Thu Aug 25 17:19:07 2022

Number of Points = 9925

Depth (nm)	Load (N)	Time (s)
1.902282	101.341957	0.000000
1.680128	110.618258	0.005005
1.687709	97.718275	0.010010
1.539839	95.321162	0.015014
1.543040	91.824687	0.020019
1.416660	91.294013	0.025024
1.608514	85.989926	0.030029
1.455383	82.100326	0.035034
1.064486	73.964200	0.040038
0.789218	65.664425	0.045043
0.692875	59.130492	0.050048
0.144334	48.083077	0.055053
-0.442399	30.812152	0.060058
-0.709261	40.035309	0.065062
-0.530724	28.744270	0.070067
-1.373495	28.120199	0.075072
-1.391643	31.704477	0.080077
-1.361083	19.835509	0.085082
-1.719273	23.327531	0.090086
-2.011744	8.244156	0.095091
-2.307538	6.458696	0.100096
-2.563799	6.929149	0.105101
-2.696166	2.501634	0.110106
-3.433290	-2.558795	0.115110
-3.156286	-2.016871	0.120115
-3.598925	-1.485578	0.125120
-4.379116	-3.226777	0.130125
-4.464240	-4.513728	0.135130
-4.748778	-7.775272	0.140134
-4.655756	-5.315744	0.145139
-4.733589	-8.954527	0.150144
-5.951715	-4.435586	0.155149
-6.009164	-13.867284	0.160154
-6.153518	-4.400751	0.165158
-6.277166	-13.603775	0.170163
-6.519616	-13.496158	0.175168
-6.439218	-5.959946	0.180173
-6.548344	-8.375771	0.185178
-6.875153	-4.974093	0.190182
-7.538343	-4.246891	0.195187
-7.580243	-5.081866	0.200192
-8.098143	-6.345301	0.205197
-8.067907	-4.907327	0.210202
-8.096215	-0.957629	0.215206
-8.573096	-4.442139	0.220211
-9.114247	-0.608240	0.225216
-9.772514	8.527530	0.230221
-9.182687	1.117306	0.235226
-9.249109	1.266946	0.240230
-9.825250	5.137966	0.245235
-10.209907	-5.131491	0.250240
-10.775002	1.971184	0.255245
-10.927318	-5.889072	0.260250
-10.850911	0.613211	0.265254
-10.856401	-2.021334	0.270259
-10.720722	-4.640033	0.275264
-11.938664	-2.772369	0.280269
-11.973131	-4.526006	0.285274
-12.441699	7.351514	0.290278
-12.437215	-3.216200	0.295283
-12.595843	-1.024128	0.300288
-13.234922	-2.993082	0.305293
-13.343698	-3.096236	0.310298
-14.103232	1.556499	0.315302
-13.787940	-1.343446	0.320307
-13.897689	-5.293607	0.325312
-14.116592	-0.124463	0.330317
-13.433933	1.590940	0.335322
-14.182596	-2.407812	0.340326
-14.502792	-9.419178	0.345331
-14.735271	-7.990662	0.350336
-15.500175	-0.524484	0.355341
-15.999771	-1.237124	0.360346
-16.384675	0.167818	0.365350
-16.331718	-2.431592	0.370355
-16.410087	-6.275937	0.375360
-16.838490	-1.115097	0.380365
-16.434810	-5.727841	0.385370
-16.944068	-0.199988	0.390374
-17.913702	4.811537	0.395379
-17.606893	-4.522213	0.400384
-18.130434	-5.822729	0.405389
-18.045091	-9.259287	0.410394
-18.088548	-12.982550	0.415398
-18.470289	-1.374907	0.420403
-19.068966	-4.726436	0.425408
-19.439232	4.531887	0.430413
-19.367123	-0.329466	0.435418
-19.372841	-5.083709	0.440422
-19.312649	-9.924209	0.445427
-20.247267	-9.913785	0.450432
-20.848266	0.399426	0.455437
-21.016968	-6.853978	0.460442
-21.256618	-4.155662	0.465446
-20.951324	-5.320286	0.470451
-21.014996	-0.150155	0.475456
-21.677003	1.956273	0.480461
-22.053734	-2.879044	0.485466
-22.544963	-1.628286	0.490470
-22.540315	1.636035	0.495475
-22.360911	-2.843491	0.500480
-22.813420	-2.225229	0.505485
-22.958482	7.608418	0.510490
-23.853720	-0.521414	0.515494
-24.149510	0.755669	0.520499
-23.899331	4.471907	0.525504
-24.180278	-8.275220	0.530509
-24.121737	-4.883301	0.535514
-24.737063	10.294893	0.540518
-25.475463	0.017587	0.545523
-25.322464	-1.433226	0.550528
-25.797971	3.361669	0.555533
-25.721488	-2.528597	0.560538
-25.770140	-2.508293	0.565542
-25.714983	0.570943	0.570547
-25.940874	-9.005208	0.575552
-26.714121	-4.932461	0.580557
-26.780507	-3.555279	0.585562
-27.013986	-5.891507	0.590566
-27.713136	-1.972740	0.595571
-27.985483	-13.885971	0.600576
-28.537535	1.772688	0.605581
-28.499473	-5.582716	0.610586
-28.530328	4.755059	0.615590
-28.209356	0.531762	0.620595
-28.085662	0.835113	0.625600
-28.969776	-3.107612	0.630605
-29.130533	-3.281715	0.635610
-29.530535	-2.522982	0.640614
-29.996100	6.652196	0.645619
-30.691925	-5.925521	0.650624
-31.285251	-3.814035	0.655629
-30.537099	-9.205259	0.660634
-31.065063	0.985775	0.665638
-31.395450	-2.964616	0.670643
-31.137630	-6.181424	0.675648
-31.372845	-4.176671	0.680653
-31.297374	0.319920	0.685658
-31.927513	1.832891	0.690662
-32.687187	2.192396	0.695667
-32.211081	-6.604726	0.700672
-33.141803	-0.533104	0.705677
-34.012611	-2.937150	0.710682
-34.209071	4.158385	0.715686
-33.564639	-7.487205	0.720691
-33.497053	-5.887404	0.725696
-34.094475	12.584647	0.730701
-34.268711	-3.741623	0.735706
-34.506849	-1.891437	0.740710
-35.098368	-4.870759	0.745715
-35.446519	-0.953204	0.750720
-35.901904	2.047838	0.755725
-35.831428	-5.565748	0.760730
-35.901132	2.022458	0.765734
-35.876523	-2.242987	0.770739
-36.084291	-5.564015	0.775744
-36.715280	-1.462937	0.780749
-37.163206	-2.003336	0.785754
-37.047497	-1.186202	0.790758
-37.288769	2.648167	0.795763
-37.689530	6.248098	0.800768
-38.212425	15.777115	0.805773
-38.360744	2.540962	0.810778
-38.295369	-2.594584	0.815782
-38.608588	-0.308686	0.820787
-38.331837	-6.654277	0.825792
-39.880590	-3.554685	0.830797
-39.559666	-3.000662	0.835802
-39.660313	-6.676999	0.840806
-40.145357	-0.972605	0.845811
-39.916042	-4.267205	0.850816
-40.652815	2.697853	0.855821
-41.342408	-4.461277	0.860826
-41.181666	-0.183694	0.865830
-41.660893	0.543160	0.870835
-41.468286	0.728144	0.875840
-41.931929	5.470561	0.880845
-41.901750	-2.427780	0.885850
-41.892724	6.666708	0.890854
-42.294337	6.625257	0.895859
-42.962413	1.063627	0.900864
-43.356864	-1.070206	0.905869
-43.484722	-7.596011	0.910874
-43.359359	-4.641673	0.915878
-43.481190	1.448740	0.920883
-43.408053	-5.700186	0.925888
-44.168113	2.600474	0.930893
-44.439258	-0.944745	0.935898
-44.445747	-1.794759	0.940902
-44.815533	0.806889	0.945907
-45.022834	-4.073957	0.950912
-45.596534	1.134961	0.955917
-46.093154	-9.452306	0.960922
-46.275189	-5.867668	0.965926
-46.308702	2.281184	0.970931
-46.397841	-2.950374	0.975936
-46.257159	-8.328673	0.980941
-46.918696	-6.133732	0.985946
-47.388412	-4.449742	0.990950
-47.659011	4.008344	0.995955
-47.829319	-2.988541	1.000960
-48.127251	-0.787297	1.005965
-47.749932	-8.151564	1.010970
-48.557240	-8.072499	1.015974
-48.991423	3.638276	1.020979
-49.100617	1.193989	1.025984
-49.254722	0.405069	1.030989
-49.355865	-3.125656	1.035994
-49.835716	-11.621126	1.040998
-50.845197	-0.380199	1.046003
-50.432826	-1.491999	1.051008
-50.666395	5.846635	1.056013
-50.589827	0.196802	1.061018
-50.903456	-7.385071	1.066022
-51.275903	-5.013962	1.071027
-51.117030	-17.393392	1.076032
-51.786234	-1.760674	1.081037
-52.050940	3.073959	1.086042
-52.381023	7.384158	1.091046
-52.504346	4.669998	1.096051
-52.238697	-6.966861	1.101056
-52.981633	-0.668396	1.106061
-53.293369	-5.592989	1.111066
-53.765900	-2.538640	1.116070
-53.907373	8.313181	1.121075
-53.579406	-3.121472	1.126080
-54.171877	2.568119	1.131085
-54.746249	-6.270049	1.136090
-55.232134	-4.172234	1.141094
-55.289552	3.097669	1.146099
-55.193194	-3.096270	1.151104
-55.571807	1.541073	1.156109
-55.810069	-6.387970	1.161114
-55.887106	1.938545	1.166118
-56.058852	-0.666785	1.171123
-56.492278	1.198183	1.176128
-56.573162	3.276833	1.181133
-56.597816	-1.354219	1.186138
-57.117289	4.864941	1.191142
-58.159045	-2.283301	1.196147
-57.973760	-6.792222	1.201152
-58.516039	2.360172	1.206157
-58.215981	-0.461455	1.211162
-58.357419	-9.408587	1.216166
-58.557232	2.724212	1.221171
-58.464785	-10.663551	1.226176
-59.654312	-4.753859	1.231181
-59.844050	-0.968694	1.236186
-59.617770	-2.529067	1.241190
-59.914610	-1.188542	1.246195
-59.689132	-8.222130	1.251200
-60.170963	-3.483193	1.256205
-60.892750	-3.170752	1.261210
-61.309240	2.810807	1.266214
-61.361031	3.976892	1.271219
-61.188602	-16.010393	1.276224
-61.956145	0.745058	1.281229
-62.037432	-2.586297	1.286234
-61.965870	-9.817232	1.291238
-62.187044	-3.429678	1.296243
-62.840686	-19.060710	1.301248
-63.724310	-14.442317	1.306253
-63.997102	-9.704498	1.311258
-63.027929	-11.017440	1.316262
-63.829993	-14.435171	1.321267
-63.647044	-15.571135	1.326272
-63.905880	-2.710914	1.331277
-64.475795	-9.037735	1.336282
-64.752094	-13.800197	1.341286
-65.411820	-15.313489	1.346291
-65.060663	-7.101530	1.351296
-65.528400	-11.217058	1.356301
-65.450090	-14.785391	1.361306
-65.806155	-1.796039	1.366310
-66.932407	3.562736	1.371315
-66.784404	-1.902134	1.376320
-66.562144	-5.948609	1.381325
-67.083849	-5.294192	1.386330
-67.097040	-13.328100	1.391334
-67.851924	-9.403764	1.396339
-67.932967	-8.071743	1.401344
-68.266128	-13.638386	1.406349
-68.737243	-10.340649	1.411354
-68.389032	-7.829359	1.416358
-68.894887	-3.902913	1.421363
-68.231822	-18.509550	1.426368
-69.239610	-14.112149	1.431373
-69.675647	-5.248491	1.436378
-69.645819	-5.588499	1.441382
-70.149690	-1.333330	1.446387
-70.151764	-9.723326	1.451392
-70.790914	-12.673034	1.456397
-70.929908	-11.689440	1.461402
-71.363605	-1.279059	1.466406
-71.581092	3.117901	1.471411
-71.616488	-5.978726	1.476416
-71.598588	2.522739	1.481421
-71.701652	-3.576675	1.486426
-72.126118	-6.908039	1.491430
-72.401563	-4.776758	1.496435
-72.582732	-6.092951	1.501440
-72.796611	-4.192782	1.506445
-73.200022	-2.224948	1.511450
-73.338876	-4.091942	1.516454
-73.728496	-3.967590	1.521459
-73.954423	-3.919508	1.526464
-74.916194	-3.126533	1.531469
-74.744733	-8.762756	1.536474
-74.933706	-10.125183	1.541478
-75.781576	-0.548417	1.546483
-75.745837	-11.855015	1.551488
-76.150185	-2.638815	1.556493
-76.345938	-8.669919	1.561498
-76.030529	-0.208745	1.566502
-76.178237	-7.313573	1.571507
-76.105441	-12.516716	1.576512
-76.330984	2.211248	1.581517
-76.826747	-14.004513	1.586522
-77.314291	-8.692038	1.591526
-77.608732	-1.157207	1.596531
-77.517929	-6.556164	1.601536
-77.982737	6.693844	1.606541
-78.622014	-6.243903	1.611546
-79.121246	-9.933713	1.616550
-79.452238	-4.573000	1.621555
-79.393746	-9.694808	1.626560
-79.278849	-3.230200	1.631565
-79.083421	-11.122790	1.636570
-79.130545	-10.700925	1.641574
-80.096865	-13.627841	1.646579
-80.117092	-10.590581	1.651584
-80.477126	-4.409063	1.656589
-80.548173	-11.475280	1.661594
-81.366309	-7.268946	1.666598
-81.993895	-6.892169	1.671603
-82.096119	-9.941828	1.676608
-82.216141	1.371701	1.681613
-81.605165	0.342676	1.686618
-81.839023	-3.246347	1.691622
-82.409139	1.658287	1.696627
-82.359446	-7.745903	1.701632
-83.152374	-3.752327	1.706637
-83.507807	-8.477079	1.711642
-83.718040	-2.046947	1.716646
-83.870784	-0.140537	1.721651
-83.622843	-15.694539	1.726656
-84.737727	-4.342185	1.731661
-85.140311	-0.118705	1.736666
-85.032336	-12.844502	1.741670
-85.532357	-10.418602	1.746675
-85.299918	-12.346938	1.751680
-85.349751	-6.289957	1.756685
-85.346604	-3.458841	1.761690
-85.795457	-8.355617	1.766694
-86.375574	-3.800597	1.771699
-86.621113	-4.176552	1.776704
-86.807925	-5.333672	1.781709
-86.488252	-13.372280	1.786714
-87.467888	-12.541702	1.791718
-88.359783	1.765486	1.796723
-87.762492	-12.897288	1.801728
-88.119826	-5.222889	1.806733
-88.217990	-3.518022	1.811738
-88.116145	-6.346556	1.816742
-89.036599	-3.332751	1.821747
-89.479675	-5.610823	1.826752
-89.782240	-6.240436	1.831757
-89.486740	-5.188882	1.836762
-89.539648	-6.063260	1.841766
-89.993957	-2.815611	1.846771
-90.107009	-6.505821	1.851776
-90.820478	-1.161106	1.856781
-91.270685	-6.326592	1.861786
-91.284233	-8.067686	1.866790
-91.227099	-2.761462	1.871795
-91.124804	-3.062205	1.876800
-91.882083	-2.737872	1.881805
-92.583135	-1.840214	1.886810
-92.404778	-6.499910	1.891814
-92.948814	-1.577217	1.896819
-92.756081	-0.458938	1.901824
-92.735749	4.245608	1.906829
-92.722207	-3.849440	1.911834
-93.199843	-8.194372	1.916838
-93.923553	-0.573294	1.921843
-93.699756	-7.970452	1.926848
-94.755117	2.837901	1.931853
-95.390029	2.298330	1.936858
-95.182032	-7.386930	1.941862
-95.715739	-4.019272	1.946867
-95.280956	-4.682165	1.951872
-95.795804	1.071194	1.956877
-96.066762	-7.849312	1.961882
-95.750539	-10.303309	1.966886
-95.898446	-8.400822	1.971891
-96.005916	-13.167590	1.976896
-96.697272	-10.828768	1.981901
-97.265218	0.975729	1.986906
-97.143546	-12.565305	1.991910
-97.801774	0.088576	1.996915
-98.100078	-7.511713	2.006912
-97.609878	-10.851338	2.016909
-97.451206	-7.366194	2.026906
-97.013124	-13.406147	2.036902
-96.257197	-8.348311	2.046899
-95.509052	-2.323065	2.056896
-94.758811	-2.418397	2.066893
-94.790647	-4.868426	2.076890
-94.403772	-3.183521	2.086886
-93.473197	-5.321851	2.096883
-93.220286	-5.630694	2.106880
-92.276337	-4.441729	2.116877
-92.179794	-2.955253	2.126874
-91.997898	-4.463081	2.136870
-90.760270	-4.375021	2.146867
-90.489198	-5.779612	2.156864
-90.497951	-8.873159	2.166861
-89.610247	-6.405081	2.176858
-89.331940	-4.025247	2.186854
-88.580948	-9.439485	2.196851
-87.837700	-5.155778	2.206848
-87.494289	-5.418614	2.216845
-87.353766	-4.487064	2.226842
-86.644196	-11.006719	2.236838
-86.393668	1.197745	2.246835
-85.512746	-7.857684	2.256832
-84.986203	-8.659236	2.266829
-84.761819	-6.008023	2.276826
-84.003076	-4.124792	2.286822
-83.418823	-0.937583	2.296819
-83.475429	-3.675171	2.306816
-82.770620	-3.437097	2.316813
-82.242823	1.428406	2.326810
-81.594710	-3.260118	2.336806
-80.843467	-3.533004	2.346803
-80.524544	-3.114086	2.356800
-80.229369	-3.733664	2.366797
-79.329743	0.753626	2.376794
-79.413832	-5.432594	2.386790
-78.652215	-7.107287	2.396787
-77.971781	-6.190645	2.406784
-77.651540	-5.176381	2.416781
-77.230231	-2.708080	2.426778
-76.269701	-5.535354	2.436774
-76.178891	-3.303538	2.446771
-75.742833	-5.415065	2.456768
-75.034524	-0.954818	2.466765
-74.850065	-0.898138	2.476762
-74.061729	-6.581158	2.486758
-73.323425	-4.754912	2.496755
-73.127007	-10.788677	2.506752
-72.389551	-6.187278	2.516749
-71.911187	1.388132	2.526746
-71.676235	1.617467	2.536742
-71.238457	-2.195456	2.546739
-70.422380	-5.988458	2.556736
-70.412497	-8.128241	2.566733
-69.407980	-2.859093	2.576730
-69.066124	-1.879894	2.586726
-68.851111	-7.295679	2.596723
-67.799733	-9.826739	2.606720
-67.541009	-9.667654	2.616717
-67.226051	-0.200787	2.626714
-66.429658	7.701767	2.636710
-66.248813	-3.683200	2.646707
-65.597008	-9.420852	2.656704
-65.117708	-8.624749	2.666701
-64.792879	-7.725246	2.676698
-64.219356	-5.727459	2.686694
-63.881793	-2.587126	2.696691
-62.980330	-11.500050	2.706688
-62.255172	-4.346619	2.716685
-62.159419	-10.484989	2.726682
-61.763699	-0.371867	2.736678
-61.002446	-4.831027	2.746675
-60.670563	-9.219740	2.756672
-59.755963	-8.938508	2.766669
-59.341511	-4.707817	2.776666
-59.287436	-8.888272	2.786662
-58.441836	-9.340669	2.796659
-58.040156	-6.191375	2.806656
-57.599102	-1.676579	2.816653
-56.742168	-2.659780	2.826650
-56.734596	3.259765	2.836646
-56.438015	-0.743278	2.846643
-55.258529	6.329467	2.856640
-54.984658	-1.864230	2.866637
-54.769406	3.227648	2.876634
-53.553613	2.356113	2.886630
-53.723702	7.273952	2.896627
-53.262021	-0.879481	2.906624
-52.524773	4.076753	2.916621
-52.101530	-1.511046	2.926618
-51.398732	4.910957	2.936614
-50.767706	-0.839282	2.946611
-50.431524	2.317109	2.956608
-50.303004	-3.620489	2.966605
-49.649231	4.640203	2.976602
-49.172002	-3.445972	2.986598
-48.118059	-6.382915	2.996595
-47.964189	-1.157874	3.006592
-47.822880	-12.048796	3.016589
-47.003566	-3.649319	3.026586
-46.654121	4.785772	3.036582
-46.068279	0.940146	3.046579
-44.981052	-0.443439	3.056576
-44.649960	-0.403398	3.066573
-44.750164	0.907998	3.076570
-44.194826	1.806231	3.086566
-43.626121	2.391922	3.096563
-42.936414	-1.888132	3.106560
-42.611887	-5.464728	3.116557
-41.926118	2.005329	3.126554
-41.686655	2.949888	3.136550
-40.746540	-5.303851	3.146547
-40.249378	-5.742831	3.156544
-40.001018	-1.321386	3.166541
-39.934697	4.598459	3.176538
-38.924551	1.072825	3.186534
-38.693932	3.175029	3.196531
-37.579581	-1.893827	3.206528
-37.164837	-6.526776	3.216525
-37.089334	-7.156282	3.226522
-37.269974	1.007069	3.236518
-36.004314	-4.437124	3.246515
-35.242291	-11.310290	3.256512
-34.320097	-7.719861	3.266509
-34.583512	2.091062	3.276506
-34.118594	-3.851729	3.286502
-33.825179	-3.603043	3.296499
-32.969486	-8.982998	3.306496
-32.363367	-6.258547	3.316493
-31.649597	1.346508	3.326490
-31.188099	-0.322339	3.336486
-30.897930	-3.237810	3.346483
-31.179950	-4.128080	3.356480
-30.085267	-7.796839	3.366477
-29.139471	-3.459330	3.376474
-28.997625	-0.792013	3.386470
-28.008862	-0.747314	3.396467
-28.175912	-1.737962	3.406464
-27.667622	-0.737321	3.416461
-27.411438	0.743150	3.426458
-26.260000	4.117097	3.436454
-25.663562	2.401763	3.446451
-25.423007	-2.878641	3.456448
-25.295308	-3.060158	3.466445
-24.238687	-6.368155	3.476442
-24.285681	1.064662	3.486438
-23.498789	2.116685	3.496435
-22.888698	2.328424	3.506432
-22.608073	1.983561	3.516429
-21.606942	5.067444	3.526426
-20.985303	2.815966	3.536422
-20.551778	0.647817	3.546419
-20.808283	0.038653	3.556416
-20.215995	-5.588303	3.566413
-19.630062	2.787561	3.576410
-19.116916	1.639649	3.586406
-18.267633	1.474952	3.596403
-17.740439	-9.501778	3.606400
-17.561525	-11.135851	3.616397
-16.800871	-8.898115	3.626394
-16.579365	-7.206302	3.636390
-16.264462	-12.286108	3.646387
-15.295761	-7.866656	3.656384
-15.018072	-4.035854	3.666381
-14.258258	-3.749371	3.676378
-13.820752	-10.197886	3.686374
-13.772827	-4.633125	3.696371
-12.691142	-6.814131	3.706368
-12.165762	-11.340868	3.716365
-12.153421	-14.523253	3.726362
-11.593455	-10.020751	3.736358
-10.819061	-7.072405	3.746355
-10.626644	-10.564943	3.756352
-9.540862	-12.528010	3.766349
-9.290046	1.453573	3.776346
-9.199720	-1.943775	3.786342
-8.253596	-6.222821	3.796339
-7.986640	-10.338431	3.806336
-7.765607	-10.043557	3.816333
-6.906583	-5.746302	3.826330
-6.606044	-9.350817	3.836326
-5.949049	-0.149779	3.846323
-5.176097	-1.363739	3.856320
-4.967917	-1.567369	3.866317
-4.724110	1.524302	3.876314
-4.671768	11.364954	3.886310
-3.961962	20.871344	3.896307
-2.747626	34.936406	3.906304
-2.446172	37.033853	3.916301
-2.584804	47.053336	3.926298
-2.016223	62.740164	3.936294
-1.370452	83.249049	3.946291
-0.704554	97.238532	3.956288
-0.074058	109.418393	3.966285
0.000000	121.440678	3.971290
0.167027	117.080121	3.976294
0.583612	127.708537	3.981299
0.968608	126.420684	3.986304
0.784973	121.314626	3.991309
0.166994	125.334598	3.996314
0.802228	129.522050	4.001318
0.722454	141.133094	4.006323
0.916866	138.435568	4.011328
0.997278	148.309898	4.016333
1.153112	151.746716	4.021338
1.391652	140.183608	4.026342
1.011365	138.294313	4.031347
0.361485	119.644284	4.036352
1.385599	133.970916	4.041357
1.096658	136.493475	4.046362
0.705409	128.420656	4.051366
0.808555	144.324801	4.056371
1.202820	140.589870	4.061376
1.006844	139.351915	4.066381
0.764894	141.231187	4.071386
1.283438	145.136365	4.076390
1.018871	149.119951	4.081395
0.991836	146.017352	4.086400
1.205993	142.880126	4.091405
0.996328	144.131069	4.096410
1.297666	139.790592	4.101414
1.495274	147.438220	4.106419
1.672019	127.291899	4.111424
1.128958	124.589700	4.116429
0.672477	126.391851	4.121434
0.871402	124.753495	4.126438
1.024521	136.407141	4.131443
1.374981	144.328216	4.136448
1.201692	138.698504	4.141453
1.240508	141.002028	4.146458
1.223356	135.942649	4.151462
1.349026	146.708408	4.156467
1.334964	140.186863	4.161472
1.274485	140.889239	4.166477
0.953058	148.089836	4.171482
1.185844	148.249544	4.176486
1.163312	148.155022	4.181491
1.064048	143.817199	4.186496
1.090273	144.910958	4.191501
0.915815	160.289128	4.196506
1.392309	152.380898	4.201510
0.746297	155.816800	4.206515
1.104510	161.961771	4.211520
1.606115	165.198879	4.216525
1.492245	171.405166	4.221530
1.553756	169.731388	4.226534
1.233383	168.386369	4.231539
1.394439	163.096576	4.236544
1.343111	166.521562	4.241549
1.167372	182.314410	4.246554
1.571858	176.163879	4.251558
1.418356	177.523086	4.256563
1.351899	174.730385	4.261568
1.821362	176.381133	4.266573
1.767038	180.005911	4.271578
1.599823	175.745168	4.276582
1.775931	179.618584	4.281587
1.531665	177.758593	4.286592
1.654983	169.627278	4.291597
1.630201	189.696104	4.296602
1.879293	173.338139	4.301606
1.716742	169.620842	4.306611
1.430795	161.863709	4.311616
1.800179	166.481974	4.316621
1.723943	174.235797	4.321626
1.999007	164.081176	4.326630
1.860085	163.100040	4.331635
1.448038	160.573465	4.336640
1.590885	154.365858	4.341645
1.294690	162.169959	4.346650
1.370005	163.999523	4.351654
1.857843	182.757299	4.356659
1.779202	176.438852	4.361664
2.096642	176.158182	4.366669
2.089592	181.363789	4.371674
2.095899	171.225964	4.376678
2.194901	168.812307	4.381683
1.806717	154.604362	4.386688
1.625241	154.620167	4.391693
1.752328	158.045670	4.396698
2.115655	157.400300	4.401702
1.551048	156.159990	4.406707
1.725241	166.437259	4.411712
2.191205	174.871771	4.416717
1.823430	176.707485	4.421722
2.075642	183.077884	4.426726
2.001213	171.339163	4.431731
1.791125	160.988472	4.436736
1.993109	175.763497	4.441741
1.960521	174.753044	4.446746
2.049561	171.448752	4.451750
2.008567	177.381026	4.456755
2.122615	171.266512	4.461760
1.848309	160.182387	4.466765
1.805059	167.620985	4.471770
2.114091	176.004155	4.476774
2.238178	169.767844	4.481779
1.798116	180.783619	4.486784
2.073738	171.660311	4.491789
2.092844	178.839202	4.496794
1.827279	172.157732	4.501798
2.005409	177.565281	4.506803
2.003517	174.597945	4.511808
2.105860	179.235908	4.516813
1.601591	179.409858	4.521818
1.691283	176.731899	4.526822
1.886178	179.507692	4.531827
1.811039	178.845598	4.536832
2.497007	198.300025	4.541837
2.345166	203.629566	4.546842
2.399035	193.424164	4.551846
2.476381	184.540728	4.556851
2.108950	183.756749	4.561856
1.941847	177.556568	4.566861
2.246425	186.051175	4.571866
2.219420	188.893375	4.576870
2.110759	206.782838	4.581875
2.231436	204.147477	4.586880
2.864725	188.203875	4.591885
2.535257	201.182884	4.596890
2.517557	202.796067	4.601894
2.515210	191.729423	4.606899
2.078398	189.162430	4.611904
2.300379	191.408788	4.616909
2.227228	197.713109	4.621914
2.304108	191.050744	4.626918
2.297872	198.274744	4.631923
2.331232	195.611935	4.636928
2.544025	201.001405	4.641933
2.070331	208.042382	4.646938
2.313080	198.791331	4.651942
2.522865	199.682322	4.656947
2.879108	199.474667	4.661952
2.632940	200.130208	4.666957
2.464571	206.329227	4.671962
2.429311	201.437185	4.676966
2.562123	200.065450	4.681971
1.968548	205.907140	4.686976
2.591845	193.853433	4.691981
2.702018	211.797200	4.696986
2.827690	197.242947	4.701990
2.361957	205.526057	4.706995
2.262007	203.630796	4.712000
2.184203	208.512132	4.717005
2.515849	230.031136	4.722010
2.305405	225.112750	4.727014
2.741935	225.686635	4.732019
2.988070	228.764462	4.737024
3.112579	231.769596	4.742029
2.992693	225.115901	4.747034
2.771356	221.597633	4.752038
3.045099	216.448359	4.757043
2.727920	207.639382	4.762048
2.724342	200.534030	4.767053
2.535342	203.151673	4.772058
2.860639	213.981109	4.777062
2.756960	218.686164	4.782067
3.015550	227.966296	4.787072
2.655734	217.743438	4.792077
2.912436	211.916613	4.797082
2.573145	222.438888	4.802086
2.949214	234.076647	4.807091
2.955133	233.512585	4.812096
2.971411	220.598495	4.817101
3.167807	229.600465	4.822106
2.955559	228.289122	4.827110
3.152351	232.637047	4.832115
2.601041	227.756249	4.837120
3.149215	217.470220	4.842125
2.791463	227.150649	4.847130
2.732619	219.430675	4.852134
2.951587	222.984167	4.857139
3.124039	230.737016	4.862144
3.154316	229.950833	4.867149
3.149147	227.958460	4.872154
3.051731	222.497171	4.877158
3.104095	233.755369	4.882163
2.952771	236.547452	4.887168
3.406982	229.227988	4.892173
3.004517	239.715877	4.897178
2.963360	229.237435	4.902182
3.208871	227.768945	4.907187
3.163138	232.449105	4.912192
3.233935	229.799409	4.917197
3.161050	225.055627	4.922202
3.310083	226.864156	4.927206
3.239600	229.975773	4.932211
2.875399	231.741329	4.937216
3.279673	225.805954	4.942221
2.971238	237.057410	4.947226
2.965728	238.966086	4.952230
2.884240	228.471817	4.957235
2.745148	221.390852	4.962240
2.948893	231.359802	4.967245
3.033467	226.259147	4.972250
3.292020	235.184940	4.977254
3.559368	244.115688	4.982259
3.290475	246.660432	4.987264
3.520844	233.206577	4.992269
3.505581	236.385475	4.997274
3.058053	229.068090	5.002278
3.151722	235.390580	5.007283
3.176398	243.445005	5.012288
3.405583	252.957553	5.017293
3.554206	254.940159	5.022298
3.286272	251.492463	5.027302
3.183089	258.851903	5.032307
3.224760	264.242893	5.037312
3.635098	259.271526	5.042317
3.214928	256.031184	5.047322
2.959872	251.717745	5.052326
3.338574	252.082387	5.057331
3.455667	258.761892	5.062336
3.593358	256.861030	5.067341
3.354287	260.056016	5.072346
3.388955	256.924746	5.077350
3.655345	259.189465	5.082355
3.690474	254.492028	5.087360
3.445621	253.587598	5.092365
3.377928	253.481168	5.097370
3.271166	271.860792	5.102374
3.513136	274.471033	5.107379
3.486232	278.401590	5.112384
3.813729	274.749861	5.117389
3.479412	282.616936	5.122394
3.345827	286.624324	5.127398
3.863900	282.256181	5.132403
3.194020	285.993248	5.137408
4.094188	280.885013	5.142413
3.905078	288.653408	5.147418
3.850947	282.236168	5.152422
3.754196	284.883663	5.157427
3.826122	289.418849	5.162432
4.001948	280.769878	5.167437
3.949877	285.036583	5.172442
3.883602	282.522253	5.177446
3.708250	288.311096	5.182451
3.798290	283.652506	5.187456
3.861739	287.116480	5.192461
3.954109	280.157418	5.197466
3.643157	284.853836	5.202470
3.735961	279.603177	5.207475
3.824960	288.827653	5.212480
3.999706	282.339750	5.217485
3.696811	285.940220	5.222490
3.721190	286.651453	5.227494
3.726782	287.384612	5.232499
3.632479	282.777052	5.237504
4.049567	276.966206	5.242509
4.125894	284.284875	5.247514
3.819214	290.736553	5.252518
3.708511	282.236882	5.257523
3.716712	288.481032	5.262528
4.227500	292.893672	5.267533
3.899192	297.754169	5.272538
4.068521	294.589138	5.277542
4.043735	296.428073	5.282547
4.327077	303.413749	5.287552
4.194070	295.104233	5.292557
4.193289	293.563593	5.297562
4.195797	281.369808	5.302566
3.960969	285.946729	5.307571
3.830448	294.984135	5.312576
4.069958	299.081768	5.317581
4.376339	304.621125	5.322586
4.000398	298.963001	5.327590
4.297322	306.035138	5.332595
4.234685	306.329723	5.337600
4.658039	301.293028	5.342605
4.453890	299.657699	5.347610
4.234150	284.145068	5.352614
3.799401	286.671511	5.357619
4.019315	308.290375	5.362624
4.371225	293.580370	5.367629
4.012575	309.557018	5.372634
4.182654	314.763385	5.377638
4.734965	312.519135	5.382643
4.685071	304.278852	5.387648
4.797326	297.247063	5.392653
4.654710	284.553981	5.397658
4.369424	278.255221	5.402662
4.295119	287.938729	5.407667
4.110564	292.605853	5.412672
4.432556	281.083365	5.417677
4.409993	286.414822	5.422682
4.383195	297.641171	5.427686
4.388953	290.319179	5.432691
4.226877	302.382996	5.437696
4.453480	310.412140	5.442701
4.541637	304.156100	5.447706
4.663835	310.069176	5.452710
4.703444	302.419164	5.457715
4.399164	307.930813	5.462720
4.516264	293.140537	5.467725
4.639188	303.179139	5.472730
4.384028	307.224563	5.477734
4.449750	310.862197	5.482739
4.479363	309.044703	5.487744
4.717441	304.635002	5.492749
4.184650	313.346295	5.497754
4.440545	301.843641	5.502758
4.613014	309.780023	5.507763
4.350153	312.918633	5.512768
4.454489	308.207175	5.517773
4.719804	309.190714	5.522778
4.346859	313.631091	5.527782
4.772811	306.619752	5.532787
4.347996	310.302606	5.537792
4.678519	309.614913	5.542797
4.600242	312.221551	5.547802
4.844007	314.249370	5.552806
4.685090	307.335998	5.557811
4.577243	323.592910	5.562816
4.848587	321.101608	5.567821
4.837594	330.759400	5.572826
4.568506	338.625771	5.577830
4.789924	343.934837	5.582835
4.677099	343.326099	5.587840
5.255895	337.467750	5.592845
5.115341	342.536130	5.597850
5.156577	337.641556	5.602854
4.775765	314.257184	5.607859
4.613310	330.082884	5.612864
4.954352	321.230832	5.617869
4.869931	330.118660	5.622874
4.800102	338.573924	5.627878
5.165482	338.981786	5.632883
4.728010	340.084933	5.637888
4.946663	334.830358	5.642893
4.897598	341.668810	5.647898
4.859873	342.348645	5.652902
5.234012	338.328918	5.657907
5.030306	352.114094	5.662912
5.311049	340.911251	5.667917
5.018548	338.527275	5.672922
5.143680	340.073797	5.677926
4.944334	341.705962	5.682931
4.793081	335.557028	5.687936
4.965119	339.206485	5.692941
5.126323	348.217192	5.697946
5.004905	345.268556	5.702950
5.289462	338.883653	5.707955
4.912905	341.533867	5.712960
5.284217	338.232775	5.717965
5.139777	343.991481	5.722970
4.926882	344.183056	5.727974
5.241875	337.435870	5.732979
4.846303	344.429858	5.737984
5.363359	339.315194	5.742989
5.282192	348.129753	5.747994
5.022150	343.911988	5.752998
5.489723	341.421576	5.758003
5.419175	349.168256	5.763008
5.457611	350.731527	5.768013
5.219351	341.571587	5.773018
5.217728	346.222719	5.778022
4.954794	343.925860	5.783027
5.035562	347.298545	5.788032
5.183764	345.835801	5.793037
5.203692	335.062980	5.798042
5.301366	348.611102	5.803046
5.569499	342.890014	5.808051
5.101934	342.162847	5.813056
5.203379	359.541802	5.818061
5.302542	362.174431	5.823066
5.462620	371.504876	5.828070
5.836779	367.662314	5.833075
5.536504	381.253830	5.838080
5.607324	369.976289	5.843085
5.538924	357.977065	5.848090
5.216630	349.947125	5.853094
5.683326	355.648047	5.858099
5.234481	363.615362	5.863104
5.609053	367.742470	5.868109
5.530715	371.329920	5.873114
5.463257	368.818927	5.878118
5.534757	365.194636	5.883123
5.471015	365.337530	5.888128
5.587355	367.733344	5.893133
6.034319	364.834858	5.898138
5.547318	368.002269	5.903142
5.747600	363.873730	5.908147
5.658804	373.999330	5.913152
5.555715	370.440358	5.918157
5.584728	369.822052	5.923162
5.387933	372.573822	5.928166
5.732833	368.454262	5.933171
5.542660	378.133827	5.938176
5.615760	373.882840	5.943181
5.475621	373.613749	5.948186
5.349970	367.543052	5.953190
5.608957	365.737072	5.958195
5.482376	375.042828	5.963200
5.657262	362.913730	5.968205
5.658953	377.242564	5.973210
5.920717	380.397065	5.978214
5.944012	371.044264	5.983219
5.648476	377.731516	5.988224
5.858912	364.239556	5.993229
5.625007	366.753524	5.998234
5.450345	373.089631	6.003238
5.987982	382.604541	6.008243
5.728671	390.225786	6.013248
6.450578	380.747700	6.018253
6.123392	369.409130	6.023258
5.890410	368.360460	6.028262
6.272547	363.153030	6.033267
5.856237	369.776943	6.038272
6.174056	367.895304	6.043277
5.773866	368.027637	6.048282
6.177871	360.282539	6.053286
6.216169	359.118596	6.058291
5.790111	359.273966	6.063296
5.978809	365.224098	6.068301
6.053984	352.319669	6.073306
5.866133	347.052850	6.078310
5.707666	340.525383	6.083315
5.854434	335.921167	6.088320
5.827368	326.870517	6.093325
5.760191	330.665024	6.098330
5.884426	328.427731	6.103334
5.774373	334.076640	6.108339
5.299404	334.853458	6.113344
5.573641	341.600124	6.118349
5.857316	346.636837	6.123354
5.787911	359.606852	6.128358
5.792465	355.550112	6.133363
5.730318	366.449839	6.138368
5.878554	357.624814	6.143373
5.809106	361.669627	6.148378
5.896378	362.121064	6.153382
6.034826	353.987294	6.158387
5.931612	371.062959	6.163392
5.807940	358.888891	6.168397
6.061837	347.092284	6.173402
5.891349	337.355399	6.178406
6.078886	336.829317	6.183411
5.727808	336.156667	6.188416
6.055670	336.288826	6.193421
6.076428	335.013734	6.198426
5.351980	331.786251	6.203430
5.678850	331.326926	6.208435
5.611615	339.528676	6.213440
5.483978	330.348246	6.218445
5.821076	345.697044	6.223450
5.568901	340.547877	6.228454
5.748712	348.179397	6.233459
5.994163	359.284032	6.238464
6.052114	354.004009	6.243469
6.027051	348.243435	6.248474
5.696224	338.822745	6.253478
5.812772	327.069818	6.258483
5.622099	341.609102	6.263488
5.318690	334.003330	6.268493
5.597642	353.635598	6.273498
5.971636	358.705621	6.278502
6.052326	361.806230	6.283507
6.052489	371.680602	6.288512
5.560859	354.710845	6.293517
5.640746	351.477558	6.298522
6.016546	361.305724	6.303526
6.024469	361.238068	6.308531
5.490382	349.789555	6.313536
5.709606	358.202702	6.318541
5.924639	359.548473	6.323546
5.881600	365.275479	6.328550
5.690533	345.199198	6.333555
5.848664	350.056260	6.338560
5.859208	349.899606	6.343565
5.699605	342.853445	6.348570
5.849740	345.465430	6.353574
5.971979	336.062342	6.358579
5.641046	344.020665	6.363584
5.611602	350.669379	6.368589
5.946969	361.111338	6.373594
5.648338	355.105715	6.378598
6.065830	356.220442	6.383603
5.833361	358.436782	6.388608
5.805158	353.591050	6.393613
5.786667	344.554867	6.398618
5.817872	351.570576	6.403622
5.769874	333.528391	6.408627
6.017892	342.073064	6.413632
5.959721	339.013276	6.418637
6.001090	337.715972	6.423642
5.539555	339.518935	6.428646
5.816679	335.770679	6.433651
5.782056	339.901782	6.438656
6.008314	332.744546	6.443661
5.728838	337.138645	6.448666
5.793964	339.393779	6.453670
6.175447	324.552561	6.458675
5.901892	339.418050	6.463680
5.613598	343.424380	6.468685
6.007272	338.531534	6.473690
5.566550	348.917910	6.478694
5.663549	329.055947	6.483699
5.532939	345.993508	6.488704
5.833833	343.627291	6.493709
5.790948	342.396973	6.498714
6.107175	341.123044	6.503718
6.200012	339.884116	6.508723
5.907665	345.128144	6.513728
5.529097	337.423412	6.518733
5.838999	338.713187	6.523738
5.572927	346.338636	6.528742
5.934297	331.810621	6.533747
5.896976	341.339663	6.538752
5.996372	335.565920	6.543757
5.837139	333.787504	6.548762
5.372947	326.959921	6.553766
5.989693	332.105800	6.558771
6.054536	331.924818	6.563776
5.778999	335.305870	6.568781
5.996740	337.888278	6.573786
5.346587	341.207801	6.578790
5.773035	330.845864	6.583795
5.465516	342.188994	6.588800
5.884013	340.649097	6.593805
6.036230	329.225947	6.598810
5.663942	334.495152	6.603814
5.567045	339.578837	6.608819
5.713546	337.227320	6.613824
5.752392	340.546459	6.618829
5.890676	341.110130	6.623834
5.790311	338.968140	6.628838
5.762218	342.057315	6.633843
5.757985	337.764668	6.638848
5.908011	331.796327	6.643853
5.799696	335.040443	6.648858
5.705267	339.051199	6.653862
5.629518	334.026255	6.658867
5.800350	339.874771	6.663872
5.651842	335.528798	6.668877
5.752629	333.197099	6.673882
5.606295	351.326734	6.678886
5.962376	353.384417	6.683891
6.030298	358.632114	6.688896
6.121910	353.406930	6.693901
6.173955	336.121046	6.698906
5.893393	333.244804	6.703910
6.176772	339.088341	6.708915
6.000641	338.062404	6.713920
5.605611	343.967944	6.718925
5.715119	335.136344	6.723930
5.602880	339.792150	6.728934
5.910940	336.399726	6.733939
5.565418	341.136377	6.738944
5.490314	336.323309	6.743949
6.091464	343.480675	6.748954
5.809388	338.912013	6.753958
6.045598	335.024632	6.758963
6.159848	337.952295	6.763968
5.967750	336.245469	6.768973
5.763077	335.012027	6.773978
5.971935	336.690967	6.778982
5.954706	337.146122	6.783987
6.109985	341.057640	6.788992
5.680636	336.423466	6.793997
5.926560	333.062925	6.799002
5.697547	338.024937	6.804006
5.963864	342.156345	6.809011
5.517400	343.858868	6.814016
5.373377	337.626541	6.819021
5.649713	328.800442	6.824026
5.867663	330.750048	6.829030
5.821556	332.529050	6.834035
5.610702	333.786520	6.839040
5.587384	331.831781	6.844045
5.816879	341.803085	6.849050
5.712221	340.522333	6.854054
5.779739	338.638785	6.859059
5.462796	338.144289	6.864064
5.757542	333.054967	6.869069
5.589048	329.629642	6.874074
5.429740	335.083782	6.879078
5.992047	327.016494	6.884083
5.575106	335.118007	6.889088
5.706368	328.912154	6.894093
5.851004	339.516866	6.899098
5.675932	347.102747	6.904102
6.631853	348.955711	6.909107
5.763086	339.321905	6.914112
5.846964	346.775462	6.919117
5.848179	333.945910	6.924122
5.773780	336.735447	6.929126
5.770106	326.390285	6.934131
5.834247	327.183876	6.939136
5.923545	333.668443	6.944141
6.031209	337.751940	6.949146
5.799929	346.602674	6.954150
5.966732	337.334976	6.959155
5.655116	334.340209	6.964160
5.606995	334.138961	6.969165
5.623532	335.942951	6.974170
5.530397	338.438022	6.979174
5.682404	340.094232	6.984179
5.586320	345.484684	6.989184
5.789875	338.887840	6.994189
5.811384	334.395002	6.999194
5.735369	331.189311	7.004198
5.761845	338.863835	7.009203
5.749204	345.807316	7.014208
5.665428	349.756292	7.019213
5.954464	348.148091	7.024218
5.501877	346.646598	7.029222
5.865653	355.628734	7.034227
5.915184	362.682706	7.039232
6.339241	357.750293	7.044237
5.703747	336.471788	7.049242
5.650123	340.624851	7.054246
5.806314	328.549327	7.059251
5.999531	333.400888	7.064256
5.466599	332.946562	7.069261
5.821861	338.142904	7.074266
5.874211	344.924337	7.079270
5.928188	329.783243	7.084275
5.974768	335.015293	7.089280
5.523495	330.027042	7.094285
5.874773	330.532028	7.099290
5.613988	334.878905	7.104294
5.804551	329.590767	7.109299
5.556618	344.496539	7.114304
5.796783	346.860293	7.119309
6.133275	343.251435	7.124314
5.725544	338.724608	7.129318
6.057624	347.588316	7.134323
5.785090	336.165272	7.139328
5.799024	337.166053	7.144333
5.849749	334.108187	7.149338
5.717250	346.882428	7.154342
5.946886	337.260026	7.159347
5.835315	337.790076	7.164352
5.752157	335.996576	7.169357
6.025085	336.134178	7.174362
5.970548	333.102296	7.179366
6.139624	332.591763	7.184371
5.875653	330.222301	7.189376
5.533771	329.823464	7.194381
6.091034	319.615049	7.199386
5.977733	333.689775	7.204390
5.749794	337.575912	7.209395
5.756188	340.137649	7.214400
5.783247	334.201229	7.219405
5.863384	330.683162	7.224410
6.041472	338.542744	7.229414
5.923040	326.829798	7.234419
5.802222	327.614404	7.239424
5.908894	342.050151	7.244429
6.288908	327.142720	7.249434
5.772548	333.453256	7.254438
5.702653	327.019487	7.259443
6.060039	332.905212	7.264448
5.634646	331.089404	7.269453
5.906809	331.897860	7.274458
5.630805	334.712657	7.279462
5.805570	331.407559	7.284467
5.948780	331.774299	7.289472
5.850796	327.876005	7.294477
6.340928	330.267032	7.299482
5.503396	320.606197	7.304486
5.613159	307.402142	7.309491
5.603513	316.297231	7.314496
5.780330	323.907063	7.319501
5.751559	327.062783	7.324506
5.660319	330.490890	7.329510
5.879546	325.163459	7.334515
5.541231	332.009262	7.339520
5.605625	324.143380	7.344525
5.932790	322.019828	7.349530
6.047680	326.886824	7.354534
6.291620	327.282075	7.359539
5.927469	329.579157	7.364544
5.939836	325.989449	7.369549
5.798877	314.270549	7.374554
5.865260	306.502441	7.379558
5.784546	293.812309	7.384563
5.718732	302.820598	7.389568
5.326545	300.468065	7.394573
5.737085	310.550194	7.399578
5.669789	327.670812	7.404582
5.779186	328.074488	7.409587
5.517543	326.413362	7.414592
5.664915	327.254026	7.419597
5.994670	320.381144	7.424602
5.997468	328.204910	7.429606
6.192421	319.929421	7.434611
6.146723	330.117848	7.439616
5.591398	316.726921	7.444621
6.177194	309.105226	7.449626
5.830009	310.513773	7.454630
5.577809	297.262033	7.459635
5.706963	316.300783	7.464640
5.568599	317.202035	7.469645
6.010810	325.526443	7.474650
5.857231	318.020592	7.479654
5.787041	307.885183	7.484659
5.917257	304.201082	7.489664
5.739189	306.190588	7.494669
5.807393	299.501067	7.499674
5.511869	305.951003	7.504678
5.752549	313.721672	7.509683
5.880035	320.004092	7.514688
6.173598	332.730549	7.519693
6.091265	323.492402	7.524698
5.856253	322.855352	7.529702
5.882443	308.142585	7.534707
5.669136	305.293776	7.539712
5.377109	305.823625	7.544717
5.926250	302.415580	7.549722
5.879449	317.599872	7.554726
5.710239	305.521563	7.559731
5.998201	303.271276	7.564736
5.870431	304.227817	7.569741
6.118999	297.510037	7.574746
5.936924	297.858138	7.579750
6.030179	296.214177	7.584755
5.946173	304.054697	7.589760
6.105784	304.235364	7.594765
5.891012	296.593573	7.599770
5.444348	299.767307	7.604774
5.777192	301.521733	7.609779
5.587437	298.776806	7.614784
5.766190	296.293687	7.619789
5.877417	300.117183	7.624794
5.759412	296.778868	7.629798
6.250959	302.776443	7.634803
5.830440	307.088227	7.639808
5.726120	303.845846	7.644813
5.904643	294.955993	7.649818
6.032612	295.334612	7.654822
5.911789	296.774131	7.659827
5.788929	300.571028	7.664832
5.584800	304.472411	7.669837
5.980233	298.636476	7.674842
6.011450	295.325402	7.679846
5.783855	291.013978	7.684851
5.811432	294.126061	7.689856
5.515646	294.447686	7.694861
6.046940	288.754987	7.699866
5.818833	306.922699	7.704870
5.950902	301.248255	7.709875
5.844601	300.679626	7.714880
5.692184	297.716872	7.719885
5.558110	297.332934	7.724890
5.631719	296.356456	7.729894
5.600813	297.345278	7.734899
5.872061	307.281546	7.739904
5.938122	301.016315	7.744909
6.107787	300.401283	7.749914
5.785556	302.327953	7.754918
5.822070	302.157738	7.759923
5.728070	290.289124	7.764928
5.395741	296.320869	7.769933
5.871075	289.039201	7.774938
5.778021	298.023281	7.779942
5.934327	296.875655	7.784947
5.883699	298.041577	7.789952
5.613089	296.074967	7.794957
5.968571	298.044150	7.799962
5.825370	300.679942	7.804966
6.156504	304.997344	7.809971
5.954206	296.439250	7.814976
5.643768	302.676381	7.819981
5.802023	300.633083	7.824986
5.717341	306.822187	7.829990
5.754264	298.109548	7.834995
5.558001	300.655575	7.840000
5.323398	312.075848	7.845005
5.711206	304.108680	7.850010
5.566466	303.384718	7.855014
5.671343	298.451709	7.860019
5.921698	296.099744	7.865024
5.744409	298.462460	7.870029
6.076368	294.692966	7.875034
5.759313	299.785824	7.880038
5.605310	302.783986	7.885043
5.523677	300.300535	7.890048
5.275948	303.212140	7.895053
5.649268	296.110973	7.900058
5.512613	315.052160	7.905062
5.910667	323.500548	7.910067
5.955090	327.894516	7.915072
5.739906	324.296168	7.920077
