Thu Aug 25 17:16:17 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
1.146219	96.594882	0.000000
0.613658	93.530417	0.005005
0.891239	87.845943	0.010010
0.803851	91.896720	0.015014
0.444258	90.551573	0.020019
0.471781	65.648241	0.025024
0.228188	73.728855	0.030029
0.101411	49.257851	0.035034
-0.134133	53.474203	0.040038
-0.437096	35.870948	0.045043
-0.532726	30.225985	0.050048
-1.058120	17.985422	0.055053
-1.473457	21.264982	0.060058
-1.646005	6.577318	0.065062
-2.507819	1.286532	0.070067
-2.601103	-5.829947	0.075072
-3.152746	-8.907223	0.080077
-3.166288	-1.897245	0.085082
-2.955296	-7.678824	0.090086
-3.783728	-8.475937	0.095091
-3.841833	-1.825975	0.100096
-3.677736	-12.320571	0.105101
-4.353055	-1.521097	0.110106
-5.271996	-14.209345	0.115110
-5.549291	-7.594646	0.120115
-5.569471	-12.201041	0.125120
-5.529756	-4.193326	0.130125
-5.618355	-3.078372	0.135130
-5.632890	-12.535731	0.140134
-6.347232	-15.739375	0.145139
-6.491521	-17.836426	0.150144
-7.084040	-10.599694	0.155149
-7.190450	-11.630158	0.160154
-7.307565	-20.650658	0.165158
-7.471574	-9.700346	0.170163
-7.113372	-15.919443	0.175168
-7.746218	0.729538	0.180173
-8.153778	-5.508787	0.185178
-8.109374	-10.099992	0.190182
-8.786065	-14.980011	0.195187
-9.448887	-17.552643	0.200192
-9.756882	-7.680766	0.205197
-9.883291	-6.692767	0.210202
-10.540647	-8.601862	0.215206
-10.377796	-8.029348	0.220211
-10.580840	-8.702983	0.225216
-10.186416	-6.477292	0.230221
-10.306399	-7.182924	0.235226
-10.146393	-13.579778	0.240230
-10.762144	-5.352303	0.245235
-11.157559	-9.687932	0.250240
-11.513751	-0.624756	0.255245
-12.102920	-6.280963	0.260250
-12.347687	-10.412403	0.265254
-12.887577	-9.046404	0.270259
-12.853770	-7.251434	0.275264
-13.063919	-7.443060	0.280269
-13.309723	-4.563394	0.285274
-13.127645	-12.836666	0.290278
-14.087973	-2.966982	0.295283
-14.191796	-7.446376	0.300288
-14.392638	-5.219167	0.305293
-14.448407	-11.604359	0.310298
-14.286506	-15.578051	0.315302
-15.160654	-10.679519	0.320307
-15.529520	-14.449825	0.325312
-16.142953	-13.183036	0.330317
-15.992680	-8.922745	0.335322
-15.816923	-13.572494	0.340326
-16.063589	-10.249765	0.345331
-15.998031	-12.946013	0.350336
-16.692915	-7.993310	0.355341
-17.345385	-7.397453	0.360346
-17.186196	-9.168728	0.365350
-17.751085	-10.994233	0.370355
-17.480629	-2.051390	0.375360
-17.916435	1.680631	0.380365
-18.451045	-7.483269	0.385370
-18.719196	-9.677973	0.390374
-18.848536	-5.819964	0.395379
-18.794752	-9.647002	0.400384
-19.354459	-11.311965	0.405389
-19.114879	-10.144028	0.410394
-20.199309	-15.083547	0.415398
-20.573396	-11.826275	0.420403
-20.018374	-12.188413	0.425408
-20.509980	-11.215960	0.430413
-20.852727	-0.683732	0.435418
-20.579230	-4.269948	0.440422
-21.493607	1.106294	0.445427
-22.247094	-12.310235	0.450432
-22.131450	1.117799	0.455437
-22.146500	-6.662676	0.460442
-22.171327	-10.126217	0.465446
-22.341984	-7.742385	0.470451
-22.439889	-8.815311	0.475456
-22.881298	-6.730744	0.480461
-23.497103	-11.402002	0.485466
-23.590146	-4.816172	0.490470
-24.217620	-4.385584	0.495475
-23.795965	-8.181676	0.500480
-23.840716	-7.200144	0.505485
-24.233091	-5.762345	0.510490
-24.544167	-13.284460	0.515494
-25.563368	-11.723136	0.520499
-25.155593	-17.592492	0.525504
-25.199664	-11.748335	0.530509
-26.490603	-16.006921	0.535514
-26.327484	-18.572921	0.540518
-27.014613	-10.818323	0.545523
-26.847558	-16.966341	0.550528
-26.809369	-13.640788	0.555533
-26.602649	-12.860011	0.560538
-26.586639	-19.031818	0.565542
-26.985106	-11.834982	0.570547
-27.264243	-9.415170	0.575552
-27.467413	-18.384220	0.580557
-28.148513	-10.019957	0.585562
-28.716805	-17.204372	0.590566
-29.226417	-2.707093	0.595571
-29.106008	-3.754114	0.600576
-29.435561	-4.559788	0.605581
-29.248314	-11.400676	0.610586
-29.469365	-19.579141	0.615590
-30.361919	-13.779212	0.620595
-30.169167	-12.964609	0.625600
-30.300156	-10.083951	0.630605
-30.774147	-18.112052	0.635610
-31.325374	-11.565167	0.640614
-31.910389	-10.818525	0.645619
-31.955974	-12.241337	0.650624
-32.668110	-11.079305	0.655629
-32.285015	-7.741354	0.660634
-31.918909	-13.338425	0.665638
-32.281616	-8.548501	0.670643
-32.066985	-7.509533	0.675648
-32.970320	-18.960014	0.680653
-33.547749	-4.410981	0.685658
-33.707983	-17.275047	0.690662
-33.798695	-8.474938	0.695667
-34.083717	-16.580105	0.700672
-34.141916	-7.579444	0.705677
-34.641240	-5.476311	0.710682
-35.035586	-13.997788	0.715686
-35.567345	-9.026351	0.720691
-35.710794	-13.189482	0.725696
-35.550672	-11.278262	0.730701
-35.580680	-11.026710	0.735706
-35.674841	-10.132350	0.740710
-36.245994	-10.906496	0.745715
-36.737466	-11.193249	0.750720
-36.876789	-9.231946	0.755725
-37.076499	-13.085703	0.760730
-36.754171	-12.889357	0.765734
-37.262164	-4.163070	0.770739
-37.652519	-15.507266	0.775744
-38.334424	-14.043083	0.780749
-38.584545	-7.616142	0.785754
-38.381121	-10.137837	0.790758
-38.966625	-13.519854	0.795763
-39.357518	-22.064014	0.800768
-39.203157	-5.848437	0.805773
-39.486330	-9.695445	0.810778
-39.373989	-12.642634	0.815782
-40.153328	-10.043206	0.820787
-40.810278	-5.479262	0.825792
-40.991731	-14.942102	0.830797
-41.044689	-12.342592	0.835802
-40.928055	-13.148573	0.840806
-41.361907	-10.432435	0.845811
-41.064309	-6.062349	0.850816
-41.236198	-8.908056	0.855821
-42.325806	0.406079	0.860826
-42.722527	-15.992844	0.865830
-42.641859	-10.737713	0.870835
-43.003588	-18.378439	0.875840
-43.120730	-16.784446	0.880845
-43.036942	-14.766353	0.885850
-43.452378	-17.975697	0.890854
-44.132604	-9.532476	0.895859
-44.310767	-12.266467	0.900864
-44.424143	-9.192414	0.905869
-44.534780	-9.880527	0.910874
-44.481836	-16.118233	0.915878
-44.838025	-12.734050	0.920883
-45.570948	-4.659060	0.925888
-45.939982	-12.912417	0.930893
-45.939671	-14.722074	0.935898
-45.769430	-6.462729	0.940902
-45.939020	-6.815736	0.945907
-46.757835	-11.461509	0.950912
-47.138078	-12.524997	0.955917
-47.664684	-9.212189	0.960922
-47.344184	-10.331691	0.965926
-47.535342	-10.026414	0.970931
-47.725146	-8.781707	0.975936
-47.908352	-11.508580	0.980941
-48.728388	-9.617789	0.985946
-48.475918	-12.849529	0.990950
-48.892595	-7.117832	0.995955
-49.086649	-3.806509	1.000960
-49.393949	-5.713502	1.005965
-49.674069	-7.055272	1.010970
-50.179587	-10.076495	1.015974
-50.023229	-3.235512	1.020979
-50.125791	-9.126148	1.025984
-49.976025	-12.057055	1.030989
-50.709744	-7.072955	1.035994
-50.811290	-8.771739	1.040998
-51.391146	-8.142964	1.046003
-51.432605	-9.227898	1.051008
-51.959043	-12.663461	1.056013
-52.679284	-6.729175	1.061018
-52.340744	-14.982666	1.066022
-53.046622	0.845681	1.071027
-53.120922	-8.358701	1.076032
-53.054343	-15.696376	1.081037
-53.397608	-10.665888	1.086042
-53.117342	-7.713626	1.091046
-53.410535	-8.857193	1.096051
-54.491350	-13.990264	1.101056
-54.184496	-3.072602	1.106061
-54.260586	-2.475305	1.111066
-54.674922	-11.053761	1.116070
-55.376458	-4.321968	1.121075
-55.834280	-8.309290	1.126080
-56.389257	-8.064067	1.131085
-56.444519	-7.498508	1.136090
-56.302776	-8.767172	1.141094
-56.018175	-5.483392	1.146099
-55.851568	-7.135607	1.151104
-56.405942	-6.808220	1.156109
-57.243417	-8.372709	1.161114
-57.259813	-11.524355	1.166118
-57.517129	-10.180484	1.171123
-57.637621	-5.517098	1.176128
-58.438903	-10.374427	1.181133
-58.841074	-7.653760	1.186138
-58.762437	-17.442089	1.191142
-59.019588	-10.419258	1.196147
-59.471268	-12.512436	1.201152
-59.181570	-8.058856	1.206157
-59.127319	-9.408725	1.211162
-59.065985	-10.123784	1.216166
-60.399688	-8.209454	1.221171
-60.455390	-14.699057	1.226176
-60.701062	-11.534673	1.231181
-61.107288	-11.850600	1.236186
-60.915623	-14.285031	1.241190
-61.521505	-10.671896	1.246195
-61.984670	-11.665442	1.251200
-62.160254	-16.307595	1.256205
-61.908930	-2.692020	1.261210
-61.683815	-19.039673	1.266214
-62.716819	-9.648990	1.271219
-63.253491	0.793399	1.276224
-63.474979	-3.427109	1.281229
-63.769588	-6.642731	1.286234
-63.468800	-1.428417	1.291238
-63.502884	-0.524487	1.296243
-63.696839	-10.039152	1.301248
-64.553136	-11.224201	1.306253
-65.092178	0.964967	1.311258
-65.111976	-1.600848	1.316262
-65.430728	-1.576138	1.321267
-65.069490	-6.356192	1.326272
-65.071033	-10.680765	1.331277
-66.383559	-2.983195	1.336282
-66.210809	-8.360144	1.341286
-66.867510	-1.970735	1.346291
-67.035272	-8.303576	1.351296
-66.752022	-2.776463	1.356301
-66.960845	-3.572579	1.361306
-66.845192	-4.378407	1.366310
-68.014957	2.923470	1.371315
-68.374968	-6.340549	1.376320
-68.115640	-5.102940	1.381325
-68.157996	2.477867	1.386330
-68.198068	-3.947749	1.391334
-68.657639	-2.015360	1.396339
-69.212895	-4.354903	1.401344
-69.638554	0.764429	1.406349
-69.754061	-4.526224	1.411354
-69.836677	-14.033021	1.416358
-69.676954	-5.158257	1.421363
-70.361837	-9.100508	1.426368
-70.807102	-0.801667	1.431373
-71.421738	-8.791911	1.436378
-71.487491	-2.896900	1.441382
-71.217909	-7.589825	1.446387
-71.234931	-5.410401	1.451392
-71.663544	-10.677302	1.456397
-72.494542	0.681245	1.461402
-72.553545	-7.782044	1.466406
-73.135504	-6.248097	1.471411
-72.961217	-8.917089	1.476416
-72.783732	-2.107891	1.481421
-73.069876	-5.277383	1.486426
-73.872298	-5.581850	1.491430
-74.234077	-3.566707	1.496435
-74.562089	-15.882455	1.501440
-74.496695	-6.489871	1.506445
-74.695251	-5.708868	1.511450
-74.375265	-11.681530	1.516454
-74.784072	-7.849335	1.521459
-75.032034	-9.079083	1.526464
-75.161506	-12.390182	1.531469
-75.824799	-6.271828	1.536474
-76.347640	-12.479425	1.541478
-76.393043	1.628739	1.546483
-76.792393	-1.219291	1.551488
-76.723188	-3.311829	1.556493
-77.060104	-8.109039	1.561498
-77.664639	-17.170219	1.566502
-78.323352	-3.462673	1.571507
-78.541615	-4.874246	1.576512
-78.432130	-12.449599	1.581517
-78.632297	-3.075514	1.586522
-78.529693	-5.897791	1.591526
-78.765096	2.516865	1.596531
-78.878336	-3.438537	1.601536
-78.872072	-0.421196	1.606541
-80.118053	-1.640097	1.611546
-80.113588	-8.325792	1.616550
-80.040377	-6.207964	1.621555
-80.130422	-0.631851	1.626560
-80.352679	2.301075	1.631565
-81.257652	-1.344096	1.636570
-81.443741	-6.392733	1.641574
-81.469273	-5.638841	1.646579
-81.818676	-3.249147	1.651584
-81.677639	-4.859389	1.656589
-81.895278	-3.436312	1.661594
-82.180507	-8.409301	1.666598
-82.638799	-6.821965	1.671603
-83.289443	-7.504557	1.676608
-83.375471	-3.093346	1.681613
-83.110658	-0.211430	1.686618
-83.527754	-4.432924	1.691622
-84.629145	-13.125184	1.696627
-84.565315	-1.685387	1.701632
-84.559524	-12.310197	1.706637
-85.350112	-4.441307	1.711642
-84.330264	-14.161980	1.716646
-84.735374	-8.030296	1.721651
-85.052625	-12.014331	1.726656
-85.848003	-6.144201	1.731661
-86.091016	-3.514910	1.736666
-86.147823	-15.930101	1.741670
-86.211420	-17.770872	1.746675
-86.582896	-11.973493	1.751680
-87.115072	-11.462920	1.756685
-87.315265	-2.019227	1.761690
-87.532804	-16.443543	1.766694
-87.476306	-8.359371	1.771699
-87.862237	-11.399329	1.776704
-88.607014	-14.471643	1.781709
-89.025552	-10.637924	1.786714
-89.312049	-14.984284	1.791718
-88.382034	-12.178129	1.796723
-88.916705	-12.676411	1.801728
-88.946049	-21.027279	1.806733
-89.827240	-12.527259	1.811738
-90.281161	-13.212202	1.816742
-90.602347	-9.523452	1.821747
-90.832772	-18.114898	1.826752
-90.714370	-24.233141	1.831757
-90.966217	-11.858029	1.836762
-90.693693	-13.264246	1.841766
-91.140436	-8.568723	1.846771
-91.918956	-14.271179	1.851776
-92.213036	-23.175354	1.856781
-92.148863	-10.925690	1.861786
-92.265922	-9.654416	1.866790
-92.202363	-10.762132	1.871795
-93.172372	-10.780907	1.876800
-93.465096	-12.740801	1.881805
-93.503095	-14.506489	1.886810
-93.658379	-18.506409	1.891814
-93.683726	-15.547393	1.896819
-93.964959	-14.104860	1.901824
-94.693661	-16.891788	1.906829
-95.488371	-11.420400	1.911834
-95.519693	-11.953259	1.916838
-95.697366	-6.993011	1.921843
-95.688379	-12.856829	1.926848
-95.439068	-13.322929	1.931853
-95.801131	-1.433581	1.936858
-95.416427	-11.431223	1.941862
-96.163369	-12.905489	1.946867
-96.679734	-9.860041	1.951872
-96.712819	-8.367805	1.956877
-97.129127	-4.455339	1.961882
-97.760758	-11.319773	1.966886
-97.725455	-5.253935	1.971891
-98.224847	-9.335980	1.976896
-98.231796	-10.568691	1.981901
-97.985052	-2.903473	1.986906
-98.551251	-9.572514	1.991910
-99.093323	-1.217376	1.996915
-99.022237	-12.303068	2.006912
-99.384552	-9.949469	2.016909
-98.410140	-6.145382	2.026906
-98.380033	-10.112907	2.036902
-97.612983	-10.799990	2.046899
-96.965849	-7.679558	2.056896
-96.481855	-7.514492	2.066893
-95.558238	-6.252549	2.076890
-95.602222	-12.806086	2.086886
-95.200840	-14.500263	2.096883
-94.453845	-19.939116	2.106880
-94.134506	-11.534066	2.116877
-93.309928	-7.402389	2.126874
-92.934161	-12.624684	2.136870
-92.767424	-15.799484	2.146867
-91.789646	-12.433086	2.156864
-91.378358	-14.379073	2.166861
-91.426884	-9.486524	2.176858
-90.248580	-9.395405	2.186854
-89.912849	-14.430860	2.196851
-89.629687	-12.263934	2.206848
-88.923214	-9.856057	2.216845
-88.436611	-8.639679	2.226842
-88.478546	-16.501851	2.236838
-87.485013	-12.383976	2.246835
-86.825338	-21.176551	2.256832
-86.310340	-20.683720	2.266829
-85.834982	-10.494285	2.276826
-85.834938	-14.685182	2.286822
-84.626239	-15.390782	2.296819
-84.371807	-17.606800	2.306816
-84.260846	-13.170067	2.316813
-83.629754	-14.174804	2.326810
-82.921400	-4.531893	2.336806
-82.698633	-6.343803	2.346803
-81.570480	-8.940649	2.356800
-81.521205	-11.073836	2.366797
-81.219307	-10.056599	2.376794
-79.890312	-14.173796	2.386790
-80.098526	-11.445196	2.396787
-80.065719	-13.933767	2.406784
-78.606690	-17.349072	2.416781
-78.386352	-11.073128	2.426778
-78.231337	-7.318044	2.436774
-77.162202	-10.821146	2.446771
-76.817762	-15.401797	2.456768
-76.642133	-9.270903	2.466765
-76.091702	-10.212315	2.476762
-75.692074	-9.821784	2.486758
-74.943206	-8.332884	2.496755
-74.391684	-4.788817	2.506752
-73.846003	-7.170849	2.516749
-73.244282	-6.501536	2.526746
-73.106608	-12.519664	2.536742
-72.589849	-9.676577	2.546739
-71.674494	-10.136638	2.556736
-71.458447	-10.512466	2.566733
-71.305778	-9.573217	2.576730
-70.611286	-6.697790	2.586726
-69.916449	-9.876144	2.596723
-69.034506	-12.437577	2.606720
-68.529103	-4.904318	2.616717
-68.587059	-6.079857	2.626714
-68.291369	-5.923298	2.636710
-67.335489	-9.421324	2.646707
-67.117402	-2.698359	2.656704
-66.025080	-3.693001	2.666701
-65.806808	-6.144109	2.676698
-65.657566	-7.149372	2.686694
-65.104869	-11.271643	2.696691
-64.160619	-6.084818	2.706688
-64.359077	-0.348304	2.716685
-63.293026	0.536528	2.726682
-62.701855	-5.768074	2.736678
-62.610633	-6.723064	2.746675
-61.967735	-7.140433	2.756672
-61.622772	-6.700153	2.766669
-60.806139	-4.873408	2.776666
-60.097881	-12.701075	2.786662
-59.881499	-9.639858	2.796659
-59.595150	-12.899925	2.806656
-58.697176	-11.988758	2.816653
-58.338697	-17.300210	2.826650
-58.132900	-12.399993	2.836646
-57.047265	-17.318530	2.846643
-56.937710	-16.267987	2.856640
-56.711244	-14.035155	2.866637
-55.747573	-11.949512	2.876634
-55.355759	-8.522972	2.886630
-55.107655	-2.517471	2.896627
-54.081984	-12.282902	2.906624
-53.792634	-5.203634	2.916621
-53.689616	-4.180577	2.926618
-53.056378	-3.693599	2.936614
-52.483661	-7.397685	2.946611
-51.766109	-8.403296	2.956608
-51.184279	-6.051913	2.966605
-51.196290	-10.408819	2.976602
-50.226154	-11.317790	2.986598
-49.971387	-14.328986	2.996595
-49.419655	-15.143887	3.006592
-48.592071	-13.204815	3.016589
-48.367160	-8.488158	3.026586
-48.081827	-8.608744	3.036582
-47.348749	-11.846942	3.046579
-46.931663	-10.166668	3.056576
-46.264509	-13.020732	3.066573
-45.265578	-14.970095	3.076570
-45.250622	-10.103331	3.086566
-45.067988	-6.324062	3.096563
-44.639694	-13.300064	3.106560
-44.237554	-10.714616	3.116557
-43.242158	-9.441740	3.126554
-42.596129	-11.696941	3.136550
-42.651086	-15.020740	3.146547
-41.970560	-13.007940	3.156544
-41.135975	-19.423537	3.166541
-40.914822	-11.899592	3.176538
-40.434008	-12.614682	3.186534
-39.482507	-12.453172	3.196531
-39.442310	-14.455055	3.206528
-38.876921	-10.298599	3.216525
-38.118532	-5.871438	3.226522
-37.951469	-7.243794	3.236518
-37.705943	-7.852325	3.246515
-36.806476	-14.021495	3.256512
-36.402288	-11.205116	3.266509
-35.568969	-6.232157	3.276506
-35.222172	-7.433101	3.286502
-35.143146	-3.520388	3.296499
-34.331324	-7.962029	3.306496
-34.170188	-11.224652	3.316493
-33.266598	-9.493893	3.326490
-32.178471	-14.178399	3.336486
-32.192143	-11.778058	3.346483
-31.810942	-9.803889	3.356480
-31.585078	-5.448511	3.366477
-30.813385	-15.110788	3.376474
-30.424738	-10.403946	3.386470
-29.972927	-14.507239	3.396467
-29.186787	-9.653601	3.406464
-29.308969	-5.075795	3.416461
-28.288921	-11.704188	3.426458
-28.041570	-5.841120	3.436454
-27.190519	-5.967982	3.446451
-26.138101	-13.935104	3.456448
-26.453249	-2.418018	3.466445
-26.373525	-11.281287	3.476442
-25.119350	-13.039390	3.486438
-24.803349	-12.553389	3.496435
-24.279959	-10.037624	3.506432
-23.314657	-11.538219	3.516429
-23.041208	-10.807963	3.526426
-22.947097	-8.050705	3.536422
-22.754602	-12.994026	3.546419
-22.152296	-12.749290	3.556416
-21.020233	-13.227461	3.566413
-20.463614	-10.545839	3.576410
-20.164772	-8.169121	3.586406
-20.212933	-8.123411	3.596403
-19.322926	-10.895181	3.606400
-18.964326	-9.861484	3.616397
-18.519549	-10.371352	3.626394
-17.499874	-12.273278	3.636390
-17.503147	-14.987448	3.646387
-16.523449	-12.340437	3.656384
-16.040871	-13.027292	3.666381
-16.013461	-13.509779	3.676378
-15.278644	-9.028238	3.686374
-14.662344	-7.075064	3.696371
-14.397601	-13.616789	3.706368
-14.020931	-14.112819	3.716365
-13.070196	-14.524564	3.726362
-13.022359	-14.177112	3.736358
-12.303101	-9.281314	3.746355
-11.751868	-10.387576	3.756352
-11.348185	-12.044097	3.766349
-10.583565	-14.276695	3.776346
-10.035561	-14.932618	3.786342
-9.937142	-19.275148	3.796339
-9.434248	-19.306276	3.806336
-8.531586	-10.333703	3.816333
-8.210587	-12.699535	3.826330
-7.963508	-11.613517	3.836326
-7.024393	-10.426853	3.846323
-6.768416	-9.085635	3.856320
-6.467067	-8.457953	3.866317
-5.955620	-8.389050	3.876314
-5.476571	-3.037458	3.886310
-4.368352	-1.186701	3.896307
-4.325305	-1.570268	3.906304
-4.009092	-0.796026	3.916301
-3.565730	9.328754	3.926298
-3.315905	17.180844	3.936294
-2.802743	32.531139	3.946291
-1.894596	43.704531	3.956288
-1.760254	52.613785	3.966285
-1.408488	68.024244	3.976282
-0.632965	83.814989	3.986278
-0.737487	106.111022	3.996275
0.000000	120.920449	4.001280
0.620569	135.936800	4.006285
0.224758	136.641145	4.011290
0.213143	135.288929	4.016294
0.208703	160.147762	4.021299
0.534163	149.051975	4.026304
0.871314	169.725363	4.031309
0.751021	161.474076	4.036314
0.656037	167.411693	4.041318
0.641185	175.753911	4.046323
0.611391	180.289239	4.051328
1.061695	188.400392	4.056333
0.977060	188.448529	4.061338
1.191422	187.522821	4.066342
1.205436	188.995039	4.071347
1.412110	197.865719	4.076352
1.458653	184.709671	4.081357
1.224665	178.301713	4.086362
1.303369	181.513385	4.091366
0.890023	179.727392	4.096371
1.280545	188.515476	4.101376
1.148535	194.468394	4.106381
1.122674	197.145949	4.111386
1.322682	187.373288	4.116390
1.501812	190.600865	4.121395
1.175679	181.562391	4.126400
1.260948	182.805142	4.131405
1.075742	187.848886	4.136410
1.356432	192.901893	4.141414
1.374198	189.444295	4.146419
1.224452	197.174895	4.151424
1.444366	200.383429	4.156429
1.285853	198.181011	4.161434
1.433364	193.184449	4.166438
1.360291	199.080678	4.171443
1.306611	198.165328	4.176448
1.645888	203.000346	4.181453
1.164699	198.697088	4.186458
1.905306	193.183647	4.191462
1.408820	192.002313	4.196467
1.133087	171.224511	4.201472
1.725169	179.487455	4.206477
1.229241	187.063480	4.211482
1.553416	184.548148	4.216486
1.269372	190.692569	4.221491
1.707788	195.328551	4.226496
1.675162	195.011028	4.231501
1.164752	193.996393	4.236506
1.712383	189.009909	4.241510
1.471463	191.313026	4.246515
1.611324	198.397125	4.251520
1.645514	190.634159	4.256525
1.485227	194.338869	4.261530
1.989724	191.497885	4.266534
1.495697	181.536571	4.271539
1.541044	186.439785	4.276544
1.560715	189.686019	4.281549
1.434172	192.645109	4.286554
1.696077	195.353507	4.291558
1.756397	196.919713	4.296563
1.466066	189.884650	4.301568
1.397518	187.373903	4.306573
1.727107	194.849061	4.311578
1.977916	202.365041	4.316582
1.448040	204.656485	4.321587
1.448153	191.653243	4.326592
1.606420	192.185352	4.331597
1.871197	197.946386	4.336602
1.684462	195.102971	4.341606
1.964141	201.105285	4.346611
1.706501	203.369893	4.351616
1.833624	198.161385	4.356621
1.694843	212.290682	4.361626
1.863154	197.669680	4.366630
1.558822	198.894379	4.371635
2.042317	197.284247	4.376640
1.910217	198.909076	4.381645
1.650770	197.706420	4.386650
1.956571	195.886843	4.391654
1.970132	203.414685	4.396659
1.934936	198.579629	4.401664
1.979092	196.636528	4.406669
1.577114	197.006476	4.411674
1.788588	195.419982	4.416678
2.008837	207.401737	4.421683
2.177760	211.301648	4.426688
1.999573	205.954309	4.431693
1.974670	203.281693	4.436698
2.107451	213.796490	4.441702
1.883006	217.270807	4.446707
1.801689	214.116636	4.451712
2.187942	223.076252	4.456717
1.833135	232.110855	4.461722
2.032565	217.703264	4.466726
2.050684	238.433046	4.471731
2.303851	231.148292	4.476736
2.185012	224.706456	4.481741
2.065443	234.748264	4.486746
2.413437	223.870368	4.491750
2.109749	223.588988	4.496755
2.184752	225.190862	4.501760
2.389047	227.234396	4.506765
2.090660	221.073800	4.511770
2.302782	231.285104	4.516774
2.208974	230.148244	4.521779
1.818500	231.974914	4.526784
2.383032	226.666225	4.531789
2.616886	229.252470	4.536794
2.339952	226.967361	4.541798
2.754580	233.473736	4.546803
2.435815	226.006507	4.551808
2.413415	212.962483	4.556813
1.934304	202.138261	4.561818
2.153612	214.499827	4.566822
2.389418	227.988303	4.571827
2.728002	222.841570	4.576832
2.572384	221.499256	4.581837
2.198691	224.740689	4.586842
2.225938	222.708483	4.591846
2.297034	229.119983	4.596851
2.056639	231.445170	4.601856
2.417764	235.723104	4.606861
2.199710	233.925489	4.611866
2.406507	228.818386	4.616870
2.259773	231.385168	4.621875
2.218728	233.312116	4.626880
2.279567	235.343326	4.631885
1.901685	228.508632	4.636890
2.526612	244.264727	4.641894
2.530351	246.757313	4.646899
2.763817	246.470866	4.651904
2.768903	248.843015	4.656909
2.676840	246.364418	4.661914
2.429897	235.817018	4.666918
2.607536	239.452971	4.671923
2.434841	233.851657	4.676928
2.734960	242.540035	4.681933
2.567842	252.181169	4.686938
2.701047	247.256438	4.691942
2.955266	256.967604	4.696947
2.342090	252.242076	4.701952
2.645206	250.429241	4.706957
2.430680	258.742671	4.711962
2.890759	261.907259	4.716966
2.568374	260.818867	4.721971
2.653127	262.020574	4.726976
2.684838	250.417079	4.731981
2.347999	259.569105	4.736986
2.365487	253.232452	4.741990
2.736028	265.076801	4.746995
2.600859	261.250835	4.752000
2.739036	253.034940	4.757005
2.569848	261.663978	4.762010
2.765738	256.482645	4.767014
2.687930	266.052844	4.772019
3.089907	268.460889	4.777024
3.012376	270.181582	4.782029
2.649375	277.360321	4.787034
2.996014	273.272196	4.792038
2.931077	266.113201	4.797043
2.768209	277.769044	4.802048
3.051583	280.246295	4.807053
3.146387	290.532964	4.812058
3.075552	277.787555	4.817062
2.579733	271.404768	4.822067
2.568686	272.779677	4.827072
3.172847	272.128256	4.832077
3.130473	283.796863	4.837082
2.977980	282.855861	4.842086
2.796770	283.767038	4.847091
2.783972	285.211827	4.852096
3.147029	281.551409	4.857101
3.087258	286.164229	4.862106
3.336687	281.423765	4.867110
2.986327	291.647302	4.872115
3.000541	287.566965	4.877120
3.362206	279.610278	4.882125
2.810330	277.823832	4.887130
2.972841	281.028719	4.892134
2.880376	283.428813	4.897139
3.238979	287.175631	4.902144
3.478541	283.281456	4.907149
3.119041	286.033446	4.912154
3.315422	271.072618	4.917158
3.082149	284.688418	4.922163
2.937201	281.964995	4.927168
3.265393	279.360434	4.932173
3.048415	290.217986	4.937178
2.990231	288.651587	4.942182
3.234957	287.521794	4.947187
3.339076	302.141465	4.952192
3.269373	299.577097	4.957197
3.457646	306.413203	4.962202
3.718612	311.646509	4.967206
3.405017	301.131661	4.972211
3.230620	283.052424	4.977216
3.439066	286.237460	4.982221
3.128873	295.746007	4.987226
2.927331	300.624659	4.992230
3.679290	311.479109	4.997235
3.628383	317.248514	5.002240
3.617577	306.338198	5.007245
3.371432	319.731408	5.012250
3.387705	312.391987	5.017254
3.651827	314.103446	5.022259
3.607883	314.531197	5.027264
3.681148	310.169513	5.032269
3.380874	316.791095	5.037274
3.644092	303.142255	5.042278
3.803373	314.095896	5.047283
3.615928	298.505467	5.052288
3.427325	288.021664	5.057293
3.351386	288.916347	5.062298
3.856998	295.658433	5.067302
3.674755	309.579476	5.072307
3.341271	309.011690	5.077312
3.699305	298.875678	5.082317
3.570450	307.957175	5.087322
3.801724	311.413893	5.092326
3.609544	310.444305	5.097331
3.688864	310.280088	5.102336
3.840591	301.147698	5.107341
3.574935	308.494700	5.112346
3.728018	303.516218	5.117350
3.579432	300.125792	5.122355
3.575949	307.833524	5.127360
3.842374	304.941236	5.132365
3.360727	317.207051	5.137370
3.608456	306.208770	5.142374
3.857478	305.717398	5.147379
3.443637	313.280614	5.152384
3.819947	310.155968	5.157389
3.739550	309.665589	5.162394
3.704190	308.377194	5.167398
3.766551	311.873032	5.172403
3.660753	312.826180	5.177408
4.016313	311.286705	5.182413
3.901612	311.374356	5.187418
3.872167	314.780172	5.192422
3.904687	317.654247	5.197427
3.408862	313.210881	5.202432
4.094634	321.025765	5.207437
3.911648	327.635302	5.212442
3.741371	336.938446	5.217446
3.647009	339.269240	5.222451
3.743673	339.826825	5.227456
4.171277	333.264530	5.232461
4.110263	345.084798	5.237466
3.790094	347.501594	5.242470
3.982790	336.477115	5.247475
3.991438	349.539352	5.252480
4.015527	343.094063	5.257485
3.714599	342.654055	5.262490
4.051121	344.208637	5.267494
3.712029	342.195850	5.272499
4.075490	348.890625	5.277504
4.357337	346.701452	5.282509
4.022420	345.779537	5.287514
4.165509	336.110629	5.292518
4.033271	341.013236	5.297523
3.948429	345.766045	5.302528
4.283900	358.223409	5.307533
4.380235	367.380388	5.312538
4.386861	352.294195	5.317542
4.205015	344.175858	5.322547
4.320327	355.724889	5.327552
4.355139	349.078594	5.332557
3.984366	351.408405	5.337562
4.172594	354.473230	5.342566
4.620661	349.476991	5.347571
4.298939	351.564992	5.352576
4.415460	347.389515	5.357581
4.091547	353.432668	5.362586
4.429944	351.883222	5.367590
4.405249	352.440840	5.372595
4.620049	363.309880	5.377600
4.642473	360.193214	5.382605
4.214165	354.840726	5.387610
4.281357	348.458285	5.392614
4.088311	352.009968	5.397619
4.287080	364.678586	5.402624
4.351373	366.671304	5.407629
4.558958	372.226214	5.412634
4.658937	365.939873	5.417638
4.395715	364.769436	5.422643
4.669739	369.212915	5.427648
4.581842	362.690249	5.432653
4.750860	368.121482	5.437658
4.451069	363.903659	5.442662
4.604267	365.993182	5.447667
4.605915	372.668723	5.452672
4.680398	356.641723	5.457677
4.613322	359.123273	5.462682
4.295481	365.254065	5.467686
4.978501	358.192984	5.472691
4.434177	367.902773	5.477696
4.803092	360.903560	5.482701
4.571188	367.055691	5.487706
4.609931	367.998850	5.492710
4.721143	364.786012	5.497715
4.547787	364.794266	5.502720
4.956078	361.879741	5.507725
4.752109	371.393832	5.512730
4.232604	362.800028	5.517734
4.954230	365.012466	5.522739
4.794670	360.820131	5.527744
4.673832	360.949873	5.532749
4.413622	364.698750	5.537754
4.797136	360.905393	5.542758
4.644847	356.335421	5.547763
4.379305	366.887408	5.552768
4.840865	363.233687	5.557773
4.509188	362.697254	5.562778
4.513031	366.914138	5.567782
4.452345	367.347677	5.572787
4.210281	374.077222	5.577792
4.734755	384.302951	5.582797
4.845897	393.891072	5.587802
4.566811	388.394966	5.592806
4.941438	391.430593	5.597811
4.683407	397.045808	5.602816
4.625245	389.854064	5.607821
4.726248	398.260494	5.612826
4.819835	390.165421	5.617830
4.716984	397.670454	5.622835
5.138782	409.162008	5.627840
5.063087	413.217353	5.632845
4.946558	414.599309	5.637850
5.185168	419.266655	5.642854
5.249480	411.565314	5.647859
4.793987	404.780679	5.652864
5.146428	408.196283	5.657869
5.128200	421.787985	5.662874
5.025970	416.033199	5.667878
5.356303	414.304672	5.672883
5.408077	410.433565	5.677888
4.851052	396.612604	5.682893
4.974376	408.663467	5.687898
5.239324	413.019791	5.692902
5.548467	423.627305	5.697907
4.923961	408.924699	5.702912
5.098788	409.390944	5.707917
5.271600	411.312878	5.712922
4.935830	417.244011	5.717926
5.373729	421.642844	5.722931
4.927092	424.187037	5.727936
4.775542	418.781674	5.732941
5.000733	416.595042	5.737946
5.282241	422.812287	5.742950
5.101283	417.421024	5.747955
4.814736	428.991936	5.752960
5.303198	413.599235	5.757965
5.215068	425.354199	5.762970
5.054021	416.409966	5.767974
5.102051	432.902045	5.772979
5.461389	439.050152	5.777984
5.818201	443.382599	5.782989
5.840609	439.225011	5.787994
5.582471	429.384791	5.792998
5.474989	423.618170	5.798003
5.233014	432.957908	5.803008
5.605609	419.029242	5.808013
5.324320	414.716756	5.813018
5.783105	429.708083	5.818022
5.291309	417.626500	5.823027
5.432656	413.804635	5.828032
5.549052	420.610916	5.833037
5.257861	425.801051	5.838042
5.470357	424.109969	5.843046
5.611532	434.582451	5.848051
5.750442	439.711528	5.853056
5.891100	427.609942	5.858061
5.374023	424.242425	5.863066
5.523460	433.641063	5.868070
5.617163	428.747783	5.873075
5.378912	437.723096	5.878080
6.011055	443.575352	5.883085
5.557107	439.707543	5.888090
5.873336	445.587150	5.893094
5.845267	425.637146	5.898099
5.580327	423.821546	5.903104
5.424502	419.884884	5.908109
5.863174	435.831689	5.913114
5.970223	433.862889	5.918118
5.714859	431.349739	5.923123
5.353015	426.977103	5.928128
5.701917	434.253177	5.933133
5.290916	444.929243	5.938138
5.377758	451.183326	5.943142
5.705446	450.024706	5.948147
5.332518	449.149872	5.953152
5.808949	450.739492	5.958157
5.513965	449.137412	5.963162
5.610808	447.837785	5.968166
5.728883	445.490756	5.973171
5.944217	463.449993	5.978176
5.930642	466.233234	5.983181
5.889727	467.255321	5.988186
6.008480	476.000704	5.993190
6.058047	457.228116	5.998195
5.744256	458.043012	6.003200
6.334028	459.149786	6.008205
5.873270	454.735691	6.013210
5.749179	454.502100	6.018214
6.008839	456.989419	6.023219
5.769796	459.605499	6.028224
6.497614	461.892913	6.033229
6.041013	456.674544	6.038234
5.703794	456.917287	6.043238
5.886205	458.312521	6.048243
5.849376	460.175556	6.053248
5.991592	445.602734	6.058253
5.632980	459.659099	6.063258
5.919888	462.376276	6.068262
6.267118	465.916099	6.073267
6.088061	466.807965	6.078272
5.694328	450.455594	6.083277
5.912755	456.217646	6.088282
5.849975	455.474558	6.093286
6.296918	457.454790	6.098291
6.123679	464.309632	6.103296
5.932659	461.871820	6.108301
5.760664	461.946301	6.113306
5.980487	452.040673	6.118310
6.286814	445.320163	6.123315
5.969835	460.021761	6.128320
6.043239	449.158277	6.133325
6.288609	457.263695	6.138330
6.051571	452.650028	6.143334
6.418017	459.606977	6.148339
6.030693	462.625954	6.153344
6.069690	456.624392	6.158349
6.219493	470.658056	6.163354
6.371168	454.979554	6.168358
6.330263	456.840064	6.173363
5.820758	443.046423	6.178368
5.997936	425.076479	6.183373
5.836248	429.645191	6.188378
6.033542	433.679915	6.193382
5.956055	429.085549	6.198387
5.504766	430.415549	6.203392
6.331722	438.730402	6.208397
5.762361	436.272776	6.213402
5.944421	441.803232	6.218406
6.016634	431.389214	6.223411
5.828732	437.309840	6.228416
6.058959	425.482133	6.233421
5.614888	429.544577	6.238426
5.936906	442.731796	6.243430
6.334811	447.503910	6.248435
6.030315	445.609082	6.253440
5.677172	435.423064	6.258445
5.966438	434.279957	6.263450
5.986355	431.242768	6.268454
5.820790	428.971821	6.273459
5.832650	444.194542	6.278464
6.225229	438.801998	6.283469
5.655901	442.501243	6.288474
5.788195	444.768063	6.293478
5.882228	450.375591	6.298483
5.883803	450.327962	6.303488
5.951012	447.992066	6.308493
5.855995	453.777917	6.313498
5.921898	451.692171	6.318502
6.000200	452.277948	6.323507
6.034670	457.046895	6.328512
5.910668	452.127605	6.333517
6.065501	450.736631	6.338522
5.971816	451.282914	6.343526
6.081237	452.724386	6.348531
6.186284	449.610579	6.353536
6.282553	437.870293	6.358541
5.717274	436.690228	6.363546
5.838380	425.708549	6.368550
6.067444	428.868233	6.373555
6.057886	425.335774	6.378560
6.121771	415.483073	6.383565
5.757056	436.380639	6.388570
5.746259	431.032316	6.393574
5.950301	432.515911	6.398579
5.294027	438.424498	6.403584
5.314198	444.322017	6.408589
6.002241	454.262721	6.413594
6.154338	453.833990	6.418598
6.042442	452.817013	6.423603
5.994839	459.275669	6.428608
6.019100	457.421081	6.433613
6.171671	455.615994	6.438618
6.324581	461.290234	6.443622
5.868732	445.985348	6.448627
5.718863	458.249897	6.453632
6.198216	453.783421	6.458637
5.925985	453.886263	6.463642
5.997623	450.847295	6.468646
6.246937	450.419152	6.473651
5.769028	446.184923	6.478656
5.770024	441.717467	6.483661
5.906083	450.403177	6.488666
5.578840	455.159192	6.493670
5.849544	447.147078	6.498675
5.913898	450.734383	6.503680
6.119173	454.473622	6.508685
5.916873	448.414955	6.513690
6.156895	448.114822	6.518694
6.073623	451.013388	6.523699
6.082696	455.928688	6.528704
6.234603	453.949693	6.533709
6.236477	442.360240	6.538714
6.019114	440.030967	6.543718
6.090052	425.086502	6.548723
5.687613	419.922935	6.553728
5.933199	419.868712	6.558733
5.819050	418.421805	6.563738
5.911589	431.094460	6.568742
5.622903	421.616547	6.573747
5.903322	437.740014	6.578752
6.391799	438.846838	6.583757
6.061175	424.610719	6.588762
5.907970	412.858916	6.593766
5.913428	418.350593	6.598771
5.612346	425.079913	6.603776
5.902734	417.188119	6.608781
5.662062	420.272699	6.613786
5.818479	439.531998	6.618790
6.029084	447.848510	6.623795
5.799297	454.702717	6.628800
6.094659	452.957519	6.633805
6.130033	453.341206	6.638810
6.070730	451.651578	6.643814
5.898439	447.166977	6.648819
5.989822	444.770345	6.653824
6.151393	440.416940	6.658829
5.746603	434.804469	6.663834
5.831193	440.413473	6.668838
6.003054	455.826277	6.673843
6.091295	453.275107	6.678848
6.033053	435.728029	6.683853
6.052652	430.751443	6.688858
5.755378	439.736005	6.693862
5.515199	434.752662	6.698867
5.612025	440.568564	6.703872
5.921338	449.549842	6.708877
6.106981	454.140073	6.713882
6.072444	453.136286	6.718886
6.425694	446.566617	6.723891
5.695443	457.713505	6.728896
5.808814	439.668119	6.733901
5.773657	445.697697	6.738906
5.709062	452.446924	6.743910
6.272469	452.630816	6.748915
5.870315	458.056653	6.753920
6.205807	447.085665	6.758925
6.054400	456.202410	6.763930
5.968612	455.118065	6.768934
5.879704	452.977478	6.773939
5.933465	455.433780	6.778944
5.937247	452.259906	6.783949
5.874094	446.252206	6.788954
5.809935	444.401982	6.793958
5.979330	448.437917	6.798963
5.744913	458.326996	6.803968
6.093441	452.188350	6.808973
6.214001	447.449050	6.813978
5.875945	453.013544	6.818982
6.176284	450.543041	6.823987
5.960972	445.397606	6.828992
5.876939	429.215037	6.833997
5.852542	434.758855	6.839002
5.925528	432.456859	6.844006
6.154198	443.915417	6.849011
5.942148	439.329477	6.854016
6.252235	427.236146	6.859021
5.929860	424.401291	6.864026
5.589441	421.600902	6.869030
5.700980	426.962063	6.874035
6.038264	445.886136	6.879040
6.447202	437.820728	6.884045
6.133220	434.294834	6.889050
5.884710	424.298080	6.894054
6.110865	419.111958	6.899059
5.589490	419.832822	6.904064
5.826254	420.039418	6.909069
5.596831	419.081987	6.914074
5.915201	438.277944	6.919078
6.260089	437.917086	6.924083
6.073544	437.690117	6.929088
5.867149	432.954590	6.934093
5.740838	428.576689	6.939098
5.919638	435.047320	6.944102
6.069705	439.323571	6.949107
5.809507	433.603021	6.954112
6.051415	441.762761	6.959117
5.656751	441.223538	6.964122
5.684122	447.528068	6.969126
5.976129	441.546983	6.974131
6.096074	454.563385	6.979136
6.442162	451.588987	6.984141
6.174336	452.323912	6.989146
5.600771	431.019813	6.994150
6.111423	426.190923	6.999155
5.644968	432.098242	7.004160
6.268991	432.304275	7.009165
6.070148	434.138906	7.014170
6.182926	426.505898	7.019174
6.229649	424.796495	7.024179
6.229474	426.318414	7.029184
6.200637	426.576116	7.034189
6.105882	429.476478	7.039194
5.914205	417.407986	7.044198
5.954847	423.998340	7.049203
5.772098	434.205188	7.054208
5.658751	423.858215	7.059213
6.057223	423.416193	7.064218
5.651503	428.893202	7.069222
5.984439	423.250571	7.074227
5.885218	431.220137	7.079232
5.751400	425.331087	7.084237
5.877509	422.799299	7.089242
5.862742	430.540489	7.094246
5.676271	430.810234	7.099251
5.851490	436.503118	7.104256
6.127405	424.722038	7.109261
5.847696	418.106014	7.114266
5.571016	423.888680	7.119270
5.970944	431.694615	7.124275
5.894678	443.115526	7.129280
6.097261	444.941048	7.134285
5.499352	445.499892	7.139290
5.579352	445.265962	7.144294
6.630392	450.293259	7.149299
5.744672	446.818977	7.154304
6.441316	450.933660	7.159309
6.109219	433.420001	7.164314
5.873329	422.003860	7.169318
6.016492	428.714199	7.174323
5.931407	423.649609	7.179328
6.155839	426.417700	7.184333
6.077514	425.215125	7.189338
5.664915	430.715359	7.194342
5.900449	424.796913	7.199347
5.787022	424.052270	7.204352
5.999103	423.835612	7.209357
5.951688	424.551820	7.214362
6.142970	426.018431	7.219366
5.893887	424.678089	7.224371
6.120024	425.322963	7.229376
5.520118	420.649095	7.234381
5.617746	421.855124	7.239386
5.889874	443.184444	7.244390
6.118140	442.360952	7.249395
5.903383	447.697311	7.254400
5.926055	447.089535	7.259405
6.148471	456.679239	7.264410
6.024354	446.625015	7.269414
6.108451	437.338631	7.274419
6.065353	434.355609	7.279424
6.004517	425.860758	7.284429
6.028081	424.756118	7.289434
5.635082	427.753831	7.294438
5.886844	419.855432	7.299443
5.621079	423.766547	7.304448
5.681538	429.993118	7.309453
6.293787	443.229779	7.314458
6.117229	447.709074	7.319462
5.813584	434.025560	7.324467
6.077958	424.081328	7.329472
5.928866	434.146857	7.334477
5.983110	426.621099	7.339482
6.095625	429.602885	7.344486
5.826680	423.564160	7.349491
5.393590	430.130661	7.354496
5.536366	442.548671	7.359501
6.034334	447.207027	7.364506
6.174638	455.129583	7.369510
6.284516	446.857919	7.374515
6.107354	457.696678	7.379520
5.881779	438.527442	7.384525
6.276001	441.221474	7.389530
5.828241	438.925135	7.394534
5.769418	431.126016	7.399539
5.639003	432.595573	7.404544
6.029898	443.873684	7.409549
6.040785	444.302339	7.414554
5.821514	457.378219	7.419558
6.070147	455.953565	7.424563
5.788148	449.625800	7.429568
5.969748	451.783652	7.434573
6.076939	456.183688	7.439578
6.292281	462.753011	7.444582
5.889297	434.857158	7.449587
5.831572	434.733396	7.454592
5.633934	426.003706	7.459597
6.198114	442.668032	7.464602
5.848784	449.749781	7.469606
5.849336	452.606740	7.474611
5.892089	468.065094	7.479616
6.346099	468.573022	7.484621
5.971484	447.677509	7.489626
5.927751	437.167755	7.494630
6.253173	435.607680	7.499635
5.946138	432.137648	7.504640
5.840068	425.478596	7.509645
5.943487	431.198546	7.514650
5.889085	432.798567	7.519654
5.836228	426.586774	7.524659
5.734360	437.274513	7.529664
5.926178	430.157484	7.534669
6.262092	424.137887	7.539674
5.856512	430.620982	7.544678
6.046223	424.497737	7.549683
6.007787	428.287811	7.554688
5.954930	432.377548	7.559693
6.098536	427.685264	7.564698
5.707837	429.088031	7.569702
5.788824	432.672727	7.574707
6.138769	436.575963	7.579712
5.679289	431.326415	7.584717
6.119602	430.684842	7.589722
5.913033	441.319384	7.594726
6.217561	431.542869	7.599731
5.746734	429.886082	7.604736
5.768655	426.703043	7.609741
5.994370	422.611684	7.614746
5.758558	434.861209	7.619750
6.063356	435.060308	7.624755
6.073399	440.826531	7.629760
5.713000	428.626273	7.634765
6.258608	436.295486	7.639770
5.795993	430.660438	7.644774
5.944494	427.337339	7.649779
5.683990	427.166251	7.654784
5.666411	436.455013	7.659789
5.505527	437.913525	7.664794
5.844975	460.020120	7.669798
6.090543	460.646131	7.674803
6.312154	455.963764	7.679808
5.912394	452.954361	7.684813
6.215192	454.792657	7.689818
6.109683	458.384431	7.694822
6.297872	446.936632	7.699827
5.768052	444.801852	7.704832
5.840612	445.284120	7.709837
6.160864	435.821526	7.714842
5.736764	437.283313	7.719846
6.122723	432.037346	7.724851
5.856978	436.337616	7.729856
5.482846	431.647354	7.734861
5.648946	441.628700	7.739866
5.944712	459.676575	7.744870
6.271792	460.808689	7.749875
6.375711	453.727569	7.754880
5.678884	449.103683	7.759885
5.758750	448.708417	7.764890
5.701304	460.044130	7.769894
5.978894	458.216291	7.774899
6.165506	452.068212	7.779904
6.247683	463.790189	7.784909
6.233526	450.570688	7.789914
6.001461	446.525738	7.794918
6.078499	439.983529	7.799923
5.760033	433.623517	7.804928
5.442924	424.336725	7.809933
6.146136	436.344207	7.814938
6.190239	450.176109	7.819942
6.308699	442.124574	7.824947
6.160673	428.812164	7.829952
5.729441	424.149834	7.834957
6.253534	423.985533	7.839962
5.774639	425.588786	7.844966
6.073005	427.921336	7.849971
5.973008	430.360596	7.854976
6.087037	426.236113	7.859981
6.195096	430.832166	7.864986
6.026589	438.951801	7.869990
6.183498	427.613323	7.874995
6.257816	426.725364	7.880000
