Tue Jun 08 16:55:41 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
-0.357988	102.947142	0.000000
-0.245467	93.679855	0.005005
-1.308381	57.691784	0.010010
-3.320366	34.396923	0.015014
-7.161366	17.115275	0.020019
-12.559126	19.304278	0.025024
-17.396135	14.398578	0.030029
-21.770429	25.660903	0.035034
-26.149598	24.997576	0.040038
-29.341316	21.849240	0.045043
-33.165346	30.536095	0.050048
-36.669087	25.451541	0.055053
-40.356044	16.401991	0.060058
-44.397452	19.187746	0.065062
-47.725687	13.595910	0.070067
-51.639573	15.994306	0.075072
-55.449243	21.251861	0.080077
-59.427735	14.515966	0.085082
-63.555538	24.041975	0.090086
-66.783311	16.884883	0.095091
-70.596748	18.786897	0.100096
-74.131134	21.083532	0.105101
-77.590063	28.897086	0.110106
-81.924537	34.228865	0.115110
-85.801479	26.870884	0.120115
-89.821281	23.791961	0.125120
-93.531034	20.716319	0.130125
-97.094262	21.467900	0.135130
-100.898335	24.269055	0.140134
-104.238635	27.796681	0.145139
-108.197650	33.202248	0.150144
-112.118317	23.422365	0.155149
-115.508620	17.817937	0.160154
-119.577930	20.600253	0.165158
-123.232856	17.802187	0.170163
-127.069318	24.608488	0.175168
-130.806653	23.074992	0.180173
-134.737486	18.645954	0.185178
-138.397270	27.538387	0.190182
-141.841474	23.018010	0.195187
-145.834251	29.214864	0.200192
-149.519246	24.648950	0.205197
-153.302318	21.043209	0.210202
-157.346514	22.903557	0.215206
-160.899066	15.273723	0.220211
-164.999390	15.333181	0.225216
-168.489756	7.547046	0.230221
-172.148333	13.809358	0.235226
-176.432605	23.352423	0.240230
-180.144917	24.181342	0.245235
-184.034101	22.215678	0.250240
-187.385440	25.826958	0.255245
-191.249233	22.019189	0.260250
-194.948541	27.252006	0.265254
-198.112809	22.143313	0.270259
-201.949155	28.172869	0.275264
-206.045879	28.445282	0.280269
-210.019805	26.896380	0.285274
-213.778139	27.757297	0.290278
-217.468976	25.693702	0.295283
-221.294344	27.883259	0.300288
-224.812916	20.589072	0.305293
-228.312785	19.841449	0.310298
-232.258827	25.651833	0.315302
-236.133215	20.327484	0.320307
-239.946915	21.433558	0.325312
-243.547168	21.429424	0.330317
-247.573779	16.849956	0.335322
-251.528054	26.890657	0.340326
-255.304488	16.399391	0.345331
-258.938307	23.103147	0.350336
-262.908390	19.868236	0.355341
-266.717505	18.141920	0.360346
-270.385654	18.552843	0.365350
-273.549817	15.769014	0.370355
-277.721827	21.149673	0.375360
-281.019694	17.696465	0.380365
-284.830561	18.931949	0.385370
-288.702759	22.341737	0.390374
-292.572293	19.937832	0.395379
-296.303313	23.677464	0.400384
-300.146358	12.017102	0.405389
-303.557710	19.203744	0.410394
-307.677426	17.589944	0.415398
-311.685307	20.772386	0.420403
-315.319416	22.756727	0.425408
-319.135228	15.135480	0.430413
-322.556791	10.325208	0.435418
-326.318284	18.530271	0.440422
-330.322041	7.853487	0.445427
-334.110249	13.444260	0.450432
-337.646156	18.168009	0.455437
-341.402068	15.245751	0.460442
-345.514922	15.172532	0.465446
-349.036101	14.205651	0.470451
-352.916309	12.883154	0.475456
-356.381911	14.647980	0.480461
-360.039002	14.043474	0.485466
-364.586862	12.058335	0.490470
-368.097519	11.059667	0.495475
-372.133061	19.470051	0.500480
-375.351933	17.405363	0.505485
-379.028445	10.843747	0.510490
-382.955674	23.501940	0.515494
-386.730970	19.628250	0.520499
-390.640504	18.818408	0.525504
-394.346489	13.446768	0.530509
-397.856736	11.186573	0.535514
-402.019134	16.275187	0.540518
-405.033847	23.145985	0.545523
-408.755567	22.664307	0.550528
-412.715579	13.086460	0.555533
-416.651323	13.084364	0.560538
-420.863980	17.608109	0.565542
-424.226674	16.627125	0.570547
-428.306130	13.025504	0.575552
-432.370461	17.245152	0.580557
-435.788258	18.862901	0.585562
-439.690106	22.493805	0.590566
-443.089147	10.258113	0.595571
-446.867362	19.570917	0.600576
-450.265507	16.714077	0.605581
-454.207064	9.984857	0.610586
-458.225547	19.925422	0.615590
-461.774795	12.862873	0.620595
-465.770836	14.879428	0.625600
-469.521145	16.140201	0.630605
-472.771665	12.967551	0.635610
-477.176635	21.493501	0.640614
-480.746634	11.133211	0.645619
-484.351163	14.986673	0.650624
-488.653880	13.651921	0.655629
-491.947465	14.830014	0.660634
-496.296661	22.428723	0.665638
-499.374325	18.988822	0.670643
-503.447703	16.626000	0.675648
-507.147120	19.139552	0.680653
-510.340024	13.865895	0.685658
-514.337372	9.766360	0.690662
-518.055965	6.992975	0.695667
-522.160630	10.699003	0.700672
-526.652616	9.445310	0.705677
-529.984762	5.873453	0.710682
-533.718719	18.315846	0.715686
-536.403063	8.735554	0.720691
-540.724752	14.954427	0.725696
-544.816929	13.647154	0.730701
-548.473477	8.964616	0.735706
-552.633939	14.303273	0.740710
-556.091835	9.759539	0.745715
-560.250112	20.036777	0.750720
-563.268411	23.646045	0.755725
-566.950404	19.297465	0.760730
-570.904258	27.461517	0.765734
-574.579383	14.875053	0.770739
-578.494386	12.837205	0.775744
-582.435598	20.727537	0.780749
-586.091677	13.734740	0.785754
-589.900043	20.516056	0.790758
-593.499783	15.626850	0.795763
-597.097732	16.417938	0.800768
-601.208762	12.056173	0.805773
-604.940998	13.188046	0.810778
-609.392036	22.054363	0.815782
-612.846426	20.370105	0.820787
-615.992970	21.154010	0.825792
-619.635839	12.781061	0.830797
-623.625411	13.644896	0.835802
-627.614059	25.666890	0.840806
-630.922315	18.587213	0.845811
-635.204990	19.088886	0.850816
-638.817958	15.060868	0.855821
-642.380913	14.290850	0.860826
-646.045896	15.172027	0.865830
-650.015183	21.273693	0.870835
-653.898621	20.900493	0.875840
-657.747607	18.104212	0.880845
-661.375303	18.688105	0.885850
-665.288286	20.535859	0.890854
-668.739385	18.189557	0.895859
-672.386667	17.002622	0.900864
-676.221929	16.975621	0.905869
-680.055360	15.262918	0.910874
-684.010610	18.837276	0.915878
-687.734625	17.995864	0.920883
-691.339893	15.505130	0.925888
-695.283429	21.782794	0.930893
-698.860126	16.334771	0.935898
-702.768424	20.708260	0.940902
-706.349250	19.219051	0.945907
-710.515140	22.603810	0.950912
-714.270530	17.730764	0.955917
-717.607881	10.946658	0.960922
-721.798660	13.672988	0.965926
-725.134401	18.993413	0.970931
-729.057181	22.087804	0.975936
-732.859198	25.852995	0.980941
-736.337968	15.750418	0.985946
-739.998143	18.886585	0.990950
-744.210154	18.078843	0.995955
-747.880571	20.463282	1.000960
-751.547311	22.171755	1.005965
-754.969082	12.801854	1.010970
-759.242691	25.459387	1.015974
-762.641536	14.984331	1.020979
-766.840443	19.053304	1.025984
-770.749138	21.397743	1.030989
-774.003362	12.504325	1.035994
-777.894608	20.147050	1.040998
-781.698417	23.895222	1.046003
-785.478131	19.248634	1.051008
-789.311788	19.529326	1.056013
-793.023853	19.152099	1.061018
-796.985083	21.931858	1.066022
-800.648899	15.473830	1.071027
-804.233566	21.143721	1.076032
-807.901362	18.737233	1.081037
-811.719484	18.846345	1.086042
-815.694005	16.068202	1.091046
-818.905067	9.251455	1.096051
-823.211993	19.295500	1.101056
-827.388865	25.709634	1.106061
-830.238370	15.574130	1.111066
-834.228325	17.794819	1.116070
-837.888653	13.040955	1.121075
-841.951433	20.051650	1.126080
-845.570986	16.707781	1.131085
-849.096902	18.438343	1.136090
-853.291710	17.121349	1.141094
-856.620852	7.291996	1.146099
-860.678015	11.901151	1.151104
-864.870135	20.310005	1.156109
-868.349848	12.726714	1.161114
-872.030360	11.436715	1.166118
-875.841375	9.092369	1.171123
-879.382018	8.391344	1.176128
-883.274339	15.430440	1.181133
-886.994395	8.161953	1.186138
-891.079144	21.719862	1.191142
-894.429902	19.443750	1.196147
-897.919213	21.007422	1.201152
-902.295587	19.344702	1.206157
-905.723396	13.756051	1.211162
-909.612355	19.198017	1.216166
-913.370615	17.357367	1.221171
-916.726917	19.414101	1.226176
-921.194352	19.258617	1.231181
-924.404530	10.766286	1.236186
-928.319987	17.326669	1.241190
-932.068564	14.177905	1.246195
-936.042132	22.350769	1.251200
-939.712232	20.630392	1.256205
-942.980690	19.050264	1.261210
-947.193682	23.230366	1.266214
-950.774003	15.129595	1.271219
-954.782760	13.791421	1.276224
-958.950352	15.070562	1.281229
-962.242177	16.454738	1.286234
-965.917002	22.793465	1.291238
-969.479889	20.979321	1.296243
-973.587587	23.222323	1.301248
-977.570978	26.540870	1.306253
-981.040924	18.618134	1.311258
-985.217875	26.209429	1.316262
-988.650626	22.510353	1.321267
-992.140844	17.404161	1.326272
-995.844294	15.749159	1.331277
-999.694718	16.557871	1.336282
-1003.480625	20.401832	1.341286
-1007.364141	14.158935	1.346291
-1011.093908	19.887445	1.351296
-1015.072509	21.155903	1.356301
-1018.500248	13.681050	1.361306
-1022.755166	17.372673	1.366310
-1026.057075	19.491986	1.371315
-1029.930057	19.697545	1.376320
-1033.692514	25.587595	1.381325
-1037.450813	6.582998	1.386330
-1041.293446	22.165730	1.391334
-1045.181407	17.369035	1.396339
-1048.882606	21.763311	1.401344
-1052.728760	22.141900	1.406349
-1055.665863	13.937108	1.411354
-1059.975849	20.978200	1.416358
-1063.682498	22.081599	1.421363
-1068.186080	22.218634	1.426368
-1071.935042	36.304787	1.431373
-1074.871614	14.178333	1.436378
-1078.518669	19.762444	1.441382
-1082.297036	10.534190	1.446387
-1086.319023	22.123753	1.451392
-1090.637267	26.096687	1.456397
-1093.726446	20.882253	1.461402
-1097.841848	31.647549	1.466406
-1101.662674	22.390284	1.471411
-1105.259785	16.996255	1.476416
-1108.636991	25.021082	1.481421
-1112.320499	27.659103	1.486426
-1116.598874	33.196926	1.491430
-1120.343980	18.395704	1.496435
-1124.123441	19.928463	1.501440
-1127.737731	14.991708	1.506445
-1131.378249	14.384220	1.511450
-1135.392676	25.889245	1.516454
-1138.995373	25.976655	1.521459
-1142.694114	20.389338	1.526464
-1146.667540	18.097992	1.531469
-1150.145795	14.004272	1.536474
-1154.172820	27.225276	1.541478
-1157.873660	21.224290	1.546483
-1161.327719	33.490412	1.551488
-1165.200741	26.308837	1.556493
-1169.022465	18.619952	1.561498
-1173.010787	20.538326	1.566502
-1176.554436	12.995894	1.571507
-1180.193107	31.246239	1.576512
-1184.544622	27.600897	1.581517
-1187.917591	21.259055	1.586522
-1191.823451	32.774301	1.591526
-1195.167376	14.687835	1.596531
-1199.099601	21.704052	1.601536
-1203.089720	25.256042	1.606541
-1206.874483	17.474802	1.611546
-1210.642557	26.082306	1.616550
-1214.432816	10.727677	1.621555
-1217.732770	16.152431	1.626560
-1221.698983	18.746336	1.631565
-1225.258136	19.522598	1.636570
-1229.454784	29.437558	1.641574
-1233.395613	17.789403	1.646579
-1237.124814	20.119613	1.651584
-1240.778980	23.024257	1.656589
-1244.321505	12.245134	1.661594
-1248.233378	28.609189	1.666598
-1251.984879	23.405607	1.671603
-1255.350717	23.626502	1.676608
-1259.605920	27.086713	1.681613
-1263.230514	15.126147	1.686618
-1267.370952	21.260103	1.691622
-1270.670446	19.712796	1.696627
-1274.126616	20.782832	1.701632
-1277.691671	25.927138	1.706637
-1281.713094	11.412738	1.711642
-1285.713342	16.312870	1.716646
-1289.966796	19.931479	1.721651
-1293.233813	8.866688	1.726656
-1297.241833	18.374339	1.731661
-1300.721555	14.483088	1.736666
-1304.561136	14.351216	1.741670
-1308.183305	9.453872	1.746675
-1312.002148	13.030616	1.751680
-1315.864603	21.349307	1.756685
-1319.758245	14.003291	1.761690
-1323.630565	20.757111	1.766694
-1326.960615	15.619362	1.771699
-1330.361693	14.908953	1.776704
-1334.337043	20.052332	1.781709
-1337.993994	8.361854	1.786714
-1341.830826	16.512361	1.791718
-1346.113035	13.687324	1.796723
-1349.637122	7.981005	1.801728
-1353.900691	17.149736	1.806733
-1357.242958	19.126246	1.811738
-1361.025628	15.291424	1.816742
-1364.492291	12.731685	1.821747
-1368.411653	15.745533	1.826752
-1372.240749	25.003853	1.831757
-1376.044957	14.746999	1.836762
-1380.037099	19.815151	1.841766
-1383.515428	20.671207	1.846771
-1386.768348	15.862073	1.851776
-1390.927747	25.801168	1.856781
-1394.560401	17.277996	1.861786
-1398.716162	18.213326	1.866790
-1402.356119	10.573183	1.871795
-1405.872568	12.601359	1.876800
-1410.048067	30.906967	1.881805
-1413.648449	25.452995	1.886810
-1417.458597	26.331343	1.891814
-1421.151663	20.641875	1.896819
-1424.410325	20.633725	1.901824
-1428.684921	24.207553	1.906829
-1432.089162	17.332531	1.911834
-1436.411875	26.360332	1.916838
-1440.155352	25.209138	1.921843
-1443.665721	19.924847	1.926848
-1447.415487	20.644837	1.931853
-1450.884926	16.596044	1.936858
-1454.815080	17.655684	1.941862
-1458.906673	15.886213	1.946867
-1462.879314	26.849905	1.951872
-1466.403768	31.323105	1.956877
-1469.997504	19.636101	1.961882
-1473.810639	26.456455	1.966886
-1477.449253	21.609057	1.971891
-1481.181080	20.734559	1.976896
-1485.128505	29.474139	1.981901
-1488.626408	16.939450	1.986906
-1492.944556	24.231412	1.991910
-1496.500560	19.278664	1.996915
-1500.519602	15.904090	2.006912
-1501.398484	19.724690	2.016909
-1498.399432	16.372392	2.026906
-1495.690398	22.448174	2.036902
-1494.107708	21.497822	2.046899
-1492.038233	19.903046	2.056896
-1490.118949	17.076525	2.066893
-1488.141366	24.525640	2.076890
-1486.089488	18.650638	2.086886
-1484.445000	15.812047	2.096883
-1482.492306	20.825038	2.106880
-1480.622949	23.773560	2.116877
-1478.823344	22.135440	2.126874
-1476.685442	20.182714	2.136870
-1474.782007	21.050944	2.146867
-1473.091306	23.811612	2.156864
-1470.965916	17.795151	2.166861
-1469.110907	21.134236	2.176858
-1467.453130	19.350151	2.186854
-1465.337640	19.889108	2.196851
-1463.676165	18.903102	2.206848
-1461.652365	20.863959	2.216845
-1459.769527	14.855183	2.226842
-1457.456428	17.619595	2.236838
-1456.004369	17.358412	2.246835
-1454.346132	22.694300	2.256832
-1451.856972	16.873823	2.266829
-1450.081701	11.390581	2.276826
-1448.279347	15.308609	2.286822
-1446.636976	18.177182	2.296819
-1444.690708	14.297167	2.306816
-1442.851581	13.318196	2.316813
-1440.992083	15.748733	2.326810
-1439.125004	21.309193	2.336806
-1437.266015	19.819762	2.346803
-1435.265145	15.818922	2.356800
-1433.000241	15.738233	2.366797
-1431.311364	11.479963	2.376794
-1429.757792	12.820514	2.386790
-1427.903238	18.852241	2.396787
-1426.053047	15.991773	2.406784
-1424.209294	14.040992	2.416781
-1421.736874	12.740623	2.426778
-1420.262151	10.346975	2.436774
-1418.556139	18.064882	2.446771
-1416.605983	14.209504	2.456768
-1414.227369	20.136200	2.466765
-1412.550151	13.867939	2.476762
-1410.856991	16.451158	2.486758
-1408.905484	20.205658	2.496755
-1407.111168	20.842497	2.506752
-1405.222238	10.393733	2.516749
-1403.222027	10.224948	2.526746
-1401.395506	13.537341	2.536742
-1399.425911	13.212968	2.546739
-1398.033835	12.677164	2.556736
-1395.641837	13.337019	2.566733
-1393.655362	8.792891	2.576730
-1391.969164	6.374784	2.586726
-1390.433401	15.940295	2.596723
-1388.184935	15.414685	2.606720
-1386.296853	11.982183	2.616717
-1384.394520	9.826125	2.626714
-1382.496432	16.992546	2.636710
-1380.669194	16.411246	2.646707
-1378.763475	18.425229	2.656704
-1376.807704	16.001925	2.666701
-1375.246003	13.767243	2.676698
-1373.606980	16.198532	2.686694
-1371.478723	15.789614	2.696691
-1369.410571	19.584170	2.706688
-1367.206701	17.932776	2.716685
-1365.829890	20.971489	2.726682
-1363.966513	22.387295	2.736678
-1362.132490	26.439040	2.746675
-1359.983089	27.217256	2.756672
-1358.000122	21.051811	2.766669
-1356.375186	14.328971	2.776666
-1354.432619	11.710736	2.786662
-1352.470745	15.087246	2.796659
-1350.602259	15.343432	2.806656
-1348.733571	20.718705	2.816653
-1346.868220	9.614014	2.826650
-1345.266449	9.609729	2.836646
-1343.100942	10.123559	2.846643
-1341.289208	13.099828	2.856640
-1339.246566	8.556351	2.866637
-1337.479624	8.085019	2.876634
-1336.096623	11.020319	2.886630
-1334.241238	7.307326	2.896627
-1331.633091	12.196354	2.906624
-1329.620651	11.403843	2.916621
-1327.716858	12.508809	2.926618
-1326.729933	15.093221	2.936614
-1324.841142	14.550379	2.946611
-1322.606821	11.166723	2.956608
-1320.586212	8.323269	2.966605
-1318.678317	13.530181	2.976602
-1316.929800	10.227200	2.986598
-1315.090966	8.133850	2.996595
-1313.202867	3.455685	3.006592
-1311.204375	7.333370	3.016589
-1309.140338	1.420003	3.026586
-1307.609623	7.796699	3.036582
-1305.681770	12.193176	3.046579
-1303.719354	12.805932	3.056576
-1301.875655	10.871020	3.066573
-1299.829418	9.581081	3.076570
-1298.462044	16.064484	3.086566
-1296.339747	9.712708	3.096563
-1294.277154	13.894770	3.106560
-1292.399360	12.827416	3.116557
-1290.486935	13.905623	3.126554
-1288.715656	15.618669	3.136550
-1286.660616	15.210512	3.146547
-1284.681729	14.390192	3.156544
-1282.832016	11.927839	3.166541
-1281.418047	12.461303	3.176538
-1279.671468	10.177118	3.186534
-1277.779434	5.250496	3.196531
-1275.705392	13.079946	3.206528
-1273.739780	14.489301	3.216525
-1271.797875	7.423551	3.226522
-1269.877230	17.686560	3.236518
-1267.806329	19.006699	3.246515
-1266.437161	16.525313	3.256512
-1264.289879	18.351638	3.266509
-1262.565876	13.739217	3.276506
-1260.651620	10.999814	3.286502
-1258.333108	13.143332	3.296499
-1256.924071	17.670038	3.306496
-1254.861886	19.436289	3.316493
-1253.082084	14.234518	3.326490
-1251.481125	15.941262	3.336486
-1249.248711	17.322988	3.346483
-1247.503401	11.782918	3.356480
-1245.604082	12.269401	3.366477
-1243.560194	15.950813	3.376474
-1241.688548	14.629627	3.386470
-1240.117335	13.646167	3.396467
-1238.122375	19.507653	3.406464
-1236.185551	18.890602	3.416461
-1234.340371	13.040536	3.426458
-1232.373750	16.552243	3.436454
-1230.514295	18.663164	3.446451
-1228.838317	13.082444	3.456448
-1226.810463	15.351380	3.466445
-1224.789316	17.981108	3.476442
-1223.124648	13.436591	3.486438
-1221.240060	16.364047	3.496435
-1219.091148	12.197580	3.506432
-1217.253220	8.108232	3.516429
-1215.400805	9.089284	3.526426
-1213.754836	10.482817	3.536422
-1211.771288	12.862913	3.546419
-1210.067111	8.669676	3.556416
-1207.949748	14.750046	3.566413
-1206.136709	10.146464	3.576410
-1204.224183	10.420447	3.586406
-1202.487854	10.976830	3.596403
-1200.762180	19.133312	3.606400
-1198.677485	12.027655	3.616397
-1196.670515	16.354878	3.626394
-1194.957019	10.035012	3.636390
-1193.082306	15.727865	3.646387
-1191.077655	16.372943	3.656384
-1189.194307	16.353956	3.666381
-1187.299260	18.331133	3.676378
-1185.434666	14.405576	3.686374
-1183.904435	19.195654	3.696371
-1181.526699	15.544386	3.706368
-1179.588081	14.839317	3.716365
-1178.307771	13.808613	3.726362
-1176.323559	17.122490	3.736358
-1174.398095	19.928339	3.746355
-1172.275162	12.887264	3.756352
-1170.446082	14.128437	3.766349
-1168.538044	10.733306	3.776346
-1166.639149	19.954786	3.786342
-1164.702676	19.915227	3.796339
-1162.816352	22.210871	3.806336
-1161.240235	25.135997	3.816333
-1159.070033	13.437580	3.826330
-1157.386450	16.207511	3.836326
-1155.513027	17.854465	3.846323
-1153.527363	19.078640	3.856320
-1151.847775	15.920346	3.866317
-1150.225871	16.655274	3.876314
-1147.651976	16.709801	3.886310
-1145.746484	14.724428	3.896307
-1144.617893	11.793936	3.906304
-1142.063309	19.644497	3.916301
-1140.288346	15.735139	3.926298
-1138.586052	17.772706	3.936294
-1136.964585	18.102231	3.946291
-1135.037486	12.480003	3.956288
-1133.006263	16.215026	3.966285
-1130.757281	17.559194	3.976282
-1129.186147	19.937824	3.986278
-1127.468129	21.837536	3.996275
-1125.788891	20.578288	4.006272
-1123.549119	17.605995	4.016269
-1121.327552	11.448290	4.026266
-1119.594107	10.751999	4.036262
-1118.141948	13.751383	4.046259
-1116.056960	20.537281	4.056256
-1114.332448	16.624739	4.066253
-1112.462828	14.630522	4.076250
-1110.375928	20.537942	4.086246
-1108.625410	15.756616	4.096243
-1106.729066	14.356553	4.106240
-1104.899028	12.105136	4.116237
-1102.739481	13.890315	4.126234
-1100.802259	10.073651	4.136230
-1099.342067	14.504688	4.146227
-1097.515133	21.849072	4.156224
-1095.407196	19.055537	4.166221
-1093.373166	11.356325	4.176218
-1091.560687	17.193496	4.186214
-1089.774261	16.144288	4.196211
-1087.941021	18.231322	4.206208
-1085.951090	15.213419	4.216205
-1084.436956	19.147909	4.226202
-1082.178548	10.103223	4.236198
-1080.359068	20.140658	4.246195
-1078.732605	19.514919	4.256192
-1076.526960	13.953176	4.266189
-1074.752694	11.562749	4.276186
-1073.202473	17.543365	4.286182
-1070.969735	18.395949	4.296179
-1069.187832	22.005849	4.306176
-1067.377630	16.453909	4.316173
-1065.370756	18.977092	4.326170
-1063.311421	18.322486	4.336166
-1061.721928	22.806430	4.346163
-1059.956691	17.183961	4.356160
-1057.803665	13.559088	4.366157
-1055.759607	19.034817	4.376154
-1053.865740	15.978883	4.386150
-1052.495306	20.077962	4.396147
-1050.688192	25.845731	4.406144
-1048.713166	15.600060	4.416141
-1046.522719	15.256112	4.426138
-1044.806181	19.151521	4.436134
-1043.004117	16.175376	4.446131
-1041.032093	14.115392	4.456128
-1039.043855	15.497262	4.466125
-1037.121622	14.575729	4.476122
-1035.137821	14.170835	4.486118
-1033.490016	12.098147	4.496115
-1031.615432	8.141692	4.506112
-1029.520137	6.104023	4.516109
-1027.932857	6.184549	4.526106
-1025.789282	9.898361	4.536102
-1024.366491	5.599763	4.546099
-1022.392659	11.637695	4.556096
-1020.290389	15.426183	4.566093
-1018.430088	19.037270	4.576090
-1016.642910	10.771452	4.586086
-1014.835764	17.102401	4.596083
-1012.961923	19.051685	4.606080
-1011.044878	22.649477	4.616077
-1008.940958	19.075343	4.626074
-1007.374686	20.775493	4.636070
-1005.360702	18.429698	4.646067
-1003.484136	11.648751	4.656064
-1001.478092	20.452766	4.666061
-999.948030	17.676676	4.676058
-997.966681	15.958150	4.686054
-995.931515	13.807513	4.696051
-994.079532	14.553194	4.706048
-992.114543	8.483071	4.716045
-990.324081	12.850732	4.726042
-988.385366	12.002667	4.736038
-986.750998	15.434795	4.746035
-984.540936	11.130681	4.756032
-982.944588	16.267550	4.766029
-980.964958	13.019078	4.776026
-979.009192	12.261754	4.786022
-976.952711	9.339181	4.796019
-975.356838	9.904754	4.806016
-973.545912	5.170414	4.816013
-971.847903	14.156162	4.826010
-969.657818	10.540382	4.836006
-968.199261	10.037964	4.846003
-965.909381	11.422229	4.856000
-964.113186	13.269067	4.865997
-962.060892	9.028408	4.875994