5.979718	311.701339	7.925082
5.892577	312.509142	7.930086
5.378158	304.211925	7.935091
5.526426	313.560009	7.940096
5.846040	329.329159	7.945101
5.936012	327.812263	7.950106
5.858319	333.541525	7.955110
5.791714	329.970517	7.960115
5.976947	329.761181	7.965120
6.074895	322.592415	7.970125
5.805042	313.780030	7.975142
5.849284	312.308848	7.980160
5.975124	310.515615	7.985178
5.873042	306.549058	7.990195
5.624200	306.524958	7.995213
5.552768	300.757968	8.000230
6.041512	310.480071	8.005248
6.084416	315.964411	8.010266
6.007429	304.612581	8.015283
5.631517	305.747622	8.020301
6.063760	296.632342	8.025318
5.874282	303.513224	8.030336
5.582309	298.787479	8.035354
5.947035	297.786784	8.040371
5.441653	300.816636	8.045389
6.195074	290.997792	8.050406
5.966654	307.913798	8.055424
5.928100	301.882883	8.060442
6.109859	304.255969	8.065459
5.759148	302.717283	8.070477
5.795111	297.899132	8.075494
5.958885	298.570921	8.080512
5.505296	298.821896	8.085530
5.916975	306.646834	8.090547
5.791762	312.343704	8.095565
5.957074	319.572941	8.100582
6.090348	326.668346	8.105600
5.940875	321.386943	8.110618
6.143465	309.063508	8.115635
5.548725	302.677930	8.120653
5.851521	316.383348	8.125670
6.002265	329.847515	8.130688
5.885012	337.174680	8.135706
5.990539	324.427791	8.140723
5.796153	337.056112	8.145741
6.015558	331.341372	8.150758
6.302984	337.263928	8.155776
6.271861	329.641330	8.160794
5.719424	315.482769	8.165811
5.743161	332.977820	8.170829
5.717396	324.697985	8.175846
5.580145	327.717498	8.180864
5.696830	337.813489	8.185882
6.026399	334.571391	8.190899
5.882657	337.090155	8.195917
5.876106	331.903118	8.200934
5.828740	335.148387	8.205952
6.122932	335.029736	8.210970
6.153482	342.321121	8.215987
6.035341	342.434331	8.221005
6.028051	334.874268	8.226022
6.053232	339.635565	8.231040
5.789573	335.426077	8.236058
5.732265	327.094378	8.241075
5.793366	341.560356	8.246093
5.745784	352.300625	8.251110
5.796022	353.390989	8.256128
5.979656	366.139981	8.261146
5.982924	353.513234	8.266163
6.019526	363.684903	8.271181
6.151070	356.049430	8.276198
6.286884	356.138628	8.281216
5.919783	364.691523	8.286234
6.164591	363.176288	8.291251
5.619416	365.101552	8.296269
6.123158	358.739498	8.301286
6.130964	355.017642	8.306304
6.036546	358.194549	8.311322
6.149546	354.901174	8.316339
5.868364	359.199242	8.321357
6.208105	358.729474	8.326374
6.086035	359.423963	8.331392
5.868556	365.589738	8.336410
6.249243	359.849719	8.341427
6.241565	362.482866	8.346445
6.178489	358.194607	8.351462
6.469692	357.634615	8.356480
5.978080	365.437009	8.361498
6.030039	361.159128	8.366515
6.045019	371.555094	8.371533
6.413403	376.723370	8.376550
6.071833	380.229337	8.381568
6.333772	382.763438	8.386586
6.530152	371.946241	8.391603
6.166099	369.907871	8.396621
6.063622	367.800115	8.401638
6.436096	377.846583	8.406656
5.854712	382.201161	8.411674
6.436206	380.002016	8.416691
6.409156	393.339455	8.421709
6.393920	383.906082	8.426726
6.682534	374.611296	8.431744
6.109367	375.158716	8.436762
5.837213	367.393988	8.441779
5.750352	375.148748	8.446797
6.036292	379.761902	8.451814
6.193748	392.429809	8.456832
6.178211	391.302499	8.461850
6.169615	390.205660	8.466867
6.226343	396.937548	8.471885
6.050094	391.272158	8.476902
6.519931	394.935015	8.481920
6.158706	400.296510	8.486938
6.340053	404.563144	8.491955
6.331905	395.721941	8.496973
6.347783	398.540749	8.501990
6.284947	402.334405	8.507008
6.028932	404.883392	8.512026
6.486654	397.891068	8.517043
6.149492	407.133564	8.522061
6.046447	411.299592	8.527078
6.352334	416.471361	8.532096
6.418848	427.600894	8.537114
6.337610	432.883816	8.542131
6.593834	431.224776	8.547149
6.366318	430.493593	8.552166
6.443726	418.767207	8.557184
6.111658	418.891845	8.562202
6.506121	416.636794	8.567219
6.780693	419.588641	8.572237
6.361830	425.290532	8.577255
6.780115	421.621110	8.582272
6.223055	416.921089	8.587290
6.368537	401.955678	8.592307
6.636222	409.478178	8.597325
6.113338	413.050430	8.602343
6.193759	415.414162	8.607360
6.196448	421.283530	8.612378
6.675553	429.312551	8.617395
6.670352	431.484575	8.622413
6.620445	434.247424	8.627431
6.750384	439.882267	8.632448
6.682428	435.294954	8.637466
6.470814	425.661955	8.642483
6.554167	421.735745	8.647501
6.496430	417.686475	8.652519
6.344773	415.914621	8.657536
6.339347	427.525638	8.662554
6.600936	436.109449	8.667571
6.746827	439.163512	8.672589
6.478389	437.233228	8.677607
6.661614	430.896123	8.682624
6.938589	433.323735	8.687642
6.541204	415.546356	8.692659
6.504999	404.390043	8.697677
6.594472	406.200093	8.702695
6.474844	402.438234	8.707712
6.704323	410.392751	8.712730
6.359460	418.986368	8.717747
6.692794	418.918387	8.722765
6.546074	430.172850	8.727783
6.615284	429.489849	8.732800
6.541427	437.990520	8.737818
6.774677	436.047903	8.742835
6.692191	428.632125	8.747853
6.339134	434.992736	8.752871
6.321789	441.120868	8.757888
6.343226	443.096216	8.762906
6.390686	440.538927	8.767923
6.649021	441.719767	8.772941
6.461495	434.421431	8.777959
6.738555	430.685773	8.782976
6.682887	434.910655	8.787994
6.534046	433.927305	8.793011
6.854869	436.837195	8.798029
6.694538	437.004352	8.803047
6.699053	436.653378	8.808064
6.806067	445.330840	8.813082
6.596075	430.099212	8.818099
6.824954	430.479940	8.823117
6.566484	438.151163	8.828135
7.136377	438.825598	8.833152
6.822502	436.163979	8.838170
6.505147	441.108360	8.843187
6.508221	436.147002	8.848205
6.488052	441.931596	8.853223
6.849766	446.529739	8.858240
6.609161	440.514657	8.863258
6.507124	439.239952	8.868275
6.804343	431.142990	8.873293
6.281041	446.035131	8.878311
6.618932	449.267395	8.883328
6.663515	458.030384	8.888346
6.800931	460.483021	8.893363
6.975166	460.354762	8.898381
6.991891	474.963500	8.903399
6.644381	463.808589	8.908416
6.893611	469.074456	8.913434
6.442903	461.845747	8.918451
7.088208	465.152923	8.923469
6.715402	469.702058	8.928487
6.845318	470.461210	8.933504
6.495564	469.143265	8.938522
6.611814	466.628843	8.943539
6.673624	476.036079	8.948557
6.492335	468.036165	8.953575
6.901948	469.297445	8.958592
6.623047	472.670535	8.963610
6.465535	474.689704	8.968627
7.297033	480.160988	8.973645
6.777706	482.820670	8.978663
6.938885	476.701598	8.983680
6.927410	473.228889	8.988698
6.955721	464.880556	8.993715
7.240851	462.983456	8.998733
6.786714	469.460901	9.003751
6.985642	461.253094	9.008768
6.678733	464.352860	9.013786
6.931313	472.335343	9.018803
6.996935	473.906141	9.023821
7.014245	484.992927	9.028839
6.880958	474.732249	9.033856
7.140310	483.512093	9.038874
6.649724	485.835913	9.043891
7.211773	486.145506	9.048909
7.225981	477.111413	9.053927
6.855365	471.927730	9.058944
7.102347	467.565618	9.063962
6.721225	476.761389	9.068979
7.384866	485.348501	9.073997
6.998358	475.136965	9.079015
7.220609	479.570777	9.084032
7.136431	470.829812	9.089050
7.009428	474.538863	9.094067
7.230294	463.765111	9.099085
6.929079	474.308508	9.104103
6.859817	471.049981	9.109120
7.127330	466.504772	9.114138
7.115139	464.035721	9.119155
7.128117	468.376088	9.124173
6.858825	482.493160	9.129191
6.884805	482.233496	9.134208
7.133296	491.545219	9.139226
7.034845	495.082543	9.144243
7.275952	488.345030	9.149261
6.967848	493.404740	9.154279
7.304428	496.050238	9.159296
7.019533	497.070045	9.164314
6.897313	498.919585	9.169331
7.157713	491.263865	9.174349
7.129249	507.429207	9.179367
7.229145	503.806500	9.184384
7.278998	490.471769	9.189402
6.955174	498.292112	9.194419
7.071840	493.660079	9.199437
6.940958	505.341296	9.204455
7.000226	506.565954	9.209472
7.001768	508.307741	9.214490
6.874162	504.234686	9.219507
7.069210	502.717768	9.224525
6.892730	506.930039	9.229543
7.000442	503.296639	9.234560
7.431239	516.770717	9.239578
7.354252	522.968182	9.244595
7.465710	508.847457	9.249613
7.373949	503.500153	9.254631
7.628502	497.265457	9.259648
7.269397	492.603828	9.264666
7.102562	505.562466	9.269683
7.280860	496.881349	9.274701
7.337416	508.236554	9.279719
7.190920	504.488350	9.284736
7.250524	511.674267	9.289754
7.045787	497.704079	9.294771
7.367223	494.680977	9.299789
7.376256	501.773828	9.304807
7.417649	501.293998	9.309824
7.426635	505.483521	9.314842
7.586669	507.004815	9.319859
7.515304	497.678006	9.324877
7.220631	505.197140	9.329895
7.002524	496.991543	9.334912
7.263093	498.415033	9.339930
7.171753	503.996204	9.344947
7.415149	507.877600	9.349965
7.409705	519.952583	9.354983
7.624845	512.070416	9.360000
7.537492	504.327167	9.365018
7.296872	507.542786	9.370035
7.614338	504.756990	9.375053
7.492531	509.418287	9.380071
7.451225	517.664587	9.385088
7.484506	508.580152	9.390106
7.315933	508.748602	9.395123
7.762595	500.337860	9.400141
7.562888	503.916297	9.405159
7.371210	508.345544	9.410176
7.382786	501.148528	9.415194
7.179006	503.455815	9.420211
7.342949	495.445978	9.425229
7.549820	492.115780	9.430247
7.235065	499.347724	9.435264
7.263410	503.344865	9.440282
7.443875	514.087369	9.445299
7.586756	521.234995	9.450317
7.692752	532.806532	9.455335
7.650715	519.615566	9.460352
7.649384	512.335361	9.465370
7.250152	512.801882	9.470387
7.635599	524.515821	9.475405
7.886799	518.354227	9.480423
7.724157	514.150959	9.485440
7.796452	508.796883	9.490458
7.214509	508.269552	9.495475
7.382851	500.877560	9.500493
7.405200	504.241325	9.505511
7.474856	518.718729	9.510528
7.720220	510.958059	9.515546
7.383033	528.595059	9.520563
7.697981	524.424256	9.525581
7.795426	527.842530	9.530599
7.591141	523.882470	9.535616
7.617129	524.888282	9.540634
7.769808	527.209149	9.545651
7.342634	522.561333	9.550669
7.267748	527.767548	9.555687
7.289909	527.439054	9.560704
7.583650	527.370965	9.565722
7.097614	532.149296	9.570739
7.351100	530.616908	9.575757
7.329474	522.405761	9.580775
7.222586	537.680858	9.585792
7.259089	543.983625	9.590810
7.382226	555.303182	9.595827
7.561130	552.258222	9.600845
8.007326	547.350480	9.605863
7.666484	559.667389	9.610880
7.878525	557.769108	9.615898
7.717241	558.125764	9.620915
7.762944	561.438543	9.625933
8.283585	557.462722	9.630951
8.006944	552.030762	9.635968
8.188876	550.635816	9.640986
7.963847	558.412304	9.646003
7.820364	547.780795	9.651021
7.886840	537.372017	9.656039
7.423838	552.586158	9.661056
7.951182	553.178902	9.666074
7.563422	556.171431	9.671091
7.684638	556.351281	9.676109
8.044182	551.169936	9.681127
7.968859	555.965973	9.686144
7.952230	556.808050	9.691162
7.690872	560.405626	9.696179
7.532854	556.372037	9.701197
7.695188	553.294959	9.706215
7.452120	566.757892	9.711232
7.563845	556.383038	9.716250
7.535801	561.222161	9.721267
8.242984	562.137023	9.726285
7.912173	552.251232	9.731303
7.931334	557.281774	9.736320
7.493754	555.895532	9.741338
7.846730	552.504561	9.746355
7.595390	559.824424	9.751373
7.829493	557.891127	9.756391
7.947100	559.299153	9.761408
8.016768	573.539913	9.766426
7.694961	570.687012	9.771443
7.752887	588.293722	9.776461
8.179059	583.196603	9.781479
7.849724	585.769727	9.786496
8.366511	582.009100	9.791514
8.010737	585.665655	9.796531
8.124917	586.433590	9.801549
8.011083	574.721286	9.806567
7.476521	567.395219	9.811584
7.799033	579.986904	9.816602
7.975059	592.544744	9.821619
7.964987	582.627617	9.826637
7.732818	590.345277	9.831655
8.218636	592.232102	9.836672
8.335844	590.585362	9.841690
8.091307	589.863151	9.846707
7.936347	593.623944	9.851725
8.168885	591.397398	9.856743
7.680236	597.119744	9.861760
8.016908	591.449664	9.866778
8.161706	591.767831	9.871795
7.566552	594.758148	9.876813
8.217382	592.803735	9.881831
8.212329	591.684238	9.886848
8.232450	590.298863	9.891866
8.123680	594.140782	9.896883
7.940604	593.563576	9.901901
8.051824	590.620733	9.906919
8.051874	588.926078	9.911936
8.307232	585.793393	9.916954
7.892687	593.126217	9.921971
7.941889	597.145358	9.926989
8.355544	589.901086	9.932007
8.210953	602.461832	9.937024
8.129639	593.127065	9.942042
8.240769	594.217371	9.947059
8.209920	598.031302	9.952077
8.418829	591.911024	9.957095
8.286936	602.402719	9.962112
8.137554	584.734638	9.967130
8.508916	586.737226	9.972147
8.143502	588.482868	9.977165
8.304036	585.153601	9.982183
8.351738	585.537474	9.987200
8.134882	583.176214	9.992218
8.606894	587.208000	9.997235
7.836770	589.768137	10.002253
8.188102	595.447236	10.007271
8.635977	601.950657	10.012288
8.421210	591.557511	10.017306
8.566302	597.922178	10.022323
8.295723	588.071112	10.027341
8.378280	587.019939	10.032359
8.209464	594.737142	10.037376
8.147558	585.112158	10.042394
8.452225	584.168197	10.047411
8.120200	599.611166	10.052429
8.353168	598.451218	10.057447
8.390476	607.852896	10.062464
8.717524	612.017855	10.067482
8.505520	599.522494	10.072499
8.043936	599.910424	10.077517
8.538598	593.956812	10.082535
8.425002	601.886273	10.087552
8.283555	600.879664	10.092570
8.417033	616.132946	10.097587
8.218426	614.084404	10.102605
8.650313	613.612816	10.107623
8.494612	613.075501	10.112640
8.601306	612.979915	10.117658
8.768255	611.801908	10.122675
8.081988	604.815176	10.127693
8.485056	597.556782	10.132711
8.432740	605.565006	10.137728
8.653967	604.772973	10.142746
8.859881	605.072096	10.147763
8.363132	606.229245	10.152781
8.621357	605.494531	10.157799
8.535640	607.748619	10.162816
8.313422	609.045791	10.167834
8.901797	607.653431	10.172851
8.060053	608.126172	10.177869
8.505290	609.205156	10.182887
8.466371	616.103593	10.187904
8.445067	614.951926	10.192922
8.790166	600.993338	10.197939
8.413318	615.117899	10.202957
8.660924	613.576959	10.207975
8.687465	608.769667	10.212992
8.513073	611.798203	10.218010
8.640383	611.992877	10.223027
8.542742	617.546668	10.228045
8.554176	613.417088	10.233063
8.229905	614.209540	10.238080
8.277682	612.516872	10.243098
8.157962	617.925798	10.248115
8.162445	622.775621	10.253133
8.788278	634.862225	10.258151
8.754948	641.283266	10.263168
8.834715	643.031745	10.268186
9.090518	643.932127	10.273203
8.746948	643.294859	10.278221
8.593133	625.075163	10.283239
8.642511	626.389742	10.288256
8.813806	632.358994	10.293274
9.033987	642.861822	10.298291
8.693630	634.728965	10.303309
8.761844	618.276463	10.308327
8.577807	616.408676	10.313344
8.853044	635.373100	10.318362
8.871943	636.004486	10.323379
8.771284	645.241606	10.328397
9.037881	636.754871	10.333415
8.691946	627.363717	10.338432
8.798433	631.105645	10.343450
8.779757	634.330693	10.348467
8.895201	641.776158	10.353485
8.753622	641.889886	10.358503
8.751351	643.338792	10.363520
8.907124	645.892721	10.368538
8.639010	638.815213	10.373555
8.746783	635.276452	10.378573
8.786872	641.471393	10.383591
8.635832	639.532161	10.388608
8.441469	648.471538	10.393626
9.056559	640.308898	10.398643
8.963494	653.833600	10.403661
9.070912	642.231755	10.408679
9.015631	645.680293	10.413696
8.623169	648.869235	10.418714
8.927412	644.709549	10.423731
8.828576	653.296288	10.428749
8.808938	642.178257	10.433767
8.835318	646.254633	10.438784
8.596600	646.948474	10.443802
8.954653	640.470292	10.448819
8.772585	646.008918	10.453837
8.631246	664.262310	10.458855
9.145407	664.904461	10.463872
9.076983	674.521557	10.468890
9.628399	662.294705	10.473907
9.067528	660.063075	10.478925
9.167585	650.769288	10.483943
8.849324	647.029032	10.488960
8.932844	656.467676	10.493978
8.999191	655.090832	10.498995
9.249145	676.037966	10.504013
8.978753	676.083513	10.509031
8.923935	679.251116	10.514048
9.003545	668.900164	10.519066
9.324756	672.112991	10.524083
8.954531	681.979352	10.529101
8.892645	674.667543	10.534119
9.339500	675.938783	10.539136
9.057892	673.802252	10.544154
9.496322	662.173777	10.549171
9.210128	663.001290	10.554189
9.098135	670.293052	10.559207
9.041844	671.482179	10.564224
9.036317	671.309500	10.569242
9.121548	668.765195	10.574259
8.891124	676.413190	10.579277
9.235821	675.674393	10.584295
9.357633	669.315268	10.589312
9.114353	675.706100	10.594330
9.236321	673.743023	10.599347
9.432426	680.604660	10.604365
9.131090	675.974957	10.609383
9.373512	669.180365	10.614400
9.335299	677.233748	10.619418
9.358898	671.246620	10.624435
9.211784	678.364006	10.629453
9.173997	673.364803	10.634471
9.371881	671.317248	10.639488
8.882875	679.245602	10.644506
9.158801	670.078886	10.649523
9.154400	670.650806	10.654541
9.227654	676.436617	10.659559
9.448335	672.031240	10.664576
9.073960	674.999600	10.669594
9.257056	680.054984	10.674611
9.686259	689.878144	10.679629
9.165734	686.358921	10.684647
9.622280	691.365151	10.689664
9.407605	688.059940	10.694682
9.488877	675.455458	10.699699
9.485683	669.762865	10.704717
9.230914	671.308140	10.709735
9.316276	675.779228	10.714752
9.470661	701.228959	10.719770
9.566474	705.344963	10.724787
9.249789	699.736193	10.729805
9.485349	704.309988	10.734823
9.701987	701.782959	10.739840
9.293636	704.428441	10.744858
9.406937	698.181094	10.749875
9.285794	697.445856	10.754893
9.471711	706.278341	10.759911
9.693152	702.491381	10.764928
9.711081	699.711462	10.769946
9.810430	700.181920	10.774963
9.695345	701.241404	10.779981
9.319767	699.551943	10.784999
9.808478	690.740044	10.790016
9.490706	695.864442	10.795034
9.497353	702.165631	10.800051
9.676980	701.316995	10.805069
9.420119	703.623158	10.810087
9.677719	698.363069	10.815104
9.414931	700.108421	10.820122
9.479359	704.497588	10.825139
10.057422	711.536079	10.830157
9.703025	708.792405	10.835175
10.182421	701.916488	10.840192
9.269792	698.821619	10.845210
9.140391	695.768136	10.850227
9.891430	693.738051	10.855245
9.328267	708.074917	10.860263
9.701940	696.686941	10.865280
9.665784	705.547909	10.870298
9.502932	702.831029	10.875315
9.276721	698.842807	10.880333
9.738505	705.145269	10.885351
10.056090	700.200832	10.890368
9.998571	702.134931	10.895386
9.450083	707.667870	10.900403
9.618077	708.683001	10.905421
9.613637	705.051353	10.910439
9.925897	697.703004	10.915456
9.855073	706.982819	10.920474
9.666377	701.161489	10.925491
9.580159	696.498074	10.930509
9.416684	693.314229	10.935527
10.172922	705.503527	10.940544
10.147213	710.594792	10.945562
10.202230	698.704471	10.950579
10.169136	704.226084	10.955597
9.853079	706.775054	10.960615
10.144502	699.792890	10.965632
9.831588	703.546896	10.970650
9.690349	701.268447	10.975667
10.147949	696.033827	10.980685
9.849394	698.466443	10.985703
10.010460	703.493727	10.990720
9.969242	696.153425	10.995738
9.944322	700.736473	11.000755
9.688320	695.758831	11.005773
9.547624	699.668891	11.010791
9.795628	689.629217	11.015808
9.903258	709.923342	11.020826
9.899111	715.550877	11.025843
10.193281	719.982948	11.030861
10.094846	724.984625	11.035879
9.947625	707.057305	11.040896
9.860795	717.314787	11.045914
9.894151	723.706474	11.050931
9.982521	723.231901	11.055949
9.936103	725.650263	11.060967
10.299027	720.136977	11.065984
10.081103	726.539633	11.071002
9.930250	732.142823	11.076019
10.083753	722.973170	11.081037
10.226976	730.082956	11.086055
9.916795	732.653100	11.091072
10.415378	730.425878	11.096090
9.798778	727.922101	11.101107
10.086816	714.868624	11.106125
10.370603	732.146594	11.111143
10.099047	722.103100	11.116160
9.919758	722.295321	11.121178
10.289376	723.300953	11.126195
10.180295	717.274636	11.131213
10.021897	722.771707	11.136231
10.212855	726.658211	11.141248
10.347806	722.487162	11.146266
10.329049	723.733528	11.151283
10.448397	710.318317	11.156301
10.474681	716.726889	11.161319
10.411718	723.553394	11.166336
10.540907	725.985266	11.171354
10.332849	728.280629	11.176371
10.427157	712.291018	11.181389
10.237905	724.918808	11.186407
10.032633	721.214481	11.191424
10.139667	720.011141	11.196442
10.167802	722.717625	11.201459
10.073867	721.716189	11.206477
10.141064	729.342821	11.211495
10.512339	722.111448	11.216512
10.473120	724.257279	11.221530
9.900395	726.893804	11.226547
10.000424	721.936111	11.231565
10.312782	733.440731	11.236583
10.274736	726.819451	11.241600
10.292927	723.944811	11.246618
10.377773	732.016808	11.251635
10.639299	731.963235	11.256653
10.060723	739.025169	11.261671
9.965039	741.520680	11.266688
10.438027	749.175260	11.271706
10.425501	752.298379	11.276723
10.623999	748.811654	11.281741
10.475710	751.640460	11.286759
10.599096	757.544677	11.291776
10.520551	750.588902	11.296794
10.803094	749.383307	11.301811
10.815380	742.264979	11.306829
10.443713	757.793191	11.311847
10.493603	744.385682	11.316864
10.492508	739.630023	11.321882
10.496516	747.998719	11.326899
10.597444	749.803854	11.331917
10.887969	745.690476	11.336935
10.845843	755.148858	11.341952
10.472849	747.645921	11.346970
10.544365	743.210248	11.351987
10.684468	737.725557	11.357005
10.720634	750.696747	11.362023
10.562430	754.092004	11.367040
10.749910	746.529653	11.372058
10.344290	759.974018	11.377075
11.023438	751.485706	11.382093
10.829771	746.829647	11.387111
10.674042	748.700242	11.392128
10.710438	750.509176	11.397146
10.989058	747.088793	11.402163
10.986605	731.351013	11.407181
10.474854	727.401212	11.412199
10.482870	734.601613	11.417216
10.684358	737.549185	11.422234
10.669689	749.026158	11.427251
10.784989	746.701196	11.432269
10.761356	747.853652	11.437287
10.690624	749.673060	11.442304
11.014791	740.558710	11.447322
10.843358	755.001495	11.452339
10.526376	749.768301	11.457357
10.667634	757.812536	11.462375
10.647563	751.627093	11.467392
10.874900	746.753589	11.472410
10.626673	759.182357	11.477427
10.738767	753.638934	11.482445
10.939928	750.606232	11.487463
10.818664	752.465116	11.492480
10.946854	754.540538	11.497498
10.725439	753.155125	11.502515
10.728881	744.678013	11.507533
10.785098	760.994420	11.512551
10.647552	753.252615	11.517568
10.669322	746.429449	11.522586
11.114833	769.018648	11.527603
10.977813	773.922241	11.532621
10.674511	772.148864	11.537639
10.966186	783.284366	11.542656
11.232356	784.647042	11.547674
11.192359	785.139336	11.552691
11.004247	784.140028	11.557709
11.164019	775.275484	11.562727
10.908414	782.555079	11.567744
11.174261	774.503904	11.572762
11.086352	786.491000	11.577779
11.435461	775.008992	11.582797
10.962770	760.998530	11.587815
10.783726	764.337093	11.592832
11.094989	767.759782	11.597850
10.743452	782.622134	11.602867
11.357468	780.903847	11.607885
11.344635	786.996676	11.612903
11.262636	780.312834	11.617920
11.220824	782.080376	11.622938
10.655982	777.722310	11.627955
10.701091	781.795782	11.632973
11.421349	783.551220	11.637991
11.230536	789.880223	11.643008
11.174789	780.992639	11.648026
11.051361	785.679507	11.653043
11.411791	780.450620	11.658061
11.076214	778.802222	11.663079
11.253000	791.558902	11.668096
11.091557	784.950623	11.673114
10.825408	780.785601	11.678131
10.972253	781.721997	11.683149
11.003331	786.248956	11.688167
10.949313	800.228405	11.693184
11.776456	801.821929	11.698202
11.498715	800.934495	11.703219
11.597644	790.473147	11.708237
11.492966	778.421599	11.713255
11.164683	781.234430	11.718272
11.314773	771.399403	11.723290
11.027548	786.485214	11.728307
11.458488	788.989739	11.733325
11.903454	797.260965	11.738343
11.163069	793.182867	11.743360
11.519147	790.450939	11.748378
11.451291	794.864012	11.753395
11.503294	786.862116	11.758413
11.450238	780.726013	11.763431
11.313140	792.206416	11.768448
11.437826	787.377388	11.773466
11.692720	799.093028	11.778483
11.563075	793.527507	11.783501
11.677951	787.986792	11.788519
11.361659	778.373160	11.793536
12.011212	776.213798	11.798554
11.658946	775.836667	11.803571
11.487882	779.909295	11.808589
11.830591	770.526933	11.813607
11.593492	783.600924	11.818624
11.627828	778.186443	11.823642
11.688915	780.054628	11.828659
11.648353	771.830554	11.833677
11.642938	767.795098	11.838695
11.254156	778.595394	11.843712
11.588649	776.655812	11.848730
11.285794	780.408258	11.853747
11.720665	788.106697	11.858765
11.624897	785.846359	11.863783
11.336705	806.502417	11.868800
11.579748	807.032417	11.873818
11.331031	809.523512	11.878835
11.644904	806.659337	11.883853
11.543780	810.616870	11.888871
11.606491	804.528893	11.893888
11.266168	801.883986	11.898906
11.345068	811.575905	11.903923
11.577985	807.742942	11.908941
11.644099	812.400120	11.913959
11.074811	835.337756	11.918976
11.997468	831.043262	11.923994
11.757974	834.994079	11.929011
11.443478	834.203922	11.934029
11.889942	828.989944	11.939047
11.567627	833.562817	11.944064
11.742683	837.366629	11.949082
11.795506	837.784420	11.954099
11.616107	846.327068	11.959117
11.999828	833.473112	11.964135
11.890368	842.755895	11.969152
11.752141	834.449263	11.974170
11.954306	838.400309	11.979187
12.074064	834.865942	11.984205
12.140869	830.437298	11.989223
12.119027	842.562405	11.994240
12.167324	847.108772	11.999258
12.225842	843.202140	12.004275
12.039743	837.531840	12.009293
12.222783	832.431720	12.014311
12.102146	837.957623	12.019328
12.045373	840.538571	12.024346
12.044791	842.675206	12.029363
12.240620	844.957796	12.034381
12.298264	837.018111	12.039399
12.216475	829.914488	12.044416
12.250544	835.308852	12.049434
12.073648	826.001563	12.054451
11.835862	832.956488	12.059469
12.138282	830.955654	12.064487
11.899900	833.322054	12.069504
11.776923	832.186304	12.074522
11.933390	831.429655	12.079539
11.811285	833.900915	12.084557
12.263486	838.832128	12.089575
12.113392	833.282422	12.094592
12.112411	835.791510	12.099610
12.104170	832.056289	12.104627
11.912896	833.743111	12.109645
12.274890	848.932384	12.114663
12.132875	851.409923	12.119680
12.180262	861.845277	12.124698
12.556392	856.468739	12.129715
12.552882	853.546985	12.134733
12.447847	842.208676	12.139751
12.286332	846.658527	12.144768
12.231108	837.792923	12.149786
12.501992	828.661630	12.154803
11.623146	833.744587	12.159821
12.357329	846.827391	12.164839
12.150285	859.716844	12.169856
12.429109	853.112142	12.174874
12.405619	860.399582	12.179891
12.025389	862.652510	12.184909
12.367326	858.669909	12.189927
12.386638	860.188036	12.194944
12.499888	862.180603	12.199962
12.331302	864.719112	12.204979
12.098168	861.514593	12.209997
12.350405	857.571293	12.215015
12.263859	868.542043	12.220032
12.298177	867.230163	12.225050
12.555913	863.203949	12.230067
12.225934	853.352575	12.235085
12.375802	860.016395	12.240103
12.351248	873.713569	12.245120
12.277266	881.387633	12.250138
12.513907	889.372800	12.255155
12.696021	888.908782	12.260173
12.537557	887.469313	12.265191
12.676763	895.125760	12.270208
12.416691	891.644583	12.275226
13.010052	891.649472	12.280243
12.845262	888.951802	12.285261
12.975499	886.507715	12.290279
12.983837	881.292939	12.295296
12.826717	866.892115	12.300314
12.342329	870.275384	12.305331
12.744863	866.242260	12.310349
12.642954	858.497982	12.315367
12.769825	867.065238	12.320384
12.910051	869.899352	12.325402
13.050245	859.100132	12.330419
12.616612	864.350030	12.335437
12.713058	856.502089	12.340455
12.521049	863.295217	12.345472
12.726882	876.605995	12.350490
13.105033	877.035931	12.355507
12.953121	876.617937	12.360525
13.181838	856.147898	12.365543
13.349131	860.498896	12.370560
12.896431	860.645592	12.375578
13.007194	854.770980	12.380595
12.984558	854.357979	12.385613
12.701266	856.434768	12.390631
12.562070	849.636783	12.395648
12.887276	853.647451	12.400666
13.260503	853.008320	12.405683
12.534303	862.075315	12.410701
12.658038	855.510691	12.415719
12.478398	856.400414	12.420736
13.006885	871.645673	12.425754
13.041919	876.178346	12.430771
13.006875	888.595893	12.435789
13.347577	882.375970	12.440807
13.317354	869.097686	12.445824
12.793485	863.900029	12.450842
13.156954	850.459087	12.455859
12.611727	857.799871	12.460877
12.854272	874.096654	12.465895
12.914625	879.146079	12.470912
12.740873	889.663437	12.475930
12.973716	890.905108	12.480947
12.850913	887.705387	12.485965
13.297133	889.194498	12.490983
13.433287	883.050805	12.496000
13.048077	885.844169	12.501018
13.198343	876.731751	12.506035
13.262645	889.294682	12.511053
13.333045	882.170349	12.516071
13.148030	877.326703	12.521088
12.616947	879.495969	12.526106
12.928244	877.935560	12.531123
13.150087	887.264288	12.536141
13.118497	885.495666	12.541159
13.341712	887.802373	12.546176
12.848736	894.017806	12.551194
13.114418	892.723324	12.556211
13.236368	906.852014	12.561229
12.869615	906.549735	12.566247
13.013938	911.462933	12.571264
13.042410	914.567034	12.576282
13.345632	908.823199	12.581299
13.033311	918.017882	12.586317
13.444874	910.912669	12.591335
13.435949	912.185910	12.596352
13.192896	916.187796	12.601370
13.477062	915.594176	12.606387
13.458580	913.722509	12.611405
13.529390	914.124859	12.616423
13.875720	909.709204	12.621440
13.604956	922.043785	12.626458
13.586086	917.950441	12.631475
13.449524	909.305834	12.636493
13.437634	914.369745	12.641511
13.823375	915.032027	12.646528
13.851229	912.521925	12.651546
13.738888	904.236451	12.656563
13.991108	908.463698	12.661581
13.652888	903.959637	12.666599
13.739908	902.336534	12.671616
13.219630	915.423431	12.676634
13.567323	906.996448	12.681651
13.532209	908.636717	12.686669
13.814899	905.004224	12.691687
13.520026	909.052098	12.696704
13.598868	910.513563	12.701722
13.686862	909.082815	12.706739
13.598755	901.557267	12.711757
13.722772	911.554601	12.716775
13.751691	903.704596	12.721792
13.508257	903.543944	12.726810
13.603663	896.706027	12.731827
13.655033	906.667403	12.736845
13.329619	912.724043	12.741863
13.605671	903.531941	12.746880
13.435090	916.052796	12.751898
13.816711	914.254142	12.756915
13.589995	921.324135	12.761933
13.900643	925.131968	12.766951
14.111082	920.456729	12.771968
13.886661	922.508522	12.776986
13.807342	924.376631	12.782003
13.922244	927.132669	12.787021
13.791451	932.849545	12.792039
14.295145	935.831853	12.797056
14.276482	921.264121	12.802074
14.227882	907.496371	12.807091
13.964378	906.808677	12.812109
13.811552	908.647275	12.817127
13.809371	899.855382	12.822144
13.694352	898.424885	12.827162
13.968105	901.108692	12.832179
14.279447	900.747505	12.837197
14.013690	898.999791	12.842215
14.092838	898.138486	12.847232
13.937135	905.301490	12.852250
14.084064	900.939171	12.857267
13.739158	910.019033	12.862285
14.001102	923.478848	12.867303
14.156596	927.456161	12.872320
13.981015	933.710243	12.877338
14.225603	927.303387	12.882355
14.440298	935.093193	12.887373
14.054156	927.759501	12.892391
14.320237	932.091882	12.897408
14.153916	927.743922	12.902426
14.323523	932.176628	12.907443
14.447231	928.237672	12.912461
13.947099	938.058253	12.917479
14.164100	928.607140	12.922496
14.243167	938.396933	12.927514
14.101460	932.763829	12.932531
14.209139	933.914659	12.937549
14.291449	931.011005	12.942567
14.117222	925.351439	12.947584
14.380358	937.498234	12.952602
14.322653	938.302582	12.957619
14.658043	934.579773	12.962637
14.202272	938.722292	12.967655
14.418763	932.648048	12.972672
14.304378	939.580525	12.977690
13.946852	941.580590	12.982707
14.364742	941.944339	12.987725
14.397785	938.688633	12.992743
14.160082	941.405244	12.997760
14.285998	947.391179	13.002778
14.167771	929.686317	13.007795
14.427033	933.530606	13.012813
14.163594	944.055736	13.017831
14.268514	951.152676	13.022848
14.834342	965.994524	13.027866
14.543242	956.714528	13.032883
14.754371	962.005446	13.037901
14.374491	957.558393	13.042919
14.611520	953.857303	13.047936
14.607578	960.788263	13.052954
14.462278	959.987369	13.057971
14.415049	956.747393	13.062989
14.287143	970.173649	13.068007
14.318911	966.043958	13.073024
14.710560	967.737290	13.078042
14.594450	966.774029	13.083059
14.867025	960.687832	13.088077
14.515877	963.841953	13.093095
14.748662	954.501966	13.098112
14.661016	965.103709	13.103130
14.818827	974.294189	13.108147
14.829022	958.516358	13.113165
14.875183	964.981866	13.118183
14.745749	953.426397	13.123200
14.672844	959.800103	13.128218
14.557070	955.384255	13.133235
14.522011	961.193440	13.138253
14.499971	973.927753	13.143271
14.976761	980.423628	13.148288
15.139111	988.240594	13.153306
14.701540	974.388567	13.158323
14.709915	976.378644	13.163341
14.713239	987.613103	13.168359
14.953256	985.640964	13.173376
14.888442	993.386225	13.178394
14.874863	993.905944	13.183411
15.143020	981.246719	13.188429
14.815471	990.068275	13.193447
14.882059	986.930384	13.198464
15.157621	987.714077	13.203482
14.927614	989.804623	13.208499
15.005402	988.025164	13.213517
15.278183	995.439813	13.218535
15.226368	999.017267	13.223552
15.015820	997.507053	13.228570
14.963701	989.492978	13.233587
15.159039	991.693610	13.238605
15.052570	999.701027	13.243623
15.100689	992.835768	13.248640
15.151292	990.845968	13.253658
15.212025	994.923353	13.258675
15.126886	995.801432	13.263693
14.945089	995.220856	13.268711
15.199076	997.415456	13.273728
15.571657	985.879142	13.278746
15.289371	992.572851	13.283763
15.593840	993.973725	13.288781
15.211670	991.963368	13.293799
15.123267	994.230549	13.298816
15.285222	983.576171	13.303834
15.454542	989.227108	13.308851
15.741456	989.352598	13.313869
15.482177	988.556938	13.318887
15.454927	989.880395	13.323904
15.520851	994.704912	13.328922
15.300428	988.115266	13.333939
15.476311	985.563025	13.338957
15.353679	992.506281	13.343975
15.199139	995.844203	13.348992
15.513151	988.006299	13.354010
15.483701	991.801159	13.359027
15.705466	983.100373	13.364045
15.307670	990.080431	13.369063
15.239388	995.342553	13.374080
15.540044	986.818757	13.379098
15.841565	997.327985	13.384115
15.852465	978.214251	13.389133
15.727769	987.786682	13.394151
15.675494	985.863496	13.399168
15.556479	992.850369	13.404186
15.397826	994.781409	13.409203
15.990787	991.753553	13.414221
15.506229	990.750187	13.419239
15.490820	997.499916	13.424256
15.634204	987.173503	13.429274
15.793185	990.386560	13.434291
15.754658	992.002125	13.439309
15.667424	984.441690	13.444327
15.615881	994.109962	13.449344
15.461284	991.997675	13.454362
15.171581	1001.109960	13.459379
15.550005	982.595062	13.464397
15.447244	991.321437	13.469415
15.693658	1012.515678	13.474432
16.081641	1016.194646	13.479450
15.840116	1010.712860	13.484467
15.987423	1010.519388	13.489485
15.903882	1012.908889	13.494503
15.789514	1010.815544	13.499520
15.973120	1017.218509	13.504538
15.635661	1018.890381	13.509555
15.971162	1003.389753	13.514573
15.921255	1012.997818	13.519591
15.960206	1013.979535	13.524608
16.014699	1020.263872	13.529626
15.754601	1021.106247	13.534643
16.091171	1006.037807	13.539661
15.906195	1012.242894	13.544679
15.715537	1020.607503	13.549696
15.927735	1005.356573	13.554714
15.787097	1012.138552	13.559731
15.983671	1015.721275	13.564749
15.998863	1013.279416	13.569767
15.914397	1011.954578	13.574784
16.048358	1011.485479	13.579802
16.122756	1011.776813	13.584819
15.948324	1007.808812	13.589837
16.235509	1018.096230	13.594855
16.125120	1023.241877	13.599872
16.253113	1019.081318	13.604890
16.231948	1034.561163	13.609907
15.970538	1028.394503	13.614925
16.317111	1025.212736	13.619943
16.308143	1032.564245	13.624960
16.440583	1024.221427	13.629978
16.325339	1027.303883	13.634995
16.490862	1031.131321	13.640013
16.771264	1034.868175	13.645031
16.439850	1023.161266	13.650048
16.573780	1006.272066	13.655066
16.469414	1011.356805	13.660083
16.302247	1005.273219	13.665101
16.267037	1006.462220	13.670119
16.238840	1006.895865	13.675136
16.522441	1007.656208	13.680154
16.311349	1014.509189	13.685171
16.522600	1022.984402	13.690189
16.508050	1027.802601	13.695207
16.298195	1031.966573	13.700224
16.511023	1025.088119	13.705242
16.478005	1034.734575	13.710259
17.074195	1032.318451	13.715277
16.961586	1025.206955	13.720295
16.639853	1013.615303	13.725312
16.421644	1000.883942	13.730330
16.374542	1010.658828	13.735347
16.567798	1011.676330	13.740365
16.854470	1026.628241	13.745383
16.365338	1036.055821	13.750400
16.770327	1025.846192	13.755418
16.962838	1034.987084	13.760435
16.645560	1032.893969	13.765453
16.789343	1028.620477	13.770471
16.421975	1032.957455	13.775488
16.374957	1021.376406	13.780506
16.365873	1028.317665	13.785523
16.373332	1025.930666	13.790541
16.456784	1020.745108	13.795559
16.315154	1022.446260	13.800576
16.961700	1020.129547	13.805594
16.620072	1025.425038	13.810611
16.710888	1049.174730	13.815629
17.297538	1044.434202	13.820647
17.034241	1040.114032	13.825664
17.025269	1032.276220	13.830682
16.655281	1029.440261	13.835699
16.825149	1040.418278	13.840717
17.348439	1047.673775	13.845735
16.768800	1042.907694	13.850752
17.195831	1041.054575	13.855770
17.045041	1050.801546	13.860787
17.237497	1039.934067	13.865805
17.035948	1037.330499	13.870823
16.948402	1031.035607	13.875840
17.033334	1027.598180	13.880858
16.823693	1045.244106	13.885875
17.047468	1045.155421	13.890893
17.101289	1046.362034	13.895911
17.543609	1061.235937	13.900928
17.193867	1053.435728	13.905946
17.301949	1053.570302	13.910963
17.266856	1051.313048	13.915981
17.114195	1049.178359	13.920999
17.042105	1054.564175	13.926016
17.408271	1049.870814	13.931034
17.578520	1057.733912	13.936051
17.457231	1046.792507	13.941069
17.465621	1034.625238	13.946087
17.228081	1039.576212	13.951104
16.993227	1023.959797	13.956122
17.363077	1041.436026	13.961139
17.367097	1043.360520	13.966157
16.985163	1048.573968	13.971175
17.121026	1047.085214	13.976192
17.328418	1043.802171	13.981210
17.348987	1050.940771	13.986227
17.226239	1047.198199	13.991245
17.688316	1055.949717	13.996263
17.534548	1038.048339	14.001280
17.270976	1047.759329	14.006298
17.443353	1046.444741	14.011315
17.264311	1048.483126	14.016333
17.520304	1041.320183	14.021351
17.236792	1045.965927	14.026368
17.611307	1048.119558	14.031386
17.343365	1047.309473	14.036403
17.682861	1060.425871	14.041421
17.656108	1059.041493	14.046439
17.505042	1064.417595	14.051456
17.723269	1066.863967	14.056474
17.752860	1070.299289	14.061491
17.784569	1077.631819	14.066509
17.998786	1076.755655	14.071527
17.524627	1056.657454	14.076544
17.633612	1062.904865	14.081562
17.826854	1065.449829	14.086579
17.610051	1080.938276	14.091597
18.002440	1079.024307	14.096615
18.078117	1078.687417	14.101632
17.756590	1069.677225	14.106650
17.608084	1072.714406	14.111667
17.765641	1074.712679	14.116685
18.228118	1060.833176	14.121703
17.987074	1072.150159	14.126720
18.282719	1072.586715	14.131738
18.000677	1049.031113	14.136755
17.862230	1046.291421	14.141773
17.779206	1047.860312	14.146791
17.633436	1065.332144	14.151808
17.793427	1071.237041	14.156826
18.280526	1073.824328	14.161843
17.833537	1074.301501	14.166861
17.872184	1070.969151	14.171879
17.775285	1078.883583	14.176896
17.766083	1065.939541	14.181914
18.054434	1075.399963	14.186931
18.178491	1069.696772	14.191949
18.080484	1069.339758	14.196967
17.931595	1081.276644	14.201984
18.152840	1080.898011	14.207002
18.358149	1081.784237	14.212019
18.007828	1073.640116	14.217037
18.021145	1074.521708	14.222055
17.930992	1077.720165	14.227072
17.959618	1093.359523	14.232090
17.813319	1096.263814	14.237107
17.985225	1106.806038	14.242125
18.622974	1101.546231	14.247143
18.434610	1097.397350	14.252160
18.503431	1101.782771	14.257178
18.537815	1094.348406	14.262195
18.191316	1090.760807	14.267213
18.758775	1098.725794	14.272231
18.746376	1100.952677	14.277248
18.583510	1101.031872	14.282266
18.779793	1096.213634	14.287283
18.713981	1102.311715	14.292301
18.634869	1085.354832	14.297319
18.668225	1075.266520	14.302336
18.468319	1066.590735	14.307354
18.474017	1074.148253	14.312371
17.845600	1070.185094	14.317389
18.625583	1084.393866	14.322407
18.659213	1087.670763	14.327424
18.674591	1102.838820	14.332442
18.792791	1100.074687	14.337459
18.648574	1100.526512	14.342477
18.753307	1094.731664	14.347495
18.705335	1093.404258	14.352512
18.705229	1099.084932	14.357530
18.785731	1100.442008	14.362547
18.739623	1094.102731	14.367565
18.769329	1085.965335	14.372583
18.589115	1090.560191	14.377600
18.532460	1092.257503	14.382618
18.692473	1088.915602	14.387635
18.280668	1097.788283	14.392653
18.486298	1096.963958	14.397671
18.529442	1096.837299	14.402688
18.590918	1115.485421	14.407706
19.018756	1113.524867	14.412723
18.713528	1122.854247	14.417741
18.662677	1124.288712	14.422759
18.987788	1115.880949	14.427776
18.877916	1117.848542	14.432794
19.438391	1117.953263	14.437811
19.129178	1121.340690	14.442829
19.339316	1115.567191	14.447847
19.147152	1124.796804	14.452864
19.005096	1127.990778	14.457882
18.980661	1120.256339	14.462899
19.192071	1115.577741	14.467917
19.191085	1125.373868	14.472935
19.512554	1113.763426	14.477952
19.494584	1122.637531	14.482970
19.720603	1098.374233	14.487987
19.352038	1104.238875	14.493005
18.740677	1096.337622	14.498023
18.660066	1093.721409	14.503040
18.778039	1108.964917	14.508058
19.269199	1114.350866	14.513075
19.105327	1126.286973	14.518093
18.985657	1122.165194	14.523111
19.240192	1115.781959	14.528128
19.010142	1123.515295	14.533146
19.455024	1121.286973	14.538163
19.506099	1130.771978	14.543181
19.374443	1121.511097	14.548199
19.981938	1123.899642	14.553216
19.344228	1125.669062	14.558234
19.517542	1122.268264	14.563251
19.269499	1126.816951	14.568269
19.469738	1122.007553	14.573287
19.301261	1124.744904	14.578304
19.062355	1129.427864	14.583322
19.079919	1129.734417	14.588339
19.428804	1143.130282	14.593357
19.447586	1152.986444	14.598375
19.885995	1153.646796	14.603392
19.417022	1149.923735	14.608410
19.755641	1142.113466	14.613427
19.731015	1154.239221	14.618445
19.488015	1139.712773	14.623463
19.645388	1139.511410	14.628480
19.704481	1146.659791	14.633498
20.032941	1142.259504	14.638515
19.941863	1153.726616	14.643533
19.903895	1138.811425	14.648551
