Thu Aug 25 17:21:59 2022

Number of Points = 9926

Depth (nm)	Load (N)	Time (s)
1.955703	97.797127	0.000000
1.531824	95.971615	0.005005
1.188874	106.744355	0.010010
1.388157	96.092262	0.015014
1.471127	107.345608	0.020019
1.864697	103.598137	0.025024
1.560377	87.535749	0.030029
1.443069	89.278432	0.035034
1.038749	68.723308	0.040038
0.748557	50.159337	0.045043
0.286164	41.464934	0.050048
0.483111	24.324304	0.055053
-0.375797	19.434806	0.060058
-0.311055	13.498910	0.065062
-1.069026	2.436864	0.070067
-0.975060	0.710562	0.075072
-1.199765	-12.564257	0.080077
-2.035286	-9.067047	0.085082
-2.023230	-17.136562	0.090086
-2.681907	-21.633474	0.095091
-3.790258	-17.489235	0.100096
-3.709156	-32.757680	0.105101
-3.390266	-22.566447	0.110106
-3.436816	-15.133719	0.115110
-3.355473	-21.657505	0.120115
-3.655185	-20.740475	0.125120
-4.139365	-30.042040	0.130125
-4.847964	-20.082125	0.135130
-4.408974	-31.227286	0.140134
-5.360337	-19.176038	0.145139
-6.430822	-17.777571	0.150144
-5.752956	-26.033660	0.155149
-6.080422	-20.240053	0.160154
-6.571502	-29.891717	0.165158
-6.618527	-24.939325	0.170163
-6.973019	-17.660832	0.175168
-6.467977	-35.393848	0.180173
-6.661236	-10.698673	0.185178
-7.075362	-22.121463	0.190182
-7.605914	-17.409688	0.195187
-8.265156	-18.594028	0.200192
-7.964830	-23.215887	0.205197
-8.248754	-19.314718	0.210202
-8.605024	-20.274442	0.215206
-8.940163	-22.942757	0.220211
-9.630344	-19.101322	0.225216
-9.282907	-26.543166	0.230221
-9.356387	-26.829019	0.235226
-9.849628	-22.698900	0.240230
-10.056823	-14.111531	0.245235
-10.751993	-9.940278	0.250240
-10.749034	-30.498987	0.255245
-11.076333	-16.226465	0.260250
-10.846603	-13.127118	0.265254
-11.266987	-19.524835	0.270259
-12.061845	-17.233072	0.275264
-12.041047	-18.327807	0.280269
-12.302220	-22.795250	0.285274
-12.364479	-23.848497	0.290278
-11.951329	-23.258297	0.295283
-13.815982	-16.088040	0.300288
-13.620027	-22.044482	0.305293
-13.691818	-19.483194	0.310298
-14.076123	-20.571404	0.315302
-14.112149	-19.376147	0.320307
-13.930277	-25.061460	0.325312
-13.942213	-28.489102	0.330317
-14.528080	-20.177765	0.335322
-14.877947	-26.627658	0.340326
-15.078690	-21.920102	0.345331
-15.525709	-22.236014	0.350336
-15.439076	-29.693942	0.355341
-15.836760	-15.388244	0.360346
-16.393438	-19.312672	0.365350
-16.562841	-28.362997	0.370355
-16.967329	-15.894392	0.375360
-16.840944	-21.324237	0.380365
-16.803354	-17.166556	0.385370
-17.745538	-24.425322	0.390374
-18.014136	-24.541397	0.395379
-18.264073	-14.346457	0.400384
-17.979971	-23.670322	0.405389
-18.295604	-15.967643	0.410394
-18.435584	-20.779944	0.415398
-18.693177	-28.098515	0.420403
-19.501414	-14.222041	0.425408
-19.817182	-22.980513	0.430413
-19.965495	-21.210836	0.435418
-19.785901	-24.924754	0.440422
-19.957563	-23.872762	0.445427
-20.388679	-25.288998	0.450432
-21.049177	-29.668560	0.455437
-21.592087	-23.980405	0.460442
-21.244268	-29.438615	0.465446
-21.191362	-18.367303	0.470451
-21.242520	-22.307661	0.475456
-21.304005	-19.327204	0.480461
-22.324596	-22.919513	0.485466
-22.757363	-28.533831	0.490470
-22.541852	-34.142154	0.495475
-22.938747	-29.539909	0.500480
-23.328876	-29.668579	0.505485
-23.526905	-16.213586	0.510490
-24.036454	-27.241764	0.515494
-24.313367	-25.300077	0.520499
-24.645108	-19.047052	0.525504
-24.158595	-26.846048	0.530509
-24.424254	-21.878382	0.535514
-24.378267	-26.365476	0.540518
-25.117442	-26.126242	0.545523
-25.503756	-18.858582	0.550528
-25.540629	-31.412997	0.555533
-25.855237	-29.813419	0.560538
-26.858320	-28.254666	0.565542
-26.963956	-28.794911	0.570547
-27.273588	-29.205115	0.575552
-27.427107	-31.598162	0.580557
-27.520734	-34.487814	0.585562
-27.524631	-34.037917	0.590566
-27.295746	-24.139472	0.595571
-27.589548	-26.599124	0.600576
-27.812853	-32.097562	0.605581
-28.381014	-26.288391	0.610586
-28.672093	-17.672063	0.615590
-28.756547	-32.253334	0.620595
-29.125227	-14.326487	0.625600
-29.538205	-26.448647	0.630605
-29.970946	-21.138424	0.635610
-30.280265	-26.885981	0.640614
-30.335976	-28.794474	0.645619
-30.758710	-20.325199	0.650624
-30.652904	-35.034356	0.655629
-30.683492	-29.046822	0.660634
-31.133433	-28.166365	0.665638
-31.314381	-26.116326	0.670643
-31.824982	-17.405490	0.675648
-31.974704	-30.176342	0.680653
-32.059394	-16.821367	0.685658
-32.355332	-17.999353	0.690662
-32.724059	-21.633685	0.695667
-32.861681	-18.267972	0.700672
-32.712391	-24.261395	0.705677
-33.402598	-19.983353	0.710682
-34.245444	-24.087568	0.715686
-34.347290	-30.911680	0.720691
-34.645838	-24.717642	0.725696
-34.616894	-28.591454	0.730701
-34.604497	-26.404029	0.735706
-34.613237	-24.422102	0.740710
-35.016553	-24.305094	0.745715
-35.948458	-20.191663	0.750720
-35.875867	-31.336361	0.755725
-36.145215	-29.686927	0.760730
-36.294961	-21.377486	0.765734
-36.148855	-31.733264	0.770739
-36.628769	-25.589904	0.775744
-37.032504	-19.692598	0.780749
-37.569377	-15.476545	0.785754
-37.709324	-22.902136	0.790758
-37.492130	-27.188262	0.795763
-37.930178	-18.953871	0.800768
-38.486621	-14.424701	0.805773
-38.762400	-21.145632	0.810778
-38.979264	-14.828347	0.815782
-38.870083	-25.567489	0.820787
-39.282544	-24.306922	0.825792
-39.323961	-26.265113	0.830797
-39.556366	-18.040796	0.835802
-40.121030	-20.230216	0.840806
-40.479788	-20.604249	0.845811
-40.546111	-24.238506	0.850816
-40.303036	-18.293847	0.855821
-40.850426	-21.988771	0.860826
-41.603432	-24.854204	0.865830
-41.756240	-28.433780	0.870835
-42.124212	-24.101824	0.875840
-42.344058	-22.324102	0.880845
-41.965591	-27.796606	0.885850
-42.430821	-25.461577	0.890854
-42.470985	-29.495405	0.895859
-43.613099	-19.799761	0.900864
-43.580303	-21.940424	0.905869
-43.563485	-26.236284	0.910874
-43.817555	-21.656416	0.915878
-43.595971	-27.012589	0.920883
-43.843325	-25.350782	0.925888
-44.061990	-25.288016	0.930893
-44.844297	-19.726866	0.935898
-45.215013	-20.624213	0.940902
-45.130150	-31.862582	0.945907
-45.497377	-17.637591	0.950912
-46.268697	-16.447347	0.955917
-46.523604	-20.267194	0.960922
-46.812592	-19.639747	0.965926
-46.762786	-26.841965	0.970931
-47.037931	-14.640402	0.975936
-46.894938	-27.153396	0.980941
-47.170511	-14.739793	0.985946
-47.036843	-22.116506	0.990950
-47.359993	-28.463012	0.995955
-48.274542	-21.188518	1.000960
-48.317554	-20.381311	1.005965
-48.515739	-14.930666	1.010970
-48.382946	-22.063630	1.015974
-48.977795	-18.534526	1.020979
-49.431562	-20.858382	1.025984
-49.699675	-14.991815	1.030989
-49.654410	-16.757942	1.035994
-49.989501	-19.809081	1.040998
-49.693583	-26.040614	1.046003
-50.872799	-18.427253	1.051008
-51.027698	-21.025729	1.056013
-51.477291	-11.093738	1.061018
-51.446063	-12.247055	1.066022
-51.076454	-10.118763	1.071027
-51.734973	-13.742491	1.076032
-52.050141	-19.090495	1.081037
-52.408625	-18.679951	1.086042
-52.741362	-11.411193	1.091046
-52.775217	-20.122085	1.096051
-52.990838	-12.827385	1.101056
-52.919078	-20.390553	1.106061
-53.611619	-17.738328	1.111066
-54.359597	-23.910702	1.116070
-54.158511	-18.971876	1.121075
-54.414928	-16.533520	1.126080
-54.066741	-20.270692	1.131085
-54.488487	-20.324804	1.136090
-55.423768	-16.353212	1.141094
-55.413942	-17.607581	1.146099
-56.000184	-13.016792	1.151104
-55.755808	-14.646437	1.156109
-55.517885	-21.818020	1.161114
-56.102908	-11.083354	1.166118
-56.489824	-22.225660	1.171123
-57.006043	-15.665315	1.176128
-57.246781	-18.405367	1.181133
-57.174030	-19.372200	1.186138
-57.473746	-15.705839	1.191142
-57.524663	-19.681036	1.196147
-58.265524	-13.670792	1.201152
-58.496774	-21.439583	1.206157
-58.533592	-19.288740	1.211162
-59.055791	-14.271384	1.216166
-58.953857	-25.768697	1.221171
-58.934591	-18.444364	1.226176
-59.850367	-18.259714	1.231181
-60.078431	-17.597520	1.236186
-60.110593	-20.038056	1.241190
-60.165842	-23.281739	1.246195
-60.599468	-15.209392	1.251200
-60.538919	-29.316668	1.256205
-61.050899	-26.063143	1.261210
-61.831016	-24.529831	1.266214
-61.661810	-22.132857	1.271219
-62.030813	-18.667614	1.276224
-61.676383	-17.970138	1.281229
-62.159265	-27.214952	1.286234
-62.741874	-16.980545	1.291238
-63.184610	-31.432907	1.296243
-63.616929	-21.671308	1.301248
-63.676368	-27.688971	1.306253
-63.612006	-24.538408	1.311258
-63.948469	-14.715895	1.316262
-63.527280	-20.552602	1.321267
-63.871254	-15.658087	1.326272
-64.748434	-25.904150	1.331277
-64.849074	-19.450053	1.336282
-65.365380	-22.966345	1.341286
-64.884873	-25.819407	1.346291
-65.764354	-15.582776	1.351296
-66.249968	-21.916481	1.356301
-66.444972	-25.366058	1.361306
-66.463708	-18.190796	1.366310
-66.233142	-29.980346	1.371315
-66.517995	-23.405637	1.376320
-66.610479	-24.251665	1.381325
-67.122775	-29.129011	1.386330
-67.919653	-28.991464	1.391334
-67.828888	-32.102998	1.396339
-68.102692	-28.102176	1.401344
-68.317246	-28.055873	1.406349
-68.512940	-26.259789	1.411354
-69.096642	-26.241067	1.416358
-69.258478	-27.164814	1.421363
-69.618739	-23.564899	1.426368
-69.403642	-26.518744	1.431373
-69.360516	-18.653980	1.436378
-69.998338	-22.575179	1.441382
-70.373770	-25.740217	1.446387
-71.161956	-23.009730	1.451392
-71.166905	-25.818364	1.456397
-71.008988	-16.731383	1.461402
-71.068399	-15.507151	1.466406
-71.057219	-14.967867	1.471411
-72.028613	-23.981110	1.476416
-72.230329	-28.150976	1.481421
-72.503777	-22.277249	1.486426
-72.531010	-19.555263	1.491430
-72.390595	-28.021370	1.496435
-73.383173	-11.812778	1.501440
-73.723787	-25.613585	1.506445
-73.655502	-27.313715	1.511450
-74.120177	-19.932537	1.516454
-73.828885	-22.347824	1.521459
-74.352322	-17.988342	1.526464
-74.653528	-28.878313	1.531469
-75.225324	-26.036198	1.536474
-75.447497	-21.461328	1.541478
-75.315994	-16.609677	1.546483
-75.260148	-20.674369	1.551488
-75.427414	-24.242187	1.556493
-75.467611	-23.476551	1.561498
-76.521877	-25.858173	1.566502
-76.573518	-19.364298	1.571507
-77.065164	-14.652289	1.576512
-76.985036	-21.166390	1.581517
-76.974809	-22.151899	1.586522
-77.778569	-13.958280	1.591526
-77.955896	-25.497256	1.596531
-78.457148	-24.305034	1.601536
-78.291624	-17.788237	1.606541
-78.559941	-23.232164	1.611546
-78.860676	-19.606774	1.616550
-79.229555	-27.907658	1.621555
-79.606009	-23.416183	1.626560
-79.797903	-28.125431	1.631565
-79.541584	-18.737492	1.636570
-79.949854	-13.459575	1.641574
-80.098683	-15.283875	1.646579
-80.920078	-25.203315	1.651584
-81.047762	-28.992472	1.656589
-81.066891	-27.891613	1.661594
-81.452248	-27.679339	1.666598
-80.961826	-28.778056	1.671603
-81.811847	-19.403428	1.676608
-82.418094	-23.978148	1.681613
-82.465823	-18.440347	1.686618
-82.792190	-18.019016	1.691622
-82.719321	-31.039877	1.696627
-82.764397	-12.578440	1.701632
-83.357663	-29.380051	1.706637
-83.829326	-21.058136	1.711642
-83.845547	-27.917808	1.716646
-84.017437	-20.506578	1.721651
-84.143650	-16.937007	1.726656
-84.758676	-15.091036	1.731661
-85.296000	-21.505223	1.736666
-85.531801	-10.028003	1.741670
-85.564438	-20.090020	1.746675
-85.709581	-18.551795	1.751680
-86.076997	-27.178778	1.756685
-85.535911	-24.102913	1.761690
-86.114342	-21.224956	1.766694
-86.522830	-22.989586	1.771699
-86.782793	-18.092416	1.776704
-87.073190	-22.678662	1.781709
-87.150867	-21.160500	1.786714
-87.773945	-12.413056	1.791718
-88.261026	-18.705401	1.796723
-88.368234	-20.969661	1.801728
-88.785604	-19.974080	1.806733
-88.634891	-25.249545	1.811738
-88.931118	-16.024965	1.816742
-88.511760	-22.598547	1.821747
-89.324417	-25.900721	1.826752
-89.717754	-20.419499	1.831757
-89.913627	-21.439154	1.836762
-90.453866	-22.211858	1.841766
-90.073817	-23.954511	1.846771
-90.124722	-16.568564	1.851776
-90.964750	-24.096427	1.856781
-91.269252	-24.266985	1.861786
-91.742923	-18.754193	1.866790
-91.744788	-20.221866	1.871795
-91.742462	-22.136289	1.876800
-91.909854	-24.780263	1.881805
-92.207716	-13.347106	1.886810
-92.715679	-17.101988	1.891814
-92.620957	-22.359189	1.896819
-93.022445	-24.371690	1.901824
-93.885408	-16.459863	1.906829
-94.023374	-19.826627	1.911834
-94.452017	-20.069483	1.916838
-94.655428	-22.517986	1.921843
-95.007057	-22.149644	1.926848
-94.562478	-26.857381	1.931853
-94.247377	-24.619311	1.936858
-94.755267	-25.507816	1.941862
-94.961384	-27.047889	1.946867
-95.773114	-13.705548	1.951872
-96.112127	-15.186832	1.956877
-95.780278	-23.499438	1.961882
-96.607146	-13.546298	1.966886
-96.282389	-19.687438	1.971891
-97.083645	-21.706902	1.976896
-97.705753	-26.845452	1.981901
-97.515319	-32.437189	1.986906
-98.193731	-24.696653	1.991910
-97.716559	-30.693991	1.996915
-97.854605	-26.755297	2.006912
-97.993737	-22.612087	2.016909
-97.951596	-23.461274	2.026906
-97.134415	-19.616798	2.036902
-96.602637	-19.627205	2.046899
-95.532528	-16.322878	2.056896
-95.152776	-13.781530	2.066893
-94.780998	-19.773079	2.076890
-94.850126	-15.194172	2.086886
-94.105718	-10.520989	2.096883
-93.389551	-17.222244	2.106880
-92.347574	-16.888104	2.116877
-92.028821	-10.881091	2.126874
-91.972627	-21.365865	2.136870
-91.980258	-17.373140	2.146867
-91.325314	-13.927730	2.156864
-90.304538	-14.122464	2.166861
-89.597027	-19.805487	2.176858
-89.388031	-14.829830	2.186854
-89.280892	-21.755604	2.196851
-88.262691	-12.269033	2.206848
-87.989201	-12.362513	2.216845
-87.375726	-13.789071	2.226842
-86.449578	-16.896056	2.236838
-86.308064	-18.907571	2.246835
-86.468375	-17.735636	2.256832
-85.604535	-18.846626	2.266829
-85.102907	-17.768908	2.276826
-84.414283	-24.294781	2.286822
-83.762880	-22.093777	2.296819
-83.468909	-16.748126	2.306816
-82.952790	-18.225953	2.316813
-82.300312	-21.169679	2.326810
-82.097078	-13.890103	2.336806
-81.269509	-16.943627	2.346803
-81.075264	-17.883173	2.356800
-80.485313	-15.387433	2.366797
-79.783162	-14.787799	2.376794
-79.610358	-22.024807	2.386790
-78.678789	-12.705227	2.396787
-78.404488	-16.543214	2.406784
-78.370185	-12.446183	2.416781
-77.155901	-15.940443	2.426778
-76.920763	-13.395442	2.436774
-76.247264	-10.447120	2.446771
-75.842365	-17.318182	2.456768
-75.416268	-11.172763	2.466765
-75.227136	-13.689090	2.476762
-74.110844	-12.523948	2.486758
-74.298622	-4.118707	2.496755
-73.358963	-12.860223	2.506752
-72.828889	-15.990678	2.516749
-72.324681	-22.582690	2.526746
-71.358225	-16.170312	2.536742
-71.121878	-12.808199	2.546739
-71.340464	-17.319733	2.556736
-70.245825	-24.995791	2.566733
-69.823543	-19.572043	2.576730
-69.542814	-23.997085	2.586726
-68.730480	-23.965918	2.596723
-68.466769	-21.843549	2.606720
-68.166168	-20.262324	2.616717
-66.852343	-18.668797	2.626714
-66.702652	-13.379734	2.636710
-66.907206	-13.319112	2.646707
-65.685470	-22.982312	2.656704
-65.307969	-16.468146	2.666701
-65.043628	-24.188337	2.676698
-64.097270	-22.397847	2.686694
-63.794779	-20.715547	2.696691
-63.610066	-20.386465	2.706688
-62.655139	-15.743098	2.716685
-62.392486	-21.369086	2.726682
-61.854077	-18.773401	2.736678
-61.101917	-19.683156	2.746675
-60.712446	-16.256336	2.756672
-60.760759	-21.757571	2.766669
-60.273433	-19.654400	2.776666
-59.051109	-19.028563	2.786662
-58.516061	-20.214746	2.796659
-57.994413	-15.864622	2.806656
-57.878165	-14.770867	2.816653
-57.781597	-18.349754	2.826650
-56.853419	-11.272464	2.836646
-56.489493	-16.879475	2.846643
-55.790664	-16.336340	2.856640
-55.034493	-17.918303	2.866637
-54.723621	-16.002896	2.876634
-54.639836	-25.585993	2.886630
-53.821894	-17.743824	2.896627
-53.477568	-25.381512	2.906624
-52.538331	-21.264715	2.916621
-52.028842	-22.633795	2.926618
-52.110169	-22.256692	2.936614
-51.868542	-20.168875	2.946611
-50.876620	-25.177360	2.956608
-50.050452	-21.080859	2.966605
-49.266003	-19.676817	2.976602
-49.084320	-23.997641	2.986598
-49.084744	-21.536108	2.996595
-48.727557	-20.508616	3.006592
-47.730202	-17.877134	3.016589
-47.289441	-22.463469	3.026586
-46.828737	-18.816558	3.036582
-46.503133	-18.411348	3.046579
-45.860578	-19.094850	3.056576
-45.282186	-13.457971	3.066573
-45.106644	-15.801105	3.076570
-44.059376	-13.503730	3.086566
-43.841012	-17.713093	3.096563
-43.435384	-21.612838	3.106560
-42.496699	-17.369239	3.116557
-42.176218	-19.377116	3.126554
-41.952988	-15.271673	3.136550
-41.527019	-17.958158	3.146547
-40.711803	-11.427040	3.156544
-40.426294	-13.084145	3.166541
-39.794994	-19.787939	3.176538
-39.100935	-19.034978	3.186534
-38.817919	-8.185074	3.196531
-37.795194	-17.310239	3.206528
-37.557313	-11.778396	3.216525
-37.496544	-15.057066	3.226522
-37.109317	-11.557031	3.236518
-36.132043	-13.541106	3.246515
-35.887508	-21.312049	3.256512
-35.302954	-14.405832	3.266509
-34.743323	-20.591543	3.276506
-34.550546	-17.643923	3.286502
-33.774921	-10.926035	3.296499
-33.517855	-17.545850	3.306496
-32.893320	-16.902372	3.316493
-31.969934	-21.915957	3.326490
-32.053394	-21.155212	3.336486
-30.875529	-18.688228	3.346483
-30.549759	-20.925019	3.356480
-30.348705	-17.338793	3.366477
-29.873241	-17.996114	3.376474
-28.879709	-16.548801	3.386470
-28.850629	-21.105478	3.396467
-28.678875	-20.140798	3.406464
-27.625514	-25.339474	3.416461
-27.315426	-15.966858	3.426458
-26.556579	-15.806929	3.436454
-25.863793	-18.642925	3.446451
-25.772084	-18.916998	3.456448
-25.679918	-16.669545	3.466445
-24.890408	-17.455267	3.476442
-24.328103	-12.601487	3.486438
-23.857947	-16.793281	3.496435
-23.016614	-15.084533	3.506432
-22.879491	-13.591733	3.516429
-22.195232	-18.254234	3.526426
-21.627802	-14.826784	3.536422
-21.419001	-14.900623	3.546419
-20.627074	-20.270582	3.556416
-20.110914	-17.630226	3.566413
-20.066842	-15.001432	3.576410
-19.258425	-16.176592	3.586406
-18.980744	-22.954860	3.596403
-17.785549	-14.598414	3.606400
-17.471758	-19.690716	3.616397
-17.288724	-19.136454	3.626394
-17.017448	-18.041646	3.636390
-15.961686	-16.958879	3.646387
-15.914986	-16.148835	3.656384
-15.474658	-13.924255	3.666381
-14.631659	-16.333954	3.676378
-14.058056	-21.128005	3.686374
-13.778647	-17.167579	3.696371
-12.704971	-14.066539	3.706368
-12.622707	-14.345468	3.716365
-12.393317	-14.327497	3.726362
-12.127516	-11.505359	3.736358
-11.304762	-8.631101	3.746355
-10.773115	-10.703744	3.756352
-9.863607	-13.317102	3.766349
-9.341231	-18.967947	3.776346
-9.450874	-20.002430	3.786342
-8.940820	-15.615638	3.796339
-8.316692	-9.060910	3.806336
-7.875750	-9.104596	3.816333
-7.022723	-14.100821	3.826330
-6.864984	-9.345210	3.836326
-6.522303	-3.215223	3.846323
-5.939605	1.565675	3.856320
-5.405245	6.772303	3.866317
-4.900482	8.226510	3.876314
-4.233453	22.250635	3.886310
-3.676758	18.032603	3.896307
-3.507255	26.768360	3.906304
-2.956599	37.424305	3.916301
-2.669146	50.896531	3.926298
-2.253599	63.854512	3.936294
-1.641147	73.179803	3.946291
-1.136836	82.002514	3.956288
-0.702754	98.290199	3.966285
-0.199740	107.562962	3.976282
0.000000	122.029704	3.981286
0.416005	133.056876	3.986291
0.364303	136.200345	3.991296
0.569127	140.429939	3.996301
0.862783	157.329352	4.001306
0.881337	167.593063	4.006310
0.948927	165.187492	4.011315
1.287165	164.808653	4.016320
1.535024	160.647393	4.021325
0.903523	169.367771	4.026330
1.270297	163.201001	4.031334
1.325918	161.559786	4.036339
1.105402	171.016217	4.041344
0.734639	158.880984	4.046349
0.865724	163.599873	4.051354
0.877622	168.078005	4.056358
0.945653	172.515705	4.061363
1.096629	171.786548	4.066368
1.077019	167.395106	4.071373
1.044953	160.449252	4.076378
1.050568	171.914079	4.081382
1.314118	168.130018	4.086387
0.891330	170.777966	4.091392
0.941010	174.579450	4.096397
1.206338	189.341427	4.101402
1.241353	195.650961	4.106406
1.592785	192.489053	4.111411
1.154104	198.167275	4.116416
1.171509	193.776354	4.121421
1.339052	195.749669	4.126426
1.360199	197.179598	4.131430
1.363381	192.265711	4.136435
1.543718	193.756120	4.141440
1.734475	197.367823	4.146445
1.608552	198.529723	4.151450
1.526101	203.089087	4.156454
1.525835	194.771464	4.161459
1.598094	196.978013	4.166464
1.523519	190.934169	4.171469
1.636838	197.924312	4.176474
1.695451	189.442440	4.181478
1.304093	168.926300	4.186483
1.343033	182.407593	4.191488
1.423894	185.862501	4.196493
1.530482	193.011888	4.201498
1.334971	199.022177	4.206502
1.828901	203.554509	4.211507
1.572992	201.610917	4.216512
1.354199	196.462883	4.221517
1.342011	202.548856	4.226522
1.736704	199.342204	4.231526
1.618919	195.602065	4.236531
1.496144	211.070288	4.241536
1.575084	195.406508	4.246541
1.471802	202.572962	4.251546
1.197853	210.316666	4.256550
1.498997	194.216266	4.261555
1.370144	202.313727	4.266560
1.434273	197.817406	4.271565
1.591464	208.907323	4.276570
1.856876	225.431567	4.281574
1.920909	218.983174	4.286579
1.622124	227.474275	4.291584
1.939207	222.843400	4.296589
2.072815	222.945885	4.301594
1.752074	210.758485	4.306598
1.526839	213.343849	4.311603
2.222157	213.367816	4.316608
1.899524	213.117833	4.321613
1.832347	209.015414	4.326618
1.540167	197.858119	4.331622
1.870836	211.116550	4.336627
1.764642	225.607729	4.341632
1.980338	217.322700	4.346637
2.170014	227.173646	4.351642
2.328423	232.824767	4.356646
2.054723	210.455122	4.361651
1.634080	201.083368	4.366656
1.715082	202.326744	4.371661
2.363791	218.319516	4.376666
2.063515	212.839388	4.381670
1.781912	199.623948	4.386675
1.758304	216.962277	4.391680
1.479918	222.422398	4.396685
2.173140	223.417988	4.401690
1.499222	229.202681	4.406694
1.906066	226.800896	4.411699
1.488613	230.577505	4.416704
2.017917	225.305923	4.421709
1.837658	219.481113	4.426714
2.123590	237.454350	4.431718
2.256471	234.934134	4.436723
2.068055	234.264478	4.441728
2.222722	238.815174	4.446733
2.464155	236.135577	4.451738
2.482310	231.962833	4.456742
2.392229	226.674399	4.461747
2.140516	238.008740	4.466752
2.234201	232.125186	4.471757
2.266265	228.459641	4.476762
2.170631	231.486620	4.481766
2.582466	231.766980	4.486771
2.178394	233.456529	4.491776
2.553604	233.812232	4.496781
2.399509	228.660380	4.501786
1.787772	236.469675	4.506790
1.796781	231.491588	4.511795
2.093868	229.730274	4.516800
2.151285	236.083770	4.521805
2.347220	244.361321	4.526810
2.221314	245.703560	4.531814
2.511098	239.450748	4.536819
2.113526	243.591248	4.541824
2.341855	244.159795	4.546829
2.437231	252.918189	4.551834
2.314673	246.492694	4.556838
2.627281	239.011903	4.561843
2.324749	243.191298	4.566848
2.645227	241.856599	4.571853
2.531896	238.220160	4.576858
2.376786	246.470455	4.581862
2.667089	241.328066	4.586867
2.785516	250.120814	4.591872
2.786353	246.036204	4.596877
2.550523	247.063463	4.601882
2.570838	246.294662	4.606886
2.438381	246.147763	4.611891
2.244405	246.940668	4.616896
2.389212	240.739045	4.621901
2.468761	242.957112	4.626906
2.631419	248.050737	4.631910
2.593749	245.873625	4.636915
2.492534	251.910287	4.641920
2.438125	249.523820	4.646925
2.585435	234.453585	4.651930
2.475286	243.335928	4.656934
2.692198	236.483915	4.661939
2.626006	241.138820	4.666944
2.177117	247.916506	4.671949
2.390951	251.939066	4.676954
2.444644	265.098562	4.681958
2.870687	271.296235	4.686963
2.494287	265.492651	4.691968
2.624323	265.443831	4.696973
2.531237	263.161501	4.701978
2.756466	271.646453	4.706982
2.947989	268.148909	4.711987
2.747592	271.698524	4.716992
2.597439	270.247731	4.721997
3.235144	265.769096	4.727002
2.976893	275.800985	4.732006
3.240794	273.250743	4.737011
2.530241	278.266051	4.742016
2.392235	276.772225	4.747021
2.859150	269.248262	4.752026
2.599077	269.836384	4.757030
2.720269	261.082074	4.762035
3.050115	288.223606	4.767040
3.089065	291.814819	4.772045
3.077963	277.917842	4.777050
2.912134	277.133912	4.782054
3.146138	277.511740	4.787059
2.944283	282.902939	4.792064
2.965787	278.685367	4.797069
3.158494	289.342651	4.802074
3.021851	288.339006	4.807078
3.409802	278.451367	4.812083
3.166049	279.660208	4.817088
2.707873	274.537004	4.822093
3.406215	275.174282	4.827098
3.027938	285.781818	4.832102
2.835975	278.256678	4.837107
3.165890	282.083882	4.842112
3.203953	289.595230	4.847117
3.563943	294.430154	4.852122
3.181436	287.532830	4.857126
3.071696	270.490638	4.862131
3.275296	278.460112	4.867136
3.206812	284.051883	4.872141
3.271407	280.558406	4.877146
3.336475	286.847444	4.882150
3.235825	270.936482	4.887155
3.029981	282.374399	4.892160
3.482317	292.424679	4.897165
3.427157	293.040809	4.902170
3.164459	286.646747	4.907174
3.373486	283.333125	4.912179
3.333166	302.123194	4.917184
3.309421	289.477907	4.922189
3.340349	291.516932	4.927194
3.412457	304.970973	4.932198
3.486325	290.440561	4.937203
3.583341	298.926630	4.942208
3.149717	293.407257	4.947213
3.510870	288.620760	4.952218
3.149707	301.481441	4.957222
3.566720	298.274438	4.962227
3.542030	296.104777	4.967232
3.365540	294.968166	4.972237
3.447162	295.616650	4.977242
3.204876	299.255092	4.982246
3.663129	300.047051	4.987251
3.668437	302.039470	4.992256
3.618675	296.153059	4.997261
3.897330	302.291576	5.002266
3.377263	305.502130	5.007270
3.454659	297.434891	5.012275
3.218356	304.555787	5.017280
3.372524	304.098215	5.022285
3.500230	305.922756	5.027290
3.360710	292.431878	5.032294
3.458908	303.274826	5.037299
3.610868	301.438165	5.042304
3.215209	297.026514	5.047309
3.673737	290.402387	5.052314
3.530896	300.077676	5.057318
3.492737	293.515550	5.062323
3.985076	314.117315	5.067328
3.656845	308.533966	5.072333
3.555748	298.023732	5.077338
3.713577	314.277005	5.082342
4.211486	318.160155	5.087347
3.975581	311.179740	5.092352
3.688761	303.457473	5.097357
3.674694	302.358690	5.102362
3.601430	300.772458	5.107366
3.798351	299.782990	5.112371
3.739292	318.069797	5.117376
4.244407	325.564931	5.122381
4.027088	316.604198	5.127386
3.459501	304.771794	5.132390
3.579892	306.205164	5.137395
3.822027	315.000708	5.142400
3.857014	319.652436	5.147405
3.788355	321.729214	5.152410
3.604757	326.013383	5.157414
3.752856	317.735735	5.162419
3.639982	327.561372	5.167424
3.518059	326.944571	5.172429
3.529229	322.364765	5.177434
3.761951	337.755251	5.182438
4.138257	350.516240	5.187443
4.281864	356.375369	5.192448
4.088404	352.270556	5.197453
4.058653	331.251468	5.202458
4.164884	336.543790	5.207462
4.549565	336.420271	5.212467
4.297041	332.849916	5.217472
4.126305	328.143581	5.222477
4.249772	336.729931	5.227482
4.141648	337.484078	5.232486
4.244733	331.257323	5.237491
4.178489	333.011012	5.242496
3.964577	321.958438	5.247501
4.187323	325.327866	5.252506
3.897620	333.456916	5.257510
4.065801	312.270793	5.262515
4.186678	326.036758	5.267520
4.145536	334.452740	5.272525
4.276433	334.830905	5.277530
3.978484	339.066553	5.282534
4.843015	344.448881	5.287539
4.528730	339.081643	5.292544
3.994289	339.921569	5.297549
4.420306	333.087378	5.302554
4.225453	340.995920	5.307558
4.004030	335.307240	5.312563
4.177274	337.684651	5.317568
4.269040	354.954416	5.322573
4.462905	354.715256	5.327578
4.417047	365.052449	5.332582
4.392389	361.958930	5.337587
4.287805	367.863277	5.342592
4.690146	365.895628	5.347597
4.761324	352.026832	5.352602
4.305817	345.634484	5.357606
4.353156	338.457814	5.362611
4.481882	353.263476	5.367616
4.792781	347.491388	5.372621
4.222360	337.244495	5.377626
4.248522	343.235919	5.382630
4.392454	350.591497	5.387635
4.497026	363.493150	5.392640
4.272414	359.032537	5.397645
4.464367	355.965193	5.402650
4.630046	360.811596	5.407654
4.474892	356.915923	5.412659
4.498593	368.688100	5.417664
4.235895	368.514147	5.422669
4.327823	358.850021	5.427674
4.369042	363.269823	5.432678
4.697431	359.424941	5.437683
4.793782	368.167420	5.442688
4.360051	363.717424	5.447693
4.505029	362.758238	5.452698
4.223130	366.007419	5.457702
4.343300	380.972637	5.462707
4.698210	393.398476	5.467712
4.737134	396.613215	5.472717
4.810939	392.295670	5.477722
4.842297	394.119496	5.482726
5.078657	388.074326	5.487731
4.977321	391.772964	5.492736
4.849138	388.654530	5.497741
4.505459	384.994039	5.502746
4.431644	390.947359	5.507750
4.812897	386.951815	5.512755
4.633047	390.817783	5.517760
4.434235	390.763538	5.522765
5.168922	389.749921	5.527770
5.249285	392.059631	5.532774
5.245036	379.262524	5.537779
5.500547	387.704820	5.542784
4.839936	384.233196	5.547789
5.340010	382.076220	5.552794
4.861719	367.388640	5.557798
4.698333	365.794377	5.562803
4.926541	371.760482	5.567808
5.122370	383.258919	5.572813
5.111803	376.875942	5.577818
4.849219	370.247708	5.582822
5.074310	368.500825	5.587827
4.805079	372.162487	5.592832
4.989211	387.313848	5.597837
5.025493	387.229096	5.602842
5.083326	385.027512	5.607846
5.029048	394.179595	5.612851
5.296894	388.037740	5.617856
5.073463	392.584438	5.622861
4.974194	391.078206	5.627866
4.643219	392.696202	5.632870
5.056521	389.622647	5.637875
5.286337	377.997461	5.642880
5.102248	383.686473	5.647885
5.144010	380.152259	5.652890
4.806223	382.948277	5.657894
5.372871	378.540860	5.662899
5.168103	387.178663	5.667904
5.128809	387.820785	5.672909
5.070830	388.709451	5.677914
5.181145	389.052876	5.682918
5.436718	386.855111	5.687923
5.297941	390.546960	5.692928
5.134950	390.306763	5.697933
5.415005	388.285502	5.702938
5.074721	385.772959	5.707942
5.159173	393.422621	5.712947
5.303107	389.831266	5.717952
5.190435	387.447582	5.722957
5.172529	389.304437	5.727962
5.623786	400.879928	5.732966
5.280709	388.502910	5.737971
5.065725	394.826374	5.742976
5.120885	409.988470	5.747981
5.285235	407.409513	5.752986
5.341632	415.161659	5.757990
5.301056	417.724447	5.762995
5.701767	416.231627	5.768000
5.731107	415.654401	5.773005
5.924650	420.138938	5.778010
5.377738	417.158875	5.783014
5.616208	424.275036	5.788019
5.769411	418.454864	5.793024
5.305752	414.414519	5.798029
6.012823	412.848387	5.803034
5.547890	412.642843	5.808038
5.651763	405.270621	5.813043
5.440508	400.058070	5.818048
5.623314	408.635158	5.823053
5.635521	408.848417	5.828058
5.340316	413.814505	5.833062
5.643088	415.070607	5.838067
5.807470	413.716059	5.843072
5.457240	413.283728	5.848077
5.555629	417.523737	5.853082
5.533730	422.431186	5.858086
5.877719	411.639169	5.863091
5.588192	405.891532	5.868096
5.584089	411.473256	5.873101
5.438439	417.535919	5.878106
5.733356	416.907590	5.883110
5.475672	420.219428	5.888115
5.575578	417.561979	5.893120
5.583320	425.416668	5.898125
5.506637	404.487108	5.903130
5.559618	419.073731	5.908134
5.910707	418.759315	5.913139
5.803048	428.666451	5.918144
5.738009	439.598335	5.923149
5.737669	439.797742	5.928154
6.263549	454.272333	5.933158
6.034709	434.657436	5.938163
5.783194	425.632400	5.943168
5.764165	437.458775	5.948173
6.090372	444.421988	5.953178
5.891518	441.229193	5.958182
5.857228	442.164772	5.963187
5.873797	435.584527	5.968192
6.270600	453.926603	5.973197
6.060274	439.772803	5.978202
5.820927	444.606756	5.983206
6.210240	441.021240	5.988211
6.174957	436.859986	5.993216
5.532914	431.439665	5.998221
5.953283	430.760042	6.003226
5.785823	439.670444	6.008230
5.871521	444.399683	6.013235
6.167675	440.869894	6.018240
6.051719	444.409476	6.023245
6.404516	447.119449	6.028250
6.394926	445.646619	6.033254
5.992380	426.242452	6.038259
5.792714	417.380146	6.043264
5.711788	424.033804	6.048269
6.087223	440.047446	6.053274
6.059211	447.524919	6.058278
6.147910	446.682118	6.063283
5.964146	450.004527	6.068288
6.048049	449.311179	6.073293
6.489957	438.386741	6.078298
5.987066	430.834319	6.083302
5.948515	424.411417	6.088307
5.970128	428.343907	6.093312
5.947739	421.570448	6.098317
6.075231	422.967913	6.103322
6.127848	426.693058	6.108326
5.860507	424.213375	6.113331
5.930106	422.085875	6.118336
5.672288	422.876136	6.123341
6.036573	430.719258	6.128346
5.930479	439.642193	6.133350
5.876927	448.199383	6.138355
5.914422	439.894713	6.143360
5.820055	441.886945	6.148365
6.171854	438.867312	6.153370
5.929829	443.261907	6.158374
6.290828	443.730577	6.163379
6.087368	438.162440	6.168384
6.038368	437.186185	6.173389
5.816246	432.892848	6.178394
5.841571	424.893824	6.183398
6.060444	431.721983	6.188403
6.290573	442.433609	6.193408
5.804001	443.446380	6.198413
6.221607	436.490077	6.203418
5.793599	443.334170	6.208422
6.007376	445.331908	6.213427
6.394379	447.223408	6.218432
5.778691	445.744298	6.223437
6.217726	431.552039	6.228442
5.616823	436.768517	6.233446
5.897045	444.286283	6.238451
6.492556	444.174024	6.243456
6.057608	439.790641	6.248461
5.917625	430.226090	6.253466
6.066584	432.464944	6.258470
5.467953	432.710633	6.263475
6.046295	434.746166	6.268480
5.971432	454.810517	6.273485
6.026327	445.826051	6.278490
6.128203	441.374377	6.283494
5.690431	450.149961	6.288499
6.293410	445.186322	6.293504
5.644932	446.841415	6.298509
5.832457	436.754130	6.303514
6.277398	451.307841	6.308518
6.602037	450.678018	6.313523
6.163252	447.744286	6.318528
5.569468	440.867350	6.323533
6.095807	443.050241	6.328538
6.080762	436.395853	6.333542
6.247635	441.216780	6.338547
6.179142	421.719148	6.343552
5.655536	421.908788	6.348557
5.976656	428.958216	6.353562
6.265150	437.743393	6.358566
5.719299	425.986599	6.363571
5.792879	431.562485	6.368576
6.196763	435.526835	6.373581
6.045749	443.305162	6.378586
5.873235	436.359059	6.383590
5.862542	443.960372	6.388595
6.047867	442.134288	6.393600
5.775496	457.439495	6.398605
5.723308	443.956966	6.403610
5.695260	446.783560	6.408614
5.513571	441.879587	6.413619
5.773630	442.085652	6.418624
5.934382	449.707564	6.423629
6.155292	449.242695	6.428634
6.106288	443.125154	6.433638
5.998861	454.927425	6.438643
6.063752	453.847900	6.443648
5.942083	454.651632	6.448653
6.022033	439.762628	6.453658
5.624593	448.772346	6.458662
5.854166	453.083561	6.463667
6.364376	451.475502	6.468672
5.990405	450.240104	6.473677
5.988094	441.077935	6.478682
6.143759	446.644128	6.483686
6.058700	444.825605	6.488691
6.223991	445.302792	6.493696
5.889761	445.915194	6.498701
6.165166	451.051325	6.503706
6.063117	455.101277	6.508710
5.665995	454.679456	6.513715
5.960199	449.897078	6.518720
5.743979	452.253264	6.523725
5.769106	447.870563	6.528730
5.830702	444.152889	6.533734
5.383834	450.091909	6.538739
5.885965	467.427205	6.543744
6.181731	476.046740	6.548749
6.028624	469.556345	6.553754
5.959499	480.719857	6.558758
6.082712	470.073133	6.563763
5.808297	476.804585	6.568768
5.242279	469.334807	6.573773
6.166137	470.449307	6.578778
5.999437	474.408149	6.583782
6.059636	476.917189	6.588787
6.409746	470.192920	6.593792
6.183946	485.914812	6.598797
6.627331	476.758726	6.603802
6.329780	469.246885	6.608806
6.011778	460.149988	6.613811
6.214057	454.888447	6.618816
5.768097	456.435878	6.623821
5.789377	451.806996	6.628826
6.197648	450.430052	6.633830
6.132197	447.165733	6.638835
6.022010	443.459155	6.643840
5.822793	451.292496	6.648845
5.926333	448.878091	6.653850
5.904113	449.277086	6.658854
5.588445	459.976158	6.663859
6.055665	460.871128	6.668864
5.934807	465.632736	6.673869
6.301266	469.343520	6.678874
6.337096	475.741613	6.683878
6.185218	464.432450	6.688883
6.213664	454.699122	6.693888
6.171923	457.445602	6.698893
5.944820	448.736281	6.703898
6.218982	446.700118	6.708902
5.941073	451.407232	6.713907
6.236771	451.364095	6.718912
5.570602	454.926610	6.723917
5.889808	452.285417	6.728922
5.926022	454.912112	6.733926
6.220543	454.217402	6.738931
6.219592	446.842604	6.743936
6.221933	457.988577	6.748941
6.033162	438.921074	6.753946
6.276613	455.392023	6.758950
6.092463	454.550841	6.763955
5.897184	453.221004	6.768960
5.931628	462.821146	6.773965
6.181681	463.082565	6.778970
6.066140	457.209571	6.783974
5.886285	458.506492	6.788979
6.190786	450.514337	6.793984
5.860549	453.011779	6.798989
5.962601	445.418354	6.803994
5.598712	451.489911	6.808998
5.863861	456.751042	6.814003
6.110579	454.668556	6.819008
5.873848	455.987044	6.824013
6.116247	454.389307	6.829018
6.221843	456.448290	6.834022
6.087942	457.681061	6.839027
5.983005	458.709971	6.844032
6.092037	457.114146	6.849037
5.997375	450.253920	6.854042
6.014919	457.388890	6.859046
5.481518	458.715894	6.864051
6.138003	454.677211	6.869056
6.186169	453.141545	6.874061
6.159210	448.855593	6.879066
6.381768	447.026839	6.884070
6.215074	454.836103	6.889075
6.281903	449.665392	6.894080
6.001422	453.290867	6.899085
6.026125	462.417955	6.904090
5.790056	453.615119	6.909094
5.890626	449.628736	6.914099
6.437764	451.200907	6.919104
5.906141	457.982143	6.924109
6.190555	450.034265	6.929114
6.163297	452.784804	6.934118
5.985933	452.749346	6.939123
6.512818	455.128313	6.944128
6.282989	453.585581	6.949133
6.037713	429.936169	6.954138
6.146106	427.043262	6.959142
5.914864	430.044064	6.964147
5.986742	416.706638	6.969152
5.706367	427.204002	6.974157
5.828277	420.452228	6.979162
6.065498	426.850389	6.984166
6.012492	431.740567	6.989171
6.141731	417.198212	6.994176
5.848529	426.954078	6.999181
5.886822	417.269849	7.004186
6.371255	431.162437	7.009190
6.226546	425.686343	7.014195
6.360698	426.424681	7.019200
6.258224	424.245044	7.024205
6.319270	418.837958	7.029210
6.252308	416.877393	7.034214
6.074698	420.553185	7.039219
6.007410	416.238756	7.044224
5.790499	423.410447	7.049229
5.791200	419.813054	7.054234
5.727479	420.598214	7.059238
5.723165	417.802065	7.064243
5.924333	413.474050	7.069248
5.952144	414.238541	7.074253
5.861525	423.326728	7.079258
5.717914	422.735469	7.084262
5.492655	428.364504	7.089267
6.440062	428.950110	7.094272
6.092084	432.165362	7.099277
6.021069	424.576915	7.104282
6.117702	414.304561	7.109286
6.065639	414.733541	7.114291
6.101401	416.547188	7.119296
5.913727	413.741802	7.124301
5.885660	418.539481	7.129306
6.034233	416.184466	7.134310
6.094739	413.789463	7.139315
6.156312	415.912288	7.144320
5.521708	430.805975	7.149325
5.755292	423.663367	7.154330
5.991743	432.671838	7.159334
5.589458	445.580197	7.164339
6.165594	446.878895	7.169344
6.023846	445.565981	7.174349
6.176507	446.624135	7.179354
6.219177	451.360117	7.184358
6.314728	449.687309	7.189363
6.158474	429.962965	7.194368
6.026527	424.285548	7.199373
6.272296	417.235950	7.204378
6.075837	420.196498	7.209382
5.806158	433.122036	7.214387
5.919025	419.993328	7.219392
5.495308	422.546543	7.224397
5.851418	425.923569	7.229402
6.029813	442.679955	7.234406
5.945135	444.177106	7.239411
6.007627	443.604176	7.244416
6.116234	439.853826	7.249421
6.245147	451.498838	7.254426
6.321754	429.776410	7.259430
5.899387	428.985209	7.264435
5.778006	417.838982	7.269440
5.932248	419.811242	7.274445
6.196177	436.956032	7.279450
6.462198	426.954533	7.284454
5.833883	430.343427	7.289459
6.192360	418.685401	7.294464
6.167588	421.827864	7.299469
6.093026	420.906237	7.304474
5.995543	420.975326	7.309478
5.603921	426.719015	7.314483
5.806581	417.046999	7.319488
5.874872	423.544396	7.324493
5.969858	430.297049	7.329498
6.216251	421.570502	7.334502
6.190333	417.132529	7.339507
6.182572	411.359726	7.344512
5.800765	418.718608	7.349517
6.172246	417.103813	7.354522
6.383037	417.994664	7.359526
6.028303	420.132095	7.364531
6.127147	417.667808	7.369536
5.976208	425.939679	7.374541
6.156993	418.602858	7.379546
6.078930	428.328181	7.384550
6.066907	426.143864	7.389555
6.061135	411.027861	7.394560
6.212371	420.945051	7.399565
6.057286	421.200341	7.404570
6.189752	423.163358	7.409574
5.790782	420.429044	7.414579
6.185545	412.378469	7.419584
5.876797	422.541742	7.424589
5.767668	425.947369	7.429594
6.081593	418.203696	7.434598
5.927214	432.712084	7.439603
5.983383	424.398168	7.444608
5.825599	427.260906	7.449613
5.704043	429.985085	7.454618
5.959971	423.645762	7.459622
5.953311	432.622719	7.464627
5.762651	429.137567	7.469632
5.678620	422.690152	7.474637
6.176324	428.493825	7.479642
5.850542	419.078617	7.484646
5.685911	430.272881	7.489651
6.205907	434.412034	7.494656
6.068735	436.607132	7.499661
5.856109	431.989593	7.504666
5.895517	425.010291	7.509670
6.017901	450.571004	7.514675
6.348032	443.033597	7.519680
6.303956	430.707783	7.524685
5.837183	423.023151	7.529690
6.047019	423.461719	7.534694
5.762128	424.322663	7.539699
6.023180	427.907579	7.544704
5.997173	420.214002	7.549709
5.628197	421.224166	7.554714
5.896343	434.008489	7.559718
5.951175	443.820570	7.564723
6.106014	448.032758	7.569728
6.106483	446.615301	7.574733
6.040944	449.318051	7.579738
6.660951	445.063615	7.584742
6.063131	432.523993	7.589747
6.198011	415.927406	7.594752
5.449980	429.355012	7.599757
5.889175	429.004645	7.604762
6.012931	431.437279	7.609766
6.409932	424.705680	7.614771
5.944161	418.878082	7.619776
6.200142	415.867137	7.624781
6.010191	429.631260	7.629786
5.903066	421.304965	7.634790
5.903716	425.746957	7.639795
6.108659	421.595526	7.644800
6.149377	420.149618	7.649805
5.598157	418.701539	7.654810
6.045144	414.784278	7.659814
5.720129	420.144193	7.664819
6.222327	420.609722	7.669824
6.054271	426.849911	7.674829
6.095378	427.631303	7.679834
6.326900	417.745950	7.684838
6.057363	431.244124	7.689843
5.861384	418.439063	7.694848
5.831266	423.474355	7.699853
5.945849	419.789514	7.704858
5.860632	418.502547	7.709862
5.743053	426.791339	7.714867
5.851131	430.751413	7.719872
5.795008	449.385919	7.724877
5.949552	447.751326	7.729882
5.963298	452.181781	7.734886
6.054145	456.055972	7.739891
6.418006	435.563570	7.744896
6.192762	439.658132	7.749901
6.162107	439.115616	7.754906
6.180467	427.238782	7.759910
5.931140	428.856644	7.764915
6.185713	416.430261	7.769920
6.195068	421.918127	7.774925
5.978500	428.403208	7.779930
6.259365	424.549939	7.784934
5.797444	423.897818	7.789939
5.829274	429.499228	7.794944
5.795803	424.717575	7.799949
5.909705	427.544072	7.804954
5.879677	415.877314	7.809958
5.887733	432.546481	7.814963
6.201926	435.427022	7.819968
5.904380	430.696234	7.824973
5.896261	427.998759	7.829978