-960.331479	12.274686	4.885990
-958.484663	18.288614	4.895987
-956.698734	16.417907	4.905984
-954.683468	14.361603	4.915981
-952.570612	13.307790	4.925978
-950.686243	19.484822	4.935974
-949.059456	13.993262	4.945971
-947.205721	15.127548	4.955968
-945.415778	18.495047	4.965965
-943.844649	14.090779	4.975962
-941.227517	18.204315	4.985958
-939.833031	13.715365	4.995955
-938.134446	16.961017	5.005952
-935.639054	20.250499	5.015949
-933.771620	21.217243	5.025946
-932.242962	22.812035	5.035942
-930.464209	25.256673	5.045939
-928.206887	18.260210	5.055936
-926.790543	23.125670	5.065933
-924.356916	22.298591	5.075930
-922.477553	16.838771	5.085926
-921.277075	19.326165	5.095923
-919.216474	16.681532	5.105920
-916.838020	15.011463	5.115917
-914.962248	10.354538	5.125914
-913.807130	14.218329	5.135910
-911.681732	11.831320	5.145907
-909.566135	17.021362	5.155904
-907.836781	16.119163	5.165901
-905.797687	13.556480	5.175898
-903.903632	17.973981	5.185894
-902.035409	19.891873	5.195891
-900.143108	22.898386	5.205888
-898.631668	16.708151	5.215885
-896.569988	9.047744	5.225882
-894.958451	11.263028	5.235878
-892.814651	12.863690	5.245875
-890.819429	21.705591	5.255872
-888.944516	15.943027	5.265869
-887.006835	15.960692	5.275866
-885.119753	14.734230	5.285862
-883.252656	17.095352	5.295859
-881.667093	13.371153	5.305856
-879.562226	22.051568	5.315853
-877.834738	15.872865	5.325850
-875.728961	19.749356	5.335846
-874.040704	16.122932	5.345843
-872.320440	21.616005	5.355840
-870.308032	17.846206	5.365837
-868.510904	13.846989	5.375834
-866.489419	16.123523	5.385830
-864.574244	15.647493	5.395827
-863.003670	18.682767	5.405824
-860.686040	12.101230	5.415821
-858.973160	23.269994	5.425818
-857.054546	11.036291	5.435814
-855.541222	14.690807	5.445811
-853.247370	17.250992	5.455808
-851.448359	13.866405	5.465805
-849.488112	16.650237	5.475802
-847.780878	17.778097	5.485798
-845.966824	13.014019	5.495795
-843.983837	17.084705	5.505792
-842.129864	18.730399	5.515789
-840.345404	12.437990	5.525786
-838.198320	16.207027	5.535782
-836.495540	17.580291	5.545779
-834.579875	17.855088	5.555776
-832.558264	17.399534	5.565773
-830.837175	16.264424	5.575770
-829.062372	14.291342	5.585766
-827.054619	14.887450	5.595763
-825.209811	9.705504	5.605760
-823.265702	15.462117	5.615757
-821.500622	15.614167	5.625754
-819.518005	14.333791	5.635750
-817.707811	15.896506	5.645747
-816.013835	16.932595	5.655744
-813.988502	17.236003	5.665741
-812.048694	17.936260	5.675738
-810.008337	10.192205	5.685734
-808.256045	12.431580	5.695731
-806.499689	18.092380	5.705728
-804.829021	17.380114	5.715725
-802.808001	17.744340	5.725722
-800.765234	17.665361	5.735718
-798.955149	22.574345	5.745715
-796.810183	18.923706	5.755712
-795.501328	22.870623	5.765709
-793.364964	21.180516	5.775706
-791.415531	18.493763	5.785702
-789.629908	15.102406	5.795699
-787.714499	19.787019	5.805696
-785.970529	16.537579	5.815693
-783.701364	18.517130	5.825690
-781.756269	23.852305	5.835686
-780.152664	21.035209	5.845683
-778.583295	23.633623	5.855680
-776.567476	19.321444	5.865677
-774.599924	21.004191	5.875674
-772.483592	17.608645	5.885670
-770.787951	20.973833	5.895667
-768.991031	18.321564	5.905664
-766.840472	18.254532	5.915661
-765.220548	12.265850	5.925658
-763.473943	19.717063	5.935654
-761.597170	21.003982	5.945651
-759.244913	17.316598	5.955648
-757.893220	16.676087	5.965645
-755.937244	16.182432	5.975642
-753.652834	22.445040	5.985638
-752.206779	18.043326	5.995635
-750.199698	20.459923	6.005632
-748.112817	23.957954	6.015629
-746.306025	25.194052	6.025626
-744.456311	22.564347	6.035622
-742.778417	21.739020	6.045619
-740.476986	22.234577	6.055616
-738.933408	19.275246	6.065613
-737.190486	25.092518	6.075610
-735.174958	24.863718	6.085606
-733.301701	25.921241	6.095603
-731.454665	26.935839	6.105600
-729.501494	20.345374	6.115597
-727.723608	23.019077	6.125594
-725.850649	19.564144	6.135590
-723.879725	19.614908	6.145587
-721.954661	21.672517	6.155584
-720.024831	25.142580	6.165581
-718.156921	14.820951	6.175578
-716.532730	15.837834	6.185574
-714.437745	16.628091	6.195571
-712.562393	10.414979	6.205568
-711.035814	16.731784	6.215565
-708.654405	19.665120	6.225562
-706.908952	21.821140	6.235558
-705.327388	17.206089	6.245555
-703.455326	22.825346	6.255552
-701.280717	18.206931	6.265549
-699.346853	17.528580	6.275546
-697.742908	20.839979	6.285542
-695.606813	21.180950	6.295539
-693.869832	21.733085	6.305536
-691.926560	15.214682	6.315533
-689.915554	18.224240	6.325530
-688.283481	16.644437	6.335526
-686.542822	13.652093	6.345523
-684.689259	24.374327	6.355520
-682.697932	21.659483	6.365517
-680.289232	18.910167	6.375514
-678.525061	21.836018	6.385510
-677.045199	21.374699	6.395507
-675.286264	16.039974	6.405504
-673.189884	19.660508	6.415501
-671.610716	14.073662	6.425498
-669.468671	18.023081	6.435494
-667.338956	22.537397	6.445491
-665.881945	12.571638	6.455488
-663.830113	16.652732	6.465485
-661.884374	15.856168	6.475482
-659.976534	16.446577	6.485478
-658.364389	15.248025	6.495475
-656.689683	20.277924	6.505472
-654.457810	10.761744	6.515469
-652.375383	9.483284	6.525466
-650.451505	14.298510	6.535462
-648.953051	16.638818	6.545459
-647.077491	18.895447	6.555456
-644.984090	21.843464	6.565453
-643.255213	18.284845	6.575450
-641.238437	16.010660	6.585446
-639.501731	20.086560	6.595443
-637.569239	22.912012	6.605440
-635.568100	20.539338	6.615437
-633.945244	22.275371	6.625434
-632.103046	25.634047	6.635430
-630.130040	32.529151	6.645427
-628.291325	30.396974	6.655424
-626.515879	26.012282	6.665421
-624.145080	22.352609	6.675418
-622.377901	23.232358	6.685414
-620.617965	27.467900	6.695411
-618.950965	27.233748	6.705408
-616.760181	30.721528	6.715405
-614.932047	26.364159	6.725402
-613.108997	24.959097	6.735398
-611.550546	21.366103	6.745395
-609.588897	20.668796	6.755392
-607.309608	24.733024	6.765389
-605.627392	18.539650	6.775386
-603.859019	17.595305	6.785382
-601.788030	23.150048	6.795379
-600.148222	22.337633	6.805376
-598.374134	19.516639	6.815373
-596.076991	18.438489	6.825370
-594.109257	25.694946	6.835366
-592.946724	20.833684	6.845363
-590.962231	26.659372	6.855360
-588.702051	29.152370	6.865357
-586.829891	25.495280	6.875354
-584.770654	24.004255	6.885350
-583.453129	26.325046	6.895347
-581.267896	23.962700	6.905344
-579.546275	19.666304	6.915341
-577.527943	18.453811	6.925338
-575.559422	21.669112	6.935334
-573.687601	25.446002	6.945331
-571.977010	24.914304	6.955328
-570.163480	26.226387	6.965325
-568.025447	22.967903	6.975322
-566.216461	16.569414	6.985318
-564.370928	17.941613	6.995315
-562.720451	22.889555	7.005312
-560.536410	23.387169	7.015309
-558.727428	21.263284	7.025306
-556.831174	25.291296	7.035302
-555.019559	30.077620	7.045299
-553.222796	24.562154	7.055296
-551.622078	23.142306	7.065293
-549.139069	20.070463	7.075290
-547.358267	24.807931	7.085286
-545.792789	23.627701	7.095283
-543.522108	16.893512	7.105280
-541.722722	18.114764	7.115277
-539.996669	13.151693	7.125274
-538.099186	13.732472	7.135270
-536.503137	21.203304	7.145267
-534.372436	26.847827	7.155264
-532.322094	27.076334	7.165261
-530.701401	24.075383	7.175258
-528.758161	21.172435	7.185254
-527.035154	19.117062	7.195251
-525.191070	22.714564	7.205248
-523.269248	20.158337	7.215245
-521.155035	20.115447	7.225242
-519.259800	20.924657	7.235238
-517.400333	23.987571	7.245235
-515.355503	21.728387	7.255232
-513.562088	25.448410	7.265229
-511.979352	21.247398	7.275226
-510.130714	22.665723	7.285222
-508.304413	25.754092	7.295219
-506.603076	24.650159	7.305216
-504.190459	22.434983	7.315213
-502.366361	15.248638	7.325210
-500.480314	20.739918	7.335206
-498.753272	19.397613	7.345203
-497.038874	26.080266	7.355200
-494.948326	22.861183	7.365197
-492.893882	20.169580	7.375194
-491.377399	20.979758	7.385190
-489.181279	14.818005	7.395187
-487.453582	20.955358	7.405184
-485.687949	20.029709	7.415181
-483.687774	14.906597	7.425178
-481.886307	21.940678	7.435174
-479.898341	21.351152	7.445171
-478.132830	27.113688	7.455168
-475.812247	24.003353	7.465165
-474.014051	20.177595	7.475162
-472.572284	19.635539	7.485158
-470.591982	20.302918	7.495155
-468.735698	20.409429	7.505152
-466.930024	22.594345	7.515149
-464.812838	22.971476	7.525146
-462.974357	23.358877	7.535142
-461.091540	25.178823	7.545139
-459.400328	25.801348	7.555136
-457.512234	20.327159	7.565133
-455.697615	27.326592	7.575130
-453.901080	17.737363	7.585126
-451.743783	18.519825	7.595123
-449.993720	22.626715	7.605120
-447.802955	18.713860	7.615117
-446.305652	21.459928	7.625114
-444.688730	24.179548	7.635110
-442.240945	19.498575	7.645107
-440.274138	24.576867	7.655104
-438.893239	23.873346	7.665101
-436.792100	29.649858	7.675098
-434.685634	28.353146	7.685094
-433.084049	30.874636	7.695091
-430.744199	27.288739	7.705088
-429.370878	28.934869	7.715085
-427.399460	26.302590	7.725082
-425.745237	24.471281	7.735078
-423.634229	27.351972	7.745075
-421.737863	28.787442	7.755072
-419.875641	25.197726	7.765069
-418.427535	24.700839	7.775066
-416.102005	29.405786	7.785062
-414.138031	34.144303	7.795059
-412.341517	30.374578	7.805056
-410.369673	23.895243	7.815053
-408.718634	19.807829	7.825050
-406.757325	24.888662	7.835046
-405.085440	21.177866	7.845043
-403.045469	23.922154	7.855040
-400.787362	24.217046	7.865037
-399.294955	15.883820	7.875034
-397.545663	14.025148	7.885030
-395.370376	22.811142	7.895027
-393.383024	21.858956	7.905024
-391.946836	16.797057	7.915021
-390.018561	14.792679	7.925018
-388.150246	19.424307	7.935014
-385.890694	13.370676	7.945011
-384.310750	13.978328	7.955008
-382.202288	17.371274	7.965005
-380.440527	22.105761	7.975002
-378.805959	17.256448	7.984998
-376.744515	25.616975	7.994995
-374.941120	18.099083	8.004992
-372.920573	24.988140	8.014989
-371.273549	19.571144	8.024986
-369.157239	11.006019	8.034982
-367.106161	14.190659	8.044979
-365.709952	17.068313	8.054976
-364.026197	16.427081	8.064973
-361.486682	18.511456	8.074970
-359.884141	9.490258	8.084966
-357.881754	20.555080	8.094963
-356.286252	21.931922	8.104960
-353.939228	11.035791	8.114957
-352.538919	19.360343	8.124954
-350.567198	19.571199	8.134950
-348.717828	14.004101	8.144947
-346.742633	14.127021	8.154944
-344.936438	14.034294	8.164941
-342.912638	11.442468	8.174938
-340.843761	11.454471	8.184934
-339.209859	14.589747	8.194931
-337.575914	19.280571	8.204928
-335.692585	13.236165	8.214925
-333.305846	10.599084	8.224922
-331.678075	9.409824	8.234918
-329.742772	11.865414	8.244915
-327.958995	16.649895	8.254912
-326.264243	19.720596	8.264909
-324.133599	16.803372	8.274906
-322.120288	17.719278	8.284902
-320.262052	20.269902	8.294899
-318.850892	19.610233	8.304896
-316.747603	19.654285	8.314893
-314.766687	15.837556	8.324890
-312.965051	17.112266	8.334886
-311.164852	17.403542	8.344883
-309.299329	23.465564	8.354880
-307.334562	20.305683	8.364877
-305.290017	21.778627	8.374874
-303.345691	16.457283	8.384870
-301.933951	19.286451	8.394867
-299.903202	19.733817	8.404864
-297.511518	17.725873	8.414861
-296.180730	14.294148	8.424858
-294.206658	22.495417	8.434854
-292.229692	12.297096	8.444851
-290.350964	11.127645	8.454848
-288.883269	9.169899	8.464845
-286.611203	9.193711	8.474842
-284.545514	15.098499	8.484838
-283.120330	21.111172	8.494835
-281.260439	23.412942	8.504832
-279.364923	19.985535	8.514829
-277.315386	22.080490	8.524826
-275.025906	16.075522	8.534822
-273.485560	17.609664	8.544819
-271.679710	24.994440	8.554816
-269.963987	28.776904	8.564813
-268.093619	22.773078	8.574810
-266.007428	25.108364	8.584807
-263.924674	15.765326	8.594803
-262.275986	21.598978	8.604800
-260.397688	17.122873	8.614797
-258.283092	18.083881	8.624794
-256.028970	6.645290	8.634791
-254.717022	11.503612	8.644787
-253.669592	11.561214	8.654784
-251.003585	6.274202	8.664781
-249.140265	12.229525	8.674778
-247.300161	11.871763	8.684775
-245.477031	11.074275	8.694771
-243.279034	13.712888	8.704768
-241.574000	12.735283	8.714765
-239.820308	17.590569	8.724762
-237.784077	11.199854	8.734759
-236.151595	12.596877	8.744755
-234.230089	14.326897	8.754752
-232.171478	11.182965	8.764749
-230.437237	6.690478	8.774746
-228.769564	5.344625	8.784743
-226.707040	11.067002	8.794739
-224.974320	10.242345	8.804736
-222.783330	7.617155	8.814733
-220.826249	8.387432	8.824730
-219.053127	9.688413	8.834727
-217.432205	6.199838	8.844723
-215.369204	11.091798	8.854720
-213.446270	12.620024	8.864717
-211.567883	8.843054	8.874714
-209.615050	9.539370	8.884711
-207.815940	9.662118	8.894707
-205.679142	10.580217	8.904704
-203.980325	6.509182	8.914701
-202.607159	7.088336	8.924698
-200.463997	6.771099	8.934695
-198.724616	12.242225	8.944691
-196.744791	15.080315	8.954688
-194.652457	8.824248	8.964685
-192.533027	6.602209	8.974682
-190.646724	9.078122	8.984679
-188.866727	10.674345	8.994675
-187.436027	14.367396	9.004672
-185.744705	9.153117	9.014669
-183.733045	9.678900	9.024666
-181.221339	2.479082	9.034663
-179.836544	4.894381	9.044659
-178.029710	6.900188	9.054656
-176.038507	1.498533	9.064653
-174.089285	9.895008	9.074650
-172.243745	7.669361	9.084647
-170.040654	10.765189	9.094643
-168.676010	6.466130	9.104640
-166.713441	4.676491	9.114637
-164.865081	9.805659	9.124634
-162.553668	8.055396	9.134631
-160.938631	4.088852	9.144627
-159.249179	9.781576	9.154624
-157.225081	4.409461	9.164621
-155.248883	8.696644	9.174618
-153.507149	11.317116	9.184615
-151.565946	9.893951	9.194611
-149.910110	5.627166	9.204608
-147.997239	5.650201	9.214605
-145.598127	4.640554	9.224602
-143.878956	7.725320	9.234599
-142.383422	14.119612	9.244595
-140.558505	12.671734	9.254592
-138.645026	4.904638	9.264589
-136.396075	10.455187	9.274586
-134.751209	8.016564	9.284583
-132.787792	16.092088	9.294579
-130.923849	10.324567	9.304576
-129.095571	15.478934	9.314573
-127.007762	10.649596	9.324570
-125.335622	11.772697	9.334567
-123.515317	11.201803	9.344563
-121.815828	7.376106	9.354560
-119.889597	12.573752	9.364557
-117.697919	12.273132	9.374554
-115.965971	10.498557	9.384551
-114.111657	12.252009	9.394547
-112.296708	16.145965	9.404544
-110.139122	13.310372	9.414541
-108.344922	9.070855	9.424538
-106.589093	9.618015	9.434535
-104.567820	18.438885	9.444531
-102.958716	20.792036	9.454528
-100.831643	10.987360	9.464525
-98.911112	8.886416	9.474522
-97.384846	12.163156	9.484519
-95.250428	10.517577	9.494515
-93.288669	9.661599	9.504512
-91.830741	12.983653	9.514509
-89.614001	13.627655	9.524506
-87.745406	12.407855	9.534503
-85.705270	8.019862	9.544499
-84.079168	14.624964	9.554496
-82.160766	18.597627	9.564493
-80.404864	13.055740	9.574490
-78.174476	14.670422	9.584487
-76.659562	15.293682	9.594483
-74.953996	17.047364	9.604480
-72.692987	14.898718	9.614477
-70.632096	16.747978	9.624474
-69.105469	21.149050	9.634471
-67.262000	20.937802	9.644467
-65.556788	17.617804	9.654464
-63.396923	16.077349	9.664461
-61.519374	19.639287	9.674458
-59.597208	21.497321	9.684455
-57.683905	12.837492	9.694451
-55.757690	19.499437	9.704448
-53.794692	19.065351	9.714445
-52.283148	11.057746	9.724442
-50.397637	15.534822	9.734439
-48.481078	16.169452	9.744435
-46.267075	17.032893	9.754432
-44.389492	15.717113	9.764429
-42.689710	13.303092	9.774426
-40.669428	10.726225	9.784423
-39.443914	2.657802	9.794419
-37.531902	11.331055	9.804416
-35.208294	15.831428	9.814413
-33.259345	12.742347	9.824410
-31.528144	14.380595	9.834407
-29.839991	14.112208	9.844403
-27.648703	11.708770	9.854400
-25.742316	7.041001	9.864397
-23.874317	7.162286	9.874394
-22.245742	11.251855	9.884391
-20.250705	10.518646	9.894387
-18.361619	7.566699	9.904384
-16.285805	20.439081	9.914381
-14.470468	8.719725	9.924378
-12.943056	10.467616	9.934375
-11.141925	12.972045	9.944371
-8.982155	15.194060	9.954368
-7.202151	15.551364	9.964365
-5.629068	16.327108	9.974362
-3.903396	32.850449	9.984359
-2.450078	66.086295	9.994355
-0.936211	114.112257	10.004352
0.000000	160.179776	10.009357
0.302761	189.146350	10.014362
0.995727	209.883019	10.019367
1.274960	241.597373	10.024371
1.839315	268.731981	10.029376
2.422339	281.637127	10.034381
2.437723	295.287730	10.039386
2.856711	308.844279	10.044391
2.960731	319.491317	10.049395
3.357559	324.137821	10.054400
3.024976	326.419125	10.059405
2.967887	332.638640	10.064410
2.900677	331.833555	10.069415
3.250615	333.093545	10.074419
2.960789	342.146371	10.079424
3.394561	338.736313	10.084429
3.279761	348.381602	10.089434
3.390563	350.350454	10.094439
3.516749	358.081502	10.099443
3.704066	357.525261	10.104448
3.610870	367.979579	10.109453
3.887215	375.008345	10.114458
3.914553	366.394943	10.119463
4.001494	367.780550	10.124467
3.883309	362.749288	10.129472
3.693550	354.354684	10.134477
3.791505	369.720053	10.139482
3.833261	370.247399	10.144487
3.862991	376.537305	10.149491
4.297213	375.322972	10.154496
4.404297	373.663043	10.159501
4.402984	377.793250	10.164506
4.492042	369.582927	10.169511
4.116151	371.671541	10.174515
4.002776	359.351406	10.179520
4.084829	372.616060	10.184525
4.332606	390.345773	10.189530
4.309050	382.494998	10.194535
4.331812	394.232018	10.199539
4.049747	386.413327	10.204544
4.424967	387.385580	10.209549
4.480767	398.899451	10.214554
4.669005	396.629582	10.219559
4.996980	397.630067	10.224563
4.367104	395.766900	10.229568
4.328850	403.157893	10.234573
4.245040	406.099153	10.239578
4.899292	396.391848	10.244583
4.636494	405.700196	10.249587
4.882530	419.361096	10.254592
4.930590	429.823604	10.259597
4.884658	434.473030	10.264602
5.454926	429.986836	10.269607
5.285408	441.394902	10.274611
4.976512	425.348938	10.279616
4.931795	431.351249	10.284621
5.148370	439.496689	10.289626
5.169911	439.346613	10.294631
5.196632	429.751222	10.299635
5.270947	443.561186	10.304640
5.371155	445.612389	10.309645
4.891000	444.028664	10.314650
4.959866	454.594195	10.319655
5.161505	456.299208	10.324659
5.398551	444.929010	10.329664
5.682069	467.607982	10.334669
5.783440	477.161421	10.339674
5.870180	477.256734	10.344679
5.677375	477.945873	10.349683
5.670834	467.314892	10.354688
5.458670	471.460749	10.359693
5.703168	488.093816	10.364698
5.885540	481.935372	10.369703
5.703942	487.687239	10.374707
5.956675	485.772994	10.379712
6.233303	488.545107	10.384717
5.699848	493.601414	10.389722
5.953343	490.532483	10.394727
5.854151	486.749580	10.399731
5.747968	491.324095	10.404736
6.034445	500.576218	10.409741
6.188610	521.503179	10.414746
6.463953	521.112623	10.419751
6.219200	519.047626	10.424755
6.301811	529.553222	10.429760
6.437412	526.217140	10.434765
6.434892	528.022294	10.439770
6.887504	526.747168	10.444775
6.628727	536.667511	10.449779
6.638201	529.882666	10.454784
6.316827	524.434233	10.459789
6.421130	530.823911	10.464794
6.702288	529.609364	10.469799
6.758041	529.375268	10.474803
6.879355	533.311603	10.479808
6.955858	528.473083	10.484813
6.844731	540.216196	10.489818
6.897331	528.148116	10.494823
6.821546	537.776964	10.499827
6.963622	548.909458	10.504832
7.347297	556.888551	10.509837
7.475931	565.708320	10.514842
7.648409	554.737124	10.519847
7.271294	551.640121	10.524851
7.349363	539.956861	10.529856
7.445068	541.804384	10.534861
7.136612	538.822712	10.539866
7.211106	551.085433	10.544871
7.122083	559.685947	10.549875
7.094477	565.638010	10.554880
7.558200	568.296747	10.559885
7.811032	574.223625	10.564890
8.133063	570.822808	10.569895
8.119815	577.382259	10.574899
7.814276	578.604264	10.579904
7.980352	573.820238	10.584909
7.614340	581.372901	10.589914
7.710968	578.308348	10.594919
7.696622	584.295249	10.599923
7.519394	576.713477	10.604928
7.818152	578.544742	10.609933
7.701897	584.320571	10.614938
7.940373	581.330773	10.619943
7.751159	592.867849	10.624947
8.017654	601.095205	10.629952
8.400874	612.322973	10.634957
8.269420	614.291949	10.639962
8.458237	612.110368	10.644967
8.455027	613.044496	10.649971
8.264735	619.505640	10.654976
8.338142	619.998753	10.659981
8.107336	620.756780	10.664986
8.579085	618.288276	10.669991
8.446479	622.321852	10.674995
8.768517	631.371383	10.680000
9.048263	625.273554	10.685005
8.746045	632.323084	10.690010
8.897267	620.975762	10.695015
8.713180	621.228822	10.700019
8.902384	618.142864	10.705024
8.947722	618.037652	10.710029
8.864988	630.845270	10.715034
9.259583	634.744250	10.720039
8.819120	627.950850	10.725043
9.117215	630.152091	10.730048
9.032238	619.523007	10.735053
9.007374	634.737596	10.740058
9.133881	630.808598	10.745063
8.850713	630.716684	10.750067
8.689576	633.573747	10.755072
9.079683	642.037687	10.760077
8.988834	660.432062	10.765082
9.341536	654.968665	10.770087
9.598434	652.504231	10.775091
9.462025	657.186604	10.780096
9.700986	651.230754	10.785101
9.685423	660.019248	10.790106
9.654420	656.742886	10.795111
9.630619	669.386883	10.800115
9.754982	662.957271	10.805120
9.857943	648.700797	10.810125
9.779332	651.748181	10.815130
10.014709	655.375264	10.820135
9.967335	654.539920	10.825139
9.874937	664.098670	10.830144
9.971938	650.248599	10.835149
9.587058	650.922126	10.840154
9.746841	650.245468	10.845159
9.793882	658.101547	10.850163
10.064634	671.065296	10.855168
10.501272	676.439664	10.860173
10.236433	668.699584	10.865178
10.437987	667.987739	10.870183
10.528874	661.803859	10.875187
10.340629	673.784892	10.880192
10.179676	657.832134	10.885197
10.356764	681.092542	10.890202
10.495210	681.118994	10.895207
10.527714	681.929770	10.900211
10.517475	683.610348	10.905216
10.715234	682.260094	10.910221
10.341895	693.237909	10.915226
10.792149	680.219718	10.920231
10.802848	685.956055	10.925235
10.755447	690.591600	10.930240
10.921914	685.859576	10.935245
11.035073	681.071169	10.940250
11.068800	683.864043	10.945255
10.919791	686.231552	10.950259
11.065424	689.107079	10.955264
11.127105	681.491400	10.960269
11.127492	694.546127	10.965274
11.040303	686.308226	10.970279
10.858368	694.478310	10.975283
10.909319	697.049951	10.980288
11.268767	686.803688	10.985293
11.204167	692.580569	10.990298
11.317814	695.679075	10.995303