19.980901	1141.810128	14.653568
19.799600	1141.513501	14.658586
20.043104	1134.507117	14.663603
19.908048	1134.187466	14.668621
19.832808	1130.459524	14.673639
20.078087	1128.893658	14.678656
19.667848	1145.116237	14.683674
20.011894	1140.580959	14.688691
19.615968	1141.662379	14.693709
19.750706	1139.214396	14.698727
19.716684	1134.388050	14.703744
19.743218	1139.872052	14.708762
20.237053	1136.487306	14.713779
20.066608	1135.027602	14.718797
20.083909	1133.718369	14.723815
20.060205	1135.653528	14.728832
20.018723	1137.828166	14.733850
19.756418	1141.574333	14.738867
20.321504	1140.810455	14.743885
20.195137	1140.877619	14.748903
20.211208	1134.752655	14.753920
19.797105	1149.713478	14.758938
20.544533	1153.276194	14.763955
20.290330	1142.103082	14.768973
20.154078	1146.741559	14.773991
20.402856	1150.164646	14.779008
20.055033	1158.421396	14.784026
20.691777	1162.891424	14.789043
20.458286	1162.732367	14.794061
20.385445	1153.992448	14.799079
20.414835	1151.838690	14.804096
20.218401	1146.488658	14.809114
20.508429	1158.382072	14.814131
20.740551	1162.154921	14.819149
20.424242	1144.196849	14.824167
20.610121	1133.005285	14.829184
20.454556	1143.737700	14.834202
20.573083	1133.901108	14.839219
20.340683	1141.622196	14.844237
20.668407	1141.050148	14.849255
20.514827	1136.252001	14.854272
20.582793	1151.124670	14.859290
20.480327	1149.408153	14.864307
20.818596	1160.924769	14.869325
20.590542	1166.802131	14.874343
20.793171	1160.423857	14.879360
20.908242	1171.628300	14.884378
21.037075	1158.731994	14.889395
20.516907	1143.734554	14.894413
20.463040	1143.708305	14.899431
20.310775	1156.829238	14.904448
20.650156	1161.626734	14.909466
20.674023	1168.162083	14.914483
20.687028	1170.523855	14.919501
20.924856	1171.875222	14.924519
20.933660	1162.305124	14.929536
20.735157	1166.230654	14.934554
20.855129	1156.286522	14.939571
20.727630	1161.400175	14.944589
20.495199	1167.896783	14.949607
20.944247	1165.478448	14.954624
20.970356	1170.527009	14.959642
21.013683	1169.608186	14.964659
21.049347	1172.244129	14.969677
20.845832	1178.701495	14.974695
21.126833	1177.612884	14.979712
20.818494	1186.523047	14.984730
21.215883	1195.597207	14.989747
21.357170	1190.115349	14.994765
21.492444	1187.026623	14.999783
21.421812	1185.854245	15.004800
21.001781	1176.919395	15.009818
21.047800	1183.031541	15.014835
21.772795	1180.314339	15.019853
21.357298	1180.931752	15.024871
21.377315	1163.062981	15.029888
21.021242	1159.991283	15.034906
21.243159	1164.911330	15.039923
21.699918	1171.902737	15.044941
21.284803	1182.672685	15.049959
21.514456	1174.475518	15.054976
21.519897	1185.971711	15.059994
21.381337	1177.674439	15.065011
21.350298	1169.663292	15.070029
21.286349	1172.892375	15.075047
21.434556	1180.538066	15.080064
20.882422	1183.881512	15.085082
21.249684	1177.010362	15.090099
21.276800	1175.122055	15.095117
21.063033	1192.238577	15.100135
21.505644	1175.938350	15.105152
21.200005	1195.287882	15.110170
21.568832	1207.121643	15.115187
21.555024	1204.674834	15.120205
21.444604	1212.443115	15.125223
21.674963	1210.112690	15.130240
21.660956	1211.061688	15.135258
21.635652	1211.914623	15.140275
21.966653	1208.217693	15.145293
21.894540	1205.085716	15.150311
22.296051	1194.147517	15.155328
22.323342	1201.329306	15.160346
22.514119	1192.544908	15.165363
22.553181	1174.900368	15.170381
22.130836	1171.444561	15.175399
22.291683	1164.088186	15.180416
22.568678	1173.155950	15.185434
22.366379	1167.544889	15.190451
22.392798	1155.494638	15.195469
22.124537	1148.243374	15.200487
22.015700	1140.859833	15.205504
22.201516	1134.720896	15.210522
21.992699	1141.078091	15.215539
22.270001	1138.828685	15.220557
21.842710	1142.483933	15.225575
21.899975	1142.585444	15.230592
21.831397	1151.647379	15.235610
21.886082	1152.626639	15.240627
22.027503	1155.438520	15.245645
22.291236	1167.484388	15.250663
22.223163	1166.545149	15.255680
22.072323	1163.327680	15.260698
22.104844	1180.598114	15.265715
22.047256	1171.530737	15.270733
21.971051	1169.090553	15.275751
21.986444	1169.886615	15.280768
22.030994	1171.230394	15.285786
22.494496	1183.147140	15.290803
22.683227	1178.670903	15.295821
22.470333	1182.478767	15.300839
22.446374	1176.789265	15.305856
22.520627	1173.094698	15.310874
22.550254	1175.176146	15.315891
22.611091	1176.482658	15.320909
22.442385	1176.676381	15.325927
22.323019	1181.574163	15.330944
22.197936	1188.915526	15.335962
22.317020	1193.807509	15.340979
22.296345	1194.820670	15.345997
22.345551	1203.548585	15.351015
22.811959	1201.948066	15.356032
22.608051	1205.334789	15.361050
22.524083	1206.648212	15.366067
22.702668	1207.052619	15.371085
22.510437	1206.991242	15.376103
22.267373	1203.071821	15.381120
22.524900	1214.260282	15.386138
22.551972	1225.945624	15.391155
22.755398	1219.904889	15.396173
22.552678	1227.122727	15.401191
22.433888	1221.665829	15.406208
23.097486	1220.387876	15.411226
23.137337	1229.205635	15.416243
23.062886	1223.896430	15.421261
22.909161	1235.010478	15.426279
22.811140	1229.752303	15.431296
22.488045	1224.504147	15.436314
22.806096	1225.306441	15.441331
23.257104	1237.600736	15.446349
23.502900	1244.426402	15.451367
23.204447	1231.417103	15.456384
23.101316	1225.891475	15.461402
22.961442	1221.930635	15.466419
23.194195	1219.524091	15.471437
23.189707	1237.822899	15.476455
23.290159	1253.223916	15.481472
23.559137	1243.865484	15.486490
23.094981	1240.122713	15.491507
23.191469	1231.558205	15.496525
23.409218	1239.041541	15.501543
23.577209	1233.022133	15.506560
23.414150	1237.974115	15.511578
23.122408	1225.670697	15.516595
23.288529	1239.016371	15.521613
23.755932	1250.414978	15.526631
23.611729	1238.202048	15.531648
23.643993	1219.169920	15.536666
23.172052	1227.143180	15.541683
23.854392	1224.347444	15.546701
23.464515	1223.161965	15.551719
23.228747	1221.557848	15.556736
23.449378	1239.329062	15.561754
23.633189	1248.547169	15.566771
23.662393	1248.050294	15.571789
23.946150	1252.373672	15.576807
23.680977	1247.504614	15.581824
23.847949	1251.230883	15.586842
23.658425	1243.399175	15.591859
24.170640	1257.003073	15.596877
24.041225	1229.554144	15.601895
23.856308	1228.989828	15.606912
23.441667	1217.614579	15.611930
23.708158	1228.000039	15.616947
24.068823	1239.472169	15.621965
24.061176	1253.813951	15.626983
24.272076	1237.322745	15.632000
23.965538	1222.500059	15.637018
23.950105	1231.651542	15.642035
23.770148	1227.375076	15.647053
23.997232	1231.814630	15.652071
23.589975	1243.555411	15.657088
24.090712	1246.080625	15.662106
23.869362	1251.171137	15.667123
24.120893	1247.171057	15.672141
24.145167	1242.834184	15.677159
23.848004	1246.506936	15.682176
24.008985	1247.232852	15.687194
23.442333	1249.843251	15.692211
23.807466	1252.162486	15.697229
23.847283	1246.279926	15.702247
24.330445	1265.332367	15.707264
23.831861	1262.374502	15.712282
23.853107	1274.796121	15.717299
24.082352	1269.777004	15.722317
24.526047	1269.732759	15.727335
24.364393	1282.145168	15.732352
24.630423	1274.835387	15.737370
24.394103	1275.831845	15.742387
24.595537	1267.784230	15.747405
24.612192	1270.767162	15.752423
24.413887	1274.074122	15.757440
24.377413	1267.300910	15.762458
24.451347	1275.163415	15.767475
24.466681	1270.297739	15.772493
24.077113	1264.211039	15.777511
24.622845	1274.783157	15.782528
25.009902	1280.134972	15.787546
24.622468	1275.985680	15.792563
24.534472	1269.725490	15.797581
24.901462	1280.966273	15.802599
24.624506	1281.467304	15.807616
24.667128	1286.667951	15.812634
24.279584	1300.078328	15.817651
24.870603	1297.347385	15.822669
24.884587	1291.759205	15.827687
24.731716	1300.733432	15.832704
25.285598	1293.296488	15.837722
25.058198	1299.139075	15.842739
25.161124	1299.747851	15.847757
25.334030	1293.535141	15.852775
24.803606	1283.402496	15.857792
24.858108	1274.689905	15.862810
24.932265	1293.238390	15.867827
25.063920	1285.618285	15.872845
24.988054	1298.979826	15.877863
24.834099	1297.921486	15.882880
25.090460	1284.048858	15.887898
25.004892	1305.254436	15.892915
24.966350	1299.620831	15.897933
25.319189	1293.783889	15.902951
25.142428	1291.889642	15.907968
24.880940	1292.918448	15.912986
25.106270	1291.450372	15.918003
25.012808	1301.687136	15.923021
25.291382	1291.765418	15.928039
25.080000	1303.459768	15.933056
25.246816	1298.081179	15.938074
24.957171	1316.468929	15.943091
25.393881	1319.266129	15.948109
25.432893	1316.063071	15.953127
25.107406	1332.499767	15.958144
25.331530	1323.170414	15.963162
25.514296	1322.709439	15.968179
25.291973	1318.398562	15.973197
25.151829	1316.473327	15.978215
25.618313	1320.301013	15.983232
25.635021	1322.535986	15.988250
25.442173	1323.702369	15.993267
25.682350	1328.928882	15.998285
25.639180	1331.908575	16.003303
25.857061	1339.773802	16.008320
26.054569	1326.525772	16.013338
25.982083	1327.559682	16.018355
25.528218	1314.568361	16.023373
25.939420	1305.881921	16.028391
25.795459	1321.438061	16.033408
25.841680	1315.374586	16.038426
25.797129	1318.761610	16.043443
26.205786	1337.428152	16.048461
26.502871	1327.304690	16.053479
26.061819	1319.291442	16.058496
26.158406	1313.314755	16.063514
26.109712	1311.716034	16.068531
26.034091	1306.605812	16.073549
26.303031	1305.465432	16.078567
25.565477	1306.745562	16.083584
25.982817	1309.331191	16.088602
26.205185	1317.855298	16.093619
26.238863	1314.618359	16.098637
26.700887	1323.518348	16.103655
26.113577	1307.066932	16.108672
26.333637	1304.368863	16.113690
25.968260	1308.541486	16.118707
26.251099	1326.479772	16.123725
26.015380	1321.132686	16.128743
26.657074	1337.361042	16.133760
26.522176	1328.580265	16.138778
26.474001	1337.929445	16.143795
26.407745	1335.493992	16.148813
26.147089	1336.781457	16.153831
26.440809	1343.662771	16.158848
26.398793	1325.282827	16.163866
26.546753	1337.713040	16.168883
26.854157	1336.490889	16.173901
26.763348	1344.417107	16.178919
26.409825	1342.859833	16.183936
26.280201	1336.375757	16.188954
26.643085	1338.281927	16.193971
26.750132	1337.712889	16.198989
26.544705	1327.220016	16.204007
26.453777	1332.817160	16.209024
26.811694	1328.816172	16.214042
26.611123	1333.013475	16.219059
26.989852	1333.197169	16.224077
26.941470	1327.549318	16.229095
26.756763	1335.550208	16.234112
26.927794	1337.369666	16.239130
26.735797	1331.482372	16.244147
26.577981	1337.714874	16.249165
26.739731	1340.116482	16.254183
26.782776	1344.474442	16.259200
27.171144	1350.211099	16.264218
27.102124	1349.234126	16.269235
27.154965	1355.405226	16.274253
27.241900	1350.111724	16.279271
27.657888	1346.417230	16.284288
27.620900	1334.462004	16.289306
27.469095	1322.890865	16.294323
27.297149	1326.345189	16.299341
27.364197	1315.875906	16.304359
27.181758	1313.774254	16.309376
27.404466	1316.055849	16.314394
27.228394	1318.343119	16.319411
27.216301	1319.102466	16.324429
27.031895	1327.141176	16.329447
27.197453	1336.056062	16.334464
27.560864	1325.994795	16.339482
27.339890	1324.331544	16.344499
27.695429	1334.725206	16.349517
27.570368	1331.099707	16.354535
27.607420	1335.455447	16.359552
27.255508	1326.607683	16.364570
27.495495	1335.643457	16.369587
27.643729	1346.028578	16.374605
27.817034	1349.510868	16.379623
27.521986	1354.294205	16.384640
27.662373	1351.476062	16.389658
27.737755	1354.090028	16.394675
27.467805	1354.271212	16.399693
27.603923	1337.943117	16.404711
27.354020	1354.967622	16.409728
27.423400	1348.180950	16.414746
27.719550	1342.712653	16.419763
27.909952	1348.388804	16.424781
27.838012	1347.046199	16.429799
28.179605	1339.525727	16.434816
27.784247	1340.294631	16.439834
28.060103	1351.868488	16.444851
27.907468	1350.948800	16.449869
28.025657	1361.490123	16.454887
28.331513	1366.365514	16.459904
28.004360	1358.725741	16.464922
28.356059	1358.178334	16.469939
27.718689	1358.571727	16.474957
28.094952	1362.407246	16.479975
28.238703	1361.210734	16.484992
28.103820	1355.396538	16.490010
28.134364	1352.434652	16.495027
28.183071	1365.587368	16.500045
28.384491	1357.577587	16.505063
28.148395	1370.746526	16.510080
27.813874	1359.648981	16.515098
28.273865	1364.702203	16.520115
28.352415	1370.399043	16.525133
28.177389	1362.460865	16.530151
28.350827	1372.311852	16.535168
28.605125	1384.409841	16.540186
28.468370	1370.564024	16.545203
28.319417	1381.115655	16.550221
28.417575	1389.551955	16.555239
28.582295	1381.522665	16.560256
28.739182	1393.225648	16.565274
28.967285	1388.146714	16.570291
28.483884	1385.836575	16.575309
28.520857	1383.287107	16.580327
28.584350	1383.778982	16.585344
28.252290	1382.742230	16.590362
28.724469	1379.262998	16.595379
28.465847	1393.600032	16.600397
28.462500	1380.291910	16.605415
28.777222	1394.406562	16.610432
28.776507	1406.014320	16.615450
29.284518	1407.077209	16.620467
29.378169	1412.112099	16.625485
28.819336	1401.835508	16.630503
28.843605	1406.928607	16.635520
28.814618	1420.497500	16.640538
29.106245	1408.026811	16.645555
29.047785	1419.536322	16.650573
29.203175	1409.832665	16.655591
29.185293	1410.608704	16.660608
29.222467	1411.297217	16.665626
29.404852	1400.475281	16.670643
29.363864	1414.071297	16.675661
29.416165	1408.051021	16.680679
29.242941	1416.627689	16.685696
29.140512	1411.401710	16.690714
29.482186	1403.082741	16.695731
29.295174	1402.843811	16.700749
29.417607	1410.465236	16.705767
29.188095	1407.250582	16.710784
29.030886	1410.768888	16.715802
29.462221	1406.996234	16.720819
29.148049	1409.567098	16.725837
29.761067	1425.800027	16.730855
29.964259	1432.443083	16.735872
29.725452	1421.276851	16.740890
30.288911	1421.043420	16.745907
30.308077	1418.361031	16.750925
29.809603	1406.162466	16.755943
29.901717	1403.569640	16.760960
29.948202	1406.399591	16.765978
30.259139	1406.896880	16.770995
30.184573	1405.024481	16.776013
30.176848	1400.471667	16.781031
30.259329	1401.304567	16.786048
30.087030	1405.674190	16.791066
30.191874	1399.456327	16.796083
29.916100	1404.855226	16.801101
29.730765	1408.327444	16.806119
29.808862	1402.943788	16.811136
29.750058	1410.003444	16.816154
29.902664	1387.461789	16.821171
30.291443	1398.809691	16.826189
29.910040	1396.275277	16.831207
29.812578	1405.947810	16.836224
29.602687	1395.171560	16.841242
30.002907	1409.323323	16.846259
30.070626	1420.844626	16.851277
30.273329	1415.195278	16.856295
30.083631	1418.829135	16.861312
30.034548	1417.148411	16.866330
30.323276	1430.386652	16.871347
30.442822	1433.508133	16.876365
30.282902	1429.815488	16.881383
30.576659	1425.502624	16.886400
30.122459	1434.565158	16.891418
29.945203	1434.293140	16.896435
30.066722	1445.667166	16.901453
30.422694	1444.715123	16.906471
30.404273	1451.708505	16.911488
30.188163	1452.297842	16.916506
30.755066	1447.105844	16.921523
31.164174	1446.483165	16.926541
31.110166	1447.375324	16.931559
30.957288	1444.366418	16.936576
30.976844	1443.902608	16.941594
31.246097	1451.996534	16.946611
30.961278	1448.727418	16.951629
30.884169	1448.515452	16.956647
30.607528	1445.585900	16.961664
30.535829	1455.532149	16.966682
30.717310	1453.370305	16.971699
30.855352	1456.744526	16.976717
30.966911	1452.936754	16.981735
31.310691	1459.889169	16.986752
31.056192	1463.192343	16.991770
31.855178	1467.971563	16.996787
31.514363	1461.744606	17.001805
31.373424	1455.407434	17.006823
31.193509	1444.825283	17.011840
30.758503	1446.319963	17.016858
31.266262	1450.463119	17.021875
31.456147	1449.903191	17.026893
31.117703	1452.206450	17.031911
31.355166	1466.942367	17.036928
31.345996	1465.492083	17.041946
31.426622	1465.327990	17.046963
31.527250	1473.322106	17.051981
31.539005	1470.265309	17.056999
31.882127	1471.044751	17.062016
31.711237	1475.376299	17.067034
31.724918	1463.971655	17.072051
31.562126	1467.519251	17.077069
31.532333	1473.495044	17.082087
31.893831	1458.072006	17.087104
31.748926	1472.722663	17.092122
31.754477	1461.309826	17.097139
31.733452	1467.303179	17.102157
31.567416	1461.926197	17.107175
31.864798	1473.913349	17.112192
31.732934	1465.908399	17.117210
31.642412	1461.056101	17.122227
31.825221	1463.732151	17.127245
31.746722	1460.519074	17.132263
31.863993	1469.905520	17.137280
32.266016	1487.310871	17.142298
32.126370	1483.094303	17.147315
32.325627	1485.625760	17.152333
32.120209	1487.090784	17.157351
32.284141	1488.135001	17.162368
32.182896	1489.315444	17.167386
32.201720	1494.595625	17.172403
32.498785	1484.958097	17.177421
32.117999	1491.670580	17.182439
32.617487	1498.235677	17.187456
32.433107	1489.516225	17.192474
32.409901	1479.108327	17.197491
32.602147	1491.165615	17.202509
32.405629	1486.815938	17.207527
32.478043	1486.807774	17.212544
32.061817	1483.915866	17.217562
32.081320	1486.339781	17.222579
32.288808	1486.323077	17.227597
32.148380	1485.811746	17.232615
32.725209	1490.960313	17.237632
32.633378	1493.007176	17.242650
32.248622	1487.109003	17.247667
32.444547	1493.093621	17.252685
32.545725	1509.836036	17.257703
32.914912	1514.142937	17.262720
32.830971	1518.173677	17.267738
32.902057	1514.186031	17.272755
32.880253	1515.316158	17.277773
32.846882	1518.171262	17.282791
33.072933	1509.286504	17.287808
32.963598	1511.661177	17.292826
32.818045	1517.333212	17.297843
33.072451	1511.672577	17.302861
33.464393	1512.428593	17.307879
33.205528	1515.467358	17.312896
33.266446	1506.343372	17.317914
33.476058	1508.930018	17.322931
33.615084	1509.056592	17.327949
33.810448	1516.808654	17.332967
33.803014	1506.107919	17.337984
33.314114	1489.726126	17.343002
33.268761	1484.866745	17.348019
33.309418	1479.018692	17.353037
33.467328	1503.667396	17.358055
33.548696	1495.812069	17.363072
33.352327	1506.361736	17.368090
33.215753	1509.914700	17.373107
32.978388	1497.567859	17.378125
33.071423	1510.473882	17.383143
33.320610	1506.477268	17.388160
32.985765	1511.421525	17.393178
33.509706	1529.022420	17.398195
33.488674	1525.181756	17.403213
33.392047	1534.677493	17.408231
33.485442	1533.163793	17.413248
33.911488	1537.849978	17.418266
33.532730	1534.936411	17.423283
34.107425	1531.302225	17.428301
33.920524	1532.975802	17.433319
33.949995	1532.374729	17.438336
33.762174	1536.529053	17.443354
33.803838	1553.069381	17.448371
34.158041	1552.243850	17.453389
34.155779	1555.387593	17.458407
34.122013	1562.673774	17.463424
34.245433	1558.479090	17.468442
34.194670	1561.870289	17.473459
34.194870	1553.238658	17.478477
34.143811	1560.647474	17.483495
34.431908	1557.178114	17.488512
34.302759	1552.729498	17.493530
33.996248	1557.514684	17.498547
34.316993	1560.030274	17.503565
34.508271	1553.265454	17.508583
34.598505	1552.509685	17.513600
34.669241	1550.936415	17.518618
34.519325	1552.272820	17.523635
34.768310	1544.189227	17.528653
34.846514	1552.938017	17.533671
34.650858	1541.080101	17.538688
34.551211	1544.412679	17.543706
34.653325	1553.934096	17.548723
34.564650	1548.380855	17.553741
34.840756	1545.134296	17.558759
34.808852	1552.120361	17.563776
34.692420	1541.502959	17.568794
34.623669	1548.759898	17.573811
34.374101	1537.910879	17.578829
34.747565	1554.007880	17.583847
34.866703	1563.087951	17.588864
35.116367	1565.419008	17.593882
34.662733	1573.541038	17.598899
35.051729	1577.197873	17.603917
35.070253	1572.375799	17.608935
35.024238	1575.046691	17.613952
35.357095	1576.032886	17.618970
35.239074	1584.004501	17.623987
35.052803	1574.994953	17.629005
35.027073	1573.913350	17.634023
35.243234	1576.893479	17.639040
35.307568	1567.573254	17.644058
34.997774	1571.216491	17.649075
35.259037	1580.318487	17.654093
35.302894	1595.684482	17.659111
35.260908	1598.430490	17.664128
35.814925	1592.495656	17.669146
35.280121	1596.417163	17.674163
35.010929	1591.848459	17.679181
35.145812	1597.694344	17.684199
35.332315	1602.408609	17.689216
35.298865	1605.421540	17.694234
35.433144	1616.544352	17.699251
36.110984	1620.051792	17.704269
35.979587	1620.952929	17.709287
36.099821	1621.420141	17.714304
36.556387	1617.523562	17.719322
36.108087	1615.611861	17.724339
36.252691	1596.025212	17.729357
36.165867	1595.757958	17.734375
36.086206	1590.585167	17.739392
36.290125	1583.373360	17.744410
35.803674	1586.056453	17.749427
36.420582	1587.916537	17.754445
36.396110	1592.881619	17.759463
36.244767	1593.003193	17.764480
36.503611	1585.110553	17.769498
36.246895	1591.121939	17.774515
36.263850	1584.087757	17.779533
36.556357	1591.284957	17.784551
36.239478	1584.688110	17.789568
36.588960	1584.538700	17.794586
36.292350	1588.994120	17.799603
36.654301	1587.665571	17.804621
36.559240	1595.097075	17.809639
36.227591	1585.718956	17.814656
36.291647	1584.875764	17.819674
36.470700	1603.849975	17.824691
36.565076	1606.158027	17.829709
36.645839	1611.075066	17.834727
36.807539	1610.383841	17.839744
36.973650	1606.864153	17.844762
37.339692	1616.407371	17.849779
37.159857	1609.078944	17.854797
36.992889	1621.397741	17.859815
37.306981	1610.258379	17.864832
37.024217	1588.946091	17.869850
36.880096	1588.536327	17.874867
37.116606	1583.572792	17.879885
36.832711	1573.941030	17.884903
37.134120	1589.023655	17.889920
37.306117	1609.693747	17.894938
37.055096	1604.954924	17.899955
37.257314	1610.136973	17.904973
37.178111	1610.042105	17.909991
37.477755	1615.167862	17.915008
37.374545	1605.930676	17.920026
37.344392	1616.265004	17.925043
37.185625	1608.541933	17.930061
37.240140	1607.087971	17.935079
37.496635	1608.821480	17.940096
37.663941	1604.411614	17.945114
37.834905	1612.164384	17.950131
37.596811	1605.331110	17.955149
37.645552	1608.577332	17.960167
37.108102	1600.225588	17.965184
37.391979	1607.345247	17.970202
37.739542	1615.105065	17.975219
37.523667	1612.424756	17.980237
37.147801	1609.062572	17.985255
37.198525	1619.901814	17.990272
37.457226	1615.723794	17.995290
37.523534	1629.429402	18.000307
37.191250	1633.947230	18.005325
37.700422	1642.792652	18.010343
37.811950	1647.616512	18.015360
37.669496	1650.722273	18.020378
37.857565	1658.516568	18.025395
38.049178	1654.727771	18.030413
38.106310	1651.465005	18.035431
38.171984	1656.592716	18.040448
38.195304	1651.384837	18.045466
38.215088	1661.168534	18.050483
38.160278	1651.245201	18.055501
38.136429	1654.963580	18.060519
38.675152	1653.304354	18.065536
38.195384	1662.086967	18.070554
38.305281	1661.826762	18.075571
38.623345	1682.777029	18.080589
38.865040	1676.651245	18.085607
38.754778	1683.015281	18.090624
38.655622	1660.317056	18.095642
38.594485	1667.115230	18.100659
38.678050	1677.346564	18.105677
39.068326	1678.674086	18.110695
38.751192	1681.785129	18.115712
39.555403	1667.188855	18.120730
39.049592	1657.841141	18.125747
38.944406	1648.487471	18.130765
38.688301	1645.134920	18.135783
38.890878	1651.958046	18.140800
39.062557	1646.723767	18.145818
38.681804	1649.705908	18.150835
38.860981	1668.648609	18.155853
39.467183	1660.474280	18.160871
39.399912	1668.835639	18.165888
39.478459	1671.764757	18.170906
39.536877	1673.210549	18.175923
39.491209	1664.696511	18.180941
39.248296	1650.586226	18.185959
38.940213	1653.361310	18.190976
39.328359	1668.367292	18.195994
39.408316	1668.263266	18.201011
39.475059	1668.899817	18.206029
39.764044	1665.597566	18.211047
39.489268	1670.043273	18.216064
39.817054	1669.840453	18.221082
39.777598	1673.305645	18.226099
39.606796	1681.086745	18.231117
39.813465	1667.953801	18.236135
39.679795	1675.536565	18.241152
40.096692	1673.501923	18.246170
39.739256	1677.581862	18.251187
39.690466	1673.385729	18.256205
39.690569	1664.305907	18.261223
39.701301	1671.215906	18.266240
39.779325	1683.325936	18.271258
39.516420	1672.807149	18.276275
39.880228	1678.696094	18.281293
39.933360	1676.371285	18.286311
39.273524	1675.808775	18.291328
39.663234	1682.766706	18.296346
39.918347	1684.273206	18.301363
39.874697	1694.199412	18.306381
39.885230	1688.876753	18.311399
39.694539	1695.550060	18.316416
39.943578	1705.136905	18.321434
40.226611	1721.232445	18.326451
40.198852	1727.204848	18.331469
40.291646	1717.053211	18.336487
40.150398	1731.870774	18.341504
40.363256	1730.979013	18.346522
40.245137	1730.577795	18.351539
39.975601	1740.170164	18.356557
40.585407	1748.554873	18.361575
40.322724	1751.717361	18.366592
40.825918	1746.633097	18.371610
40.797027	1745.021767	18.376627
41.042088	1742.875176	18.381645
41.139760	1734.528008	18.386663
41.085111	1744.402313	18.391680
41.021846	1742.824773	18.396698
41.004028	1746.469638	18.401715
40.740891	1741.120410	18.406733
41.053645	1740.373953	18.411751
40.896755	1761.430288	18.416768
41.180583	1760.738859	18.421786
41.028549	1768.870531	18.426803
40.825752	1772.137256	18.431821
41.134306	1772.515002	18.436839
41.144655	1766.062492	18.441856
41.538189	1758.956615	18.446874
41.376066	1765.003735	18.451891
41.316243	1762.321046	18.456909
41.541423	1757.122537	18.461927
41.750939	1763.774194	18.466944
41.425894	1773.706660	18.471962
41.547643	1768.155099	18.476979
41.782871	1773.474044	18.481997
41.765488	1762.118262	18.487015
41.662125	1773.947482	18.492032
41.896679	1764.559457	18.497050
42.048913	1757.762805	18.502067
41.944882	1758.082109	18.507085
41.638550	1767.623450	18.512103
41.749582	1766.807605	18.517120
42.251698	1780.798522	18.522138
42.269578	1787.969396	18.527155
42.077074	1794.409478	18.532173
42.231873	1794.255853	18.537191
42.527030	1794.458960	18.542208
42.249010	1779.697619	18.547226
42.009575	1769.541197	18.552243
42.146154	1775.001840	18.557261
42.362935	1778.256480	18.562279
42.074512	1784.301303	18.567296
42.133241	1781.701029	18.572314
42.671071	1783.990121	18.577331
42.225160	1783.908522	18.582349
42.540579	1781.476328	18.587367
42.402625	1782.425840	18.592384
42.598084	1778.873116	18.597402
42.650394	1774.127752	18.602419
42.314129	1779.312161	18.607437
42.494478	1784.573432	18.612455
42.295332	1786.315226	18.617472
42.189876	1799.331458	18.622490
42.668575	1796.794779	18.627507
42.934883	1806.315852	18.632525
42.930349	1811.221061	18.637543
42.949166	1807.954802	18.642560
42.610877	1808.837867	18.647578
42.596177	1805.602108	18.652595
43.193628	1807.888174	18.657613
44.096161	1800.693063	18.662631
44.006852	1791.475696	18.667648
44.067168	1791.267442	18.672666
43.891290	1777.724106	18.677683
43.939545	1766.746228	18.682701
43.970879	1755.357569	18.687719
44.222334	1755.416034	18.692736
43.963369	1752.631994	18.697754
44.183958	1742.280427	18.702771
43.892695	1735.161923	18.707789
43.946935	1723.772851	18.712807
43.750622	1730.121981	18.717824
43.877052	1729.338442	18.722842
43.745438	1728.522745	18.727859
43.510182	1732.267951	18.732877
43.561661	1727.043014	18.737895
43.950971	1731.391000	18.742912
43.979520	1744.626054	18.747930
44.070254	1750.800821	18.752947
43.804180	1755.384051	18.757965
44.206964	1746.701874	18.762983
44.062229	1749.435599	18.768000
43.600077	1760.850778	18.773018
43.970685	1749.087052	18.778035
43.972919	1755.439799	18.783053
44.168181	1749.930378	18.788071
44.040362	1749.016248	18.793088
44.288642	1748.788013	18.798106
44.622782	1745.526013	18.803123
44.350260	1747.806356	18.808141
44.014146	1741.979378	18.813159
44.395397	1757.311586	18.818176
44.156274	1770.714838	18.823194
44.588612	1769.072270	18.828211
44.166762	1774.377392	18.833229
44.228330	1775.948941	18.838247
44.477332	1775.988854	18.843264
44.451211	1788.317258	18.848282
44.677162	1787.792698	18.853299
44.594856	1800.104665	18.858317
44.879848	1801.805324	18.863335
44.879827	1800.467196	18.868352
44.622113	1808.665940	18.873370
45.248058	1802.997499	18.878387
44.841842	1808.928232	18.883405
44.830502	1805.609890	18.888423
44.801876	1808.391709	18.893440
44.755010	1808.263368	18.898458
45.088306	1822.962472	18.903475
45.142439	1827.202039	18.908493
45.056008	1834.275658	18.913511
45.249041	1833.869872	18.918528
45.128790	1838.581764	18.923546
45.337420	1836.522927	18.928563
45.325051	1833.122684	18.933581
45.231812	1836.258638	18.938599
45.529900	1843.666520	18.943616
45.290935	1854.825867	18.948634
45.304093	1863.092658	18.953651
45.421025	1865.252032	18.958669
45.762082	1861.862686	18.963687
45.670584	1857.234512	18.968704
45.863388	1860.070014	18.973722
45.941838	1855.279504	18.978739
45.929714	1862.518230	18.983757
45.748293	1861.770295	18.988775
46.070955	1856.638541	18.993792
46.095994	1867.046424	18.998810
46.065731	1875.670344	19.003827
45.974628	1878.815439	19.008845
45.945845	1885.337206	19.013863
46.177946	1875.940040	19.018880
46.139558	1886.900711	19.023898
46.346365	1880.139647	19.028915
46.335866	1879.421740	19.033933
46.407946	1878.807668	19.038951
46.383578	1879.493217	19.043968
46.296475	1882.773396	19.048986
46.504429	1880.998704	19.054003
46.822200	1900.421746	19.059021
46.835302	1898.740702	19.064039
46.897657	1888.890405	19.069056
46.532445	1901.432973	19.074074
46.919614	1903.654161	19.079091
46.894640	1906.624786	19.084109
46.972439	1905.703680	19.089127
46.934107	1892.788853	19.094144
46.915319	1907.363295	19.099162
47.202476	1909.022596	19.104179
47.149406	1903.107034	19.109197
47.279313	1895.373326	19.114215
47.475056	1885.912418	19.119232
47.114881	1899.082248	19.124250
47.497504	1890.488375	19.129267
47.212023	1894.702267	19.134285
47.268177	1894.043349	19.139303
47.561089	1890.188134	19.144320
47.330326	1897.783047	19.149338
47.208408	1900.260736	19.154355
47.476351	1893.253385	19.159373
47.510705	1891.240783	19.164391
47.668526	1901.536356	19.169408
47.665185	1910.048769	19.174426
48.040801	1912.688367	19.179443
47.952103	1915.088264	19.184461
47.775434	1922.387511	19.189479
48.404868	1917.255017	19.194496
47.785755	1919.962099	19.199514
48.123231	1911.968626	19.204531
48.256037	1909.142117	19.209549
47.937774	1909.343498	19.214567
48.393668	1907.488927	19.219584
48.197453	1913.847575	19.224602
48.124842	1912.331450	19.229619
48.246287	1914.887785	19.234637
48.528332	1916.071324	19.239655
48.770157	1902.434045	19.244672
48.299379	1906.673815	19.249690
48.492396	1904.166102	19.254707
48.610428	1906.912333	19.259725
48.459512	1900.166281	19.264743
48.645869	1896.633896	19.269760
48.460593	1899.951552	19.274778
48.597748	1898.490931	19.279795
48.648125	1902.109363	19.284813
48.387619	1899.612742	19.289831
48.703348	1897.436124	19.294848
48.671684	1892.164201	19.299866
48.403341	1911.978912	19.304883
48.871807	1909.813079	19.309901
49.048356	1927.396208	19.314919
49.190113	1910.523867	19.319936
48.600832	1921.211082	19.324954
48.985014	1925.559919	19.329971
49.015650	1919.422937	19.334989
48.697091	1926.637112	19.340007
49.111193	1940.720845	19.345024
49.476345	1948.667417	19.350042
49.489504	1950.937742	19.355059
49.471124	1951.638136	19.360077
49.352451	1956.614922	19.365095
49.686486	1947.586786	19.370112
49.882110	1961.275543	19.375130
49.612139	1954.371384	19.380147
49.557756	1948.724277	19.385165
49.351427	1953.471779	19.390183
49.496071	1946.452165	19.395200
49.591342	1962.182834	19.400218
49.808657	1976.158561	19.405235
50.163927	1974.329218	19.410253
49.913151	1988.119497	19.415271
49.732186	1968.040609	19.420288
49.681471	1973.896760	19.425306
49.882332	1975.610617	19.430323
50.347765	1972.668861	19.435341
49.964484	1986.442027	19.440359
50.441338	1997.909066	19.445376
50.575096	1998.320516	19.450394
51.266471	1992.846909	19.455411
50.525893	1978.148409	19.460429
50.383216	1969.478998	19.465447
50.948847	1964.593192	19.470464
50.880088	1965.648646	19.475482
50.845745	1967.232083	19.480499
50.742007	1956.252654	19.485517
50.854686	1958.147597	19.490535
50.955043	1956.642240	19.495552
51.337795	1960.435844	19.500570
50.840347	1958.919999	19.505587
51.030862	1956.923952	19.510605
50.689331	1957.198412	19.515623
51.656679	1965.157947	19.520640
51.434080	1954.702111	19.525658
51.350923	1960.575965	19.530675
51.309865	1951.183685	19.535693
51.142594	1959.589251	19.540711
51.344664	1956.534114	19.545728
51.422594	1956.427248	19.550746
51.740187	1968.301104	19.555763
51.538871	1963.447092	19.560781
51.221208	1969.502870	19.565799
51.357738	1971.435106	19.570816
51.414585	1970.678239	19.575834
51.499883	1985.804527	19.580851
51.635306	1979.461743	19.585869
51.525814	1980.419430	19.590887
51.728048	1978.320550	19.595904
51.883141	1975.241210	19.600922
51.534904	1974.579371	19.605939
51.767367	1986.737998	19.610957
51.569996	2007.816744	19.615975
51.720392	1996.361936	19.620992
51.568464	1997.414643	19.626010
51.945461	2007.369799	19.631027
52.079448	2001.974051	19.636045
52.038927	2015.270623	19.641063
52.116486	2032.175030	19.646080
52.190438	2035.098615	19.651098
52.277554	2029.464030	19.656115
52.331931	2020.375524	19.661133
52.030651	2027.486037	19.666151
52.453157	2028.202571	19.671168
52.766655	2030.716208	19.676186
52.696523	2037.083550	19.681203
53.058132	2040.782646	19.686221
52.999898	2051.828585	19.691239
52.886068	2035.984022	19.696256
53.078871	2043.758807	19.701274
52.779751	2056.180665	19.706291
53.013757	2055.408662	19.711309
52.883604	2056.581047	19.716327
52.814685	2057.955296	19.721344
53.239127	2047.309660	19.726362
52.976724	2054.587676	19.731379
52.911094	2047.455789	19.736397
53.202525	2063.278900	19.741415
53.053592	2060.266115	19.746432
53.402398	2073.517512	19.751450
53.375217	2086.250264	19.756467
53.368354	2079.970766	19.761485
53.526642	2079.280059	19.766503
53.358560	2082.667645	19.771520
53.548123	2078.512975	19.776538
53.738151	2085.417134	19.781555
53.757605	2076.169956	19.786573
53.628784	2086.239122	19.791591
53.813369	2104.458694	19.796608
53.790950	2097.177993	19.801626
54.028024	2104.614480	19.806643
54.202410	2100.203384	19.811661
54.222103	2095.614536	19.816679
54.466200	2095.642595	19.821696
54.240324	2097.300237	19.826714
54.285619	2096.955466	19.831731
54.255127	2096.616256	19.836749
54.472933	2092.495031	19.841767
54.173365	2098.103009	19.846784
54.511078	2096.506799	19.851802
54.498586	2096.347822	19.856819
54.430542	2088.263160	19.861837
54.563073	2105.048559	19.866855
54.603290	2118.714444	19.871872
54.779094	2119.387576	19.876890
54.804650	2117.631971	19.881907
54.722906	2113.611327	19.886925
54.883468	2118.651714	19.891943
54.915443	2105.769903	19.896960
54.951784	2111.988034	19.901978
54.994902	2116.854300	19.906995
55.173791	2113.070556	19.912013
55.247070	2122.268560	19.917031
55.102172	2122.101923	19.922048
55.433325	2123.353529	19.927066
55.783038	2133.085791	19.932083
55.782502	2116.292361	19.937101
55.786644	2106.198579	19.942119
55.789833	2107.432134	19.947136
55.742974	2097.437874	19.952154
55.492715	2103.113874	19.957171
55.872857	2100.157056	19.962189
55.828861	2101.991347	19.967207
55.739644	2104.138864	19.972224
55.738879	2098.293944	19.977242
55.884180	2114.162087	19.982259
56.126344	2121.913392	19.987277
56.401369	2124.316295	19.992295
55.978346	2124.209014	19.997312
56.176114	2126.128516	20.002330
56.027464	2118.264772	20.007347
56.357175	2131.822188	20.012365
56.347607	2123.460080	20.017383
56.401664	2125.929165	20.022400
56.453178	2117.002019	20.027418
56.459794	2124.439905	20.032435
56.520258	2121.589979	20.037453
56.647759	2118.252982	20.042471
56.128552	2125.546014	20.047488
56.322896	2117.615906	20.052506
56.322941	2124.707651	20.057523
56.485078	2139.657914	20.062541
56.534208	2146.846129	20.067559
56.855100	2152.353755	20.072576
56.789409	2141.488184	20.077594
56.878433	2149.168811	20.082611
57.013268	2142.295838	20.087629
57.164527	2159.308749	20.092647
57.321369	2172.435647	20.097664
57.292490	2171.651174	20.102682
57.580763	2179.032328	20.107699
57.377826	2168.200868	20.112717
57.449668	2174.706975	20.117735
57.595894	2178.023240	20.122752
57.255647	2168.428391	20.127770
57.553806	2172.948572	20.132787
57.364018	2172.214558	20.137805
57.660261	2170.075678	20.142823
57.376767	2167.503719	20.147840
58.146425	2188.983482	20.152858
57.851187	2199.833093	20.157875
58.069615	2190.194886	20.162893
58.472896	2192.565079	20.167911
58.378975	2201.120227	20.172928
58.525329	2186.841222	20.177946
58.282601	2176.378942	20.182963
57.879459	2173.538523	20.187981
58.542655	2177.376605	20.192999
58.143108	2187.898538	20.198016
58.529701	2188.106262	20.203034
58.332510	2191.684638	20.208051
58.613058	2190.113157	20.213069
58.810972	2194.529118	20.218087
58.259669	2195.354048	20.223104
58.718313	2189.973656	20.228122
58.780678	2191.885975	20.233139
58.629652	2187.699428	20.238157
58.642076	2189.515420	20.243175
58.574096	2195.857232	20.248192
58.973776	2200.506695	20.253210
58.888130	2209.638116	20.258227
58.982022	2216.361710	20.263245
59.385124	2207.534083	20.268263
59.392970	2218.077419	20.273280
59.655824	2203.511879	20.278298
59.627127	2215.424374	20.283315
59.587495	2199.536481	20.288333
59.837371	2202.577712	20.293351
59.495798	2200.336769	20.298368
59.652049	2204.371060	20.303386
59.766268	2206.837042	20.308403
59.492156	2208.186641	20.313421
59.997763	2205.225929	20.318439
59.620460	2212.357895	20.323456
59.589816	2205.255180	20.328474
59.733177	2211.308241	20.333491
59.629738	2211.494903	20.338509
59.670670	2206.820641	20.343527
59.944143	2223.041219	20.348544
60.187187	2233.538246	20.353562
60.082615	2232.566794	20.358579
59.861247	2242.536928	20.363597
60.245977	2232.134114	20.368615
59.851381	2239.167803	20.373632
60.111710	2236.933547	20.378650
60.331858	2251.262530	20.383667
60.843499	2252.937190	20.388685
60.923288	2251.902136	20.393703
60.851726	2249.991303	20.398720
60.845459	2254.079473	20.403738
61.053391	2254.949568	20.408755
60.984404	2251.955786	20.413773
61.228036	2249.077142	20.418791
61.180861	2250.631053	20.423808
61.239173	2247.592078	20.428826
61.557361	2247.176143	20.433843
61.070385	2251.639459	20.438861
61.361036	2237.789129	20.443879
61.805845	2250.031441	20.448896
61.569680	2236.282589	20.453914
61.645905	2230.173075	20.458931
61.563466	2228.178734	20.463949
61.732864	2234.827384	20.468967
61.550929	2238.075144	20.473984
62.033278	2234.325888	20.479002
61.765448	2237.877468	20.484019
61.868602	2230.577038	20.489037
61.876963	2231.740357	20.494055
62.216747	2233.738616	20.499072
61.704424	2228.731268	20.504090
62.094133	2229.787498	20.509107
61.813482	2234.360507	20.514125
61.757770	2226.867198	20.519143
61.980734	2240.491919	20.524160
62.293490	2260.578922	20.529178
62.394063	2259.723665	20.534195
62.403289	2261.300301	20.539213
62.620864	2247.167894	20.544231
62.460165	2253.972421	20.549248
62.539669	2251.154209	20.554266
62.466638	2258.816088	20.559283
62.219581	2257.216801	20.564301
62.619940	2254.742832	20.569319
62.929549	2278.769173	20.574336
62.831492	2280.394181	20.579354
63.274354	2277.055086	20.584371
63.326924	2283.144489	20.589389
63.520863	2279.251045	20.594407
63.265988	2283.649598	20.599424
63.109369	2286.786093	20.604442
63.351798	2275.401903	20.609459
62.989380	2282.509471	20.614477
63.232528	2281.887520	20.619495
63.395572	2286.902317	20.624512
63.090291	2284.854513	20.629530
63.470238	2275.680151	20.634547
63.315127	2282.225012	20.639565
63.301897	2294.886292	20.644583
63.331263	2311.416622	20.649600
63.445403	2306.980197	20.654618
63.654116	2314.001451	20.659635
63.792877	2321.551271	20.664653
64.268806	2326.586492	20.669671
64.209357	2331.920212	20.674688
64.024465	2337.008473	20.679706
64.373199	2336.527784	20.684723
64.219646	2336.744392	20.689741
64.626264	2330.753509	20.694759
64.707996	2338.252305	20.699776
64.284377	2336.090478	20.704794
64.525488	2330.554760	20.709811
64.475969	2325.875702	20.714829
64.411385	2319.854498	20.719847
64.776098	2330.878528	20.724864
64.689729	2322.825036	20.729882
64.841674	2319.853438	20.734899
64.359037	2330.606244	20.739917
64.659149	2339.377460	20.744935
64.704494	2355.851674	20.749952
64.875140	2356.156357	20.754970
65.378192	2354.051333	20.759987
65.057404	2348.755139	20.765005
65.348272	2360.816499	20.770023
65.687260	2371.055552	20.775040
65.408582	2369.101410	20.780058
65.714196	2365.588123	20.785075
65.869131	2373.122806	20.790093
66.072974	2369.978950	20.795111
65.834761	2363.953373	20.800128
65.809125	2367.814206	20.805146
65.837598	2369.220561	20.810163
66.121931	2369.305440	20.815181
65.758867	2364.419850	20.820199
66.012704	2371.544521	20.825216
65.744417	2375.358158	20.830234
65.683423	2365.580580	20.835251
65.792502	2369.770637	20.840269
65.801768	2388.822779	20.845287
66.006130	2397.056702	20.850304
66.170926	2398.356485	20.855322
66.288125	2387.806129	20.860339
66.846169	2403.111192	20.865357
66.456004	2390.980198	20.870375
66.690629	2401.847910	20.875392
66.675185	2415.939352	20.880410
67.054034	2416.040984	20.885427
67.102435	2412.915162	20.890445
67.246704	2412.239264	20.895463
67.686654	2414.745770	20.900480
67.125595	2414.906291	20.905498
67.705733	2409.150156	20.910515
66.903586	2403.992486	20.915533
67.487913	2399.921075	20.920551
67.714459	2410.035742	20.925568
67.245420	2408.565904	20.930586
67.375631	2405.174775	20.935603
67.351528	2415.817916	20.940621
67.988512	2404.277144	20.945639
67.742036	2403.854991	20.950656
67.513174	2411.667596	20.955674
67.870984	2400.539834	20.960691
67.556794	2409.230588	20.965709
67.577190	2403.025610	20.970727
68.090413	2405.855184	20.975744
67.862827	2423.319062	20.980762
67.964904	2431.023014	20.985779
67.883484	2429.984802	20.990797
68.174258	2429.396414	20.995815
68.251102	2428.904667	21.000832
68.041704	2432.257761	21.005850
68.281866	2427.773157	21.010867
68.117229	2443.298790	21.015885
68.257667	2447.717507	21.020903
68.733461	2445.124385	21.025920
68.706089	2458.450786	21.030938
68.655645	2452.193767	21.035955
