	154922.829324	35.802752
1298.291028	155167.277010	35.807770
1299.685172	155414.156258	35.812788
1301.191444	155661.831447	35.817805
1302.913932	155906.033607	35.822823
1303.786761	156158.837101	35.827840
1305.330412	156401.660204	35.832858
1306.431355	156640.135831	35.837876
1307.656101	156895.286685	35.842893
1308.870901	157140.601681	35.847911
1310.218967	157400.051631	35.852928
1311.388385	157647.787834	35.857946
1312.917050	157898.731436	35.862964
1314.466335	158157.607260	35.867981
1315.668215	158400.834715	35.872999
1317.147703	158656.651369	35.878016
1318.646076	158894.984828	35.883034
1319.998896	159139.905443	35.888052
1321.095724	159390.249914	35.893069
1322.577530	159639.367161	35.898087
1323.328411	159897.423133	35.903104
1324.596323	160144.519222	35.908122
1325.900177	160403.392100	35.913140
1326.881765	160661.821360	35.918157
1328.485533	160915.025255	35.923175
1329.022901	161183.669980	35.928192
1330.781933	161450.182162	35.933210
1331.770692	161713.299295	35.938228
1333.022195	161981.695932	35.943245
1334.821428	162240.320988	35.948263
1335.792450	162520.850249	35.953280
1337.138114	162772.159387	35.958298
1338.169669	163022.198271	35.963316
1339.415494	163284.367417	35.968333
1340.676856	163550.407497	35.973351
1341.830816	163815.678294	35.978368
1342.990859	164081.304692	35.983386
1344.794963	164354.537981	35.988404
1345.793258	164612.980317	35.993421
1347.221276	164878.682196	35.998439
1348.781445	165156.070551	36.003456
1350.242733	165437.208286	36.008474
1351.683624	165709.577059	36.013492
1352.703209	165978.127703	36.018509
1354.415279	166266.161922	36.023527
1355.225367	166529.859295	36.028544
1357.170393	166806.102155	36.033562
1358.942662	167075.593061	36.038580
1359.701976	167354.639222	36.043597
1361.167751	167629.576384	36.048615
1362.058855	167921.910499	36.053632
1363.364716	168192.862637	36.058650
1365.073497	168475.611770	36.063668
1366.702063	168773.065110	36.068685
1367.871427	169058.770507	36.073703
1369.090263	169341.713993	36.078720
1370.552865	169631.781664	36.083738
1371.553796	169913.720293	36.088756
1372.861979	170217.260877	36.093773
1374.518141	170504.520962	36.098791
1375.819239	170801.576670	36.103808
1376.970483	171103.812194	36.108826
1378.706478	171403.989281	36.113844
1379.592757	171706.598823	36.118861
1381.248741	172003.832260	36.123879
1382.306339	172313.591557	36.128896
1383.547829	172621.304372	36.133914
1385.098593	172936.271231	36.138932
1386.744369	173238.501244	36.143949
1387.988202	173551.944089	36.148967
1389.185598	173869.865124	36.153984
1390.538394	174174.595281	36.159002
1391.997642	174493.303184	36.164020
1393.732159	174805.366253	36.169037
1395.292240	175122.156142	36.174055
1396.565788	175434.090608	36.179072
1397.686366	175756.107214	36.184090
1398.897722	176070.403002	36.189108
1400.566970	176391.942553	36.194125
1402.584834	176705.098630	36.199143
1404.074311	177014.452857	36.204160
1405.844262	177318.430951	36.209178
1406.947506	177626.501821	36.214196
1408.176291	177946.617792	36.219213
1409.700436	178260.491792	36.224231
1411.100981	178571.846538	36.229248
1413.488130	178863.568147	36.234266
1415.053077	179166.238751	36.239284
1416.472779	179462.228159	36.244301
1417.803001	179766.385208	36.249319
1419.548789	180071.519549	36.254336
1420.737653	180370.722802	36.259354
1422.024228	180660.006553	36.264372
1422.722633	180960.533002	36.269389
1424.010622	181271.609947	36.274407
1425.557297	181584.272926	36.279424
1426.986923	181892.942346	36.284442
1428.062869	182198.950512	36.289460
1429.284484	182510.422924	36.294477
1430.881704	182799.309087	36.299495
1432.206604	183104.417636	36.304512
1433.481491	183413.370171	36.309530
1434.966433	183714.214006	36.314548
1436.022556	184022.008958	36.319565
1437.142098	184319.457589	36.324583
1438.690449	184631.596792	36.329600
1439.409341	184958.598239	36.334618
1441.312619	185280.081543	36.339636
1442.536452	185607.158435	36.344653
1444.301619	185937.021755	36.349671
1445.702841	186255.360971	36.354688
1447.223854	186574.444388	36.359706
1449.003410	186898.923801	36.364724
1450.246815	187222.345137	36.369741
1451.360493	187618.430865	36.374759
1452.846980	187951.011025	36.379776
1454.270344	188287.335853	36.384794
1456.375430	188611.947235	36.389812
1457.817291	188940.676569	36.394829
1459.226333	189266.033788	36.399847
1460.971093	189600.381848	36.404864
1461.921687	189934.042374	36.409882
1463.686679	190265.087167	36.414900
1465.480240	190603.316730	36.419917
1466.849900	190926.449548	36.424935
1468.872621	191233.148504	36.429952
1470.644115	191564.703920	36.434970
1472.441105	191878.958417	36.439988
1473.868678	192210.645621	36.445005
1475.642259	192523.457587	36.450023
1477.186521	192856.982508	36.455040
1478.364793	193170.422678	36.460058
1480.433232	193476.993039	36.465076
1481.556349	193802.407241	36.470093
1483.198703	194120.654085	36.475111
1484.806439	194427.044783	36.480128
1485.952327	194757.893633	36.485146
1487.547326	195079.020524	36.490164
1488.297227	195398.832569	36.495181
1489.872230	195726.339848	36.500199
1491.345603	196050.866437	36.505216
1492.922558	196390.491463	36.510234
1494.387760	196708.975288	36.515252
1495.535627	197045.493837	36.520269
1496.984788	197379.273431	36.525287
1498.709072	197727.286504	36.530304
1499.878554	198080.619996	36.535322
1501.276129	198411.056943	36.540340
1502.596986	198766.781520	36.545357
1503.914432	199106.910637	36.550375
1505.472951	199457.747820	36.555392
1506.822858	199816.721695	36.560410
1508.226132	200166.517845	36.565428
1509.873419	200525.472149	36.570445
1511.221942	200876.065847	36.575463
1512.703901	201239.467555	36.580480
1513.988183	201602.926380	36.585498
1515.764645	201948.349432	36.590516
1517.319230	202313.316979	36.595533
1518.887602	202681.814064	36.600551
1520.347302	203028.152469	36.605568
1521.843556	203398.948517	36.610586
1523.113739	203764.420720	36.615604
1524.967740	204134.501752	36.620621
1526.678345	204493.606541	36.625639
1528.318801	204846.727901	36.630656
1529.917401	205208.493401	36.635674
1531.297721	205550.200019	36.640692
1533.220434	205896.979104	36.645709
1534.231654	206232.393869	36.650727
1535.954898	206574.175486	36.655744
1537.444554	206914.851057	36.660762
1538.977465	207257.959074	36.665780
1540.326816	207600.461260	36.670797
1542.313579	207945.810957	36.675815
1543.767409	208290.050617	36.680832
1544.761473	208643.076034	36.685850
1546.642207	208983.032920	36.690868
1548.266459	209343.048211	36.695885
1550.281488	209680.393874	36.700903
1551.931144	210031.108520	36.705920
1553.699051	210379.747440	36.710938
1555.467625	210716.726520	36.715956
1556.695844	211072.106471	36.720973
1557.884751	211420.659470	36.725991
1559.243126	211766.137933	36.731008
1560.787741	212136.737162	36.736026
1562.258231	212492.436526	36.741044
1563.805578	212864.966851	36.746061
1565.108853	213217.136669	36.751079
1566.738255	213584.040746	36.756096
1568.247421	213958.331094	36.761114
1570.003707	214321.913589	36.766132
1571.687502	214703.163385	36.771149
1572.939444	215073.074849	36.776167
1574.631762	215455.035340	36.781184
1575.845819	215840.754583	36.786202
1577.541228	216216.161086	36.791220
1579.038731	216597.568780	36.796237
1580.557542	216980.853331	36.801255
1582.061075	217378.315944	36.806272
1583.285725	217777.931031	36.811290
1584.983948	218176.354518	36.816308
1586.806274	218565.359395	36.821325
1588.158183	218962.669024	36.826343
1590.095446	219361.919604	36.831360
1591.332348	219760.035223	36.836378
1593.541054	220154.010535	36.841396
1595.414828	220544.786742	36.846413
1596.575508	220941.720884	36.851431
1598.538253	221343.305624	36.856448
1600.281969	221735.245853	36.861466
1601.926551	222132.917639	36.866484
1603.714651	222530.719508	36.871501
1605.430872	222920.327215	36.876519
1607.342359	223304.163126	36.881536
1608.714045	223693.774099	36.886554
1610.456062	224083.276363	36.891572
1612.470684	224480.738292	36.896589
1613.896051	224863.253249	36.901607
1615.290769	225244.909275	36.906624
1616.727412	225631.690364	36.911642
1618.660567	226011.305994	36.916660
1620.108886	226408.475480	36.921677
1621.625096	226806.345610	36.926695
1623.586502	227199.090593	36.931712
1624.931053	227600.493210	36.936730
1626.699250	227997.129681	36.941748
1628.329546	228388.478177	36.946765
1629.362820	228770.799934	36.951783
1631.066371	229162.949645	36.956800
1632.864978	229572.308262	36.961818
1634.486748	229966.147117	36.966836
1635.888296	230366.015600	36.971853
1637.545016	230762.566832	36.976871
1639.472309	231137.964801	36.981888
1640.822478	231515.434393	36.986906
1642.383059	231906.563563	36.991924
1643.962607	232295.199929	36.996941
1645.470042	232683.847319	37.001959
1646.904217	233055.358267	37.006976
1648.350982	233459.155306	37.011994
1650.364236	233840.380951	37.017012
1651.868020	234245.946680	37.022029
1653.403488	234633.089324	37.027047
1655.406561	235018.380179	37.032064
1656.783987	235426.250918	37.037082
1658.657201	235825.152344	37.042100
1660.191030	236229.517459	37.047117
1662.284080	236630.238102	37.052135
1664.201591	237014.524200	37.057152
1665.352098	237417.245916	37.062170
1667.696764	237809.415601	37.067188
1669.350444	238205.757518	37.072205
1670.496428	238622.780646	37.077223
1672.380086	239022.260966	37.082240
1674.041489	239439.100686	37.087258
1675.383472	239839.985633	37.092276
1676.815866	240247.968803	37.097293
1678.349320	240663.785178	37.102311
1680.232663	241089.555044	37.107328
1681.718378	241524.455395	37.112346
1683.089663	241930.794280	37.117364
1685.229708	242365.514544	37.122381
1686.883252	242797.464997	37.127399
1688.815482	243215.069102	37.132416
1690.541551	243642.865913	37.137434
1692.255008	244073.026348	37.142452
1693.815409	244505.648561	37.147469
1695.344527	244931.314398	37.152487
1697.251952	245355.091154	37.157504
1698.987441	245805.693852	37.162522
1700.959446	246235.174264	37.167540
1702.369658	246671.117708	37.172557
1703.750962	247110.468624	37.177575
1705.748226	247552.186159	37.182592
1708.301436	247980.250706	37.187610
1710.239126	248405.997325	37.192628
1711.740510	248845.096620	37.197645
1713.469159	249273.820504	37.202663
1715.393427	249704.062229	37.207680
1716.556455	250134.320360	37.212698
1717.706966	250577.966221	37.217716
1719.735520	251014.030664	37.222733
1720.975132	251473.079115	37.227751
1722.970483	251916.004770	37.232768
1724.348312	252368.272029	37.237786
1726.015657	252815.310673	37.242804
1727.993725	253270.885095	37.247821
1729.608189	253725.244912	37.252839
1731.906502	254168.649843	37.257856
1733.383086	254625.771717	37.262874
1734.967145	255093.086594	37.267892
1736.383503	255543.686710	37.272909
1738.297616	255999.516264	37.277927
1740.091706	256444.389778	37.282944
1742.105574	256908.633723	37.287962
1743.772140	257363.201809	37.292980
1745.516699	257813.920545	37.297997
1747.039350	258275.518479	37.303015
1749.208491	258726.675479	37.308032
1750.652526	259186.555046	37.313050
1752.197414	259633.589869	37.318068
1754.137477	260083.253601	37.323085
1755.335711	260514.972142	37.328103
1757.608439	260958.814586	37.333120
1759.437765	261408.820692	37.338138
1761.260626	261848.031053	37.343156
1762.929229	262280.761470	37.348173
1764.828708	262735.348609	37.353191
1766.148752	263171.228813	37.358208
1767.801488	263622.828281	37.363226
1769.373166	264073.219344	37.368244
1771.241097	264532.274070	37.373261
1772.674305	264990.861411	37.378279
1774.238210	265456.461788	37.383296
1775.922718	265925.495411	37.388314
1777.951647	266404.556273	37.393332
1779.926168	266858.935806	37.398349
1781.515266	267325.717252	37.403367
1783.463315	267783.423831	37.408384
1785.642403	268269.208017	37.413402
1787.721105	268737.556865	37.418420
1789.741846	269199.994693	37.423437
1791.100088	269670.534237	37.428455
1793.013607	270149.111778	37.433472
1794.857848	270625.818212	37.438490
1796.301704	271108.476998	37.443508
1798.358550	271575.849599	37.448525
1799.645086	272063.302507	37.453543
1801.659473	272552.568976	37.458560
1803.288744	273044.458025	37.463578
1804.836294	273533.842741	37.468596
1806.830550	274032.373716	37.473613
1808.425322	274527.230941	37.478631
1810.087182	275025.401634	37.483648
1811.663343	275528.585763	37.488666
1813.849101	276040.229853	37.493684
1815.740110	276550.951762	37.498701
1817.045174	277055.235375	37.503719
1819.393735	277568.647251	37.508736
1821.202183	278088.133574	37.513754
1822.647041	278597.794553	37.518772
1824.802884	279112.927794	37.523789
1826.722797	279632.665527	37.528807
1828.584197	280142.377906	37.533824
1830.467267	280658.939920	37.538842
1832.605542	281174.391813	37.543860
1834.962342	281685.590436	37.548877
1836.657822	282198.768079	37.553895
1838.421863	282712.769313	37.558912
1840.253434	283224.470832	37.563930
1841.963853	283736.847815	37.568948
1844.302879	284254.455255	37.573965
1845.930019	284777.401179	37.578983
1847.600521	285289.747505	37.584000
1849.895055	285803.972949	37.589018
1851.560911	286319.206968	37.594036
1853.628727	286817.005794	37.599053
1855.572390	287336.175053	37.604071
1857.371082	287837.055342	37.609088
1860.015015	288339.780075	37.614106
1861.641053	288844.056702	37.619124
1863.749815	289327.661487	37.624141