11.653408	720.297456	11.000307
11.923145	720.427710	11.005312
11.440574	694.043384	11.010317
11.470978	698.036004	11.015322
11.539488	697.006321	11.020327
11.886014	715.285115	11.025331
11.880757	719.001627	11.030336
11.738405	704.254282	11.035341
11.797638	706.098999	11.040346
12.077517	697.571190	11.045351
11.514802	702.206671	11.050355
11.608735	712.813078	11.055360
12.073757	717.036311	11.060365
11.910685	725.057524	11.065370
12.177135	714.834687	11.070375
12.309334	722.092400	11.075379
12.409707	718.467851	11.080384
12.384766	718.145748	11.085389
12.095008	725.473833	11.090394
12.472231	713.537053	11.095399
11.898808	723.851714	11.100403
12.142908	718.421521	11.105408
12.326551	718.016288	11.110413
12.198364	729.726154	11.115418
12.423639	718.316330	11.120423
12.517543	721.939264	11.125427
12.346786	725.309558	11.130432
12.592736	724.105375	11.135437
12.318083	723.881741	11.140442
12.193769	721.416736	11.145447
12.608712	724.529905	11.150451
13.013415	743.797809	11.155456
13.204402	739.295638	11.160461
13.003402	736.414316	11.165466
13.154888	726.269603	11.170471
13.002629	718.864265	11.175475
12.665275	722.592323	11.180480
13.081754	731.047053	11.185485
12.915672	742.987236	11.190490
13.290692	751.003440	11.195495
13.149808	755.115046	11.200499
13.293518	751.641345	11.205504
13.695992	749.371799	11.210509
13.428717	755.856460	11.215514
13.301957	744.638417	11.220519
13.401603	744.673495	11.225523
13.256919	750.389130	11.230528
13.588901	748.539422	11.235533
13.551769	757.102728	11.240538
13.464233	750.987692	11.245543
13.727981	755.404124	11.250547
13.202297	748.648570	11.255552
13.581878	745.921910	11.260557
13.428505	754.898686	11.265562
13.552239	752.940212	11.270567
13.479446	754.835991	11.275571
13.423874	755.238331	11.280576
14.244140	765.923528	11.285581
14.201800	771.515836	11.290586
13.990642	753.353617	11.295591
14.177284	756.395016	11.300595
13.987462	761.814455	11.305600
14.057034	771.954959	11.310605
13.907250	788.273063	11.315610
14.281623	782.897484	11.320615
14.331978	782.859699	11.325619
14.482930	785.986169	11.330624
14.618269	784.334773	11.335629
14.629811	786.239780	11.340634
14.750536	769.353635	11.345639
14.811532	767.569333	11.350643
14.253955	759.294413	11.355648
14.423005	751.930679	11.360653
14.740072	776.517590	11.365658
14.534216	779.074064	11.370663
14.688602	779.873423	11.375667
14.567465	769.398458	11.380672
15.096129	772.093070	11.385677
14.767361	782.931862	11.390682
15.078848	776.998265	11.395687
15.079633	772.838161	11.400691
14.755352	784.546952	11.405696
15.210035	776.017551	11.410701
15.060605	779.018288	11.415706
15.042475	772.846344	11.420711
15.451998	769.486141	11.425715
15.503924	775.695431	11.430720
15.452989	769.710293	11.435725
14.996727	771.812738	11.440730
15.138948	770.279371	11.445735
15.244431	772.334056	11.450739
15.026677	777.262116	11.455744
15.140486	778.203033	11.460749
15.027130	781.816123	11.465754
15.290419	780.542649	11.470759
15.420059	795.515780	11.475763
15.535280	801.984617	11.480768
16.180161	811.338105	11.485773
15.704508	808.953849	11.490778
15.918702	803.158499	11.495783
16.076872	804.935346	11.500787
15.924145	799.512767	11.505792
16.374535	797.172633	11.510797
16.147046	780.748798	11.515802
15.851011	777.131413	11.520807
15.603834	783.191071	11.525811
15.890548	791.473483	11.530816
16.119985	795.489240	11.535821
16.048342	807.461832	11.540826
15.970639	809.446089	11.545831
16.166476	804.309924	11.550835
15.871691	804.550388	11.555840
16.228386	811.269926	11.560845
15.917776	811.206400	11.565850
16.080106	806.680702	11.570855
16.189295	811.107861	11.575859
16.449569	833.254917	11.580864
16.830947	827.818518	11.585869
16.483041	833.465607	11.590874
16.783578	832.307714	11.595879
16.947110	837.143185	11.600883
16.781392	837.664278	11.605888
16.929902	826.283325	11.610893
17.341114	835.706890	11.615898
17.271134	813.849024	11.620903
17.254578	812.961415	11.625907
16.579164	806.861098	11.630912
17.019950	807.894769	11.635917
16.826841	807.745571	11.640922
16.858470	814.677551	11.645927
17.307301	824.927142	11.650931
16.875071	839.491395	11.655936
16.882938	836.420300	11.660941
16.774096	842.775204	11.665946
16.922429	839.650026	11.670951
17.151150	829.098854	11.675955
17.312913	836.935750	11.680960
17.241950	835.735763	11.685965
17.198359	841.944878	11.690970
17.671658	854.099990	11.695975
17.767053	857.704543	11.700979
17.872092	856.920424	11.705984
18.104607	838.706115	11.710989
17.542074	840.477848	11.715994
17.435684	822.990334	11.720999
17.568698	837.964900	11.726003
17.668354	850.767480	11.731008
18.084845	855.709584	11.736013
18.455116	868.385258	11.741018
18.156529	850.097785	11.746023
18.515861	844.524637	11.751027
18.115901	831.913400	11.756032
18.106315	830.048431	11.761037
17.870451	833.657274	11.766042
17.767375	832.553186	11.771047
17.925866	846.945116	11.776051
18.033270	865.261138	11.781056
18.406840	859.200026	11.786061
18.240579	865.013742	11.791066
18.345900	868.596070	11.796071
18.390908	861.966038	11.801075
18.432019	861.240246	11.806080
18.480686	860.568026	11.811085
18.790517	868.017584	11.816090
18.933583	864.569626	11.821095
18.595492	862.366641	11.826099
18.704986	869.529238	11.831104
18.890379	865.845080	11.836109
18.886862	868.842922	11.841114
18.594678	866.411016	11.846119
18.729351	859.385093	11.851123
18.892657	871.275216	11.856128
18.707106	868.618190	11.861133
18.885889	869.838099	11.866138
18.972160	870.015600	11.871143
19.083377	876.804885	11.876147
18.913808	882.838645	11.881152
19.510349	891.015886	11.886157
19.329572	891.666665	11.891162
19.215628	891.052717	11.896167
19.993653	886.873007	11.901171
19.445829	872.417647	11.906176
19.669080	858.337723	11.911181
19.269425	866.666407	11.916186
19.066382	858.881690	11.921191
19.185139	867.985160	11.926195
19.219426	887.823190	11.931200
19.179623	885.415905	11.936205
19.289818	889.919886	11.941210
19.589273	890.409778	11.946215
19.664612	892.775168	11.951219
19.541854	905.196722	11.956224
19.858550	904.164736	11.961229
20.018223	918.046537	11.966234
20.240619	907.181797	11.971239
20.383957	896.294698	11.976243
20.223124	896.436803	11.981248
20.221553	876.357617	11.986253
19.910842	883.784498	11.991258
20.030099	891.810679	11.996263
20.301435	884.748287	12.001267
20.122955	888.945320	12.006272
19.962571	894.478965	12.011277
20.050574	902.257883	12.016282
20.520968	917.229155	12.021287
20.471083	911.249309	12.026291
20.447753	913.274387	12.031296
20.571277	896.307889	12.036301
20.337057	899.337396	12.041306
20.455763	899.572493	12.046311
20.756523	888.504465	12.051315
20.184204	893.587297	12.056320
20.564288	891.402096	12.061325
20.647570	888.442006	12.066330
20.525942	893.719537	12.071335
20.705158	883.104186	12.076339
20.434678	890.595224	12.081344
20.579583	887.556280	12.086349
20.139199	884.430583	12.091354
20.205487	882.618519	12.096359
20.603113	883.566439	12.101363
20.221549	885.885824	12.106368
20.105587	872.035358	12.111373
19.781659	878.082159	12.116378
20.061724	885.268018	12.121383
20.227332	894.311368	12.126387
20.366138	903.710233	12.131392
20.499317	895.754564	12.136397
20.285233	899.585869	12.141402
20.388247	896.121087	12.146407
20.385997	900.073964	12.151411
20.386974	895.303147	12.156416
20.637227	898.459982	12.161421
20.330760	896.898138	12.166426
20.761311	871.602327	12.171431
20.620087	870.468856	12.176435
20.169693	874.840397	12.181440
20.140994	867.430777	12.186445
20.069344	869.506371	12.191450
20.313280	869.453949	12.196455
20.379347	862.866489	12.201459
20.277006	869.272789	12.206464
20.655566	860.770209	12.211469
20.602700	871.126372	12.216474
20.491594	868.128563	12.221479
20.695867	864.915632	12.226483
20.211797	868.554012	12.231488
20.274484	864.211957	12.236493
20.293109	867.526128	12.241498
20.147959	861.798287	12.246503
20.498568	859.543934	12.251507
20.372796	870.141145	12.256512
20.675423	869.980768	12.261517
20.419287	872.989554	12.266522
20.386043	865.755974	12.271527
20.978103	861.882886	12.276531
20.306706	845.518906	12.281536
20.485353	835.125917	12.286541
20.406900	842.079151	12.291546
20.158473	847.145911	12.296551
20.371945	837.660747	12.301555
20.260613	843.632797	12.306560
20.075844	841.703917	12.311565
20.281398	838.465115	12.316570
20.133028	841.770412	12.321575
20.457010	829.061899	12.326579
19.872163	841.625390	12.331584
20.499569	840.744212	12.336589
20.709249	838.602838	12.341594
20.375323	842.862430	12.346599
20.504422	836.937186	12.351603
20.231128	836.230959	12.356608
20.466458	836.440139	12.361613
20.009676	832.280312	12.366618
19.830056	839.802325	12.371623
20.461310	836.924345	12.376627
19.988559	842.583367	12.381632
19.850662	837.048104	12.386637
20.129782	849.819915	12.391642
20.001795	874.635651	12.396647
19.979996	867.953124	12.401651
19.940017	871.883648	12.406656
20.377553	871.784218	12.411661
20.059559	877.784608	12.416666
20.004395	881.399981	12.421671
20.459880	877.429517	12.426675
20.232177	885.919385	12.431680
20.318186	886.816523	12.436685
20.234932	880.276367	12.441690
20.547744	887.687530	12.446695
20.508818	880.756885	12.451699
20.303783	886.849226	12.456704
20.302874	882.381099	12.461709
20.410981	885.576512	12.466714
20.420132	891.424110	12.471719
20.571033	886.330754	12.476723
20.274977	882.732688	12.481728
20.739766	885.112620	12.486733
20.478619	879.100719	12.491738
20.243050	864.047499	12.496743
20.263972	856.212542	12.501747
20.012076	860.146239	12.506752
20.309337	867.796106	12.511757
20.358835	878.964446	12.516762
20.513546	875.765537	12.521767
20.235338	864.293904	12.526771
20.042702	868.534805	12.531776
20.300379	877.376047	12.536781
20.468438	882.386806	12.541786
20.509779	882.272410	12.546791
20.340611	860.219515	12.551795
20.236005	855.360629	12.556800
20.217400	852.144467	12.561805
20.152124	854.467251	12.566810
20.074980	857.840075	12.571815
20.597654	873.152861	12.576819
20.413980	872.439950	12.581824
20.087370	866.894795	12.586829
20.337455	862.957182	12.591834
20.062444	869.007435	12.596839
20.490091	872.710551	12.601843
20.274224	867.421535	12.606848
20.468961	860.765043	12.611853
20.370170	864.346839	12.616858
20.503652	858.489914	12.621863
20.400450	857.573342	12.626867
19.882650	858.326901	12.631872
19.906392	858.040263	12.636877
20.185097	865.051876	12.641882
20.482459	881.814457	12.646887
20.805983	883.219943	12.651891
20.459215	869.558258	12.656896
20.564553	865.767432	12.661901
20.160067	862.242435	12.666906
20.198724	870.027429	12.671911
20.650292	860.811292	12.676915
20.795656	864.107680	12.681920
20.359067	860.339902	12.686925
19.935969	855.303521	12.691930
19.925296	852.848616	12.696935
20.061754	856.857831	12.701939
20.150569	864.365017	12.706944
20.321380	859.135627	12.711949
20.798141	860.630099	12.716954
20.407130	863.843978	12.721959
20.700528	856.261905	12.726963
20.305936	869.374235	12.731968
20.785948	859.231924	12.736973
20.786142	860.760341	12.741978
20.605447	859.685743	12.746983
20.516448	838.528984	12.751987
20.273029	840.799415	12.756992
20.384475	829.671124	12.761997
19.993497	831.877249	12.767002
19.708537	829.360824	12.772007
19.867538	837.551870	12.777011
19.735427	853.600570	12.782016
19.863472	860.453673	12.787021
20.077201	863.039274	12.792026
20.045259	861.820754	12.797031
20.471046	866.106807	12.802035
20.054915	864.569294	12.807040
20.232396	865.847452	12.812045
20.192857	872.305352	12.817050
20.223530	866.310922	12.822055
20.180879	860.231567	12.827059
19.936708	869.392921	12.832064
20.460936	877.558475	12.837069
20.528178	888.359838	12.842074
20.386382	873.715260	12.847079
20.676724	865.972657	12.852083
20.216348	873.326116	12.857088
20.067409	866.629862	12.862093
20.453694	875.177085	12.867098
20.119684	871.259483	12.872103
20.481752	870.811814	12.877107
20.322885	867.016945	12.882112
20.286618	865.642458	12.887117
20.180925	875.528480	12.892122
20.021453	865.942638	12.897127
20.097014	863.499788	12.902131
20.154837	873.235407	12.907136
20.235320	896.882169	12.912141
20.776207	893.227448	12.917146
20.579444	881.036457	12.922151
20.586387	875.852129	12.927155
20.252042	870.841973	12.932160
20.176768	866.269760	12.937165
20.275092	879.816263	12.942170
20.162169	877.334280	12.947175
20.226764	876.491963	12.952179
19.950476	876.807018	12.957184
20.226029	877.094564	12.962189
20.671088	877.100421	12.967194
20.492273	873.818566	12.972199
20.408745	873.124801	12.977203
19.908823	883.209468	12.982208
20.091166	878.079935	12.987213
20.334449	874.225589	12.992218
20.087148	885.573501	12.997223
20.753366	874.769267	13.002227
20.186753	874.399505	13.007232
20.340009	870.210471	13.012237
20.824315	877.845643	13.017242
20.542659	881.820762	13.022247
20.648356	883.237542	13.027251
20.793987	888.046889	13.032256
20.446813	884.582716	13.037261
20.466424	883.847189	13.042266
20.140496	891.324839	13.047271
20.492977	872.497038	13.052275
20.389078	868.483143	13.057280
20.253625	863.716779	13.062285
20.191253	865.154083	13.067290
20.019002	871.095536	13.072295
20.416847	884.492403	13.077299
20.329232	883.281057	13.082304
20.472723	878.232789	13.087309
20.171358	871.496746	13.092314
20.295677	881.758592	13.097319
20.502809	881.242357	13.102323
20.072111	865.994436	13.107328
20.017912	869.743848	13.112333
20.362450	874.772504	13.117338
20.302835	883.853278	13.122343
20.427324	882.356098	13.127347
20.634298	890.385792	13.132352
20.628779	874.371425	13.137357
20.357459	863.645045	13.142362
20.328893	864.019073	13.147367
20.547273	860.517941	13.152371
20.412022	856.085486	13.157376
20.525737	852.382831	13.162381
20.371022	860.507283	13.167386
20.374829	861.991661	13.172391
20.396060	856.883441	13.177395
20.340980	864.204512	13.182400
20.607222	859.749798	13.187405
20.467429	851.974371	13.192410
20.501682	860.682203	13.197415
19.995485	860.467870	13.202419
20.199153	855.934281	13.207424
20.038870	850.451008	13.212429
20.416327	855.760983	13.217434
20.161556	865.327169	13.222439
21.000359	858.525912	13.227443
20.851094	860.947963	13.232448
20.545985	847.102711	13.237453
20.384739	835.730649	13.242458
20.562665	832.821447	13.247463
20.410321	822.018251	13.252467
20.366409	834.781882	13.257472
20.566027	831.273710	13.262477
20.421568	829.609098	13.267482
20.153478	833.478066	13.272487
20.390760	829.452264	13.277491
19.883432	837.660448	13.282496
19.928478	834.487060	13.287501
20.002864	831.588505	13.292506
20.101591	823.758383	13.297511
19.872859	826.139975	13.302515
19.676554	842.649266	13.307520
20.084285	858.956330	13.312525
20.218708	862.535641	13.317530
20.404892	866.282917	13.322535
20.207575	863.238311	13.327539
20.379360	873.466751	13.332544
20.381894	872.726257	13.337549
20.625014	867.522756	13.342554
20.153136	872.176658	13.347559
20.605802	864.491487	13.352563
20.353156	865.087088	13.357568
20.528253	862.629936	13.362573
20.184498	853.028724	13.367578
20.141233	871.202036	13.372583
20.599008	866.318568	13.377587
20.092499	852.198374	13.382592
20.038275	853.750330	13.387597
20.239243	864.808613	13.392602
20.095696	872.945762	13.397607
20.272738	874.250047	13.402611
20.294477	875.081626	13.407616
20.169723	877.746973	13.412621
20.193196	869.242901	13.417626
19.857979	875.140455	13.422631
20.458575	872.069965	13.427635
20.076656	872.690098	13.432640
20.032450	865.451293	13.437645
20.552664	864.367048	13.442650
19.968617	870.924225	13.447655
20.001192	865.560247	13.452659
19.949195	870.447286	13.457664
20.172664	872.972799	13.462669
20.145952	870.218278	13.467674
20.072630	868.438047	13.472679
20.186938	880.131318	13.477683
20.365276	895.445926	13.482688
20.298382	899.261863	13.487693
20.635506	893.160409	13.492698
20.415770	891.816191	13.497703
20.312060	873.777511	13.502707
20.177672	871.232500	13.507712
20.234696	870.038593	13.512717
20.217330	871.334763	13.517722
20.606701	872.333044	13.522727
20.516995	863.107867	13.527731
20.552537	874.336227	13.532736
20.637133	876.415822	13.537741
20.699213	872.992405	13.542746
20.370302	884.349571	13.547751
20.688451	867.701439	13.552755
20.631650	883.380818	13.557760
20.733476	859.993457	13.562765
20.216429	849.378294	13.567770
19.964140	852.628781	13.572775
20.205828	849.913508	13.577779
20.376520	866.590819	13.582784
20.037526	870.861945	13.587789
20.458807	868.238244	13.592794
20.399608	871.576021	13.597799
20.421417	858.884555	13.602803
20.549179	854.983706	13.607808
19.955594	847.559236	13.612813
19.840768	843.169466	13.617818
19.932781	863.083224	13.622823
20.721599	870.672499	13.627827
20.446824	876.363116	13.632832
20.490655	887.491381	13.637837
20.683042	858.518859	13.642842
20.460229	851.611070	13.647847
20.343257	838.651315	13.652851
20.116925	846.023844	13.657856
20.155214	836.155830	13.662861
20.081069	845.845770	13.667866
20.039733	848.636544	13.672871
20.416611	853.866882	13.677875
20.057108	863.972856	13.682880
20.134408	875.827992	13.687885
20.257113	868.088077	13.692890
20.271750	880.638816	13.697895
20.476303	869.653216	13.702899
20.006130	876.836254	13.707904
20.017672	883.852234	13.712909
20.543852	883.632608	13.717914
19.915225	891.280574	13.722919
20.399894	881.113373	13.727923
20.232387	882.422259	13.732928
20.249697	884.852859	13.737933
20.580445	881.702713	13.742938
20.171102	889.686892	13.747943
20.065653	884.508806	13.752947
19.768816	875.703995	13.757952
20.357721	885.875533	13.762957
20.212907	886.345675	13.767962
19.676358	885.792736	13.772967
20.049812	881.194505	13.777971
19.934125	886.415753	13.782976
20.225025	886.770930	13.787981
20.199047	897.282761	13.792986
20.197983	911.897893	13.797991
20.500742	913.455754	13.802995
20.071217	910.806998	13.808000
20.327941	913.745231	13.813005
20.388944	907.162173	13.818010
20.514233	918.510964	13.823015
20.712967	889.506112	13.828019
20.644445	885.563909	13.833024
20.257654	896.758906	13.838029
20.439757	881.450904	13.843034
20.100417	885.925380	13.848039
20.312111	881.691981	13.853043
20.116778	885.224809	13.858048
20.175117	882.679516	13.863053
20.423968	876.459784	13.868058
19.755007	886.436464	13.873063
20.366499	878.678661	13.878067
20.469421	882.064039	13.883072
20.081151	887.194260	13.888077
20.365863	885.744214	13.893082
20.168664	883.479176	13.898087
20.261793	886.686631	13.903091
20.022047	891.699023	13.908096
20.405197	899.246156	13.913101
20.654092	898.073034	13.918106
20.516163	894.821665	13.923111
20.337392	885.401353	13.928115
20.370830	894.384864	13.933120
20.065702	886.001463	13.938125
20.658026	894.508634	13.943130
20.235465	888.016780	13.948135
20.540664	885.238508	13.953139
20.083749	886.069654	13.958144
20.235188	892.940075	13.963149
20.534986	881.093810	13.968154
20.491683	889.101282	13.973159
20.235137	888.897041	13.978163
20.385697	887.195262	13.983168
20.439323	895.623875	13.988173
20.754519	881.853423	13.993178
20.408364	893.778411	13.998183
20.667560	891.373940	14.003187
20.429804	891.452655	14.008192
20.147393	895.626558	14.013210
20.345816	894.425993	14.018227
20.328013	891.652961	14.023245
20.505305	889.966228	14.028263
20.681017	887.803362	14.033280
19.958182	873.283617	14.038298
20.193245	872.653575	14.043315
20.093712	888.871602	14.048333
20.638054	885.535629	14.053351
20.490507	894.514244	14.058368
20.367764	892.361600	14.063386
20.772286	890.551258	14.068403
20.295620	883.858642	14.073421
20.620307	880.959171	14.078439
20.516703	890.279876	14.083456
20.394001	891.888067	14.088474
20.597408	882.181052	14.093491
20.491743	891.755274	14.098509
20.494079	885.556156	14.103527
20.406662	892.657820	14.108544
20.496722	895.352038	14.113562
20.409420	893.356319	14.118579
20.720783	902.996852	14.123597
20.705707	886.532023	14.128615
20.473409	888.166485	14.133632
20.716900	892.614025	14.138650
20.902417	888.024144	14.143667
20.464602	900.859436	14.148685
20.457792	896.089916	14.153703
21.022813	894.247726	14.158720
21.056427	892.918716	14.163738
21.216700	890.249806	14.168755
21.065211	902.333608	14.173773
20.945606	895.425823	14.178791
21.106527	897.828743	14.183808
20.678567	903.061129	14.188826
20.791648	889.040215	14.193843
20.637104	900.971774	14.198861
20.752679	900.380330	14.203879
20.808570	902.264219	14.208896
20.513362	903.616932	14.213914
20.916778	914.636258	14.218931
20.716718	927.655232	14.223949
20.996954	922.635691	14.228967
21.182419	922.268891	14.233984
21.004857	928.286356	14.239002
21.159086	928.082007	14.244019
21.248424	929.959378	14.249037
21.116492	923.245437	14.254055
21.512298	913.611722	14.259072
21.191397	926.484474	14.264090
21.276542	921.649571	14.269107
21.105817	921.131229	14.274125
21.067100	921.046186	14.279143
21.246101	927.286393	14.284160
20.777088	925.567937	14.289178
21.374929	925.306036	14.294195
21.280871	922.073997	14.299213
21.220666	919.493673	14.304231
21.284988	922.625799	14.309248
20.955479	922.091370	14.314266
21.367493	925.184359	14.319283
21.325335	925.852706	14.324301
21.500506	921.962661	14.329319
21.513408	922.379821	14.334336
21.463071	927.472665	14.339354
21.624318	917.592137	14.344371
21.439694	918.056943	14.349389
21.262207	926.190660	14.354407
21.663125	920.285023	14.359424
21.282428	924.968337	14.364442
21.782506	928.794697	14.369459
21.984759	935.177780	14.374477
22.063670	928.315477	14.379495
22.071099	922.048144	14.384512
21.892218	916.997471	14.389530
22.218921	915.828064	14.394547
21.762459	917.713572	14.399565
21.776871	919.667965	14.404583
22.119587	918.774176	14.409600
21.711157	926.915202	14.414618
21.681047	921.757126	14.419635
21.721539	927.853355	14.424653
21.751792	915.047870	14.429671
21.752158	919.161882	14.434688
21.618752	923.603574	14.439706
21.741657	910.631805	14.444723
21.743585	920.665578	14.449741
21.660189	916.575757	14.454759
21.796494	914.212545	14.459776
21.934913	911.514305	14.464794
21.743640	917.271897	14.469811
21.632500	914.745979	14.474829
21.494137	920.324412	14.479847
21.920572	930.569679	14.484864
21.741370	949.268502	14.489882
22.084589	940.920635	14.494899
22.322524	947.097199	14.499917