6.055723	438.202582	7.834982
5.753163	446.504546	7.839987
6.460022	441.502485	7.844992
6.232172	436.001448	7.849997
6.088399	429.512769	7.855002
6.318103	424.550672	7.860006
6.141601	428.583808	7.865011
5.960785	427.084022	7.870016
5.752520	426.189670	7.875021
5.846662	433.344267	7.880026
5.755411	427.603524	7.885030
5.538564	430.570432	7.890035
6.435876	437.785858	7.895040
6.216690	432.125271	7.900045
5.884423	429.026151	7.905050
5.916901	431.615461	7.910054
5.624016	428.507007	7.915059
6.128853	437.213993	7.920064
6.212069	443.686911	7.925069
5.967726	442.848833	7.930074
6.019353	436.538352	7.935078
5.829433	442.301064	7.940083
6.111846	439.858634	7.945088
5.741931	433.731264	7.950093
6.264693	447.788708	7.955098
6.163616	445.175400	7.960102
6.029997	440.051917	7.965107
5.817382	422.108178	7.970112
6.133037	423.995035	7.975117
6.033359	429.528462	7.980122
6.077572	423.856504	7.985139
5.521214	428.226115	7.990157
6.216857	444.631426	7.995174
6.204705	448.123671	8.000192
6.409655	438.002509	8.005210
6.446311	436.131721	8.010227
6.341229	434.346256	8.015245
6.051257	426.060423	8.020262
6.284132	429.864566	8.025280
5.873280	426.183041	8.030298
6.084950	430.230347	8.035315
6.115413	428.332128	8.040333
6.298581	417.895655	8.045350
6.007563	413.841908	8.050368
5.976765	422.092847	8.055386
6.163802	429.817356	8.060403
5.919082	432.481349	8.065421
5.759422	416.351891	8.070438
5.738365	419.463675	8.075456
5.598528	427.043737	8.080474
5.915791	431.162862	8.085491
6.010963	443.679642	8.090509
6.077422	452.407661	8.095526
6.214658	451.644576	8.100544
5.864013	448.909820	8.105562
5.992591	453.260484	8.110579
6.214931	454.377544	8.115597
6.228668	459.175391	8.120614
6.316103	454.418556	8.125632
6.286481	445.334530	8.130650
6.249708	446.700470	8.135667
5.925276	445.690984	8.140685
6.162939	446.982367	8.145702
6.052535	448.350376	8.150720
5.822898	445.249523	8.155738
6.472598	449.947725	8.160755
6.288000	453.514327	8.165773
6.529900	445.905698	8.170790
6.301432	440.466218	8.175808
5.944653	460.485722	8.180826
6.452935	450.074030	8.185843
6.135227	455.734847	8.190861
6.135275	453.450072	8.195878
6.227273	453.694463	8.200896
5.950881	461.911316	8.205914
6.345781	452.240066	8.210931
6.198386	459.310088	8.215949
6.258157	455.087761	8.220966
6.466486	459.612123	8.225984
6.062131	464.125185	8.231002
6.327394	454.950770	8.236019
5.984457	459.274327	8.241037
6.120868	458.233661	8.246054
5.989038	455.792823	8.251072
5.713899	463.002781	8.256090
6.141296	458.969006	8.261107
6.413667	448.209271	8.266125
6.010607	452.914630	8.271142
6.082153	452.966566	8.276160
6.029751	469.751036	8.281178
6.404680	471.980277	8.286195
6.329634	474.122231	8.291213
5.969830	472.152610	8.296230
6.148401	480.755780	8.301248
6.278633	479.018648	8.306266
6.284586	482.687944	8.311283
6.218920	478.056076	8.316301
6.031141	482.847634	8.321318
6.346312	476.171097	8.326336
6.536813	476.538910	8.331354
6.683569	476.001550	8.336371
6.709317	476.682355	8.341389
6.543550	487.106728	8.346406
6.556372	478.751338	8.351424
6.440714	483.348559	8.356442
6.952470	479.907476	8.361459
6.546920	467.114312	8.366477
6.321802	457.972548	8.371494
6.748571	453.055249	8.376512
6.426663	460.480817	8.381530
6.299278	449.149399	8.386547
6.015308	451.118958	8.391565
5.782426	453.866306	8.396582
6.261159	462.955768	8.401600
6.331697	481.077979	8.406618
6.658473	477.517557	8.411635
6.426266	478.484931	8.416653
6.334353	493.385288	8.421670
6.750798	477.010876	8.426688
6.491167	486.806172	8.431706
6.391789	478.108600	8.436723
6.425743	485.708795	8.441741
6.394785	485.076203	8.446758
6.284025	488.012705	8.451776
6.656928	482.523170	8.456794
6.650169	482.079290	8.461811
6.734377	476.073257	8.466829
6.304042	484.812858	8.471846
6.503379	477.570646	8.476864
6.548949	483.127216	8.481882
6.510645	484.130481	8.486899
6.635579	478.433647	8.491917
6.258228	479.237569	8.496934
6.672426	478.058704	8.501952
6.510960	480.523468	8.506970
6.506319	477.128581	8.511987
6.682776	478.830343	8.517005
6.064677	479.324848	8.522022
6.523532	483.652174	8.527040
6.581882	480.130652	8.532058
6.264056	474.897666	8.537075
6.568255	485.668125	8.542093
6.391452	477.497081	8.547110
6.723821	476.236362	8.552128
6.573393	485.948276	8.557146
6.836731	482.981616	8.562163
6.964934	478.666511	8.567181
6.516356	480.655552	8.572199
6.428621	477.781769	8.577216
6.384635	483.513317	8.582234
6.557588	480.879555	8.587251
6.278337	481.545031	8.592269
6.337681	480.958251	8.597287
6.899838	488.440974	8.602304
6.802183	491.280749	8.607322
6.842809	495.168677	8.612339
6.834661	479.523507	8.617357
6.590307	479.956298	8.622375
6.528826	477.441319	8.627392
6.525909	472.095877	8.632410
6.604256	478.237445	8.637427
7.123676	490.290156	8.642445
6.617974	487.519728	8.647463
6.755253	470.617861	8.652480
6.859298	472.024855	8.657498
6.638380	478.882342	8.662515
6.622529	480.140865	8.667533
6.493905	490.338514	8.672551
6.537318	494.001943	8.677568
6.792799	500.970988	8.682586
7.001631	508.341821	8.687603
7.070923	504.342054	8.692621
6.296762	486.052411	8.697639
6.661101	497.690769	8.702656
6.943646	501.900556	8.707674
6.805938	505.863764	8.712691
6.714377	501.652515	8.717709
6.801228	505.340698	8.722727
6.968204	513.592250	8.727744
7.062663	510.626799	8.732762
6.945213	498.687878	8.737779
6.949848	490.011873	8.742797
6.599741	495.400068	8.747815
6.689348	477.953397	8.752832
6.582059	487.645930	8.757850
6.565456	506.889508	8.762867
6.398480	512.668737	8.767885
6.755899	516.958315	8.772903
6.839157	511.353207	8.777920
7.007455	504.974227	8.782938
6.753669	513.995449	8.787955
6.913023	502.814731	8.792973
6.494916	508.074729	8.797991
7.047592	503.914018	8.803008
6.732841	511.363732	8.808026
6.700448	520.451255	8.813043
7.171081	505.933410	8.818061
6.871485	515.394156	8.823079
6.710446	508.871115	8.828096
6.721729	509.800340	8.833114
6.642240	515.477501	8.838131
6.900866	509.519868	8.843149
6.650707	518.136581	8.848167
6.955555	527.613082	8.853184
6.959229	537.124153	8.858202
7.248175	543.302174	8.863219
7.290904	525.219017	8.868237
6.674024	514.068394	8.873255
6.841523	517.633490	8.878272
6.977978	518.861841	8.883290
7.175593	530.901883	8.888307
7.139552	522.670894	8.893325
7.301860	520.351219	8.898343
7.203198	520.281500	8.903360
7.043077	520.483343	8.908378
6.821964	521.521565	8.913395
7.201445	509.728839	8.918413
6.998022	514.557570	8.923431
6.867880	513.019021	8.928448
7.001411	507.895188	8.933466
6.897228	513.516256	8.938483
7.226451	508.702588	8.943501
7.167272	513.783274	8.948519
7.045732	513.022862	8.953536
6.770877	511.314482	8.958554
6.852246	519.118702	8.963571
7.410610	518.567343	8.968589
7.042025	525.163961	8.973607
7.134779	530.533272	8.978624
7.129215	513.786289	8.983642
7.106677	528.420185	8.988659
7.273948	513.820476	8.993677
6.804564	516.753212	8.998695
7.128586	521.272086	9.003712
7.278439	529.093982	9.008730
7.281019	531.589854	9.013747
7.560823	513.245501	9.018765
7.014884	511.964604	9.023783
7.341216	512.292201	9.028800
7.339264	514.220735	9.033818
7.246008	505.478009	9.038835
7.269183	500.175809	9.043853
7.318954	517.023209	9.048871
6.580091	518.246693	9.053888
7.074811	505.426056	9.058906
7.010769	512.741815	9.063923
7.437667	509.497059	9.068941
6.962640	511.300900	9.073959
6.946013	526.953194	9.078976
7.105634	529.153061	9.083994
7.334643	539.408313	9.089011
7.446289	532.678437	9.094029
7.510027	538.715017	9.099047
7.231522	528.467580	9.104064
7.287755	532.176345	9.109082
7.250606	541.999928	9.114099
7.236218	530.272057	9.119117
7.376400	539.244188	9.124135
7.177757	541.575929	9.129152
7.179324	536.251857	9.134170
6.872104	545.549711	9.139187
7.216849	532.165572	9.144205
7.247782	541.527207	9.149223
7.524028	532.224800	9.154240
7.404543	545.330707	9.159258
7.155817	544.659649	9.164275
6.866602	534.429666	9.169293
7.007156	536.234889	9.174311
6.882596	535.733725	9.179328
7.432673	529.067701	9.184346
7.076290	533.308175	9.189363
6.913633	538.796402	9.194381
7.094493	548.175575	9.199399
7.090297	559.300512	9.204416
7.643789	559.504156	9.209434
7.402581	572.906867	9.214451
7.960281	562.982831	9.219469
7.817029	566.262109	9.224487
7.604268	550.166096	9.229504
7.516474	537.777533	9.234522
7.349121	542.597464	9.239539
7.506771	545.741230	9.244557
7.168815	540.097967	9.249575
7.064461	536.428358	9.254592
7.672553	545.153609	9.259610
7.454629	550.729394	9.264627
7.483140	545.457902	9.269645
7.527160	551.974104	9.274663
7.316549	550.202006	9.279680
7.638197	549.195428	9.284698
7.232605	561.528818	9.289715
7.640100	565.412929	9.294733
7.588640	567.469147	9.299751
7.488798	557.130584	9.304768
7.606264	556.310632	9.309786
7.531049	564.783191	9.314803
7.247539	561.119556	9.319821
7.875904	563.548943	9.324839
7.365710	558.626940	9.329856
7.632109	559.386808	9.334874
7.579335	564.072027	9.339891
7.432367	557.231182	9.344909
7.558075	558.549582	9.349927
7.420019	566.205164	9.354944
7.592271	555.770321	9.359962
7.169860	565.354478	9.364979
7.677680	559.941611	9.369997
7.620418	565.040946	9.375015
7.572726	563.416891	9.380032
7.743156	556.627302	9.385050
7.629920	564.512525	9.390067
7.882126	561.124717	9.395085
8.023716	562.143982	9.400103
8.027675	563.380471	9.405120
7.868703	548.225934	9.410138
7.651934	543.358948	9.415155
7.586966	537.114334	9.420173
7.763024	537.048910	9.425191
7.420991	532.495043	9.430208
7.506530	529.818166	9.435226
7.404111	550.104031	9.440243
7.686622	557.166693	9.445261
7.720628	555.245815	9.450279
7.594357	557.096002	9.455296
8.137200	559.122220	9.460314
7.955055	569.123172	9.465331
7.689717	557.153734	9.470349
7.866100	543.167958	9.475367
7.454416	543.282983	9.480384
7.655741	541.484214	9.485402
7.569280	565.384159	9.490419
7.587839	562.036114	9.495437
7.698891	556.492909	9.500455
7.683736	564.280714	9.505472
7.873666	557.661639	9.510490
7.613828	566.371410	9.515507
7.607810	561.234712	9.520525
8.000278	558.358261	9.525543
7.927603	562.393344	9.530560
7.829871	566.025253	9.535578
7.653589	566.870260	9.540595
7.785230	562.958541	9.545613
8.191727	565.416379	9.550631
7.710536	568.414089	9.555648
7.718799	560.185608	9.560666
7.370281	570.099018	9.565683
7.481210	566.086401	9.570701
7.808991	568.868999	9.575719
7.767604	565.763876	9.580736
8.154404	557.529736	9.585754
8.024662	561.611630	9.590771
7.649298	560.575403	9.595789
7.884202	565.250263	9.600807
7.687531	568.130811	9.605824
8.053884	562.048985	9.610842
8.130976	562.996304	9.615859
7.843866	565.247235	9.620877
8.054814	556.617768	9.625895
7.998744	557.835260	9.630912
7.905300	556.745395	9.635930
7.961251	558.879457	9.640947
8.092627	550.789482	9.645965
8.258497	558.258586	9.650983
8.154874	555.693393	9.656000
8.118497	554.768157	9.661018
7.903077	558.759332	9.666035
7.568535	552.064644	9.671053
7.799834	559.239473	9.676071
7.876618	558.662581	9.681088
7.508984	564.429085	9.686106
7.382603	572.278501	9.691123
7.538790	577.492719	9.696141
7.741524	584.435348	9.701159
7.653252	589.482743	9.706176
7.999013	578.351668	9.711194
8.196141	580.024954	9.716211
8.052126	573.698039	9.721229
8.033197	569.983480	9.726247
7.721808	590.611402	9.731264
8.315563	602.759841	9.736282
8.609674	606.317741	9.741299
8.286099	599.517174	9.746317
8.451430	584.734674	9.751335
8.164490	581.507075	9.756352
8.312286	581.673297	9.761370
8.259761	584.360848	9.766387
7.884200	590.781857	9.771405
8.189678	581.664194	9.776423
8.263897	585.360685	9.781440
8.219644	582.423267	9.786458
8.593395	590.014448	9.791475
8.183454	587.923281	9.796493
8.550095	582.551463	9.801511
8.125483	588.828677	9.806528
8.205080	583.053706	9.811546
8.071389	582.620244	9.816563
8.316627	592.525844	9.821581
8.223416	583.050922	9.826599
7.777836	585.673825	9.831616
8.450326	583.545607	9.836634
8.337793	567.550640	9.841651
7.838332	585.468775	9.846669
8.283237	580.460237	9.851687
7.996105	581.470936	9.856704
8.204308	582.826905	9.861722
8.367496	578.963889	9.866739
8.286152	585.995209	9.871757
8.309979	579.600968	9.876775
8.151907	576.987499	9.881792
8.245926	580.254851	9.886810
8.428367	577.913079	9.891827
7.937488	582.304027	9.896845
8.120093	585.626928	9.901863
8.091984	599.201398	9.906880
8.523218	607.623030	9.911898
8.706154	607.073686	9.916915
8.734818	612.197441	9.921933
8.440582	593.381210	9.926951
8.371868	596.342700	9.931968
8.324638	583.733153	9.936986
8.275579	585.053691	9.942003
8.358154	587.451830	9.947021
8.346702	591.041824	9.952039
8.511328	601.212524	9.957056
8.394667	597.541675	9.962074
8.585770	586.008790	9.967091
8.357467	588.367275	9.972109
8.347731	583.603540	9.977127
8.680604	596.537623	9.982144
8.474752	582.463381	9.987162
8.555791	584.079117	9.992179
8.475896	583.930718	9.997197
8.298399	583.993272	10.002215
8.778944	592.896323	10.007232
8.406713	594.579922	10.012250
8.567820	588.672257	10.017267
8.346656	597.944032	10.022285
8.692783	602.778201	10.027303
8.724340	595.909370	10.032320
8.617441	591.334427	10.037338
8.686287	594.220715	10.042355
8.508921	595.946367	10.047373
8.388036	588.949944	10.052391
8.666032	594.558495	10.057408
8.417412	592.173807	10.062426
8.566813	587.416695	10.067443
8.255451	595.790568	10.072461
8.396044	602.657733	10.077479
8.959644	607.053885	10.082496
8.929661	613.887819	10.087514
8.587778	598.111797	10.092531
8.720245	595.547479	10.097549
8.766684	588.237659	10.102567
8.651581	587.656117	10.107584
8.731924	597.300376	10.112602
8.606599	582.702273	10.117619
8.734630	592.859768	10.122637
8.447207	590.383329	10.127655
8.709156	590.200305	10.132672
8.250994	591.657525	10.137690
8.692968	597.221450	10.142707
8.655920	601.276206	10.147725
8.790551	604.442525	10.152743
8.904636	610.600629	10.157760
8.851474	625.053209	10.162778
8.932175	608.721814	10.167795
8.649328	602.445043	10.172813
8.900652	599.111015	10.177831
8.695819	589.416892	10.182848
8.515656	591.174540	10.187866
8.635106	599.017009	10.192883
8.726611	603.244129	10.197901
8.627786	610.562222	10.202919
9.011782	622.494229	10.207936
8.908471	623.371987	10.212954
8.910047	611.180810	10.217971
8.765246	612.203924	10.222989
9.078013	613.767577	10.228007
8.885393	617.534285	10.233024
8.982396	618.046139	10.238042
9.295595	611.682288	10.243059
8.557676	605.864983	10.248077
8.814837	595.350541	10.253095
8.710788	598.989759	10.258112
8.641514	609.490603	10.263130
9.256017	613.752548	10.268147
9.032498	620.455861	10.273165
9.120149	609.917476	10.278183
9.153044	592.880369	10.283200
8.655433	588.259345	10.288218
8.948429	587.411890	10.293235
8.638494	595.927552	10.298253
9.104964	598.091973	10.303271
9.116728	602.126459	10.308288
8.501290	609.484468	10.313306
9.031405	608.075993	10.318323
8.902129	609.942435	10.323341
8.667050	610.869240	10.328359
9.134423	610.373161	10.333376
8.835781	618.132822	10.338394
9.011954	600.072862	10.343411
9.312270	619.049155	10.348429
8.611030	620.566554	10.353447
8.916264	615.791330	10.358464
9.006950	622.729439	10.363482
8.734384	618.363483	10.368499
8.836210	623.355857	10.373517
8.900368	618.706768	10.378535
9.009007	621.416411	10.383552
8.747423	612.210853	10.388570
8.824364	612.391333	10.393587
9.118951	625.915264	10.398605
9.164634	644.732662	10.403623
9.371616	640.184268	10.408640
8.955405	624.732295	10.413658
9.058482	624.223866	10.418675
9.148425	637.571584	10.423693
9.225272	641.150909	10.428711
9.363019	648.144770	10.433728
9.003206	633.125771	10.438746
9.011507	626.105936	10.443763
9.162508	641.482757	10.448781
9.112300	647.029138	10.453799
9.329418	644.896521	10.458816
8.894391	650.809312	10.463834
8.976997	654.857956	10.468851
8.944780	648.608173	10.473869
9.016750	652.737379	10.478887
9.356915	650.020589	10.483904
9.161066	639.482424	10.488922
8.885678	651.675554	10.493939
9.147344	645.638504	10.498957
9.094231	656.780634	10.503975
9.126650	646.474945	10.508992
8.927348	658.896003	10.514010
9.388440	653.196937	10.519027
9.781366	667.819501	10.524045
9.378364	650.563455	10.529063
9.306025	652.638733	10.534080
9.130706	657.333709	10.539098
9.519988	647.780001	10.544115
9.414469	648.364613	10.549133
9.168944	652.417331	10.554151
9.357771	651.002364	10.559168
8.914580	652.053297	10.564186
9.414218	668.792486	10.569203
9.536635	677.123679	10.574221
9.643818	679.748351	10.579239
9.542433	667.784709	10.584256
9.771027	665.391514	10.589274
9.802908	656.162044	10.594291
9.269515	651.180533	10.599309
9.303288	647.157897	10.604327
9.440544	639.937969	10.609344
9.522606	650.209997	10.614362
9.136145	646.104879	10.619379
9.441937	645.567844	10.624397
9.276871	650.090797	10.629415
9.797156	659.356887	10.634432
9.735167	657.214350	10.639450
9.336279	644.142302	10.644467
9.507329	647.460713	10.649485
9.215114	649.643026	10.654503
9.572818	659.366938	10.659520
9.798137	678.291927	10.664538
9.805196	663.269070	10.669555
9.955902	648.842262	10.674573
9.892433	648.161109	10.679591
9.879214	639.232206	10.684608
9.692615	639.946288	10.689626
9.712539	640.075741	10.694643
9.622467	642.728158	10.699661
9.365879	644.718694	10.704679
9.722130	633.589096	10.709696
9.324796	637.744492	10.714714
9.629876	646.337387	10.719731
9.654040	642.054323	10.724749
9.370740	646.097179	10.729767
9.488489	640.862171	10.734784
9.653704	647.501431	10.739802
9.789681	643.696313	10.744819
10.008738	637.902629	10.749837
9.517096	643.171032	10.754855
9.515274	638.204069	10.759872
9.542495	644.931221	10.764890
9.461367	638.900546	10.769907
10.173889	651.541654	10.774925
9.503008	653.123727	10.779943
9.455833	650.464469	10.784960
9.536873	656.574118	10.789978
9.829319	673.096462	10.794995
9.757826	678.188591	10.800013
9.862719	680.472792	10.805031
10.121414	664.539496	10.810048
10.071868	672.613606	10.815066
9.814198	668.633472	10.820083
9.909383	645.596779	10.825101
9.808150	650.665158	10.830119
9.757126	646.927209	10.835136
9.869752	660.072573	10.840154
9.684671	671.661427	10.845171
10.022326	666.903201	10.850189
10.022373	671.040524	10.855207
10.219973	656.363363	10.860224
10.096413	650.648603	10.865242
9.755520	641.237704	10.870259
10.020671	643.641959	10.875277
9.793710	642.670839	10.880295
9.742845	639.043321	10.885312
9.912386	640.670442	10.890330
9.936787	656.246993	10.895347
10.039613	647.681761	10.900365
9.712962	657.304612	10.905383
10.406375	658.079631	10.910400
9.916486	651.491296	10.915418
9.944788	650.489649	10.920435
9.922568	648.646998	10.925453
9.878628	657.496557	10.930471
10.045185	661.882347	10.935488
10.276482	665.857203	10.940506
10.113904	662.404975	10.945523
10.128874	646.330000	10.950541
9.830567	650.419390	10.955559
9.760829	657.568841	10.960576
10.040040	668.027742	10.965594
10.110984	678.490879	10.970611
10.285714	673.379478	10.975629
10.114054	684.025797	10.980647
10.136397	671.610417	10.985664
10.301737	667.728110	10.990682
10.084556	673.739321	10.995699
10.272049	667.931638	11.000717
10.033342	675.896530	11.005735
10.271612	668.064311	11.010752
10.225173	664.574951	11.015770
10.223316	674.875921	11.020787
10.341860	666.551216	11.025805
10.272360	665.517554	11.030823
10.093350	663.465935	11.035840
10.097176	664.756102	11.040858
10.334708	671.671222	11.045875
10.347277	663.180084	11.050893
9.800272	672.364093	11.055911
9.760029	665.471771	11.060928
10.311594	666.975922	11.065946
10.378835	676.710640	11.070963
10.425424	667.175899	11.075981
10.278472	673.141393	11.080999
10.236781	667.432736	11.086016
10.177192	663.058647	11.091034
9.957532	675.953125	11.096051
10.299274	670.941791	11.101069
9.932269	670.301883	11.106087
10.211088	673.625505	11.111104
10.398465	675.754769	11.116122
10.215697	676.723874	11.121139
9.944825	666.399421	11.126157
10.208887	670.340743	11.131175
10.426435	679.553290	11.136192
10.427781	680.878560	11.141210
10.494595	697.676123	11.146227
10.159962	688.586114	11.151245
10.359576	698.991232	11.156263
10.206298	694.063763	11.161280
10.421761	689.037496	11.166298
10.531036	696.682784	11.171315
10.527031	691.160721	11.176333
10.535029	705.938302	11.181351
10.649056	697.658472	11.186368
10.752833	689.332914	11.191386
10.620050	701.207086	11.196403
10.453453	694.233562	11.201421
10.448809	694.483631	11.206439
10.207627	699.479275	11.211456
10.563356	690.467294	11.216474
10.473327	696.673188	11.221491
10.654125	689.272848	11.226509
10.570948	698.254808	11.231527
10.513442	699.131704	11.236544
10.876948	686.767002	11.241562
10.741716	697.546479	11.246579
10.609827	693.505606	11.251597
10.532577	694.271986	11.256615
10.836609	702.394852	11.261632
10.962586	693.333659	11.266650
10.417261	693.589546	11.271667
10.672856	696.487617	11.276685
10.780085	699.449960	11.281703
10.525492	700.657540	11.286720
11.015059	701.802175	11.291738
10.507046	699.139374	11.296755
10.580097	691.689642	11.301773
10.734800	694.098586	11.306791
10.574588	689.554061	11.311808
10.732447	694.853260	11.316826
10.548122	708.569055	11.321843
10.347007	707.275142	11.326861
10.488571	694.437118	11.331879
10.545623	693.727612	11.336896
10.532547	692.006602	11.341914
10.539279	707.175707	11.346931
10.379443	693.958868	11.351949
10.531185	703.573062	11.356967
10.556627	714.071751	11.361984
11.000615	716.902438	11.367002
10.779531	721.727679	11.372019
11.131384	720.255606	11.377037
11.162197	721.509990	11.382055
10.737092	716.347391	11.387072
10.951287	719.851562	11.392090
11.156464	726.838046	11.397107
10.897785	721.447395	11.402125
10.769381	713.861957	11.407143
10.999933	723.608983	11.412160
10.984818	716.330846	11.417178
10.815270	727.888900	11.422195
10.947635	716.967901	11.427213
10.970329	717.980557	11.432231
11.202163	719.597925	11.437248
11.467504	716.918095	11.442266
10.771865	706.363522	11.447283
11.018149	698.558437	11.452301
10.982202	701.909291	11.457319
10.605210	704.546711	11.462336
10.817977	708.123688	11.467354
10.992054	711.384832	11.472371
11.169395	718.176855	11.477389
11.054605	722.745599	11.482407
10.861570	721.772314	11.487424
10.989187	719.063569	11.492442
10.816282	715.717092	11.497459
11.253893	718.675012	11.502477
11.170322	723.308293	11.507495
11.299175	726.046343	11.512512
10.965336	722.428430	11.517530
11.075493	726.813605	11.522547
11.196957	722.070303	11.527565
11.535251	721.818510	11.532583
11.174017	723.544580	11.537600
11.333171	716.624152	11.542618
11.104548	722.185887	11.547635
11.072924	718.817273	11.552653
11.105857	716.688260	11.557671
11.022977	724.433096	11.562688
11.051442	723.320964	11.567706
10.995136	723.938894	11.572723
11.059235	725.617258	11.577741
11.144007	723.836732	11.582759
10.826116	722.141386	11.587776
11.246981	720.920435	11.592794
11.086533	735.468809	11.597811
10.941455	729.978305	11.602829
11.089199	744.165969	11.607847
10.858281	749.608150	11.612864
11.161623	741.560574	11.617882
11.150848	742.086162	11.622899
11.363808	750.415827	11.627917
11.400872	740.453345	11.632935
11.270812	755.227350	11.637952
11.242310	744.757579	11.642970
11.072024	753.939410	11.647987
10.934438	756.368911	11.653005
11.704409	762.430616	11.658023
11.983202	770.948794	11.663040
11.762864	753.730301	11.668058
11.822190	745.263357	11.673075
11.376914	752.399101	11.678093
11.303382	751.293480	11.683111
11.481141	756.393917	11.688128
11.574790	741.783467	11.693146
11.677699	749.533918	11.698163
11.683625	750.262021	11.703181
11.858385	747.877249	11.708199
11.528362	752.678542	11.713216
11.851504	749.768741	11.718234
11.686888	748.465950	11.723251
11.737533	746.015417	11.728269
11.575347	736.854182	11.733287
11.487445	745.868465	11.738304
11.381818	741.744570	11.743322
11.373133	751.358679	11.748339
11.345694	750.750772	11.753357
11.668312	743.536475	11.758375
11.255374	751.493985	11.763392
11.458347	741.912611	11.768410
11.446491	749.308654	11.773427
11.701018	750.064079	11.778445
11.537075	760.898586	11.783463
11.560064	773.306984	11.788480
11.612164	774.154088	11.793498
11.733905	771.853360	11.798515
11.734505	779.594608	11.803533
11.957284	771.070483	11.808551
12.035853	781.696590	11.813568
12.004585	763.489084	11.818586
12.064327	748.625161	11.823603
11.597340	756.584829	11.828621
11.667180	741.646745	11.833639
11.616327	749.979874	11.838656
11.761556	755.069627	11.843674
11.531634	765.583110	11.848691
11.724247	784.213530	11.853709
11.994525	768.877939	11.858727
12.139255	778.606883	11.863744
12.189442	773.221473	11.868762
12.132905	761.885068	11.873779
11.574040	752.183209	11.878797
11.975121	766.773018	11.883815
11.855827	770.717620	11.888832
11.855770	769.284901	11.893850
12.160943	771.704994	11.898867
11.790402	764.217435	11.903885
12.075213	763.055669	11.908903
12.121009	778.651065	11.913920
12.135497	772.958818	11.918938
11.574164	754.493540	11.923955
11.688848	762.882790	11.928973
12.230514	766.215740	11.933991
11.788188	779.220920	11.939008
11.704678	774.314056	11.944026
12.135663	773.189348	11.949043
11.800948	777.101431	11.954061
12.154979	771.277089	11.959079
11.979165	771.819070	11.964096
11.692747	773.744865	11.969114
12.151434	780.789480	11.974131
11.749235	774.973168	11.979149
11.772655	777.528927	11.984167
11.838197	784.455259	11.989184
11.599934	798.807589	11.994202
11.980914	799.445372	11.999219
11.741548	804.658515	12.004237
12.257380	804.435711	12.009255
12.273066	815.611342	12.014272
12.191576	805.377059	12.019290
12.018347	803.962002	12.024307
12.251835	798.421630	12.029325
12.094375	800.355626	12.034343
12.338688	804.416838	12.039360
12.458334	798.600808	12.044378
12.483591	792.133683	12.049395
12.070895	805.809593	12.054413
12.214627	799.983477	12.059431
12.830256	803.727731	12.064448
12.467994	804.295769	12.069466
12.286614	793.067269	12.074483
12.275256	803.319307	12.079501
12.693644	804.061684	12.084519
12.399188	797.445830	12.089536
12.228067	800.587504	12.094554
12.465279	793.380257	12.099571
12.285529	796.229787	12.104589
12.673836	796.771746	12.109607
12.643812	801.759581	12.114624
12.432816	795.610342	12.119642
12.244068	797.404070	12.124659
12.057374	808.791289	12.129677
12.638149	794.483177	12.134695
12.552885	795.437011	12.139712
12.271742	790.236055	12.144730
12.316807	794.451561	12.149747
12.587585	799.950853	12.154765
12.377211	803.045028	12.159783
12.453754	798.245627	12.164800
12.162241	805.221598	12.169818
12.165274	795.469548	12.174835
12.470585	812.384488	12.179853
12.347610	814.912695	12.184871
12.426764	829.720255	12.189888
12.455930	829.775677	12.194906
12.981727	820.970518	12.199923
12.745863	824.100249	12.204941
12.633584	824.073688	12.209959
12.935854	830.375956	12.214976
12.594532	822.883794	12.219994
12.967717	816.425264	12.225011
12.658119	810.768004	12.230029
12.363651	802.037724	12.235047
12.593988	821.848875	12.240064
12.810523	823.033141	12.245082
12.838195	828.643117	12.250099
12.499979	830.564410	12.255117
12.559900	824.760885	12.260135
13.245317	825.707582	12.265152
12.296203	827.642538	12.270170
12.767492	826.609343	12.275187
12.841599	834.171836	12.280205
12.462623	833.278173	12.285223
12.798857	830.943831	12.290240
12.269985	826.750529	12.295258
12.821810	819.402458	12.300275
12.587206	834.994498	12.305293
12.618882	833.667257	12.310311
12.812383	829.976166	12.315328
12.748871	831.305298	12.320346
13.006809	834.660625	12.325363
13.035687	849.845316	12.330381
13.480400	838.181013	12.335399
12.741947	826.550615	12.340416
12.587800	832.346872	12.345434
13.245916	833.742824	12.350451
12.990535	838.232637	12.355469
12.898837	825.083922	12.360487
12.840086	829.735433	12.365504
12.922991	851.595782	12.370522
13.097698	846.108788	12.375539
13.130190	852.566944	12.380557
13.220211	844.571680	12.385575
13.609891	844.725253	12.390592
13.331516	837.624018	12.395610
13.241641	818.261124	12.400627
12.884172	822.940501	12.405645
12.973183	828.092733	12.410663
13.510755	819.074287	12.415680
12.922465	820.267886	12.420698
12.907090	818.862810	12.425715
13.089465	815.804637	12.430733
12.966244	827.387055	12.435751
13.374925	831.062752	12.440768
13.104949	829.211563	12.445786
13.074297	834.600300	12.450803
13.252007	846.009345	12.455821
13.225597	848.907443	12.460839
13.453854	841.202953	12.465856
13.076099	852.206717	12.470874
13.391427	854.442190	12.475891
13.285875	856.371214	12.480909
13.401988	851.843315	12.485927
13.527950	839.818690	12.490944
13.277441	837.775098	12.495962
13.281403	827.663116	12.500979
13.375345	832.587355	12.505997
13.494678	835.532045	12.511015
13.181971	826.031424	12.516032
13.024880	842.425539	12.521050
12.900574	836.272171	12.526067
13.224801	847.891795	12.531085
13.345697	848.996372	12.536103
13.551182	837.817685	12.541120
13.243505	845.654599	12.546138
13.509943	845.281518	12.551155
13.621150	840.293634	12.556173
13.331077	843.744292	12.561191
13.441514	848.000062	12.566208
13.419374	846.425627	12.571226
13.662376	852.254342	12.576243
13.814805	850.441112	12.581261
13.323618	849.214727	12.586279
13.847402	841.444998	12.591296
13.235400	848.963516	12.596314
13.681280	851.875980	12.601331
14.081710	843.803679	12.606349
13.629771	842.208221	12.611367
13.957471	838.322529	12.616384
13.766783	840.356411	12.621402
13.889298	833.299664	12.626419
13.977267	836.470179	12.631437
13.621854	843.456177	12.636455
13.795818	834.747163	12.641472
13.625182	840.770073	12.646490
13.858121	839.114646	12.651507
14.285412	839.394873	12.656525
13.973906	824.920420	12.661543
13.992505	815.071244	12.666560
13.652948	819.028277	12.671578
13.665649	807.277045	12.676595
13.355608	805.286966	12.681613
13.907322	818.499352	12.686631
14.041516	822.331665	12.691648
13.704458	816.580873	12.696666
13.692687	821.452243	12.701683
13.878759	831.335687	12.706701
13.883270	831.041515	12.711719
13.912242	833.624814	12.716736
13.572910	834.135611	12.721754
13.951094	840.586938	12.726771
14.017842	840.393469	12.731789
13.877268	836.808369	12.736807
14.322354	830.609973	12.741824
13.886535	842.793655	12.746842
13.804555	841.673573	12.751859
14.079905	835.678498	12.756877
13.854616	839.488241	12.761895
13.948621	838.507847	12.766912
14.183403	842.157143	12.771930
14.161573	848.522821	12.776947
13.946396	846.022404	12.781965
13.899013	848.270523	12.786983
13.923105	836.640566	12.792000
14.005444	843.365469	12.797018
13.638388	842.387884	12.802035
13.789170	846.649957	12.807053
13.861026	851.009605	12.812071
13.810215	845.772544	12.817088
13.736603	854.459588	12.822106
14.130857	868.372038	12.827123
14.227046	863.023576	12.832141
14.279755	874.641576	12.837159
14.515700	872.111499	12.842176
14.212696	874.024124	12.847194
14.516858	866.487615	12.852211
14.291361	859.368618	12.857229
14.172011	851.434557	12.862247
14.073076	838.204914	12.867264
14.081315	848.220374	12.872282
14.319539	862.750570	12.877299
14.546291	860.629042	12.882317
14.216811	872.897071	12.887335
14.547450	869.771477	12.892352
14.417835	875.945765	12.897370
14.411962	873.731293	12.902387
14.535139	852.722330	12.907405
14.128474	850.905178	12.912423
14.701654	861.002547	12.917440
14.282643	856.050395	12.922458
14.118719	866.629338	12.927475
14.223951	868.238153	12.932493
14.375020	878.777217	12.937511
14.282035	870.343546	12.942528
14.219261	880.897181	12.947546
14.203886	879.492100	12.952563
14.456706	868.684682	12.957581
14.130199	870.512624	12.962599
14.558188	871.966727	12.967616
14.677265	870.502711	12.972634
14.460778	873.402191	12.977651
14.720313	873.140646	12.982669
14.486599	876.459401	12.987687
14.882959	866.898155	12.992704
14.846316	874.850411	12.997722
14.135381	873.245035	13.002739
14.455734	868.644105	13.007757
14.308432	883.007499	13.012775
14.739562	883.318684	13.017792
14.612881	898.180643	13.022810
14.614846	898.268729	13.027827
14.840310	896.368310	13.032845
14.731307	898.348374	13.037863
14.381344	891.435062	13.042880
14.641537	898.204704	13.047898
14.816760	893.828483	13.052915
15.083099	898.580559	13.057933
14.921030	888.324139	13.062951
15.062039	891.584185	13.067968
15.048767	899.671648	13.072986
14.832538	905.266212	13.078003
15.031943	894.694371	13.083021
14.602887	897.201117	13.088039
15.209071	890.526170	13.093056
14.847561	893.432596	13.098074
14.480417	896.907963	13.103091
14.662530	888.169244	13.108109
14.566904	891.223363	13.113127
14.980200	894.453372	13.118144
15.504876	891.114332	13.123162
15.127419	897.018184	13.128179
15.295170	888.322740	13.133197
14.900742	897.558699	13.138215
15.035650	893.116209	13.143232
14.800106	894.103062	13.148250
14.602975	900.672954	13.153267
14.669530	884.599150	13.158285
14.639819	897.094789	13.163303
14.859711	896.706908	13.168320
14.998312	901.359075	13.173338
14.829882	915.596413	13.178355
15.264568	915.648260	13.183373
15.120069	920.338476	13.188391
15.201055	919.925020	13.193408
15.068259	914.053829	13.198426
15.110252	920.775615	13.203443
14.979391	920.452157	13.208461
15.295178	925.414248	13.213479
15.589677	915.588063	13.218496
15.445242	920.578077	13.223514
15.310872	932.623068	13.228531
15.497707	916.795484	13.233549
15.254671	922.277486	13.238567
15.457529	917.641303	13.243584
15.602370	917.950006	13.248602
14.817298	908.356089	13.253619
15.535708	898.343571	13.258637
15.270124	909.534928	13.263655
15.220572	913.124644	13.268672
15.350207	923.080098	13.273690
15.382782	922.311301	13.278707
15.570020	915.739855	13.283725
15.605258	928.051766	13.288743
15.767705	921.402149	13.293760
15.715312	918.686863	13.298778
15.674752	912.211071	13.303795
15.931150	902.813750	13.308813
15.482809	896.152541	13.313831
15.079840	889.294873	13.318848
15.165975	896.991211	13.323866
15.122970	913.601051	13.328883
15.256674	913.920967	13.333901
15.140746	918.193286	13.338919
15.293057	918.756445	13.343936
15.539714	911.074289	13.348954
15.120705	921.096769	13.353971
15.465362	923.116211	13.358989
15.581086	931.571651	13.364007
16.130625	941.227791	13.369024
16.018762	934.157233	13.374042
15.763293	930.040993	13.379059
15.908293	909.909035	13.384077
15.581012	917.562856	13.389095
15.584419	924.612588	13.394112
15.904098	910.660880	13.399130
15.577184	917.579324	13.404147
16.084566	914.798424	13.409165
15.858257	924.497217	13.414183
15.833749	916.740777	13.419200
15.822184	910.926333	13.424218
15.811464	922.683695	13.429235
15.714295	911.486108	13.434253
16.061990	927.551897	13.439271
15.664236	926.314023	13.444288
16.171098	928.854020	13.449306
16.000725	923.859736	13.454323
15.344143	923.132642	13.459341
15.244078	930.782428	13.464359
15.384892	941.925909	13.469376
16.070356	945.154310	13.474394
15.743581	943.018511	13.479411
15.827549	947.130126	13.484429
15.849494	943.860377	13.489447
15.923792	944.195913	13.494464
15.877979	946.942428	13.499482
15.903950	966.444925	13.504499
16.313510	971.158801	13.509517
16.533252	972.998999	13.514535
16.333235	957.724310	13.519552
16.367969	945.145848	13.524570
16.274547	946.145152	13.529587
16.236373	942.389348	13.534605
16.633344	938.461223	13.539623
16.555551	944.163500	13.544640
16.765222	944.099120	13.549658
16.459193	940.924940	13.554675
16.274250	943.664851	13.559693
16.523428	943.998234	13.564711
16.443433	942.546467	13.569728
16.839041	932.783328	13.574746
16.169221	922.780015	13.579763
16.531434	920.943377	13.584781
16.472940	909.878591	13.589799
16.059731	910.224235	13.594816
16.161086	913.168599	13.599834
16.216389	912.109056	13.604851
16.323560	927.395157	13.609869
16.642385	936.560410	13.614887
16.340653	936.778133	13.619904
16.653749	936.637586	13.624922
16.587481	928.278598	13.629939
16.373500	927.662043	13.634957
16.543938	933.498998	13.639975
16.027465	935.527128	13.644992
16.518946	934.796885	13.650010
16.385597	946.724958	13.655027
16.290201	937.758287	13.660045
16.233255	942.863992	13.665063
16.376132	940.036055	13.670080
16.427110	940.776042	13.675098
16.623031	940.600204	13.680115
16.388436	936.474380	13.685133
16.483718	940.432738	13.690151
16.107127	945.885178	13.695168
16.684718	947.388433	13.700186
16.511108	970.699799	13.705203
16.795821	963.324091	13.710221
16.701716	968.899541	13.715239
16.501367	970.556244	13.720256
16.786113	966.112351	13.725274
16.916600	964.949504	13.730291
16.722828	968.435592	13.735309
16.531655	979.353394	13.740327
16.631687	974.670189	13.745344
16.908730	970.006590	13.750362
17.036662	973.738928	13.755379
16.669274	969.343560	13.760397
17.062313	967.076042	13.765415
17.046262	973.014814	13.770432
16.710206	962.466867	13.775450
16.942199	972.128594	13.780467
17.184403	972.071740	13.785485
16.992538	962.324888	13.790503
16.727145	970.133140	13.795520
16.916872	961.797146	13.800538
16.901208	965.249015	13.805555
16.949664	971.676310	13.810573
17.081869	959.369753	13.815591
17.152817	965.335918	13.820608
17.176688	961.425218	13.825626
17.145809	962.985939	13.830643
17.115218	967.396381	13.835661
17.306229	962.913525	13.840679
17.069944	964.733653	13.845696
17.123186	959.019496	13.850714
16.989678	965.484766	13.855731
16.897083	959.907070	13.860749
17.112544	962.391740	13.865767
16.713143	967.226051	13.870784
17.173209	981.809950	13.875802
17.196306	983.728299	13.880819
17.795413	989.939933	13.885837
17.805532	981.212336	13.890855
17.175218	973.957899	13.895872
17.035662	968.759953	13.900890
17.273191	971.203296	13.905907
17.211077	987.286009	13.910925
17.416093	972.774689	13.915943
17.333130	997.378426	13.920960
17.635253	989.646519	13.925978
17.580292	980.080185	13.930995
17.422878	992.829435	13.936013
17.523595	994.912353	13.941031
17.229334	990.887385	13.946048
17.440339	986.016372	13.951066
17.708072	992.911105	13.956083
17.584388	982.938959	13.961101
17.592843	991.881462	13.966119
17.331536	996.867718	13.971136
17.481551	985.546147	13.976154
17.867222	986.028564	13.981171
17.658652	990.425871	13.986189
17.722287	978.054303	13.991207
17.728243	988.783431	13.996224
17.656063	988.823173	14.001242
17.305747	983.674024	14.006259
17.558566	989.359230	14.011277
17.806308	988.717668	14.016295
17.629925	978.829523	14.021312
17.667671	980.133333	14.026330
17.661049	982.198353	14.031347
17.487200	983.295468	14.036365
17.576528	983.966331	14.041383
17.663610	985.918837	14.046400
17.490593	989.849814	14.051418
17.686147	989.980154	14.056435
17.650232	985.772695	14.061453
17.942069	977.853052	14.066471
17.272380	991.553589	14.071488
17.773427	1002.094698	14.076506
18.100026	1005.347778	14.081523
17.655662	1015.339568	14.086541
17.860916	1010.841845	14.091559
17.847394	1013.434985	14.096576
18.203319	1018.185680	14.101594
18.413903	1009.877954	14.106611
18.286213	1015.837387	14.111629
18.310330	1008.224772	14.116647
18.121837	1018.059705	14.121664
18.385716	1003.125716	14.126682
18.296329	993.911917	14.131699
18.042361	989.142157	14.136717
17.832659	985.956033	14.141735
17.904897	997.261776	14.146752
17.995425	1006.664812	14.151770
18.400672	1013.591658	14.156787
18.137569	1017.887060	14.161805
18.125589	1010.759796	14.166823
18.078127	1014.876239	14.171840
18.409744	1017.087090	14.176858
18.626067	1008.431316	14.181875
18.550879	1017.910816	14.186893
18.541324	1006.150317	14.191911
18.261693	992.768985	14.196928
18.072472	987.364214	14.201946
18.199573	988.480451	14.206963
18.680337	1009.196186	14.211981
18.551938	1005.012680	14.216999
17.888181	1002.563588	14.222016
18.345726	1009.567447	14.227034
18.269678	1007.281900	14.232051
18.430952	1012.829974	14.237069
18.529305	1010.864250	14.242087
18.380942	1008.293378	14.247104
18.412582	1006.398069	14.252122
18.708741	1006.746184	14.257139
18.419915	1011.970292	14.262157
18.707409	999.465803	14.267175
18.607457	1006.673777	14.272192
18.817635	1012.450881	14.277210
18.477568	1006.706811	14.282227
18.066689	1010.731867	14.287245
18.936090	1006.786513	14.292263
18.349350	1011.912127	14.297280
18.571862	1012.284404	14.302298
18.809724	1009.356365	14.307315
18.201062	1005.241794	14.312333
18.389760	1004.745186	14.317351
18.820428	1025.049055	14.322368
18.608027	1036.677139	14.327386
19.103985	1024.865827	14.332403
18.773403	1034.401130	14.337421
19.078950	1022.395584	14.342439
18.730840	1026.316132	14.347456
18.949359	1026.755309	14.352474
19.189287	1009.423428	14.357491
18.548173	1023.760160	14.362509
18.597299	1026.921015	14.367527
18.864023	1029.842644	14.372544
18.784611	1031.717097	14.377562
19.192751	1030.292987	14.382579
19.094656	1048.981854	14.387597
19.165668	1034.699770	14.392615
19.435267	1035.942011	14.397632
19.143173	1026.507482	14.402650
19.176335	1024.779196	14.407667
18.740967	1023.408349	14.412685
19.131655	1031.416800	14.417703
19.195229	1028.370893	14.422720
19.134222	1037.314835	14.427738
19.209777	1032.783777	14.432755
18.904087	1031.919647	14.437773
18.973958	1033.619227	14.442791
19.069523	1043.438072	14.447808
18.820079	1033.469822	14.452826
19.222314	1031.226103	14.457843
19.307666	1037.070111	14.462861
19.327784	1026.109704	14.467879
19.454614	1033.976455	14.472896
19.521148	1038.283333	14.477914
19.676924	1031.281260	14.482931
19.270576	1032.660966	14.487949
19.275434	1031.887039	14.492967
19.312406	1032.386220	14.497984
19.664141	1031.608439	14.503002
19.405908	1033.009121	14.508019
19.316464	1032.470883	14.513037
19.198633	1032.625078	14.518055
19.378780	1031.252469	14.523072
19.213896	1034.109175	14.528090
19.279711	1029.365043	14.533107
19.061565	1033.217890	14.538125
19.321901	1041.426656	14.543143
19.736477	1056.030367	14.548160
19.512163	1059.802133	14.553178
19.765233	1050.222214	14.558195
19.771707	1051.565644	14.563213
19.838122	1053.543488	14.568231
19.651694	1039.125005	14.573248
19.503001	1050.698934	14.578266
19.839882	1047.307236	14.583283
19.871404	1055.709654	14.588301