1865.825177	289835.744848	37.629159
1867.515535	290345.103125	37.634176
1869.235285	290845.870610	37.639194
1870.962734	291342.519597	37.644212
1872.844519	291840.562294	37.649229
1875.187295	292342.438878	37.654247
1877.051266	292832.097541	37.659264
1878.738242	293300.020982	37.664282
1880.560038	293784.600554	37.669300
1882.196333	294256.231293	37.674317
1884.144048	294734.664585	37.679335
1885.935815	295207.202775	37.684352
1887.548593	295684.893646	37.689370
1888.995862	296169.740623	37.694388
1890.920727	296658.570895	37.699405
1892.419917	297158.558140	37.704423
1893.859298	297667.918420	37.709440
1895.732667	298177.256961	37.714458
1897.158429	298694.023216	37.719476
1898.864977	299205.815636	37.724493
1900.424187	299737.275758	37.729511
1902.443210	300265.536225	37.734528
1904.314750	300805.543113	37.739546
1905.965325	301343.370584	37.744564
1907.796693	301888.983196	37.749581
1909.278522	302446.068396	37.754599
1910.936388	303000.987814	37.759616
1912.802411	303557.848819	37.764634
1914.702853	304134.574719	37.769652
1916.307322	304706.009762	37.774669
1918.401893	305280.788616	37.779687
1920.368880	305866.851380	37.784704
1922.312915	306449.560312	37.789722
1924.113607	307039.163774	37.794740
1926.144544	307618.139538	37.799757
1927.985704	308218.155068	37.804775
1929.799977	308814.461654	37.809792
1931.952599	309414.921429	37.814810
1933.959189	310009.914154	37.819828
1936.435161	310599.622886	37.824845
1937.879920	311200.678745	37.829863
1940.345828	311798.521520	37.834880
1942.475751	312404.860961	37.839898
1944.237813	313007.722261	37.844916
1946.695194	313601.177939	37.849933
1948.514373	314200.639251	37.854951
1950.753804	314797.108364	37.859968
1952.677059	315389.660037	37.864986
1954.608469	315990.171503	37.870004
1956.882158	316585.342735	37.875021
1958.571310	317192.017484	37.880039
1960.850810	317794.277399	37.885056
1962.540883	318385.785283	37.890074
1964.308257	318996.204120	37.895092
1966.617443	319604.144231	37.900109
1968.544916	320206.806541	37.905127
1970.497947	320811.613318	37.910144
1972.819806	321411.684752	37.915162
1974.869087	322015.317448	37.920180
1977.212480	322613.110068	37.925197
1979.731208	323202.518593	37.930215
1982.102751	323783.949024	37.935232
1984.315984	324359.737752	37.940250
1986.637728	324951.765622	37.945268
1988.818860	325513.562552	37.950285
1990.839282	326080.552833	37.955303
1992.571658	326660.342377	37.960320
1994.878014	327224.962950	37.965338
1996.614167	327802.908597	37.970356
1998.722936	328384.212617	37.975373
2000.547874	328954.287936	37.980391
2002.553153	329513.341447	37.985408
2004.285639	330083.643123	37.990426
2006.371255	330663.420106	37.995444
2008.296493	331228.651604	38.000461
2010.196256	331780.839233	38.005479
2011.901226	332339.264614	38.010496
2014.037868	332889.014498	38.015514
2015.498033	333447.284288	38.020532
2017.587032	334002.834582	38.025549
2019.196350	334566.213947	38.030567
2021.057359	335129.520045	38.035584
2023.228273	335698.375001	38.040602
2024.851805	336278.011149	38.045620
2026.852967	336858.010260	38.050637
2028.710027	337439.341668	38.055655
2030.777525	338025.247174	38.060672
2032.981601	338610.690610	38.065690
2034.525914	339197.495904	38.070708
2036.480153	339796.706139	38.075725
2038.829822	340395.362507	38.080743
2040.474175	341009.412594	38.085760
2042.415727	341612.068676	38.090778
2044.562205	342230.355711	38.095796
2046.734417	342840.512197	38.100813
2048.669237	343450.289294	38.105831
2050.912423	344073.549656	38.110848
2052.824732	344689.927249	38.115866
2054.586311	345326.046731	38.120884
2056.790189	345953.640618	38.125901
2059.037173	346581.647162	38.130919
2060.965700	347213.394000	38.135936
2062.815031	347852.951308	38.140954
2064.866428	348498.322094	38.145972
2067.236631	349129.430852	38.150989
2069.575475	349771.384671	38.156007
2071.379950	350418.176272	38.161024
2073.705961	351051.283227	38.166042
2076.108709	351701.530641	38.171060
2077.711487	352357.087587	38.176077
2080.067798	352997.301251	38.181095
2082.483500	353639.140672	38.186112
2084.645625	354285.189876	38.191130
2086.678732	354924.401052	38.196148
2088.976987	355573.622142	38.201165
2091.390154	356219.059840	38.206183
2093.564596	356871.011101	38.211200
2095.495820	357510.742787	38.216218
2097.669026	358160.081300	38.221236
2099.835714	358794.806282	38.226253
2102.190437	359437.093014	38.231271
2104.062410	360076.906901	38.236288
2106.182542	360726.984587	38.241306
2108.598372	361378.852209	38.246324
2110.729392	362009.003425	38.251341
2112.644075	362657.981332	38.256359
2114.710434	363311.052459	38.261376
2116.720001	363958.263475	38.266394
2118.750164	364609.359884	38.271412
2120.761323	365266.476367	38.276429
2123.157000	365917.511648	38.281447
2125.323822	366569.961858	38.286464
2127.304067	367219.790949	38.291482
2129.208775	367876.991252	38.296500
2131.611972	368530.550783	38.301517
2133.888035	369177.780239	38.306535
2135.953029	369859.235483	38.311552
2138.699709	370486.799532	38.316570
2140.796005	371142.145463	38.321588
2142.903670	371786.933908	38.326605
2145.613642	372426.647143	38.331623
2147.757058	373071.070667	38.336640
2149.880822	373697.696666	38.341658
2152.029556	374313.410403	38.346676
2154.193324	374922.495612	38.351693
2156.588546	375531.226927	38.356711
2158.551021	376134.210923	38.361728
2160.657817	376739.616088	38.366746
2162.984321	377355.182005	38.371764
2164.650855	377968.151833	38.376781
2166.889314	378578.029010	38.381799
2168.964468	379199.290967	38.386816
2170.711208	379819.145867	38.391834
2172.750980	380447.172234	38.396852
2174.681617	381085.635905	38.401869
2177.129567	381709.034248	38.406887
2178.856874	382355.806041	38.411904
2181.362283	382989.143461	38.416922
2182.972624	383648.184501	38.421940
2184.955179	384297.400122	38.426957
2186.820751	384955.405165	38.431975
2188.818619	385620.868356	38.436992
2191.050070	386289.594847	38.442010
2192.958207	386973.497077	38.447028
2194.803351	387662.151028	38.452045
2197.403215	388338.361810	38.457063
2199.740061	389032.167782	38.462080
2202.131738	389730.731170	38.467098
2204.147139	390421.282155	38.472116
2206.264035	391108.151988	38.477133
2208.388408	391810.445116	38.482151
2210.549457	392510.484350	38.487168
2212.815788	393209.676774	38.492186
2214.970755	393919.397581	38.497204
2217.589300	394632.518331	38.502221
2220.095865	395337.484251	38.507239
2222.181204	396053.227991	38.512256
2224.636526	396748.186696	38.517274
2227.116048	397464.129859	38.522292
2229.228087	398178.640687	38.527309
2231.567574	398885.399861	38.532327
2234.145153	399594.327600	38.537344
2236.446229	400303.530042	38.542362
2239.382785	401005.170835	38.547380
2241.699918	401702.331887	38.552397
2243.868000	402408.251046	38.557415
2246.182419	403106.635086	38.562432
2248.120887	403813.508284	38.567450
2250.727697	404513.878307	38.572468
2252.876066	405228.265650	38.577485
2255.060318	405922.939476	38.582503
2257.081610	406639.427185	38.587520
2259.286816	407340.834487	38.592538
2261.840747	408058.053455	38.597556
2263.902338	408762.575454	38.602573
2266.601569	409469.252042	38.607591
2268.804997	410180.536995	38.612608
2271.342333	410887.041412	38.617626
2273.850255	411588.316579	38.622644
2276.249528	412289.434316	38.627661
2278.576042	412990.540703	38.632679
2280.729528	413684.164498	38.637696
2282.785961	414386.481701	38.642714
2285.340985	415091.834017	38.647732
2287.371698	415799.774078	38.652749
2290.071032	416498.329775	38.657767
2292.468094	417192.205875	38.662784
2294.919946	417900.515494	38.667802
2297.221759	418609.077547	38.672820
2299.796471	419300.630830	38.677837
2302.432934	419967.573645	38.682855
2304.521206	420644.897075	38.687872
2306.803597	421305.025260	38.692890
2308.875925	421967.541801	38.697908
2311.476672	422616.048881	38.702925
2313.886218	423270.835209	38.707943
2316.543576	423916.359472	38.712960
2318.371237	424565.683932	38.717978
2321.201858	425221.099988	38.722996
2322.673837	425886.667046	38.728013
2325.037561	426544.994852	38.733031
2326.898991	427217.130247	38.738048
2329.067939	427888.032250	38.743066
2331.715671	428569.755638	38.748084
2333.338701	429255.912536	38.753101
2335.327463	429938.854538	38.758119
2337.607308	430642.198099	38.763136
2339.659465	431342.367882	38.768154
2341.794402	432052.153091	38.773172
2343.356575	432771.806747	38.778189
2345.961543	433497.031950	38.783207
2348.279347	434228.794033	38.788224
2350.196649	434962.258646	38.793242
2352.467700	435700.945810	38.798260
2354.715881	436468.965930	38.803277
2356.864618	437208.776202	38.808295
2359.449026	437978.148237	38.813312
2361.419320	438736.823548	38.818330
2364.110039	439497.477616	38.823348
2366.744068	440268.415822	38.828365
2368.844742	441036.172634	38.833383
2371.477619	441810.432185	38.838400
2374.452194	442579.453712	38.843418
2377.171547	443357.827861	38.848436
2379.696078	444132.259979	38.853453
2381.922362	444894.533974	38.858471
2384.639634	445666.042918	38.863488
2387.212749	446437.188326	38.868506
2389.357310	447205.287579	38.873524
2391.782464	447981.996188	38.878541
2394.659513	448753.399629	38.883559
2397.032278	449524.041017	38.888576
2399.322011	450294.308877	38.893594
2401.908591	451070.202503	38.898612
2404.443557	451847.938480	38.903629
2406.425299	452619.517239	38.908647
2408.643839	453415.358245	38.913664
2411.065821	454197.249282	38.918682
2413.600874	454980.299347	38.923700
2415.820732	455774.569472	38.928717
2418.062454	456550.326517	38.933735
2420.649569	457344.820948	38.938752
2423.142216	458142.725666	38.943770
2425.624552	458924.899843	38.948788
2427.661777	459724.821279	38.953805
2430.468369	460518.680962	38.958823
2433.245049	461330.825487	38.963840
2435.325430	462119.224136	38.968858
2437.666312	462923.590250	38.973876
2439.700183	463731.396940	38.978893
2442.510567	464533.695705	38.983911
2444.862850	465326.745335	38.988928
2447.019854	466143.497450	38.993946
2449.306835	466947.578433	38.998964
2452.025248	467763.255319	39.003981
2454.543693	468572.114143	39.008999
2457.190931	469386.309831	39.014016
2459.256473	470203.279612	39.019034
2461.927933	470998.680799	39.024052
2464.863448	471792.640397	39.029069
2467.381774	472549.210411	39.034087
2469.966719	473333.114819	39.039104
2471.848921	474107.611976	39.044122
2474.918765	474885.718020	39.049140
2477.139994	475666.792863	39.054157
2479.415655	476439.704486	39.059175
2481.785511	477221.234754	39.064192
2484.090279	478016.750536	39.069210
2486.911950	478794.503346	39.074228
2489.095077	479582.701007	39.079245
2491.531594	480382.159961	39.084263
2494.225879	481181.537938	39.089280
2496.347501	481981.015094	39.094298
2499.140549	482776.516391	39.099316
2501.775035	483590.747311	39.104333
2503.930492	484383.494567	39.109351
2506.992410	485202.915067	39.114368
2509.244369	486005.842637	39.119386
2511.978397	486817.419067	39.124404
2514.696356	487620.441150	39.129421
2517.227408	488441.585293	39.134439
2519.761964	489266.210652	39.139456
2522.247235	490081.883459	39.144474
2524.860209	490896.484954	39.149492
2527.422666	491720.216615	39.154509
2529.697430	492550.998715	39.159527
2532.400505	493378.293711	39.164544
2535.080081	494204.942261	39.169562
2538.091035	495031.090230	39.174580
2540.346346	495867.229359	39.179597
2542.692214	496696.761883	39.184615
2545.467798	497533.077711	39.189632
2547.585091	498367.737268	39.194650
2550.388673	499206.369700	39.199668
2552.631546	500046.904071	39.204685
2555.411498	500893.043848	39.209703
2557.977324	501742.237878	39.214720
2560.188151	502602.811457	39.219738
2562.694297	503453.474281	39.224756
2565.096266	504304.253986	39.229773
2567.550903	505170.422538	39.234791
2570.227431	506034.692485	39.239808
2572.668422	506916.153416	39.244826
2575.280743	507790.087073	39.249844
2577.925692	508661.345700	39.254861
2580.238070	509545.932616	39.259879
2583.223963	510422.964482	39.264896
2585.937210	511302.850912	39.269914
2588.398091	512171.053350	39.274932
2590.848082	513055.899522	39.279949
2593.653933	513940.080413	39.284967
2596.886841	514822.730002	39.289984
2599.334181	515703.585519	39.295002
2602.249081	516573.099646	39.300020
2604.753217	517462.933364	39.305037
2607.086551	518341.977893	39.310055
2609.634224	519227.366294	39.315072
2612.582967	520108.562776	39.320090
2615.354580	520989.025854	39.325108
2617.468473	521863.603892	39.330125
2619.939052	522755.909397	39.335143
2622.929955	523637.370667	39.340160
2625.334994	524529.819272	39.345178
2627.985136	525414.884314	39.350196
2630.770536	526306.500910	39.355213
2633.076040	527191.601598	39.360231
2635.766748	528066.987947	39.365248
2638.717442	528928.713067	39.370266
2641.398158	529788.665776	39.375284
2644.022478	530652.086375	39.380301
2646.414345	531507.249903	39.385319
2648.474289	532348.147290	39.390336
2651.118786	533229.622286	39.395354
2653.268608	534091.482111	39.400372
2655.788849	534955.033768	39.405389
2658.314342	535835.947244	39.410407
2661.279685	536719.542506	39.415424
2663.691361	537616.364927	39.420442
2666.228174	538507.884444	39.425460
2668.684794	539401.813124	39.430477
2671.347542	540314.315622	39.435495
2673.734369	541220.321663	39.440512
2676.171351	542133.781375	39.445530
2679.402092	543047.401574	39.450548