6.507591	430.742374	7.885005
6.276792	426.741524	7.890010
6.028532	423.540704	7.895014
5.794142	411.915521	7.900019
6.034170	414.823540	7.905024
6.044574	412.999602	7.910029
6.232940	397.976647	7.915034
5.803765	407.013498	7.920038
5.771790	404.104671	7.925043
5.818954	406.663244	7.930048
5.352092	400.940283	7.935053
6.046025	409.614497	7.940058
5.884306	420.254655	7.945062
6.564167	422.954551	7.950067
6.064269	416.344553	7.955072
5.823698	413.860726	7.960077
6.015585	406.604485	7.965082
5.782885	413.490772	7.970086
5.774828	402.877369	7.975091
5.803940	413.639488	7.980096
6.045689	420.615959	7.985101
6.406450	427.997744	7.990106
5.887834	422.339835	7.995110
5.959075	414.729159	8.000115
5.771489	407.312559	8.005133
5.904634	406.130444	8.010150
5.681749	417.892344	8.015168
6.013990	429.295876	8.020186
6.069838	426.017803	8.025203
5.970764	435.040025	8.030221
6.092345	428.302374	8.035238
6.162829	418.227596	8.040256
5.970606	411.690596	8.045274
5.705202	404.458168	8.050291
5.558224	403.973191	8.055309
5.728136	426.011908	8.060326
6.025723	425.596129	8.065344
5.544674	428.170961	8.070362
5.909843	425.737511	8.075379
5.970932	431.455773	8.080397
5.875922	430.637606	8.085414
6.217759	421.994063	8.090432
5.559541	428.064866	8.095450
6.172878	427.624862	8.100467
5.857374	424.477556	8.105485
6.095001	427.321635	8.110502
6.092063	421.954173	8.115520
6.049543	427.253169	8.120538
6.122544	424.133354	8.125555
5.607697	429.872426	8.130573
5.640418	431.533631	8.135590
6.247981	430.867315	8.140608
6.257708	453.044771	8.145626
6.051662	442.259072	8.150643
6.175597	431.027204	8.155661
6.069389	437.835181	8.160678
6.094154	430.790807	8.165696
5.974813	440.747166	8.170714
5.983284	443.601906	8.175731
6.492304	442.660695	8.180749
6.333542	447.334128	8.185766
6.342475	432.566855	8.190784
5.983756	432.582109	8.195802
6.149419	432.508891	8.200819
6.250274	423.555969	8.205837
5.863340	425.200875	8.210854
6.226513	420.337782	8.215872
6.060894	425.665531	8.220890
6.231848	427.639591	8.225907
6.026196	420.991084	8.230925
6.024738	436.852386	8.235942
6.517626	434.354743	8.240960
5.869249	434.869815	8.245978
6.126790	440.696154	8.250995
6.255827	456.505470	8.256013
6.384861	457.125954	8.261030
6.452411	445.211792	8.266048
6.156280	447.202234	8.271066
6.293962	432.023470	8.276083
6.181212	428.797059	8.281101
6.253115	433.222909	8.286118
6.225221	427.679476	8.291136
6.330390	434.072483	8.296154
6.023488	426.351089	8.301171
6.413306	443.975138	8.306189
5.918353	445.460247	8.311206
6.485334	445.687066	8.316224
6.275960	450.974341	8.321242
6.394278	449.478967	8.326259
6.335529	442.498167	8.331277
5.884634	441.704202	8.336294
6.582836	441.067864	8.341312
6.318647	451.097416	8.346330
6.180041	448.209567	8.351347
5.997970	455.190383	8.356365
6.251858	451.625657	8.361382
6.149588	448.631129	8.366400
6.335670	452.673022	8.371418
6.433960	459.338514	8.376435
6.870461	451.027263	8.381453
6.290478	459.241225	8.386470
6.554488	459.622811	8.391488
6.075846	451.388674	8.396506
6.241792	452.675559	8.401523
6.205600	454.309694	8.406541
5.849632	455.672042	8.411558
5.971605	444.939087	8.416576
6.271986	457.559454	8.421594
6.392220	450.093017	8.426611
6.747046	457.642961	8.431629
6.420662	458.060246	8.436646
6.491162	449.238299	8.441664
6.549554	452.003167	8.446682
6.562764	449.874168	8.451699
6.554437	443.298876	8.456717
6.323565	445.989146	8.461734
6.571215	449.336584	8.466752
6.156438	449.726694	8.471770
6.204056	455.844704	8.476787
6.517364	448.392198	8.481805
6.055624	454.088243	8.486822
6.426529	454.311070	8.491840
6.194132	462.618896	8.496858
6.215095	451.835492	8.501875
6.599562	444.842051	8.506893
6.523937	460.266872	8.511910
6.560301	456.568970	8.516928
6.331169	456.207315	8.521946
6.347074	461.531880	8.526963
6.535345	456.273305	8.531981
6.487691	465.846062	8.536998
6.790466	458.268970	8.542016
6.884132	454.060319	8.547034
6.481029	452.507786	8.552051
6.848513	453.794651	8.557069
6.460729	453.713474	8.562087
6.532315	444.645207	8.567104
6.563898	451.579922	8.572122
6.405335	462.703771	8.577139
6.663685	457.068143	8.582157
6.341550	447.275770	8.587175
6.780556	460.281516	8.592192
6.363320	461.524076	8.597210
6.360047	455.115244	8.602227
6.874169	456.814634	8.607245
6.427247	460.274057	8.612263
6.637891	449.012813	8.617280
6.473699	448.704100	8.622298
6.245002	451.539196	8.627315
6.427143	459.182469	8.632333
6.097264	464.021572	8.637351
6.606998	470.215504	8.642368
6.738263	475.790241	8.647386
6.860122	484.339217	8.652403
6.907326	466.025113	8.657421
6.371932	462.978525	8.662439
6.515122	468.036997	8.667456
7.201312	468.740598	8.672474
6.395631	469.832582	8.677491
6.564718	466.123350	8.682509
6.399556	476.746470	8.687527
6.863443	479.592976	8.692544
6.791227	474.072252	8.697562
6.681242	478.371978	8.702579
6.942333	473.247154	8.707597
6.726366	474.382441	8.712615
6.468847	464.649362	8.717632
6.466365	462.866801	8.722650
6.622634	483.080521	8.727667
6.827301	478.422127	8.732685
6.444147	478.927203	8.737703
7.049883	480.208299	8.742720
7.110457	477.538545	8.747738
6.763009	476.201352	8.752755
6.926578	464.262666	8.757773
6.443320	470.823620	8.762791
6.867917	479.041138	8.767808
7.252371	472.076090	8.772826
6.937459	460.679433	8.777843
6.568018	462.656117	8.782861
6.556938	455.166071	8.787879
6.544973	459.933271	8.792896
6.579791	466.820148	8.797914
6.591649	473.603329	8.802931
6.883742	468.337950	8.807949
6.904492	479.386377	8.812967
6.756904	474.981992	8.817984
6.894909	486.343410	8.823002
6.620357	480.065437	8.828019
7.247333	475.041075	8.833037
6.784064	473.090870	8.838055
6.831048	472.982598	8.843072
6.711059	473.960836	8.848090
6.576110	481.309818	8.853107
6.752118	481.525313	8.858125
6.556814	471.517395	8.863143
6.476028	471.577465	8.868160
6.887914	469.682643	8.873178
6.374848	479.776452	8.878195
6.926543	478.897981	8.883213
6.841806	483.433593	8.888231
6.975831	485.845790	8.893248
6.742103	479.690808	8.898266
6.740690	490.111555	8.903283
7.237983	494.647494	8.908301
7.026295	493.001851	8.913319
7.039924	488.966677	8.918336
6.927898	473.801757	8.923354
6.583770	480.807973	8.928371
7.130515	487.690389	8.933389
6.731504	484.802309	8.938407
6.813610	490.870746	8.943424
6.927907	492.923118	8.948442
7.096522	503.001652	8.953459
7.487871	498.301381	8.958477
7.085175	495.719989	8.963495
6.684485	484.844841	8.968512
7.166411	486.934285	8.973530
7.017417	510.815568	8.978547
6.668060	507.301167	8.983565
7.021596	512.295136	8.988583
7.017611	509.023266	8.993600
6.961023	507.138726	8.998618
7.424204	509.044918	9.003635
7.414355	503.372402	9.008653
7.031446	496.537044	9.013671
7.183801	494.824894	9.018688
7.314546	484.743793	9.023706
7.014161	479.612266	9.028723
6.792720	483.774822	9.033741
6.974950	479.252488	9.038759
6.766507	496.806224	9.043776
7.242986	493.522194	9.048794
7.097824	509.096807	9.053811
7.423783	499.461637	9.058829
7.298652	494.024937	9.063847
7.032705	482.522764	9.068864
7.327493	478.932690	9.073882
6.797151	479.908951	9.078899
6.863161	491.625635	9.083917
7.245359	504.372070	9.088935
6.973875	510.366527	9.093952
7.506422	504.545911	9.098970
7.064842	520.649816	9.103987
7.127572	511.955287	9.109005
7.315746	511.386236	9.114023
7.038451	507.810051	9.119040
7.062368	514.023313	9.124058
7.158551	507.564166	9.129075
6.864312	508.121584	9.134093
7.122037	506.948345	9.139111
7.107083	512.555470	9.144128
7.509765	510.021458	9.149146
7.154353	512.409359	9.154163
7.190398	510.418786	9.159181
7.305780	501.952697	9.164199
7.113929	503.232530	9.169216
7.321983	493.514851	9.174234
7.092592	503.728329	9.179251
7.389283	508.535543	9.184269
7.103842	505.837948	9.189287
7.149314	508.327139	9.194304
7.415857	498.508775	9.199322
7.236799	502.671007	9.204339
7.168842	500.191801	9.209357
6.930671	496.928225	9.214375
6.733367	512.324818	9.219392
7.169111	516.658968	9.224410
7.440362	526.109207	9.229427
7.440099	524.383097	9.234445
7.383752	530.577383	9.239463
7.096955	522.032288	9.244480
7.362744	513.933948	9.249498
7.568141	523.871030	9.254515
7.331817	528.686024	9.259533
7.712704	521.364911	9.264551
7.445201	521.750882	9.269568
7.578659	510.741534	9.274586
7.163146	511.314796	9.279603
7.074681	503.186759	9.284621
7.476945	513.474843	9.289639
7.381610	528.075990	9.294656
7.631855	526.878675	9.299674
6.759956	518.696656	9.304691
7.023200	524.465324	9.309709
7.682879	531.314283	9.314727
7.472967	534.465185	9.319744
7.652756	535.039850	9.324762
7.463781	529.925568	9.329779
7.464990	535.530168	9.334797
7.567102	536.265327	9.339815
7.571351	538.360193	9.344832
7.734539	535.532342	9.349850
7.377893	542.098730	9.354867
7.901683	541.593859	9.359885
7.352534	531.802295	9.364903
7.351946	531.370116	9.369920
7.486919	528.032290	9.374938
7.619236	539.211597	9.379955
7.497034	529.627694	9.384973
7.633802	536.615390	9.389991
7.552390	538.569043	9.395008
7.656604	534.456550	9.400026
7.757857	534.983560	9.405043
7.247192	522.718129	9.410061
7.244778	524.867687	9.415079
7.308271	534.341015	9.420096
7.363111	538.643332	9.425114
7.370606	537.029614	9.430131
7.748784	536.623297	9.435149
7.355687	536.890091	9.440167
7.497648	539.698684	9.445184
7.629418	532.921527	9.450202
7.562625	534.106028	9.455219
7.087621	531.220380	9.460237
7.620854	530.663536	9.465255
7.206676	534.562812	9.470272
7.627355	540.559283	9.475290
7.669369	548.252952	9.480307
7.658839	552.505554	9.485325
7.828541	558.484550	9.490343
7.627461	548.464871	9.495360
8.089431	539.739333	9.500378
7.476231	535.392107	9.505395
7.268994	532.552867	9.510413
7.890227	551.649240	9.515431
7.763560	558.274276	9.520448
7.864139	552.227835	9.525466
7.839332	544.790396	9.530483
7.709273	537.864912	9.535501
7.642460	528.600536	9.540519
7.429270	542.588999	9.545536
7.808812	555.083422	9.550554
7.774651	567.424922	9.555571
7.809814	563.774523	9.560589
7.765382	560.480579	9.565607
7.402072	560.253555	9.570624
8.203662	562.848347	9.575642
7.918566	561.599208	9.580659
7.375047	564.310079	9.585677
7.780653	564.489601	9.590695
8.209439	571.399998	9.595712
8.147066	557.751485	9.600730
8.110126	556.599165	9.605747
7.937959	543.340252	9.610765
7.731128	539.686748	9.615783
7.822311	542.799944	9.620800
7.937178	534.936680	9.625818
7.857854	541.276581	9.630835
7.515219	537.802146	9.635853
8.065079	543.809936	9.640871
8.067510	555.748063	9.645888
7.522056	537.280591	9.650906
7.981901	551.214102	9.655923
7.950513	552.658145	9.660941
8.221153	549.415823	9.665959
7.971925	548.571321	9.670976
7.638472	534.438279	9.675994
7.866575	542.632964	9.681011
7.763150	554.363613	9.686029
7.970824	549.045166	9.691047
7.927322	557.806278	9.696064
8.072569	562.391082	9.701082
7.815733	552.572641	9.706099
8.239401	567.149307	9.711117
8.162721	560.281723	9.716135
7.479790	550.261800	9.721152
7.441278	556.964542	9.726170
7.729613	557.077231	9.731187
7.738644	559.666813	9.736205
8.142853	565.640627	9.741223
7.978307	567.963916	9.746240
7.932269	558.036704	9.751258
8.113643	564.004406	9.756275
7.769302	568.864737	9.761293
8.056433	561.324767	9.766311
7.855122	574.244728	9.771328
7.836819	566.216124	9.776346
7.943257	562.794399	9.781363
7.721268	567.837532	9.786381
8.068046	574.363147	9.791399
8.002584	585.516666	9.796416
8.337100	591.308903	9.801434
8.341312	584.485441	9.806451
7.743284	573.126759	9.811469
8.348308	579.905405	9.816487
7.991132	589.028105	9.821504
8.582620	589.487773	9.826522
8.344371	573.746095	9.831539
7.772730	574.258615	9.836557
8.325848	568.400042	9.841575
8.304641	567.677602	9.846592
7.881886	571.174286	9.851610
8.121221	569.107673	9.856627
8.239111	580.671119	9.861645
8.209183	582.190675	9.866663
8.140396	593.571939	9.871680
7.943397	589.948443	9.876698
7.945254	589.547438	9.881715
8.367712	586.852526	9.886733
8.496275	594.194981	9.891751
8.440895	599.953636	9.896768
8.227141	593.448345	9.901786
8.559712	595.210908	9.906803
8.299152	584.490469	9.911821
8.127630	566.731242	9.916839
8.240759	566.410634	9.921856
7.930447	586.482980	9.926874
8.077000	583.960685	9.931891
7.932139	586.943614	9.936909
8.265494	598.053588	9.941927
8.487399	596.384181	9.946944
8.157160	589.736196	9.951962
8.442516	587.245802	9.956979
7.906706	586.736535	9.961997
7.829030	585.284481	9.967015
8.570353	593.250454	9.972032
8.477840	589.364433	9.977050
8.457155	588.452562	9.982067
8.052913	593.880866	9.987085
8.862695	583.308306	9.992103
8.423758	594.119558	9.997120
8.368747	597.429239	10.002138
8.424401	587.047420	10.007155
8.576817	594.420852	10.012173
8.528512	580.464003	10.017191
8.607117	589.467931	10.022208
8.215958	591.634224	10.027226
8.506065	589.490226	10.032243
8.222842	588.562685	10.037261
8.242872	590.134375	10.042279
8.452971	593.238415	10.047296
8.207398	581.442651	10.052314
8.384893	587.250022	10.057331
7.952696	590.577774	10.062349
8.519734	597.766323	10.067367
8.680040	603.488029	10.072384
8.462508	601.754928	10.077402
8.436186	605.909031	10.082419
8.625010	604.472025	10.087437
8.685758	596.532007	10.092455
8.242257	594.638651	10.097472
8.731202	608.813801	10.102490
8.911664	599.053051	10.107507
8.507067	596.200542	10.112525
8.515609	588.423342	10.117543
8.435482	591.017431	10.122560
8.602066	589.748013	10.127578
8.574434	586.249460	10.132595
8.500649	584.935653	10.137613
8.729421	598.002841	10.142631
8.665019	594.831941	10.147648
8.458073	590.765033	10.152666
8.641084	597.742351	10.157683
8.439061	607.588680	10.162701
8.684284	612.372429	10.167719
9.005234	615.115120	10.172736
9.120162	607.131894	10.177754
9.158524	590.232856	10.182771
8.596201	586.874884	10.187789
8.872343	586.973705	10.192807
8.873508	584.104959	10.197824
8.567354	584.941957	10.202842
8.424152	581.180645	10.207859
8.418617	589.143714	10.212877
8.447569	589.568445	10.217895
8.641927	591.188560	10.222912
8.496090	592.697876	10.227930
8.781262	603.206330	10.232947
8.972402	618.116117	10.237965
8.951517	608.828724	10.242983
8.404992	599.134542	10.248000
8.762416	613.270342	10.253018
9.158824	611.087595	10.258035
9.068063	604.553562	10.263053
8.536814	600.483814	10.268071
8.826908	596.866049	10.273088
8.718359	601.932443	10.278106
8.823872	603.787388	10.283123
8.866402	616.871147	10.288141
8.833205	610.586870	10.293159
9.043622	607.918866	10.298176
9.024657	611.487991	10.303194
8.987580	588.989724	10.308211
8.675546	590.026461	10.313229
8.572373	596.540531	10.318247
8.711732	585.931001	10.323264
8.972663	602.966329	10.328282
8.859327	604.549449	10.333299
9.234147	612.364571	10.338317
9.032436	613.024259	10.343335
8.901878	603.883441	10.348352
8.989710	609.417688	10.353370
8.935907	607.955580	10.358387
8.887566	604.132063	10.363405
9.005817	609.194482	10.368423
8.946922	605.928042	10.373440
8.740582	613.493393	10.378458
8.518797	607.850895	10.383475
8.876528	610.026086	10.388493
8.986754	609.090547	10.393511
9.418565	604.390220	10.398528
9.044261	610.946777	10.403546
9.190090	605.593822	10.408563
9.168718	609.267465	10.413581
9.144881	610.378969	10.418599
9.073599	609.197312	10.423616
9.051116	611.024974	10.428634
9.123447	612.885119	10.433651
9.485925	611.562916	10.438669
8.765611	604.376437	10.443687
8.855563	603.103246	10.448704
9.011245	608.226072	10.453722
9.090850	611.378964	10.458739
8.960074	611.235426	10.463757
8.992636	617.068671	10.468775
9.308499	602.587684	10.473792
9.273157	618.788974	10.478810
9.228794	611.076858	10.483827
9.004487	605.340081	10.488845
9.138953	602.803899	10.493863
9.410678	616.019006	10.498880
9.013942	618.634302	10.503898
9.198588	621.272118	10.508915
9.308558	617.638389	10.513933
9.434525	614.118920	10.518951
9.160284	606.783653	10.523968
9.243568	610.712300	10.528986
8.808790	611.708308	10.534003
9.213903	612.667396	10.539021
9.107350	618.235258	10.544039
9.327407	614.697891	10.549056
8.905421	617.935685	10.554074
8.965755	624.310538	10.559091
9.392636	622.618480	10.564109
9.416804	624.476704	10.569127
9.624268	613.373646	10.574144
9.136723	613.298631	10.579162
9.257294	617.789486	10.584179
9.315625	615.110595	10.589197
9.572234	616.175003	10.594215
9.478881	614.823233	10.599232
8.990246	625.276215	10.604250
9.498925	619.680210	10.609267
9.354812	615.385700	10.614285
9.148573	619.536437	10.619303
9.395378	618.159774	10.624320
9.482534	628.257453	10.629338
9.627420	622.008386	10.634355
9.450126	621.783774	10.639373
9.220264	620.519665	10.644391
9.687176	607.482466	10.649408
9.548665	617.243110	10.654426
9.879957	608.938803	10.659443
9.738891	617.172429	10.664461
9.371542	620.306989	10.669479
9.453092	621.282059	10.674496
9.467691	617.874714	10.679514
9.318810	619.905219	10.684531
9.534622	619.934597	10.689549
9.163484	622.085134	10.694567
9.459164	613.294096	10.699584
9.583552	623.849845	10.704602
9.260452	611.267785	10.709619
9.206127	612.349351	10.714637
9.300504	616.140561	10.719655
9.585051	609.705513	10.724672
9.210299	615.659381	10.729690
9.593575	624.331567	10.734707
9.829655	614.221265	10.739725
9.451880	615.303017	10.744743
9.591398	611.869788	10.749760
9.470043	619.428138	10.754778
9.785036	628.735878	10.759795
9.439257	620.626013	10.764813
9.322951	626.435248	10.769831
9.604539	631.055512	10.774848
9.663068	641.896148	10.779866
9.654653	645.558301	10.784883
10.138575	652.232872	10.789901
9.452370	649.818955	10.794919
9.715423	646.129678	10.799936
9.899813	649.278781	10.804954
9.676062	641.572668	10.809971
9.533983	642.415520	10.814989
9.293974	640.894221	10.820007
9.813379	638.679576	10.825024
9.709760	643.732587	10.830042
9.790100	654.191113	10.835059
9.858147	641.500409	10.840077
9.939996	643.163404	10.845095
10.107716	641.764416	10.850112
9.875283	640.503864	10.855130
9.910238	632.561559	10.860147
9.649963	626.618970	10.865165
9.674471	628.653868	10.870183
9.740506	631.546956	10.875200
9.974539	643.726567	10.880218
9.520849	643.368534	10.885235
9.809590	631.971861	10.890253
9.585645	647.558939	10.895271
9.473606	636.483836	10.900288
9.940552	645.000910	10.905306
8.925394	643.537946	10.910323
9.626720	639.458106	10.915341
9.411580	647.709664	10.920359
9.758813	665.747707	10.925376
9.835821	670.882878	10.930394
9.629378	668.163413	10.935411
9.975780	668.169175	10.940429
9.794171	672.934609	10.945447
9.909103	666.655505	10.950464
10.338060	668.737492	10.955482
10.075535	664.512016	10.960499
10.419772	663.927976	10.965517
9.983921	675.410985	10.970535
9.903039	668.383071	10.975552
9.912370	669.517784	10.980570
9.443013	670.740121	10.985587
10.172817	666.649502	10.990605
10.340074	682.232120	10.995623
9.948813	668.754975	11.000640
9.764970	668.569258	11.005658
9.794259	680.522195	11.010675
10.143768	679.880524	11.015693
9.961036	680.256371	11.020711
9.878826	668.819965	11.025728
10.248352	673.527450	11.030746
9.835088	671.518893	11.035763
10.508770	670.075343	11.040781
10.015955	676.682050	11.045799
10.074051	669.764905	11.050816
10.161763	669.760705	11.055834
10.015630	679.995952	11.060851
10.494863	666.723248	11.065869
10.227930	675.165972	11.070887
10.116641	679.074627	11.075904
10.494196	675.430519	11.080922
10.288631	679.300296	11.085939
10.221212	674.886456	11.090957
10.080235	680.159927	11.095975
10.016494	673.097766	11.100992
10.430674	670.912228	11.106010
10.296018	684.522420	11.111027
10.262780	678.960811	11.116045
10.380969	671.519849	11.121063
10.333503	668.942735	11.126080
10.324619	672.257826	11.131098
10.025551	676.470459	11.136115
10.212522	674.459376	11.141133
10.618444	667.598188	11.146151
10.472626	666.926827	11.151168
10.590316	669.474154	11.156186
10.743901	670.873445	11.161203
10.759133	672.408024	11.166221
10.485775	680.214279	11.171239
10.621709	668.964603	11.176256
10.330740	649.914338	11.181274
10.287401	645.506200	11.186291
9.962641	648.015549	11.191309
10.438392	663.969542	11.196327
10.222805	663.908721	11.201344
10.301587	666.351689	11.206362
10.466365	672.123210	11.211379
10.230518	665.488809	11.216397
10.226879	670.942732	11.221415
10.118205	665.553894	11.226432
10.172189	677.992114	11.231450
10.013910	676.770434	11.236467
10.194216	663.257388	11.241485
10.137537	676.322021	11.246503
10.188158	690.777354	11.251520
10.542338	691.286831	11.256538
10.266650	693.905263	11.261555
10.422512	689.680500	11.266573
10.739529	696.870393	11.271591
10.434812	691.401810	11.276608
10.541449	681.163427	11.281626
10.531271	694.343865	11.286643
10.470669	689.569188	11.291661
10.773144	693.091122	11.296679
10.251674	691.503464	11.301696
10.612622	703.521218	11.306714
10.301473	691.650448	11.311731
10.429831	695.767713	11.316749
10.720782	688.943466	11.321767
10.588848	688.333046	11.326784
10.906278	693.626215	11.331802
10.535542	694.754206	11.336819
10.323321	684.108185	11.341837
10.367828	691.953005	11.346855
10.277298	708.074659	11.351872
10.828294	704.974577	11.356890
10.401152	722.158853	11.361907
10.768130	709.272939	11.366925
10.750400	719.361857	11.371943
10.523457	711.829785	11.376960
11.010965	722.682152	11.381978
10.851373	723.653985	11.386995
10.971551	712.021737	11.392013
10.780010	713.102718	11.397031
10.809592	719.974734	11.402048
11.458801	705.832760	11.407066
11.144576	707.175962	11.412083
11.069570	699.096220	11.417101
10.724612	698.759020	11.422119
11.237101	685.979713	11.427136
10.928480	685.106640	11.432154
10.947074	695.972500	11.437171
11.113677	695.312148	11.442189
10.912350	679.574059	11.447207
10.937088	686.926508	11.452224
11.117140	686.339790	11.457242
11.252236	688.755003	11.462259
10.954626	681.915677	11.467277
10.817533	677.064624	11.472295
11.069892	688.345137	11.477312
11.186231	686.316717	11.482330
11.200365	684.055000	11.487347
11.144520	692.455192	11.492365
11.221061	689.107556	11.497383
10.741999	695.604817	11.502400
11.145362	682.088366	11.507418
11.201048	686.415834	11.512435
11.077530	686.952819	11.517453
10.970338	685.448576	11.522471
10.848732	683.874008	11.527488
10.964876	687.160045	11.532506
11.244306	688.823646	11.537523
11.084798	682.565445	11.542541
11.230471	684.376236	11.547559
11.168131	686.071295	11.552576
11.088639	685.894474	11.557594
10.906733	682.262283	11.562611
11.112382	683.782807	11.567629
11.278813	683.466469	11.572647
11.005079	696.732384	11.577664
10.832902	685.843400	11.582682
11.233494	691.357071	11.587699
10.943953	690.641956	11.592717
11.247705	685.403090	11.597735
10.754800	692.401141	11.602752
11.219214	685.221510	11.607770
11.335844	689.249092	11.612787
11.090754	686.541991	11.617805
11.453027	686.065579	11.622823
11.059231	691.568015	11.627840
11.129479	684.538506	11.632858
10.921990	690.756528	11.637875
11.086934	704.758455	11.642893
11.691330	709.602720	11.647911
11.361967	706.328146	11.652928
11.452949	695.290625	11.657946
11.197949	688.428841	11.662963
11.458561	694.762872	11.667981
11.363021	697.782273	11.672999
10.998500	699.751899	11.678016
11.180596	694.863454	11.683034
11.124897	718.383254	11.688051
11.201961	712.277327	11.693069
11.497402	715.099771	11.698087
11.355134	713.534749	11.703104
11.298873	712.704186	11.708122
11.194233	711.448853	11.713139
11.333930	713.651907	11.718157
11.154930	720.689150	11.723175
11.132135	721.857302	11.728192
11.658832	721.336191	11.733210
11.467453	716.954387	11.738227
11.119693	724.788098	11.743245
11.361003	720.063940	11.748263
11.507867	731.266334	11.753280
11.533685	739.672687	11.758298
11.571034	744.709950	11.763315
11.771079	742.027773	11.768333
11.921465	723.495265	11.773351
11.423949	723.229304	11.778368
11.378705	719.203303	11.783386
11.670433	725.384145	11.788403
11.374977	728.791485	11.793421
11.724572	733.764043	11.798439
11.794494	738.089292	11.803456
11.763362	731.956129	11.808474
12.070421	719.250012	11.813491
11.403681	722.418874	11.818509
11.321155	704.762332	11.823527
11.413137	725.762735	11.828544
12.070581	738.393628	11.833562
11.782748	729.122751	11.838579
11.578921	733.582410	11.843597
11.943627	730.596721	11.848615
11.633065	722.042629	11.853632
11.796967	721.647791	11.858650
11.665902	720.794233	11.863667
11.411309	733.239814	11.868685
12.060380	738.215945	11.873703
12.143886	738.919313	11.878720
11.935372	725.779569	11.883738
11.760603	709.797448	11.888755
11.674246	720.780753	11.893773
11.690766	719.739969	11.898791
11.958204	734.685236	11.903808
11.853852	726.644794	11.908826
12.016662	734.641513	11.913843
11.740316	728.941252	11.918861
11.941128	730.932759	11.923879
11.859337	748.624689	11.928896
11.946234	740.620549	11.933914
12.044032	742.924847	11.938931
11.603952	742.309056	11.943949
12.304306	750.682312	11.948967
12.259152	746.476408	11.953984
12.290084	736.092063	11.959002
11.710098	726.513508	11.964019
11.586353	719.154615	11.969037
12.115584	733.904227	11.974055
12.144522	740.138872	11.979072
11.937019	737.391160	11.984090
12.051149	732.933081	11.989107
11.765586	752.301137	11.994125
12.442602	745.700406	11.999143
11.886868	743.060903	12.004160
11.909731	742.391513	12.009178
12.150021	737.995718	12.014195
12.343508	740.938283	12.019213
12.201648	733.632715	12.024231
12.335435	738.238295	12.029248
11.970571	728.474553	12.034266
12.194732	730.433999	12.039283
11.915293	733.059337	12.044301
12.228292	738.015539	12.049319
12.219038	740.358701	12.054336
12.190369	748.350712	12.059354
12.296271	742.581088	12.064371
12.080571	748.734144	12.069389
12.103132	735.611837	12.074407
11.994581	745.386791	12.079424
11.940144	749.043553	12.084442
12.046366	744.776062	12.089459
12.073315	745.137992	12.094477
12.481326	739.030697	12.099495
12.354969	737.109726	12.104512
12.377542	741.729576	12.109530
12.455424	736.557643	12.114547
12.083333	737.606953	12.119565
12.268142	742.277125	12.124583
12.110782	736.858023	12.129600
12.156859	741.565711	12.134618
12.263644	732.103614	12.139635
12.260011	742.897245	12.144653
12.117931	746.520401	12.149671
12.556174	743.311745	12.154688
12.162822	737.004957	12.159706
12.624168	747.100880	12.164723
11.824811	743.208808	12.169741
12.369071	750.378897	12.174759
12.272415	763.336247	12.179776
12.646161	772.884169	12.184794
12.399752	761.037924	12.189811
12.727007	767.238460	12.194829
12.737089	767.514671	12.199847
12.683344	770.429704	12.204864
12.512087	763.905069	12.209882
12.752854	769.260767	12.214899
12.675691	766.565213	12.219917
12.485733	758.481365	12.224935
12.350395	758.253333	12.229952
12.656978	762.557287	12.234970
12.877941	761.711688	12.239987
12.790366	760.573600	12.245005
12.596618	741.233447	12.250023
12.516383	747.892303	12.255040
12.824123	753.306931	12.260058
12.679900	744.089286	12.265075
12.423222	754.922572	12.270093
12.417259	755.605244	12.275111
12.551098	758.181612	12.280128
12.737771	770.258275	12.285146
12.836093	764.022766	12.290163
12.846088	769.395686	12.295181
13.101936	771.561614	12.300199
12.983652	766.123758	12.305216
12.300819	759.300577	12.310234
12.370762	751.169699	12.315251
12.834327	763.035713	12.320269
12.718704	759.554068	12.325287
13.085729	760.282444	12.330304
12.565614	765.605875	12.335322
12.810118	760.704479	12.340339
12.656481	763.893942	12.345357
12.614655	764.377104	12.350375
13.195679	770.591530	12.355392
12.765345	762.681044	12.360410
12.701747	766.891518	12.365427
12.894399	772.147457	12.370445
12.659310	762.278155	12.375463
12.389440	756.895611	12.380480
12.762412	761.141825	12.385498
12.933903	769.332862	12.390515
12.785878	775.639427	12.395533
12.775323	779.513386	12.400551
12.802763	779.752162	12.405568
13.494435	785.589491	12.410586
13.163767	781.494585	12.415603
13.314526	788.335018	12.420621
12.964728	782.898717	12.425639
13.055332	780.325200	12.430656
13.160060	775.833869	12.435674
13.618205	765.578235	12.440691
12.701895	760.325377	12.445709
12.903004	756.374379	12.450727
13.232262	762.637718	12.455744
13.004261	762.566217	12.460762
13.335328	759.219715	12.465779
12.943725	766.321845	12.470797
13.431325	775.290188	12.475815
13.463016	764.886773	12.480832
12.928289	756.617100	12.485850
13.114703	748.019844	12.490867
13.148123	758.561523	12.495885
13.206755	768.127256	12.500903
13.535942	767.684429	12.505920
13.186406	770.071442	12.510938
13.650765	759.161576	12.515955
13.115124	755.502741	12.520973
13.046112	755.557811	12.525991
13.386372	759.083305	12.531008
13.212788	770.484257	12.536026
13.457831	765.147267	12.541043
13.413925	763.368011	12.546061
13.020506	771.963144	12.551079
13.353600	773.337474	12.556096
13.188763	776.235200	12.561114
13.048604	777.942460	12.566131
13.545870	788.556650	12.571149
13.728456	782.692946	12.576167
13.764276	771.951204	12.581184
13.326911	777.886532	12.586202
13.403097	774.179169	12.591219
13.942690	783.628527	12.596237
13.486786	770.341316	12.601255
13.566623	759.759944	12.606272
13.272789	763.129166	12.611290
13.834458	768.027480	12.616307
13.671205	759.835304	12.621325
13.292473	762.817034	12.626343
13.480008	757.542707	12.631360
13.499399	774.735966	12.636378
13.813693	770.255983	12.641395
13.773050	778.006884	12.646413
13.434037	777.542516	12.651431
13.707828	767.157972	12.656448
13.460065	770.646211	12.661466
13.637708	772.098546	12.666483
13.484468	773.208243	12.671501
13.389421	775.668995	12.676519
13.669734	780.068589	12.681536
13.347367	783.133011	12.686554
13.547660	779.958476	12.691571
13.808912	779.882904	12.696589
13.376499	780.622926	12.701607
13.782357	773.259928	12.706624
13.554839	784.208584	12.711642
13.805906	776.030381	12.716659
13.822813	786.846067	12.721677
13.672528	785.042450	12.726695
13.860745	782.687172	12.731712
13.621923	784.990568	12.736730
13.584564	783.175570	12.741747
13.890068	783.219298	12.746765
13.760112	790.848496	12.751783
14.027551	781.395916	12.756800
13.568474	786.441543	12.761818
13.626068	798.939243	12.766835
13.779953	800.815032	12.771853
13.883582	805.800902	12.776871
14.277632	804.287543	12.781888
13.987173	800.262074	12.786906
14.268155	801.827611	12.791923
14.168368	795.358039	12.796941
13.943779	783.322164	12.801959
14.468551	777.890849	12.806976
13.742487	767.183274	12.811994
14.111818	775.933460	12.817011
14.219459	782.957374	12.822029
13.944960	769.701702	12.827047
14.325161	772.555057	12.832064
14.145901	776.253473	12.837082
14.190052	771.112062	12.842099
14.356429	774.762635	12.847117
14.017982	776.803924	12.852135
14.465604	772.826922	12.857152
14.503417	773.512204	12.862170
14.216401	770.092126	12.867187
13.758184	777.056372	12.872205
13.872424	773.235748	12.877223
14.364363	772.032107	12.882240
14.330449	778.311327	12.887258
14.316797	767.186013	12.892275
14.254853	777.079917	12.897293
14.273740	781.151237	12.902311
14.080655	777.179945	12.907328
14.067923	781.767467	12.912346
13.857716	771.367234	12.917363
14.360135	775.747807	12.922381
14.468352	778.407088	12.927399
14.566466	770.233917	12.932416
14.533229	779.012464	12.937434
14.201253	774.106712	12.942451
14.514670	778.232871	12.947469
13.918863	779.948406	12.952487
14.512187	772.060567	12.957504
14.247871	780.824827	12.962522
14.345897	779.676593	12.967539
14.642519	791.278445	12.972557
14.401184	797.107325	12.977575
14.544644	793.288430	12.982592
14.568371	799.669081	12.987610
14.518232	793.658797	12.992627
14.518402	792.137724	12.997645
14.351854	793.315781	13.002663
14.572533	799.678197	13.007680
14.670736	806.312274	13.012698
14.355115	798.664669	13.017715
14.441000	796.325423	13.022733
14.366423	800.872146	13.027751
14.715970	794.392134	13.032768
14.704807	803.334495	13.037786
14.198730	797.484011	13.042803
14.708242	794.743870	13.047821
14.873369	799.395049	13.052839
14.578007	795.969962	13.057856
14.680907	804.982816	13.062874
14.627445	802.192024	13.067891
14.612402	797.059880	13.072909
14.268892	801.093309	13.077927
14.873919	796.132260	13.082944
13.906868	795.804164	13.087962
14.198662	805.286047	13.092979
14.666826	818.240148	13.097997
14.596443	823.174391	13.103015
14.567464	819.369885	13.108032
14.488359	827.622303	13.113050
14.423588	830.109876	13.118067
14.552603	822.856507	13.123085
14.773162	835.880974	13.128103
15.194056	823.497781	13.133120
14.904562	823.748345	13.138138
14.904423	832.262952	13.143155
15.009224	821.848049	13.148173
14.874145	833.299813	13.153191
15.212679	821.232488	13.158208
15.012129	821.914092	13.163226
14.857329	819.505254	13.168243
14.748547	816.467503	13.173261
14.812639	828.815880	13.178279
15.254344	824.259116	13.183296
15.243956	825.229668	13.188314
14.824086	832.345720	13.193331
15.190318	827.605117	13.198349
15.281277	829.888407	13.203367
15.094386	828.084209	13.208384
14.949528	826.768896	13.213402
14.774494	826.938409	13.218419
14.927142	837.925366	13.223437
15.291380	852.369563	13.228455
15.632464	847.191074	13.233472
15.403862	838.898645	13.238490
15.218738	827.992667	13.243507
15.629195	821.929143	13.248525
15.138337	826.736759	13.253543
15.230048	812.104528	13.258560
15.289810	828.830758	13.263578
15.190589	827.864907	13.268595
15.366926	821.228984	13.273613
15.353761	824.541618	13.278631
15.084009	819.130634	13.283648
15.435692	821.224747	13.288666
15.066917	826.120534	13.293683
15.131470	821.919514	13.298701
15.485951	833.616472	13.303719
15.471384	828.601011	13.308736
15.538062	831.497186	13.313754
15.108202	831.618262	13.318771
14.992775	829.241124	13.323789
15.503001	849.481852	13.328807
15.532373	850.136901	13.333824
15.956986	859.433898	13.338842
15.396938	853.841165	13.343859
15.617697	843.348119	13.348877
15.962307	849.741629	13.353895
15.595238	832.385169	13.358912
15.473644	824.145409	13.363930
15.349861	833.556719	13.368947
15.318718	826.587222	13.373965
15.347613	841.254368	13.378983
15.767957	848.598550	13.384000
15.895395	838.934341	13.389018
15.686809	842.842497	13.394035
16.130501	838.383249	13.399053
15.519782	823.674871	13.404071
15.643242	822.607857	13.409088
16.167815	809.662464	13.414106
15.608618	824.630026	13.419123
15.922203	810.016683	13.424141
16.018221	806.678597	13.429159
15.759700	803.421308	13.434176
16.070903	813.051636	13.439194
15.675554	812.223703	13.444211
16.011679	804.975760	13.449229
15.950946	815.443861	13.454247
15.935737	813.211972	13.459264
16.253311	815.453442	13.464282
15.663707	814.384541	13.469299
16.244481	811.910948	13.474317
15.859807	817.134277	13.479335
15.601496	814.097863	13.484352
15.837693	811.690882	13.489370
15.607758	813.983421	13.494387
15.710201	812.351647	13.499405
15.896223	822.310867	13.504423
15.774637	818.763872	13.509440
15.457970	814.275439	13.514458
15.848495	820.674368	13.519475
15.901861	829.000707	13.524493
15.984584	837.483398	13.529511
16.309349	841.610951	13.534528
16.422999	831.267240	13.539546
15.866877	824.884936	13.544563
15.894812	820.923187	13.549581
16.206388	829.594084	13.554599
16.275324	838.034754	13.559616
16.631416	827.889749	13.564634
15.749912	825.995565	13.569651
16.217012	808.543144	13.574669
16.366067	810.662692	13.579687
15.994366	821.406740	13.584704
16.092528	813.782661	13.589722
16.017447	828.327230	13.594739
16.169605	836.013233	13.599757
16.192198	838.240962	13.604775
16.360746	843.759479	13.609792
16.335299	828.179898	13.614810
16.377931	844.489097	13.619827
16.434336	835.176853	13.624845
16.593752	836.698323	13.629863
16.460610	829.075764	13.634880
16.526040	843.030275	13.639898
16.377949	844.539964	13.644915
16.599246	833.399888	13.649933
16.205645	834.212728	13.654951
15.999470	823.663507	13.659968
16.130718	826.502227	13.664986
16.354217	845.639143	13.670003
16.588784	844.564187	13.675021
16.353781	848.429145	13.680039
16.147413	847.470612	13.685056
16.351839	834.108296	13.690074
15.922214	847.244110	13.695091
16.193635	840.536477	13.700109
16.319879	860.234610	13.705127
16.445085	865.097193	13.710144
16.769892	861.006868	13.715162
16.277906	868.708602	13.720179
16.676505	862.602739	13.725197
16.609778	864.077591	13.730215
16.680010	865.003955	13.735232
17.069539	857.132231	13.740250
16.864700	866.385840	13.745267
16.909258	857.649809	13.750285
16.588811	856.863787	13.755303
16.926029	861.989802	13.760320
17.190256	867.960404	13.765338
16.644673	850.770753	13.770355
16.667976	864.422606	13.775373
16.745884	864.552489	13.780391
16.553528	868.751603	13.785408
16.921812	866.762584	13.790426
16.638380	868.369222	13.795443
16.731624	863.942786	13.800461
16.789634	865.123533	13.805479
16.718946	861.675855	13.810496
16.826501	856.887409	13.815514
16.574219	861.913280	13.820531
16.399052	858.065397	13.825549
16.542672	865.487658	13.830567
16.785848	874.813091	13.835584
17.028645	879.329043	13.840602
16.932106	884.983783	13.845619
16.962238	886.904218	13.850637
17.284427	890.836521	13.855655
17.175344	892.892380	13.860672
17.309867	879.765049	13.865690
17.158090	885.434755	13.870707
17.486621	882.249577	13.875725
17.381646	871.381509	13.880743
17.167970	870.266327	13.885760
17.236982	859.288953	13.890778
17.126484	855.613979	13.895795
17.159127	862.144737	13.900813
17.319020	851.579170	13.905831
17.276404	850.645475	13.910848
17.344165	845.595019	13.915866
17.298792	855.953438	13.920883
17.572206	856.822719	13.925901
17.494365	854.408130	13.930919
17.675245	857.529419	13.935936
17.557345	856.456037	13.940954
17.649472	855.122526	13.945971
17.536326	855.029874	13.950989
17.233824	854.528224	13.956007
17.410125	855.889257	13.961024
17.480795	845.451285	13.966042
17.247366	854.728304	13.971059
17.382517	865.389809	13.976077
17.806546	842.680118	13.981095
17.343020	847.616004	13.986112
17.121109	849.055207	13.991130
17.240174	849.718294	13.996147
17.216247	853.790027	14.001165
17.218669	846.480741	14.006183
17.323860	856.695647	14.011200
17.347447	874.487959	14.016218
17.356683	873.886972	14.021235
17.537310	887.788754	14.026253
17.729014	883.391068	14.031271
17.628488	881.819491	14.036288
17.939118	876.333335	14.041306
17.847405	883.467420	14.046323
17.739695	881.707617	14.051341
17.876533	884.072090	14.056359
17.674692	880.051653	14.061376
17.837752	881.992286	14.066394
17.598498	874.231696	14.071411
17.522074	888.038051	14.076429
17.853603	876.501972	14.081447
17.481649	873.404457	14.086464
17.640963	877.270756	14.091482
17.282439	874.928545	14.096499
17.086606	874.306039	14.101517
18.070099	879.232968	14.106535
17.767925	895.416354	14.111552
18.190457	897.537246	14.116570
17.795544	885.124037	14.121587
17.954432	885.348532	14.126605
18.202643	893.597034	14.131623
17.438654	891.065879	14.136640
17.481350	894.830531	14.141658
18.242474	898.801364	14.146675
18.067805	904.443104	14.151693
18.371263	905.594865	14.156711
18.233599	906.585363	14.161728
18.404832	906.953094	14.166746
18.234438	892.484943	14.171763
17.960878	889.757025	14.176781
18.220980	885.140335	14.181799
18.145927	895.774831	14.186816
17.798052	890.543327	14.191834
18.182669	894.639423	14.196851
18.121529	896.072375	14.201869
18.516145	908.214383	14.206887
18.315827	910.780012	14.211904
18.319865	904.732799	14.216922
18.224557	900.004530	14.221939
18.227262	916.105451	14.226957
18.635060	907.236742	14.231975
18.433406	904.765804	14.236992
18.426268	890.032230	14.242010
18.178801	882.642160	14.247027
18.080249	896.388870	14.252045
18.048986	903.788054	14.257063
18.270315	902.219696	14.262080
18.301262	902.511575	14.267098
18.475586	906.757390	14.272115
18.308218	900.364642	14.277133
18.355280	894.541070	14.282151
18.680291	900.540030	14.287168
18.482771	893.012739	14.292186
18.640454	897.788189	14.297203
18.235938	902.011084	14.302221
18.531255	899.323424	14.307239
18.384062	895.824608	14.312256
18.669831	897.247389	14.317274
18.572970	887.703506	14.322291
18.627402	893.470297	14.327309
18.624569	894.101990	14.332327
18.558422	902.122033	14.337344
18.296991	899.325940	14.342362
18.955804	909.053338	14.347379
19.017287	917.630916	14.352397
18.440337	905.795337	14.357415
18.572123	910.559069	14.362432
18.828980	916.287840	14.367450
19.000048	919.981890	14.372467
18.890135	933.544212	14.377485
18.743719	928.704019	14.382503
18.589601	931.347620	14.387520
18.620114	930.793792	14.392538
18.709153	925.790474	14.397555
18.627545	927.911461	14.402573
19.102124	925.915250	14.407591
18.926954	931.487648	14.412608
18.954343	933.970264	14.417626
18.862880	931.396850	14.422643
19.084591	942.126891	14.427661
19.253864	931.215817	14.432679
19.283748	923.356231	14.437696
19.382061	921.639885	14.442714
19.230130	914.771331	14.447731
19.113633	926.731496	14.452749
19.409006	920.935284	14.457767
19.269549	925.511139	14.462784
19.123903	926.837412	14.467802
18.881392	914.457110	14.472819
18.736577	926.323879	14.477837
18.932117	930.525349	14.482855
18.997284	918.248319	14.487872
18.953112	918.069119	14.492890
19.487905	921.734584	14.497907
19.040548	923.865538	14.502925
19.577592	910.185956	14.507943
19.384833	923.319429	14.512960
19.467124	926.459332	14.517978
19.434805	920.342070	14.522995
19.202024	919.327710	14.528013
19.335073	918.357021	14.533031
19.658238	919.272160	14.538048
19.583486	921.811805	14.543066
19.434029	920.055382	14.548083
19.052522	922.999703	14.553101
19.085803	916.480836	14.558119
19.148392	919.207249	14.563136
19.375013	933.818244	14.568154
19.767154	939.784608	14.573171
19.808033	944.616242	14.578189
19.737271	940.029287	14.583207
19.593045	925.670621	14.588224
19.128841	924.676741	14.593242
19.773335	939.070786	14.598259
19.565574	947.311858	14.603277
19.628166	941.470059	14.608295
19.738601	948.907022	14.613312
19.685137	955.321914	14.618330
20.120729	941.393110	14.623347
19.715839	944.218019	14.628365
19.827784	946.065680	14.633383
19.899790	947.512490	14.638400
19.737046	949.851325	14.643418