68.486301	2461.717167	21.040973
68.784134	2473.562893	21.045991
68.790251	2478.359307	21.051008
68.962274	2481.482218	21.056026
68.972723	2478.687415	21.061043
69.025269	2482.687518	21.066061
69.496060	2479.826902	21.071079
69.476911	2468.571947	21.076096
69.455984	2489.989725	21.081114
69.747186	2503.323057	21.086131
69.685932	2506.267903	21.091149
70.055427	2503.252723	21.096167
70.249892	2489.754978	21.101184
69.538578	2487.676081	21.106202
69.977830	2483.879873	21.111219
69.722455	2494.186869	21.116237
70.236057	2502.050463	21.121255
69.816370	2497.138990	21.126272
70.311303	2496.739545	21.131290
70.425055	2492.230544	21.136307
70.308512	2487.997494	21.141325
70.307819	2491.428365	21.146343
70.498770	2489.883521	21.151360
70.165439	2498.094424	21.156378
70.383496	2489.011599	21.161395
70.355482	2508.760906	21.166413
70.774181	2519.098021	21.171431
70.579072	2515.704186	21.176448
71.240605	2524.882823	21.181466
71.213542	2515.323935	21.186483
71.002317	2521.041292	21.191501
70.867227	2517.720114	21.196519
71.474559	2512.407860	21.201536
71.295671	2511.040893	21.206554
71.089586	2502.194945	21.211571
71.253300	2514.446763	21.216589
71.192425	2524.982108	21.221607
71.622172	2528.001526	21.226624
71.445644	2538.614966	21.231642
71.917370	2535.394393	21.236659
71.711566	2540.328180	21.241677
71.776508	2538.165530	21.246695
72.016919	2532.550956	21.251712
71.570154	2534.470488	21.256730
71.352658	2537.739654	21.261747
71.671069	2540.337811	21.266765
71.517957	2557.430348	21.271783
72.269460	2556.028074	21.276800
71.807813	2573.793886	21.281818
72.258717	2565.974881	21.286835
72.057183	2567.720280	21.291853
72.314242	2585.547089	21.296871
72.539444	2584.659667	21.301888
72.523641	2581.483908	21.306906
72.655353	2585.162326	21.311923
72.731814	2592.718865	21.316941
72.368103	2591.245133	21.321959
72.915747	2582.423083	21.326976
72.402554	2591.946770	21.331994
72.428761	2600.025641	21.337011
72.801961	2605.667240	21.342029
72.678085	2602.824027	21.347047
73.176988	2600.280918	21.352064
73.011282	2625.644662	21.357082
73.371232	2628.242636	21.362099
73.886883	2626.675314	21.367117
74.569001	2628.534766	21.372135
74.448906	2607.423025	21.377152
74.341136	2599.341200	21.382170
74.269695	2590.328930	21.387187
74.528885	2591.266760	21.392205
73.920952	2589.645078	21.397223
74.365344	2584.797040	21.402240
74.182678	2587.341151	21.407258
74.482131	2589.112213	21.412275
74.535705	2580.569567	21.417293
74.623065	2586.669403	21.422311
74.572351	2581.807408	21.427328
74.570134	2588.498857	21.432346
74.805238	2588.793446	21.437363
74.846972	2583.162641	21.442381
75.009765	2583.774708	21.447399
75.141510	2583.321698	21.452416
74.710390	2589.906757	21.457434
74.707253	2583.023671	21.462451
74.672941	2583.253161	21.467469
74.571470	2579.273377	21.472487
74.867403	2593.439264	21.477504
75.043376	2607.513490	21.482522
74.840339	2605.837838	21.487539
75.142959	2605.130811	21.492557
75.099287	2615.515174	21.497575
74.786933	2611.303305	21.502592
75.438982	2633.269143	21.507610
75.504465	2637.734368	21.512627
75.435063	2628.709135	21.517645
75.309822	2640.368762	21.522663
75.877759	2643.221365	21.527680
75.787936	2660.906914	21.532698
75.703904	2654.165879	21.537715
76.077194	2656.212592	21.542733
75.825152	2663.476606	21.547751
76.143009	2662.915530	21.552768
76.061041	2669.174483	21.557786
76.343350	2688.111571	21.562803
76.342723	2692.694478	21.567821
75.691960	2694.292495	21.572839
76.140787	2689.787759	21.577856
76.261958	2704.274638	21.582874
76.376877	2702.362946	21.587891
76.378838	2706.907577	21.592909
76.427700	2716.781979	21.597927
76.466004	2722.081562	21.602944
76.549564	2734.712205	21.607962
77.008780	2736.410909	21.612979
77.213659	2737.426692	21.617997
77.451429	2743.102179	21.623015
77.431247	2753.394567	21.628032
77.401573	2763.186613	21.633050
77.309954	2766.480285	21.638067
77.840583	2763.026354	21.643085
77.593939	2759.918292	21.648103
77.757182	2756.209459	21.653120
77.954603	2767.645025	21.658138
77.900521	2764.592010	21.663155
77.780138	2764.389963	21.668173
77.721002	2759.453491	21.673191
78.049948	2756.633993	21.678208
77.929117	2773.172499	21.683226
78.164211	2789.768878	21.688243
78.256504	2794.785433	21.693261
77.930007	2791.443693	21.698279
78.272169	2793.665735	21.703296
78.528393	2797.119535	21.708314
78.538642	2811.425039	21.713331
78.833182	2817.896488	21.718349
78.400558	2820.836445	21.723367
78.755281	2816.778822	21.728384
78.793591	2814.143725	21.733402
78.663287	2824.576499	21.738419
78.986659	2828.411156	21.743437
79.195098	2835.158066	21.748455
79.447546	2833.963367	21.753472
79.410556	2847.253687	21.758490
79.058935	2843.625502	21.763507
79.695080	2827.416555	21.768525
79.788396	2837.454494	21.773543
79.726840	2829.649385	21.778560
79.762255	2850.146619	21.783578
79.688699	2852.209709	21.788595
79.834685	2858.609760	21.793613
79.900679	2866.553113	21.798631
80.206083	2865.217553	21.803648
80.351062	2857.146513	21.808666
80.051220	2864.935715	21.813683
80.421515	2857.574241	21.818701
80.344307	2879.787198	21.823719
80.797122	2882.317004	21.828736
80.727499	2884.221671	21.833754
80.803831	2885.835191	21.838771
80.896938	2877.021088	21.843789
80.827210	2881.491777	21.848807
80.858082	2876.818918	21.853824
81.141938	2883.039567	21.858842
80.710297	2881.219800	21.863859
80.819284	2873.618356	21.868877
81.180180	2883.346119	21.873895
81.086805	2887.362862	21.878912
81.308334	2900.480157	21.883930
81.385519	2906.168230	21.888947
81.621877	2891.981878	21.893965
81.607513	2902.841560	21.898983
81.481977	2896.028031	21.904000
82.009453	2910.037954	21.909018
82.004706	2920.504768	21.914035
82.409724	2916.931615	21.919053
82.118935	2924.807798	21.924071
82.257591	2922.317931	21.929088
82.466443	2910.474638	21.934106
81.971695	2920.740475	21.939123
82.346030	2919.867546	21.944141
82.505010	2906.491830	21.949159
82.350561	2911.468171	21.954176
82.653004	2914.135166	21.959194
82.303982	2917.503911	21.964211
82.855785	2934.464270	21.969229
82.678577	2944.920244	21.974247
82.529908	2945.186592	21.979264
82.900042	2942.439519	21.984282
83.019476	2950.990001	21.989299
83.101289	2942.284948	21.994317
83.179622	2946.536769	21.999335
82.977603	2952.012946	22.004352
83.325801	2952.031011	22.009370
83.326666	2976.539061	22.014387
83.637334	2971.967527	22.019405
83.602212	2969.530130	22.024423
83.618693	2963.022574	22.029440
83.615931	2969.092472	22.034458
83.790646	2995.334489	22.039475
84.027847	2996.168474	22.044493
84.103277	2996.162995	22.049511
84.107894	2999.892973	22.054528
84.076573	2997.347664	22.059546
83.923100	3007.222363	22.064563
84.200322	3010.019574	22.069581
84.509026	3020.513086	22.074599
83.978675	3041.165459	22.079616
84.379764	3029.828531	22.084634
84.051809	3033.664279	22.089651
84.698206	3042.160648	22.094669
84.625861	3054.645505	22.099687
85.245220	3048.277026	22.104704
85.801398	3023.104064	22.109722
85.662096	3027.115408	22.114739
86.124982	3021.945577	22.119757
85.893156	3019.583178	22.124775
86.098919	3012.427325	22.129792
86.391942	3002.470842	22.134810
86.255280	2998.417573	22.139827
86.563679	2987.044694	22.144845
86.625183	2987.271802	22.149863
86.968528	2980.949747	22.154880
86.886091	2971.007919	22.159898
86.219903	2961.845613	22.164915
86.306300	2969.883658	22.169933
86.449613	2955.945394	22.174951
86.194246	2962.124303	22.179968
86.588169	2962.772765	22.184986
86.392800	2986.632983	22.190003
86.724560	2986.350626	22.195021
86.830565	2988.360349	22.200039
86.568992	2988.107826	22.205056
86.879072	2986.007716	22.210074
86.976415	2991.639002	22.215091
86.743219	2980.666604	22.220109
86.738908	2987.693091	22.225127
86.714975	2999.491734	22.230144
86.822267	2997.000458	22.235162
87.034757	3009.150283	22.240179
87.178592	2999.094083	22.245197
86.742968	3018.702655	22.250215
86.648510	3033.229895	22.255232
87.221569	3032.543607	22.260250
87.263229	3053.829156	22.265267
87.300108	3066.265346	22.270285
87.816222	3063.419634	22.275303
88.027289	3073.707537	22.280320
88.313029	3079.179927	22.285338
88.035850	3085.084545	22.290355
88.177820	3081.543104	22.295373
88.028779	3081.689575	22.300391
87.828166	3088.626918	22.305408
88.580850	3092.911996	22.310426
88.449978	3115.174682	22.315443
88.476957	3114.008978	22.320461
88.567879	3120.919595	22.325479
88.362406	3114.238446	22.330496
88.957442	3115.855939	22.335514
89.024247	3135.887766	22.340531
89.152620	3139.200695	22.345549
89.188587	3134.403876	22.350567
89.242974	3137.946178	22.355584
89.415898	3133.522436	22.360602
89.429918	3136.648123	22.365619
89.146123	3138.864122	22.370637
89.646812	3156.173575	22.375655
89.642069	3160.637307	22.380672
90.116850	3153.537095	22.385690
90.059149	3153.217910	22.390707
90.638602	3156.892578	22.395725
90.549194	3152.323711	22.400743
90.163132	3155.442646	22.405760
90.287957	3142.728611	22.410778
90.567521	3146.428168	22.415795
90.440403	3137.626348	22.420813
90.651999	3138.297070	22.425831
90.962425	3152.861972	22.430848
91.372992	3152.573578	22.435866
91.061580	3145.997390	22.440883
90.985245	3151.469717	22.445901
91.533521	3155.622710	22.450919
91.245538	3172.418177	22.455936
91.450403	3164.927840	22.460954
91.570513	3166.354619	22.465971
91.326883	3168.318140	22.470989
91.549601	3163.877120	22.476007
91.683707	3172.428564	22.481024
91.847756	3166.488038	22.486042
91.884476	3165.538586	22.491059
91.783288	3156.050940	22.496077
92.259173	3161.528284	22.501095
91.658388	3161.130059	22.506112
91.930563	3168.905522	22.511130
92.142753	3183.167056	22.516147
92.240593	3183.098097	22.521165
92.510452	3181.162080	22.526183
92.398146	3191.768998	22.531200
92.552704	3185.968828	22.536218
92.287794	3202.224140	22.541235
92.559913	3207.544046	22.546253
93.094272	3206.563970	22.551271
93.076287	3209.035022	22.556288
92.794994	3216.086056	22.561306
93.001220	3220.223216	22.566323
92.543836	3234.289849	22.571341
93.293115	3235.144618	22.576359
93.202485	3239.441918	22.581376
93.202164	3242.127990	22.586394
93.358568	3248.911616	22.591411
93.229339	3269.381465	22.596429
93.623758	3262.644149	22.601447
93.866620	3271.879297	22.606464
94.021754	3279.919336	22.611482
94.060480	3292.516362	22.616499
94.250148	3297.009639	22.621517
94.373423	3295.109201	22.626535
94.497684	3289.951316	22.631552
94.324007	3283.473437	22.636570
94.475037	3281.521308	22.641587
94.532902	3290.744418	22.646605
94.737054	3292.180134	22.651623
94.705467	3307.935011	22.656640
94.757737	3317.641925	22.661658
94.883920	3313.566341	22.666675
94.908883	3312.577692	22.671693
94.858107	3309.754477	22.676711
94.544618	3324.663459	22.681728
94.858203	3336.134844	22.686746
95.099180	3336.295962	22.691763
95.338644	3347.835780	22.696781
95.501909	3357.815705	22.701799
95.650010	3370.288336	22.706816
95.844495	3360.012528	22.711834
96.174375	3355.813488	22.716851
96.441702	3355.954697	22.721869
96.571921	3357.083215	22.726887
96.458911	3358.600191	22.731904
96.360564	3349.635945	22.736922
96.695085	3350.716673	22.741939
96.530754	3347.384140	22.746957
96.644933	3358.539587	22.751975
96.744062	3373.027302	22.756992
96.955689	3367.227602	22.762010
96.835602	3366.195393	22.767027
96.777284	3376.314202	22.772045
97.272449	3368.308009	22.777063
96.717121	3380.603632	22.782080
97.494540	3380.456607	22.787098
97.412797	3391.813211	22.792115
97.404689	3393.373724	22.797133
97.962199	3390.442569	22.802151
97.528721	3391.791971	22.807168
97.577176	3394.997528	22.812186
97.996385	3400.152412	22.817203
97.714005	3403.154142	22.822221
98.089624	3410.695718	22.827239
97.986898	3420.764696	22.832256
98.034732	3413.434580	22.837274
98.244435	3407.417384	22.842291
98.358852	3432.230205	22.847309
98.248835	3443.177794	22.852327
98.216101	3448.378248	22.857344
98.494626	3449.467755	22.862362
98.644772	3448.004976	22.867379
99.126850	3459.759361	22.872397
99.806351	3445.190672	22.877415
99.923988	3455.641778	22.882432
100.010783	3446.623227	22.887450
99.722760	3449.556409	22.892467
99.807852	3447.583030	22.897485
99.972388	3443.037430	22.902503
99.905756	3446.870197	22.907520
99.825878	3441.220302	22.912538
100.585112	3439.352778	22.917555
100.097154	3444.510925	22.922573
100.018700	3446.076151	22.927591
100.491522	3449.155261	22.932608
100.035236	3451.998023	22.937626
100.325427	3446.034486	22.942643
100.315743	3449.460635	22.947661
100.559975	3452.547153	22.952679
100.693337	3465.170506	22.957696
100.195968	3483.154278	22.962714
100.830000	3471.951021	22.967731
100.741063	3481.847431	22.972749
100.885398	3482.374045	22.977767
101.100515	3496.155607	22.982784
101.039972	3500.656573	22.987802
101.438851	3495.736517	22.992819
101.071968	3502.210838	22.997837
101.393035	3509.016108	23.002855
101.756751	3518.320825	23.007872
101.611208	3523.870391	23.012890
102.329475	3517.012804	23.017907
101.826250	3518.007007	23.022925
102.119360	3515.846369	23.027943
101.950885	3530.000532	23.032960
101.958781	3525.460515	23.037978
102.390262	3524.720641	23.042995
101.852365	3540.883304	23.048013
102.062756	3539.063882	23.053031
101.895101	3555.004421	23.058048
102.384074	3568.402249	23.063066
102.534371	3574.139048	23.068083
102.784427	3576.290398	23.073101
102.859943	3578.267088	23.078119
103.163436	3596.030809	23.083136
102.902925	3613.952351	23.088154
103.312953	3605.372313	23.093171
103.151344	3604.936832	23.098189
103.185749	3615.259035	23.103207
103.626555	3625.211407	23.108224
103.361855	3635.021809	23.113242
103.765832	3631.906352	23.118259
103.815084	3644.015897	23.123277
104.483422	3654.159894	23.128295
104.476655	3662.459039	23.133312
104.332698	3656.907494	23.138330
104.574259	3656.995929	23.143347
104.661372	3663.405491	23.148365
104.290929	3653.003393	23.153383
104.846963	3656.277822	23.158400
104.689543	3672.942823	23.163418
104.970322	3668.259013	23.168435
104.922172	3672.167841	23.173453
104.908348	3675.522085	23.178471
105.174238	3676.632524	23.183488
105.534017	3685.688593	23.188506
105.641014	3700.298435	23.193523
105.238366	3709.761195	23.198541
105.436295	3704.822065	23.203559
105.820778	3697.233928	23.208576
105.549491	3704.580281	23.213594
105.936669	3719.228307	23.218611
106.327504	3731.701035	23.223629
106.365148	3724.413423	23.228647
106.903843	3721.904961	23.233664
106.447946	3729.933615	23.238682
106.521392	3719.566094	23.243699
106.642235	3721.901836	23.248717
106.819628	3721.848819	23.253735
106.821179	3734.281534	23.258752
107.123782	3738.634129	23.263770
107.260422	3733.575183	23.268787
107.294325	3745.119054	23.273805
107.510937	3732.368130	23.278823
107.669434	3737.131536	23.283840
107.293310	3738.506695	23.288858
107.714206	3734.119710	23.293875
107.527686	3768.079953	23.298893
107.638102	3762.791536	23.303911
108.161513	3750.813190	23.308928
108.343471	3755.765463	23.313946
108.240941	3756.867345	23.318963
108.503801	3752.697653	23.323981
108.433821	3752.083681	23.328999
108.734978	3756.764770	23.334016
108.360592	3752.947427	23.339034
108.833984	3771.843091	23.344051
108.784125	3771.888805	23.349069
108.820199	3780.376987	23.354087
108.911858	3781.337973	23.359104
108.735379	3780.223040	23.364122
108.854006	3767.506382	23.369139
109.337649	3785.819682	23.374157
109.378084	3793.079356	23.379175
109.586773	3796.180971	23.384192
109.514305	3799.471829	23.389210
109.668806	3800.236744	23.394227
109.457481	3799.859550	23.399245
109.831913	3820.954985	23.404263
110.098568	3817.980954	23.409280
109.687504	3822.413816	23.414298
110.036664	3822.103472	23.419315
110.345458	3835.283529	23.424333
110.423529	3845.220256	23.429351
110.802341	3841.714158	23.434368
110.579085	3846.351175	23.439386
110.450511	3837.864881	23.444403
111.142356	3860.574049	23.449421
110.589042	3866.405395	23.454439
111.385752	3873.186786	23.459456
111.114176	3872.957910	23.464474
111.040784	3870.172871	23.469491
111.232059	3881.338657	23.474509
111.230183	3894.201288	23.479527
111.696317	3891.439035	23.484544
111.660786	3894.948228	23.489562
112.053099	3910.056438	23.494579
112.719288	3907.212338	23.499597
112.518384	3914.894952	23.504615
112.852886	3916.499681	23.509632
112.807399	3913.151580	23.514650
112.597439	3912.392245	23.519667
113.002446	3908.541139	23.524685
112.984837	3907.044634	23.529703
112.960297	3900.135993	23.534720
112.894986	3907.955180	23.539738
112.992509	3897.621662	23.544755
113.412430	3908.486505	23.549773
113.244671	3919.689627	23.554791
113.413004	3924.918688	23.559808
114.015537	3938.895561	23.564826
113.609356	3934.189897	23.569843
113.887117	3932.568204	23.574861
113.607638	3932.078584	23.579879
114.063548	3940.138079	23.584896
114.163515	3949.115042	23.589914
114.373920	3954.577408	23.594931
114.451076	3956.282431	23.599949
114.484185	3964.275608	23.604967
114.437017	3949.728829	23.609984
114.405733	3967.015088	23.615002
114.429036	3979.630792	23.620019
114.493143	3984.948797	23.625037
114.648931	3986.360584	23.630055
115.054447	3995.633748	23.635072
115.056512	4009.395422	23.640090
114.829316	4014.408713	23.645107
115.553911	4019.190820	23.650125
114.905523	4038.044720	23.655143
115.978646	4029.979255	23.660160
115.567732	4043.082835	23.665178
115.569410	4043.912737	23.670195
115.761956	4058.326392	23.675213
116.046155	4068.679160	23.680231
116.464271	4061.536972	23.685248
116.619291	4068.343218	23.690266
116.561232	4068.724798	23.695283
116.732985	4066.690428	23.700301
116.556716	4079.488976	23.705319
117.010415	4078.493088	23.710336
117.002734	4095.043480	23.715354
116.923298	4094.705587	23.720371
117.051695	4094.795972	23.725389
117.132262	4097.605226	23.730407
117.198627	4106.546498	23.735424
117.030441	4104.249738	23.740442
117.287038	4103.635093	23.745459
117.512483	4112.431500	23.750477
117.599580	4132.805302	23.755495
117.615805	4142.660345	23.760512
117.704116	4148.612207	23.765530
118.086118	4147.747492	23.770547
118.362025	4159.058013	23.775565
118.291247	4162.389705	23.780583
118.467866	4160.263026	23.785600
118.629257	4167.393424	23.790618
118.848580	4175.158664	23.795635
118.966529	4176.232341	23.800653
118.973519	4174.577294	23.805671
119.123421	4179.629400	23.810688
119.452448	4189.208197	23.815706
119.623098	4193.240680	23.820723
119.568042	4202.605047	23.825741
119.645056	4215.733314	23.830759
120.080529	4207.303674	23.835776
120.022556	4201.299745	23.840794
119.766510	4205.749446	23.845811
120.088836	4218.668834	23.850829
120.005417	4225.222101	23.855847
120.243361	4236.222972	23.860864
120.110868	4237.275917	23.865882
120.399389	4255.699174	23.870899
121.282574	4252.798931	23.875917
120.753689	4261.969264	23.880935
120.970072	4256.774577	23.885952
120.859212	4259.531779	23.890970
120.992068	4272.338849	23.895987
121.422551	4279.247214	23.901005
121.447367	4283.056360	23.906023
121.610296	4276.408600	23.911040
121.412963	4296.849243	23.916058
121.237626	4308.416784	23.921075
121.794214	4306.827131	23.926093
122.073897	4334.153096	23.931111
122.324559	4326.576195	23.936128
122.501652	4334.004063	23.941146
122.222201	4336.860288	23.946163
122.593437	4322.424422	23.951181
122.948254	4343.182640	23.956199
123.144519	4348.246468	23.961216
123.087364	4352.169479	23.966234
123.202915	4353.331924	23.971251
123.189689	4351.632681	23.976269
123.370477	4355.098602	23.981287
123.496478	4352.279093	23.986304
123.450824	4350.117773	23.991322
123.543156	4370.948711	23.996339
123.988936	4373.189440	24.001357
123.846223	4388.249301	24.006375
123.880215	4383.559782	24.011392
124.348123	4377.953190	24.016410
124.446126	4394.294752	24.021427
124.439906	4397.644782	24.026445
124.260361	4404.989668	24.031463
124.308820	4400.490424	24.036480
124.559075	4394.163527	24.041498
124.931377	4424.076059	24.046515
125.229448	4433.268431	24.051533
125.002716	4429.831840	24.056551
125.044103	4425.557809	24.061568
125.348608	4426.592804	24.066586
125.213133	4445.379392	24.071603
125.721108	4450.877356	24.076621
126.006895	4452.085736	24.081639
125.940763	4454.258321	24.086656
125.944941	4450.517248	24.091674
125.783903	4460.463364	24.096691
126.451796	4469.083306	24.101709
126.507426	4470.804377	24.106727
126.652682	4471.668621	24.111744
127.033660	4467.319281	24.116762
126.770472	4461.622032	24.121779
127.316214	4451.773520	24.126797
127.172998	4468.263417	24.131815
127.051707	4473.885227	24.136832
127.840558	4479.389701	24.141850
127.221972	4486.743431	24.146867
127.506793	4476.610664	24.151885
127.549517	4487.010973	24.156903
127.684363	4497.990277	24.161920
127.901430	4494.439953	24.166938
127.823861	4517.772375	24.171955
127.934345	4507.657435	24.176973
128.108448	4523.217004	24.181991
128.188327	4537.263598	24.187008
128.685251	4535.538074	24.192026
129.043304	4544.493837	24.197043
128.948135	4542.416007	24.202061
128.934048	4548.649190	24.207079
129.265143	4569.117829	24.212096
129.459083	4560.855284	24.217114
129.072279	4569.157566	24.222131
129.607828	4563.859128	24.227149
129.747530	4579.048509	24.232167
129.517515	4589.450571	24.237184
129.584678	4581.384644	24.242202
129.852401	4597.103217	24.247219
130.041780	4592.821743	24.252237
130.043082	4604.042990	24.257255
129.971511	4602.741117	24.262272
130.685898	4603.424664	24.267290
130.395265	4630.332226	24.272307
130.244147	4624.289088	24.277325
130.315874	4637.721515	24.282343
130.903952	4664.437800	24.287360
131.304826	4662.932487	24.292378
131.039242	4666.297948	24.297395
131.356110	4665.541268	24.302413
131.863661	4690.338411	24.307431
131.651979	4702.618959	24.312448
131.771104	4697.284715	24.317466
131.658630	4701.330102	24.322483
131.923643	4708.340314	24.327501
132.004333	4721.837685	24.332519
132.213632	4721.198865	24.337536
132.448011	4718.801079	24.342554
132.481940	4743.580956	24.347571
132.939878	4741.463798	24.352589
133.286437	4747.296484	24.357607
133.271469	4744.366425	24.362624
133.510232	4747.340388	24.367642
133.277728	4742.149602	24.372659
133.376357	4743.545152	24.377677
133.567139	4732.609432	24.382695
133.187058	4752.078592	24.387712
133.323394	4766.081796	24.392730
133.330625	4771.869799	24.397747
133.938034	4786.714615	24.402765
133.860033	4797.841082	24.407783
133.580106	4807.184173	24.412800
133.920999	4823.065088	24.417818
134.222461	4831.499557	24.422835
134.549793	4835.311930	24.427853
134.766473	4851.827860	24.432871
134.487651	4859.813482	24.437888
135.015845	4851.050208	24.442906
134.864640	4869.372525	24.447923
134.836395	4873.508921	24.452941
135.432221	4880.047548	24.457959
135.742084	4885.390447	24.462976
136.164346	4882.679113	24.467994
136.358535	4881.427124	24.473011
136.254470	4882.999642	24.478029
136.755227	4880.717931	24.483047
136.249621	4879.654492	24.488064
136.760034	4874.978591	24.493082
137.119094	4872.100393	24.498099
137.147715	4874.302375	24.503117
137.178387	4872.615146	24.508135
137.413838	4892.287895	24.513152
137.602026	4889.976239	24.518170
137.691807	4899.431909	24.523187
137.755269	4895.776154	24.528205
137.724641	4896.323908	24.533223
137.423007	4899.808696	24.538240
137.502432	4905.348688	24.543258
137.750769	4917.453144	24.548275
137.694765	4928.061723	24.553293
138.230970	4936.061736	24.558311
138.289055	4954.083041	24.563328
138.332694	4955.376741	24.568346
138.260991	4966.540204	24.573363
138.079682	4979.958864	24.578381
138.506427	4987.994988	24.583399
138.818582	5008.896384	24.588416
139.055058	4994.825169	24.593434
139.339578	5019.168431	24.598451
139.058406	5027.987835	24.603469
139.765651	5029.531114	24.608487
139.675352	5039.119237	24.613504
139.775329	5038.680616	24.618522
140.164372	5054.450023	24.623539
140.211138	5060.841147	24.628557
140.262041	5057.673443	24.633575
140.266857	5067.221427	24.638592
140.762335	5078.517061	24.643610
140.855494	5088.502610	24.648627
141.192625	5086.660024	24.653645
141.306617	5086.894720	24.658663
141.032686	5091.505268	24.663680
141.302061	5097.312280	24.668698
141.496535	5109.207497	24.673715
141.738464	5119.362308	24.678733
141.997849	5120.091910	24.683751
141.650716	5126.535298	24.688768
141.721485	5144.033962	24.693786
141.853937	5151.039860	24.698803
142.032189	5151.261332	24.703821
142.581958	5153.148112	24.708839
142.374385	5168.326102	24.713856
142.502996	5169.521277	24.718874
142.888271	5175.275434	24.723891
142.980903	5178.606964	24.728909
143.148151	5193.341145	24.733927
143.128424	5198.000279	24.738944
143.034852	5191.644902	24.743962
143.350804	5206.680929	24.748979
143.615620	5215.402258	24.753997
143.683869	5216.739470	24.759015
143.692514	5234.049086	24.764032
144.085750	5249.372921	24.769050
143.748916	5258.128553	24.774067
143.908029	5260.862548	24.779085
144.572694	5258.286800	24.784103
145.038414	5262.295390	24.789120
145.276266	5264.335217	24.794138
145.380232	5265.991971	24.799155
145.175005	5264.262748	24.804173
145.645440	5270.196148	24.809191
145.573480	5290.220525	24.814208
145.859359	5283.594173	24.819226
145.886088	5288.725861	24.824243
145.947448	5286.708653	24.829261
146.278072	5295.757470	24.834279
146.135121	5304.410147	24.839296
146.296880	5306.139923	24.844314
146.793556	5315.711991	24.849331
146.796151	5315.351753	24.854349
146.702764	5315.047589	24.859367
146.777876	5333.502218	24.864384
147.274350	5336.628459	24.869402
147.285152	5333.990993	24.874419
146.842859	5354.247075	24.879437
147.622976	5357.461461	24.884455
147.403169	5367.111083	24.889472
147.548381	5376.447834	24.894490
148.009107	5394.529603	24.899507
147.761420	5402.535836	24.904525
147.843311	5398.438317	24.909543
148.021924	5415.083832	24.914560
148.386497	5426.494892	24.919578
148.361096	5428.793790	24.924595
148.593670	5437.542374	24.929613
148.929404	5443.234931	24.934631
149.082658	5462.621290	24.939648
149.157807	5479.077889	24.944666
149.593984	5482.652380	24.949683
149.223069	5483.941618	24.954701
149.786307	5492.344853	24.959719
149.608682	5501.157731	24.964736
150.113650	5509.585887	24.969754
150.039560	5518.660340	24.974771
150.283581	5523.795933	24.979789
150.371943	5523.466447	24.984807
150.421214	5533.635890	24.989824
150.609855	5552.290764	24.994842
150.781421	5552.835271	24.999859
150.865393	5574.565393	25.004877
151.123963	5571.810159	25.009895
151.541090	5579.649181	25.014912
151.456735	5585.265546	25.019930
151.872542	5591.248647	25.024947
151.994916	5600.219758	25.029965
152.312893	5607.379854	25.034983
152.606604	5608.242993	25.040000
152.704297	5606.387362	25.045018
152.762910	5599.373505	25.050035
152.601357	5607.094857	25.055053
152.449120	5609.249501	25.060071
152.726656	5621.899116	25.065088
153.012569	5628.505509	25.070106
152.855600	5636.481848	25.075123
152.845753	5646.868957	25.080141
153.139709	5654.739936	25.085159
153.302776	5666.930854	25.090176
153.510461	5679.632489	25.095194
153.614853	5686.014804	25.100211
153.668274	5692.383010	25.105229
153.838531	5700.904729	25.110247
153.979824	5704.168755	25.115264
154.819074	5707.411822	25.120282
155.638903	5711.803819	25.125299
155.494330	5713.404850	25.130317
156.008360	5705.025353	25.135335
156.215444	5719.150787	25.140352
156.158037	5713.275695	25.145370
156.224608	5688.418831	25.150387
156.313510	5679.733456	25.155405
156.048133	5674.689605	25.160423
156.098931	5682.450325	25.165440
156.287734	5689.226633	25.170458
156.724377	5701.538863	25.175475
156.679949	5699.052049	25.180493
156.726117	5696.794108	25.185511
156.809826	5706.847767	25.190528
157.036664	5727.731788	25.195546
157.490130	5732.320082	25.200563
157.420636	5728.770221	25.205581
157.494658	5734.207140	25.210599
157.494770	5737.957327	25.215616
157.231193	5750.944342	25.220634
157.688021	5755.235384	25.225651
157.624274	5777.462398	25.230669
158.013637	5785.596278	25.235687
158.260399	5792.123632	25.240704
157.676678	5810.091651	25.245722
158.175456	5821.305156	25.250739
158.611529	5846.118229	25.255757
158.513943	5849.485996	25.260775
158.424244	5855.930345	25.265792
158.649136	5875.571086	25.270810
159.067167	5885.705049	25.275827
158.974951	5904.252760	25.280845
159.221830	5917.832309	25.285863
159.326984	5931.478266	25.290880
159.619801	5948.286310	25.295898
160.327604	5954.435288	25.300915
160.463257	5961.062185	25.305933
160.898193	5962.670309	25.310951
160.804229	5968.433507	25.315968
160.645758	5988.611098	25.320986
160.898395	5978.899237	25.326003
161.132602	5997.907298	25.331021
161.369254	6007.526783	25.336039
161.746000	6010.495121	25.341056
161.572397	6016.381297	25.346074
161.588674	6024.857843	25.351091
161.838590	6027.015824	25.356109
161.884615	6038.114145	25.361127
162.188122	6060.110343	25.366144
162.555995	6063.477833	25.371162
163.028308	6063.384924	25.376179
162.997219	6065.274413	25.381197
163.057430	6079.489427	25.386215
163.294215	6089.920225	25.391232
163.211969	6089.592204	25.396250
163.829867	6087.506659	25.401267
163.822062	6092.738686	25.406285
163.897028	6090.296250	25.411303
164.433590	6095.802867	25.416320
164.157512	6102.715294	25.421338
164.267849	6100.216806	25.426355
164.440789	6107.033635	25.431373
164.335141	6099.745426	25.436391
164.964645	6108.299563	25.441408
165.165618	6128.667225	25.446426
164.944238	6129.213332	25.451443
165.132382	6138.824701	25.456461
165.376961	6145.024218	25.461479
165.266001	6150.929034	25.466496
165.397556	6162.332866	25.471514
165.713243	6172.833427	25.476531
165.784070	6175.243615	25.481549
165.996749	6198.763156	25.486567
166.320614	6200.622305	25.491584
166.346061	6212.607858	25.496602
166.624128	6223.379512	25.501619
166.772604	6241.214300	25.506637
166.868723	6232.454927	25.511655
167.009772	6245.221061	25.516672
167.412574	6265.929759	25.521690
167.669337	6265.548624	25.526707
167.428374	6282.977257	25.531725
167.348893	6289.325453	25.536743
167.953374	6308.960856	25.541760
168.220115	6316.040867	25.546778
168.141417	6328.749938	25.551795
168.471517	6340.211167	25.556813
168.453997	6343.879005	25.561831
168.992097	6345.265809	25.566848
168.855101	6363.394828	25.571866
169.211037	6376.951319	25.576883
169.568377	6378.489560	25.581901
169.106715	6404.608902	25.586919
169.609943	6396.486488	25.591936
169.585760	6415.409190	25.596954
169.718004	6422.655527	25.601971
169.750482	6436.218541	25.606989
170.199856	6450.120328	25.612007
170.902331	6452.437910	25.617024
170.469962	6469.874608	25.622042
171.010966	6482.174173	25.627059
171.036573	6483.559199	25.632077
171.446922	6496.687394	25.637095
172.095076	6504.620054	25.642112
172.004180	6509.161240	25.647130
171.932982	6504.939087	25.652147
172.096137	6511.845991	25.657165
172.178273	6521.846677	25.662183
172.728857	6525.062513	25.667200
172.549904	6530.062616	25.672218
172.656230	6524.458357	25.677236
173.063780	6535.481399	25.682253
172.963126	6550.968937	25.687271
173.609568	6542.198966	25.692288
173.575240	6551.633896	25.697306
173.616816	6562.212349	25.702324
173.793434	6578.398333	25.707341
173.657918	6587.135684	25.712359
174.051701	6587.566489	25.717376
174.324983	6597.006917	25.722394
174.239767	6605.610121	25.727412
174.552684	6611.612836	25.732429
174.541889	6626.893792	25.737447
175.008369	6631.028844	25.742464
175.255436	6641.489914	25.747482
175.051340	6646.430850	25.752500
175.445172	6659.836398	25.757517
175.452979	6664.905142	25.762535
175.895226	6664.169784	25.767552
175.636344	6675.215237	25.772570
175.863558	6688.754243	25.777588
176.362694	6695.703288	25.782605
176.178879	6704.637673	25.787623
175.907014	6718.513753	25.792640
176.395055	6733.943944	25.797658
176.378250	6742.394434	25.802676
176.870987	6754.004072	25.807693
176.801704	6778.083101	25.812711
177.407831	6786.773809	25.817728
177.133226	6812.122553	25.822746
177.701136	6817.132003	25.827764
177.520129	6834.371821	25.832781
177.517467	6854.380734	25.837799
177.982125	6858.531908	25.842816
178.149734	6874.965804	25.847834
178.723951	6891.572783	25.852852
179.018901	6904.605701	25.857869
179.263584	6920.487730	25.862887
179.144653	6928.180860	25.867904
179.481935	6934.097784	25.872922
179.509824	6941.202829	25.877940
179.484322	6952.480225	25.882957
179.922265	6956.730315	25.887975
180.529630	6970.677198	25.892992
180.828625	6975.409972	25.898010
180.982613	6977.317914	25.903028
180.868532	6979.163674	25.908045
180.738322	7000.414460	25.913063
181.305330	7003.823539	25.918080
181.365279	7014.503552	25.923098
181.628357	7026.805984	25.928116
181.627078	7028.839279	25.933133
181.767827	7047.585258	25.938151
181.623129	7055.610800	25.943168
181.937613	7062.787800	25.948186
182.257731	7083.548258	25.953204
182.564208	7095.174665	25.958221
182.530596	7098.033839	25.963239
183.149165	7110.583702	25.968256
183.002070	7115.474792	25.973274
183.208221	7131.309372	25.978292
183.280625	7146.003158	25.983309
183.424359	7151.069683	25.988327
183.778354	7161.706873	25.993344
184.430320	7169.168839	25.998362
184.085637	7173.128026	26.003380
184.454112	7184.801602	26.008397
184.768419	7191.271520	26.013415
185.374622	7187.650247	26.018432
185.782610	7188.855457	26.023450
185.848710	7195.162215	26.028468
185.729211	7198.199022	26.033485
185.358469	7209.072900	26.038503
185.975490	7211.239809	26.043520
186.408966	7218.884403	26.048538
186.723201	7220.148499	26.053556
186.858492	7233.108797	26.058573
186.995867	7240.187335	26.063591
187.452074	7227.866836	26.068608
187.603575	7221.904865	26.073626
187.550458	7231.851359	26.078644
187.934575	7214.396298	26.083661
187.764603	7216.402372	26.088679
187.915349	7225.234085	26.093696
188.117222	7212.359930	26.098714
188.150671	7217.345884	26.103732
188.042845	7222.742280	26.108749
188.404788	7237.640181	26.113767
188.313131	7243.687543	26.118784
188.268395	7251.871144	26.123802
188.451688	7267.589457	26.128820
188.685431	7274.311957	26.133837
188.684034	7295.647083	26.138855
189.303183	7302.792233	26.143872
190.069008	7318.870779	26.148890
189.652377	7329.171031	26.153908
190.278695	7322.197016	26.158925
189.927923	7343.028143	26.163943
190.250627	7353.503027	26.168960
190.324404	7352.601222	26.173978
190.385948	7369.311050	26.178996
190.746546	7371.268748	26.184013
190.875933	7393.899966	26.189031
190.917824	7421.422491	26.194048
191.128899	7422.715392	26.199066
191.339742	7430.041368	26.204084
191.751294	7447.280479	26.209101
191.996959	7468.517117	26.214119
192.236452	7475.747069	26.219136
191.959295	7492.020731	26.224154
192.340608	7513.397178	26.229172
192.360831	7507.559862	26.234189
192.324583	7536.897459	26.239207
192.839037	7549.075621	26.244224
193.269860	7568.269183	26.249242
193.458995	7586.026294	26.254260
193.299689	7599.039316	26.259277
193.777834	7612.072450	26.264295
194.450733	7620.153258	26.269312
194.713229	7638.157804	26.274330
194.443041	7642.200131	26.279348
194.727392	7662.767952	26.284365
195.188277	7663.623947	26.289383
195.182759	7667.492220	26.294400
195.245536	7684.524158	26.299418
195.507650	7696.438872	26.304436
195.935582	7700.646507	26.309453
196.288895	7715.479848	26.314471
196.261578	7715.171605	26.319488
196.325709	7716.427564	26.324506
196.598165	7739.368283	26.329524
196.846063	7740.939573	26.334541
197.351974	7767.442802	26.339559
197.237014	7771.457682	26.344576
197.670605	7777.422932	26.349594
197.433406	7790.678757	26.354612
197.927685	7803.599002	26.359629
197.544296	7810.153184	26.364647
197.999812	7814.476493	26.369664
198.552078	7815.333965	26.374682
198.171628	7830.361277	26.379700
198.637243	7841.912713	26.384717
198.863277	7855.938953	26.389735
199.271262	7865.346303	26.394752
199.241789	7878.563334	26.399770
199.258216	7889.316971	26.404788
199.897660	7904.787570	26.409805
199.670514	7914.215518	26.414823
199.651089	7929.615717	26.419840
199.977275	7932.516523	26.424858
200.006930	7951.309239	26.429876
200.795265	7968.088861	26.434893
200.624575	7972.365082	26.439911
200.741619	7996.343896	26.444928
201.284607	8005.060862	26.449946
200.777678	8021.727738	26.454964
201.258287	8037.368559	26.459981
201.499935	8054.451743	26.464999
201.730441	8064.897276	26.470016
201.905639	8082.906460	26.475034
201.610587	8099.593884	26.480052
202.116238	8117.857574	26.485069
202.232844	8127.932660	26.490087
202.393923	8146.114603	26.495104
203.435539	8159.618663	26.500122
203.013954	8184.269329	26.505140
203.273520	8195.300767	26.510157
203.656359	8212.172550	26.515175
203.763292	8234.309486	26.520192
204.430482	8234.384948	26.525210
204.266896	8269.653828	26.530228
204.521057	8274.573919	26.535245
204.622708	8287.994858	26.540263
204.824712	8301.460070	26.545280
205.166600	8312.181909	26.550298
205.207880	8330.651158	26.555316
205.782716	8344.900957	26.560333
206.209000	8342.810460	26.565351
206.253938	8348.606311	26.570368
206.924183	8353.514912	26.575386
206.559890	8368.120224	26.580404
207.124875	8378.084160	26.585421
207.454403	8383.323977	26.590439
207.578754	8393.555852	26.595456
208.123342	8385.186150	26.600474
208.369986	8389.510745	26.605492
208.392874	8403.629212	26.610509
208.246139	8406.904113	26.615527
208.385873	8412.508331	26.620544
208.920420	8420.368067	26.625562
208.905156	8436.873046	26.630580
209.160693	8425.770291	26.635597
209.331907	8439.549832	26.640615
208.965183	8465.006826	26.645632
209.624222	8461.493851	26.650650
209.751874	8489.121344	26.655668
210.095614	8497.872916	26.660685
210.302881	8504.252723	26.665703
210.205697	8524.120392	26.670720
210.534760	8524.302499	26.675738
210.767789	8546.435841	26.680756
210.740788	8551.062233	26.685773
211.432169	8562.152531	26.690791
211.644959	8577.201168	26.695808
211.715379	8582.816297	26.700826
212.143827	8587.349248	26.705844
212.454992	8596.980516	26.710861
212.527004	8598.768868	26.715879
212.611320	8625.443563	26.720896
212.813002	8619.217548	26.725914
213.180047	8635.789101	26.730932
213.650611	8647.801220	26.735949
213.597242	8650.098587	26.740967
213.778897	8655.431105	26.745984
214.138803	8654.361283	26.751002
214.390028	8660.251203	26.756020
214.315059	8675.537591	26.761037
214.624647	8680.831132	26.766055
214.681699	8682.331371	26.771072
214.952029	8686.008253	26.776090
214.701723	8706.582065	26.781108
215.087450	8713.865367	26.786125
215.464841	8711.469925	26.791143
215.557049	8736.075561	26.796160
215.919728	8742.109066	26.801178
215.798714	8762.921578	26.806196
215.556891	8764.812784	26.811213
216.069646	8781.156419	26.816231
215.771120	8799.821445	26.821248
216.480834	8822.489787	26.826266
216.610572	8845.100624	26.831284
216.791206	8868.764352	26.836301
217.247823	8873.978085	26.841319
217.479618	8902.666502	26.846336
217.811953	8913.257582	26.851354
218.182468	8928.266009	26.856372
218.399881	8937.084939	26.861389
218.860867	8950.494266	26.866407
218.700629	8965.544826	26.871424
219.289173	8975.173882	26.876442
219.354803	8997.229796	26.881460
219.312207	8999.405542	26.886477
219.560239	9012.980881	26.891495
219.560498	9028.650433	26.896512
220.070687	9047.577360	26.901530
220.079066	9068.647784	26.906548
220.322431	9075.918802	26.911565
220.808243	9097.751146	26.916583
220.549837	9111.368006	26.921600
221.562683	9125.186701	26.926618
221.696692	9139.263061	26.931636
221.601557	9154.164654	26.936653
222.199357	9165.440470	26.941671
222.763700	9158.781743	26.946688
223.401187	9168.254840	26.951706
223.921355	9164.460390	26.956724
224.014098	9157.364061	26.961741
224.523855	9149.539374	26.966759
224.725232	9156.374979	26.971776
224.876892	9144.580835	26.976794
224.833244	9155.499325	26.981812
224.758767	9150.724552	26.986829
224.900969	9147.560788	26.991847
225.229248	9154.932197	26.996864
225.090116	9143.619316	27.001882
225.279986	9163.398496	27.006900
225.301464	9173.700593	27.011917
225.625732	9178.382618	27.016935
225.609642	9195.680884	27.021952
226.244052	9205.754371	27.026970
226.323165	9215.422314	27.031988
226.125620	9240.152942	27.037005
226.473773	9244.850186	27.042023
226.164647	9264.540307	27.047040
226.553533	9278.838902	27.052058
226.577094	9298.688482	27.057076
226.753312	9325.204548	27.062093
226.988731	9342.599314	27.067111
226.639665	9369.743951	27.072128
227.105105	9385.855576	27.077146
227.990356	9396.303482	27.082164
227.940344	9421.450108	27.087181
228.555197	9439.584332	27.092199
228.593096	9450.256576	27.097216
228.801301	9473.872552	27.102234
228.887706	9488.670196	27.107252
228.909047	9514.459342	27.112269
229.335641	9526.422088	27.117287
229.636078	9544.495163	27.122304
230.086891	9568.234278	27.127322
230.303865	9578.600693	27.132340
230.000955	9590.775641	27.137357
230.642039	9607.245142	27.142375
230.830538	9633.207180	27.147392
230.947402	9652.660477	27.152410
231.373690	9657.314012	27.157428
231.299872	9690.857062	27.162445
231.637953	9707.576192	27.167463
232.031898	9728.706941	27.172480
232.361555	9739.990384	27.177498
232.979613	9750.672950	27.182516
232.771436	9783.583632	27.187533
233.020406	9793.389451	27.192551
232.646171	9813.425035	27.197568
233.487405	9826.033435	27.202586
233.738517	9845.058596	27.207604
233.907968	9872.694225	27.212621
234.200100	9882.537533	27.217639
234.530447	9901.234596	27.222656
234.653409	9916.850941	27.227674
235.117228	9936.673276	27.232692
235.154894	9952.530348	27.237709
235.710497	9972.856163	27.242727
236.130821	9980.674468	27.247744
235.844228	9995.982460	27.252762
236.384996	10018.340885	27.257780
236.582608	10030.803972	27.262797
237.367568	10030.636825	27.267815
237.580648	10048.594619	27.272832
238.045692	10050.122620	27.277850
238.690545	10046.895750	27.282868
238.702433	10055.381143	27.287885