2681.766966	543975.840765	39.455565
2684.229748	544909.162023	39.460583
2687.321769	545841.712733	39.465600
2689.557434	546785.613110	39.470618
2692.272454	547730.620212	39.475636
2694.830226	548691.427434	39.480653
2697.408386	549641.073364	39.485671
2700.074048	550595.596126	39.490688
2702.849090	551563.364386	39.495706
2705.767986	552525.818824	39.500724
2708.253499	553502.151233	39.505741
2710.975521	554482.428078	39.510759
2714.038301	555450.140909	39.515776
2716.246744	556437.957374	39.520794
2719.058401	557420.786743	39.525812
2721.872613	558417.716341	39.530829
2724.585837	559407.362549	39.535847
2727.625158	560390.361584	39.540864
2730.703206	561388.102115	39.545882
2733.369037	562386.824406	39.550900
2736.080417	563383.150364	39.555917
2738.660697	564392.434432	39.560935
2741.628684	565400.468671	39.565952
2743.960286	566404.258358	39.570970
2746.846708	567409.676944	39.575988
2749.401724	568420.317061	39.581005
2752.013446	569444.477166	39.586023
2754.780435	570458.809897	39.591040
2758.126747	571477.116701	39.596058
2760.816532	572497.487312	39.601076
2763.952837	573514.643636	39.606093
2766.493553	574546.614280	39.611111
2769.509771	575553.047166	39.616128
2772.219147	576570.245249	39.621146
2775.252535	577595.555209	39.626164
2778.229160	578616.327946	39.631181
2781.029185	579634.133750	39.636199
2783.636154	580638.422564	39.641216
2786.560913	581666.775740	39.646234
2789.069483	582682.946925	39.651252
2792.508825	583712.979152	39.656269
2794.789670	584732.896676	39.661287
2797.678574	585751.674289	39.666304
2800.270532	586776.101793	39.671322
2803.335406	587802.058326	39.676340
2806.197417	588823.651496	39.681357
2808.566433	589860.566956	39.686375
2811.819357	590875.758239	39.691392
2814.151383	591912.082203	39.696410
2816.870758	592947.296212	39.701428
2819.758957	593973.491799	39.706445
2822.324741	594972.766454	39.711463
2825.131065	595968.213632	39.716480
2828.041245	596968.994437	39.721498
2830.717278	597962.726149	39.726516
2833.756545	598970.637240	39.731533
2836.522566	599973.202229	39.736551
2839.265133	600981.914954	39.741568
2841.700465	601998.464936	39.746586
2844.280011	603012.647123	39.751604
2846.703223	604024.908149	39.756621
2849.549324	605067.693116	39.761639
2852.198872	606097.729894	39.766656
2855.005590	607148.193991	39.771674
2857.981759	608196.279159	39.776692
2860.816421	609245.825340	39.781709
2863.668952	610292.766926	39.786727
2866.954484	611339.682600	39.791744
2870.319701	612405.575991	39.796762
2872.610149	613475.513794	39.801780
2875.641890	614530.465159	39.806797
2878.292259	615597.977231	39.811815
2881.423005	616660.316028	39.816832
2884.541206	617747.861748	39.821850
2887.320556	618816.803752	39.826868
2890.833043	619896.777076	39.831885
2893.336349	620976.341942	39.836903
2896.567761	622052.685849	39.841920
2899.463487	623132.750145	39.846938
2902.474402	624217.309449	39.851956
2905.423512	625296.031107	39.856973
2907.998320	626386.094965	39.861991
2910.893411	627491.321581	39.867008
2913.637272	628586.937192	39.872026
2916.314778	629683.185643	39.877044
2919.220829	630805.055567	39.882061
2922.142981	631920.919546	39.887079
2925.029932	633033.374834	39.892096
2927.555468	634164.365237	39.897114
2930.608294	635293.994618	39.902132
2933.471918	636426.453946	39.907149
2936.457744	637566.815973	39.912167
2939.210493	638699.467799	39.917184
2942.261480	639860.180166	39.922202
2944.678818	641012.445511	39.927220
2947.990659	642160.451979	39.932237
2950.359892	643320.393874	39.937255
2953.445107	644487.881893	39.942272
2956.355793	645656.641451	39.947290
2958.861137	646834.260158	39.952308
2961.885230	648007.772003	39.957325
2964.756398	649190.645518	39.962343
2967.853367	650370.847383	39.967360
2970.782605	651572.624849	39.972378
2973.645586	652767.848335	39.977396
2976.745236	653949.124583	39.982413
2979.571956	655157.939617	39.987431
2982.561282	656356.540703	39.992448
2985.684954	657566.673137	39.997466
2988.947770	658767.440182	40.002484
2991.915858	659971.465569	40.007501
2994.567296	661181.677797	40.012519
2998.107445	662374.473368	40.017536
3001.383359	663589.566252	40.022554
3004.409589	664790.001363	40.027572
3007.533237	665984.505825	40.032589
3010.582345	667184.659313	40.037607
3014.222005	668378.359590	40.042624
3017.345177	669562.015209	40.047642
3020.256647	670719.377857	40.052660
3023.329911	671857.781842	40.057677
3026.427208	673000.441121	40.062695
3029.979580	674131.880828	40.067712
3033.188329	675269.416132	40.072730
3036.065187	676406.951182	40.077748
3038.704217	677524.268669	40.082765
3041.672188	678672.083384	40.087783
3044.568299	679820.150117	40.092800
3047.337868	680972.535450	40.097818
3050.427431	682122.882328	40.102836
3053.680371	683273.788624	40.107853
3056.286357	684438.639546	40.112871
3059.095293	685605.819442	40.117888
3062.368512	686782.655628	40.122906
3064.591935	687965.374467	40.127924
3068.089423	689150.791198	40.132941
3070.856932	690345.545666	40.137959
3073.877593	691544.091506	40.142976
3076.626882	692756.344105	40.147994
3079.642743	693962.099764	40.153012
3082.832107	695174.320873	40.158029
3085.649524	696406.428066	40.163047
3088.809802	697623.970199	40.168064
3092.097119	698869.559462	40.173082
3095.024258	700102.766690	40.178100
3098.389641	701337.839649	40.183117
3100.741159	702594.453751	40.188135
3103.889886	703847.883333	40.193152
3107.394872	705102.688971	40.198170
3110.086606	706370.302132	40.203188
3113.386634	707635.743060	40.208205
3116.430495	708923.563557	40.213223
3119.687337	710190.328433	40.218240
3123.066175	711472.649345	40.223258
3125.631858	712771.798149	40.228276
3129.136633	714054.958240	40.233293
3132.181087	715354.391044	40.238311
3135.538930	716640.055643	40.243328
3139.060446	717938.044841	40.248346
3142.051476	719235.012143	40.253364
3145.544929	720522.373776	40.258381
3148.576303	721838.153256	40.263399
3151.338814	723121.499352	40.268416
3154.676250	724417.437302	40.273434
3158.005043	725726.444931	40.278452
3161.398789	727030.197064	40.283469
3164.262530	728337.054615	40.288487
3167.889449	729649.272771	40.293504
3171.271661	730947.774338	40.298522
3174.186280	732257.729604	40.303540
3177.873726	733560.795155	40.308557
3180.506259	734869.156029	40.313575
3184.109879	736179.936230	40.318592
3187.558867	737481.417431	40.323610
3190.191348	738790.215951	40.328628
3193.444215	740100.158577	40.333645
3196.794122	741411.227505	40.338663
3200.097533	742714.408239	40.343680
3203.480187	744021.222586	40.348698
3206.499684	745338.609452	40.353716
3209.920536	746643.326227	40.358733
3213.073923	747953.590794	40.363751
3216.235932	749278.089300	40.368768
3219.484738	750589.380294	40.373786
3222.291678	751892.653504	40.378804
3225.369902	753210.896679	40.383821
3228.421287	754516.741824	40.388839
3231.437270	755805.539731	40.393856
3235.282435	757077.114794	40.398874
3237.936330	758360.407177	40.403892
3241.096487	759624.280430	40.408909
3244.140799	760922.231736	40.413927
3247.134924	762196.982346	40.418944
3250.494047	763492.742588	40.423962
3253.853487	764791.492835	40.428980
3257.029128	766085.134541	40.433997
3259.943662	767391.494708	40.439015
3263.321438	768692.300309	40.444032
3266.841882	770001.496432	40.449050
3269.866490	771324.165975	40.454068
3273.306385	772639.669420	40.459085
3276.419785	773971.446258	40.464103
3278.840740	775297.743094	40.469120
3282.156343	776633.952722	40.474138
3285.736444	777991.942238	40.479156
3288.877295	779342.497455	40.484173
3291.971827	780708.271502	40.489191
3294.680491	782073.925706	40.494208
3298.290855	783453.855364	40.499226
3301.574351	784833.306749	40.504244
3305.175924	786214.569674	40.509261
3308.266516	787604.553503	40.514279
3311.705505	788994.971308	40.519296
3315.204831	790389.475827	40.524314
3317.980826	791799.059298	40.529332
3321.428164	793210.672249	40.534349
3324.733662	794625.511687	40.539367
3328.026114	796048.280956	40.544384
3331.518398	797470.658765	40.549402
3334.497683	798910.874345	40.554420
3338.090335	800326.276768	40.559437
3341.273822	801757.497872	40.564455
3344.288697	803212.324896	40.569472
3347.754351	804666.020905	40.574490
3351.162288	806117.643367	40.579508
3354.500094	807572.836796	40.584525
3358.235152	809029.433558	40.589543
3360.998036	810496.445390	40.594560
3364.812888	811963.729171	40.599578
3368.492211	813428.553434	40.604596
3372.475657	814878.898543	40.609613
3375.736703	816352.528758	40.614631
3378.951414	817816.979583	40.619648
3382.444424	819271.525945	40.624666
3385.530722	820750.742528	40.629684
3389.139579	822217.973795	40.634701
3392.541246	823685.663863	40.639719
3395.882707	825163.197846	40.644736
3399.559164	826636.055377	40.649754
3402.886458	828107.351315	40.654772
3406.436184	829579.419701	40.659789
3410.000700	831053.454189	40.664807
3413.316882	832531.721729	40.669824
3416.788228	834002.337576	40.674842
3420.224955	835484.800737	40.679860
3423.895040	836953.209425	40.684877
3427.071756	838428.496823	40.689895
3430.155285	839925.496459	40.694912
3434.037989	841382.425397	40.699930
3437.175698	842867.257742	40.704948
3440.457850	844367.648704	40.709965
3443.919689	845846.264706	40.714983
3447.556790	847327.669953	40.720000
3450.713845	848816.214909	40.725018
3453.971430	850289.405185	40.730023
3456.979977	851721.865041	40.735028
3460.329896	853120.425839	40.740032
3463.358064	854454.440365	40.745037
3466.808308	855726.061536	40.750042
3469.556376	856952.530626	40.755047
3472.180440	858107.092672	40.760052
3475.405859	859210.563278	40.765056
3477.960575	860242.578063	40.770061
3480.387795	861214.013194	40.775066
3483.075673	862129.380980	40.780071
3485.314767	862971.812068	40.785076
3487.828998	863768.568352	40.790080
3489.749162	864501.353268	40.795085
3491.623961	865180.634455	40.800090
3493.821916	865815.259070	40.805095
3495.998609	866387.526587	40.810100
3497.497259	866912.429405	40.815104
3499.079507	867389.089247	40.820109
3500.642514	867808.941633	40.825114
3501.993976	868219.045036	40.830119
3503.272107	868557.211603	40.835124
3504.753579	868862.119751	40.840128
3505.794790	869141.597520	40.845133
3506.959841	869371.044198	40.850138
3507.675037	869586.363724	40.855143
3508.622555	869764.673732	40.860148
3509.298996	869909.723902	40.865152
3510.286849	870043.236992	40.870157
3510.968296	870129.312974	40.875162
3511.260695	870213.421804	40.880167
3511.951181	870270.059582	40.885172
3513.079711	870304.142659	40.890176
3513.131704	870318.996363	40.895181
3513.685840	870314.277567	40.900186
3514.459539	870306.822304	40.905191
3514.701662	870265.866213	40.910196
3515.015409	870211.966742	40.915200
3515.211584	870147.469280	40.920205
3515.751294	870071.915344	40.925210
3515.875215	869977.895351	40.930215
3516.345630	869871.272993	40.935220
3516.494942	869770.200120	40.940224
3516.560619	869650.993444	40.945229
3516.840881	869521.519723	40.950234
3517.182255	869387.883058	40.955239
3517.242735	869238.843379	40.960244
3517.800409	869083.640871	40.965248
3517.830159	868926.972131	40.970253
3518.053165	868759.843386	40.975258
3517.905794	868583.114088	40.980263
3517.666994	868409.965411	40.985268
3518.302619	868225.669046	40.990272
3518.132952	868033.189720	40.995277
3518.377360	867838.997759	41.000282
3518.046069	867639.192573	41.005287
3518.290782	867447.014591	41.010292
3518.331955	867238.640156	41.015296
3517.920209	867037.957152	41.020301
3518.223403	866820.642627	41.025306
3518.252188	866624.800840	41.030311
3517.891495	866415.589632	41.035316
3517.704836	866201.128361	41.040320
3517.763509	865987.489792	41.045325
3517.540036	865775.818891	41.050330
3517.513543	865562.853628	41.055335
3517.415799	865341.971058	41.060340
3517.447134	865128.787196	41.065344
3517.312026	864921.417163	41.070349
3517.206737	864707.755780	41.075354
3517.193846	864503.442542	41.080359
3517.025607	864294.122576	41.085364
3516.956982	864069.224757	41.090368
3516.907217	863862.575444	41.095373
3516.628740	863634.987934	41.100378
3516.825573	863429.250456	41.105383
3516.672010	863213.317858	41.110388
3516.643217	862994.458616	41.115392
3516.342375	862789.742030	41.120397
3516.348476	862570.184525	41.125402
3516.343447	862365.889594	41.130407
3516.108979	862157.854036	41.135412
3515.994849	861942.640071	41.140416
3515.956885	861736.877941	41.145421
3515.449643	861523.449285	41.150426
3515.486234	861322.493278	41.155431
3515.350969	861119.817116	41.160436
3515.622343	860899.670300	41.165440
3515.066591	860709.805182	41.170445
3515.286254	860500.381304	41.175450
3515.167740	860306.180776	41.180455
3515.065429	860100.562911	41.185460
3515.019196	859896.475797	41.190464
3514.735928	859700.346730	41.195469
3514.962244	859502.100779	41.200474
3514.734228	859306.529684	41.205479
3514.371469	859104.977774	41.210484
3514.443200	858910.700022	41.215488
3514.233532	858723.035465	41.220493
3514.129054	858513.009140	41.225498
3513.839497	858317.220401	41.230503
3514.056690	858134.595433	41.235508
3514.048741	857955.384895	41.240512
3513.681135	857768.777607	41.245517
3513.653984	857582.497908	41.250522
3513.835569	857397.630407	41.255527
3513.499021	857211.000101	41.260532
3513.415963	857028.096628	41.265536
3513.034972	856844.653490	41.270541
3512.979320	856660.282990	41.275546