22.207583	943.636832	14.504935
22.308832	942.127315	14.509952
21.733977	952.267478	14.514970
22.011983	944.576104	14.519987
22.370748	944.541030	14.525005
22.048061	933.986723	14.530023
22.160430	933.472997	14.535040
22.291420	936.933086	14.540058
22.305274	939.732509	14.545075
22.446786	932.986644	14.550093
22.116151	946.901301	14.555111
22.581732	944.363907	14.560128
22.356725	944.189929	14.565146
22.435130	942.555974	14.570163
22.224346	945.051766	14.575181
21.975994	941.689080	14.580199
22.351294	941.140117	14.585216
22.173383	943.542472	14.590234
22.563611	936.946495	14.595251
22.567353	942.319852	14.600269
22.222494	949.105029	14.605287
22.496622	940.597737	14.610304
22.593150	952.614644	14.615322
22.481782	950.433662	14.620339
22.410569	947.959557	14.625357
22.041388	950.806542	14.630375
21.988334	945.994932	14.635392
22.053289	965.695678	14.640410
22.716881	964.927592	14.645427
22.846750	974.865838	14.650445
22.701578	978.332337	14.655463
22.977270	968.412075	14.660480
22.772804	978.861611	14.665498
22.604838	978.940862	14.670515
23.077627	974.088697	14.675533
23.265898	977.759067	14.680551
23.210455	965.093438	14.685568
23.087036	959.500138	14.690586
22.799492	944.772223	14.695603
22.790180	946.023557	14.700621
22.725553	942.173833	14.705639
23.011918	939.346280	14.710656
22.788646	950.883732	14.715674
22.706204	945.345620	14.720691
22.915500	957.951108	14.725709
23.174881	969.877112	14.730727
23.487412	968.514844	14.735744
23.332909	960.304271	14.740762
23.212475	942.858960	14.745779
23.208452	942.151790	14.750797
22.663677	943.996534	14.755815
23.142121	942.048702	14.760832
23.059957	946.286721	14.765850
22.864709	949.461780	14.770867
23.485097	946.917136	14.775885
22.755976	952.735850	14.780903
23.031898	953.622909	14.785920
22.971283	978.111237	14.790938
23.439774	970.850212	14.795955
23.596781	973.770776	14.800973
23.303872	977.686252	14.805991
23.287963	978.096936	14.811008
23.259808	977.623837	14.816026
23.109945	973.856833	14.821043
23.324048	968.025336	14.826061
23.015333	980.592875	14.831079
23.465124	975.533223	14.836096
23.347096	977.705618	14.841114
23.652551	969.538236	14.846131
23.984838	973.298881	14.851149
23.809679	975.351534	14.856167
23.982140	963.461056	14.861184
23.853029	949.921008	14.866202
23.802504	941.912316	14.871219
23.822123	928.648379	14.876237
23.963017	933.038320	14.881255
23.738943	936.864420	14.886272
23.679445	936.079355	14.891290
23.602126	941.262267	14.896307
23.133517	934.458792	14.901325
23.165806	943.743630	14.906343
23.485203	938.988646	14.911360
23.337740	953.892044	14.916378
23.565184	966.725150	14.921395
23.578091	968.410106	14.926413
23.700034	969.327109	14.931431
23.743976	973.065925	14.936448
23.462535	969.802613	14.941466
23.342414	968.134578	14.946483
23.770969	970.394767	14.951501
23.740029	975.098451	14.956519
23.848419	986.352279	14.961536
23.912800	993.220471	14.966554
24.233129	997.573760	14.971571
24.300628	990.794888	14.976589
23.932540	973.495946	14.981607
24.100414	966.964064	14.986624
23.649332	978.217345	14.991642
23.774056	995.953037	14.996659
24.331907	995.113703	15.001677
23.897346	1002.047361	15.006695
24.156671	998.765743	15.011712
24.247026	991.774671	15.016730
24.641462	988.372247	15.021747
24.679658	976.278780	15.026765
24.787421	970.637179	15.031783
24.978498	952.532112	15.036800
24.599327	957.440384	15.041818
24.517095	952.221545	15.046835
25.131998	946.844206	15.051853
24.606782	949.637622	15.056871
24.506402	931.442384	15.061888
24.398355	932.193686	15.066906
24.218269	921.952753	15.071923
24.545805	928.453339	15.076941
24.901753	942.255791	15.081959
24.476705	926.171070	15.086976
24.437977	923.552021	15.091994
24.447422	925.702554	15.097011
24.722825	917.181275	15.102029
24.389782	922.628510	15.107047
24.648900	912.649311	15.112064
24.411542	917.161975	15.117082
24.605421	929.547630	15.122099
25.003498	934.013563	15.127117
25.132562	929.879438	15.132135
24.928330	922.760546	15.137152
24.861086	914.908287	15.142170
24.411585	919.301015	15.147187
24.543424	910.004701	15.152205
24.443704	924.909730	15.157223
24.568594	925.185242	15.162240
24.747296	941.126867	15.167258
24.675370	947.061264	15.172275
25.220284	941.289996	15.177293
25.013165	947.149141	15.182311
24.985484	945.639285	15.187328
25.185751	947.390153	15.192346
24.758812	939.904293	15.197363
24.904745	933.474225	15.202381
24.929350	947.072844	15.207399
24.749233	945.801341	15.212416
25.029906	947.460466	15.217434
24.906062	953.980966	15.222451
24.880601	946.239252	15.227469
24.565779	957.539633	15.232487
24.708853	956.396194	15.237504
24.853333	945.794070	15.242522
24.645542	958.727382	15.247539
25.137454	973.350697	15.252557
25.158516	987.216903	15.257575
25.279729	985.099590	15.262592
25.323401	985.105152	15.267610
24.937344	986.741575	15.272627
25.064515	988.980994	15.277645
25.097317	992.071684	15.282663
25.448794	996.716896	15.287680
25.192021	989.535717	15.292698
24.671191	988.232462	15.297715
25.170851	985.697881	15.302733
25.268076	991.562346	15.307751
25.376392	1011.852605	15.312768
26.046946	1000.239718	15.317786
25.605953	1002.571431	15.322803
26.048715	998.930389	15.327821
25.542166	993.831925	15.332839
25.590848	990.070643	15.337856
26.111268	981.580555	15.342874
25.687352	989.588434	15.347891
25.935377	982.398275	15.352909
25.834765	982.717962	15.357927
25.239107	993.446795	15.362944
25.383654	983.698624	15.367962
25.392178	983.420824	15.372979
25.863365	987.700606	15.377997
25.971630	1002.651945	15.383015
25.835525	994.287796	15.388032
26.039766	989.063927	15.393050
25.606679	988.976414	15.398067
26.113658	993.522125	15.403085
25.936942	988.052527	15.408103
25.789615	987.447882	15.413120
25.828304	991.498647	15.418138
25.708663	996.430550	15.423155
25.918667	1006.694470	15.428173
25.918947	1009.984059	15.433191
25.510082	1006.022067	15.438208
25.805681	1006.739603	15.443226
25.723113	1008.401953	15.448243
26.159728	1008.657489	15.453261
25.854416	1007.457842	15.458279
25.961156	1009.103878	15.463296
26.316080	1008.848583	15.468314
26.004176	1009.349388	15.473331
26.360190	1028.794788	15.478349
26.236309	1030.270903	15.483367
26.349252	1037.178823	15.488384
26.564490	1026.765706	15.493402
26.359360	1022.279771	15.498419
26.087563	1008.859023	15.503437
26.508293	1015.657861	15.508455
26.357714	1026.992342	15.513472
26.416542	1026.660638	15.518490
26.680692	1032.644935	15.523507
26.601181	1029.675357	15.528525
26.537609	1013.709292	15.533543
26.283534	1013.908431	15.538560
26.719558	1015.381076	15.543578
26.413263	1025.229163	15.548595
26.921609	1026.432700	15.553613
26.965710	1020.052734	15.558631
26.584295	1004.452215	15.563648
26.700445	1004.270537	15.568666
26.560891	996.988544	15.573683
26.076760	996.161703	15.578701
26.893112	1010.945191	15.583719
26.906989	1025.820209	15.588736
26.959619	1024.044986	15.593754
26.917365	1027.724573	15.598771
26.916317	1025.378200	15.603789
27.220270	1018.222140	15.608807
26.674519	1013.556402	15.613824
27.004092	1010.923410	15.618842
27.002878	1016.157477	15.623859
26.970911	1020.821190	15.628877
26.521031	1017.811957	15.633895
26.732821	1034.613415	15.638912
27.227507	1021.142351	15.643930
27.128930	1031.125313	15.648947
27.067004	1028.598813	15.653965
27.143450	1022.925551	15.658983
27.043629	1032.881954	15.664000
27.042827	1026.655756	15.669018
26.971331	1028.750490	15.674035
27.032419	1019.896978	15.679053
27.075928	1032.578986	15.684071
27.026229	1033.835283	15.689088
27.059599	1029.691946	15.694106
27.298112	1035.960973	15.699123
26.819433	1035.475344	15.704141
26.914630	1039.314451	15.709159
27.091249	1057.142110	15.714176
27.471475	1058.071926	15.719194
27.630889	1057.351692	15.724211
27.534112	1050.902553	15.729229
27.728320	1059.928189	15.734247
27.421392	1056.071550	15.739264
27.383831	1052.958546	15.744282
27.566741	1056.474331	15.749299
27.282407	1053.121727	15.754317
27.383096	1053.741177	15.759335
27.464788	1054.460742	15.764352
27.587965	1049.370050	15.769370
27.272453	1054.376894	15.774387
27.540116	1049.623659	15.779405
27.878939	1053.055228	15.784423
27.800661	1056.502007	15.789440
27.832021	1048.711520	15.794458
28.016352	1048.800060	15.799475
27.872334	1057.521848	15.804493
27.954158	1053.899366	15.809511
27.726655	1054.626662	15.814528
27.807723	1046.093747	15.819546
27.661642	1043.600572	15.824563
27.767929	1051.353002	15.829581
27.692746	1047.878314	15.834599
27.560093	1072.842559	15.839616
28.230267	1064.368880	15.844634
28.564876	1083.747542	15.849651
28.584949	1076.805885	15.854669
28.743885	1046.856201	15.859687
28.133234	1050.008005	15.864704
28.414235	1044.806786	15.869722
28.296605	1042.865463	15.874739
28.565237	1044.293970	15.879757
28.419714	1037.767755	15.884775
28.189019	1038.231014	15.889792
28.304276	1048.009204	15.894810
28.611818	1034.781252	15.899827
28.502081	1039.683515	15.904845
29.021060	1033.709167	15.909863
28.499000	1040.624770	15.914880
28.597804	1027.528287	15.919898
28.452640	1016.314707	15.924915
28.382456	1009.090504	15.929933
28.345458	1015.641025	15.934951
28.515788	1035.988011	15.939968
28.193733	1040.069927	15.944986
28.461713	1040.894963	15.950003
28.197072	1059.966465	15.955021
28.687045	1038.664960	15.960039
28.586460	1044.677935	15.965056
28.427045	1049.637541	15.970074
28.399689	1040.304266	15.975091
28.642749	1052.753639	15.980109
28.770124	1041.303144	15.985127
28.310243	1045.791000	15.990144
28.373364	1051.384545	15.995162
28.573031	1054.371438	16.000179
28.673844	1072.648754	16.005197
29.021197	1068.259042	16.010215
28.887657	1082.455010	16.015232
29.191416	1077.192788	16.020250
28.711734	1076.942779	16.025267
28.634971	1081.598047	16.030285
28.579656	1076.065081	16.035303
28.685474	1086.759937	16.040320
28.546238	1079.630223	16.045338
28.833517	1073.521950	16.050355
28.691124	1083.286064	16.055373
28.971131	1091.702873	16.060391
29.021964	1105.399109	16.065408
29.382219	1108.549044	16.070426
29.844462	1101.222491	16.075443
29.424031	1103.615658	16.080461
29.445439	1081.586498	16.085479
29.280658	1081.609688	16.090496
28.909369	1070.734857	16.095514
29.215642	1088.114703	16.100531
29.152541	1097.565604	16.105549
29.143244	1099.112245	16.110567
29.619249	1110.769705	16.115584
29.732454	1106.448869	16.120602
29.654206	1107.299408	16.125619
29.622125	1105.762337	16.130637
29.978725	1096.925444	16.135655
29.690833	1099.275413	16.140672
29.889092	1084.957809	16.145690
29.484566	1081.735262	16.150707
29.280584	1079.646916	16.155725
29.620523	1079.480810	16.160743
29.710043	1094.792956	16.165760
29.725101	1102.461440	16.170778
30.082216	1101.130890	16.175795
30.187497	1095.431397	16.180813
30.056053	1078.405961	16.185831
30.032059	1073.857063	16.190848
29.723067	1071.209912	16.195866
29.895507	1068.922376	16.200883
29.562236	1069.599299	16.205901
29.792103	1076.545461	16.210919
30.052014	1091.829967	16.215936
30.008663	1104.181625	16.220954
30.346233	1097.728083	16.225971
30.042649	1101.226492	16.230989
30.215022	1089.161512	16.236007
30.188763	1082.627036	16.241024
30.085989	1082.075383	16.246042
29.970929	1084.522892	16.251059
29.711625	1091.680890	16.256077
30.312020	1096.207861	16.261095
30.188124	1103.757245	16.266112
30.123240	1101.887191	16.271130
30.294481	1099.186049	16.276147
30.344628	1101.493418	16.281165
30.345685	1096.913052	16.286183
30.324540	1100.794957	16.291200
30.202925	1101.064307	16.296218
30.591284	1095.419439	16.301235
30.058965	1100.979252	16.306253
30.267713	1087.659524	16.311271
30.290719	1100.814820	16.316288
30.042720	1101.359005	16.321306
30.580823	1107.211711	16.326323
30.159654	1130.158832	16.331341
30.587649	1136.484003	16.336359
30.656295	1136.577810	16.341376
30.729868	1136.216802	16.346394
30.844833	1130.823927	16.351411
30.602953	1131.657636	16.356429
30.765745	1130.604118	16.361447
30.731984	1130.656423	16.366464
30.337337	1131.583651	16.371482
30.847786	1121.015915	16.376499
30.447543	1133.610687	16.381517
30.648712	1125.400863	16.386535
30.865956	1129.486017	16.391552
30.619445	1129.050350	16.396570
31.281015	1141.280394	16.401587
30.827189	1138.176531	16.406605
31.171198	1149.057380	16.411623
31.290718	1154.930685	16.416640
31.157500	1149.513418	16.421658
31.565177	1131.811986	16.426675
31.155474	1140.252181	16.431693
31.130220	1121.678459	16.436711
31.161664	1121.410902	16.441728
31.236007	1130.081118	16.446746
31.374155	1123.025883	16.451763
31.011922	1136.984711	16.456781
31.325891	1148.128210	16.461799
31.687611	1149.387213	16.466816
31.377796	1153.716684	16.471834
31.283486	1150.538581	16.476851
31.544274	1156.850299	16.481869
31.518535	1157.494579	16.486887
31.814621	1159.084939	16.491904
31.642637	1155.039772	16.496922
31.647379	1143.601172	16.501939
31.615278	1134.763571	16.506957
31.199282	1119.592911	16.511975
31.231046	1145.611838	16.516992
31.238921	1142.174074	16.522010
31.690485	1144.661859	16.527027
31.803321	1152.693946	16.532045
31.776621	1148.421889	16.537063
31.604114	1148.674373	16.542080
31.583246	1154.049267	16.547098
31.856357	1145.513690	16.552115
31.471760	1158.618435	16.557133
31.575203	1148.056676	16.562151
31.849143	1168.542382	16.567168
31.593380	1175.110791	16.572186
31.988145	1171.874819	16.577203
31.874381	1180.961595	16.582221
32.016334	1183.758786	16.587239
32.276776	1175.936442	16.592256
32.110540	1174.016822	16.597274
32.566380	1175.448288	16.602291
32.522533	1180.900365	16.607309
32.179059	1178.225245	16.612327
32.534208	1179.243628	16.617344
32.577013	1177.379120	16.622362
32.819885	1165.265771	16.627379
32.304529	1155.311710	16.632397
32.155942	1150.871165	16.637415
32.400748	1145.705648	16.642432
32.296100	1144.485761	16.647450
32.707008	1149.300765	16.652467
32.590061	1141.539202	16.657485
32.275021	1141.672805	16.662503
32.531717	1140.163785	16.667520
32.525911	1145.664056	16.672538
32.470335	1161.239350	16.677555
32.011626	1175.725815	16.682573
32.147456	1176.646355	16.687591
32.662464	1177.664104	16.692608
32.319309	1183.746281	16.697626
32.356295	1187.193406	16.702643
32.231597	1192.130568	16.707661
32.571025	1199.124149	16.712679
33.479533	1190.654821	16.717696
33.432849	1186.064502	16.722714
33.527138	1174.714471	16.727731
33.153009	1169.721207	16.732749
33.022682	1166.296895	16.737767
33.288227	1152.657508	16.742784
33.161595	1154.469171	16.747802
33.181441	1159.026791	16.752819
33.417494	1153.421400	16.757837
33.131340	1154.404444	16.762855
33.367961	1162.917319	16.767872
33.478923	1157.537720	16.772890
33.798266	1148.435512	16.777907
33.659590	1139.494125	16.782925
33.106960	1130.239827	16.787943
33.667115	1127.552717	16.792960
32.958197	1129.459876	16.797978
32.950853	1115.618864	16.802995
33.091468	1130.324212	16.808013
32.937950	1143.552725	16.813031
33.190535	1151.460451	16.818048
32.974820	1159.811882	16.823066
33.385154	1161.675984	16.828083
33.252830	1153.627660	16.833101
33.022966	1164.613209	16.838119
33.143191	1163.683137	16.843136
33.015687	1179.564504	16.848154
33.604799	1183.995003	16.853171
33.486836	1191.474903	16.858189
33.921348	1188.896731	16.863207
33.932832	1180.627266	16.868224
33.598093	1188.614838	16.873242
33.663858	1181.601911	16.878259
33.522539	1180.170181	16.883277
33.630668	1185.776532	16.888295
34.319840	1178.513407	16.893312
34.009947	1189.966272	16.898330
33.694993	1182.955226	16.903347
33.883778	1189.690356	16.908365
33.836312	1199.352041	16.913383
33.962030	1206.034994	16.918400
34.475319	1195.643505	16.923418
34.899002	1199.596033	16.928435
34.784783	1181.324523	16.933453
34.615788	1169.239261	16.938471
34.885248	1163.057231	16.943488
34.553669	1165.615108	16.948506
34.814667	1160.781481	16.953523
34.865922	1142.289899	16.958541
34.611475	1139.209337	16.963559
34.520216	1127.261578	16.968576
34.340419	1130.905712	16.973594
34.335931	1137.595998	16.978611
34.599244	1132.758044	16.983629
34.283390	1142.088121	16.988647
34.447758	1128.772817	16.993664
34.422792	1127.289252	16.998682
34.449371	1133.439132	17.003699
34.373491	1135.158620	17.008717
34.470283	1160.491965	17.013735
34.607768	1168.150123	17.018752
34.384980	1172.555630	17.023770
34.613140	1163.615120	17.028787
34.598013	1168.257091	17.033805
34.248275	1159.450310	17.038823
34.753275	1158.431434	17.043840
34.486110	1168.246129	17.048858
34.774897	1169.112097	17.053875
34.720203	1186.219269	17.058893
34.912886	1192.787972	17.063911
35.259037	1190.558439	17.068928
34.900101	1194.729007	17.073946
35.283470	1194.430642	17.078963
35.498349	1195.734118	17.083981
35.142863	1208.698471	17.088999
35.242860	1198.262869	17.094016
35.405605	1199.518980	17.099034
35.049463	1197.225192	17.104051
34.939248	1187.546164	17.109069
34.729294	1196.407689	17.114087
35.092733	1190.930064	17.119104
35.044118	1199.144591	17.124122
35.165176	1200.460216	17.129139
35.093636	1196.879350	17.134157
35.090181	1203.278519	17.139175
35.490524	1213.277249	17.144192
35.570588	1215.833069	17.149210
35.812170	1216.197644	17.154227
35.868356	1226.249480	17.159245
35.705724	1228.743360	17.164263
36.260763	1223.304927	17.169280
35.882857	1208.726514	17.174298
35.559290	1201.054681	17.179315
35.784834	1200.224276	17.184333
35.595289	1210.349730	17.189351
35.451200	1216.936808	17.194368
35.711782	1225.164486	17.199386
35.815671	1231.460611	17.204403
35.897229	1229.521731	17.209421
35.864843	1225.257321	17.214439
36.156130	1213.416365	17.219456
35.963912	1227.910343	17.224474
35.917606	1233.581381	17.229491
36.110249	1213.443300	17.234509
36.011728	1229.069729	17.239527
35.926174	1224.411648	17.244544
36.080396	1222.329592	17.249562
36.195167	1224.566447	17.254579
36.311451	1222.599565	17.259597
35.912638	1233.324341	17.264615
35.769677	1239.158814	17.269632
35.996215	1250.845371	17.274650
36.190294	1255.938941	17.279667
36.196766	1252.078131	17.284685
36.366041	1262.245258	17.289703
36.346183	1258.121616	17.294720
36.162484	1249.826912	17.299738
36.402671	1257.725006	17.304755
36.687824	1265.058263	17.309773
36.661399	1279.171080	17.314791
37.249501	1280.373565	17.319808
37.108117	1265.968345	17.324826
36.886661	1259.426313	17.329843
36.827874	1248.314300	17.334861
36.757226	1247.841785	17.339879
36.509692	1247.986257	17.344896
36.832810	1246.558760	17.349914
37.091923	1253.827967	17.354931
37.183097	1245.608197	17.359949
36.959275	1249.980829	17.364967
37.193272	1244.949033	17.369984
37.156591	1249.104527	17.375002
36.935558	1252.119881	17.380019
36.771312	1242.078793	17.385037
36.877010	1254.557785	17.390055
37.208056	1267.254078	17.395072
37.354834	1274.220875	17.400090
37.036173	1280.145727	17.405107
37.102628	1273.045231	17.410125
36.599344	1278.242619	17.415143
36.558091	1279.445121	17.420160
36.831486	1283.241926	17.425178
36.943150	1301.979894	17.430195
37.911414	1289.060138	17.435213
37.837089	1290.016716	17.440231
37.861446	1291.565480	17.445248
38.101579	1284.250936	17.450266
38.006048	1269.848482	17.455283
38.105168	1256.919088	17.460301
38.146796	1260.664671	17.465319
38.241454	1256.408396	17.470336
38.022570	1262.222033	17.475354
37.882075	1263.360439	17.480371
37.681406	1258.466157	17.485389
37.836637	1261.231951	17.490407
37.741213	1252.405534	17.495424
38.116845	1263.203084	17.500442
38.082047	1262.911444	17.505459
38.553273	1256.036860	17.510477
37.802289	1267.147654	17.515495
38.009916	1259.048079	17.520512
38.157660	1262.639632	17.525530
38.028365	1265.931410	17.530547
38.389221	1265.017169	17.535565
37.988592	1263.186940	17.540583
37.892704	1256.337924	17.545600
38.080737	1260.397016	17.550618
37.810320	1265.250514	17.555635
37.805791	1256.705386	17.560653
37.814123	1271.379605	17.565671
38.151040	1280.919135	17.570688
38.328922	1288.566489	17.575706
37.955456	1291.794614	17.580723
38.358202	1292.426073	17.585741
38.490498	1292.653469	17.590759
38.013313	1292.720768	17.595776
38.693982	1306.020592	17.600794
38.383535	1320.848338	17.605811
38.753900	1322.099969	17.610829
38.720595	1325.602487	17.615847
38.497112	1317.665384	17.620864
38.716345	1322.259740	17.625882
38.320526	1329.395577	17.630899
38.994352	1323.105573	17.635917
38.954146	1324.315380	17.640935
38.811460	1325.585674	17.645952
38.965702	1311.366362	17.650970
38.791869	1316.484836	17.655987
39.006505	1321.669006	17.661005
38.911060	1316.697999	17.666023
38.905251	1325.071016	17.671040
39.160431	1326.193957	17.676058
39.203384	1337.493515	17.681075
39.372588	1335.982153	17.686093
39.461753	1345.467340	17.691111
39.740898	1343.746561	17.696128
40.047584	1329.937354	17.701146
39.334790	1319.825288	17.706163
39.518948	1307.447856	17.711181
39.543817	1311.090804	17.716199
39.306302	1305.926817	17.721216
39.729120	1305.154325	17.726234
39.636252	1312.213017	17.731251
39.340007	1305.521569	17.736269
39.497090	1308.670155	17.741287
39.536185	1326.134267	17.746304
39.684252	1331.471991	17.751322
39.731709	1336.902956	17.756339
39.800759	1336.071026	17.761357
39.998097	1345.477033	17.766375
39.826205	1341.916095	17.771392
40.334804	1336.747419	17.776410
40.222319	1332.095497	17.781427
40.243516	1324.727517	17.786445
39.935194	1317.847961	17.791463
39.900152	1325.255042	17.796480
40.294524	1325.833603	17.801498
40.338410	1325.202461	17.806515
40.523968	1328.873380	17.811533
40.505199	1312.262265	17.816551
40.049088	1304.292604	17.821568
40.288965	1294.822408	17.826586
40.082718	1299.331029	17.831603
40.201465	1317.858336	17.836621
40.278488	1330.762813	17.841639
40.063812	1334.019239	17.846656
40.519054	1316.632699	17.851674
40.619750	1334.781593	17.856691
40.494344	1325.485432	17.861709
40.794951	1321.206823	17.866727
40.495978	1327.250768	17.871744
40.747553	1326.509997	17.876762
40.742448	1329.991539	17.881779
40.585948	1329.879438	17.886797
40.476548	1336.806712	17.891815
40.373840	1334.233605	17.896832
40.723806	1321.779700	17.901850
40.402664	1326.992337	17.906867
40.811545	1338.417364	17.911885
41.110945	1344.892632	17.916903
41.002660	1351.405512	17.921920
41.096907	1347.138258	17.926938
40.849809	1342.786207	17.931955
40.977505	1343.612475	17.936973