20.439821	935.886975	14.648435
19.492673	936.373128	14.653453
20.030476	924.817323	14.658471
19.505229	925.597143	14.663488
19.838390	933.709275	14.668506
20.078008	939.667977	14.673523
19.825644	941.853591	14.678541
19.817462	947.188386	14.683559
20.165001	949.453582	14.688576
20.044521	941.762717	14.693594
19.892571	935.572673	14.698611
19.669912	950.490766	14.703629
19.818504	939.412510	14.708647
19.847865	950.794402	14.713664
19.630120	960.596050	14.718682
19.599743	944.385963	14.723699
19.585109	958.558240	14.728717
20.240861	965.852964	14.733735
20.256636	977.006622	14.738752
19.951309	982.148137	14.743770
20.260444	972.165047	14.748787
20.244547	980.300331	14.753805
20.369271	969.863285	14.758823
20.387542	968.531870	14.763840
19.970168	979.838604	14.768858
20.490002	968.045740	14.773875
20.588734	973.625730	14.778893
20.626096	978.855567	14.783911
20.523148	967.141345	14.788928
20.561055	961.003598	14.793946
20.647982	948.666333	14.798963
20.607172	945.400153	14.803981
20.263515	948.635201	14.808999
20.475301	932.551288	14.814016
20.189666	947.116319	14.819034
20.474360	944.272522	14.824051
20.252950	948.984303	14.829069
20.335840	949.428994	14.834087
20.210028	963.962687	14.839104
20.269128	968.958735	14.844122
20.815531	965.038800	14.849139
20.572385	969.766616	14.854157
20.567176	960.378751	14.859175
20.420445	963.444088	14.864192
20.447327	968.653472	14.869210
20.774008	966.181800	14.874227
20.489557	965.106104	14.879245
20.530744	964.610564	14.884263
20.462661	972.649877	14.889280
20.384245	967.316169	14.894298
20.419728	966.240840	14.899315
20.551878	985.265983	14.904333
20.803200	989.010590	14.909351
21.452991	989.183419	14.914368
20.969971	991.130615	14.919386
20.920702	986.587619	14.924403
20.521369	982.790611	14.929421
20.864802	989.414736	14.934439
21.185662	987.669827	14.939456
21.030378	986.431876	14.944474
20.902223	976.321633	14.949491
21.018359	982.419621	14.954509
20.704619	980.193458	14.959527
21.239869	988.949312	14.964544
21.048459	990.175459	14.969562
20.888543	983.645810	14.974579
21.111719	989.310452	14.979597
21.163993	984.410710	14.984615
21.071721	987.735769	14.989632
21.173882	990.099377	14.994650
21.342480	988.248933	14.999667
21.326714	987.986384	15.004685
21.119771	976.821795	15.009703
21.307902	981.930177	15.014720
20.855566	992.942588	15.019738
21.150984	982.137955	15.024755
21.204832	982.438870	15.029773
21.435786	980.897401	15.034791
21.223591	975.313245	15.039808
20.945465	977.212558	15.044826
21.509963	988.056181	15.049843
21.396463	989.951793	15.054861
21.365167	996.988093	15.059879
21.760722	1002.985502	15.064896
21.589756	999.073813	15.069914
21.615490	989.453861	15.074931
21.388733	974.672574	15.079949
21.740342	982.074919	15.084967
21.669040	982.849890	15.089984
21.447595	979.495239	15.095002
21.891254	984.333206	15.100019
21.717938	971.421302	15.105037
21.307033	982.843793	15.110055
21.712686	990.266076	15.115072
21.734494	1000.273217	15.120090
21.835230	991.787100	15.125107
22.168833	986.606588	15.130125
21.737109	981.864733	15.135143
21.863401	979.639055	15.140160
21.606895	979.827647	15.145178
21.961244	981.536343	15.150195
21.929305	973.373988	15.155213
21.496883	973.454439	15.160231
21.553378	973.600301	15.165248
21.889744	1000.786145	15.170266
21.937197	998.676962	15.175283
22.378379	1000.122740	15.180301
22.280728	992.797516	15.185319
21.967173	982.706850	15.190336
21.947114	979.898172	15.195354
22.357940	969.911774	15.200371
22.291879	970.695391	15.205389
21.653040	977.504973	15.210407
22.020695	971.227193	15.215424
21.844401	979.469661	15.220442
21.919488	985.675070	15.225459
22.317558	1002.058115	15.230477
22.055670	1018.146934	15.235495
22.268129	1003.931141	15.240512
22.561208	1004.873091	15.245530
22.097472	995.007925	15.250547
22.158830	994.632303	15.255565
22.225708	999.059081	15.260583
22.229565	999.797030	15.265600
22.182766	1010.222035	15.270618
22.118078	1006.116963	15.275635
22.358450	1004.580328	15.280653
22.134078	1009.431448	15.285671
22.407218	1001.871395	15.290688
22.342213	1007.177240	15.295706
22.334024	1004.177346	15.300723
22.390997	995.874814	15.305741
22.301275	1006.514831	15.310759
22.273690	992.213577	15.315776
21.901724	1013.956059	15.320794
22.329365	1017.865557	15.325811
22.303100	1029.395074	15.330829
22.441476	1035.969291	15.335847
22.520160	1027.701214	15.340864
22.102166	1035.530285	15.345882
22.514878	1034.405315	15.350899
22.614188	1027.273285	15.355917
22.669787	1034.775681	15.360935
22.732892	1022.558866	15.365952
22.793049	1037.429564	15.370970
22.890060	1029.758235	15.375987
23.259043	1029.391220	15.381005
22.756586	1029.315381	15.386023
23.341784	1033.878714	15.391040
23.140755	1032.076711	15.396058
22.743264	1028.011153	15.401075
23.102655	1023.921685	15.406093
22.757633	1024.739545	15.411111
23.142914	1028.813477	15.416128
23.025343	1033.281786	15.421146
22.962537	1029.053334	15.426163
23.108060	1023.047031	15.431181
22.991986	1024.094115	15.436199
23.329242	1021.889029	15.441216
23.282180	1025.131269	15.446234
23.049380	1024.574511	15.451251
23.388528	1028.431603	15.456269
22.800078	1026.725016	15.461287
23.176690	1022.875854	15.466304
23.299976	1038.437270	15.471322
23.027956	1022.126114	15.476339
23.451265	1018.004541	15.481357
23.151789	1026.420970	15.486375
23.452241	1037.454321	15.491392
23.270993	1029.697198	15.496410
23.148517	1030.704258	15.501427
23.101634	1021.389165	15.506445
23.083245	1022.304175	15.511463
23.069025	1022.161307	15.516480
23.526714	1016.715184	15.521498
23.577833	1023.546072	15.526515
23.602614	1022.898462	15.531533
23.319107	1028.487865	15.536551
23.291758	1022.063667	15.541568
23.199324	1036.415458	15.546586
23.288533	1037.925855	15.551603
23.273781	1041.200907	15.556621
23.530718	1049.564882	15.561639
23.105885	1041.097971	15.566656
23.326345	1036.998709	15.571674
23.502947	1046.116906	15.576691
23.766627	1041.638475	15.581709
23.254375	1040.813067	15.586727
23.359771	1038.634839	15.591744
23.726801	1051.810090	15.596762
23.797223	1069.273356	15.601779
24.464522	1060.995093	15.606797
24.338781	1054.400101	15.611815
24.187310	1038.253084	15.616832
24.276272	1041.758047	15.621850
24.031543	1043.434377	15.626867
24.501747	1024.308634	15.631885
24.344674	1033.924086	15.636903
24.182494	1035.985125	15.641920
24.076258	1033.625455	15.646938
23.696513	1045.443902	15.651955
24.288818	1034.728424	15.656973
23.923900	1031.020690	15.661991
24.331399	1039.471528	15.667008
24.363079	1033.158001	15.672026
24.142565	1034.571753	15.677043
24.577301	1038.644251	15.682061
23.839339	1028.538001	15.687079
24.048917	1018.160218	15.692096
24.622506	1034.604158	15.697114
24.384527	1020.638812	15.702131
24.086032	1016.169571	15.707149
24.158119	1024.095425	15.712167
24.268356	1023.153551	15.717184
24.514376	1036.871630	15.722202
24.104688	1034.288097	15.727219
24.585254	1032.546564	15.732237
24.178606	1029.877347	15.737255
24.430974	1033.037960	15.742272
24.479124	1031.035964	15.747290
24.350505	1037.049239	15.752307
24.297833	1033.743875	15.757325
24.203759	1033.392606	15.762343
24.482516	1031.730031	15.767360
24.347951	1023.517458	15.772378
24.319476	1039.465582	15.777395
24.577514	1025.507725	15.782413
24.433421	1031.214145	15.787431
24.514406	1031.403508	15.792448
24.703546	1051.199299	15.797466
24.724836	1061.386441	15.802483
24.640845	1056.924608	15.807501
24.431992	1059.848211	15.812519
24.690376	1059.968754	15.817536
24.595237	1057.894529	15.822554
24.580773	1063.160913	15.827571
24.766382	1052.556484	15.832589
24.839819	1059.065143	15.837607
24.718766	1054.656457	15.842624
25.217860	1049.898135	15.847642
24.642361	1061.242319	15.852659
25.271398	1053.708535	15.857677
24.902604	1047.688131	15.862695
24.531401	1056.548170	15.867712
24.488324	1067.234565	15.872730
24.930286	1074.196745	15.877747
25.225519	1079.401987	15.882765
25.010393	1076.674352	15.887783
24.884379	1082.829250	15.892800
25.190243	1082.614139	15.897818
25.007922	1086.635000	15.902835
25.394653	1080.111189	15.907853
25.238179	1088.312731	15.912871
25.406562	1086.897826	15.917888
25.544133	1078.601563	15.922906
25.584275	1087.479222	15.927923
25.742939	1078.744140	15.932941
25.577861	1085.956075	15.937959
25.504574	1081.492559	15.942976
25.632438	1066.065480	15.947994
25.175002	1066.490686	15.953011
25.340297	1063.331053	15.958029
25.432944	1074.665238	15.963047
25.395273	1078.395182	15.968064
25.612328	1078.755737	15.973082
24.884322	1078.273410	15.978099
25.451277	1079.516447	15.983117
25.621534	1084.416213	15.988135
25.164559	1081.350918	15.993152
25.480954	1078.915556	15.998170
25.589807	1084.168937	16.003187
25.537084	1075.826750	16.008205
25.415084	1087.440734	16.013223
25.064051	1098.345817	16.018240
25.526998	1094.382124	16.023258
25.510652	1102.558561	16.028275
25.552371	1096.290778	16.033293
26.012761	1100.441324	16.038311
25.625607	1097.526037	16.043328
25.798028	1088.037689	16.048346
25.965796	1092.136248	16.053363
25.867603	1096.380624	16.058381
26.173200	1106.337047	16.063399
26.086698	1100.259772	16.068416
26.230543	1092.262332	16.073434
26.397620	1092.176267	16.078451
26.071739	1091.738235	16.083469
26.008913	1095.039765	16.088487
26.025607	1096.220690	16.093504
26.132693	1088.740267	16.098522
26.044145	1107.090040	16.103539
26.085771	1116.210485	16.108557
26.244980	1111.309734	16.113575
26.291043	1117.336693	16.118592
26.645583	1116.110376	16.123610
26.470491	1119.587296	16.128627
26.522353	1120.008449	16.133645
26.588059	1111.796017	16.138663
26.299770	1108.959915	16.143680
26.082500	1098.958242	16.148698
26.007466	1107.194372	16.153715
26.187057	1114.835170	16.158733
26.500116	1111.794392	16.163751
26.146219	1121.147229	16.168768
26.358663	1114.246756	16.173786
26.353892	1118.754220	16.178803
26.344167	1118.184599	16.183821
26.591971	1113.352019	16.188839
26.673080	1115.223465	16.193856
26.834421	1120.402359	16.198874
26.726884	1118.715091	16.203891
26.715477	1108.236175	16.208909
26.702517	1111.567765	16.213927
26.912486	1117.111437	16.218944
26.861594	1112.385619	16.223962
26.484696	1113.789164	16.228979
27.085222	1129.250639	16.233997
26.894783	1120.390347	16.239015
26.850427	1118.434395	16.244032
26.881002	1117.542868	16.249050
27.135337	1125.983030	16.254067
27.282182	1135.964343	16.259085
26.901823	1125.022499	16.264103
26.649362	1123.316910	16.269120
27.230374	1123.001883	16.274138
27.068641	1135.723537	16.279155
27.464206	1146.647377	16.284173
27.585435	1129.722222	16.289191
27.282244	1113.870317	16.294208
26.927349	1109.372018	16.299226
26.622142	1122.816755	16.304243
26.984394	1130.788715	16.309261
27.546559	1138.839813	16.314279
27.416027	1136.900517	16.319296
27.274393	1136.613503	16.324314
27.435744	1143.272526	16.329331
27.513496	1136.229041	16.334349
27.683756	1133.848128	16.339367
27.080370	1138.010714	16.344384
27.511408	1142.642413	16.349402
27.395197	1134.751973	16.354419
27.391598	1140.341737	16.359437
27.984801	1134.060121	16.364455
27.635753	1133.493169	16.369472
27.503718	1137.342056	16.374490
27.465147	1133.236018	16.379507
27.794499	1134.651991	16.384525
27.629098	1120.028233	16.389543
27.755949	1139.597187	16.394560
27.998009	1134.270024	16.399578
27.550999	1136.738631	16.404595
27.193322	1136.090978	16.409613
27.455928	1134.841193	16.414631
27.374619	1138.284486	16.419648
27.458560	1142.200524	16.424666
27.931147	1161.570161	16.429683
27.774103	1168.339042	16.434701
27.965663	1147.764075	16.439719
28.107221	1156.973029	16.444736
28.198187	1164.179594	16.449754
28.061074	1158.488939	16.454771
27.908941	1160.359062	16.459789
28.190881	1172.250652	16.464807
28.402818	1163.371477	16.469824
28.118526	1162.813314	16.474842
28.130536	1156.023127	16.479859
27.756850	1156.990655	16.484877
28.073068	1152.349325	16.489895
28.313699	1156.729984	16.494912
28.553976	1144.049809	16.499930
28.113889	1153.009054	16.504947
27.800072	1151.770683	16.509965
28.071462	1150.295451	16.514983
28.079650	1159.070850	16.520000
28.317148	1165.007869	16.525018
28.452023	1169.600767	16.530035
28.339910	1176.207971	16.535053
28.637954	1178.585097	16.540071
28.540257	1178.196521	16.545088
28.601788	1182.188665	16.550106
29.155581	1174.666620	16.555123
28.551707	1163.740836	16.560141
29.068324	1155.000128	16.565159
28.883272	1159.337025	16.570176
28.920112	1153.625428	16.575194
28.605904	1146.315135	16.580211
28.613898	1149.271051	16.585229
28.733669	1148.962017	16.590247
28.815559	1158.265530	16.595264
28.283217	1150.923138	16.600282
28.432729	1157.069606	16.605299
28.747226	1171.499765	16.610317
29.022873	1175.641403	16.615335
28.995984	1178.785833	16.620352
28.904482	1183.559376	16.625370
29.328074	1169.051586	16.630387
28.707125	1174.289946	16.635405
28.853394	1181.143857	16.640423
28.794530	1177.804722	16.645440
28.889819	1179.790722	16.650458
29.174811	1173.592097	16.655475
29.004321	1173.211771	16.660493
29.106138	1178.198029	16.665511
29.298961	1172.654498	16.670528
29.015658	1173.538436	16.675546
29.213765	1171.771715	16.680563
28.797721	1178.240340	16.685581
29.097792	1187.484437	16.690599
29.361619	1198.997016	16.695616
29.440070	1205.972020	16.700634
29.490026	1203.786678	16.705651
29.204741	1196.430806	16.710669
29.785615	1202.402403	16.715687
29.532430	1200.210908	16.720704
29.885573	1197.937037	16.725722
29.532874	1195.675924	16.730739
29.826199	1207.067117	16.735757
29.836256	1199.257855	16.740775
29.671765	1196.083594	16.745792
29.854641	1192.880156	16.750810
29.794818	1193.385084	16.755827
29.540968	1196.590325	16.760845
30.018111	1190.588815	16.765863
29.531544	1198.946272	16.770880
29.836576	1200.624846	16.775898
29.908278	1191.767629	16.780915
29.485749	1205.211874	16.785933
29.581801	1193.469480	16.790951
29.244742	1190.328570	16.795968
29.528855	1200.231606	16.800986
29.898055	1207.804865	16.806003
29.882003	1229.094196	16.811021
30.086860	1216.612032	16.816039
30.131052	1209.255027	16.821056
30.356422	1214.619584	16.826074
30.556020	1215.008125	16.831091
30.563107	1208.430136	16.836109
30.452191	1196.584463	16.841127
30.335156	1191.196776	16.846144
30.225715	1184.106858	16.851162
30.271284	1177.421862	16.856179
30.038189	1188.570462	16.861197
30.477512	1198.480738	16.866215
30.184986	1206.034594	16.871232
30.301925	1206.682248	16.876250
30.542502	1210.106682	16.881267
30.276394	1217.059933	16.886285
30.479556	1225.094733	16.891303
30.580688	1217.321688	16.896320
30.460758	1216.011908	16.901338
30.667281	1214.325919	16.906355
30.798515	1219.569522	16.911373
30.505168	1211.208165	16.916391
30.685911	1214.411591	16.921408
30.330592	1212.034117	16.926426
30.090860	1201.133311	16.931443
30.275536	1208.031710	16.936461
30.428687	1209.686743	16.941479
30.432511	1217.127897	16.946496
30.966917	1238.757045	16.951514
31.251418	1228.408428	16.956531
31.214516	1234.022375	16.961549
31.327386	1219.260259	16.966567
31.106844	1207.870428	16.971584
31.212310	1200.850978	16.976602
31.275567	1196.040980	16.981619
30.796297	1199.859074	16.986637
30.706930	1202.075987	16.991655
31.013373	1209.286681	16.996672
31.280004	1224.188303	17.001690
31.756311	1221.364936	17.006707
31.296124	1212.278607	17.011725
31.209406	1206.412777	17.016743
31.044575	1200.918962	17.021760
31.242529	1214.231282	17.026778
31.544841	1215.790359	17.031795
31.461983	1215.478355	17.036813
31.271019	1213.008855	17.041831
31.285098	1221.991654	17.046848
31.107698	1223.010486	17.051866
31.550350	1223.484027	17.056883
31.619461	1223.236579	17.061901
31.522206	1219.392190	17.066919
31.444866	1226.883936	17.071936
31.370938	1237.827741	17.076954
31.563521	1224.845701	17.081971
31.519056	1233.168620	17.086989
31.589981	1229.935377	17.092007
31.621698	1231.688337	17.097024
31.437561	1229.479707	17.102042
31.596216	1227.195278	17.107059
31.425286	1243.531990	17.112077
31.581181	1248.907443	17.117095
32.035638	1247.611812	17.122112
31.968022	1256.421228	17.127130
32.298974	1243.089277	17.132147
31.579074	1253.534674	17.137165
32.025070	1255.670870	17.142183
32.155296	1248.587559	17.147200
32.026925	1247.244384	17.152218
31.897537	1246.434721	17.157235
32.122316	1251.486944	17.162253
31.891976	1254.123599	17.167271
31.736930	1236.979687	17.172288
31.619975	1253.266924	17.177306
32.103945	1259.739738	17.182323
32.131211	1273.176679	17.187341
32.303294	1273.793604	17.192359
32.420023	1268.441855	17.197376
32.517468	1277.679874	17.202394
32.831755	1261.286105	17.207411
32.649475	1272.489914	17.212429
32.445407	1271.821344	17.217447
32.984746	1271.178315	17.222464
32.620671	1268.322502	17.227482
33.228306	1249.051906	17.232499
33.034310	1242.366549	17.237517
33.044713	1240.932201	17.242535
33.226884	1227.797149	17.247552
33.260734	1231.919878	17.252570
33.376831	1223.980377	17.257587
33.242444	1220.965504	17.262605
32.879173	1216.926099	17.267623
32.770043	1204.502606	17.272640
32.878002	1202.134601	17.277658
32.974837	1199.105595	17.282675
33.344783	1191.069529	17.287693
32.915975	1197.574876	17.292711
33.179539	1200.203570	17.297728
33.034739	1192.109292	17.302746
33.180104	1193.926496	17.307763
33.042132	1189.946476	17.312781
32.764084	1197.652701	17.317799
33.184147	1195.141119	17.322816
33.219149	1205.310415	17.327834
33.080379	1203.138863	17.332851
33.134857	1208.823695	17.337869
33.478419	1220.159687	17.342887
33.242856	1221.250750	17.347904
33.211766	1242.428840	17.352922
33.461045	1227.171955	17.357939
33.245779	1219.994458	17.362957
33.223851	1229.699298	17.367975
33.569478	1224.703034	17.372992
33.257008	1225.676754	17.378010
32.946493	1214.607141	17.383027
33.606459	1230.905181	17.388045
33.392843	1229.420722	17.393063
33.490808	1229.913553	17.398080
33.128077	1236.569513	17.403098
33.483357	1246.732835	17.408115
33.634400	1256.035033	17.413133
33.399522	1250.618452	17.418151
33.743232	1243.246064	17.423168
33.931854	1260.672063	17.428186
33.544141	1256.488150	17.433203
33.696257	1256.366558	17.438221
33.747334	1263.500514	17.443239
33.850757	1261.426715	17.448256
33.947273	1280.874339	17.453274
34.022405	1277.577310	17.458291
34.222797	1280.455764	17.463309
34.028961	1281.799080	17.468327
34.135467	1280.409634	17.473344
33.922213	1281.197391	17.478362
34.033318	1268.256489	17.483379
34.231812	1275.357885	17.488397
34.111616	1276.714911	17.493415
34.245967	1275.299011	17.498432
34.037153	1281.337556	17.503450
34.067040	1285.893282	17.508467
34.390483	1274.314032	17.513485
33.923582	1281.639610	17.518503
34.603589	1289.546076	17.523520
34.213686	1305.797228	17.528538
34.386431	1301.456063	17.533555
34.596633	1298.630194	17.538573
34.573051	1301.152407	17.543591
34.554614	1299.163970	17.548608
34.646393	1299.184381	17.553626
34.636939	1292.075598	17.558643
34.936315	1297.589539	17.563661
34.844091	1301.233398	17.568679
34.884800	1300.845226	17.573696
34.756687	1301.764817	17.578714
34.577578	1303.197350	17.583731
34.635110	1293.783701	17.588749
34.669427	1300.825620	17.593767
35.107930	1291.630004	17.598784
35.141460	1288.901249	17.603802
34.972718	1297.644474	17.608819
35.060849	1291.688102	17.613837
35.004483	1307.539844	17.618855
34.829654	1319.894435	17.623872
35.329248	1317.187331	17.628890
35.356768	1312.774238	17.633907
35.449296	1318.790829	17.638925
35.292943	1323.309470	17.643943
35.672799	1316.657257	17.648960
35.257484	1320.143449	17.653978
35.452203	1323.452008	17.658995
35.766450	1308.860247	17.664013
35.713187	1304.589207	17.669031
35.550864	1290.861115	17.674048
35.364110	1286.172318	17.679066
35.691555	1306.843010	17.684083
35.855897	1298.542451	17.689101
35.533657	1298.069128	17.694119
35.767865	1291.335598	17.699136
35.609189	1306.922490	17.704154
35.435848	1308.379367	17.709171
35.785983	1306.576190	17.714189
35.494051	1312.283770	17.719207
35.933496	1317.693716	17.724224
35.832612	1318.104091	17.729242
35.947864	1315.069024	17.734259
36.233463	1303.180091	17.739277
35.772843	1311.852284	17.744295
36.255368	1313.313704	17.749312
36.085917	1307.416619	17.754330
35.681429	1308.300614	17.759347
35.970631	1308.047085	17.764365
36.041433	1312.984590	17.769383
35.854658	1306.411691	17.774400
35.913546	1330.466633	17.779418
35.582184	1336.890487	17.784435
36.238535	1332.602937	17.789453
35.936354	1340.180454	17.794471
36.209294	1343.334743	17.799488
36.260740	1341.382692	17.804506
36.124320	1345.854033	17.809523
36.942260	1345.312525	17.814541
36.509030	1356.577797	17.819559
36.678704	1345.322409	17.824576
36.538716	1343.441379	17.829594
36.820491	1344.340935	17.834611
36.976058	1340.532651	17.839629
36.693088	1344.155910	17.844647
36.598421	1347.973739	17.849664
36.391407	1346.980564	17.854682
36.797796	1363.056511	17.859699
36.882239	1366.189843	17.864717
37.107747	1372.150902	17.869735
37.372067	1355.509242	17.874752
37.545842	1337.979183	17.879770
36.802676	1336.255777	17.884787
37.316703	1323.532585	17.889805
36.972188	1329.923782	17.894823
37.222945	1330.130733	17.899840
37.301393	1328.127113	17.904858
36.807473	1320.112725	17.909875
37.163898	1333.138361	17.914893
37.165085	1331.938990	17.919911
37.150080	1334.220011	17.924928
37.373828	1351.407054	17.929946
37.116883	1356.929277	17.934963
37.769051	1353.311440	17.939981
37.538082	1357.835469	17.944999
37.266413	1354.056249	17.950016
37.543448	1352.447566	17.955034
37.544081	1358.563780	17.960051
37.588749	1347.476306	17.965069
37.417429	1349.595620	17.970087
37.380469	1347.187182	17.975104
37.391965	1353.415306	17.980122
37.466549	1362.350824	17.985139
37.542969	1357.980553	17.990157
37.339941	1356.077839	17.995175
37.536113	1363.978091	18.000192
37.938496	1375.437516	18.005210
37.704241	1381.824080	18.010227
38.615851	1369.941166	18.015245
37.866424	1386.725270	18.020263
37.959088	1377.485962	18.025280
38.243848	1382.910696	18.030298
38.054115	1386.102768	18.035315
38.057217	1381.071760	18.040333
38.313521	1386.459926	18.045351
37.856897	1378.565907	18.050368
38.084486	1374.799982	18.055386
38.251649	1379.700316	18.060403
38.373718	1374.808468	18.065421
38.336963	1372.418931	18.070439
38.582551	1376.117180	18.075456
38.446116	1366.913772	18.080474
38.433327	1370.115990	18.085491
38.577601	1371.125458	18.090509
38.541400	1371.266911	18.095527
38.451356	1375.472204	18.100544
38.376789	1370.989881	18.105562
38.355770	1381.231173	18.110579
38.134805	1375.165403	18.115597
38.462322	1382.426517	18.120615
38.621212	1386.962057	18.125632
38.697216	1385.993969	18.130650
38.367429	1387.544795	18.135667
38.737515	1386.101420	18.140685
38.399131	1385.362366	18.145703
38.520584	1398.188168	18.150720
38.895912	1412.381762	18.155738
39.055754	1409.232390	18.160755
39.223284	1412.116015	18.165773
38.758282	1416.907111	18.170791
38.961607	1410.074229	18.175808
38.875876	1410.362305	18.180826
39.319382	1410.876745	18.185843
39.169661	1406.620793	18.190861
39.574238	1415.627718	18.195879
39.399409	1409.990231	18.200896
39.372921	1414.684217	18.205914
39.168041	1417.124393	18.210931
39.315745	1408.706464	18.215949
39.283109	1416.276496	18.220967
39.081267	1424.630474	18.225984
39.731116	1423.521979	18.231002
39.930778	1430.654814	18.236019
39.845380	1436.699322	18.241037
40.038172	1434.450546	18.246055
39.827016	1425.034742	18.251072
39.957166	1413.829687	18.256090
39.886462	1405.474383	18.261107
39.929110	1403.564731	18.266125
39.883637	1395.915570	18.271143
40.029402	1400.582564	18.276160
40.206982	1405.850520	18.281178
40.116855	1406.151909	18.286195
40.075726	1394.310950	18.291213
40.156575	1392.644635	18.296231
40.295391	1398.792863	18.301248
39.853865	1389.810822	18.306266
40.303668	1398.930579	18.311283
40.272984	1396.173996	18.316301
40.261793	1398.747932	18.321319
40.296571	1398.019844	18.326336
40.393494	1411.092507	18.331354
40.310625	1414.005896	18.336371
40.440577	1421.184365	18.341389
40.474576	1413.664763	18.346407
40.715180	1421.984134	18.351424
40.315803	1420.333093	18.356442
40.399496	1428.396171	18.361459
40.564425	1426.423175	18.366477
40.855982	1423.398338	18.371495
40.440906	1427.026531	18.376512
40.699213	1414.927194	18.381530
40.473304	1427.094193	18.386547
40.441874	1422.188510	18.391565
40.499368	1427.412168	18.396583
40.373859	1434.034189	18.401600
40.893090	1432.759957	18.406618
40.939299	1449.419461	18.411635
41.206808	1452.959650	18.416653
41.007992	1449.475124	18.421671
41.003720	1459.193102	18.426688
41.496201	1445.264463	18.431706
41.060007	1458.155587	18.436723
40.988522	1453.287731	18.441741
41.160596	1446.873163	18.446759
41.113550	1444.725082	18.451776
41.108864	1440.926106	18.456794
41.087269	1453.174725	18.461811
41.156501	1461.685075	18.466829
41.275761	1468.836835	18.471847
41.084344	1475.604905	18.476864
41.789620	1470.492260	18.481882
41.515884	1476.828236	18.486899
41.641731	1478.727426	18.491917
41.480122	1468.057226	18.496935
41.574107	1466.669728	18.501952
41.878985	1475.329366	18.506970
41.727678	1475.526726	18.511987
41.726966	1468.918304	18.517005
41.970262	1472.285556	18.522023
41.791184	1468.504428	18.527040
42.109362	1479.469002	18.532058
41.944818	1484.301408	18.537075
42.210547	1491.190374	18.542093
42.184902	1495.480284	18.547111
42.071880	1501.320847	18.552128
42.008378	1496.757859	18.557146
42.146589	1503.262844	18.562163
42.196839	1495.784845	18.567181
42.704728	1500.717039	18.572199
42.281458	1500.814990	18.577216
42.643864	1493.550031	18.582234
42.277010	1500.923141	18.587251
42.077424	1493.840912	18.592269
42.678548	1496.640836	18.597287
42.226721	1499.258577	18.602304
42.226017	1495.629387	18.607322
42.342105	1495.854284	18.612339
42.261524	1501.683453	18.617357
42.323429	1499.799178	18.622375
42.427384	1519.791881	18.627392
42.709635	1515.474534	18.632410
42.988236	1516.317790	18.637427
43.257893	1509.786919	18.642445
43.504717	1505.459346	18.647463
43.431263	1504.312685	18.652480
43.086225	1489.675741	18.657498
43.171344	1467.056232	18.662515
43.090528	1467.359319	18.667533
43.335057	1474.472518	18.672551
42.865707	1475.950538	18.677568
43.346158	1484.162929	18.682586
43.524083	1483.178866	18.687603
43.261062	1476.217042	18.692621
43.598206	1468.309075	18.697639
42.909165	1477.329578	18.702656
43.164944	1483.566813	18.707674
43.640462	1487.730862	18.712691
43.429546	1489.389310	18.717709
43.741299	1484.732815	18.722727
43.874095	1499.930207	18.727744
44.010034	1486.145766	18.732762
43.726114	1494.430581	18.737779
44.000237	1495.025215	18.742797
43.929791	1494.714417	18.747815
43.773716	1494.596927	18.752832
43.967280	1484.174043	18.757850
43.838064	1492.639757	18.762867
43.863087	1489.584082	18.767885
44.157988	1483.093449	18.772903
43.992572	1497.589596	18.777920
44.147660	1491.537455	18.782938
44.179398	1487.685422	18.787955
44.180081	1489.847234	18.792973
44.089401	1493.178448	18.797991
44.048889	1491.449083	18.803008
44.485739	1491.809927	18.808026
44.231688	1485.746147	18.813043
44.292327	1487.892253	18.818061
44.170734	1484.966854	18.823079
44.078198	1480.875503	18.828096
44.294851	1497.498879	18.833114
44.591686	1507.267542	18.838131
44.285650	1517.604063	18.843149
44.672880	1512.298228	18.848167
44.633313	1516.599792	18.853184
44.480280	1520.029149	18.858202
44.527591	1515.647621	18.863219
44.601251	1516.374655	18.868237
44.534276	1515.971790	18.873255
44.400506	1527.764638	18.878272
44.965665	1536.781181	18.883290
45.108419	1535.701635	18.888307
45.271331	1538.841639	18.893325
45.400796	1533.724514	18.898343
45.096616	1552.124307	18.903360
45.203981	1547.957437	18.908378
45.264979	1554.739641	18.913395
45.201326	1547.692900	18.918413
45.048155	1543.263877	18.923431
45.219094	1539.554134	18.928448
44.876185	1545.061479	18.933466
45.214806	1539.558112	18.938483
45.187441	1543.649476	18.943501
45.445687	1537.464386	18.948519
45.434746	1536.112258	18.953536
45.295058	1546.892975	18.958554
46.157293	1560.821041	18.963571
45.596752	1569.745713	18.968589
45.944105	1563.909591	18.973607
45.970144	1574.878967	18.978624
45.764163	1568.160649	18.983642
45.998016	1567.729586	18.988659
45.957397	1563.642706	18.993677
45.849874	1568.971159	18.998695
46.102489	1568.268897	19.003712
46.127754	1566.873222	19.008730
46.124141	1563.067739	19.013747
45.970946	1564.679280	19.018765
46.060113	1559.656829	19.023783
45.928515	1568.388055	19.028800
46.012033	1569.738432	19.033818
46.375528	1563.735670	19.038835
46.097634	1570.239598	19.043853
46.382883	1561.007893	19.048871
46.355160	1570.309859	19.053888
46.216053	1585.922332	19.058906
46.260845	1582.084013	19.063923
46.217131	1597.889846	19.068941
46.569576	1590.863107	19.073959
46.275002	1596.684807	19.078976
46.462498	1593.906633	19.083994
46.304409	1596.954921	19.089011
46.801271	1614.115207	19.094029
47.071243	1614.669467	19.099047
46.947514	1610.873325	19.104064
47.075892	1616.925428	19.109082
47.337670	1610.105404	19.114099
47.308313	1613.897277	19.119117
47.314554	1609.869320	19.124135
47.120375	1614.226692	19.129152
47.106239	1613.698775	19.134170
47.358171	1613.937106	19.139187
47.167132	1611.587489	19.144205
47.249292	1605.164860	19.149223
47.414884	1605.088495	19.154240
47.310430	1602.778966	19.159258
47.406678	1597.941599	19.164275
47.324731	1605.213305	19.169293
47.415512	1598.464261	19.174311
47.241863	1607.795421	19.179328
47.223074	1624.279067	19.184346
47.625144	1626.772508	19.189363
47.644581	1629.537351	19.194381
48.041794	1618.621706	19.199399
48.305121	1628.190546	19.204416
47.977538	1629.154030	19.209434
48.381316	1625.022757	19.214451
48.103921	1622.172241	19.219469
48.129813	1622.518575	19.224487
48.489265	1624.182353	19.229504
48.172517	1625.529172	19.234522
48.155697	1618.162622	19.239539
48.107204	1625.542711	19.244557
47.955358	1621.668916	19.249575
48.133155	1622.019855	19.254592
48.337656	1619.276885	19.259610
48.275137	1623.449520	19.264627
48.035720	1619.794586	19.269645
47.986635	1628.998937	19.274663
48.304742	1636.914922	19.279680
48.391901	1651.542044	19.284698
48.515021	1642.846973	19.289715
48.665003	1654.295627	19.294733
48.680717	1642.881126	19.299751
48.343898	1646.045793	19.304768
48.477943	1651.042914	19.309786
48.682880	1656.849491	19.314803
49.006831	1679.200157	19.319821
49.219311	1673.776477	19.324839
49.202469	1672.879729	19.329856
49.094219	1671.949961	19.334874
49.195896	1664.820463	19.339891
49.001708	1671.762621	19.344909
49.265505	1667.331358	19.349927
49.403849	1669.727260	19.354944
49.422520	1662.677044	19.359962
49.487015	1676.812245	19.364979
48.890521	1660.848006	19.369997
49.684329	1662.857171	19.375015
49.474535	1666.327008	19.380032
49.524257	1669.970795	19.385050
49.732789	1664.093271	19.390067
49.664459	1674.105442	19.395085
49.586786	1662.550917	19.400103
49.466236	1662.241654	19.405120
49.772880	1680.457509	19.410138
49.989107	1691.949460	19.415155
49.928076	1692.287323	19.420173
49.658456	1691.654254	19.425191
49.950023	1693.347611	19.430208
49.918170	1690.998291	19.435226
50.627355	1682.198754	19.440243
50.400293	1697.717800	19.445261
50.750131	1682.646758	19.450279
50.387591	1683.505261	19.455296
50.711050	1686.077303	19.460314
50.793280	1681.658703	19.465331
50.440221	1686.678500	19.470349
50.506276	1682.063606	19.475367
50.527005	1679.677645	19.480384
50.512831	1691.641224	19.485402
50.647635	1680.564671	19.490419
50.539793	1690.166448	19.495437
50.318264	1685.842780	19.500455
50.890777	1685.538547	19.505472
50.398874	1683.267619	19.510490
51.189048	1685.706574	19.515507
50.654352	1679.096524	19.520525
51.050512	1684.857370	19.525543
50.696261	1678.985960	19.530560
50.832195	1692.197893	19.535578
50.551389	1694.021955	19.540595
51.300179	1696.154950	19.545613
50.944074	1699.770802	19.550631
51.159966	1690.310041	19.555648
51.215416	1707.122981	19.560666
51.546806	1698.546740	19.565683
51.327864	1710.671811	19.570701
51.067993	1704.025006	19.575719
51.361792	1705.755886	19.580736
51.286900	1724.394504	19.585754
51.246074	1722.431621	19.590771
51.744419	1724.660666	19.595789
51.680390	1723.929109	19.600807
51.921272	1722.941482	19.605824
51.659539	1732.864060	19.610842
51.694190	1729.611162	19.615859
51.871023	1719.477961	19.620877
51.764326	1719.507377	19.625895
51.977095	1726.786610	19.630912
51.738881	1735.061218	19.635930
52.010037	1739.901173	19.640947
52.359676	1748.998931	19.645965
51.898054	1751.034378	19.650983
52.659893	1743.782481	19.656000
52.844759	1742.207141	19.661018
52.287582	1731.945922	19.666035
52.394461	1733.472545	19.671053
52.728998	1735.948178	19.676071
52.922663	1735.618089	19.681088
52.974426	1745.245386	19.686106
52.775074	1738.955184	19.691123
52.809396	1726.297399	19.696141
52.831658	1733.691695	19.701159
53.189846	1736.400325	19.706176
52.928687	1737.249258	19.711194
52.926955	1730.110688	19.716211
53.034277	1734.389291	19.721229
53.121951	1737.711543	19.726247
52.974647	1732.240066	19.731264
52.632653	1730.324368	19.736282
52.987436	1734.917674	19.741299
53.588113	1731.399356	19.746317
53.100830	1739.144905	19.751335
52.943962	1725.396689	19.756352
53.025615	1734.122988	19.761370
53.388340	1741.675398	19.766387
53.083103	1738.826069	19.771405
53.240717	1747.436325	19.776423
53.351071	1752.288853	19.781440
53.481919	1764.116143	19.786458
53.335829	1761.996165	19.791475
53.479581	1764.287084	19.796493
53.255370	1775.598770	19.801511
53.550600	1778.326737	19.806528
53.696403	1786.793685	19.811546
53.862526	1776.030925	19.816563
54.042252	1782.169720	19.821581
53.752982	1790.635402	19.826599
54.182468	1781.358894	19.831616
54.109675	1785.520552	19.836634
54.303098	1796.596392	19.841651
54.372448	1800.811527	19.846669
54.299848	1807.157134	19.851687
54.445458	1804.448612	19.856704
54.449280	1801.617127	19.861722
54.396893	1807.574531	19.866739
54.582029	1809.530745	19.871757
54.401522	1810.297613	19.876775
54.505948	1803.028764	19.881792
54.869513	1805.695533	19.886810
54.953306	1809.930500	19.891827
54.685513	1796.849750	19.896845
54.554740	1800.708049	19.901863
54.838505	1795.538270	19.906880
54.677727	1810.589404	19.911898
55.164723	1815.408187	19.916915
55.280694	1817.807614	19.921933
55.046007	1827.583985	19.926951
54.879975	1823.380985	19.931968
54.865282	1833.814063	19.936986
55.254969	1830.271974	19.942003
55.388116	1824.870147	19.947021
55.473312	1818.592144	19.952039
55.586915	1822.516308	19.957056
55.875352	1830.916745	19.962074
55.455314	1834.555264	19.967091
55.590821	1819.296765	19.972109
55.549109	1821.673558	19.977127
55.666746	1820.313887	19.982144
55.668024	1826.853068	19.987162
55.558893	1839.241908	19.992179
55.986834	1840.986501	19.997197
55.779082	1848.921849	20.002215
55.926310	1851.329008	20.007232
56.014412	1851.015456	20.012250
56.070882	1843.949778	20.017267
56.147971	1846.393174	20.022285
56.057984	1855.392595	20.027303
56.219727	1839.476668	20.032320
55.786465	1849.864874	20.037338
55.602698	1851.582223	20.042355
56.119766	1861.136680	20.047373
56.034475	1872.521342	20.052391
56.268851	1877.064117	20.057408
55.965581	1877.550397	20.062426
56.248493	1894.217414	20.067443
56.518401	1898.568420	20.072461
56.565947	1903.784307	20.077479
57.207004	1900.464774	20.082496
57.195431	1899.519848	20.087514
56.839750	1891.559287	20.092531
56.696985	1899.058408	20.097549
56.440577	1901.743425	20.102567
56.770263	1903.443454	20.107584
57.376396	1910.020453	20.112602
57.189558	1927.512239	20.117619
57.494625	1924.712439	20.122637
57.720842	1918.383902	20.127655
57.816270	1917.122385	20.132672
57.972910	1916.125855	20.137690
58.071622	1911.508941	20.142707
58.107603	1915.659898	20.147725
58.056631	1902.513541	20.152743
57.828174	1895.969047	20.157760
57.854588	1895.273809	20.162778
57.426167	1885.481516	20.167795
57.897245	1890.246004	20.172813
57.817906	1905.997725	20.177831
58.023353	1909.733936	20.182848
58.032508	1904.158992	20.187866
58.133781	1908.337591	20.192883
58.347757	1910.005252	20.197901
58.218615	1914.879568	20.202919
58.108071	1899.473345	20.207936
58.370397	1911.497899	20.212954
57.934755	1911.648286	20.217971
58.163608	1904.757564	20.222989
58.532132	1930.494314	20.228007
58.529686	1935.916875	20.233024
58.413173	1940.584075	20.238042
58.604606	1940.232240	20.243059
58.798773	1932.914562	20.248077
58.658052	1934.609393	20.253095
59.108715	1942.952906	20.258112
59.299856	1930.983676	20.263130
58.736192	1935.585222	20.268147
58.823395	1932.576538	20.273165
58.891307	1928.750303	20.278183
58.957689	1926.486555	20.283200
58.947298	1933.668282	20.288218
59.155692	1944.359985	20.293235
59.328267	1952.819661	20.298253
59.544180	1953.827407	20.303271
59.572588	1951.285560	20.308288
59.480807	1954.449762	20.313306
59.365849	1958.362425	20.318323
59.809332	1957.087402	20.323341
59.377854	1960.465786	20.328359
59.406063	1954.038861	20.333376
59.754057	1952.324327	20.338394
59.542874	1952.123941	20.343411
59.845478	1940.553841	20.348429
59.523101	1959.758540	20.353447
60.045778	1973.961056	20.358464
60.186657	1972.159040	20.363482
59.779465	1981.990926	20.368499
60.065006	1975.640450	20.373517
60.196396	1989.604457	20.378535
60.162137	1981.356792	20.383552
60.664461	1979.741163	20.388570
60.381881	1968.382659	20.393587
60.819664	1967.165338	20.398605
60.891041	1974.612004	20.403623
60.605240	1982.114633	20.408640
60.661953	1971.567730	20.413658
60.157882	1980.950853	20.418675
60.437679	1989.087609	20.423693
60.935296	1999.456297	20.428711
61.086208	2012.063311	20.433728
61.543988	1995.479119	20.438746
61.542331	2000.608061	20.443763
61.478720	1991.967326	20.448781
61.294158	1986.485828	20.453799
61.219738	1984.474526	20.458816
61.535038	1986.271499	20.463834
61.350579	1987.862726	20.468851
61.698039	1990.648821	20.473869
61.171268	1989.326979	20.478887
61.681406	1993.501504	20.483904
61.788931	1981.109804	20.488922
61.670026	1988.415861	20.493939
61.390938	1985.915874	20.498957
61.366956	1983.451665	20.503975
61.494655	1984.242841	20.508992
61.524608	1980.753929	20.514010
61.296742	1994.859441	20.519027
61.821173	2001.496616	20.524045
61.954024	2013.825571	20.529063
62.020431	2016.223322	20.534080
62.062700	2010.157123	20.539098
62.049723	2007.949983	20.544115
62.499787	2010.013047	20.549133
62.691715	2009.749502	20.554151
62.764697	2015.059275	20.559168
62.856181	2004.775170	20.564186
62.825957	1996.807756	20.569203
62.960036	1992.762840	20.574221
62.560604	2000.340090	20.579239
62.900616	1994.899489	20.584256
63.007324	1987.355630	20.589274
62.876392	1990.664838	20.594291
62.945793	1994.141492	20.599309
63.348532	2006.068366	20.604327
63.168237	2005.752677	20.609344
63.296249	2003.564478	20.614362
63.434042	2016.075712	20.619379
63.423887	2003.727682	20.624397
63.175735	2003.157516	20.629415
63.431915	2014.428803	20.634432
63.193302	2012.339072	20.639450
63.418366	2004.688292	20.644467
63.590700	2003.361067	20.649485
63.742394	2016.334066	20.654503
63.900922	2011.998113	20.659520
64.126272	2002.280065	20.664538
63.918734	2006.342954	20.669555
64.374447	2000.757981	20.674573
64.150124	2012.697890	20.679591
63.780272	2009.713462	20.684608
64.021561	2001.305841	20.689626
63.297639	2008.425807	20.694643
63.890671	1998.422917	20.699661
63.833031	1993.896756	20.704679
64.026632	2016.413446	20.709696
64.226226	2016.666296	20.714714
64.124185	2037.777541	20.719731
64.241577	2032.848374	20.724749
64.389592	2033.267109	20.729767
64.070240	2035.273984	20.734784
64.473285	2041.239012	20.739802
63.912704	2060.629475	20.744819
64.384554	2063.667515	20.749837
64.737416	2060.156401	20.754855
64.385723	2075.240824	20.759872
64.981666	2085.543660	20.764890
65.224006	2085.527859	20.769907
65.497144	2081.088719	20.774925
65.279700	2090.827813	20.779943
65.038125	2094.873963	20.784960
64.937450	2086.485163	20.789978
65.100358	2089.022453	20.794995
65.403592	2087.128711	20.800013
65.056334	2100.192568	20.805031
65.673108	2118.729541	20.810048
65.819254	2111.324632	20.815066
65.493111	2120.913500	20.820083
65.801698	2113.025507	20.825101
65.850812	2114.895759	20.830119
65.843132	2120.723174	20.835136
65.941936	2113.360398	20.840154
65.686487	2120.741555	20.845171
65.951975	2134.814065	20.850189
66.390238	2139.299715	20.855207
66.440985	2149.041007	20.860224
66.319924	2154.870417	20.865242
66.313774	2147.574569	20.870259
66.478799	2137.957426	20.875277
66.433378	2143.894913	20.880295
66.317103	2151.074379	20.885312
66.470172	2135.822329	20.890330
66.491893	2146.013177	20.895347
66.874300	2159.862243	20.900365
66.726844	2164.736339	20.905383
67.265542	2171.989937	20.910400
67.278070	2171.233742	20.915418
66.957376	2169.062170	20.920435
66.733882	2164.991180	20.925453
66.840068	2163.207205	20.930471
66.650625	2163.192776	20.935488
66.797625	2169.286334	20.940506
67.303169	2183.961960	20.945523
67.926876	2176.655787	20.950541
68.098599	2177.629441	20.955559
67.676407	2173.747385	20.960576
68.389900	2172.733030	20.965594
68.371919	2169.399928	20.970611
68.140900	2147.826418	20.975629
68.485482	2145.686329	20.980647
68.320121	2143.114849	20.985664
68.165606	2140.263933	20.990682
68.084031	2143.136208	20.995699
67.863333	2148.245857	21.000717
67.974226	2145.826772	21.005735
68.277189	2149.623501	21.010752
68.472486	2145.202853	21.015770
68.384872	2138.954970	21.020787
68.119962	2148.335425	21.025805
68.464863	2147.053743	21.030823
68.093414	2158.811654	21.035840
68.754067	2164.553310	21.040858
68.856771	2172.519061	21.045875
68.636446	2176.880665	21.050893
68.748309	2167.170841	21.055911