19.747087	1053.636797	14.593319
19.650867	1056.160846	14.598336
19.949234	1057.234474	14.603354
20.000406	1052.237002	14.608371
20.032911	1040.690803	14.613389
19.719069	1030.442301	14.618407
19.779157	1028.804472	14.623424
19.996244	1047.093651	14.628442
19.671653	1044.001258	14.633459
20.063182	1047.332539	14.638477
20.035674	1050.499093	14.643495
20.009257	1052.339998	14.648512
19.802344	1052.561801	14.653530
20.177434	1050.243435	14.658547
20.269661	1055.821276	14.663565
19.853136	1049.082438	14.668583
20.065861	1037.138764	14.673600
19.646654	1042.402244	14.678618
20.034846	1051.764978	14.683635
19.907763	1053.725800	14.688653
20.000280	1058.296863	14.693671
20.331495	1050.614022	14.698688
19.983099	1056.598582	14.703706
19.875114	1058.464890	14.708723
19.492830	1058.379644	14.713741
19.896612	1059.039112	14.718759
20.239592	1058.007074	14.723776
20.014886	1064.489824	14.728794
19.946971	1068.628420	14.733811
20.076029	1069.684393	14.738829
20.055209	1076.384520	14.743847
20.293222	1072.730588	14.748864
20.225367	1072.466686	14.753882
20.350898	1073.299142	14.758899
20.182784	1071.056415	14.763917
20.260962	1068.771943	14.768935
20.505621	1065.098036	14.773952
20.200594	1073.606842	14.778970
20.201797	1073.720296	14.783987
20.625400	1077.551502	14.789005
20.229377	1069.193620	14.794023
20.642278	1068.955381	14.799040
20.609082	1096.126676	14.804058
20.432953	1100.282234	14.809075
20.415972	1091.811303	14.814093
20.360395	1098.671523	14.819111
20.706724	1094.369434	14.824128
20.676557	1106.918941	14.829146
20.626109	1096.029510	14.834163
20.749876	1095.467331	14.839181
20.615685	1099.228141	14.844199
21.073544	1094.485685	14.849216
20.969600	1094.902801	14.854234
20.940623	1089.876849	14.859251
20.724976	1090.440859	14.864269
20.794320	1094.479058	14.869287
20.778968	1088.958649	14.874304
20.710609	1097.408295	14.879322
21.145392	1095.150001	14.884339
20.964376	1087.029831	14.889357
20.739286	1088.927114	14.894375
20.838224	1084.509149	14.899392
20.691837	1084.191276	14.904410
20.755149	1091.304275	14.909427
21.104147	1086.373743	14.914445
21.022645	1084.291018	14.919463
21.032960	1078.596172	14.924480
21.052425	1090.348914	14.929498
20.930667	1095.572118	14.934515
20.948940	1092.369191	14.939533
20.786818	1086.704516	14.944551
21.041008	1090.511773	14.949568
20.935828	1094.473171	14.954586
20.808065	1090.728217	14.959603
21.325891	1113.322345	14.964621
21.249659	1112.901958	14.969639
21.297567	1100.305544	14.974656
21.289841	1089.807068	14.979674
21.320827	1091.575864	14.984691
21.161286	1104.079365	14.989709
21.181802	1112.660265	14.994727
21.334929	1106.251890	14.999744
21.380166	1112.910122	15.004762
21.380071	1117.760807	15.009779
21.486866	1128.240681	15.014797
21.460077	1124.401002	15.019815
21.786897	1115.024095	15.024832
21.393561	1121.624809	15.029850
21.463690	1122.595341	15.034867
21.526821	1123.005216	15.039885
21.851784	1112.849091	15.044903
21.573427	1105.473180	15.049920
21.554329	1100.808607	15.054938
21.808925	1105.518395	15.059955
21.505516	1092.165962	15.064973
21.332646	1092.795855	15.069991
21.697518	1102.143334	15.075008
21.531577	1108.181377	15.080026
21.813969	1112.312436	15.085043
22.036293	1116.279332	15.090061
21.611334	1126.189245	15.095079
21.663251	1118.202985	15.100096
21.439197	1117.812070	15.105114
21.938650	1113.795265	15.110131
21.719521	1110.620063	15.115149
21.295557	1110.831691	15.120167
21.705946	1112.840857	15.125184
22.042132	1111.061928	15.130202
21.711036	1124.397080	15.135219
22.113353	1111.085544	15.140237
21.892041	1108.847990	15.145255
21.495518	1111.974539	15.150272
21.566141	1112.600999	15.155290
21.925704	1114.798015	15.160307
21.923112	1111.371128	15.165325
21.797352	1133.801021	15.170343
21.800172	1147.591976	15.175360
21.953029	1145.147465	15.180378
22.063873	1136.826905	15.185395
21.988932	1134.680028	15.190413
21.909469	1142.860026	15.195431
21.877576	1150.300400	15.200448
22.004974	1139.266309	15.205466
22.189743	1138.072855	15.210483
22.215496	1134.682550	15.215501
21.867031	1140.585094	15.220519
22.675713	1133.316577	15.225536
22.475979	1142.720979	15.230554
22.076707	1140.426095	15.235571
22.192284	1134.840975	15.240589
22.085377	1135.403729	15.245607
22.128051	1134.131549	15.250624
22.520968	1154.820190	15.255642
22.329926	1156.686899	15.260659
22.629278	1145.310270	15.265677
22.597054	1164.970429	15.270695
22.486102	1152.218981	15.275712
22.857595	1138.909097	15.280730
22.556824	1130.763488	15.285747
22.654052	1131.480457	15.290765
22.285279	1132.402987	15.295783
22.651717	1145.685673	15.300800
22.787866	1138.342638	15.305818
22.731138	1143.864946	15.310835
22.653387	1131.711092	15.315853
22.815998	1134.592244	15.320871
22.683736	1129.352082	15.325888
22.869021	1133.978060	15.330906
22.838014	1136.864301	15.335923
22.704274	1125.804858	15.340941
22.648709	1133.924301	15.345959
22.931436	1131.181724	15.350976
22.824929	1135.439995	15.355994
22.648395	1146.178873	15.361011
23.076588	1150.687899	15.366029
22.745930	1159.718333	15.371047
23.153515	1161.775283	15.376064
22.825662	1156.420585	15.381082
22.497427	1156.967522	15.386099
23.232631	1148.530197	15.391117
23.121256	1156.958207	15.396135
22.999302	1152.508559	15.401152
23.261427	1156.936305	15.406170
23.138466	1151.290720	15.411187
23.170502	1156.309958	15.416205
23.039040	1153.752197	15.421223
23.072307	1147.962211	15.426240
23.554976	1155.473451	15.431258
23.259482	1159.035476	15.436275
23.266994	1155.092582	15.441293
23.549386	1149.598091	15.446311
23.271537	1143.127834	15.451328
23.285109	1136.056479	15.456346
23.116749	1153.352081	15.461363
23.611273	1148.285118	15.466381
23.668531	1160.227652	15.471399
23.508723	1151.857968	15.476416
23.337206	1139.718799	15.481434
23.308546	1126.777743	15.486451
23.508776	1127.415456	15.491469
23.375532	1133.773444	15.496487
23.493536	1140.246710	15.501504
23.537270	1135.783730	15.506522
23.451193	1148.843817	15.511539
23.425365	1136.874335	15.516557
23.322298	1159.512151	15.521575
23.362542	1147.046298	15.526592
23.508617	1152.603109	15.531610
23.354814	1155.981981	15.536627
23.592300	1150.608138	15.541645
23.811638	1152.846066	15.546663
23.504156	1148.914655	15.551680
23.370118	1150.652506	15.556698
23.277874	1148.432597	15.561715
23.705915	1147.469280	15.566733
23.598539	1149.824671	15.571751
23.463327	1168.465828	15.576768
24.155090	1170.071140	15.581786
23.809090	1183.452854	15.586803
24.078197	1177.556477	15.591821
23.901783	1176.495353	15.596839
24.135706	1174.394757	15.601856
24.199094	1170.439949	15.606874
23.801848	1156.379462	15.611891
23.933601	1149.482097	15.616909
23.729863	1165.180045	15.621927
23.971460	1180.268570	15.626944
24.422947	1164.310936	15.631962
23.872982	1175.054689	15.636979
24.125759	1168.640147	15.641997
23.994617	1179.996807	15.647015
24.237263	1171.368390	15.652032
24.178666	1170.566528	15.657050
23.986830	1176.801163	15.662067
24.220170	1171.371157	15.667085
24.138827	1173.892892	15.672103
24.175412	1176.449801	15.677120
24.200545	1169.162018	15.682138
23.870815	1175.904270	15.687155
24.250208	1172.916159	15.692173
24.315178	1169.223045	15.697191
24.229313	1183.141535	15.702208
24.450947	1177.363054	15.707226
24.390206	1198.829752	15.712243
24.745539	1198.796200	15.717261
24.503402	1183.190232	15.722279
24.205180	1190.277861	15.727296
24.706502	1192.597850	15.732314
24.321582	1199.692754	15.737331
24.437062	1194.303299	15.742349
24.881935	1192.860798	15.747367
24.601765	1195.309542	15.752384
24.652460	1191.482955	15.757402
24.456284	1191.412732	15.762419
24.616560	1188.263281	15.767437
24.857216	1190.251711	15.772455
24.340115	1200.125606	15.777472
24.782833	1193.359390	15.782490
24.519689	1193.864570	15.787507
24.687473	1196.678648	15.792525
24.987720	1197.859291	15.797543
24.804080	1193.697020	15.802560
24.798438	1205.144490	15.807578
24.640107	1198.955301	15.812595
25.159638	1197.182353	15.817613
24.695249	1199.028775	15.822631
24.752219	1211.978130	15.827648
24.908867	1207.522688	15.832666
25.073157	1222.462408	15.837683
25.091643	1230.393560	15.842701
24.957338	1229.452073	15.847719
24.952639	1229.383408	15.852736
25.311251	1222.365260	15.857754
24.994970	1226.609081	15.862771
25.309365	1229.677915	15.867789
25.469594	1218.490302	15.872807
24.727341	1223.785513	15.877824
25.219021	1214.568925	15.882842
25.217504	1215.841034	15.887859
25.037987	1215.203288	15.892877
25.184704	1214.984662	15.897895
24.905258	1223.691512	15.902912
25.153257	1216.987354	15.907930
25.164870	1221.328128	15.912947
25.427698	1234.415666	15.917965
25.574256	1237.725402	15.922983
25.652012	1244.851978	15.928000
26.009577	1231.582080	15.933018
25.799171	1220.581929	15.938035
25.194689	1212.130403	15.943053
25.836665	1213.781391	15.948071
25.618447	1222.046284	15.953088
25.920829	1205.689080	15.958106
25.689660	1221.230423	15.963123
25.854371	1215.849027	15.968141
25.913644	1210.493622	15.973159
25.634154	1201.091741	15.978176
25.769371	1200.111182	15.983194
25.949389	1204.788499	15.988211
25.632633	1209.338515	15.993229
25.806955	1205.498868	15.998247
25.843015	1204.612743	16.003264
25.934599	1202.493418	16.008282
25.626487	1202.169322	16.013299
25.976221	1197.282828	16.018317
25.967021	1200.651676	16.023335
25.801834	1212.237761	16.028352
26.133067	1217.169111	16.033370
25.878027	1207.457271	16.038387
25.776414	1212.626857	16.043405
25.962923	1224.871088	16.048423
26.071186	1229.209345	16.053440
25.980940	1233.051664	16.058458
25.950404	1234.565015	16.063475
26.431058	1243.338983	16.068493
26.202839	1229.861051	16.073511
25.760236	1238.221070	16.078528
26.175315	1236.647528	16.083546
26.261202	1236.716155	16.088563
26.164306	1229.242332	16.093581
26.374433	1225.289769	16.098599
26.209553	1238.403295	16.103616
26.173727	1236.796254	16.108634
26.183633	1243.908214	16.113651
26.478007	1248.277278	16.118669
27.083528	1248.996668	16.123687
26.885447	1237.963016	16.128704
26.608669	1222.277231	16.133722
26.787788	1231.963163	16.138739
26.550480	1227.458984	16.143757
26.640070	1224.402656	16.148775
26.360167	1225.671043	16.153792
26.194944	1228.553080	16.158810
26.426232	1227.876217	16.163827
26.415060	1235.827798	16.168845
26.750478	1246.947292	16.173863
27.103153	1250.953758	16.178880
27.093661	1246.341293	16.183898
26.962177	1232.049751	16.188915
26.799011	1228.461800	16.193933
27.041268	1221.259903	16.198951
26.531875	1230.261569	16.203968
26.822985	1218.898809	16.208986
26.789944	1228.419156	16.214003
26.659082	1236.430518	16.219021
26.972450	1243.485463	16.224039
27.003594	1251.790198	16.229056
27.065534	1255.015361	16.234074
27.348030	1247.822928	16.239091
27.013042	1256.936144	16.244109
27.239919	1245.602366	16.249127
27.196317	1245.419871	16.254144
27.370359	1240.002292	16.259162
26.891224	1248.424846	16.264179
27.363731	1248.451834	16.269197
27.864080	1251.021302	16.274215
27.146494	1226.659474	16.279232
27.051804	1221.836293	16.284250
27.344920	1227.439520	16.289267
27.275437	1236.634208	16.294285
27.765718	1229.585960	16.299303
27.113664	1238.559487	16.304320
27.456149	1235.974796	16.309338
27.535558	1238.941588	16.314355
27.381006	1239.530746	16.319373
27.592997	1241.915009	16.324391
27.107455	1241.530345	16.329408
27.322031	1241.739763	16.334426
27.689407	1243.746216	16.339443
27.756573	1251.076434	16.344461
27.633665	1241.037747	16.349479
27.398700	1246.613260	16.354496
27.742122	1234.664758	16.359514
27.952695	1239.671825	16.364531
27.410260	1246.895573	16.369549
27.933212	1238.081189	16.374567
27.968443	1243.563873	16.379584
27.480105	1239.992152	16.384602
27.552869	1236.768038	16.389619
27.649087	1237.583003	16.394637
27.668126	1242.055168	16.399655
27.495127	1255.135264	16.404672
27.751915	1266.393327	16.409690
28.195490	1262.637719	16.414707
28.128940	1274.315692	16.419725
28.091378	1265.264054	16.424743
28.192461	1268.978569	16.429760
28.060802	1275.371074	16.434778
28.466082	1272.426230	16.439795
28.395423	1270.486958	16.444813
28.513807	1257.582733	16.449831
27.907926	1250.198115	16.454848
27.914690	1261.025113	16.459866
28.151956	1258.027696	16.464883
27.993766	1266.321076	16.469901
28.162684	1265.587709	16.474919
28.117057	1265.815803	16.479936
28.099570	1267.560652	16.484954
28.091215	1258.962052	16.489971
27.851494	1268.483243	16.494989
28.073899	1277.868916	16.500007
28.583611	1287.190642	16.505024
28.547499	1294.290896	16.510042
28.513540	1291.304410	16.515059
28.428758	1297.916807	16.520077
28.738598	1292.553677	16.525095
29.137447	1299.693086	16.530112
28.805888	1304.725150	16.535130
28.584012	1278.770728	16.540147
28.967339	1276.706675	16.545165
28.923662	1277.316333	16.550183
28.843112	1271.395811	16.555200
28.811635	1269.226328	16.560218
28.940992	1266.700273	16.565235
28.605213	1260.264297	16.570253
28.929553	1259.938943	16.575271
28.834875	1261.938893	16.580288
28.618570	1266.583643	16.585306
28.949880	1281.430970	16.590323
28.954022	1286.798612	16.595341
29.048492	1288.541702	16.600359
29.084322	1288.330981	16.605376
28.900697	1284.771472	16.610394
29.074470	1293.382098	16.615411
28.806644	1292.537269	16.620429
28.743020	1293.651848	16.625447
29.112895	1287.241008	16.630464
29.322779	1295.555630	16.635482
29.320170	1285.526473	16.640499
29.392846	1296.608266	16.645517
29.385959	1284.859789	16.650535
29.331323	1293.686090	16.655552
29.263777	1302.429208	16.660570
29.650130	1285.755804	16.665587
28.946118	1296.738370	16.670605
29.627807	1297.123922	16.675623
29.649054	1298.250451	16.680640
29.310853	1292.161998	16.685658
29.600596	1293.388478	16.690675
29.284585	1286.589617	16.695693
29.454058	1288.387231	16.700711
29.493933	1288.005455	16.705728
29.459785	1285.612317	16.710746
29.901652	1279.284878	16.715763
29.386961	1284.099465	16.720781
29.360542	1303.279163	16.725799
29.752613	1307.708679	16.730816
29.541237	1307.845973	16.735834
30.000021	1306.858896	16.740851
29.741882	1318.320752	16.745869
29.698770	1314.587735	16.750887
29.624449	1302.846656	16.755904
29.748432	1310.426784	16.760922
29.922026	1300.985421	16.765939
29.956788	1312.758005	16.770957
29.746956	1306.810387	16.775975
30.058692	1301.513233	16.780992
29.844845	1314.296801	16.786010
30.046453	1301.489962	16.791027
29.658636	1313.713781	16.796045
29.883322	1323.894419	16.801063
29.952871	1330.741436	16.806080
29.875332	1337.636749	16.811098
30.391286	1332.342305	16.816115
30.230407	1335.305733	16.821133
30.023007	1333.911767	16.826151
30.348638	1332.936083	16.831168
30.102644	1331.450329	16.836186
30.277397	1325.474009	16.841203
30.412542	1334.276908	16.846221
30.233087	1335.005676	16.851239
30.426175	1343.733226	16.856256
30.403965	1356.423679	16.861274
30.477678	1354.300824	16.866291
30.824632	1362.054333	16.871309
30.734442	1352.509099	16.876327
30.597647	1341.983357	16.881344
30.692073	1356.659568	16.886362
30.667665	1355.549369	16.891379
30.882916	1354.846611	16.896397
30.836550	1341.138121	16.901415
30.763780	1338.280790	16.906432
30.380582	1342.121692	16.911450
30.894304	1346.645771	16.916467
30.974596	1358.764718	16.921485
30.808435	1344.677344	16.926503
30.874460	1348.510983	16.931520
30.525101	1352.532786	16.936538
30.735665	1349.429080	16.941555
30.708773	1356.925564	16.946573
31.148458	1348.761676	16.951591
30.912267	1352.286044	16.956608
30.852588	1348.293671	16.961626
30.699089	1343.347121	16.966643
30.891498	1344.658286	16.971661
31.281561	1367.878698	16.976679
31.627947	1363.286187	16.981696
31.001656	1357.956095	16.986714
31.246591	1364.889261	16.991731
31.754383	1371.860144	16.996749
31.532421	1364.693051	17.001767
31.796645	1354.883993	17.006784
31.273749	1348.054404	17.011802
31.403428	1347.882630	17.016819
31.233021	1350.206895	17.021837
31.129461	1359.908782	17.026855
31.692689	1366.037805	17.031872
31.470271	1367.489708	17.036890
31.716179	1370.121151	17.041907
32.124469	1373.803336	17.046925
31.844101	1361.643198	17.051943
32.072455	1349.078300	17.056960
31.475010	1343.210337	17.061978
31.529437	1341.342981	17.066995
31.929898	1353.616899	17.072013
31.983150	1354.741574	17.077031
32.083020	1345.687297	17.082048
31.845203	1339.403210	17.087066
31.647729	1343.843048	17.092083
31.806182	1354.627401	17.097101
31.572424	1368.483996	17.102119
32.013028	1365.120172	17.107136
31.737030	1367.981716	17.112154
31.660925	1363.231328	17.117171
32.125719	1358.370946	17.122189
31.763585	1363.748660	17.127207
31.970358	1367.159444	17.132224
31.887904	1370.609232	17.137242
32.099042	1371.071667	17.142259
32.202805	1379.920533	17.147277
32.424689	1394.210712	17.152295
32.265502	1385.651463	17.157312
32.250332	1391.539741	17.162330
32.505292	1384.632449	17.167347
32.445489	1383.884418	17.172365
32.584429	1397.089320	17.177383
32.832079	1394.099722	17.182400
32.315962	1388.692396	17.187418
32.578415	1384.138278	17.192435
32.703742	1384.538415	17.197453
32.528175	1398.464815	17.202471
32.321305	1387.230467	17.207488
32.419844	1397.535058	17.212506
32.573855	1395.797269	17.217523
33.162097	1396.648768	17.222541
32.668121	1403.255884	17.227559
32.529720	1399.364202	17.232576
32.707754	1398.389548	17.237594
32.731965	1394.229379	17.242611
33.063030	1392.242933	17.247629
32.816855	1400.531223	17.252647
32.882516	1392.678394	17.257664
32.514137	1391.278086	17.262682
32.632650	1387.109455	17.267699
32.737677	1378.874905	17.272717
32.488814	1389.757812	17.277735
33.077645	1403.343534	17.282752
32.663050	1415.167653	17.287770
32.333782	1425.454078	17.292787
32.742459	1409.954237	17.297805
32.925351	1420.242470	17.302823
33.253476	1435.693214	17.307840
33.328862	1426.159870	17.312858
33.539576	1430.254894	17.317875
33.780001	1427.588331	17.322893
33.355299	1425.158530	17.327911
33.324701	1412.665720	17.332928
33.704491	1420.051173	17.337946
33.359173	1409.128851	17.342963
33.731187	1416.225172	17.347981
33.606671	1418.599063	17.352999
33.549661	1404.557660	17.358016
33.669423	1409.023553	17.363034
33.493270	1423.906323	17.368051
33.768312	1420.723071	17.373069
33.890239	1430.923027	17.378087
33.954214	1421.946923	17.383104
33.767039	1425.050193	17.388122
34.021220	1426.342217	17.393139
33.722553	1408.816611	17.398157
33.697456	1419.572954	17.403175
33.770876	1422.105192	17.408192
34.046946	1422.645821	17.413210
33.703381	1425.344382	17.418227
34.063584	1426.521960	17.423245
33.847318	1422.087022	17.428263
33.946921	1423.415889	17.433280
34.086535	1429.923745	17.438298
34.025336	1431.965808	17.443315
34.403808	1427.431374	17.448333
34.264833	1431.107792	17.453351
34.224186	1420.731050	17.458368
34.181240	1423.515061	17.463386
34.220948	1432.033144	17.468403
34.776144	1413.142924	17.473421
34.270757	1431.646683	17.478439
34.178211	1425.096795	17.483456
34.104921	1413.857281	17.488474
34.158143	1425.532367	17.493491
34.174165	1440.107315	17.498509
34.677190	1454.056833	17.503527
34.724087	1453.336265	17.508544
34.687595	1456.696813	17.513562
34.835672	1456.342265	17.518579
34.915447	1458.153949	17.523597
34.733584	1454.698277	17.528615
34.762674	1452.983210	17.533632
35.039726	1447.069721	17.538650
35.229058	1448.334036	17.543667
34.801262	1430.677153	17.548685
34.857670	1427.417696	17.553703
34.676623	1417.406955	17.558720
34.955898	1427.383430	17.563738
34.413396	1434.701941	17.568755
34.717166	1441.925736	17.573773
34.413979	1441.572460	17.578791
34.503959	1448.877093	17.583808
34.452780	1452.498731	17.588826
34.901448	1470.483802	17.593843
35.115677	1466.268598	17.598861
35.306146	1473.607992	17.603879
35.062450	1469.227835	17.608896
35.759888	1474.764636	17.613914
35.322971	1475.132938	17.618931
35.316670	1471.630820	17.623949
35.683400	1467.682071	17.628967
35.202558	1481.403887	17.633984
35.684224	1476.853273	17.639002
35.127854	1475.299364	17.644019
35.482756	1468.458437	17.649037
35.376796	1476.961493	17.654055
35.447477	1470.843631	17.659072
35.807322	1473.387807	17.664090
35.160936	1474.824089	17.669107
35.702866	1476.478155	17.674125
35.501391	1479.277544	17.679143
35.698017	1490.573579	17.684160
36.235149	1494.974102	17.689178
35.856674	1481.213392	17.694195
36.175758	1473.655355	17.699213
35.760802	1464.138852	17.704231
36.017479	1465.152763	17.709248
36.290788	1477.430907	17.714266
35.958579	1476.245843	17.719283
36.039177	1463.568308	17.724301
36.171611	1471.809936	17.729319
36.175880	1474.567621	17.734336
36.385672	1473.449125	17.739354
36.201433	1461.469529	17.744371
36.327158	1466.859204	17.749389
36.043200	1466.790108	17.754407
36.726261	1476.255198	17.759424
36.250961	1469.042544	17.764442
36.120512	1476.214457	17.769459
36.208792	1482.424246	17.774477
36.153677	1481.501897	17.779495
36.704658	1483.252381	17.784512
36.893626	1486.962640	17.789530
36.666368	1488.235420	17.794547
36.991741	1482.872957	17.799565
36.959897	1477.367636	17.804583
36.667089	1485.148847	17.809600
36.727104	1480.241394	17.814618
36.515664	1486.056306	17.819635
37.144992	1486.535279	17.824653
37.084153	1483.145850	17.829671
36.353651	1477.267129	17.834688
36.897851	1480.808114	17.839706
36.390850	1483.049425	17.844723
36.837424	1474.619299	17.849741
36.734062	1478.993930	17.854759
36.992840	1481.588657	17.859776
37.039185	1477.049440	17.864794
36.784305	1471.055174	17.869811
37.092534	1483.498274	17.874829
37.089375	1473.712109	17.879847
36.577534	1478.996541	17.884864
36.815556	1487.994848	17.889882
37.027847	1510.564762	17.894899
37.329860	1504.612628	17.899917
37.530109	1509.523554	17.904935
37.623481	1512.614443	17.909952
37.388972	1508.479003	17.914970
37.259475	1510.964146	17.919987
37.321962	1503.253785	17.925005
37.351185	1503.842561	17.930023
37.460126	1503.626695	17.935040
37.832191	1499.503525	17.940058
37.424112	1504.055299	17.945075
37.534520	1502.403231	17.950093
37.521174	1495.436942	17.955111
37.562439	1500.843017	17.960128
38.056828	1505.752040	17.965146
37.947497	1505.794447	17.970163
37.679424	1501.566433	17.975181
38.172327	1505.809777	17.980199
38.121672	1506.240645	17.985216
38.006556	1498.586516	17.990234
37.828237	1500.454422	17.995251
38.027185	1493.410689	18.000269
38.194602	1499.977335	18.005287
37.896986	1522.510384	18.010304
38.237152	1523.530153	18.015322
38.087783	1528.508485	18.020339
38.251384	1518.945491	18.025357
38.437129	1522.252296	18.030375
38.353012	1514.681671	18.035392
38.574442	1514.053682	18.040410
38.338234	1525.515390	18.045427
38.322815	1517.129224	18.050445
38.119144	1514.039895	18.055463
38.155802	1513.889006	18.060480
38.403321	1519.524717	18.065498
38.411052	1517.929762	18.070515
38.152784	1525.131190	18.075533
38.315655	1535.653013	18.080551
38.532747	1540.917935	18.085568
38.772949	1547.059760	18.090586
38.684314	1546.811730	18.095603
38.534768	1554.497937	18.100621
38.984232	1550.359473	18.105639
39.149312	1538.053680	18.110656
38.950175	1541.307175	18.115674
38.991062	1542.547415	18.120691
39.168264	1544.744654	18.125709
39.218779	1538.074475	18.130727
39.049599	1535.361612	18.135744
39.393498	1536.841572	18.140762
39.016542	1538.011570	18.145779
38.901692	1535.817246	18.150797
38.944336	1537.824115	18.155815
39.009035	1536.608420	18.160832
38.889264	1527.774668	18.165850
39.127539	1535.845099	18.170867
39.017259	1540.994046	18.175885
39.293524	1551.008934	18.180903
38.818798	1565.111730	18.185920
39.491091	1559.098407	18.190938
39.670577	1558.442273	18.195955
39.587378	1556.312419	18.200973
39.589933	1550.296728	18.205991
39.737018	1559.640698	18.211008
39.742761	1558.595194	18.216026
39.727400	1555.659401	18.221043
39.624417	1564.411355	18.226061
39.995949	1554.298181	18.231079
39.423170	1555.565137	18.236096
39.559992	1555.676281	18.241114
40.003096	1556.127625	18.246131
39.748535	1556.767178	18.251149
39.810984	1556.628027	18.256167
39.904318	1566.220278	18.261184
40.225517	1577.351674	18.266202
40.394117	1582.412755	18.271219
40.159245	1578.996923	18.276237
40.423894	1569.645301	18.281255
40.033971	1565.704622	18.286272
40.345988	1564.800491	18.291290
40.514596	1570.704218	18.296307
40.339450	1571.356576	18.301325
40.334873	1557.770768	18.306343
40.073340	1571.925380	18.311360
40.064173	1574.795645	18.316378
40.538804	1572.780374	18.321395
40.179561	1581.976454	18.326413
40.611924	1571.374028	18.331431
40.371557	1578.089804	18.336448
40.409915	1573.040543	18.341466
40.619199	1585.363509	18.346483
40.772685	1580.621275	18.351501
40.804765	1579.350724	18.356519
40.703919	1588.537882	18.361536
40.557776	1574.857470	18.366554
40.546006	1594.066745	18.371571
40.354865	1602.734693	18.376589
40.904696	1597.819897	18.381607
40.802768	1608.528427	18.386624
41.040646	1600.699020	18.391642
41.537676	1606.125243	18.396659
41.169623	1600.827204	18.401677
41.326708	1601.089818	18.406695
41.343348	1608.649019	18.411712
41.078235	1604.057576	18.416730
41.224231	1608.945470	18.421747
41.172889	1612.248410	18.426765
41.414250	1603.875624	18.431783
41.284142	1607.361328	18.436800
41.610779	1609.336334	18.441818
41.362540	1604.391931	18.446835
41.595286	1622.884386	18.451853
41.600125	1619.793930	18.456871
41.715445	1636.152402	18.461888
41.861313	1622.883823	18.466906
41.730923	1615.159449	18.471923
41.427713	1627.247140	18.476941
41.606415	1626.023045	18.481959
41.706775	1626.701672	18.486976
41.770142	1625.584016	18.491994
41.950980	1623.513778	18.497011
41.716099	1626.103815	18.502029
41.759603	1618.257515	18.507047
41.986115	1628.024605	18.512064
41.922688	1627.024650	18.517082
41.899826	1627.956127	18.522099
41.823333	1642.170170	18.527117
42.213005	1648.878785	18.532135
42.222695	1647.646453	18.537152
42.061448	1651.755622	18.542170
42.546541	1640.169687	18.547187
42.184808	1648.346800	18.552205
42.562194	1641.306613	18.557223
42.351501	1648.399643	18.562240
42.528782	1647.021125	18.567258
42.704864	1641.189669	18.572275
42.063041	1651.866041	18.577293
42.559044	1647.363634	18.582311
42.448225	1649.520801	18.587328
42.600933	1648.906731	18.592346
42.466176	1641.350298	18.597363
41.912091	1661.089609	18.602381
42.564785	1668.605989	18.607399
42.833869	1677.792042	18.612416
42.715471	1676.696549	18.617434
43.096576	1670.785620	18.622451
42.769708	1680.945574	18.627469
42.978889	1665.221133	18.632487
42.937419	1667.831370	18.637504
43.099737	1667.906960	18.642522
43.210869	1673.803946	18.647539
43.103160	1669.740127	18.652557
43.183407	1660.338449	18.657575
43.283118	1661.676785	18.662592
43.202781	1673.944197	18.667610
43.604365	1675.244706	18.672627
43.600931	1686.344976	18.677645
43.587073	1685.539237	18.682663
43.327977	1668.051361	18.687680
43.637209	1679.793806	18.692698
43.790263	1682.556617	18.697715
43.472281	1682.436042	18.702733
43.510855	1687.874154	18.707751
44.026582	1683.750526	18.712768
43.796696	1691.547216	18.717786
43.775159	1685.118660	18.722803
43.551028	1690.610557	18.727821
43.864849	1678.404448	18.732839
43.762133	1679.982798	18.737856
43.905299	1690.533048	18.742874
43.721560	1672.187549	18.747891
43.750780	1684.986949	18.752909
44.009030	1676.668292	18.757927
43.895452	1678.990007	18.762944
43.901087	1691.007259	18.767962
44.210014	1692.871433	18.772979
43.943455	1701.011567	18.777997
44.223402	1706.029989	18.783015
44.423603	1701.204660	18.788032
44.521274	1701.056834	18.793050
44.520394	1688.852684	18.798067
44.448418	1691.676001	18.803085
44.787233	1695.848853	18.808103
44.641504	1689.897376	18.813120
44.424591	1688.444907	18.818138
45.080302	1689.087022	18.823155
44.443715	1695.486199	18.828173
44.675054	1683.829532	18.833191
44.697421	1691.283723	18.838208
44.565984	1687.147873	18.843226
44.656482	1688.929496	18.848243
44.499669	1704.718401	18.853261
44.961176	1710.775113	18.858279
45.073644	1718.070020	18.863296
44.940995	1725.135073	18.868314
45.179364	1724.469708	18.873331
45.016451	1722.055657	18.878349
45.190478	1722.694342	18.883367
45.097001	1720.136859	18.888384
45.093040	1718.161840	18.893402
45.437565	1714.771978	18.898419
45.320322	1719.284550	18.903437
45.509105	1714.173809	18.908455
45.555305	1714.636847	18.913472
45.313323	1714.725286	18.918490
45.374238	1704.168354	18.923507
45.601539	1712.152216	18.928525
45.845441	1710.270917	18.933543
45.511367	1713.211046	18.938560
45.660161	1726.424117	18.943578
46.021625	1740.752670	18.948595
45.827822	1748.739405	18.953613
45.823370	1728.478454	18.958631
46.129696	1738.334092	18.963648
45.904349	1742.828892	18.968666
46.092484	1746.722385	18.973683
46.349844	1742.973762	18.978701
45.738431	1737.764308	18.983719
46.047676	1741.780846	18.988736
46.103899	1735.472642	18.993754
45.962830	1725.550145	18.998771
46.145672	1740.888207	19.003789
46.519155	1727.754314	19.008807
46.480534	1729.161669	19.013824
46.314804	1728.313446	19.018842
46.296273	1737.282642	19.023859
46.633000	1735.576158	19.028877
46.610351	1733.941760	19.033895
46.665430	1729.707245	19.038912
46.653774	1734.130690	19.043930
47.048209	1728.763646	19.048947
46.784011	1726.393868	19.053965
46.677957	1730.361854	19.058983
46.805412	1726.737736	19.064000
46.537160	1731.835744	19.069018
46.619581	1725.794856	19.074035
46.682345	1742.584567	19.079053
46.774445	1753.366933	19.084071
47.078263	1759.893367	19.089088
46.931070	1758.578303	19.094106
46.892400	1751.306592	19.099123
46.927167	1755.369293	19.104141
46.802246	1758.750065	19.109159
46.963912	1747.719699	19.114176
46.595725	1763.434467	19.119194
47.018314	1780.114185	19.124211
47.129621	1790.161364	19.129229
47.456977	1783.223641	19.134247
47.699052	1776.223537	19.139264
47.367383	1778.415320	19.144282
47.178417	1780.149214	19.149299
47.432355	1784.960279	19.154317
47.540681	1799.044496	19.159335
47.599230	1796.860845	19.164352
47.954622	1798.506296	19.169370
48.028451	1797.020890	19.174387
48.073574	1794.716257	19.179405
47.932873	1794.545813	19.184423
48.010775	1791.336575	19.189440
47.930280	1790.213044	19.194458
48.530607	1783.257801	19.199475
48.209601	1793.237006	19.204493
48.152985	1791.027214	19.209511
48.408010	1788.743347	19.214528
48.208424	1796.087178	19.219546
48.567129	1784.259002	19.224563
48.600878	1785.434100	19.229581
48.783902	1784.783716	19.234599
48.640569	1777.673570	19.239616
48.561584	1792.370995	19.244634
48.192878	1790.490988	19.249651
48.629799	1779.584746	19.254669
48.621390	1781.795315	19.259687
48.493464	1781.979502	19.264704
48.582423	1786.415600	19.269722
48.999563	1780.388528	19.274739
48.584384	1783.038397	19.279757
48.820970	1784.446822	19.284775
49.007653	1776.265573	19.289792
48.730492	1785.259534	19.294810
48.754261	1781.345515	19.299827
48.906214	1776.470917	19.304845
48.842905	1800.921188	19.309863
48.888422	1799.541211	19.314880
49.328938	1811.632431	19.319898
48.936805	1802.655009	19.324915
48.880349	1810.402486	19.329933
49.079609	1802.970391	19.334951
49.459618	1804.627766	19.339968
48.844206	1806.112872	19.344986
49.291356	1815.854964	19.350003
49.491154	1826.831955	19.355021
49.220971	1830.216563	19.360039
49.498906	1829.854286	19.365056
49.424877	1829.929036	19.370074
49.273719	1821.554526	19.375091
49.834478	1819.241691	19.380109
50.312863	1827.962652	19.385127
49.944453	1817.564444	19.390144
49.816604	1825.727085	19.395162
50.199749	1823.041260	19.400179
50.302564	1811.754968	19.405197
50.122891	1823.372122	19.410215
50.566666	1821.244885	19.415232
50.314377	1822.022955	19.420250
50.455632	1825.273667	19.425267
50.275306	1820.425868	19.430285
49.979346	1816.489347	19.435303
50.462119	1818.790235	19.440320
50.376625	1837.298056	19.445338
50.448592	1849.813145	19.450355
50.795960	1853.602813	19.455373
50.630714	1850.065559	19.460391
50.617815	1851.623539	19.465408
50.684527	1846.175253	19.470426
50.530798	1852.574577	19.475443
50.920551	1851.449955	19.480461
50.274128	1856.285331	19.485479
50.888431	1842.801175	19.490496
50.460463	1849.824177	19.495514
50.435454	1851.623914	19.500531
50.734017	1860.963245	19.505549
50.377596	1877.752482	19.510567
50.868048	1879.897528	19.515584
51.076364	1879.621904	19.520602
50.880712	1870.957674	19.525619
51.346315	1886.835428	19.530637
51.298397	1898.914863	19.535655
51.605067	1894.397875	19.540672
51.253080	1902.529391	19.545690
51.379954	1903.285932	19.550707
51.850310	1900.668489	19.555725
51.674686	1906.111823	19.560743
51.861306	1898.918373	19.565760
51.434467	1901.538525	19.570778
51.745274	1897.740468	19.575795
51.982165	1892.981928	19.580813
51.564604	1895.029380	19.585831
52.020544	1893.840733	19.590848
52.033076	1892.065098	19.595866
51.991067	1892.324194	19.600883
52.206856	1886.738921	19.605901
52.133797	1892.150400	19.610919
52.294482	1890.581946	19.615936
52.277314	1888.687878	19.620954
52.359373	1887.444192	19.625971
52.287260	1878.975213	19.630989
51.944415	1890.229781	19.636007
52.601496	1882.404006	19.641024
52.364276	1884.937638	19.646042
52.338760	1885.181526	19.651059
52.655076	1882.143217	19.656077
52.570479	1885.795427	19.661095
52.726115	1898.395279	19.666112
52.687825	1902.134918	19.671130
52.782035	1917.695317	19.676147
52.803186	1915.593256	19.681165
53.146720	1919.992658	19.686183
52.888852	1914.153357	19.691200
52.917467	1902.903881	19.696218
52.674477	1915.692442	19.701235
52.654144	1905.356422	19.706253
52.942751	1912.134624	19.711271
52.646815	1911.780200	19.716288
53.292154	1916.738278	19.721306
53.279852	1923.737213	19.726323
53.668744	1929.054235	19.731341
53.381372	1938.330761	19.736359
53.369972	1937.960162	19.741376
53.712144	1936.095004	19.746394
53.509737	1936.868420	19.751411
53.835676	1939.850356	19.756429
53.561476	1941.408255	19.761447
53.577460	1942.147455	19.766464
53.515009	1933.194060	19.771482
53.708279	1940.962432	19.776499
53.607326	1930.869420	19.781517
53.515651	1934.759453	19.786535
53.711912	1932.907688	19.791552
53.845262	1942.124611	19.796570
53.865086	1949.743423	19.801587
53.818771	1956.043897	19.806605
54.033563	1962.732689	19.811623
54.156707	1955.965762	19.816640
54.183131	1949.100372	19.821658
53.906113	1955.436992	19.826675
54.233201	1972.823030	19.831693
54.067280	1978.766680	19.836711
54.494356	1982.221968	19.841728
54.815631	1982.547234	19.846746
54.625571	1985.171329	19.851763
55.153276	1978.558777	19.856781
54.767687	1975.952343	19.861799
54.633626	1978.763339	19.866816
54.969706	1980.093071	19.871834
54.857870	1984.270319	19.876851
54.853276	1977.138357	19.881869
55.037915	1974.982270	19.886887
54.773627	1979.836708	19.891904
55.002750	1973.065795	19.896922
54.776268	1982.591601	19.901939
55.003225	1998.566810	19.906957
55.150578	2010.180188	19.911975
55.039575	2004.554552	19.916992
55.569989	2006.229411	19.922010
55.264680	2004.487783	19.927027
55.740390	1991.823716	19.932045
55.328584	1996.688648	19.937063
55.427177	1992.996409	19.942080
55.765999	1997.409193	19.947098
55.417936	1996.179235	19.952115
55.801729	1997.359469	19.957133
55.751478	2000.826425	19.962151
55.674267	1995.485857	19.967168
56.071024	2004.778318	19.972186
55.906408	2010.036906	19.977203
56.574015	2010.942281	19.982221
56.362417	2013.393015	19.987239
56.034221	2011.393017	19.992256
56.360716	2005.992351	19.997274
56.441813	2007.532463	20.002291
56.401518	2009.287269	20.007309
56.491727	1997.526269	20.012327
56.231614	1992.956034	20.017344
56.614291	2007.717015	20.022362
56.578935	2015.436026	20.027379
56.885317	2009.157966	20.032397
56.677871	2014.006664	20.037415
56.597675	2010.781128	20.042432
57.176796	2008.395959	20.047450
57.131110	2005.729954	20.052467
56.986569	2004.234559	20.057485
56.938687	1996.541278	20.062503
56.926393	2002.239941	20.067520
57.532700	2003.505245	20.072538
57.098615	2018.665624	20.077555
56.804632	2010.537483	20.082573
57.043600	2003.136957	20.087591
56.746589	2007.488403	20.092608
57.087986	2002.688213	20.097626
57.026176	2013.431727	20.102643
56.985965	2023.152452	20.107661
57.258342	2035.857197	20.112679
56.931394	2042.277416	20.117696
57.524949	2032.649942	20.122714
57.279902	2035.838128	20.127731
57.274500	2025.184092	20.132749
57.487354	2040.467211	20.137767
57.543876	2050.478935	20.142784
57.693500	2052.844675	20.147802
57.795288	2069.098356	20.152819
57.681123	2055.235826	20.157837
57.930761	2063.320496	20.162855
57.881252	2064.019464	20.167872
58.017409	2071.910461	20.172890
58.127498	2069.207416	20.177907
58.250740	2077.021535	20.182925
58.326951	2077.631373	20.187943
58.290845	2079.142512	20.192960
58.762609	2073.100474	20.197978
58.548625	2086.739910	20.202995
58.569364	2074.330122	20.208013
58.822154	2086.605588	20.213031
58.694905	2087.988983	20.218048
58.870408	2075.210933	20.223066
58.667187	2076.315871	20.228083
58.808282	2082.037869	20.233101
58.854420	2081.348955	20.238119
58.990350	2095.687880	20.243136
58.828747	2099.197550	20.248154
59.187657	2103.054897	20.253171
59.236005	2105.865739	20.258189
59.368588	2099.924174	20.263207
59.021470	2099.789223	20.268224
59.331540	2097.061154	20.273242
59.393133	2103.142784	20.278259
59.241440	2093.038694	20.283277
59.283459	2098.874059	20.288295
59.203128	2099.126537	20.293312
59.382877	2093.912953	20.298330
59.416913	2109.290425	20.303347
59.475953	2107.204498	20.308365
59.858143	2112.248045	20.313383
59.595118	2113.491755	20.318400
59.978376	2117.042305	20.323418
59.992809	2120.884193	20.328435
60.082667	2119.465684	20.333453
59.994772	2120.072830	20.338471
59.616936	2117.998539	20.343488
59.730197	2122.654995	20.348506
60.299856	2130.648528	20.353523
60.558367	2139.192631	20.358541
60.295797	2137.384328	20.363559
60.069123	2148.352587	20.368576
60.120764	2145.005376	20.373594
60.423404	2143.010678	20.378611
60.548214	2135.918345	20.383629
60.887283	2137.500108	20.388647
60.476706	2142.667870	20.393664
60.850854	2141.747667	20.398682
61.084049	2163.030598	20.403699
61.188092	2161.931785	20.408717
61.210815	2155.830672	20.413735
60.858528	2146.543849	20.418752
61.157085	2156.571365	20.423770
61.157277	2154.854447	20.428787
60.762633	2163.911188	20.433805
61.216325	2158.484236	20.438823
61.221566	2164.653618	20.443840
61.266085	2170.627482	20.448858
61.581952	2162.520501	20.453875
61.418117	2168.561725	20.458893
61.625684	2155.889058	20.463911
61.565657	2168.844811	20.468928
61.578368	2179.983886	20.473946
61.853405	2185.669151	20.478963
61.930666	2188.677467	20.483981
62.146050	2194.842340	20.488999
62.056566	2194.345101	20.494016
62.156185	2191.817264	20.499034
62.256494	2192.192935	20.504051
62.184258	2185.459688	20.509069
62.058381	2189.020588	20.514087
62.278618	2186.764215	20.519104
62.018390	2194.183987	20.524122
61.723870	2194.823508	20.529139
61.806323	2187.232813	20.534157
61.826521	2199.456427	20.539175
61.877366	2223.182421	20.544192
62.094116	2217.622144	20.549210
62.686167	2235.014265	20.554227
62.663471	2242.033889	20.559245
62.900775	2235.618236	20.564263
63.085367	2242.778969	20.569280
63.323067	2239.427839	20.574298
63.164354	2237.363389	20.579315
63.085223	2245.060951	20.584333
63.090029	2226.836837	20.589351
63.407035	2239.582076	20.594368
63.385138	2231.300743	20.599386
63.667181	2229.830022	20.604403
63.623268	2230.679613	20.609421
63.745876	2230.136519	20.614439
63.352863	2226.713777	20.619456
63.414248	2225.719483	20.624474
63.553681	2227.708110	20.629491
63.330281	2231.479976	20.634509
63.811107	2225.537463	20.639527
63.512788	2225.205498	20.644544
63.609372	2228.106641	20.649562
64.014577	2240.449861	20.654579
63.626653	2252.327159	20.659597
64.088876	2246.122440	20.664615
64.212247	2246.194668	20.669632
64.386038	2252.050466	20.674650
64.243574	2249.601579	20.679667
64.310706	2252.314817	20.684685
64.509422	2246.217662	20.689703
64.060272	2258.290766	20.694720
64.131484	2252.415577	20.699738
64.583459	2247.014116	20.704755
64.474125	2251.528739	20.709773
64.492841	2266.930839	20.714791
64.728072	2267.023415	20.719808
64.584987	2267.528748	20.724826
64.739077	2268.038020	20.729843
64.809039	2270.873907	20.734861
64.766756	2263.324816	20.739879
64.621771	2267.630412	20.744896
64.780958	2290.490524	20.749914
64.996567	2285.293359	20.754931
64.735887	2288.256799	20.759949
65.212609	2287.531978	20.764967
65.156239	2287.389345	20.769984
65.193773	2299.200015	20.775002
65.588492	2311.538615	20.780019
65.583739	2310.074947	20.785037
65.970511	2305.551619	20.790055
66.200941	2309.681631	20.795072
65.983123	2314.702466	20.800090
66.302344	2303.113689	20.805107
66.301993	2307.835336	20.810125
66.499855	2304.092764	20.815143
66.292403	2290.948483	20.820160
66.667717	2283.864185	20.825178
66.323685	2269.822888	20.830195
66.092641	2278.383792	20.835213
66.329797	2274.202682	20.840231
66.172141	2285.005561	20.845248
65.950053	2298.993600	20.850266
66.478249	2294.672203	20.855283
66.580560	2306.034028	20.860301
66.794862	2300.458329	20.865319
66.867842	2306.251036	20.870336
66.770003	2309.611887	20.875354
66.834879	2302.708776	20.880371
66.559836	2294.782688	20.885389
66.771776	2309.558044	20.890407
66.794984	2309.983670	20.895424
66.850148	2324.859349	20.900442
67.076058	2321.544768	20.905459
66.920045	2335.913844	20.910477
67.425204	2333.565472	20.915495
67.109764	2325.926594	20.920512
67.135787	2333.355229	20.925530
67.643956	2338.047710	20.930547
67.439964	2343.031668	20.935565
67.895003	2344.790961	20.940583
68.057280	2347.347282	20.945600
68.010209	2342.948727	20.950618
67.912635	2334.218408	20.955635
67.905281	2343.738478	20.960653
67.810723	2335.610507	20.965671
67.630590	2345.334391	20.970688
67.801769	2345.500125	20.975706
68.007764	2340.266578	20.980723
67.950588	2350.299438	20.985741
68.403628	2351.134298	20.990759