3513.069346	856481.011063	41.280551
3512.642330	856309.166893	41.285556
3512.610416	856133.289207	41.290560
3512.673593	855959.616517	41.295565
3512.477171	855783.947360	41.300570
3512.102447	855612.461194	41.305575
3512.056815	855446.530450	41.310580
3512.176118	855271.667123	41.315584
3511.784158	855125.036687	41.320589
3511.799937	854954.340742	41.325594
3511.967670	854794.550914	41.330599
3511.590940	854631.454752	41.335604
3511.517299	854470.822735	41.340608
3511.219855	854325.802352	41.345613
3511.435241	854156.406461	41.350618
3511.181546	853995.595798	41.355623
3511.330245	853859.881865	41.360628
3511.295638	853703.384132	41.365632
3510.777666	853555.184870	41.370637
3510.619949	853400.053222	41.375642
3510.572388	853249.352764	41.380647
3510.411923	853103.215513	41.385652
3510.538896	852957.610436	41.390656
3510.264121	852816.226997	41.395661
3510.209831	852674.612027	41.400666
3510.077813	852537.168445	41.405671
3509.784197	852397.617055	41.410676
3510.062151	852261.361361	41.415680
3509.833478	852137.961075	41.420685
3510.016431	851990.580286	41.425690
3509.811353	851855.842807	41.430695
3509.577455	851714.910180	41.435700
3509.940852	851590.534302	41.440704
3509.644213	851465.774811	41.445709
3509.697944	851323.238507	41.450714
3509.657252	851195.528378	41.455719
3509.788899	851070.306118	41.460724
3509.362410	850924.542822	41.465728
3509.051162	850803.644735	41.470733
3509.097927	850674.166422	41.475738
3509.033943	850558.938034	41.480743
3509.082410	850428.679267	41.485748
3509.121075	850304.907682	41.490752
3508.571959	850183.162269	41.495757
3508.980612	850064.460581	41.500762
3508.727112	849954.867043	41.505767
3508.237859	849833.201795	41.510772
3508.673965	849714.682389	41.515776
3508.538614	849596.153048	41.520781
3508.129948	849492.580129	41.525786
3508.193273	849379.826788	41.530791
3507.856608	849273.914093	41.535796
3508.066916	849168.010832	41.540800
3507.804150	849061.210950	41.545805
3507.605218	848948.296527	41.550810
3507.958375	848847.014712	41.555815
3507.620109	848738.186476	41.560820
3507.901708	848640.980822	41.565824
3507.652359	848535.331673	41.570829
3507.633821	848418.406973	41.575834
3507.341879	848321.866914	41.580839
3507.413786	848222.555775	41.585844
3507.593703	848126.713760	41.590848
3507.217673	848036.576232	41.595853
3507.179141	847931.658257	41.600858
3506.969513	847839.263347	41.605863
3506.881635	847744.716436	41.610868
3506.826022	847652.100717	41.615872
3506.867290	847561.599963	41.620877
3507.169268	847474.351357	41.625882
3506.784124	847393.700668	41.630887
3506.855509	847298.055820	41.635892
3506.964017	847205.116686	41.640896
3506.220084	847128.491145	41.645901
3506.341607	847029.636472	41.650906
3506.310639	846942.819584	41.655911
3506.218613	846864.441376	41.660916
3506.200918	846783.434127	41.665920
3506.174876	846708.628917	41.670925
3506.461110	846615.265024	41.675930
3506.563285	846541.988131	41.680935
3505.936645	846467.758263	41.685940
3506.079273	846380.905911	41.690944
3505.754144	846302.653534	41.695949
3505.837220	846223.851741	41.700954
3505.907039	846149.702794	41.705959
3505.929980	846080.115213	41.710964
3505.987311	846003.834260	41.715968
3505.639976	845921.025226	41.720973
3505.963358	845846.929734	41.725978
3505.634849	845782.433301	41.730983
3505.531950	845704.816639	41.735988
3505.678776	845628.807584	41.740992
3505.484711	845572.623093	41.745997
3505.361412	845498.205335	41.751002
3505.524290	845437.311403	41.756007
3505.104825	845364.973675	41.761012
3505.464223	845301.042901	41.766016
3505.035925	845235.005214	41.771021
3505.521480	845157.483187	41.776026
3505.350181	845082.001434	41.781031
3505.037420	845018.366519	41.786036
3505.423582	844948.127152	41.791040
3505.074584	844889.633953	41.796045
3504.907874	844831.208611	41.801050
3505.117595	844774.565626	41.806055
3504.741105	844720.340215	41.811060
3504.851598	844646.165928	41.816064
3504.786529	844589.951873	41.821069
3504.781551	844526.360456	41.826074
3504.542173	844477.733886	41.831079
3504.832630	844410.895994	41.836084
3504.659562	844355.569058	41.841088
3504.701372	844292.840288	41.846093
3504.715395	844231.472422	41.851098
3504.483697	844184.975016	41.856103
3504.577993	844135.324000	41.861108
3504.630297	844071.718717	41.866112
3504.407921	844018.820008	41.871117
3504.402172	843958.518818	41.876122
3504.378800	843908.981238	41.881127
3504.489908	843860.682580	41.886132
3504.433395	843804.847493	41.891136
3504.379856	843758.803630	41.896141
3504.349173	843687.160099	41.901146
3504.269695	843644.900595	41.906151
3504.054664	843597.426398	41.911156
3504.255843	843544.748086	41.916160
3503.928731	843499.326696	41.921165
3504.349078	843452.527665	41.926170
3504.271200	843406.193979	41.931175
3503.864313	843359.426563	41.936180
3503.949182	843305.019027	41.941184
3503.788522	843261.605945	41.946189
3503.747232	843219.046537	41.951194
3503.975339	843177.220406	41.956199
3503.946974	843135.918885	41.961204
3503.932736	843083.851909	41.966208
3503.848545	843038.776851	41.971213
3503.842435	843001.058589	41.976218
3504.158570	842952.817414	41.981223
3504.125104	842911.224221	41.986228
3504.335126	842856.599055	41.991232
3503.756845	842815.090349	41.996237
3503.919116	842766.774738	42.001242
3503.997822	842716.823311	42.006247
3503.919074	842671.356717	42.011252
3503.868015	842622.976308	42.016256
3503.597848	842577.344969	42.021261
3503.708587	842543.775315	42.026266
3503.472136	842497.168360	42.031271
3503.161892	842454.742457	42.036276
3503.834544	842418.368980	42.041280
3503.479267	842380.313436	42.046285
3503.454059	842334.447978	42.051290
3503.756849	842301.525759	42.056295
3503.323264	842271.433823	42.061300
3503.797796	842237.805564	42.066304
3503.225256	842200.558644	42.071309
3503.593526	842155.600072	42.076314
3503.332551	842117.819031	42.081319
3503.649283	842082.371946	42.086324
3503.581470	842038.644414	42.091328
3503.164495	842001.565882	42.096333
3503.620517	841968.229930	42.101338
3503.566998	841935.264390	42.106343
3503.183108	841897.598138	42.111348
3503.447308	841847.416401	42.116352
3503.109676	841816.046352	42.121357
3503.007326	841777.559448	42.126362
3503.273978	841752.204657	42.131367
3502.891021	841724.041726	42.136372
3503.077751	841695.886594	42.141376
3503.112273	841670.470754	42.146381
3503.573581	841625.687588	42.151386
3503.071641	841595.020963	42.156391
3503.083903	841559.909310	42.161396
3503.274649	841512.354910	42.166400
3502.913701	841483.896425	42.171405
3503.077789	841452.930969	42.176410
3503.134943	841418.975347	42.181415
3503.009482	841395.232180	42.186420
3503.111382	841361.851185	42.191424
3502.648267	841337.481624	42.196429
3502.363793	841311.726140	42.201434
3502.951909	841273.903968	42.206439
3502.926485	841255.576229	42.211444
3502.854164	841219.117866	42.216448
3502.681921	841199.745967	42.221453
3502.827351	841164.999134	42.226458
3502.537386	841138.855774	42.231463
3502.460320	841121.505648	42.236468
3502.460587	841090.272918	42.241472
3502.496476	841072.614003	42.246477
3502.600660	841039.036838	42.251482
3502.731721	841018.161975	42.256487
3502.574783	840999.660007	42.261492
3502.640691	840974.430269	42.266496
3502.570672	840960.473508	42.271501
3502.599944	840930.690380	42.276506
3502.589288	840909.061294	42.281511
3502.357188	840884.362754	42.286516
3502.435768	840849.527522	42.291520
3502.609241	840827.772356	42.296525
3502.289750	840814.339251	42.301530
3502.445344	840792.489750	42.306535
3502.429246	840769.502988	42.311540
3502.464401	840744.568084	42.316544
3502.048327	840731.052886	42.321549
3502.316929	840713.162518	42.326554
3502.268034	840686.688468	42.331559
3502.109602	840680.796111	42.336564
3502.519572	840652.989142	42.341568
3502.632074	840630.757767	42.346573
3502.645607	840601.848483	42.351578
3502.456360	840580.634133	42.356583
3502.334692	840558.051072	42.361588
3502.518602	840525.040565	42.366592
3502.172059	840521.990617	42.371597
3502.666714	840498.825959	42.376602
3502.523619	840474.499821	42.381607
3502.118229	840455.355945	42.386612
3502.293697	840436.606242	42.391616
3502.035272	840419.088395	42.396621
3502.209380	840401.308867	42.401626
3502.232731	840377.247333	42.406631
3502.436969	840370.036869	42.411636
3502.118686	840346.319638	42.416640
3502.127958	840336.423370	42.421645
3502.108116	840307.808896	42.426650
3502.284663	840301.766787	42.431655
3502.181507	840282.381087	42.436660
3502.367416	840257.614591	42.441664
3502.221854	840246.093206	42.446669
3502.309675	840222.506017	42.451674
3502.250826	840200.202806	42.456679
3501.887417	840187.163184	42.461684
3501.989863	840164.931637	42.466688
3501.792078	840158.171806	42.471693
3501.751748	840147.797919	42.476698
3502.055762	840123.788497	42.481703
3501.995511	840111.283392	42.486708
3501.933365	840098.196481	42.491712
3501.877870	840078.802665	42.496717
3502.224119	840075.256135	42.501722
3501.971036	840054.922998	42.506727
3502.067556	840034.050074	42.511732
3501.917137	840023.499151	42.516736
3502.009097	840012.619279	42.521741
3502.159162	840000.081063	42.526746
3502.229645	839984.062742	42.531751
3501.758287	839972.688767	42.536756
3501.995072	839961.592134	42.541760
3501.859854	839942.501380	42.546765
3501.959001	839927.739622	42.551770
3501.958022	839915.612901	42.556775
3501.847580	839895.936030	42.561780
3502.065417	839883.386974	42.566784
3501.726933	839870.342758	42.571789
3501.873305	839858.192885	42.576794
3501.719007	839858.023033	42.581799
3501.893600	839837.525280	42.586804
3501.897767	839821.225835	42.591808
3501.678467	839823.394553	42.596813
3502.018922	839803.452858	42.601818
3502.152368	839786.551005	42.606823
3502.170578	839773.644852	42.611828
3501.928819	839756.025421	42.616832
3501.978183	839760.383582	42.621837
3502.015865	839733.018581	42.626842
3502.134593	839720.193618	42.631847
3502.068947	839702.740536	42.636852
3501.891169	839683.073486	42.641856
3501.840931	839675.901961	42.646861
3501.818470	839652.523789	42.651866
3502.275041	839637.317358	42.656871
3501.609750	839637.809498	42.661876
3501.903561	839611.471120	42.666880
3501.867120	839603.812249	42.671885
3501.861192	839600.708574	42.676890
3501.830664	839573.353500	42.681895
3501.433016	839574.579975	42.686900
3501.915677	839561.406717	42.691904
3501.642831	839551.747284	42.696909
3501.465687	839533.437940	42.701914
3501.938203	839532.684985	42.706919
3501.375856	839527.533770	42.711924
3501.568820	839517.510401	42.716928
3501.618417	839507.412403	42.721933
3501.840140	839492.339337	42.726938
3501.949454	839495.718097	42.731943
3501.857620	839475.551812	42.736948
3501.884671	839460.703142	42.741952
3501.821660	839459.839846	42.746957
3501.995277	839431.676024	42.751962
3502.036418	839418.377421	42.756967
3501.826784	839416.954896	42.761972
3501.829149	839392.892655	42.766976
3501.740632	839392.324409	42.771981
3502.000644	839387.238568	42.776986
3502.249281	839370.802648	42.781991
3501.643980	839357.119838	42.786996
3501.653005	839338.974841	42.792001
3501.538289	839318.229449	42.797005
3501.616652	839315.306500	42.802010
3501.865831	839311.774694	42.807015
3501.837015	839301.106452	42.812020
3501.829232	839285.098481	42.817025
3501.834042	839283.254299	42.822029
3502.019807	839258.774742	42.827034
3501.818915	839253.857863	42.832039
3501.905434	839241.619062	42.837044
3501.928786	839215.806346	42.842049
3501.652834	839211.483326	42.847053
3501.912262	839204.068771	42.852058
3501.849534	839190.397787	42.857063
3501.758729	839183.037954	42.862068
3501.604516	839163.462526	42.867073
3501.511229	839149.699198	42.872077
3501.797672	839146.840667	42.877082
3501.593523	839138.819300	42.882087
3501.925874	839131.587312	42.887092
3501.927800	839104.904208	42.892097
3502.094585	839103.519794	42.897101
3501.905835	839092.682120	42.902106
3501.977772	839070.257191	42.907111
3501.730529	839060.107808	42.912116
3501.814227	839043.017560	42.917121
3501.803975	839039.817239	42.922125
3501.423714	839030.755927	42.927130
3501.779680	839030.506283	42.932135
3501.620264	839003.847946	42.937140
3501.622245	838985.800004	42.942145
3501.680206	838986.955374	42.947149
3501.474506	838982.912297	42.952154
3501.739167	838954.537924	42.957159
3501.570544	838963.782307	42.962164
3501.857713	838956.848265	42.967169
3501.716470	838934.941306	42.972173
3501.791523	838922.897706	42.977178
3501.562262	838922.254382	42.982183
3501.279706	838919.775785	42.987188
3501.587711	838905.269938	42.992193
3501.820957	838903.875089	42.997197
3501.628614	838895.851548	43.002202
3501.693810	838891.280901	43.007207
3501.811515	838872.632332	43.012212
3501.719585	838853.531310	43.017217
3501.521083	838861.325029	43.022221
3501.200681	838859.337486	43.027226
3501.581749	838836.863354	43.032231
3501.521695	838824.840676	43.037236
3501.589660	838820.851742	43.042241
3502.013297	838812.052564	43.047245
3501.886341	838796.547076	43.052250
3501.813023	838783.070879	43.057255
3502.039903	838779.542247	43.062260
3502.009871	838766.059244	43.067265
3501.863098	838756.961014	43.072269
3501.697372	838737.677087	43.077274
3502.021941	838717.152032	43.082279
3501.562492	838710.819592	43.087284
3501.596065	838713.531391	43.092289
3501.931232	838704.163672	43.097293
3501.985294	838686.009644	43.102298