41.023436	1342.752222	17.941991
41.221042	1341.873446	17.947008
41.425446	1336.113955	17.952026
41.185441	1343.961731	17.957043
41.583464	1342.201278	17.962061
41.459980	1347.201672	17.967079
41.457195	1344.617339	17.972096
41.488309	1345.491270	17.977114
41.388003	1345.651056	17.982131
41.494973	1336.129993	17.987149
41.837419	1342.086026	17.992167
41.518109	1343.880345	17.997184
41.826614	1342.299820	18.002202
41.422999	1342.432072	18.007219
41.938099	1344.950734	18.012237
42.108444	1336.933108	18.017255
41.834067	1345.227367	18.022272
41.865159	1332.111132	18.027290
41.658780	1337.773034	18.032307
41.820054	1333.938030	18.037325
41.836463	1341.474893	18.042343
41.812115	1341.603150	18.047360
41.565617	1331.241038	18.052378
41.545489	1346.967935	18.057395
41.766805	1356.698212	18.062413
42.021878	1365.639569	18.067431
41.786569	1376.889216	18.072448
42.020878	1367.252593	18.077466
42.075749	1374.838000	18.082483
42.120611	1374.005097	18.087501
41.919606	1371.204721	18.092519
42.235563	1389.888084	18.097536
42.524673	1396.979366	18.102554
42.439644	1400.763234	18.107571
42.702915	1399.198727	18.112589
42.929554	1395.130042	18.117607
42.774733	1400.120076	18.122624
42.798526	1376.070225	18.127642
42.484160	1364.953911	18.132659
42.890948	1369.997271	18.137677
42.958072	1372.722673	18.142695
42.546475	1363.591312	18.147712
42.806187	1365.505674	18.152730
42.898099	1376.887032	18.157747
42.748486	1383.548756	18.162765
43.244660	1382.240410	18.167783
42.743650	1383.005949	18.172800
43.190937	1379.913308	18.177818
43.262828	1382.747353	18.182835
43.302425	1379.692321	18.187853
43.002479	1362.980132	18.192871
42.877708	1374.391943	18.197888
43.102032	1379.567778	18.202906
42.914418	1390.261177	18.207923
43.103139	1380.857185	18.212941
43.125833	1380.145415	18.217959
42.810132	1384.118446	18.222976
43.373451	1384.977521	18.227994
43.377451	1385.180453	18.233011
43.039072	1392.917155	18.238029
43.436415	1400.797829	18.243047
43.224633	1412.094259	18.248064
43.435626	1421.534195	18.253082
43.779407	1421.966695	18.258099
43.577705	1413.209593	18.263117
43.722128	1411.960764	18.268135
43.224671	1428.058973	18.273152
43.557272	1414.833885	18.278170
43.545243	1423.069032	18.283187
44.269629	1435.822842	18.288205
44.367459	1434.097703	18.293223
43.913579	1432.293119	18.298240
43.888460	1419.246296	18.303258
44.054762	1423.094570	18.308275
44.112145	1438.987814	18.313293
44.349914	1440.368891	18.318311
44.378658	1442.602414	18.323328
44.408760	1438.954850	18.328346
44.592130	1435.111309	18.333363
44.308769	1420.676344	18.338381
44.462551	1415.447203	18.343399
44.116867	1417.355511	18.348416
44.113064	1429.062793	18.353434
44.332759	1431.694720	18.358451
44.131816	1440.908020	18.363469
44.428105	1438.083797	18.368487
44.370935	1437.266020	18.373504
44.253263	1442.380813	18.378522
44.687650	1442.904483	18.383539
44.335551	1451.343630	18.388557
44.977719	1461.188453	18.393575
45.164194	1466.664140	18.398592
44.909230	1465.296753	18.403610
44.857824	1467.538509	18.408627
44.818892	1468.089386	18.413645
45.658899	1462.481926	18.418663
45.464621	1460.638738	18.423680
45.359710	1435.580450	18.428698
45.331855	1430.823430	18.433715
45.107799	1430.752834	18.438733
45.020715	1431.911232	18.443751
44.880446	1434.611172	18.448768
45.171070	1434.635032	18.453786
45.248157	1449.359448	18.458803
44.992588	1455.920459	18.463821
45.464055	1456.040886	18.468839
45.407798	1464.356085	18.473856
45.666085	1465.887598	18.478874
45.708150	1452.081915	18.483891
45.721644	1460.529655	18.488909
46.118390	1454.347345	18.493927
46.169774	1457.338083	18.498944
45.654997	1449.945781	18.503962
45.274965	1440.147878	18.508979
45.234135	1457.279744	18.513997
45.761065	1449.541904	18.519015
46.079813	1465.601409	18.524032
46.265694	1457.319222	18.529050
45.997198	1460.515998	18.534067
45.827260	1460.040024	18.539085
46.181155	1458.225308	18.544103
45.888046	1462.061401	18.549120
45.996803	1449.199101	18.554138
45.657010	1453.014059	18.559155
45.854532	1465.975556	18.564173
46.106556	1471.580178	18.569191
46.446531	1480.976381	18.574208
46.515727	1488.851542	18.579226
46.196767	1484.684228	18.584243
46.235589	1494.915609	18.589261
46.244525	1489.235247	18.594279
46.010287	1490.884277	18.599296
46.091989	1496.065703	18.604314
46.464926	1496.954275	18.609331
46.446549	1519.269470	18.614349
46.948936	1506.334519	18.619367
46.956126	1523.058580	18.624384
46.882998	1514.545545	18.629402
47.013354	1514.536641	18.634419
47.054160	1511.562880	18.639437
47.007027	1510.196475	18.644455
47.148847	1515.766458	18.649472
47.055094	1513.960365	18.654490
47.392088	1508.116262	18.659507
47.023686	1513.838292	18.664525
47.367029	1511.441070	18.669543
47.436397	1509.494796	18.674560
47.454123	1502.925435	18.679578
47.382217	1506.902373	18.684595
47.065274	1517.844038	18.689613
47.510345	1505.059872	18.694631
47.565788	1514.651742	18.699648
47.310507	1505.153307	18.704666
47.282910	1504.146581	18.709683
47.207451	1509.682940	18.714701
47.426953	1512.931902	18.719719
47.073972	1513.774440	18.724736
47.390938	1512.777150	18.729754
47.616813	1511.788785	18.734771
47.292343	1537.320568	18.739789
47.793594	1536.629117	18.744807
47.975465	1545.261443	18.749824
47.400538	1547.082678	18.754842
47.770461	1535.013410	18.759859
47.816948	1547.655952	18.764877
47.608280	1540.519818	18.769895
47.826793	1549.729386	18.774912
47.969077	1562.247238	18.779930
48.203775	1561.278225	18.784947
48.496253	1565.833322	18.789965
48.809005	1562.618814	18.794983
48.737074	1567.270643	18.800000
48.501214	1550.972897	18.805018
48.624302	1528.193318	18.810035
48.304513	1535.156749	18.815053
48.837684	1526.901608	18.820071
48.458758	1522.747715	18.825088
48.219592	1533.771735	18.830106
48.627353	1550.748836	18.835123
48.508779	1560.414272	18.840141
48.774031	1553.312641	18.845159
48.779652	1562.215375	18.850176
48.677688	1565.837209	18.855194
49.060839	1562.414549	18.860211
48.669559	1564.227137	18.865229
48.921971	1564.788705	18.870247
48.803406	1560.096414	18.875264
48.746788	1564.495198	18.880282
48.776564	1557.516227	18.885299
48.658522	1579.443436	18.890317
49.147183	1582.215122	18.895335
49.462681	1585.042088	18.900352
49.098687	1593.959384	18.905370
49.464736	1582.663656	18.910387
49.429087	1583.657720	18.915405
49.119685	1579.024128	18.920423
49.675615	1580.912933	18.925440
49.308520	1585.284628	18.930458
49.551505	1580.049589	18.935475
49.523676	1583.538627	18.940493
49.341792	1577.251906	18.945511
50.017782	1601.540512	18.950528
49.606672	1612.041647	18.955546
50.157440	1606.454588	18.960563
50.258634	1609.198997	18.965581
49.874017	1595.495082	18.970599
49.772329	1589.134366	18.975616
49.846203	1602.994035	18.980634
50.201763	1606.318520	18.985651
50.356296	1611.436312	18.990669
50.185035	1610.088816	18.995687
50.564133	1601.338738	19.000704
50.187580	1591.670078	19.005722
50.306646	1589.965299	19.010739
50.518675	1594.025090	19.015757
50.289261	1589.312421	19.020775
50.507893	1593.566769	19.025792
50.359351	1610.707426	19.030810
50.635129	1607.422863	19.035827
50.411033	1608.357100	19.040845
50.686924	1612.870956	19.045863
50.995913	1617.914627	19.050880
50.641138	1612.539514	19.055898
50.784489	1600.813795	19.060915
50.848233	1611.853662	19.065933
51.012252	1601.005199	19.070951
51.184556	1609.795910	19.075968
51.076945	1603.166097	19.080986
51.243583	1604.286127	19.086003
50.978012	1601.127056	19.091021
51.193940	1608.524319	19.096039
51.315497	1599.540808	19.101056
50.921671	1600.740388	19.106074
50.898756	1596.464409	19.111091
50.978139	1598.152998	19.116109
50.860950	1602.209778	19.121127
51.208800	1599.053032	19.126144
50.923702	1613.049852	19.131162
51.408235	1618.899341	19.136179
51.244589	1633.105695	19.141197
51.210414	1632.184349	19.146215
51.506701	1626.514128	19.151232
51.502286	1631.817855	19.156250
51.334831	1627.252836	19.161267
51.853495	1643.225096	19.166285
51.717155	1656.855864	19.171303
52.098739	1651.038320	19.176320
52.110795	1654.015758	19.181338
52.101099	1659.990549	19.186355
52.148918	1654.999991	19.191373
52.145807	1655.778222	19.196391
52.442136	1649.410668	19.201408
51.999074	1658.590400	19.206426
52.315897	1653.681691	19.211443
52.314108	1654.688459	19.216461
52.170830	1652.694757	19.221479
52.460789	1644.502908	19.226496
52.315772	1662.354509	19.231514
52.664893	1647.395896	19.236531
52.596016	1656.980029	19.241549
52.528454	1658.515058	19.246567
52.472326	1651.333034	19.251584
52.061376	1651.382676	19.256602
52.749902	1651.594253	19.261619
52.785875	1648.297245	19.266637
52.740100	1656.345367	19.271655
52.873981	1658.013594	19.276672
52.999392	1675.066800	19.281690
52.858345	1678.617006	19.286707
53.074647	1689.275222	19.291725
52.895602	1685.375631	19.296743
53.296428	1683.873744	19.301760
53.272757	1684.886629	19.306778
53.404281	1681.840190	19.311795
53.519135	1680.147148	19.316813
53.007135	1682.854162	19.321831
53.244006	1689.440699	19.326848
53.277071	1689.592978	19.331866
53.394811	1679.382385	19.336883
53.413683	1678.089698	19.341901
53.309265	1684.151217	19.346919
53.589717	1679.847618	19.351936
53.481595	1679.726826	19.356954
53.634650	1701.431727	19.361971
53.655512	1712.104566	19.366989
53.589515	1721.786681	19.372007
53.880746	1716.772091	19.377024
53.695670	1717.545297	19.382042
54.028028	1718.108521	19.387059
54.083349	1718.008139	19.392077
53.891802	1715.517923	19.397095
53.997350	1705.930730	19.402112
54.095088	1710.409796	19.407130
53.945393	1707.298561	19.412147
54.263704	1704.284669	19.417165
53.976329	1726.504136	19.422183
54.392017	1727.031811	19.427200
54.389210	1728.942796	19.432218
54.106992	1734.105187	19.437235
54.705080	1718.043863	19.442253
54.655703	1726.768303	19.447271
54.954308	1723.651869	19.452288
54.901921	1722.272959	19.457306
54.436587	1722.478003	19.462323
55.059043	1718.265383	19.467341
54.993050	1722.841034	19.472359
55.281561	1714.937617	19.477376
55.091080	1715.929884	19.482394
55.317045	1720.240103	19.487411
55.648569	1716.972735	19.492429
55.449902	1722.079455	19.497447
55.627019	1714.341215	19.502464
55.295055	1719.649940	19.507482
55.544534	1723.395043	19.512499
55.830005	1707.668852	19.517517
55.584151	1713.510904	19.522535
55.638518	1713.899715	19.527552
55.454114	1714.926377	19.532570
55.409773	1718.252509	19.537587
55.129628	1721.226899	19.542605
54.763570	1719.226495	19.547623
55.279347	1716.959935	19.552640
55.234035	1729.724674	19.557658
55.354462	1743.494195	19.562675
55.520504	1747.118554	19.567693
55.298338	1751.813518	19.572711
55.471096	1758.967045	19.577728
56.075567	1768.940589	19.582746
55.960038	1769.840472	19.587763
56.160629	1772.755685	19.592781
56.411794	1771.079820	19.597799
56.152148	1769.767545	19.602816
56.160364	1763.582819	19.607834
56.230389	1767.023228	19.612851
56.551376	1762.192126	19.617869
56.497704	1765.947869	19.622887
56.940242	1762.459861	19.627904
56.519406	1765.358369	19.632922
56.760660	1754.793836	19.637939
56.774365	1763.880358	19.642957
56.608994	1762.842505	19.647975
56.658935	1755.593817	19.652992
56.654503	1767.618426	19.658010
56.665738	1761.960014	19.663027
56.576248	1780.142820	19.668045
56.717431	1792.428342	19.673063
56.898227	1797.286940	19.678080
57.103481	1801.425515	19.683098
57.212537	1795.133320	19.688115
57.369380	1789.110527	19.693133
57.179710	1806.719920	19.698151
57.552703	1788.438193	19.703168
57.201540	1790.955033	19.708186
57.056871	1796.162769	19.713203
57.526654	1789.964656	19.718221
57.428710	1811.711954	19.723239
57.889042	1811.228320	19.728256
57.939159	1814.871388	19.733274
57.715092	1806.502982	19.738291
57.958731	1800.615715	19.743309
57.959155	1806.556146	19.748327
58.126856	1805.758072	19.753344
58.006748	1809.131075	19.758362
57.823894	1811.313123	19.763379
58.346108	1799.308105	19.768397
57.890472	1806.159496	19.773415
58.133337	1801.763084	19.778432
57.989776	1804.653437	19.783450
57.855946	1809.372648	19.788467
58.066894	1796.918182	19.793485
58.166667	1809.154906	19.798503
58.242945	1813.002567	19.803520
58.378859	1824.348752	19.808538
58.398847	1841.765530	19.813555
58.871212	1845.366927	19.818573
58.644477	1848.689313	19.823591
58.646124	1842.258803	19.828608
58.935575	1845.691929	19.833626
58.559619	1842.738762	19.838643
58.729277	1836.107776	19.843661
58.750478	1834.793809	19.848679
58.628607	1837.969066	19.853696
58.924233	1832.684363	19.858714
58.859343	1837.498862	19.863731
59.069470	1851.788597	19.868749
59.144424	1863.699264	19.873767
59.130862	1867.563522	19.878784
59.408824	1864.499424	19.883802
59.608133	1865.536699	19.888819
59.770881	1857.902832	19.893837
59.687780	1866.402396	19.898855
59.806801	1861.909075	19.903872
59.890923	1853.554745	19.908890
59.761271	1863.416778	19.913907
59.799059	1854.183278	19.918925
59.824401	1852.015349	19.923943
59.515683	1851.413530	19.928960
59.731600	1853.426812	19.933978
59.787043	1859.200332	19.938995
59.917057	1849.206447	19.944013
59.764107	1857.394321	19.949031
60.096249	1858.622627	19.954048
59.871487	1868.515538	19.959066
60.191633	1886.963319	19.964083
60.097799	1888.456412	19.969101
60.418019	1896.274568	19.974119
60.214936	1886.707102	19.979136
60.370463	1881.407814	19.984154
60.059358	1888.885328	19.989171
60.653429	1885.954850	19.994189
60.854195	1888.294789	19.999207
60.808989	1888.465213	20.004224
61.077324	1882.142921	20.009242
60.741828	1884.179473	20.014259
60.879224	1890.095667	20.019277
61.103826	1904.451873	20.024295
61.158141	1911.297784	20.029312
61.354044	1908.893493	20.034330
61.355415	1908.299936	20.039347
61.370722	1892.011142	20.044365
61.222869	1900.123351	20.049383
61.279668	1902.567905	20.054400
61.433498	1906.854712	20.059418
61.212030	1907.929084	20.064435
61.808390	1903.131054	20.069453
61.572607	1903.899968	20.074471
61.397954	1904.486728	20.079488
61.231359	1907.528704	20.084506
61.393917	1909.747229	20.089523
61.751449	1905.342154	20.094541
61.962568	1907.935471	20.099559
61.866829	1902.750127	20.104576
61.859333	1899.973179	20.109594
61.819550	1907.545148	20.114611
61.936064	1918.964816	20.119629
62.370752	1929.942888	20.124647
62.412626	1931.732050	20.129664
62.044567	1926.683948	20.134682
61.764651	1938.537386	20.139699
61.994835	1928.501471	20.144717
61.977441	1932.751883	20.149735
62.005426	1937.735160	20.154752
62.096496	1940.211250	20.159770
62.541166	1961.566087	20.164787
62.466115	1959.461423	20.169805
62.471898	1960.152701	20.174823
62.554927	1963.336561	20.179840
62.873831	1956.581501	20.184858
62.756299	1955.409039	20.189875
62.578200	1950.058249	20.194893
62.946989	1978.009222	20.199911
62.877069	1986.935779	20.204928
63.309057	1986.071124	20.209946
63.026011	1991.826730	20.214963
63.248645	1988.450793	20.219981
63.532120	1984.694300	20.224999
63.630063	1993.335358	20.230016
64.237994	1980.900888	20.235034
64.268142	1984.838007	20.240051
63.917183	1980.649269	20.245069
63.675290	1957.201230	20.250087
63.192978	1964.923119	20.255104
63.817602	1961.938958	20.260122
63.699662	1982.101927	20.265139
63.737900	1983.344799	20.270157
63.926921	1986.591605	20.275175
63.587093	1989.127795	20.280192
64.081831	1983.079286	20.285210
63.612540	1992.427115	20.290227
64.014481	2000.753034	20.295245
64.099912	2006.355698	20.300263
63.960966	2014.358158	20.305280
64.217783	2011.468151	20.310298
64.149742	2016.272615	20.315315
64.416936	2015.829569	20.320333
64.559977	2007.779269	20.325351
64.470671	2021.533410	20.330368
64.747053	2029.165030	20.335386
64.551654	2044.285979	20.340403
64.674782	2047.918947	20.345421
64.804152	2046.238341	20.350439
64.528904	2046.868733	20.355456
64.742222	2034.660948	20.360474
64.638028	2038.459281	20.365491
64.668848	2043.609449	20.370509
65.093487	2058.349668	20.375527
64.993304	2064.996119	20.380544
65.220629	2064.717408	20.385562
65.257715	2075.355820	20.390579
65.060801	2073.965037	20.395597
65.540915	2064.898526	20.400615
65.242382	2072.757093	20.405632
65.786533	2069.308693	20.410650
65.733104	2076.198347	20.415667
65.729924	2080.588114	20.420685
66.085419	2075.778170	20.425703
66.193507	2073.193609	20.430720
66.657430	2058.063722	20.435738
65.969291	2057.591517	20.440755
66.432645	2056.392699	20.445773
66.681219	2049.421674	20.450791
66.131834	2055.158781	20.455808
66.567141	2050.552907	20.460826
66.376909	2052.103492	20.465843
66.339414	2051.745756	20.470861
66.111128	2049.114916	20.475879
66.262393	2057.294839	20.480896
66.710211	2065.290838	20.485914
66.678754	2080.648319	20.490931
66.413245	2090.743656	20.495949
66.978203	2082.871413	20.500967
66.671749	2086.788301	20.505984
66.909661	2077.485710	20.511002
67.039844	2087.324995	20.516019
66.818831	2078.455065	20.521037
67.008440	2075.397018	20.526055
67.090397	2079.572555	20.531072
67.328386	2073.660167	20.536090
67.333869	2077.993323	20.541107
67.257801	2083.163404	20.546125
67.498494	2081.123113	20.551143
67.314219	2078.748143	20.556160
68.062385	2091.019616	20.561178
67.824346	2082.123465	20.566195
67.428234	2071.744770	20.571213
67.574160	2083.872996	20.576231
67.486083	2099.587492	20.581248
67.416789	2105.970362	20.586266
67.559246	2095.939537	20.591283
67.431534	2105.085546	20.596301
67.664637	2120.602462	20.601319
67.553567	2132.266053	20.606336
68.137509	2129.743230	20.611354
68.186170	2127.945331	20.616371
67.911427	2133.221940	20.621389
68.264934	2135.894442	20.626407
68.079815	2152.645845	20.631424
68.516138	2153.841353	20.636442
68.721460	2154.712240	20.641459
68.667978	2153.712271	20.646477
68.854452	2150.307061	20.651495
68.812587	2159.119443	20.656512
68.944086	2151.669163	20.661530
68.915626	2144.632976	20.666547
68.832608	2147.581131	20.671565
69.177868	2145.219713	20.676583
69.030325	2137.871616	20.681600
69.319405	2140.939468	20.686618
69.198567	2142.217499	20.691635
69.140353	2149.662019	20.696653
69.470233	2138.726868	20.701671
69.363421	2150.631902	20.706688
69.356768	2161.558225	20.711706
69.727155	2179.143684	20.716723
69.814809	2173.096380	20.721741
70.043118	2174.523641	20.726759
70.020430	2177.869390	20.731776
70.080457	2169.052816	20.736794
70.117756	2166.939494	20.741811
70.047928	2173.173250	20.746829
70.206294	2166.773621	20.751847
70.219082	2171.515449	20.756864
70.086437	2169.005612	20.761882
70.134950	2174.446925	20.766899
70.101105	2180.989520	20.771917
70.727342	2166.994856	20.776935
70.340705	2176.357367	20.781952
70.837766	2173.515527	20.786970
70.889842	2171.965891	20.791987
70.753817	2179.039065	20.797005
70.734357	2173.987425	20.802023
70.485100	2173.793961	20.807040
70.586711	2167.320191	20.812058
70.537109	2170.959569	20.817075
70.705012	2187.407148	20.822093
70.372484	2194.799097	20.827111
70.358348	2203.676445	20.832128
70.817356	2213.861855	20.837146
70.865976	2233.167734	20.842163
71.171431	2232.787425	20.847181
71.429463	2228.073683	20.852199
71.204861	2230.051497	20.857216
71.398077	2231.736391	20.862234
71.437717	2232.771926	20.867251
71.609941	2251.281724	20.872269
72.107355	2250.779516	20.877287
71.755755	2254.868382	20.882304
71.905261	2245.957674	20.887322
71.798735	2247.224597	20.892339
72.025927	2254.813178	20.897357
71.867508	2251.825393	20.902375
72.072569	2247.678287	20.907392
72.482052	2251.622499	20.912410
72.286174	2244.822479	20.917427
72.183378	2247.451950	20.922445
72.410060	2238.917835	20.927463
72.410615	2262.193974	20.932480
72.638611	2276.216429	20.937498
72.963784	2281.668233	20.942515
73.119247	2279.034565	20.947533
72.789457	2269.520086	20.952551
73.275831	2272.680931	20.957568
73.284664	2272.894859	20.962586
73.248186	2253.779903	20.967603
72.531893	2253.845665	20.972621
72.916319	2256.864906	20.977639
73.008928	2272.957320	20.982656
72.919429	2271.697338	20.987674
72.959356	2270.703399	20.992691
72.930840	2271.402540	20.997709
73.196001	2293.188270	21.002727
73.186249	2303.391889	21.007744
73.251043	2299.786215	21.012762
73.180172	2298.671878	21.017779
73.068750	2309.270939	21.022797
73.775640	2325.787308	21.027815
73.703324	2334.194318	21.032832
73.560224	2324.250890	21.037850
74.076266	2322.310629	21.042867
74.092342	2334.503048	21.047885
74.492512	2336.627348	21.052903
74.335452	2341.139645	21.057920
74.668197	2350.425394	21.062938
74.739562	2357.585554	21.067955
74.399239	2354.779350	21.072973
74.717676	2353.547867	21.077991
74.950678	2360.627553	21.083008
74.939877	2362.538805	21.088026
75.293754	2359.573425	21.093043
75.035753	2349.346485	21.098061
75.030170	2336.657018	21.103079
75.210492	2343.540186	21.108096
74.727413	2347.272031	21.113114
75.042949	2353.943806	21.118131
74.794750	2357.875580	21.123149
75.321760	2356.537463	21.128167
75.134740	2360.220131	21.133184
75.185595	2348.407727	21.138202
75.151901	2361.095387	21.143219
75.151544	2375.553202	21.148237
75.583391	2385.791421	21.153255
75.357556	2381.976458	21.158272
75.362337	2384.504820	21.163290
75.802507	2390.740219	21.168307
75.756601	2406.947870	21.173325
76.195938	2401.695830	21.178343
76.108468	2402.139688	21.183360
76.103428	2403.290785	21.188378
76.525232	2394.000189	21.193395
76.383255	2401.479663	21.198413
76.364055	2400.175331	21.203431
76.565965	2396.031089	21.208448
76.880283	2397.539310	21.213466
76.968882	2383.052285	21.218483
76.632680	2402.367644	21.223501
76.847381	2386.493434	21.228519
76.774824	2394.306726	21.233536
76.459844	2391.349692	21.238554
77.065450	2386.655856	21.243571
76.909803	2389.024291	21.248589
77.111268	2406.275525	21.253607
77.597275	2409.693195	21.258624
77.322312	2414.641538	21.263642
77.740079	2410.835935	21.268659
77.575182	2418.292571	21.273677
77.517767	2421.652988	21.278695
77.942799	2410.028398	21.283712
77.873002	2404.413965	21.288730
78.410720	2399.619936	21.293747
78.100803	2392.812626	21.298765
77.859661	2373.611332	21.303783
78.005929	2366.428144	21.308800
78.089489	2384.760358	21.313818
78.056711	2392.871601	21.318835
78.014508	2404.106989	21.323853
78.294154	2399.496594	21.328871
78.377762	2400.541928	21.333888
78.122685	2405.004896	21.338906
78.124730	2409.128464	21.343923