68.208104	2363.590658	20.995776
68.035628	2374.055050	21.000794
68.441704	2364.762918	21.005811
68.044952	2367.514135	21.010829
68.261000	2363.585646	21.015847
68.512030	2372.127877	21.020864
68.671800	2387.618446	21.025882
68.961172	2390.776620	21.030899
68.945228	2394.995750	21.035917
68.957148	2394.230126	21.040935
69.121868	2385.263007	21.045952
68.896581	2384.231558	21.050970
68.940617	2391.818359	21.055987
68.931320	2391.734629	21.061005
69.139039	2390.764741	21.066023
69.571094	2394.607536	21.071040
69.467563	2420.055979	21.076058
69.332727	2414.332953	21.081075
69.447365	2422.028637	21.086093
69.321498	2418.279951	21.091111
69.541030	2406.959218	21.096128
69.494904	2415.017795	21.101146
69.846449	2424.222874	21.106163
69.906641	2439.965800	21.111181
70.284754	2439.073366	21.116199
70.366461	2438.549299	21.121216
70.154001	2432.200886	21.126234
70.481646	2434.182141	21.131251
70.541322	2433.184947	21.136269
70.706154	2437.486230	21.141287
70.838152	2433.801292	21.146304
70.862142	2441.441752	21.151322
70.667560	2433.594524	21.156339
70.629648	2442.352490	21.161357
70.891865	2430.024557	21.166375
70.772511	2430.377838	21.171392
70.965766	2423.653405	21.176410
71.228551	2427.961432	21.181427
70.894089	2429.449909	21.186445
71.057666	2433.476802	21.191463
70.945093	2425.619885	21.196480
70.747910	2431.325558	21.201498
71.241145	2429.720736	21.206515
70.998417	2438.513946	21.211533
71.121956	2449.392801	21.216551
71.390382	2454.410084	21.221568
71.477864	2450.473313	21.226586
71.442952	2455.585464	21.231603
71.525588	2447.423368	21.236621
71.713421	2454.542648	21.241639
72.016232	2461.448236	21.246656
71.701172	2480.870096	21.251674
72.072598	2480.297480	21.256691
72.289748	2483.811007	21.261709
72.175479	2481.913153	21.266727
72.102668	2471.398816	21.271744
72.083185	2478.840953	21.276762
72.088451	2472.969711	21.281779
72.085601	2475.624513	21.286797
71.952311	2478.154568	21.291815
72.448996	2489.139105	21.296832
72.611395	2506.018073	21.301850
72.636679	2495.011773	21.306867
72.986286	2495.260020	21.311885
72.759071	2500.001480	21.316903
72.889676	2506.599512	21.321920
72.738098	2505.023117	21.326938
73.052489	2501.618894	21.331955
72.756083	2496.789098	21.336973
72.898838	2515.485943	21.341991
73.457082	2524.548224	21.347008
73.080365	2524.679867	21.352026
73.363757	2524.392472	21.357043
73.346295	2519.657838	21.362061
73.183783	2529.884047	21.367079
73.421804	2514.138566	21.372096
73.239356	2532.548670	21.377114
73.547353	2544.503341	21.382131
73.549352	2538.316973	21.387149
74.057756	2541.503981	21.392167
73.934849	2544.461657	21.397184
73.888477	2547.442060	21.402202
74.213235	2545.147175	21.407219
74.313213	2544.913766	21.412237
74.270106	2546.716408	21.417255
74.357523	2553.617904	21.422272
74.570727	2573.591488	21.427290
74.598223	2578.075286	21.432307
74.560575	2576.455786	21.437325
74.679130	2576.108999	21.442343
75.020413	2575.452730	21.447360
74.996706	2576.141363	21.452378
75.132795	2571.559404	21.457395
74.744785	2576.070426	21.462413
74.498415	2573.296907	21.467431
74.720882	2571.961739	21.472448
74.928329	2581.183163	21.477466
75.160446	2585.814806	21.482483
75.267602	2590.282970	21.487501
75.012853	2593.131908	21.492519
75.356633	2585.127674	21.497536
75.592425	2586.694098	21.502554
75.417339	2594.659337	21.507571
75.772566	2607.657656	21.512589
75.465908	2615.400492	21.517607
75.636153	2611.883116	21.522624
75.793348	2614.336118	21.527642
75.931969	2614.541674	21.532659
76.117135	2615.225990	21.537677
75.974608	2612.458288	21.542695
76.253093	2625.847385	21.547712
76.303911	2639.571999	21.552730
76.254561	2636.518263	21.557747
76.576571	2638.014372	21.562765
76.622893	2639.105496	21.567783
76.648692	2645.697907	21.572800
76.600383	2639.276360	21.577818
76.466539	2632.416883	21.582835
76.583988	2640.279498	21.587853
76.658287	2658.002487	21.592871
76.989012	2661.340446	21.597888
77.226696	2668.120601	21.602906
77.249300	2656.265608	21.607923
77.514588	2663.079311	21.612941
77.317203	2661.895134	21.617959
77.500989	2663.201436	21.622976
77.662983	2663.125587	21.627994
77.977838	2656.025368	21.633011
77.727065	2654.985271	21.638029
77.621353	2664.874414	21.643047
77.613845	2648.580233	21.648064
78.046834	2652.306159	21.653082
77.429145	2647.242602	21.658099
78.046501	2650.305250	21.663117
77.726151	2648.812095	21.668135
77.903782	2663.927674	21.673152
78.023494	2672.620026	21.678170
78.192162	2670.545264	21.683187
78.056214	2668.534008	21.688205
77.975219	2674.167899	21.693223
78.483023	2684.358611	21.698240
78.597778	2697.612448	21.703258
78.667131	2701.890879	21.708275
78.669873	2702.995147	21.713293
78.667297	2699.318614	21.718311
78.859849	2698.726674	21.723328
79.217826	2705.595308	21.728346
78.858085	2701.728550	21.733363
79.231391	2694.641251	21.738381
78.798683	2703.953564	21.743399
79.249438	2703.415856	21.748416
79.178789	2721.972760	21.753434
79.150774	2716.501177	21.758451
79.672303	2724.300522	21.763469
79.546808	2719.368140	21.768487
79.514766	2719.379502	21.773504
79.769074	2719.254471	21.778522
79.534063	2733.576273	21.783539
80.069941	2745.227097	21.788557
80.233703	2746.546012	21.793575
80.106419	2743.690684	21.798592
80.687971	2750.287592	21.803610
80.367634	2741.692974	21.808627
80.331303	2747.499794	21.813645
80.372547	2745.258771	21.818663
80.428390	2740.799808	21.823680
80.470340	2748.923640	21.828698
80.115166	2745.340215	21.833715
80.669634	2754.286425	21.838733
80.745483	2767.628471	21.843751
81.032851	2761.555127	21.848768
81.373315	2761.489191	21.853786
80.914584	2771.020237	21.858803
81.217778	2755.990262	21.863821
80.893900	2760.901588	21.868839
81.538947	2755.283513	21.873856
81.318345	2760.696276	21.878874
81.397383	2757.597155	21.883891
81.583952	2778.398910	21.888909
81.682259	2778.942186	21.893927
81.914284	2789.128822	21.898944
81.582369	2786.128799	21.903962
81.715646	2791.675501	21.908979
81.855840	2779.536882	21.913997
81.843817	2790.471901	21.919015
82.043564	2786.416470	21.924032
82.187150	2786.122570	21.929050
81.993574	2805.573088	21.934067
82.428429	2806.445539	21.939085
82.394144	2807.943829	21.944103
82.136685	2810.629101	21.949120
82.580802	2802.612209	21.954138
82.402668	2815.160841	21.959155
82.732401	2812.151839	21.964173
82.747742	2820.819585	21.969191
82.857464	2828.513058	21.974208
83.048957	2822.552557	21.979226
82.960291	2833.247112	21.984243
83.292154	2827.479241	21.989261
83.098369	2832.572202	21.994279
83.087578	2832.049991	21.999296
83.355701	2823.359982	22.004314
83.226306	2825.365544	22.009331
83.546785	2843.223738	22.014349
83.741561	2856.607185	22.019367
83.847347	2857.613256	22.024384
83.882188	2860.899766	22.029402
83.557565	2862.579265	22.034419
84.220816	2847.338149	22.039437
84.275018	2846.376509	22.044455
83.955622	2850.876848	22.049472
84.048412	2846.614069	22.054490
84.421712	2850.264171	22.059507
84.387472	2842.038146	22.064525
84.176532	2862.166877	22.069543
84.377731	2876.196357	22.074560
84.886829	2871.843099	22.079578
84.708092	2876.173065	22.084595
84.640052	2879.873381	22.089613
84.707519	2876.791834	22.094631
84.703777	2873.093355	22.099648
84.898621	2880.347424	22.104666
84.887860	2896.253364	22.109683
85.000692	2901.156276	22.114701
85.108464	2899.905335	22.119719
85.026918	2901.281632	22.124736
85.115969	2916.487050	22.129754
85.310846	2927.317143	22.134771
85.761064	2924.030435	22.139789
85.509848	2919.357568	22.144807
85.156724	2930.282988	22.149824
85.249846	2938.632449	22.154842
85.526023	2953.455083	22.159859
85.652845	2962.926052	22.164877
85.564007	2972.033128	22.169895
85.732750	2980.743197	22.174912
86.045471	2977.938833	22.179930
86.061595	2998.745451	22.184947
86.366132	2996.463147	22.189965
86.597001	3004.260808	22.194983
87.172963	3006.660880	22.200000
87.562284	2998.409455	22.205018
87.517594	3006.158759	22.210035
87.371850	2993.531389	22.215053
87.964881	2993.274383	22.220071
87.553793	2986.717019	22.225088
87.528092	2970.406460	22.230106
87.399757	2968.570727	22.235123
87.381061	2969.725713	22.240141
87.563246	2972.326348	22.245159
87.265465	2978.767577	22.250176
87.586574	2993.879892	22.255194
87.775424	2995.999737	22.260211
87.890949	2989.094742	22.265229
87.631708	2987.405765	22.270247
87.889036	2988.754226	22.275264
88.221778	2996.876798	22.280282
88.226334	3009.343287	22.285299
88.211754	3019.183627	22.290317
88.281979	3024.935967	22.295335
88.291305	3016.728287	22.300352
88.501452	3017.153048	22.305370
88.358612	3028.695769	22.310387
88.263414	3016.903183	22.315405
88.383257	3022.347904	22.320423
88.587563	3041.521714	22.325440
88.777914	3028.434508	22.330458
88.782791	3041.970938	22.335475
89.203915	3038.644580	22.340493
89.034727	3039.927306	22.345511
89.149545	3051.783173	22.350528
89.211518	3049.415772	22.355546
89.341361	3056.916814	22.360563
89.572698	3058.648104	22.365581
89.755700	3054.693080	22.370599
89.503863	3057.462727	22.375616
89.548151	3057.702006	22.380634
89.558764	3067.904551	22.385651
90.195342	3081.209478	22.390669
90.301918	3073.791382	22.395687
89.876794	3085.230020	22.400704
89.998682	3080.164094	22.405722
90.392793	3089.324971	22.410739
90.226834	3085.434082	22.415757
90.548896	3099.078674	22.420775
90.327037	3101.846787	22.425792
91.109874	3103.797834	22.430810
90.773951	3103.856806	22.435827
90.821689	3101.908254	22.440845
91.123588	3097.208653	22.445863
91.046217	3106.503376	22.450880
91.280725	3102.751742	22.455898
91.629893	3112.939146	22.460915
91.646124	3099.913886	22.465933
91.599589	3102.143216	22.470951
91.554308	3119.850675	22.475968
91.809709	3121.208917	22.480986
91.627896	3124.396855	22.486003
92.061489	3121.412563	22.491021
91.806064	3122.143832	22.496039
92.123183	3117.198809	22.501056
92.320778	3108.260900	22.506074
92.117355	3120.191922	22.511091
92.032310	3112.715457	22.516109
92.475151	3121.856091	22.521127
92.329447	3136.552440	22.526144
92.283163	3136.992130	22.531162
92.230903	3142.533289	22.536179
92.439278	3142.014607	22.541197
92.579429	3150.104296	22.546215
92.439709	3168.464166	22.551232
92.896368	3167.316361	22.556250
93.133807	3175.053098	22.561267
92.982333	3176.661310	22.566285
93.522807	3184.549420	22.571303
93.497283	3195.076482	22.576320
93.616055	3186.397074	22.581338
93.379525	3199.655816	22.586355
93.161120	3199.791064	22.591373
93.735966	3180.693920	22.596391
93.519605	3188.091444	22.601408
94.121106	3200.268852	22.606426
94.022014	3220.456208	22.611443
93.726433	3223.119106	22.616461
93.642848	3211.435044	22.621479
93.889092	3220.193056	22.626496
94.115625	3227.473863	22.631514
94.362889	3238.475844	22.636531
94.662927	3240.508860	22.641549
94.627978	3235.836748	22.646567
94.802223	3239.126736	22.651584
94.960632	3232.546340	22.656602
94.960325	3240.607575	22.661619
95.333291	3246.252585	22.666637
95.691615	3249.491642	22.671655
95.386435	3248.649411	22.676672
95.787478	3238.401266	22.681690
95.735106	3235.811877	22.686707
95.502135	3235.097210	22.691725
95.697320	3230.985582	22.696743
95.608156	3243.520572	22.701760
96.155765	3238.223776	22.706778
95.987601	3246.440720	22.711795
95.744573	3258.128691	22.716813
96.040524	3246.924869	22.721831
95.991232	3249.738563	22.726848
96.119033	3254.266783	22.731866
96.140680	3252.252865	22.736883
96.120721	3272.636197	22.741901
96.501239	3272.819645	22.746919
96.204588	3271.619415	22.751936
96.561515	3276.585189	22.756954
96.607280	3271.733137	22.761971
97.058305	3299.431594	22.766989
96.936919	3293.324268	22.772007
96.805295	3307.049566	22.777024
97.070776	3300.682780	22.782042
97.510321	3305.518834	22.787059
97.259174	3319.307056	22.792077
97.521397	3320.743152	22.797095
97.519631	3330.651093	22.802112
97.702093	3322.223614	22.807130
97.770352	3326.347706	22.812147
97.629678	3318.984028	22.817165
97.873034	3330.529561	22.822183
97.809874	3341.378236	22.827200
98.094908	3338.095240	22.832218
98.322712	3346.698388	22.837235
98.213495	3346.658716	22.842253
98.662309	3359.728137	22.847271
98.547854	3363.312728	22.852288
98.718965	3372.234089	22.857306
98.866611	3366.201372	22.862323
99.212982	3364.878299	22.867341
99.344496	3360.486237	22.872359
99.080130	3372.228125	22.877376
99.025423	3361.243298	22.882394
99.177145	3364.618903	22.887411
99.461517	3381.293359	22.892429
99.341126	3387.539656	22.897447
99.398089	3385.775851	22.902464
99.464852	3394.176997	22.907482
99.529020	3391.067473	22.912499
99.436679	3409.524322	22.917517
100.231522	3407.667006	22.922535
100.198877	3409.307123	22.927552
100.364119	3411.768442	22.932570
100.206737	3414.475999	22.937587
100.296952	3413.448717	22.942605
100.479969	3409.698775	22.947623
100.308791	3426.078510	22.952640
100.379009	3423.716080	22.957658
100.883588	3424.416669	22.962675
100.755286	3422.284190	22.967693
101.174774	3416.499248	22.972711
101.212526	3429.816189	22.977728
101.192328	3435.257725	22.982746
101.263917	3439.362382	22.987763
101.281094	3452.284866	22.992781
101.730539	3450.402751	22.997799
101.810420	3456.983829	23.002816
101.645621	3445.826820	23.007834
102.151090	3443.468792	23.012851
101.602585	3442.929804	23.017869
102.639922	3445.428095	23.022887
102.289813	3446.407779	23.027904
102.444090	3443.820704	23.032922
102.133976	3438.478320	23.037939
101.788143	3449.324000	23.042957
102.271646	3462.416469	23.047975
102.479016	3470.139106	23.052992
102.758930	3474.754023	23.058010
102.477916	3475.880699	23.063027
102.533978	3475.707817	23.068045
102.974478	3483.368685	23.073063
103.239645	3494.352236	23.078080
102.976719	3502.988152	23.083098
103.458887	3492.417835	23.088115
103.294849	3495.580958	23.093133
103.031306	3505.024993	23.098151
103.371682	3518.061018	23.103168
103.552150	3523.698398	23.108186
104.171033	3513.381251	23.113203
104.010896	3520.520751	23.118221
104.100822	3518.792801	23.123239
104.269731	3515.853070	23.128256
104.523629	3518.111134	23.133274
104.744625	3524.714317	23.138291
104.496442	3539.622741	23.143309
104.604277	3540.622218	23.148327
104.318517	3551.452235	23.153344
104.390784	3550.348848	23.158362
104.479509	3545.026011	23.163379
104.411125	3561.822184	23.168397
105.024012	3567.786374	23.173415
104.985490	3571.542177	23.178432
105.029461	3575.850043	23.183450
104.871303	3582.885097	23.188467
105.321197	3594.897145	23.193485
105.456926	3598.571996	23.198503
105.631500	3607.436116	23.203520
105.834693	3607.887233	23.208538
106.308973	3612.891529	23.213555
105.859349	3624.220715	23.218573
105.977998	3617.299209	23.223591
105.840879	3621.231444	23.228608
106.052720	3626.658778	23.233626
106.048814	3626.498446	23.238643
106.106934	3645.765240	23.243661
106.459449	3649.740712	23.248679
106.614747	3651.329311	23.253696
106.678635	3664.415072	23.258714
107.031407	3661.026715	23.263731
107.127293	3661.728217	23.268749
107.305818	3665.689918	23.273767
107.218784	3668.386491	23.278784
107.172630	3677.342041	23.283802
107.874947	3682.638892	23.288819
107.993505	3689.179275	23.293837
107.974393	3689.235957	23.298855
108.203159	3688.227986	23.303872
107.849274	3694.384714	23.308890
108.122326	3682.328837	23.313907
108.213973	3686.155805	23.318925
108.685029	3688.196800	23.323943
108.498653	3689.772648	23.328960
108.190563	3683.359865	23.333978
108.478499	3682.440471	23.338995
108.850265	3709.384979	23.344013
108.533065	3710.482618	23.349031
108.906704	3711.408898	23.354048
108.829829	3709.849099	23.359066
109.066567	3710.247619	23.364083
108.778175	3710.908323	23.369101
109.075793	3727.890348	23.374119
109.300882	3739.593667	23.379136
108.774655	3746.711701	23.384154
109.199583	3744.214749	23.389171
109.244107	3767.334582	23.394189
109.555077	3772.819026	23.399207
109.604919	3764.743540	23.404224
109.826364	3778.596950	23.409242
110.115750	3783.778611	23.414259
110.601959	3783.790846	23.419277
110.777403	3779.145602	23.424295
111.088962	3773.604717	23.429312
110.634781	3768.969739	23.434330
110.855033	3776.431666	23.439347
111.080145	3780.597572	23.444365
111.076548	3776.393865	23.449383
111.438138	3774.658050	23.454400
110.974235	3778.114400	23.459418
111.149455	3784.838479	23.464435
111.217177	3797.541813	23.469453
111.500988	3794.388340	23.474471
111.898342	3787.729274	23.479488
111.900618	3796.835115	23.484506
112.132770	3787.351717	23.489523
112.037001	3785.886407	23.494541
111.809016	3807.496045	23.499559
112.085581	3819.478583	23.504576
111.893677	3823.536230	23.509594
112.291629	3816.539327	23.514611
112.478114	3833.715621	23.519629
112.601474	3837.083132	23.524647
112.841659	3846.016000	23.529664
112.358671	3848.446368	23.534682
112.875711	3850.413894	23.539699
113.270993	3869.107299	23.544717
113.052997	3876.947254	23.549735
112.865451	3865.648355	23.554752
113.124516	3882.223077	23.559770
113.345112	3882.576784	23.564787
113.290113	3899.153380	23.569805
113.540870	3902.576697	23.574823
113.837328	3901.548640	23.579840
113.652534	3921.579758	23.584858
113.829775	3926.195094	23.589875
114.089438	3936.649500	23.594893
114.228244	3933.970087	23.599911
114.288720	3935.469406	23.604928
114.378560	3955.552227	23.609946
114.249821	3954.275140	23.614963
114.762691	3961.167336	23.619981
114.890743	3955.153276	23.624999
115.013962	3965.660639	23.630016
114.801745	3991.920580	23.635034
115.189062	3986.288852	23.640051
115.158300	3989.939364	23.645069
115.228798	3990.884743	23.650087
115.410504	3998.778918	23.655104
115.521086	4005.005022	23.660122
115.734879	4000.981842	23.665139
116.134841	4006.042081	23.670157
116.058544	4014.671096	23.675175
116.218313	4018.253886	23.680192
116.355078	4031.868243	23.685210
116.350543	4026.967055	23.690227
116.610225	4021.544697	23.695245
116.645880	4028.568498	23.700263
117.153420	4025.360996	23.705280
116.532327	4030.278192	23.710298
116.823343	4027.079360	23.715315
116.810761	4044.271259	23.720333
117.161319	4048.344975	23.725351
117.640852	4046.325518	23.730368
117.623715	4052.710531	23.735386
117.675962	4053.535673	23.740403
117.678826	4052.042263	23.745421
117.575092	4057.503385	23.750439
117.534295	4068.588880	23.755456
117.581611	4076.065399	23.760474
118.076377	4078.490966	23.765491
118.196560	4088.433875	23.770509
117.889093	4091.237643	23.775527
118.021820	4100.080153	23.780544
118.064302	4106.941936	23.785562
118.616582	4125.626792	23.790579
118.731825	4127.461599	23.795597
118.908300	4134.902124	23.800615
119.060583	4130.973776	23.805632
119.133786	4140.431668	23.810650
119.190556	4138.850894	23.815667
119.732873	4149.198012	23.820685
119.658544	4152.602866	23.825703
119.229822	4152.692158	23.830720
119.511537	4162.963323	23.835738
119.449256	4163.260347	23.840755
120.051206	4168.279518	23.845773
119.785852	4175.943946	23.850791
120.402778	4176.712191	23.855808
120.350118	4185.179761	23.860826
120.656042	4197.151637	23.865843
120.758152	4201.267469	23.870861
120.595287	4207.839503	23.875879
120.729008	4201.846569	23.880896
121.265724	4195.563236	23.885914
121.043185	4206.686757	23.890931
121.255637	4214.996017	23.895949
121.572790	4225.072278	23.900967
121.550675	4228.775143	23.905984
121.706863	4224.966108	23.911002
121.639398	4221.280494	23.916019
121.755313	4224.131585	23.921037
121.842506	4242.018242	23.926055
122.259417	4249.616847	23.931072
122.092429	4244.943065	23.936090
122.095609	4252.025700	23.941107
122.266030	4254.663086	23.946125
122.616692	4270.756657	23.951143
122.592194	4272.584963	23.956160
122.497380	4280.977114	23.961178
122.491755	4282.540477	23.966195
123.058364	4291.867487	23.971213
122.984592	4298.652862	23.976231
123.273803	4306.580832	23.981248
123.194072	4308.149495	23.986266
123.255223	4317.940797	23.991283
123.727542	4322.885627	23.996301
123.968264	4327.775203	24.001319
124.240234	4318.784014	24.006336
124.023657	4327.188949	24.011354
123.585482	4320.464889	24.016371
124.352671	4338.775397	24.021389
124.542431	4351.781960	24.026407
124.498332	4347.196219	24.031424
124.540124	4344.304679	24.036442
124.467293	4344.710679	24.041459
124.702333	4359.465156	24.046477
124.872661	4372.143348	24.051495
124.727079	4368.129042	24.056512
124.842775	4376.990138	24.061530
125.231980	4385.183404	24.066547
125.399099	4391.217707	24.071565
125.404905	4400.973535	24.076583
125.788001	4396.544965	24.081600
125.991127	4403.810975	24.086618
125.797613	4422.199479	24.091635
126.197535	4427.597588	24.096653
126.094888	4421.452223	24.101671
126.262592	4413.679947	24.106688
126.438113	4430.325076	24.111706
126.108587	4447.664862	24.116723
126.722563	4447.735997	24.121741
126.557482	4454.018069	24.126759
126.955425	4465.303371	24.131776
127.318473	4467.566552	24.136794
127.008191	4477.469792	24.141811
127.434685	4475.777405	24.146829
127.226604	4472.536741	24.151847
127.567285	4485.264079	24.156864
127.893915	4488.830291	24.161882
127.767086	4500.207299	24.166899
128.196124	4492.144683	24.171917
128.083028	4499.614942	24.176935
128.419566	4513.993803	24.181952
128.586454	4525.634149	24.186970
128.375171	4529.865440	24.191987
128.376846	4525.610230	24.197005
128.441460	4532.762262	24.202023
129.008134	4539.639938	24.207040
128.749128	4551.290206	24.212058
128.597415	4554.820894	24.217075
129.054850	4564.929027	24.222093
129.266381	4572.099093	24.227111
129.441033	4572.709377	24.232128
129.681120	4580.383172	24.237146
129.655344	4602.542873	24.242163
129.488995	4591.009775	24.247181
129.386167	4604.071827	24.252199
130.021748	4614.710783	24.257216
130.081002	4623.590312	24.262234
130.385039	4634.227560	24.267251
130.730026	4638.141301	24.272269
130.536232	4648.512490	24.277287
130.706613	4656.598117	24.282304
130.942571	4651.542292	24.287322
131.050736	4663.690659	24.292339
131.260738	4673.282067	24.297357
131.538005	4680.918514	24.302375
131.563415	4675.242265	24.307392
132.140699	4672.696068	24.312410
131.373384	4682.961422	24.317427
131.634274	4686.942009	24.322445
131.944896	4699.620546	24.327463
131.852697	4699.347775	24.332480
132.474033	4705.939175	24.337498
132.610712	4720.390545	24.342515
132.669045	4721.258956	24.347533
132.706383	4713.787908	24.352551
132.624952	4726.032307	24.357568
133.048448	4716.651024	24.362586
133.065528	4742.841403	24.367603
133.815644	4742.045257	24.372621
133.359868	4734.708272	24.377639
133.994998	4734.924454	24.382656
134.441375	4719.412727	24.387674
134.474165	4729.603263	24.392691
134.503511	4723.765397	24.397709
134.718346	4706.563326	24.402727
134.240474	4692.654743	24.407744
134.657573	4701.001609	24.412762
134.649779	4716.754010	24.417779
134.865199	4719.371789	24.422797
134.794686	4707.848854	24.427815
135.070034	4707.982512	24.432832
135.323810	4713.779233	24.437850
135.350018	4723.642516	24.442867
135.419388	4710.579366	24.447885
135.443651	4714.265594	24.452903
135.636776	4710.498020	24.457920
135.683040	4720.086696	24.462938
135.652752	4728.352151	24.467955
135.898071	4731.359816	24.472973
135.679127	4735.690208	24.477991
135.781978	4746.693636	24.483008
135.959376	4751.034539	24.488026
136.265633	4765.604580	24.493043
136.243833	4765.888958	24.498061
136.243328	4779.702148	24.503079
136.369956	4787.273857	24.508096
136.698037	4800.603136	24.513114
136.687128	4812.306243	24.518131
136.665346	4812.555897	24.523149
136.676208	4841.758752	24.528167
136.776709	4847.611094	24.533184
137.509417	4861.738770	24.538202
136.986573	4870.078299	24.543219
137.808885	4890.912301	24.548237
137.531891	4906.817521	24.553255
137.557014	4914.566171	24.558272
138.124548	4932.842272	24.563290
138.277624	4932.714152	24.568307
138.534210	4942.323657	24.573325
138.566688	4940.718211	24.578343
138.778535	4965.483187	24.583360
138.988084	4967.855707	24.588378
138.689379	4973.846389	24.593395
139.002590	4980.085276	24.598413
139.152903	4980.986638	24.603431
139.301526	5000.903575	24.608448
140.212816	5004.873879	24.613466
140.127790	5020.016792	24.618483
140.341702	5021.378526	24.623501
140.377769	5013.238356	24.628519
140.403685	5012.120047	24.633536
140.526993	5013.701153	24.638554
140.416745	5026.812019	24.643571
140.637760	5037.743448	24.648589
140.925067	5037.752129	24.653607
140.804408	5035.914981	24.658624
141.271541	5055.172855	24.663642
141.063667	5056.414430	24.668659
141.424095	5060.543650	24.673677
141.707002	5057.358537	24.678695
141.355850	5077.631636	24.683712
141.759626	5076.027984	24.688730
142.121679	5084.835047	24.693747
142.275361	5086.499785	24.698765
142.348929	5087.106985	24.703783
142.434481	5104.227691	24.708800
142.824664	5108.181803	24.713818
142.814828	5117.523792	24.718835
142.679158	5117.434595	24.723853
143.098788	5105.976667	24.728871
142.808935	5110.529749	24.733888
143.384482	5123.735268	24.738906
143.153510	5130.684471	24.743923
143.328305	5126.537733	24.748941
143.609031	5131.575934	24.753959
143.670768	5147.065284	24.758976
143.825850	5165.851320	24.763994
143.569282	5171.087346	24.769011
144.128885	5178.487217	24.774029
144.138210	5186.134288	24.779047
144.182425	5194.255704	24.784064
144.594021	5195.447589	24.789082
144.420495	5204.666905	24.794099
144.529892	5216.509255	24.799117
144.618637	5216.536417	24.804135
144.661805	5245.602278	24.809152
145.027028	5240.797511	24.814170
145.360006	5257.002053	24.819187
145.523031	5268.902324	24.824205
145.798940	5270.087062	24.829223
145.749720	5279.586822	24.834240
145.678935	5295.589496	24.839258
146.060459	5296.527254	24.844275
146.557006	5312.674653	24.849293
146.662809	5310.716769	24.854311
146.828421	5335.224332	24.859328
146.868649	5328.402850	24.864346
147.177338	5338.143295	24.869363
147.105534	5336.049087	24.874381
147.054985	5342.850151	24.879399
147.483639	5350.848276	24.884416
147.244874	5353.884533	24.889434
147.536149	5362.469226	24.894451
147.651373	5375.942758	24.899469
147.872803	5377.707393	24.904487
147.626043	5383.450164	24.909504
148.025820	5395.013545	24.914522
147.759783	5401.611640	24.919539
147.948658	5425.219187	24.924557
148.100589	5429.538989	24.929575
148.619675	5439.603229	24.934592
149.004350	5443.031114	24.939610
149.474888	5462.588769	24.944627
149.588418	5469.600926	24.949645
150.174675	5469.565930	24.954663
149.991680	5475.008326	24.959680
150.191053	5462.202060	24.964698
150.246232	5470.034624	24.969715
150.500096	5470.553613	24.974733
150.582404	5456.471454	24.979751
150.529973	5472.177836	24.984768
150.852824	5487.449794	24.989786
150.996670	5487.809247	24.994803
151.058089	5487.872258	24.999821
151.304366	5479.149686	25.004839
151.024197	5495.153770	25.009856
151.341481	5502.926346	25.014874
151.430563	5511.283938	25.019891
151.504344	5527.964950	25.024909
151.463749	5527.709335	25.029927
151.938824	5532.635126	25.034944
152.224978	5540.766143	25.039962
152.054037	5545.231256	25.044979
151.986272	5556.047247	25.049997
152.400530	5570.367417	25.055015
152.108876	5578.279617	25.060032
152.218118	5577.590157	25.065050
152.642655	5589.560152	25.070067
152.539516	5600.864686	25.075085
153.075352	5603.372418	25.080103
153.196656	5629.326771	25.085120
153.374210	5628.033147	25.090138
153.572736	5639.205214	25.095155
153.516866	5651.291549	25.100173
154.126735	5649.254661	25.105191
153.910041	5663.181305	25.110208
154.156479	5683.061566	25.115226
154.153546	5683.952247	25.120243
154.153996	5691.357854	25.125261
154.214453	5699.344367	25.130279
154.691784	5716.909344	25.135296
155.035112	5718.875886	25.140314
155.295646	5737.342945	25.145331
155.329387	5742.426323	25.150349
155.449671	5747.076301	25.155367
155.359669	5759.092293	25.160384
155.947145	5765.440006	25.165402
156.135579	5763.383897	25.170419
156.020560	5780.236770	25.175437
156.440530	5783.365615	25.180455
156.513536	5793.462055	25.185472
156.606976	5792.251046	25.190490
156.616562	5799.592130	25.195507
156.508766	5822.990972	25.200525
157.056467	5814.000049	25.205543
157.161527	5829.391645	25.210560
157.245984	5853.858952	25.215578
157.614070	5841.660495	25.220595
157.320076	5865.590484	25.225613
157.653275	5877.540254	25.230631
157.692064	5882.382967	25.235648
158.070745	5889.268514	25.240666
158.270962	5890.212612	25.245683
158.412625	5904.588377	25.250701
159.190951	5905.407184	25.255719
159.261481	5911.674940	25.260736
159.415992	5911.281424	25.265754
159.723179	5911.214389	25.270771
159.545612	5913.493000	25.275789
160.205133	5904.730741	25.280807
160.050447	5906.017704	25.285824
160.184799	5911.669366	25.290842
160.498459	5931.646695	25.295859
160.294798	5937.916379	25.300877
160.658478	5930.472627	25.305895
160.786203	5930.313750	25.310912
160.325907	5939.385799	25.315930
160.992996	5936.913754	25.320947
160.707501	5954.544802	25.325965
161.108874	5954.403033	25.330983
161.431440	5963.854373	25.336000
161.397253	5977.983107	25.341018
161.563723	5982.594342	25.346035
161.431126	5997.111006	25.351053
161.559661	6000.901116	25.356071
161.846762	6015.307849	25.361088
161.844358	6019.424682	25.366106
162.152909	6036.558677	25.371123
162.269037	6046.743205	25.376141
162.301012	6053.007580	25.381159
162.526734	6064.857510	25.386176
162.904359	6072.803968	25.391194
162.896072	6080.545719	25.396211
163.101781	6098.365121	25.401229
163.438543	6094.426393	25.406247
163.597490	6104.661067	25.411264
163.327387	6125.989619	25.416282
163.950085	6122.135519	25.421299
164.247258	6125.829786	25.426317
164.049217	6133.276137	25.431335
164.426821	6144.268932	25.436352
164.829390	6144.963524	25.441370
164.949199	6144.790101	25.446387
164.988098	6168.052758	25.451405
165.056528	6181.524743	25.456423
165.471148	6182.324780	25.461440
165.202245	6183.683322	25.466458
165.549852	6197.692433	25.471475
165.373461	6202.322712	25.476493
165.511695	6209.214481	25.481511
165.473386	6227.088020	25.486528
165.893781	6238.405632	25.491546
166.216888	6250.647654	25.496563
166.320607	6258.021527	25.501581
166.801838	6261.421815	25.506599
166.854611	6279.858833	25.511616
166.635043	6290.080303	25.516634
167.146423	6294.451330	25.521651
167.458851	6313.488537	25.526669
167.273419	6312.419044	25.531687
167.361852	6321.446353	25.536704
167.579782	6336.896457	25.541722
168.208214	6339.168810	25.546739
167.990164	6368.201612	25.551757
168.235129	6363.001849	25.556775
168.774832	6382.713810	25.561792
168.926938	6390.357957	25.566810
169.173219	6382.528341	25.571827
169.033457	6386.944577	25.576845
169.254757	6393.087859	25.581863
170.547165	6403.523951	25.586880
170.187352	6403.526683	25.591898
171.029751	6395.616300	25.596915
171.261702	6399.743857	25.601933
171.249217	6390.174322	25.606951
171.165802	6390.932432	25.611968
171.051468	6395.259452	25.616986
171.260023	6382.340617	25.622003
171.296913	6377.062959	25.627021
171.464611	6392.088493	25.632039
171.554587	6385.179904	25.637056
171.374831	6380.889548	25.642074
171.407472	6385.610242	25.647091
171.314101	6395.783588	25.652109
171.338555	6413.663261	25.657127
171.488268	6426.955381	25.662144
171.609015	6440.981278	25.667162
172.140581	6463.703072	25.672180
172.172560	6475.959285	25.677197
172.529037	6480.824995	25.682215
172.742822	6499.865223	25.687232
172.686724	6512.397278	25.692250
173.144630	6523.702877	25.697268
173.197092	6531.413203	25.702285
173.452310	6542.782136	25.707303
173.605400	6538.183894	25.712320
173.626349	6564.360488	25.717338
173.781179	6578.775759	25.722356
173.837805	6594.866939	25.727373
174.310489	6601.046675	25.732391
174.715018	6615.214503	25.737408
174.511084	6618.144490	25.742426
174.799351	6621.903391	25.747444
174.922740	6633.220425	25.752461
174.869820	6639.608790	25.757479
175.657169	6649.079222	25.762496
175.309620	6667.595128	25.767514
175.449786	6663.996454	25.772532
175.697353	6674.605859	25.777549
175.440800	6695.794045	25.782567
175.805958	6700.661611	25.787584
176.302176	6721.908683	25.792602
176.582223	6721.975332	25.797620
176.463827	6742.775729	25.802637
176.745508	6752.855791	25.807655
176.849636	6761.994507	25.812672
177.109504	6776.071474	25.817690
177.533442	6775.212707	25.822708
177.915090	6783.098865	25.827725
177.816011	6805.537895	25.832743
178.374612	6803.575213	25.837760
178.362471	6813.455100	25.842778
178.494187	6818.191953	25.847796
178.693795	6821.254481	25.852813
178.392399	6831.002905	25.857831
179.032632	6856.874543	25.862848
179.296786	6856.599578	25.867866
179.546415	6848.099975	25.872884
179.706388	6872.376866	25.877901
179.855901	6889.511319	25.882919
180.080597	6884.175682	25.887936
179.903625	6900.224802	25.892954
180.073290	6910.688702	25.897972
180.424512	6916.451918	25.902989
180.580021	6929.948694	25.908007
181.010902	6942.641520	25.913024
181.298134	6947.420338	25.918042
181.289774	6952.093933	25.923060
181.767719	6963.425077	25.928077
181.752807	6967.064229	25.933095
181.808864	6962.875699	25.938112
181.925938	6980.832964	25.943130
182.355284	6987.177467	25.948148
182.518296	7001.096149	25.953165
182.207057	7003.525269	25.958183
182.347597	6996.832672	25.963200
182.324138	7011.995996	25.968218
182.452712	7030.305085	25.973236
182.873432	7051.545424	25.978253
182.866197	7061.468874	25.983271
183.130446	7072.369492	25.988288
183.568002	7089.721033	25.993306
183.953704	7095.949290	25.998324
183.810183	7105.076462	26.003341
183.734730	7123.105068	26.008359
184.193900	7131.080254	26.013376
184.073536	7146.596664	26.018394
184.667730	7163.677493	26.023412
185.123204	7174.336698	26.028429
184.901130	7189.742799	26.033447
184.962934	7186.917130	26.038464
185.119274	7215.684253	26.043482
185.554179	7222.492043	26.048500
185.594160	7243.602833	26.053517
186.379602	7242.835792	26.058535
186.546976	7234.541473	26.063552
186.908686	7258.130617	26.068570
186.999835	7263.672657	26.073588
187.732988	7254.374170	26.078605
187.851069	7262.614366	26.083623
188.187473	7245.766555	26.088640
188.523824	7249.593820	26.093658
188.370875	7238.363179	26.098676
188.385846	7233.653809	26.103693
188.430027	7234.581383	26.108711
188.972545	7235.064678	26.113728
188.766199	7243.002108	26.118746
188.610924	7240.494566	26.123764
188.827801	7240.747905	26.128781
188.731394	7243.907389	26.133799
188.736590	7252.319957	26.138816
189.132018	7273.182521	26.143834
189.263336	7286.872768	26.148852
189.377940	7296.710960	26.153869
189.412422	7309.538750	26.158887
189.669618	7319.139940	26.163904
189.864069	7342.821693	26.168922
189.955698	7353.834760	26.173940
190.226452	7362.243660	26.178957
190.050248	7387.451541	26.183975
190.842927	7399.882800	26.188992
190.963118	7420.188818	26.194010
191.022399	7419.412407	26.199028
191.472400	7445.118941	26.204045
191.209656	7459.796054	26.209063
191.289285	7468.670613	26.214080
191.461091	7486.872358	26.219098
191.244179	7504.794059	26.224116
191.736964	7521.206034	26.229133
192.017715	7540.906138	26.234151
192.380457	7562.023555	26.239168
192.318707	7582.421395	26.244186
192.841976	7596.574537	26.249204
193.393033	7610.429731	26.254221
193.614533	7616.658634	26.259239
193.485898	7643.134856	26.264256
193.480587	7649.636080	26.269274
193.936204	7665.836170	26.274292
194.223657	7674.709841	26.279309
194.271689	7705.218447	26.284327
195.034864	7714.989985	26.289344
195.072905	7715.347117	26.294362
195.130444	7728.127387	26.299380
195.550651	7726.669323	26.304397
195.605566	7744.911735	26.309415
195.790685	7747.421044	26.314432
196.145161	7761.089311	26.319450
196.156445	7771.038654	26.324468
196.540003	7777.535831	26.329485
196.492853	7786.515644	26.334503
197.006087	7802.548975	26.339520
197.159949	7812.084526	26.344538
197.251810	7823.710310	26.349556
197.757895	7829.408512	26.354573
197.446236	7839.054890	26.359591
197.896516	7846.665559	26.364608
197.895726	7860.837862	26.369626
198.325474	7872.019264	26.374644
198.896161	7869.142184	26.379661
198.623100	7886.864683	26.384679
198.846004	7896.727270	26.389696
199.178865	7900.716232	26.394714
198.972937	7910.579708	26.399732
199.313570	7921.737217	26.404749
199.404160	7924.766495	26.409767
199.624072	7943.399990	26.414784
199.747679	7948.315202	26.419802
199.849514	7953.925231	26.424820
200.372301	7963.725090	26.429837
200.697969	7960.251803	26.434855
200.438029	7972.936751	26.439872
201.065939	7980.753275	26.444890
201.291126	7989.055945	26.449908
201.347888	7992.466229	26.454925
201.282352	8011.861175	26.459943
201.789193	8023.137935	26.464960
201.856825	8023.878762	26.469978
202.197854	8040.895883	26.474996
202.260193	8053.293616	26.480013
202.546833	8060.819511	26.485031
202.629671	8075.499801	26.490048
202.994921	8082.214638	26.495066
202.887735	8100.062897	26.500084
203.577818	8109.318857	26.505101
204.518881	8086.708515	26.510119
204.936782	8077.048581	26.515136
205.006968	8072.254577	26.520154
205.017340	8079.315463	26.525172
205.422922	8074.367887	26.530189
205.145235	8071.541596	26.535207
205.483947	8070.279387	26.540224
205.605241	8079.185597	26.545242
205.626058	8101.781060	26.550260
205.727573	8103.106965	26.555277
205.555561	8104.905090	26.560295
205.962066	8114.827432	26.565312
206.009194	8130.438399	26.570330
206.226444	8141.984754	26.575348
206.558126	8154.356146	26.580365
206.120906	8166.554386	26.585383
206.362035	8183.265261	26.590400
206.906201	8194.053236	26.595418
206.786419	8214.375620	26.600436
207.060778	8223.122164	26.605453
207.120205	8238.349280	26.610471
206.957170	8268.471979	26.615488
207.564631	8284.232081	26.620506
207.673597	8305.797379	26.625524
208.015101	8324.885785	26.630541
208.306990	8345.285894	26.635559
208.242176	8355.089613	26.640576
208.817530	8368.221738	26.645594
208.866194	8400.262619	26.650612
209.240375	8404.352561	26.655629
209.536993	8417.869363	26.660647
209.835306	8434.852495	26.665664
209.998841	8455.275990	26.670682
210.086288	8460.316976	26.675700
210.489539	8484.693635	26.680717
210.746095	8492.631697	26.685735
211.080596	8509.880748	26.690752
211.182233	8511.825474	26.695770
211.311988	8527.815323	26.700788
211.800032	8539.029043	26.705805
211.673488	8555.728394	26.710823
211.576389	8569.464845	26.715840
212.138422	8573.260192	26.720858
211.849923	8599.323972	26.725876
212.764310	8610.862440	26.730893
212.874634	8628.004645	26.735911
212.780177	8637.525850	26.740928
213.411113	8656.941809	26.745946
213.423342	8669.073125	26.750964
213.442102	8671.788585	26.755981
213.912405	8681.852784	26.760999
214.010079	8693.014091	26.766016
214.258014	8699.775948	26.771034
214.332513	8717.646853	26.776052
214.766318	8737.501061	26.781069
214.719996	8747.172644	26.786087
215.127626	8763.027605	26.791104
215.484036	8780.829150	26.796122
215.262845	8781.116410	26.801140
215.750707	8796.570491	26.806157
215.950702	8806.222460	26.811175
215.823777	8823.894543	26.816192
216.030139	8831.310196	26.821210
216.463735	8853.734564	26.826228
216.465916	8871.822168	26.831245
217.054564	8872.130954	26.836263
217.639001	8870.577618	26.841280
218.273660	8881.509683	26.846298
217.684693	8901.019128	26.851316
218.147659	8902.424230	26.856333
218.686411	8916.822228	26.861351
218.524813	8938.695857	26.866368
218.736048	8925.446475	26.871386
218.881471	8950.609252	26.876404
218.588435	8957.013931	26.881421
218.681674	8975.763027	26.886439
218.509711	9000.795627	26.891456
219.553837	9021.624847	26.896474
219.521041	9042.382843	26.901492
219.840334	9068.437311	26.906509
220.063368	9083.446896	26.911527
220.391927	9095.042712	26.916544
220.807128	9118.707940	26.921562
220.715442	9119.678995	26.926580
221.194471	9150.684459	26.931597
221.298168	9163.092240	26.936615
221.524684	9179.926280	26.941632
221.930854	9193.372812	26.946650
222.177444	9214.630290	26.951668
222.429242	9230.188017	26.956685
222.419828	9241.682161	26.961703
222.734211	9247.994941	26.966720
223.031691	9270.115931	26.971738
223.061475	9276.498563	26.976756
223.182333	9292.941962	26.981773
223.469079	9311.032774	26.986791
223.425444	9334.397592	26.991808
224.040535	9348.506121	26.996826
223.895008	9370.371424	27.001844
224.396350	9384.838793	27.006861
224.366871	9407.105886	27.011879
224.502212	9430.370167	27.016896
225.061373	9438.488559	27.021914
225.438102	9455.760291	27.026932
225.251319	9473.565503	27.031949
225.751439	9492.412405	27.036967
225.580132	9515.693257	27.041984
226.556426	9528.479235	27.047002
226.877964	9529.710786	27.052020
227.289668	9552.041548	27.057037
227.771674	9552.483878	27.062055
227.459433	9562.128078	27.067072
227.857332	9577.356943	27.072090
228.111273	9594.000776	27.077108
228.248255	9594.917089	27.082125
228.413407	9604.852781	27.087143
228.350114	9614.817952	27.092160
228.553340	9622.104960	27.097178
228.711647	9645.732168	27.102196
229.403433	9664.198749	27.107213
229.300392	9671.372728	27.112231
229.282954	9683.269390	27.117248
229.736658	9700.684003	27.122266
230.255701	9712.566105	27.127284
230.206546	9729.396466	27.132301
230.675569	9725.177352	27.137319
230.825281	9736.425856	27.142336
231.533617	9741.950887	27.147354
231.382656	9750.673216	27.152372
232.120741	9741.278008	27.157389
232.213730	9756.257990	27.162407
232.539482	9763.866859	27.167424
233.077180	9763.741610	27.172442
233.014944	9778.445972	27.177460
232.898056	9770.021399	27.182477
233.245692	9775.438760	27.187495
233.267753	9797.698245	27.192512
233.250099	9799.955434	27.197530
233.847577	9814.635413	27.202548
233.694249	9825.088412	27.207565
233.902002	9834.477635	27.212583
233.955102	9847.162179	27.217600
234.324068	9872.067005	27.222618
234.492638	9889.535935	27.227636
234.903415	9899.180712	27.232653
234.820369	9918.217282	27.237671
234.741770	9944.003777	27.242688
235.300724	9958.380475	27.247706
235.671121	9974.643299	27.252724
235.890341	10002.034563	27.257741