3501.860678	838680.692223	43.107303
3501.965647	838649.915469	43.112308
3502.094384	838637.183645	43.117313
3501.703924	838632.781065	43.122317
3501.981953	838616.144398	43.127322
3502.028006	838608.762460	43.132327
3501.709304	838607.744934	43.137332
3501.782408	838584.735773	43.142337
3501.868445	838578.706069	43.147341
3501.624365	838574.474638	43.152346
3501.625766	838560.209956	43.157351
3501.567068	838541.976078	43.162356
3501.963985	838535.024391	43.167361
3501.433900	838532.681362	43.172365
3501.456765	838503.469296	43.177370
3501.741461	838504.977471	43.182375
3501.686274	838507.703239	43.187380
3501.613159	838507.811767	43.192385
3501.492514	838483.182845	43.197389
3501.840168	838475.074323	43.202394
3501.221803	838463.914502	43.207399
3501.226034	838468.474745	43.212404
3501.325291	838471.855661	43.217409
3501.490326	838469.598023	43.222413
3501.593648	838447.359921	43.227418
3501.542727	838433.685352	43.232423
3501.748192	838446.753648	43.237428
3501.436622	838429.723429	43.242433
3501.336340	838414.212774	43.247437
3501.528481	838407.584071	43.252442
3501.221681	838403.750483	43.257447
3501.379037	838397.612407	43.262452
3501.150173	838408.419712	43.267457
3501.102028	838407.553938	43.272461
3501.404552	838405.759985	43.277466
3501.528139	838393.707728	43.282471
3500.811885	838386.832840	43.287476
3501.195482	838368.044087	43.292481
3501.399198	838382.859531	43.297485
3501.363530	838366.659368	43.302490
3501.482614	838377.606420	43.307495
3501.435735	838382.077678	43.312500
3501.639241	838368.460228	43.317505
3501.384953	838354.914309	43.322509
3501.420124	838348.310078	43.327514
3501.456609	838346.945859	43.332519
3501.239006	838340.478174	43.337524
3501.731634	838340.595310	43.342529
3501.608955	838325.282007	43.347533
3501.559687	838315.294484	43.352538
3501.598363	838319.170166	43.357543
3501.781372	838315.939244	43.362548
3501.696344	838298.776196	43.367553
3501.480244	838288.426539	43.372557
3501.758181	838281.590201	43.377562
3501.739957	838268.977607	43.382567
3501.527402	838256.783535	43.387572
3502.000440	838237.495177	43.392577
3501.401377	838248.942898	43.397581
3501.542501	838234.170380	43.402586
3501.678672	838221.436507	43.407591
3501.082466	838216.677604	43.412596
3501.388485	838212.262878	43.417601
3501.287193	838213.637380	43.422605
3501.141738	838214.145395	43.427610
3501.679303	838210.956037	43.432615
3501.306227	838190.150053	43.437620
3501.478497	838183.038989	43.442625
3501.435305	838176.640905	43.447629
3501.342129	838183.642691	43.452634
3501.820861	838180.947732	43.457639
3501.578814	838163.905884	43.462644
3501.789559	838151.548382	43.467649
3501.449043	838148.690341	43.472653
3501.238438	838145.714946	43.477658
3501.355181	838143.852913	43.482663
3501.501214	838130.632083	43.487668
3501.428430	838115.213395	43.492673
3501.468807	838121.806197	43.497677
3501.336800	838106.784925	43.502682
3501.529339	838115.974163	43.507687
3501.498345	838115.784980	43.512692
3501.950783	838093.976211	43.517697
3501.443094	838090.562002	43.522701
3501.682461	838089.166010	43.527706
3501.719480	838086.734150	43.532711
3501.393337	838069.996314	43.537716
3501.644407	838060.058461	43.542721
3501.495597	838055.035398	43.547725
3501.296123	838063.024401	43.552730
3501.670789	838055.978593	43.557735
3501.451618	838028.160674	43.562740
3501.256266	838021.786209	43.567745
3501.505255	838027.376041	43.572749
3501.231208	838037.608801	43.577754
3501.347849	838024.586423	43.582759
3501.622822	838016.682735	43.587764
3501.577678	837994.951387	43.592769
3501.388452	837999.056996	43.597773
3501.318986	838007.608031	43.602778
3501.654979	838000.956390	43.607783
3501.376258	837991.683521	43.612788
3501.402870	837969.843817	43.617793
3501.260378	837968.798632	43.622797
3501.160636	837962.700300	43.627802
3501.558142	837968.558113	43.632807
3501.328203	837969.273449	43.637812
3500.727237	837965.291464	43.642817
3500.960194	837971.466138	43.647821
3501.420808	837975.276086	43.652826
3501.426044	837955.089473	43.657831
3501.181866	837947.557990	43.662836
3501.977299	837931.420821	43.667841
3501.475058	837938.972079	43.672845
3501.367495	837933.651322	43.677850
3501.374239	837915.696440	43.682855
3501.134139	837904.379384	43.687860
3501.508369	837899.953767	43.692865
3501.096875	837896.524408	43.697869
3501.322837	837904.447118	43.702874
3501.626476	837898.673858	43.707879
3501.182484	837903.401648	43.712884
3501.253702	837894.656214	43.717889
3501.382197	837881.534623	43.722893
3501.415229	837873.086273	43.727898
3501.303000	837863.981276	43.732903
3501.510599	837872.780340	43.737908
3501.378309	837871.442396	43.742913
3501.397696	837874.544991	43.747917
3501.465899	837858.715405	43.752922
3501.607712	837858.305101	43.757927
3501.085885	837850.816898	43.762932
3501.413623	837850.183431	43.767937
3501.348188	837858.539951	43.772941
3500.836227	837857.552501	43.777946
3501.227851	837856.812000	43.782951
3501.308978	837845.735765	43.787956
3501.415362	837821.747964	43.792961
3501.349051	837828.357768	43.797965
3501.476433	837822.709036	43.802970
3501.462396	837827.951973	43.807975
3501.680873	837827.238534	43.812980
3501.404816	837805.639642	43.817985
3501.243907	837795.959850	43.822989
3501.251730	837795.958688	43.827994
3501.251004	837799.064466	43.832999
3501.213259	837802.758330	43.838004
3501.408170	837797.584268	43.843009
3501.183191	837806.742202	43.848013
3501.540897	837793.390486	43.853018
3501.543361	837767.380657	43.858023
3500.605964	837763.839327	43.863028
3501.236265	837750.930158	43.868033
3501.415589	837759.442658	43.873037
3501.036447	837748.147040	43.878042
3501.451443	837756.622703	43.883047
3501.277865	837767.034322	43.888052
3501.341260	837755.572490	43.893057
3501.315520	837768.484317	43.898061
3501.406697	837745.177939	43.903066
3501.419082	837736.053266	43.908071
3501.010452	837726.897341	43.913076
3501.224651	837724.243534	43.918081
3501.181226	837735.799477	43.923085
3500.907897	837726.234196	43.928090
3501.127881	837728.626151	43.933095
3501.105345	837738.626003	43.938100
3501.201054	837738.611103	43.943105
3501.000944	837738.254241	43.948109
3501.266057	837735.204275	43.953114
3501.530155	837739.433300	43.958119
3501.441434	837719.163525	43.963124
3501.348876	837703.067502	43.968129
3501.524837	837691.199743	43.973133
3501.532424	837704.785861	43.978138
3501.441232	837697.327197	43.983143
3501.167802	837680.968233	43.988148
3501.555829	837676.928504	43.993153
3501.464737	837673.643033	43.998157
3501.122331	837677.190495	44.003162
3500.997035	837671.484067	44.008167
3500.628253	837681.441088	44.013172
3501.285085	837675.806507	44.018177
3501.095615	837676.030290	44.023181
3501.478688	837676.649833	44.028186
3501.371181	837684.333809	44.033191
3501.509825	837663.154834	44.038196
3501.087490	837646.430842	44.043201
3501.313404	837655.324419	44.048205
3501.164454	837660.200383	44.053210
3501.772075	837657.679151	44.058215
3501.246028	837663.875741	44.063220
3501.345807	837644.352663	44.068225
3501.604067	837633.151292	44.073229
3501.474834	837623.951533	44.078234
3501.544452	837621.029123	44.083239
3501.339390	837627.078521	44.088244
3501.387485	837621.733152	44.093249
3501.422069	837608.431535	44.098253
3501.325196	837606.214515	44.103258
3501.464721	837597.263862	44.108263
3501.447379	837598.625381	44.113268
3501.388309	837608.242950	44.118273
3501.168426	837608.083276	44.123277
3501.204558	837580.320410	44.128282
3501.430067	837558.545163	44.133287
3501.222580	837572.068149	44.138292
3501.130900	837561.212508	44.143297
3501.537297	837568.525137	44.148301
3501.281372	837579.241117	44.153306
3501.570825	837575.604944	44.158311
3501.571600	837568.714066	44.163316
3501.494197	837545.045043	44.168321
3501.583490	837540.372542	44.173325
3501.424724	837540.397421	44.178330
3501.401160	837534.966122	44.183335
3501.153770	837518.117368	44.188340
3501.288535	837510.817259	44.193345
3501.192923	837504.329592	44.198349
3501.142593	837506.084508	44.203354
3501.485343	837506.030991	44.208359
3500.966146	837508.150364	44.213364
3501.461106	837510.596478	44.218369
3501.300447	837515.280281	44.223373
3501.026928	837512.217347	44.228378
3501.694981	837503.378043	44.233383
3501.404797	837498.667774	44.238388
3501.395511	837484.790409	44.243393
3501.574149	837482.433220	44.248397
3501.176409	837488.221712	44.253402
3501.306461	837479.854695	44.258407
3501.275221	837475.783316	44.263412
3501.317919	837461.121327	44.268417
3501.343570	837458.690988	44.273421
3501.259571	837456.083677	44.278426
3501.375243	837448.495309	44.283431
3501.241357	837460.842372	44.288436
3501.594648	837456.322648	44.293441
3501.450939	837449.842440	44.298445
3501.522295	837425.955580	44.303450
3501.597985	837421.382168	44.308455
3501.420661	837421.798173	44.313460
3501.269571	837422.210077	44.318465
3501.521667	837423.335405	44.323469
3501.138394	837409.807495	44.328474
3501.441394	837391.319443	44.333479
3501.333104	837390.074694	44.338484
3501.202804	837383.883489	44.343489
3501.106662	837385.451488	44.348493
3501.039766	837387.111972	44.353498
3501.375815	837394.338757	44.358503
3501.466470	837393.062909	44.363508
3501.253136	837372.811436	44.368513
3501.170644	837371.562650	44.373517
3501.123029	837361.767385	44.378522
3501.291856	837365.040999	44.383527
3501.061141	837368.182953	44.388532
3501.276169	837371.740512	44.393537
3501.429396	837365.116739	44.398541
3501.366338	837366.097228	44.403546
3501.507859	837366.269281	44.408551
3501.037130	837335.284564	44.413556
3501.339554	837331.063871	44.418561
3501.352436	837342.805888	44.423565
3501.192647	837337.880992	44.428570
3501.508478	837329.581782	44.433575
3501.375415	837335.911392	44.438580
3501.525339	837331.520422	44.443585
3501.302433	837309.426133	44.448589
3501.175539	837312.163655	44.453594
3501.553070	837304.631229	44.458599
3501.464555	837306.683347	44.463604
3501.582663	837312.585486	44.468609
3501.434188	837296.400049	44.473613
3501.322825	837270.697022	44.478618
3501.547766	837277.164849	44.483623
3501.241262	837279.736345	44.488628
3501.081617	837270.152559	44.493633
3501.471786	837276.691616	44.498637
3501.201477	837279.451571	44.503642
3501.311797	837258.081470	44.508647
3501.191844	837249.559094	44.513652
3501.236148	837240.428674	44.518657
3501.065577	837240.455398	44.523661
3501.279587	837248.672029	44.528666
3501.446809	837249.034186	44.533671
3501.001012	837236.389187	44.538676
3501.201463	837234.999084	44.543681
3501.435974	837239.815448	44.548685
3501.103870	837247.243916	44.553690
3500.872911	837247.377140	44.558695
3500.921107	837250.572615	44.563700
3500.840268	837251.264726	44.568705
3501.555737	837242.902924	44.573709
3501.282019	837230.619250	44.578714
3501.747774	837218.899373	44.583719
3501.651731	837226.388026	44.588724
3501.671694	837214.349588	44.593729
3501.760932	837196.670827	44.598733
3501.557223	837188.646756	44.603738
3501.536913	837181.952847	44.608743
3501.450972	837182.354582	44.613748
3501.536912	837174.770515	44.618753
3501.165838	837169.199086	44.623757
3500.953675	837158.846847	44.628762
3501.772043	837151.924742	44.633767
3501.228168	837158.804061	44.638772
3501.398108	837154.603954	44.643777
3501.117406	837165.906909	44.648781
3501.121006	837174.350655	44.653786
3501.428766	837152.464011	44.658791
3501.318479	837140.348724	44.663796
3501.323964	837127.535888	44.668801
3501.741289	837129.606055	44.673805
3501.325275	837121.226837	44.678810
3501.517713	837126.243991	44.683815
3501.504052	837105.378030	44.688820
3501.206233	837083.585798	44.693825
3501.207259	837092.806555	44.698829
3501.175489	837095.917552	44.703834
3501.445899	837095.390035	44.708839
3501.113357	837101.071645	44.713844
3501.460282	837097.037954	44.718849
3501.152607	837088.835877	44.723853
3501.131904	837070.688621	44.728858
3501.484419	837072.089505	44.733863
3501.423109	837072.196212	44.738868
3501.152600	837063.114733	44.743873
3501.300683	837069.400676	44.748877
3501.428651	837071.321971	44.753882
3501.449538	837061.806691	44.758887
3501.037318	837061.580004	44.763892
3501.179659	837048.745606	44.768897
3500.754371	837048.423899	44.773901
3500.698260	837050.373976	44.778906
3500.940444	837051.209740	44.783911
3501.163980	837066.607735	44.788916
3501.057290	837056.918266	44.793921
3501.020175	837058.477123	44.798925
3500.793924	837049.194580	44.803930
3500.764582	837050.072788	44.808935
3500.719700	837063.668567	44.813940
3501.158114	837077.771137	44.818945
3501.367305	837066.770502	44.823949
3500.996228	837052.463377	44.828954
3501.374926	837048.715874	44.833959
3501.271061	837054.361781	44.838964
3500.934432	837046.358296	44.843969
3501.283693	837050.768626	44.848973
3501.225154	837054.077954	44.853978
3501.263001	837054.363285	44.858983
3501.091948	837063.222738	44.863988
3501.449317	837055.790215	44.868993
3501.165885	837048.069603	44.873997
3501.122011	837036.040785	44.879002
3501.358023	837031.733201	44.884007
3501.346850	837030.376132	44.889012
3501.311434	837029.411104	44.894017
3501.545553	837028.889254	44.899021
3501.370850	837025.810620	44.904026
3501.393338	837010.471246	44.909031
3501.236948	837000.498265	44.914036
3501.115439	836989.840373	44.919041
3501.437150	836984.645790	44.924045