78.402758	2405.057010	21.348941
78.589398	2419.589123	21.353959
78.755084	2423.470435	21.358976
78.473365	2431.639338	21.363994
78.946254	2424.335552	21.369011
79.149011	2426.244850	21.374029
79.304175	2428.854541	21.379047
79.065491	2422.186211	21.384064
79.219290	2431.646016	21.389082
79.536801	2427.686704	21.394099
79.495576	2428.194299	21.399117
79.312586	2431.821166	21.404135
79.420196	2432.204806	21.409152
79.166899	2425.679158	21.414170
79.385476	2438.367734	21.419187
79.699328	2458.124561	21.424205
79.325519	2458.539544	21.429223
79.871703	2456.225538	21.434240
79.658169	2455.760943	21.439258
79.547517	2455.304698	21.444275
79.734134	2473.060992	21.449293
79.942095	2475.055245	21.454311
80.472080	2473.381123	21.459328
80.393172	2474.875649	21.464346
80.650250	2478.643654	21.469363
80.078627	2482.615942	21.474381
80.401167	2474.228284	21.479399
80.422253	2469.905540	21.484416
80.830146	2507.212865	21.489434
81.207462	2511.790319	21.494451
81.077783	2507.324093	21.499469
81.292093	2502.889462	21.504487
80.662730	2485.635202	21.509504
80.815881	2496.717462	21.514522
81.166902	2503.518672	21.519539
81.137962	2506.452111	21.524557
81.043767	2498.272913	21.529575
81.130172	2501.140112	21.534592
81.156231	2515.422634	21.539610
81.276905	2530.125239	21.544627
81.583492	2531.567860	21.549645
81.306314	2537.629399	21.554663
81.528040	2531.523140	21.559680
81.352171	2536.151334	21.564698
81.806194	2549.157175	21.569715
82.041810	2561.855530	21.574733
81.790317	2561.836880	21.579751
81.963308	2557.205347	21.584768
81.982745	2561.756753	21.589786
82.226482	2563.425934	21.594803
82.766852	2571.531152	21.599821
82.482056	2590.726887	21.604839
82.724804	2592.303313	21.609856
82.748046	2590.770392	21.614874
83.044813	2581.272738	21.619891
83.037943	2582.007558	21.624909
82.957357	2586.043747	21.629927
83.087546	2587.289016	21.634944
83.014331	2591.314493	21.639962
82.514425	2578.424488	21.644979
82.845321	2593.727439	21.649997
82.896584	2600.746250	21.655015
83.499389	2612.127158	21.660032
83.397512	2617.179772	21.665050
83.315139	2613.401586	21.670067
83.455231	2622.914258	21.675085
83.528365	2634.095387	21.680103
83.961688	2638.304948	21.685120
83.966731	2646.175940	21.690138
84.039339	2645.721348	21.695155
83.747237	2643.785713	21.700173
83.730576	2649.473445	21.705191
84.307783	2649.273350	21.710208
83.987928	2677.590918	21.715226
84.457044	2677.940152	21.720243
84.655694	2682.256898	21.725261
84.624196	2688.108631	21.730279
84.996878	2674.854746	21.735296
84.878781	2676.426100	21.740314
84.533916	2673.775761	21.745331
84.961171	2677.300430	21.750349
84.879327	2677.821297	21.755367
84.936500	2666.960490	21.760384
84.789195	2680.268774	21.765402
84.935290	2686.746079	21.770419
85.018806	2695.907016	21.775437
84.829016	2713.015390	21.780455
85.282800	2700.892659	21.785472
85.471655	2696.142599	21.790490
85.416791	2703.604132	21.795507
85.790037	2711.176560	21.800525
85.819205	2723.300884	21.805543
86.551865	2716.478506	21.810560
86.052396	2723.632739	21.815578
86.365938	2721.564127	21.820595
86.587468	2712.577017	21.825613
86.467766	2707.971204	21.830631
86.646639	2690.930186	21.835648
86.550856	2681.325722	21.840666
86.414642	2690.899193	21.845683
86.396540	2699.725524	21.850701
86.610089	2706.657496	21.855719
86.990241	2705.683957	21.860736
86.595558	2709.325915	21.865754
86.590179	2714.816426	21.870771
87.295917	2711.809563	21.875789
86.773683	2719.978895	21.880807
86.917108	2705.955484	21.885824
87.129843	2726.235584	21.890842
86.898023	2730.826962	21.895859
87.367896	2742.795421	21.900877
87.374469	2742.291507	21.905895
87.418594	2734.942952	21.910912
87.037638	2749.029275	21.915930
87.333766	2767.927963	21.920947
87.707830	2770.122953	21.925965
87.634778	2768.798683	21.930983
87.935079	2766.073163	21.936000
88.291354	2769.401324	21.941018
88.046202	2772.830227	21.946035
88.294674	2784.235780	21.951053
88.441156	2787.581008	21.956071
88.989310	2780.417727	21.961088
88.925419	2785.932470	21.966106
89.103316	2787.270383	21.971123
89.532273	2778.033464	21.976141
89.232414	2751.809819	21.981159
89.194340	2745.625947	21.986176
89.367743	2750.903901	21.991194
89.408184	2751.050201	21.996211
89.600783	2743.501355	22.001229
89.108572	2752.398756	22.006247
89.088020	2737.838762	22.011264
89.226218	2744.809657	22.016282
89.160907	2742.911521	22.021299
89.332575	2754.644447	22.026317
89.342975	2770.658536	22.031335
89.272550	2774.277210	22.036352
89.529757	2778.509914	22.041370
89.542626	2779.624105	22.046387
89.464591	2790.947817	22.051405
89.528618	2807.962379	22.056423
90.023419	2803.851299	22.061440
89.938667	2811.324307	22.066458
89.961491	2815.847642	22.071475
90.342718	2819.633036	22.076493
90.391030	2838.460100	22.081511
90.336859	2833.391753	22.086528
90.733182	2841.086295	22.091546
90.357093	2840.135288	22.096563
90.722700	2843.358696	22.101581
90.806490	2861.354359	22.106599
90.816240	2860.500226	22.111616
90.809102	2859.409575	22.116634
91.021989	2863.846000	22.121651
91.426134	2858.098177	22.126669
91.096008	2868.162562	22.131687
91.516970	2869.134343	22.136704
91.701704	2875.738986	22.141722
91.770985	2883.518755	22.146739
92.028360	2878.893926	22.151757
91.678307	2882.485744	22.156775
91.775414	2880.624326	22.161792
91.960244	2880.706498	22.166810
91.848283	2884.133855	22.171827
92.207145	2869.526021	22.176845
92.062748	2883.839675	22.181863
92.415218	2896.452903	22.186880
92.705770	2906.918088	22.191898
92.852793	2905.306426	22.196915
93.243256	2901.484124	22.201933
92.972269	2907.063552	22.206951
93.262102	2905.230520	22.211968
93.223567	2901.017898	22.216986
92.901763	2902.295002	22.222003
93.448324	2899.479991	22.227021
92.952393	2909.213704	22.232039
93.064288	2905.669909	22.237056
93.482302	2897.725587	22.242074
93.173059	2897.822367	22.247091
93.358674	2905.645995	22.252109
93.486350	2918.363144	22.257127
93.512127	2924.150019	22.262144
93.697006	2931.176786	22.267162
93.614996	2943.101401	22.272179
93.921673	2933.920007	22.277197
93.533948	2948.037594	22.282215
93.673987	2953.501684	22.287232
93.781089	2965.508878	22.292250
93.850343	2970.144006	22.297267
94.116844	2978.157778	22.302285
94.139365	2994.937093	22.307303
94.408767	2987.079632	22.312320
94.704341	2979.421665	22.317338
94.669960	2994.740376	22.322355
95.132656	2998.169262	22.327373
94.843591	3012.963039	22.332391
94.840808	3019.301407	22.337408
95.235056	3007.520208	22.342426
95.766945	3008.455657	22.347443
95.777707	3011.808450	22.352461
95.639453	3014.258264	22.357479
95.643703	3020.144158	22.362496
95.947182	3008.162730	22.367514
95.697034	3010.856179	22.372531
96.065033	3002.821148	22.377549
96.146855	3004.674071	22.382567
96.084639	3010.836761	22.387584
95.830499	3009.693937	22.392602
95.950424	3003.232436	22.397619
96.094312	3019.764155	22.402637
96.078802	3044.112130	22.407655
96.130832	3042.004829	22.412672
96.652283	3039.313019	22.417690
96.076830	3048.683999	22.422707
96.495272	3068.797756	22.427725
96.781860	3070.614795	22.432743
96.618847	3073.594163	22.437760
97.089235	3071.754575	22.442778
96.870684	3078.856869	22.447795
97.053303	3082.617309	22.452813
97.217506	3091.963897	22.457831
97.481312	3095.143381	22.462848
97.488585	3089.435160	22.467866
97.703181	3101.816234	22.472883
97.639809	3094.744259	22.477901
97.763984	3106.713982	22.482919
98.152701	3122.772257	22.487936
98.363920	3122.098576	22.492954
98.267693	3125.909980	22.497971
98.399472	3120.939609	22.502989
98.430964	3126.039615	22.508007
98.579801	3114.353962	22.513024
98.818814	3113.973213	22.518042
98.686156	3121.650683	22.523059
98.836072	3124.270842	22.528077
99.330293	3114.068020	22.533095
98.984494	3110.553813	22.538112
99.165607	3111.498212	22.543130
98.928713	3117.057692	22.548147
99.183101	3105.498074	22.553165
98.805993	3115.626587	22.558183
99.096416	3136.189233	22.563200
99.252583	3135.077655	22.568218
99.006207	3140.974270	22.573235
99.632825	3148.250669	22.578253
99.594203	3148.632619	22.583271
99.642607	3169.557335	22.588288
100.125884	3163.186265	22.593306
99.844577	3177.690619	22.598323
100.137650	3167.459241	22.603341
100.178342	3168.186722	22.608359
100.075195	3177.060190	22.613376
100.191414	3175.580578	22.618394
100.381581	3183.533512	22.623411
100.500105	3193.228218	22.628429
100.685722	3192.771564	22.633447
100.773282	3204.746064	22.638464
101.248455	3193.442293	22.643482
100.978552	3201.822209	22.648499
100.795134	3196.178142	22.653517
101.001047	3207.056544	22.658535
101.030684	3223.896313	22.663552
101.434251	3219.698385	22.668570
101.358417	3221.940640	22.673587
101.651975	3217.993902	22.678605
101.913196	3212.984774	22.683623
101.621488	3220.925040	22.688640
101.959841	3224.033491	22.693658
101.753328	3237.117702	22.698675
102.185446	3244.822059	22.703693
102.583020	3245.564758	22.708711
102.547929	3246.334374	22.713728
102.793639	3237.727939	22.718746
102.769213	3244.019703	22.723763
102.925718	3233.792792	22.728781
103.467832	3233.304163	22.733799
103.230064	3236.351506	22.738816
103.429692	3227.423775	22.743834
103.356945	3232.321168	22.748851
103.023135	3234.860457	22.753869
103.007474	3237.118389	22.758887
103.082868	3232.775100	22.763904
103.482423	3222.227732	22.768922
103.134656	3234.754934	22.773939
103.218662	3240.957228	22.778957
103.618379	3259.180347	22.783975
103.534083	3266.590488	22.788992
103.640990	3265.195160	22.794010
103.274230	3271.106947	22.799027
103.785611	3279.242708	22.804045
103.791101	3282.612214	22.809063
103.766039	3304.533375	22.814080
104.008100	3309.112200	22.819098
104.406207	3319.256798	22.824115
104.212779	3318.250030	22.829133
104.500115	3334.577924	22.834151
104.601610	3348.397781	22.839168
105.381054	3334.586895	22.844186
105.594293	3338.520138	22.849203
105.479358	3334.641037	22.854221
105.685318	3325.051395	22.859239
105.524739	3334.852315	22.864256
105.959272	3330.623060	22.869274
105.724992	3327.104650	22.874291
105.597132	3336.751899	22.879309
106.089550	3328.354357	22.884327
105.945819	3334.628019	22.889344
106.084110	3329.682456	22.894362
105.897696	3331.438064	22.899379
105.833462	3329.174240	22.904397
105.788113	3326.036128	22.909415
106.039560	3358.484649	22.914432
106.535407	3357.011611	22.919450
106.055198	3354.978182	22.924467
106.205249	3363.781572	22.929485
106.429640	3374.732531	22.934503
106.608812	3388.196513	22.939520
106.808580	3380.338983	22.944538
106.780146	3388.876857	22.949555
106.755106	3411.082476	22.954573
107.529223	3413.330265	22.959591
107.413417	3429.261913	22.964608
107.312139	3419.036544	22.969626
107.697495	3424.918688	22.974643
108.067239	3424.803774	22.979661
108.528465	3410.750458	22.984679
108.724543	3400.834046	22.989696
108.786162	3388.988301	22.994714
108.725978	3391.745332	22.999731
108.974844	3398.459700	23.004749
108.907295	3386.869221	23.009767
108.399564	3393.366758	23.014784
108.916593	3385.635978	23.019802
108.841169	3383.745011	23.024819
108.725146	3390.438446	23.029837
109.042789	3382.541805	23.034855
108.866284	3387.770485	23.039872
109.211707	3383.378502	23.044890
109.156018	3393.993153	23.049907
109.304237	3409.082496	23.054925
109.322968	3414.710094	23.059943
109.346177	3415.784753	23.064960
109.606318	3418.808206	23.069978
109.716723	3415.307081	23.074995
109.539612	3434.846878	23.080013
109.974512	3436.773213	23.085031
109.901462	3447.227060	23.090048
110.046688	3444.534312	23.095066
109.892310	3455.135994	23.100083
110.025886	3472.326796	23.105101
110.465918	3469.667776	23.110119
110.248684	3483.039130	23.115136
110.295529	3480.186824	23.120154
110.837166	3485.557841	23.125171
110.738537	3506.390074	23.130189
110.957426	3509.743523	23.135207
111.070997	3509.418924	23.140224
110.986863	3507.649934	23.145242
111.025214	3510.972901	23.150259
111.185170	3537.298308	23.155277
111.649560	3537.913006	23.160295
111.673599	3543.151463	23.165312
111.657050	3539.101080	23.170330
111.849483	3534.076078	23.175347
111.653012	3549.464857	23.180365
112.270924	3558.846568	23.185383
112.218581	3562.157529	23.190400
112.191416	3566.538433	23.195418
112.669064	3559.187634	23.200435
112.623491	3571.053710	23.205453
112.788966	3561.598454	23.210471
112.747706	3563.741108	23.215488
112.605452	3576.056930	23.220506
113.264699	3581.803184	23.225523
112.917690	3591.874860	23.230541
113.328445	3586.078389	23.235559
113.063003	3585.437572	23.240576
113.407636	3594.373127	23.245594
113.615601	3601.529340	23.250611
113.315544	3626.870518	23.255629
113.578287	3621.497138	23.260647
113.617330	3622.178455	23.265664
113.401858	3636.381325	23.270682
113.937267	3642.914363	23.275699
113.714651	3653.592458	23.280717
114.160522	3646.247854	23.285735
114.397902	3667.188091	23.290752
114.843064	3678.139219	23.295770
114.773969	3678.771344	23.300787
115.025686	3685.324680	23.305805
115.292835	3672.961485	23.310823
115.261364	3677.808622	23.315840
115.132759	3676.455993	23.320858
115.749385	3665.485203	23.325875
115.706181	3667.702237	23.330893
115.673416	3666.539528	23.335911
115.682403	3672.263398	23.340928
115.667188	3667.785094	23.345946
115.867430	3684.415752	23.350963
115.800025	3697.792319	23.355981
116.004168	3694.483774	23.360999
115.915670	3695.497268	23.366016
115.845188	3693.446323	23.371034
116.295824	3705.994547	23.376051
116.496459	3718.204444	23.381069
116.375374	3727.458551	23.386087
116.486411	3725.239445	23.391104
116.829792	3711.847949	23.396122
117.323010	3723.334307	23.401139
117.115460	3730.948515	23.406157
117.758116	3734.119105	23.411175
117.439457	3736.616496	23.416192
117.298443	3747.047538	23.421210
117.676886	3744.945619	23.426227
117.426230	3748.996295	23.431245
117.415930	3742.810420	23.436263
117.476979	3737.890573	23.441280
117.705244	3750.967621	23.446298
118.023853	3762.359501	23.451315
117.749101	3777.726479	23.456333
118.221175	3770.554534	23.461351
118.357779	3771.370352	23.466368
117.946810	3785.865199	23.471386
118.535690	3800.368229	23.476403
118.365170	3800.022230	23.481421
118.538630	3803.668638	23.486439
118.629191	3825.140676	23.491456
118.988892	3826.250616	23.496474
119.261504	3828.577353	23.501491
118.943028	3840.678650	23.506509
119.060091	3862.174548	23.511527
119.409588	3864.078561	23.516544
119.548682	3853.151699	23.521562
120.193227	3851.560979	23.526579
120.397491	3862.425942	23.531597
120.798356	3854.740841	23.536615
120.649012	3846.860228	23.541632
120.169275	3846.282914	23.546650
121.076569	3856.022385	23.551667
120.729495	3865.848515	23.556685
120.888437	3879.377819	23.561703
121.035079	3872.960214	23.566720
121.053710	3875.871576	23.571738
121.678276	3868.211128	23.576755
121.283201	3870.409751	23.581773
121.268091	3869.597630	23.586791
121.311917	3871.005877	23.591808
121.058040	3876.420466	23.596826
121.600141	3874.447994	23.601843
121.134817	3895.394008	23.606861
121.199229	3899.092212	23.611879
121.610809	3909.295528	23.616896
121.426518	3927.895986	23.621914
121.821631	3930.526230	23.626931
122.041255	3943.630910	23.631949
122.466276	3956.112053	23.636967
122.590827	3955.425630	23.641984
122.801365	3959.976972	23.647002
123.111350	3953.202117	23.652019
122.837659	3963.760797	23.657037
123.154469	3971.516786	23.662055
123.504860	3984.195832	23.667072
122.908119	3994.112096	23.672090
123.301432	3989.269893	23.677107
123.457764	3997.829193	23.682125
123.751616	3989.988311	23.687143
123.788036	3995.602845	23.692160
123.109646	4016.665092	23.697178
123.893306	4019.239770	23.702195
123.906856	4026.980039	23.707213
123.728007	4023.302324	23.712231
124.270538	4034.403195	23.717248
124.380873	4046.648517	23.722266
124.660952	4037.038651	23.727283
124.821318	4049.372274	23.732301
124.801201	4045.624025	23.737319
124.942737	4058.746125	23.742336
125.043376	4072.291103	23.747354
125.690511	4066.809935	23.752371
125.931401	4066.196501	23.757389
125.979974	4056.587716	23.762407
126.554943	4053.309254	23.767424
126.280045	4057.398030	23.772442
126.451975	4048.387161	23.777459
126.102370	4041.942717	23.782477
126.265039	4051.108991	23.787495
126.299409	4056.004027	23.792512
126.208637	4054.395997	23.797530
126.623345	4050.950469	23.802547
126.780771	4052.755114	23.807565
126.683749	4057.108750	23.812583
126.720961	4058.654404	23.817600
126.981256	4073.924436	23.822618
126.732140	4082.316216	23.827635
126.893788	4078.042971	23.832653
126.742225	4087.226903	23.837671
127.155090	4093.910306	23.842688
127.068831	4105.234796	23.847706
127.393131	4113.453472	23.852723
127.123697	4139.236007	23.857741
127.318476	4156.832922	23.862759
127.797345	4164.917225	23.867776
127.679965	4176.518826	23.872794
127.905105	4178.088984	23.877811
128.310652	4195.545846	23.882829
128.394713	4209.339519	23.887847
129.045533	4206.266979	23.892864
128.920319	4207.413605	23.897882
129.381506	4189.999654	23.902899
128.994556	4198.992443	23.907917
129.026107	4219.001510	23.912935
129.578302	4223.459706	23.917952
130.014262	4231.196974	23.922970
129.997396	4219.970523	23.927987
129.987200	4228.613628	23.933005
130.005291	4223.415878	23.938023
130.308448	4225.093172	23.943040
130.197089	4225.335607	23.948058
130.249893	4215.695283	23.953075
130.315795	4229.897707	23.958093
130.200683	4248.264575	23.963111
130.330492	4257.797329	23.968128
130.608941	4259.600943	23.973146
130.667250	4268.405601	23.978163
130.751413	4282.684492	23.983181
130.490857	4294.687991	23.988199
130.673524	4294.290099	23.993216
130.908934	4317.616442	23.998234
131.101095	4326.432056	24.003251
131.315975	4330.162850	24.008269
131.389591	4350.535054	24.013287
131.846817	4357.309418	24.018304
131.799930	4357.447863	24.023322
131.988514	4357.972046	24.028339
132.277087	4383.345849	24.033357
132.394812	4381.213719	24.038375
132.836622	4369.574582	24.043392
132.594307	4373.069500	24.048410
133.078146	4370.460322	24.053427
133.293309	4369.620515	24.058445
133.062804	4377.224003	24.063463
133.291722	4382.968714	24.068480
133.527836	4399.813724	24.073498
133.148273	4398.875022	24.078515
133.927559	4404.003989	24.083533
133.887227	4409.835822	24.088551
133.942937	4399.619924	24.093568
133.675316	4418.495157	24.098586
133.828700	4419.738175	24.103603
134.065039	4431.459693	24.108621
133.930568	4438.655298	24.113639
134.479629	4443.741831	24.118656
134.806969	4450.565281	24.123674
135.002748	4449.123110	24.128691
135.010325	4452.202662	24.133709
134.912282	4451.718990	24.138727
135.506277	4473.873544	24.143744
135.143946	4483.174173	24.148762
135.491192	4485.032180	24.153779
135.672341	4484.709368	24.158797
135.693615	4480.749137	24.163815
136.126672	4493.867308	24.168832
136.291828	4501.832286	24.173850
136.307550	4498.949689	24.178867
136.313560	4499.620956	24.183885
136.225544	4509.455057	24.188903
136.576999	4508.766733	24.193920
136.398801	4526.403580	24.198938
136.570880	4538.548910	24.203955
136.750297	4539.895380	24.208973
136.965825	4535.958546	24.213991
136.979623	4551.299650	24.219008
137.215763	4559.183965	24.224026
137.419235	4560.120684	24.229043
137.335164	4559.193541	24.234061
137.381443	4566.777238	24.239079
137.658204	4578.811714	24.244096
137.773324	4598.491096	24.249114
137.721748	4594.569317	24.254131
138.423285	4602.089539	24.259149
137.904646	4619.235868	24.264167
138.277478	4622.838052	24.269184
138.353381	4616.472442	24.274202
138.806991	4638.641842	24.279219
138.794807	4649.977651	24.284237
138.740506	4660.708696	24.289255
139.073835	4652.093565	24.294272
139.040740	4672.151306	24.299290
138.975878	4682.619530	24.304307
139.512660	4686.244820	24.309325
139.611178	4697.914548	24.314343
139.841105	4708.204659	24.319360
139.842388	4719.546086	24.324378
139.976758	4720.585238	24.329395
140.436454	4718.870963	24.334413
140.544178	4733.176938	24.339431
140.826841	4740.740677	24.344448
141.116900	4735.186596	24.349466
141.202707	4737.097327	24.354483
141.226297	4731.542456	24.359501
141.391829	4731.291629	24.364519
141.146854	4738.160539	24.369536
141.420207	4748.989066	24.374554
141.700797	4767.351714	24.379571
141.970006	4765.006107	24.384589
141.941951	4770.412217	24.389607
142.112952	4762.514039	24.394624
141.895679	4773.013963	24.399642
141.880101	4789.810381	24.404659
142.803149	4787.347174	24.409677
142.426259	4801.140828	24.414695
142.714000	4793.681031	24.419712
142.844265	4809.237137	24.424730
142.937171	4825.904726	24.429747
143.461193	4818.268152	24.434765
143.098708	4836.066894	24.439783
143.313009	4823.796142	24.444800
143.109748	4833.154772	24.449818
143.175767	4852.929527	24.454835
143.606262	4853.694235	24.459853
143.708876	4868.410785	24.464871
143.795717	4881.513802	24.469888
143.826991	4891.743568	24.474906
144.151829	4895.052373	24.479923
144.538323	4905.084993	24.484941
144.578613	4909.309779	24.489959
144.591111	4903.659080	24.494976
145.254049	4925.378697	24.499994
146.211925	4903.341182	24.505011
146.857205	4893.780830	24.510029
146.717396	4877.155979	24.515047
146.841490	4863.795592	24.520064
146.691404	4849.029013	24.525082
146.665043	4835.282502	24.530099
146.790568	4829.002031	24.535117
146.681999	4832.656068	24.540135
146.791526	4830.204712	24.545152
146.482718	4837.144468	24.550170
146.717766	4836.819500	24.555187
147.074468	4829.492003	24.560205
146.982025	4840.922835	24.565223
147.081239	4838.150312	24.570240
147.188608	4838.330843	24.575258
146.864229	4850.684390	24.580275
147.000815	4843.591530	24.585293
147.002108	4866.400378	24.590311
147.378704	4878.363621	24.595328
147.115393	4890.039593	24.600346
147.300727	4910.183853	24.605363
147.749341	4918.594306	24.610381
147.976358	4932.672075	24.615399
148.040179	4946.213086	24.620416
148.021031	4964.910899	24.625434
147.995515	4979.544758	24.630451
148.543894	4978.081481	24.635469
148.417214	4987.488510	24.640487
148.323593	5003.892105	24.645504
148.808636	5017.706750	24.650522
148.896292	5038.508278	24.655539
148.831284	5043.452162	24.660557
149.166611	5058.948945	24.665575
149.600533	5077.508575	24.670592
149.857529	5080.293444	24.675610
149.962139	5097.094789	24.680627
150.181587	5105.424115	24.685645