236.302480	10010.889823	27.262759
236.361659	10025.348022	27.267776
237.017263	10042.087206	27.272794
237.349045	10044.940120	27.277812
237.229502	10051.033822	27.282829
237.873604	10068.712597	27.287847
238.026424	10087.898680	27.292864
238.056007	10097.044405	27.297882
238.720286	10109.949130	27.302900
238.775197	10121.155882	27.307917
239.469224	10118.713821	27.312935
239.508016	10131.943884	27.317952
239.878854	10129.981866	27.322970
240.108272	10133.987519	27.327988
240.286206	10150.309064	27.333005
240.780959	10152.539702	27.338023
240.850048	10151.679549	27.343040
240.850678	10168.373050	27.348058
240.849330	10179.591808	27.353076
240.688158	10190.077814	27.358093
241.500805	10201.570070	27.363111
241.320184	10215.380808	27.368128
241.795536	10228.128920	27.373146
241.873843	10239.051062	27.378164
242.146939	10261.997996	27.383181
242.378125	10270.187079	27.388199
242.690491	10291.100787	27.393216
243.038647	10306.871659	27.398234
243.428291	10304.600400	27.403252
243.837384	10312.938451	27.408269
244.296874	10321.849592	27.413287
244.366805	10339.024960	27.418304
244.230744	10347.072684	27.423322
244.562441	10352.262214	27.428340
244.774119	10371.613031	27.433357
244.736847	10371.315779	27.438375
244.722067	10391.826166	27.443392
244.997230	10403.146987	27.448410
245.429530	10424.439904	27.453428
245.213867	10442.105315	27.458445
245.742995	10459.404625	27.463463
245.484560	10485.463166	27.468480
245.722758	10497.850766	27.473498
246.296032	10514.085437	27.478516
246.302357	10532.461337	27.483533
247.300448	10547.726433	27.488551
247.442111	10569.740758	27.493568
247.366679	10590.254548	27.498586
247.749623	10612.546881	27.503604
247.723420	10618.398801	27.508621
247.781909	10637.458135	27.513639
248.347083	10655.544527	27.518656
248.540529	10678.365517	27.523674
248.653536	10694.044092	27.528692
248.694534	10723.011537	27.533709
249.252723	10746.716429	27.538727
249.497004	10756.163545	27.543744
249.570854	10782.006251	27.548762
250.207485	10801.423561	27.553780
250.049476	10828.928807	27.558797
250.093498	10856.778199	27.563815
250.381634	10873.244149	27.568832
250.504609	10899.849774	27.573850
251.143609	10915.392457	27.578868
251.297115	10953.802812	27.583885
252.016578	10971.518002	27.588903
252.360092	10998.108165	27.593920
252.497196	11028.819818	27.598938
253.008233	11031.764794	27.603956
253.165278	11047.885149	27.608973
253.583671	11056.739928	27.613991
253.775820	11067.161601	27.619008
254.131246	11088.151552	27.624026
254.737634	11091.359473	27.629044
254.759764	11102.985597	27.634061
254.852844	11107.947477	27.639079
255.158341	11134.499581	27.644096
255.572703	11151.637525	27.649114
255.730323	11151.824425	27.654132
255.586907	11171.995845	27.659149
256.686923	11184.754116	27.664167
256.375416	11200.553296	27.669184
256.189547	11220.330396	27.674202
256.952945	11222.866425	27.679220
257.102098	11249.421080	27.684237
257.910615	11268.028849	27.689255
257.740230	11277.838007	27.694272
257.923687	11296.010077	27.699290
258.177661	11301.739378	27.704308
258.252728	11322.369328	27.709325
258.595096	11336.913642	27.714343
259.009137	11353.638166	27.719360
258.983919	11371.448287	27.724378
259.078810	11386.722939	27.729396
259.442297	11410.471801	27.734413
259.863900	11425.363747	27.739431
260.251061	11445.701801	27.744448
259.988835	11461.945029	27.749466
260.644840	11469.044996	27.754484
260.666964	11493.974736	27.759501
260.906044	11520.926188	27.764519
261.239508	11538.500291	27.769536
261.246235	11550.931162	27.774554
261.816405	11568.967131	27.779572
261.481012	11589.014342	27.784589
262.005746	11604.692334	27.789607
262.357059	11625.579326	27.794624
262.595729	11644.781973	27.799642
262.662289	11665.498891	27.804660
263.313981	11687.674616	27.809677
263.544819	11699.183156	27.814695
263.237723	11720.069187	27.819712
263.821192	11743.881901	27.824730
264.577416	11764.042491	27.829748
264.430420	11789.431726	27.834765
264.815702	11814.406049	27.839783
265.151635	11831.771628	27.844800
265.238781	11848.610956	27.849818
266.005707	11866.025887	27.854836
265.855850	11885.990667	27.859853
265.976966	11904.548863	27.864871
266.662629	11910.886489	27.869888
266.969599	11931.746032	27.874906
266.891462	11950.370222	27.879924
266.903442	11982.944016	27.884941
267.197161	11990.009358	27.889959
267.651533	12010.343810	27.894976
268.176673	12024.815816	27.899994
268.692031	12050.066908	27.905012
268.520004	12062.497697	27.910029
268.968281	12075.952342	27.915047
269.220183	12102.359476	27.920064
269.573467	12123.404602	27.925082
269.911553	12138.196516	27.930100
270.194686	12167.301931	27.935117
270.322297	12185.521501	27.940135
271.228185	12191.471049	27.945152
271.369641	12210.724238	27.950170
271.345235	12229.479230	27.955188
271.512083	12244.673832	27.960205
271.611655	12254.671729	27.965223
272.057045	12284.203476	27.970240
272.685429	12292.400695	27.975258
272.686445	12314.754876	27.980276
273.081121	12332.762229	27.985293
273.249988	12352.709151	27.990311
273.448979	12359.562108	27.995328
273.578175	12375.902695	28.000346
274.275681	12393.976351	28.005364
274.262440	12409.477188	28.010381
274.986217	12423.883648	28.015399
275.682468	12424.971438	28.020416
275.700812	12437.318968	28.025434
275.988014	12440.513970	28.030452
276.228458	12453.846707	28.035469
276.498728	12476.117849	28.040487
276.663164	12491.644604	28.045504
276.962048	12487.552588	28.050522
277.174386	12505.872877	28.055540
277.189643	12514.106240	28.060557
277.689445	12528.936285	28.065575
278.040166	12536.062377	28.070592
277.675971	12565.860333	28.075610
278.293849	12568.315139	28.080628
278.331829	12590.474383	28.085645
278.517656	12610.377868	28.090663
278.908862	12626.990261	28.095680
279.007089	12654.262238	28.100698
279.522309	12671.489979	28.105716
279.700724	12690.785236	28.110733
279.362109	12712.713090	28.115751
279.700326	12736.281266	28.120768
280.001950	12756.299397	28.125786
280.355016	12781.681103	28.130804
280.593302	12810.273478	28.135821
280.518535	12833.293833	28.140839
281.103972	12849.206514	28.145856
281.206742	12883.684498	28.150874
281.495001	12908.789154	28.155892
281.757814	12939.130536	28.160909
282.109346	12966.729604	28.165927
282.524898	12992.111277	28.170944
282.960158	13014.518262	28.175962
283.321974	13035.698860	28.180980
283.595594	13056.650135	28.185997
284.030473	13080.895192	28.191015
284.234587	13101.961618	28.196032
284.588319	13125.597324	28.201050
284.962407	13144.748704	28.206068
285.070495	13171.596712	28.211085
285.351940	13196.623867	28.216103
285.942040	13200.238931	28.221120
285.828392	13227.709138	28.226138
286.249380	13243.306850	28.231156
286.980500	13263.911943	28.236173
286.865536	13291.227706	28.241191
287.418801	13301.215087	28.246208
287.704034	13329.175607	28.251226
288.420398	13337.504770	28.256244
288.773224	13363.825221	28.261261
288.772385	13382.388181	28.266279
288.963038	13398.448435	28.271296
288.931806	13417.777272	28.276314
289.053265	13428.820823	28.281332
289.462544	13461.420189	28.286349
289.823700	13479.446518	28.291367
290.413120	13501.384648	28.296384
290.365146	13520.972014	28.301402
290.426756	13538.963213	28.306420
291.096761	13565.433215	28.311437
291.528216	13590.560555	28.316455
292.240237	13607.174082	28.321472
292.206197	13625.474046	28.326490
292.711966	13646.885421	28.331508
292.937268	13659.892943	28.336525
292.876438	13688.685084	28.341543
293.067843	13699.818894	28.346560
293.235917	13725.461381	28.351578
293.492853	13741.653655	28.356596
293.660149	13767.997413	28.361613
294.170855	13797.976053	28.366631
294.269654	13815.547980	28.371648
294.481329	13854.956229	28.376666
294.722863	13874.302805	28.381684
295.427122	13890.387237	28.386701
295.497533	13916.291611	28.391719
295.772319	13947.807543	28.396736
295.926845	13970.540706	28.401754
296.183379	13998.263531	28.406772
296.818208	14013.882068	28.411789
297.094981	14047.861187	28.416807
297.662182	14063.692479	28.421824
297.976381	14092.274893	28.426842
298.155928	14112.345159	28.431860
299.243534	14126.838046	28.436877
299.009263	14144.516139	28.441895
299.694024	14158.042600	28.446912
299.642227	14187.629932	28.451930
299.973058	14197.962131	28.456948
300.585119	14210.479936	28.461965
300.540750	14219.209732	28.466983
300.782516	14227.389406	28.472000
301.046871	14247.414948	28.477018
301.199722	14265.575714	28.482036
301.697693	14274.119519	28.487053
301.780133	14298.051834	28.492071
301.909723	14319.431308	28.497088
302.286339	14343.456558	28.502106
302.793390	14355.712990	28.507124
303.439314	14360.977579	28.512141
303.152419	14390.428352	28.517159
303.753327	14408.339052	28.522176
304.242363	14415.902125	28.527194
304.053830	14445.419688	28.532212
304.285232	14452.899964	28.537229
304.548113	14469.881474	28.542247
305.073082	14502.050777	28.547264
305.403327	14522.363158	28.552282
305.415747	14545.706693	28.557300
305.973788	14568.118387	28.562317
305.806414	14593.688259	28.567335
306.486800	14616.014522	28.572352
306.981250	14637.630913	28.577370
307.372717	14661.129972	28.582388
307.572019	14677.723691	28.587405
307.902987	14699.384710	28.592423
308.438033	14722.138118	28.597440
308.380968	14749.611127	28.602458
308.756484	14778.219704	28.607476
309.420057	14800.536184	28.612493
309.129507	14822.487355	28.617511
309.921669	14845.525934	28.622528
310.020551	14865.306435	28.627546
310.325181	14880.269960	28.632564
310.805331	14907.996977	28.637581
310.616238	14932.834828	28.642599
311.288638	14956.375517	28.647616
311.297733	14977.152422	28.652634
311.317312	15003.546291	28.657652
311.651501	15023.710147	28.662669
312.097009	15061.558806	28.667687
312.634487	15089.333956	28.672704
313.002829	15113.228822	28.677722
312.863441	15144.773709	28.682740
313.596197	15175.604059	28.687757
313.716175	15205.507154	28.692775
313.701084	15233.495403	28.697792
314.338984	15264.315488	28.702810
314.482890	15298.030236	28.707828
314.947691	15323.460996	28.712845
315.064110	15349.123228	28.717863
315.279158	15385.265223	28.722880
316.085684	15409.426605	28.727898
316.281328	15442.574474	28.732916
316.875965	15469.036821	28.737933
317.081404	15491.814352	28.742951
317.424517	15512.160510	28.747968
317.961781	15533.319562	28.752986
318.392468	15559.678223	28.758004
318.577294	15581.451568	28.763021
318.732022	15610.250734	28.768039
319.280625	15618.600869	28.773056
319.790412	15638.554681	28.778074
320.133159	15677.008112	28.783092
320.203116	15678.756408	28.788109
320.810149	15708.325004	28.793127
320.713395	15727.053708	28.798144
321.095518	15746.787592	28.803162
321.588143	15759.697819	28.808180
322.344832	15779.177241	28.813197
322.013807	15801.214828	28.818215
322.393250	15818.596188	28.823232
322.992982	15822.046017	28.828250
323.087363	15857.490842	28.833268
323.150473	15869.290332	28.838285
323.561910	15887.649013	28.843303
323.622820	15911.782538	28.848320
324.432263	15930.824305	28.853338
324.520514	15958.377349	28.858356
324.975781	15972.699078	28.863373
325.076368	16000.449232	28.868391
325.542702	16027.371472	28.873408
325.837233	16048.433303	28.878426
325.911324	16068.717963	28.883444
326.579166	16092.478699	28.888461
326.902285	16115.112196	28.893479
326.931853	16151.549998	28.898496
327.255608	16176.343862	28.903514
327.662716	16207.665913	28.908532
327.889531	16224.165065	28.913549
327.882822	16259.402212	28.918567
328.257807	16290.868404	28.923584
328.958938	16322.466751	28.928602
328.948297	16349.701045	28.933620
329.336823	16369.955719	28.938637
329.820120	16406.711426	28.943655
330.100740	16441.028989	28.948672
330.623211	16463.331610	28.953690
331.093313	16485.961471	28.958708
331.797245	16509.833935	28.963725
331.928185	16526.199913	28.968743
332.226925	16553.442885	28.973760
332.580372	16576.975517	28.978778
332.784723	16597.890989	28.983796
333.145758	16623.188115	28.988813
333.734303	16656.153346	28.993831
334.063915	16671.187002	28.998848
334.208417	16691.736083	29.003866
334.706618	16715.002999	29.008884
335.311396	16727.305660	29.013901
335.285038	16756.387591	29.018919
335.395714	16784.342600	29.023936
335.869229	16817.964159	29.028954
336.161594	16845.322251	29.033972
336.370024	16860.874094	29.038989
336.503880	16890.284892	29.044007
337.496877	16918.405110	29.049024
337.764489	16942.741283	29.054042
337.801982	16969.551975	29.059060
338.089244	16996.614172	29.064077
338.360389	17010.242194	29.069095
339.119029	17044.823924	29.074112
339.523566	17069.334642	29.079130
339.072230	17099.513369	29.084148
339.822277	17122.769756	29.089165
340.207638	17153.474499	29.094183
340.548443	17179.593610	29.099200
341.103218	17206.601562	29.104218
340.942424	17238.680719	29.109236
341.524456	17265.425475	29.114253
341.865224	17289.693769	29.119271
341.890301	17328.686688	29.124288
342.375926	17351.631000	29.129306
342.517595	17380.220065	29.134324
342.950476	17404.878385	29.139341
343.816337	17423.176825	29.144359
344.242336	17437.589514	29.149376
344.571281	17468.790032	29.154394
344.703847	17482.136861	29.159412
345.105548	17503.982641	29.164429
345.431278	17520.388440	29.169447
345.357522	17541.342178	29.174464
346.119728	17568.634015	29.179482
345.980803	17592.775672	29.184500
346.674415	17619.174934	29.189517
347.059862	17639.658852	29.194535
346.996891	17674.206153	29.199552
347.452364	17703.877363	29.204570
348.036742	17731.544744	29.209588
348.591962	17751.060885	29.214605
349.202104	17782.957005	29.219623
349.460047	17798.362861	29.224640
349.806578	17818.638269	29.229658
349.622113	17847.872954	29.234676
350.159179	17867.253070	29.239693
350.822381	17877.952146	29.244711
351.009938	17908.695390	29.249728
351.528088	17930.536046	29.254746
351.565398	17960.721694	29.259764
352.427511	17971.370713	29.264781
352.658303	18000.559533	29.269799
353.145822	18017.414226	29.274816
353.281399	18035.259060	29.279834
353.487820	18066.877739	29.284852
353.841801	18090.709055	29.289869
354.205909	18118.089295	29.294887
354.329950	18145.071265	29.299904
355.200129	18155.908650	29.304922
355.028232	18200.525246	29.309940
355.525756	18229.331478	29.314957
355.851271	18248.132304	29.319975
356.048180	18287.201313	29.324992
356.416787	18313.311279	29.330010
356.704563	18340.691154	29.335028
356.849084	18369.173828	29.340045
357.162513	18404.004620	29.345063
357.654299	18436.577393	29.350080
358.416103	18468.204494	29.355098
358.298926	18497.296941	29.360116
358.676224	18530.266866	29.365133
359.477511	18563.776936	29.370151
359.712887	18597.539969	29.375168
359.987513	18619.065753	29.380186
360.160861	18647.797029	29.385204
360.342772	18686.635431	29.390221
360.997472	18723.630874	29.395239
361.164575	18754.347067	29.400256
361.806523	18782.114332	29.405274
361.666282	18812.727132	29.410292
362.480990	18847.941397	29.415309
362.607579	18884.849289	29.420327
362.591776	18925.412314	29.425344
363.461665	18951.918454	29.430362
363.688895	18984.615716	29.435380
364.350603	19022.627805	29.440397
364.397023	19050.040165	29.445415
364.902583	19085.770808	29.450432
365.509947	19120.114585	29.455450
365.857113	19143.897714	29.460468
366.371896	19175.343531	29.465485
366.731503	19202.770227	29.470503
367.117297	19233.149657	29.475520
367.902962	19247.153549	29.480538
368.104611	19278.699126	29.485556
367.874420	19307.355586	29.490573
368.560263	19329.083096	29.495591
368.626633	19350.263229	29.500608
368.703907	19383.092052	29.505626
369.139976	19415.435104	29.510644
369.306783	19446.973773	29.515661
370.278380	19477.280777	29.520679
370.510286	19506.648581	29.525696
370.752906	19531.528942	29.530714
371.125302	19560.843232	29.535732
371.097106	19598.743376	29.540749
371.705437	19621.115159	29.545767
372.179961	19662.127306	29.550784
372.703099	19691.051730	29.555802
373.142190	19726.806594	29.560820
373.354879	19759.444246	29.565837
373.437283	19799.387160	29.570855
373.645803	19836.505146	29.575872
374.216171	19873.699205	29.580890
374.649636	19905.272660	29.585908
374.857361	19947.413918	29.590925
375.320410	19977.510721	29.595943
375.994715	20023.009832	29.600960
376.365560	20050.303274	29.605978
376.892015	20086.342064	29.610996
376.825517	20119.352594	29.616013
377.388487	20152.062397	29.621031
377.960270	20188.808237	29.626048
378.252948	20231.758172	29.631066
378.726358	20260.021488	29.636084
379.355095	20297.390438	29.641101
379.504012	20331.271096	29.646119
379.690532	20370.156342	29.651136
380.007075	20395.405318	29.656154
380.196878	20441.878492	29.661172
380.850798	20467.921372	29.666189
381.786120	20505.703934	29.671207
382.420549	20540.930534	29.676224
382.793376	20569.001545	29.681242
383.148588	20590.270458	29.686260
383.400940	20617.810710	29.691277
383.960932	20639.786852	29.696295
384.307856	20662.409278	29.701312
384.919333	20696.161245	29.706330
385.279054	20711.635598	29.711348
385.397027	20751.012533	29.716365
385.785228	20762.931507	29.721383
386.267900	20796.943923	29.726400
386.444943	20822.840825	29.731418
386.987322	20849.394523	29.736436
386.811262	20881.482040	29.741453
387.136015	20910.066545	29.746471
387.359988	20957.060016	29.751488
387.880739	20989.127021	29.756506
388.227146	21016.659417	29.761524
388.490905	21057.859135	29.766541
389.073623	21091.464640	29.771559
389.442638	21129.545619	29.776576
389.915031	21170.839265	29.781594
390.623428	21201.664058	29.786612
390.797062	21235.675090	29.791629
391.217829	21262.482181	29.796647
391.803112	21304.485063	29.801664
392.402230	21325.899806	29.806682
392.557591	21347.561002	29.811700
392.682183	21390.223858	29.816717
393.511501	21415.791898	29.821735
394.121447	21440.655050	29.826752
394.190673	21465.369139	29.831770
394.404624	21492.316355	29.836788
394.467175	21521.157650	29.841805
395.303830	21545.151358	29.846823
395.246040	21576.178892	29.851840
396.118717	21607.920075	29.856858
396.520480	21640.588098	29.861876
396.415863	21672.400320	29.866893
396.902098	21691.836425	29.871911
397.191863	21726.089177	29.876928
397.739030	21770.582287	29.881946
398.042690	21796.568052	29.886964
398.096580	21836.298399	29.891981
398.488510	21871.698056	29.896999
398.848162	21917.819522	29.902016
399.170848	21950.797427	29.907034
399.422882	21992.316869	29.912052
400.072539	22041.818003	29.917069
400.728064	22079.805383	29.922087
401.173275	22113.535267	29.927104
401.443324	22161.282645	29.932122
401.825121	22201.733266	29.937140
402.221789	22241.827781	29.942157
402.464454	22273.567613	29.947175
403.030593	22315.537726	29.952192
403.392654	22358.576201	29.957210
403.930009	22396.778585	29.962228
404.155590	22438.454759	29.967245
404.908420	22481.760879	29.972263
405.357158	22526.473310	29.977280
405.670751	22566.075972	29.982298
406.175767	22593.042283	29.987316
406.800024	22632.691202	29.992333
407.326862	22659.559400	29.997351
407.799710	22697.033138	30.002368
408.204543	22724.470291	30.007386
408.937888	22751.438967	30.012404
408.981337	22783.962787	30.017421
409.469107	22816.695105	30.022439
409.875835	22846.786148	30.027456
410.055510	22885.696364	30.032474
410.617941	22911.535632	30.037492
410.748703	22950.466274	30.042509
411.363896	22992.190007	30.047527
411.725584	23028.500101	30.052544
412.032742	23061.905665	30.057562
412.777306	23094.566621	30.062580
412.938375	23134.447072	30.067597
413.607321	23162.627040	30.072615
413.931428	23201.824892	30.077632
414.391662	23237.532244	30.082650
414.640274	23260.842877	30.087668
414.910579	23300.611761	30.092685
415.564179	23336.333238	30.097703
415.850634	23365.685593	30.102720
416.276816	23403.439699	30.107738
417.035842	23443.890632	30.112756
417.087230	23476.199480	30.117773
417.195084	23511.836132	30.122791
418.139840	23531.543464	30.127808
418.589310	23576.359246	30.132826
418.983227	23602.080460	30.137844
419.320475	23646.332598	30.142861
419.958031	23680.281466	30.147879
420.286780	23717.722820	30.152896
420.682356	23744.853179	30.157914
421.390527	23768.642209	30.162932
421.475969	23804.706292	30.167949
421.700291	23826.422581	30.172967
422.222538	23857.621911	30.177984
422.584294	23887.405598	30.183002
423.041699	23920.662677	30.188020
423.364682	23949.700517	30.193037
423.643261	23987.535720	30.198055
424.017637	24014.606572	30.203072
424.156313	24062.183175	30.208090
424.597673	24097.509533	30.213108
425.008389	24142.427445	30.218125
425.326054	24185.540011	30.223143
426.240470	24215.812698	30.228160
426.304034	24248.872910	30.233178
426.602807	24288.803608	30.238196
427.046322	24337.205214	30.243213
427.510727	24376.648815	30.248231
428.320828	24408.998318	30.253248
428.619293	24465.423559	30.258266
428.889552	24490.956738	30.263284
429.298893	24543.364514	30.268301
429.449023	24593.139814	30.273319
429.553059	24631.066766	30.278336
429.919448	24690.439602	30.283354
430.723783	24732.838827	30.288372
431.093138	24783.711486	30.293389
431.354522	24836.010485	30.298407
431.853601	24879.709139	30.303424
432.260757	24934.140592	30.308442
432.704181	24974.599813	30.313460
433.103417	25033.292300	30.318477
433.479766	25089.062472	30.323495
434.292161	25133.180267	30.328512
434.328659	25193.351996	30.333530
435.163542	25238.193280	30.338548
435.582698	25287.517367	30.343565
436.019878	25333.830488	30.348583
436.411455	25380.612210	30.353600
436.753032	25442.443268	30.358618
437.298875	25478.665757	30.363636
437.689102	25538.448152	30.368653
438.036019	25586.602455	30.373671
438.306967	25633.523737	30.378688
438.798725	25693.189568	30.383706
439.389016	25737.065393	30.388724
440.096840	25785.504922	30.393741
440.183927	25848.976051	30.398759
440.893260	25895.690236	30.403776
441.732149	25937.941225	30.408794
442.177179	25976.095378	30.413812
442.601216	26029.206242	30.418829
442.745086	26073.506647	30.423847
443.621278	26106.815508	30.428864
443.710654	26155.201108	30.433882
444.679690	26199.770712	30.438900
445.062119	26246.006016	30.443917
445.599420	26286.491084	30.448935
446.049622	26327.407009	30.453952
446.494867	26376.306213	30.458970
447.135132	26403.951691	30.463988
447.740204	26434.194011	30.469005
447.656314	26486.077343	30.474023
448.410481	26513.762012	30.479040
448.743419	26559.879379	30.484058
449.489812	26594.113173	30.489076
449.809188	26635.606394	30.494093
450.255557	26675.841031	30.499111
450.895912	26709.124621	30.504128
450.958943	26741.771855	30.509146
451.554895	26769.683907	30.514164
452.072734	26809.225018	30.519181
451.991422	26846.938663	30.524199
452.337808	26881.406244	30.529216
453.269301	26927.348529	30.534234
453.707258	26950.741224	30.539252
454.095564	26990.625317	30.544269
454.653048	27032.846824	30.549287
455.323657	27067.655804	30.554304
455.356297	27101.016261	30.559322
455.772321	27134.386249	30.564340
456.138747	27163.971789	30.569357
456.506190	27213.409792	30.574375
457.421514	27248.825441	30.579392
457.522981	27289.993862	30.584410
457.979042	27322.681595	30.589428
458.690160	27363.602984	30.594445
458.668653	27413.860857	30.599463
459.057370	27453.802678	30.604480
459.227920	27507.848308	30.609498
459.515893	27555.757373	30.614516
460.154264	27600.154306	30.619533
460.387581	27655.682155	30.624551
461.771315	27704.342751	30.629568
461.960852	27756.034793	30.634586
462.364172	27804.115994	30.639604
462.611987	27853.397307	30.644621
462.950990	27910.394652	30.649639
463.918113	27957.275465	30.654656
464.162814	27996.052612	30.659674
464.858805	28038.096490	30.664692
465.293377	28092.342500	30.669709
465.936708	28141.878597	30.674727
466.521998	28183.914831	30.679744
467.138325	28222.242313	30.684762
467.527497	28258.734491	30.689780
467.891919	28298.384692	30.694797
468.259786	28338.868777	30.699815
469.142827	28372.022263	30.704832
469.837569	28413.169552	30.709850
469.924026	28453.906529	30.714868
470.688740	28492.432505	30.719885
470.859358	28539.072798	30.724903
471.512100	28574.974342	30.729920
471.937320	28620.064249	30.734938
472.213881	28662.946256	30.739956
472.711457	28696.786414	30.744973
472.947887	28752.986770	30.749991
474.027182	28788.474226	30.755008
474.041973	28827.933695	30.760026
474.147600	28874.964188	30.765044
474.971642	28920.605425	30.770061
475.473251	28970.854713	30.775079
475.956122	29010.089513	30.780096
475.924737	29060.795442	30.785114
476.383790	29112.480297	30.790132
477.203985	29158.539855	30.795149
477.499951	29205.971125	30.800167
477.949809	29261.892920	30.805184
478.106015	29315.484121	30.810202
478.736156	29363.166826	30.815220
478.892623	29399.501525	30.820237
479.648778	29457.796876	30.825255
480.207198	29516.755480	30.830272
480.479755	29565.095172	30.835290
480.759128	29619.116676	30.840308
481.418585	29678.565614	30.845325
481.268402	29732.123710	30.850343
482.147377	29790.268018	30.855360
482.755370	29844.510455	30.860378
483.257979	29896.234702	30.865396
483.586991	29944.971003	30.870413
483.966493	30005.596246	30.875431
484.399570	30055.201494	30.880448
484.865761	30109.390981	30.885466
485.190378	30171.643575	30.890484
485.978659	30221.958476	30.895501
486.436115	30284.614137	30.900519
486.987076	30339.220804	30.905536
487.594063	30395.076809	30.910554
488.160073	30448.347582	30.915572
489.399044	30479.666072	30.920589
489.659153	30537.909415	30.925607
490.180455	30577.608968	30.930624
490.805002	30622.830074	30.935642
491.062903	30671.332685	30.940660
491.931946	30716.389270	30.945677
492.264320	30767.017122	30.950695
492.611421	30812.655069	30.955712
493.012394	30853.549810	30.960730
493.403280	30921.490026	30.965748
494.002597	30968.264631	30.970765
494.938559	31018.994531	30.975783
495.443232	31064.943400	30.980800
495.619604	31107.422623	30.985818
496.102574	31158.154275	30.990836
496.542000	31201.129832	30.995853
496.854304	31255.005044	31.000871
497.494026	31313.696843	31.005888
497.845788	31363.336922	31.010906
498.265875	31422.253078	31.015924
499.370545	31463.076734	31.020941
499.715920	31525.070943	31.025959
500.516405	31575.134346	31.030976
500.935372	31620.851316	31.035994
501.273246	31664.804652	31.041012
501.617161	31700.968624	31.046029
501.963350	31760.055356	31.051047
502.499190	31804.654420	31.056064
503.022969	31861.361888	31.061082
503.127626	31930.974954	31.066100
503.853255	31979.274595	31.071117
504.231091	32027.009270	31.076135
504.530899	32089.593911	31.081152
505.284043	32152.834764	31.086170
505.962506	32216.940975	31.091188
506.159984	32273.454109	31.096205
506.510125	32334.097061	31.101223
507.534708	32391.840209	31.106240
507.702491	32445.083635	31.111258
507.963564	32510.899858	31.116276
508.769706	32563.885552	31.121293
509.460320	32624.747870	31.126311
509.595322	32680.892561	31.131328
510.048901	32745.844848	31.136346
510.300689	32805.771199	31.141364
511.211571	32867.769327	31.146381
511.854781	32923.019506	31.151399
512.302546	32980.298266	31.156416
513.098699	33035.701810	31.161434
513.771070	33091.877236	31.166452
514.174176	33155.213874	31.171469
514.540350	33204.426149	31.176487
514.833712	33256.760521	31.181504
515.704636	33313.733667	31.186522
516.156434	33366.397547	31.191540
516.823774	33415.917200	31.196557
517.123203	33476.729456	31.201575
517.446795	33528.705716	31.206592
518.151192	33569.792179	31.211610
518.457425	33631.166508	31.216628
519.056367	33683.580529	31.221645
519.726884	33731.058278	31.226663
520.167649	33778.768115	31.231680
520.687855	33832.851327	31.236698
520.847603	33895.754120	31.241716
521.713743	33945.610588	31.246733
522.269044	34006.776293	31.251751
522.107942	34060.656991	31.256768
523.182579	34118.049309	31.261786
523.784523	34179.941629	31.266804
524.089414	34237.151345	31.271821
524.525774	34294.979210	31.276839
525.316376	34366.743759	31.281856
525.982253	34419.686550	31.286874
526.219081	34481.251255	31.291892
527.099612	34537.574969	31.296909
527.653187	34597.503405	31.301927
527.817058	34651.315740	31.306944
528.340405	34703.883234	31.311962
528.922240	34777.268881	31.316980
529.319049	34830.090449	31.321997
529.485268	34900.241123	31.327015
530.064038	34966.457847	31.332032
531.040655	35028.534234	31.337050
531.375196	35108.029685	31.342068
532.163625	35170.034794	31.347085
532.566356	35221.756227	31.352103
533.010275	35285.541782	31.357120
533.818990	35341.758746	31.362138
534.519151	35401.318734	31.367156
535.138255	35459.873586	31.372173
535.551262	35522.823739	31.377191
536.435058	35580.003315	31.382208
537.359736	35635.273412	31.387226
537.696215	35693.746712	31.392244
538.065659	35744.241637	31.397261
538.743179	35804.040251	31.402279
539.100238	35863.427638	31.407296
540.226067	35908.353985	31.412314
540.123634	35968.502849	31.417332
540.589367	36021.322903	31.422349
541.055702	36069.508125	31.427367
541.943290	36139.334914	31.432384
542.296078	36197.402357	31.437402
542.755252	36264.210936	31.442420
543.365995	36315.934063	31.447437
544.038844	36362.791342	31.452455
544.873188	36428.378201	31.457472
545.608121	36471.280283	31.462490
545.763580	36539.376651	31.467508
546.146799	36591.547093	31.472525
546.573352	36644.627757	31.477543
547.159061	36704.373716	31.482560
547.829301	36762.487824	31.487578
548.313120	36822.964611	31.492596
548.765361	36885.210741	31.497613
549.029952	36947.979666	31.502631
549.352085	37013.724421	31.507648
550.043489	37068.592125	31.512666
550.403552	37148.634990	31.517684
551.110720	37210.620816	31.522701
551.428132	37278.517106	31.527719
551.806954	37347.662374	31.532736
552.357049	37413.846915	31.537754
552.785477	37472.222141	31.542772
553.358887	37536.000452	31.547789
554.115243	37592.364335	31.552807
554.427808	37664.815595	31.557824
555.068771	37733.453099	31.562842
555.454497	37796.964367	31.567860
555.931481	37878.022388	31.572877
556.547066	37944.621990	31.577895
556.531054	38019.098896	31.582912
557.357423	38090.876686	31.587930
557.467164	38186.892132	31.592948
558.367182	38261.643776	31.597965
559.222409	38331.963376	31.602983
559.071841	38417.099386	31.608000
560.193303	38493.758571	31.613018
560.708316	38578.639202	31.618036
561.378622	38653.466122	31.623053
561.833772	38728.421856	31.628071
562.428877	38807.257810	31.633088
563.138239	38889.851571	31.638106
563.868317	38972.663742	31.643124
564.444210	39041.853133	31.648141
565.335875	39116.204301	31.653159
565.784499	39196.076457	31.658176
566.659961	39253.045777	31.663194
567.300474	39324.818824	31.668212
567.661426	39403.156066	31.673229
568.641979	39460.337141	31.678247
569.031459	39539.157364	31.683264
569.960858	39595.619528	31.688282
570.137258	39668.250594	31.693300
571.065180	39734.547490	31.698317
571.981313	39794.806784	31.703335
571.961432	39865.002793	31.708352
572.979040	39920.680425	31.713370
573.769334	39995.632312	31.718388
574.168703	40055.125803	31.723405
574.676132	40121.768003	31.728423
575.483677	40189.710492	31.733440
575.910581	40246.524990	31.738458
576.468192	40314.140196	31.743476
576.777378	40377.544515	31.748493
577.357342	40442.538312	31.753511
577.886890	40512.188668	31.758528
578.684609	40578.774150	31.763546
579.165511	40643.107339	31.768564
579.716013	40709.504255	31.773581
580.351975	40775.445272	31.778599
581.138568	40846.270743	31.783616
581.870620	40905.100962	31.788634
582.732231	40978.761166	31.793652
582.686579	41039.098629	31.798669
583.226765	41104.682484	31.803687
583.853185	41165.686642	31.808704
584.441114	41238.410262	31.813722
584.968752	41298.614379	31.818740
585.141005	41371.846268	31.823757
586.284764	41433.427916	31.828775
586.692518	41514.851853	31.833792
587.374531	41579.339708	31.838810
587.948650	41646.216441	31.843828
588.773926	41701.574544	31.848845
589.733199	41759.030611	31.853863
590.383819	41818.483214	31.858880
590.966426	41872.697011	31.863898
591.300778	41941.212376	31.868916
591.759922	41989.873596	31.873933
592.404348	42060.440628	31.878951
592.925835	42115.385632	31.883968
593.324436	42156.751433	31.888986
594.457051	42213.669221	31.894004
594.970732	42264.485635	31.899021
595.558036	42318.782018	31.904039
596.109434	42374.469329	31.909056
596.454092	42435.704559	31.914074
597.541471	42488.234265	31.919092
597.238160	42553.322036	31.924109
597.875697	42614.948321	31.929127
597.883558	42691.499363	31.934144
598.377182	42757.114404	31.939162
598.825682	42833.970108	31.944180
599.181936	42911.099856	31.949197
600.145228	42989.399834	31.954215
600.695380	43067.790092	31.959232
601.350028	43152.331337	31.964250
601.879002	43235.298628	31.969268
602.286664	43316.121991	31.974285
603.169182	43407.851961	31.979303
603.637073	43482.878869	31.984320
604.170541	43565.460845	31.989338
604.988160	43644.437456	31.994356
605.210405	43729.807657	31.999373
606.238314	43805.190722	32.004391
606.332331	43894.516030	32.009408
607.540765	43979.460746	32.014426
607.893904	44063.717424	32.019444
608.225019	44153.373512	32.024461
608.799757	44232.459825	32.029479
609.520248	44321.935424	32.034496
610.339810	44404.374492	32.039514
610.832498	44492.545431	32.044532
611.208787	44581.620533	32.049549
612.207360	44664.209641	32.054567
612.916051	44748.109584	32.059584
613.391480	44830.876122	32.064602
614.666915	44917.616733	32.069620
615.047030	45001.202192	32.074637
615.534786	45084.663566	32.079655
616.077515	45182.292710	32.084672
616.489827	45259.466073	32.089690
617.702097	45343.744836	32.094708
618.063344	45418.269896	32.099725
618.973499	45505.557077	32.104743
619.660821	45589.735526	32.109760
620.358001	45670.091892	32.114778
620.854903	45734.000843	32.119796
621.747615	45820.128005	32.124813
622.294668	45888.533624	32.129831
622.696304	45969.481377	32.134848
623.819531	46043.819587	32.139866
624.382608	46119.700756	32.144884
624.672868	46193.214677	32.149901
625.626620	46262.949472	32.154919
626.844896	46326.747130	32.159936
627.388361	46389.473992	32.164954
628.061710	46466.015951	32.169972
628.826411	46538.520424	32.174989
629.696606	46599.324156	32.180007
629.886617	46668.490259	32.185024
630.669775	46735.020543	32.190042
631.130646	46800.184419	32.195060
631.371363	46870.159281	32.200077
631.887772	46938.066776	32.205095
632.315909	47020.171846	32.210112
632.878929	47093.215783	32.215130
633.822874	47151.295459	32.220148
633.888708	47221.868162	32.225165
634.662289	47293.842248	32.230183
635.592710	47372.548586	32.235200
635.548269	47442.911494	32.240218
636.422097	47517.129117	32.245236
636.495960	47603.859462	32.250253
637.182414	47678.739602	32.255271
637.938025	47766.926440	32.260288
638.148386	47856.831254	32.265306
638.761325	47937.879469	32.270324
639.347415	48039.126604	32.275341
639.806082	48121.629438	32.280359
640.334291	48220.532946	32.285376
640.735646	48321.025758	32.290394
641.831468	48414.748257	32.295412
642.384236	48524.246425	32.300429
642.882726	48610.445913	32.305447
643.946308	48694.368169	32.310464
645.161232	48787.877415	32.315482
645.844398	48875.415564	32.320500
646.284478	48964.630765	32.325517
647.175091	49052.200369	32.330535
647.554795	49135.465791	32.335552
648.292394	49230.127163	32.340570
649.429437	49305.068600	32.345588
649.883206	49396.991261	32.350605
650.506113	49486.103932	32.355623
651.127376	49563.904530	32.360640
652.053285	49645.789226	32.365658
652.898915	49730.603552	32.370676
653.263942	49830.362067	32.375693
654.131537	49905.189480	32.380711
654.842561	49998.934420	32.385728
655.277342	50070.014898	32.390746
656.603336	50149.004170	32.395764
656.930816	50231.092223	32.400781
657.578979	50317.420191	32.405799
658.447190	50397.930936	32.410816
658.678902	50474.827546	32.415834
659.699587	50560.965212	32.420852
660.118178	50647.697345	32.425869
661.082352	50726.169470	32.430887
661.408725	50804.045736	32.435904
662.083342	50894.199750	32.440922
662.619822	50978.415351	32.445940
663.332347	51063.211119	32.450957
664.131101	51140.078078	32.455975
665.116712	51225.976939	32.460992
665.731032	51311.750766	32.466010
666.035061	51400.825836	32.471028
666.854833	51480.354507	32.476045
667.194419	51566.191279	32.481063
667.815237	51656.166846	32.486080
667.961727	51746.742233	32.491098
668.744135	51834.003955	32.496116
669.466036	51935.322843	32.501133
670.103197	52039.021991	32.506151
670.840647	52134.169828	32.511168
670.886765	52232.185204	32.516186
671.903239	52323.018900	32.521204
672.565741	52428.462264	32.526221
672.912854	52520.749368	32.531239
673.835695	52621.881567	32.536256
673.943846	52732.013443	32.541274
674.984258	52831.280398	32.546292
675.808737	52933.694922	32.551309
676.500862	53017.298676	32.556327
677.704730	53122.616086	32.561344
678.140085	53201.255286	32.566362
678.657333	53287.089525	32.571380
679.803638	53376.533791	32.576397
680.014283	53465.555400	32.581415
680.813205	53553.833426	32.586432
681.470951	53645.658645	32.591450
682.558829	53733.423814	32.596468
682.892554	53827.179936	32.601485
683.543523	53921.835976	32.606503
684.380360	54006.059724	32.611520
684.782618	54097.224279	32.616538
685.818048	54188.967152	32.621556
687.061162	54274.773579	32.626573
687.388425	54365.147220	32.631591
688.476542	54448.637080	32.636608
688.834296	54548.492798	32.641626
689.779390	54629.341460	32.646644
690.278529	54723.537198	32.651661
691.138730	54818.664000	32.656679
691.824198	54901.522386	32.661696
692.634270	54980.064522	32.666714
693.314530	55059.171496	32.671732
694.048837	55141.466163	32.676749
695.055532	55237.077980	32.681767
695.843795	55317.592819	32.686784
696.237773	55411.624223	32.691802
696.816120	55502.538769	32.696820
697.694531	55577.635746	32.701837
698.085115	55668.580329	32.706855
698.752738	55753.241807	32.711872
699.247535	55861.327822	32.716890
699.711415	55958.641355	32.721908
700.467856	56055.150018	32.726925
701.004055	56163.363817	32.731943
701.816915	56260.902394	32.736960
702.161767	56350.527682	32.741978
702.997052	56456.075833	32.746996
703.752085	56563.162276	32.752013
704.123494	56673.581318	32.757031
704.716668	56771.415858	32.762048
705.702916	56885.271134	32.767066
706.588945	56986.465672	32.772084
706.933245	57089.675820	32.777101
707.677287	57203.741416	32.782119
708.327420	57311.423561	32.787136
708.753986	57427.989287	32.792154
709.703171	57539.106626	32.797172
710.080541	57653.098855	32.802189
710.837975	57764.899164	32.807207
711.494155	57874.260108	32.812224
712.204833	57997.087993	32.817242
713.138031	58112.716902	32.822260
713.770005	58221.956621	32.827277
714.425603	58347.972225	32.832295
715.377654	58450.839834	32.837312
716.036768	58578.001699	32.842330
717.074259	58676.723783	32.847348
717.892085	58797.564157	32.852365
718.683273	58895.205384	32.857383
719.678429	58993.979693	32.862400
720.446482	59102.239972	32.867418
721.124473	59223.053719	32.872436
721.825480	59319.755005	32.877453
722.608686	59432.964126	32.882471
723.327816	59526.947983	32.887488
723.842737	59625.439263	32.892506
724.474902	59721.051552	32.897524
725.254831	59829.667660	32.902541
725.953803	59929.612498	32.907559
727.162356	60012.469825	32.912576
727.896351	60110.276781	32.917594
728.313463	60207.177946	32.922612
728.967875	60307.745298	32.927629
729.491612	60405.826892	32.932647
730.342849	60494.767849	32.937664
730.925414	60597.670713	32.942682
731.730784	60707.027321	32.947700
732.477893	60806.575733	32.952717
732.867293	60924.974366	32.957735
733.576449	61032.543432	32.962752
734.175873	61146.441230	32.967770
735.166891	61249.795589	32.972788
736.067614	61356.703059	32.977805
736.524217	61470.922234	32.982823
737.596859	61579.937010	32.987840
738.177964	61686.668071	32.992858
738.915778	61792.400196	32.997876
739.581977	61891.820056	33.002893
740.205210	62015.295809	33.007911
741.192243	62130.555422	33.012928
742.037353	62244.324840	33.017946
742.359906	62349.921796	33.022964
743.267252	62461.707386	33.027981
743.894399	62578.240869	33.032999
745.082913	62694.110916	33.038016
745.879483	62806.155957	33.043034
746.479921	62913.383036	33.048052
747.423976	63021.841867	33.053069
747.947983	63144.420828	33.058087
748.982611	63249.239042	33.063104
749.819009	63365.034402	33.068122
750.905206	63469.877119	33.073140
751.636756	63578.358981	33.078157
751.948602	63692.516050	33.083175
752.567300	63796.787610	33.088192
753.357893	63913.979112	33.093210
753.998093	64028.117942	33.098228
755.158741	64134.528149	33.103245
755.779353	64259.920982	33.108263
756.356336	64357.826226	33.113280
757.278136	64468.782840	33.118298
758.121711	64584.057231	33.123316
759.467414	64692.169164	33.128333
759.863730	64808.040087	33.133351
760.975106	64912.929197	33.138368
762.241402	65020.447194	33.143386
762.801645	65114.913906	33.148404
763.584400	65212.201452	33.153421
764.441901	65318.163968	33.158439
765.382613	65412.439257	33.163456
766.166592	65505.150317	33.168474
766.799341	65604.628120	33.173492
767.984986	65691.724505	33.178509
768.332149	65803.220142	33.183527
768.916789	65895.349711	33.188544
769.747413	65996.235260	33.193562
770.014465	66104.205567	33.198580
771.091564	66202.989329	33.203597
771.889353	66310.681130	33.208615
772.508848	66416.938753	33.213632
773.549487	66530.215734	33.218650
774.156762	66637.286610	33.223668
774.828845	66726.923562	33.228685
775.427077	66835.326293	33.233703
775.860322	66935.011480	33.238720
776.561165	67023.878853	33.243738
776.828889	67140.844234	33.248756
777.863251	67237.498615	33.253773
778.607707	67356.498750	33.258791
779.267343	67457.739756	33.263808
779.935434	67570.877067	33.268826
780.482134	67681.798790	33.273844
781.434781	67798.792878	33.278861