239.131770	10047.972836	27.292903
239.161494	10046.070577	27.297920
238.939354	10052.464510	27.302938
239.498570	10065.587714	27.307956
239.233225	10080.605119	27.312973
239.685695	10081.790931	27.317991
240.192691	10080.641155	27.323008
240.617649	10092.711876	27.328026
241.002268	10085.174789	27.333044
240.739536	10096.033425	27.338061
241.030268	10095.624799	27.343079
241.337812	10117.735708	27.348096
241.272104	10111.266914	27.353114
241.911320	10124.693375	27.358132
241.973093	10140.553145	27.363149
242.203638	10140.946470	27.368167
242.445104	10140.071941	27.373184
242.882326	10170.911940	27.378202
243.057106	10165.191665	27.383220
242.914759	10173.353952	27.388237
243.068053	10181.678323	27.393255
243.589051	10196.901013	27.398272
243.453816	10200.480700	27.403290
243.323835	10211.766969	27.408308
243.719477	10233.409537	27.413325
243.677048	10252.383217	27.418343
244.190026	10273.363323	27.423360
244.151600	10286.472953	27.428378
244.396628	10298.837224	27.433396
244.214181	10324.195261	27.438413
244.581535	10345.630838	27.443431
244.897923	10365.066251	27.448448
245.320813	10388.580288	27.453466
245.572677	10403.775843	27.458484
245.803676	10425.772808	27.463501
245.708612	10448.010328	27.468519
246.107739	10463.767004	27.473536
246.519770	10496.146042	27.478554
246.639453	10518.337374	27.483572
246.927681	10538.598337	27.488589
246.940668	10553.244134	27.493607
247.127058	10579.173084	27.498624
247.431771	10601.180810	27.503642
247.789358	10622.018300	27.508660
248.216523	10655.424603	27.513677
248.386308	10668.062983	27.518695
248.836888	10689.359614	27.523712
249.033612	10720.124522	27.528730
249.538743	10740.970608	27.533748
249.622306	10753.973042	27.538765
250.348361	10770.360797	27.543783
251.095829	10770.714207	27.548800
250.877582	10787.082554	27.553818
251.362941	10806.551949	27.558836
251.250876	10810.497559	27.563853
251.601762	10824.822240	27.568871
252.011039	10844.733025	27.573888
251.988344	10860.666631	27.578906
252.209665	10875.248467	27.583924
252.553450	10890.063737	27.588941
252.560268	10903.975054	27.593959
252.854015	10930.146595	27.598976
253.013482	10946.500117	27.603994
253.103308	10961.765715	27.609012
253.056434	10980.197719	27.614029
252.966404	11003.720255	27.619047
254.044337	11036.437976	27.624064
253.990051	11059.405557	27.629082
254.602068	11076.310349	27.634100
254.487197	11090.793452	27.639117
254.908148	11110.942671	27.644135
255.546888	11123.697352	27.649152
255.777910	11154.246038	27.654170
256.056116	11165.004762	27.659188
256.401549	11181.038853	27.664205
257.045580	11192.867563	27.669223
257.142318	11205.243033	27.674240
257.020342	11216.361296	27.679258
257.056010	11238.793992	27.684276
257.732254	11250.920828	27.689293
257.936377	11277.624749	27.694311
258.289491	11284.945749	27.699328
258.150329	11314.147527	27.704346
258.639857	11325.100590	27.709364
258.991768	11341.904274	27.714381
259.045776	11354.447577	27.719399
259.361918	11361.995436	27.724416
259.367654	11402.074939	27.729434
259.802341	11406.989688	27.734452
260.195069	11429.388781	27.739469
259.982169	11439.757259	27.744487
260.682900	11455.009658	27.749504
260.600073	11482.977690	27.754522
261.097883	11494.096913	27.759540
261.504465	11516.010811	27.764557
261.777628	11534.086925	27.769575
261.967070	11551.156233	27.774592
262.093584	11568.709071	27.779610
262.368502	11576.203478	27.784628
262.235031	11580.730462	27.789645
262.870573	11613.218512	27.794663
263.443834	11628.396289	27.799680
263.016159	11655.111303	27.804698
263.523965	11666.396422	27.809716
263.957360	11680.986712	27.814733
263.829492	11704.522366	27.819751
264.069153	11717.598904	27.824768
264.289596	11735.036134	27.829786
264.915152	11764.794570	27.834804
265.089766	11784.092619	27.839821
265.235873	11803.398311	27.844839
265.562928	11820.859971	27.849856
266.198318	11846.174042	27.854874
266.594844	11864.433245	27.859892
267.023941	11877.988617	27.864909
267.076249	11887.722137	27.869927
267.629285	11901.583360	27.874944
267.796368	11920.519586	27.879962
267.892069	11927.480126	27.884980
268.296744	11933.520723	27.889997
268.731140	11966.062997	27.895015
268.495129	11964.552685	27.900032
268.768102	11994.388822	27.905050
268.956283	12012.709226	27.910068
269.500195	12028.327699	27.915085
269.194868	12039.213072	27.920103
269.804635	12066.290341	27.925120
269.878530	12085.787628	27.930138
269.924544	12107.682914	27.935156
270.403160	12134.307156	27.940173
270.513049	12151.471573	27.945191
271.138187	12177.820299	27.950208
271.448527	12207.944596	27.955226
271.871156	12223.099084	27.960244
271.773831	12238.691871	27.965261
272.207056	12249.158518	27.970279
272.675413	12276.166664	27.975296
272.776638	12299.089288	27.980314
272.710635	12322.764439	27.985332
273.152509	12345.728491	27.990349
273.184289	12370.803095	27.995367
274.340549	12380.196567	28.000384
274.334128	12408.586624	28.005402
274.519748	12420.465818	28.010420
274.748902	12431.652946	28.015437
274.659592	12456.074009	28.020455
275.564325	12484.157238	28.025472
275.585498	12507.727385	28.030490
275.694472	12519.871278	28.035508
275.833108	12542.131500	28.040525
276.028467	12564.114444	28.045543
276.939993	12586.768378	28.050560
277.129799	12607.214356	28.055578
277.055089	12624.509172	28.060596
277.287674	12648.343218	28.065613
277.567255	12670.562565	28.070631
278.533150	12686.516533	28.075648
278.512870	12710.260794	28.080666
279.087934	12719.142325	28.085684
279.133591	12735.969966	28.090701
279.337621	12753.262288	28.095719
279.723529	12759.805040	28.100736
280.042996	12782.848801	28.105754
280.477904	12812.493493	28.110772
280.646168	12804.657639	28.115789
281.066191	12823.994097	28.120807
281.408224	12834.917464	28.125824
281.260219	12847.051296	28.130842
281.657449	12850.892285	28.135860
282.137861	12872.913040	28.140877
282.403461	12891.386381	28.145895
282.831678	12883.626616	28.150912
282.530406	12896.005543	28.155930
282.649984	12922.529245	28.160948
283.224940	12941.083649	28.165965
283.140387	12961.127719	28.170983
283.676047	12975.971418	28.176000
284.203818	13002.093388	28.181018
284.465369	13020.526435	28.186036
284.313882	13030.832477	28.191053
284.483283	13062.309711	28.196071
285.024625	13072.870409	28.201088
285.161469	13097.872673	28.206106
285.386208	13132.489843	28.211124
285.852178	13154.693193	28.216141
285.619619	13174.315399	28.221159
286.010537	13192.513606	28.226176
286.373081	13227.377790	28.231194
287.163434	13247.701962	28.236212
287.180527	13258.644896	28.241229
287.562864	13287.578546	28.246247
287.796974	13309.676289	28.251264
287.763984	13335.049692	28.256282
287.922328	13361.425824	28.261300
288.410579	13372.945567	28.266317
289.114712	13396.394043	28.271335
289.608924	13418.931185	28.276352
290.129370	13441.517932	28.281370
290.351794	13459.344880	28.286388
290.982934	13467.820070	28.291405
291.075466	13491.860281	28.296423
291.265348	13499.321405	28.301440
291.577096	13518.552372	28.306458
291.434539	13544.852731	28.311476
292.240975	13541.839984	28.316493
292.096129	13582.149806	28.321511
292.494463	13599.046129	28.326528
292.692456	13619.226641	28.331546
292.854993	13634.653544	28.336564
293.315594	13655.411934	28.341581
293.604919	13681.556403	28.346599
293.790183	13708.333031	28.351616
293.987712	13725.586203	28.356634
294.179578	13750.520704	28.361652
294.709808	13772.642076	28.366669
294.511513	13800.240014	28.371687
294.861691	13814.428125	28.376704
295.873416	13833.426594	28.381722
295.612102	13852.877150	28.386740
296.277063	13876.913445	28.391757
296.363678	13902.290975	28.396775
296.972919	13925.022292	28.401792
297.325713	13942.134489	28.406810
297.288212	13966.451476	28.411828
297.934329	13975.243518	28.416845
298.171307	13993.776104	28.421863
298.700929	14016.706332	28.426880
299.197889	14028.869365	28.431898
299.149726	14045.359154	28.436916
299.604351	14066.311575	28.441933
299.599921	14081.291277	28.446951
300.044446	14093.509938	28.451968
300.221586	14099.678462	28.456986
299.961349	14128.751949	28.462004
300.615280	14142.725342	28.467021
300.937789	14168.975818	28.472039
301.009174	14192.878110	28.477056
301.197426	14209.836310	28.482074
301.447101	14234.064438	28.487092
301.703757	14253.333201	28.492109
302.024639	14288.199540	28.497127
302.331121	14308.565910	28.502144
302.551149	14334.643177	28.507162
302.793720	14366.651153	28.512180
303.555006	14380.724757	28.517197
303.449339	14408.040618	28.522215
304.097371	14430.621188	28.527232
304.313371	14452.969434	28.532250
304.310403	14483.244327	28.537268
304.926841	14513.501193	28.542285
305.069470	14537.468554	28.547303
305.545540	14566.149442	28.552320
305.720383	14583.141656	28.557338
305.753668	14614.652254	28.562356
306.450787	14638.753956	28.567373
307.063161	14665.575561	28.572391
307.122757	14690.554118	28.577408
307.416596	14709.214296	28.582426
307.811353	14735.473183	28.587444
308.389823	14753.583500	28.592461
308.799823	14782.372969	28.597479
309.237222	14796.023882	28.602496
309.479800	14818.605261	28.607514
309.530534	14835.156036	28.612532
310.161123	14855.794361	28.617549
310.056232	14877.264844	28.622567
310.931822	14902.450630	28.627584
311.045128	14920.978224	28.632602
311.026363	14945.334578	28.637620
311.183233	14954.336362	28.642637
311.205917	14987.759988	28.647655
311.694261	15015.504780	28.652672
312.372618	15026.370409	28.657690
312.871843	15046.078875	28.662708
313.473241	15070.028730	28.667725
313.995686	15088.536611	28.672743
314.056656	15097.266081	28.677760
314.832192	15113.368780	28.682778
314.913251	15128.225370	28.687796
315.183591	15140.743603	28.692813
315.548500	15160.277414	28.697831
315.617740	15181.623053	28.702848
315.987594	15187.837541	28.707866
315.945671	15210.059685	28.712884
316.409781	15231.634089	28.717901
316.914733	15248.057220	28.722919
316.956560	15265.920464	28.727936
317.298629	15278.617051	28.732954
317.900428	15306.938260	28.737972
318.087715	15316.857682	28.742989
318.212303	15339.840317	28.748007
318.299107	15360.147470	28.753024
318.805276	15373.503774	28.758042
319.475180	15385.675327	28.763060
319.672381	15405.137750	28.768077
319.748765	15428.491251	28.773095
320.047334	15440.304106	28.778112
320.515970	15463.779390	28.783130
320.585712	15491.198810	28.788148
321.216883	15498.528424	28.793165
321.463333	15518.327508	28.798183
321.714704	15540.933629	28.803200
322.132331	15553.883866	28.808218
322.148461	15572.335720	28.813236
321.981325	15583.653107	28.818253
322.739899	15608.662338	28.823271
322.926866	15627.807594	28.828288
323.362215	15648.411034	28.833306
323.477009	15680.700212	28.838324
324.097070	15695.261197	28.843341
324.865805	15715.616666	28.848359
324.466255	15741.982409	28.853376
325.059093	15761.471654	28.858394
325.285679	15777.490351	28.863412
325.458595	15799.657415	28.868429
325.799470	15816.918447	28.873447
326.314960	15846.403636	28.878464
326.566473	15860.378161	28.883482
327.011093	15884.536783	28.888500
327.205629	15908.491411	28.893517
328.093509	15936.910867	28.898535
328.286790	15961.232135	28.903552
328.569551	15985.394129	28.908570
328.558958	16005.840402	28.913588
329.126950	16019.307493	28.918605
329.349448	16048.655699	28.923623
329.307190	16079.905751	28.928640
329.509055	16097.567826	28.933658
330.128752	16126.402271	28.938676
330.633519	16153.988217	28.943693
331.354931	16166.562802	28.948711
331.255451	16186.410446	28.953728
332.033926	16201.493418	28.958746
332.405208	16229.785772	28.963764
332.446004	16249.074566	28.968781
332.737089	16270.535112	28.973799
332.923131	16294.336785	28.978816
333.538347	16311.789017	28.983834
333.401158	16343.376533	28.988852
333.876999	16372.233882	28.993869
334.462806	16398.127161	28.998887
334.690428	16429.032287	29.003904
335.064740	16447.845795	29.008922
335.122511	16477.779515	29.013940
335.555026	16513.327290	29.018957
335.663655	16533.951275	29.023975
335.688195	16561.742531	29.028992
335.775650	16594.056474	29.034010
336.386242	16628.707969	29.039028
336.737873	16651.511313	29.044045
337.534850	16690.953669	29.049063
337.468697	16726.254619	29.054080
338.509456	16747.670911	29.059098
338.833128	16778.160413	29.064116
339.018542	16797.228111	29.069133
338.906468	16817.599541	29.074151
338.783638	16856.267172	29.079168
339.359341	16885.248624	29.084186
339.722341	16913.625402	29.089204
340.208167	16949.772080	29.094221
341.047889	16989.944305	29.099239
341.306698	17020.453825	29.104256
341.721520	17033.099116	29.109274
342.169203	17064.286648	29.114292
342.336476	17090.053743	29.119309
342.757346	17116.551852	29.124327
343.150884	17139.181800	29.129344
343.571245	17165.199944	29.134362
343.724622	17185.744967	29.139380
343.985720	17210.398319	29.144397
344.392663	17232.381915	29.149415
344.645145	17269.766028	29.154432
344.871185	17282.207314	29.159450
345.325945	17311.688465	29.164468
345.652519	17345.188606	29.169485
345.963899	17366.410293	29.174503
345.912153	17397.979828	29.179520
346.730839	17423.455807	29.184538
347.105685	17458.186782	29.189556
346.827850	17485.887748	29.194573
347.644983	17510.189054	29.199591
347.615813	17546.562818	29.204608
347.837409	17574.545768	29.209626
348.387110	17601.555023	29.214644
348.270113	17648.701281	29.219661
349.234283	17674.615973	29.224679
349.638751	17708.218254	29.229696
350.117869	17735.535671	29.234714
350.608972	17751.107098	29.239732
351.301087	17786.622868	29.244749
351.554246	17811.524611	29.249767
352.015441	17836.532783	29.254784
352.436612	17855.608816	29.259802
352.604583	17881.503204	29.264820
352.757484	17906.660838	29.269837
353.331536	17931.095513	29.274855
352.934050	17960.294195	29.279872
353.732124	17989.747871	29.284890
354.048864	18023.004340	29.289908
353.759133	18062.041664	29.294925
354.628322	18068.273635	29.299943
355.512275	18097.303382	29.304960
356.104763	18134.844382	29.309978
356.550851	18148.919597	29.314996
356.956472	18170.601221	29.320013
357.427036	18192.550671	29.325031
357.695303	18211.695230	29.330048
357.796766	18228.882206	29.335066
357.989779	18263.238779	29.340084
358.289008	18286.718767	29.345101
358.394631	18303.734582	29.350119
358.556644	18339.625013	29.355136
359.193815	18368.011516	29.360154
359.686955	18397.140836	29.365172
359.725692	18431.926203	29.370189
360.468104	18464.049061	29.375207
360.456516	18493.775637	29.380224
360.991163	18514.300249	29.385242
361.608024	18536.151359	29.390260
361.430701	18569.492471	29.395277
361.877172	18597.195278	29.400295
362.110878	18632.512740	29.405312
362.607197	18669.235895	29.410330
363.151746	18697.416267	29.415348
363.466303	18743.221388	29.420365
363.593670	18766.931045	29.425383
363.939471	18796.993804	29.430400
364.512524	18841.507740	29.435418
364.745480	18866.325549	29.440436
364.750661	18901.325496	29.445453
365.406483	18924.402916	29.450471
365.709395	18955.767794	29.455488
366.089104	18982.565520	29.460506
366.481983	19021.839001	29.465524
366.875590	19061.371481	29.470541
367.348555	19092.078153	29.475559
367.670043	19125.108316	29.480576
367.751952	19157.184151	29.485594
368.396492	19176.043273	29.490612
368.530742	19216.229530	29.495629
368.906709	19248.164683	29.500647
369.042940	19276.883698	29.505664
369.413896	19314.126822	29.510682
370.263344	19347.118886	29.515700
370.363131	19377.536973	29.520717
370.926630	19406.460923	29.525735
371.378975	19438.542374	29.530752
371.418935	19471.320274	29.535770
372.222014	19499.069592	29.540788
372.074981	19533.355304	29.545805
372.904827	19564.190039	29.550823
373.373756	19596.780913	29.555840
373.926056	19625.176225	29.560858
374.628184	19650.060534	29.565876
374.711850	19685.491855	29.570893
375.083300	19703.970953	29.575911
375.804421	19729.048250	29.580928
375.929082	19755.615309	29.585946
376.424580	19777.114054	29.590964
376.693525	19806.539639	29.595981
376.876630	19825.370579	29.600999
377.117721	19862.256001	29.606016
377.124640	19893.782474	29.611034
377.977920	19922.396434	29.616052
378.082408	19959.290800	29.621069
378.426321	19996.615276	29.626087
378.624894	20034.051044	29.631104
378.719199	20076.943191	29.636122
379.359658	20102.109419	29.641140
380.051697	20142.494522	29.646157
380.633806	20170.285725	29.651175
381.263026	20194.139639	29.656192
381.591116	20228.168911	29.661210
382.096644	20251.511537	29.666228
383.168198	20290.106294	29.671245
383.432058	20298.841075	29.676263
383.431119	20318.421600	29.681280
383.565079	20341.841490	29.686298
384.750173	20370.397814	29.691316
384.821715	20400.278537	29.696333
385.015418	20415.513265	29.701351
385.522554	20439.089640	29.706368
385.129675	20461.518081	29.711386
386.178885	20492.294646	29.716404
386.552955	20519.518688	29.721421
387.112749	20533.217670	29.726439
388.030414	20553.248466	29.731456
388.152971	20570.314146	29.736474
388.706514	20583.660314	29.741492
388.794049	20609.008579	29.746509
388.947114	20623.605360	29.751527
389.075371	20652.649874	29.756544
389.179233	20680.301886	29.761562
389.796474	20711.013772	29.766580
389.962018	20736.255205	29.771597
390.581492	20763.794978	29.776615
390.758000	20796.060862	29.781632
391.002874	20838.501431	29.786650
391.626595	20870.204546	29.791668
391.542479	20895.725392	29.796685
391.773282	20928.779116	29.801703
392.753865	20946.974418	29.806720
393.219663	20976.920630	29.811738
394.075561	21006.237118	29.816756
394.283880	21029.147017	29.821773
394.436780	21058.883306	29.826791
394.853828	21074.816509	29.831808
394.691095	21099.724398	29.836826
395.058489	21130.684586	29.841844
395.275967	21174.096905	29.846861
395.553625	21211.029676	29.851879
395.958787	21243.879697	29.856896
396.168195	21286.920732	29.861914
396.867049	21315.087020	29.866932
397.634273	21353.643078	29.871949
397.584920	21385.338717	29.876967
398.439171	21423.135682	29.881984
398.701323	21447.124439	29.887002
399.119152	21483.176427	29.892020
399.351815	21524.754727	29.897037
399.546788	21556.140666	29.902055
400.065699	21591.633613	29.907072
400.393107	21645.108062	29.912090
401.032017	21678.882636	29.917108
401.018471	21717.030929	29.922125
401.551234	21758.499526	29.927143
401.788312	21800.690633	29.932160
402.111242	21842.324967	29.937178
402.683222	21883.433832	29.942196
403.123527	21913.157981	29.947213
403.799453	21959.779668	29.952231
404.306923	21991.799780	29.957248
404.767764	22027.214140	29.962266
405.429987	22055.785310	29.967284
405.958553	22088.301462	29.972301
406.256505	22130.148836	29.977319
406.576722	22163.715084	29.982336
407.012326	22197.711956	29.987354
407.502338	22226.057591	29.992372
407.860117	22264.287788	29.997389
408.311346	22300.500325	30.002407
408.589880	22327.571214	30.007424
408.656941	22371.155053	30.012442
409.134018	22403.932546	30.017460
409.441900	22454.669812	30.022477
409.574359	22495.716094	30.027495
410.077177	22541.146700	30.032512
410.242307	22591.704469	30.037530
410.472578	22631.016937	30.042548
411.187270	22681.665786	30.047565
411.527837	22727.311803	30.052583
412.290421	22771.836537	30.057600
412.034091	22823.478280	30.062618
412.773320	22873.750948	30.067636
413.196884	22917.488671	30.072653
413.733448	22961.720640	30.077671
414.681240	22993.395356	30.082688
415.285536	23032.365671	30.087706
415.582931	23068.066573	30.092724
416.480300	23098.081097	30.097741
417.117681	23131.807833	30.102759
417.639628	23162.614283	30.107776
417.928462	23198.714870	30.112794
418.178281	23216.325305	30.117812
418.485451	23250.931781	30.122829
418.913284	23281.007489	30.127847
419.692385	23317.442248	30.132864
419.756769	23352.661980	30.137882
420.013602	23378.770854	30.142900
420.457822	23404.180568	30.147917
420.402665	23447.476259	30.152935
420.893194	23472.284793	30.157952
421.402660	23506.841069	30.162970
422.131303	23540.181363	30.167988
422.017518	23564.528570	30.173005
422.075810	23609.361393	30.178023
422.824138	23645.163319	30.183040
423.355892	23685.346949	30.188058
423.191987	23727.137313	30.193076
423.767786	23763.528899	30.198093
424.833983	23782.427502	30.203111
425.051601	23814.053592	30.208128
425.588430	23860.827911	30.213146
425.777534	23903.795636	30.218164
426.596638	23936.212426	30.223181
426.804941	23980.036751	30.228199
427.316031	24015.238236	30.233216
427.653860	24053.765685	30.238234
428.044366	24096.120885	30.243252
428.668959	24136.625812	30.248269
428.666308	24173.791256	30.253287
429.167976	24210.258462	30.258304
429.584941	24251.611361	30.263322
429.560853	24300.762238	30.268340
430.117187	24341.587929	30.273357
430.345453	24389.252315	30.278375
431.066055	24441.320290	30.283392
431.197777	24488.165846	30.288410
431.711267	24534.035369	30.293428
432.497502	24578.402439	30.298445
432.627977	24624.313202	30.303463
433.284565	24664.352849	30.308480
433.206125	24719.889805	30.313498
434.081043	24764.944882	30.318516
434.943117	24815.746688	30.323533
435.140552	24859.018499	30.328551
435.704370	24899.496568	30.333568
435.847463	24952.136624	30.338586
436.118428	25009.660931	30.343604
436.889087	25047.465235	30.348621
437.218573	25085.553586	30.353639
438.642154	25121.321902	30.358656
439.314807	25168.318148	30.363674
439.977038	25192.185546	30.368692
440.379120	25218.520538	30.373709
440.518939	25249.187819	30.378727
441.209032	25280.837012	30.383744
441.575687	25311.746932	30.388762
441.928937	25350.590446	30.393780
442.559856	25381.541240	30.398797
442.793182	25407.321482	30.403815
443.414180	25425.084276	30.408832
443.951327	25464.467996	30.413850
443.890349	25503.736922	30.418868
444.792607	25521.240869	30.423885
444.852926	25561.179781	30.428903
445.078146	25591.808926	30.433920
446.006751	25619.913720	30.438938
445.808853	25660.152390	30.443956
446.578422	25704.505596	30.448973
446.981375	25744.359602	30.453991
447.162538	25770.862639	30.459008
448.004858	25821.391999	30.464026
447.925042	25863.584426	30.469044
448.668485	25890.701073	30.474061
448.617756	25930.493786	30.479079
449.060919	25967.807590	30.484096
449.498788	26020.644423	30.489114
449.466177	26070.110630	30.494132
450.318991	26105.894260	30.499149
450.322391	26165.928615	30.504167
450.934843	26194.184852	30.509184
451.430334	26247.632626	30.514202
451.649872	26293.716519	30.519220
452.359744	26340.166129	30.524237
452.492617	26390.321377	30.529255
452.987691	26430.453034	30.534272
453.528413	26490.416828	30.539290
453.664416	26530.238351	30.544308
454.133817	26574.741606	30.549325
454.464592	26635.200090	30.554343
454.880932	26679.421153	30.559360
455.730741	26734.780325	30.564378
455.976887	26783.654740	30.569396
456.857867	26831.816765	30.574413
457.210664	26880.636787	30.579431
457.886879	26930.512334	30.584448
458.870429	26969.209666	30.589466
459.775510	27009.101278	30.594484
460.255303	27030.920017	30.599501
460.694272	27055.652562	30.604519
461.151526	27104.747500	30.609536
461.876257	27136.571147	30.614554
461.925349	27173.019789	30.619572
462.827006	27204.341796	30.624589
463.197854	27232.314981	30.629607
463.764979	27262.918380	30.634624
464.364400	27301.019183	30.639642
464.757167	27341.370921	30.644660
465.325618	27365.470475	30.649677
465.199223	27403.192154	30.654695
465.492302	27433.529028	30.659712
466.029195	27478.699989	30.664730
465.875403	27518.436104	30.669748
466.640120	27557.642876	30.674765
466.597987	27617.783455	30.679783
467.478657	27658.514482	30.684800
467.749367	27705.276182	30.689818
467.689335	27767.745990	30.694836
468.524943	27815.367558	30.699853
468.816563	27861.077112	30.704871
469.626578	27907.116417	30.709888
470.034946	27963.919663	30.714906
470.490407	28021.796532	30.719924
470.915884	28055.969227	30.724941
471.914107	28098.926578	30.729959
472.280808	28146.818307	30.734976
472.976804	28185.348088	30.739994
472.954282	28246.599896	30.745012
473.672336	28283.072154	30.750029
474.226089	28336.623740	30.755047
474.792275	28382.474758	30.760064
475.456360	28421.768482	30.765082
475.617969	28469.629880	30.770100
476.378668	28515.665639	30.775117
476.632416	28554.758413	30.780135
476.665671	28599.290154	30.785152
477.072036	28645.969547	30.790170
478.014809	28691.755953	30.795188
478.526872	28724.866931	30.800205
479.002674	28780.726383	30.805223
479.522047	28825.827212	30.810240
479.995148	28868.640876	30.815258
480.746470	28908.149424	30.820276
481.292174	28950.376678	30.825293
481.538267	28996.209673	30.830311
482.129854	29032.930632	30.835328
482.576314	29062.095471	30.840346
482.818274	29105.900308	30.845364
483.927421	29133.545541	30.850381
484.163945	29166.769921	30.855399
484.518840	29209.141372	30.860416
485.097471	29236.174518	30.865434
485.797340	29265.767716	30.870452
486.738213	29302.997028	30.875469
487.574367	29333.390722	30.880487
487.653568	29361.994042	30.885504
488.545986	29383.719063	30.890522
488.431390	29418.844615	30.895540
488.427878	29451.089347	30.900557
488.848627	29486.219661	30.905575
488.991084	29529.927204	30.910592
489.716272	29572.424719	30.915610
489.777022	29624.198452	30.920628
489.829210	29665.632147	30.925645
490.363158	29726.276542	30.930663
490.685169	29770.070253	30.935680
491.123889	29831.064897	30.940698
491.466596	29890.545008	30.945716
491.938128	29950.719420	30.950733
492.361372	30015.636241	30.955751
493.065555	30074.421811	30.960768
493.682253	30134.807912	30.965786
494.076789	30208.225741	30.970804
494.273682	30261.515841	30.975821
495.195378	30323.024180	30.980839
495.507135	30385.197163	30.985856
496.138028	30438.666279	30.990874
496.214445	30510.611536	30.995892
496.374089	30583.043404	31.000909
497.568496	30633.023797	31.005927
498.234085	30705.092380	31.010944
498.948932	30755.040714	31.015962
499.410775	30812.747424	31.020980
499.955262	30869.967232	31.025997
500.404386	30920.071372	31.031015
500.586543	30986.109986	31.036032
501.568512	31037.003333	31.041050
501.988248	31103.403372	31.046068
502.963926	31153.160093	31.051085
503.290035	31193.523505	31.056103
503.968267	31251.937181	31.061120
504.704479	31306.409833	31.066138
505.408308	31348.402284	31.071156
505.500243	31400.908888	31.076173
506.229721	31454.700235	31.081191
506.377271	31502.842694	31.086208
507.232458	31552.429590	31.091226
507.646854	31615.374081	31.096244
507.820964	31659.327704	31.101261
508.134635	31713.854959	31.106279
508.585298	31781.093120	31.111296
509.316990	31823.613202	31.116314
509.618761	31887.353743	31.121332
509.918926	31948.300446	31.126349
510.413201	32006.435277	31.131367
511.134320	32065.394524	31.136384
511.669971	32120.185204	31.141402
512.263204	32188.571910	31.146420
512.371775	32237.860125	31.151437
512.980221	32292.134094	31.156455
513.424754	32355.347941	31.161472
514.136968	32430.424479	31.166490
514.274210	32479.885790	31.171508
514.910693	32551.061262	31.176525
515.312726	32600.139991	31.181543
515.532475	32670.002918	31.186560
516.620442	32715.933542	31.191578
517.459356	32756.529444	31.196596
518.303427	32808.276920	31.201613
519.107604	32854.410352	31.206631
519.476311	32899.341329	31.211648
520.433724	32939.027596	31.216666
521.323542	32987.727369	31.221684
521.389259	33033.888345	31.226701
521.937140	33069.858306	31.231719
522.357821	33113.864876	31.236736
523.495437	33142.984101	31.241754
523.719390	33181.710920	31.246772
524.309079	33218.205659	31.251789
525.127210	33244.637512	31.256807
525.363856	33283.305630	31.261824
525.717654	33327.177709	31.266842
526.230409	33362.603632	31.271860
526.645380	33413.755965	31.276877
527.283481	33460.751293	31.281895
527.825772	33502.356099	31.286912
528.160829	33549.380121	31.291930
528.361540	33594.256705	31.296948
528.952907	33650.174369	31.301965
529.453777	33686.209650	31.306983
529.661647	33742.952639	31.312000
530.021562	33788.342109	31.317018
530.790018	33857.086157	31.322036
530.744248	33920.198155	31.327053
531.464980	33972.796067	31.332071
532.017963	34047.125653	31.337088
532.106087	34102.137018	31.342106
532.984517	34159.560099	31.347124
532.929491	34231.741048	31.352141
533.787303	34275.036676	31.357159
534.472497	34356.238287	31.362176
535.445939	34406.945170	31.367194
535.617583	34479.066171	31.372212
536.164211	34539.520230	31.377229
536.667878	34598.760908	31.382247
537.417592	34671.563396	31.387264
538.057856	34731.908498	31.392282
538.458499	34788.592485	31.397300
538.883580	34854.782258	31.402317
539.276103	34916.121426	31.407335
539.951894	34978.826394	31.412352
540.905949	35043.896966	31.417370
541.341403	35096.219888	31.422388
541.429372	35165.289744	31.427405
542.468817	35226.579070	31.432423
543.015580	35283.797909	31.437440
543.950758	35338.578649	31.442458
544.737709	35386.762627	31.447476
545.137811	35447.134731	31.452493
546.009588	35484.076075	31.457511
546.444928	35539.656437	31.462528
547.298432	35593.837297	31.467546
548.007121	35638.885250	31.472564
548.256043	35690.410536	31.477581
549.064157	35732.793767	31.482599
549.377217	35784.827725	31.487616
549.843809	35833.296843	31.492634
550.261313	35876.917630	31.497652
550.590188	35935.101840	31.502669
551.345739	35978.745768	31.507687
551.361301	36035.954980	31.512704
551.751964	36091.196005	31.517722
552.576705	36139.420032	31.522740
552.464766	36202.220365	31.527757
552.783129	36253.533792	31.532775
553.304315	36318.182850	31.537792
554.152483	36377.519962	31.542810
554.883967	36442.711874	31.547828
555.224673	36508.161210	31.552845
555.965358	36555.387618	31.557863
556.656839	36616.887205	31.562880
556.963111	36678.662293	31.567898
557.608689	36728.945498	31.572916
557.970036	36801.632720	31.577933
558.980829	36867.180553	31.582951
559.026779	36932.304270	31.587968
559.293457	36992.138856	31.592986
560.118314	37057.368604	31.598004
560.522309	37122.904756	31.603021
561.045441	37193.582404	31.608039
561.787298	37263.840294	31.613056
562.419041	37332.383016	31.618074
563.167702	37393.768377	31.623092
563.207486	37469.081899	31.628109
564.361092	37536.696184	31.633127
564.401611	37597.231851	31.638144
564.761267	37681.488167	31.643162
565.607702	37741.392128	31.648180
566.056690	37817.856918	31.653197
566.617616	37892.401020	31.658215
567.321189	37969.294426	31.663232
567.832935	38041.747278	31.668250
568.679465	38107.071672	31.673268
569.063059	38179.962426	31.678285
570.121953	38242.591667	31.683303
570.644750	38322.581679	31.688320
571.214948	38394.925381	31.693338
572.182513	38447.470373	31.698356
572.733147	38517.306984	31.703373
572.976631	38584.074252	31.708391
573.486359	38652.867943	31.713408
574.155096	38716.628403	31.718426
575.302886	38766.388716	31.723444
575.866440	38841.745146	31.728461
576.282371	38906.665101	31.733479
576.846679	38967.641135	31.738496
577.368353	39029.737045	31.743514
578.238272	39088.730409	31.748532
578.509110	39151.466735	31.753549
579.263338	39215.588394	31.758567
579.623556	39280.322146	31.763584
579.948067	39344.770774	31.768602
580.846215	39408.725009	31.773620
581.400273	39473.055854	31.778637
582.620355	39520.865069	31.783655
583.483592	39579.962003	31.788672
584.070195	39637.179869	31.793690
584.694857	39688.700143	31.798708
584.813402	39746.048519	31.803725
585.871605	39800.796077	31.808743
585.996217	39852.451972	31.813760
586.239688	39917.566387	31.818778
586.554973	39976.446651	31.823796
587.213857	40037.682820	31.828813
588.281766	40095.800455	31.833831
588.559341	40158.835872	31.838848
588.656862	40226.895912	31.843866
589.497009	40288.003205	31.848884
590.072295	40358.879072	31.853901
589.974122	40425.028787	31.858919
590.869870	40494.741808	31.863936
591.052260	40564.813427	31.868954
591.863456	40625.451864	31.873972
592.661198	40687.673701	31.878989
593.988509	40743.159392	31.884007
594.363351	40796.738926	31.889024
595.710770	40857.116940	31.894042
596.082053	40912.670572	31.899060
596.646645	40959.889908	31.904077
596.891746	41017.911177	31.909095
597.347072	41086.151860	31.914112
597.745049	41144.143196	31.919130
598.707193	41208.238151	31.924148
598.799592	41274.961425	31.929165
598.995815	41335.419857	31.934183
599.643630	41393.979894	31.939200
600.232216	41474.388603	31.944218
600.772062	41542.788234	31.949236
600.974182	41626.667060	31.954253
601.550403	41700.899242	31.959271
602.700031	41784.250787	31.964288
602.985722	41864.164425	31.969306
603.676134	41929.878925	31.974324
604.458988	42017.254475	31.979341
604.941980	42094.184330	31.984359
605.501917	42159.357032	31.989376
605.847764	42248.218719	31.994394
606.490072	42319.128364	31.999412
607.977557	42391.550366	32.004429
608.871890	42460.833426	32.009447
609.536815	42527.755449	32.014464
609.836553	42594.627342	32.019482
610.579908	42657.995455	32.024500
611.187447	42730.202176	32.029517
611.809334	42805.063428	32.034535
612.380940	42874.853735	32.039552
612.997947	42951.322825	32.044570
613.910696	43015.171443	32.049588
614.112619	43091.320188	32.054605
615.247484	43152.395612	32.059623
615.600688	43212.840922	32.064640
615.893576	43304.169323	32.069658
616.817730	43359.408494	32.074676
617.101642	43431.332944	32.079693
617.950657	43507.603158	32.084711
618.548478	43574.387043	32.089728
618.924613	43664.135205	32.094746
619.525475	43726.991034	32.099764
619.668171	43808.667227	32.104781
620.171254	43881.570867	32.109799
621.229472	43962.459049	32.114816
622.285198	44047.484762	32.119834
622.967400	44106.147798	32.124852
623.492822	44186.354854	32.129869
624.610250	44263.951929	32.134887
625.167902	44326.949053	32.139904
625.638097	44399.524284	32.144922
626.175647	44451.195847	32.149940
627.094289	44524.004877	32.154957
627.570133	44599.464340	32.159975
628.547453	44665.300147	32.164992
628.694218	44733.271453	32.170010
629.702476	44796.079142	32.175028
630.098761	44859.318110	32.180045
630.967108	44930.542269	32.185063
631.884445	44993.124374	32.190080
632.080370	45063.277680	32.195098
632.832632	45128.340402	32.200116
633.299764	45188.615075	32.205133
633.500279	45247.014951	32.210151
634.451782	45302.273630	32.215168
634.876519	45373.480109	32.220186
635.627350	45425.107865	32.225204
636.551983	45499.342442	32.230221
636.895334	45568.841651	32.235239
637.737501	45627.211609	32.240256
637.809703	45696.589204	32.245274
638.885168	45770.674537	32.250292
638.988674	45830.697908	32.255309
639.177427	45913.924415	32.260327
639.974195	45976.787509	32.265344
640.264889	46070.873019	32.270362
641.199603	46145.607904	32.275380
641.656378	46230.077788	32.280397
641.858897	46313.265654	32.285415
642.680458	46397.002142	32.290432
643.325808	46485.713575	32.295450
644.090281	46574.552202	32.300468
644.650746	46662.107281	32.305485
645.333218	46755.185353	32.310503
645.998594	46836.506009	32.315520
646.677389	46930.078821	32.320538
647.601324	47020.425180	32.325556
648.175782	47106.644938	32.330573
648.484757	47192.545999	32.335591
649.296780	47280.816904	32.340608
649.902516	47373.213629	32.345626
650.822825	47448.081598	32.350644
651.676098	47534.619920	32.355661
652.148018	47626.222521	32.360679
653.069940	47711.630982	32.365696
653.449170	47807.797568	32.370714
654.107325	47883.435574	32.375732
654.848708	47976.452483	32.380749
655.221530	48071.697507	32.385767
655.899049	48159.303285	32.390784
656.643628	48245.083155	32.395802
656.774731	48335.843598	32.400820
657.447189	48439.166650	32.405837
658.402809	48533.259444	32.410855
659.031132	48641.107589	32.415872
659.375287	48734.860426	32.420890
660.289697	48834.509483	32.425908
661.112527	48924.898204	32.430925
661.307722	49032.664177	32.435943
662.179917	49120.546834	32.440960
662.575522	49222.664055	32.445978
663.693391	49322.194790	32.450996
664.783270	49401.262662	32.456013
665.465720	49498.837730	32.461031
666.574583	49581.193274	32.466048
667.203470	49674.228365	32.471066
667.876064	49749.009793	32.476084
668.618114	49837.801359	32.481101
669.123759	49918.746737	32.486119
669.891515	50004.675077	32.491136
670.430825	50095.188723	32.496154
671.463956	50177.007797	32.501172
672.207133	50256.702347	32.506189
672.663196	50345.338183	32.511207
673.357152	50420.820762	32.516224
674.496295	50498.555968	32.521242
674.608814	50593.871185	32.526260
675.453623	50671.362011	32.531277
676.136004	50753.263364	32.536295
677.338109	50819.803098	32.541312
677.695512	50904.318448	32.546330
678.052647	50973.907864	32.551348
679.433387	51035.877189	32.556365
679.699802	51122.818320	32.561383
680.063688	51188.794368	32.566400
680.707310	51268.349803	32.571418
681.242751	51344.758714	32.576436
681.941587	51428.159482	32.581453
682.225985	51515.656084	32.586471
683.156794	51601.640741	32.591488
683.975711	51689.756646	32.596506
684.350615	51769.798808	32.601524
685.345007	51850.212472	32.606541
685.562757	51948.155371	32.611559
686.343130	52039.493075	32.616576
687.038118	52138.361805	32.621594
687.372084	52216.095971	32.626612
688.402356	52311.559239	32.631629
689.486684	52391.283615	32.636647
690.409591	52467.800046	32.641664
691.032110	52556.127155	32.646682
691.975082	52639.785099	32.651700
692.812103	52708.526213	32.656717
692.918424	52805.098021	32.661735
693.576393	52881.828148	32.666752
693.964448	52978.571696	32.671770
695.049692	53074.143366	32.676788
695.871141	53150.000823	32.681805
696.363999	53252.379958	32.686823
697.029554	53330.717673	32.691840
697.704673	53426.449922	32.696858
698.370626	53529.347366	32.701876
699.258519	53618.415262	32.706893
699.389743	53720.612597	32.711911
700.228259	53810.062309	32.716928
700.917701	53900.371022	32.721946
701.475041	54008.717132	32.726964
702.092814	54111.339888	32.731981
702.645542	54212.163397	32.736999
703.052901	54318.028424	32.742016
704.020529	54416.946302	32.747034
704.810758	54520.524712	32.752052
705.789982	54624.624546	32.757069
706.169082	54733.318300	32.762087
707.001359	54831.442742	32.767104
707.834042	54932.630491	32.772122
708.499060	55040.913828	32.777140
709.333044	55138.653235	32.782157
710.401098	55250.317110	32.787175
710.986183	55343.622070	32.792192
711.495426	55443.824763	32.797210
711.965282	55552.343502	32.802228
713.045780	55640.439543	32.807245
713.728944	55746.413295	32.812263
714.682136	55846.389938	32.817280
715.452267	55939.991014	32.822298
715.552234	56044.152475	32.827316
716.845499	56147.152886	32.832333
717.746410	56252.474563	32.837351
718.729278	56331.810412	32.842368
719.631054	56421.671416	32.847386
720.328940	56511.140653	32.852404
721.060735	56592.092569	32.857421
721.939443	56683.856833	32.862439
722.102760	56779.056165	32.867456
723.012789	56864.904997	32.872474
723.624672	56969.148529	32.877492
724.715541	57056.406403	32.882509
725.388759	57147.559059	32.887527
725.388155	57230.735385	32.892544
726.427792	57313.919980	32.897562
726.581438	57416.439752	32.902580
727.344294	57498.054407	32.907597
728.371968	57597.450731	32.912615
729.106917	57688.918553	32.917632
729.632406	57773.065002	32.922650
730.484857	57878.755823	32.927668
731.354860	57966.108541	32.932685
731.915194	58072.959902	32.937703
732.090782	58153.953530	32.942720
732.965801	58256.642384	32.947738
733.246481	58374.956959	32.952756
734.123236	58474.614706	32.957773
734.624484	58585.787882	32.962791
735.246028	58691.847536	32.967808
736.048402	58801.923859	32.972826
736.385262	58926.485824	32.977844
737.222771	59041.501060	32.982861
737.932194	59163.037347	32.987879
738.332325	59285.679714	32.992896
739.817692	59404.000523	32.997914
740.146137	59529.940412	33.002932
741.029077	59636.634185	33.007949
741.783111	59760.938858	33.012967
742.981862	59883.174323	33.017984
744.216202	59979.370497	33.023002
744.843583	60099.177271	33.028020
745.759726	60203.538951	33.033037
746.631271	60311.592031	33.038055
747.583976	60410.315301	33.043072
748.214645	60522.711345	33.048090
748.848670	60629.258521	33.053108
749.434721	60741.086526	33.058125
750.246094	60844.897641	33.063143
751.011276	60961.167564	33.068160
751.644233	61071.590790	33.073178
752.206242	61186.830146	33.078196
753.090291	61308.615577	33.083213
753.683832	61423.971373	33.088231
754.402319	61543.416417	33.093248
755.204926	61653.201649	33.098266
755.713172	61773.282094	33.103284
756.356031	61889.290677	33.108301
757.235358	62012.397003	33.113319
757.983734	62144.291934	33.118336
759.153846	62251.825647	33.123354
759.740294	62373.245111	33.128372
760.375626	62493.594003	33.133389
760.619631	62610.579991	33.138407
761.980375	62741.717500	33.143424
763.588989	62851.590717	33.148442
764.336958	62958.566870	33.153460
765.146472	63059.785705	33.158477
766.375004	63173.486538	33.163495
766.979795	63275.459991	33.168512
767.828972	63374.306242	33.173530
768.608591	63483.773956	33.178548
769.600690	63578.293786	33.183565
770.320635	63674.755802	33.188583
770.991059	63777.860550	33.193600
772.290648	63881.899112	33.198618
772.755465	63978.484547	33.203636
773.960366	64064.337701	33.208653
775.223550	64153.550021	33.213671
776.086613	64238.026532	33.218688
777.068047	64308.829111	33.223706
777.439116	64390.933134	33.228724
778.240442	64467.816692	33.233741
779.011882	64560.209603	33.238759
779.521806	64631.086924	33.243776
779.854719	64707.424131	33.248794
780.591984	64791.675291	33.253812
781.508912	64875.493414	33.258829
782.332453	64962.137416	33.263847
782.500544	65063.825639	33.268864
783.274147	65145.913400	33.273882
784.130686	65255.117201	33.278900
784.772235	65353.326312	33.283917
785.431999	65445.195471	33.288935
785.876482	65553.724338	33.293952
786.197019	65656.125480	33.298970
786.839509	65771.379665	33.303988