3501.420444	836996.101924	44.929050
3501.276884	836994.571416	44.934055
3501.543025	837006.953946	44.939060
3501.779423	836994.881234	44.944065
3501.637945	836980.440982	44.949069
3501.178109	836970.515386	44.954074
3501.478734	836962.023917	44.959079
3501.551566	836975.407368	44.964084
3501.515750	836949.885278	44.969089
3501.434424	836949.800988	44.974093
3501.157112	836938.584976	44.979098
3501.488440	836929.020956	44.984103
3501.406435	836931.169249	44.989108
3501.487566	836925.332773	44.994113
3501.079857	836908.216162	44.999117
3501.282541	836903.234244	45.004122
3501.640546	836905.022570	45.009127
3501.314023	836900.414569	45.014132
3501.400695	836900.109888	45.019137
3501.546640	836905.425691	45.024141
3500.750029	836887.884491	45.029146
3501.344086	836870.514112	45.034151
3501.138826	836868.216694	45.039156
3501.381301	836867.596460	45.044161
3501.318781	836877.118679	45.049165
3500.919678	836876.016347	45.054170
3500.906174	836876.697974	45.059175
3501.176440	836879.955999	45.064180
3501.291095	836879.646942	45.069185
3501.392197	836881.960759	45.074189
3500.965940	836887.074830	45.079194
3501.216285	836886.453368	45.084199
3500.937327	836885.526386	45.089204
3501.097312	836890.742943	45.094209
3501.452207	836892.628823	45.099213
3501.015876	836860.180287	45.104218
3501.236096	836851.604166	45.109223
3500.855356	836847.004599	45.114228
3501.186930	836843.943795	45.119233
3501.490570	836843.411063	45.124237
3501.337545	836859.936178	45.129242
3501.515160	836855.249335	45.134247
3501.332687	836857.219228	45.139252
3501.229099	836830.833635	45.144257
3501.560719	836823.307784	45.149261
3501.213313	836833.359935	45.154266
3501.300708	836821.116033	45.159271
3501.044389	836821.253228	45.164276
3501.309164	836822.376691	45.169281
3501.289299	836831.406985	45.174285
3500.965838	836828.545634	45.179290
3501.422804	836826.532945	45.184295
3501.346035	836805.967000	45.189300
3501.422354	836795.763168	45.194305
3501.111429	836795.811832	45.199309
3501.042976	836791.842870	45.204314
3501.340588	836782.380954	45.209319
3501.114393	836790.472897	45.214324
3501.088840	836789.020956	45.219329
3501.496106	836788.472020	45.224333
3501.265048	836786.178603	45.229338
3501.410448	836768.975130	45.234343
3501.650977	836761.754642	45.239348
3501.362696	836772.477122	45.244353
3501.672455	836764.954615	45.249357
3501.728375	836765.819536	45.254362
3501.533792	836742.165648	45.259367
3501.332175	836736.955591	45.264372
3501.466604	836738.196513	45.269377
3501.345634	836736.080003	45.274381
3501.510086	836735.860222	45.279386
3501.536798	836715.568992	45.284391
3501.567842	836711.972694	45.289396
3501.742441	836696.705804	45.294401
3501.765520	836699.420161	45.299405
3501.819342	836680.871799	45.304410
3502.263722	836671.677971	45.309415
3501.535617	836668.394454	45.314420
3501.664688	836637.506487	45.319425
3501.594633	836637.614567	45.324429
3501.284287	836629.509343	45.329434
3501.718511	836615.269421	45.334439
3501.477449	836622.490291	45.339444
3501.663264	836590.913728	45.344449
3501.638196	836590.238219	45.349453
3501.766549	836584.394029	45.354458
3501.766593	836571.969132	45.359463
3501.568812	836563.457941	45.364468
3501.486415	836556.773037	45.369473
3501.728550	836555.958685	45.374477
3501.854906	836538.369246	45.379482
3501.664701	836525.197427	45.384487
3501.455117	836523.677117	45.389492
3501.739954	836517.031833	45.394497
3501.211132	836506.922104	45.399501
3501.443449	836496.887518	45.404506
3501.625628	836482.201324	45.409511
3501.402155	836492.720030	45.414516
3501.509375	836488.043905	45.419521
3501.514130	836470.570347	45.424525
3501.730124	836462.576760	45.429530
3501.496150	836456.497869	45.434535
3501.610177	836461.819058	45.439540
3501.692175	836440.256318	45.444545
3501.754695	836423.550170	45.449549
3501.246329	836419.746799	45.454554
3501.677207	836420.067796	45.459559
3501.592282	836410.568020	45.464564
3501.670201	836391.917922	45.469569
3501.939054	836384.886700	45.474573
3501.352323	836378.668725	45.479578
3501.635891	836358.821500	45.484583
3501.822979	836349.182032	45.489588
3501.675580	836346.584145	45.494593
3501.443936	836334.971562	45.499597
3501.042785	836316.104895	45.504602
3501.309497	836303.734829	45.509607
3501.607260	836304.464939	45.514612
3501.707682	836307.264458	45.519617
3501.632528	836311.450462	45.524621
3501.464913	836295.944822	45.529626
3501.917988	836283.351434	45.534631
3501.660405	836282.518087	45.539636
3501.434642	836275.758205	45.544641
3501.673658	836252.325821	45.549645
3501.630175	836246.508163	45.554650
3501.539036	836245.940019	45.559655
3501.407965	836251.785085	45.564660
3501.535730	836234.874061	45.569665
3501.492874	836216.436447	45.574669
3501.471156	836209.935820	45.579674
3501.746422	836204.941979	45.584679
3501.527022	836195.948262	45.589684
3501.655612	836175.639276	45.594689
3501.536874	836166.435627	45.599693
3501.536829	836171.677830	45.604698
3501.666497	836171.948850	45.609703
3501.494700	836146.444587	45.614708
3501.428431	836137.232691	45.619713
3501.564170	836133.231371	45.624717
3501.678147	836136.902546	45.629722
3501.961038	836125.403277	45.634727
3501.759902	836109.611163	45.639732
3501.711172	836102.046789	45.644737
3501.856622	836087.365369	45.649741
3501.310699	836073.859848	45.654746
3501.667186	836047.204720	45.659751
3501.867057	836052.221620	45.664756
3501.786457	836046.312491	45.669761
3501.972764	836025.993975	45.674765
3501.669949	836019.440004	45.679770
3501.655909	836017.694837	45.684775
3501.351099	836002.889437	45.689780
3501.504083	835995.875872	45.694785
3501.611689	835985.180371	45.699789
3501.458465	835993.359060	45.704794
3501.717116	835985.746490	45.709799
3501.702872	835959.925563	45.714804
3501.459667	835952.197240	45.719809
3501.637429	835948.092148	45.724813
3501.338504	835949.498059	45.729818
3501.635628	835932.268465	45.734823
3501.489873	835908.894886	45.739828
3501.349887	835852.124299	45.744833
3501.588530	835742.869135	45.749837
3501.397934	835586.204203	45.754842
3501.164424	835378.084723	45.759847
3501.010968	835130.525710	45.764852
3500.540984	834806.881102	45.769857
3500.681287	834453.603979	45.774861
3499.910924	834054.806525	45.779866
3499.777423	833595.087334	45.784871
3499.143788	833106.467674	45.789876
3498.918932	832546.156266	45.794881
3498.861853	831952.834578	45.799885
3498.082985	831298.262748	45.804890
3497.456607	830594.041417	45.809895
3496.709215	829861.672569	45.814900
3496.283246	829055.688840	45.819905
3495.248583	828221.990002	45.824909
3494.724189	827335.696399	45.829914
3494.057057	826408.749913	45.834919
3492.993280	825425.223133	45.839924
3492.098766	824406.593518	45.844929
3491.506981	823331.615556	45.849933
3490.500231	822205.237299	45.854938
3489.344308	821029.238479	45.859943
3488.305812	819816.884885	45.864948
3487.578840	818548.945968	45.869953
3486.313516	817249.086762	45.874957
3485.096117	815894.502300	45.879962
3484.091209	814504.031740	45.884967
3482.859810	813051.605877	45.889972
3481.828742	811560.508008	45.894977
3480.672275	810027.350548	45.899981
3478.817183	808446.294022	45.904986
3477.788307	806825.014933	45.909991
3476.234309	805155.060758	45.914996
3474.682552	803450.951040	45.920001
3473.006322	801712.582369	45.925005
3471.206336	799932.409938	45.930010
3470.061696	798096.116700	45.935015
3468.466981	796242.959006	45.940020
3466.596209	794335.271739	45.945025
3464.864687	792380.813957	45.950029
3462.876354	790391.929517	45.955034
3461.419028	788359.516296	45.960039
3459.560583	786298.066469	45.965044
3457.804486	784204.198202	45.970049
3455.743278	782064.142330	45.975053
3453.836976	779892.330318	45.980058
3451.928665	777679.157883	45.985063
3450.233831	775439.451371	45.990068
3448.102406	773164.809508	45.995073
3446.053467	770852.030751	46.000077
3443.897546	768503.317626	46.005082
3441.924607	766119.132100	46.010087
3439.554364	763700.170893	46.015092
3437.479575	761250.664354	46.020097
3435.752956	758762.177248	46.025101
3432.823494	756254.080122	46.030106
3431.004782	753688.636237	46.035111
3428.844587	751113.174946	46.040116
3426.890849	748505.075185	46.045121
3424.097109	745849.264803	46.050125
3422.020053	743164.653102	46.055130
3419.505906	740459.422267	46.060135
3417.041201	737721.853136	46.065140
3414.645982	734945.062722	46.070145
3411.812575	732154.286724	46.075149
3409.626876	729330.111527	46.080154
3407.362729	726464.577953	46.085159
3404.469101	723585.817490	46.090164
3401.903098	720668.885770	46.095169
3399.535915	717725.819868	46.100173
3396.575464	714768.828438	46.105178
3394.142281	711769.304131	46.110183
3391.493687	708752.494145	46.115188
3389.004372	705692.504399	46.120193
3386.039014	702618.394912	46.125197
3382.650719	699523.614787	46.130202
3380.449358	696400.171141	46.135207
3377.201958	693265.979178	46.140212
3374.505511	690086.337099	46.145217
3371.742260	686891.943195	46.150221
3368.576227	683687.307465	46.155226
3365.809586	680446.746227	46.160231
3362.709580	677197.795913	46.165236
3359.994250	673911.739513	46.170241
3356.821137	670612.822092	46.175245
3353.652558	667294.556091	46.180250
3350.537911	663949.862558	46.185255
3347.560345	660600.246244	46.190260
3344.149755	657214.554622	46.195265
3341.461978	653824.682959	46.200269
3338.436660	650406.056217	46.205274
3335.307955	646981.282191	46.210279
3332.224176	643525.377021	46.215284
3328.861795	640046.942879	46.220289
3326.026082	636558.208538	46.225293
3322.152100	633062.363154	46.230298
3319.060654	629536.170063	46.235303
3315.917215	626008.495339	46.240308
3312.393922	622442.544366	46.245313
3309.294945	618877.031581	46.250317
3305.949910	615292.983953	46.255322
3302.839589	611695.569162	46.260327
3299.497609	608092.761387	46.265332
3295.764567	604460.228119	46.270337
3292.567530	600830.838683	46.275341
3289.179058	597179.390510	46.280346
3285.734811	593508.758044	46.285351
3282.064133	589845.064421	46.290356
3278.515476	586159.358467	46.295361
3275.226398	582461.135908	46.300365
3271.672877	578755.094187	46.305370
3268.320292	575029.829056	46.310375
3264.754241	571309.187966	46.315380
3261.599731	567567.138456	46.320385
3257.887679	563817.735783	46.325389
3253.992779	560060.677625	46.330394
3250.696093	556302.532248	46.335399
3247.237312	552527.498423	46.340404
3243.608368	548738.643387	46.345409
3240.150777	544946.025162	46.350413
3236.325359	541156.984293	46.355418
3232.751949	537333.798158	46.360423
3229.085470	533518.086708	46.365428
3225.388343	529703.718544	46.370433
3222.079601	525887.874003	46.375437
3218.434559	522053.650113	46.380442
3215.188859	518201.233550	46.385447
3211.031541	514348.322605	46.390452
3207.255965	510503.705933	46.395457
3203.873122	506634.869460	46.400461
3200.014694	502768.887396	46.405466
3196.545620	498896.759744	46.410471
3192.548631	495026.616561	46.415476
3188.764567	491153.258931	46.420481
3184.993746	487269.407388	46.425485
3181.271442	483386.531921	46.430490
3177.653485	479484.578441	46.435495
3173.937300	475599.618727	46.440500
3170.002788	471709.251933	46.445505
3166.873194	467810.295386	46.450509
3162.899987	463918.494122	46.455514
3159.250987	459992.756282	46.460519
3155.350690	456087.462522	46.465524
3151.034594	452176.600896	46.470529
3147.362063	448256.929278	46.475533
3143.561717	444354.150036	46.480538
3139.943849	440435.623482	46.485543
3136.126574	436535.001511	46.490548
3132.221180	432618.142270	46.495553
3128.491993	428704.166584	46.500557
3124.591188	424793.551446	46.505562
3120.696070	420882.331891	46.510567
3116.721450	416960.343849	46.515572
3112.850430	413065.200260	46.520577
3108.961092	409152.919462	46.525581
3104.760461	405250.442968	46.530586
3101.028618	401346.454578	46.535591
3096.852256	397444.917867	46.540596
3093.367391	393548.107935	46.545601
3089.498087	389649.584982	46.550605
3085.582741	385765.838059	46.555610
3081.636955	381871.773387	46.560615
3077.197112	377977.352665	46.565620
3073.408341	374094.247749	46.570625
3069.753997	370217.224351	46.575629
3065.694635	366351.008017	46.580634
3061.708708	362474.249081	46.585639
3057.527479	358617.877225	46.590644
3053.522142	354753.542499	46.595649
3049.888264	350890.224286	46.600653
3045.656989	347052.952175	46.605658
3041.433814	343201.558608	46.610663
3037.395260	339374.396681	46.615668
3033.427389	335544.778116	46.620673
3029.883261	331723.953361	46.625677
3025.275650	327908.788501	46.630682
3021.361628	324090.069794	46.635687
3017.381834	320289.019182	46.640692
3012.885338	316483.641032	46.645697
3008.952479	312688.715138	46.650701
3004.841313	308928.243039	46.655706
3000.892722	305161.906878	46.660711
2996.781594	301401.985751	46.665716
2992.519691	297664.196548	46.670721
2988.438461	293924.425078	46.675725
2983.939116	290197.720026	46.680730
2980.059106	286477.035333	46.685735
2976.196869	282780.350761	46.690740
2971.671808	279082.558216	46.695745
2967.693304	275398.579258	46.700749
2963.192011	271733.229467	46.705754
2959.289269	268075.220526	46.710759
2955.265231	264431.833339	46.715764
2950.701968	260801.695210	46.720769
2946.444267	257174.118739	46.725773
2942.019542	253571.651224	46.730778
2938.213406	249977.222162	46.735783
2933.854434	246399.838483	46.740788
2929.687527	242831.526294	46.745793