782.204972	67926.098861	33.283879
782.958015	68036.559241	33.288896
784.112489	68151.820074	33.293914
784.491791	68267.880316	33.298932
785.422357	68378.789251	33.303949
786.304035	68501.945899	33.308967
787.025434	68620.708537	33.313984
787.513342	68736.639901	33.319002
788.382706	68866.391791	33.324020
789.417263	68968.808424	33.329037
790.146554	69098.893681	33.334055
790.591569	69224.547318	33.339072
791.487970	69360.863822	33.344090
792.239049	69481.778674	33.349108
793.466476	69604.284859	33.354125
793.967761	69725.740201	33.359143
794.859249	69845.266997	33.364160
795.692552	69974.137215	33.369178
796.724143	70095.036315	33.374196
797.579913	70213.379916	33.379213
798.432744	70349.645087	33.384231
799.048463	70470.522392	33.389248
799.921574	70594.614812	33.394266
800.585241	70712.028221	33.399284
801.712147	70839.666224	33.404301
802.092912	70967.928287	33.409319
803.028224	71098.333194	33.414336
804.006623	71224.248539	33.419354
804.854186	71344.460303	33.424372
806.162039	71448.148375	33.429389
807.367379	71572.028738	33.434407
808.791819	71665.263197	33.439424
809.908280	71769.185148	33.444442
810.811501	71874.863402	33.449460
811.844537	71968.540186	33.454477
812.225005	72083.686267	33.459495
813.122195	72201.449711	33.464512
813.307113	72289.408925	33.469530
814.210483	72395.253886	33.474548
814.945258	72493.513553	33.479565
815.618080	72614.657723	33.484583
816.458570	72733.648326	33.489600
817.364628	72833.718981	33.494618
817.744573	72953.377979	33.499636
818.641592	73065.090947	33.504653
819.362822	73178.009854	33.509671
820.196516	73300.740547	33.514688
820.844612	73419.359022	33.519706
821.636633	73541.616031	33.524724
822.403405	73661.926943	33.529741
822.500793	73785.243808	33.534759
823.684447	73911.443754	33.539776
824.649947	74029.419909	33.544794
824.957702	74173.541982	33.549812
826.261974	74287.260932	33.554829
827.048154	74419.098808	33.559847
827.402223	74548.851651	33.564864
828.363531	74674.393329	33.569882
829.021095	74806.810582	33.574900
829.929280	74937.580544	33.579917
830.592129	75056.862619	33.584935
831.298515	75189.679448	33.589952
832.578510	75306.041241	33.594970
832.851270	75437.635145	33.599988
833.617876	75561.387365	33.605005
834.382729	75691.233375	33.610023
835.374529	75820.360435	33.615040
836.438955	75953.872317	33.620058
836.984248	76096.776715	33.625076
837.923187	76231.475014	33.630093
838.859491	76361.563397	33.635111
839.601853	76499.891395	33.640128
840.649051	76619.322835	33.645146
841.265940	76759.660623	33.650164
842.383047	76894.942354	33.655181
843.456175	77028.762166	33.660199
843.993239	77153.773680	33.665216
845.072762	77288.581860	33.670234
845.606321	77434.370726	33.675252
846.451672	77571.877259	33.680269
847.286398	77708.714729	33.685287
848.012712	77846.101923	33.690304
849.181357	77984.598694	33.695322
849.968307	78119.406087	33.700340
850.335457	78264.376624	33.705357
851.407315	78412.873438	33.710375
852.113805	78558.983224	33.715392
853.003609	78705.685842	33.720410
853.677133	78851.954360	33.725428
854.659588	79001.279128	33.730445
855.818999	79151.881882	33.735463
856.691578	79295.233070	33.740480
857.219828	79446.987773	33.745498
858.008069	79589.606211	33.750516
859.220561	79739.443692	33.755533
860.464099	79882.676472	33.760551
861.508190	80027.917619	33.765568
862.497234	80167.593643	33.770586
863.291957	80321.807231	33.775604
864.055126	80453.563678	33.780621
864.918894	80597.847802	33.785639
865.585168	80736.779023	33.790656
866.567563	80866.577308	33.795674
867.707274	81028.355207	33.800692
868.214746	81166.692603	33.805709
869.194170	81311.063634	33.810727
869.853327	81462.111908	33.815744
870.734330	81592.626258	33.820762
871.664646	81755.682772	33.825780
872.747741	81893.578835	33.830797
873.107839	82051.899037	33.835815
874.367467	82198.409992	33.840832
875.175499	82343.319937	33.845850
876.078935	82495.678523	33.850868
876.955254	82641.643606	33.855885
878.418958	82787.745533	33.860903
879.231452	82926.778646	33.865920
879.970134	83071.094968	33.870938
880.839210	83217.824372	33.875956
881.802958	83359.712152	33.880973
882.798452	83506.930075	33.885991
883.498935	83641.663458	33.891008
884.322141	83778.671695	33.896026
885.478364	83921.419084	33.901044
886.145408	84073.164201	33.906061
887.708510	84199.959765	33.911079
889.212379	84323.534017	33.916096
890.273330	84437.548026	33.921114
890.946029	84557.376033	33.926132
891.496630	84683.141164	33.931149
892.629388	84793.774765	33.936167
893.233775	84915.629703	33.941184
893.831664	85034.140902	33.946202
894.822834	85155.733544	33.951220
895.515627	85289.170664	33.956237
896.186591	85418.100708	33.961255
896.761230	85551.304100	33.966272
898.121191	85685.006053	33.971290
898.619691	85817.386248	33.976308
899.680315	85968.724864	33.981325
899.982090	86101.884794	33.986343
900.611886	86250.390454	33.991360
901.659832	86387.540583	33.996378
902.540141	86548.148372	34.001396
902.996605	86697.101620	34.006413
903.988305	86855.159210	34.011431
904.501556	87013.558685	34.016448
905.366922	87177.416376	34.021466
906.201328	87340.405427	34.026484
906.985724	87513.528576	34.031501
907.991449	87680.573244	34.036519
908.929752	87847.413978	34.041536
910.036743	88008.944698	34.046554
910.724535	88195.089223	34.051572
911.316250	88361.771684	34.056589
912.561260	88524.728317	34.061607
913.854751	88691.391458	34.066624
915.174513	88860.586044	34.071642
916.354927	89024.607400	34.076660
917.077340	89188.878797	34.081677
917.949285	89339.275731	34.086695
918.910740	89507.237408	34.091712
920.353642	89658.205564	34.096730
921.380855	89815.120087	34.101748
922.081276	89967.067855	34.106765
923.316277	90117.931469	34.111783
924.200759	90288.482326	34.116800
925.176415	90436.713990	34.121818
926.227676	90592.906401	34.126836
926.793076	90754.257938	34.131853
928.232097	90905.372378	34.136871
929.031958	91057.234027	34.141888
930.117709	91203.424367	34.146906
931.165302	91360.990124	34.151924
931.967929	91511.218645	34.156941
932.994238	91666.203774	34.161959
933.471870	91820.743277	34.166976
934.652594	91978.367435	34.171994
935.607129	92132.821175	34.177012
936.137200	92284.452357	34.182029
937.528705	92447.724141	34.187047
937.968411	92604.580332	34.192064
938.807144	92760.525638	34.197082
940.042665	92926.498772	34.202100
940.972185	93097.489276	34.207117
941.862465	93258.346900	34.212135
942.412262	93409.283427	34.217152
943.792130	93570.116723	34.222170
944.641709	93717.332042	34.227188
945.948910	93876.403790	34.232205
946.829982	94038.090809	34.237223
947.818605	94186.452717	34.242240
948.826215	94349.769345	34.247258
949.556211	94508.186862	34.252276
950.971272	94669.730187	34.257293
951.632947	94815.522453	34.262311
952.506444	94958.861184	34.267328
953.500610	95104.374580	34.272346
954.043421	95259.035182	34.277364
955.145940	95411.149799	34.282381
955.815056	95566.616075	34.287399
956.949757	95736.562239	34.292416
957.682009	95883.223073	34.297434
958.545183	96039.954264	34.302452
959.200394	96199.165296	34.307469
959.822637	96368.383837	34.312487
961.049906	96528.356271	34.317504
961.847558	96695.267367	34.322522
962.716388	96875.579862	34.327540
963.076307	97050.167226	34.332557
964.728335	97210.406192	34.337575
965.832234	97390.443954	34.342592
966.922566	97570.091883	34.347610
968.265078	97738.038705	34.352628
969.261191	97902.212242	34.357645
970.179155	98079.849059	34.362663
970.883518	98244.539079	34.367680
971.819453	98424.976611	34.372698
973.151759	98594.045109	34.377716
973.986707	98771.242381	34.382733
975.259375	98940.005109	34.387751
976.235104	99104.580989	34.392768
976.715207	99294.450630	34.397786
977.717348	99470.332475	34.402804
978.754112	99649.696176	34.407821
979.639038	99820.362457	34.412839
980.672289	99998.600334	34.417856
981.697134	100171.287658	34.422874
983.327583	100338.023937	34.427892
984.212863	100519.647456	34.432909
985.695910	100689.920386	34.437927
986.599410	100861.806304	34.442944
987.243946	101037.422989	34.447962
988.156115	101205.328440	34.452980
989.109382	101383.561051	34.457997
990.410448	101552.548429	34.463015
991.454218	101731.389991	34.468032
992.477092	101895.237247	34.473050
993.805419	102057.947145	34.478068
994.767445	102226.040177	34.483085
995.788796	102392.539951	34.488103
996.845885	102560.302833	34.493120
997.598345	102739.613859	34.498138
998.547880	102899.597882	34.503156
999.600218	103081.196697	34.508173
1000.730665	103244.298409	34.513191
1002.260408	103410.533505	34.518208
1003.359159	103569.926832	34.523226
1004.010368	103736.630756	34.528244
1004.888710	103901.360036	34.533261
1005.699574	104067.647556	34.538279
1006.963855	104245.035366	34.543296
1007.817587	104406.943497	34.548314
1008.846848	104576.711523	34.553332
1009.364518	104757.490217	34.558349
1010.760179	104935.976891	34.563367
1011.434360	105105.853889	34.568384
1012.143803	105285.261339	34.573402
1012.930538	105468.030450	34.578420
1013.879695	105655.618806	34.583437
1014.491192	105836.845038	34.588455
1016.036830	106013.703554	34.593472
1016.797999	106195.136495	34.598490
1018.274242	106377.409450	34.603508
1019.244097	106552.928055	34.608525
1019.849763	106719.603065	34.613543
1020.831977	106899.255258	34.618560
1021.818146	107087.365564	34.623578
1023.000724	107250.643251	34.628596
1023.461561	107431.127992	34.633613
1024.606280	107615.919434	34.638631
1025.791936	107804.496957	34.643648
1026.889309	107975.983090	34.648666
1028.199150	108151.646812	34.653684
1028.904339	108337.981883	34.658701
1030.068695	108522.737038	34.663719
1031.589340	108704.229112	34.668736
1031.929357	108881.075509	34.673754
1033.489288	109063.653866	34.678772
1034.436766	109256.118904	34.683789
1035.564884	109434.658111	34.688807
1036.599510	109609.091449	34.693824
1037.583160	109804.571970	34.698842
1038.862670	109991.130268	34.703860
1039.687636	110176.454525	34.708877
1040.792090	110363.219736	34.713895
1041.962033	110548.149526	34.718912
1042.398384	110738.977977	34.723930
1043.937241	110935.481125	34.728948
1044.689172	111140.808286	34.733965
1045.522704	111318.096885	34.738983
1046.666752	111512.268148	34.744000
1047.489288	111721.468267	34.749018
1049.298677	111917.630095	34.754036
1050.062127	112107.285933	34.759053
1051.146983	112311.857480	34.764071
1052.133279	112500.922483	34.769088
1053.145861	112702.425762	34.774106
1054.314271	112897.475771	34.779124
1055.146009	113104.704016	34.784141
1056.226325	113301.203111	34.789159
1057.520655	113496.705882	34.794176
1058.646037	113697.372652	34.799194
1059.955628	113892.951254	34.804212
1061.033542	114096.037375	34.809229
1062.156654	114296.124376	34.814247
1063.357427	114492.433460	34.819264
1064.063888	114685.992661	34.824282
1065.389839	114880.787620	34.829300
1066.416330	115078.737873	34.834317
1067.579313	115268.461749	34.839335
1068.757310	115463.041959	34.844352
1070.214801	115649.677682	34.849370
1071.415392	115838.282448	34.854388
1072.764655	116026.598541	34.859405
1073.726261	116214.063058	34.864423
1075.438626	116396.438992	34.869440
1076.132059	116583.440001	34.874458
1076.896771	116751.874437	34.879476
1077.739172	116943.597647	34.884493
1079.013546	117134.556591	34.889511
1080.097036	117312.519969	34.894528
1080.853833	117507.151389	34.899546
1082.161799	117698.133296	34.904564
1082.970833	117887.329708	34.909581
1084.080920	118080.171036	34.914599
1085.339837	118271.138139	34.919616
1085.808569	118470.208356	34.924634
1087.114965	118663.110694	34.929652
1088.062813	118861.892309	34.934669
1089.135771	119060.173357	34.939687
1090.105327	119245.266954	34.944704
1090.685658	119437.297462	34.949722
1091.938546	119630.086195	34.954740
1093.005209	119818.186308	34.959757
1093.823748	120017.755228	34.964775
1094.363387	120211.546465	34.969792
1095.823375	120429.778071	34.974810
1096.906166	120636.907111	34.979828
1098.164893	120840.495932	34.984845
1098.445173	121033.355112	34.989863
1100.335150	121232.128263	34.994880
1101.353753	121444.117397	34.999898
1102.455843	121653.189653	35.004916
1103.259804	121858.757770	35.009933
1103.975045	122071.698446	35.014951
1105.520757	122293.453590	35.019968
1106.093765	122523.493766	35.024986
1107.451266	122741.513245	35.030004
1108.390210	122964.356621	35.035021
1109.204423	123192.536150	35.040039
1110.335849	123415.808606	35.045056
1111.651565	123649.861941	35.050074
1113.060406	123876.379212	35.055092
1114.236581	124101.919292	35.060109
1115.430408	124333.940536	35.065127
1116.735306	124553.107186	35.070144
1117.965735	124782.575329	35.075162
1119.229815	125003.323916	35.080180
1120.395544	125226.588342	35.085197
1121.550584	125457.467613	35.090215
1122.975133	125672.536490	35.095232
1124.174678	125897.118700	35.100250
1125.420652	126114.552211	35.105268
1126.895193	126330.466728	35.110285
1127.919427	126542.278877	35.115303
1129.341836	126753.979031	35.120320
1130.490962	126967.524612	35.125338
1131.609338	127175.836329	35.130356
1132.982768	127388.232494	35.135373
1133.787953	127605.857035	35.140391
1135.247963	127811.352629	35.145408
1136.138045	128029.740013	35.150426
1137.096499	128249.627634	35.155444
1138.069904	128457.283314	35.160461
1138.886782	128683.868994	35.165479
1140.467285	128897.813650	35.170496
1141.584199	129123.821837	35.175514
1142.685516	129339.264763	35.180532
1144.145938	129553.992795	35.185549
1144.974555	129779.554778	35.190567
1146.717273	129986.577308	35.195584
1147.800523	130205.059859	35.200602
1149.137755	130416.461875	35.205620
1150.172914	130625.641042	35.210637
1151.246231	130846.805609	35.215655
1152.683884	131054.667714	35.220672
1153.775199	131267.431981	35.225690
1155.078856	131475.012561	35.230708
1156.765717	131675.936147	35.235725
1157.793832	131891.974298	35.240743
1159.279268	132087.500630	35.245760
1160.514202	132283.587286	35.250778
1161.800046	132479.946001	35.255796
1162.701242	132679.829836	35.260813
1163.689733	132876.554091	35.265831
1164.869662	133081.065588	35.270848
1165.892911	133276.352340	35.275866
1166.698814	133482.091623	35.280884
1167.949441	133665.416860	35.285901
1169.147919	133877.682120	35.290919
1170.017127	134066.245863	35.295936
1171.110059	134262.211245	35.300954
1172.010895	134462.915268	35.305972
1172.822591	134667.034877	35.310989
1174.009199	134862.188786	35.316007
1175.409298	135063.692895	35.321024
1176.423221	135284.647883	35.326042
1177.423945	135501.431154	35.331060
1178.688327	135708.656983	35.336077
1179.729199	135928.735302	35.341095
1180.677644	136139.844828	35.346112
1182.059167	136358.793263	35.351130
1182.816809	136581.951919	35.356148
1184.100548	136807.402311	35.361165
1185.281688	137038.631112	35.366183
1186.640852	137255.417327	35.371200
1187.446487	137489.892363	35.376218
1188.366281	137722.637539	35.381236
1189.659887	137952.990359	35.386253
1190.467567	138198.483749	35.391271
1191.315245	138443.248813	35.396288
1193.075113	138694.420608	35.401306
1193.859743	138936.939215	35.406324
1195.299387	139183.734766	35.411341
1196.050729	139439.433950	35.416359
1197.643404	139681.322245	35.421376
1199.515003	139923.688426	35.426394
1200.172599	140182.972372	35.431412
1201.596674	140416.210265	35.436429
1202.984037	140673.783570	35.441447
1203.879938	140919.162979	35.446464
1205.005146	141173.784911	35.451482
1206.564670	141418.809144	35.456500
1207.850296	141670.565752	35.461517
1208.879252	141920.434766	35.466535
1210.057206	142167.426180	35.471552
1211.412831	142419.251829	35.476570
1212.365968	142681.218795	35.481588
1213.623598	142932.186691	35.486605
1214.827973	143201.795459	35.491623
1216.027970	143450.452435	35.496640
1217.249230	143708.727651	35.501658
1218.403805	143974.160119	35.506676
1219.686626	144239.891211	35.511693
1221.074842	144498.207812	35.516711
1222.703765	144751.208186	35.521728
1224.307180	145003.985359	35.526746
1225.167679	145263.099224	35.531764
1226.777890	145506.206434	35.536781
1227.923092	145768.540185	35.541799
1229.258991	146011.413504	35.546816
1230.696385	146265.885594	35.551834
1231.634043	146518.101760	35.556852
1232.817211	146766.612591	35.561869
1233.819063	147029.635194	35.566887
1234.901866	147275.968356	35.571904
1236.506054	147527.425054	35.576922
1237.592595	147788.293150	35.581940
1238.699697	148043.384096	35.586957
1240.094112	148305.551990	35.591975
1241.038115	148552.940972	35.596992
1242.589483	148809.324199	35.602010
1243.522397	149072.456623	35.607028
1245.890623	149306.273070	35.612045
1246.989540	149565.777089	35.617063
1248.277621	149813.663837	35.622080
1249.666570	150042.965673	35.627098
1250.497065	150281.342772	35.632116
1251.748258	150517.306783	35.637133
1252.979677	150758.364978	35.642151
1253.955820	150989.880607	35.647168
1254.983488	151226.948919	35.652186
1256.362864	151469.040633	35.657204
1257.910422	151706.169249	35.662221
1259.610832	151949.177526	35.667239
1260.787976	152183.408528	35.672256
1262.377416	152415.709981	35.677274
1263.675996	152659.203146	35.682292
1264.752059	152885.354215	35.687309
1266.158848	153130.089176	35.692327
1267.166567	153363.678836	35.697344
1268.366652	153605.998260	35.702362
1268.897951	153850.835291	35.707380
1270.380860	154095.092805	35.712397
1271.539010	154361.858321	35.717415
1272.581366	154609.411324	35.722432
1273.638462	154860.250918	35.727450
1275.209928	155130.458926	35.732468
1276.356917	155386.427959	35.737485
1277.533807	155648.118667	35.742503
1278.851357	155917.684558	35.747520
1280.009904	156183.772850	35.752538
1281.105162	156460.091483	35.757556
1282.077794	156725.246512	35.762573
1283.265512	157009.322418	35.767591
1284.617071	157287.674024	35.772608
1285.962947	157568.795307	35.777626
1287.480074	157834.987164	35.782644
1289.069280	158113.495806	35.787661
1290.183751	158395.901266	35.792679
1291.426375	158674.580980	35.797696
1293.262118	158943.673086	35.802714
1294.114037	159225.844170	35.807732
1295.968260	159502.857681	35.812749
1297.235095	159778.885265	35.817767
1298.707773	160044.090715	35.822784
1300.289485	160320.122183	35.827802
1301.550649	160591.609245	35.832820
1302.722865	160862.997138	35.837837
1304.223897	161137.534029	35.842855
1305.125919	161407.976280	35.847872
1306.308602	161684.342757	35.852890
1307.790105	161954.468081	35.857908
1309.793858	162223.230502	35.862925
1311.190552	162497.078567	35.867943
1312.357497	162773.109371	35.872960
1314.084298	163032.066396	35.877978
1314.839456	163314.435784	35.882996
1316.423664	163577.149928	35.888013
1317.437623	163854.466133	35.893031
1318.528754	164122.718986	35.898048
1320.116666	164401.369604	35.903066
1321.109682	164678.375098	35.908084
1322.508923	164953.350199	35.913101
1323.644893	165223.809597	35.918119
1325.349519	165515.269963	35.923136
1326.759021	165796.950625	35.928154
1327.384056	166080.177257	35.933172
1328.993571	166358.464304	35.938189
1330.629691	166634.005812	35.943207
1331.861079	166915.490367	35.948224
1333.166147	167187.581570	35.953242
1334.284036	167471.498515	35.958260
1335.732472	167746.591288	35.963277
1337.155913	168011.341010	35.968295
1338.226026	168262.396157	35.973312
1340.029082	168527.570856	35.978330
1341.347822	168791.412963	35.983348
1342.541711	169052.774236	35.988365
1344.122235	169306.546492	35.993383
1345.515212	169572.868466	35.998400
1347.135505	169827.347349	36.003418
1347.916970	170097.080930	36.008436
1348.925120	170362.259745	36.013453
1350.524050	170625.899524	36.018471
1351.553569	170910.884921	36.023488
1352.990834	171171.961641	36.028506
1354.214215	171452.969816	36.033524
1355.779180	171725.138820	36.038541
1357.344464	172004.457522	36.043559
1358.641304	172283.476422	36.048576
1360.293561	172553.603070	36.053594
1361.200271	172822.615672	36.058612
1362.487209	173112.444920	36.063629
1364.207859	173389.865015	36.068647
1365.258520	173671.111448	36.073664
1366.538954	173962.798738	36.078682
1367.862254	174251.128110	36.083700
1368.833761	174540.250072	36.088717
1370.210266	174833.017524	36.093735
1371.464644	175130.325692	36.098752
1372.999819	175425.737055	36.103770
1374.301376	175726.176459	36.108788
1375.291200	176026.602259	36.113805
1376.898393	176318.615101	36.118823
1378.655000	176624.878558	36.123840
1380.305579	176908.226369	36.128858
1382.046912	177211.903871	36.133876
1383.243867	177518.156574	36.138893
1384.941388	177808.611205	36.143911
1386.125160	178113.674430	36.148928
1387.550522	178409.913450	36.153946
1388.847782	178713.995919	36.158964
1390.015882	179011.216944	36.163981
1391.888400	179314.474917	36.168999
1392.833120	179621.231634	36.174016
1394.424862	179922.478411	36.179034
1396.055176	180228.113978	36.184052
1397.068392	180531.180386	36.189069
1398.670332	180833.241321	36.194087
1399.983334	181146.117251	36.199104
1401.333570	181448.371984	36.204122
1402.808632	181757.592670	36.209140
1404.490832	182057.079796	36.214157
1405.751989	182359.452993	36.219175
1406.985022	182680.143852	36.224192
1408.358420	182967.668694	36.229210
1409.857385	183282.249678	36.234228
1410.868032	183603.562573	36.239245
1412.574646	183913.465120	36.244263
1413.623709	184233.021537	36.249280
1415.295376	184542.144151	36.254298
1416.536865	184856.414855	36.259316
1417.875713	185173.515996	36.264333
1419.556206	185490.082063	36.269351
1420.879068	185805.993902	36.274368
1422.002877	186127.551115	36.279386
1424.024968	186435.126030	36.284404
1425.535572	186751.290733	36.289421
1427.212307	187044.469161	36.294439
1428.700879	187445.727965	36.299456
1429.684978	187751.792762	36.304474
1431.360283	188061.712600	36.309492
1432.634806	188358.462705	36.314509
1434.336172	188647.374412	36.319527
1435.534882	188950.005347	36.324544
1436.646992	189240.814212	36.329562
1437.543431	189545.881658	36.334580
1439.076442	189863.194783	36.339597
1440.525137	190171.885880	36.344615
1441.628538	190485.788110	36.349632
1443.065013	190790.063088	36.354650
1444.804288	191103.435625	36.359668
1446.187654	191428.574341	36.364685
1448.217829	191744.265266	36.369703
1449.594343	192049.086224	36.374720
1450.833818	192364.013479	36.379738
1452.922094	192679.646905	36.384756
1454.155100	192987.718526	36.389773
1455.779729	193298.523701	36.394791
1457.289184	193614.961277	36.399808
1458.385870	193919.652742	36.404826
1459.977538	194249.871768	36.409844
1461.598003	194569.977443	36.414861
1463.236733	194884.213341	36.419879
1464.532525	195210.086639	36.424896
1465.764377	195527.969296	36.429914
1467.186764	195851.766796	36.434932
1468.211183	196185.076687	36.439949
1470.024285	196510.059228	36.444967
1470.794751	196848.287520	36.449984
1472.112687	197184.779811	36.455002
1473.914624	197536.057126	36.460020
1474.930652	197881.920696	36.465037
1476.294301	198225.419091	36.470055
1477.765845	198581.373705	36.475072
1479.072241	198934.586179	36.480090
1480.777921	199281.361058	36.485108
1482.000831	199651.455147	36.490125
1483.626855	200002.714831	36.495143
1484.801793	200366.975584	36.500160
1486.545050	200726.296366	36.505178
1488.347272	201084.643406	36.510196
1489.929984	201451.027297	36.515213
1491.670590	201808.420210	36.520231
1493.125931	202164.689990	36.525248
1494.235471	202538.212096	36.530266
1495.812749	202890.120408	36.535284
1497.414018	203263.109795	36.540301
1499.078322	203618.790860	36.545319
1500.181481	203989.192371	36.550336
1501.862888	204360.342380	36.555354
1503.442948	204721.932102	36.560372
1505.210573	205101.935581	36.565389
1506.609767	205458.118725	36.570407
1507.894704	205820.620288	36.575424
1509.667492	206194.706082	36.580442
1511.019390	206559.687913	36.585460
1512.976812	206924.880417	36.590477
1514.707225	207291.480813	36.595495
1516.151741	207657.720094	36.600512
1517.952583	208014.708232	36.605530
1519.602246	208373.320969	36.610548
1521.160532	208739.950559	36.615565
1523.177123	209084.560524	36.620583
1524.398210	209452.031430	36.625600
1525.583584	209797.305914	36.630618
1527.482924	210148.667531	36.635636
1529.083150	210500.178030	36.640653
1530.983483	210844.452826	36.645671
1532.688407	211177.377864	36.650688
1533.821736	211507.318916	36.655706
1535.072959	211842.729044	36.660724
1536.380416	212169.264895	36.665741
1538.054650	212499.808256	36.670759
1539.442869	212846.553419	36.675776
1540.695833	213188.493421	36.680794
1542.677385	213526.382169	36.685812
1543.792776	213872.917039	36.690829
1545.459053	214222.109625	36.695847
1547.013634	214565.121507	36.700864
1548.114175	214913.361718	36.705882
1549.631950	215266.592286	36.710900
1551.237066	215624.712422	36.715917
1552.698389	215977.393540	36.720935
1554.955087	216333.684822	36.725952
1556.128779	216688.520029	36.730970
1557.944964	217048.462739	36.735988
1559.207849	217404.935755	36.741005
1560.701004	217758.832583	36.746023
1562.149075	218121.780494	36.751040
1563.739618	218483.385330	36.756058
1565.535189	218845.440967	36.761076
1566.721495	219217.067844	36.766093
1568.604584	219586.299513	36.771111
1570.287422	219958.103109	36.776128
1571.523505	220335.997552	36.781146
1572.964457	220700.853240	36.786164
1574.842848	221088.682073	36.791181
1576.338245	221456.501801	36.796199
1577.990216	221836.668922	36.801216
1579.580131	222208.462532	36.806234
1581.483926	222591.816778	36.811252
1582.964194	222970.588456	36.816269
1584.522511	223351.710574	36.821287
1586.347461	223731.419209	36.826304
1587.638020	224119.315430	36.831322
1589.575797	224491.867948	36.836340
1590.912538	224878.105739	36.841357
1592.303230	225265.249644	36.846375
1593.836061	225645.715430	36.851392
1595.320093	226040.923206	36.856410
1597.102303	226422.162846	36.861428
1598.719353	226808.686934	36.866445
1600.186996	227209.562242	36.871463
1602.004495	227591.558303	36.876480
1603.495889	227986.434364	36.881498
1605.627978	228376.967571	36.886516
1607.067582	228766.262619	36.891533
1609.191106	229155.882368	36.896551
1610.609992	229533.570736	36.901568
1611.891180	229931.527504	36.906586
1613.723523	230307.397962	36.911604
1615.404063	230705.418878	36.916621
1616.808156	231092.940192	36.921639
1618.839196	231483.843515	36.926656
1619.910703	231876.446408	36.931674
1621.600895	232263.058513	36.936692
1623.477067	232660.285493	36.941709
1625.054976	233047.879977	36.946727
1626.635313	233442.307434	36.951744
1628.314892	233833.441948	36.956762
1629.920623	234226.797828	36.961780
1631.426278	234619.991200	36.966797
1632.784761	235012.648363	36.971815
1634.372145	235411.264620	36.976832
1636.227553	235811.007106	36.981850
1638.317237	236185.257995	36.986868
1639.420516	236565.962990	36.991885
1641.329123	236941.460818	36.996903
1643.580301	237311.519059	37.001920
1644.602468	237691.295580	37.006938
1646.683452	238063.284886	37.011956
1648.517823	238426.776760	37.016973
1650.492376	238790.627320	37.021991
1651.860329	239153.861072	37.027008
1653.228509	239530.913811	37.032026
1655.072884	239900.880187	37.037044
1656.385659	240288.178155	37.042061
1657.722770	240660.941049	37.047079
1659.653836	241035.109260	37.052096
1660.797987	241432.821887	37.057114
1662.333915	241817.847171	37.062132
1663.741283	242219.480249	37.067149
1665.176012	242619.965230	37.072167
1666.922821	243025.100261	37.077184
1668.394188	243436.577635	37.082202
1669.831538	243835.358075	37.087220
1671.305219	244262.126160	37.092237
1672.359253	244670.948406	37.097255
1674.469695	245088.774965	37.102272
1675.996100	245530.240465	37.107290
1677.973227	245951.337668	37.112308
1679.820126	246383.733142	37.117325
1681.738682	246798.537810	37.122343
1683.718201	247224.483758	37.127360
1685.105789	247656.973598	37.132378
1686.568152	248083.328715	37.137396
1688.313260	248511.315123	37.142413
1690.211539	248952.180898	37.147431
1692.092802	249377.019376	37.152448
1693.313770	249834.932168	37.157466
1695.444208	250263.819151	37.162484
1697.044591	250704.574510	37.167501
1698.544661	251150.323142	37.172519
1700.406188	251582.855753	37.177536
1702.221986	252025.682058	37.182554
1703.975104	252463.893760	37.187572
1705.669250	252907.346157	37.192589
1707.355042	253351.560574	37.197607
1709.332089	253796.007469	37.202624
1710.656696	254244.314495	37.207642
1712.707375	254685.851307	37.212660
1714.372850	255137.582108	37.217677
1715.734298	255589.181181	37.222695
1717.932343	256024.238689	37.227712
1719.378397	256484.229262	37.232730
1721.502147	256927.144327	37.237748
1723.230370	257381.854961	37.242765
1724.734149	257838.377140	37.247783
1726.527843	258274.531742	37.252800
1728.228600	258737.623968	37.257818
1729.596539	259189.006088	37.262836
1731.313975	259648.612347	37.267853
1732.771425	260096.420970	37.272871
1735.232210	260549.049308	37.277888
1737.131642	261015.886169	37.282906
1738.857418	261470.200696	37.287924
1740.431049	261917.780826	37.292941
1741.868549	262380.163132	37.297959
1743.820642	262832.988885	37.302976
1745.870268	263287.804049	37.307994
1747.676063	263745.576377	37.313012
1749.667531	264194.529495	37.318029
1751.369412	264647.208893	37.323047
1753.639134	265069.013699	37.328064
1755.469025	265496.041597	37.333082
1757.389049	265904.004395	37.338100
1759.464925	266326.951848	37.343117
1761.385696	266740.854429	37.348135
1763.530837	267131.658217	37.353152
1764.911405	267546.708660	37.358170
1766.736164	267948.379048	37.363188
1768.576593	268362.820633	37.368205
1770.172712	268780.244819	37.373223
1771.878517	269187.033591	37.378240
1773.295463	269612.431681	37.383258
1775.130658	270035.324162	37.388276
1776.830611	270456.940557	37.393293
1778.037234	270876.143214	37.398311
1779.553746	271300.857459	37.403328
1781.293959	271739.274626	37.408346
1783.056206	272180.327464	37.413364
1784.773138	272631.239222	37.418381
1786.344113	273069.879331	37.423399
1788.449090	273508.357432	37.428416
1789.862482	273969.671511	37.433434
1791.659964	274420.815120	37.438452
1793.232631	274876.080274	37.443469
1795.158783	275337.458884	37.448487
1797.037618	275792.391667	37.453504
1798.621761	276260.243757	37.458522
1800.230794	276718.540383	37.463540
1802.121763	277193.399013	37.468557
1804.164542	277654.238082	37.473575
1806.667933	278115.738809	37.478592
1808.437878	278584.284437	37.483610
1809.911511	279043.020274	37.488628
1812.063672	279515.208041	37.493645
1813.465481	279983.243935	37.498663
1816.049091	280442.330829	37.503680
1818.199532	280922.864758	37.508698
1819.691941	281390.471246	37.513716
1821.297927	281850.514902	37.518733
1822.712561	282337.147617	37.523751
1824.750224	282795.746390	37.528768
1826.745142	283270.727751	37.533786
1828.201463	283752.747977	37.538804
1830.134936	284219.301898	37.543821
1832.136619	284708.543403	37.548839
1834.220656	285185.275229	37.553856
1835.803803	285674.854622	37.558874
1837.547862	286157.320770	37.563892
1839.422194	286631.282013	37.568909
1841.091648	287114.336933	37.573927
1843.269200	287601.371522	37.578944
1845.079666	288086.911022	37.583962
1847.082578	288567.998639	37.588980
1849.177497	289049.703048	37.593997
1850.766039	289535.266350	37.599015
1852.563955	290020.133005	37.604032
1854.488925	290496.038476	37.609050
1856.452186	290978.840579	37.614068
1858.737938	291459.531837	37.619085
1860.693200	291939.407785	37.624103
1862.608936	292415.376086	37.629120
1864.415316	292896.105662	37.634138
1865.947493	293376.239567	37.639156
1868.070425	293860.314100	37.644173
1869.538542	294347.153014	37.649191
1871.834996	294823.651921	37.654208
1873.729446	295302.240957	37.659226
1875.212862	295782.362908	37.664244
1877.538737	296245.567332	37.669261
1879.198482	296718.113543	37.674279
1881.094355	297179.752841	37.679296
1882.740404	297636.527631	37.684314
1884.274592	298104.334415	37.689332
1886.280100	298561.705506	37.694349
1887.497147	299042.120778	37.699367
1889.157270	299513.678676	37.704384
1890.979034	299989.294486	37.709402
1892.978371	300472.570459	37.714420
1894.899521	300960.500034	37.719437
1896.263160	301455.290479	37.724455
1898.243753	301948.507439	37.729472
1899.854468	302442.564645	37.734490
1901.407353	302957.188353	37.739508
1903.296458	303457.081856	37.744525
1905.362518	303981.033033	37.749543
1906.845499	304485.524056	37.754560
1909.145657	305014.860391	37.759578
1910.747806	305543.995848	37.764596
1912.730117	306061.795924	37.769613
1914.536317	306594.137587	37.774631
1916.328721	307132.923084	37.779648
1918.152684	307663.118381	37.784666
1919.924659	308216.896606	37.789684
1922.096678	308752.482988	37.794701
1924.187468	309307.011231	37.799719
1925.961575	309845.845971	37.804736
1928.071600	310398.759620	37.809754
1929.710307	310948.999454	37.814772
1931.644769	311504.135921	37.819789
1933.746066	312071.625497	37.824807
1935.651680	312637.844430	37.829824
1937.606333	313192.094837	37.834842
1939.721017	313755.881714	37.839860
1941.825436	314315.602591	37.844877
1943.473549	314881.478988	37.849895
1945.143434	315445.796829	37.854912
1947.288498	316012.165059	37.859930
1949.143363	316593.265466	37.864948
1951.500692	317162.961198	37.869965
1953.442860	317743.423842	37.874983
1955.597720	318314.633666	37.880000
1957.805868	318885.726189	37.885018
1959.286916	319464.258768	37.890036
1961.236928	320035.706427	37.895053
1963.129719	320619.995571	37.900071
1965.413148	321189.091856	37.905088
1967.523521	321773.458002	37.910106
1969.465646	322355.254157	37.915124
1971.563006	322934.607388	37.920141
1973.466205	323509.567866	37.925159
1975.342170	324097.947291	37.930176
1977.597852	324679.611099	37.935194
1979.629136	325263.280842	37.940212
1982.105948	325833.653399	37.945229
1983.708730	326415.318442	37.950247
1985.859959	326995.443073	37.955264
1987.630485	327570.037133	37.960282
1989.509566	328155.540857	37.965300
1991.365487	328731.601628	37.970317
1993.447447	329330.198210	37.975335
1995.146344	329913.674328	37.980352
1997.433366	330497.658545	37.985370
1999.625391	331097.783613	37.990388
2001.529385	331680.896548	37.995405
2003.458995	332271.226581	38.000423
2005.044852	332862.945738	38.005440
2006.732500	333431.961057	38.010458
2008.931797	334015.194843	38.015476
2011.245990	334588.483124	38.020493
2013.173300	335158.982060	38.025511
2014.565364	335725.294449	38.030528
2017.247125	336306.920143	38.035546
2018.177105	336878.487015	38.040564
2020.204557	337462.175183	38.045581
2022.503664	338051.670642	38.050599
2024.417188	338637.462914	38.055616
2026.582082	339221.608386	38.060634
2028.115348	339821.187858	38.065652
2030.212098	340420.998764	38.070669
2031.970934	341024.276268	38.075687
2034.032118	341629.981578	38.080704
2036.122459	342238.867372	38.085722
2038.009301	342861.900420	38.090740
2040.028335	343482.390870	38.095757
2041.936922	344104.434373	38.100775
2043.894628	344739.062615	38.105792
2046.173063	345363.637343	38.110810
2048.026111	345989.585753	38.115828
2050.330211	346626.989943	38.120845
2052.536293	347267.922063	38.125863
2054.198683	347884.127548	38.130880
2056.937215	348520.083630	38.135898
2059.188117	349152.046737	38.140916
2060.980255	349793.653928	38.145933
2063.509804	350428.439350	38.150951
2065.795430	351074.660173	38.155968
2068.091894	351704.893186	38.160986
2070.286552	352351.837904	38.166004
2072.509449	352971.358245	38.171021
2074.554321	353607.677910	38.176039
2076.444868	354238.051154	38.181056
2078.631044	354866.261342	38.186074
2080.833927	355503.963043	38.191092
2082.867198	356137.292573	38.196109
2085.381313	356770.280455	38.201127
2087.338727	357422.557512	38.206144
2089.564403	358043.041644	38.211162
2091.718117	358685.881939	38.216180
2093.673917	359318.600393	38.221197
2095.572748	359962.290042	38.226215
2097.328990	360608.117411	38.231232
2099.679502	361248.870006	38.236250
2101.953468	361899.936618	38.241268
2103.861787	362545.622269	38.246285
2105.990045	363188.674251	38.251303
2108.035636	363856.866611	38.256320
2110.134151	364503.239907	38.261338
2112.193867	365166.660856	38.266356
2114.590636	365803.632344	38.271373
2117.144092	366451.969162	38.276391
2118.948909	367099.825632	38.281408
2121.512374	367746.459099	38.286426
2123.282508	368395.381264	38.291444
2125.502373	369043.610076	38.296461
2127.824278	369693.024317	38.301479
2129.491738	370345.693249	38.306496
2131.849390	370992.994037	38.311514
2134.222754	371653.097999	38.316532
2135.929826	372313.265146	38.321549
2138.234711	372957.183889	38.326567
2140.067015	373618.085588	38.331584
2142.535013	374264.937684	38.336602
2144.540348	374920.181776	38.341620
2146.923698	375580.594965	38.346637
2148.856871	376222.670628	38.351655
2150.907474	376861.140705	38.356672
2153.108797	377484.854162	38.361690
2155.381382	378120.244919	38.366708
2157.325744	378753.999988	38.371725
2159.109073	379381.660511	38.376743
2161.366165	380013.563286	38.381760
2164.110612	380649.401866	38.386778
2165.872093	381281.072935	38.391796
2167.808114	381933.495301	38.396813
2170.463501	382563.197047	38.401831
2172.394617	383203.887038	38.406848
2174.432429	383841.682547	38.411866
2176.798178	384500.050766	38.416884
2179.167179	385136.394547	38.421901
2181.745954	385780.236025	38.426919
2183.708472	386419.016901	38.431936
2186.181962	387053.574054	38.436954
2188.443407	387708.684314	38.441972
2190.431285	388367.061279	38.446989
2192.813272	389001.203395	38.452007
2194.853869	389651.258216	38.457024
2197.282669	390308.830918	38.462042
2199.479411	390957.662112	38.467060
2201.372252	391618.423008	38.472077
2203.933976	392271.061130	38.477095
2206.020329	392934.692762	38.482112
2208.450264	393595.518318	38.487130
2210.161630	394263.425092	38.492148
2212.096111	394936.442479	38.497165
2214.653246	395594.256571	38.502183
2216.672232	396272.488236	38.507200
2218.836866	396956.600745	38.512218
2221.191346	397641.372435	38.517236
2222.927444	398316.400349	38.522253
2225.276003	399005.334708	38.527271
2227.201494	399703.628673	38.532288
2229.800118	400395.013668	38.537306
2231.894047	401086.608781	38.542324
2233.988163	401784.813508	38.547341
2236.167033	402493.764138	38.552359
2238.283590	403203.512283	38.557376
2240.325369	403913.857291	38.562394
2242.653027	404629.499705	38.567412
2244.962499	405342.591970	38.572429
2247.309892	406057.882264	38.577447
2249.478385	406781.881343	38.582464
2251.378010	407492.641498	38.587482
2253.808371	408218.931096	38.592500
2256.143889	408949.563077	38.597517
2258.547486	409676.669043	38.602535
2260.754886	410402.870899	38.607552
2262.920197	411121.466296	38.612570
2265.192654	411856.311508	38.617588
2268.817738	412549.538150	38.622605
2272.006494	413258.594145	38.627623
2274.290038	413958.511114	38.632640
2276.897529	414658.759219	38.637658
2279.660884	415353.244118	38.642676
2281.483449	416045.526770	38.647693
2284.350670	416740.405261	38.652711
2286.393905	417435.136878	38.657728
2288.277361	418130.578609	38.662746
2290.746333	418827.524050	38.667764
2292.751969	419524.822139	38.672781
2294.925095	420217.367549	38.677799
2296.974381	420910.667730	38.682816
2298.493337	421616.062690	38.687834
2300.752853	422311.912373	38.692852
2302.832941	423011.356560	38.697869
2305.089750	423691.939918	38.702887
2307.040638	424370.829306	38.707904
2309.476593	425052.906438	38.712922
2312.220448	425747.602286	38.717940
2313.977959	426437.271787	38.722957
2316.148631	427135.295460	38.727975
2318.089650	427834.190081	38.732992
2320.266149	428540.605906	38.738010
2322.986810	429252.572911	38.743028
2325.738484	429959.808604	38.748045
2327.790044	430660.608151	38.753063
2330.152667	431374.677413	38.758080
2332.391957	432081.512531	38.763098
2334.526927	432797.688142	38.768116
2336.558326	433537.302953	38.773133
2339.268397	434258.843257	38.778151
2341.466384	434988.724203	38.783168
2343.230193	435727.993733	38.788186
2346.014089	436463.335984	38.793204
2347.956111	437209.493491	38.798221
2350.367171	437953.830496	38.803239
2352.934723	438711.199457	38.808256
2355.257252	439471.506637	38.813274
2357.458173	440226.295480	38.818292
2359.882001	440991.324678	38.823309
2361.944460	441742.285231	38.828327
2364.120949	442526.182987	38.833344
2366.272891	443296.817485	38.838362
2369.079388	444076.156585	38.843380
2371.632238	444865.250239	38.848397
2373.832424	445635.829813	38.853415
2376.282708	446429.064037	38.858432
2378.394750	447219.135089	38.863450
2380.941555	448011.073176	38.868468
2383.333719	448808.050376	38.873485
2385.685276	449608.280772	38.878503
2388.332193	450410.045022	38.883520
2391.405974	451192.268142	38.888538
2393.593309	451978.685034	38.893556
2396.028483	452778.457317	38.898573
2398.826578	453571.271040	38.903591
2401.386035	454363.682585	38.908608
2403.423101	455160.430728	38.913626
2406.128983	455955.826573	38.918644
2408.257121	456761.320725	38.923661
2411.052132	457551.178601	38.928679
2413.410559	458354.947657	38.933696
2415.576915	459147.505765	38.938714
2418.496358	459943.694359	38.943732
2420.885274	460746.539426	38.948749
2423.325030	461549.237873	38.953767
2425.613253	462343.748117	38.958784
2427.845634	463151.146256	38.963802
2430.602621	463948.333316	38.968820
2432.488615	464754.851185	38.973837
2435.168375	465556.615426	38.978855
2437.632065	466360.443263	38.983872
2439.743857	467174.325429	38.988890
2442.435692	467986.866424	38.993908
2444.731851	468805.078415	38.998925
2447.273612	469615.242661	39.003943
2450.341981	470419.989178	39.008960
2452.338178	471235.555029	39.013978
2454.777299	472040.471496	39.018996
2457.020702	472850.925508	39.024013
2459.470111	473664.029605	39.029031
2461.976062	474468.210019	39.034048