787.516833	65881.443616	33.309005
788.163830	66001.877110	33.314023
788.624987	66126.499951	33.319040
789.451930	66249.818845	33.324058
790.174259	66378.207161	33.329076
791.007701	66512.182024	33.334093
791.558481	66641.111369	33.339111
792.416244	66764.282300	33.344128
793.191828	66892.354617	33.349146
794.028015	67036.772459	33.354164
794.884754	67162.015880	33.359181
795.515152	67291.632506	33.364199
796.075720	67426.376686	33.369216
797.066380	67562.333222	33.374234
798.226475	67698.574199	33.379252
798.538037	67844.338745	33.384269
799.421726	67963.009500	33.389287
800.620003	68102.868412	33.394304
801.831569	68237.229964	33.399322
802.418724	68363.116638	33.404340
803.377427	68497.291192	33.409357
803.944554	68632.293924	33.414375
804.922898	68762.021757	33.419392
806.571933	68884.661020	33.424410
807.322248	69005.795269	33.429428
808.339053	69129.136234	33.434445
809.539057	69241.158988	33.439463
810.184120	69360.038153	33.444480
811.533983	69478.864485	33.449498
811.817959	69592.159314	33.454516
812.580954	69700.016255	33.459533
813.674047	69813.128356	33.464551
813.924047	69942.798832	33.469568
814.821591	70060.565174	33.474586
815.548636	70184.463094	33.479604
816.144086	70315.347787	33.484621
817.215751	70425.363046	33.489639
817.589006	70551.420451	33.494656
818.382777	70673.005240	33.499674
819.643101	70799.938123	33.504692
819.986841	70933.448961	33.509709
820.668093	71056.978226	33.514727
821.284127	71187.142136	33.519744
821.794388	71323.364540	33.524762
822.877513	71468.566260	33.529780
823.767759	71609.188807	33.534797
824.772252	71734.557764	33.539815
825.503913	71880.260072	33.544832
826.325930	72007.330736	33.549850
826.994757	72145.014412	33.554868
828.530168	72273.899813	33.559885
829.737050	72378.025204	33.564903
830.687805	72489.701891	33.569920
831.394798	72606.116226	33.574938
832.147511	72718.800153	33.579956
832.860352	72834.277299	33.584973
833.999811	72944.761087	33.589991
834.364265	73071.300528	33.595008
835.414916	73180.139952	33.600026
836.273989	73301.979924	33.605044
836.572141	73417.537199	33.610061
837.090249	73536.011762	33.615079
837.559260	73676.584552	33.620096
838.406188	73807.687796	33.625114
839.738725	73939.665624	33.630132
840.128810	74074.730302	33.635149
841.184175	74210.755476	33.640167
841.864988	74353.388629	33.645184
842.703673	74482.533136	33.650202
843.632472	74621.493543	33.655220
844.231109	74759.100351	33.660237
845.310805	74892.515800	33.665255
846.019191	75041.950392	33.670272
847.090906	75165.982241	33.675290
848.330444	75304.365495	33.680308
849.009883	75442.064466	33.685325
850.500536	75573.987546	33.690343
851.238577	75703.711010	33.695360
851.831450	75843.008979	33.700378
852.556145	75960.739816	33.705396
853.450248	76110.290561	33.710413
854.041261	76236.986740	33.715431
855.145986	76376.789999	33.720448
856.069291	76511.821353	33.725466
856.880035	76651.406034	33.730484
857.739943	76798.875743	33.735501
858.715543	76929.099892	33.740519
859.300226	77074.942034	33.745536
860.757339	77211.768108	33.750554
861.601556	77358.837917	33.755572
862.584240	77488.265530	33.760589
863.242854	77613.551345	33.765607
864.373910	77751.976683	33.770624
865.751311	77881.040304	33.775642
866.564217	77995.320321	33.780660
867.098862	78121.755341	33.785677
867.874497	78255.551568	33.790695
868.970401	78385.649769	33.795712
870.114995	78514.702137	33.800730
871.039727	78641.015111	33.805748
871.901973	78769.327425	33.810765
872.853500	78891.950767	33.815783
873.528265	79030.162581	33.820800
874.258013	79156.457760	33.825818
875.013919	79276.022232	33.830836
875.889278	79408.680882	33.835853
876.974047	79546.096263	33.840871
877.749577	79680.190768	33.845888
878.120844	79820.823151	33.850906
878.848450	79950.580943	33.855924
879.637579	80099.206911	33.860941
880.812757	80239.474806	33.865959
881.448397	80390.634884	33.870976
882.521930	80532.098415	33.875994
883.117078	80663.628640	33.881012
883.373411	80814.837726	33.886029
884.317038	80947.366290	33.891047
885.543548	81096.841273	33.896064
886.236418	81245.817799	33.901082
887.262001	81386.051496	33.906100
887.783475	81525.199193	33.911117
889.240962	81666.468938	33.916135
889.470145	81817.383570	33.921152
890.183202	81948.381854	33.926170
891.550987	82094.064307	33.931188
892.087845	82236.874771	33.936205
892.820512	82382.860878	33.941223
893.714493	82542.531809	33.946240
894.601346	82685.505121	33.951258
895.694321	82842.865902	33.956276
896.617092	82997.884805	33.961293
897.130386	83146.139194	33.966311
898.038888	83302.188304	33.971328
899.122261	83453.852140	33.976346
900.338096	83602.949200	33.981364
901.395334	83754.010517	33.986381
902.653484	83892.053430	33.991399
903.219494	84042.432923	33.996416
903.755920	84203.385532	34.001434
904.784326	84356.671974	34.006452
905.210787	84515.641500	34.011469
906.368270	84675.295731	34.016487
907.314766	84841.040800	34.021504
907.976197	85004.474563	34.026522
909.336804	85159.626641	34.031540
910.775035	85313.094746	34.036557
911.952825	85457.582227	34.041575
913.104960	85602.644671	34.046592
914.358842	85748.097405	34.051610
915.187973	85879.412244	34.056628
916.203182	86040.730936	34.061645
917.843210	86173.516792	34.066663
918.292102	86314.359083	34.071680
919.462944	86458.219016	34.076698
920.260296	86598.513904	34.081716
920.981735	86732.789380	34.086733
921.618307	86876.367528	34.091751
922.787900	87025.350037	34.096768
923.284225	87178.455870	34.101786
924.351159	87312.984040	34.106804
924.961787	87471.484637	34.111821
925.683578	87620.578293	34.116839
926.456148	87773.504565	34.121856
927.177417	87933.979928	34.126874
928.258912	88088.468893	34.131892
928.674067	88258.561900	34.136909
929.550024	88426.264585	34.141927
930.894741	88590.726570	34.146944
931.630457	88765.790798	34.151962
932.933029	88925.965064	34.156980
933.501754	89099.942166	34.161997
934.540183	89270.095443	34.167015
935.452587	89423.464551	34.172032
936.491373	89595.938851	34.177050
937.397399	89747.460297	34.182068
939.093233	89902.800320	34.187085
940.194467	90047.208199	34.192103
941.510059	90194.802324	34.197120
942.249733	90353.868371	34.202138
943.678022	90487.315062	34.207156
944.624821	90644.259034	34.212173
945.586129	90789.402120	34.217191
947.013226	90923.991584	34.222208
947.229249	91076.033323	34.227226
948.728458	91211.398567	34.232244
949.578357	91352.696197	34.237261
950.006715	91505.099739	34.242279
950.756131	91646.046915	34.247296
951.909780	91792.888394	34.252314
953.028325	91920.901913	34.257332
953.383242	92073.509915	34.262349
954.137951	92218.096481	34.267367
955.068310	92351.249104	34.272384
955.773379	92509.951634	34.277402
956.517781	92651.512622	34.282420
957.303039	92808.594455	34.287437
957.922468	92973.827627	34.292455
959.165507	93126.111694	34.297472
960.145678	93289.616994	34.302490
960.717876	93456.406498	34.307508
961.244578	93630.302086	34.312525
962.575404	93804.098099	34.317543
963.614014	93964.771261	34.322560
964.118546	94146.886784	34.327578
964.990948	94320.770151	34.332596
966.366280	94489.936528	34.337613
966.996480	94672.415720	34.342631
967.775177	94842.716826	34.347648
968.350995	95043.624362	34.352666
969.593642	95223.944753	34.357684
970.716990	95414.425528	34.362701
971.624762	95602.824340	34.367719
972.693287	95788.106173	34.372736
973.716776	95974.410236	34.377754
974.774538	96157.579031	34.382772
975.993102	96351.308350	34.387789
977.298092	96528.812358	34.392807
978.792583	96697.781862	34.397824
980.041047	96869.199310	34.402842
981.216311	97033.428903	34.407860
983.077600	97185.686687	34.412877
983.862463	97350.257931	34.417895
985.218605	97513.777155	34.422912
986.117356	97685.088969	34.427930
986.793697	97844.710478	34.432948
988.146324	98007.991930	34.437965
988.985625	98169.579817	34.442983
989.567475	98312.104596	34.448000
990.415390	98481.007332	34.453018
991.870409	98641.791283	34.458036
992.888902	98813.787636	34.463053
993.672046	98971.128819	34.468071
994.541592	99123.056706	34.473088
995.182086	99301.085860	34.478106
995.989468	99469.353584	34.483124
997.306142	99651.322905	34.488141
997.612410	99823.119213	34.493159
998.699378	99992.486864	34.498176
999.467816	100184.458941	34.503194
1000.540283	100354.883003	34.508212
1002.036947	100537.539068	34.513229
1003.334675	100708.436827	34.518247
1004.381586	100883.976864	34.523264
1005.481722	101050.330591	34.528282
1006.224707	101221.837690	34.533300
1007.546273	101384.709995	34.538317
1008.556133	101561.248362	34.543335
1009.680187	101724.571660	34.548352
1011.016032	101898.956199	34.553370
1012.032524	102068.725989	34.558388
1012.883098	102228.658742	34.563405
1013.569181	102402.577140	34.568423
1014.973296	102560.117327	34.573440
1015.805944	102730.971628	34.578458
1016.907545	102897.549988	34.583476
1017.927952	103055.254033	34.588493
1019.125883	103205.640667	34.593511
1020.945305	103344.291404	34.598528
1021.800685	103504.166154	34.603546
1022.636158	103641.463379	34.608564
1023.806706	103792.883953	34.613581
1024.496629	103928.227201	34.618599
1025.493338	104068.429821	34.623616
1026.465908	104228.949003	34.628634
1027.166532	104377.770464	34.633652
1028.030284	104536.456968	34.638669
1029.345509	104692.106543	34.643687
1030.152943	104853.275849	34.648704
1030.741165	105013.465880	34.653722
1031.837322	105172.182384	34.658740
1032.859140	105351.769369	34.663757
1033.357950	105516.071317	34.668775
1034.611127	105683.996499	34.673792
1035.389476	105865.082497	34.678810
1036.265968	106040.549550	34.683828
1036.920678	106229.632533	34.688845
1037.877231	106418.441061	34.693863
1039.203717	106595.615724	34.698880
1040.510099	106776.864803	34.703898
1041.679520	106955.739707	34.708916
1042.943819	107122.199297	34.713933
1043.594199	107324.299036	34.718951
1044.848666	107508.730207	34.723968
1046.124060	107686.615914	34.728986
1046.851019	107882.353966	34.734004
1047.734009	108072.489184	34.739021
1048.662684	108258.636527	34.744039
1049.818188	108441.782037	34.749056
1050.556199	108647.299593	34.754074
1051.919834	108837.313013	34.759092
1053.603565	109023.752019	34.764109
1053.980499	109221.023393	34.769127
1055.181370	109401.313578	34.774144
1055.988662	109607.345850	34.779162
1056.985020	109807.579721	34.784180
1058.040093	110012.205984	34.789197
1059.060991	110212.882162	34.794215
1060.011409	110416.360454	34.799232
1061.420704	110622.380485	34.804250
1062.343518	110813.944655	34.809268
1063.849473	111013.496842	34.814285
1064.137933	111224.629049	34.819303
1065.079360	111422.471087	34.824320
1066.117146	111641.972640	34.829338
1066.919901	111856.325372	34.834356
1068.399693	112066.958976	34.839373
1069.292345	112286.639379	34.844391
1070.463115	112504.958621	34.849408
1071.477146	112708.757051	34.854426
1072.142250	112933.727514	34.859444
1073.609576	113148.719461	34.864461
1074.830166	113368.621426	34.869479
1075.677208	113579.718018	34.874496
1077.037616	113796.810492	34.879514
1078.148993	114007.893543	34.884532
1079.541257	114218.134813	34.889549
1081.034760	114437.721466	34.894567
1081.921117	114641.284348	34.899584
1082.864457	114847.122393	34.904602
1083.821886	115056.218957	34.909620
1084.948068	115258.872562	34.914637
1085.890246	115479.122478	34.919655
1086.904706	115687.414629	34.924672
1088.314849	115901.214041	34.929690
1089.183306	116101.908610	34.934708
1090.460606	116301.170423	34.939725
1091.897217	116492.658637	34.944743
1093.613423	116663.125175	34.949760
1094.824878	116855.944237	34.954778
1095.940196	117037.845862	34.959796
1097.627467	117220.622799	34.964813
1098.735375	117395.424323	34.969831
1099.584547	117568.922656	34.974848
1100.658963	117745.291178	34.979866
1101.327938	117941.232216	34.984884
1102.396564	118125.759325	34.989901
1103.285483	118309.351460	34.994919
1104.395178	118506.913424	34.999936
1105.743269	118695.699535	35.004954
1106.652670	118893.903711	35.009972
1108.496310	119073.278337	35.014989
1109.468276	119260.908407	35.020007
1110.180101	119457.763810	35.025024
1111.942394	119637.153807	35.030042
1112.851555	119817.819833	35.035060
1114.445330	119999.318200	35.040077
1115.147527	120192.652475	35.045095
1115.972782	120371.520283	35.050112
1117.106981	120571.042493	35.055130
1118.276270	120754.653141	35.060148
1119.603676	120945.407004	35.065165
1120.957549	121128.457739	35.070183
1122.367265	121311.792349	35.075200
1123.091565	121500.601014	35.080218
1124.015685	121699.261218	35.085236
1125.461923	121886.246186	35.090253
1126.436543	122080.384389	35.095271
1127.632971	122276.581940	35.100288
1128.578047	122456.201639	35.105306
1129.133704	122666.722032	35.110324
1130.478508	122864.611835	35.115341
1131.704804	123067.011957	35.120359
1133.610262	123251.153281	35.125376
1134.521468	123437.861438	35.130394
1135.567643	123638.415137	35.135412
1136.979049	123833.673316	35.140429
1138.297121	124015.385588	35.145447
1138.995955	124225.980579	35.150464
1140.177695	124406.942105	35.155482
1141.163956	124618.014279	35.160500
1142.402336	124805.007404	35.165517
1143.500825	125012.562627	35.170535
1144.335947	125214.603453	35.175552
1145.844261	125412.124968	35.180570
1146.377502	125619.797150	35.185588
1147.603766	125811.719206	35.190605
1148.751372	126031.349646	35.195623
1149.913273	126236.617546	35.200640
1150.799550	126444.505056	35.205658
1151.809968	126661.216979	35.210676
1152.689811	126870.363648	35.215693
1153.809875	127086.578528	35.220711
1154.304731	127317.672934	35.225728
1155.701792	127540.203070	35.230746
1156.603421	127766.973383	35.235764
1157.552969	127987.063878	35.240781
1159.211209	128226.050335	35.245799
1159.951410	128447.977636	35.250816
1161.143972	128686.823929	35.255834
1162.011120	128929.642996	35.260852
1162.981267	129159.417059	35.265869
1164.120791	129395.420922	35.270887
1165.055789	129624.454425	35.275904
1166.425941	129854.461444	35.280922
1167.249474	130087.663830	35.285940
1168.824722	130311.931612	35.290957
1169.761012	130547.047426	35.295975
1170.896856	130772.414138	35.300992
1172.693540	131000.939452	35.306010
1174.196242	131217.496166	35.311028
1175.508827	131445.198742	35.316045
1176.781220	131669.749382	35.321063
1177.986307	131898.854203	35.326080
1179.131822	132118.770336	35.331098
1180.369924	132352.516384	35.336116
1181.170564	132576.511103	35.341133
1182.507380	132809.267098	35.346151
1183.515016	133023.309066	35.351168
1185.072538	133263.075206	35.356186
1185.953926	133497.048121	35.361204
1187.382787	133732.725717	35.366221
1188.146229	133963.991409	35.371239
1189.256024	134204.226077	35.376256
1190.560908	134443.682827	35.381274
1191.629742	134701.260073	35.386292
1192.862601	134926.290237	35.391309
1194.676087	135164.732191	35.396327
1195.799182	135409.463272	35.401344
1197.114908	135649.736854	35.406362
1197.951116	135890.200980	35.411380
1199.388156	136131.257558	35.416397
1200.466200	136374.401971	35.421415
1201.608049	136623.920677	35.426432
1203.075355	136873.427856	35.431450
1204.273653	137116.912686	35.436468
1205.350779	137363.679109	35.441485
1206.772461	137607.144236	35.446503
1207.853311	137849.940653	35.451520
1209.077740	138089.048375	35.456538
1210.454990	138344.757708	35.461556
1211.642236	138588.480385	35.466573
1212.829400	138833.676430	35.471591
1213.922581	139088.076394	35.476608
1215.182250	139320.547720	35.481626
1216.242993	139583.851520	35.486644
1217.491157	139843.244076	35.491661
1219.663190	140066.020109	35.496679
1220.754631	140305.032941	35.501696
1222.720988	140531.688663	35.506714
1224.154004	140767.414144	35.511732
1225.934450	140980.382154	35.516749
1227.885911	141186.534607	35.521767
1228.920139	141412.122039	35.526784
1230.363871	141626.084739	35.531802
1231.203518	141830.713353	35.536820
1232.188472	142050.194274	35.541837
1233.268881	142271.361875	35.546855
1234.517761	142500.271243	35.551872
1236.070476	142694.981374	35.556890
1237.300133	142921.014741	35.561908
1238.884555	143121.724679	35.566925
1240.961394	143301.442554	35.571943
1242.416140	143505.639156	35.576960
1243.920375	143689.725164	35.581978
1245.176421	143890.235771	35.586996
1245.925533	144085.635583	35.592013
1247.272574	144271.791720	35.597031
1247.925468	144470.495283	35.602048
1249.108926	144672.759165	35.607066
1249.846364	144874.738299	35.612084
1250.624709	145078.501415	35.617101
1251.513482	145275.559315	35.622119
1252.433314	145485.914503	35.627136
1253.228940	145695.642697	35.632154
1254.346098	145919.841375	35.637172
1255.102441	146140.937123	35.642189
1256.033963	146368.454127	35.647207
1256.573991	146611.987816	35.652224
1257.841552	146850.839457	35.657242
1258.610352	147101.777436	35.662260
1259.339566	147361.226875	35.667277
1260.721737	147623.837406	35.672295
1261.758967	147886.909415	35.677312
1262.737100	148152.276693	35.682330
1263.872387	148423.941756	35.687348
1264.861473	148710.519923	35.692365
1266.337964	148987.110086	35.697383
1267.731663	149278.489388	35.702400
1268.310964	149561.201401	35.707418
1269.464858	149862.090493	35.712436
1270.847556	150158.718574	35.717453
1272.294645	150452.850297	35.722471
1273.490748	150762.026528	35.727488
1275.159331	151045.438898	35.732506
1276.689498	151348.016293	35.737524
1278.009342	151635.154729	35.742541
1279.907632	151927.675088	35.747559
1281.267664	152222.401103	35.752576
1283.166054	152493.675056	35.757594
1284.614839	152777.295695	35.762612
1285.643693	153075.949674	35.767629
1286.800327	153353.932050	35.772647
1288.160076	153647.180365	35.777664
1289.807351	153920.480754	35.782682
1291.462301	154215.958033	35.787700
1292.104826	154494.800786	35.792717
1294.131713	154781.692197	35.797735
1294.813092	155074.216159	35.802752
1296.094406	155358.535918	35.807770
1297.804710	155645.570009	35.812788
1299.550548	155928.372647	35.817805
1301.328561	156189.527237	35.822823
1302.454729	156468.316401	35.827840
1304.667762	156725.799967	35.832858
1305.977681	156994.432420	35.837876
1307.374518	157258.634659	35.842893
1309.013975	157519.486707	35.847911
1310.219284	157786.641080	35.852928
1311.136966	158042.454208	35.857946
1312.547840	158305.820960	35.862964
1313.612598	158590.342363	35.867981
1314.878302	158852.718585	35.872999
1316.129616	159127.514141	35.878016
1317.028596	159392.781111	35.883034
1318.578263	159672.623207	35.888052
1319.358222	159958.718940	35.893069
1320.925812	160219.136679	35.898087
1322.226532	160502.538109	35.903104
1323.950783	160776.847947	35.908122
1325.238096	161035.814854	35.913140
1326.520592	161315.642604	35.918157
1328.311784	161581.591666	35.923175
1329.362637	161859.210905	35.928192
1330.530430	162127.113396	35.933210
1331.657293	162400.596910	35.938228
1332.864495	162678.512588	35.943245
1334.160209	162955.298345	35.948263
1335.373844	163242.800913	35.953280
1336.744606	163504.456209	35.958298
1338.107629	163767.815039	35.963316
1339.229684	164038.944638	35.968333
1340.275130	164298.635284	35.973351
1341.618034	164567.802624	35.978368
1342.752909	164834.464326	35.983386
1343.754326	165110.264010	35.988404
1345.126409	165396.138587	35.993421
1346.642836	165682.182217	35.998439
1348.131713	165989.295002	36.003456
1349.502642	166269.358362	36.008474
1350.575221	166547.768197	36.013492
1351.793988	166845.937801	36.018509
1353.320933	167131.757233	36.023527
1354.560925	167424.161625	36.028544
1355.832848	167728.167206	36.033562
1357.235155	168013.285991	36.038580
1358.457951	168309.531205	36.043597
1359.881535	168607.752349	36.048615
1361.163517	168908.968018	36.053632
1362.620719	169210.703489	36.058650
1364.304926	169502.957942	36.063668
1365.757267	169801.535006	36.068685
1367.170126	170096.322960	36.073703
1368.714350	170406.061733	36.078720
1369.740893	170708.238973	36.083738
1371.096147	171007.928063	36.088756
1372.494361	171314.417498	36.093773
1373.687517	171608.941056	36.098791
1375.154843	171926.862666	36.103808
1376.566464	172240.235846	36.108826
1378.094789	172540.551457	36.113844
1379.910374	172841.559740	36.118861
1381.134623	173142.128437	36.123879
1382.816871	173445.559808	36.128896
1383.945203	173762.081732	36.133914
1385.715351	174056.206801	36.138932
1386.665183	174371.882929	36.143949
1388.456316	174675.403532	36.148967
1389.641682	174993.927694	36.153984
1391.103145	175304.448132	36.159002
1392.975461	175603.515132	36.164020
1393.975201	175903.545189	36.169037
1395.443450	176218.677485	36.174055
1396.695915	176537.641559	36.179072
1398.237526	176839.774288	36.184090
1400.027791	177143.977121	36.189108
1401.356851	177439.618255	36.194125
1403.101879	177741.646162	36.199143
1404.833323	178048.020174	36.204160
1406.295024	178338.488009	36.209178
1408.116126	178624.303638	36.214196
1409.268542	178913.272557	36.219213
1411.271940	179198.959931	36.224231
1412.911884	179497.022950	36.229248
1413.993547	179789.561460	36.234266
1416.010826	180072.176339	36.239284
1417.253858	180349.071785	36.244301
1418.792249	180623.077278	36.249319
1419.823886	180904.909296	36.254336
1421.174596	181198.095967	36.259354
1422.833541	181479.044208	36.264372
1423.445956	181767.878159	36.269389
1424.737034	182059.629170	36.274407
1425.673355	182353.189097	36.279424
1426.816039	182667.468172	36.284442
1428.133571	182952.512581	36.289460
1429.504164	183261.271836	36.294477
1430.807922	183553.634971	36.299495
1432.827840	183832.222344	36.304512
1434.583747	184099.752534	36.309530
1435.651063	184379.430307	36.314548
1436.955892	184676.216000	36.319565
1438.495792	184960.063053	36.324583
1440.013761	185259.763389	36.329600
1441.250231	185549.704571	36.334618
1442.394868	185844.766198	36.339636
1443.645454	186150.936996	36.344653
1444.742795	186450.478027	36.349671
1446.298002	186753.021583	36.354688
1447.155493	187084.148126	36.359706
1448.897997	187387.400754	36.364724
1449.747531	187723.254844	36.369741
1450.844120	188103.317763	36.374759
1451.922377	188445.005622	36.379776
1453.122148	188787.818511	36.384794
1455.040117	189117.261213	36.389812
1456.231952	189465.640015	36.394829
1457.777611	189805.607835	36.399847
1459.440924	190151.857509	36.404864
1460.491621	190503.919176	36.409882
1462.078310	190849.903503	36.414900
1463.649416	191204.654447	36.419917
1465.408820	191554.677862	36.424935
1467.061242	191899.130890	36.429952
1467.996025	192255.787948	36.434970
1469.911298	192611.225736	36.439988
1471.286811	192972.946823	36.445005
1473.123999	193320.270558	36.450023
1474.738461	193673.929543	36.455040
1476.197559	194029.468089	36.460058
1477.959688	194383.791718	36.465076
1479.546343	194733.190524	36.470093
1481.100530	195080.258406	36.475111
1482.817708	195439.595912	36.480128
1484.262719	195780.738752	36.485146
1486.020722	196121.909647	36.490164
1487.548625	196461.694899	36.495181
1488.847875	196817.468947	36.500199
1490.792643	197160.111796	36.505216
1492.142551	197516.438469	36.510234
1493.728383	197866.023010	36.515252
1494.990059	198209.461059	36.520269
1496.742965	198551.984740	36.525287
1498.274347	198899.675051	36.530304
1499.624049	199251.789121	36.535322
1501.267363	199601.749654	36.540340
1502.672247	199943.645000	36.545357
1504.466983	200286.369127	36.550375
1506.056899	200639.236109	36.555392
1507.348434	200992.607781	36.560410
1508.837739	201334.899231	36.565428
1510.502169	201685.089496	36.570445
1512.175427	202025.854787	36.575463
1513.709978	202374.822041	36.580480
1515.417804	202706.920987	36.585498
1517.784466	203039.146049	36.590516
1519.616705	203357.229893	36.595533
1521.522855	203679.417941	36.600551
1523.391355	203997.547998	36.605568
1525.059298	204316.395844	36.610586
1526.694528	204623.462443	36.615604
1527.861187	204937.360002	36.620621
1529.136718	205251.012384	36.625639
1531.294726	205551.266821	36.630656
1532.292427	205856.199611	36.635674
1534.259989	206156.814962	36.640692
1535.587806	206453.593396	36.645709
1536.964073	206740.228844	36.650727
1537.946082	207044.683109	36.655744
1539.223496	207343.071017	36.660762
1540.231400	207646.683735	36.665780
1541.986338	207966.641181	36.670797
1543.050275	208273.014883	36.675815
1544.790824	208585.557676	36.680832
1545.883980	208909.913094	36.685850
1547.182961	209231.315339	36.690868
1548.599734	209569.618168	36.695885
1549.476337	209910.241472	36.700903
1551.222426	210247.655318	36.705920
1552.450704	210606.540307	36.710938
1553.725485	210944.511432	36.715956
1555.179906	211300.846964	36.720973
1556.684697	211665.227961	36.725991
1558.152928	212029.386488	36.731008
1559.580953	212402.341373	36.736026
1560.924813	212767.561766	36.741044
1562.010138	213142.323987	36.746061
1563.602400	213530.420417	36.751079
1565.358813	213912.648738	36.756096
1566.663929	214301.502253	36.761114
1568.058139	214685.261479	36.766132
1569.517727	215078.994533	36.771149
1571.757425	215474.104702	36.776167
1573.071832	215869.944345	36.781184
1574.922174	216261.331008	36.786202
1576.143027	216652.257640	36.791220
1578.262924	217042.408789	36.796237
1579.767703	217459.889494	36.801255
1581.648384	217853.762263	36.806272
1583.630516	218251.099774	36.811290
1584.557207	218643.877599	36.816308
1586.480158	219033.171833	36.821325
1588.478824	219435.105629	36.826343
1590.194404	219826.566703	36.831360
1592.108374	220228.336362	36.836378
1593.761332	220613.888492	36.841396
1595.726481	220982.879309	36.846413
1597.510836	221381.545078	36.851431
1599.113175	221753.184168	36.856448
1600.433906	222151.490901	36.861466
1602.104112	222540.699210	36.866484
1603.778055	222925.486724	36.871501
1605.231937	223312.696745	36.876519
1606.858560	223703.690412	36.881536
1608.415969	224095.431686	36.886554
1609.974117	224484.429244	36.891572
1611.868006	224879.318841	36.896589
1613.312952	225286.269439	36.901607
1615.108365	225670.530144	36.906624
1616.406740	226050.778562	36.911642
1618.302871	226450.392927	36.916660
1619.876503	226835.374158	36.921677
1621.855395	227225.398124	36.926695
1623.297118	227608.316731	36.931712
1625.070909	227989.404998	36.936730
1627.048833	228372.417331	36.941748
1629.151590	228744.562485	36.946765
1630.468869	229132.555547	36.951783
1632.788565	229493.590335	36.956800
1634.192677	229876.361691	36.961818
1635.833868	230251.728614	36.966836
1637.639948	230611.674737	36.971853
1639.223756	230987.888618	36.976871
1640.305444	231345.940831	36.981888
1642.372650	231702.288976	36.986906
1643.204544	232060.405289	36.991924
1644.579690	232414.498760	36.996941
1646.363966	232785.853446	37.001959
1647.784465	233148.170214	37.006976
1649.456017	233521.802968	37.011994
1650.909628	233897.832103	37.017012
1652.393225	234270.045670	37.022029
1653.686422	234650.443349	37.027047
1655.448414	235029.420927	37.032064
1657.008628	235410.411231	37.037082
1658.481470	235805.539324	37.042100
1660.199032	236194.023748	37.047117
1661.363395	236596.871210	37.052135
1662.991961	236989.382497	37.057152
1664.368908	237404.110081	37.062170
1666.153825	237818.214426	37.067188
1667.684811	238219.859430	37.072205
1669.537999	238636.543190	37.077223
1671.663289	239044.114751	37.082240
1673.205047	239454.546045	37.087258
1674.807689	239865.881746	37.092276
1676.783917	240275.456349	37.097293
1678.994977	240688.296017	37.102311
1680.580552	241105.805518	37.107328
1682.929031	241501.729195	37.112346
1684.772402	241905.555485	37.117364
1686.690335	242307.997668	37.122381
1687.915717	242709.251992	37.127399
1689.788132	243112.970082	37.132416
1691.527802	243516.174767	37.137434
1693.774991	243915.869895	37.142452
1695.524904	244317.242496	37.147469
1696.581748	244722.711060	37.152487
1698.383956	245124.937643	37.157504
1700.379120	245526.117129	37.162522
1701.937955	245934.883310	37.167540
1703.925502	246344.038801	37.172557
1705.314309	246758.189833	37.177575
1707.269753	247160.362875	37.182592
1709.020038	247565.158212	37.187610
1710.399539	247984.617098	37.192628
1711.942983	248387.639388	37.197645
1713.229867	248820.472464	37.202663
1714.997558	249223.838765	37.207680
1716.665472	249650.564373	37.212698
1717.853332	250084.120990	37.217716
1719.402226	250510.507376	37.222733
1720.961798	250958.762110	37.227751
1723.049813	251396.797501	37.232768
1724.639174	251821.395894	37.237786
1726.249659	252262.958216	37.242804
1728.440353	252691.879992	37.247821
1730.291288	253129.083837	37.252839
1732.091189	253564.719462	37.257856
1734.339724	253999.496116	37.262874
1735.869261	254435.958841	37.267892
1737.447519	254875.663951	37.272909
1739.151944	255308.438767	37.277927
1740.761278	255745.672291	37.282944
1742.423653	256180.101964	37.287962
1743.769845	256626.137146	37.292980
1745.529781	257064.231764	37.297997
1747.405615	257502.560757	37.303015
1749.319810	257946.724400	37.308032
1751.402715	258371.911164	37.313050
1753.221417	258807.120231	37.318068
1755.233155	259225.685613	37.323085
1756.639571	259640.051593	37.328103
1758.825068	260051.627177	37.333120
1760.628621	260459.832055	37.338138
1762.423707	260878.095269	37.343156
1764.240758	261289.190708	37.348173
1765.920055	261698.020214	37.353191
1767.662378	262104.831776	37.358208
1769.031415	262521.580761	37.363226
1770.708222	262934.190652	37.368244
1772.588065	263365.486674	37.373261
1774.852747	263785.011587	37.378279
1776.249149	264208.074222	37.383296
1777.711449	264631.150234	37.388314
1779.291710	265064.619710	37.393332
1781.624243	265497.258460	37.398349
1782.806551	265929.059397	37.403367
1784.809860	266363.879454	37.408384
1786.553948	266797.366639	37.413402
1788.231916	267244.298112	37.418420
1790.053006	267689.351043	37.423437
1791.645651	268137.612456	37.428455
1793.450893	268584.187602	37.433472
1795.901163	269027.180152	37.438490
1797.385343	269475.121991	37.443508
1798.979502	269932.162279	37.448525
1800.950693	270383.629971	37.453543
1802.567691	270837.411220	37.458560
1804.826236	271285.121367	37.463578
1806.366423	271743.506961	37.468596
1808.270959	272198.379124	37.473613
1810.236814	272656.413945	37.478631
1811.858972	273119.503308	37.483648
1813.827371	273568.643918	37.488666
1815.345776	274036.188953	37.493684
1817.386844	274489.173563	37.498701
1819.251958	274956.582984	37.503719
1820.993102	275430.815334	37.508736
1822.643456	275895.637172	37.513754
1824.781964	276363.097308	37.518772
1826.735191	276836.831063	37.523789
1828.229012	277304.081791	37.528807
1829.940881	277784.755223	37.533824
1832.220026	278246.442783	37.538842
1833.843668	278720.394437	37.543860
1835.561963	279190.493687	37.548877
1837.658995	279679.856240	37.553895
1839.458817	280155.980678	37.558912
1841.511516	280623.885454	37.563930
1843.210247	281104.311282	37.568948
1845.199865	281583.926605	37.573965
1846.711615	282066.660810	37.578983
1848.659331	282541.121332	37.584000
1850.450469	283015.831736	37.589018
1852.213683	283511.416790	37.594036
1854.278109	283982.979890	37.599053
1856.056007	284468.296932	37.604071
1857.992026	284960.314953	37.609088
1860.160193	285434.619713	37.614106
1862.309158	285919.284347	37.619124
1864.333621	286387.586842	37.624141
1866.031415	286857.384523	37.629159
1867.920828	287331.744853	37.634176
1869.576489	287806.773132	37.639194
1871.510749	288289.651177	37.644212
1873.438683	288766.204119	37.649229
1875.289446	289247.132907	37.654247
1876.972272	289720.289262	37.659264
1878.963926	290173.715762	37.664282
1880.057845	290639.340078	37.669300
1881.919483	291100.829078	37.674317
1883.875208	291564.407319	37.679335
1885.433603	292030.227793	37.684352
1887.891311	292502.886246	37.689370
1889.393571	292977.290072	37.694388
1890.916470	293445.898101	37.699405
1893.122837	293926.353923	37.704423
1894.635091	294409.402606	37.709440
1896.136537	294889.884735	37.714458
1898.284399	295381.991389	37.719476
1900.399008	295874.073692	37.724493
1902.313346	296357.297216	37.729511
1904.023167	296856.136977	37.734528
1906.603588	297334.678148	37.739546
1908.826686	297833.530554	37.744564
1910.575634	298314.351459	37.749581
1912.315445	298808.294855	37.754599
1914.154322	299309.529807	37.759616
1916.238692	299796.327477	37.764634
1918.065535	300298.367654	37.769652
1920.033534	300803.960575	37.774669
1921.954086	301305.037459	37.779687
1924.101878	301805.718701	37.784704
1926.655457	302291.405006	37.789722
1928.267282	302788.251457	37.794740
1930.469827	303287.260059	37.799757
1932.497623	303789.007418	37.804775
1933.926794	304287.162819	37.809792
1935.888374	304796.881538	37.814810
1938.137500	305300.661075	37.819828
1939.915001	305804.128662	37.824845
1942.196121	306303.704894	37.829863
1943.702285	306824.491001	37.834880
1945.456297	307329.647672	37.839898
1947.116086	307848.571451	37.844916
1948.988179	308366.745842	37.849933
1951.100730	308890.156653	37.854951
1953.106181	309410.710428	37.859968
1955.212082	309931.522088	37.864986
1957.129619	310462.357889	37.870004
1959.251075	310987.622788	37.875021
1961.593651	311501.476631	37.880039
1963.224143	312026.121551	37.885056
1965.390582	312542.022050	37.890074
1968.043628	313052.307851	37.895092
1970.290777	313566.509277	37.900109
1972.363247	314064.210231	37.905127
1974.147643	314573.219244	37.910144
1976.411145	315091.207904	37.915162
1978.416971	315602.962430	37.920180
1980.301218	316104.883358	37.925197
1982.534886	316623.011356	37.930215
1984.076121	317148.372833	37.935232
1986.288528	317652.889654	37.940250
1988.598271	318162.638554	37.945268
1990.432128	318660.884109	37.950285
1992.094391	319177.929522	37.955303
1994.081633	319689.157500	37.960320
1995.977614	320196.079773	37.965338
1997.985776	320707.089370	37.970356
1999.748528	321228.357535	37.975373
2001.373615	321752.026094	37.980391
2003.247291	322263.926114	37.985408
2005.503129	322787.203984	37.990426
2007.742916	323301.977466	37.995444
2009.504835	323832.474989	38.000461
2012.085132	324315.693661	38.005479
2013.950186	324817.820119	38.010496
2015.731577	325307.774502	38.015514
2017.764660	325805.320763	38.020532
2018.975078	326297.306229	38.025549
2021.232503	326807.009123	38.030567
2023.063672	327317.837837	38.035584
2024.708759	327827.927984	38.040602
2027.042382	328344.170485	38.045620
2028.785594	328860.574724	38.050637
2030.765625	329375.844199	38.055655
2032.747339	329908.129883	38.060672
2034.478570	330433.470823	38.065690
2035.807270	330976.879807	38.070708
2037.536832	331530.721140	38.075725
2039.823374	332076.577703	38.080743
2041.738875	332635.498376	38.085760
2043.926073	333206.646317	38.090778
2045.475614	333771.949395	38.095796
2047.141048	334346.078917	38.100813
2049.503070	334910.857162	38.105831
2051.466838	335482.512644	38.110848
2053.686818	336074.462602	38.115866
2056.118792	336650.973028	38.120884
2057.820717	337243.644644	38.125901
2060.065382	337818.415713	38.130919
2061.718406	338425.888590	38.135936
2063.701560	339021.378579	38.140954
2065.658365	339622.011537	38.145972
2067.712590	340223.887261	38.150989
2069.767768	340828.669286	38.156007
2071.798572	341445.466347	38.161024
2073.625072	342073.646502	38.166042
2075.960879	342682.511901	38.171060
2078.310958	343299.251541	38.176077
2080.433883	343913.352857	38.181095
2082.849236	344535.994386	38.186112
2085.059766	345152.443558	38.191130
2087.585957	345772.103434	38.196148
2089.299131	346386.224207	38.201165
2091.437455	347002.701595	38.206183
2093.930266	347622.662190	38.211200
2096.200431	348230.068986	38.216218
2098.218441	348847.139552	38.221236
2100.501035	349477.849410	38.226253
2102.572161	350083.148583	38.231271
2104.693530	350717.865891	38.236288
2106.767415	351333.334074	38.241306
2108.981680	351951.608208	38.246324
2111.160239	352574.262188	38.251341
2112.975570	353181.520807	38.256359
2115.158405	353808.713549	38.261376
2117.809316	354426.136112	38.266394
2119.800028	355051.584903	38.271412
2121.830709	355669.865937	38.276429
2124.056081	356289.270374	38.281447
2126.078440	356914.778227	38.286464
2128.078060	357538.198297	38.291482
2130.080690	358161.706643	38.296500
2132.071372	358791.845464	38.301517
2134.326196	359414.959207	38.306535
2136.577418	360044.473612	38.311552
2138.509507	360673.340430	38.316570
2140.152716	361305.103409	38.321588
2142.564734	361948.265131	38.326605
2144.634518	362582.418187	38.331623
2146.813916	363217.326191	38.336640
2148.763044	363850.457086	38.341658
2151.435918	364457.914612	38.346676
2153.185161	365072.701454	38.351693
2155.346864	365679.149052	38.356711
2157.610457	366301.812297	38.361728
2159.611151	366926.454506	38.366746
2161.909824	367533.627205	38.371764
2163.800347	368143.182165	38.376781
2166.461153	368747.535556	38.381799
2168.791550	369365.053536	38.386816
2170.465543	369986.968274	38.391834
2173.076110	370599.347543	38.396852
2174.501198	371226.417357	38.401869
2177.064873	371849.570353	38.406887
2178.730912	372483.237744	38.411904
2180.763833	373120.152193	38.416922
2183.020442	373761.805258	38.421940
2185.152508	374411.848555	38.426957
2187.365537	375055.910127	38.431975
2189.848867	375717.166260	38.436992
2191.557789	376377.058019	38.442010
2193.410906	377030.071283	38.447028
2195.351572	377692.503625	38.452045
2197.924433	378366.346213	38.457063
2199.619270	379047.654838	38.462080
2201.422221	379721.507345	38.467098
2204.072579	380401.643587	38.472116
2206.121814	381097.509140	38.477133
2207.728732	381792.868080	38.482151
2210.225680	382489.867349	38.487168
2212.368043	383195.387588	38.492186
2214.881943	383887.205112	38.497204
2216.856414	384602.083382	38.502221
2219.085602	385317.762752	38.507239
2221.183656	386029.846478	38.512256
2223.645711	386758.059760	38.517274
2225.683670	387471.783389	38.522292
2228.259413	388178.920239	38.527309
2230.914878	388901.672677	38.532327
2233.330614	389611.933497	38.537344
2235.691844	390330.790906	38.542362
2238.111131	391039.288269	38.547380
2240.409982	391761.759305	38.552397
2242.770876	392469.363464	38.557415
2245.189310	393195.368154	38.562432
2246.986183	393905.803295	38.567450
2249.348591	394624.432181	38.572468
2251.743253	395350.527353	38.577485
2254.010752	396077.177172	38.582503
2256.135552	396792.993357	38.587520
2258.171901	397528.089118	38.592538
2260.753414	398241.157461	38.597556
2263.507604	398960.707063	38.602573
2265.711353	399686.091073	38.607591
2267.864247	400403.209816	38.612608
2270.133986	401129.297573	38.617626
2272.375740	401849.900524	38.622644
2274.508937	402576.267595	38.627661
2276.779786	403306.385816	38.632679
2279.199414	404028.410503	38.637696
2281.357865	404761.637232	38.642714
2284.041513	405479.981116	38.647732
2286.678804	406198.410478	38.652749
2288.631296	406931.294966	38.657767
2291.227665	407647.659985	38.662784
2293.051326	408375.760539	38.667802
2295.403592	409101.275142	38.672820
2297.622504	409829.265879	38.677837
2299.885244	410542.452111	38.682855
2302.192455	411235.219327	38.687872
2304.798336	411945.118646	38.692890
2307.091223	412634.605626	38.697908
2309.290134	413334.455737	38.702925
2310.933797	414040.794341	38.707943
2313.488856	414744.286123	38.712960
2315.345529	415447.611046	38.717978
2318.189255	416160.621575	38.722996
2320.516247	416881.073483	38.728013
2322.333845	417607.245142	38.733031
2324.828882	418325.395937	38.738048
2326.641011	419060.874631	38.743066
2328.784177	419784.340584	38.748084
2330.898972	420516.939021	38.753101
2333.345255	421256.589841	38.758119
2335.741420	422003.806971	38.763136
2337.714345	422755.108308	38.768154
2340.147012	423503.124670	38.773172
2342.348201	424260.857522	38.778189
2344.695188	425012.219377	38.783207
2347.114667	425778.153047	38.788224
2349.182777	426559.531948	38.793242
2351.630856	427330.811406	38.798260
2354.233476	428109.467984	38.803277
2356.557655	428883.386004	38.808295
2358.901111	429663.892523	38.813312
2361.326992	430448.651669	38.818330
2364.087588	431222.864654	38.823348
2365.628451	432005.071771	38.828365
2368.116092	432802.615059	38.833383
2370.479141	433592.817208	38.838400
2372.733405	434403.875194	38.843418
2375.163127	435197.841978	38.848436
2377.831786	436020.288604	38.853453
2380.120300	436815.069548	38.858471
2382.764864	437629.517623	38.863488
2385.030825	438443.535268	38.868506
2387.653586	439244.528347	38.873524
2390.474796	440043.182923	38.878541
2393.216299	440852.222709	38.883559
2395.902256	441647.596884	38.888576
2398.156590	442458.360790	38.893594
2400.337702	443263.039348	38.898612
2403.253841	444063.880732	38.903629
2405.401980	444873.949209	38.908647
2407.926479	445674.428135	38.913664
2410.205200	446485.314003	38.918682
2412.863826	447289.084784	38.923700
2415.227702	448098.016873	38.928717
2417.648436	448907.762298	38.933735
2420.005575	449714.704111	38.938752
2422.434253	450530.383938	38.943770
2425.313893	451338.231181	38.948788
2427.904192	452123.923327	38.953805
2430.849593	452927.043283	38.958823
2433.542575	453726.935371	38.963840
2435.808896	454525.192037	38.968858
2438.522618	455317.587969	38.973876
2440.769784	456105.730569	38.978893
2443.205019	456902.842803	38.983911
2445.393101	457685.270112	38.988928
2447.764448	458483.682374	38.993946
2450.019483	459288.434602	38.998964
2453.110207	460081.815476	39.003981
2455.270001	460887.264559	39.008999
2457.404842	461678.500541	39.014016
2459.770873	462486.162894	39.019034
2462.191441	463274.151504	39.024052
2464.341305	464056.343715	39.029069
2466.355378	464840.437906	39.034087
2469.004441	465625.253734	39.039104
2471.446821	466411.527948	39.044122
2472.811235	467200.153136	39.049140