150.003797	5115.724520	24.690663
150.583581	5118.674608	24.695680
150.814089	5126.831915	24.700698
151.121643	5151.567270	24.705715
151.529018	5144.338065	24.710733
151.594750	5136.168677	24.715751
151.690746	5139.871209	24.720768
151.881052	5129.529373	24.725786
151.883083	5137.187093	24.730803
152.038401	5140.628981	24.735821
151.886482	5164.352211	24.740839
152.425512	5162.244639	24.745856
153.009943	5159.442446	24.750874
152.905934	5163.676282	24.755891
153.334942	5150.785604	24.760909
152.978584	5162.458034	24.765927
152.530728	5162.229644	24.770944
152.631178	5161.257444	24.775962
152.817736	5186.894987	24.780979
152.926818	5190.545666	24.785997
153.164602	5200.600815	24.791015
152.954139	5221.809710	24.796032
153.450854	5226.731401	24.801050
153.832484	5237.628346	24.806067
153.724504	5247.718379	24.811085
153.754816	5264.034833	24.816103
153.927235	5266.126910	24.821120
153.944757	5279.496555	24.826138
154.012813	5286.784640	24.831155
154.645148	5296.246844	24.836173
154.694444	5325.420346	24.841191
154.987471	5333.426050	24.846208
155.249615	5318.537170	24.851226
155.272996	5347.906559	24.856243
155.417191	5344.924594	24.861261
155.712328	5348.937251	24.866279
155.609088	5349.770636	24.871296
155.684641	5371.375735	24.876314
155.829909	5377.770011	24.881331
156.055070	5384.152958	24.886349
156.286284	5404.170254	24.891367
156.335617	5410.803900	24.896384
156.571272	5412.929267	24.901402
156.966570	5434.545806	24.906419
157.502719	5436.988296	24.911437
157.254782	5438.421492	24.916455
157.544539	5448.678987	24.921472
157.747277	5437.848825	24.926490
157.969140	5453.698631	24.931507
158.434359	5452.941147	24.936525
158.343424	5451.712660	24.941543
158.290304	5455.544013	24.946560
158.578726	5449.645753	24.951578
158.314587	5452.342793	24.956595
158.588363	5470.230882	24.961613
159.009667	5469.194212	24.966631
159.512568	5468.758728	24.971648
159.683152	5474.279111	24.976666
159.180326	5478.369510	24.981683
159.430205	5488.772498	24.986701
159.143648	5498.482921	24.991719
159.244704	5509.994489	24.996736
159.437021	5523.250094	25.001754
159.674861	5533.714251	25.006771
159.785583	5555.937413	25.011789
160.523258	5563.229781	25.016807
160.263937	5573.134076	25.021824
160.611137	5578.653364	25.026842
160.897731	5602.801468	25.031859
161.068856	5595.383343	25.036877
161.600356	5596.756198	25.041895
161.523221	5606.192908	25.046912
161.979882	5618.098878	25.051930
162.011353	5632.184794	25.056947
162.237773	5632.047972	25.061965
162.374461	5630.242465	25.066983
162.522294	5638.183417	25.072000
162.592405	5621.153167	25.077018
162.585169	5630.254172	25.082035
162.382726	5627.652949	25.087053
162.647439	5621.965850	25.092071
162.643426	5646.277262	25.097088
162.614293	5656.500547	25.102106
162.894457	5666.795273	25.107123
163.099310	5687.218377	25.112141
162.963203	5693.029289	25.117159
163.314647	5709.828356	25.122176
163.474041	5721.463984	25.127194
163.812934	5738.143927	25.132211
163.988780	5751.007126	25.137229
164.296179	5744.918823	25.142247
164.052562	5762.915624	25.147264
164.483161	5778.917444	25.152282
164.647098	5785.265361	25.157299
164.746563	5799.353949	25.162317
164.984757	5801.957850	25.167335
164.725423	5817.293434	25.172352
165.218580	5823.195813	25.177370
165.648984	5845.557566	25.182387
165.713293	5851.832791	25.187405
166.022406	5858.939608	25.192423
165.750901	5875.491171	25.197440
166.449922	5871.379759	25.202458
166.423919	5890.574507	25.207475
166.934588	5911.098290	25.212493
167.347026	5914.757000	25.217511
167.437418	5916.280329	25.222528
167.248538	5909.866643	25.227546
167.215626	5916.405896	25.232563
167.118741	5932.158792	25.237581
167.544907	5927.140236	25.242599
167.418699	5939.796212	25.247616
167.641473	5958.911376	25.252634
167.991128	5969.825335	25.257651
168.043546	5982.954854	25.262669
168.366362	5989.560767	25.267687
168.410201	6004.684658	25.272704
169.185722	6005.569095	25.277722
169.475519	6018.828097	25.282739
169.674607	6013.391571	25.287757
169.989972	6020.128745	25.292775
169.551549	6025.950639	25.297792
169.767154	6025.629771	25.302810
169.903514	6024.171653	25.307827
170.053042	6037.050623	25.312845
170.620624	6034.355148	25.317863
170.715079	6044.239265	25.322880
171.015573	6044.642711	25.327898
170.954113	6042.284284	25.332915
170.866101	6042.518803	25.337933
171.108292	6038.599874	25.342951
170.761161	6068.131778	25.347968
171.018436	6075.808425	25.352986
171.140275	6082.637090	25.358003
171.220465	6100.418861	25.363021
171.930497	6111.396389	25.368039
172.253068	6094.941495	25.373056
172.522910	6092.033955	25.378074
172.956529	6110.669681	25.383091
172.801769	6117.938840	25.388109
173.384898	6110.202513	25.393127
173.321919	6120.989594	25.398144
173.393368	6120.279101	25.403162
173.433803	6113.290383	25.408179
173.766596	6118.991140	25.413197
173.961862	6118.555601	25.418215
173.669395	6134.312290	25.423232
173.862468	6141.346964	25.428250
174.209459	6147.704610	25.433267
174.057001	6146.378698	25.438285
174.227401	6147.735520	25.443303
174.416806	6169.578980	25.448320
174.744209	6183.766685	25.453338
174.645086	6189.667538	25.458355
174.775669	6218.499480	25.463373
174.826159	6220.040706	25.468391
174.749239	6237.595131	25.473408
174.710993	6251.098821	25.478426
174.985588	6265.715503	25.483443
174.781757	6291.190157	25.488461
175.464444	6300.402507	25.493479
175.769732	6333.429233	25.498496
176.068939	6340.583653	25.503514
176.481012	6347.064135	25.508531
176.862924	6378.830862	25.513549
177.061097	6380.535054	25.518567
176.803784	6389.591922	25.523584
177.568449	6391.354191	25.528602
177.957792	6394.003177	25.533619
178.133075	6404.554253	25.538637
178.118839	6395.393583	25.543655
178.260174	6407.141514	25.548672
178.670132	6417.631891	25.553690
178.849524	6420.843069	25.558707
178.999562	6427.220409	25.563725
179.054953	6417.509776	25.568743
179.078672	6427.557498	25.573760
179.183059	6435.957662	25.578778
179.459495	6450.348121	25.583795
179.345105	6446.202698	25.588813
179.719641	6451.355254	25.593831
180.000094	6469.232296	25.598848
179.979619	6475.584530	25.603866
180.542095	6480.359857	25.608883
180.372004	6489.632634	25.613901
180.641526	6483.401664	25.618919
180.118816	6497.587278	25.623936
180.398935	6518.842203	25.628954
180.810458	6519.793007	25.633971
181.066625	6538.742448	25.638989
181.691409	6535.403755	25.644007
181.756650	6533.737218	25.649024
182.099970	6535.317294	25.654042
182.442194	6546.851291	25.659059
182.409398	6558.633121	25.664077
182.320404	6559.547625	25.669095
182.338579	6559.336212	25.674112
182.785839	6572.178760	25.679130
183.084278	6577.166374	25.684148
183.132802	6596.204254	25.689165
183.041642	6590.990586	25.694183
183.047969	6603.944188	25.699200
183.280838	6614.338227	25.704218
183.772446	6610.072342	25.709236
184.091307	6634.522122	25.714253
184.493574	6643.770138	25.719271
184.284355	6655.541318	25.724288
184.321403	6657.357447	25.729306
184.755964	6663.610489	25.734324
184.577439	6682.148580	25.739341
184.752189	6684.107320	25.744359
185.257210	6705.302673	25.749376
185.227515	6715.257327	25.754394
185.319629	6710.836964	25.759412
185.638191	6733.033232	25.764429
185.941109	6738.738547	25.769447
185.821082	6754.291408	25.774464
186.041378	6776.883483	25.779482
186.649165	6777.314627	25.784500
186.179458	6790.754877	25.789517
186.639738	6807.333212	25.794535
186.868770	6818.922257	25.799552
186.855485	6836.711419	25.804570
187.463760	6841.990251	25.809588
187.692006	6853.178496	25.814605
188.346960	6852.016618	25.819623
188.618154	6855.871489	25.824640
188.705099	6864.231542	25.829658
188.874822	6853.877154	25.834676
188.506002	6864.538342	25.839693
188.994988	6875.117096	25.844711
188.936377	6891.240131	25.849728
188.984773	6889.900208	25.854746
189.113472	6895.926121	25.859764
189.142524	6918.472403	25.864781
190.029559	6903.827060	25.869799
190.139350	6905.804840	25.874816
190.356506	6933.641702	25.879834
190.757629	6927.580214	25.884852
191.069404	6932.161541	25.889869
191.331913	6936.423611	25.894887
191.169445	6937.640621	25.899904
190.906194	6937.637356	25.904922
191.244737	6939.306520	25.909940
191.515081	6949.083849	25.914957
191.928868	6959.885090	25.919975
192.141994	6961.930242	25.924992
191.806398	6975.836850	25.930010
192.065005	6966.233634	25.935028
192.171770	6992.895294	25.940045
192.344289	7004.947119	25.945063
192.469444	7002.470697	25.950080
192.395811	7017.107584	25.955098
192.758407	7030.029610	25.960116
192.473738	7046.523981	25.965133
193.167946	7062.477184	25.970151
193.177891	7077.607901	25.975168
193.337545	7096.233450	25.980186
193.957367	7108.459975	25.985204
194.129954	7129.502545	25.990221
193.986119	7132.151670	25.995239
194.315154	7140.260827	26.000256
194.124173	7158.515648	26.005274
194.711127	7170.301982	26.010292
194.891552	7187.605369	26.015309
194.868723	7193.375349	26.020327
195.446000	7215.999023	26.025344
195.581224	7232.085236	26.030362
195.927932	7238.624556	26.035380
195.876453	7243.938624	26.040397
196.321272	7260.538200	26.045415
196.872896	7271.472792	26.050432
196.625039	7272.855714	26.055450
197.091617	7284.723426	26.060468
197.305773	7302.286631	26.065485
197.131537	7314.625003	26.070503
197.315619	7316.183613	26.075520
197.089291	7336.946641	26.080538
197.561515	7343.930059	26.085556
197.852269	7359.964533	26.090573
197.984744	7370.807971	26.095591
198.309655	7386.614466	26.100608
198.881246	7395.061882	26.105626
199.370374	7388.882727	26.110644
199.259450	7402.115461	26.115661
199.563195	7415.699374	26.120679
200.061881	7421.999233	26.125696
199.967421	7422.249055	26.130714
200.061357	7416.196712	26.135732
200.302292	7430.039551	26.140749
200.558177	7446.274669	26.145767
201.040580	7439.764995	26.150784
201.346740	7442.677355	26.155802
201.539272	7429.047068	26.160820
201.865005	7428.463878	26.165837
201.911097	7427.590667	26.170855
202.411073	7424.288946	26.175872
202.214170	7432.681407	26.180890
202.058339	7426.218903	26.185908
202.286792	7430.423922	26.190925
202.311281	7441.066917	26.195943
202.767488	7450.168298	26.200960
202.390873	7470.201785	26.205978
202.646986	7457.383799	26.210996
202.663966	7487.220644	26.216013
202.826687	7492.920326	26.221031
203.215985	7512.955716	26.226048
203.211993	7531.179697	26.231066
203.260137	7539.319086	26.236084
203.569035	7564.089471	26.241101
203.569913	7581.316134	26.246119
203.997592	7596.958695	26.251136
203.970787	7624.384815	26.256154
204.379977	7631.673008	26.261172
204.235275	7660.825733	26.266189
204.411243	7671.341292	26.271207
204.722406	7690.130630	26.276224
204.816841	7723.845507	26.281242
205.277907	7732.773691	26.286260
205.675340	7758.359528	26.291277
205.952733	7771.850575	26.296295
206.654514	7785.989717	26.301312
206.723105	7794.896977	26.306330
207.056409	7799.289735	26.311348
207.177702	7816.080844	26.316365
206.941530	7813.135261	26.321383
207.301082	7828.166584	26.326400
207.422922	7840.620045	26.331418
207.598412	7860.000836	26.336436
208.448389	7863.689784	26.341453
208.319054	7864.130722	26.346471
208.977583	7877.458055	26.351488
209.331632	7890.465749	26.356506
209.536267	7894.563107	26.361524
209.994996	7895.089167	26.366541
210.325445	7888.822792	26.371559
210.219679	7880.510448	26.376576
210.136735	7891.219423	26.381594
210.482284	7886.162877	26.386612
210.912594	7898.324808	26.391629
210.828748	7911.676216	26.396647
211.210716	7912.060239	26.401664
210.964856	7920.275425	26.406682
210.931859	7916.084943	26.411700
211.136699	7935.827908	26.416717
211.083281	7954.443710	26.421735
211.623067	7970.150140	26.426752
211.496331	7981.805738	26.431770
211.686067	7992.848549	26.436788
211.946431	8014.289255	26.441805
212.559357	8018.567970	26.446823
213.042688	8020.595306	26.451840
212.975922	8034.388996	26.456858
213.386044	8039.980292	26.461876
213.687097	8042.688023	26.466893
213.621257	8049.972749	26.471911
213.977524	8053.253991	26.476928
214.085856	8062.891184	26.481946
214.141709	8066.217619	26.486964
214.347887	8074.208871	26.491981
214.576339	8104.446270	26.496999
214.699220	8107.992839	26.502016
215.014634	8119.575113	26.507034
215.151056	8134.032845	26.512052
215.557082	8142.646906	26.517069
215.037654	8165.732489	26.522087
215.403565	8174.507853	26.527104
215.469960	8194.086580	26.532122
215.860454	8206.614024	26.537140
215.890837	8223.963943	26.542157
216.303078	8245.659387	26.547175
216.206575	8267.974622	26.552192
216.435657	8291.040016	26.557210
216.539486	8308.301019	26.562228
217.085358	8320.239419	26.567245
217.378855	8350.358988	26.572263
217.733389	8360.108571	26.577280
217.888771	8373.760482	26.582298
217.845537	8396.723805	26.587316
218.464909	8411.689871	26.592333
218.759576	8432.862912	26.597351
219.164002	8443.916504	26.602368
219.054807	8466.793544	26.607386
219.330038	8467.484221	26.612404
219.877000	8488.473071	26.617421
219.753287	8497.931283	26.622439
220.021414	8516.406746	26.627456
220.122273	8530.034259	26.632474
220.113653	8547.135167	26.637492
220.413869	8554.322713	26.642509
220.846945	8593.284232	26.647527
220.954817	8600.117155	26.652544
221.092594	8618.752160	26.657562
221.570432	8628.343689	26.662580
221.788664	8650.152504	26.667597
221.640827	8667.763495	26.672615
222.205570	8681.606274	26.677632
223.181850	8676.392528	26.682650
224.235258	8661.055309	26.687668
224.924969	8651.485133	26.692685
225.261220	8646.682839	26.697703
225.192398	8636.942523	26.702720
225.256745	8623.894134	26.707738
225.393594	8625.274254	26.712756
225.473044	8616.146679	26.717773
225.577668	8616.896543	26.722791
225.879171	8603.003147	26.727808
225.853634	8579.368382	26.732826
225.822773	8582.307996	26.737844
225.683205	8570.473192	26.742861
225.624246	8579.610737	26.747879
225.757731	8590.395740	26.752896
226.057248	8611.739146	26.757914
225.429520	8618.908511	26.762932
225.835592	8636.108607	26.767949
225.600170	8657.352320	26.772967
226.005050	8680.507891	26.777984
226.255326	8700.359820	26.783002
226.084326	8741.094659	26.788020
226.368247	8761.341117	26.793037
226.181675	8790.730748	26.798055
226.826226	8817.052727	26.803072
226.940466	8854.765654	26.808090
227.107798	8881.754901	26.813108
228.004716	8901.424547	26.818125
227.626667	8920.195586	26.823143
227.975987	8946.334389	26.828160
228.473715	8986.126410	26.833178
228.767379	9015.070149	26.838196
228.803743	9040.912941	26.843213
229.283122	9071.657491	26.848231
229.578950	9087.114539	26.853248
229.870344	9107.854135	26.858266
229.687186	9143.393811	26.863284
230.591576	9164.687058	26.868301
230.365847	9190.061329	26.873319
230.704628	9201.705772	26.878336
231.399194	9229.174064	26.883354
231.507529	9241.218874	26.888372
231.598408	9265.035758	26.893389
232.038733	9284.287782	26.898407
232.433537	9296.888611	26.903424
233.164844	9297.738301	26.908442
233.190233	9314.524563	26.913460
233.835301	9312.664602	26.918477
234.102534	9309.077801	26.923495
234.190712	9308.907929	26.928512
235.112017	9310.035473	26.933530
234.751871	9312.506153	26.938548
235.048706	9325.654817	26.943565
234.757032	9342.604178	26.948583
235.183133	9345.129188	26.953600
236.135494	9343.884664	26.958618
235.326824	9359.184625	26.963636
235.557722	9371.882938	26.968653
235.541489	9384.247020	26.973671
235.895348	9400.504351	26.978688
235.874269	9422.920919	26.983706
236.035565	9446.467579	26.988724
236.270545	9447.240049	26.993741
236.840918	9462.842642	26.998759
237.320817	9475.126482	27.003776
237.398768	9485.348820	27.008794
237.394644	9502.658755	27.013812
237.785861	9514.492981	27.018829
238.029813	9531.032432	27.023847
238.183544	9547.696090	27.028864
238.235333	9562.138094	27.033882
238.367273	9581.982239	27.038900
238.559502	9593.288085	27.043917
238.875178	9625.446839	27.048935
238.785903	9632.963991	27.053952
239.276997	9656.216490	27.058970
239.295847	9683.550830	27.063988
240.087451	9691.213270	27.069005
240.215248	9726.272319	27.074023
240.419782	9730.423742	27.079040
241.196013	9744.633011	27.084058
240.950422	9764.181237	27.089076
241.065904	9777.852994	27.094093
241.101862	9796.818815	27.099111
241.349566	9809.435804	27.104128
242.317655	9819.200082	27.109146
241.942563	9840.461405	27.114164
242.503351	9857.375496	27.119181
242.307554	9886.357416	27.124199
242.460388	9892.101405	27.129216
242.575556	9914.867186	27.134234
242.656487	9949.936326	27.139252
243.259441	9967.746233	27.144269
243.762480	9991.110625	27.149287
243.939539	10013.443623	27.154304
244.721952	10023.577072	27.159322
244.812001	10041.323695	27.164340
245.207532	10037.873901	27.169357
245.555853	10059.203765	27.174375
245.999486	10068.875295	27.179392
246.196322	10068.428361	27.184410
246.522288	10089.965375	27.189428
246.784231	10101.286417	27.194445
247.049116	10109.745299	27.199463
246.930188	10109.691283	27.204480
246.826414	10124.650527	27.209498
247.611395	10140.008987	27.214516
247.647299	10155.070383	27.219533
247.638043	10171.062959	27.224551
247.526782	10181.409563	27.229568
248.216114	10195.859469	27.234586
248.555457	10215.484471	27.239604
248.753021	10228.937685	27.244621
248.842845	10245.912421	27.249639
249.166734	10265.819053	27.254656
249.422456	10272.371272	27.259674
249.329717	10299.968453	27.264692
249.960197	10302.277368	27.269709
250.217591	10325.444820	27.274727
249.944993	10342.013754	27.279744
250.487571	10350.020179	27.284762
250.738625	10370.828191	27.289780
250.792236	10377.890996	27.294797
251.000840	10410.681083	27.299815
251.329809	10426.886984	27.304832
252.086908	10419.104623	27.309850
252.624950	10425.378444	27.314868
252.803474	10436.731353	27.319885
253.101435	10455.884685	27.324903
252.973505	10458.771151	27.329920
253.207138	10463.218761	27.334938
253.655136	10489.286417	27.339956
253.919325	10478.551864	27.344973
254.483347	10508.499873	27.349991
254.337149	10527.574985	27.355008
254.701998	10521.341102	27.360026
254.955937	10536.991093	27.365044
254.862578	10542.865758	27.370061
255.287185	10557.148621	27.375079
255.208590	10581.981394	27.380096
255.537079	10595.098878	27.385114
255.607291	10624.879602	27.390132
255.883120	10643.906154	27.395149
255.915025	10662.637303	27.400167
255.853414	10690.297573	27.405184
256.537324	10708.709009	27.410202
256.621736	10742.187642	27.415220
256.677931	10762.731717	27.420237
257.063235	10786.308117	27.425255
257.233176	10821.844525	27.430272
257.630386	10830.255890	27.435290
257.769903	10870.879819	27.440308
257.915418	10899.863351	27.445325
258.366247	10914.480851	27.450343
258.076253	10938.559306	27.455360
258.824512	10962.089510	27.460378
259.214553	11001.794633	27.465396
259.659333	11022.233036	27.470413
260.452144	11030.293040	27.475431
260.321906	11062.838372	27.480448
260.755003	11073.216737	27.485466
261.060497	11089.436779	27.490484
261.219930	11109.145704	27.495501
261.530291	11124.695188	27.500519
261.634117	11139.455888	27.505536
261.993207	11167.345859	27.510554
262.349322	11179.795623	27.515572
262.946583	11208.418615	27.520589
263.356281	11215.803698	27.525607
263.945877	11218.543678	27.530624
264.355636	11236.851417	27.535642
264.248921	11242.049402	27.540660
263.714946	11241.789157	27.545677
264.134385	11250.534177	27.550695
264.622144	11272.896027	27.555712
264.932156	11278.452825	27.560730
264.976116	11289.613493	27.565748
264.911841	11313.647510	27.570765
265.511263	11312.042582	27.575783
265.397721	11339.073029	27.580800
265.718031	11350.890812	27.585818
266.064043	11368.448452	27.590836
265.992996	11385.190345	27.595853
266.217069	11417.554310	27.600871
266.342093	11445.522698	27.605888
266.940468	11462.904808	27.610906
267.008430	11495.946547	27.615924
267.074250	11516.754680	27.620941
267.544540	11540.224627	27.625959
267.567988	11560.444371	27.630976
267.701187	11591.825107	27.635994
268.168744	11627.260256	27.641012
268.284638	11646.721989	27.646029
268.761854	11664.810621	27.651047
269.434665	11690.548545	27.656064
270.005346	11706.503117	27.661082
270.521054	11723.248804	27.666100
270.671209	11739.316459	27.671117
271.161023	11738.327568	27.676135
272.069106	11741.774244	27.681152
273.209837	11738.071876	27.686170
273.329876	11722.376445	27.691188
273.811477	11721.395267	27.696205
273.695458	11706.849786	27.701223
273.912229	11706.889518	27.706240
273.956018	11688.630494	27.711258
274.301671	11694.152960	27.716276
274.112315	11698.003625	27.721293
274.359424	11707.932032	27.726311
274.267844	11721.628307	27.731328
274.662578	11730.823820	27.736346
274.382211	11734.686941	27.741364
274.557485	11770.791852	27.746381
274.725872	11773.125028	27.751399
274.470059	11813.355727	27.756416
274.819101	11837.841322	27.761434
275.248095	11858.007688	27.766452
274.887532	11892.734322	27.771469
275.378201	11913.769582	27.776487
275.644769	11953.424115	27.781504
275.509765	11985.994165	27.786522
276.002273	12014.140093	27.791540
276.264443	12050.564838	27.796557
276.576502	12076.833274	27.801575
276.733599	12120.213716	27.806592
277.188452	12155.149445	27.811610
277.758424	12180.199721	27.816628
277.846500	12214.213435	27.821645
278.183946	12240.003404	27.826663
278.496040	12259.202142	27.831680
278.961237	12291.078923	27.836698
279.296111	12313.747361	27.841716
279.323770	12339.240705	27.846733
279.609508	12365.022397	27.851751
280.019628	12398.484851	27.856768
280.159731	12425.328624	27.861786
280.693812	12454.982750	27.866804
280.677009	12475.867729	27.871821
281.331808	12489.074234	27.876839
281.861208	12518.964108	27.881856
281.927093	12540.482750	27.886874
282.341752	12570.108696	27.891892
282.676532	12596.123481	27.896909
282.634163	12610.738778	27.901927
282.881880	12632.533705	27.906944
283.200762	12657.741223	27.911962
283.627815	12682.159551	27.916980
283.584844	12713.805888	27.921997
283.859212	12742.781639	27.927015
284.517598	12765.574927	27.932032
284.222687	12792.566356	27.937050
284.744028	12827.980706	27.942068
284.961701	12857.956148	27.947085
285.195232	12885.131396	27.952103
285.390236	12917.854775	27.957120
285.727784	12942.399156	27.962138
286.203288	12976.089572	27.967156