2463.883362	475270.175122	39.039066
2466.521308	476049.904102	39.044084
2468.791917	476851.380345	39.049101
2471.100015	477641.266550	39.054119
2473.648787	478442.568768	39.059136
2475.990505	479238.217486	39.064154
2478.565489	480038.426648	39.069172
2480.779080	480830.234877	39.074189
2483.154706	481656.298329	39.079207
2485.475702	482452.896253	39.084224
2488.111230	483279.790642	39.089242
2490.786861	484082.951768	39.094260
2493.234422	484916.389293	39.099277
2495.331010	485743.941786	39.104295
2497.822635	486558.792668	39.109312
2500.292013	487396.525951	39.114330
2502.737367	488239.002758	39.119348
2505.212632	489092.006594	39.124365
2507.427948	489934.022477	39.129383
2510.139706	490780.950581	39.134400
2512.847929	491638.508919	39.139418
2515.863618	492481.617189	39.144436
2517.821349	493347.152365	39.149453
2520.189623	494195.955756	39.154471
2522.666724	495066.647559	39.159488
2525.319694	495946.625808	39.164506
2528.375795	496814.355014	39.169524
2530.884316	497689.267571	39.174541
2533.151848	498557.722045	39.179559
2535.832143	499429.382721	39.184576
2538.212957	500314.376876	39.189594
2540.779655	501189.523706	39.194612
2542.734744	502083.536272	39.199629
2545.783011	502984.066137	39.204647
2548.297090	503864.896788	39.209664
2550.491707	504766.001999	39.214682
2553.485583	505670.598477	39.219700
2555.892305	506576.336219	39.224717
2558.514718	507475.995590	39.229735
2560.985440	508377.985889	39.234752
2563.463727	509289.223421	39.239770
2566.512532	510203.330645	39.244788
2569.460873	511104.115589	39.249805
2572.746575	512005.493752	39.254823
2575.785279	512889.803749	39.259840
2578.372187	513791.678200	39.264858
2581.069163	514675.726435	39.269876
2583.911994	515564.119833	39.274893
2586.556242	516440.973324	39.279911
2589.185657	517341.502345	39.284928
2591.695333	518232.489511	39.289946
2594.290468	519115.814579	39.294964
2596.524481	520011.453317	39.299981
2599.011278	520898.951459	39.304999
2601.636908	521783.152960	39.310016
2603.641472	522687.394571	39.315034
2606.508687	523585.962884	39.320052
2608.896602	524487.510265	39.325069
2610.832951	525388.614999	39.330087
2613.502267	526302.154273	39.335104
2616.262280	527237.519576	39.340122
2618.306742	528156.102209	39.345140
2621.003625	529081.601007	39.350157
2623.668869	530015.778727	39.355175
2626.053787	530931.652347	39.360192
2628.633128	531871.988291	39.365210
2631.368367	532791.442439	39.370228
2634.260233	533718.087441	39.375245
2636.841819	534630.756401	39.380263
2639.775023	535528.746119	39.385280
2642.206394	536432.072703	39.390298
2644.555168	537323.551811	39.395316
2647.402101	538220.713129	39.400333
2649.189184	539125.254438	39.405351
2652.201782	540042.889213	39.410368
2654.412182	540963.091856	39.415386
2657.304963	541869.622092	39.420404
2660.325936	542804.667114	39.425421
2662.566874	543728.274702	39.430439
2665.273982	544647.827777	39.435456
2667.596893	545588.241456	39.440474
2670.303422	546516.936528	39.445492
2673.036026	547469.984239	39.450509
2675.334067	548425.634078	39.455527
2678.451459	549374.311175	39.460544
2680.836686	550338.975444	39.465562
2683.513377	551292.185829	39.470580
2685.866783	552257.254617	39.475597
2688.212433	553237.037142	39.480615
2691.166338	554219.652830	39.485632
2693.994075	555205.466188	39.490650
2696.691566	556193.073416	39.495668
2699.594485	557176.357153	39.500685
2702.366211	558172.008319	39.505703
2705.800037	559150.636027	39.510720
2708.426106	560145.994032	39.515738
2711.000679	561122.839306	39.520756
2714.317756	562125.136654	39.525773
2717.373241	563102.694032	39.530791
2720.720122	564080.374607	39.535808
2723.332048	565059.340258	39.540826
2725.906097	566043.788231	39.545844
2728.881028	567029.141505	39.550861
2731.296479	568022.609724	39.555879
2734.408605	568991.751330	39.560896
2736.897835	569975.076189	39.565914
2739.986829	570962.027234	39.570932
2742.646621	571949.260404	39.575949
2745.505320	572941.832211	39.580967
2748.406902	573926.053104	39.585984
2750.645990	574917.547845	39.591002
2753.471739	575899.857215	39.596020
2756.606782	576904.796809	39.601037
2758.750933	577893.542456	39.606055
2761.735840	578894.024609	39.611072
2764.046782	579898.573804	39.616090
2767.018776	580904.229161	39.621108
2769.878690	581926.513759	39.626125
2772.447090	582929.847627	39.631143
2775.121798	583945.673405	39.636160
2778.096919	584969.807377	39.641178
2780.068554	585984.454225	39.646196
2783.305933	587007.306381	39.651213
2785.820045	588035.373468	39.656231
2788.370458	589051.742881	39.661248
2791.448886	590091.320908	39.666266
2794.279838	591123.742058	39.671284
2796.836402	592156.756412	39.676301
2799.533202	593205.685463	39.681319
2802.885117	594242.670260	39.686336
2805.342078	595277.046771	39.691354
2807.564003	596317.552113	39.696372
2810.579885	597373.461450	39.701389
2813.163557	598425.787472	39.706407
2816.067381	599480.953791	39.711424
2818.614974	600522.191168	39.716442
2821.538491	601550.337393	39.721460
2824.418921	602566.559611	39.726477
2827.578279	603582.089844	39.731495
2830.593003	604590.656539	39.736512
2833.273012	605603.917433	39.741530
2835.892902	606620.181448	39.746548
2838.931789	607641.567554	39.751565
2841.671920	608673.922703	39.756583
2844.531119	609688.996783	39.761600
2847.666360	610713.552037	39.766618
2850.336941	611742.764164	39.771636
2853.195837	612763.963852	39.776653
2855.955906	613802.127126	39.781671
2859.033541	614848.459085	39.786688
2861.774119	615895.382676	39.791706
2864.301240	616942.529176	39.796724
2867.326904	617980.118449	39.801741
2869.978527	619047.905945	39.806759
2872.549064	620103.234225	39.811776
2875.433414	621161.240645	39.816794
2878.326498	622241.001309	39.821812
2881.613918	623308.477843	39.826829
2884.289793	624383.006047	39.831847
2887.261758	625461.801976	39.836864
2890.546525	626541.027101	39.841882
2893.147866	627619.741338	39.846900
2895.890461	628694.231211	39.851917
2899.052092	629789.691337	39.856935
2901.606574	630888.506259	39.861952
2904.682380	631979.350494	39.866970
2907.790411	633091.064130	39.871988
2910.610020	634178.960635	39.877005
2914.060903	635295.537973	39.882023
2917.042716	636405.292271	39.887040
2919.737106	637512.673459	39.892058
2922.651151	638634.710124	39.897076
2925.348320	639730.640681	39.902093
2928.106211	640858.253938	39.907111
2930.910430	641990.695275	39.912128
2933.868068	643117.258753	39.917146
2936.737401	644248.371382	39.922164
2939.796820	645374.197648	39.927181
2942.611238	646523.179394	39.932199
2945.484739	647656.706357	39.937216
2948.665135	648797.447223	39.942234
2951.166181	649948.235250	39.947252
2954.458080	651088.821779	39.952269
2957.333443	652247.753507	39.957287
2960.998361	653379.155171	39.962304
2964.667814	654509.471365	39.967322
2967.433549	655659.295335	39.972340
2970.133569	656798.013806	39.977357
2973.354771	657933.776766	39.982375
2975.866487	659083.151893	39.987392
2978.925624	660226.686944	39.992410
2981.349962	661387.487043	39.997428
2984.750647	662536.127934	40.002445
2987.337576	663704.187660	40.007463
2990.127783	664855.448951	40.012480
2993.326848	666018.890724	40.017498
2996.543609	667188.818170	40.022516
2999.452434	668353.680268	40.027533
3002.357689	669518.833161	40.032551
3005.644832	670679.706524	40.037568
3009.036839	671849.326425	40.042586
3011.982192	673003.351300	40.047604
3014.664487	674159.045822	40.052621
3018.114552	675302.528468	40.057639
3021.123693	676438.053360	40.062656
3024.255538	677553.602055	40.067674
3027.172345	678663.493195	40.072692
3029.981081	679779.097297	40.077709
3033.165488	680896.871380	40.082727
3035.954924	682006.047102	40.087744
3039.083531	683120.813048	40.092762
3041.684829	684255.847852	40.097780
3044.602472	685385.584003	40.102797
3047.590241	686525.691718	40.107815
3050.033489	687661.277433	40.112832
3053.280188	688814.482552	40.117850
3055.787792	689972.932804	40.122868
3058.546199	691138.003248	40.127885
3061.594916	692305.532483	40.132903
3064.569796	693493.812019	40.137920
3067.541970	694681.524144	40.142938
3070.448904	695879.745296	40.147956
3073.963016	697067.173161	40.152973
3077.214761	698281.732292	40.157991
3080.370512	699471.728419	40.163008
3083.427535	700682.648274	40.168026
3086.508935	701888.445111	40.173044
3089.327440	703104.961357	40.178061
3092.563431	704319.450542	40.183079
3095.320913	705555.542076	40.188096
3098.707417	706777.330865	40.193114
3101.574063	708020.718386	40.198132
3104.477188	709262.622229	40.203149
3107.730033	710511.031958	40.208167
3110.877800	711771.290874	40.213184
3114.172526	713043.254637	40.218202
3117.149960	714301.505684	40.223220
3120.715089	715551.674751	40.228237
3123.641320	716802.038094	40.233255
3126.497066	718069.010902	40.238272
3130.062420	719341.773065	40.243290
3132.994811	720615.852027	40.248308
3136.291395	721894.586889	40.253325
3139.685691	723160.833251	40.258343
3142.381026	724438.448609	40.263360
3145.901473	725711.192309	40.268378
3148.804173	726984.311120	40.273396
3152.083241	728267.390812	40.278413
3155.424208	729558.261056	40.283431
3158.997834	730834.904699	40.288448
3162.225639	732113.843819	40.293466
3164.799242	733413.710422	40.298484
3168.470011	734691.499361	40.303501
3171.763342	735986.035599	40.308519
3174.548309	737271.825163	40.313536
3177.716946	738566.125972	40.318554
3180.729992	739867.002984	40.323572
3184.091110	741163.174663	40.328589
3186.989376	742466.604572	40.333607
3189.763045	743777.284359	40.338624
3193.662055	745082.103230	40.343642
3196.498010	746394.706739	40.348660
3199.650846	747693.625854	40.353677
3202.746192	748999.679715	40.358695
3205.886051	750327.417011	40.363712
3209.279074	751645.305109	40.368730
3212.294209	752973.699431	40.373748
3215.592706	754280.622185	40.378765
3218.594682	755601.615467	40.383783
3221.527181	756927.568494	40.388800
3224.684133	758244.515753	40.393818
3227.932151	759571.049908	40.398836
3231.241450	760873.568013	40.403853
3234.541299	762153.318069	40.408871
3237.321607	763438.496873	40.413888
3240.631308	764724.922484	40.418906
3243.885128	766012.636007	40.423924
3247.783966	767295.996606	40.428941
3251.011190	768587.541497	40.433959
3254.171015	769888.589584	40.438976
3257.605515	771166.507904	40.443994
3260.761194	772470.881897	40.449012
3263.299397	773760.387418	40.454029
3267.001698	775061.442857	40.459047
3270.353380	776376.623389	40.464064
3273.333622	777684.814863	40.469082
3277.009877	779001.828573	40.474100
3279.958291	780319.919688	40.479117
3283.178922	781648.599548	40.484135
3286.354293	782979.073574	40.489152
3289.482286	784313.829742	40.494170
3292.450063	785661.618250	40.499188
3295.851791	787017.165291	40.504205
3299.032325	788361.346678	40.509223
3302.180524	789738.962484	40.514240
3305.884443	791094.308229	40.519258
3308.826572	792468.751041	40.524276
3311.975350	793845.602666	40.529293
3315.498047	795222.300379	40.534311
3318.930914	796609.781030	40.539328
3322.132549	797991.107000	40.544346
3325.221949	799393.146203	40.549364
3328.582053	800781.058803	40.554381
3332.404452	802185.589301	40.559399
3335.652058	803600.998852	40.564416
3339.073193	804994.511979	40.569434
3342.012586	806406.185081	40.574452
3345.714357	807826.909958	40.579469
3348.934091	809236.742500	40.584487
3352.340385	810657.024172	40.589504
3356.109492	812065.555478	40.594522
3359.595216	813492.864201	40.599540
3362.846679	814919.981547	40.604557
3366.594950	816334.940822	40.609575
3370.214362	817757.659869	40.614592
3373.657587	819164.253312	40.619610
3377.291199	820575.448425	40.624628
3380.706271	821987.228644	40.629645
3384.469506	823407.072543	40.634663
3387.405968	824824.583033	40.639680
3390.836710	826233.347049	40.644698
3394.373347	827662.325990	40.649716
3397.705139	829076.653900	40.654733
3401.303338	830485.667586	40.659751
3404.606981	831908.643098	40.664768
3408.169436	833330.176910	40.669786
3411.564029	834750.238816	40.674804
3414.962252	836163.185962	40.679821
3418.178944	837584.540216	40.684839
3421.418493	839012.617295	40.689856
3424.564068	840429.142063	40.694874
3428.030581	841856.016011	40.699892
3431.487430	843305.854849	40.704909
3434.868600	844724.118510	40.709927
3438.335343	846167.546321	40.714944
3441.373244	847600.441738	40.719962
3444.831180	849040.842914	40.724980
3448.310443	850482.333677	40.729997
3451.832004	851920.466607	40.735015
3454.759809	853361.636515	40.740020
3458.471833	854745.027000	40.745024
3461.562922	856085.420367	40.750029
3464.770836	857375.862989	40.755034
3468.384996	858594.390552	40.760039
3471.037858	859777.422192	40.765044
3474.591505	860858.472283	40.770048
3477.519102	861891.767232	40.775053
3480.229807	862865.866148	40.780058
3482.711395	863777.226262	40.785063
3484.765715	864630.448846	40.790068
3487.659844	865414.544008	40.795072
3490.342833	866138.396460	40.800077
3492.757028	866810.632549	40.805082
3495.084802	867410.965764	40.810087
3497.035618	867961.766395	40.815092
3498.669635	868459.853864	40.820096
3500.287010	868907.318884	40.825101
3501.781642	869319.633599	40.830106
3503.419092	869678.040285	40.835111
3504.585090	870002.719369	40.840116
3505.964253	870277.935916	40.845120
3507.069507	870515.160477	40.850125
3508.440044	870730.718156	40.855130
3509.441589	870892.964040	40.860135
3510.334351	871049.818674	40.865140
3511.284675	871160.634472	40.870144
3512.196878	871260.261422	40.875149
3512.637342	871325.804074	40.880154
3513.472657	871357.996545	40.885159
3514.232572	871374.859356	40.890164
3514.741856	871363.104953	40.895168
3515.421833	871344.859246	40.900173
3515.236891	871306.775865	40.905178
3515.922413	871247.714735	40.910183
3516.453002	871172.370492	40.915188
3516.926245	871091.051764	40.920192
3517.536412	870986.841716	40.925197
3517.513262	870882.246252	40.930202
3517.892342	870754.040793	40.935207
3517.961797	870622.503328	40.940212
3517.948032	870476.404059	40.945216
3518.628106	870325.946330	40.950221
3518.454559	870151.394745	40.955226
3518.706192	869986.904808	40.960231
3518.495545	869815.726394	40.965236
3518.734515	869625.844857	40.970240
3519.266546	869438.324058	40.975245
3518.913661	869253.444902	40.980250
3518.923335	869049.101240	40.985255
3519.255465	868848.657437	40.990260
3519.173766	868630.315979	40.995264
3519.190066	868428.458528	41.000269
3518.974165	868217.072611	41.005274
3519.029324	867995.209584	41.010279
3518.982154	867783.008591	41.015284
3519.016729	867562.966120	41.020288
3519.141233	867343.190643	41.025293
3518.845368	867109.857413	41.030298
3519.089656	866880.485732	41.035303
3518.872246	866658.129725	41.040308
3518.930770	866430.410388	41.045312
3518.751342	866202.043017	41.050317
3518.446532	865974.362041	41.055322
3518.718062	865733.349904	41.060327
3518.548856	865506.401500	41.065332
3518.466027	865277.208873	41.070336
3518.514469	865031.178893	41.075341
3518.278821	864805.082034	41.080346
3518.636291	864572.314413	41.085351
3518.177406	864341.500356	41.090356
3517.858176	864102.443113	41.095360
3517.994606	863866.686067	41.100365
3517.776832	863630.201621	41.105370
3517.694846	863393.202957	41.110375
3517.875485	863169.584484	41.115380
3517.511939	862935.219607	41.120384
3517.533749	862702.234326	41.125389
3517.235226	862471.608885	41.130394
3517.062377	862237.088716	41.135399
3517.270926	862014.483431	41.140404
3516.904282	861774.078994	41.145408
3517.376061	861554.893987	41.150413
3516.910818	861318.448524	41.155418
3517.015146	861083.064145	41.160423
3516.535098	860866.611300	41.165428
3516.486510	860633.648896	41.170432
3516.511208	860409.752857	41.175437
3515.816260	860195.531596	41.180442
3515.791130	859974.236531	41.185447
3515.929317	859766.443233	41.190452
3516.024441	859548.593515	41.195456
3515.965517	859329.309186	41.200461
3515.457340	859116.661978	41.205466
3515.304403	858910.526873	41.210471
3515.362305	858702.417322	41.215476
3514.912758	858480.937336	41.220480
3515.017260	858274.062101	41.225485
3514.485346	858080.915459	41.230490
3514.788819	857865.193436	41.235495
3514.367184	857669.210876	41.240500
3514.221142	857470.276824	41.245504
3514.107794	857269.783126	41.250509
3514.108258	857084.741459	41.255514
3514.031806	856891.773722	41.260519
3513.718675	856698.256075	41.265524
3513.586414	856506.735166	41.270528
3513.602349	856326.600371	41.275533
3513.598135	856127.307365	41.280538
3513.415220	855937.420084	41.285543
3513.109973	855765.735109	41.290548
3512.959964	855581.732823	41.295552
3513.215042	855386.727614	41.300557
3512.381320	855221.011266	41.305562
3512.407816	855039.866908	41.310567
3512.619711	854867.396944	41.315572
3512.239810	854692.885382	41.320576
3512.414267	854526.217278	41.325581
3512.355102	854356.387274	41.330586
3512.215195	854183.661526	41.335591
3511.808516	854022.489324	41.340596
3511.554904	853856.836615	41.345600
3511.835690	853703.968286	41.350605
3511.252103	853547.746610	41.355610
3511.389029	853383.567909	41.360615
3511.374503	853227.635790	41.365620
3510.964850	853078.537051	41.370624
3510.942115	852920.661989	41.375629
3510.584156	852772.224870	41.380634
3510.667970	852620.713928	41.385639
3510.668915	852471.438549	41.390644
3510.573486	852325.175497	41.395648
3510.697146	852177.035067	41.400653
3510.696325	852042.658011	41.405658
3510.524578	851892.523377	41.410663
3510.113251	851746.779190	41.415668
3510.652459	851598.171733	41.420672
3510.296013	851442.341808	41.425677
3509.907126	851319.918089	41.430682
3509.913045	851172.060872	41.435687
3509.836158	851035.057972	41.440692
3509.738877	850902.993548	41.445696
3509.557750	850769.874033	41.450701
3509.372659	850648.178975	41.455706
3509.381861	850512.118662	41.460711
3509.169224	850386.936190	41.465716
3508.933136	850268.436947	41.470720
3509.219821	850132.614911	41.475725
3508.996510	850013.043155	41.480730
3508.757269	849894.730486	41.485735
3508.581559	849769.141542	41.490740
3508.594890	849658.048519	41.495744
3508.761412	849530.851266	41.500749
3508.706351	849422.766999	41.505754
3508.592296	849299.773468	41.510759
3508.488648	849183.943529	41.515764
3508.337493	849068.699900	41.520768
3508.403180	848945.573932	41.525773
3508.209486	848839.340975	41.530778
3508.230885	848725.225999	41.535783
3507.834175	848610.592919	41.540788
3507.628406	848516.271186	41.545792
3507.835247	848414.230302	41.550797
3507.698247	848306.525652	41.555802
3507.558571	848194.556769	41.560807
3507.816047	848103.159187	41.565812
3507.359902	848000.730315	41.570816
3507.609979	847897.026646	41.575821
3507.335627	847804.351154	41.580826
3507.256924	847694.591516	41.585831
3507.375313	847593.712775	41.590836
3507.074158	847507.431414	41.595840
3507.198525	847407.711211	41.600845
3506.864966	847318.040907	41.605850
3506.839573	847220.569470	41.610855
3506.836349	847135.592577	41.615860
3506.915497	847038.876942	41.620864
3506.664860	846946.862435	41.625869
3506.733528	846857.994298	41.630874
3506.818182	846772.998406	41.635879
3506.474099	846692.138254	41.640884
3506.542377	846601.425115	41.645888
3506.637277	846510.803318	41.650893
3506.155088	846427.247710	41.655898
3506.399416	846340.282421	41.660903
3506.391250	846260.817445	41.665908
3506.306332	846180.975741	41.670912
3505.992176	846097.970642	41.675917
3505.914212	846023.455943	41.680922
3506.007136	845942.904795	41.685927
3505.802040	845862.108376	41.690932
3505.442917	845790.348351	41.695936
3505.691112	845724.501531	41.700941
3505.634087	845649.203448	41.705946
3505.471557	845577.700853	41.710951
3505.614425	845500.431174	41.715956
3505.650048	845433.935863	41.720960
3505.834559	845366.931898	41.725965
3505.503429	845303.012498	41.730970
3505.610644	845227.101769	41.735975
3505.403338	845162.967632	41.740980
3504.996074	845084.324543	41.745984
3505.275742	845011.485836	41.750989
3505.078691	844951.321971	41.755994
3505.148813	844891.018791	41.760999
3505.340025	844819.354733	41.766004
3505.095518	844760.553417	41.771008
3505.380791	844703.607426	41.776013
3504.834964	844646.790802	41.781018
3505.090198	844571.236217	41.786023
3505.098477	844505.219367	41.791028
3504.708144	844446.049940	41.796032
3504.727110	844378.769771	41.801037
3504.585015	844329.351481	41.806042
3504.699978	844270.295183	41.811047
3504.831708	844218.797345	41.816052
3504.664488	844158.426814	41.821056
3505.010678	844101.174639	41.826061
3505.068224	844041.543345	41.831066
3504.988780	843978.733566	41.836071
3505.052538	843912.798349	41.841076
3504.829994	843855.535743	41.846080
3504.620135	843804.378530	41.851085
3504.570082	843742.240292	41.856090
3504.272341	843682.370044	41.861095
3504.741872	843628.487363	41.866100
3504.249060	843581.929292	41.871104
3504.145437	843528.135288	41.876109
3504.304821	843487.776647	41.881114
3504.251374	843429.804772	41.886119
3504.366787	843379.465640	41.891124
3503.770749	843329.528168	41.896128
3504.219541	843278.651266	41.901133
3503.939888	843234.190241	41.906138
3504.300462	843179.641771	41.911143
3504.405680	843134.828950	41.916148
3503.979667	843091.068461	41.921152
3504.386543	843044.462465	41.926157
3504.527218	842995.182707	41.931162
3504.303853	842936.941657	41.936167
3503.942199	842886.866827	41.941172
3503.831936	842846.352018	41.946176
3503.769265	842790.217673	41.951181
3503.740566	842753.568193	41.956186
3503.566709	842702.977603	41.961191
3503.665335	842672.222844	41.966196
3503.320554	842638.240244	41.971200
3503.500821	842591.084273	41.976205
3503.896784	842561.930971	41.981210
3503.793703	842511.424647	41.986215
3503.853652	842468.844217	41.991220
3503.651239	842424.655934	41.996224
3503.484437	842385.310486	42.001229
3503.378223	842360.307622	42.006234
3503.289724	842318.234186	42.011239
3503.284770	842269.068110	42.016244
3503.277548	842237.551823	42.021248
3503.579655	842200.265337	42.026253
3503.464158	842170.220280	42.031258
3503.451386	842123.575647	42.036263
3503.611416	842095.911615	42.041268
3503.434312	842050.940745	42.046272
3503.620763	842017.647370	42.051277
3503.086002	841982.429941	42.056282
3502.964044	841950.445153	42.061287
3503.220972	841909.090661	42.066292
3503.279864	841878.241000	42.071296
3503.490607	841849.695043	42.076301
3503.208874	841807.648179	42.081306
3502.998606	841776.549111	42.086311
3503.183363	841751.013261	42.091316
3502.948322	841720.499680	42.096320
3503.151767	841678.570026	42.101325
3503.058858	841646.191106	42.106330
3502.998546	841615.940632	42.111335
3503.312315	841582.430932	42.116340
3503.046149	841566.081615	42.121344
3502.902812	841526.144850	42.126349
3502.905705	841505.873759	42.131354
3503.178666	841466.550440	42.136359
3502.823546	841436.636102	42.141364
3502.620278	841409.898566	42.146368
3503.205242	841369.943890	42.151373
3502.925224	841343.703008	42.156378
3502.719237	841318.032390	42.161383
3502.934695	841293.168712	42.166388
3502.780932	841274.085226	42.171392
3502.939890	841240.694787	42.176397
3502.968678	841223.716455	42.181402
3502.740336	841185.924541	42.186407
3502.736710	841151.589073	42.191412
3502.652937	841121.921711	42.196416
3502.665989	841109.310297	42.201421
3502.669899	841083.508855	42.206426
3503.086125	841061.910685	42.211431
3503.096835	841035.622990	42.216436
3502.593651	840996.708870	42.221440
3502.843059	840964.272709	42.226445
3502.785326	840938.480271	42.231450
3502.720122	840925.007714	42.236455
3502.793541	840894.829649	42.241460
3502.398114	840876.461650	42.246464
3502.721641	840833.052252	42.251469
3502.655459	840811.043580	42.256474
3502.719991	840783.776350	42.261479
3503.073988	840758.112768	42.266484
3502.628617	840727.723946	42.271488
3502.605330	840708.230231	42.276493
3502.384776	840688.961294	42.281498
3502.721388	840670.090212	42.286503
3503.092000	840646.169597	42.291508
3502.445477	840616.781679	42.296512
3502.541146	840589.314681	42.301517
3502.932884	840558.988144	42.306522
3502.380600	840530.846127	42.311527
3502.805906	840505.073299	42.316532
3502.642284	840486.473841	42.321536
3502.553511	840458.065010	42.326541
3502.452114	840438.291600	42.331546
3502.522427	840410.827739	42.336551
3502.348265	840393.199705	42.341556
3502.341643	840377.970617	42.346560
3502.396213	840342.651291	42.351565
3502.264652	840325.501436	42.356570
3502.209603	840314.451111	42.361575
3502.286719	840289.119810	42.366580
3502.195578	840277.687023	42.371584
3502.449752	840253.200973	42.376589
3502.262140	840242.365255	42.381594
3502.225496	840223.357083	42.386599
3502.400346	840197.525064	42.391604
3502.095425	840189.617899	42.396608
3502.412555	840165.994744	42.401613
3502.250876	840145.259670	42.406618
3502.272868	840134.002943	42.411623
3502.542147	840105.536453	42.416628
3502.360066	840084.513321	42.421632
3502.222336	840065.714470	42.426637
3502.006403	840052.942580	42.431642
3502.301094	840033.979020	42.436647
3502.144174	840010.720391	42.441652
3502.191237	840008.772794	42.446656
3501.861676	839981.078413	42.451661
3502.155600	839977.637007	42.456666
3502.315440	839950.351049	42.461671
3502.502825	839928.299463	42.466676
3502.137037	839917.102943	42.471680
3502.318596	839898.835742	42.476685
3501.859928	839881.056628	42.481690
3502.122704	839862.097509	42.486695
3502.479817	839845.063908	42.491700
3502.021489	839828.351760	42.496704
3502.081172	839811.655606	42.501709
3502.246019	839790.092115	42.506714
3502.239547	839780.682492	42.511719
3502.452869	839753.096217	42.516724
3502.072021	839739.670307	42.521728
3502.194026	839720.732744	42.526733
3502.463463	839708.563366	42.531738
3502.220128	839687.645420	42.536743
3502.226666	839664.456901	42.541748
3501.960656	839656.542939	42.546752
3502.190062	839638.752557	42.551757
3502.168774	839628.374813	42.556762
3502.194444	839594.898932	42.561767
3502.192055	839588.690035	42.566772
3502.082788	839564.549024	42.571776
3502.333857	839543.650306	42.576781
3501.690653	839528.615570	42.581786
3501.862449	839511.512962	42.586791
3502.087206	839517.008088	42.591796
3501.653169	839502.425696	42.596800
3502.001390	839483.063927	42.601805
3501.824816	839487.748617	42.606810
3501.935064	839466.095464	42.611815
3502.295915	839446.828625	42.616820
3502.104027	839431.432024	42.621824
3502.281257	839404.334888	42.626829
3502.153978	839395.234609	42.631834
3502.416908	839386.461414	42.636839
3502.483391	839367.531406	42.641844
3502.200225	839345.842289	42.646848
3501.987442	839318.902755	42.651853
3501.812803	839310.100824	42.656858
3501.821145	839298.165473	42.661863
3501.909834	839289.904498	42.666868
3501.932655	839282.235961	42.671872
3501.790697	839257.031532	42.676877
3501.735069	839250.636552	42.681882
3501.638149	839240.269953	42.686887
3502.109216	839217.395179	42.691892
3501.773703	839222.590054	42.696896
3501.953119	839195.491626	42.701901
3501.896956	839187.544233	42.706906
3501.882517	839174.835981	42.711911
3501.724581	839156.231462	42.716916
3501.810895	839157.091246	42.721920
3501.717473	839146.723937	42.726925
3501.977051	839137.659817	42.731930
3501.625542	839118.891385	42.736935
3501.828192	839115.269698	42.741940
3501.760661	839106.450721	42.746944
3501.812627	839097.321966	42.751949
3501.829611	839077.719574	42.756954
3501.968483	839076.630580	42.761959
3502.112929	839055.649788	42.766964
3501.559456	839057.870975	42.771968
3501.883543	839051.804541	42.776973
3501.850153	839028.037606	42.781978
3501.533287	839023.914897	42.786983
3501.894531	839012.603014	42.791988
3501.651205	839001.288587	42.796993
3501.921901	838983.974945	42.801997
3501.785835	838981.958609	42.807002
3501.446525	838973.764100	42.812007
3501.537148	838950.268560	42.817012
3502.021777	838943.982859	42.822017
3501.715257	838938.403009	42.827021
3501.806621	838934.410486	42.832026
3501.515538	838911.944772	42.837031
3501.924917	838893.541843	42.842036
3501.858997	838897.239381	42.847041
3501.644517	838873.694200	42.852045
3501.786638	838863.483641	42.857050
3501.628666	838863.314301	42.862055
3501.564971	838851.195249	42.867060
3501.502251	838843.248421	42.872065
3501.566502	838827.907247	42.877069
3501.713484	838823.711889	42.882074
3501.301220	838825.037791	42.887079
3501.798958	838808.270344	42.892084
3501.394315	838800.473941	42.897089
3501.620571	838795.101772	42.902093
3501.803545	838787.116462	42.907098
3501.729019	838775.678184	42.912103
3502.252019	838761.720633	42.917108
3501.886333	838754.694351	42.922113
3501.565039	838735.822950	42.927117
3501.873778	838732.475551	42.932122
3501.642161	838724.846069	42.937127
3501.969159	838712.956767	42.942132
3501.988337	838704.705847	42.947137
3501.680258	838690.878045	42.952141
3501.911467	838681.720633	42.957146
3501.509055	838666.840134	42.962151
3502.111427	838654.131385	42.967156
3501.373710	838661.136258	42.972161
3501.679235	838644.107292	42.977165
3501.754219	838623.038799	42.982170
3501.549221	838614.628725	42.987175
3501.565343	838615.984742	42.992180
3501.508460	838622.592124	42.997185
3501.535054	838585.520080	43.002189
3501.677909	838585.206669	43.007194
3501.378531	838579.334253	43.012199
3501.702572	838578.604371	43.017204
3501.394255	838572.248161	43.022209
3501.173269	838551.225680	43.027213
3500.850967	838550.984980	43.032218
3500.956951	838547.475098	43.037223
3501.408403	838544.590473	43.042228
3501.347828	838549.839989	43.047233
3501.460762	838553.412744	43.052237
3501.747594	838551.039042	43.057242
3501.647089	838556.585905	43.062247
3501.616567	838535.824709	43.067252
3501.452085	838534.685999	43.072257
3501.660564	838530.771936	43.077261
3501.552626	838534.573304	43.082266
3501.157598	838519.788319	43.087271
3501.362863	838502.192393	43.092276
3501.432218	838491.507382	43.097281
3501.425264	838486.559545	43.102285
3501.611356	838495.069853	43.107290
3501.489771	838504.307511	43.112295
3501.542021	838481.495386	43.117300
3501.359899	838467.550335	43.122305
3501.296641	838452.810359	43.127309
3501.279445	838462.225842	43.132314
3501.518042	838461.897458	43.137319
3501.826254	838472.717638	43.142324
3501.388726	838464.246662	43.147329
3501.625123	838437.718112	43.152333
3501.496972	838431.236548	43.157338
3501.523684	838431.523519	43.162343
3501.730851	838428.482947	43.167348
3501.483638	838413.577552	43.172353
3501.236960	838399.351314	43.177357
3501.523789	838394.357476	43.182362
3501.632305	838399.774771	43.187367
3501.786041	838399.556689	43.192372
3501.420690	838380.496967	43.197377
3501.396295	838370.214553	43.202381
3501.794900	838371.607877	43.207386
3501.790621	838373.549379	43.212391
3501.762818	838349.972943	43.217396
3501.722099	838334.743949	43.222401
3501.678472	838331.451410	43.227405
3501.776540	838331.533150	43.232410
3501.290235	838307.834138	43.237415
3501.529749	838296.928097	43.242420
3501.321016	838297.737087	43.247425
3501.670655	838295.644591	43.252429
3501.824149	838296.785124	43.257434
3501.039831	838267.601172	43.262439
3501.424586	838257.351647	43.267444
3501.729301	838271.666254	43.272449
3501.662209	838262.845957	43.277453
3501.585261	838263.246183	43.282458
3501.455554	838252.009608	43.287463
3501.401813	838231.348021	43.292468
3501.069599	838226.450813	43.297473
3501.248795	838240.008776	43.302477
3501.134392	838232.263296	43.307482
3501.465914	838234.055309	43.312487
3501.679395	838229.752097	43.317492
3501.500529	838217.164545	43.322497
3501.318795	838200.695696	43.327501
3501.218479	838194.500652	43.332506
3501.498224	838202.802653	43.337511
3501.533921	838201.729629	43.342516
3501.580938	838204.245426	43.347521
3501.723398	838192.480979	43.352525
3501.958341	838170.609537	43.357530
3501.516161	838183.682502	43.362535
3501.529897	838171.452919	43.367540
3501.401982	838150.511516	43.372545
3501.274902	838147.134876	43.377549
3501.481098	838145.161795	43.382554
3501.339252	838142.466768	43.387559
3501.734600	838139.881854	43.392564
3501.393355	838144.302205	43.397569
3501.283752	838119.961294	43.402573
3501.652671	838108.161280	43.407578
3501.321383	838110.153987	43.412583
3501.512860	838107.018661	43.417588
3501.567895	838115.355910	43.422593
3501.450963	838103.922970	43.427597
3501.240322	838077.947923	43.432602
3501.478338	838080.530961	43.437607
3501.592533	838080.707229	43.442612
3501.551922	838085.371763	43.447617
3501.897673	838078.815735	43.452621
3501.895669	838064.841584	43.457626
3501.472276	838054.329860	43.462631
3501.586324	838052.177063	43.467636
3501.710766	838045.849684	43.472641
3501.730377	838027.990246	43.477645
3501.550688	838021.419245	43.482650
3501.234217	838026.126948	43.487655
3501.715686	838016.541214	43.492660
3501.516949	837997.357171	43.497665
3501.787166	837990.618762	43.502669
3501.730174	837975.585486	43.507674
3501.447124	837982.520071	43.512679
3501.381779	837971.078811	43.517684
3501.385072	837960.500222	43.522689
3501.313465	837955.465004	43.527693
3501.760647	837960.247478	43.532698
3501.618608	837962.307696	43.537703
3501.828634	837944.806430	43.542708
3501.883125	837932.375891	43.547713
3501.489847	837918.462560	43.552717
3501.754136	837910.463368	43.557722
3501.698699	837895.817839	43.562727
3501.689948	837890.966837	43.567732
3501.440797	837885.182928	43.572737
3501.350103	837885.973520	43.577741
3501.793586	837878.043321	43.582746
3501.724495	837853.986136	43.587751
3501.711614	837846.903624	43.592756
3501.531687	837848.678657	43.597761
3501.726853	837839.040346	43.602765
3501.817138	837815.346287	43.607770
3501.346534	837811.829057	43.612775
3501.845203	837812.430480	43.617780
3502.086711	837804.531757	43.622785
3501.914450	837789.224882	43.627789
3501.875094	837779.137886	43.632794
3501.780995	837771.000432	43.637799
3501.701705	837750.729373	43.642804
3501.540332	837750.366426	43.647809
3501.650103	837741.032458	43.652813
3501.708478	837724.330656	43.657818
3501.584603	837718.915205	43.662823
3501.702923	837709.968054	43.667828
3502.118430	837706.409296	43.672833
3501.619205	837683.195068	43.677837
3501.997165	837683.038963	43.682842
3501.398075	837672.456976	43.687847
3501.883568	837646.953541	43.692852
3501.415829	837642.077032	43.697857
3501.247754	837643.753221	43.702861
3501.597685	837641.951612	43.707866
3501.225105	837636.477911	43.712871
3501.350900	837616.077283	43.717876
3501.374402	837609.668169	43.722881
3501.398929	837611.702469	43.727885
3501.493645	837611.493588	43.732890
3501.456724	837613.149283	43.737895
3501.524966	837610.809383	43.742900
3501.332894	837610.645331	43.747905
3501.450821	837591.992798	43.752909
3501.573025	837577.901036	43.757914
3501.241887	837589.210982	43.762919
3501.380367	837582.783866	43.767924
3501.410431	837584.234992	43.772929
3501.590929	837579.451206	43.777933
3501.416630	837565.599871	43.782938
3501.449509	837563.168427	43.787943
3501.761787	837546.620544	43.792948
3501.939959	837551.736563	43.797953
3501.503347	837527.444350	43.802957
3501.470401	837510.659172	43.807962
3501.278673	837520.297533	43.812967
3501.714630	837517.803062	43.817972
3501.389026	837518.921585	43.822977
3501.258544	837510.983570	43.827981
3501.457592	837494.453243	43.832986
3501.270087	837494.773747	43.837991
3501.529569	837491.142197	43.842996
3501.324430	837490.009640	43.848001
3501.447658	837483.487747	43.853005
3502.051832	837482.034567	43.858010
3501.416794	837465.537489	43.863015
3501.550120	837447.561482	43.868020
3501.390938	837456.806637	43.873025
3501.156121	837458.202144	43.878029
3501.792202	837443.641517	43.883034
3501.427931	837443.407323	43.888039
3501.438118	837425.159332	43.893044
3501.311911	837417.414635	43.898049
3501.260755	837414.316877	43.903053
3501.544142	837422.328233	43.908058
3501.218099	837419.952838	43.913063
3501.690001	837416.385093	43.918068
3501.645637	837396.204425	43.923073
3501.519963	837384.771470	43.928077
3501.693376	837395.905853	43.933082
3501.463218	837387.983256	43.938087
3501.499394	837371.963332	43.943092
3501.271228	837363.555108	43.948097
3501.062982	837366.014106	43.953101
3501.531676	837358.370451	43.958106
3501.161099	837378.616170	43.963111
3501.240119	837363.463033	43.968116
3501.432180	837361.783077	43.973121
3501.347658	837372.084315	43.978125
3501.464606	837336.155056	43.983130
3501.369442	837334.519991	43.988135
3501.588798	837323.712384	43.993140
3501.096488	837334.756833	43.998145
3501.202957	837330.275591	44.003149
3501.517524	837326.635332	44.008154
3501.285576	837336.280276	44.013159
3501.284250	837313.957346	44.018164
3501.372160	837300.258521	44.023169
3501.164204	837298.641078	44.028173
3501.657678	837307.007980	44.033178
3501.107801	837305.541045	44.038183
3501.718773	837300.107399	44.043188
3501.464087	837299.273722	44.048193
3501.464414	837280.638599	44.053197
3501.602941	837271.493518	44.058202
3501.189322	837281.652240	44.063207
3501.436954	837281.613560	44.068212
3501.759583	837274.963212	44.073217
3501.524369	837257.917767	44.078221
3501.508038	837248.117449	44.083226
3501.045111	837246.733965	44.088231
3501.131085	837250.894070	44.093236
3501.426414	837243.762663	44.098241
3501.333632	837246.106602	44.103245
3501.484017	837249.965463	44.108250
3501.385891	837251.630825	44.113255
3501.738868	837218.381598	44.118260
3501.438572	837221.340339	44.123265
3501.460324	837212.310480	44.128269
3501.535706	837207.931066	44.133274
3501.362196	837221.352366	44.138279
3501.698511	837185.582029	44.143284
3501.600236	837181.423860	44.148289
3501.181609	837179.742257	44.153293
3501.731330	837179.656354	44.158298
3501.755606	837164.705390	44.163303
3501.642215	837137.449264	44.168308
3501.491628	837141.743484	44.173313
3501.630985	837141.430549	44.178317
3501.376247	837131.084945	44.183322
3501.367980	837120.021371	44.188327
3501.650968	837106.097485	44.193332
3501.325995	837107.701287	44.198337
3501.365970	837113.809894	44.203341
3501.695791	837112.884820	44.208346
3501.289694	837107.998232	44.213351
3501.691832	837081.340688	44.218356
3501.676524	837076.490048	44.223361
3501.240800	837077.528803	44.228365
3501.742286	837079.488727	44.233370
3501.520627	837068.555476	44.238375
3501.546701	837052.633336	44.243380
3501.857380	837046.275788	44.248385
3501.357340	837041.306769	44.253389
3501.598217	837037.289607	44.258394
3501.784005	837018.430551	44.263399
3501.741543	837014.554728	44.268404
3501.816634	837010.757589	44.273409
3501.780294	837010.375050	44.278413
3501.994449	836988.114280	44.283418
3501.784598	836988.535365	44.288423
3501.761466	836974.853152	44.293428
3501.957648	836955.312831	44.298433
3501.495108	836951.405570	44.303437
3501.695132	836942.541563	44.308442
3501.591073	836927.221813	44.313447
3501.635360	836907.219761	44.318452
3501.569195	836907.036005	44.323457
3501.642781	836905.374443	44.328461
3501.777857	836888.270057	44.333466
3501.728494	836876.338877	44.338471
3501.483765	836871.329804	44.343476
3501.626475	836873.928269	44.348481
3501.559432	836864.135248	44.353485
3501.791268	836841.482911	44.358490
3501.863782	836832.347478	44.363495
3501.539878	836834.436510	44.368500
3501.846281	836822.643740	44.373505
3501.931715	836810.400160	44.378509
3501.686790	836802.284959	44.383514
3501.661909	836789.476187	44.388519
3501.502086	836776.397282	44.393524
3502.290065	836765.790980	44.398529
3501.683305	836761.809071	44.403533
3501.737739	836726.759518	44.408538
3501.668664	836736.768235	44.413543
3501.723252	836723.267430	44.418548
3501.926628	836714.693764	44.423553
3501.436974	836688.950414	44.428557
3501.737018	836687.253392	44.433562
3501.520756	836687.384295	44.438567
3501.538721	836680.683848	44.443572
3501.696823	836668.234482	44.448577
3501.372479	836661.587523	44.453581
3501.731733	836653.377674	44.458586
3501.991900	836660.617142	44.463591
3501.881961	836639.570555	44.468596
3501.841488	836627.346282	44.473601
3501.534634	836628.559102	44.478605
3501.737127	836599.018562	44.483610
3501.571530	836600.985858	44.488615
3501.494430	836583.331354	44.493620
3501.631893	836584.183519	44.498625
3501.871992	836575.603913	44.503629
3502.368080	836558.636291	44.508634
3501.939054	836550.646595	44.513639
3501.369156	836525.400432	44.518644
3501.881563	836507.265271	44.523649
3501.638587	836513.612864	44.528653
3501.843178	836505.232849	44.533658
3501.702639	836490.305962	44.538663
3501.890711	836472.997963	44.543668
3501.993391	836465.604535	44.548673
3501.918766	836442.998595	44.553677
3502.132484	836420.735785	44.558682
3501.599708	836427.031698	44.563687
3501.386111	836406.971213	44.568692
3501.546158	836397.627290	44.573697
3501.176399	836398.752915	44.578701
3501.524970	836400.542830	44.583706
3501.293749	836406.112120	44.588711
3501.263188	836401.166244	44.593716
3501.503000	836403.652665	44.598721
3501.532907	836377.438464	44.603725
3501.538344	836380.058604	44.608730
3501.656763	836374.409909	44.613735
3501.539882	836362.876548	44.618740
3501.727903	836341.296969	44.623745
3501.338857	836332.912437	44.628749
3501.317141	836339.128554	44.633754
3501.112831	836345.955645	44.638759
3500.987499	836336.462090	44.643764
3501.107524	836338.967263	44.648769
3501.052772	836332.569012	44.653773
3501.384148	836335.526515	44.658778
3501.092841	836345.861845	44.663783
3501.437911	836337.168416	44.668788
3501.219408	836317.302544	44.673793
3500.835951	836317.847883	44.678797
3501.663469	836310.340957	44.683802
3501.272628	836309.916714	44.688807
3501.017311	836305.976630	44.693812
3501.401923	836303.004323	44.698817
3500.930302	836303.272223	44.703821
3501.109199	836304.312100	44.708826
3501.281930	836312.439324	44.713831