68.849113	2170.585799	21.060928
69.074873	2168.836743	21.065946
68.957116	2163.559339	21.070963
69.051474	2162.522056	21.075981
69.056282	2162.003778	21.080999
68.849665	2172.564961	21.086016
68.894015	2180.539859	21.091034
69.465413	2192.210037	21.096051
69.331985	2194.935795	21.101069
69.710143	2187.743836	21.106087
69.263498	2188.221026	21.111104
69.054444	2199.161339	21.116122
69.642003	2215.768300	21.121139
69.299149	2220.865547	21.126157
69.731238	2218.228856	21.131175
69.262341	2220.385424	21.136192
69.436222	2235.030996	21.141210
70.140173	2236.199004	21.146227
70.275969	2238.364987	21.151245
71.011327	2232.613041	21.156263
70.785853	2237.202706	21.161280
71.042397	2230.421142	21.166298
70.791737	2220.502973	21.171315
70.844480	2207.194962	21.176333
70.876678	2199.646907	21.181351
70.703799	2197.332241	21.186368
70.457375	2190.077175	21.191386
70.879218	2207.079356	21.196403
70.837528	2217.330676	21.201421
71.052501	2218.316493	21.206439
71.113701	2224.925333	21.211456
71.144496	2225.321409	21.216474
71.281342	2215.970596	21.221491
71.128865	2233.877058	21.226509
71.245354	2223.270144	21.231527
71.344384	2224.454024	21.236544
71.068269	2215.979031	21.241562
71.184006	2225.290421	21.246579
71.239236	2234.204157	21.251597
71.277957	2242.732284	21.256615
71.227374	2246.571801	21.261632
71.336208	2257.055206	21.266650
71.617731	2264.768898	21.271667
71.118575	2273.902069	21.276685
71.872367	2272.187050	21.281703
71.839177	2269.932548	21.286720
72.053638	2274.087186	21.291738
72.201608	2281.673473	21.296755
72.040576	2290.352850	21.301773
72.430326	2295.319558	21.306791
72.638588	2297.739308	21.311808
72.728056	2300.060894	21.316826
73.031076	2296.049408	21.321843
72.537380	2299.608032	21.326861
72.854422	2295.389202	21.331879
72.971717	2293.663440	21.336896
72.864232	2283.255699	21.341914
72.941500	2286.851110	21.346931
72.897780	2296.664093	21.351949
73.007961	2286.897658	21.356967
73.123838	2288.864776	21.361984
72.655039	2292.735109	21.367002
73.355931	2286.553003	21.372019
72.846747	2290.464380	21.377037
73.141196	2301.240654	21.382055
73.067396	2316.395360	21.387072
73.329344	2312.301934	21.392090
73.622449	2311.419715	21.397107
73.352721	2317.572301	21.402125
73.632508	2325.125330	21.407143
73.579599	2340.254689	21.412160
73.385369	2338.666103	21.417178
73.889113	2341.774942	21.422195
73.659871	2347.899103	21.427213
73.830153	2348.980300	21.432231
73.792353	2367.509622	21.437248
74.044370	2358.440523	21.442266
74.303242	2366.710131	21.447283
74.525261	2361.748702	21.452301
74.662714	2357.611649	21.457319
74.354730	2355.049858	21.462336
74.615144	2387.217458	21.467354
74.669387	2381.619521	21.472371
74.661405	2389.763674	21.477389
74.691221	2390.620702	21.482407
74.756499	2385.863723	21.487424
74.870785	2390.371790	21.492442
75.190810	2383.406635	21.497459
74.942090	2397.862904	21.502477
75.559692	2400.887636	21.507495
75.842899	2405.675387	21.512512
75.523358	2410.592291	21.517530
75.885169	2398.428736	21.522547
75.978656	2408.135067	21.527565
75.462420	2392.946632	21.532583
75.951522	2391.516096	21.537600
75.908514	2401.830851	21.542618
76.180164	2389.261661	21.547635
76.047179	2400.297486	21.552653
76.434201	2404.526116	21.557671
76.376303	2396.439771	21.562688
76.157603	2409.098660	21.567706
76.462110	2405.762331	21.572723
76.313257	2407.849842	21.577741
76.348207	2399.938316	21.582759
76.571483	2399.534142	21.587776
76.152052	2403.582976	21.592794
76.542777	2388.413411	21.597811
76.391038	2393.060998	21.602829
76.337086	2410.488247	21.607847
76.653071	2414.819537	21.612864
76.462035	2427.824436	21.617882
76.559272	2422.106130	21.622899
76.516990	2430.113648	21.627917
77.154522	2448.748708	21.632935
77.204346	2449.634167	21.637952
77.210627	2452.379105	21.642970
77.731836	2446.487056	21.647987
77.138763	2455.410946	21.653005
77.653308	2449.570439	21.658023
77.595426	2451.088221	21.663040
77.698458	2454.124147	21.668058
77.641725	2452.059522	21.673075
78.012569	2458.670434	21.678093
78.008708	2473.776441	21.683111
78.385905	2476.677888	21.688128
78.038380	2477.594040	21.693146
78.023823	2469.765988	21.698163
78.115639	2477.032916	21.703181
77.988533	2472.883631	21.708199
78.427723	2479.853112	21.713216
78.443871	2477.852814	21.718234
78.351048	2475.588691	21.723251
78.340121	2476.559416	21.728269
78.490082	2479.960420	21.733287
78.632510	2491.574913	21.738304
78.570209	2502.571320	21.743322
78.792180	2493.434270	21.748339
78.593244	2499.964034	21.753357
78.910555	2500.151107	21.758375
79.192100	2501.420032	21.763392
79.050618	2524.094010	21.768410
78.761263	2527.516509	21.773427
79.033245	2535.061380	21.778445
79.301359	2526.362103	21.783463
79.099674	2537.102627	21.788480
79.487563	2546.033835	21.793498
79.491096	2544.423714	21.798515
79.595832	2554.762751	21.803533
79.889455	2555.859355	21.808551
79.668137	2561.111244	21.813568
79.660002	2567.847852	21.818586
80.010993	2580.982560	21.823603
80.046100	2580.465835	21.828621
80.246690	2580.901596	21.833639
80.384800	2578.456096	21.838656
80.221138	2583.386499	21.843674
80.648895	2578.755736	21.848691
80.601297	2588.399053	21.853709
80.635869	2593.449896	21.858727
81.298363	2602.877814	21.863744
81.177622	2606.122415	21.868762
81.201944	2603.622147	21.873779
81.213772	2596.986095	21.878797
81.197478	2591.130870	21.883815
81.405269	2590.230443	21.888832
81.213085	2597.169486	21.893850
81.218550	2599.191811	21.898867
81.286581	2592.786825	21.903885
81.088734	2588.355073	21.908903
81.354882	2583.162581	21.913920
81.404912	2584.922273	21.918938
81.623776	2602.347995	21.923955
82.039352	2606.881504	21.928973
81.966673	2602.657382	21.933991
82.408076	2605.646633	21.939008
81.823923	2605.694042	21.944026
82.015956	2600.977115	21.949043
81.784203	2600.754694	21.954061
82.026060	2597.892102	21.959079
82.473945	2603.765078	21.964096
82.391192	2609.837971	21.969114
82.742211	2616.928630	21.974131
82.678491	2620.268453	21.979149
82.776999	2618.652913	21.984167
83.172326	2616.792032	21.989184
83.020333	2615.727040	21.994202
83.663066	2606.874346	21.999219
83.582828	2616.267141	22.004237
83.214194	2597.495242	22.009255
83.529027	2586.165838	22.014272
83.068064	2585.878330	22.019290
83.645775	2590.146564	22.024307
83.943980	2599.224410	22.029325
83.598042	2596.305570	22.034343
83.430846	2582.817120	22.039360
83.539664	2598.271693	22.044378
83.859083	2602.182720	22.049395
83.739319	2605.613381	22.054413
83.532130	2607.867863	22.059431
83.777627	2604.367154	22.064448
83.665300	2600.632139	22.069466
84.120598	2617.597906	22.074483
84.248529	2635.943730	22.079501
83.900483	2633.170399	22.084519
84.181055	2635.758769	22.089536
83.893767	2625.609401	22.094554
84.565006	2648.620163	22.099571
84.596922	2654.914975	22.104589
84.598310	2660.807424	22.109607
84.906725	2656.536207	22.114624
84.631170	2661.465225	22.119642
84.843670	2656.505206	22.124659
84.887268	2652.928810	22.129677
84.718705	2678.791812	22.134695
84.888207	2678.882110	22.139712
84.737655	2685.637918	22.144730
85.206047	2692.482972	22.149747
85.417155	2704.228870	22.154765
85.432098	2711.921397	22.159783
85.403469	2699.897716	22.164800
85.318252	2708.540166	22.169818
85.865329	2704.064268	22.174835
86.252360	2718.594780	22.179853
85.937998	2724.681904	22.184871
86.481823	2720.503194	22.189888
86.394946	2732.036989	22.194906
86.370853	2721.436026	22.199923
86.319757	2722.223687	22.204941
86.348830	2721.786808	22.209959
86.944944	2717.751404	22.214976
86.669159	2710.926813	22.219994
86.622713	2722.331176	22.225011
86.600555	2713.642568	22.230029
86.470463	2729.800641	22.235047
86.949191	2730.757789	22.240064
86.990683	2741.671801	22.245082
86.993358	2738.995002	22.250099
87.359061	2732.795825	22.255117
87.062841	2740.287776	22.260135
87.273537	2750.720791	22.265152
87.229160	2756.487882	22.270170
87.602457	2759.086992	22.275187
87.644101	2774.410211	22.280205
87.558293	2769.026625	22.285223
87.744222	2771.175349	22.290240
87.815086	2770.031245	22.295258
88.262889	2788.301860	22.300275
88.352151	2793.833403	22.305293
88.212811	2795.294539	22.310311
88.029737	2797.706232	22.315328
87.979519	2793.096646	22.320346
88.165763	2797.401013	22.325363
88.340295	2793.860886	22.330381
88.423720	2819.419489	22.335399
88.683139	2821.711360	22.340416
88.485243	2826.353664	22.345434
88.540870	2822.920535	22.350451
88.410029	2821.729124	22.355469
88.680130	2830.495868	22.360487
88.803504	2846.611179	22.365504
88.845513	2847.071792	22.370522
89.155932	2850.154199	22.375539
89.344399	2851.513482	22.380557
88.920869	2867.559840	22.385575
88.913816	2872.560472	22.390592
89.366561	2872.385459	22.395610
89.210917	2876.898064	22.400627
89.927391	2895.350785	22.405645
90.024753	2898.605455	22.410663
89.887013	2899.861194	22.415680
90.398184	2901.049985	22.420698
90.462928	2901.655380	22.425715
90.789603	2901.784179	22.430733
90.657493	2900.987490	22.435751
90.686886	2900.553714	22.440768
90.574397	2899.918074	22.445786
90.714154	2905.757363	22.450803
90.670335	2899.057326	22.455821
90.804284	2902.164233	22.460839
91.149064	2896.066122	22.465856
91.154298	2913.326773	22.470874
91.253096	2916.922093	22.475891
91.237645	2921.157090	22.480909
91.191172	2922.335407	22.485927
90.983646	2912.397473	22.490944
91.338429	2920.772247	22.495962
91.123935	2918.561849	22.500979
91.665880	2940.015127	22.505997
91.367384	2956.755284	22.511015
91.786175	2960.041668	22.516032
91.371370	2954.128823	22.521050
91.678880	2959.398975	22.526067
92.055149	2963.566298	22.531085
91.909326	2977.558724	22.536103
91.842996	2972.405586	22.541120
91.859519	2988.932294	22.546138
92.043108	3006.262933	22.551155
92.749686	3001.054976	22.556173
92.520163	3006.412436	22.561191
92.816248	3000.697511	22.566208
93.215994	2993.037885	22.571226
93.055868	2997.727972	22.576243
93.295190	3001.676885	22.581261
93.239915	3009.964446	22.586279
93.814172	3008.353242	22.591296
93.859338	3012.995388	22.596314
93.820111	3003.747503	22.601331
93.874841	2983.264470	22.606349
93.646928	3002.101978	22.611367
93.618222	3005.007137	22.616384
94.165866	3018.291261	22.621402
94.077985	3018.333511	22.626419
94.030599	3013.840205	22.631437
93.812746	3020.054339	22.636455
93.333297	3019.854937	22.641472
94.006251	3029.865349	22.646490
93.902456	3045.460928	22.651507
94.568324	3038.807463	22.656525
94.511369	3043.815960	22.661543
94.347179	3049.778666	22.666560
94.386100	3052.777394	22.671578
94.713397	3063.454292	22.676595
94.762266	3068.828123	22.681613
94.752507	3073.671421	22.686631
95.126735	3063.730634	22.691648
95.180190	3070.640843	22.696666
95.098742	3069.381708	22.701683
95.352651	3071.573475	22.706701
95.183960	3076.473236	22.711719
95.308355	3081.560644	22.716736
95.885649	3090.806482	22.721754
95.480805	3089.796857	22.726771
95.663286	3089.004528	22.731789
95.605973	3098.154106	22.736807
95.965237	3104.224195	22.741824
96.096220	3099.564047	22.746842
95.996644	3110.787603	22.751859
96.132413	3109.406059	22.756877
96.076617	3118.946786	22.761895
95.969019	3119.446627	22.766912
96.409033	3134.057548	22.771930
96.374536	3143.190950	22.776947
96.708320	3140.686311	22.781965
96.375377	3152.208425	22.786983
96.703677	3167.954196	22.792000
97.027045	3168.721083	22.797018
96.609025	3178.425905	22.802035
96.913266	3171.191482	22.807053
96.927458	3189.382093	22.812071
97.159528	3194.566289	22.817088
97.271221	3190.581427	22.822106
97.286847	3206.975911	22.827123
97.774561	3211.858088	22.832141
97.838185	3210.853968	22.837159
98.124115	3210.260053	22.842176
98.159182	3214.114764	22.847194
98.021946	3218.634038	22.852211
98.672848	3202.536116	22.857229
98.238249	3209.841625	22.862247
98.317470	3214.049234	22.867264
98.372277	3228.537519	22.872282
98.335756	3232.722233	22.877299
98.830549	3241.870605	22.882317
99.042851	3231.983502	22.887335
99.056230	3225.245976	22.892352
98.950303	3223.255252	22.897370
99.192012	3237.436509	22.902387
99.350817	3243.954680	22.907405
99.324060	3264.376963	22.912423
99.403102	3263.591365	22.917440
99.647413	3253.935957	22.922458
99.866396	3256.818132	22.927475
99.783760	3254.504971	22.932493
99.809026	3261.899424	22.937511
99.762951	3265.059849	22.942528
100.110806	3275.973531	22.947546
99.603425	3288.132224	22.952563
100.388392	3277.615650	22.957581
100.336094	3283.156897	22.962599
100.142781	3281.179857	22.967616
100.650537	3288.397728	22.972634
100.605512	3303.592942	22.977651
100.716929	3305.090583	22.982669
100.504036	3303.296517	22.987687
101.006597	3309.341069	22.992704
100.965204	3308.277645	22.997722
101.016617	3312.634823	23.002739
101.181845	3323.229952	23.007757
100.918390	3334.110035	23.012775
100.862173	3330.141979	23.017792
101.014206	3330.932561	23.022810
101.070897	3353.860598	23.027827
101.411794	3355.994583	23.032845
101.490460	3364.955708	23.037863
101.836324	3364.008362	23.042880
101.878694	3376.387146	23.047898
101.734467	3399.166809	23.052915
101.517886	3389.968607	23.057933
102.148361	3386.480029	23.062951
102.383811	3404.405781	23.067968
102.365733	3411.538800	23.072986
102.679653	3410.233480	23.078003
102.763683	3413.181012	23.083021
102.841997	3412.139860	23.088039
102.603439	3416.053264	23.093056
102.897786	3415.773656	23.098074
103.199140	3435.747031	23.103091
102.869319	3437.146527	23.108109
103.199091	3430.482452	23.113127
103.306212	3437.362298	23.118144
103.500816	3439.108892	23.123162
103.272515	3454.418167	23.128179
104.144378	3464.388190	23.133197
103.963227	3461.853712	23.138215
103.985149	3463.942994	23.143232
104.342553	3464.341585	23.148250
103.620363	3467.481720	23.153267
104.099817	3468.356732	23.158285
104.174848	3482.021408	23.163303
104.145777	3487.366542	23.168320
104.844579	3487.733741	23.173338
104.507124	3490.046615	23.178355
105.048481	3486.411008	23.183373
104.712091	3488.950971	23.188391
104.853236	3505.098804	23.193408
105.144399	3501.770680	23.198426
105.063364	3509.314455	23.203443
104.957712	3507.408877	23.208461
105.601839	3514.760134	23.213479
106.005550	3527.707364	23.218496
105.973511	3529.565227	23.223514
105.487851	3542.582365	23.228531
106.165680	3530.722051	23.233549
105.942819	3526.363425	23.238567
105.933565	3537.478405	23.243584
106.036408	3527.216905	23.248602
106.159062	3532.588783	23.253619
106.418235	3549.554593	23.258637
106.739435	3545.053910	23.263655
106.537219	3558.086623	23.268672
106.627254	3564.874505	23.273690
106.626716	3552.132522	23.278707
106.764176	3558.092323	23.283725
107.200550	3578.963198	23.288743
106.875564	3581.817022	23.293760
107.124443	3579.107839	23.298778
107.261271	3588.258812	23.303795
107.534405	3583.730930	23.308813
107.619484	3582.013250	23.313831
107.460693	3598.574294	23.318848
107.123158	3605.536494	23.323866
107.483737	3603.021283	23.328883
107.801958	3604.268761	23.333901
108.698565	3616.191928	23.338919
108.495936	3622.122967	23.343936
108.939747	3613.351455	23.348954
108.954842	3616.246693	23.353971
109.032270	3619.551961	23.358989
109.318568	3594.483657	23.364007
108.836510	3589.572231	23.369024
108.990485	3584.349683	23.374042
108.987804	3590.028442	23.379059
108.940061	3593.523759	23.384077
109.413193	3601.072284	23.389095
109.230182	3615.740174	23.394112
109.408878	3606.479933	23.399130
109.391835	3606.829877	23.404147
109.472501	3617.795095	23.409165
109.474226	3618.303072	23.414183
109.677138	3624.650341	23.419200
109.826950	3636.321229	23.424218
110.180736	3638.623672	23.429235
109.994171	3646.689054	23.434253
109.970736	3643.545915	23.439271
110.325828	3646.877126	23.444288
110.391289	3647.132080	23.449306
110.737565	3661.455105	23.454323
110.197376	3672.353495	23.459341
110.302926	3668.246393	23.464359
110.513940	3662.888632	23.469376
110.390481	3689.525632	23.474394
110.796989	3700.752331	23.479411
110.716912	3698.236704	23.484429
111.081960	3709.716100	23.489447
110.983424	3728.054325	23.494464
111.508339	3717.287856	23.499482
111.186513	3732.012308	23.504499
111.256236	3746.445012	23.509517
111.704159	3751.093688	23.514535
112.084786	3760.544284	23.519552
111.880155	3757.836686	23.524570
112.110102	3772.443161	23.529587
112.038267	3784.069960	23.534605
112.256216	3772.341510	23.539623
112.153012	3792.306065	23.544640
112.459677	3796.118348	23.549658
112.795734	3794.692748	23.554675
113.127228	3803.680764	23.559693
113.325944	3792.725471	23.564711
113.317363	3791.357022	23.569728
113.289537	3809.845227	23.574746
113.276867	3811.084589	23.579763
113.556582	3812.044571	23.584781
113.829663	3814.280772	23.589799
113.336739	3813.515319	23.594816
113.797274	3815.652711	23.599834
113.860781	3822.173396	23.604851
114.177940	3833.919198	23.609869
114.421754	3839.644639	23.614887
114.365098	3845.114143	23.619904
114.027832	3845.088147	23.624922
114.272252	3836.751784	23.629939
114.497704	3860.569376	23.634957
114.891581	3855.097688	23.639975
114.741406	3859.556021	23.644992
114.913810	3864.389929	23.650010
114.995764	3852.436536	23.655027
114.629710	3869.933026	23.660045
115.149605	3881.006348	23.665063
115.310955	3881.176841	23.670080
114.911676	3879.023681	23.675098
115.628966	3884.043678	23.680115
115.670715	3901.526811	23.685133
115.336553	3902.355713	23.690151
115.708136	3907.849680	23.695168
116.032507	3920.598143	23.700186
116.271538	3924.329514	23.705203
116.175484	3941.982627	23.710221
116.382372	3926.256645	23.715239
116.436276	3929.925485	23.720256
116.132766	3932.630803	23.725274
117.016723	3948.943577	23.730291
116.819343	3954.854963	23.735309
117.303998	3950.319104	23.740327
116.930663	3949.812672	23.745344
117.020136	3958.377847	23.750362
117.065703	3956.445374	23.755379
117.136156	3979.277354	23.760397
117.156125	3979.921365	23.765415
117.756168	3982.996471	23.770432
117.529709	3985.806513	23.775450
118.115448	3993.930967	23.780467
117.636096	4011.407467	23.785485
118.226042	4013.047990	23.790503
117.889296	4011.538395	23.795520
117.878514	4024.639299	23.800538
118.510612	4037.285975	23.805555
118.285324	4030.257273	23.810573
118.547914	4039.780168	23.815591
118.632610	4043.977643	23.820608
118.496098	4054.301675	23.825626
118.916664	4059.510249	23.830643
118.864575	4066.980278	23.835661
119.314458	4072.455715	23.840679
118.948703	4086.552893	23.845696
119.176298	4079.323806	23.850714
119.652814	4103.500093	23.855731
119.280082	4115.486732	23.860749
119.569519	4110.299628	23.865767
119.610800	4125.721897	23.870784
120.011191	4134.232132	23.875802
120.373520	4131.905961	23.880819
120.556531	4135.456767	23.885837
120.587518	4146.622631	23.890855
121.134189	4158.578888	23.895872
120.826126	4156.881714	23.900890
121.034019	4157.360563	23.905907
121.145263	4170.366700	23.910925
120.967468	4154.018997	23.915943
121.262189	4167.182617	23.920960
121.222240	4168.363148	23.925978
121.808119	4168.091517	23.930995
121.998688	4178.373846	23.936013
121.570308	4176.992226	23.941031
122.233759	4173.009086	23.946048
122.034573	4171.383233	23.951066
122.591088	4180.153110	23.956083
122.637556	4192.913739	23.961101
122.608686	4198.921906	23.966119
122.863641	4203.379980	23.971136
122.477886	4202.847078	23.976154
122.979028	4191.496956	23.981171
123.141289	4205.707202	23.986189
122.792967	4196.276713	23.991207
123.254227	4189.298212	23.996224
122.754871	4202.207490	24.001242
122.682306	4214.857369	24.006259
122.835892	4223.501005	24.011277
123.068231	4228.638111	24.016295
123.821629	4240.539940	24.021312
123.603122	4257.846394	24.026330
123.988959	4257.782865	24.031347
124.140268	4270.981654	24.036365
124.059526	4267.642215	24.041383
124.335474	4274.240257	24.046400
124.011593	4280.395676	24.051418
124.651192	4281.292989	24.056435
124.583767	4301.012606	24.061453
124.691472	4302.037442	24.066471
125.251177	4295.873628	24.071488
125.194651	4297.220901	24.076506
125.296722	4289.809383	24.081523
125.102639	4292.750127	24.086541
125.054300	4298.070110	24.091559
125.843586	4307.823120	24.096576
125.926069	4314.527241	24.101594
126.156720	4319.620446	24.106611
125.964858	4309.549874	24.111629
125.933474	4308.592142	24.116647
126.005931	4311.573200	24.121664
126.120846	4329.878590	24.126682
126.192042	4329.384571	24.131699
126.283454	4338.363119	24.136717
126.615283	4343.942360	24.141735
127.020439	4350.018307	24.146752
126.819764	4363.998298	24.151770
127.119085	4358.342417	24.156787
127.220479	4372.205647	24.161805
127.314836	4367.156353	24.166823
127.433147	4378.886315	24.171840
127.603971	4391.614976	24.176858
127.858648	4384.432029	24.181875
128.022795	4388.241515	24.186893
127.492740	4395.909664	24.191911
128.115747	4405.811881	24.196928
128.002616	4424.623411	24.201946
128.336138	4425.537120	24.206963
128.313460	4421.301583	24.211981
128.248035	4423.524607	24.216999
128.532767	4438.268234	24.222016
128.364908	4448.086049	24.227034
128.873283	4452.930609	24.232051
128.928060	4465.355540	24.237069
128.984059	4477.906547	24.242087
128.981442	4476.388756	24.247104
129.183146	4496.331567	24.252122
129.695900	4507.845147	24.257139
129.580823	4507.411871	24.262157
129.627510	4515.027591	24.267175
129.880885	4527.588745	24.272192
129.745999	4545.141204	24.277210
130.000688	4529.157849	24.282227
130.093026	4545.500490	24.287245
130.582832	4557.718442	24.292263
130.458391	4556.948885	24.297280
130.475415	4565.415219	24.302298
130.988528	4578.358688	24.307315
130.653730	4586.618160	24.312333
130.788885	4595.293270	24.317351
131.197413	4612.208268	24.322368
131.222791	4616.389916	24.327386
131.554268	4618.190939	24.332403
131.699903	4617.903050	24.337421
131.733083	4632.613645	24.342439
132.497423	4637.048841	24.347456
132.556758	4644.002919	24.352474
132.507855	4633.098542	24.357491
132.654055	4641.320560	24.362509
132.328478	4644.414535	24.367527
132.818981	4636.184455	24.372544
132.404166	4643.610539	24.377562
132.991502	4653.130228	24.382579
132.940133	4654.012710	24.387597
133.037105	4659.161676	24.392615
133.230681	4650.602481	24.397632
133.064733	4672.654827	24.402650
133.288672	4671.483467	24.407667
133.502499	4681.970769	24.412685
133.378753	4683.663194	24.417703
133.570534	4697.114788	24.422720
133.506553	4710.155077	24.427738
134.164055	4722.864541	24.432755
134.298040	4729.172492	24.437773
134.097843	4734.898335	24.442791
135.089536	4740.039726	24.447808
134.833859	4738.056512	24.452826
134.830613	4742.722469	24.457843
135.139346	4750.612888	24.462861
135.080284	4761.310285	24.467879
135.456824	4756.323998	24.472896
135.347687	4770.138445	24.477914
135.350682	4760.393785	24.482931
135.860906	4769.931929	24.487949
135.392482	4784.957973	24.492967
135.736400	4780.740676	24.497984
135.700939	4792.861155	24.503002
136.189331	4807.077596	24.508019
136.426495	4809.666771	24.513037
136.460542	4811.934233	24.518055
136.872856	4811.661379	24.523072
136.802693	4817.357407	24.528090
136.800958	4822.001051	24.533107
137.222078	4830.678820	24.538125
136.944973	4836.416744	24.543143
137.538320	4829.871852	24.548160
137.424116	4839.037532	24.553178
137.516813	4851.242139	24.558195
137.623199	4851.705345	24.563213
137.725349	4854.643961	24.568231
137.910841	4865.902853	24.573248
138.101589	4885.285938	24.578266
138.452949	4893.185524	24.583283
138.800696	4882.392467	24.588301
138.472801	4887.103009	24.593319
138.313060	4902.731043	24.598336
138.772637	4913.113689	24.603354
138.886843	4918.288438	24.608371
138.911320	4921.917897	24.613389
138.957714	4941.689820	24.618407
139.434229	4938.764850	24.623424
139.186046	4948.557639	24.628442
139.352894	4960.049941	24.633459
139.412279	4961.338068	24.638477
139.233878	4972.300498	24.643495
139.610960	4992.806658	24.648512
140.057474	4996.335291	24.653530
140.300077	5008.835334	24.658547
140.646805	5012.512179	24.663565
140.492527	5016.782041	24.668583
140.768182	5015.015431	24.673600
140.790240	5027.982492	24.678618
140.747864	5036.578301	24.683635
141.143195	5046.298734	24.688653
141.047501	5050.142755	24.693671
141.054409	5055.495339	24.698688
141.353908	5063.235824	24.703706
141.569020	5078.240250	24.708723
141.829428	5085.121959	24.713741
141.845447	5093.670768	24.718759
141.948169	5089.257599	24.723776
142.412740	5108.736913	24.728794
142.069824	5115.198627	24.733811
142.336590	5111.937168	24.738829
142.266628	5120.224834	24.743847
142.871294	5132.204217	24.748864
142.806801	5137.694276	24.753882
143.331495	5143.821209	24.758899
143.327634	5135.794620	24.763917
143.557673	5151.579607	24.768935
143.818858	5150.058311	24.773952
143.787463	5172.895119	24.778970
144.121717	5168.328862	24.783987
144.534055	5167.399425	24.789005
144.274508	5152.351532	24.794023
144.303675	5160.740481	24.799040
144.698503	5168.481860	24.804058
144.823632	5185.662755	24.809075
145.001069	5182.626772	24.814093
145.078320	5194.884535	24.819111
145.396349	5196.855025	24.824128
145.634677	5187.499412	24.829146
145.346729	5187.692959	24.834163
145.467954	5185.050890	24.839181
145.655578	5202.341962	24.844199
145.929095	5204.868679	24.849216
145.874270	5213.940016	24.854234
145.551692	5212.061929	24.859251
145.843928	5223.632609	24.864269
146.121783	5238.046516	24.869287
146.527962	5245.157980	24.874304
146.548102	5259.605967	24.879322
146.567449	5262.784899	24.884339
147.258333	5261.303600	24.889357
146.702972	5273.849923	24.894375
146.881702	5287.512336	24.899392
147.342880	5288.093585	24.904410
147.490627	5291.104044	24.909427
147.854730	5300.971555	24.914445
147.838343	5322.066889	24.919463
147.573177	5309.680798	24.924480
148.023162	5323.868939	24.929498
148.221170	5336.679231	24.934515
148.834599	5342.309363	24.939533
148.692000	5341.631003	24.944551
148.532150	5349.320465	24.949568
148.667880	5358.156838	24.954586
148.947266	5369.303476	24.959603
149.351542	5370.594419	24.964621
149.151763	5375.666969	24.969639
149.251499	5392.227019	24.974656
149.488514	5393.433686	24.979674
149.227661	5403.048772	24.984691
149.874942	5415.100583	24.989709
149.946059	5433.846407	24.994727
150.091128	5427.008518	24.999744
150.473980	5447.586890	25.004762
150.088882	5451.413200	25.009779
150.543413	5455.237394	25.014797
150.690416	5464.024702	25.019815
151.146670	5473.186559	25.024832
151.033925	5479.849092	25.029850
151.096791	5484.463844	25.034867
151.124406	5495.744703	25.039885
151.329460	5506.893600	25.044903
151.408287	5511.935167	25.049920
151.772568	5521.461849	25.054938
151.711068	5531.456139	25.059955
152.098138	5532.894998	25.064973
151.783628	5549.775779	25.069991
152.041854	5558.479418	25.075008
152.327192	5567.586025	25.080026
152.406593	5566.124742	25.085043
152.892385	5578.344011	25.090061
152.770218	5585.210086	25.095079
152.844983	5577.167829	25.100096
153.222242	5593.305781	25.105114
153.234124	5606.063348	25.110131
153.455062	5604.728252	25.115149
153.420668	5619.207163	25.120167
153.609874	5636.350033	25.125184
153.909216	5632.448882	25.130202
153.982276	5660.165974	25.135219
154.323718	5663.966893	25.140237
154.090435	5669.628763	25.145255
154.808671	5686.332092	25.150272
154.900803	5691.115930	25.155290
155.002448	5697.438754	25.160307
155.350880	5698.189203	25.165325
155.220652	5710.675532	25.170343
155.254509	5723.398171	25.175360
155.604233	5713.639720	25.180378
155.753407	5732.016912	25.185395
155.599849	5742.107815	25.190413
155.908043	5744.073593	25.195431
156.226820	5754.863899	25.200448
156.303469	5772.621151	25.205466
156.091010	5773.904573	25.210483
156.797312	5787.926651	25.215501
156.568440	5806.612526	25.220519
156.945404	5808.573851	25.225536
157.201060	5810.219567	25.230554
157.382771	5821.795316	25.235571
157.588346	5835.772764	25.240589
157.699795	5838.129243	25.245607
157.656193	5853.241128	25.250624
158.183386	5850.169182	25.255642
158.302574	5852.470785	25.260659
158.462285	5851.707163	25.265677
158.371662	5858.031753	25.270695
158.418442	5874.044950	25.275712
159.027334	5877.459929	25.280730
158.879247	5894.169745	25.285747
158.806661	5902.123560	25.290765
159.135710	5905.449803	25.295783
159.000676	5915.332710	25.300800
159.699024	5921.719966	25.305818
159.761755	5933.039788	25.310835
160.013381	5936.968478	25.315853
159.999757	5955.964870	25.320871
160.241968	5958.373484	25.325888
160.601475	5959.273734	25.330906
160.518942	5958.626977	25.335923
160.830674	5975.170127	25.340941
161.315663	5981.969642	25.345959
161.185102	5975.619832	25.350976
161.394729	5969.933314	25.355994
161.412033	5987.485412	25.361011
161.749669	5992.069873	25.366029
162.317026	5995.882820	25.371047
162.369308	6000.893956	25.376064
162.704455	5996.321043	25.381082
162.571811	5997.563565	25.386099
162.218424	5993.834047	25.391117
162.522217	5999.481326	25.396135
162.304778	6019.279963	25.401152
162.995058	6015.049162	25.406170
162.984471	6026.898237	25.411187
163.209069	6021.266180	25.416205
163.526435	6044.330388	25.421223
163.187991	6054.415702	25.426240
163.540050	6052.226645	25.431258
163.349056	6071.834947	25.436275
163.614899	6081.402598	25.441293
163.982251	6085.048021	25.446311
163.340136	6095.124110	25.451328
163.612143	6106.288138	25.456346
163.795484	6123.186154	25.461363
164.065429	6142.334034	25.466381
164.468746	6156.959458	25.471399
164.530361	6176.297851	25.476416
164.541580	6180.955594	25.481434
164.894123	6197.940816	25.486451
164.934991	6213.999432	25.491469
165.587147	6218.550460	25.496487
165.142748	6240.869293	25.501504
165.731176	6250.550650	25.506522
165.550043	6271.426655	25.511539
165.860899	6282.025949	25.516557
165.847169	6294.806949	25.521575
166.100171	6308.641585	25.526592
166.636215	6317.475686	25.531610
167.137263	6338.892043	25.536627
167.151626	6344.973062	25.541645
167.252022	6337.526252	25.546663
167.336416	6354.370533	25.551680
167.925128	6353.640701	25.556698
168.066047	6363.054445	25.561715
168.033546	6373.527645	25.566733
168.336540	6384.649107	25.571751
168.198128	6393.134324	25.576768
168.446250	6393.168135	25.581786
168.578369	6418.683125	25.586803
168.613026	6416.742631	25.591821
169.020431	6430.281682	25.596839
169.006767	6445.929184	25.601856
169.665346	6445.159992	25.606874
169.459304	6452.434135	25.611891
170.122476	6462.621617	25.616909
170.417257	6458.465303	25.621927
170.144955	6466.286496	25.626944
170.423187	6460.093454	25.631962
170.718997	6478.306366	25.636979
170.644092	6492.817567	25.641997
171.026286	6488.660180	25.647015
170.950854	6492.656013	25.652032
171.306599	6508.832869	25.657050
171.399584	6512.783380	25.662067
171.541347	6523.513482	25.667085
171.737211	6532.306276	25.672103
171.745485	6544.354769	25.677120
172.017930	6548.027781	25.682138
172.218941	6561.738166	25.687156
172.218310	6560.103087	25.692173
172.884610	6573.693235	25.697191
172.981083	6578.596586	25.702208
173.020336	6576.892120	25.707226
172.769385	6587.851096	25.712244
173.339486	6595.025801	25.717261
173.154306	6599.774400	25.722279
173.350854	6612.772070	25.727296
173.293751	6622.744168	25.732314
173.553812	6636.618985	25.737332
173.469739	6653.183716	25.742349
174.075152	6660.867485	25.747367
174.104122	6671.801599	25.752384
174.474886	6673.164185	25.757402
174.937203	6679.099372	25.762420
174.857905	6691.253229	25.767437
175.041938	6703.148016	25.772455
174.916657	6709.358367	25.777472
175.378169	6709.835438	25.782490
175.451811	6715.411662	25.787508
175.424950	6731.958030	25.792525
175.615793	6738.159905	25.797543
176.339136	6751.453972	25.802560
176.452208	6759.584270	25.807578
176.515583	6771.340159	25.812596
176.256810	6767.725091	25.817613
176.828463	6777.172589	25.822631
176.764323	6786.647088	25.827648
176.805079	6792.866180	25.832666
177.016893	6816.260429	25.837684
177.112803	6822.079435	25.842701
177.258865	6845.430354	25.847719
177.761834	6862.632552	25.852736
177.634799	6870.847869	25.857754
178.097069	6882.891755	25.862772
178.124656	6891.666888	25.867789
178.615433	6893.619973	25.872807
178.664923	6914.507931	25.877824
179.032782	6915.912030	25.882842
179.288842	6930.949444	25.887860
179.431966	6936.827385	25.892877
179.597904	6930.714917	25.897895
179.481313	6942.249713	25.902912
179.882189	6954.754704	25.907930
180.066086	6957.289394	25.912948
180.071208	6981.641213	25.917965
180.274598	6974.114873	25.922983
180.252427	6989.849407	25.928000
180.515794	6998.846521	25.933018
180.957469	7005.388023	25.938036
181.035036	7028.614157	25.943053
181.038569	7046.718731	25.948071
181.329906	7044.343342	25.953088
181.771757	7054.606868	25.958106
182.134291	7063.029699	25.963124
182.216316	7065.772937	25.968141
182.412966	7071.301586	25.973159
182.462744	7083.473364	25.978176
182.584675	7097.247049	25.983194
182.948165	7097.550072	25.988212
182.944574	7108.047573	25.993229
183.146011	7110.860505	25.998247
183.845641	7113.358618	26.003264
183.805338	7115.006623	26.008282
184.054220	7125.773963	26.013300
184.282540	7136.743419	26.018317
184.423740	7126.764333	26.023335
184.321348	7138.606408	26.028352
184.464486	7132.036530	26.033370
184.952234	7140.294561	26.038388
184.937919	7147.387407	26.043405
185.389007	7155.048209	26.048423
184.933763	7156.546549	26.053440
185.728389	7162.328812	26.058458
185.726400	7170.051128	26.063476
186.242803	7174.140652	26.068493
186.080103	7166.472697	26.073511
186.475297	7181.797901	26.078528
186.342128	7190.699383	26.083546
186.522673	7186.664984	26.088564
186.412401	7202.053607	26.093581
186.665499	7211.036650	26.098599
186.590026	7222.388388	26.103616
186.931982	7220.349157	26.108634
187.205401	7244.400421	26.113652
187.082597	7258.926043	26.118669
187.461978	7263.671606	26.123687
187.467498	7278.660158	26.128704
187.639182	7297.278479	26.133722
188.145625	7308.229722	26.138740
188.230500	7324.560228	26.143757
188.306481	7334.252987	26.148775
188.441328	7350.484134	26.153792
188.708806	7364.996053	26.158810
189.027852	7371.503228	26.163828
188.657422	7395.333541	26.168845
188.973404	7406.254697	26.173863
189.340402	7413.278438	26.178880
189.270471	7435.183308	26.183898
189.948667	7442.458223	26.188916
189.907199	7465.501507	26.193933
190.267662	7474.884585	26.198951
190.336828	7484.281731	26.203968
190.754629	7502.407092	26.208986
190.913277	7516.251107	26.214004
190.867501	7528.412892	26.219021
191.663181	7535.991456	26.224039
191.685527	7542.611471	26.229056
191.661156	7551.603421	26.234074
191.847302	7573.016882	26.239092
191.807922	7579.242480	26.244109
192.150316	7598.844613	26.249127
192.294419	7605.998058	26.254144
192.301302	7626.189477	26.259162
192.677075	7630.673666	26.264180
193.059052	7649.319381	26.269197
193.215968	7655.703676	26.274215
193.350115	7669.270666	26.279232
193.026487	7678.331659	26.284250
193.962493	7706.535428	26.289268
193.478444	7722.106164	26.294285
194.248971	7727.946054	26.299303
194.520979	7737.914550	26.304320
195.112989	7756.467487	26.309338
195.291636	7760.745810	26.314356
195.135477	7754.336254	26.319373
195.641836	7769.136245	26.324391
196.153949	7775.433366	26.329408
196.149668	7795.882442	26.334426
196.358223	7790.700665	26.339444
196.587397	7793.348346	26.344461
196.422301	7798.596079	26.349479
196.525314	7809.298273	26.354496
196.845955	7817.999523	26.359514
197.179681	7826.244108	26.364532
197.561490	7841.174167	26.369549
197.481382	7840.359638	26.374567
197.624894	7848.274125	26.379584
197.709020	7860.542061	26.384602
197.765559	7868.842718	26.389620
198.041241	7888.613464	26.394637
198.499483	7894.243449	26.399655
198.431615	7917.802880	26.404672
198.435388	7924.716394	26.409690
198.807969	7916.108698	26.414708
198.931948	7939.950655	26.419725
199.323113	7953.960626	26.424743
199.318439	7953.768850	26.429760
199.616862	7978.202319	26.434778
199.687722	7990.646061	26.439796
199.810088	7996.287653	26.444813
199.913748	8008.915694	26.449831
200.075980	8013.035635	26.454848
200.248821	8040.933265	26.459866
200.676975	8046.754280	26.464884
200.521831	8065.301448	26.469901
200.604518	8070.377841	26.474919
200.667818	8072.660067	26.479936
201.100371	8111.036632	26.484954
201.531144	8118.265337	26.489972
201.868451	8138.648650	26.494989
202.034957	8146.865904	26.500007
202.671136	8154.482343	26.505024
202.378509	8168.362813	26.510042
202.862262	8184.274834	26.515060
202.983168	8185.982922	26.520077
202.992833	8215.611231	26.525095
203.286341	8224.601066	26.530112
203.298284	8246.029969	26.535130
203.602849	8253.051184	26.540148
203.921181	8265.964643	26.545165
204.146251	8272.982533	26.550183
204.227871	8286.624505	26.555200
204.311860	8313.099959	26.560218
204.845400	8319.444425	26.565236
204.851260	8339.324223	26.570253
204.996880	8355.892382	26.575271
205.402361	8365.723493	26.580288
205.591710	8376.901851	26.585306
205.742388	8389.781675	26.590324
205.953862	8400.211488	26.595341
205.864981	8411.793372	26.600359
206.452797	8422.735690	26.605376
206.580831	8441.478818	26.610394
206.744244	8451.818317	26.615412
207.033136	8479.480581	26.620429
206.996141	8487.789853	26.625447
207.716527	8505.521507	26.630464
207.981162	8511.204112	26.635482
208.352586	8511.376476	26.640500
208.615488	8531.667691	26.645517
208.745376	8527.205245	26.650535
209.166116	8525.605011	26.655552
208.802287	8546.872126	26.660570
209.361715	8555.037479	26.665588
209.542506	8555.268122	26.670605
209.621233	8576.415424	26.675623
210.166153	8581.457431	26.680640
210.522757	8570.136743	26.685658
210.637654	8571.444843	26.690676
210.930608	8589.066735	26.695693
211.127693	8591.214407	26.700711
211.606774	8601.299320	26.705728
211.245546	8599.998385	26.710746
211.587999	8604.124954	26.715764
211.779919	8608.032002	26.720781
211.902640	8618.551616	26.725799
212.154035	8622.651411	26.730816
211.800584	8630.009486	26.735834
212.050517	8649.033663	26.740852
212.328490	8655.052045	26.745869
212.719667	8678.092204	26.750887
212.777489	8672.693847	26.755904
212.555984	8697.730658	26.760922
212.749114	8714.219078	26.765940
212.828229	8730.523312	26.770957
212.979086	8749.913565	26.775975
213.126678	8763.406635	26.780992
213.323854	8790.449127	26.786010
213.832565	8800.857860	26.791028
213.806907	8829.346603	26.796045
214.174589	8846.669724	26.801063
214.762726	8859.591847	26.806080
214.296413	8874.516687	26.811098
214.847765	8892.650907	26.816116
215.073478	8913.624019	26.821133
215.251017	8936.012841	26.826151
215.104782	8951.935812	26.831168
215.874025	8968.662562	26.836186
216.313654	8986.744916	26.841204
216.125577	8993.347897	26.846221
215.955583	9007.285555	26.851239
216.743070	9035.104178	26.856256
216.916634	9045.947583	26.861274
217.721236	9057.970838	26.866292
217.768493	9074.135129	26.871309
217.966094	9081.050282	26.876327
218.399904	9090.637388	26.881344
218.512377	9095.302105	26.886362
218.631817	9115.392265	26.891380
218.760102	9120.363927	26.896397
218.871119	9147.227840	26.901415
219.669759	9153.193235	26.906432
219.458362	9158.641198	26.911450
219.545693	9169.662364	26.916468
220.082899	9185.475312	26.921485
219.931583	9202.551710	26.926503
220.446020	9220.616259	26.931520
220.669761	9229.475434	26.936538
220.798325	9240.534385	26.941556
221.159853	9258.834466	26.946573
221.348650	9263.648292	26.951591
221.570833	9266.410946	26.956608
221.521870	9297.148911	26.961626
222.017373	9301.658956	26.966644
222.433791	9317.118374	26.971661
222.123052	9320.876990	26.976679
222.143597	9342.034278	26.981696
222.362852	9362.011190	26.986714
222.745380	9373.248292	26.991732
223.339364	9395.316683	26.996749
223.113758	9415.031822	27.001767
223.525060	9426.798040	27.006784
224.248509	9438.316452	27.011802
224.155511	9436.900817	27.016820
224.382440	9455.465293	27.021837
224.747204	9464.305645	27.026855
224.908296	9473.319989	27.031872
225.232862	9491.626089	27.036890
225.638117	9500.709547	27.041908
225.992805	9512.348921	27.046925
225.994431	9522.913276	27.051943
226.162414	9518.147834	27.056960
226.634189	9542.278359	27.061978
226.401361	9547.069903	27.066996
226.549397	9557.983911	27.072013
226.680458	9576.058347	27.077031
227.093017	9593.899259	27.082048
227.124326	9611.531536	27.087066
227.451326	9624.763479	27.092084
227.746480	9631.395178	27.097101
227.315051	9658.354278	27.102119
227.689433	9666.830121	27.107136
227.814306	9693.424273	27.112154
227.930283	9714.023961	27.117172
228.654441	9732.943383	27.122189
228.684425	9742.726700	27.127207
228.699581	9761.593035	27.132224
228.841206	9778.901920	27.137242
229.255650	9796.625907	27.142260
229.495709	9807.585636	27.147277
229.817717	9848.597447	27.152295
230.027183	9848.523662	27.157312
230.525409	9872.492601	27.162330
230.537985	9883.232260	27.167348
230.782680	9905.283354	27.172365
230.878647	9910.399217	27.177383
231.522498	9924.724727	27.182400
231.809126	9947.135564	27.187418
231.808560	9949.655361	27.192436
232.663685	9962.343826	27.197453
232.820216	9977.920285	27.202471
233.387573	9983.012841	27.207488
233.553304	9983.621599	27.212506
233.478675	10013.395429	27.217524
233.375559	10010.134229	27.222541
233.855884	10024.488591	27.227559
234.072667	10032.935613	27.232576
234.180316	10055.838764	27.237594
234.518655	10071.705723	27.242612
234.683401	10078.143304	27.247629
234.457022	10100.022143	27.252647
234.701005	10100.789150	27.257664
235.616437	10120.619926	27.262682
235.942459	10116.120062	27.267700
236.406132	10131.856927	27.272717
236.900989	10139.452124	27.277735
237.066948	10136.395033	27.282752
237.265936	10145.719512	27.287770
237.546925	10163.139536	27.292788
237.918440	10167.744997	27.297805
237.683292	10166.218961	27.302823
237.934045	10164.171602	27.307840