2925.406441	239275.859708	46.750797
2920.814742	235737.236114	46.755802
2916.672597	232219.673981	46.760807
2912.988394	228710.677841	46.765812
2908.289305	225218.868028	46.770817
2903.948673	221739.506778	46.775821
2899.608107	218280.377470	46.780826
2895.655713	214823.830373	46.785831
2891.314623	211401.221381	46.790836
2886.641310	207986.751210	46.795841
2882.374705	204581.306965	46.800845
2878.075583	201207.250457	46.805850
2873.896630	197843.097001	46.810855
2869.564253	194500.485180	46.815860
2865.279119	191179.518559	46.820865
2861.144543	187854.672547	46.825869
2856.736378	184558.362047	46.830874
2852.218589	181277.021141	46.835879
2847.823621	178009.831285	46.840884
2843.462530	174777.080518	46.845889
2839.506166	171498.719311	46.850893
2834.997807	168252.065185	46.855898
2830.932473	165066.001472	46.860903
2826.550382	161888.689596	46.865908
2822.297425	158733.735990	46.870913
2818.200397	155587.573808	46.875917
2813.624114	152474.895949	46.880922
2809.637719	149371.816625	46.885927
2804.957701	146293.163179	46.890932
2800.319945	143231.303504	46.895937
2796.389427	140173.159837	46.900941
2792.300015	137157.168728	46.905946
2788.140117	134141.435274	46.910951
2783.368736	131151.403382	46.915956
2779.157964	128179.717094	46.920961
2775.217510	125223.791615	46.925965
2770.607783	122295.210475	46.930970
2766.347517	119374.662577	46.935975
2762.011970	116476.181074	46.940980
2757.992765	113591.860432	46.945985
2753.832038	110724.584726	46.950989
2749.190768	107889.372164	46.955994
2744.818009	105067.378564	46.960999
2740.693308	102254.224124	46.966004
2736.549355	99470.277202	46.971009
2732.397937	96688.489387	46.976013
2728.196085	93956.513591	46.981018
2723.861605	91208.191232	46.986023
2719.370141	88490.520541	46.991028
2715.271796	85797.720653	46.996033
2710.816155	83111.652560	47.001037
2706.127668	80458.364197	47.006042
2701.996010	77822.600936	47.011047
2697.606268	75212.668334	47.016052
2693.421406	72618.624456	47.021057
2689.265200	70034.516309	47.026061
2684.475011	67482.653968	47.031066
2680.247746	64936.859122	47.036071
2675.888166	62435.919327	47.041076
2671.208974	59936.974374	47.046081
2667.542943	57469.762955	47.051085
2662.768223	55034.611072	47.056090
2658.580266	52604.659422	47.061095
2654.134775	50193.471094	47.066100
2649.869559	47809.874264	47.071105
2645.589987	45442.218400	47.076109
2640.784539	43110.912580	47.081114
2636.295757	40781.373747	47.086119
2631.808158	38478.456404	47.091124
2627.320123	36212.349329	47.096129
2622.680890	33969.819403	47.101133
2617.740119	31757.686381	47.106138
2613.383966	29566.051509	47.111143
2609.019944	27406.074011	47.116148
2604.040910	25282.701273	47.121153
2599.613820	23172.053479	47.126157
2594.526104	21094.545687	47.131162
2589.653961	19053.934640	47.136167
2584.863596	17063.063651	47.141172
2579.899385	15077.692837	47.146177
2575.222966	13130.756908	47.151181
2569.844193	11220.640732	47.156186
2564.557176	9355.111809	47.161191
2559.022048	7543.742004	47.166196
2552.343928	5786.733008	47.171201
2545.373830	4097.940866	47.176205
2536.245382	2524.354380	47.181210
2524.949921	1102.117459	47.186215
2496.949442	217.665973	47.191220
2445.731946	186.958473	47.196225
2412.456715	212.210368	47.201229
2399.636899	230.861159	47.206234
2402.456909	239.759868	47.211239
2412.059488	238.564616	47.216244
2422.778127	247.157877	47.221249
2431.057822	249.301844	47.226253
2435.272962	254.606448	47.231258
2435.913542	244.239461	47.236263
2434.711993	230.579130	47.241268
2431.601843	234.574486	47.246273
2427.789146	226.979677	47.251277
2424.052367	225.776710	47.256282
2420.330401	225.476298	47.261287
2417.793233	222.665083	47.266292
2414.787210	223.878912	47.271297
2412.147251	213.974522	47.276301
2409.510518	220.265572	47.281306
2406.649527	213.059756	47.286311
2403.525614	211.507810	47.291316
2399.917317	205.181404	47.296321
2397.190849	200.162944	47.301325
2394.053836	205.975412	47.306330
2390.997037	202.571590	47.311335
2387.702760	202.618752	47.316340
2384.210010	206.291138	47.321345
2381.427535	196.437538	47.326349
2378.186750	200.953230	47.331354
2374.620409	195.794075	47.336359
2370.912929	202.951853	47.341364
2367.559127	200.211460	47.346369
2364.952344	198.050257	47.351373
2361.679436	198.698386	47.356378
2358.372209	209.036534	47.361383
2355.140200	202.765178	47.366388
2351.411546	206.044191	47.371393
2348.548124	194.811157	47.376397
2344.852483	206.095958	47.381402
2341.420240	207.354338	47.386407
2338.162385	204.655893	47.391412
2334.491078	201.490599	47.396417
2331.042645	198.119590	47.401421
2327.697613	190.359922	47.406426
2324.748874	198.446255	47.411431
2321.500667	201.264118	47.416436
2317.722505	193.584869	47.421441
2314.161291	200.998201	47.426445
2310.883472	200.846650	47.431450
2307.669602	202.254382	47.436455
2304.454005	201.134442	47.441460
2300.903708	206.249093	47.446465
2297.276754	198.112742	47.451469
2293.526808	205.163286	47.456474
2290.344805	196.305567	47.461479
2287.019952	198.926614	47.466484
2282.976580	193.348558	47.471489
2280.414518	192.322542	47.476493
2276.232844	197.972592	47.481498
2272.898218	204.948673	47.486503
2270.016939	198.524396	47.491508
2266.435439	199.467614	47.496513
2263.217621	192.732147	47.501517
2259.912975	203.512852	47.506522
2256.304756	194.000464	47.511527
2252.625610	198.005780	47.516532
2249.077841	198.029365	47.521537
2246.078014	193.695986	47.526541
2241.942324	195.061287	47.531546
2238.674775	188.276661	47.536551
2235.587297	191.164315	47.541556
2231.469980	193.070933	47.546561
2228.182069	187.839797	47.551565
2224.790263	201.744238	47.556570
2221.572188	192.860551	47.561575
2217.739934	199.231102	47.566580
2214.611409	198.031125	47.571585
2211.025841	195.934509	47.576589
2207.862174	195.793604	47.581594
2204.424421	195.929710	47.586599
2200.673724	202.929774	47.591604
2197.022648	200.849739	47.596609
2193.930928	197.796305	47.601613
2190.464956	195.377252	47.606618
2187.043134	190.670137	47.611623
2183.289723	196.329145	47.616628
2179.486566	201.828253	47.621633
2176.263532	194.239385	47.626637
2172.838803	191.459531	47.631642
2169.263038	194.572303	47.636647
2166.099421	195.991194	47.641652
2162.543011	194.453203	47.646657
2159.074113	185.884044	47.651661
2154.948899	189.155554	47.656666
2151.828544	198.167313	47.661671
2149.008386	191.157688	47.666676
2144.994384	192.307825	47.671681
2141.750900	183.276282	47.676685
2138.254603	184.633333	47.681690
2134.503911	188.722645	47.686695
2130.959309	180.228622	47.691700
2127.417097	182.684396	47.696705
2124.150838	185.473497	47.701709
2120.712330	193.696612	47.706714
2117.165023	182.826946	47.711719
2114.050529	182.080403	47.716724
2109.768456	187.676608	47.721729
2106.590226	183.209832	47.726733
2103.076775	183.591940	47.731738
2099.690495	182.141252	47.736743
2096.639366	183.533070	47.741748
2092.668517	191.836321	47.746753
2089.316516	185.900226	47.751757
2085.676133	188.766858	47.756762
2082.456408	185.182975	47.761767
2079.047862	180.780720	47.766772
2075.612925	183.741764	47.771777
2072.231898	184.359436	47.776781
2068.174221	190.743153	47.781786
2064.702159	184.183587	47.786791
2061.497306	182.704524	47.791796
2057.893431	180.272294	47.796801
2054.630444	175.163877	47.801805
2050.562919	188.905141	47.806810
2047.277841	183.110457	47.811815
2044.069791	189.415026	47.816820
2040.495567	184.627404	47.821825
2037.536162	185.046232	47.826829
2033.691136	178.431139	47.831834
2030.124732	180.897056	47.836839
2026.484296	181.112390	47.841844
2022.873175	186.116404	47.846849
2019.728023	176.598108	47.851853
2015.470477	193.697509	47.856858
2012.074187	190.761395	47.861863
2009.091453	185.738858	47.866868
2005.227390	187.011121	47.871873
2002.121016	182.817885	47.876877
1998.440923	180.078051	47.881882
1995.128790	183.617874	47.886887
1991.864202	183.628871	47.891892
1988.166150	185.520594	47.896897
1984.872781	178.724284	47.901901
1981.013174	180.631796	47.906906
1977.235860	175.856996	47.911911
1974.080035	180.796107	47.916916
1970.617034	182.578286	47.921921
1967.283759	175.525627	47.926925
1963.876175	181.975335	47.931930
1960.118378	178.213089	47.936935
1956.826578	174.779738	47.941940
1952.898118	181.497623	47.946945
1949.691362	172.444592	47.951949
1946.174931	174.839437	47.956954
1942.510119	172.071924	47.961959
1939.334563	175.466999	47.966964
1935.253407	180.987530	47.971969
1932.560115	168.623851	47.976973
1928.994654	175.613980	47.981978
1925.245599	169.898276	47.986983
1921.500518	168.497466	47.991988
1918.429311	173.970697	47.996993
1914.867204	168.228908	48.001997
1911.441982	173.934714	48.007002
1907.366379	172.452748	48.012007
1904.000945	176.241390	48.017012
1900.485257	171.295963	48.022017
1897.110120	175.646130	48.027021
1893.988904	174.394486	48.032026
1890.407611	170.585666	48.037031
1886.886756	175.556608	48.042036
1882.914316	180.538107	48.047041
1879.607727	165.751983	48.052045
1876.351387	175.769031	48.057050
1872.877570	166.840084	48.062055
1869.479190	173.066903	48.067060
1865.822578	172.136340	48.072065
1862.430291	178.533058	48.077069
1858.512187	173.653783	48.082074
1854.928961	178.371895	48.087079
1851.755169	171.325963	48.092084
1848.083495	176.007296	48.097089
1844.809630	162.266473	48.102093
1841.431877	168.420466	48.107098
1837.681726	168.422071	48.112103
1834.113281	168.537617	48.117108
1830.507902	165.979152	48.122113
1827.135900	161.954102	48.127117
1823.812402	168.868427	48.132122
1820.823985	168.801456	48.137127
1816.950695	165.484464	48.142132
1812.933244	165.660791	48.147137
1809.828516	160.331540	48.152141
1806.347728	165.362675	48.157146
1802.587231	166.077781	48.162151
1799.300804	164.579930	48.167156
1795.747076	170.334352	48.172161
1792.325250	158.369490	48.177165
1788.540374	162.442110	48.182170
1785.179585	162.009466	48.187175
1781.926920	161.078996	48.192180
1778.353107	174.676617	48.197185
1775.052554	161.481022	48.202189
1771.126127	167.825305	48.207194
1767.899858	171.690287	48.212199
1764.188456	164.345696	48.217204
1760.660217	173.990854	48.222209
1757.178818	169.305880	48.227213
1753.740535	172.023925	48.232218
1750.063667	172.308333	48.237223
1746.577666	170.683538	48.242228
1743.119220	178.571329	48.247233
1739.859584	172.098875	48.252237
1736.203655	172.984308	48.257242
1732.742632	171.646684	48.262247
1729.431556	165.773929	48.267252
1725.515385	175.378565	48.272257
1722.336167	171.383492	48.277261
1718.666877	174.492053	48.282266
1714.997780	179.071781	48.287271
1711.701972	173.522519	48.292276
1708.558477	179.013444	48.297281
1705.514644	165.777699	48.302285
1701.336224	171.819746	48.307290
1697.511205	168.539541	48.312295
1693.974311	165.691989	48.317300
1690.450169	166.458733	48.322305
1687.172882	160.995173	48.327309
1683.924679	162.386308	48.332314
1680.361335	163.988122	48.337319
1676.664634	160.191119	48.342324
1673.137044	171.462419	48.347329
1670.129389	157.009275	48.352333
1666.643057	176.003427	48.357338
1662.851546	168.424634	48.362343
1659.418541	164.529417	48.367348
1655.674361	171.171094	48.372353
1652.218228	161.404215	48.377357
1648.718934	168.399884	48.382362
1645.315466	165.177115	48.387367
1641.799156	163.161619	48.392372
1637.829787	162.988792	48.397377
1634.586353	161.560199	48.402381
1631.452552	164.246446	48.407386
1627.779951	166.327300	48.412391
1624.538931	162.977871	48.417396
1620.713295	167.189808	48.422401
1616.992417	161.491970	48.427405
1613.601239	163.709123	48.432410
1610.367822	160.301560	48.437415
1606.969213	164.614351	48.442420
1603.145224	162.280017	48.447425
1599.721582	162.379308	48.452429
1596.463401	164.800285	48.457434
1592.391481	162.052328	48.462439
1588.986407	161.275492	48.467444
1585.530578	167.375333	48.472449
1582.237840	157.589240	48.477453
1578.714486	159.232286	48.482458
1575.477258	161.928408	48.487463
1571.920586	162.086496	48.492468
1568.477724	161.416825	48.497473
1564.764802	153.341711	48.502477
1561.114492	154.270620	48.507482
1557.541176	158.357660	48.512487
1554.164868	153.089990	48.517492
1550.366834	145.759058	48.522497
1547.149313	150.578211	48.527501
1543.758244	159.594489	48.532506
1540.200521	153.849002	48.537511
1536.862497	160.373355	48.542516
1533.048885	158.012114	48.547521
1529.569503	155.975061	48.552525
1525.959764	153.974232	48.557530
1522.880296	161.094054	48.562535
1519.729088	154.794550	48.567540
1515.894027	164.819995	48.572545
1512.330553	158.119934	48.577549
1508.694671	160.565252	48.582554
1504.948723	158.829367	48.587559
1501.714069	152.609372	48.592564
1497.987092	160.317783	48.597569
1494.707220	153.073452	48.602573
1491.122369	156.554859	48.607578
1487.877694	160.859410	48.612583
1484.306276	151.980712	48.617588
1480.402400	163.000895	48.622593
1477.258132	160.968356	48.627597
1473.510496	158.549355	48.632602
1470.396458	155.499654	48.637607
1466.916245	156.351350	48.642612
1462.772001	157.161448	48.647617
1459.762062	149.011150	48.652621
1456.637065	163.968645	48.657626
1452.938646	158.972900	48.662631
1449.318230	148.554766	48.667636
1445.643779	155.976550	48.672641
1442.090231	153.444922	48.677645
1438.487696	155.628772	48.682650
1435.352188	152.474873	48.687655
1431.532463	158.271037	48.692660
1427.769022	161.875335	48.697665