3501.273715	836310.887459	44.718836
3501.323257	836310.976818	44.723841
3500.965256	836318.313334	44.728845
3501.157607	836314.303277	44.733850
3501.333248	836311.363639	44.738855
3501.201502	836297.211485	44.743860
3500.996942	836280.935046	44.748865
3501.061106	836285.002161	44.753869
3501.372125	836277.964230	44.758874
3501.202840	836289.930844	44.763879
3501.385671	836290.096441	44.768884
3501.469212	836279.890627	44.773889
3501.230317	836287.693933	44.778893
3501.406109	836297.568033	44.783898
3501.286747	836277.007011	44.788903
3500.810941	836252.424503	44.793908
3500.958120	836256.575735	44.798913
3501.389897	836252.819433	44.803917
3501.315769	836258.946751	44.808922
3501.537995	836259.882788	44.813927
3501.198598	836266.731086	44.818932
3501.454533	836260.575416	44.823937
3501.196450	836263.916322	44.828941
3501.421301	836270.967636	44.833946
3501.350953	836252.049131	44.838951
3501.444398	836229.901486	44.843956
3501.587542	836224.637085	44.848961
3501.466536	836223.102828	44.853965
3501.470514	836224.267138	44.858970
3500.985877	836227.837629	44.863975
3500.995345	836231.136730	44.868980
3501.189783	836222.952058	44.873985
3501.352409	836226.809671	44.878989
3501.117876	836204.907353	44.883994
3501.050007	836191.521566	44.888999
3500.757482	836189.431658	44.894004
3501.119802	836201.315348	44.899009
3501.257899	836208.768600	44.904013
3501.349648	836198.755515	44.909018
3501.181235	836203.732721	44.914023
3501.358917	836200.210258	44.919028
3501.340551	836202.348819	44.924033
3501.117491	836207.334565	44.929037
3501.506863	836206.205899	44.934042
3501.497968	836203.392131	44.939047
3501.587676	836188.719724	44.944052
3501.669272	836174.533929	44.949057
3501.106621	836171.515482	44.954061
3501.477000	836170.778082	44.959066
3501.225524	836176.641979	44.964071
3501.200553	836181.499705	44.969076
3501.389986	836167.588264	44.974081
3500.991368	836151.244731	44.979085
3501.405608	836142.346056	44.984090
3501.375534	836139.050186	44.989095
3501.181469	836130.634890	44.994100
3501.267832	836135.766479	44.999105
3501.079941	836142.979541	45.004109
3501.331214	836140.027998	45.009114
3500.883204	836149.902778	45.014119
3501.095862	836153.364312	45.019124
3501.127720	836148.602622	45.024129
3501.411682	836139.724308	45.029133
3501.578480	836128.243226	45.034138
3501.201190	836122.574706	45.039143
3501.042535	836110.659081	45.044148
3501.517350	836105.633961	45.049153
3501.301965	836112.754279	45.054157
3501.056755	836118.326023	45.059162
3500.850356	836123.212157	45.064167
3501.100511	836118.998780	45.069172
3501.848562	836117.425722	45.074177
3501.109003	836122.006893	45.079181
3501.085480	836102.109825	45.084186
3501.362013	836101.095856	45.089191
3501.151044	836093.265612	45.094196
3501.348300	836089.060483	45.099201
3501.269748	836085.675085	45.104205
3501.588832	836083.489533	45.109210
3501.368637	836084.494757	45.114215
3501.033758	836091.925013	45.119220
3501.084513	836090.460949	45.124225
3501.217315	836098.012243	45.129229
3501.193699	836088.793626	45.134234
3501.222978	836069.082349	45.139239
3501.200237	836059.863550	45.144244
3501.363298	836060.226401	45.149249
3501.252349	836065.680128	45.154253
3500.960408	836065.046250	45.159258
3500.737008	836069.838007	45.164263
3500.803114	836071.769255	45.169268
3501.468585	836063.996123	45.174273
3501.247660	836062.962833	45.179277
3501.432238	836056.138563	45.184282
3501.223896	836061.413363	45.189287
3501.543127	836062.431346	45.194292
3501.548995	836050.198649	45.199297
3501.256175	836038.206774	45.204301
3501.554224	836030.005643	45.209306
3501.571707	836031.264957	45.214311
3501.223905	836033.940467	45.219316
3501.515350	836032.827078	45.224321
3501.193629	836021.810470	45.229325
3501.356346	836008.873621	45.234330
3501.151256	836005.896272	45.239335
3501.264577	836009.567576	45.244340
3501.319071	836003.248974	45.249345
3501.273116	836008.110121	45.254349
3501.301284	836008.105747	45.259354
3501.397167	836009.935282	45.264359
3501.657569	835997.468532	45.269364
3501.635406	835974.852622	45.274369
3501.352937	835974.508490	45.279373
3501.402039	835968.481932	45.284378
3501.683580	835981.058244	45.289383
3501.140552	835976.386283	45.294388
3501.722179	835957.947406	45.299393
3501.602773	835948.840626	45.304397
3501.352751	835943.928678	45.309402
3501.447757	835940.516066	45.314407
3501.206966	835941.621613	45.319412
3501.582060	835948.067345	45.324417
3501.148514	835922.894396	45.329421
3501.347417	835902.282335	45.334426
3501.391568	835906.158675	45.339431
3501.103709	835912.222677	45.344436
3501.374071	835906.064389	45.349441
3501.325638	835912.382205	45.354445
3501.337776	835908.594209	45.359450
3501.277441	835909.865713	45.364455
3501.019695	835905.537422	45.369460
3501.358547	835897.912214	45.374465
3501.378941	835890.725100	45.379469
3501.274155	835875.985250	45.384474
3501.213775	835886.964836	45.389479
3501.248110	835878.998884	45.394484
3501.352834	835882.380368	45.399489
3501.028204	835888.547223	45.404493
3501.603471	835882.826651	45.409498
3501.565721	835876.522335	45.414503
3501.102887	835856.596044	45.419508
3501.450096	835856.735960	45.424513
3501.540973	835851.964808	45.429517
3501.596195	835841.568512	45.434522
3501.209973	835852.890340	45.439527
3500.925511	835847.789533	45.444532
3501.460609	835850.715434	45.449537
3501.021241	835845.056352	45.454541
3501.215046	835829.395981	45.459546
3501.456602	835822.271294	45.464551
3501.394277	835828.397207	45.469556
3501.475199	835831.297033	45.474561
3501.142842	835825.815368	45.479565
3501.556305	835817.595906	45.484570
3501.917994	835828.995029	45.489575
3501.529477	835805.562014	45.494580
3501.590429	835789.825224	45.499585
3501.416382	835796.454045	45.504589
3501.581725	835792.253698	45.509594
3501.735260	835773.201599	45.514599
3501.654715	835765.933031	45.519604
3501.026632	835758.264633	45.524609
3501.044892	835762.339279	45.529613
3501.133002	835759.607222	45.534618
3501.480889	835754.019156	45.539623
3501.488124	835760.037182	45.544628
3501.643647	835731.761781	45.549633
3501.670259	835725.253078	45.554637
3501.547067	835722.845284	45.559642
3501.498826	835718.289940	45.564647
3501.164480	835722.905150	45.569652
3501.162429	835704.653820	45.574657
3500.987794	835696.720291	45.579661
3501.379301	835686.950745	45.584666
3501.247805	835691.534268	45.589671
3501.091679	835690.296614	45.594676
3501.448699	835685.677895	45.599681
3501.401770	835682.869828	45.604685
3501.381756	835697.920973	45.609690
3501.595238	835695.363455	45.614695
3501.740371	835682.622819	45.619700
3501.474215	835656.645910	45.624705
3501.532212	835665.180288	45.629709
3501.597729	835648.180319	45.634714
3501.603994	835660.509084	45.639719
3501.269736	835635.222317	45.644724
3501.613783	835615.460343	45.649729
3501.461448	835621.503452	45.654733
3501.430205	835608.304805	45.659738
3501.284087	835612.405249	45.664743
3501.194027	835623.292872	45.669748
3501.031438	835608.755569	45.674753
3501.048479	835596.908540	45.679757
3500.977845	835594.298307	45.684762
3501.351769	835591.715666	45.689767
3501.076734	835597.486724	45.694772
3501.417387	835601.122742	45.699777
3501.447059	835593.739652	45.704781
3501.226232	835593.385859	45.709786
3501.048103	835595.937953	45.714791
3501.347806	835597.541583	45.719796
3501.502023	835585.867260	45.724801
3501.050948	835577.394273	45.729805
3501.069884	835567.003172	45.734810
3501.013532	835567.303268	45.739815
3501.505349	835567.614760	45.744820
3501.196355	835556.498217	45.749825
3501.268129	835505.128338	45.754829
3500.942497	835401.392597	45.759834
3500.746886	835241.322183	45.764839
3500.328117	835050.212328	45.769844
3500.957241	834791.643800	45.774849
3500.484688	834505.270762	45.779853
3499.972398	834155.867102	45.784858
3499.822477	833740.057056	45.789863
3499.401912	833300.756977	45.794868
3499.342463	832801.050638	45.799873
3499.143869	832249.160975	45.804877
3498.391413	831657.962206	45.809882
3498.028508	831025.546489	45.814887
3497.312664	830323.546214	45.819892
3497.124769	829586.785240	45.824897
3496.446200	828796.262944	45.829901
3495.305629	827956.717187	45.834906
3494.798244	827068.637194	45.839911
3493.830384	826138.104460	45.844916
3493.036575	825152.357757	45.849921
3492.339339	824130.836700	45.854925
3491.491424	823053.132355	45.859930
3490.486231	821928.947003	45.864935
3489.102673	820767.730492	45.869940
3488.594982	819549.019358	45.874945
3487.028625	818293.625987	45.879949
3486.326297	816986.913035	45.884954
3485.187719	815641.812035	45.889959
3483.602789	814242.712615	45.894964
3482.597928	812795.460689	45.899969
3481.196110	811316.064391	45.904973
3479.884117	809797.796476	45.909978
3478.735799	808220.578694	45.914983
3477.140029	806608.215533	45.919988
3476.080260	804947.502579	45.924993
3474.323980	803262.018882	45.929997
3473.142275	801504.348408	45.935002
3471.526506	799720.632421	45.940007
3469.867064	797901.071508	45.945012
3468.321947	796027.733114	45.950017
3466.549814	794133.855145	45.955021
3465.040520	792180.241213	45.960026
3463.377083	790186.219229	45.965031
3461.603868	788156.590281	45.970036
3459.829372	786087.637974	45.975041
3457.770876	783989.797140	45.980045
3455.808331	781852.213716	45.985050
3454.369622	779666.019932	45.990055
3451.966479	777463.247270	45.995060
3449.979935	775218.331635	46.000065
3448.077837	772940.944164	46.005069
3446.212117	770623.217761	46.010074
3444.112248	768281.836498	46.015079
3441.924431	765897.963326	46.020084
3440.078891	763474.584151	46.025089
3437.892711	761017.711035	46.030093
3435.349006	758534.930277	46.035098
3433.399218	756009.215479	46.040103
3431.057347	753461.179229	46.045108
3428.940623	750868.429673	46.050113
3426.407776	748264.771319	46.055117
3423.884655	745614.698930	46.060122
3421.881123	742931.330788	46.065127
3419.257391	740231.066599	46.070132
3417.010735	737486.296581	46.075137
3414.382015	734722.872553	46.080141
3411.566109	731939.024335	46.085146
3409.106836	729115.711346	46.090151
3406.544551	726266.142166	46.095156
3404.217942	723383.084444	46.100161
3401.609959	720493.252783	46.105165
3398.859676	717561.405618	46.110170
3396.193348	714595.472951	46.115175
3393.091609	711614.636354	46.120180
3390.537263	708612.007776	46.125185
3387.792520	705577.099179	46.130189
3385.376006	702526.232251	46.135194
3382.973552	699433.404415	46.140199
3379.705429	696327.540094	46.145204
3377.086843	693185.951243	46.150209
3374.157696	690035.820232	46.155213
3370.902153	686845.959575	46.160218
3368.125939	683639.273935	46.165223
3364.884562	680437.190670	46.170228
3362.529163	677186.693495	46.175233
3359.342746	673930.963754	46.180237
3356.590103	670632.398265	46.185242
3353.010607	667334.345367	46.190247
3350.073232	664009.092223	46.195252
3347.257239	660654.362841	46.200257
3343.739194	657295.191817	46.205261
3340.860987	653913.307236	46.210266
3337.527674	650510.858101	46.215271
3334.051012	647091.420521	46.220276
3331.365963	643646.918034	46.225281
3328.085969	640210.950750	46.230285
3324.573943	636745.883090	46.235290
3321.780252	633251.147451	46.240295
3318.706207	629755.824370	46.245300
3315.172154	626218.468273	46.250305
3312.213108	622704.006609	46.255309
3308.729391	619140.658888	46.260314
3305.545404	615576.183689	46.265319
3302.125715	611997.878193	46.270324
3298.838113	608397.481397	46.275329
3295.623837	604798.206072	46.280333
3292.068916	601168.902362	46.285338
3288.739359	597533.494681	46.290343
3285.127480	593890.266857	46.295348
3281.734930	590221.561545	46.300353
3278.220890	586555.133742	46.305357
3275.177946	582879.075816	46.310362
3271.539178	579171.894585	46.315367
3267.924233	575471.451538	46.320372
3264.796488	571744.825882	46.325377
3260.995915	568017.236698	46.330381
3257.714922	564280.727682	46.335386
3254.056295	560531.627519	46.340391
3250.571330	556783.720520	46.345396
3246.949624	553010.180621	46.350401
3243.233787	549247.996323	46.355405
3239.828104	545457.498508	46.360410
3236.246522	541656.863105	46.365415
3232.397837	537873.184263	46.370420
3229.086564	534056.077877	46.375425
3225.593633	530249.096790	46.380429
3222.093432	526433.349557	46.385434
3218.507242	522603.968748	46.390439
3214.866837	518774.207164	46.395444
3211.226172	514925.166993	46.400449
3207.768769	511084.199415	46.405453
3204.199663	507219.091568	46.410458
3200.401503	503350.795155	46.415463
3196.380760	499487.346079	46.420468
3192.542533	495598.563988	46.425473
3188.948528	491715.437218	46.430477
3185.479574	487851.186281	46.435482
3181.531076	483957.842100	46.440487
3177.748209	480082.493026	46.445492
3174.409418	476186.408187	46.450497
3170.353220	472301.720513	46.455501
3166.637685	468400.728846	46.460506
3162.727065	464495.912779	46.465511
3159.158651	460601.315982	46.470516
3155.226400	456685.394225	46.475521
3151.369066	452779.561649	46.480525
3147.651769	448872.186573	46.485530
3143.731579	444957.463306	46.490535
3140.053854	441062.226140	46.495540
3136.098620	437142.309901	46.500545
3132.233276	433231.300228	46.505549
3128.714646	429327.454739	46.510554
3124.468353	425420.215308	46.515559
3120.738893	421510.414477	46.520564
3116.838903	417602.737133	46.525569
3113.481194	413703.427675	46.530573
3109.682902	409779.536195	46.535578
3105.964950	405868.779956	46.540583
3101.889942	401964.399236	46.545588
3097.812369	398053.263149	46.550593
3093.715700	394148.380428	46.555597
3089.610108	390239.867907	46.560602
3086.155532	386333.068690	46.565607
3082.009955	382448.471082	46.570612
3078.002740	378546.404083	46.575617
3074.169221	374661.666169	46.580621
3069.942073	370776.408547	46.585626
3066.292095	366894.812919	46.590631
3062.357469	363017.919556	46.595636
3058.515408	359139.256422	46.600641
3054.289603	355266.536715	46.605645
3050.228963	351402.894123	46.610650
3046.746056	347553.823863	46.615655
3042.202418	343700.634361	46.620660
3038.368988	339854.173446	46.625665
3034.181640	336011.623086	46.630669
3030.332140	332179.604787	46.635674
3026.272481	328343.773923	46.640679
3021.799782	324524.729101	46.645684
3017.950072	320694.927429	46.650689
3013.599999	316895.365683	46.655693
3009.720655	313101.918957	46.660698
3005.983834	309316.511213	46.665703
3001.984760	305535.683665	46.670708
2997.709022	301757.798621	46.675713
2993.628002	297995.980645	46.680717
2989.247574	294243.425371	46.685722
2985.143937	290494.380872	46.690727
2981.486761	286766.679698	46.695732
2977.073375	283036.595331	46.700737
2973.105279	279325.822229	46.705741
2968.581922	275622.081900	46.710746
2964.847492	271928.105742	46.715751
2960.456798	268246.323255	46.720756
2956.062850	264576.620558	46.725761
2951.756639	260919.073270	46.730765
2947.404936	257287.517908	46.735770
2943.664534	253649.676200	46.740775
2939.076157	250029.599370	46.745780
2935.056901	246418.750762	46.750785
2930.654092	242832.368542	46.755789
2926.594971	239259.196359	46.760794
2922.180124	235700.170301	46.765799
2918.102769	232157.129081	46.770804
2913.739732	228620.554110	46.775809
2909.426113	225105.659858	46.780813
2905.024983	221610.237184	46.785818
2901.027339	218102.358052	46.790823
2897.114255	214645.092685	46.795828
2892.610266	211185.683171	46.800833
2888.194246	207737.022285	46.805837
2883.877017	204308.795679	46.810842
2879.734704	200900.236310	46.815847
2875.373416	197500.692879	46.820852
2871.087504	194128.336649	46.825857
2866.713212	190762.420868	46.830861
2862.195633	187415.262377	46.835866
2858.331685	184082.720786	46.840871
2853.902356	180780.832366	46.845876
2849.259103	177481.437721	46.850881
2845.369326	174169.232039	46.855885
2840.987956	170859.454562	46.860890
2837.180488	167608.656743	46.865895
2832.983986	164382.392822	46.870900
2828.273498	161158.183716	46.875905
2824.396512	157966.334535	46.880909
2819.887727	154783.278216	46.885914
2815.838511	151617.911627	46.890919
2811.173259	148477.763118	46.895924
2806.963294	145345.553741	46.900929
2802.671665	142234.250159	46.905933
2798.569315	139133.698702	46.910938
2794.579822	136061.829484	46.915943
2790.208596	133006.190802	46.920948
2785.991512	129948.016222	46.925953
2781.931774	126929.605358	46.930957
2777.700563	123919.414819	46.935962
2773.572759	120910.666188	46.940967
2768.917991	117938.117421	46.945972
2764.496225	114974.092924	46.950977
2760.580513	112026.679082	46.955981
2756.367828	109098.381248	46.960986
2752.160508	106196.183704	46.965991
2747.453621	103305.978945	46.970996
2743.658008	100433.535841	46.976001
2739.658395	97576.996577	46.981005
2735.309466	94735.597571	46.986010
2731.664139	91893.050680	46.991015
2726.911915	89098.536816	46.996020
2722.860227	86302.014365	47.001025
2718.588751	83519.118641	47.006029
2713.986537	80769.988627	47.011034
2709.706912	78031.821098	47.016039
2705.732309	75303.172945	47.021044
2701.141917	72606.983930	47.026049
2696.825972	69930.146310	47.031053
2692.525035	67274.895951	47.036058
2688.539346	64626.039505	47.041063
2683.928083	62000.634015	47.046068
2679.888582	59397.328139	47.051073
2675.420943	56810.514252	47.056077
2670.869879	54245.631925	47.061082
2666.405499	51708.557892	47.066087
2662.206954	49188.793058	47.071092
2657.623479	46698.329749	47.076097
2652.945758	44213.202022	47.081101
2648.503223	41761.445093	47.086106
2644.112895	39321.205991	47.091111
2640.034893	36924.319722	47.096116
2635.021123	34538.692582	47.101121
2630.818018	32186.520251	47.106125
2625.728296	29855.214095	47.111130
2621.509777	27551.827169	47.116135
2616.378522	25284.254600	47.121140
2611.669967	23039.189564	47.126145
2607.542432	20831.115501	47.131149
2602.034340	18646.280786	47.136154
2596.878618	16496.806849	47.141159
2591.824319	14402.123802	47.146164
2585.956475	12346.896619	47.151169
2580.079513	10355.535397	47.156173
2571.188447	8461.161325	47.161178
2560.359991	6709.844740	47.166183
2548.683676	5063.478361	47.171188
2535.642875	3588.446736	47.176193
2522.847945	2260.310905	47.181197
2509.607098	1121.903274	47.186202
2492.846265	246.125570	47.191207
2452.884541	201.504602	47.196212
2425.899142	207.311207	47.201217
2415.669297	206.725311	47.206221
2417.123242	230.293540	47.211226
2424.536079	217.025701	47.216231
2433.125278	231.318044	47.221236
2439.235664	230.514059	47.226241
2442.395305	227.820902	47.231245
2442.680708	234.993135	47.236250
2441.152666	217.587152	47.241255
2437.713077	221.621359	47.246260
2434.638731	208.348876	47.251265
2431.557179	206.103695	47.256269
2427.927631	218.634199	47.261274
2425.216850	208.051106	47.266279
2422.140506	210.421232	47.271284
2418.911066	207.284824	47.276289
2416.403823	197.163467	47.281293
2413.253111	192.195511	47.286298
2410.515599	191.152582	47.291303
2407.461310	199.328163	47.296308
2404.273803	192.657464	47.301313
2401.107770	186.552910	47.306317
2398.154273	194.007176	47.311322
2394.618367	200.122477	47.316327
2391.737783	194.789552	47.321332
2388.049957	195.818939	47.326337
2385.054541	194.553760	47.331341
2381.714038	196.696289	47.336346
2378.539733	193.902463	47.341351
2375.330253	195.559405	47.346356
2372.014940	192.771821	47.351361
2368.617044	184.200916	47.356365
2365.401374	197.663296	47.361370
2362.141309	195.819402	47.366375
2359.004024	193.358327	47.371380
2355.075654	203.407638	47.376385
2351.937171	193.995687	47.381389
2347.737432	199.208736	47.386394
2344.724096	188.014926	47.391399
2341.934848	190.596431	47.396404
2338.638576	183.740286	47.401409
2335.347050	189.194082	47.406413
2331.540394	187.593904	47.411418
2328.027907	188.975546	47.416423
2325.069329	189.482725	47.421428
2320.717051	190.040257	47.426433
2318.221910	189.241019	47.431437
2314.555860	196.094903	47.436442
2311.138643	176.757175	47.441447
2307.851025	189.120292	47.446452
2303.792256	192.735684	47.451457
2300.988092	186.273981	47.456461
2297.547493	192.431346	47.461466
2294.155450	186.646936	47.466471
2290.399331	193.049826	47.471476
2287.120004	188.592436	47.476481
2283.764945	182.941456	47.481485
2280.094232	185.534323	47.486490
2276.849976	187.190405	47.491495
2273.726791	185.473827	47.496500
2270.069867	191.206279	47.501505
2267.221701	182.065334	47.506509
2263.316825	188.811055	47.511514
2259.524133	184.383369	47.516519
2256.475575	185.784203	47.521524
2252.466920	186.560095	47.526529
2249.305179	181.521152	47.531533
2245.448828	189.056585	47.536538
2242.785057	181.013142	47.541543
2239.159361	186.949532	47.546548
2235.535715	185.001204	47.551553
2231.903630	184.867103	47.556557
2227.948119	191.769460	47.561562
2225.029682	183.284955	47.566567
2221.719303	176.108345	47.571572
2217.821906	186.026282	47.576577
2214.811366	181.549013	47.581581
2211.089110	181.118966	47.586586
2207.922228	178.032957	47.591591
2204.716464	181.227010	47.596596
2201.110748	175.811439	47.601601
2197.335382	174.060877	47.606605
2193.270181	185.587015	47.611610
2190.046770	174.625463	47.616615
2186.917348	172.716892	47.621620
2183.325164	177.705215	47.626625
2179.998750	176.555160	47.631629
2176.749488	183.862744	47.636634
2173.445214	175.505069	47.641639
2169.596097	169.118317	47.646644
2165.855059	172.250589	47.651649
2162.549301	168.063147	47.656653
2158.899785	174.028593	47.661658
2154.817433	167.529637	47.666663
2152.036975	180.424056	47.671668
2148.557216	174.238958	47.676673
2145.568732	170.523921	47.681677
2141.894433	175.458662	47.686682
2137.978316	173.233414	47.691687
2134.891545	169.068669	47.696692
2131.066665	173.267641	47.701697
2128.191544	158.407517	47.706701
2124.399107	162.139488	47.711706
2120.597243	176.620629	47.716711
2117.576154	170.816214	47.721716
2113.487369	180.488864	47.726721
2110.045660	174.905293	47.731725
2106.796121	182.712828	47.736730
2102.904510	171.783093	47.741735
2099.725126	174.346598	47.746740
2096.425304	175.068588	47.751745
2093.012707	166.006532	47.756749
2089.142202	173.632808	47.761754
2086.103640	167.676108	47.766759
2082.699213	166.449702	47.771764
2078.784981	167.388059	47.776769
2075.691180	163.816079	47.781773
2071.589300	173.965368	47.786778
2068.545626	163.991352	47.791783
2065.058778	173.829267	47.796788
2061.218033	172.367405	47.801793
2058.077476	160.073614	47.806797
2054.598182	171.618840	47.811802
2051.045277	168.371813	47.816807
2047.972619	170.567441	47.821812
2043.695052	171.192488	47.826817
2040.466297	176.725123	47.831821
2036.930602	171.602391	47.836826
2033.661117	171.240772	47.841831
2030.176285	163.012653	47.846836
2026.472659	169.442200	47.851841
2023.230516	164.994907	47.856845
2019.658629	170.847001	47.861850
2015.944950	170.874442	47.866855
2012.736828	168.918125	47.871860
2008.867529	164.034276	47.876865
2005.610192	162.338773	47.881869
2002.035350	165.157179	47.886874
1998.689098	173.343715	47.891879
1995.012655	163.335856	47.896884
1991.153616	165.879183	47.901889
1988.244743	161.189922	47.906893
1984.443395	169.071170	47.911898
1981.484429	171.144619	47.916903
1977.688015	161.598483	47.921908
1974.277775	166.789356	47.926913
1970.925944	159.271307	47.931917
1967.325569	167.519759	47.936922
1963.590209	171.999017	47.941927
1960.333607	162.852493	47.946932
1956.326422	159.195677	47.951937
1953.228707	154.871349	47.956941
1949.746922	167.014958	47.961946
1946.183968	163.095636	47.966951
1943.249505	161.422400	47.971956
1939.469891	160.802100	47.976961
1935.741178	155.567241	47.981965
1931.808108	155.379097	47.986970
1928.683318	152.631457	47.991975
1925.302849	156.172471	47.996980
1921.688790	171.234891	48.001985
1918.404956	156.752032	48.006989
1914.616312	153.415391	48.011994
1911.507580	163.244790	48.016999
1908.035334	155.508319	48.022004
1903.997485	154.504483	48.027009
1900.999432	147.753711	48.032013
1897.392157	155.705853	48.037018
1893.597146	164.554277	48.042023
1890.258682	155.806586	48.047028
1886.519588	162.232230	48.052033
1883.181545	158.065759	48.057037
1879.500854	157.088303	48.062042
1876.207436	150.086355	48.067047
1872.815007	155.828143	48.072052
1869.730143	152.495287	48.077057
1866.132688	150.100054	48.082061
1862.191029	158.844879	48.087066
1858.586794	158.570500	48.092071
1855.208434	150.164439	48.097076
1851.539935	166.918568	48.102081
1848.189729	152.667600	48.107085
1844.918500	152.932758	48.112090
1841.380310	158.874542	48.117095
1838.003725	155.694918	48.122100
1834.247380	151.695169	48.127105
1831.101676	156.841518	48.132109
1827.226412	155.783795	48.137114
1823.320070	162.460264	48.142119
1820.209529	155.198754	48.147124
1816.548547	153.800607	48.152129
1813.385919	150.451464	48.157133
1809.806203	161.692904	48.162138
1806.294342	157.284733	48.167143
1803.080160	149.536395	48.172148
1799.407582	152.006313	48.177153
1796.008329	154.803630	48.182157
1792.617455	160.437627	48.187162
1788.867037	155.291648	48.192167
1785.480961	148.959155	48.197172
1781.881109	152.926861	48.202177
1778.153159	142.189989	48.207181
1774.641279	159.653632	48.212186
1771.215555	151.251852	48.217191
1767.855348	153.926005	48.222196
1764.161599	144.984025	48.227201
1760.626645	145.856813	48.232205
1757.453721	158.284328	48.237210
1753.992845	159.275244	48.242215
1750.483009	150.943586	48.247220
1746.826356	154.992961	48.252225
1743.322737	156.110796	48.257229
1739.837516	158.640001	48.262234
1736.191598	160.634352	48.267239
1732.905715	154.289361	48.272244
1729.207083	155.472523	48.277249
1725.828474	156.469556	48.282253
1722.132974	151.637725	48.287258
1718.411497	152.577685	48.292263
1715.486840	143.670392	48.297268
1711.882255	156.029425	48.302273
1708.225297	156.402450	48.307277
1705.044978	160.959444	48.312282
1701.493712	148.834489	48.317287
1698.263397	149.719735	48.322292
1694.279888	151.051900	48.327297
1690.768122	146.843084	48.332301
1686.974161	148.022196	48.337306
1683.303228	154.709323	48.342311
1680.356516	144.153958	48.347316
1676.887626	150.293756	48.352321
1673.324456	143.890944	48.357325
1669.847684	149.582709	48.362330
1666.255316	143.829897	48.367335
1662.982858	145.275425	48.372340
1659.011637	155.388560	48.377345
1655.763702	150.417104	48.382349
1652.094430	143.189319	48.387354
1648.959115	148.568213	48.392359
1645.582195	150.928632	48.397364
1641.492445	149.977317	48.402369
1638.357617	141.719900	48.407373
1635.132453	145.492962	48.412378
1631.225899	148.464642	48.417383
1627.905133	141.191816	48.422388
1624.069861	147.230777	48.427393
1620.610461	150.958244	48.432397
1617.260555	143.465348	48.437402
1613.439323	149.068667	48.442407
1610.105301	144.211946	48.447412
1606.478201	144.219655	48.452417
1603.348624	140.783151	48.457421
1599.887484	146.080170	48.462426
1596.609177	150.048229	48.467431
1592.885307	149.409842	48.472436
1589.406018	156.747233	48.477441
1585.612465	144.340705	48.482445
1582.142007	145.070576	48.487450
1578.353947	151.355273	48.492455
1575.605711	141.699060	48.497460
1572.061163	152.102954	48.502465
1568.384434	135.476552	48.507469
1564.629957	144.726856	48.512474
1561.062437	147.816345	48.517479
1557.834451	140.585974	48.522484
1554.182846	146.871466	48.527489
1551.049167	146.286257	48.532493
1547.424024	146.157634	48.537498
1543.869312	146.707711	48.542503
1540.574591	136.823825	48.547508
1536.421547	148.942862	48.552513
1533.047480	144.038652	48.557517
1529.687745	133.500539	48.562522
1526.110649	141.802408	48.567527
1522.855412	135.671012	48.572532
1518.990527	146.412967	48.577537
1515.827800	139.254659	48.582541
1512.103125	143.539388	48.587546
1508.638489	132.906968	48.592551
1505.615548	132.294950	48.597556
1501.344396	136.000807	48.602561
1498.293598	135.972136	48.607565
1495.091219	136.976462	48.612570
1491.377057	136.108796	48.617575
1487.694497	130.104415	48.622580
1483.977641	136.618444	48.627585
1480.996657	141.435368	48.632589
1477.414010	139.594801	48.637594
1473.457060	136.854176	48.642599
1470.182204	133.133565	48.647604
1466.909571	137.173540	48.652609
1463.260826	135.302195	48.657613
1459.558447	143.130132	48.662618
1456.231087	142.837869	48.667623
1452.799169	132.175042	48.672628
1449.080780	139.543564	48.677633
1446.047927	141.033914	48.682637
1442.206705	137.553828	48.687642
1438.383182	146.362546	48.692647
1435.385629	139.808021	48.697652
1431.427290	145.334780	48.702657
1428.186673	132.810148	48.707661
1424.802725	137.781913	48.712666
1420.748483	134.110547	48.717671
1417.530765	138.360247	48.722676
1414.176929	127.536516	48.727681
1410.903393	142.061654	48.732685
1407.166033	132.256605	48.737690
1403.706565	130.779612	48.742695
1400.038111	132.084719	48.747700
1396.686277	135.542308	48.752705
1393.227544	141.588843	48.757709
1389.679911	133.247441	48.762714
1386.164609	136.854011	48.767719
1382.764664	133.273239	48.772724
1379.242840	134.602859	48.777729
1375.988037	136.096333	48.782733
1372.167124	138.235262	48.787738
1368.466669	137.251598	48.792743
1365.132893	131.540695	48.797748
1361.451769	131.465197	48.802753
1358.420700	128.924548	48.807757
1354.579829	134.470910	48.812762
1350.700237	135.511684	48.817767
1348.035584	128.458980	48.822772
1344.311315	136.651054	48.827777
1340.633825	129.617690	48.832781
1336.491735	132.990187	48.837786
1333.335106	141.666066	48.842791
1330.114155	128.739756	48.847796
1326.728493	127.380956	48.852801
1323.377602	126.143268	48.857805
1319.555268	128.314076	48.862810
1316.464705	134.970570	48.867815
1312.575972	129.371871	48.872820
1308.887351	136.226396	48.877825
1305.758325	132.438722	48.882829
1302.424874	134.150181	48.887834
1298.767429	135.599139	48.892839
1295.348465	131.897986	48.897844
1291.574448	130.906885	48.902849
1288.103833	132.266487	48.907853
1284.358692	129.938888	48.912858
1280.763543	125.347807	48.917863
1277.304094	130.220698	48.922868
1273.906859	136.896738	48.927873
1270.555288	127.072492	48.932877
1267.147009	119.778715	48.937882
1263.508090	129.479259	48.942887
1260.248378	118.523804	48.947892
1256.684239	131.354343	48.952897
1252.956556	133.687534	48.957901
1249.655472	134.555524	48.962906
1246.083646	127.714474	48.967911
1242.846942	125.275660	48.972916
1238.956462	129.402931	48.977921
1235.424696	124.428613	48.982925
1232.187996	133.974450	48.987930
1228.203887	137.929718	48.992935
1224.958932	127.509816	48.997940
1221.651857	123.553889	49.002945
1217.797236	121.101085	49.007949
1214.550108	129.604488	49.012954
1210.946581	134.711934	49.017959
1207.686002	126.294038	49.022964
1204.274060	129.273863	49.027969
1200.780315	127.163213	49.032973
1196.980471	123.439468	49.037978
1193.318305	136.348649	49.042983
1189.980600	127.756166	49.047988
1186.232067	134.487227	49.052993
1182.888693	129.692249	49.057997
1179.849483	125.374853	49.063002
1175.838615	142.138411	49.068007
1172.518992	130.758918	49.073012
1169.102013	142.822945	49.078017
1165.391842	136.183924	49.083021
1162.013517	132.473296	49.088026
1158.338768	136.399140	49.093031
1154.702373	134.968920	49.098036
1151.276569	141.535570	49.103041
1148.035992	130.836595	49.108045
1144.968641	132.038197	49.113050
1140.871755	132.287308	49.118055
1137.658616	130.490265	49.123060
1134.117529	136.853499	49.128065
1130.391045	133.032870	49.133069
1126.731016	130.663536	49.138074
1123.359129	137.360961	49.143079
1120.216252	134.986595	49.148084
1116.076258	135.267777	49.153089
1112.759365	144.101683	49.158093
1109.416584	129.729684	49.163098
1105.959030	142.189231	49.168103
1102.752017	128.802082	49.173108
1099.269643	129.416923	49.178113
1095.364799	132.328417	49.183117
1092.063316	137.768275	49.188122
1088.122173	133.291553	49.193127
1084.919174	131.856783	49.198132
1081.252813	135.578855	49.203137
1077.628780	132.014299	49.208141
1074.589006	128.064034	49.213146
1071.166702	125.996034	49.218151
1067.514277	125.637737	49.223156
1064.015849	123.319059	49.228161
1060.430976	127.471316	49.233165
1057.057033	122.345808	49.238170
1053.368171	122.024859	49.243175
1049.893700	116.282328	49.248180
1046.229620	128.780543	49.253185
1042.565214	127.392719	49.258189
1039.391528	119.666827	49.263194
1035.875954	131.464734	49.268199
1032.589188	120.178246	49.273204
1028.835405	130.659328	49.278209
1025.355226	121.639960	49.283213
1022.015989	128.066537	49.288218
1018.407063	123.996591	49.293223
1014.754327	115.368090	49.298228
1011.233121	128.495696	49.303233
1007.918024	122.905400	49.308237
1004.518332	124.434334	49.313242
1000.982160	128.164523	49.318247
997.562567	118.831954	49.323252
993.946221	125.295598	49.328257
989.873861	127.404435	49.333261
986.887568	123.483794	49.338266
983.307289	119.434690	49.343271
979.972998	122.522655	49.348276
975.864453	120.796263	49.353281
972.786892	126.887646	49.358285
969.684897	124.582866	49.363290
965.850438	127.527682	49.368295
962.431092	115.433061	49.373300
958.437337	123.737049	49.378305
955.228806	115.880603	49.383309
951.921899	114.712094	49.388314
948.234634	123.629338	49.393319
944.515393	116.428681	49.398324
940.997786	121.336093	49.403329
937.989677	121.952664	49.408333
934.770729	115.312771	49.413338
931.017810	122.063581	49.418343
927.350794	114.955998	49.423348
923.411040	125.719335	49.428353
919.951029	109.293486	49.433357
916.908673	112.202878	49.438362
913.346778	123.001966	49.443367
910.139580	120.805432	49.448372
906.518490	121.758445	49.453377
902.777114	117.677651	49.458381
899.352854	117.109681	49.463386
895.451982	121.463337	49.468391
891.658882	121.658659	49.473396
888.715088	121.847549	49.478401
885.366576	119.840834	49.483405
881.857074	117.055715	49.488410
878.458487	131.799859	49.493415
874.734985	117.579348	49.498420
871.113970	115.767173	49.503425
867.489485	114.129553	49.508429
864.476992	111.472267	49.513434
860.773602	120.471158	49.518439
857.270889	113.151213	49.523444
853.865777	119.787474	49.528449
850.036643	124.648783	49.533453
846.982949	120.868463	49.538458
843.309147	123.050995	49.543463
839.909438	121.938187	49.548468
836.137611	124.335393	49.553473
832.467065	130.741138	49.558477
829.029011	119.200014	49.563482
825.323856	121.390626	49.568487
821.947757	116.325664	49.573492
818.674841	115.303744	49.578497
815.710593	115.002302	49.583501
811.852859	113.008915	49.588506
807.690575	120.004208	49.593511
804.723634	115.068177	49.598516
801.250128	124.961257	49.603521
797.535886	120.923716	49.608525
794.779632	116.315373	49.613530
790.843909	122.449435	49.618535
787.127958	119.196797	49.623540
783.527889	113.964439	49.628545
780.185988	115.149034	49.633549
776.775679	107.204038	49.638554
772.964133	119.016718	49.643559
769.760726	121.448326	49.648564
766.135398	120.826469	49.653569
762.204491	123.615619	49.658573
759.229454	118.547990	49.663578
755.424198	125.768976	49.668583
752.451210	112.497217	49.673588
748.632692	113.326179	49.678593
745.216243	112.700095	49.683597
741.417547	108.622022	49.688602
737.938732	116.234826	49.693607
734.544039	115.966016	49.698612
731.122822	111.139118	49.703617
727.340194	115.085168	49.708621
724.036544	105.810504	49.713626
720.424379	107.214617	49.718631
717.411839	107.322576	49.723636
713.893576	118.428105	49.728641
709.995576	114.726272	49.733645
706.544592	107.819084	49.738650
702.745578	118.329490	49.743655
699.376956	111.466354	49.748660
696.120267	113.412772	49.753665
692.372666	116.666800	49.758669
689.181928	114.413983	49.763674
685.541100	114.968366	49.768679
682.010730	118.672444	49.773684
678.756736	118.805572	49.778689
674.711524	121.944860	49.783693
671.343937	108.355276	49.788698
667.635145	120.607489	49.793703
664.877168	115.259124	49.798708
661.113295	118.635937	49.803713
657.397842	117.031632	49.808717
654.310073	113.617397	49.813722
650.891977	118.202430	49.818727
647.309458	114.185457	49.823732
643.577514	115.934233	49.828737
640.053912	120.064382	49.833741
636.831439	114.921653	49.838746
632.841555	113.714686	49.843751
629.573439	114.413204	49.848756
626.361228	117.928266	49.853761
622.540237	119.890318	49.858765
619.368802	110.958830	49.863770
615.624692	117.417296	49.868775
611.781063	113.406429	49.873780
608.202144	112.628667	49.878785
604.560017	115.280902	49.883789
601.493023	117.577302	49.888794
598.011276	122.128029	49.893799
594.160464	114.220460	49.898804
591.089447	119.285842	49.903809
587.486877	114.038142	49.908813
584.011389	107.419590	49.913818
580.161546	117.482405	49.918823
576.937574	112.532928	49.923828
573.558780	116.045622	49.928833
570.166229	121.363853	49.933837
566.402411	110.978055	49.938842
562.852342	107.924167	49.943847
559.748711	110.751513	49.948852
555.492732	105.558709	49.953857
552.543976	110.016480	49.958861
549.145298	107.644420	49.963866
545.370176	116.357246	49.968871
541.811466	105.945667	49.973876
538.372096	113.457440	49.978881
534.736433	108.309864	49.983885
531.681917	109.740608	49.988890
527.990533	112.574596	49.993895
524.243468	113.307036	49.998900
520.862025	109.701561	50.003905
517.363862	110.309597	50.008909
514.281443	112.573638	50.013914
510.198852	111.068028	50.018919
506.655583	108.035246	50.023924
503.317149	107.213533	50.028929
499.588118	110.667209	50.033933
496.598050	107.329482	50.038938
492.770244	119.714285	50.043943
489.207365	114.359170	50.048948
485.872780	107.715428	50.053953
482.477153	115.283645	50.058957
479.047330	104.029316	50.063962
475.690020	114.353549	50.068967
472.202863	111.315156	50.073972
468.261197	111.454826	50.078977
464.713625	117.445955	50.083981
461.313602	112.160260	50.088986
457.855350	113.543531	50.093991
453.983147	110.609749	50.098996
450.557255	106.027316	50.104001
446.709545	114.178893	50.109005
443.960973	107.528804	50.114010
440.256159	118.970523	50.119015
436.778234	112.906085	50.124020
433.840679	105.358602	50.129025
429.821934	111.505801	50.134029
426.572402	100.185295	50.139034
422.543709	115.771729	50.144039
419.159277	112.790035	50.149044
415.662668	105.912269	50.154049
412.253207	113.444708	50.159053
409.257709	105.751284	50.164058
405.510330	111.802202	50.169063
402.023921	106.938198	50.174068
398.779335	110.505861	50.179073
394.229867	117.153831	50.184077
390.916417	105.618718	50.189082
387.585761	116.138122	50.194087
384.338895	109.259216	50.199092
381.159248	112.740781	50.204097
377.231749	115.039161	50.209101
373.642683	105.581565	50.214106
370.153449	116.091011	50.219111
366.572279	111.953724	50.224116
363.354842	106.455970	50.229121
359.679594	116.592753	50.234125
356.150872	113.273011	50.239130
352.830246	106.620812	50.244135
348.981150	109.729515	50.249140
345.595597	109.570153	50.254145
342.215911	112.627476	50.259149
339.205570	100.415311	50.264154
335.318392	111.221224	50.269159
331.724808	100.932274	50.274164
328.501131	103.031837	50.279169
324.639982	110.128846	50.284173
321.425482	104.636978	50.289178
317.337283	104.663625	50.294183
314.239292	101.732021	50.299188
310.759377	103.650261	50.304193
307.380738	104.730047	50.309197
303.672575	92.513318	50.314202
299.964484	104.578857	50.319207
296.553040	101.149021	50.324212
293.398725	102.563838	50.329217
289.724448	94.663579	50.334221
286.325325	96.173696	50.339226
282.492336	106.835091	50.344231
278.828391	101.669916	50.349236
275.687712	100.232006	50.354241
271.705396	103.978552	50.359245
268.914475	99.442266	50.364250
265.549514	97.159954	50.369255
261.740759	98.838655	50.374260
258.262414	100.544694	50.379265
254.450873	99.265669	50.384269
251.026888	98.862423	50.389274
247.633760	101.747874	50.394279
243.903685	98.225604	50.399284
240.887453	97.796451	50.404289
237.219099	98.273066	50.409293
233.665796	98.658892	50.414298
230.183943	103.861505	50.419303
226.354492	99.962497	50.424308
223.327355	96.747740	50.429313
219.856949	101.119644	50.434317
216.273738	87.836168	50.439322
212.638128	98.283160	50.444327
209.298771	87.963945	50.449332
205.967409	87.761346	50.454337
201.646174	103.276608	50.459341
198.284233	101.768983	50.464346
194.662106	99.878171	50.469351
191.339189	99.604650	50.474356
188.038909	95.407622	50.479361
184.232119	108.614979	50.484365
181.417615	101.753852	50.489370
177.273521	105.772560	50.494375
173.813865	110.459179	50.499380
170.551317	99.039590	50.504385
166.939619	103.300768	50.509389
163.736169	109.212777	50.514394
160.032703	106.771562	50.519399
156.418516	114.250734	50.524404
152.840815	96.562394	50.529409
149.266913	109.204921	50.534413
146.291191	104.533111	50.539418
142.925580	113.124971	50.544423
139.201812	101.613134	50.549428
135.556719	103.601613	50.554433
131.914442	105.247960	50.559437
128.951992	99.254769	50.564442
125.039333	98.678191	50.569447
121.258076	103.415212	50.574452
118.198264	102.451918	50.579457
114.550639	97.619628	50.584461
110.850712	96.617415	50.589466
107.319809	101.868885	50.594471
103.893344	93.740064	50.599476
100.549186	99.525436	50.604481
96.746813	107.508680	50.609485
93.557372	103.585395	50.614490
90.070999	105.197842	50.619495
86.217129	111.176977	50.624500
83.077643	103.430314	50.629505
79.242997	104.512025	50.634509
76.371437	94.575166	50.639514
72.745556	102.125798	50.644519
69.267718	106.729880	50.649524
65.289210	99.646199	50.654529
61.622681	99.182951	50.659533
58.583637	92.249484	50.664538
54.833400	93.324309	50.669543
51.442592	103.726675	50.674548
48.198254	97.967510	50.679553
44.263938	108.954917	50.684557
40.853455	99.409396	50.689562
37.180272	103.515739	50.694567
33.788668	101.313627	50.699572
30.604093	95.083191	50.704577
26.918690	108.777789	50.709581
23.448568	100.440704	50.714586
20.003698	94.301677	50.719591
16.001636	97.924872	50.724596
12.980155	93.342545	50.729601
9.258147	99.155511	50.734605
5.720549	95.074838	50.739610
2.624458	97.765139	50.744615