238.100896	10189.121157	27.312858
238.096233	10191.477440	27.317876
238.778856	10201.603962	27.322893
238.417214	10215.171543	27.327911
238.595155	10221.588162	27.332928
238.918104	10242.317041	27.337946
239.049654	10257.717671	27.342964
239.724554	10271.508127	27.347981
239.583508	10296.092427	27.352999
239.669520	10305.055785	27.358016
240.176211	10315.573042	27.363034
240.032234	10341.304032	27.368052
240.519866	10350.722327	27.373069
240.624154	10368.997489	27.378087
240.883517	10388.956589	27.383104
241.381202	10403.134860	27.388122
241.571004	10428.911565	27.393140
241.522514	10426.336388	27.398157
241.757120	10452.305030	27.403175
242.105380	10467.217200	27.408192
242.384272	10489.702524	27.413210
242.440448	10511.616518	27.418228
242.417741	10529.485465	27.423245
243.179270	10555.216986	27.428263
243.249172	10564.896595	27.433280
243.857606	10583.699238	27.438298
243.457637	10601.463161	27.443316
244.379623	10605.268893	27.448333
244.837752	10628.278876	27.453351
244.652523	10642.419063	27.458368
244.685643	10650.437292	27.463386
244.824121	10668.707391	27.468404
245.255825	10677.698870	27.473421
245.825504	10699.011644	27.478439
245.989400	10711.455260	27.483456
246.212100	10715.597905	27.488474
246.292782	10728.581882	27.493492
246.786467	10748.858305	27.498509
246.982123	10758.009946	27.503527
246.900003	10765.679999	27.508544
247.620040	10785.055828	27.513562
247.333356	10805.991349	27.518580
247.420429	10817.982906	27.523597
247.417463	10840.092846	27.528615
247.763875	10860.007236	27.533632
248.251941	10875.242008	27.538650
247.975178	10898.837928	27.543668
248.286741	10915.151862	27.548685
249.002209	10934.676969	27.553703
249.327398	10953.533829	27.558720
249.831035	10965.283398	27.563738
249.641292	10993.586427	27.568756
250.452858	11008.890620	27.573773
250.813523	11023.030833	27.578791
251.563095	11040.807705	27.583808
251.822339	11033.817250	27.588826
251.902993	11044.291143	27.593844
252.275517	11064.296388	27.598861
252.518609	11064.747814	27.603879
252.363563	11077.876318	27.608896
252.773049	11085.472647	27.613914
253.184277	11101.802707	27.618932
253.228800	11112.310717	27.623949
253.380069	11127.731076	27.628967
253.520312	11140.983879	27.633984
254.120838	11143.731753	27.639002
253.941765	11165.904398	27.644020
254.095389	11178.330987	27.649037
253.962052	11199.050307	27.654055
254.400180	11214.312124	27.659072
254.749195	11237.406260	27.664090
254.867983	11259.706026	27.669108
255.171404	11282.254769	27.674125
255.451445	11294.336392	27.679143
255.513892	11309.935013	27.684160
255.931412	11336.413028	27.689178
256.319259	11353.864786	27.694196
256.369899	11372.073545	27.699213
256.898926	11387.734920	27.704231
257.228375	11399.385742	27.709248
257.866267	11411.875562	27.714266
257.734983	11437.059784	27.719284
258.129745	11446.262671	27.724301
258.249264	11466.033260	27.729319
258.441515	11479.660235	27.734336
258.716009	11503.274760	27.739354
259.107068	11513.671869	27.744372
259.249661	11534.449379	27.749389
259.501485	11552.607851	27.754407
259.545568	11587.146345	27.759424
260.081800	11593.131540	27.764442
260.301021	11615.624404	27.769460
259.877107	11624.838790	27.774477
260.521183	11647.912470	27.779495
261.074215	11673.460308	27.784512
261.443580	11690.817385	27.789530
261.167281	11718.165639	27.794548
261.466127	11734.665426	27.799565
261.526021	11743.156745	27.804583
261.599954	11768.151374	27.809600
262.132538	11785.947157	27.814618
262.252993	11808.780971	27.819636
262.847876	11820.084172	27.824653
263.251416	11844.332564	27.829671
263.545511	11859.838513	27.834688
263.862059	11877.595598	27.839706
264.152306	11897.371472	27.844724
264.059984	11904.209936	27.849741
264.354068	11939.461461	27.854759
264.636967	11956.999690	27.859776
265.013642	11964.680461	27.864794
264.937352	11997.542839	27.869812
265.269772	12020.858423	27.874829
265.746900	12041.126207	27.879847
265.808018	12070.534672	27.884864
266.127069	12080.722331	27.889882
266.431394	12108.144398	27.894900
266.730455	12132.804253	27.899917
266.850264	12154.580723	27.904935
267.180175	12177.988470	27.909952
267.789701	12192.617934	27.914970
268.316264	12217.346469	27.919988
268.872271	12220.698307	27.925005
269.057771	12239.919385	27.930023
268.946844	12252.239708	27.935040
269.513956	12272.828374	27.940058
269.822370	12288.225067	27.945076
270.194235	12299.115082	27.950093
270.329737	12305.371698	27.955111
270.925925	12323.761173	27.960128
271.196266	12320.993689	27.965146
271.713772	12338.558678	27.970164
271.692087	12334.229599	27.975181
272.210987	12337.220963	27.980199
272.640866	12366.922643	27.985216
273.015446	12368.108230	27.990234
273.350360	12375.959919	27.995252
273.484512	12373.557966	28.000269
273.834180	12382.556802	28.005287
273.681008	12388.261834	28.010304
273.994553	12398.340003	28.015322
273.939895	12416.013642	28.020340
273.856226	12432.545542	28.025357
274.362847	12445.959762	28.030375
274.312248	12470.734833	28.035392
274.830759	12480.948305	28.040410
275.226291	12514.833448	28.045428
275.079336	12531.252191	28.050445
275.362605	12544.868837	28.055463
275.423160	12573.267655	28.060480
275.611694	12589.864419	28.065498
275.764620	12616.155158	28.070516
276.238461	12646.264073	28.075533
276.181385	12678.205679	28.080551
276.265822	12704.927269	28.085568
276.991484	12727.642125	28.090586
277.233593	12752.630658	28.095604
277.307645	12778.046606	28.100621
277.944534	12801.893357	28.105639
278.137018	12831.386639	28.110656
278.298346	12860.171156	28.115674
278.851726	12884.700573	28.120692
278.893055	12903.537537	28.125709
279.155866	12925.283019	28.130727
279.359586	12952.886285	28.135744
279.972318	12974.687537	28.140762
280.056157	12992.750550	28.145780
280.655898	13021.245578	28.150797
280.643984	13029.098186	28.155815
280.992735	13057.534689	28.160832
281.405754	13087.126456	28.165850
281.873139	13104.453690	28.170868
281.877556	13113.728016	28.175885
282.494118	13131.101381	28.180903
282.610716	13163.392395	28.185920
282.782646	13173.338421	28.190938
282.925594	13192.374496	28.195956
282.906007	13218.573091	28.200973
283.831778	13233.412780	28.205991
283.794828	13266.255405	28.211008
284.439391	13278.445415	28.216026
284.852907	13296.984459	28.221044
284.716886	13321.960344	28.226061
285.453282	13343.850021	28.231079
285.410155	13352.819270	28.236096
285.814074	13371.906225	28.241114
286.180456	13391.895956	28.246132
286.509366	13420.806657	28.251149
287.084600	13434.046615	28.256167
286.852122	13451.496432	28.261184
287.094965	13474.401508	28.266202
287.623199	13491.820621	28.271220
287.727862	13519.478125	28.276237
288.083551	13539.425474	28.281255
288.113058	13567.334830	28.286272
288.465495	13589.499686	28.291290
288.778327	13615.845712	28.296308
288.743035	13642.584220	28.301325
289.456448	13653.235189	28.306343
290.092258	13668.603826	28.311360
290.367970	13702.310905	28.316378
290.799045	13701.621314	28.321396
290.949962	13722.952584	28.326413
291.467237	13737.231364	28.331431
291.628081	13753.501887	28.336448
292.194840	13752.851044	28.341466
292.501711	13769.695581	28.346484
292.748250	13778.360692	28.351501
293.335422	13789.628391	28.356519
293.586341	13810.546176	28.361536
293.687926	13831.932668	28.366554
293.911249	13830.223975	28.371572
294.474512	13856.730065	28.376589
295.127443	13859.331184	28.381607
295.108615	13878.008001	28.386624
295.034080	13887.190855	28.391642
295.599035	13896.598822	28.396660
295.661589	13914.583936	28.401677
295.879716	13919.413314	28.406695
295.655497	13938.119206	28.411712
296.098478	13962.736792	28.416730
296.505613	13987.012634	28.421748
296.527014	14016.345068	28.426765
296.976651	14037.516205	28.431783
297.392522	14057.830488	28.436800
297.451599	14074.410932	28.441818
297.988229	14096.964400	28.446836
298.096441	14119.894501	28.451853
298.277883	14146.217631	28.456871
298.291915	14160.705046	28.461888
298.611402	14190.281602	28.466906
299.111311	14205.245615	28.471924
299.091761	14238.444061	28.476941
299.260874	14262.631214	28.481959
299.572070	14288.425750	28.486976
299.785517	14310.985883	28.491994
300.344043	14348.288008	28.497012
300.479606	14361.111131	28.502029
300.721140	14397.389230	28.507047
301.046416	14420.111990	28.512064
301.458966	14450.732363	28.517082
301.898237	14469.290626	28.522100
301.932303	14503.523337	28.527117
302.562780	14521.495855	28.532135
302.806358	14556.693833	28.537152
303.246172	14572.883457	28.542170
303.739899	14594.449400	28.547188
303.545360	14622.168005	28.552205
304.002223	14646.714820	28.557223
304.528252	14685.791300	28.562240
304.531851	14706.136114	28.567258
304.821091	14735.127664	28.572276
305.154731	14748.428495	28.577293
305.666321	14771.795192	28.582311
305.914030	14801.955582	28.587328
306.240251	14824.735524	28.592346
306.676855	14847.791919	28.597364
307.088659	14884.217974	28.602381
307.202380	14905.360581	28.607399
307.536209	14930.511313	28.612416
307.798790	14964.162672	28.617434
308.062950	14979.862201	28.622452
308.489198	15009.274863	28.627469
309.000923	15035.392724	28.632487
309.116252	15066.828106	28.637504
309.186977	15083.919245	28.642522
309.735935	15099.678484	28.647540
310.038296	15143.180965	28.652557
310.363904	15165.058134	28.657575
310.659998	15194.725184	28.662592
311.096445	15212.757174	28.667610
311.592914	15242.171828	28.672628
311.671081	15259.603056	28.677645
312.272297	15280.634971	28.682663
312.794350	15294.478324	28.687680
312.806043	15324.578600	28.692698
313.333182	15342.618615	28.697716
313.544106	15364.040226	28.702733
313.749030	15387.383073	28.707751
313.960898	15414.420126	28.712768
314.119867	15433.408552	28.717786
314.153114	15454.706496	28.722804
314.576653	15487.635565	28.727821
315.206932	15513.593381	28.732839
315.884995	15538.968926	28.737856
316.071574	15562.987592	28.742874
316.533357	15588.476041	28.747892
316.170513	15612.520825	28.752909
316.637258	15628.729235	28.757927
317.160411	15650.474946	28.762944
317.505779	15675.523780	28.767962
318.026660	15707.822093	28.772980
317.942175	15730.026294	28.777997
318.399175	15759.299480	28.783015
319.104678	15782.776007	28.788032
319.096818	15794.952975	28.793050
319.267032	15824.479639	28.798068
319.821170	15848.377918	28.803085
319.897099	15870.936163	28.808103
320.219802	15902.732074	28.813120
320.404935	15930.509954	28.818138
320.858368	15951.278339	28.823156
321.389780	15969.608851	28.828173
321.568612	15985.976368	28.833191
321.892988	16018.293351	28.838208
321.686283	16037.718669	28.843226
322.286539	16049.156216	28.848244
322.591108	16085.067572	28.853261
322.953273	16107.634951	28.858279
323.540800	16129.314269	28.863296
323.637049	16154.118489	28.868314
324.075043	16170.401348	28.873332
324.337477	16198.821310	28.878349
324.643567	16224.192860	28.883367
324.849977	16241.159543	28.888384
325.248703	16275.306707	28.893402
325.691595	16302.384623	28.898420
325.927232	16328.440105	28.903437
326.419318	16357.481295	28.908455
326.395660	16387.317139	28.913472
326.492461	16409.948550	28.918490
327.196490	16440.507493	28.923508
327.324547	16465.809335	28.928525
327.515229	16503.302778	28.933543
327.591152	16532.741066	28.938560
327.875289	16574.155535	28.943578
328.847993	16604.063054	28.948596
328.878823	16631.060687	28.953613
329.069094	16665.948709	28.958631
329.942626	16684.510583	28.963648
330.251173	16718.925342	28.968666
330.290494	16745.451179	28.973684
330.909728	16769.589934	28.978701
330.996200	16799.159635	28.983719
331.616111	16822.164422	28.988736
331.563972	16859.646055	28.993754
332.281397	16882.319780	28.998772
332.486776	16917.019533	29.003789
333.021242	16941.743487	29.008807
333.675508	16953.517401	29.013824
334.138795	16983.161020	29.018842
335.023538	16983.635275	29.023860
335.343488	17011.772627	29.028877
335.529592	17031.636472	29.033895
335.800853	17041.790054	29.038912
336.073962	17056.826571	29.043930
336.539549	17069.659821	29.048948
336.894433	17094.190998	29.053965
336.868296	17109.899838	29.058983
337.351211	17123.033637	29.064000
337.598037	17148.396734	29.069018
337.967716	17170.360883	29.074036
337.984953	17190.883070	29.079053
338.368497	17206.559401	29.084071
338.806574	17227.249445	29.089088
338.708041	17252.445672	29.094106
338.966445	17283.176833	29.099124
339.418906	17301.691551	29.104141
339.660771	17334.623808	29.109159
340.170518	17366.370723	29.114176
339.973004	17394.823431	29.119194
340.704219	17415.714134	29.124212
340.969662	17454.461180	29.129229
340.664963	17491.427670	29.134247
341.123206	17516.827624	29.139264
341.611745	17563.765172	29.144282
341.818245	17596.457036	29.149300
342.222092	17641.664435	29.154317
342.343676	17672.430280	29.159335
343.047635	17698.316329	29.164352
343.400891	17720.125738	29.169370
343.478440	17751.043907	29.174388
343.950450	17787.093293	29.179405
344.163773	17817.724967	29.184423
344.836230	17840.368957	29.189440
345.219925	17874.000108	29.194458
345.612675	17903.889934	29.199476
345.802971	17931.688834	29.204493
345.728625	17961.468708	29.209511
346.543780	17994.653430	29.214528
346.684809	18033.282134	29.219546
347.004748	18067.271071	29.224564
348.039976	18083.837889	29.229581
348.749279	18103.797769	29.234599
349.078925	18123.311735	29.239616
349.697551	18142.786771	29.244634
349.878492	18168.502673	29.249652
350.272678	18189.965049	29.254669
350.720247	18199.447228	29.259687
351.397376	18213.865409	29.264704
351.665569	18229.345840	29.269722
351.533081	18254.030639	29.274740
351.930372	18277.868051	29.279757
352.208693	18296.253058	29.284775
352.326773	18311.738115	29.289792
352.835209	18341.029270	29.294810
352.885645	18356.701853	29.299828
353.046443	18389.471705	29.304845
353.449073	18417.648688	29.309863
354.408054	18443.956977	29.314880
354.141454	18475.239772	29.319898
354.500277	18505.470676	29.324916
354.860423	18523.836762	29.329933
354.742161	18566.601015	29.334951
355.748651	18595.909304	29.339968
355.868606	18631.023520	29.344986
356.173854	18660.972441	29.350004
356.804003	18687.471561	29.355021
356.976397	18729.009219	29.360039
357.356777	18750.449106	29.365056
357.446548	18780.956340	29.370074
357.820869	18814.944382	29.375092
357.983885	18847.575664	29.380109
358.312803	18893.669569	29.385127
359.103109	18921.761284	29.390144
359.343375	18971.887404	29.395162
359.779906	19005.202659	29.400180
360.235830	19022.682348	29.405197
360.687755	19056.525980	29.410215
360.728839	19082.757790	29.415232
361.252410	19118.283500	29.420250
361.951406	19139.869762	29.425268
362.218042	19175.006205	29.430285
362.895894	19200.285510	29.435303
363.720973	19220.847563	29.440320
364.357222	19235.411902	29.445338
364.284303	19256.108336	29.450356
364.592450	19263.989164	29.455373
365.067800	19301.828813	29.460391
365.335767	19311.794563	29.465408
365.709626	19333.444605	29.470426
365.681397	19364.697801	29.475444
366.035033	19385.188560	29.480461
366.507291	19422.144409	29.485479
366.862970	19445.200018	29.490496
367.400136	19465.365167	29.495514
367.304824	19501.891993	29.500532
367.720440	19516.383697	29.505549
367.927422	19539.810202	29.510567
368.274897	19567.270911	29.515584
368.577374	19600.658725	29.520602
369.203323	19621.056532	29.525620
369.583824	19644.234849	29.530637
369.507189	19686.729670	29.535655
370.085502	19706.541129	29.540672
370.148146	19745.204452	29.545690
370.635242	19778.026610	29.550708
370.883900	19800.676089	29.555725
371.110179	19831.624801	29.560743
371.609324	19874.882787	29.565760
371.934351	19909.291133	29.570778
372.110854	19946.287979	29.575796
372.813609	19982.956055	29.580813
372.820154	20025.729215	29.585831
373.459238	20059.134584	29.590848
373.620085	20095.704526	29.595866
374.081712	20133.371021	29.600884
374.707426	20174.651192	29.605901
374.788360	20213.628484	29.610919
375.022559	20247.192367	29.615936
375.241093	20289.566437	29.620954
375.898456	20328.251480	29.625972
376.861841	20365.498638	29.630989
376.702513	20405.227912	29.636007
376.958334	20442.308042	29.641024
377.419008	20479.539386	29.646042
377.950573	20523.191777	29.651060
378.443139	20548.546078	29.656077
378.774040	20597.828133	29.661095
379.337727	20628.074456	29.666112
380.036043	20664.024204	29.671130
380.331154	20694.597026	29.676148
381.033531	20730.369344	29.681165
380.956302	20767.824495	29.686183
381.351672	20796.486242	29.691200
381.554193	20827.794076	29.696218
382.017695	20863.894702	29.701236
382.477278	20885.533031	29.706253
382.568716	20932.035395	29.711271
383.439877	20960.768180	29.716288
383.781654	20998.183410	29.721306
384.096570	21033.555719	29.726324
385.063141	21059.582017	29.731341
385.193358	21097.807752	29.736359
385.516811	21122.544792	29.741376
385.806447	21151.432130	29.746394
386.281610	21182.678866	29.751412
386.849861	21213.923707	29.756429
386.801996	21245.410433	29.761447
387.299385	21272.319282	29.766464
387.838824	21310.790941	29.771482
388.021367	21343.461223	29.776500
388.463948	21365.671418	29.781517
388.933146	21405.000958	29.786535
389.116534	21431.693827	29.791552
389.938743	21463.802851	29.796570
389.941385	21492.723005	29.801588
390.226927	21524.878278	29.806605
391.214501	21562.155509	29.811623
391.118459	21591.116539	29.816640
391.536029	21629.045544	29.821658
391.679584	21663.769722	29.826676
392.385832	21691.884897	29.831693
392.627076	21727.491144	29.836711
393.032543	21779.765870	29.841728
393.601196	21792.661915	29.846746
393.854372	21823.495804	29.851764
394.520460	21849.582852	29.856781
394.483201	21882.162076	29.861799
394.762444	21913.845059	29.866816
395.408781	21936.542122	29.871834
395.910494	21968.575793	29.876852
395.831823	22002.899376	29.881869
396.117745	22040.963530	29.886887
396.426172	22081.419075	29.891904
397.592603	22094.803018	29.896922
398.523275	22108.470335	29.901940
398.881876	22146.396930	29.906957
399.404544	22164.854709	29.911975
399.854559	22187.266868	29.916992
400.291066	22197.871166	29.922010
400.239416	22236.279240	29.927028
400.908860	22255.270176	29.932045
401.613531	22282.103701	29.937063
401.314127	22308.513196	29.942080
401.843844	22328.758279	29.947098
402.025836	22360.842664	29.952116
402.297977	22391.952501	29.957133
402.656999	22422.189399	29.962151
403.037855	22460.884023	29.967168
403.671637	22489.441373	29.972186
403.749629	22531.115579	29.977204
404.049933	22559.314530	29.982221
404.261966	22596.531939	29.987239
404.812899	22641.715178	29.992256
405.217370	22676.090626	29.997274
405.550949	22719.898942	30.002292
406.172967	22752.268902	30.007309
406.617769	22787.282770	30.012327
407.118253	22824.626039	30.017344
407.667567	22857.405661	30.022362
407.802708	22903.836294	30.027380
408.245333	22933.991365	30.032397
409.265224	22946.507848	30.037415
409.427664	22982.533113	30.042432
410.175793	23008.533008	30.047450
410.262199	23040.677696	30.052468
410.617324	23079.169020	30.057485
411.149866	23106.472964	30.062503
411.126266	23140.688776	30.067520
411.593001	23171.118475	30.072538
412.016012	23219.065592	30.077556
412.188687	23253.073915	30.082573
412.862156	23285.550430	30.087591
412.868093	23330.839556	30.092608
413.513669	23367.838836	30.097626
413.777025	23409.902915	30.102644
414.309569	23457.814491	30.107661
414.393533	23489.701194	30.112679
414.642317	23532.595641	30.117696
415.280507	23577.299705	30.122714
415.427866	23624.621125	30.127732
416.372800	23666.142950	30.132749
416.559300	23696.964910	30.137767
417.256956	23727.649978	30.142784
418.065939	23757.925854	30.147802
418.428794	23794.502575	30.152820
419.325924	23830.622833	30.157837
419.823013	23861.952506	30.162855
420.110744	23887.678096	30.167872
420.793393	23905.069730	30.172890
421.087998	23950.302404	30.177908
421.464763	23974.516453	30.182925
421.838078	23997.479819	30.187943
422.063571	24022.621302	30.192960
422.519949	24041.211278	30.197978
422.509803	24072.330035	30.202996
422.555141	24099.528387	30.208013
423.111165	24138.502163	30.213031
423.873582	24158.775856	30.218048
424.519262	24182.985953	30.223066
424.855996	24222.487164	30.228084
424.911182	24249.513549	30.233101
425.580862	24287.300699	30.238119
425.938364	24316.592776	30.243136
426.633504	24344.226841	30.248154
426.863623	24388.017103	30.253172
427.271069	24416.536834	30.258189
427.629584	24441.234595	30.263207
427.833406	24477.982825	30.268224
428.643366	24510.686420	30.273242
428.934181	24544.646834	30.278260
429.462758	24574.835158	30.283277
430.082398	24612.978341	30.288295
430.051197	24648.878944	30.293312
430.633384	24674.401432	30.298330
431.014478	24718.958727	30.303348
431.200521	24759.306156	30.308365
431.415968	24798.126011	30.313383
431.465334	24849.883146	30.318400
432.739853	24876.858421	30.323418
432.504550	24929.652547	30.328436
433.353132	24973.328254	30.333453
434.014989	25001.720491	30.338471
433.848001	25058.188681	30.343488
434.948209	25083.478875	30.348506
435.124582	25132.019024	30.353524
435.534432	25168.211700	30.358541
436.267667	25206.186541	30.363559
436.197017	25251.902785	30.368576
436.776662	25295.848831	30.373594
437.065359	25334.715125	30.378612
437.216912	25386.558750	30.383629
437.886873	25435.243513	30.388647
438.153940	25484.332776	30.393664
438.307746	25532.959583	30.398682
438.598821	25584.238347	30.403700
439.043336	25639.721267	30.408717
439.664515	25682.574616	30.413735
440.129394	25735.096856	30.418752
441.008328	25784.217410	30.423770
441.101570	25840.697585	30.428788
441.262967	25894.316899	30.433805
441.999559	25949.224036	30.438823
442.176875	26003.188749	30.443840
442.561868	26061.450347	30.448858
443.163921	26108.251338	30.453876
444.004520	26160.267104	30.458893
444.174602	26206.390207	30.463911
444.625695	26268.484697	30.468928
444.999621	26307.699761	30.473946
445.580163	26364.926694	30.478964
445.807447	26415.509693	30.483981
446.771911	26454.537741	30.488999
446.687855	26514.618491	30.494016
447.222910	26564.995650	30.499034
447.802617	26613.608903	30.504052
448.611443	26665.277008	30.509069
449.533576	26707.895781	30.514087
449.689314	26750.963341	30.519104
450.363614	26798.784823	30.524122
450.904775	26838.688917	30.529140
451.148381	26879.385498	30.534157
451.881773	26902.580192	30.539175
452.091634	26940.823560	30.544192
452.670681	26968.902876	30.549210
453.202813	27017.436063	30.554228
453.513812	27057.667376	30.559245
454.314299	27082.292822	30.564263
454.500372	27132.928304	30.569280
454.780525	27168.771966	30.574298
455.468954	27205.107942	30.579316
455.582529	27249.263959	30.584333
455.775747	27285.614440	30.589351
456.049601	27335.775282	30.594368
456.794218	27375.180845	30.599386
456.873615	27427.616152	30.604404
457.187131	27472.695735	30.609421
458.354138	27519.575827	30.614439
458.186722	27575.577042	30.619456
458.838346	27626.330447	30.624474
459.408530	27679.043481	30.629492
459.526632	27724.021495	30.634509
460.081859	27782.191832	30.639527
460.262291	27827.387853	30.644544
460.868206	27873.876274	30.649562
461.605538	27931.753047	30.654580
462.164346	27975.050811	30.659597
462.957676	28026.080088	30.664615
463.141718	28067.066480	30.669632
463.649914	28117.616025	30.674650
464.613603	28158.809164	30.679668
464.788637	28195.928924	30.684685
465.340711	28243.273601	30.689703
466.067523	28296.475679	30.694720
466.412367	28339.870937	30.699738
467.230747	28385.037798	30.704756
467.429266	28425.833015	30.709773
467.909952	28463.619641	30.714791
468.195134	28501.892060	30.719808
468.770144	28545.011509	30.724826
469.131988	28590.035419	30.729844
469.580941	28640.658744	30.734861
470.235570	28691.490175	30.739879
470.327514	28740.734816	30.744896
471.217071	28786.491903	30.749914
471.455346	28825.891081	30.754932
471.869764	28884.655492	30.759949
472.065093	28921.969337	30.764967
472.641173	28975.847849	30.769984
472.793963	29011.980172	30.775002
473.673771	29062.669795	30.780020
473.695355	29125.605094	30.785037
474.226817	29167.449499	30.790055
475.123352	29208.301290	30.795072
476.242127	29256.166368	30.800090
476.757759	29290.200636	30.805108
477.675599	29331.384353	30.810125
478.161414	29365.404453	30.815143
478.336988	29406.622405	30.820160
478.385259	29445.369846	30.825178
479.094946	29480.138894	30.830196
479.636242	29523.802978	30.835213
480.006315	29557.563392	30.840231
480.489772	29608.329083	30.845248
481.129380	29641.213019	30.850266
481.229274	29689.162836	30.855284
481.635077	29737.305058	30.860301
482.076441	29767.976207	30.865319
482.624239	29817.967466	30.870336
482.531565	29851.914623	30.875354
483.080218	29900.629051	30.880372
483.492635	29959.156633	30.885389
483.766046	29989.690064	30.890407
484.589194	30039.638733	30.895424
484.664888	30093.073871	30.900442
485.303051	30138.746916	30.905460
485.988808	30187.522725	30.910477
486.772661	30235.391968	30.915495
486.862117	30284.482650	30.920512
487.071880	30327.726257	30.925530
487.860546	30370.272425	30.930548
488.085436	30431.763860	30.935565
488.565204	30473.214439	30.940583
489.335506	30533.185777	30.945600
489.470360	30578.609908	30.950618
490.422168	30627.522086	30.955636
490.590158	30686.937092	30.960653
491.184247	30732.814319	30.965671
491.986242	30775.346590	30.970688
492.257731	30834.644663	30.975706
493.270141	30880.842314	30.980724
493.593000	30928.823295	30.985741
494.021976	30978.317597	30.990759
494.886500	31018.571113	30.995776
495.254612	31072.196874	31.000794
495.701236	31115.588352	31.005812
496.394645	31166.735891	31.010829
496.943123	31211.161013	31.015847
497.118644	31253.381477	31.020864
497.738557	31306.026469	31.025882
498.097458	31354.476916	31.030900
498.459381	31403.325272	31.035917
498.783867	31448.070462	31.040935
499.788386	31499.391354	31.045952
500.070070	31555.920949	31.050970
500.589598	31602.469243	31.055988
501.024559	31659.771661	31.061005
501.620617	31699.202456	31.066023
502.204589	31754.654785	31.071040
502.457086	31807.756870	31.076058
503.281877	31849.864206	31.081076
503.495658	31913.441661	31.086093
504.029692	31952.888972	31.091111
504.156853	32013.723945	31.096128
504.774529	32061.876306	31.101146
505.284740	32116.784820	31.106164
505.694149	32188.298143	31.111181
506.281856	32229.868080	31.116199
507.442824	32282.146307	31.121216
507.972263	32338.101844	31.126234
508.085281	32381.301649	31.131252
509.066735	32439.361444	31.136269
509.474778	32488.729848	31.141287
509.852607	32531.995964	31.146304
510.186625	32583.045215	31.151322
510.618643	32629.110057	31.156340
510.984558	32685.477784	31.161357
511.788076	32732.432988	31.166375
512.592447	32779.407131	31.171392
512.802885	32828.661876	31.176410
513.562251	32880.233194	31.181428
513.727332	32939.933245	31.186445
514.302604	32981.955500	31.191463
514.766820	33034.471181	31.196480
515.122274	33085.164251	31.201498
516.007725	33132.695490	31.206516
516.295654	33185.371926	31.211533
516.997685	33221.577275	31.216551
517.947075	33260.582660	31.221568
518.150480	33310.181040	31.226586
518.876910	33347.824276	31.231604
519.172804	33393.166081	31.236621
519.213902	33444.143179	31.241639
519.823618	33485.136825	31.246656
519.927052	33537.647046	31.251674
520.811546	33582.416569	31.256692
521.010364	33634.754032	31.261709
521.856086	33696.979754	31.266727
522.503386	33749.108165	31.271744
522.794550	33798.339892	31.276762
523.411686	33852.850532	31.281780
523.367893	33915.639824	31.286797
523.989938	33974.499892	31.291815
524.576155	34041.490198	31.296832
524.602402	34100.279546	31.301850
525.472903	34156.338250	31.306868
525.571764	34227.445602	31.311885
525.784634	34292.901886	31.316903
526.762640	34357.618916	31.321920
527.150701	34431.577426	31.326938
527.549260	34487.976478	31.331956
528.320615	34567.635388	31.336973
529.080610	34642.118068	31.341991
529.651099	34704.965236	31.347008
530.186586	34770.423049	31.352026
530.681193	34839.510418	31.357044
531.084189	34899.931159	31.362061
531.690504	34963.690289	31.367079
532.449603	35024.966098	31.372096
533.029987	35087.363929	31.377114
533.996680	35153.748077	31.382132
534.401795	35221.965505	31.387149
535.004158	35274.332338	31.392167
535.576063	35332.666589	31.397184
535.816586	35394.359799	31.402202
536.740328	35453.088205	31.407220
536.793835	35513.603366	31.412237
537.161671	35584.268465	31.417255
537.927690	35654.504699	31.422272
538.232678	35727.228774	31.427290
539.210380	35790.110221	31.432308
539.672613	35853.161109	31.437325
540.542438	35909.426895	31.442343
541.624343	35970.427241	31.447360
542.031619	36016.756268	31.452378
542.976056	36059.485599	31.457396
543.517248	36101.588947	31.462413
544.192034	36161.578668	31.467431
544.788579	36200.745916	31.472448
545.501356	36251.738377	31.477466
546.081600	36292.172985	31.482484
546.527375	36335.796665	31.487501
546.843926	36391.865833	31.492519
547.175588	36439.611380	31.497536
547.559792	36483.592783	31.502554
548.092855	36531.680064	31.507572
549.058930	36585.719412	31.512589
549.049358	36634.157489	31.517607
549.765622	36691.088042	31.522624
550.318147	36749.637874	31.527642
550.549369	36798.633004	31.532660
551.060567	36859.554545	31.537677
551.498358	36909.295350	31.542695
551.645399	36963.938185	31.547712
552.289109	37037.195418	31.552730
552.989702	37070.966727	31.557748
553.414151	37140.104154	31.562765
553.642905	37196.619173	31.567783
553.971625	37254.566764	31.572800
554.862928	37313.950367	31.577818
555.627312	37374.296218	31.582836
556.343125	37430.463658	31.587853
556.608059	37498.779866	31.592871
557.209506	37544.537961	31.597888
557.656010	37615.096266	31.602906
558.082721	37670.715194	31.607924
558.498114	37734.803383	31.612941
559.199119	37809.015467	31.617959
559.762631	37870.981409	31.622976
560.251709	37934.976445	31.627994
560.663556	38009.601281	31.633012
561.584879	38069.551403	31.638029
561.589589	38141.382132	31.643047
562.332951	38215.917817	31.648064
563.246182	38286.487430	31.653082
563.743137	38350.634236	31.658100
564.417984	38412.799307	31.663117
564.534505	38497.590216	31.668135
565.298230	38558.477014	31.673152
565.601858	38622.427245	31.678170
566.200030	38694.116271	31.683188
567.276995	38767.874362	31.688205
567.750080	38836.845187	31.693223
568.404986	38900.279573	31.698240
568.861811	38977.303814	31.703258
569.339955	39038.312577	31.708276
569.763896	39116.702125	31.713293
570.401827	39181.468040	31.718311
571.153452	39265.315058	31.723328
571.611026	39336.990285	31.728346
572.049655	39398.897949	31.733364
572.976413	39472.138087	31.738381
573.470053	39545.117449	31.743399
574.321318	39618.211799	31.748416
574.966570	39687.689594	31.753434
575.601289	39742.598253	31.758452
576.304312	39813.768618	31.763469
576.704392	39885.808815	31.768487
577.323813	39948.998850	31.773504
577.616115	40029.202074	31.778522
577.894137	40095.456370	31.783540
578.392090	40159.836039	31.788557
579.395647	40240.997460	31.793575
580.043717	40307.453744	31.798592
580.596034	40380.774554	31.803610
581.161562	40449.147842	31.808628
582.335096	40515.876631	31.813645
582.593556	40578.758204	31.818663
583.524554	40641.907772	31.823680
584.155354	40719.315690	31.828698
584.294931	40776.492775	31.833716
585.252314	40839.278284	31.838733
585.602348	40910.969198	31.843751
586.141949	40977.121952	31.848768
586.593848	41043.908451	31.853786
587.355951	41103.069683	31.858804
588.165459	41169.629794	31.863821
588.384846	41249.697116	31.868839
588.674564	41304.189383	31.873856
589.489240	41372.880715	31.878874
590.361059	41436.364401	31.883892
590.967122	41499.738098	31.888909
591.251255	41562.833511	31.893927
591.882878	41624.046826	31.898944
592.723868	41689.952133	31.903962
593.220528	41745.406073	31.908980
594.052104	41793.648014	31.913997
594.716146	41859.183077	31.919015
595.545321	41909.664638	31.924032
596.086863	41964.264572	31.929050
596.328536	42010.948588	31.934068
597.439555	42068.912974	31.939085
597.592003	42140.740041	31.944103
597.997927	42195.178363	31.949120
598.469450	42261.427866	31.954138
599.037343	42333.342293	31.959156
599.715782	42388.155859	31.964173
599.738308	42454.431984	31.969191
600.489846	42523.668094	31.974208
601.065141	42595.822566	31.979226
602.111628	42659.655601	31.984244
602.847013	42720.849385	31.989261
603.316252	42798.561895	31.994279
603.841098	42861.262789	31.999296
604.700262	42922.279617	32.004314
605.734967	42970.637798	32.009332
607.311314	43018.829030	32.014349
607.521409	43081.459663	32.019367
608.255021	43132.926741	32.024384
608.801112	43179.793255	32.029402
609.318038	43239.896800	32.034420
610.014478	43294.001368	32.039437
610.141810	43352.951788	32.044455
610.746711	43407.614941	32.049472
611.563122	43469.595088	32.054490
612.174980	43533.973108	32.059508
612.933535	43584.981907	32.064525
613.211660	43651.145671	32.069543
613.552465	43709.197032	32.074560
614.147248	43765.222600	32.079578
614.749432	43842.095643	32.084596
615.462425	43891.910456	32.089613
615.602888	43970.133985	32.094631
616.324295	44040.492824	32.099648
616.731438	44107.181725	32.104666
617.309291	44185.919452	32.109684
617.741235	44244.242579	32.114701
618.276301	44330.824826	32.119719
619.016665	44408.816777	32.124736
619.310319	44477.871340	32.129754
619.549629	44573.154231	32.134772
620.136245	44648.988766	32.139789
620.343655	44738.065593	32.144807
621.252334	44831.631713	32.149824
621.876674	44922.225395	32.154842
622.329684	45010.164168	32.159860
622.874168	45096.406310	32.164877
623.563761	45203.393582	32.169895
624.383206	45290.776330	32.174912
625.129116	45366.746489	32.179930
625.574176	45465.878679	32.184948
626.388722	45539.453827	32.189965
626.839236	45639.711934	32.194983
627.550516	45726.550310	32.200000
628.529312	45812.246409	32.205018
628.962372	45910.053983	32.210036
630.155501	45980.294427	32.215053
630.602244	46075.228572	32.220071
630.918340	46157.854106	32.225088
632.212178	46222.993393	32.230106
632.482998	46292.664407	32.235124
633.336755	46361.327056	32.240141
634.061686	46438.955231	32.245159
634.853423	46503.244020	32.250176
635.805017	46572.549910	32.255194
635.985518	46645.044970	32.260212
637.031968	46712.786519	32.265229
637.332611	46778.234781	32.270247
638.021731	46853.636831	32.275264
639.036530	46913.400222	32.280282
639.248281	46986.543085	32.285300
639.989086	47065.543725	32.290317
640.540406	47139.943448	32.295335
641.085342	47203.058222	32.300352
641.618746	47281.510072	32.305370
642.027351	47361.284971	32.310388
643.060763	47429.827830	32.315405
643.497792	47507.314960	32.320423
644.246060	47586.031553	32.325440
645.098609	47663.662914	32.330458
645.633885	47754.288227	32.335476
645.783244	47822.078683	32.340493
646.623216	47903.401187	32.345511
647.470334	47985.045517	32.350528
648.479485	48057.067345	32.355546
648.930567	48140.412837	32.360564
649.666406	48215.679228	32.365581
650.191447	48290.719488	32.370599
650.895404	48372.628037	32.375616
651.396830	48451.949349	32.380634
652.083586	48541.636695	32.385652
652.704358	48622.401378	32.390669
653.580629	48705.505193	32.395687
654.074844	48776.066203	32.400704
654.987744	48870.983300	32.405722
655.228267	48957.072611	32.410740
655.645629	49029.708982	32.415757
656.568529	49114.521552	32.420775
656.768718	49209.545338	32.425792
657.702564	49292.667572	32.430810
658.112518	49389.582634	32.435828
658.860036	49475.505910	32.440845
659.625089	49564.596584	32.445863
659.722772	49661.447808	32.450880
660.417453	49755.112020	32.455898
660.578445	49851.644102	32.460916
661.529419	49947.375872	32.465933
662.672755	50048.032052	32.470951
663.375553	50140.949959	32.475968
664.199505	50230.419937	32.480986
665.344644	50328.792950	32.486004
665.723216	50401.730772	32.491021
666.605120	50493.457838	32.496039
667.290673	50592.542998	32.501056
668.249666	50669.301021	32.506074
668.432737	50762.505289	32.511092
668.901373	50841.346434	32.516109
670.114441	50924.639621	32.521127
670.436026	51016.627346	32.526144
671.146014	51106.827226	32.531162
671.784904	51194.450668	32.536180
672.357874	51277.301204	32.541197
672.971644	51371.351619	32.546215
673.701391	51463.296173	32.551232
674.545447	51547.022705	32.556250
674.941026	51646.132460	32.561268
675.392745	51733.926451	32.566285
676.121865	51823.708492	32.571303
676.670737	51914.398648	32.576320
677.751606	52000.981452	32.581338
678.264196	52095.075943	32.586356
678.735267	52177.262245	32.591373
679.917602	52268.019090	32.596391
680.428962	52354.705050	32.601408
681.161192	52419.405701	32.606426
681.629141	52508.712397	32.611444
682.355486	52602.376802	32.616461
683.028323	52688.779269	32.621479
683.587614	52784.881471	32.626496
684.386034	52868.461689	32.631514
684.708079	52964.740994	32.636532
685.920696	53060.318041	32.641549
686.454738	53137.764549	32.646567
687.040612	53234.857919	32.651584
688.282767	53316.503485	32.656602
688.741492	53417.850961	32.661620
689.335902	53500.895853	32.666637
690.326936	53585.125557	32.671655
690.596801	53677.087539	32.676672
691.674891	53770.252217	32.681690
692.017279	53864.114667	32.686708
692.915144	53952.967175	32.691725
693.836327	54049.327945	32.696743
694.221008	54144.975769	32.701760
695.065744	54227.534711	32.706778
695.254263	54327.953857	32.711796
695.859200	54417.917136	32.716813
696.661404	54515.089474	32.721831
697.192521	54623.372962	32.726848
698.296965	54717.189065	32.731866
699.833056	54799.768302	32.736884
700.711260	54880.754835	32.741901
701.628158	54969.867645	32.746919
702.021324	55059.322273	32.751936
703.066550	55137.998948	32.756954
704.088795	55217.964171	32.761972
704.572898	55300.437768	32.766989
705.621698	55352.230970	32.772007
706.623631	55442.768817	32.777024
707.622852	55504.797099	32.782042
708.266602	55573.507267	32.787060
709.127527	55641.436845	32.792077
709.353905	55712.149333	32.797095
709.929312	55789.939783	32.802112
710.527870	55858.385716	32.807130
711.109760	55948.997593	32.812148
711.547835	56016.140079	32.817165
712.169484	56101.151710	32.822183
712.643754	56185.718394	32.827200
713.295369	56265.378102	32.832218
713.777390	56361.949921	32.837236
714.040416	56456.923582	32.842253
715.034277	56541.353192	32.847271
715.204466	56651.411200	32.852288
715.909242	56751.531859	32.857306
716.433058	56850.042076	32.862324
716.665398	56962.566394	32.867341
717.515883	57066.494579	32.872359
718.175194	57170.332899	32.877376
719.068487	57283.198241	32.882394
719.576573	57400.725687	32.887412
719.998197	57511.127992	32.892429
721.037439	57615.731519	32.897447
721.918055	57736.360506	32.902464
722.741447	57825.340352	32.907482
723.558103	57930.378838	32.912500
724.757986	58035.180548	32.917517
725.447367	58130.929496	32.922535
726.360088	58214.466259	32.927552
727.355748	58296.724457	32.932570
727.874700	58390.418770	32.937588
728.795590	58473.113342	32.942605
729.433007	58571.403917	32.947623
729.730005	58659.507191	32.952640
731.098133	58738.607143	32.957658
732.084924	58822.324284	32.962676
732.565421	58907.007126	32.967693
733.632978	58995.092219	32.972711
734.100899	59083.448760	32.977728
735.236115	59167.738823	32.982746
735.867796	59264.222843	32.987764
736.317549	59360.564834	32.992781
736.959040	59440.445467	32.997799
737.636081	59539.911056	33.002816
738.439177	59631.806007	33.007834
739.004047	59726.131236	33.012852
739.394169	59814.971004	33.017869
740.181445	59920.041670	33.022887
740.582870	60030.116766	33.027904
741.643600	60123.783536	33.032922
742.195449	60226.980785	33.037940
743.337608	60324.990494	33.042957
743.745322	60431.528017	33.047975
744.272886	60544.199906	33.052992
745.037000	60650.511659	33.058010
745.596595	60753.709906	33.063028
746.051702	60867.331454	33.068045
747.196549	60973.338110	33.073063
747.586269	61084.078077	33.078080
748.491245	61197.940873	33.083098
749.491518	61317.201512	33.088116
750.226410	61431.288251	33.093133
751.156938	61533.615086	33.098151
751.343536	61643.604427	33.103168
752.052823	61765.938629	33.108186
753.167288	61877.340942	33.113204
753.822062	62004.274290	33.118221
755.145956	62099.135430	33.123239
756.135703	62204.279079	33.128256
756.977926	62304.907405	33.133274
758.169219	62404.550910	33.138292
759.148970	62508.659229	33.143309
759.934354	62600.067912	33.148327
761.248870	62684.114045	33.153344
762.098684	62775.196759	33.158362
762.901187	62873.225447	33.163380
763.334415	62962.354650	33.168397
764.027175	63043.479698	33.173415
764.719197	63142.849831	33.178432
765.001171	63227.173436	33.183450
765.945934	63334.278722	33.188468
766.470862	63423.559805	33.193485
767.189587	63520.692540	33.198503
768.195787	63627.447604	33.203520
768.601570	63729.371843	33.208538
769.119862	63830.652134	33.213556
769.771462	63947.719901	33.218573
770.526753	64049.115899	33.223591
771.734034	64152.207828	33.228608
772.352866	64252.302872	33.233626
773.162026	64356.021426	33.238644
773.545725	64466.030311	33.243661
774.372607	64563.118485	33.248679
775.395246	64683.930132	33.253696
775.937699	64786.362720	33.258714
776.453245	64870.826199	33.263732
777.330835	64974.846802	33.268749
777.892069	65076.264658	33.273767
778.362272	65183.939625	33.278784
779.502277	65291.871037	33.283802
779.926249	65403.466805	33.288820
780.408440	65511.248915	33.293837
781.311626	65623.865902	33.298855
781.790018	65744.413291	33.303872
782.794765	65868.854856	33.308890
783.854405	65977.662821	33.313908
784.202509	66105.177740	33.318925
784.952049	66222.930813	33.323943