1424.565261	152.894820	48.702669
1421.003513	153.651723	48.707674
1417.893286	158.817962	48.712679
1414.211630	150.203331	48.717684
1410.398507	150.490206	48.722689
1407.393389	150.641113	48.727693
1404.174365	148.610810	48.732698
1399.991197	156.722861	48.737703
1396.580728	154.861736	48.742708
1392.873261	149.354892	48.747713
1389.588391	148.938972	48.752717
1386.489672	145.861593	48.757722
1382.489068	153.464167	48.762727
1379.269559	154.040959	48.767732
1375.671807	153.591760	48.772737
1372.438863	144.948041	48.777741
1368.511407	148.979841	48.782746
1364.571033	153.931181	48.787751
1361.480882	143.107372	48.792756
1358.261448	149.372754	48.797761
1354.574970	144.742192	48.802765
1350.861274	148.439971	48.807770
1347.420428	155.366459	48.812775
1344.162825	158.897932	48.817780
1340.564042	161.296370	48.822785
1336.998942	147.009734	48.827789
1333.828884	151.207731	48.832794
1330.533551	146.800694	48.837799
1326.685455	146.656465	48.842804
1322.643555	154.471174	48.847809
1319.767712	146.189204	48.852813
1315.789711	148.748255	48.857818
1312.446066	154.267445	48.862823
1308.933006	151.362523	48.867828
1305.460446	151.390476	48.872833
1302.119907	147.142392	48.877837
1298.692371	149.805110	48.882842
1295.187101	157.276389	48.887847
1291.749571	152.939082	48.892852
1287.638350	156.474481	48.897857
1284.704859	144.800415	48.902861
1280.921947	149.477190	48.907866
1277.296118	146.393776	48.912871
1274.095240	144.515706	48.917876
1270.513675	150.768198	48.922881
1267.212923	142.805873	48.927885
1263.705880	142.794946	48.932890
1259.767025	152.153319	48.937895
1256.884050	143.040398	48.942900
1253.153635	151.290436	48.947905
1249.504120	139.111528	48.952909
1246.035871	151.088663	48.957914
1242.199466	146.690431	48.962919
1239.173253	146.404917	48.967924
1235.548854	150.136215	48.972929
1231.895727	135.872910	48.977933
1228.403052	144.604605	48.982938
1224.579623	142.118475	48.987943
1221.686108	142.979650	48.992948
1218.109891	148.560586	48.997953
1214.651426	145.479471	49.002957
1211.324517	150.597426	49.007962
1207.244870	147.303503	49.012967
1203.964413	143.530119	49.017972
1200.607065	145.530129	49.022977
1197.254891	145.494980	49.027981
1193.598911	143.049089	49.032986
1189.763278	145.968725	49.037991
1186.457777	141.889211	49.042996
1182.848161	155.473581	49.048001
1179.315210	144.523009	49.053005
1175.757045	146.127347	49.058010
1172.430163	148.992654	49.063015
1168.613683	137.709982	49.068020
1165.507810	148.231986	49.073025
1162.107014	142.538022	49.078029
1158.459242	134.424424	49.083034
1155.119755	144.495772	49.088039
1151.275505	131.116670	49.093044
1147.789981	145.981952	49.098049
1144.639320	144.826911	49.103053
1140.903409	146.117395	49.108058
1137.104885	144.560735	49.113063
1133.990214	134.778602	49.118068
1130.306015	146.992058	49.123073
1127.070173	144.936010	49.128077
1123.621414	138.458612	49.133082
1119.817790	142.129420	49.138087
1116.668416	149.187515	49.143092
1112.802560	154.567053	49.148097
1109.640970	140.951370	49.153101
1105.717585	149.864432	49.158106
1102.537261	142.860947	49.163111
1098.929321	145.251410	49.168116
1095.236544	149.983743	49.173121
1091.935512	152.958926	49.178125
1088.472235	143.038392	49.183130
1084.686286	144.599330	49.188135
1081.373948	139.888159	49.193140
1077.568775	139.594936	49.198145
1074.101822	142.691017	49.203149
1070.995394	144.234157	49.208154
1067.366123	141.201989	49.213159
1064.417617	143.846733	49.218164
1060.496394	149.734843	49.223169
1056.801192	136.971545	49.228173
1053.322618	150.636670	49.233178
1049.769495	160.336530	49.238183
1046.533139	144.593822	49.243188
1042.586154	156.956023	49.248193
1039.394209	149.270990	49.253197
1035.926344	155.053327	49.258202
1032.275988	146.250468	49.263207
1029.104570	147.019166	49.268212
1025.012395	150.580160	49.273217
1021.762585	154.335142	49.278221
1018.511699	152.148605	49.283226
1014.971398	145.612814	49.288231
1011.730943	146.075943	49.293236
1007.413309	152.155857	49.298241
1004.402429	156.604281	49.303245
1000.914336	155.283816	49.308250
997.306295	158.439981	49.313255
993.672560	148.406967	49.318260
990.562336	153.086090	49.323265
986.960374	153.510915	49.328269
983.475494	149.380466	49.333274
979.586778	153.320921	49.338279
975.975917	150.795283	49.343284
972.505567	142.135117	49.348289
969.343951	149.745676	49.353293
965.900606	148.551099	49.358298
962.233284	145.135779	49.363303
958.810985	143.925255	49.368308
954.737534	149.087409	49.373313
951.581838	142.820465	49.378317
948.080895	146.583152	49.383322
944.597882	140.481360	49.388327
941.559611	144.639852	49.393332
937.657430	153.821742	49.398337
934.192144	141.519225	49.403341
931.123854	144.790219	49.408346
927.107318	153.664142	49.413351
923.345912	146.194878	49.418356
920.023454	139.799031	49.423361
916.820783	147.491963	49.428365
913.791615	151.092204	49.433370
909.948777	145.711172	49.438375
906.545760	140.036644	49.443380
902.866727	146.231744	49.448385
898.981481	148.899824	49.453389
895.515062	148.376456	49.458394
891.797226	142.463319	49.463399
888.553481	140.927463	49.468404
885.191160	145.551174	49.473409
881.858097	138.334407	49.478413
878.239828	141.596620	49.483418
874.332066	150.143473	49.488423
871.299521	144.521681	49.493428
867.832971	147.791779	49.498433
864.447903	141.260222	49.503437
860.957630	147.378323	49.508442
857.187278	143.011047	49.513447
853.880417	142.940449	49.518452
850.001360	149.331409	49.523457
846.761854	141.948142	49.528461
843.078768	141.607421	49.533466
839.316969	140.196998	49.538471
836.062084	132.449143	49.543476
832.463006	147.240530	49.548481
829.206620	131.507403	49.553485
825.956908	138.306031	49.558490
822.512733	142.344615	49.563495
818.940258	141.907488	49.568500
815.455196	143.481526	49.573505
811.415100	139.403290	49.578509
808.056212	141.014521	49.583514
804.610781	142.569701	49.588519
801.272249	142.481934	49.593524
797.192445	151.160161	49.598529
793.873223	136.398691	49.603533
790.806971	137.685686	49.608538
787.477092	139.710008	49.613543
783.577759	130.161631	49.618548
779.788758	137.968561	49.623553
776.462154	134.667649	49.628557
773.365681	130.995336	49.633562
769.530564	140.929256	49.638567
766.130220	132.909972	49.643572
762.483239	145.165160	49.648577
758.850043	131.275475	49.653581
755.731008	134.921471	49.658586
752.132102	138.867246	49.663591
748.452412	134.321305	49.668596
744.952320	145.984006	49.673601
741.598285	142.684238	49.678605
738.205395	138.365477	49.683610
734.463517	142.381106	49.688615
731.065352	126.879047	49.693620
727.349282	146.750903	49.698625
723.863950	133.932763	49.703629
720.685745	130.346037	49.708634
717.189127	140.331371	49.713639
713.887825	136.311496	49.718644
710.043393	138.704332	49.723649
706.553218	131.866595	49.728653
702.840182	140.110918	49.733658
699.203867	141.075919	49.738663
696.139289	131.985331	49.743668
692.355076	135.656421	49.748673
689.097706	134.610000	49.753677
685.833416	130.710894	49.758682
682.451132	139.365345	49.763687
678.698212	133.081307	49.768692
674.950846	144.684673	49.773697
671.259472	143.073461	49.778701
667.818294	136.924107	49.783706
664.320848	137.051107	49.788711
661.030851	133.690722	49.793716
657.290966	130.562151	49.798721
654.435034	135.685609	49.803725
650.731568	134.895730	49.808730
647.015578	144.649682	49.813735
643.414717	138.307042	49.818740
639.466200	140.130899	49.823745
636.045846	139.499173	49.828749
633.089003	139.497226	49.833754
629.803028	128.255139	49.838759
626.135493	124.118647	49.843764
622.234791	131.750129	49.848769
619.283170	129.029645	49.853773
615.749188	131.152430	49.858778
611.896725	127.962415	49.863783
608.801282	129.453360	49.868788
604.759885	135.847683	49.873793
601.211335	121.982796	49.878797
597.789633	131.810892	49.883802
593.877770	132.300222	49.888807
590.792676	128.287665	49.893812
587.564506	127.676481	49.898817
584.210026	131.818157	49.903821
580.738600	133.190823	49.908826
576.787493	131.901910	49.913831
573.556156	127.314303	49.918836
569.524506	129.410642	49.923841
566.126983	129.414459	49.928845
562.715829	126.234445	49.933850
559.572708	130.763814	49.938855
556.122508	121.100923	49.943860
552.300220	127.435636	49.948865
548.693186	122.644284	49.953869
545.557891	132.193415	49.958874
541.710663	130.274467	49.963879
538.706925	117.526539	49.968884
535.235422	130.962878	49.973889
531.689252	128.152043	49.978893
528.200363	127.970864	49.983898
524.285004	130.858946	49.988903
521.025079	127.908368	49.993908
517.290431	129.866461	49.998913
513.755798	127.860601	50.003917
510.282285	132.843539	50.008922
506.416486	128.975438	50.013927
503.141109	124.809217	50.018932
499.741738	127.755701	50.023937
496.817596	132.649434	50.028941
493.140012	126.382160	50.033946
489.539960	130.423122	50.038951
485.918481	121.078161	50.043956
482.355344	133.734751	50.048961
478.595066	128.163820	50.053965
475.240500	128.391902	50.058970
471.618991	132.107195	50.063975
468.565566	130.494227	50.068980
464.938548	123.526171	50.073985
461.231755	130.390169	50.078989
457.821157	133.559894	50.083994
454.061105	128.893791	50.088999
450.669005	121.556746	50.094004
446.784608	140.853901	50.099009
443.855630	127.290688	50.104013
440.410302	131.253649	50.109018
436.627069	130.590252	50.114023
433.402380	126.931821	50.119028
429.641495	128.944680	50.124033
426.434438	125.305637	50.129037
422.553548	125.628834	50.134042
418.813218	128.881858	50.139047
416.143591	121.786011	50.144052
412.441804	129.917932	50.149057
409.253872	128.373511	50.154061
405.437374	120.372121	50.159066
401.477622	126.120969	50.164071
398.202145	126.687875	50.169076
394.010928	139.110673	50.174081
391.365105	136.684061	50.179085
387.948094	130.132405	50.184090
384.167795	124.096411	50.189095
380.918942	131.765084	50.194100
376.732022	138.688502	50.199105
373.675459	135.089181	50.204109
370.417432	132.635083	50.209114
366.800241	136.479456	50.214119
363.299114	122.480710	50.219124
359.582631	130.801617	50.224129
356.194135	134.322263	50.229133
352.817980	129.833359	50.234138
348.995584	134.943770	50.239143
345.847245	129.352978	50.244148
342.270609	134.250885	50.249153
338.872708	127.506429	50.254157
335.735585	132.269051	50.259162
331.631079	134.712270	50.264167
328.294776	132.403330	50.269172
324.546823	131.025760	50.274177
321.195802	130.661711	50.279181
317.929757	118.888295	50.284186
313.776591	127.603494	50.289191
310.373294	120.594138	50.294196
306.898255	138.102925	50.299201
303.426880	136.368821	50.304205
300.226551	133.681080	50.309210
296.700395	138.355958	50.314215
293.508623	128.659031	50.319220
289.369026	138.128270	50.324225
285.926143	135.693670	50.329229
282.541218	124.925999	50.334234
278.985592	132.003669	50.339239
275.679081	130.348156	50.344244
272.440261	134.190241	50.349249
268.802590	133.792020	50.354253
265.377078	130.642850	50.359258
261.091824	135.825803	50.364263
258.097979	126.414269	50.369268
254.300630	132.798972	50.374273
251.196600	131.434459	50.379277
247.838733	125.335519	50.384282
244.104420	131.321202	50.389287
241.218382	130.501521	50.394292
237.055262	127.540681	50.399297
233.247164	129.377514	50.404301
229.969217	128.207936	50.409306
226.342816	130.044783	50.414311
223.199985	121.004625	50.419316
219.716640	122.309690	50.424321
216.112214	120.321215	50.429325
212.783612	114.897929	50.434330
208.978401	124.359101	50.439335
205.408130	128.360701	50.444340
201.582284	127.814815	50.449345
198.482117	129.411043	50.454349
194.892723	129.717148	50.459354
191.666466	130.425118	50.464359
188.025502	124.560383	50.469364
184.211664	134.832856	50.474369
180.755968	134.418819	50.479373
177.461124	126.047911	50.484378
173.801844	126.409266	50.489383
170.428258	117.446414	50.494388
166.947283	133.279342	50.499393
163.520078	128.472643	50.504397
160.108511	121.720919	50.509402
156.242185	125.288019	50.514407
153.115704	129.609261	50.519412
149.733683	128.563588	50.524417
146.434118	126.166707	50.529421
142.775169	127.882134	50.534426
138.491669	131.245675	50.539431
135.582626	117.900952	50.544436
132.038064	134.572770	50.549441
128.886761	131.754027	50.554445
124.841687	126.819515	50.559450
121.414233	125.271598	50.564455
117.866052	124.353212	50.569460
114.171921	134.366506	50.574465
111.013950	133.004167	50.579469
107.816415	127.769198	50.584474
104.032476	130.532461	50.589479
100.583000	129.737825	50.594484
96.900730	136.863875	50.599489
93.396645	127.228624	50.604493
90.039157	125.986139	50.609498
86.107996	129.724780	50.614503
82.837791	118.202070	50.619508
79.582701	130.234699	50.624513
75.896747	120.185022	50.629517
72.424572	124.130173	50.634522
68.833963	126.543615	50.639527
65.199192	118.871436	50.644532
62.039202	125.061438	50.649537
58.600287	125.021315	50.654541
55.258475	118.954748	50.659546
51.737911	121.876087	50.664551
48.078018	118.285998	50.669556
44.240773	123.496930	50.674561
40.387289	123.986847	50.679565
37.499066	124.733661	50.684570
33.919964	127.309833	50.689575
30.712007	122.905448	50.694580
26.574906	121.278929	50.699585
23.030745	116.193222	50.704589
20.047445	115.290778	50.709594
16.441327	119.310719	50.714599
12.956709	113.769593	50.719604
9.314687	112.593869	50.724609
5.239019	126.153486	50.729613
2.214351	117.961796	50.734618