2475.058594	467991.477869	39.054157
2477.323966	468800.616881	39.059175
2480.105300	469605.751990	39.064192
2482.592128	470430.108564	39.069210
2484.413461	471247.114519	39.074228
2486.831942	472071.247762	39.079245
2488.953103	472899.369333	39.084263
2491.511804	473732.926635	39.089280
2494.025008	474581.221034	39.094298
2495.902368	475437.384833	39.099316
2498.510882	476297.320905	39.104333
2500.722662	477162.263518	39.109351
2503.748701	478017.504525	39.114368
2506.529373	478894.261247	39.119386
2508.646216	479768.855441	39.124404
2511.120236	480639.665998	39.129421
2513.697704	481520.542028	39.134439
2516.497407	482402.089629	39.139456
2519.156953	483295.098680	39.144474
2521.714008	484176.281378	39.149492
2524.711301	485055.077679	39.154509
2527.429267	485947.773402	39.159527
2530.524158	486827.662458	39.164544
2533.262568	487713.501266	39.169562
2535.892565	488600.212359	39.174580
2538.504520	489472.770511	39.179597
2541.119818	490362.151447	39.184615
2543.278087	491244.198094	39.189632
2546.246484	492139.916128	39.194650
2548.628941	493014.521190	39.199668
2551.034043	493910.724997	39.204685
2553.419282	494815.488497	39.209703
2556.339542	495698.512715	39.214720
2559.241588	496593.771920	39.219738
2562.071648	497476.905294	39.224756
2564.722742	498358.805377	39.229773
2567.264841	499252.247278	39.234791
2570.239497	500128.503084	39.239808
2572.789466	501021.130585	39.244826
2575.784365	501908.298620	39.249844
2578.448168	502789.525453	39.254861
2580.856804	503668.272428	39.259879
2583.732622	504545.684853	39.264896
2586.241431	505423.855615	39.269914
2588.833812	506312.877351	39.274932
2591.566792	507183.759902	39.279949
2593.859564	508067.234691	39.284967
2596.773728	508940.445800	39.289984
2599.258932	509828.911151	39.295002
2601.929528	510704.263992	39.300020
2604.763441	511576.820553	39.305037
2607.093239	512464.740374	39.310055
2609.738641	513342.999236	39.315072
2612.583148	514226.752954	39.320090
2615.162184	515118.134517	39.325108
2617.531110	515989.731532	39.330125
2619.839253	516880.538324	39.335143
2622.745027	517767.976172	39.340160
2625.636591	518650.080178	39.345178
2627.850639	519543.542719	39.350196
2630.556049	520421.388569	39.355213
2633.063488	521305.490727	39.360231
2635.805549	522185.728904	39.365248
2638.061117	523037.240764	39.370266
2640.741603	523901.897889	39.375284
2643.503630	524745.935390	39.380301
2645.944371	525606.700564	39.385319
2648.881509	526468.789169	39.390336
2651.687572	527330.942503	39.395354
2653.741479	528185.119705	39.400372
2656.286128	529056.293100	39.405389
2658.619815	529925.784059	39.410407
2660.824888	530811.208274	39.415424
2663.275600	531702.911787	39.420442
2665.649833	532596.574653	39.425460
2668.349487	533503.682399	39.430477
2670.805565	534403.986173	39.435495
2672.953581	535322.248790	39.440512
2675.816455	536235.715232	39.445530
2677.844383	537182.428213	39.450548
2680.363823	538114.337092	39.455565
2683.282674	539061.122259	39.460583
2685.765311	540001.681590	39.465600
2688.846062	540960.042990	39.470618
2691.592370	541905.738364	39.475636
2694.281715	542878.616832	39.480653
2697.285447	543840.232215	39.485671
2700.465197	544785.993028	39.490688
2703.674959	545726.560338	39.495706
2706.490858	546687.282294	39.500724
2709.282976	547633.136971	39.505741
2712.244931	548598.953447	39.510759
2715.286663	549549.486294	39.515776
2718.417388	550502.789560	39.520794
2720.789349	551465.162271	39.525812
2723.247704	552411.150723	39.530829
2726.017849	553380.679317	39.535847
2729.067746	554344.923016	39.540864
2731.624816	555310.870771	39.545882
2734.185826	556276.840386	39.550900
2736.867247	557242.663039	39.555917
2739.601463	558227.191485	39.560935
2741.884414	559203.190494	39.565952
2744.972364	560181.388243	39.570970
2747.584733	561175.360931	39.575988
2750.422987	562158.042978	39.581005
2752.993871	563143.088976	39.586023
2755.713401	564139.298518	39.591040
2758.812997	565128.602301	39.596058
2761.178423	566133.060586	39.601076
2764.260785	567127.505093	39.606093
2767.070000	568120.204340	39.611111
2769.522300	569124.038586	39.616128
2772.002957	570121.623081	39.621146
2775.028711	571125.442746	39.626164
2777.845506	572131.158855	39.631181
2780.725223	573143.182421	39.636199
2783.726892	574144.237081	39.641216
2786.493797	575141.436821	39.646234
2789.423640	576156.035145	39.651252
2792.085271	577163.279352	39.656269
2794.972346	578177.601500	39.661287
2797.727803	579185.049191	39.666304
2801.188776	580195.196386	39.671322
2803.783563	581199.235573	39.676340
2806.613344	582199.096289	39.681357
2809.281864	583202.691872	39.686375
2812.527159	584211.955558	39.691392
2815.887458	585205.960135	39.696410
2818.822808	586201.040563	39.701428
2821.699512	587184.042906	39.706445
2824.527217	588149.570745	39.711463
2826.636697	589119.572775	39.716480
2829.717750	590071.296020	39.721498
2831.892865	591029.222870	39.726516
2834.654369	591984.124766	39.731533
2837.821606	592959.311123	39.736551
2840.366916	593929.660213	39.741568
2843.014932	594898.905899	39.746586
2845.531417	595874.926170	39.751604
2848.382538	596849.206127	39.756621
2851.412280	597831.357982	39.761639
2853.974167	598821.130839	39.766656
2856.793532	599820.106350	39.771674
2859.850531	600809.763918	39.776692
2862.402861	601808.491433	39.781709
2865.269755	602815.259511	39.786727
2867.778160	603829.871320	39.791744
2870.791985	604843.705864	39.796762
2873.818867	605873.256141	39.801780
2876.566562	606896.311045	39.806797
2879.252183	607921.917701	39.811815
2882.128361	608960.261325	39.816832
2884.859307	610010.143296	39.821850
2887.770565	611060.237840	39.826868
2890.326324	612102.549972	39.831885
2893.305099	613167.325571	39.836903
2895.914241	614241.269888	39.841920
2898.957905	615310.345597	39.846938
2901.787059	616378.244230	39.851956
2904.830325	617448.337754	39.856973
2907.738461	618534.085199	39.861991
2910.905298	619606.767797	39.867008
2914.109269	620686.154255	39.872026
2917.321170	621768.061852	39.877044
2919.833010	622847.867890	39.882061
2923.034011	623942.240145	39.887079
2926.011693	625030.399344	39.892096
2929.432657	626106.765387	39.897114
2933.073348	627189.849079	39.902132
2935.985907	628263.416733	39.907149
2939.276488	629335.760745	39.912167
2941.816988	630425.025945	39.917184
2945.417740	631510.269355	39.922202
2947.792847	632591.401489	39.927220
2950.501234	633659.074117	39.932237
2953.675859	634742.176226	39.937255
2956.292038	635850.115076	39.942272
2959.371096	636922.835122	39.947290
2962.373269	638025.087029	39.952308
2965.274683	639120.263755	39.957325
2968.040121	640210.958473	39.962343
2970.747609	641317.643492	39.967360
2974.264816	642412.090443	39.972378
2977.239795	643514.496040	39.977396
2979.595005	644615.525783	39.982413
2983.155735	645722.447752	39.987431
2986.077784	646831.026198	39.992448
2988.743331	647945.671703	39.997466
2991.733362	649055.908715	40.002484
2994.815508	650177.718528	40.007501
2997.571817	651288.565167	40.012519
3000.575079	652403.110804	40.017536
3003.780965	653514.359818	40.022554
3006.854539	654627.677357	40.027572
3009.760986	655738.749141	40.032589
3013.325637	656843.475949	40.037607
3016.132269	657965.653633	40.042624
3019.336476	659073.040029	40.047642
3022.540265	660151.810499	40.052660
3025.058199	661215.823710	40.057677
3028.121961	662287.808278	40.062695
3030.875464	663361.050504	40.067712
3034.285469	664420.174241	40.072730
3037.646728	665491.673252	40.077748
3040.835003	666567.381694	40.082765
3044.019014	667630.862954	40.087783
3046.601601	668710.665352	40.092800
3049.431517	669782.216843	40.097818
3052.610319	670866.019409	40.102836
3055.226564	671956.215336	40.107853
3059.063177	673034.886456	40.112871
3061.854180	674135.975579	40.117888
3064.931505	675226.576770	40.122906
3067.656984	676329.276451	40.127924
3070.731435	677430.194628	40.132941
3074.135645	678524.284619	40.137959
3076.473301	679640.726144	40.142976
3079.394500	680749.158316	40.147994
3082.759049	681874.202166	40.153012
3085.441448	683008.851527	40.158029
3088.816489	684138.390588	40.163047
3091.305821	685290.424415	40.168064
3094.355806	686432.467490	40.173082
3097.715688	687594.434021	40.178100
3100.406329	688742.694641	40.183117
3103.745136	689912.251427	40.188135
3106.639352	691091.302416	40.193152
3109.692253	692265.513512	40.198170
3112.369923	693445.348127	40.203188
3115.462283	694647.035734	40.208205
3118.729020	695827.323843	40.213223
3121.334388	697039.801786	40.218240
3124.744376	698245.403698	40.223258
3127.754209	699457.703556	40.228276
3131.114068	700663.742554	40.233293
3134.342507	701871.645425	40.238311
3137.618771	703087.602368	40.243328
3140.930719	704302.825965	40.248346
3144.050150	705523.717412	40.253364
3147.477075	706739.044691	40.258381
3150.505808	707961.401033	40.263399
3153.780062	709195.959662	40.268416
3157.118162	710423.953163	40.273434
3160.266688	711667.365946	40.278452
3163.224442	712904.202202	40.283469
3166.295166	714132.839599	40.288487
3169.368468	715376.462682	40.293504
3172.294869	716619.761847	40.298522
3175.758340	717862.432636	40.303540
3178.294751	719125.935211	40.308557
3181.964259	720372.061051	40.313575
3185.115372	721639.142632	40.318592
3188.436253	722882.846618	40.323610
3191.822862	724130.177593	40.328628
3194.811933	725392.624821	40.333645
3198.297174	726637.117172	40.338663
3201.710519	727894.947403	40.343680
3204.739949	729139.738563	40.348698
3208.675871	730393.183566	40.353716
3211.646166	731657.242193	40.358733
3214.737693	732894.023895	40.363751
3218.080493	734145.605373	40.368768
3220.910326	735394.008878	40.373786
3224.266039	736636.566502	40.378804
3227.393750	737889.417627	40.383821
3230.490743	739125.454709	40.388839
3234.009963	740352.277860	40.393856
3237.044849	741575.189772	40.398874
3240.314521	742786.713528	40.403892
3243.076181	743996.348005	40.408909
3246.347710	745206.143498	40.413927
3249.315647	746420.594728	40.418944
3252.327437	747638.025060	40.423962
3255.858921	748863.902320	40.428980
3259.124818	750102.023549	40.433997
3262.230845	751335.149502	40.439015
3265.362853	752575.660067	40.444032
3268.916937	753815.251663	40.449050
3272.138084	755056.297170	40.454068
3274.999968	756311.346834	40.459085
3278.358944	757555.707252	40.464103
3281.769529	758829.385003	40.469120
3284.831390	760095.097854	40.474138
3288.421049	761351.487960	40.479156
3291.328260	762639.295724	40.484173
3294.517396	763913.896301	40.489191
3297.649644	765202.223617	40.494208
3300.956322	766488.522664	40.499226
3304.670705	767786.262960	40.504244
3307.499472	769101.754981	40.509261
3310.694042	770404.465226	40.514279
3314.341640	771729.060412	40.519296
3317.244074	773043.932164	40.524314
3320.628268	774353.733331	40.529332
3323.620022	775687.097935	40.534349
3326.915827	777006.665686	40.539367
3330.904845	778342.674790	40.544384
3334.599122	779681.982454	40.549402
3337.978932	781009.986374	40.554420
3341.410756	782356.957725	40.559437
3344.608419	783689.683505	40.564455
3347.976672	785037.735203	40.569472
3351.263362	786386.112025	40.574490
3355.396424	787715.786504	40.579508
3359.002770	789053.422077	40.584525
3362.406908	790390.427773	40.589543
3366.329077	791723.277408	40.594560
3369.424111	793059.202870	40.599578
3372.942234	794384.797657	40.604596
3376.390825	795723.242094	40.609613
3379.670779	797064.457988	40.614631
3383.274676	798397.601001	40.619648
3386.268697	799734.022122	40.624666
3389.778879	801077.096827	40.629684
3392.651427	802429.239662	40.634701
3396.185444	803771.114190	40.639719
3399.825131	805119.697376	40.644736
3403.090985	806475.253651	40.649754
3406.644746	807833.005047	40.654772
3409.674226	809185.684851	40.659789
3413.081062	810539.474747	40.664807
3417.057589	811893.273696	40.669824
3420.241494	813257.401687	40.674842
3423.276840	814617.174879	40.679860
3426.543896	815975.644572	40.684877
3429.745671	817345.386689	40.689895
3433.038563	818720.444922	40.694912
3436.323541	820093.160548	40.699930
3439.961918	821471.436936	40.704948
3443.342996	822851.871348	40.709965
3446.873927	824223.919599	40.714983
3450.720986	825608.124023	40.720000
3453.661578	826992.932397	40.725018
3457.515913	828340.703187	40.730023
3460.797046	829668.999940	40.735028
3463.802849	830941.472786	40.740032
3467.338062	832165.704557	40.745037
3470.213896	833331.226239	40.750042
3473.189499	834436.301929	40.755047
3475.673887	835481.930634	40.760052
3478.435077	836453.947589	40.765056
3481.362472	837365.508311	40.770061
3483.626269	838238.895723	40.775066
3486.021072	839049.647782	40.780071
3488.478332	839786.255499	40.785076
3490.816014	840479.719843	40.790080
3492.653337	841110.037207	40.795085
3494.631153	841700.695213	40.800090
3496.308347	842219.481082	40.805095
3498.027324	842706.311868	40.810100
3499.353385	843143.228358	40.815104
3501.297838	843555.970800	40.820109
3502.277359	843921.911617	40.825114
3504.106542	844226.912792	40.830119
3504.676008	844521.237794	40.835124
3505.815603	844769.026847	40.840128
3506.954634	844978.614290	40.845133
3507.637574	845161.416165	40.850138
3508.772252	845328.148859	40.855143
3509.844184	845456.892333	40.860148
3510.494755	845565.442033	40.865152
3511.252450	845642.473593	40.870157
3511.711045	845701.329873	40.875162
3512.381162	845734.953373	40.880167
3513.030086	845755.883543	40.885172
3513.352498	845748.758037	40.890176
3513.965131	845721.621642	40.895181
3514.358642	845698.202357	40.900186
3514.895618	845648.398008	40.905191
3515.312010	845583.589133	40.910196
3515.470294	845499.919785	40.915200
3515.685790	845405.869300	40.920205
3515.952820	845305.799784	40.925210
3516.673503	845199.841929	40.930215
3516.938377	845080.480067	40.935220
3517.058031	844938.553128	40.940224
3517.305975	844794.470131	40.945229
3517.500822	844645.545015	40.950234
3517.562647	844477.636590	40.955239
3517.596508	844323.687579	40.960244
3517.460868	844152.892462	40.965248
3518.181339	843968.676562	40.970253
3517.912648	843793.819971	40.975258
3517.794677	843601.676655	40.980263
3518.013841	843416.358403	40.985268
3518.145075	843222.418526	40.990272
3518.083213	843022.975482	40.995277
3517.989388	842821.009530	41.000282
3518.204263	842606.673058	41.005287
3518.183991	842404.487421	41.010292
3518.009045	842191.651450	41.015296
3517.999658	841985.182725	41.020301
3517.538948	841779.068296	41.025306
3517.991381	841564.365948	41.030311
3517.921960	841352.065200	41.035316
3517.680677	841138.134783	41.040320
3517.855401	840913.170714	41.045325
3517.389411	840700.132599	41.050330
3517.151528	840467.164876	41.055335
3517.474143	840259.420011	41.060340
3517.345574	840039.514724	41.065344
3517.421468	839818.987227	41.070349
3517.004360	839592.125244	41.075354
3517.097266	839374.295162	41.080359
3517.283843	839176.333137	41.085364
3517.143830	838954.837054	41.090368
3517.068135	838729.732383	41.095373
3516.812957	838507.752488	41.100378
3516.678197	838274.003391	41.105383
3516.853269	838056.209268	41.110388
3516.922546	837836.676840	41.115392
3516.576638	837599.440519	41.120397
3516.381533	837402.449742	41.125402
3516.377999	837164.172030	41.130407
3516.033087	836950.301233	41.135412
3515.692018	836738.363520	41.140416
3515.806742	836531.977136	41.145421
3515.560596	836313.797010	41.150426
3515.526736	836111.690608	41.155431
3515.154886	835895.747664	41.160436
3515.383827	835690.867707	41.165440
3515.269390	835486.422771	41.170445
3515.180071	835284.200022	41.175450
3515.069234	835070.807984	41.180455
3514.758516	834873.363602	41.185460
3514.609557	834667.148368	41.190464
3514.961561	834471.432078	41.195469
3514.623506	834272.709854	41.200474
3514.284191	834066.892187	41.205479
3514.194995	833867.923447	41.210484
3513.749068	833681.240606	41.215488
3513.838150	833481.551393	41.220493
3513.364250	833288.742178	41.225498
3513.561565	833108.642500	41.230503
3513.386652	832928.109978	41.235508
3513.409539	832738.410729	41.240512
3513.294768	832555.623608	41.245517
3513.205744	832368.552852	41.250522
3513.242824	832185.439356	41.255527
3513.251685	832010.679074	41.260532
3512.581910	831831.065344	41.265536
3513.061854	831646.117616	41.270541
3512.797441	831465.360991	41.275546
3512.816465	831287.760774	41.280551
3512.377626	831110.518386	41.285556
3512.159174	830933.139185	41.290560
3512.267388	830763.379656	41.295565
3512.033297	830609.409816	41.300570
3511.915597	830428.987929	41.305575
3511.686128	830263.153916	41.310580
3511.646393	830095.536561	41.315584
3511.643770	829935.002693	41.320589
3511.549924	829783.808067	41.325594
3511.469929	829613.657010	41.330599
3511.431755	829455.156818	41.335604
3510.990219	829318.291067	41.340608
3511.566761	829137.722211	41.345613
3511.134948	828984.908273	41.350618
3511.135061	828818.901670	41.355623
3510.983671	828666.521856	41.360628
3510.702151	828520.865341	41.365632
3510.835653	828361.726567	41.370637
3511.129012	828206.349624	41.375642
3510.568682	828065.780428	41.380647
3510.288872	827914.957156	41.385652
3510.070753	827764.023288	41.390656
3510.262740	827625.173328	41.395661
3510.227208	827487.619579	41.400666
3509.835299	827336.313408	41.405671
3509.959332	827207.478055	41.410676
3509.810338	827066.043695	41.415680
3509.495855	826928.618153	41.420685
3509.125411	826806.949058	41.425690
3509.154399	826661.005032	41.430695
3509.271685	826535.170637	41.435700
3508.992515	826411.923690	41.440704
3508.822884	826280.294889	41.445709
3508.895724	826166.419786	41.450714
3508.912079	826041.368889	41.455719
3508.725300	825921.306487	41.460724
3508.590880	825808.429520	41.465728
3508.748245	825688.114253	41.470733
3508.291304	825571.588022	41.475738
3508.257541	825440.989609	41.480743
3508.361711	825339.639283	41.485748
3507.837015	825223.116999	41.490752
3508.519801	825100.179474	41.495757
3508.520659	824998.256119	41.500762
3508.093407	824876.557441	41.505767
3507.965552	824769.787513	41.510772
3507.594639	824662.178367	41.515776
3507.774453	824545.046734	41.520781
3507.489797	824454.635986	41.525786
3507.355634	824342.996379	41.530791
3507.417893	824243.287984	41.535796
3507.301544	824152.846472	41.540800
3507.275114	824048.674390	41.545805
3507.010042	823952.319642	41.550810
3506.959524	823843.867859	41.555815
3507.059903	823763.211402	41.560820
3507.126101	823663.492968	41.565824
3507.284541	823562.007479	41.570829
3506.823774	823465.383838	41.575834
3506.960113	823365.260475	41.580839
3506.788975	823284.737459	41.585844
3506.391653	823179.246635	41.590848
3506.600363	823085.625470	41.595853
3506.192490	822997.741946	41.600858
3506.082896	822916.523468	41.605863
3505.944249	822845.329333	41.610868
3506.238389	822765.310515	41.615872
3506.281464	822679.492352	41.620877
3505.955535	822592.952324	41.625882
3506.259779	822513.707007	41.630887
3506.227523	822423.810654	41.635892
3505.993971	822349.220228	41.640896
3506.191408	822266.777601	41.645901
3505.411913	822183.416281	41.650906
3505.813488	822115.826669	41.655911
3506.127697	822030.638185	41.660916
3505.708213	821955.488234	41.665920
3506.079095	821884.592547	41.670925
3505.483837	821801.683779	41.675930
3505.732422	821721.853138	41.680935
3505.720607	821647.024925	41.685940
3505.354016	821578.868344	41.690944
3505.491365	821507.323656	41.695949
3505.535988	821436.765756	41.700954
3505.327792	821369.165968	41.705959
3505.571569	821291.082142	41.710964
3505.384398	821231.262711	41.715968
3505.508061	821149.497882	41.720973
3505.246537	821078.399838	41.725978
3505.065255	821008.553578	41.730983
3504.979264	820945.698672	41.735988
3505.066244	820876.976827	41.740992
3504.815795	820808.209643	41.745997
3504.928410	820752.036941	41.751002
3504.949808	820694.710102	41.756007
3504.804524	820619.306343	41.761012
3504.722414	820564.427602	41.766016
3505.113743	820499.839000	41.771021
3504.571763	820437.147524	41.776026
3504.601960	820373.587335	41.781031
3504.876019	820327.605072	41.786036
3504.607739	820267.399659	41.791040
3504.812012	820210.623724	41.796045
3504.385395	820144.504637	41.801050
3504.433802	820086.486604	41.806055
3504.634098	820024.550906	41.811060
3504.524735	819976.095272	41.816064
3504.265941	819903.912588	41.821069
3504.014559	819851.876733	41.826074
3504.063783	819804.465671	41.831079
3504.121074	819752.283388	41.836084
3503.939486	819704.031589	41.841088
3503.989626	819663.530406	41.846093
3503.784479	819617.812460	41.851098
3504.006465	819577.186509	41.856103
3504.156146	819519.439352	41.861108
3504.085792	819468.150709	41.866112
3503.879976	819412.404990	41.871117
3503.931179	819377.645070	41.876122
3503.774037	819318.094450	41.881127
3504.026540	819265.390820	41.886132
3503.721767	819225.721025	41.891136
3503.473158	819173.386988	41.896141
3503.675623	819129.840719	41.901146
3503.786672	819089.910354	41.906151
3503.204468	819043.857713	41.911156
3503.202246	819006.670315	41.916160
3503.391021	818956.407781	41.921165
3503.203976	818927.815708	41.926170
3503.507800	818893.110932	41.931175
3503.465658	818850.963873	41.936180
3503.294358	818814.483223	41.941184
3503.526747	818767.911776	41.946189
3503.210414	818731.258599	41.951194
3503.241275	818689.975227	41.956199
3503.725452	818649.496922	41.961204
3503.312648	818619.575731	41.966208
3503.416167	818582.466616	41.971213
3503.050922	818547.475069	41.976218
3503.058958	818503.760083	41.981223
3502.875032	818466.305773	41.986228
3502.782461	818436.723075	41.991232
3503.119557	818401.912993	41.996237
3503.285574	818376.183980	42.001242
3503.103645	818334.736787	42.006247
3503.297029	818291.867584	42.011252
3502.917884	818264.568181	42.016256
3502.854755	818228.553984	42.021261
3502.884771	818204.695412	42.026266
3503.116715	818166.005922	42.031271
3503.134216	818128.712814	42.036276
3503.028135	818105.167227	42.041280
3503.155130	818055.199147	42.046285
3503.487317	818024.963894	42.051290
3502.840169	817987.287006	42.056295
3503.299764	817951.384221	42.061300
3502.747421	817919.923589	42.066304
3503.092425	817892.898819	42.071309
3502.529984	817858.031572	42.076314
3502.475361	817818.118923	42.081319
3502.807785	817790.900937	42.086324
3502.670713	817770.766860	42.091328
3502.542298	817741.186449	42.096333
3502.763097	817721.288380	42.101338
3502.573685	817685.193401	42.106343
3502.648053	817656.554599	42.111348
3502.515543	817639.535276	42.116352
3502.722708	817608.441195	42.121357
3502.608468	817585.479147	42.126362
3502.548692	817549.752607	42.131367
3502.749966	817529.564857	42.136372
3502.208439	817513.193367	42.141376
3502.360676	817477.433268	42.146381
3502.137134	817468.509781	42.151386
3502.416774	817431.463633	42.156391
3502.260650	817421.458412	42.161396
3502.624989	817392.480940	42.166400
3502.927543	817365.557892	42.171405
3502.430998	817344.017981	42.176410
3502.732483	817317.484399	42.181415
3502.639679	817282.248369	42.186420
3502.515677	817258.702375	42.191424
3502.589127	817227.529916	42.196429
3502.574712	817196.371036	42.201434
3502.523905	817174.176583	42.206439
3502.593952	817145.438724	42.211444
3502.285281	817124.063439	42.216448
3502.375231	817104.475994	42.221453
3502.529932	817079.522428	42.226458
3502.311124	817053.263815	42.231463
3502.612418	817024.489250	42.236468
3502.379987	817015.858645	42.241472
3502.355118	816994.243785	42.246477
3502.192846	816968.560269	42.251482
3502.334480	816945.263709	42.256487
3502.420358	816918.956900	42.261492
3502.334257	816884.301867	42.266496
3502.223460	816866.692729	42.271501
3502.021199	816853.674899	42.276506
3502.065253	816830.587933	42.281511
3502.662923	816805.271870	42.286516
3502.437162	816785.051077	42.291520
3502.525666	816756.990238	42.296525
3502.723406	816729.009582	42.301530
3502.507792	816712.098095	42.306535
3502.748666	816681.773209	42.311540
3502.237454	816661.596637	42.316544
3502.281719	816625.848526	42.321549
3502.254558	816611.439387	42.326554
3502.173247	816591.682325	42.331559
3502.386049	816559.803021	42.336564
3502.352710	816552.504092	42.341568
3502.425754	816536.131336	42.346573
3502.265730	816500.706609	42.351578
3502.228173	816487.857046	42.356583
3502.648651	816466.365516	42.361588
3502.157501	816444.529466	42.366592
3502.613968	816424.493026	42.371597
3502.301413	816403.894997	42.376602
3502.180288	816373.722593	42.381607
3502.168252	816344.799088	42.386612
3502.173922	816332.039838	42.391616
3502.311426	816310.884186	42.396621
3502.048608	816289.596254	42.401626
3502.319050	816268.322283	42.406631
3502.263380	816252.358476	42.411636
3502.260845	816237.652443	42.416640
3502.084933	816207.779981	42.421645
3502.345947	816190.500385	42.426650
3502.399288	816161.078834	42.431655
3502.378142	816152.998371	42.436660
3502.487146	816123.275755	42.441664
3502.258633	816091.950025	42.446669
3502.102910	816074.150876	42.451674
3502.143754	816055.736567	42.456679
3502.230745	816034.198286	42.461684
3501.718083	816010.805721	42.466688
3502.217983	815982.579688	42.471693
3502.066030	815978.220563	42.476698
3501.856341	815963.448867	42.481703
3501.827397	815939.493428	42.486708
3501.818209	815924.105905	42.491712
3501.908395	815910.163795	42.496717
3501.985224	815895.834144	42.501722
3502.474516	815882.706177	42.506727
3502.302865	815862.668726	42.511732
3501.952362	815853.275763	42.516736
3501.724139	815823.994037	42.521741
3501.691005	815809.291776	42.526746
3501.608857	815799.077577	42.531751
3501.877165	815775.951649	42.536756
3502.116098	815780.102569	42.541760
3501.890118	815744.586452	42.546765
3501.971985	815741.164624	42.551770
3501.796103	815725.218259	42.556775
3502.079371	815701.894915	42.561780
3502.240708	815691.642478	42.566784
3501.873454	815678.160967	42.571789
3501.925037	815656.626917	42.576794
3501.812111	815635.410720	42.581799
3502.050151	815618.620151	42.586804
3501.924496	815599.256487	42.591808
3502.296932	815582.055196	42.596813
3501.922983	815562.730232	42.601818
3501.618622	815554.595861	42.606823
3502.125549	815537.665637	42.611828
3502.011070	815515.183011	42.616832
3502.153768	815496.751131	42.621837
3502.096245	815487.117004	42.626842
3501.759837	815471.389894	42.631847
3501.934411	815442.530439	42.636852
3501.715293	815433.505928	42.641856
3501.579094	815417.747385	42.646861
3501.675591	815406.043515	42.651866
3501.701454	815403.604327	42.656871
3501.981916	815372.779859	42.661876
3501.454610	815368.186759	42.666880
3501.563146	815361.253887	42.671885
3501.374643	815340.827761	42.676890
3501.521609	815326.972881	42.681895
3502.077537	815315.197023	42.686900
3501.448808	815315.879783	42.691904
3501.448169	815300.879019	42.696909
3501.632278	815295.785022	42.701914
3501.431135	815284.030043	42.706919
3501.720573	815259.729997	42.711924
3501.905159	815261.551942	42.716928
3501.550145	815248.944268	42.721933
3501.514282	815240.572695	42.726938
3501.363757	815223.744398	42.731943
3501.591823	815219.033105	42.736948
3501.657132	815211.132726	42.741952
3501.289256	815192.779763	42.746957
3501.272184	815188.788639	42.751962
3501.527152	815187.969526	42.756967
3501.709031	815180.343116	42.761972
3501.126370	815165.822653	42.766976
3501.461700	815146.775165	42.771981
3501.702853	815160.472413	42.776986
3501.292321	815149.626609	42.781991
3501.361926	815127.016397	42.786996
3501.138954	815130.071025	42.792001
3501.424436	815120.674946	42.797005
3501.443784	815122.522762	42.802010
3501.400747	815104.898051	42.807015
3501.713101	815087.217735	42.812020
3501.742567	815078.446085	42.817025
3501.593303	815062.591275	42.822029
3501.749245	815055.261004	42.827034
3501.808419	815058.758622	42.832039
3501.855199	815033.716334	42.837044
3501.604619	815016.805706	42.842049
3501.448287	815018.583603	42.847053
3501.858916	814989.685157	42.852058
3501.423805	814979.914445	42.857063
3501.769617	814967.878542	42.862068
3501.520880	814952.526071	42.867073
3501.576096	814938.587259	42.872077
3501.674146	814928.148636	42.877082
3501.430927	814926.238396	42.882087
3501.416265	814901.692255	42.887092
3501.192173	814906.987704	42.892097
3501.505866	814903.236936	42.897101
3501.227783	814895.000178	42.902106
3501.627072	814881.786772	42.907111
3501.423747	814867.401143	42.912116
3501.336677	814869.655330	42.917121
3501.346068	814871.309946	42.922125
3501.502752	814854.627460	42.927130
3501.146227	814846.792562	42.932135
3501.653184	814842.037391	42.937140
3501.549374	814832.312073	42.942145
3501.357793	814825.035858	42.947149
3501.326021	814810.233616	42.952154
3501.341205	814802.925053	42.957159
3501.568293	814802.792164	42.962164
3501.393242	814784.310439	42.967169
3501.585050	814762.946223	42.972173
3501.504195	814765.881393	42.977178
3501.508591	814762.665976	42.982183
3501.359470	814749.148352	42.987188
3501.533619	814746.490893	42.992193
3501.447684	814735.983293	42.997197
3501.810576	814735.244670	43.002202
3501.657585	814711.109074	43.007207
3501.527302	814702.751540	43.012212
3501.373156	814704.529182	43.017217
3501.402193	814690.496492	43.022221
3501.551294	814677.614021	43.027226
3501.410379	814666.043298	43.032231
3501.583217	814663.386009	43.037236
3501.407717	814653.671619	43.042241
3501.376866	814639.648177	43.047245
3501.534694	814638.162249	43.052250
3501.571673	814639.715195	43.057255
3501.553905	814614.389061	43.062260
3501.137542	814605.589021	43.067265
3501.330003	814602.149284	43.072269
3501.550721	814606.888354	43.077274
3501.455919	814581.768969	43.082279
3501.205474	814572.455847	43.087284
3501.188008	814572.750863	43.092289
3501.344768	814570.777987	43.097293
3501.511683	814565.978345	43.102298
3501.465570	814559.750700	43.107303
3501.198246	814534.365832	43.112308
3501.279430	814532.307338	43.117313
3501.191346	814530.470144	43.122317
3501.546705	814531.681086	43.127322
3501.415133	814508.418142	43.132327
3501.405111	814499.944116	43.137332
3501.703454	814498.046506	43.142337
3501.339339	814499.272503	43.147341
3501.360861	814475.790664	43.152346
3501.665378	814470.287489	43.157351
3501.443903	814445.869309	43.162356
3501.252777	814460.415046	43.167361
3501.352009	814438.869352	43.172365
3501.416831	814432.819083	43.177370
3501.369091	814442.958453	43.182375
3501.711005	814438.715889	43.187380
3501.898301	814414.136263	43.192385
3501.405743	814396.872092	43.197389
3501.800979	814398.758786	43.202394
3501.318193	814375.939941	43.207399
3501.476619	814363.639904	43.212404
3501.515302	814362.659652	43.217409
3501.332657	814356.745417	43.222413
3501.585813	814333.324257	43.227418
3501.449699	814327.013026	43.232423
3501.273314	814324.312761	43.237428
3501.273622	814326.650908	43.242433
3501.532904	814298.844595	43.247437
3501.661929	814297.265666	43.252442
3501.200577	814298.019780	43.257447
3501.532049	814292.804509	43.262452
3501.449820	814273.137671	43.267457
3501.408180	814264.083721	43.272461
3501.340170	814251.818861	43.277466
3501.291221	814258.256574	43.282471
3501.537066	814252.080408	43.287476
3501.262397	814234.392027	43.292481
3501.527962	814227.238502	43.297485
3501.622305	814227.710906	43.302490
3501.277096	814220.847702	43.307495
3501.508591	814196.162887	43.312500
3501.209597	814205.270235	43.317505
3501.614261	814203.161067	43.322509
3501.430933	814199.487577	43.327514
3500.937741	814185.243113	43.332519
3501.610672	814174.615942	43.337524
3501.574951	814169.457970	43.342529
3501.224680	814170.097308	43.347533
3501.233910	814149.344096	43.352538
3501.337296	814143.969504	43.357543
3501.329365	814133.935831	43.362548
3501.185772	814127.722994	43.367553
3501.053036	814135.635332	43.372557
3501.328584	814143.483837	43.377562
3501.282559	814111.729932	43.382567
3501.513509	814094.254395	43.387572
3501.185105	814087.875553	43.392577
3501.342857	814104.023844	43.397581
3501.269798	814090.492905	43.402586
3500.605917	814085.433058	43.407591
3500.752710	814089.404660	43.412596
3500.843436	814104.978862	43.417601
3501.107101	814101.625149	43.422605
3501.203755	814083.488585	43.427610
3501.287363	814084.449816	43.432615
3501.113607	814078.241644	43.437620
3501.416863	814070.887195	43.442625
3501.176215	814071.704261	43.447629
3501.552866	814060.928359	43.452634
3501.115086	814051.254031	43.457639
3501.445492	814044.674731	43.462644
3501.186095	814046.274155	43.467649
3501.162765	814037.314442	43.472653
3501.423814	814029.576830	43.477658
3500.980056	814023.118526	43.482663
3501.320574	814010.302189	43.487668
3501.343421	814010.396072	43.492673
3500.796251	814007.948488	43.497677
3501.497491	814001.895746	43.502682
3501.294190	814004.947842	43.507687
3501.288167	813985.852760	43.512692
3501.251815	813981.084447	43.517697
3501.208663	813975.927477	43.522701
3501.169518	813987.235390	43.527706
3501.133939	813985.292399	43.532711
3501.324082	813972.499491	43.537716
3501.415768	813963.424264	43.542721
3501.250170	813958.383850	43.547725
3501.847962	813948.547480	43.552730
3501.143327	813944.565613	43.557735
3501.009318	813927.926101	43.562740
3501.346511	813929.627154	43.567745
3501.566221	813925.890499	43.572749
3501.632119	813915.065495	43.577754
3501.261261	813910.544279	43.582759
3501.148480	813891.660459	43.587764
3501.285492	813876.732192	43.592769
3501.130070	813887.181586	43.597773
3501.160069	813879.967061	43.602778
3500.812028	813883.139272	43.607783
3501.052046	813875.502189	43.612788
3501.088235	813885.629341	43.617793
3501.063502	813873.356974	43.622797
3501.189734	813856.384299	43.627802
3501.222490	813856.768928	43.632807
3501.185320	813846.641934	43.637812
3501.328761	813851.198799	43.642817
3501.152218	813857.559438	43.647821
3501.362552	813854.213931	43.652826
3501.030182	813837.410324	43.657831
3501.353007	813832.878045	43.662836
3501.222183	813829.975580	43.667841
3501.276118	813828.213409	43.672845
3501.151669	813816.930834	43.677850
3501.123471	813815.960951	43.682855
3501.328062	813789.135244	43.687860
3501.225123	813782.038819	43.692865
3501.124320	813775.916374	43.697869
3501.101407	813780.986456	43.702874
3501.231258	813779.504701	43.707879
3501.454748	813780.444112	43.712884
3501.053415	813759.071762	43.717889
3501.085732	813760.333358	43.722893
3501.140206	813755.745540	43.727898
3501.027383	813764.921856	43.732903
3501.419751	813767.296356	43.737908
3501.183183	813767.820524	43.742913
3501.243542	813758.457601	43.747917
3501.528398	813745.941724	43.752922
3501.414831	813733.000940	43.757927
3501.123969	813728.467085	43.762932
3500.877923	813733.961818	43.767937
3501.004284	813728.096115	43.772941
3501.084785	813727.401525	43.777946
3500.878541	813717.982784	43.782951
3501.366410	813712.937453	43.787956
3501.352353	813707.288548	43.792961
3501.128032	813703.426306	43.797965
3501.251661	813704.771073	43.802970
3501.304890	813720.157228	43.807975
3501.403296	813700.265486	43.812980
3501.538902	813682.901141	43.817985
3501.206614	813675.548147	43.822989
3501.281930	813667.741690	43.827994
3501.204712	813674.769025	43.832999
3501.133020	813657.631884	43.838004
3501.162637	813645.935180	43.843009
3501.030465	813635.238089	43.848013
3501.415653	813631.865131	43.853018
3501.308860	813635.974097	43.858023
3501.306998	813627.789918	43.863028
3501.183055	813634.727167	43.868033
3501.013348	813617.800108	43.873037
3501.219413	813611.629532	43.878042
3500.923591	813610.896323	43.883047
3501.246568	813602.563897	43.888052
3500.787584	813611.697114	43.893057
3500.722036	813610.245864	43.898061
3500.902112	813606.222912	43.903066
3500.838941	813607.012292	43.908071
3501.091236	813606.290834	43.913076
3501.104756	813607.555400	43.918081
3501.117593	813611.061073	43.923085
3501.037195	813601.719919	43.928090
3500.868646	813589.469477	43.933095
3500.850074	813582.359637	43.938100
3501.200770	813583.279194	43.943105
3501.017087	813589.933526	43.948109
3501.288909	813587.747487	43.953114
3500.687467	813597.682475	43.958119
3500.905047	813588.587026	43.963124
3501.272543	813593.498795	43.968129
3501.041894	813598.796368	43.973133
3500.840885	813596.391940	43.978138
3500.695243	813596.024993	43.983143
3500.850678	813601.944256	43.988148
3500.998598	813599.290414	43.993153
3500.870286	813605.351464	43.998157
3500.545190	813596.730598	44.003162
3500.905295	813605.930653	44.008167
3501.352911	813593.096724	44.013172
3501.165515	813581.823564	44.018177
3500.813256	813580.319691	44.023181
3501.109753	813577.740051	44.028186
3501.099039	813577.644316	44.033191
3500.859857	813572.907399	44.038196
3501.213508	813579.282874	44.043201
3501.006759	813582.238277	44.048205
3501.004213	813576.295148	44.053210
3500.995817	813584.675920	44.058215
3500.996306	813563.922135	44.063220
3501.089993	813549.097297	44.068225
3500.758707	813553.728589	44.073229
3501.183046	813548.108445	44.078234
3500.896987	813547.958316	44.083239
3500.912744	813547.371264	44.088244
3501.114328	813549.288494	44.093249
3500.678803	813558.710428	44.098253
3501.035240	813553.393209	44.103258
3500.907060	813567.931175	44.108263
3501.010320	813549.694599	44.113268
3501.254924	813559.984569	44.118273
3501.035545	813563.721440	44.123277
3501.452410	813554.692225	44.128282
3501.099286	813547.050029	44.133287
3501.147890	813538.468101	44.138292
3501.354764	813542.917839	44.143297
3501.100072	813548.219213	44.148301
3501.149151	813546.555158	44.153306
3501.230099	813539.722020	44.158311
3501.216595	813522.477977	44.163316
3501.304933	813511.356460	44.168321
3501.177906	813502.607065	44.173325
3501.403244	813502.474429	44.178330
3501.452590	813516.010398	44.183335
3501.198376	813495.003892	44.188340
3501.353370	813472.958977	44.193345
3500.965255	813478.476140	44.198349
3501.182002	813474.544808	44.203354
3500.885393	813480.632287	44.208359
3500.890516	813478.585338	44.213364
3501.299310	813474.331674	44.218369
3501.154835	813473.379915	44.223373
3500.918538	813455.878205	44.228378
3501.158406	813451.163747	44.233383
3501.020585	813450.016069	44.238388
3501.233687	813447.254538	44.243393
3501.089836	813450.297607	44.248397
3501.064411	813446.404114	44.253402
3501.312947	813458.447510	44.258407
3500.950848	813444.278296	44.263412
3501.319602	813420.445908	44.268417
3501.078612	813422.822112	44.273421
3501.120395	813427.882366	44.278426
3501.014725	813427.996348	44.283431
3501.297463	813434.577933	44.288436
3501.102938	813416.582395	44.293441
3501.263723	813417.921416	44.298445
3501.202552	813412.961675	44.303450
3501.420529	813398.701679	44.308455
3501.187421	813392.307227	44.313460
3500.917147	813392.057188	44.318465
3500.745010	813407.089588	44.323469
3501.167603	813399.715701	44.328474
3501.172286	813399.422681	44.333479
3501.306912	813388.391148	44.338484
3501.292342	813368.905768	44.343489
3501.117459	813369.322886	44.348493
3501.180873	813363.466683	44.353498
3500.560109	813367.461292	44.358503
3500.646976	813365.401528	44.363508
3500.921660	813365.358615	44.368513
3500.671058	813365.105500	44.373517
3501.018787	813368.461519	44.378522
3500.933656	813372.957025	44.383527
3500.988993	813375.384363	44.388532
3500.935599	813367.110461	44.393537
3500.998221	813369.828977	44.398541
3500.969437	813370.905327	44.403546
3501.208065	813382.658102	44.408551
3501.115290	813367.472229	44.413556
3501.339873	813353.113659	44.418561
3500.958810	813353.270692	44.423565
3501.106147	813350.909154	44.428570
3500.817327	813345.790067	44.433575
3500.907833	813346.068262	44.438580
3500.954078	813354.440800	44.443585
3500.930541	813354.639383	44.448589
3501.189600	813345.634537	44.453594
3501.035305	813350.335750	44.458599
3501.214543	813354.107871	44.463604
3501.183556	813335.112147	44.468609
3501.336823	813330.508575	44.473613
3500.925859	813318.782694	44.478618
3500.921476	813338.368682	44.483623
3501.131919	813327.812386	44.488628
3501.188460	813337.450047	44.493633
3501.079640	813333.374643	44.498637
3501.169856	813332.483614	44.503642
3501.267716	813319.801242	44.508647
3500.956129	813306.890531	44.513652
3501.335585	813303.615735	44.518657
3501.198225	813318.155714	44.523661
3501.078337	813309.989569	44.528666
3501.188766	813304.515719	44.533671
3501.180282	813306.953060	44.538676
3501.381108	813296.398215	44.543681
3501.296346	813282.672479	44.548685
3501.347972	813267.171471	44.553690
3501.385965	813272.817083	44.558695
3500.874090	813280.205126	44.563700
3501.331494	813281.887569	44.568705
3500.981312	813256.997667	44.573709
3500.975385	813239.459340	44.578714
3500.975544	813243.844166	44.583719
3500.873074	813248.050150	44.588724
3500.926293	813238.102924	44.593729
3500.994550	813240.918056	44.598733
3501.255685	813240.000296	44.603738
3501.105701	813251.814065	44.608743
3501.029221	813252.995331	44.613748
3501.266283	813240.778241	44.618753
3501.071105	813236.326510	44.623757
3500.876676	813219.889442	44.628762
3501.341513	813219.816804	44.633767
3501.392429	813223.219301	44.638772
3501.198270	813220.229011	44.643777
3500.963539	813226.696825	44.648781
3501.262035	813219.244686	44.653786
3501.047727	813211.093173	44.658791
3500.885731	813201.471854	44.663796
3500.984165	813194.635607	44.668801
3500.947757	813194.349000	44.673805
3500.874504	813182.082864	44.678810
3501.191485	813187.490059	44.683815
3500.968085	813185.283855	44.688820
3500.812730	813184.236310	44.693825
3501.015384	813184.886747	44.698829
3501.240925	813179.102469	44.703834
3501.399055	813200.612314	44.708839
3501.047001	813192.579750	44.713844
3501.316478	813168.859369	44.718849