785.533492	66348.890889	33.328960
786.194287	66485.950783	33.333978
787.045962	66609.229629	33.338996
788.190842	66743.201334	33.344013
789.136461	66865.605626	33.349031
789.197625	66987.978051	33.354048
789.773895	67112.708050	33.359066
791.055892	67248.895973	33.364084
791.818346	67384.298542	33.369101
792.552363	67512.526170	33.374119
793.550627	67629.423650	33.379136
794.732814	67767.966350	33.384154
795.740689	67884.578557	33.389172
797.704596	67987.991785	33.394189
798.998152	68081.398509	33.399207
800.117914	68175.909197	33.404224
800.948622	68278.057383	33.409242
801.477371	68380.544524	33.414260
802.022812	68491.780146	33.419277
802.918997	68593.685047	33.424295
803.838693	68692.857596	33.429312
804.651133	68801.912542	33.434330
806.044771	68888.284350	33.439348
806.606849	68997.657933	33.444365
807.057513	69097.279065	33.449383
807.523378	69200.893740	33.454400
808.278793	69309.244224	33.459418
809.019021	69419.598490	33.464436
810.030610	69517.765660	33.469453
810.902894	69615.530757	33.474471
811.523800	69732.819775	33.479488
812.528207	69838.499276	33.484506
813.435412	69941.256258	33.489524
814.337048	70062.897388	33.494541
815.498706	70144.313525	33.499559
816.912473	70237.025303	33.504576
817.869520	70329.998899	33.509594
818.438609	70417.689053	33.514612
819.022410	70527.122643	33.519629
819.856188	70621.585694	33.524647
820.269854	70721.750746	33.529664
820.635163	70826.622444	33.534682
821.564984	70923.781841	33.539700
821.900138	71038.664449	33.544717
822.881682	71156.650612	33.549735
823.790281	71269.190045	33.554752
823.828332	71388.388859	33.559770
824.731354	71490.595300	33.564788
825.287032	71611.170571	33.569805
825.725144	71743.302962	33.574823
826.549307	71873.399753	33.579840
827.185033	72011.037336	33.584858
828.224933	72128.030796	33.589876
829.078111	72259.885457	33.594893
829.729450	72383.514350	33.599911
830.518665	72507.008237	33.604928
831.259139	72617.489887	33.609946
833.215356	72718.548224	33.614964
834.511344	72825.650634	33.619981
835.498174	72921.592525	33.624999
836.690380	73035.057669	33.630016
837.076294	73145.229717	33.635034
838.280774	73240.619369	33.640052
838.774882	73348.115434	33.645069
839.559659	73444.876149	33.650087
840.615015	73551.309851	33.655104
840.985080	73664.817746	33.660122
842.100954	73768.050930	33.665140
842.429872	73881.730850	33.670157
843.406659	73982.795353	33.675175
844.216599	74096.350197	33.680192
844.499716	74209.620683	33.685210
845.448088	74333.136097	33.690228
846.242067	74457.562921	33.695245
846.946695	74590.845690	33.700263
847.952070	74710.034554	33.705280
849.085208	74835.588030	33.710298
849.687870	74949.647605	33.715316
850.714329	75080.881033	33.720333
851.847450	75208.652966	33.725351
852.981200	75308.089158	33.730368
854.570955	75420.514112	33.735386
855.648770	75526.065418	33.740404
856.823044	75625.775111	33.745421
857.184702	75726.499123	33.750439
858.301047	75834.148363	33.755456
858.584528	75945.880661	33.760474
859.807111	76050.068598	33.765492
860.586337	76159.836705	33.770509
861.301716	76272.161423	33.775527
862.433357	76391.413925	33.780544
862.605773	76499.948324	33.785562
863.507128	76616.628339	33.790580
864.093408	76734.308269	33.795597
864.707935	76870.327245	33.800615
865.645360	76993.159770	33.805632
866.358367	77114.571177	33.810650
866.976316	77242.902048	33.815668
867.389545	77378.575028	33.820685
868.708352	77504.175097	33.825703
869.610023	77643.509991	33.830720
870.168760	77773.740169	33.835738
870.851627	77920.204925	33.840756
871.665660	78055.071054	33.845773
872.266730	78203.006979	33.850791
873.118704	78340.275560	33.855808
874.154732	78482.317378	33.860826
874.964567	78632.921315	33.865844
875.637418	78773.222552	33.870861
876.554280	78923.963336	33.875879
877.636886	79058.906326	33.880896
878.214341	79210.246570	33.885914
879.634554	79342.642309	33.890932
881.806522	79458.793348	33.895949
883.119115	79594.450399	33.900967
884.542936	79705.943389	33.905984
885.302678	79826.079814	33.911002
885.982491	79935.333758	33.916020
886.886192	80066.483550	33.921037
887.699146	80180.430570	33.926055
888.804454	80290.746847	33.931072
889.071558	80411.685080	33.936090
889.884734	80512.735956	33.941108
891.185073	80623.555124	33.946125
891.505691	80734.249405	33.951143
892.151837	80849.808960	33.956160
892.715687	80966.522146	33.961178
893.533958	81091.393286	33.966196
894.631367	81210.697251	33.971213
895.597292	81332.758992	33.976231
896.068866	81449.095861	33.981248
896.972302	81584.319816	33.986266
898.068647	81706.654162	33.991284
898.821312	81838.482041	33.996301
899.671908	81973.171316	34.001319
900.620336	82096.303385	34.006336
901.097731	82244.039311	34.011354
902.063814	82377.039951	34.016372
903.142586	82519.526336	34.021389
903.602964	82658.727261	34.026407
904.629654	82787.108295	34.031424
905.655002	82942.275644	34.036442
906.157880	83078.215631	34.041460
907.330370	83224.732793	34.046477
907.909935	83375.499548	34.051495
908.819399	83519.436561	34.056512
909.760956	83669.742720	34.061530
910.689312	83824.524574	34.066548
911.603114	83971.428176	34.071565
912.743102	84116.776586	34.076583
913.320983	84265.787003	34.081600
914.084537	84432.749552	34.086618
914.682608	84583.975913	34.091636
915.758839	84743.313882	34.096653
916.900008	84907.432356	34.101671
918.536178	85065.366600	34.106688
920.074373	85200.749022	34.111706
920.811088	85339.716918	34.116724
922.123319	85482.688315	34.121741
922.858223	85635.191250	34.126759
923.698227	85772.801841	34.131776
924.563419	85921.560370	34.136794
925.409035	86069.904550	34.141812
926.731122	86199.686461	34.146829
927.260263	86351.629779	34.151847
928.348344	86489.141546	34.156864
929.091512	86638.505749	34.161882
929.816889	86773.123027	34.166900
930.899015	86924.729288	34.171917
932.035231	87074.857871	34.176935
933.111541	87210.157201	34.181952
933.657626	87369.123652	34.186970
934.952640	87523.056748	34.191988
936.267181	87662.477452	34.197005
936.518019	87813.103259	34.202023
937.511668	87953.310595	34.207040
938.715522	88112.799023	34.212058
939.578557	88260.429181	34.217076
940.350559	88416.755283	34.222093
940.718911	88569.419548	34.227111
941.927422	88714.906829	34.232128
942.927940	88879.297667	34.237146
943.650097	89033.809886	34.242164
944.941964	89180.414305	34.247181
946.047133	89339.899422	34.252199
946.745120	89482.973742	34.257216
947.315673	89645.154911	34.262234
948.521598	89793.321952	34.267252
949.698125	89944.802134	34.272269
950.540151	90101.430258	34.277287
951.510329	90232.374882	34.282304
952.776486	90385.338747	34.287322
953.293295	90523.389562	34.292340
954.362857	90665.131279	34.297357
954.879634	90818.316064	34.302375
955.861523	90964.179270	34.307392
956.859340	91124.666561	34.312410
957.706445	91267.764038	34.317428
958.604706	91423.008732	34.322445
959.442124	91584.207977	34.327463
960.793194	91726.227440	34.332480
961.797960	91877.604787	34.337498
962.539504	92038.682032	34.342516
963.501196	92192.754673	34.347533
964.731618	92351.526309	34.352551
965.744629	92505.389698	34.357568
966.560640	92665.584037	34.362586
967.231337	92820.377160	34.367604
968.116823	92984.060523	34.372621
969.174416	93146.906617	34.377639
970.440183	93309.936453	34.382656
971.113372	93461.069343	34.387674
972.026163	93633.865242	34.392692
973.288563	93797.215060	34.397709
974.055590	93961.213690	34.402727
975.224657	94128.382445	34.407744
975.946692	94296.750203	34.412762
977.083488	94465.231391	34.417780
978.461294	94634.512342	34.422797
979.226171	94807.591453	34.427815
980.394567	94957.665409	34.432832
981.600930	95124.770304	34.437850
982.357978	95289.436638	34.442868
983.499906	95451.609815	34.447885
984.143468	95624.230762	34.452903
985.537744	95783.488713	34.457920
986.363318	95955.728059	34.462938
987.136445	96131.741369	34.467956
988.268140	96289.052842	34.472973
988.762001	96454.717207	34.477991
989.795616	96625.317756	34.483008
990.994218	96806.351421	34.488026
991.834787	96991.688795	34.493044
993.197600	97144.278046	34.498061
994.484603	97316.820188	34.503079
995.063061	97493.644828	34.508096
996.026423	97674.859722	34.513114
997.040600	97840.525919	34.518132
998.053966	98015.142978	34.523149
999.122174	98197.143067	34.528167
1000.260532	98367.964752	34.533184
1001.354983	98540.543661	34.538202
1002.488187	98715.247193	34.543220
1003.062595	98880.429829	34.548237
1004.231921	99059.946923	34.553255
1005.041432	99221.025087	34.558272
1006.488556	99405.318005	34.563290
1007.038214	99580.003493	34.568308
1008.211016	99757.356069	34.573325
1008.953030	99938.986037	34.578343
1010.174404	100100.992954	34.583360
1011.732246	100279.555871	34.588378
1012.260831	100451.232039	34.593396
1014.346303	100609.226782	34.598413
1015.289012	100779.026899	34.603431
1016.457085	100932.374573	34.608448
1017.499968	101101.121082	34.613466
1018.422362	101252.619687	34.618484
1020.293131	101386.943686	34.623501
1021.149073	101531.062593	34.628519
1021.929690	101669.171730	34.633536
1022.904299	101808.823191	34.638554
1023.476109	101960.405306	34.643572
1024.691291	102097.116965	34.648589
1025.360328	102252.247848	34.653607
1026.161653	102410.959466	34.658624
1027.225147	102567.006317	34.663642
1027.666545	102731.950328	34.668660
1028.699516	102889.664387	34.673677
1029.843805	103055.463542	34.678695
1031.111592	103229.954594	34.683712
1032.021082	103388.894848	34.688730
1032.515450	103562.849425	34.693748
1033.550946	103724.180562	34.698765
1034.253071	103905.749886	34.703783
1035.548237	104078.060264	34.708800
1036.709532	104245.232017	34.713818
1037.855357	104435.610241	34.718836
1039.227825	104590.679902	34.723853
1040.236590	104770.684359	34.728871
1041.037154	104946.981904	34.733888
1042.674719	105127.194123	34.738906
1043.633199	105298.041898	34.743924
1044.446697	105468.304605	34.748941
1045.599532	105643.041730	34.753959
1046.689911	105813.998248	34.758976
1047.546748	105987.578897	34.763994
1048.077909	106178.443546	34.769012
1049.536910	106346.999221	34.774029
1051.581107	106509.187443	34.779047
1052.606403	106683.391937	34.784064
1053.970504	106851.977638	34.789082
1054.924295	107012.094551	34.794100
1056.610272	107171.070466	34.799117
1057.633112	107330.873722	34.804135
1058.725396	107493.000058	34.809152
1059.543580	107657.477929	34.814170
1060.411331	107818.829390	34.819188
1060.930503	107987.261271	34.824205
1062.319819	108155.050507	34.829223
1062.654477	108338.222635	34.834240
1063.874877	108514.536191	34.839258
1064.452354	108697.684872	34.844276
1065.429721	108873.188669	34.849293
1066.203110	109074.797553	34.854311
1067.012274	109262.554190	34.859328
1068.387611	109454.953281	34.864346
1068.587199	109657.733250	34.869364
1069.164914	109846.898822	34.874381
1070.365986	110060.671223	34.879399
1071.710687	110265.748284	34.884416
1072.966153	110469.356761	34.889434
1073.851612	110690.144560	34.894452
1075.313863	110894.813726	34.899469
1076.432778	111095.606466	34.904487
1077.285744	111309.516980	34.909504
1078.933643	111496.849789	34.914522
1079.850426	111704.132702	34.919540
1081.616411	111904.194580	34.924557
1082.764056	112085.496024	34.929575
1083.807010	112287.613603	34.934592
1085.427939	112467.866347	34.939610
1086.634010	112647.753742	34.944628
1088.150967	112830.193255	34.949645
1089.474836	113000.133638	34.954663
1090.720180	113164.392658	34.959680
1092.264708	113322.758914	34.964698
1093.241728	113478.602085	34.969716
1094.412952	113639.590056	34.974733
1095.369768	113789.793925	34.979751
1096.442064	113954.045553	34.984768
1097.424899	114102.179337	34.989786
1098.216402	114266.133890	34.994804
1099.498813	114418.382045	34.999821
1100.717264	114583.171663	35.004839
1101.117372	114746.276458	35.009856
1102.268619	114902.111094	35.014874
1102.745824	115083.266084	35.019892
1103.729020	115258.305518	35.024909
1104.981324	115437.692074	35.029927
1105.684973	115626.715973	35.034944
1106.527552	115809.161746	35.039962
1107.442723	116009.201749	35.044980
1108.077405	116211.303425	35.049997
1109.204986	116408.534612	35.055015
1110.278360	116617.304815	35.060032
1111.128732	116807.465942	35.065050
1112.445217	117025.243887	35.070068
1113.429225	117233.650993	35.075085
1115.158670	117428.218476	35.080103
1116.631009	117624.590298	35.085120
1117.968307	117822.785425	35.090138
1118.639225	118036.040567	35.095156
1119.743317	118231.724818	35.100173
1121.315532	118434.262427	35.105191
1122.293836	118634.369900	35.110208
1123.028225	118836.558803	35.115226
1124.713534	119037.331452	35.120244
1125.932177	119242.567079	35.125261
1127.093226	119435.965353	35.130279
1128.827110	119639.574909	35.135296
1130.011557	119820.667279	35.140314
1131.373401	120024.666917	35.145332
1132.762348	120206.350637	35.150349
1134.081321	120383.301987	35.155367
1135.276275	120577.043159	35.160384
1136.512828	120765.552527	35.165402
1137.658583	120950.055831	35.170420
1138.917801	121131.599277	35.175437
1139.782362	121316.059534	35.180455
1140.934023	121499.993671	35.185472
1142.158792	121682.864338	35.190490
1142.889895	121878.879148	35.195508
1143.916000	122072.781011	35.200525
1145.010364	122271.442915	35.205543
1145.613470	122459.463364	35.210560
1146.728852	122662.196026	35.215578
1147.373956	122865.295119	35.220596
1148.537943	123069.037108	35.225613
1149.661086	123267.483831	35.230631
1151.222303	123476.176639	35.235648
1152.568027	123683.026741	35.240666
1154.142509	123881.177502	35.245684
1155.037121	124075.896240	35.250701
1156.453304	124276.268434	35.255719
1157.447207	124482.188200	35.260736
1158.655656	124677.253984	35.265754
1160.020481	124867.551516	35.270772
1161.017008	125071.279121	35.275789
1162.012649	125263.869122	35.280807
1162.606509	125464.908760	35.285824
1164.002707	125672.636509	35.290842
1165.033742	125884.926260	35.295860
1165.781826	126088.532907	35.300877
1167.033727	126286.834713	35.305895
1167.969753	126494.055065	35.310912
1168.934458	126698.201724	35.315930
1170.056768	126903.745665	35.320948
1171.236529	127111.133945	35.325965
1172.591906	127317.506172	35.330983
1173.333712	127528.136883	35.336000
1174.399157	127736.764151	35.341018
1175.747423	127961.714856	35.346036
1176.655124	128168.389746	35.351053
1177.836492	128395.056329	35.356071
1178.778030	128633.155095	35.361088
1180.049969	128840.677081	35.366106
1181.347045	129070.742150	35.371124
1182.317421	129299.019889	35.376141
1183.878830	129517.385963	35.381159
1184.783284	129748.734199	35.386176
1185.853467	129979.905488	35.391194
1187.214956	130215.638175	35.396212
1188.137824	130449.398040	35.401229
1189.598609	130673.964871	35.406247
1190.679924	130909.212319	35.411264
1192.227947	131142.433989	35.416282
1193.648763	131364.295373	35.421300
1195.037910	131605.144731	35.426317
1196.949610	131821.056860	35.431335
1197.790276	132051.310841	35.436352
1198.997814	132265.559005	35.441370
1200.430998	132488.210866	35.446388
1201.778485	132721.155157	35.451405
1203.780073	132919.421271	35.456423
1205.581848	133124.013234	35.461440
1206.982572	133327.247768	35.466458
1208.413549	133531.176392	35.471476
1209.383844	133735.799833	35.476493
1210.792808	133938.553690	35.481511
1211.668418	134143.003486	35.486528
1212.507941	134347.688270	35.491546
1214.086164	134548.032822	35.496564
1214.918124	134763.125887	35.501581
1216.111161	134969.128608	35.506599
1216.841210	135189.873750	35.511616
1217.987558	135405.694716	35.516634
1219.503565	135606.053703	35.521652
1220.751744	135825.921387	35.526669
1222.152252	136040.170132	35.531687
1222.906512	136251.323232	35.536704
1224.108719	136476.581696	35.541722
1224.970749	136699.280403	35.546740
1226.002622	136933.463369	35.551757
1227.158131	137153.060052	35.556775
1228.321099	137392.224677	35.561792
1229.461033	137621.889239	35.566810
1230.822549	137848.335010	35.571828
1231.775627	138093.678147	35.576845
1233.195262	138325.434349	35.581863
1234.484323	138568.011647	35.586880
1235.581208	138808.450215	35.591898
1237.109927	139032.806989	35.596916
1238.116785	139268.046192	35.601933
1239.146517	139517.014244	35.606951
1240.236031	139751.570299	35.611968
1241.504864	139992.051403	35.616986
1242.822296	140229.289947	35.622004
1243.966592	140476.277988	35.627021
1245.733916	140713.524644	35.632039
1246.769792	140945.988239	35.637056
1248.298505	141184.772102	35.642074
1249.742051	141407.325822	35.647092
1250.642472	141625.904401	35.652109
1251.911655	141857.219010	35.657127
1252.869692	142091.591261	35.662144
1253.586590	142315.696988	35.667162
1254.924489	142535.886405	35.672180
1256.197409	142776.164904	35.677197
1257.718246	143016.646902	35.682215
1258.762582	143256.037029	35.687232
1259.509784	143501.033772	35.692250
1261.539909	143730.562738	35.697268
1262.150773	143983.655130	35.702285
1263.379440	144234.113715	35.707303
1264.104367	144484.055881	35.712320
1265.725205	144739.722734	35.717338
1266.965932	144990.246641	35.722356
1267.818432	145256.151932	35.727373
1268.999945	145511.789903	35.732391
1270.253861	145788.563092	35.737408
1271.916475	146049.141870	35.742426
1273.323154	146307.033170	35.747444
1274.592362	146574.403142	35.752461
1276.180472	146830.212474	35.757479
1277.405402	147093.517757	35.762496
1278.709061	147354.108514	35.767514
1280.343362	147604.240806	35.772532
1282.002556	147864.524592	35.777549
1283.492442	148116.928545	35.782567
1284.986835	148377.151806	35.787584
1286.689548	148629.791439	35.792602
1288.459934	148847.541343	35.797620
1289.961953	149092.167231	35.802637
1292.004123	149312.948205	35.807655
1293.416924	149545.125508	35.812672
1294.456296	149766.864988	35.817690
1296.122525	149997.824101	35.822708
1296.922365	150241.765450	35.827725
1298.276081	150468.053571	35.832743
1299.730325	150700.203947	35.837760
1300.397932	150930.625197	35.842778
1301.816493	151167.365481	35.847796
1302.484178	151407.131152	35.852813
1303.687068	151654.112926	35.857831
1305.152399	151905.992567	35.862848
1306.179028	152155.949102	35.867866
1307.186015	152408.131246	35.872884
1308.337721	152661.853218	35.877901
1309.812856	152907.135023	35.882919
1310.833973	153182.827580	35.887936
1312.092553	153424.159616	35.892954
1313.450728	153684.010466	35.897972
1314.898135	153941.297007	35.902989
1316.311841	154194.883272	35.908007
1317.525098	154464.864944	35.913024
1318.698946	154726.602735	35.918042
1320.240827	154996.776645	35.923060
1321.417525	155261.905808	35.928077
1322.421033	155514.762315	35.933095
1324.332603	155781.505257	35.938112
1325.486649	156047.161999	35.943130
1326.503504	156313.895070	35.948148
1327.401407	156587.046105	35.953165
1329.273828	156851.578429	35.958183
1330.262141	157119.398638	35.963200
1331.256190	157400.764604	35.968218
1332.952482	157664.122071	35.973236
1333.868037	157948.168820	35.978253
1334.950084	158223.443930	35.983271
1336.525479	158482.926489	35.988288
1337.653671	158756.914574	35.993306
1339.080765	159012.550559	35.998324
1340.566873	159284.694942	36.003341
1341.972306	159538.863842	36.008359
1344.067343	159791.338914	36.013376
1345.169119	160047.550601	36.018394
1347.494324	160296.779741	36.023412
1348.383453	160551.490617	36.028429
1349.868055	160795.330746	36.033447
1351.266259	161062.380292	36.038464
1352.416152	161326.359380	36.043482
1353.873465	161576.986285	36.048500
1354.930611	161828.159248	36.053517
1356.340773	162088.622083	36.058535
1357.688196	162354.720076	36.063552
1358.916027	162617.701977	36.068570
1360.440187	162875.737895	36.073588
1361.567820	163146.418694	36.078605
1363.168363	163409.980241	36.083623
1364.970479	163673.155795	36.088640
1366.584812	163926.446047	36.093658
1368.101815	164180.818983	36.098676
1369.734265	164441.053207	36.103693
1370.980285	164713.105756	36.108711
1372.097097	164967.620492	36.113728
1372.969322	165242.171389	36.118746
1374.703610	165498.038858	36.123764
1375.920738	165771.027013	36.128781
1377.022799	166046.916394	36.133799
1378.602480	166321.005373	36.138816
1379.574967	166593.032037	36.143834
1381.259483	166870.522189	36.148852
1382.810838	167134.499489	36.153869
1384.116884	167400.966670	36.158887
1385.514550	167683.012315	36.163904
1387.041721	167957.915818	36.168922
1388.444728	168220.701482	36.173940
1390.068618	168485.497762	36.178957
1391.580066	168758.718093	36.183975
1392.737458	169038.000625	36.188992
1393.669578	169319.770049	36.194010
1394.829650	169604.069723	36.199028
1396.134020	169883.129324	36.204045
1397.684028	170175.077425	36.209063
1398.909557	170461.350941	36.214080
1399.795535	170742.752098	36.219098
1401.721512	171039.711014	36.224116
1402.758496	171330.080555	36.229133
1404.153423	171632.140449	36.234151
1405.791883	171934.937978	36.239168
1407.185395	172221.331540	36.244186
1408.428670	172513.654128	36.249204
1410.289995	172811.582383	36.254221
1411.511496	173106.094627	36.259239
1413.187472	173394.810100	36.264256
1414.112655	173711.389111	36.269274
1415.767470	173998.484767	36.274292
1417.247203	174295.475222	36.279309
1418.649806	174594.497842	36.284327
1420.180168	174893.361894	36.289344
1421.666238	175185.948391	36.294362
1423.039825	175480.534463	36.299380
1424.355638	175789.759020	36.304397
1425.735636	176078.898679	36.309415
1427.056386	176373.978742	36.314432
1428.283053	176679.969789	36.319450
1430.196271	176974.603678	36.324468
1431.539384	177268.591314	36.329485
1432.761680	177545.862227	36.334503
1434.294602	177824.761629	36.339520
1435.622357	178116.316455	36.344538
1436.771872	178405.055663	36.349556
1438.304607	178696.910517	36.354573
1439.636896	178987.654829	36.359591
1441.109169	179283.584683	36.364608
1441.997527	179588.292904	36.369626
1443.380052	179877.406814	36.374644
1444.604588	180179.702437	36.379661
1445.849362	180497.615594	36.384679
1447.387292	180809.007492	36.389696
1448.325690	181137.510980	36.394714
1449.915667	181444.934779	36.399732
1451.471158	181776.493306	36.404749
1452.957959	182095.339196	36.409767
1454.530246	182411.048775	36.414784
1456.081848	182734.509175	36.419802
1457.386822	183062.479414	36.424820
1459.394631	183384.270477	36.429837
1460.607527	183716.549706	36.434855
1462.340519	184029.801127	36.439872
1463.657299	184365.749109	36.444890
1465.241692	184694.976397	36.449908
1466.611843	185027.336981	36.454925
1468.028921	185356.465613	36.459943
1469.792897	185672.181007	36.464960
1471.415982	186011.718578	36.469978
1472.948136	186339.003577	36.474996
1474.893542	186660.408435	36.480013
1476.154303	186985.629761	36.485031
1477.928470	187310.466925	36.490048
1479.047482	187642.671926	36.495066
1480.547882	187980.964997	36.500084
1482.067754	188373.103789	36.505101
1483.786607	188702.551125	36.510119
1485.609676	189020.781708	36.515136
1486.837943	189359.807364	36.520154
1488.132586	189687.774564	36.525172
1489.575131	190014.220936	36.530189
1491.296684	190344.460004	36.535207
1492.794438	190673.592014	36.540224
1494.126992	191015.578028	36.545242
1495.666053	191351.893780	36.550260
1497.391827	191685.895193	36.555277
1498.589770	192019.294316	36.560295
1499.973113	192355.154597	36.565312
1501.687670	192691.395758	36.570330
1503.045641	193024.975737	36.575348
1504.945223	193351.537366	36.580365
1506.297887	193691.901970	36.585383
1508.073291	194022.650500	36.590400
1509.607816	194360.956302	36.595418
1510.974126	194691.795941	36.600436
1512.517348	195019.662163	36.605453
1514.322147	195353.889373	36.610471
1515.907034	195679.616953	36.615488
1517.366254	196018.065690	36.620506
1519.554307	196338.061289	36.625524
1521.295008	196644.842612	36.630541
1522.911993	196974.251393	36.635559
1524.658931	197287.180301	36.640576
1525.852095	197597.300754	36.645594
1527.071665	197921.083880	36.650612
1528.361949	198244.577218	36.655629
1529.952866	198564.544136	36.660647
1531.412953	198898.477862	36.665664
1533.067244	199211.298258	36.670682
1534.142803	199515.496952	36.675700
1535.761704	199820.170037	36.680717
1537.009073	200131.226978	36.685735
1538.755289	200435.957501	36.690752
1540.366597	200760.650455	36.695770
1541.958297	201070.639186	36.700788
1543.813739	201376.268812	36.705805
1544.867678	201692.337789	36.710823
1546.415088	201999.921907	36.715840
1547.457704	202327.882134	36.720858
1548.942837	202647.416280	36.725876
1550.238959	202971.222798	36.730893
1551.775489	203314.476055	36.735911
1552.993106	203655.493617	36.740928
1554.827184	204001.495849	36.745946
1555.937849	204335.037568	36.750964
1557.408499	204679.370501	36.755981
1558.990363	205036.108605	36.760999
1560.690218	205380.051227	36.766016
1561.967783	205734.678932	36.771034
1563.549993	206093.400238	36.776052
1565.499462	206455.316251	36.781069
1566.420505	206816.885759	36.786087
1568.449411	207176.250221	36.791104
1569.776169	207540.094480	36.796122
1571.670297	207904.053740	36.801140
1573.648158	208265.053684	36.806157
1574.901960	208631.578378	36.811175
1576.999226	208982.628032	36.816192
1578.568138	209345.344774	36.821210
1579.940622	209711.141170	36.826228
1581.657310	210074.928143	36.831245
1582.930827	210445.745498	36.836263
1585.013216	210805.589487	36.841280
1586.443374	211174.427226	36.846298
1587.900121	211544.937902	36.851316
1589.450848	211905.374526	36.856333
1591.114144	212275.548925	36.861351
1592.619441	212633.656373	36.866368
1594.435896	213011.860593	36.871386
1596.068496	213389.560537	36.876404
1597.941675	213762.320331	36.881421
1598.525013	214139.143741	36.886439
1600.137919	214511.843422	36.891456
1602.014353	214899.769882	36.896474
1603.543566	215282.340056	36.901492
1605.195962	215662.935214	36.906509
1606.596749	216055.027214	36.911527
1608.273380	216439.023366	36.916544
1609.813152	216821.313790	36.921562
1611.680891	217202.664049	36.926580
1613.229760	217595.318428	36.931597
1615.020500	217980.491891	36.936615
1616.971886	218361.753670	36.941632
1618.470931	218748.802375	36.946650
1619.761847	219137.636762	36.951668
1621.762729	219525.369508	36.956685
1623.188003	219908.060937	36.961703
1624.826719	220296.104802	36.966720
1626.565468	220690.509602	36.971738
1628.099539	221075.470901	36.976756
1629.870429	221468.702409	36.981773
1631.497335	221850.702597	36.986791
1633.304484	222236.256668	36.991808
1634.572425	222626.366347	36.996826
1636.629555	223008.604373	37.001844
1638.473327	223378.021404	37.006861
1639.827398	223765.653647	37.011879
1641.634776	224123.288989	37.016896
1643.651930	224477.690621	37.021914
1644.789466	224836.421607	37.026932
1646.662921	225191.557075	37.031949
1648.097628	225567.033667	37.036967
1649.714802	225921.777360	37.041984
1651.255002	226295.763969	37.047002
1652.580281	226675.982769	37.052020
1654.110155	227044.763068	37.057037
1655.941462	227424.369075	37.062055
1657.271656	227805.196608	37.067072
1659.179010	228200.337826	37.072090
1660.380283	228572.166893	37.077108
1662.683536	228963.740159	37.082125
1664.347850	229355.768932	37.087143
1665.422879	229736.153110	37.092160
1667.104243	230128.686971	37.097178
1668.792434	230520.990942	37.102196
1670.179568	230920.302518	37.107213
1672.424781	231326.287849	37.112231
1673.531065	231727.192550	37.117248
1675.687242	232129.939602	37.122266
1676.967722	232544.433012	37.127284
1678.809706	232944.205593	37.132301
1680.627432	233349.773752	37.137319
1682.590656	233758.087833	37.142336
1684.411649	234153.315444	37.147354
1685.493511	234561.334883	37.152372
1687.649496	234972.971013	37.157389
1689.169658	235393.775382	37.162407
1690.884968	235806.571996	37.167424
1692.830803	236214.911846	37.172442
1694.480084	236636.304339	37.177460
1695.962892	237044.690313	37.182477
1697.701830	237477.321581	37.187495
1699.406212	237879.752830	37.192512
1701.406056	238296.896803	37.197530
1703.149510	238726.655082	37.202548
1704.699496	239133.884734	37.207565
1706.864632	239561.822975	37.212583
1708.512134	239975.387039	37.217600
1710.428872	240389.187788	37.222618
1712.194986	240802.757438	37.227636
1713.969262	241213.429182	37.232653
1715.599758	241629.178010	37.237671
1717.433234	242049.822599	37.242688
1719.371917	242466.156861	37.247706
1720.550050	242885.149718	37.252724
1722.997036	243286.338928	37.257741
1724.880698	243707.429935	37.262759
1726.182983	244120.558375	37.267776
1728.302668	244529.341224	37.272794
1729.703031	244941.207985	37.277812
1731.480355	245356.520524	37.282829
1732.990860	245774.973104	37.287847
1735.118638	246188.476287	37.292864
1737.229601	246593.318914	37.297882
1738.881373	247014.058364	37.302900
1740.685552	247406.957225	37.307917
1742.203219	247813.414211	37.312935
1743.866081	248219.847560	37.317952
1746.141716	248619.604870	37.322970
1748.050774	249030.595649	37.327988
1749.743228	249432.830156	37.333005
1751.516185	249828.776761	37.338023
1753.096354	250237.885495	37.343040
1754.822106	250632.821465	37.348058
1756.282239	251030.160416	37.353076
1758.456993	251410.341834	37.358093
1759.457972	251790.578992	37.363111
1761.424575	252188.318370	37.368128
1762.849326	252564.067368	37.373146
1764.590181	252970.908425	37.378164
1766.198716	253368.472071	37.383181
1767.960615	253770.887725	37.388199
1769.182961	254175.622006	37.393216
1770.903826	254580.658136	37.398234
1772.467599	254993.973098	37.403252
1774.253835	255409.639719	37.408269
1775.891388	255825.836351	37.413287
1777.071851	256261.738251	37.418304
1778.824759	256677.177524	37.423322
1780.857632	257128.209145	37.428340
1782.496375	257554.255633	37.433357
1784.280419	257999.582510	37.438375
1785.660188	258447.104710	37.443392
1787.567189	258898.962473	37.448410
1788.744488	259360.813515	37.453428
1790.554742	259818.677470	37.458445
1792.305440	260282.899032	37.463463
1793.926629	260758.543678	37.468480
1795.846727	261224.589161	37.473498
1797.747845	261696.655484	37.478516
1799.467965	262171.186521	37.483533
1801.161122	262657.759208	37.488551
1802.666391	263135.494660	37.493568
1805.108921	263614.452901	37.498586
1806.518759	264099.437835	37.503604
1808.506002	264586.209722	37.508621
1810.486357	265079.025396	37.513639
1812.546721	265560.980796	37.518656
1814.428176	266048.117872	37.523674
1816.137555	266541.019622	37.528692
1818.564731	267010.008059	37.533709
1820.243093	267498.033318	37.538727
1821.972486	267995.115349	37.543744
1824.021276	268477.591609	37.548762
1825.747826	268975.684877	37.553780
1827.736384	269454.660593	37.558797
1829.573850	269941.937168	37.563815
1831.400036	270431.498700	37.568832
1833.222189	270923.115412	37.573850
1835.072525	271412.870994	37.578868
1836.994579	271900.149099	37.583885
1839.351203	272390.658118	37.588903
1841.128074	272893.039287	37.593920
1842.905549	273370.477691	37.598938
1844.708752	273864.798199	37.603956
1846.402339	274350.574302	37.608973
1848.467932	274849.317718	37.613991
1850.104573	275340.988878	37.619008
1852.114115	275823.964040	37.624026
1854.067810	276328.328445	37.629044
1856.062714	276808.684184	37.634061
1857.799934	277303.400472	37.639079
1859.895259	277790.515141	37.644096
1862.090759	278269.281411	37.649114
1864.230875	278754.249787	37.654132
1866.065301	279245.383105	37.659149
1868.179251	279717.931257	37.664167
1869.877794	280194.274445	37.669184
1872.617462	280649.831315	37.674202
1874.662980	281127.104582	37.679220
1876.468644	281599.892092	37.684237
1878.099780	282052.972660	37.689255
1879.747059	282504.930512	37.694272
1881.608235	282948.522888	37.699290
1883.823646	283386.292714	37.704308
1884.881560	283840.162582	37.709325
1886.890715	284291.874583	37.714343
1888.636195	284758.606790	37.719360
1890.139615	285210.087177	37.724378
1891.925179	285673.251854	37.729396
1893.443477	286142.600165	37.734413
1895.263337	286611.618684	37.739431
1896.466258	287096.041907	37.744448
1898.226028	287574.178797	37.749466
1899.951174	288069.279329	37.754484
1901.575504	288564.975867	37.759501
1903.884489	289061.297811	37.764519
1905.705362	289571.327349	37.769536
1907.680325	290063.377237	37.774554
1909.696243	290553.131696	37.779572
1912.060615	291051.765281	37.784589
1913.979735	291551.429355	37.789607
1915.703315	292057.340560	37.794624
1917.619003	292563.953821	37.799642
1919.780940	293069.381775	37.804660
1921.368455	293577.256585	37.809677
1923.571104	294086.985801	37.814695
1925.393462	294598.801261	37.819712
1927.480926	295118.009728	37.824730
1929.106744	295644.140743	37.829748
1931.021961	296159.355451	37.834765
1932.929332	296678.197282	37.839783
1934.489833	297199.703629	37.844800
1936.585185	297733.637639	37.849818
1938.932409	298261.688049	37.854836
1940.989382	298789.448843	37.859853
1943.280552	299314.680041	37.864871
1945.383029	299833.284418	37.869888
1948.144553	300337.462755	37.874906
1950.651767	300856.831811	37.879924
1952.345323	301361.700811	37.884941
1954.413149	301868.080411	37.889959
1956.200900	302386.201754	37.894976
1958.126648	302890.055266	37.899994
1960.590742	303403.821426	37.905012
1962.460742	303908.536943	37.910029
1964.443888	304423.612128	37.915047
1966.027501	304944.913058	37.920064
1967.776012	305461.740666	37.925082
1969.874927	305968.176986	37.930100
1971.737502	306496.170442	37.935117
1973.657487	307004.121960	37.940135
1975.538812	307530.172434	37.945152
1977.166532	308047.398426	37.950170
1979.178254	308586.133996	37.955188
1981.129794	309107.283193	37.960205
1982.976948	309633.062641	37.965223
1985.278002	310159.552175	37.970240
1987.542045	310683.554351	37.975258
1989.468842	311214.583329	37.980276
1991.620315	311738.007728	37.985293
1994.109338	312256.957289	37.990311
1995.956926	312787.777881	37.995328
1998.155026	313300.746240	38.000346
2000.083012	313811.035549	38.005364
2001.801202	314340.767244	38.010381
2004.138102	314855.777649	38.015399
2005.857893	315367.681044	38.020416
2008.056179	315893.512711	38.025434
2009.978098	316396.693344	38.030452
2012.007864	316901.856295	38.035469
2014.120219	317401.544388	38.040487
2015.920850	317902.113057	38.045504
2017.891251	318392.016471	38.050522
2019.534403	318890.035415	38.055540
2021.704890	319392.635425	38.060557
2023.483072	319900.188579	38.065575
2025.143511	320416.534225	38.070592
2026.390314	320932.430847	38.075610
2028.097076	321463.068408	38.080628
2029.988134	321995.979603	38.085645
2031.625873	322530.598409	38.090663
2033.041126	323091.355337	38.095680
2035.054936	323647.595999	38.100698
2037.058140	324207.357773	38.105716
2038.555785	324779.547799	38.110733
2040.188346	325352.393785	38.115751
2042.221308	325951.429613	38.120768
2044.348666	326533.087257	38.125786
2046.387022	327132.256929	38.130804
2048.245209	327742.583841	38.135821
2050.251508	328342.349245	38.140839
2052.493573	328952.293005	38.145856
2054.690452	329559.189933	38.150874
2056.832242	330170.728717	38.155892
2058.479695	330788.601446	38.160909
2060.956474	331390.681854	38.165927
2063.236693	332007.700298	38.170944
2065.682349	332631.050287	38.175962
2067.845166	333240.202957	38.180980
2070.133493	333852.446331	38.185997
2072.657378	334461.497347	38.191015
2074.573769	335083.697211	38.196032
2076.935311	335686.462649	38.201050
2079.067017	336300.998497	38.206068
2080.817367	336921.722095	38.211085
2083.214462	337540.558399	38.216103
2085.190704	338157.573013	38.221120
2087.176771	338770.136834	38.226138
2089.573169	339394.876569	38.231156
2091.419970	340024.637135	38.236173
2093.649870	340637.079999	38.241191
2095.466761	341268.750644	38.246208
2097.619099	341901.371899	38.251226
2099.897632	342524.933329	38.256244
2101.765690	343160.898475	38.261261
2104.077211	343793.916802	38.266279
2106.320705	344416.739431	38.271296
2108.811151	345050.467317	38.276314
2111.239748	345668.571952	38.281332
2112.994047	346301.149013	38.286349
2115.400907	346920.425924	38.291367
2117.806019	347549.327487	38.296384
2119.666741	348184.793720	38.301402
2122.053947	348802.010098	38.306420
2123.841420	349425.622388	38.311437
2125.725575	350056.788994	38.316455
2128.427488	350680.310333	38.321472
2130.393903	351314.177998	38.326490
2132.804754	351939.825010	38.331508
2134.866251	352563.739725	38.336525
2136.716335	353178.446794	38.341543
2139.057167	353810.964142	38.346560
2141.038164	354430.646262	38.351578
2143.556508	355056.367202	38.356596
2145.312582	355685.237022	38.361613
2148.078143	356307.649277	38.366631
2150.039566	356919.933407	38.371648
2152.398531	357520.887981	38.376666
2154.521128	358111.423948	38.381684
2156.422463	358711.539554	38.386701
2158.665965	359296.786505	38.391719
2160.661605	359894.582657	38.396736
2162.642408	360480.532184	38.401754
2164.531896	361078.549563	38.406772
2166.910327	361685.146863	38.411789
2168.952063	362305.268326	38.416807
2170.832532	362906.748088	38.421824
2172.487467	363524.572755	38.426842
2174.715832	364154.383805	38.431860
2176.375118	364773.980881	38.436877
2178.766838	365405.437380	38.441895
2180.851686	366048.762997	38.446912
2182.782101	366695.266148	38.451930
2184.859684	367335.903245	38.456948
2186.966704	367987.873976	38.461965
2189.149521	368632.950758	38.466983
2191.286788	369303.359424	38.472000
2193.511444	369951.490967	38.477018
2195.776439	370616.881922	38.482036
2197.591301	371286.964234	38.487053
2200.313802	371946.094826	38.492071
2202.810076	372609.070908	38.497088
2204.954462	373288.985072	38.502106
2207.672925	373961.622711	38.507124
2209.440298	374638.598095	38.512141
2211.851742	375302.586219	38.517159
2214.004348	375979.290520	38.522176
2216.048319	376669.750441	38.527194
2218.290736	377344.531684	38.532212
2220.392468	378026.132006	38.537229
2222.700360	378718.220160	38.542247
2225.194638	379400.584961	38.547264
2227.761006	380093.913744	38.552282
2229.688718	380769.467342	38.557300
2231.946028	381457.286650	38.562317
2234.265667	382156.525964	38.567335
2236.680448	382850.083629	38.572352
2238.933501	383538.810634	38.577370
2241.307119	384239.453818	38.582388
2243.576856	384939.992708	38.587405
2245.840813	385620.963101	38.592423
2248.168754	386318.719782	38.597440
2249.830984	387022.334801	38.602458
2252.152947	387723.497259	38.607476
2254.517410	388431.571349	38.612493
2256.104227	389128.454016	38.617511
2258.572489	389842.193983	38.622528
2260.723711	390561.026644	38.627546
2263.196753	391267.078160	38.632564
2265.502503	391991.515890	38.637581
2267.976673	392702.386570	38.642599
2270.578297	393411.444312	38.647616
2272.274674	394139.963606	38.652634
2275.096211	394852.134169	38.657652
2277.547871	395567.581506	38.662669
2279.398655	396277.734983	38.667687
2282.043040	397004.752789	38.672704
2283.973733	397722.443999	38.677722
2286.718220	398430.519813	38.682740
2288.932107	399153.893703	38.687757
2291.314012	399861.071674	38.692775
2293.796745	400572.919646	38.697792
2295.658048	401298.812617	38.702810
2297.682347	402009.017655	38.707828
2300.363439	402715.200823	38.712845
2302.473164	403403.737912	38.717863
2305.153820	404096.213527	38.722880
2307.099577	404790.402342	38.727898
2309.409046	405482.640480	38.732916
2311.687024	406175.520056	38.737933
2313.996621	406852.028611	38.742951
2316.380334	407558.916211	38.747968
2318.485223	408262.738355	38.752986
2320.871547	408962.800437	38.758004
2323.127750	409665.744596	38.763021
2324.908512	410362.719859	38.768039
2327.114065	411067.397750	38.773056
2329.612604	411791.181061	38.778074
2332.017220	412516.523175	38.783092
2334.184301	413240.259276	38.788109
2336.549509	413957.869707	38.793127
2339.016441	414687.074601	38.798144
2341.239031	415423.070874	38.803162
2343.513117	416158.426645	38.808180
2345.745792	416907.318554	38.813197
2348.257811	417654.117088	38.818215
2350.501834	418393.445824	38.823232
2352.506753	419140.321323	38.828250
2355.122884	419888.895044	38.833268
2357.488431	420648.909798	38.838285
2360.061245	421404.515337	38.843303
2362.450174	422158.655499	38.848320
2364.397736	422936.450567	38.853338
2366.694536	423699.852227	38.858356
2369.353890	424459.528181	38.863373
2371.621381	425245.274687	38.868391
2374.158813	426015.730832	38.873408
2376.645742	426783.233189	38.878426
2379.026390	427553.553731	38.883444
2381.802249	428328.585055	38.888461
2384.018920	429111.407612	38.893479
2386.681281	429882.099350	38.898496
2389.097598	430666.345498	38.903514
2391.118283	431447.690745	38.908532
2393.418386	432234.722757	38.913549
2395.737055	433021.972792	38.918567
2398.184705	433804.521359	38.923584
2400.349211	434601.080675	38.928602
2402.971810	435395.463579	38.933620
2405.503032	436185.381217	38.938637
2407.547838	436983.073158	38.943655
2410.276010	437791.134272	38.948672
2412.610568	438593.917509	38.953690
2415.197927	439390.665518	38.958708
2418.081407	440191.880278	38.963725
2419.984042	440988.061429	38.968743
2422.448174	441803.417757	38.973760
2424.874157	442610.157083	38.978778
2427.413959	443410.479111	38.983796
2430.003436	444216.466203	38.988813
2432.296171	445018.474383	38.993831
2435.103611	445828.397184	38.998848
2437.595886	446628.687441	39.003866
2440.364526	447424.455273	39.008884
2442.994596	448219.048400	39.013901
2445.639347	449009.514133	39.018919
2448.520048	449801.726003	39.023936
2450.876802	450595.045139	39.028954
2454.232367	451372.723218	39.033972
2456.995743	452148.339503	39.038989
2459.455429	452920.788853	39.044007
2462.015378	453687.080410	39.049024
2464.108862	454448.716946	39.054042
2466.558626	455192.647905	39.059060
2468.875345	455929.501426	39.064077
2471.027667	456661.251685	39.069095
2473.813369	457406.650828	39.074112
2476.111344	458155.172823	39.079130
2478.600177	458899.393277	39.084148
2480.692706	459636.477504	39.089165
2482.962068	460393.838948	39.094183
2485.227719	461140.469781	39.099200
2487.332821	461902.028710	39.104218
2489.151873	462659.713126	39.109236
2491.560483	463428.573094	39.114253
2494.022073	464211.263913	39.119271
2496.669244	464986.372359	39.124288
2498.784634	465782.312219	39.129306
2501.287293	466577.649146	39.134324
2503.777604	467372.596917	39.139341
2506.041582	468183.884402	39.144359
2508.810811	468983.351673	39.149376
2510.733774	469803.540252	39.154394
2512.840133	470625.726904	39.159412
2515.733300	471456.927352	39.164429
2517.970246	472293.987157	39.169447
2520.254476	473133.719366	39.174464
2523.099670	473976.093485	39.179482
2525.445153	474817.543827	39.184500
2527.843840	475664.588449	39.189517
2530.154611	476520.071543	39.194535
2533.073106	477377.581426	39.199552
2535.442869	478239.314798	39.204570
2537.803976	479107.152156	39.209588
2540.800890	479981.646761	39.214605
2543.363445	480858.932712	39.219623
2546.235115	481727.251385	39.224640
2548.951970	482603.306743	39.229658
2551.022121	483474.626800	39.234676
2554.548296	484348.945482	39.239693
2556.844496	485215.244624	39.244711
2560.025465	486093.750882	39.249728
2562.227087	486971.453223	39.254746
2564.617494	487842.224440	39.259764
2567.708076	488718.679849	39.264781
2570.629092	489593.297873	39.269799
2573.031581	490461.851926	39.274816
2575.949662	491341.657968	39.279834
2578.512073	492210.791337	39.284852
2581.187629	493081.115624	39.289869
2583.441708	493959.512207	39.294887
2585.756318	494821.935758	39.299904
2588.469778	495699.150650	39.304922
2591.063971	496590.177800	39.309940
2593.812460	497458.270481	39.314957
2596.753150	498341.333987	39.319975
2599.298493	499215.747821	39.324992
2602.049925	500086.905890	39.330010
2604.437657	500964.209254	39.335028
2607.005268	501829.050322	39.340045
2609.844256	502724.144110	39.345063
2612.233216	503595.751615	39.350080
2614.976587	504475.654280	39.355098
2617.669053	505361.096012	39.360116
2620.221224	506256.366277	39.365133
2622.431095	507135.735431	39.370151
2625.228751	508011.587455	39.375168
2627.743766	508903.275343	39.380186
2629.917705	509804.366464	39.385204
2632.710587	510692.627755	39.390221
2635.292947	511578.350788	39.395239
2637.942062	512445.248211	39.400256
2640.850534	513309.234806	39.405274
2643.276615	514172.639513	39.410292
2645.824778	515028.981862	39.415309
2648.278949	515891.922513	39.420327
2650.905897	516760.161429	39.425344
2653.478376	517623.678357	39.430362
2656.061446	518499.957749	39.435380
2658.910612	519366.839719	39.440397
2661.350169	520241.169264	39.445415
2664.211308	521111.204701	39.450432
2667.123996	522000.675506	39.455450
2669.958401	522871.405319	39.460468
2672.932769	523756.679399	39.465485
2675.530815	524649.641351	39.470503
2677.964757	525528.752058	39.475520
2680.717400	526412.276250	39.480538
2683.459398	527299.812225	39.485556
2685.856918	528187.744157	39.490573
2688.285641	529090.629950	39.495591
2691.028502	529996.669086	39.500608
2693.444201	530910.129495	39.505626
2696.318654	531829.329711	39.510644
2699.096457	532740.445371	39.515661
2701.557239	533675.146171	39.520679
2704.241086	534598.045713	39.525696
2707.200082	535522.241678	39.530714
2709.363721	536459.146079	39.535732
2712.245657	537398.680477	39.540749
2714.774282	538341.413182	39.545767
2717.551709	539286.044537	39.550784
2720.353938	540223.725917	39.555802
2723.070759	541177.710456	39.560820
2725.778339	542134.634751	39.565837
2728.626862	543103.355365	39.570855
2731.161004	544058.152609	39.575872
2734.070950	545022.349611	39.580890
2736.637787	545997.059621	39.585908
2739.227898	546957.443932	39.590925
2742.059372	547939.884362	39.595943
2744.811148	548909.821175	39.600960
2747.693874	549883.772791	39.605978
2750.279706	550869.577122	39.610996
2753.593026	551852.129346	39.616013
2755.919577	552836.310491	39.621031
2759.131413	553813.555535	39.626048
2762.263992	554800.007248	39.631066
2764.950610	555785.395136	39.636084
2767.842147	556764.154476	39.641101
2770.174323	557742.720604	39.646119
2773.430598	558730.683012	39.651136
2776.561121	559721.789623	39.656154
2779.081510	560712.557883	39.661172
2781.673472	561694.063782	39.666189
2784.348680	562685.543561	39.671207
2787.338180	563672.382245	39.676224
2790.305023	564655.985727	39.681242
2792.790873	565651.099984	39.686260
2795.901829	566628.203868	39.691277
2798.779596	567626.041812	39.696295
2801.271151	568616.093287	39.701312
2804.132259	569609.205844	39.706330
2806.672605	570606.988140	39.711348
2809.709768	571599.249759	39.716365
2812.430982	572590.022911	39.721383
2815.174129	573589.164072	39.726400
2817.890895	574582.066060	39.731418
2820.668891	575576.872671	39.736436
2823.763907	576534.767384	39.741453
2826.738740	577501.104065	39.746471
2829.424698	578462.149883	39.751488
2832.030136	579408.769668	39.756506
2834.517654	580378.384794	39.761524
2837.708191	581334.352091	39.766541
2840.727997	582307.716042	39.771559
2843.204385	583271.178479	39.776576
2846.252035	584239.467045	39.781594
2848.592231	585223.428892	39.786612
2851.395956	586193.032666	39.791629
2854.294548	587185.078667	39.796647
2857.000509	588176.564444	39.801664
2859.638313	589167.120586	39.806682
2862.557989	590171.184029	39.811700
2865.593866	591166.341595	39.816717
2868.607745	592184.742656	39.821735
2871.378666	593185.000355	39.826752
2874.462010	594198.552745	39.831770
2876.885330	595213.560341	39.836788
2879.418191	596227.754569	39.841805
2883.149251	597263.187595	39.846823
2885.522358	598284.999713	39.851840
2888.829120	599326.038664	39.856858
2891.318102	600364.905536	39.861876
2894.203507	601405.603969	39.866893
2897.346039	602439.869234	39.871911
2900.382939	603475.994540	39.876928
2903.635691	604504.796414	39.881946
2906.642343	605556.437730	39.886964
2909.550957	606610.381914	39.891981
2912.578765	607651.228396	39.896999
2915.298224	608697.654112	39.902016
2918.451243	609747.396266	39.907034
2921.128729	610803.189026	39.912052
2923.887492	611854.770129	39.917069
2927.226868	612925.148764	39.922087
2929.583717	613992.974916	39.927104
2932.973829	615058.631810	39.932122
2935.579625	616126.989825	39.937140
2939.003895	617196.750495	39.942157
2941.857559	618261.751201	39.947175
2944.295616	619348.478695	39.952192
2947.341019	620422.386383	39.957210
2950.113077	621510.020107	39.962228
2953.411862	622594.811269	39.967245
2956.297227	623676.060676	39.972263
2959.713301	624767.416941	39.977280
2963.156715	625835.540943	39.982298
2965.892156	626923.027518	39.987316
2969.053285	627995.887667	39.992333
2972.432020	629078.949275	39.997351
2975.270233	630156.896765	40.002368
2978.193869	631239.786646	40.007386
2981.086975	632324.698929	40.012404
2984.618529	633394.858891	40.017421
2987.268243	634469.265645	40.022439
2990.340114	635558.807151	40.027456
2993.324402	636634.011121	40.032474
2995.860847	637715.180887	40.037492
2998.671748	638803.344903	40.042509
3001.803339	639899.139535	40.047527
3004.406942	640994.142848	40.052544
3007.725984	642075.384191	40.057562
3010.623373	643170.185687	40.062580
3013.360941	644262.000544	40.067597
3016.527611	645359.533383	40.072615
3019.010412	646452.173235	40.077632
3022.238738	647522.308812	40.082650
3025.093914	648602.015524	40.087668
3027.803910	649659.861459	40.092685
3030.632212	650732.615218	40.097703
3033.232935	651814.316387	40.102720
3036.138081	652893.656391	40.107738
3038.921821	653980.135428	40.112756
3041.628618	655096.181842	40.117773
3044.660247	656197.793685	40.122791
3046.947965	657312.588284	40.127808
3050.380726	658436.096618	40.132826
3053.182895	659553.211174	40.137844
3056.530546	660684.487533	40.142861
3059.370733	661824.975182	40.147879
3062.488208	662960.907920	40.152896
3065.843978	664105.038266	40.157914
3069.473499	665255.224847	40.162932
3072.365038	666399.624911	40.167949
3075.874317	667555.626547	40.172967
3078.439211	668700.024277	40.177984
3081.646093	669858.890235	40.183002
3084.452722	671020.389360	40.188020
3087.554441	672189.663291	40.193037
3090.828407	673362.665363	40.198055
3094.241620	674546.234176	40.203072
3097.440194	675711.893489	40.208090
3100.319810	676901.163220	40.213108
3103.624146	678073.119047	40.218125
3106.659044	679261.886099	40.223143
3109.656240	680459.154432	40.228160
3112.774806	681652.274864	40.233178
3115.804177	682847.219621	40.238196
3118.414762	684044.286323	40.243213
3122.047825	685254.972542	40.248231
3125.002118	686466.380728	40.253248
3128.096230	687681.151574	40.258266
3131.283369	688906.707557	40.263284
3134.270093	690119.753217	40.268301
3137.487692	691340.345505	40.273319
3140.799417	692580.858361	40.278336
3144.263476	693801.491216	40.283354
3147.442353	695027.668745	40.288372
3150.621360	696260.677187	40.293389
3153.601827	697486.959974	40.298407
3156.853631	698730.449033	40.303424
3160.275660	699947.893834	40.308442
3163.214814	701197.964883	40.313460
3166.580071	702430.842329	40.318477
3169.880426	703669.167009	40.323495
3172.968588	704912.366625	40.328512
3176.478955	706143.611883	40.333530
3179.903662	707400.925921	40.338548
3183.063480	708622.220661	40.343565
3186.544963	709862.905432	40.348583
3189.666486	711107.938279	40.353600
3192.883175	712350.835861	40.358618
3195.671799	713587.095830	40.363636
3199.292034	714822.487733	40.368653
3202.710643	716051.160622	40.373671
3205.743860	717294.924446	40.378688
3208.938562	718527.575483	40.383706
3212.817648	719764.848212	40.388724
3215.761534	720980.398426	40.393741
3219.445158	722196.132731	40.398759
3222.519244	723431.068560	40.403776
3225.631979	724648.913994	40.408794
3228.541715	725881.853577	40.413812
3231.732538	727094.421995	40.418829
3235.158919	728293.228610	40.423847
3238.108851	729475.734236	40.428864
3241.166830	730659.119122	40.433882
3244.521697	731841.090569	40.438900
3247.093002	733030.422510	40.443917
3250.506538	734218.105758	40.448935
3253.301174	735419.115460	40.453952
3256.547527	736620.892207	40.458970
3259.497886	737839.915221	40.463988
3262.881853	739057.637289	40.469005
3266.347799	740278.780065	40.474023
3269.342645	741495.422050	40.479040
3272.609957	742724.734111	40.484058
3275.883535	743953.838084	40.489076
3278.879813	745193.233897	40.494093
3282.373352	746430.426126	40.499111
3285.717758	747681.170520	40.504128
3288.868216	748922.700621	40.509146
3292.412743	750181.173497	40.514164
3295.556355	751452.338665	40.519181
3299.017577	752699.984189	40.524199
3302.205062	753981.235858	40.529216
3305.243484	755263.652720	40.534234
3308.596317	756540.299329	40.539252
3311.581359	757830.395940	40.544269
3314.623115	759112.604733	40.549287
3318.003290	760420.342088	40.554304
3321.370611	761715.593704	40.559322
3324.895017	763019.199096	40.564340
3327.961926	764334.382197	40.569357
3331.676179	765650.683877	40.574375
3334.668350	766970.959469	40.579392
3338.313418	768290.000219	40.584410
3341.523430	769626.223312	40.589428
3344.680251	770949.576104	40.594445
3348.057182	772293.813259	40.599463
3351.257879	773634.244556	40.604480
3354.686100	774978.140596	40.609498
3358.426517	776325.240885	40.614516
3361.273557	777686.676288	40.619533
3365.142006	779033.363953	40.624551
3368.024639	780395.321974	40.629568
3371.317202	781758.502464	40.634586
3374.642123	783127.698606	40.639604
3377.808350	784503.277381	40.644621
3381.513576	785872.143407	40.649639
3384.688432	787253.398572	40.654656
3387.617069	788644.355621	40.659674
3391.361823	790035.721115	40.664692
3394.406696	791425.438984	40.669709
3397.988575	792823.846319	40.674727
3401.049348	794227.348935	40.679744
3404.213199	795630.533473	40.684762
3408.107977	797053.860697	40.689780
3411.206440	798452.986440	40.694797
3414.606011	799867.199736	40.699815
3418.147216	801278.987045	40.704832
3421.482891	802695.753454	40.709850
3425.173883	804117.747680	40.714868
3428.965755	805522.964110	40.719885
3432.925046	806941.367548	40.724903
3436.148503	808346.049034	40.729920
3439.443766	809754.589298	40.734938
3442.853327	811164.839193	40.739956
3446.053945	812578.985548	40.744973
3449.668382	813991.290939	40.749991
3452.955241	815410.227084	40.755008
3455.728676	816807.910349	40.760013
3459.556214	818181.943719	40.765018
3462.593460	819493.302542	40.770023
3466.070018	820754.874932	40.775028
3469.220574	821969.242833	40.780032
3472.191217	823109.073439	40.785037
3475.026607	824170.704458	40.790042
3478.098224	825189.226321	40.795047
3480.811101	826156.001783	40.800052
3482.998951	827049.497594	40.805056
3485.670326	827886.988639	40.810061
3488.039441	828653.263428	40.815066
3489.630860	829373.302726	40.820071
3491.898618	830035.526089	40.825076
3493.441299	830655.523549	40.830080
3495.241826	831214.500373	40.835085
3497.533561	831733.615246	40.840090
3498.734681	832210.599998	40.845095
3500.810176	832627.187753	40.850100
3502.205365	833008.110196	40.855104
3503.223165	833347.305176	40.860109
3504.334828	833649.173472	40.865114
3505.694106	833916.610043	40.870119
3506.733690	834144.949808	40.875124
3507.766576	834351.724479	40.880128
3508.765309	834521.015690	40.885133
3509.609706	834670.226441	40.890138
3510.421797	834798.368171	40.895143
3511.229847	834877.765146	40.900148
3511.961042	834944.744779	40.905152
3512.249035	834996.646083	40.910157
3512.761703	835011.907067	40.915162
3513.374983	835029.676750	40.920167
3514.278961	835008.174614	40.925172
3514.453694	834988.437021	40.930176
3514.760266	834939.355745	40.935181
3515.097103	834881.336400	40.940186
3515.357907	834810.996899	40.945191
3515.997445	834721.177439	40.950196
3516.454270	834628.666363	40.955200
3516.046347	834527.355576	40.960205
3516.494616	834407.362231	40.965210
3516.842177	834283.303746	40.970215
3516.922830	834146.563144	40.975220
3516.958984	834010.506166	40.980224
3516.818593	833866.413279	40.985229
3517.361548	833709.196565	40.990234
3517.549470	833545.912761	40.995239
3517.606272	833372.932872	41.000244
3517.705150	833213.733082	41.005248
3518.055872	833027.391294	41.010253
3518.213341	832843.696467	41.015258
3518.138883	832654.301440	41.020263
3517.859803	832452.693268	41.025268
3518.087334	832257.410374	41.030272
3518.004772	832052.746782	41.035277
3518.256502	831857.155724	41.040282
3517.989095	831650.564467	41.045287
3517.861800	831440.932504	41.050292
3518.061996	831234.739691	41.055296
3517.886905	831028.015555	41.060301
3518.059319	830809.181843	41.065306
3517.981446	830602.136463	41.070311
3517.363260	830371.361881	41.075316
3517.499103	830166.211578	41.080320
3517.394620	829950.305296	41.085325
3517.704441	829733.840657	41.090330
3517.600937	829520.348410	41.095335
3517.440455	829287.906066	41.100340
3517.501939	829083.702632	41.105344
3517.076309	828864.794999	41.110349
3517.389696	828640.320882	41.115354
3516.624299	828427.671247	41.120359
3516.703679	828209.535863	41.125364
3516.772812	827994.407706	41.130368
3516.824604	827781.607727	41.135373
3516.487853	827565.944602	41.140378
3516.371563	827354.419756	41.145383
3516.632023	827135.245386	41.150388
3516.352271	826914.008628	41.155392
3516.212093	826699.548029	41.160397
3515.667002	826483.490241	41.165402
3515.578126	826287.092260	41.170407
3515.571652	826073.658348	41.175412
3515.547735	825875.875647	41.180416
3515.655579	825661.145312	41.185421
3515.505947	825454.227565	41.190426
3515.210870	825248.784329	41.195431
3515.422141	825053.661313	41.200436
3515.290009	824847.595606	41.205440
3514.739465	824634.585546	41.210445
3514.974993	824430.296291	41.215450
3514.709610	824236.291658	41.220455
3514.633888	824038.944026	41.225460
3514.406015	823846.866625	41.230464
3514.512667	823651.131665	41.235469
3514.356459	823452.999551	41.240474
3514.179312	823261.771430	41.245479
3514.277430	823056.874231	41.250484
3514.151057	822863.777342	41.255488
3513.639884	822676.961263	41.260493
3513.617612	822497.749416	41.265498
3513.240085	822315.571639	41.270503
3513.252999	822125.446038	41.275508
3513.073284	821954.221670	41.280512
3513.086199	821771.091009	41.285517
3513.026775	821595.361748	41.290522
3512.491911	821418.339424	41.295527
3512.791247	821246.436629	41.300532
3512.721095	821071.180680	41.305536
3512.537220	820897.786623	41.310541
3512.472663	820718.334992	41.315546
3511.966172	820554.519411	41.320551
3511.797361	820385.974921	41.325556
3511.968686	820234.016297	41.330560
3512.011627	820073.021990	41.335565
3512.171858	819893.413929	41.340570
3511.491652	819740.408249	41.345575
3511.647254	819578.799435	41.350580
3511.856292	819420.487741	41.355584
3511.455764	819264.214215	41.360589
3511.349150	819098.058566	41.365594
3510.873274	818949.966191	41.370599
3510.984713	818803.238768	41.375604
3510.864776	818654.986349	41.380608
3510.893198	818507.291343	41.385613
3511.100637	818357.422905	41.390618
3510.713667	818211.635645	41.395623
3510.845436	818051.353813	41.400628
3510.677808	817899.683013	41.405632
3510.591053	817758.511830	41.410637
3510.559640	817608.954776	41.415642
3510.040049	817474.855608	41.420647
3510.454386	817331.746286	41.425652
3509.910819	817181.772130	41.430656
3510.028244	817043.182014	41.435661
3509.756993	816908.155369	41.440666
3509.865182	816776.669736	41.445671
3509.736274	816636.745683	41.450676
3509.508199	816513.292824	41.455680
3509.502815	816383.374872	41.460685
3509.648222	816250.898408	41.465690
3509.172172	816118.905858	41.470695
3509.172816	815989.173538	41.475700
3509.283248	815859.323956	41.480704
3508.690841	815741.464535	41.485709
3509.026910	815618.490171	41.490714
3508.965408	815503.757578	41.495719
3508.912384	815371.196044	41.500724
3508.854525	815258.796154	41.505728
3508.164831	815137.044155	41.510733
3508.621257	815030.404414	41.515738
3508.486597	814920.348339	41.520743
3508.376816	814806.000130	41.525748
3508.525724	814682.257268	41.530752
3508.098724	814575.455612	41.535757
3508.226986	814453.659848	41.540762
3507.951588	814354.039903	41.545767
3508.258747	814243.415731	41.550772
3507.992736	814137.263398	41.555776
3507.792119	814025.350777	41.560781
3507.697020	813908.743018	41.565786
3507.786908	813823.477157	41.570791
3507.760676	813718.644281	41.575796
3507.959267	813610.071989	41.580800
3507.299440	813508.160240	41.585805
3507.652848	813399.462662	41.590810
3507.246149	813304.523561	41.595815
3507.299881	813198.889975	41.600820
3506.962063	813106.080803	41.605824
3507.037939	813006.871726	41.610829
3507.320223	812904.900337	41.615834
3507.278432	812815.451187	41.620839
3507.039339	812714.045435	41.625844
3507.193896	812625.342472	41.630848
3506.944683	812535.434506	41.635853
3507.492589	812434.680829	41.640858
3507.171677	812344.781342	41.645863
3506.601912	812251.605971	41.650868
3506.914308	812156.732000	41.655872
3506.366890	812064.330015	41.660877
3506.649006	811980.178562	41.665882
3506.299427	811897.781574	41.670887
3506.190025	811808.036263	41.675892
3506.546021	811728.255711	41.680896
3506.339025	811640.472544	41.685901
3506.487646	811561.891884	41.690906
3506.559284	811477.279277	41.695911
3505.833491	811389.281299	41.700916
3505.958545	811315.867115	41.705920
3506.027125	811230.374435	41.710925
3506.101183	811151.410421	41.715930
3505.606829	811083.158938	41.720935
3505.623569	811003.422237	41.725940
3505.916369	810925.006043	41.730944
3505.723395	810851.148777	41.735949
3505.791467	810780.661589	41.740954
3505.784478	810716.034125	41.745959
3505.620980	810648.798488	41.750964
3505.596239	810568.965295	41.755968
3505.888110	810495.028064	41.760973
3505.648931	810427.899384	41.765978
3505.496814	810353.639965	41.770983
3505.527767	810288.319790	41.775988
3505.495547	810208.580692	41.780992
3505.220375	810141.747054	41.785997
3505.357579	810068.511424	41.791002
3504.995145	810012.706374	41.796007
3505.054675	809940.066339	41.801012
3504.966354	809886.849597	41.806016
3505.062890	809819.759458	41.811021
3504.757304	809756.923727	41.816026
3504.879588	809689.048219	41.821031
3504.743181	809634.081945	41.826036
3505.136214	809574.645058	41.831040
3504.790992	809511.520589	41.836045
3504.839000	809446.189036	41.841050
3504.769385	809391.405209	41.846055
3504.606179	809328.835461	41.851060
3504.532235	809277.463857	41.856064
3504.421955	809227.072541	41.861069
3504.758459	809160.912922	41.866074
3504.783660	809109.719464	41.871079
3504.356919	809053.135947	41.876084
3504.323063	808995.905471	41.881088
3504.179912	808937.813998	41.886093
3504.385959	808888.638128	41.891098
3504.276454	808840.193763	41.896103
3504.128720	808792.145041	41.901108
3504.053589	808740.525487	41.906112
3504.071503	808690.792429	41.911117
3504.370943	808651.546217	41.916122
3503.944072	808601.345672	41.921127
3503.734731	808547.112691	41.926132
3503.945887	808506.953009	41.931136
3503.669736	808463.066192	41.936141
3503.930529	808413.683048	41.941146
3503.768651	808371.191699	41.946151
3503.918334	808318.460887	41.951156
3504.113573	808269.915762	41.956160
3504.029690	808236.675457	41.961165
3503.883203	808185.257566	41.966170
3503.733159	808140.081054	41.971175
3503.545465	808096.762985	41.976180
3503.757813	808055.966381	41.981184
3503.760021	808015.787492	41.986189
3503.482832	807969.605666	41.991194
3503.415068	807940.847296	41.996199
3503.663091	807889.901712	42.001204
3503.507457	807859.401291	42.006208
3503.136304	807823.668110	42.011213
3503.215630	807781.378910	42.016218
3503.253718	807750.750159	42.021223
3503.280152	807704.957805	42.026228
3503.386982	807670.611932	42.031232
3503.334196	807633.755120	42.036237
3503.423166	807603.654104	42.041242
3503.289858	807571.344547	42.046247
3503.321945	807529.109814	42.051252
3503.059698	807494.137979	42.056256
3503.074459	807456.830699	42.061261
3503.846793	807414.284427	42.066266
3503.336228	807390.713129	42.071271
3503.115197	807356.368042	42.076276
3503.387496	807324.188884	42.081280
3503.207091	807293.397017	42.086285
3503.425015	807246.693633	42.091290
3503.188240	807214.983633	42.096295
3503.199704	807174.651670	42.101300
3503.028904	807138.639471	42.106304
3503.138497	807107.508765	42.111309
3503.481245	807069.075048	42.116314
3503.402096	807038.607492	42.121319
3503.149205	807001.534449	42.126324
3503.442816	806964.326991	42.131328
3503.137310	806931.065718	42.136333
3502.995024	806895.730449	42.141338
3503.031279	806871.388969	42.146343
3502.822811	806834.649392	42.151348
3502.766821	806810.322098	42.156352
3502.752509	806774.332140	42.161357
3502.918218	806749.872418	42.166362
3502.612663	806729.826846	42.171367
3502.676743	806710.162364	42.176372
3502.765103	806669.912717	42.181376
3502.523110	806649.515559	42.186381
3502.954063	806627.013517	42.191386
3502.812912	806594.651442	42.196391
3503.053945	806567.301723	42.201396
3502.804302	806534.224725	42.206400
3502.303645	806502.211010	42.211405
3502.480942	806476.431575	42.216410
3502.603648	806459.293320	42.221415
3502.552059	806433.159309	42.226420
3502.673606	806412.216831	42.231424
3502.288050	806391.304782	42.236429
3502.371146	806360.711066	42.241434
3502.491295	806334.696124	42.246439
3502.483074	806324.991545	42.251444
3502.393811	806300.765049	42.256448
3502.644319	806271.949367	42.261453
3502.496730	806241.098493	42.266458
3502.484576	806219.152021	42.271463
3502.165888	806196.521773	42.276468
3502.283156	806178.017922	42.281472
3502.477480	806152.283288	42.286477
3502.254386	806130.808460	42.291482
3502.223592	806126.033388	42.296487
3502.479994	806112.531434	42.301492
3502.318105	806079.682228	42.306496
3502.035708	806078.019305	42.311501
3502.493427	806043.073257	42.316506
3502.190657	806027.951382	42.321511
3502.624746	806003.544391	42.326516
3502.351254	805994.563641	42.331520
3501.891733	805966.833093	42.336525
3502.112483	805952.068187	42.341530
3502.543150	805926.637132	42.346535
3502.812116	805909.864749	42.351540
3502.046771	805890.522498	42.356544
3502.220315	805871.374860	42.361549
3502.515443	805829.380378	42.366554
3502.469596	805822.363671	42.371559
3502.662971	805797.652080	42.376564
3502.170704	805773.340241	42.381568
3502.170968	805759.780024	42.386573
3502.297567	805727.859464	42.391578
3502.298572	805719.810977	42.396583
3502.111051	805691.890376	42.401588
3502.324240	805680.881964	42.406592
3502.252003	805656.699133	42.411597
3502.591306	805640.012603	42.416602
3502.382057	805618.826555	42.421607
3502.210497	805588.707950	42.426612
3502.351066	805577.808271	42.431616
3502.134021	805556.476896	42.436621
3502.314444	805534.936977	42.441626
3502.316345	805528.595397	42.446631
3502.302747	805500.793108	42.451636
3502.223993	805492.269004	42.456640
3502.090065	805469.070703	42.461645
3501.959628	805448.505910	42.466650
3501.838153	805439.744511	42.471655
3501.922923	805422.414277	42.476660
3502.109207	805408.385209	42.481664
3502.123261	805386.480551	42.486669
3502.017845	805375.326295	42.491674
3502.069246	805356.537671	42.496679
3501.760068	805340.244416	42.501684
3502.262076	805333.873246	42.506688
3501.972651	805302.552182	42.511693
3502.108120	805302.726206	42.516698
3502.019796	805283.617740	42.521703
3501.681400	805267.182520	42.526708
3501.896461	805255.051103	42.531712
3501.689022	805239.863667	42.536717
3502.195495	805223.686519	42.541722
3501.777618	805213.214990	42.546727
3501.428724	805188.927283	42.551732
3501.708038	805182.054170	42.556736
3501.815722	805193.208560	42.561741
3501.911964	805160.802084	42.566746
3501.587669	805149.388952	42.571751
3501.664862	805154.206435	42.576756
3501.857225	805136.761040	42.581760
3502.094666	805120.089077	42.586765
3502.327586	805104.588567	42.591770
3502.057762	805084.776132	42.596775
3501.951378	805072.060437	42.601780
3502.088917	805047.110752	42.606784
3501.501155	805045.056237	42.611789
3501.817454	805029.786429	42.616794
3501.476050	805012.375350	42.621799
3501.882318	805015.629204	42.626804
3502.172523	804993.094623	42.631808
3501.853753	804976.753152	42.636813
3502.114537	804969.346084	42.641818
3501.985832	804957.560545	42.646823
3501.892592	804943.037527	42.651828
3502.235799	804929.031661	42.656832
3501.638233	804911.611565	42.661837
3501.725922	804903.304576	42.666842
3501.581416	804897.765806	42.671847
3501.677084	804872.626846	42.676852
3501.909955	804868.590171	42.681856
3501.863997	804867.914443	42.686861
3501.726539	804837.786957	42.691866
3501.743495	804832.808311	42.696871
3501.631324	804823.800685	42.701876
3502.006917	804804.471907	42.706880
3501.788461	804796.456562	42.711885
3501.832775	804797.962053	42.716890
3501.731481	804779.439526	42.721895
3501.693939	804761.931476	42.726900
3501.685845	804761.591318	42.731904
3501.812747	804747.423725	42.736909
3501.702156	804726.511999	42.741914
3501.940112	804718.425209	42.746919
3501.668352	804706.856712	42.751924
3501.882823	804687.162478	42.756928
3501.835999	804693.463281	42.761933
3502.161013	804669.507322	42.766938
3502.070996	804658.154258	42.771943
3501.928134	804644.955549	42.776948
3501.791441	804621.169156	42.781952
3501.420659	804621.422339	42.786957
3501.525783	804614.966141	42.791962
3501.881397	804602.372435	42.796967
3501.953646	804590.847525	42.801972
3501.825097	804574.377711	42.806977
3501.743285	804554.485449	42.811981
3501.994649	804545.810900	42.816986
3502.068741	804535.846793	42.821991
3501.702553	804523.414552	42.826996
3501.749557	804505.551071	42.832001
3502.121513	804495.247613	42.837005
3501.687182	804479.215655	42.842010
3501.309864	804481.177433	42.847015
3501.445067	804469.642463	42.852020
3501.766434	804468.714121	42.857025
3501.469369	804456.173368	42.862029
3501.531785	804443.332455	42.867034
3501.550090	804443.524821	42.872039
3501.669838	804435.797668	42.877044
3501.970666	804409.502690	42.882049
3501.549275	804406.934070	42.887053
3501.481674	804397.089474	42.892058
3501.601157	804398.632098	42.897063
3501.322808	804380.136089	42.902068
3501.792712	804370.646524	42.907073
3501.864188	804368.537517	42.912077
3501.736349	804349.773950	42.917082
3501.713681	804349.728779	42.922087
3501.440622	804344.258412	42.927092
3501.419440	804342.115092	42.932097
3501.398329	804330.213996	42.937101
3501.378863	804310.652750	42.942106
3501.445381	804309.715436	42.947111
3501.565092	804307.306135	42.952116
3501.495970	804303.999359	42.957121
3501.248690	804294.182691	42.962125
3501.523649	804268.915751	42.967130
3501.625817	804270.119588	42.972135
3501.230949	804256.471575	42.977140
3501.591169	804269.637260	42.982145
3501.660764	804272.163500	42.987149
3501.676715	804249.961909	42.992154
3501.745823	804242.096071	42.997159
3501.431182	804248.097651	43.002164
3501.703689	804222.489384	43.007169
3501.655896	804206.249944	43.012173
3501.450526	804200.915242	43.017178
3501.361738	804215.956452	43.022183
3501.611861	804197.523671	43.027188
3501.503534	804174.706977	43.032193
3501.053094	804173.411344	43.037197
3501.248346	804167.672457	43.042202
3501.392212	804170.284708	43.047207
3501.486364	804171.782557	43.052212
3501.647791	804152.387710	43.057217
3501.572215	804146.252028	43.062221
3501.541069	804136.059798	43.067226
3501.557721	804136.935496	43.072231
3501.445905	804132.464337	43.077236
3501.611526	804105.554971	43.082241
3501.300264	804110.043643	43.087245
3501.504917	804103.864115	43.092250
3501.346617	804097.936481	43.097255
3501.208593	804104.788817	43.102260
3501.547356	804090.049954	43.107265
3501.157246	804078.254861	43.112269
3501.680946	804080.075911	43.117274
3501.554838	804079.705373	43.122279
3501.515121	804079.662865	43.127284
3501.427197	804056.257070	43.132289
3501.654128	804047.488084	43.137293
3501.630734	804035.781960	43.142298
3501.432135	804043.131743	43.147303
3501.249221	804031.352965	43.152308
3501.459289	804015.219104	43.157313
3501.599453	804011.245174	43.162317
3501.369272	804001.327799	43.167322
3501.438639	804007.806280	43.172327
3501.612804	804004.900440	43.177332
3501.899162	803987.437217	43.182337
3501.505401	803978.569999	43.187341
3501.576594	803972.655165	43.192346
3501.515034	803965.590078	43.197351
3501.219530	803950.803669	43.202356
3501.269799	803950.015217	43.207361
3501.100735	803946.382337	43.212365
3501.209494	803943.145152	43.217370
3501.274000	803951.478538	43.222375
3501.414992	803946.723771	43.227380
3501.729234	803939.063199	43.232385
3501.567878	803931.379381	43.237389
3501.555415	803918.793080	43.242394
3501.693610	803916.136783	43.247399
3501.303164	803902.389736	43.252404
3501.443048	803893.731732	43.257409
3501.412842	803886.905617	43.262413
3501.910954	803883.949084	43.267418
3501.581129	803880.975596	43.272423
3501.637793	803866.524278	43.277428
3501.520522	803846.732940	43.282433
3501.223663	803851.268333	43.287437
3501.281275	803847.160829	43.292442
3501.541332	803849.950219	43.297447
3501.393208	803833.286382	43.302452
3501.303861	803827.591681	43.307457
3501.205760	803836.780112	43.312461
3501.212326	803829.850603	43.317466
3501.559862	803823.794848	43.322471
3501.441927	803828.936593	43.327476
3501.460101	803811.905156	43.332481
3501.356816	803804.358485	43.337485
3501.482900	803797.946981	43.342490
3501.098919	803803.618264	43.347495
3501.499955	803799.847388	43.352500
3501.646415	803783.283750	43.357505
3501.388187	803770.881955	43.362509
3501.359856	803762.054896	43.367514
3501.403387	803766.000414	43.372519
3501.414980	803769.999715	43.377524
3501.524941	803761.736555	43.382529
3501.393211	803735.018492	43.387533
3501.368114	803735.461631	43.392538
3501.287235	803732.937091	43.397543
3501.731987	803730.037623	43.402548
3501.709264	803722.234294	43.407553
3501.508050	803715.581110	43.412557
3501.408692	803701.056222	43.417562
3501.419689	803700.127498	43.422567
3501.421940	803700.078427	43.427572
3501.710921	803693.104623	43.432577
3501.430768	803678.217595	43.437581
3501.329063	803670.133786	43.442586
3501.511912	803671.715476	43.447591
3501.428142	803669.728096	43.452596
3501.683043	803643.485945	43.457601
3501.324855	803638.662601	43.462605
3501.449133	803635.861982	43.467610
3501.529714	803634.775988	43.472615
3501.563498	803642.480256	43.477620
3501.746395	803612.492086	43.482625
3501.776166	803611.609209	43.487629
3501.580272	803604.808695	43.492634
3501.564692	803595.833029	43.497639
3501.385101	803586.151072	43.502644
3501.378983	803571.367341	43.507649
3501.336035	803571.666897	43.512653
3501.458194	803571.355108	43.517658
3501.536187	803565.829193	43.522663
3501.375081	803544.531135	43.527668
3501.434509	803532.420784	43.532673
3501.471600	803537.880092	43.537677
3501.560107	803533.182019	43.542682
3501.660184	803524.578534	43.547687
3501.319192	803519.459640	43.552692
3501.482806	803500.062475	43.557697
3501.304799	803509.068686	43.562701
3501.421405	803505.000536	43.567706
3501.524101	803498.153231	43.572711
3501.583224	803491.898274	43.577716
3501.473288	803472.299810	43.582721
3501.116581	803478.503864	43.587725
3501.558128	803475.019240	43.592730
3501.596915	803471.841550	43.597735
3501.316493	803457.490799	43.602740
3501.490599	803448.582866	43.607745
3501.317844	803444.462320	43.612749
3501.526599	803439.696585	43.617754
3501.570970	803437.591510	43.622759
3501.568750	803428.125565	43.627764
3501.519481	803409.590931	43.632769
3501.452338	803411.943704	43.637773
3501.616361	803415.333849	43.642778
3501.543493	803403.780689	43.647783
3501.332036	803394.884158	43.652788
3501.363417	803380.289307	43.657793
3501.551173	803381.675119	43.662797
3501.588046	803365.713085	43.667802
3501.286442	803374.494825	43.672807
3501.194443	803360.114400	43.677812
3501.485625	803346.113210	43.682817
3501.568813	803341.562217	43.687821
3501.305796	803342.237760	43.692826
3501.507010	803342.059992	43.697831
3501.307332	803343.701561	43.702836
3501.625860	803320.473517	43.707841
3501.291882	803328.430838	43.712845
3501.611166	803324.672467	43.717850
3501.083581	803327.292434	43.722855
3501.177191	803321.129512	43.727860
3501.339760	803323.056036	43.732865
3501.475333	803309.030293	43.737869
3501.581728	803278.174178	43.742874
3501.870402	803288.425262	43.747879
3501.020388	803296.804867	43.752884
3501.404408	803288.595850	43.757889
3501.191842	803265.304237	43.762893
3501.536749	803251.392036	43.767898
3501.196888	803251.006065	43.772903
3501.078171	803258.588243	43.777908
3501.298139	803246.257067	43.782913
3501.252419	803258.219574	43.787917
3501.509206	803246.565802	43.792922
3501.627774	803234.201657	43.797927
3501.071307	803228.140266	43.802932
3501.320590	803226.247076	43.807937
3501.265562	803230.598710	43.812941
3501.730848	803222.474499	43.817946
3501.609176	803226.348580	43.822951
3501.336175	803206.774794	43.827956
3501.479792	803190.649246	43.832961
3501.737008	803203.491653	43.837965
3501.531085	803185.273644	43.842970
3501.669820	803169.295198	43.847975
3501.320245	803158.614412	43.852980
3501.214193	803150.481827	43.857985
3501.303599	803145.734532	43.862989
3501.393639	803160.701468	43.867994
3501.716782	803157.967150	43.872999
3501.325976	803132.702207	43.878004
3501.422834	803129.661664	43.883009
3501.509574	803132.868848	43.888013
3501.254702	803129.492904	43.893018
3501.557394	803137.936512	43.898023
3501.488303	803121.453657	43.903028
3501.613826	803095.180688	43.908033
3501.380245	803095.558864	43.913037
3501.415035	803088.136158	43.918042
3501.484902	803088.369303	43.923047
3501.213599	803069.770798	43.928052
3501.606660	803059.217748	43.933057
3501.456569	803063.974743	43.938061
3501.742565	803055.975947	43.943066
3501.955675	803047.744542	43.948071
3501.657625	803031.931630	43.953076
3501.502945	803025.758438	43.958081
3501.436255	803031.575994	43.963085
3501.412952	803012.694561	43.968090
3501.359168	802993.573842	43.973095
3501.433751	802992.244684	43.978100
3501.524448	802985.789101	43.983105
3501.348715	802998.992394	43.988109
3501.323010	802989.285476	43.993114
3501.339355	802975.912031	43.998119
3501.074821	802970.878340	44.003124
3501.435069	802960.379057	44.008129
3501.398727	802960.580010	44.013133
3501.421288	802968.872435	44.018138
3501.430050	802968.041553	44.023143
3501.381688	802957.313344	44.028148
3501.837248	802943.285581	44.033153
3501.327945	802938.192528	44.038157
3501.533515	802934.549306	44.043162
3501.380267	802939.502084	44.048167
3501.327793	802921.259335	44.053172
3501.630260	802901.301858	44.058177
3501.415604	802899.676296	44.063181
3501.181180	802897.370627	44.068186
3501.425904	802902.846820	44.073191
3501.327829	802900.617437	44.078196
3501.682043	802874.210214	44.083201
3501.210891	802871.502341	44.088205
3501.635255	802862.164075	44.093210
3501.597758	802868.172415	44.098215
3501.234362	802858.030086	44.103220
3501.336218	802846.741409	44.108225
3501.241371	802845.926707	44.113229
3501.294367	802831.815230	44.118234
3501.355898	802824.241637	44.123239
3501.166271	802838.130638	44.128244
3501.628970	802835.179168	44.133249
3501.019134	802823.074496	44.138253
3501.285727	802813.663222	44.143258
3501.183499	802811.873661	44.148263
3500.883771	802817.776640	44.153268
3501.424045	802814.422631	44.158273
3501.360472	802816.628662	44.163277
3501.383029	802816.186007	44.168282
3501.294615	802816.492705	44.173287
3501.097221	802807.446755	44.178292
3501.317255	802787.989817	44.183297
3500.942167	802781.997246	44.188301
3500.882700	802783.861041	44.193306
3501.496207	802787.913266	44.198311
3501.453610	802804.121786	44.203316
3501.511859	802787.374162	44.208321
3501.334324	802791.940446	44.213325
3501.182693	802780.544875	44.218330
3501.248307	802771.799366	44.223335
3500.997637	802758.272005	44.228340
3501.242457	802753.939333	44.233345
3501.199787	802759.802181	44.238349
3501.084362	802761.674731	44.243354
3501.310424	802760.761052	44.248359
3501.258982	802768.430894	44.253364
3501.151766	802760.005190	44.258369
3501.175264	802762.051226	44.263373
3501.393729	802758.845096	44.268378
3501.508966	802727.789746	44.273383
3501.481780	802728.038076	44.278388
3501.300568	802726.846451	44.283393
3501.019751	802726.402413	44.288397
3501.022765	802722.205121	44.293402
3501.305893	802725.186606	44.298407
3501.004832	802730.260254	44.303412
3501.389786	802737.666710	44.308417
3501.434959	802714.723211	44.313421
3501.329178	802705.174783	44.318426
3501.108673	802702.134848	44.323431
3500.749009	802706.388054	44.328436
3501.075561	802699.456103	44.333441
3500.802938	802715.847208	44.338445
3500.840749	802714.621342	44.343450
3501.182306	802710.029513	44.348455
3501.001120	802707.910657	44.353460
3501.393775	802704.286861	44.358465
3501.202784	802709.538524	44.363469
3501.384588	802700.969960	44.368474
3501.345861	802703.318550	44.373479
3500.952360	802688.690940	44.378484
3501.339261	802684.336011	44.383489
3501.037736	802679.844688	44.388493
3501.175521	802685.874600	44.393498
3501.324681	802677.896725	44.398503
3501.139680	802686.905182	44.403508
3501.081619	802679.838127	44.408513
3501.105261	802671.977469	44.413517
3501.352832	802675.257344	44.418522
3501.208364	802685.381901	44.423527
3501.148645	802670.262858	44.428532
3501.259786	802656.141905	44.433537
3501.289386	802655.600535	44.438541
3500.942587	802652.482715	44.443546
3501.324264	802648.958207	44.448551
3501.276210	802662.093432	44.453556
3501.251828	802657.607572	44.458561
3501.009120	802666.625078	44.463565
3501.355942	802664.618875	44.468570
3501.173486	802644.931611	44.473575
3501.256771	802640.184898	44.478580
3501.259890	802622.664635	44.483585
3501.375804	802623.476222	44.488589
3501.271489	802631.105691	44.493594
3501.456221	802627.172742	44.498599
3501.025703	802634.121172	44.503604
3501.123221	802639.376594	44.508609
3501.498937	802630.289606	44.513613
3501.347138	802607.864533	44.518618
3501.603095	802608.361418	44.523623
3501.160493	802610.626770	44.528628
3501.018844	802599.375722	44.533633
3501.136470	802605.506466	44.538637
3501.257391	802605.048420	44.543642
3501.329126	802605.915717	44.548647
3501.162494	802591.301222	44.553652
3501.127692	802577.056502	44.558657
3501.096629	802573.694078	44.563661
3501.270605	802568.542718	44.568666
3501.451945	802571.393780	44.573671
3501.091552	802575.354373	44.578676
3501.344260	802583.220902	44.583681
3501.192060	802576.461262	44.588685
3501.119370	802572.422113	44.593690
3501.075779	802546.905368	44.598695
3500.927353	802546.587028	44.603700
3501.289552	802542.675088	44.608705
3500.992061	802547.601914	44.613709
3500.915183	802548.443648	44.618714
3501.150242	802542.648287	44.623719
3501.135314	802546.359684	44.628724
3501.062609	802548.469629	44.633729
3501.381540	802560.278831	44.638733
3501.253024	802551.612171	44.643738
3501.425049	802559.979365	44.648743
3501.118272	802558.124104	44.653748
3501.453799	802546.359149	44.658753
3501.431964	802533.283564	44.663757
3501.158628	802522.248176	44.668762
3501.506977	802521.559362	44.673767
3500.983244	802528.717688	44.678772
3501.429627	802523.426104	44.683777
3501.603372	802523.106203	44.688781
3501.380005	802497.812576	44.693786
3501.611759	802493.384167	44.698791
3501.355608	802496.938088	44.703796
3501.391182	802496.688588	44.708801
3501.504330	802496.914990	44.713805
3501.344873	802477.565235	44.718810
3501.601997	802466.983663	44.723815
3501.550582	802473.726595	44.728820
3501.300298	802471.667264	44.733825
3501.457237	802470.861957	44.738829
3501.341617	802442.525480	44.743834