3501.026042	813172.217812	44.723853
3500.962986	813161.411666	44.728858
3501.362549	813159.010628	44.733863
3500.928114	813154.888565	44.738868
3501.366171	813166.415688	44.743873
3500.901479	813160.739291	44.748877
3500.615644	813141.782820	44.753882
3501.295973	813151.323255	44.758887
3500.995496	813145.913501	44.763892
3501.226819	813139.056420	44.768897
3500.801642	813147.015719	44.773901
3500.366199	813135.293319	44.778906
3500.895281	813143.980429	44.783911
3500.963360	813135.784674	44.788916
3500.862537	813142.816295	44.793921
3500.517754	813144.721617	44.798925
3501.101648	813137.322209	44.803930
3500.812322	813145.455158	44.808935
3500.678510	813158.143553	44.813940
3500.959869	813145.627029	44.818945
3501.052406	813151.459108	44.823949
3501.011663	813158.968528	44.828954
3501.051609	813158.085333	44.833959
3500.836598	813164.452687	44.838964
3501.261132	813158.442399	44.843969
3501.248900	813165.752471	44.848973
3501.015529	813141.525942	44.853978
3501.226991	813131.553810	44.858983
3500.938641	813136.860790	44.863988
3501.415838	813122.559647	44.868993
3501.375328	813136.597694	44.873997
3501.591252	813130.814875	44.879002
3501.306050	813110.591461	44.884007
3501.179079	813097.359130	44.889012
3501.304141	813083.600159	44.894017
3501.340169	813102.790794	44.899021
3501.275323	813087.697320	44.904026
3501.633476	813072.830015	44.909031
3501.216768	813069.094897	44.914036
3501.532886	813067.486415	44.919041
3501.486669	813065.837130	44.924045
3501.240085	813042.684160	44.929050
3501.464032	813031.345707	44.934055
3501.351287	813022.008744	44.939060
3501.584508	813012.227910	44.944065
3501.079064	813007.629629	44.949069
3501.203488	812997.768335	44.954074
3501.199768	812997.671498	44.959079
3501.309563	812993.464252	44.964084
3501.311918	812990.832911	44.969089
3501.364778	812993.845450	44.974093
3501.134121	812973.807956	44.979098
3501.148731	812961.527653	44.984103
3501.250748	812961.511732	44.989108
3501.204398	812952.261731	44.994113
3501.414571	812958.855162	44.999117
3501.671102	812952.286272	45.004122
3501.534568	812935.449627	45.009127
3501.417351	812928.062130	45.014132
3501.283139	812917.948805	45.019137
3501.308034	812913.072659	45.024141
3501.273167	812891.347718	45.029146
3500.993381	812886.519180	45.034151
3500.680072	812887.542643	45.039156
3501.306845	812886.177892	45.044161
3501.033895	812888.656737	45.049165
3501.152851	812896.726182	45.054170
3501.390335	812894.155490	45.059175
3501.383345	812873.498036	45.064180
3501.186042	812861.932788	45.069185
3501.383545	812864.143208	45.074189
3501.193900	812862.613737	45.079194
3501.459229	812851.560830	45.084199
3501.280995	812851.686164	45.089204
3501.362394	812836.959012	45.094209
3500.966176	812837.703103	45.099213
3501.510142	812833.232987	45.104218
3501.347877	812839.884763	45.109223
3501.348058	812830.237522	45.114228
3501.522394	812801.853174	45.119233
3501.362454	812812.597403	45.124237
3501.614672	812799.792405	45.129242
3501.368992	812788.819270	45.134247
3501.220950	812770.522267	45.139252
3501.365679	812759.390603	45.144257
3501.298278	812762.519501	45.149261
3501.012702	812764.025888	45.154266
3501.272712	812767.980634	45.159271
3501.193196	812754.252921	45.164276
3501.133510	812732.336414	45.169281
3501.072804	812740.434146	45.174285
3501.402918	812733.561181	45.179290
3501.605574	812733.334631	45.184295
3501.247022	812719.065769	45.189300
3501.006460	812696.982516	45.194305
3500.856628	812704.996777	45.199309
3501.175083	812699.587331	45.204314
3501.116046	812696.478218	45.209319
3500.980398	812703.223426	45.214324
3501.043376	812696.489630	45.219329
3501.033952	812709.549282	45.224333
3501.007862	812696.495233	45.229338
3501.172205	812689.843032	45.234343
3500.751615	812685.133797	45.239348
3501.360794	812660.383903	45.244353
3500.971803	812667.656000	45.249357
3500.765058	812667.980693	45.254362
3501.208621	812668.496077	45.259367
3501.055891	812665.693944	45.264372
3501.051691	812662.186443	45.269377
3501.034786	812676.221830	45.274381
3501.133842	812675.134429	45.279386
3501.261792	812677.453237	45.284391
3501.218903	812660.406316	45.289396
3500.979491	812648.262559	45.294401
3500.971307	812645.730170	45.299405
3501.537955	812641.353824	45.304410
3501.173938	812642.385252	45.309415
3501.154858	812649.404646	45.314420
3501.180925	812641.312264	45.319425
3501.596879	812624.485868	45.324429
3501.053846	812617.262018	45.329434
3501.184088	812614.123275	45.334439
3501.083475	812611.118070	45.339444
3501.052015	812614.923575	45.344449
3500.969719	812608.504744	45.349453
3501.100823	812612.382290	45.354458
3501.194369	812595.216414	45.359463
3501.171694	812572.708860	45.364468
3501.311402	812572.492144	45.369473
3500.969621	812579.756963	45.374477
3500.981492	812579.950035	45.379482
3500.952461	812583.267926	45.384487
3500.975714	812572.934527	45.389492
3501.283035	812574.932981	45.394497
3501.373876	812578.037234	45.399501
3501.040939	812552.752034	45.404506
3501.574034	812542.923594	45.409511
3500.843497	812549.664510	45.414516
3501.535018	812545.560932	45.419521
3501.316262	812555.047928	45.424525
3501.251234	812532.449399	45.429530
3500.912638	812522.854644	45.434535
3500.673893	812518.993921	45.439540
3501.519819	812514.671283	45.444545
3501.214897	812525.146312	45.449549
3500.839139	812519.065619	45.454554
3501.104298	812522.337554	45.459559
3500.970459	812521.968695	45.464564
3500.962553	812527.622154	45.469569
3501.312903	812531.855282	45.474573
3500.989867	812511.246040	45.479578
3501.107257	812496.220108	45.484583
3501.287322	812499.213000	45.489588
3501.100509	812488.522492	45.494593
3501.284054	812502.039672	45.499597
3501.098703	812488.425374	45.504602
3501.090871	812478.194131	45.509607
3500.862141	812468.289760	45.514612
3501.086875	812451.005530	45.519617
3500.778841	812464.209825	45.524621
3500.651407	812467.640612	45.529626
3500.965199	812461.939334	45.534631
3500.511602	812474.289289	45.539636
3500.924325	812472.665558	45.544641
3500.903471	812465.749714	45.549645
3500.828441	812471.023906	45.554650
3501.254952	812473.296119	45.559655
3500.892681	812476.958516	45.564660
3501.269720	812466.277280	45.569665
3501.458042	812469.366349	45.574669
3500.849452	812454.258897	45.579674
3500.957410	812444.984027	45.584679
3500.773007	812446.084861	45.589684
3501.042065	812441.559992	45.594689
3501.005448	812450.433956	45.599693
3501.010592	812435.230518	45.604698
3501.027855	812435.130392	45.609703
3501.128258	812441.838981	45.614708
3500.963372	812447.614504	45.619713
3500.457390	812446.719097	45.624717
3500.889779	812447.723513	45.629722
3501.227522	812438.705072	45.634727
3501.063734	812456.272218	45.639732
3501.113798	812446.519137	45.644737
3500.898936	812450.840676	45.649741
3500.765355	812441.213747	45.654746
3501.178498	812420.391672	45.659751
3501.097890	812421.086472	45.664756
3501.190847	812407.720853	45.669761
3501.308598	812409.456634	45.674765
3501.524664	812406.012012	45.679770
3501.326716	812402.729561	45.684775
3500.848434	812391.889544	45.689780
3501.176958	812377.707407	45.694785
3501.268974	812374.964337	45.699789
3501.167242	812373.323548	45.704794
3501.318834	812382.558002	45.709799
3501.202758	812390.372479	45.714804
3501.302283	812369.989078	45.719809
3501.230967	812361.716650	45.724813
3500.893913	812359.527918	45.729818
3501.330092	812359.947031	45.734823
3501.207167	812338.623760	45.739828
3501.349206	812280.420940	45.744833
3501.244736	812172.358259	45.749837
3500.999057	812016.268415	45.754842
3500.611144	811815.949034	45.759847
3500.471621	811560.321107	45.764852
3500.477940	811259.530956	45.769857
3500.226497	810908.663902	45.774861
3499.611028	810506.948333	45.779866
3499.472136	810054.243135	45.784871
3499.000985	809556.221186	45.789876
3498.419897	809006.206633	45.794881
3498.028824	808414.475691	45.799885
3497.679246	807780.844908	45.804890
3497.006537	807094.142237	45.809895
3496.235843	806357.778265	45.814900
3496.009334	805576.806096	45.819905
3494.911571	804748.064564	45.824909
3493.897144	803855.821163	45.829914
3493.409519	802937.116774	45.834919
3492.139103	801971.206906	45.839924
3491.497603	800963.414663	45.844929
3490.932552	799903.261440	45.849933
3490.040275	798791.273212	45.854938
3488.879183	797622.530533	45.859943
3487.702454	796427.396479	45.864948
3486.906359	795167.685766	45.869953
3485.500366	793877.821820	45.874957
3484.316340	792541.772088	45.879962
3483.236445	791160.945280	45.884967
3481.816883	789737.486054	45.889972
3480.851324	788265.276636	45.894977
3479.459272	786744.912386	45.899981
3477.826018	785190.424857	45.904986
3476.800768	783581.591493	45.909991
3475.646162	781943.065748	45.914996
3474.201512	780236.999732	45.920001
3472.469853	778510.659118	45.925005
3470.681834	776738.027176	45.930010
3469.828000	774928.127869	45.935015
3467.754167	773073.476007	45.940020
3466.061457	771175.944243	45.945025
3464.569763	769242.639343	45.950029
3462.504632	767276.402092	45.955034
3461.244731	765253.680144	45.960039
3459.277561	763221.004936	45.965044
3457.421204	761120.593248	45.970049
3455.524763	759005.165835	45.975053
3453.660680	756839.078079	45.980058
3451.670300	754646.886702	45.985063
3449.833045	752419.431638	45.990068
3447.717415	750141.455567	45.995073
3445.376796	747843.407997	46.000077
3443.255631	745512.900976	46.005082
3441.567791	743152.975300	46.010087
3439.507770	740741.424635	46.015092
3437.044452	738302.936547	46.020097
3434.669311	735835.884445	46.025101
3432.879393	733326.561650	46.030106
3430.491268	730793.064864	46.035111
3427.702062	728227.402050	46.040116
3425.486712	725633.439532	46.045121
3423.195182	723015.451282	46.050125
3420.809648	720367.149902	46.055130
3418.618257	717680.166259	46.060135
3416.195819	714961.746933	46.065140
3413.544850	712218.241394	46.070145
3411.200633	709446.727450	46.075149
3408.589387	706643.265190	46.080154
3406.079471	703813.757429	46.085159
3403.638030	700953.139545	46.090164
3401.008609	698075.488984	46.095169
3398.256583	695154.035016	46.100173
3395.395508	692222.829429	46.105178
3393.006014	689256.249161	46.110183
3390.018629	686265.241984	46.115188
3387.213906	683247.137616	46.120193
3384.536138	680210.261045	46.125197
3381.632969	677151.776334	46.130202
3378.734668	674063.637325	46.135207
3375.832535	670966.737297	46.140212
3372.902665	667845.126763	46.145217
3369.897148	664684.577249	46.150221
3366.902845	661514.882418	46.155226
3364.391242	658323.232086	46.160231
3361.386901	655113.696697	46.165236
3358.285444	651867.136798	46.170241
3355.645267	648611.724321	46.175245
3352.184492	645318.265531	46.180250
3349.071641	642017.348436	46.185255
3346.229172	638704.201586	46.190260
3342.858690	635372.264341	46.195265
3339.763235	632018.807652	46.200269
3336.399830	628641.708755	46.205274
3333.857714	625246.425494	46.210279
3330.469372	621834.909165	46.215284
3327.315130	618415.578826	46.220289
3324.392497	614967.197138	46.225293
3320.922221	611498.417157	46.230298
3317.766128	608020.548183	46.235303
3313.958586	604542.249224	46.240308
3311.089071	601032.103721	46.245313
3307.799306	597512.282515	46.250317
3304.114516	593975.171968	46.255322
3301.167000	590426.952656	46.260327
3298.067862	586862.653642	46.265332
3294.717150	583286.648791	46.270337
3291.215304	579698.873618	46.275341
3287.609583	576088.637524	46.280346
3284.440008	572459.209483	46.285351
3280.655176	568820.988601	46.290356
3277.298401	565171.004883	46.295361
3274.067023	561515.737084	46.300365
3270.580610	557866.256295	46.305370
3267.272952	554182.458278	46.310375
3263.300475	550487.029571	46.315380
3259.932951	546800.392863	46.320385
3256.758651	543099.344038	46.325389
3253.067067	539386.662026	46.330394
3249.630697	535656.038721	46.335399
3245.903563	531926.840829	46.340404
3242.752271	528178.098453	46.345409
3238.818932	524419.391318	46.350413
3235.294924	520661.725481	46.355418
3231.825522	516889.344775	46.360423
3227.991480	513104.787400	46.365428
3224.634421	509317.659498	46.370433
3221.170289	505531.142031	46.375437
3217.093008	501731.301666	46.380442
3213.583243	497929.263384	46.385447
3210.182515	494131.018507	46.390452
3206.469209	490313.421640	46.395457
3202.896877	486482.867052	46.400461
3198.824616	482653.505304	46.405466
3195.429708	478812.382593	46.410471
3191.602415	474976.106584	46.415476
3187.589916	471134.545061	46.420481
3184.016724	467282.655476	46.425485
3179.935091	463443.001808	46.430490
3176.394938	459579.673083	46.435495
3172.224274	455746.847315	46.440500
3169.055196	451885.083146	46.445505
3165.284322	448021.712837	46.450509
3161.453095	444176.414317	46.455514
3157.614085	440307.724441	46.460519
3154.038339	436445.692452	46.465524
3149.914084	432566.345777	46.470529
3146.243257	428708.402985	46.475533
3142.430328	424847.147116	46.480538
3138.367733	420976.219801	46.485543
3134.533441	417113.810352	46.490548
3130.467062	413247.584566	46.495553
3126.829409	409367.458715	46.500557
3122.877651	405514.144191	46.505562
3119.149687	401649.527843	46.510567
3115.269298	397787.481851	46.515572
3111.085741	393924.340137	46.520577
3107.108776	390070.342919	46.525581
3102.916542	386221.715985	46.530586
3099.393865	382369.983901	46.535591
3095.345698	378518.063863	46.540596
3091.320489	374674.596266	46.545601
3087.760274	370832.518708	46.550605
3083.281382	367004.333556	46.555610
3079.307435	363164.758614	46.560615
3075.350015	359346.484536	46.565620
3071.316400	355518.769179	46.570625
3067.706808	351697.558757	46.575629
3063.305305	347888.855890	46.580634
3059.690371	344091.109736	46.585639
3055.629472	340289.553511	46.590644
3051.734613	336481.331970	46.595649
3047.398033	332688.780118	46.600653
3043.083894	328907.468766	46.605658
3038.976465	325128.787807	46.610663
3034.858264	321358.026016	46.615668
3031.128932	317598.520135	46.620673
3027.104440	313833.548964	46.625677
3022.685687	310099.273824	46.630682
3018.806974	306357.955984	46.635687
3014.837901	302625.993519	46.640692
3010.724551	298906.667554	46.645697
3006.435328	295203.943624	46.650701
3002.267985	291512.216192	46.655706
2998.379985	287807.545676	46.660711
2993.994537	284131.840638	46.665716
2990.030055	280459.642223	46.670721
2985.745791	276796.553021	46.675725
2981.496515	273162.263840	46.680730
2977.255727	269513.940402	46.685735
2973.480737	265887.374460	46.690740
2969.153800	262273.470175	46.695745
2964.758772	258673.259758	46.700749
2960.449829	255082.402546	46.705754
2956.191549	251495.950156	46.710759
2951.882100	247929.414322	46.715764
2947.622353	244385.745931	46.720769
2943.587850	240851.788044	46.725773
2939.212336	237343.456443	46.730778
2935.144995	233826.150848	46.735783
2930.983331	230331.449717	46.740788
2926.312128	226857.238492	46.745793
2922.521565	223391.696318	46.750797
2917.488369	219948.969613	46.755802
2913.880979	216513.038457	46.760807
2909.405940	213103.296375	46.765812
2905.203124	209697.161999	46.770817
2901.258070	206307.839540	46.775821
2896.481682	202941.034588	46.780826
2892.462200	199581.023001	46.785831
2888.310404	196241.271691	46.790836
2883.486785	192921.210692	46.795841
2879.229864	189606.036812	46.800845
2875.055958	186318.421130	46.805850
2870.533773	183038.168322	46.810855
2865.980437	179785.734198	46.815860
2862.088762	176544.847728	46.820865
2858.034917	173328.247871	46.825869
2853.568939	170099.660765	46.830874
2849.672959	166847.346220	46.835879
2845.143038	163675.904697	46.840884
2840.883582	160530.511576	46.845889
2836.890816	157393.429276	46.850893
2832.357259	154264.166789	46.855898
2828.319699	151148.498601	46.860903
2823.999090	148062.216590	46.865908
2819.753720	144987.643414	46.870913
2815.631211	141928.733800	46.875917
2811.020644	138894.162764	46.880922
2806.908888	135860.471267	46.885927
2802.728133	132861.504442	46.890932
2798.346192	129872.744946	46.895937
2794.575924	126900.073770	46.900941
2789.899907	123940.551653	46.905946
2786.023795	121002.601598	46.910951
2781.351810	118081.769465	46.915956
2777.069650	115175.138239	46.920961
2773.021915	112287.185161	46.925965
2768.424212	109415.377291	46.930970
2764.413036	106567.980096	46.935975
2760.199852	103731.629595	46.940980
2755.723850	100914.879693	46.945985
2751.407604	98126.040404	46.950989
2747.200166	95351.278506	46.955994
2743.029023	92593.809182	46.960999
2738.573985	89847.685868	46.966004
2734.535736	87126.839993	46.971009
2730.429880	84419.696087	46.976013
2725.526507	81744.800850	46.981018
2721.588055	79072.216776	46.986023
2717.090049	76423.954375	46.991028
2713.119748	73805.162105	46.996033
2708.449574	71191.330977	47.001037
2703.929692	68605.114738	47.006042
2699.874652	66040.081044	47.011047
2695.340659	63499.199791	47.016052
2690.850515	60964.844956	47.021057
2686.772673	58461.886668	47.026061
2682.599298	55974.593328	47.031066
2677.988521	53508.454552	47.036071
2673.282574	51071.229452	47.041076
2668.966489	48653.690205	47.046081
2664.786022	46248.650042	47.051085
2660.433745	43887.522519	47.056090
2655.794435	41519.073520	47.061095
2651.071439	39187.887451	47.066100
2647.177208	36873.107632	47.071105
2642.666674	34585.315823	47.076109
2637.535674	32339.890139	47.081114
2633.501038	30098.056727	47.086119
2629.014974	27894.342170	47.091124
2624.754122	25702.956633	47.096129
2619.988051	23537.374809	47.101133
2615.058246	21404.024540	47.106138
2610.789792	19289.530391	47.111143
2606.176649	17209.284577	47.116148
2601.623373	15163.443194	47.121153
2596.566395	13141.390567	47.126157
2591.520949	11163.535944	47.131162
2586.496949	9212.649064	47.136167
2581.159064	7300.616613	47.141172
2574.249142	5470.432401	47.146177
2562.740792	3810.254813	47.151181
2547.890832	2342.704190	47.156186
2532.900786	1020.260678	47.161191
2504.040182	226.880722	47.166196
2455.871311	238.215801	47.171201
2427.581324	249.772836	47.176205
2418.378078	249.801504	47.181210
2423.411377	239.218713	47.186215
2433.001868	244.821365	47.191220
2443.209311	235.912810	47.196225
2450.582258	235.642167	47.201229
2453.395806	240.656606	47.206234
2453.431520	238.176880	47.211239
2451.357424	237.555364	47.216244
2448.288287	239.804130	47.221249
2445.225559	233.664412	47.226253
2441.472234	240.879952	47.231258
2438.024328	231.446766	47.236263
2435.252464	218.813544	47.241268
2432.003971	226.756899	47.246273
2429.664007	223.297839	47.251277
2426.846772	231.274976	47.256282
2424.101148	224.636389	47.261287
2421.033954	227.242376	47.266292
2417.827281	225.785601	47.271297
2415.165638	212.938986	47.276301
2411.238482	225.832428	47.281306
2408.388976	216.334124	47.286311
2405.073886	216.726206	47.291316
2401.213669	219.415127	47.296321
2399.042510	227.218425	47.301325
2395.729433	222.133502	47.306330
2392.208062	216.941955	47.311335
2388.805823	224.542359	47.316340
2385.689669	219.265275	47.321345
2382.578399	212.990804	47.326349
2378.891851	221.660787	47.331354
2375.808169	216.843718	47.336359
2372.529717	210.943433	47.341364
2368.930239	215.986636	47.346369
2365.787406	211.678720	47.351373
2362.315292	214.866945	47.356378
2359.089204	212.302702	47.361383
2355.850547	208.057239	47.366388
2352.160688	212.972210	47.371393
2348.836197	208.708539	47.376397
2345.149249	210.642676	47.381402
2341.780072	209.154398	47.386407
2338.265665	211.754436	47.391412
2335.446935	214.675927	47.396417
2331.750623	207.148351	47.401421
2328.101234	214.407765	47.406426
2324.818235	211.235479	47.411431
2321.868731	197.412008	47.416436
2318.612203	211.795141	47.421441
2315.619187	197.497570	47.426445
2310.586035	215.183328	47.431450
2307.613186	205.039945	47.436455
2304.600263	202.217736	47.441460
2300.989616	211.894630	47.446465
2298.153537	207.086309	47.451469
2293.495814	212.469107	47.456474
2290.114590	202.835730	47.461479
2286.820824	206.293477	47.466484
2283.331112	208.589098	47.471489
2280.630602	199.981898	47.476493
2277.073910	207.125576	47.481498
2273.740554	204.679387	47.486503
2270.526551	199.246805	47.491508
2266.421904	210.478527	47.496513
2263.552125	202.385052	47.501517
2259.529407	211.000083	47.506522
2256.190093	199.316295	47.511527
2253.224466	204.864660	47.516532
2249.203711	214.276687	47.521537
2245.987679	203.222209	47.526541
2242.174671	201.768600	47.531546
2238.669709	206.072520	47.536551
2234.993898	194.697665	47.541556
2231.735618	200.016563	47.546561
2228.363021	199.364123	47.551565
2225.216775	203.368304	47.556570
2221.514731	200.236304	47.561575
2218.407700	205.398661	47.566580
2214.390264	196.889953	47.571585
2211.244995	191.541557	47.576589
2207.124143	191.888915	47.581594
2204.226904	199.524242	47.586599
2200.644139	196.699468	47.591604
2197.113075	198.169482	47.596609
2194.000843	192.316029	47.601613
2190.381664	196.296133	47.606618
2186.928962	193.191577	47.611623
2183.356811	198.777903	47.616628
2180.029464	200.225541	47.621633
2176.488976	199.532943	47.626637
2172.580570	199.201643	47.631642
2169.191383	193.245992	47.636647
2165.679002	193.947434	47.641652
2162.377404	195.622012	47.646657
2159.100112	190.854296	47.651661
2155.277748	200.785817	47.656666
2151.754812	197.897913	47.661671
2148.722850	192.845032	47.666676
2144.938192	200.590745	47.671681
2142.192401	193.218262	47.676685
2138.082692	195.177480	47.681690
2134.799615	186.677304	47.686695
2131.059038	193.913064	47.691700
2127.438604	190.382339	47.696705
2123.976101	199.798799	47.701709
2120.562442	190.556563	47.706714
2117.294221	189.739125	47.711719
2113.851177	190.483520	47.716724
2110.185987	188.592364	47.721729
2106.771168	185.146539	47.726733
2103.522612	200.050492	47.731738
2099.877539	188.196309	47.736743
2096.331287	189.539012	47.741748
2092.533711	193.752709	47.746753
2089.268377	188.448452	47.751757
2085.596037	199.966929	47.756762
2082.217786	191.801213	47.761767
2078.776985	190.488750	47.766772
2075.289659	197.798801	47.771777
2071.840526	196.465496	47.776781
2068.371265	188.247586	47.781786
2064.759833	189.208178	47.786791
2061.326134	182.490713	47.791796
2057.935211	183.530703	47.796801
2054.009840	176.371301	47.801805
2050.609866	189.242430	47.806810
2047.053690	185.625747	47.811815
2043.738301	182.126420	47.816820
2040.573089	186.130449	47.821825
2037.363914	187.562802	47.826829
2033.695780	188.981546	47.831834
2030.101605	187.810161	47.836839
2026.623575	176.815765	47.841844
2022.703270	185.813477	47.846849
2019.324991	182.728975	47.851853
2015.377423	189.313758	47.856858
2012.292745	186.945810	47.861863
2009.244070	179.835913	47.866868
2005.516681	183.719102	47.871873
2002.344864	178.229396	47.876877
1998.793361	183.777736	47.881882
1994.955820	186.880869	47.886887
1991.511541	179.304515	47.891892
1987.535137	187.820616	47.896897
1984.566080	181.220308	47.901901
1981.061838	177.339251	47.906906
1977.743470	185.752387	47.911911
1974.540408	184.649540	47.916916
1970.600478	191.479925	47.921921
1967.161568	185.218908	47.926925
1963.421776	176.382129	47.931930
1959.702739	180.330466	47.936935
1956.478494	175.342545	47.941940
1952.847787	188.313076	47.946945
1949.710084	175.525329	47.951949
1946.400694	180.390368	47.956954
1942.759895	185.728063	47.961959
1939.018529	177.866012	47.966964
1935.198942	172.344813	47.971969
1932.606524	178.154394	47.976973
1928.516910	183.081416	47.981978
1924.771701	181.674266	47.986983
1921.597454	170.891818	47.991988
1918.060184	183.158009	47.996993
1914.996032	180.249022	48.001997
1911.312706	181.613234	48.007002
1907.457015	181.286438	48.012007
1903.794323	171.966206	48.017012
1900.346615	177.235729	48.022017
1896.990825	184.174049	48.027021
1893.621918	188.864913	48.032026
1890.256040	182.405830	48.037031
1887.000352	184.373870	48.042036
1882.960767	188.454655	48.047041
1879.370693	184.172599	48.052045
1876.261742	183.624552	48.057050
1872.581688	175.892146	48.062055
1869.138733	167.470885	48.067060
1865.631461	175.192242	48.072065
1862.097975	172.227000	48.077069
1858.424119	185.071421	48.082074
1855.252577	174.766318	48.087079
1851.863752	172.980710	48.092084
1847.839930	175.024673	48.097089
1844.791508	172.135395	48.102093
1840.912297	171.037158	48.107098
1837.635317	175.099859	48.112103
1834.396851	168.057696	48.117108
1830.390741	174.746610	48.122113
1827.120551	167.722069	48.127117
1823.682818	171.990271	48.132122
1820.146603	175.017831	48.137127
1817.080395	170.394384	48.142132
1813.341526	175.836050	48.147137
1809.648308	179.736100	48.152141
1806.050875	179.672658	48.157146
1802.478982	172.382116	48.162151
1799.155980	170.098991	48.167156
1795.222537	180.427646	48.172161
1792.518096	166.493289	48.177165
1788.754110	170.651201	48.182170
1784.924556	178.366067	48.187175
1781.911822	171.288595	48.192180
1778.032870	170.250456	48.197185
1774.723054	162.279816	48.202189
1771.194436	174.263097	48.207194
1767.596588	172.877238	48.212199
1764.140007	170.460000	48.217204
1760.457981	180.103890	48.222209
1757.473659	172.743560	48.227213
1753.890239	167.644238	48.232218
1750.197682	167.972202	48.237223
1746.851319	169.043281	48.242228
1742.660360	165.681088	48.247233
1739.462167	165.415978	48.252237
1736.325937	165.542982	48.257242
1732.586397	169.127590	48.262247
1729.138663	159.688375	48.267252
1725.555892	170.702507	48.272257
1722.252568	165.682752	48.277261
1718.912146	161.817288	48.282266
1715.105114	161.647471	48.287271
1711.392906	164.987355	48.292276
1707.719416	164.594153	48.297281
1704.740156	155.530900	48.302285
1701.201353	159.068282	48.307290
1697.575193	155.250710	48.312295
1694.349049	154.702078	48.317300
1690.559556	160.588314	48.322305
1687.418347	154.821844	48.327309
1684.015534	157.417265	48.332314
1679.664055	159.987148	48.337319
1676.608125	157.073790	48.342324
1673.096394	168.858289	48.347329
1669.660918	164.548958	48.352333
1666.378921	167.093839	48.357338
1662.362846	165.048951	48.362343
1659.375786	155.569306	48.367348
1655.344067	166.476541	48.372353
1652.027525	158.516495	48.377357
1648.648780	162.145906	48.382362
1645.130320	171.881286	48.387367
1641.651713	160.868172	48.392372
1638.191917	160.371946	48.397377
1634.383638	152.643901	48.402381
1630.669789	162.118786	48.407386
1627.446455	161.468491	48.412391
1624.476310	163.281182	48.417396
1620.954322	170.501854	48.422401
1617.237476	152.704765	48.427405
1613.532352	161.776479	48.432410
1609.960516	158.754058	48.437415
1606.273364	161.985647	48.442420
1602.827028	165.584521	48.447425
1599.912829	161.744142	48.452429
1596.383477	157.269194	48.457434
1591.979580	162.340434	48.462439
1588.717783	159.358083	48.467444
1585.515716	158.989221	48.472449
1582.445234	161.111866	48.477453
1578.834767	147.749698	48.482458
1575.213104	162.528609	48.487463
1571.990677	153.987536	48.492468
1568.308112	158.034694	48.497473
1564.824968	151.733311	48.502477
1560.833926	159.308993	48.507482
1557.403466	160.330017	48.512487
1554.172083	155.982461	48.517492
1550.367961	158.137683	48.522497
1546.856166	152.223617	48.527501
1543.287694	149.944202	48.532506
1539.736823	159.286031	48.537511
1536.627730	154.789621	48.542516
1533.249593	161.794804	48.547521
1529.760926	153.440957	48.552525
1526.045315	150.263897	48.557530
1522.539732	163.445889	48.562535
1519.235638	145.615892	48.567540
1515.528356	152.530222	48.572545
1512.053023	146.208656	48.577549
1508.753309	155.840220	48.582554
1504.521946	148.561283	48.587559
1501.571206	153.968269	48.592564
1497.788327	158.360193	48.597569
1494.909535	156.678382	48.602573
1490.958079	159.954544	48.607578
1487.369397	154.615702	48.612583
1484.122560	151.355792	48.617588
1480.749492	155.544365	48.622593
1477.146552	143.193504	48.627597
1473.934661	146.012213	48.632602
1470.246703	153.065905	48.637607
1466.883526	144.837983	48.642612
1462.661124	152.465729	48.647617
1459.393734	154.774259	48.652621
1455.881303	142.396585	48.657626
1452.022673	143.908621	48.662631
1449.405314	146.665914	48.667636
1445.403597	149.753800	48.672641
1441.899751	149.637872	48.677645
1438.754578	154.097679	48.682650
1435.108713	155.579581	48.687655
1431.823815	146.228908	48.692660
1427.923594	157.479466	48.697665
1424.672640	156.532995	48.702669
1421.307296	155.844884	48.707674
1417.336483	144.450167	48.712679
1413.913326	147.263998	48.717684
1409.985928	153.472475	48.722689
1406.612615	140.244120	48.727693
1403.616338	152.210588	48.732698
1399.845289	144.283828	48.737703
1396.801144	141.988835	48.742708
1393.000929	147.702830	48.747713
1389.655270	146.698428	48.752717
1386.179508	151.064460	48.757722
1382.100212	159.217182	48.762727
1379.167725	144.556213	48.767732
1375.310193	150.184271	48.772737
1371.954316	148.583507	48.777741
1368.672348	151.796044	48.782746
1364.952947	151.160211	48.787751
1361.648040	139.983999	48.792756
1357.849563	147.399883	48.797761
1353.989277	154.145219	48.802765
1351.337085	151.706623	48.807770
1347.396194	152.709540	48.812775
1343.942739	154.923842	48.817780
1340.385469	151.035514	48.822785
1336.934847	148.247332	48.827789
1333.660722	143.365531	48.832794
1329.808434	155.320479	48.837799
1326.607231	141.758324	48.842804
1323.109399	145.729186	48.847809
1319.386664	140.873323	48.852813
1315.661030	153.612064	48.857818
1312.310428	151.605522	48.862823
1308.920439	147.276558	48.867828
1305.308580	146.222105	48.872833
1301.691038	141.973060	48.877837
1298.380087	134.113534	48.882842
1294.512383	138.047389	48.887847
1291.463543	149.107755	48.892852
1288.034592	153.852480	48.897857
1284.548475	149.519589	48.902861
1281.087904	146.903833	48.907866
1277.381214	143.434404	48.912871
1274.454551	148.176433	48.917876
1270.334586	160.451723	48.922881
1266.918686	159.230562	48.927885
1263.597419	148.936496	48.932890
1259.333761	148.037884	48.937895
1256.317293	140.303120	48.942900
1252.908639	139.305464	48.947905
1249.448879	142.609145	48.952909
1245.866263	134.377706	48.957914
1242.028339	146.355735	48.962919
1239.148861	139.343036	48.967924
1235.571702	144.307135	48.972929
1231.598638	141.970951	48.977933
1228.092877	151.638004	48.982938
1224.871844	145.495049	48.987943
1221.645719	134.094591	48.992948
1218.392093	152.324661	48.997953
1214.481731	141.388833	49.002957
1210.843187	139.595092	49.007962
1207.131454	146.152698	49.012967
1203.870370	140.038170	49.017972
1200.143868	145.300916	49.022977
1196.765077	137.382446	49.027981
1193.357129	139.535887	49.032986
1189.706089	147.941173	49.037991
1186.117404	139.688561	49.042996
1182.837260	154.230588	49.048001
1179.282805	138.192731	49.053005
1176.113144	140.482884	49.058010
1172.510898	137.813419	49.063015
1169.126933	142.446728	49.068020
1165.172371	147.979314	49.073025
1161.827420	140.435221	49.078029
1158.071758	135.622550	49.083034
1154.574899	137.328002	49.088039
1151.546092	144.835431	49.093044
1147.673666	143.448500	49.098049
1144.253347	143.920731	49.103053
1141.028173	138.768742	49.108058
1137.134137	147.335476	49.113063
1133.637223	134.329089	49.118068
1130.175810	140.638715	49.123073
1126.873614	145.401609	49.128077
1123.343621	143.233392	49.133082
1119.416632	150.625181	49.138087
1116.609447	145.309679	49.143092
1113.167475	138.343960	49.148097
1109.323089	146.624512	49.153101
1105.695022	149.185779	49.158106
1102.121596	156.512730	49.163111
1098.667581	147.365848	49.168116
1095.031115	139.054317	49.173121
1091.736666	147.577814	49.178125
1088.666121	138.589208	49.183130
1084.788633	137.193604	49.188135
1081.278058	143.378062	49.193140
1077.914803	144.122964	49.198145
1074.113875	145.338199	49.203149
1070.806110	137.592165	49.208154
1066.920358	148.657058	49.213159
1063.535765	136.895489	49.218164
1060.236578	138.652285	49.223169
1056.874235	139.561571	49.228173
1053.261035	139.703356	49.233178
1049.834068	144.552249	49.238183
1046.474027	138.611470	49.243188
1042.453891	138.968837	49.248193
1038.598807	147.580126	49.253197
1035.867131	141.863678	49.258202
1032.212142	149.545112	49.263207
1028.765713	142.260577	49.268212
1025.254542	143.370351	49.273217
1021.479644	136.327082	49.278221
1017.809894	143.852637	49.283226
1014.536331	145.444082	49.288231
1011.190888	143.389386	49.293236
1008.153117	143.741655	49.298241
1004.123967	142.072430	49.303245
1000.331837	134.481361	49.308250
996.954689	143.255118	49.313255
993.600328	141.932671	49.318260
990.131803	144.785382	49.323265
986.883782	136.289691	49.328269
983.726592	139.875123	49.333274
979.634640	144.457991	49.338279
976.187933	138.651035	49.343284
972.582738	141.601083	49.348289
968.903550	138.285668	49.353293
965.770306	130.759134	49.358298
962.085031	140.726453	49.363303
958.866634	132.526701	49.368308
954.877921	145.075767	49.373313
951.673521	135.845579	49.378317
948.285606	142.327255	49.383322
944.834493	142.516470	49.388327
941.089897	137.790747	49.393332
937.241092	144.578717	49.398337
933.812126	146.982316	49.403341
930.765929	143.216616	49.408346
927.045676	140.768212	49.413351
923.998180	129.887259	49.418356
920.251865	137.130596	49.423361
916.445797	137.698112	49.428365
912.923880	121.930565	49.433370
909.017603	134.368651	49.438375
906.058973	129.946994	49.443380
902.728386	133.654516	49.448385
899.030118	135.252387	49.453389
896.023890	132.774451	49.458394
892.123981	138.301741	49.463399
888.826709	136.616045	49.468404
885.081529	132.111907	49.473409
881.426794	140.394474	49.478413
877.918399	130.699380	49.483418
874.411239	144.517695	49.488423
871.316267	138.798078	49.493428
867.608083	134.651995	49.498433
864.080264	135.406921	49.503437
860.567031	131.249298	49.508442
856.716953	142.780079	49.513447
853.059504	138.550125	49.518452
850.043279	135.883940	49.523457
846.650181	132.425700	49.528461
843.190666	134.350047	49.533466
839.614587	149.302326	49.538471
836.071185	139.536796	49.543476
832.647657	138.367612	49.548481
829.052316	134.472801	49.553485
825.690511	129.892838	49.558490
822.182197	134.900077	49.563495
818.603273	136.033190	49.568500
814.628273	132.707215	49.573505
811.209893	134.897221	49.578509
807.797490	123.526121	49.583514
804.335317	134.682950	49.588519
800.861626	129.785151	49.593524
797.383930	132.585578	49.598529
794.235886	137.137767	49.603533
790.615288	135.578671	49.608538
786.713349	133.288494	49.613543
783.579012	126.701863	49.618548
780.101929	138.351429	49.623553
776.592753	134.604503	49.628557
773.429103	134.397579	49.633562
769.280337	134.019050	49.638567
765.937880	134.526681	49.643572
762.252605	134.961445	49.648577
759.030457	128.568912	49.653581
755.682000	131.077025	49.658586
752.059808	135.383931	49.663591
748.113251	130.351393	49.668596
744.913123	132.491424	49.673601
741.090143	128.262133	49.678605
738.093018	135.112953	49.683610
734.512616	141.757719	49.688615
730.458498	132.005782	49.693620
727.274743	132.112078	49.698625
724.120021	131.106489	49.703629
720.285582	131.637397	49.708634
717.174770	136.490670	49.713639
713.348898	137.811196	49.718644
709.825067	140.293005	49.723649
706.288747	140.315313	49.728653
703.158466	132.430907	49.733658
699.684525	131.529103	49.738663
695.806433	129.001110	49.743668
692.445956	125.357486	49.748673
688.764519	127.702629	49.753677
685.511616	129.626312	49.758682
681.844279	137.183235	49.763687
678.308877	129.896972	49.768692
674.986632	134.773878	49.773697
671.259493	130.558082	49.778701
667.585512	137.283965	49.783706
664.145551	140.698640	49.788711
660.825009	138.763566	49.793716
657.527290	129.181116	49.798721
653.816099	128.594903	49.803725
650.856240	130.251237	49.808730
646.885361	135.650524	49.813735
643.002648	133.645308	49.818740
640.041834	133.226326	49.823745
636.345517	128.508999	49.828749
632.688348	134.317915	49.833754
629.186269	138.321310	49.838759
625.541244	137.753219	49.843764
621.919457	132.169992	49.848769
618.004692	127.221125	49.853773
615.738035	130.091382	49.858778
612.156322	131.237666	49.863783
608.797879	131.501079	49.868788
605.160543	132.656076	49.873793
601.343477	132.260476	49.878797
597.667133	129.058674	49.883802
594.086496	137.310744	49.888807
590.771514	128.303681	49.893812
587.301368	133.608747	49.898817
584.010155	132.380970	49.903821
580.390411	134.118530	49.908826
576.059792	131.421014	49.913831
573.180169	123.820117	49.918836
569.969081	125.920792	49.923841
566.351778	130.600329	49.928845
562.874307	123.861881	49.933850
559.237853	132.242927	49.938855
555.504029	130.651039	49.943860
552.155088	125.433246	49.948865
548.880692	128.739768	49.953869
545.457422	134.268466	49.958874
541.434217	134.901781	49.963879
538.367539	122.881862	49.968884
534.470122	126.532746	49.973889
531.356121	124.173061	49.978893
527.734532	112.578594	49.983898
524.005739	119.746548	49.988903
520.631078	117.978198	49.993908
516.845355	124.822871	49.998913
513.275058	123.467987	50.003917
510.548252	122.259408	50.008922
506.770014	130.865162	50.013927
503.923339	124.337994	50.018932
499.943427	123.528173	50.023937
496.139785	123.114696	50.028941
492.686152	120.197604	50.033946
488.930133	122.041966	50.038951
485.498893	115.027390	50.043956
481.814673	119.809186	50.048961
478.420226	121.188787	50.053965
475.374521	123.798275	50.058970
471.695981	128.348229	50.063975
468.200764	117.395234	50.068980
464.821108	108.369893	50.073985
460.994879	118.558756	50.078989
457.882275	120.868674	50.083994
453.970995	127.011687	50.088999
450.700083	119.051340	50.094004
447.249827	114.833410	50.099009
443.841548	125.058059	50.104013
440.326747	114.256846	50.109018
436.532682	117.831468	50.114023
432.907002	120.674185	50.119028
429.606052	117.578177	50.124033
426.056366	123.079255	50.129037
422.666789	124.366363	50.134042
418.888324	121.715321	50.139047
416.022921	118.184092	50.144052
412.296040	126.791325	50.149057
408.359148	131.125501	50.154061
405.094463	121.034949	50.159066
401.352190	121.276302	50.164071
397.932219	126.146456	50.169076
394.860790	115.380221	50.174081
391.258707	119.636647	50.179085
388.079946	117.565575	50.184090
383.825663	117.842843	50.189095
380.509051	114.385470	50.194100
377.002578	114.975882	50.199105
373.284675	125.799556	50.204109
369.783166	116.502270	50.209114
366.810888	125.427922	50.214119
363.131707	123.678859	50.219124
359.612361	111.293328	50.224129
356.205750	120.549612	50.229133
352.678018	115.726914	50.234138
348.855379	120.052706	50.239143
345.461639	118.338035	50.244148
342.137337	111.556713	50.249153
338.229034	119.752617	50.254157
335.063998	114.290971	50.259162
331.259996	123.720247	50.264167
327.656672	121.168363	50.269172
324.556229	125.270303	50.274177
320.874711	119.237821	50.279181
317.620165	117.551977	50.284186
314.731192	120.254025	50.289191
310.601219	118.774922	50.294196
307.462428	118.659183	50.299201
303.384314	124.008960	50.304205
300.152908	118.526085	50.309210
296.056105	122.660724	50.314215
292.501223	121.857184	50.319220
289.416583	121.672856	50.324225
286.093334	116.612507	50.329229
282.717262	120.400127	50.334234
279.109182	121.398807	50.339239
275.650846	120.421959	50.344244
271.997998	118.181584	50.349249
268.158536	123.611051	50.354253
264.822188	110.874192	50.359258
261.525293	117.531647	50.364263
258.006986	120.882804	50.369268
254.632725	115.779838	50.374273
250.975759	118.472500	50.379277
247.148458	118.875936	50.384282
243.653134	113.725502	50.389287
240.250488	115.400709	50.394292
236.942492	118.016561	50.399297
233.452392	110.084323	50.404301
230.219657	109.986493	50.409306
226.553997	112.503352	50.414311
222.982744	110.218579	50.419316
219.763196	108.150798	50.424321
216.112551	121.624747	50.429325
212.359613	109.984580	50.434330
208.716070	114.253895	50.439335
205.408946	118.334466	50.444340
202.201238	113.996384	50.449345
198.186234	113.685753	50.454349
194.868711	109.494595	50.459354
191.436805	121.121421	50.464359
187.539492	112.025440	50.469364
184.300677	114.646291	50.474369
180.834474	121.573911	50.479373
177.564965	112.784549	50.484378
173.483613	113.458777	50.489383
170.057953	118.497581	50.494388
167.076673	119.448730	50.499393
162.961668	126.234388	50.504397
159.931989	118.331291	50.509402
156.464222	115.932255	50.514407
152.443425	121.137071	50.519412
149.412684	125.133233	50.524417
145.957782	123.358619	50.529421
142.620401	118.351165	50.534426
138.674223	128.410236	50.539431
135.163834	126.767708	50.544436
131.790242	117.469479	50.549441
128.079187	122.129060	50.554445
124.871264	119.037583	50.559450
121.497025	122.983163	50.564455
118.163957	118.130071	50.569460
114.612816	120.793551	50.574465
110.687611	128.463836	50.579469
107.211585	120.928088	50.584474
103.546240	125.482441	50.589479
99.953884	118.797004	50.594484
96.718401	106.702501	50.599489
93.392094	120.729958	50.604493
89.964145	118.764481	50.609498
86.345614	124.358725	50.614503
82.771337	116.493529	50.619508
79.600272	113.298218	50.624513
76.002466	118.180525	50.629517
72.292532	110.051848	50.634522
68.668788	108.696033	50.639527
65.086984	115.676603	50.644532
61.764874	113.798961	50.649537
57.985459	119.187464	50.654541
54.874803	110.376435	50.659546
51.102555	113.286556	50.664551
47.604291	115.653872	50.669556
44.204419	115.158348	50.674561
40.994256	112.222283	50.679565
37.566818	106.786055	50.684570
34.038354	111.236726	50.689575
30.306913	111.454393	50.694580
26.735742	109.520874	50.699585
23.108354	131.527189	50.704589
19.382927	120.563026	50.709594
15.903223	114.201673	50.714599
12.705547	108.039747	50.719604
9.318477	110.196662	50.724609
6.099137	120.970812	50.729613
2.121746	107.992836	50.734618