3501.116159	802428.407841	44.748839
3501.113268	802436.021687	44.753844
3501.273528	802427.700143	44.758849
3501.071333	802436.125998	44.763853
3501.296719	802443.557741	44.768858
3501.344476	802437.303532	44.773863
3501.071048	802434.320545	44.778868
3501.290250	802427.893117	44.783873
3501.012968	802411.636193	44.788877
3500.794705	802395.370002	44.793882
3501.227360	802402.671784	44.798887
3501.040755	802401.773762	44.803892
3501.301209	802389.776238	44.808897
3501.363540	802403.333971	44.813901
3501.387703	802401.426929	44.818906
3501.379192	802402.794834	44.823911
3501.238208	802398.083002	44.828916
3501.100001	802400.056824	44.833921
3501.251425	802379.682106	44.838925
3501.041925	802375.615415	44.843930
3500.941158	802371.775744	44.848935
3500.879680	802382.034217	44.853940
3501.153106	802379.063326	44.858945
3501.066924	802390.643347	44.863949
3501.194254	802391.355572	44.868954
3500.963850	802394.124667	44.873959
3500.996708	802392.313871	44.878964
3501.086992	802385.808946	44.883969
3501.154949	802392.484499	44.888973
3501.345755	802387.769596	44.893978
3501.192048	802381.400415	44.898983
3501.103391	802391.809532	44.903988
3501.505858	802388.672063	44.908993
3501.290502	802375.333586	44.913997
3501.299458	802364.497816	44.919002
3501.143246	802359.641924	44.924007
3500.724450	802360.634739	44.929012
3501.336004	802358.099021	44.934017
3501.417560	802365.553338	44.939021
3501.108379	802373.751980	44.944026
3501.312916	802365.179415	44.949031
3501.080945	802373.707614	44.954036
3500.957855	802350.691508	44.959041
3501.329591	802350.438256	44.964045
3501.218261	802345.868161	44.969050
3501.160364	802341.094494	44.974055
3501.158588	802339.484314	44.979060
3501.220586	802339.718717	44.984065
3501.494661	802339.822360	44.989069
3501.589388	802344.541617	44.994074
3501.530075	802322.491519	44.999079
3501.269183	802318.042392	45.004084
3501.184912	802302.194257	45.009089
3501.671872	802310.170917	45.014093
3501.038589	802302.998149	45.019098
3501.528094	802312.877775	45.024103
3501.279549	802304.717586	45.029108
3501.345931	802279.573021	45.034113
3501.348360	802276.546837	45.039117
3501.303507	802271.039011	45.044122
3501.630226	802265.521900	45.049127
3501.101772	802276.878435	45.054132
3501.093945	802266.386755	45.059137
3501.480263	802251.831460	45.064141
3500.990472	802243.562491	45.069146
3501.199722	802244.798779	45.074151
3500.773646	802242.864463	45.079156
3500.978193	802240.392324	45.084161
3501.036723	802248.436034	45.089165
3501.074408	802249.211094	45.094170
3501.487045	802248.463398	45.099175
3501.183136	802255.734076	45.104180
3501.205675	802252.704737	45.109185
3501.070216	802263.170183	45.114189
3500.900348	802261.147018	45.119194
3501.117079	802251.791522	45.124199
3501.231066	802256.459028	45.129204
3501.295495	802235.218966	45.134209
3501.348091	802226.279529	45.139213
3501.258429	802230.832474	45.144218
3501.759223	802222.506237	45.149223
3501.328257	802233.847608	45.154228
3501.101542	802217.875117	45.159233
3501.360746	802200.508888	45.164237
3501.052968	802191.040076	45.169242
3501.462311	802186.388474	45.174247
3501.013098	802201.002703	45.179252
3501.179928	802197.901978	45.184257
3501.481000	802202.589083	45.189261
3501.272820	802195.008104	45.194266
3501.385412	802193.721645	45.199271
3501.247718	802184.177429	45.204276
3501.630198	802159.812670	45.209281
3501.183619	802170.034070	45.214285
3501.235462	802171.343785	45.219290
3501.347467	802161.614086	45.224295
3501.007321	802169.671411	45.229300
3501.583389	802168.166080	45.234305
3501.064194	802156.631635	45.239309
3501.206407	802138.941891	45.244314
3501.516896	802136.160317	45.249319
3501.117372	802131.830342	45.254324
3501.078217	802130.665203	45.259329
3501.568323	802142.838864	45.264333
3501.120439	802130.317113	45.269338
3501.317373	802122.087053	45.274343
3501.220732	802119.613144	45.279348
3500.891978	802097.018722	45.284353
3501.004257	802104.224511	45.289357
3501.309960	802102.273371	45.294362
3501.548318	802108.239300	45.299367
3501.168599	802109.762907	45.304372
3501.451271	802110.158046	45.309377
3501.010086	802109.592613	45.314381
3501.024644	802102.415958	45.319386
3501.254062	802109.652235	45.324391
3501.270455	802086.564571	45.329396
3501.207502	802073.543282	45.334401
3501.372335	802072.687887	45.339405
3501.119387	802077.705720	45.344410
3501.568098	802073.877586	45.349415
3501.161727	802078.870595	45.354420
3501.066436	802080.691388	45.359425
3501.046691	802077.424547	45.364429
3501.146903	802063.303999	45.369434
3501.077811	802058.190228	45.374439
3501.120692	802049.447288	45.379444
3501.126211	802054.229510	45.384449
3501.432789	802051.399706	45.389453
3501.172789	802060.030314	45.394458
3501.546191	802053.822439	45.399463
3501.233294	802051.967984	45.404468
3501.395496	802054.627045	45.409473
3501.466173	802040.999127	45.414477
3501.251245	802021.559055	45.419482
3501.206376	802023.079143	45.424487
3501.268121	802027.315725	45.429492
3501.557068	802023.902988	45.434497
3501.284989	802026.093077	45.439501
3501.394198	802017.583758	45.444506
3501.549249	801994.327668	45.449511
3501.089293	801982.344387	45.454516
3501.215599	801984.228181	45.459521
3501.322124	801981.087971	45.464525
3501.261246	801993.640888	45.469530
3501.320721	801992.801952	45.474535
3501.007563	801998.463745	45.479540
3501.024242	801978.304043	45.484545
3500.781110	801971.557979	45.489549
3500.794188	801963.844525	45.494554
3500.952669	801978.315456	45.499559
3501.462827	801984.483047	45.504564
3501.245323	801965.824116	45.509569
3501.273220	801956.448903	45.514573
3501.314302	801958.297220	45.519578
3501.577013	801957.524123	45.524583
3501.055687	801953.749943	45.529588
3501.383900	801963.606518	45.534593
3501.623153	801951.172230	45.539597
3501.116857	801948.811099	45.544602
3501.267826	801936.341776	45.549607
3501.113002	801940.075392	45.554612
3501.008106	801936.626561	45.559617
3501.340439	801939.991181	45.564621
3501.154012	801945.730823	45.569626
3501.330810	801938.431009	45.574631
3501.040045	801954.387627	45.579636
3500.964634	801940.928754	45.584641
3501.213631	801926.491805	45.589645
3500.792640	801921.384127	45.594650
3501.085168	801913.431699	45.599655
3501.259286	801919.359040	45.604660
3501.276318	801923.846716	45.609665
3501.531827	801918.242827	45.614669
3501.187748	801925.422541	45.619674
3501.432905	801922.163018	45.624679
3501.012374	801927.500007	45.629684
3500.950268	801925.899154	45.634689
3501.147565	801928.308745	45.639693
3500.581401	801916.293136	45.644698
3501.291114	801917.646485	45.649703
3501.378082	801916.900856	45.654708
3501.202069	801894.818724	45.659713
3501.334661	801898.995509	45.664717
3501.133651	801898.929391	45.669722
3501.200648	801890.914576	45.674727
3500.948953	801900.422634	45.679732
3500.840011	801892.825784	45.684737
3501.104979	801902.399495	45.689741
3501.278549	801904.178309	45.694746
3501.063382	801903.577524	45.699751
3501.084777	801911.578655	45.704756
3500.995882	801899.732443	45.709761
3501.341274	801905.828253	45.714765
3501.329649	801879.327709	45.719770
3501.517802	801866.803631	45.724775
3501.499326	801881.107213	45.729780
3501.634537	801866.931955	45.734785
3501.283823	801865.522625	45.739789
3501.441895	801848.464101	45.744794
3501.445415	801836.261672	45.749799
3501.155363	801838.552250	45.754804
3501.127269	801832.748580	45.759809
3501.144431	801833.478090	45.764813
3501.040013	801813.336801	45.769818
3501.244521	801756.736145	45.774823
3500.950977	801657.602540	45.779828
3500.593855	801496.781243	45.784833
3500.738017	801299.463953	45.789837
3500.508613	801056.314213	45.794842
3500.190359	800760.057544	45.799847
3500.071325	800412.447878	45.804852
3499.561145	800013.080987	45.809857
3499.261124	799571.081199	45.814861
3498.892049	799082.723622	45.819866
3498.605964	798528.929194	45.824871
3497.925372	797945.846679	45.829876
3497.444459	797306.121467	45.834881
3496.836282	796619.313221	45.839885
3496.194610	795897.214807	45.844890
3496.034517	795107.194277	45.849895
3495.171048	794283.178024	45.854900
3494.429760	793401.028418	45.859905
3493.565514	792477.183608	45.864909
3492.402090	791508.280641	45.869914
3492.189940	790476.209448	45.874919
3490.940027	789422.426478	45.879924
3489.926188	788314.393541	45.884929
3489.374978	787155.325876	45.889933
3488.026806	785958.066158	45.894938
3487.023297	784713.166891	45.899943
3486.054840	783417.420011	45.904948
3484.890815	782077.490575	45.909953
3483.706456	780680.349619	45.914957
3482.520437	779248.096483	45.919962
3481.045578	777765.911717	45.924967
3479.418251	776246.040570	45.929972
3478.231583	774675.329755	45.934977
3477.027793	773079.454617	45.939981
3475.818184	771422.701704	45.944986
3474.164329	769734.033040	45.949991
3472.791861	768014.098106	45.954996
3471.201180	766238.516937	45.960001
3469.259684	764430.386870	45.965005
3468.010534	762573.221813	45.970010
3466.439454	760686.050052	45.975015
3464.489632	758750.535999	45.980020
3462.636715	756775.117303	45.985025
3461.316465	754774.538038	45.990029
3459.407810	752735.041637	45.995034
3457.908605	750648.474596	46.000039
3455.730195	748522.839743	46.005044
3454.154334	746358.101935	46.010049
3451.933322	744156.147243	46.015053
3449.747413	741925.159921	46.020058
3448.119409	739650.801318	46.025063
3446.079956	737356.046754	46.030068
3443.618536	735012.150598	46.035073
3441.631771	732636.677799	46.040077
3439.847139	730236.302649	46.045082
3437.659948	727793.439820	46.050087
3435.124358	725318.653713	46.055092
3432.849104	722808.317890	46.060097
3430.736503	720276.885774	46.065101
3428.121477	717714.023095	46.070106
3426.110992	715112.267090	46.075111
3423.557114	712493.759711	46.080116
3421.265448	709830.674120	46.085121
3418.605680	707136.721200	46.090125
3416.330462	704424.375106	46.095130
3414.190629	701670.299916	46.100135
3411.241122	698903.522853	46.105140
3408.914118	696099.394792	46.110145
3406.351183	693277.094099	46.115149
3403.844556	690411.334555	46.120154
3401.458699	687533.949452	46.125159
3398.878611	684610.065117	46.130164
3395.819306	681661.020251	46.135169
3393.303504	678685.742828	46.140173
3390.671647	675697.225971	46.145178
3387.828755	672672.283070	46.150183
3384.889494	669638.442400	46.155188
3382.002825	666577.338853	46.160193
3379.172221	663475.029700	46.165197
3376.248373	660358.462486	46.170202
3373.313469	657220.503152	46.175207
3370.464583	654068.788489	46.180212
3367.951402	650893.963319	46.185217
3364.949941	647685.233562	46.190221
3361.746955	644453.490339	46.195226
3359.088667	641203.387815	46.200231
3355.855841	637946.111353	46.205236
3353.177636	634647.968538	46.210241
3350.066426	631342.611921	46.215245
3347.045050	628018.482736	46.220250
3343.752914	624663.146059	46.225255
3340.567309	621296.700431	46.230260
3337.356384	617903.377288	46.235265
3334.272679	614494.232439	46.240269
3331.526774	611084.727845	46.245274
3328.253917	607638.598546	46.250279
3324.965383	604179.504536	46.255284
3321.646620	600696.386024	46.260289
3318.354485	597211.751642	46.265293
3314.981868	593715.411916	46.270298
3311.715521	590183.140544	46.275303
3307.930140	586655.354947	46.280308
3305.087555	583102.867430	46.285313
3301.763924	579542.638575	46.290317
3298.171718	575973.235719	46.295322
3295.198779	572377.362630	46.300327
3291.440852	568773.196577	46.305332
3288.203518	565151.299719	46.310337
3285.191341	561523.668772	46.315341
3281.610615	557892.344946	46.320346
3278.138672	554224.414122	46.325351
3274.941998	550564.874462	46.330356
3271.364512	546872.815027	46.335361
3267.844615	543188.041629	46.340365
3264.222904	539493.290216	46.345370
3260.620559	535777.524068	46.350375
3257.025339	532064.353201	46.355380
3253.552080	528330.962305	46.360385
3250.255577	524600.411410	46.365389
3246.541902	520847.363258	46.370394
3243.164641	517076.332403	46.375399
3239.466850	513320.847567	46.380404
3236.077889	509545.787958	46.385409
3232.159255	505764.751809	46.390413
3228.956353	501973.265078	46.395418
3225.548112	498170.317262	46.400423
3221.847218	494370.870788	46.405428
3218.153517	490548.587293	46.410433
3214.262427	486735.670463	46.415437
3210.808741	482912.086624	46.420442
3207.542830	479064.843850	46.425447
3203.363480	475229.848156	46.430452
3199.762836	471380.751141	46.435457
3196.135515	467518.967208	46.440461
3192.156445	463683.046057	46.445466
3188.784106	459814.384552	46.450471
3185.000970	455951.847112	46.455476
3181.420005	452082.196828	46.460481
3177.951880	448203.483560	46.465485
3174.005959	444321.024523	46.470490
3170.223742	440442.076039	46.475495
3166.269091	436563.719065	46.480500
3162.625161	432672.212865	46.485505
3158.839430	428782.838991	46.490509
3154.767372	424902.935510	46.495514
3150.765651	421000.425837	46.500519
3146.948865	417114.744853	46.505524
3142.715323	413229.933765	46.510529
3139.014180	409344.692824	46.515533
3135.377028	405461.697455	46.520538
3131.764585	401572.292692	46.525543
3127.714661	397702.598181	46.530548
3123.841470	393809.396155	46.535553
3119.802799	389928.281369	46.540557
3115.783417	386041.169087	46.545562
3111.780533	382160.615380	46.550567
3107.677172	378285.132475	46.555572
3104.053922	374417.618181	46.560577
3100.283589	370544.597948	46.565581
3096.018046	366683.999176	46.570586
3092.406655	362822.397654	46.575591
3088.418684	358969.650972	46.580596
3084.109965	355098.725143	46.585601
3080.687484	351242.026677	46.590605
3076.218493	347412.435951	46.595610
3072.240649	343555.503930	46.600615
3068.161133	339719.158411	46.605620
3063.914338	335894.275380	46.610625
3060.337595	332067.694113	46.615629
3055.634600	328252.782908	46.620634
3051.723148	324439.846863	46.625639
3047.577623	320639.491285	46.630644
3043.617297	316827.293412	46.635649
3039.360766	313041.277467	46.640653
3035.406455	309266.483347	46.645658
3031.382665	305492.372947	46.650663
3026.642613	301729.648302	46.655668
3023.109110	297985.685489	46.660673
3018.893868	294249.444063	46.665677
3014.496517	290512.612561	46.670682
3010.603435	286795.003859	46.675687
3006.761230	283093.573428	46.680692
3002.322580	279376.714614	46.685697
2998.345885	275690.433028	46.690701
2993.854763	272012.975066	46.695706
2989.555489	268332.937962	46.700711
2985.358039	264675.251640	46.705716
2981.259069	261037.002625	46.710721
2977.417948	257409.597784	46.715725
2972.632234	253788.959462	46.720730
2968.465877	250171.442652	46.725735
2964.367632	246585.287078	46.730740
2960.277265	243000.233865	46.735745
2956.115086	239425.831986	46.740749
2951.613271	235874.207104	46.745754
2947.640872	232332.042134	46.750759
2943.224354	228814.323377	46.755764
2939.057151	225293.930714	46.760769
2934.867093	221793.431980	46.765773
2930.425550	218308.467219	46.770778
2926.442099	214832.619368	46.775783
2921.728202	211385.262136	46.780788
2917.625028	207942.203945	46.785793
2913.290071	204511.022944	46.790797
2908.998037	201110.149279	46.795802
2904.812752	197705.098934	46.800807
2900.334907	194337.734207	46.805812
2896.080664	190982.413702	46.810817
2891.935433	187638.399682	46.815821
2887.482097	184312.691727	46.820826
2882.983596	180993.186506	46.825831
2878.899733	177696.294408	46.830836
2874.501336	174421.028189	46.835841
2870.288760	171144.478015	46.840845
2865.627104	167834.813772	46.845850
2862.041487	164609.157540	46.850855
2857.614492	161398.449522	46.855860
2852.775816	158203.544866	46.860865
2848.884824	155026.221975	46.865869
2844.423830	151879.258580	46.870874
2840.007010	148739.159121	46.875879
2835.739249	145626.820349	46.880884
2831.436782	142525.007087	46.885889
2827.540297	139437.574547	46.890893
2822.798391	136373.552224	46.895898
2818.853450	133324.416836	46.900903
2814.599265	130286.529185	46.905908
2810.097925	127275.007825	46.910913
2806.070894	124279.502474	46.915917
2801.896710	121314.878809	46.920922
2797.571518	118333.169150	46.925927
2793.083966	115393.654182	46.930932
2788.963215	112464.028238	46.935937
2784.552519	109548.072162	46.940941
2780.231413	106660.349036	46.945946
2775.792127	103778.695780	46.950951
2771.142385	100927.573612	46.955956
2767.124937	98099.960113	46.960961
2762.990312	95275.524277	46.965965
2758.254666	92486.648158	46.970970
2754.664688	89713.258442	46.975975
2750.256453	86960.973952	46.980980
2745.732178	84211.390993	46.985985
2742.061594	81491.215263	46.990989
2737.134292	78799.236604	46.995994
2733.153423	76115.549282	47.000999
2728.707216	73450.256091	47.006004
2724.424908	70808.032194	47.011009
2720.121986	68171.656418	47.016013
2715.221274	65576.862791	47.021018
2711.661946	62986.528351	47.026023
2706.992106	60419.437007	47.031028
2702.866234	57866.741655	47.036033
2698.321153	55350.812164	47.041037
2693.657137	52837.361033	47.046042
2689.624930	50362.565082	47.051047
2685.224722	47898.701940	47.056052
2680.258209	45465.869391	47.061057
2675.922044	43054.539375	47.066061
2671.448183	40656.255909	47.071066
2667.043485	38281.681588	47.076071
2662.188315	35937.892024	47.081076
2657.677544	33622.144604	47.086081
2653.376081	31327.184769	47.091085
2648.722698	29069.421458	47.096090
2643.972255	26831.316573	47.101095
2639.301870	24626.429403	47.106100
2634.961401	22449.739614	47.111105
2630.002721	20291.684427	47.116109
2624.176208	18181.270514	47.121114
2619.518852	16103.729832	47.126119
2613.641863	14082.883405	47.131124
2605.086728	12169.880538	47.136129
2590.977333	10482.291910	47.141133
2576.904937	8901.794922	47.146138
2564.945077	7435.198386	47.151143
2553.630670	6120.108581	47.156148
2542.795608	4929.594293	47.161153
2533.622191	3888.636462	47.166157
2524.414941	2965.733127	47.171162
2516.494795	2158.811977	47.176167
2509.047832	1461.871876	47.181172
2502.335399	893.409870	47.186177
2495.463471	393.293488	47.191181
2483.583800	135.927220	47.196186
2464.572483	198.246244	47.201191
2454.913962	205.879367	47.206196
2451.816232	217.323751	47.211201
2453.297303	215.706350	47.216205
2455.538158	221.686824	47.221210
2457.670479	216.316415	47.226215
2458.491625	220.288438	47.231220
2457.491399	215.882651	47.236225
2455.640052	209.363648	47.241229
2453.468921	214.389085	47.246234
2449.916626	205.535454	47.251239
2446.653109	197.759835	47.256244
2443.208989	197.754504	47.261249
2440.616910	191.933543	47.266253
2437.286469	195.811503	47.271258
2434.300827	192.912265	47.276263
2431.388797	193.136924	47.281268
2428.584462	196.062515	47.286273
2425.221349	197.034814	47.291277
2422.234676	199.134682	47.296282
2419.109691	193.058557	47.301287
2415.812939	196.225706	47.306292
2412.494328	200.652339	47.311297
2409.632748	197.831780	47.316301
2406.059446	196.815242	47.321306
2402.663355	190.620177	47.326311
2399.632053	192.277760	47.331316
2396.096368	193.647238	47.336321
2393.075021	199.894065	47.341325
2389.327593	202.043348	47.346330
2386.456629	196.892479	47.351335
2383.362744	197.379728	47.356340
2379.968789	198.913708	47.361345
2376.703494	188.980626	47.366349
2372.958662	196.922581	47.371354
2369.756071	192.045071	47.376359
2366.455382	190.688493	47.381364
2362.998349	193.868075	47.386369
2359.442368	188.397258	47.391373
2355.823102	202.815030	47.396378
2352.408154	186.416242	47.401383
2349.335722	188.384004	47.406388
2345.669198	195.200028	47.411393
2342.211153	189.780337	47.416397
2338.680753	195.474035	47.421402
2335.770458	195.660481	47.426407
2332.797654	192.449204	47.431412
2329.125213	189.087945	47.436417
2325.729449	188.989660	47.441421
2321.940330	187.427924	47.446426
2318.509119	188.999390	47.451431
2315.100365	183.961157	47.456436
2311.604487	193.547363	47.461441
2308.129378	179.939066	47.466445
2304.405477	190.054512	47.471450
2301.284320	184.926995	47.476455
2297.681091	190.043615	47.481460
2293.966828	189.922399	47.486465
2290.625160	180.823912	47.491469
2287.162429	188.269317	47.496474
2284.352590	181.625060	47.501479
2281.429293	178.029554	47.506484
2277.599954	194.229826	47.511489
2274.035564	178.873230	47.516493
2270.234971	192.522082	47.521498
2266.495810	189.329478	47.526503
2263.831985	181.947347	47.531508
2259.904320	184.086901	47.536513
2256.282120	186.865229	47.541517
2252.895752	181.111643	47.546522
2249.667473	183.432858	47.551527
2246.163617	185.487128	47.556532
2242.632657	186.321218	47.561537
2239.206034	176.460893	47.566541
2235.451013	186.970380	47.571546
2231.874900	173.893636	47.576551
2228.868810	181.106251	47.581556
2224.848655	188.135826	47.586561
2221.873453	180.625247	47.591565
2218.273923	187.066974	47.596570
2214.926881	187.590713	47.601575
2211.688675	173.591044	47.606580
2208.102946	180.970284	47.611585
2204.782411	175.649360	47.616589
2200.916681	190.558149	47.621594
2197.239254	183.432703	47.626599
2193.536709	181.120285	47.631604
2190.412158	178.616192	47.636609
2187.134563	179.496083	47.641613
2183.437145	182.023599	47.646618
2180.251785	174.330774	47.651623
2176.864318	174.901980	47.656628
2173.071612	177.064742	47.661633
2169.754638	170.044274	47.666637
2165.851614	177.947749	47.671642
2162.637389	175.153964	47.676647
2159.291703	169.925582	47.681652
2155.736501	174.816416	47.686657
2152.098853	176.860009	47.691661
2148.690709	185.407426	47.696666
2145.293506	173.916305	47.701671
2141.715832	181.708770	47.706676
2138.184448	179.445525	47.711681
2135.072191	176.949018	47.716685
2131.539058	177.966988	47.721690
2128.106990	182.104546	47.726695
2124.364720	182.259864	47.731700
2120.741284	174.724192	47.736705
2117.328164	175.571523	47.741709
2113.433465	178.702589	47.746714
2110.097144	180.563001	47.751719
2107.339107	185.952406	47.756724
2103.462676	184.999219	47.761729
2099.765745	182.496123	47.766733
2096.441580	180.849063	47.771738
2093.253551	171.106498	47.776743
2089.594212	172.254964	47.781748
2085.973667	178.323512	47.786753
2083.005432	169.400807	47.791757
2078.578577	174.940596	47.796762
2075.475282	173.160905	47.801767
2072.143696	173.669613	47.806772
2068.240935	181.993873	47.811777
2064.935629	164.853552	47.816781
2061.408121	173.410171	47.821786
2058.054505	169.426468	47.826791
2054.750094	172.487337	47.831796
2050.870568	174.859884	47.836801
2047.323333	179.547016	47.841805
2043.795695	172.037517	47.846810
2040.626193	174.928580	47.851815
2037.262939	174.401339	47.856820
2033.805314	175.451819	47.861825
2030.242766	168.849493	47.866829
2026.557600	170.055807	47.871834
2023.316045	165.415480	47.876839
2019.897031	171.620196	47.881844
2016.037984	170.711779	47.886849
2012.339821	158.090856	47.891853
2009.072287	163.797289	47.896858
2005.776982	167.932463	47.901863
2002.061573	175.857250	47.906868
1998.746980	169.807781	47.911873
1995.363179	166.616627	47.916877
1991.739862	173.185526	47.921882
1987.805797	168.606114	47.926887
1984.303503	163.516201	47.931892
1980.992715	169.045906	47.936897
1977.340672	171.145592	47.941901
1974.075777	167.445439	47.946906
1970.602402	164.341080	47.951911
1967.471216	167.745040	47.956916
1964.277497	165.001898	47.961921
1960.993558	154.290438	47.966925
1956.517992	166.105512	47.971930
1953.014940	157.927796	47.976935
1949.594322	166.992915	47.981940
1945.898660	165.112962	47.986945
1943.057867	163.459922	47.991949
1939.006960	166.447803	47.996954
1935.855046	162.840721	48.001959
1932.252899	151.622227	48.006964
1928.396612	171.765782	48.011969
1925.306739	165.709652	48.016973
1921.656196	178.851022	48.021978
1918.402480	165.334819	48.026983
1914.883116	168.075010	48.031988
1911.600486	168.835544	48.036993
1908.316831	160.484302	48.041997
1904.196147	162.682657	48.047002
1900.950148	158.960591	48.052007
1897.242418	163.846890	48.057012
1893.666282	165.165905	48.062017
1890.290233	158.480668	48.067021
1886.879502	158.451305	48.072026
1883.354526	163.065393	48.077031
1879.781707	154.753087	48.082036
1876.033872	157.851756	48.087041
1872.693963	158.282732	48.092045
1869.052382	162.238003	48.097050
1865.959383	161.564120	48.102055
1862.637618	155.477861	48.107060
1858.585086	154.821254	48.112065
1855.440346	154.848356	48.117069
1851.991455	162.528986	48.122074
1848.427551	161.267552	48.127079
1844.936824	149.765897	48.132084
1840.559097	156.155487	48.137089
1837.594638	161.254531	48.142093
1834.024041	160.003641	48.147098
1830.910995	163.202310	48.152103
1827.424937	160.697958	48.157108
1823.917750	160.724840	48.162113
1820.509437	160.163592	48.167117
1816.817223	165.844782	48.172122
1813.187121	158.288139	48.177127
1809.821852	160.324017	48.182132
1806.047257	163.123167	48.187137
1802.765935	152.946055	48.192141
1799.324299	148.697803	48.197146
1795.710622	153.926929	48.202151
1792.640864	145.285993	48.207156
1788.876141	157.534056	48.212161
1785.450290	152.476553	48.217165
1781.331836	159.755765	48.222170
1778.306616	153.382678	48.227175
1774.822701	149.194836	48.232180
1771.497070	146.345850	48.237185
1768.032340	146.875489	48.242189
1764.329738	150.485988	48.247194
1760.897026	146.960878	48.252199
1757.615177	153.530183	48.257204
1753.393501	155.342588	48.262209
1750.205068	148.479345	48.267213
1746.851185	150.529279	48.272218
1743.494270	151.390078	48.277223
1740.054615	141.649079	48.282228
1736.016991	145.745466	48.287233
1732.662667	147.830276	48.292237
1729.356157	155.684812	48.297242
1725.981011	153.308676	48.302247
1722.353679	142.043601	48.307252
1718.789683	152.697320	48.312257
1715.541162	141.967769	48.317261
1711.841035	145.068516	48.322266
1708.283433	147.618595	48.327271
1704.830218	144.077731	48.332276
1701.335745	136.601161	48.337281
1697.953190	148.643894	48.342285
1694.390600	150.818259	48.347290
1690.573786	144.376098	48.352295
1686.989441	148.331958	48.357300
1683.543337	153.338733	48.362305
1680.446473	148.084245	48.367309
1676.948749	146.622683	48.372314
1673.183274	144.162119	48.377319
1670.389804	146.067419	48.382324
1666.442400	145.492514	48.387329
1663.130176	136.130253	48.392333
1659.218887	141.921704	48.397338
1655.485610	141.041199	48.402343
1651.897741	141.558510	48.407348
1648.177879	144.830052	48.412353
1645.416267	136.473152	48.417357
1642.175805	136.559596	48.422362
1638.315498	137.657405	48.427367
1635.134006	139.009655	48.432372
1630.978062	145.804383	48.437377
1628.091458	143.430918	48.442381
1624.049361	146.060016	48.447386
1620.728589	142.587043	48.452391
1617.300952	139.225713	48.457396
1613.730731	134.738222	48.462401
1610.398832	136.974587	48.467405
1606.344730	146.559723	48.472410
1603.051399	145.006084	48.477415
1599.753718	139.710289	48.482420
1596.193550	152.056100	48.487425
1593.158880	144.390543	48.492429
1589.504487	136.470798	48.497434
1585.985347	144.105536	48.502439
1582.113348	128.265929	48.507444
1578.427067	144.712847	48.512449
1575.136528	135.426325	48.517453
1571.898038	137.635427	48.522458
1568.468603	133.413829	48.527463
1564.820545	130.555269	48.532468
1560.981732	142.985826	48.537473
1557.878753	131.528028	48.542477
1554.011664	142.808206	48.547482
1550.997948	140.739407	48.552487
1547.230482	132.514667	48.557492
1543.454607	136.054445	48.562497
1539.839801	136.762678	48.567501
1536.694363	139.061634	48.572506
1533.229477	138.136003	48.577511
1529.901933	133.794065	48.582516
1526.275069	135.734928	48.587521
1523.079866	132.887763	48.592525
1519.102288	139.834950	48.597530
1515.745563	131.602884	48.602535
1512.115630	129.364786	48.607540
1508.852269	137.434087	48.612545
1505.206944	134.220770	48.617549
1501.668275	147.430132	48.622554
1497.933594	148.059063	48.627559
1494.718855	132.401368	48.632564
1491.192558	136.787977	48.637569
1487.555370	132.187628	48.642573
1484.187621	137.508070	48.647578
1480.695572	129.961609	48.652583
1477.541928	133.593846	48.657588
1473.282787	134.709850	48.662593
1470.206429	137.472589	48.667597
1466.529161	143.297080	48.672602
1462.891311	142.610525	48.677607
1460.333984	133.506685	48.682612
1456.337435	137.558776	48.687617
1452.617167	133.037886	48.692621
1449.366191	134.625701	48.697626
1445.705989	147.256131	48.702631
1442.311240	137.900549	48.707636
1438.708746	138.243048	48.712641
1435.276085	137.075119	48.717645
1431.622818	138.491785	48.722650
1428.117246	140.739573	48.727655
1424.604133	134.844796	48.732660
1421.042686	138.857268	48.737665
1417.466554	134.326486	48.742669
1413.666599	132.811085	48.747674
1410.373103	130.757652	48.752679
1407.333926	130.173566	48.757684
1403.791142	137.647535	48.762689
1399.812540	130.885970	48.767693
1396.671258	126.508599	48.772698
1393.389313	139.924576	48.777703
1390.113295	138.564459	48.782708
1386.199831	136.886498	48.787713
1382.732554	132.787956	48.792717
1379.056112	133.572335	48.797722
1375.515532	134.145618	48.802727
1372.602977	133.706241	48.807732
1368.664810	135.857245	48.812737
1365.024993	136.053748	48.817741
1361.487866	133.658807	48.822746
1357.811174	130.510572	48.827751
1354.441653	127.159228	48.832756
1350.791462	129.591035	48.837761
1347.958280	120.169743	48.842765
1344.352131	130.235341	48.847770
1340.671054	131.713342	48.852775
1337.312449	121.346053	48.857780
1333.257313	134.111094	48.862785
1330.135983	130.733562	48.867789
1326.422651	132.422266	48.872794
1322.953566	128.327196	48.877799
1319.782018	135.837991	48.882804
1316.183406	136.129304	48.887809
1312.794726	130.547299	48.892813
1308.887215	125.935556	48.897818
1305.288323	130.191213	48.902823
1302.119673	128.991496	48.907828
1298.499992	125.815378	48.912833
1294.994852	123.061106	48.917837
1291.799657	123.861932	48.922842
1288.079272	129.803960	48.927847
1284.193394	122.600818	48.932852
1280.849993	127.291064	48.937857
1277.007747	119.483130	48.942861
1273.804698	121.863948	48.947866
1270.475575	125.976143	48.952871
1267.423936	125.919249	48.957876
1263.761640	126.264845	48.962881
1260.433207	120.686088	48.967885
1256.653697	121.622692	48.972890
1252.930643	127.688538	48.977895
1249.384775	127.610941	48.982900
1245.687154	122.374730	48.987905
1242.816361	114.193266	48.992909
1239.382317	128.335450	48.997914
1235.648399	131.707411	49.002919
1231.764329	118.116216	49.007924
1228.114537	135.747097	49.012929
1225.145452	120.816729	49.017933
1221.500898	123.453348	49.022938
1218.369646	125.168029	49.027943
1214.771524	125.427664	49.032948
1210.879902	128.593362	49.037953
1207.262402	118.216040	49.042957
1203.961736	111.607876	49.047962
1200.184749	122.092572	49.052967
1197.359882	121.772402	49.057972
1193.682145	122.246996	49.062977
1189.963438	115.852983	49.067981
1186.500336	123.814422	49.072986
1182.766776	127.094593	49.077991
1179.620252	124.698685	49.082996
1175.996063	121.893492	49.088001
1172.385296	121.297722	49.093005
1168.589191	123.258878	49.098010
1165.343235	125.462944	49.103015
1162.090126	118.334808	49.108020
1158.393595	121.830658	49.113025
1155.233486	113.248420	49.118029
1151.602784	120.014866	49.123034
1147.868563	124.158880	49.128039
1144.571781	122.915999	49.133044
1140.676708	127.009267	49.138049
1137.438418	116.923796	49.143053
1133.829258	115.334345	49.148058
1130.590159	130.392023	49.153063
1127.165470	115.757664	49.158068
1123.420059	118.138017	49.163073
1119.959460	118.157853	49.168077
1116.255796	116.722413	49.173082
1112.644276	121.030732	49.178087
1109.715437	117.430148	49.183092
1105.832464	122.818707	49.188097
1102.645694	123.004490	49.193101
1099.271189	121.574472	49.198106
1095.313069	119.270858	49.203111
1091.700037	108.785325	49.208116
1088.199211	122.150200	49.213121
1084.790846	115.558945	49.218125
1081.638165	108.203145	49.223130
1077.810775	123.881293	49.228135
1074.480036	120.315170	49.233140
1070.520621	124.152775	49.238145
1067.233072	119.016958	49.243149
1063.857126	122.500615	49.248154
1060.003324	126.514683	49.253159
1056.987722	119.751209	49.258164
1053.824666	114.589579	49.263169
1049.933365	118.906921	49.268173
1046.582591	119.646761	49.273178
1042.973088	122.382362	49.278183
1039.670697	117.615884	49.283188
1035.726102	123.362138	49.288193
1032.324601	119.892533	49.293197
1028.803150	124.768924	49.298202
1024.982560	116.745741	49.303207
1021.842353	119.939395	49.308212
1018.660113	121.019862	49.313217
1014.632285	120.195216	49.318221
1011.498269	115.639675	49.323226
1007.659886	125.301955	49.328231
1004.123967	122.438717	49.333236
1000.183749	113.039027	49.338241
997.319915	122.412675	49.343245
993.965679	123.608668	49.348250
990.193008	121.124199	49.353255
986.856682	113.477640	49.358260
983.247431	126.017941	49.363265
979.624242	116.097210	49.368269
976.267307	117.236682	49.373274
972.480046	120.867030	49.378279
969.749936	121.911523	49.383284
965.861240	125.089509	49.388289
962.482740	121.511923	49.393293
959.269229	117.554157	49.398298
955.199743	117.438431	49.403303
952.137593	120.626211	49.408308
948.081747	122.840096	49.413313
944.790782	114.259450	49.418317
941.189591	119.929820	49.423322
937.926330	113.084947	49.428327
934.393595	111.021689	49.433332
930.302732	120.160362	49.438337
927.195624	115.701882	49.443341
923.518386	114.550290	49.448346
920.099360	119.701750	49.453351
917.232137	110.940869	49.458356
913.137342	115.267977	49.463361
909.873696	107.508831	49.468365
906.053753	112.147253	49.473370
902.417365	115.861572	49.478375
898.950901	118.299573	49.483380
895.475377	116.556410	49.488385
892.170807	121.803855	49.493389
889.181782	116.444189	49.498394
885.305546	117.187269	49.503399
881.677685	114.506161	49.508404
877.983740	120.830170	49.513409
874.591330	113.942268	49.518413
871.217475	118.770288	49.523418
867.622095	125.344629	49.528423
864.176797	117.677218	49.533428
860.935454	122.497147	49.538433
857.316914	106.358826	49.543437
853.836488	111.969183	49.548442
850.030118	116.573863	49.553447
846.640943	106.309665	49.558452
843.134285	121.219462	49.563457
839.808676	119.823013	49.568461
836.151363	107.424092	49.573466
832.912853	121.266822	49.578471
829.343803	112.745590	49.583476
825.511741	117.936447	49.588481
822.097356	114.525892	49.593485
818.298052	118.689706	49.598490
814.967871	122.514299	49.603495
811.941698	113.145581	49.608500
808.316285	123.283951	49.613505
804.597910	122.107210	49.618509
801.351444	111.501135	49.623514
797.549653	115.386929	49.628519
794.067822	112.075535	49.633524
790.114041	120.737201	49.638529
786.659488	117.851818	49.643533
783.668928	113.080904	49.648538
780.013202	111.609620	49.653543
777.175357	110.114666	49.658548
773.162254	117.437836	49.663553
769.592536	108.489622	49.668557
766.464043	113.823428	49.673562
762.719617	118.469062	49.678567
759.497021	112.744216	49.683572
755.422980	114.688940	49.688577
752.239678	119.790884	49.693581
748.490086	112.462251	49.698586
745.034268	123.010688	49.703591
741.479075	116.597597	49.708596
737.705481	122.779101	49.713601
734.778487	114.676232	49.718605
731.252600	118.075909	49.723610
727.442429	113.794044	49.728615
724.269010	104.321873	49.733620
720.109886	109.003988	49.738625
717.137047	111.260343	49.743629
713.283074	110.263067	49.748634
710.118130	113.577751	49.753639
706.562716	104.532413	49.758644
703.396312	113.134076	49.763649
699.828795	109.583034	49.768653
695.955994	116.754544	49.773658
692.367213	121.540348	49.778663
688.797880	109.953479	49.783668
685.123274	114.803346	49.788673
681.642560	114.440506	49.793677
678.615476	107.890956	49.798682
674.930205	118.510147	49.803687
671.801540	116.795010	49.808692
667.873379	112.604418	49.813697
664.590485	119.844912	49.818701
661.182432	113.535367	49.823706
657.259457	119.626394	49.828711
654.155526	116.363444	49.833716
650.361884	119.412768	49.838721
647.222503	118.797164	49.843725
643.477776	120.731492	49.848730
639.876818	123.760136	49.853735
636.659230	109.808615	49.858740
633.244484	107.502367	49.863745
629.736902	112.731065	49.868749
625.874611	114.933753	49.873754
621.962726	117.451102	49.878759
618.951544	111.468571	49.883764
615.559623	116.641194	49.888769
611.964057	117.207549	49.893773
608.459700	118.022218	49.898778
604.666077	115.446281	49.903783
601.274944	120.818107	49.908788
597.742518	124.332754	49.913793
594.412180	115.970400	49.918797
591.073621	119.426211	49.923802
587.252452	115.348616	49.928807
583.957957	117.006805	49.933812
580.376591	125.176777	49.938817
576.988921	109.378939	49.943821
573.638060	114.345824	49.948826
569.822543	118.138940	49.953831
566.421746	118.624187	49.958836
563.025800	123.297576	49.963841
559.502595	119.192309	49.968845
556.232689	110.893277	49.973850
552.496140	116.233794	49.978855
548.583889	126.654456	49.983860
545.218679	116.943469	49.988865
541.502152	110.625341	49.993869
538.774475	107.711638	49.998874
534.922344	111.614906	50.003879
531.451189	111.990961	50.008884
528.263911	111.063355	50.013889
524.422245	113.807031	50.018893
520.834553	114.815124	50.023898
517.221929	112.027376	50.028903
513.853436	113.383961	50.033908
510.155061	117.544738	50.038913
506.873062	116.119436	50.043917
503.212065	114.196665	50.048922
499.749827	115.055399	50.053927
496.333346	112.724167	50.058932
492.717559	112.847637	50.063937
489.211396	121.031169	50.068941
485.846400	114.189762	50.073946
482.124492	120.420209	50.078951
478.719508	114.202013	50.083956
475.135051	114.687586	50.088961
471.606900	115.841399	50.093965
468.499043	109.851922	50.098970
464.762241	119.416208	50.103975
461.725497	119.404702	50.108980
458.176225	112.943354	50.113985
454.615129	110.897387	50.118989
450.742439	106.261604	50.123994
446.781874	112.342778	50.128999
443.510808	106.413678	50.134004
440.566924	105.653629	50.139009
436.886088	112.301608	50.144013
433.574360	104.575507	50.149018
429.845217	113.467873	50.154023
426.714354	112.003110	50.159028
422.727545	107.657303	50.164033
419.186877	105.168381	50.169037
415.710550	105.731955	50.174042
412.143552	106.692555	50.179047
408.640500	98.376328	50.184052
404.811956	108.097370	50.189057
401.503411	103.464996	50.194061
398.545957	108.082408	50.199066
394.674724	110.033486	50.204071
391.321459	97.343560	50.209076
387.854318	100.509524	50.214081
384.374590	107.901153	50.219085
380.672012	114.748715	50.224090
377.284708	107.828593	50.229095
373.796736	103.053490	50.234100
369.762079	108.598959	50.239105
366.668105	104.053213	50.244109
363.320049	109.845482	50.249114
359.563580	103.793132	50.254119
355.972779	110.094836	50.259124
352.298687	105.747536	50.264129
349.256206	113.776218	50.269133
345.847162	110.782644	50.274138
342.337750	103.131843	50.279143
339.044165	103.128973	50.284148
335.121394	104.936286	50.289153
331.647527	96.223211	50.294157
328.494019	93.499673	50.299162
324.442721	105.372224	50.304167
321.139119	98.701615	50.309172
317.593894	118.632227	50.314177
313.483189	107.260067	50.319181
310.736952	108.832469	50.324186
307.504006	104.023773	50.329191
304.385889	102.645646	50.334196
299.783360	104.875838	50.339201
296.117829	113.223601	50.344205
292.988007	103.377786	50.349210
289.438855	102.728423	50.354215
286.406680	93.582341	50.359220
282.901222	103.993143	50.364225
278.966357	118.251976	50.369229
275.579918	105.570461	50.374234
272.115289	115.079518	50.379239
268.829970	111.845127	50.384244
264.992654	111.854694	50.389249
261.721408	113.161335	50.394253
258.427300	108.944380	50.399258
254.524071	99.583580	50.404263
251.222601	103.884760	50.409268
247.430961	102.612164	50.414273
243.963852	105.822469	50.419277
240.566255	103.127709	50.424282
236.694070	104.579120	50.429287
233.386309	99.930875	50.434292
229.891784	100.459407	50.439297
226.907889	107.877818	50.444301
223.306210	96.932184	50.449306
219.794368	100.870854	50.454311
216.182798	96.004451	50.459316
212.104765	98.715678	50.464321
208.878786	96.316755	50.469325
205.601116	99.231637	50.474330
202.045623	105.822096	50.479335
199.021442	104.008505	50.484340
194.977828	97.665857	50.489345
191.514442	103.656585	50.494349
188.309054	101.349358	50.499354
184.739141	101.105093	50.504359
181.100071	101.836626	50.509364
177.639582	97.367358	50.514369
174.013089	106.284857	50.519373
170.730239	101.607424	50.524378
166.281023	105.439862	50.529383
163.317696	95.346560	50.534388
159.802420	99.706575	50.539393
156.020652	109.496308	50.544397
153.025952	94.592610	50.549402
149.962539	106.607855	50.554407
146.001618	100.546510	50.559412
142.421577	109.858547	50.564417
139.039659	110.458059	50.569421
135.896820	110.823961	50.574426
131.761456	109.345834	50.579431
128.167318	101.632476	50.584436
124.585301	101.374313	50.589441
121.622263	100.769237	50.594445
118.360179	99.692149	50.599450
114.152284	108.314772	50.604455
110.865598	102.366115	50.609460
107.686713	104.015852	50.614465
104.053961	103.129722	50.619469
100.586842	103.264863	50.624474
96.864969	106.334800	50.629479
93.340997	98.695890	50.634484
89.741504	106.324683	50.639489
86.201997	107.901211	50.644493
83.324058	104.644201	50.649498
79.604962	107.539701	50.654503
76.241226	104.431572	50.659508
72.154781	101.022218	50.664513
68.787726	109.962383	50.669517
65.394565	108.118063	50.674522
61.610368	103.224991	50.679527
58.783542	100.001112	50.684532
55.280990	106.279603	50.689537
51.582945	97.332861	50.694541
47.811263	95.206165	50.699546
44.068468	107.786632	50.704551
40.907197	103.640707	50.709556
37.438981	106.708891	50.714561
33.694148	105.732782	50.719565
30.686836	92.767368	50.724570
26.728298	106.738913	50.729575
23.408080	99.976124	50.734580
19.849453	102.922437	50.739585
16.423056	94.138799	50.744589
12.998475	100.942933	50.749594
9.244898	110.241076	50.754599
5.827780	101.728073	50.759604
2.208021	104.187254	50.764609