286.301294	13011.026820	27.972173
286.755226	13044.368030	27.977191
287.099241	13063.745066	27.982208
287.449389	13082.451236	27.987226
288.215995	13106.003464	27.992244
288.354327	13132.511413	27.997261
288.902275	13148.379881	28.002279
289.300564	13165.331578	28.007296
289.671942	13192.895072	28.012314
290.457193	13198.268632	28.017332
290.611291	13221.002407	28.022349
290.744840	13227.468009	28.027367
290.736771	13238.470278	28.032384
290.641203	13261.068799	28.037402
291.341809	13276.276055	28.042420
291.302644	13302.791058	28.047437
291.616192	13322.860809	28.052455
291.934554	13345.211977	28.057472
292.008053	13375.950696	28.062490
292.198787	13402.070254	28.067508
292.193770	13421.535904	28.072525
292.681813	13449.505387	28.077543
293.170792	13477.336059	28.082560
293.532308	13495.594707	28.087578
294.138923	13513.258146	28.092596
294.217301	13530.061728	28.097613
294.290875	13546.005579	28.102631
294.969778	13566.347151	28.107648
295.065742	13584.437056	28.112666
295.659057	13596.085161	28.117684
296.047863	13611.150728	28.122701
296.554396	13612.718527	28.127719
297.222881	13620.449662	28.132736
297.760696	13617.401881	28.137754
297.797106	13628.207651	28.142772
297.969632	13633.883389	28.147789
298.051305	13659.424689	28.152807
298.452448	13665.863515	28.157824
298.085429	13675.981908	28.162842
298.905834	13688.008839	28.167860
298.387528	13709.162592	28.172877
298.997984	13728.215772	28.177895
299.499718	13753.508695	28.182912
299.775275	13776.736249	28.187930
299.894156	13788.041817	28.192948
299.819425	13811.463428	28.197965
300.286183	13836.444089	28.202983
300.791751	13855.135536	28.208000
300.483549	13882.752037	28.213018
300.820112	13902.293687	28.218036
301.427715	13932.864676	28.223053
301.969004	13945.004256	28.228071
302.777700	13960.754745	28.233088
302.839796	13972.867717	28.238106
303.270117	13985.393596	28.243124
303.493559	14003.955457	28.248141
304.127885	14031.881949	28.253159
304.791956	14035.493897	28.258176
304.482460	14046.386020	28.263194
304.985748	14069.828723	28.268212
305.084085	14088.962211	28.273229
304.886723	14103.614854	28.278247
305.290679	14129.758918	28.283264
305.815442	14151.634475	28.288282
306.086575	14162.108771	28.293300
305.995246	14190.245013	28.298317
306.134599	14196.077946	28.303335
306.507133	14224.505154	28.308352
306.822162	14264.721243	28.313370
307.335109	14278.330223	28.318388
307.477202	14309.063656	28.323405
307.843821	14337.359670	28.328423
308.090615	14359.817480	28.333440
308.297408	14381.109470	28.338458
308.884130	14404.735379	28.343476
309.268092	14427.987830	28.348493
309.867933	14437.966201	28.353511
311.077437	14443.797081	28.358528
311.389257	14459.839693	28.363546
312.336326	14449.092704	28.368564
312.585722	14445.430617	28.373581
312.866395	14441.468418	28.378599
313.393805	14425.530362	28.383616
313.115661	14422.574994	28.388634
313.338857	14410.404242	28.393652
313.599251	14415.781473	28.398669
313.202335	14420.708647	28.403687
313.604941	14434.084473	28.408704
313.626278	14452.889540	28.413722
313.877025	14463.783645	28.418740
314.011359	14471.326164	28.423757
313.896143	14501.809301	28.428775
314.412156	14520.542275	28.433792
314.381151	14549.058118	28.438810
314.804114	14574.534462	28.443828
314.697834	14609.994017	28.448845
314.915997	14635.940596	28.453863
315.608222	14662.409671	28.458880
315.753255	14704.344124	28.463898
315.846879	14727.437116	28.468916
316.439250	14755.635261	28.473933
317.018748	14795.200461	28.478951
317.268630	14826.568953	28.483968
317.429983	14845.214911	28.488986
317.772256	14873.241748	28.494004
318.538493	14898.691286	28.499021
318.652578	14933.885208	28.504039
319.474352	14945.911258	28.509056
319.721083	14972.162419	28.514074
320.155983	14990.430642	28.519092
320.206525	15011.918886	28.524109
321.816870	15007.712909	28.529127
322.409885	15003.041317	28.534144
322.325749	15006.858952	28.539162
322.674871	15004.888336	28.544180
323.047638	15026.477428	28.549197
323.021712	15040.751583	28.554215
323.226504	15034.297541	28.559232
323.404634	15053.713236	28.564250
323.933241	15068.578061	28.569268
324.174027	15077.987846	28.574285
324.691897	15102.258647	28.579303
324.825612	15111.869651	28.584320
325.002623	15123.566549	28.589338
325.096796	15144.081224	28.594356
325.127599	15160.041847	28.599373
325.222181	15184.886573	28.604391
325.652514	15192.057128	28.609408
325.783713	15223.519223	28.614426
325.912665	15240.028993	28.619444
326.156609	15282.014161	28.624461
326.029406	15319.952038	28.629479
326.815687	15347.339267	28.634496
326.606464	15382.320002	28.639514
327.286278	15411.546224	28.644532
327.747275	15443.781357	28.649549
327.729590	15477.496786	28.654567
328.418638	15497.687686	28.659584
328.568803	15535.059908	28.664602
328.576806	15570.401044	28.669620
329.188112	15591.054636	28.674637
329.453675	15622.641059	28.679655
330.342614	15646.488084	28.684672
330.571574	15685.964161	28.689690
330.667058	15714.238065	28.694708
331.068028	15738.939683	28.699725
331.073829	15773.468234	28.704743
331.807109	15789.083653	28.709760
331.911883	15830.900169	28.714778
331.893866	15860.328747	28.719796
332.289778	15885.196967	28.724813
332.581776	15933.572414	28.729831
333.001463	15968.876946	28.734848
333.270974	16016.362687	28.739866
333.520268	16048.983655	28.744884
333.999498	16082.358198	28.749901
334.275632	16131.786807	28.754919
334.850823	16157.702956	28.759936
335.177597	16197.935914	28.764954
335.638880	16221.792428	28.769972
336.259373	16257.624354	28.774989
336.573518	16296.242333	28.780007
337.330304	16313.479486	28.785024
337.645349	16326.789880	28.790042
338.444721	16350.394741	28.795060
338.452450	16366.198106	28.800077
338.293547	16397.556075	28.805095
338.637869	16410.093807	28.810112
338.985396	16444.120636	28.815130
339.044718	16466.206715	28.820148
340.046329	16499.665978	28.825165
340.297233	16526.352395	28.830183
340.740635	16557.687841	28.835200
341.140844	16580.869594	28.840218
340.964830	16597.757719	28.845236
341.520690	16625.539671	28.850253
341.504199	16663.352858	28.855271
341.999160	16694.643468	28.860288
342.372000	16725.292960	28.865306
342.801415	16755.318001	28.870324
343.337407	16779.208229	28.875341
343.634473	16799.661798	28.880359
344.271244	16817.422930	28.885376
344.670886	16842.913064	28.890394
344.586619	16869.903398	28.895412
345.285480	16879.328714	28.900429
345.441704	16909.783931	28.905447
345.778117	16939.759031	28.910464
345.954831	16964.554503	28.915482
346.022525	16978.591993	28.920500
346.874402	17005.727947	28.925517
346.769990	17034.979498	28.930535
346.992151	17054.303277	28.935552
347.431835	17089.064451	28.940570
347.384801	17111.847495	28.945588
347.833802	17148.141106	28.950605
347.700264	17184.801054	28.955623
348.404250	17217.935991	28.960640
348.824931	17255.152202	28.965658
349.086789	17287.615791	28.970676
349.832603	17311.508660	28.975693
350.630936	17348.116467	28.980711
350.913871	17362.859923	28.985728
351.266208	17388.363727	28.990746
351.489794	17412.562219	28.995764
351.963945	17439.506644	29.000781
352.096901	17467.546927	29.005799
352.444439	17488.191330	29.010816
353.079807	17514.677860	29.015834
352.981971	17542.264372	29.020852
353.589987	17556.389472	29.025869
354.279927	17578.594392	29.030887
354.670885	17606.743615	29.035904
355.084878	17622.506922	29.040922
354.923764	17659.109572	29.045940
355.350606	17685.261625	29.050957
355.544008	17719.916549	29.055975
356.011819	17749.142225	29.060992
356.487936	17779.515825	29.066010
356.373808	17818.371526	29.071028
356.615184	17843.888734	29.076045
356.886996	17887.795918	29.081063
357.410020	17921.827212	29.086080
357.608214	17956.570090	29.091098
357.923830	17993.347171	29.096116
358.346362	18029.235748	29.101133
358.313992	18076.739664	29.106151
358.920574	18120.054052	29.111168
359.218467	18157.502996	29.116186
359.157703	18198.210785	29.121204
359.888690	18242.565206	29.126221
360.009383	18297.021464	29.131239
360.511479	18329.088015	29.136256
361.842186	18345.852120	29.141274
362.442868	18373.536282	29.146292
363.218227	18401.299339	29.151309
363.296948	18422.911696	29.156327
363.527644	18452.652214	29.161344
363.806306	18478.216025	29.166362
363.711666	18504.465031	29.171380
364.224377	18534.357593	29.176397
364.519964	18579.467038	29.181415
364.824030	18610.134923	29.186432
365.220810	18644.514101	29.191450
365.829160	18669.860889	29.196468
366.007593	18688.257534	29.201485
366.139398	18719.817551	29.206503
366.256371	18749.901292	29.211520
366.920014	18783.610677	29.216538
366.879976	18815.747415	29.221556
367.161201	18857.236960	29.226573
367.533772	18897.009755	29.231591
367.997161	18926.283963	29.236608
368.520324	18975.968736	29.241626
368.376767	19016.451463	29.246644
368.929136	19048.714160	29.251661
369.493906	19097.160792	29.256679
369.831157	19134.728145	29.261696
370.507557	19166.856295	29.266714
370.698526	19211.137113	29.271732
371.076166	19247.553133	29.276749
371.577566	19285.359150	29.281767
371.933630	19304.809206	29.286784
372.688041	19341.548725	29.291802
372.653913	19386.447221	29.296820
373.292673	19404.724768	29.301837
373.717616	19449.961008	29.306855
373.903700	19483.605426	29.311872
374.790651	19501.421145	29.316890
374.685760	19541.915847	29.321908
374.697596	19579.927827	29.326925
375.042022	19611.752651	29.331943
375.034133	19651.865196	29.336960
375.642407	19690.480004	29.341978
375.748073	19755.431866	29.346996
376.295290	19796.977471	29.352013
376.855192	19843.579156	29.357031
377.124591	19887.687480	29.362048
378.052167	19913.123342	29.367066
378.210132	19958.881294	29.372084
378.585102	20000.967783	29.377101
378.843262	20036.879347	29.382119
379.547915	20067.938490	29.387136
380.198897	20098.242163	29.392154
380.493039	20136.169170	29.397172
381.257765	20168.361354	29.402189
381.515210	20199.453228	29.407207
381.901311	20230.597219	29.412224
382.526494	20255.770067	29.417242
382.740544	20288.738013	29.422260
382.780381	20314.350263	29.427277
383.448541	20346.751702	29.432295
383.769165	20376.183764	29.437312
384.345369	20404.354803	29.442330
384.098796	20434.663096	29.447348
384.780300	20456.438079	29.452365
385.201090	20494.440370	29.457383
385.199249	20534.654882	29.462400
385.804829	20555.213103	29.467418
385.749550	20589.678441	29.472436
386.912336	20623.399000	29.477453
387.295778	20653.642293	29.482471
388.253896	20668.823251	29.487488
388.681685	20677.071997	29.492506
388.296758	20703.803050	29.497524
389.074017	20720.096739	29.502541
389.439006	20748.602564	29.507559
389.314765	20785.347577	29.512576
389.790651	20798.660766	29.517594
390.223493	20828.645192	29.522612
390.901741	20863.376436	29.527629
391.181971	20888.718141	29.532647
391.293482	20923.595509	29.537664
391.775326	20939.388144	29.542682
391.890284	20985.652937	29.547700
392.048918	21021.955776	29.552717
392.712235	21044.986646	29.557735
392.813495	21084.699124	29.562752
392.949568	21117.179028	29.567770
393.389502	21170.448188	29.572788
393.601516	21209.560118	29.577805
394.182862	21256.505770	29.582823
394.340788	21311.772700	29.587840
394.533901	21353.972553	29.592858
394.542214	21406.592633	29.597876
395.076175	21461.935952	29.602893
395.729817	21505.075926	29.607911
395.855000	21558.532695	29.612928
397.155580	21601.106328	29.617946
397.577363	21641.810658	29.622964
397.887404	21685.246503	29.627981
398.418290	21723.866591	29.632999
398.461076	21776.480327	29.638016
399.180273	21804.482535	29.643034
399.645101	21855.357395	29.648052
399.821170	21893.846287	29.653069
400.579523	21934.559870	29.658087
400.634127	21980.927590	29.663104
400.993120	22013.768386	29.668122
401.491370	22059.530445	29.673140
401.827902	22108.518375	29.678157
402.380987	22145.307940	29.683175
402.565053	22196.280813	29.688192
403.588267	22228.763772	29.693210
403.971270	22257.019878	29.698228
404.635332	22295.449706	29.703245
405.106793	22320.647230	29.708263
405.380540	22365.114472	29.713280
405.530890	22399.459918	29.718298
405.802080	22446.365800	29.723316
406.236760	22477.306883	29.728333
406.548488	22507.672994	29.733351
406.677289	22563.330592	29.738368
407.281766	22600.698968	29.743386
407.568486	22643.565647	29.748404
407.479451	22687.963426	29.753421
408.249785	22727.830003	29.758439
408.251988	22769.108827	29.763456
408.654244	22817.724814	29.768474
408.731100	22859.773259	29.773492
408.925591	22922.914718	29.778509
409.507870	22966.299280	29.783527
409.603002	23026.975920	29.788544
410.093305	23071.565587	29.793562
410.641637	23135.246463	29.798580
411.495537	23187.160958	29.803597
412.019277	23237.798007	29.808615
412.146809	23286.443474	29.813632
412.910335	23336.181809	29.818650
413.401203	23393.347644	29.823668
413.711889	23423.400143	29.828685
414.455882	23475.432122	29.833703
414.684962	23524.833625	29.838720
415.815351	23563.880301	29.843738
416.336105	23588.557120	29.848756
417.351191	23603.781420	29.853773
417.961031	23624.623342	29.858791
418.636588	23641.094976	29.863808
419.456331	23666.241109	29.868826
420.172037	23672.524244	29.873844
420.238662	23682.325111	29.878861
420.717324	23694.449395	29.883879
421.171775	23712.428831	29.888896
421.441015	23739.811092	29.893914
421.515263	23754.196874	29.898932
421.647775	23774.704422	29.903949
422.157859	23788.261697	29.908967
422.314639	23822.794986	29.913984
422.732410	23853.709910	29.919002
422.662871	23887.408397	29.924020
422.674800	23920.345440	29.929037
423.006241	23953.000691	29.934055
422.987077	24006.691697	29.939072
423.308130	24043.588185	29.944090
423.807104	24096.988813	29.949108
424.032712	24148.638526	29.954125
425.207358	24200.116303	29.959143
425.134442	24256.022127	29.964160
425.372165	24299.062199	29.969178
426.005471	24347.491515	29.974196
426.466920	24394.187162	29.979213
426.975643	24443.376202	29.984231
426.946862	24506.687902	29.989248
427.427542	24554.919998	29.994266
428.292138	24600.831089	29.999284
428.760635	24652.513237	30.004301
429.174111	24694.435927	30.009319
429.380492	24734.974742	30.014336
429.928421	24786.274619	30.019354
430.286220	24830.295373	30.024372
430.786504	24877.115001	30.029389
431.473756	24913.808651	30.034407
431.781146	24961.049550	30.039424
432.208524	24998.854100	30.044442
432.643325	25046.817842	30.049460
433.099104	25084.564088	30.054477
433.873822	25109.994486	30.059495
434.287726	25152.407151	30.064512
434.955455	25185.956595	30.069530
435.657362	25212.134607	30.074548
435.839659	25255.312734	30.079565
436.534711	25280.381655	30.084583
436.558686	25316.158307	30.089600
436.748385	25355.950673	30.094618
437.238135	25386.174642	30.099636
437.253224	25440.845271	30.104653
437.707635	25480.046834	30.109671
438.242739	25535.168071	30.114688
438.648469	25578.163608	30.119706
439.103529	25626.131792	30.124724
439.084178	25685.061390	30.129741
439.451938	25731.436011	30.134759
439.790436	25785.405625	30.139776
440.509737	25839.736019	30.144794
441.285431	25884.350301	30.149812
441.979737	25933.111144	30.154829
442.705211	25966.601734	30.159847
443.167769	26009.938762	30.164864
443.233686	26052.299690	30.169882
444.007998	26088.485641	30.174900
444.586974	26140.910404	30.179917
444.880996	26174.740314	30.184935
445.192733	26215.598927	30.189952
445.916483	26262.907676	30.194970
446.607552	26290.243775	30.199988
447.048068	26327.055257	30.205005
447.836975	26355.693340	30.210023
448.363416	26393.960310	30.215040
449.018698	26412.911332	30.220058
449.721150	26435.002654	30.225076
449.643553	26476.266143	30.230093
449.984849	26506.700474	30.235111
450.307477	26535.705829	30.240128
450.371343	26572.235354	30.245146
451.053192	26607.021772	30.250164
451.016347	26653.957163	30.255181
451.404029	26694.154016	30.260199
451.761101	26750.218172	30.265216
452.212493	26791.502178	30.270234
452.944269	26836.126431	30.275252
452.485425	26885.324146	30.280269
453.205067	26943.222801	30.285287
453.291918	26987.106164	30.290304
453.356181	27055.468299	30.295322
454.150497	27101.360201	30.300340
454.145629	27173.337414	30.305357
454.437647	27224.451732	30.310375
454.919164	27288.484281	30.315392
455.300630	27339.712957	30.320410
455.657682	27409.562708	30.325428
456.145942	27483.993195	30.330445
456.624813	27542.297901	30.335463
457.131393	27610.384497	30.340480
457.764568	27682.058867	30.345498
458.711574	27727.822140	30.350516
459.297392	27784.825282	30.355533
459.661996	27842.128373	30.360551
460.138782	27900.093895	30.365568
460.675475	27965.072254	30.370586
461.212724	28011.477528	30.375604
461.669854	28068.875929	30.380621
462.382916	28116.519651	30.385639
462.917009	28177.621780	30.390656
463.059188	28231.790342	30.395674
463.568646	28273.821939	30.400692
463.939184	28330.778559	30.405709
464.656391	28385.420121	30.410727
465.588722	28433.348944	30.415744
465.852735	28475.643934	30.420762
466.654035	28520.957838	30.425780
468.047444	28538.967540	30.430797
469.082870	28564.137473	30.435815
469.647693	28578.714519	30.440832
470.234421	28620.181572	30.445850
470.866908	28623.795836	30.450868
471.447157	28642.490807	30.455885
471.928233	28660.458195	30.460903
472.415022	28671.051213	30.465920
472.603405	28697.571717	30.470938
473.181547	28706.846057	30.475956
473.308625	28735.339582	30.480973
473.101030	28748.585162	30.485991
473.578567	28779.432350	30.491008
473.793426	28827.516742	30.496026
474.232749	28851.394675	30.501044
474.754544	28892.845103	30.506061
474.984204	28927.773570	30.511079
475.997549	28965.533642	30.516096
476.256368	29006.297408	30.521114
477.029594	29033.349234	30.526132
477.187809	29070.117050	30.531149
477.649663	29087.993515	30.536167
478.315495	29127.574055	30.541184
478.228248	29171.461156	30.546202
478.710991	29210.741962	30.551220
479.082962	29259.034093	30.556237
479.243689	29299.667052	30.561255
479.783815	29353.316531	30.566272
479.972339	29393.380163	30.571290
480.376828	29431.075180	30.576308
480.597805	29492.595223	30.581325
481.355206	29531.192326	30.586343
482.075944	29577.888974	30.591360
482.195864	29634.337433	30.596378
482.763444	29668.455361	30.601396
483.855216	29711.782085	30.606413
484.252300	29749.046780	30.611431
485.082162	29783.665852	30.616448
485.458226	29820.505182	30.621466
486.397576	29846.160403	30.626484
486.745753	29884.670636	30.631501
486.871751	29921.849623	30.636519
487.518222	29959.983912	30.641536
487.741398	29998.216057	30.646554
488.128892	30026.058069	30.651572
489.047733	30069.386906	30.656589
489.268289	30112.071907	30.661607
489.912144	30148.272834	30.666624
490.246670	30188.622474	30.671642
490.736422	30235.237381	30.676660
490.913729	30270.906361	30.681677
491.385382	30312.349784	30.686695
492.204035	30349.944244	30.691712
492.630960	30400.356799	30.696730
493.273929	30440.796155	30.701748
493.782850	30477.399523	30.706765
493.894860	30523.158536	30.711783
494.690359	30566.292003	30.716800
494.828554	30615.524031	30.721818
495.591472	30653.377964	30.726836
496.144413	30703.996981	30.731853
496.390040	30753.457108	30.736871
497.162977	30789.883355	30.741888
497.428237	30844.436425	30.746906
497.873446	30882.989001	30.751924
498.261361	30925.252848	30.756941
499.118795	30982.450142	30.761959
499.877403	31020.791544	30.766976
500.439637	31061.987692	30.771994
500.911504	31099.475922	30.777012
501.367775	31140.460056	30.782029
501.866110	31196.978024	30.787047
502.036873	31236.190562	30.792064
502.179614	31281.103732	30.797082
502.949290	31324.912443	30.802100
503.413123	31376.501619	30.807117
503.500671	31418.745528	30.812135
504.124207	31480.547445	30.817152
504.525822	31533.880147	30.822170
505.356590	31581.989551	30.827188
505.953942	31642.243965	30.832205
506.257649	31693.864652	30.837223
506.901790	31734.691740	30.842240
507.239630	31797.566129	30.847258
507.749744	31843.140408	30.852276
507.990201	31880.325967	30.857293
507.976055	31938.256309	30.862311
508.382244	31994.903043	30.867328
508.952251	32042.430392	30.872346
510.046770	32096.570666	30.877364
511.078270	32143.122998	30.882381
511.048905	32185.117361	30.887399
512.045988	32231.565372	30.892416
512.542007	32274.066353	30.897434
513.181812	32313.191424	30.902452
513.504230	32363.494904	30.907469
514.272604	32416.234084	30.912487
514.823650	32451.287984	30.917504
515.142487	32497.433183	30.922522
515.511679	32542.241297	30.927540
516.248906	32580.495050	30.932557
516.368921	32637.969173	30.937575
516.921867	32679.745004	30.942592
517.275220	32737.050077	30.947610
517.643323	32789.111015	30.952628
518.164901	32846.296095	30.957645
518.794984	32902.904187	30.962663
519.476398	32951.746623	30.967680
520.003841	33005.967881	30.972698
520.812797	33045.696742	30.977716
521.968877	33084.684550	30.982733
522.448466	33131.031059	30.987751
523.353084	33167.284973	30.992768
523.423884	33206.156031	30.997786
523.913119	33247.644294	31.002804
524.403409	33298.243535	31.007821
524.845075	33338.607192	31.012839
525.520530	33384.210719	31.017856
525.884247	33425.206485	31.022874
526.051987	33465.046139	31.027892
527.193801	33510.203995	31.032909
527.486101	33560.474965	31.037927
528.314383	33601.666104	31.042944
528.768577	33656.949654	31.047962
528.858279	33699.952844	31.052980
529.542874	33740.206350	31.057997
530.017219	33793.735304	31.063015
530.320130	33829.535042	31.068032
530.731204	33891.340658	31.073050
530.934450	33945.484590	31.078068
531.330071	33988.669599	31.083085
531.715894	34055.491855	31.088103
532.442636	34108.309420	31.093120
532.616408	34168.433448	31.098138
533.108292	34231.845436	31.103156
534.143066	34284.695956	31.108173
534.433136	34355.310383	31.113191
535.568215	34402.772419	31.118208
536.410142	34439.819198	31.123226
537.109476	34489.918870	31.128244
537.549222	34525.415653	31.133261
537.982140	34568.699811	31.138279
538.856645	34606.757622	31.143296
539.359312	34632.762846	31.148314
539.899441	34668.028094	31.153332
540.629363	34703.137803	31.158349
540.867222	34743.542684	31.163367
541.557021	34777.428516	31.168384
541.903825	34821.409763	31.173402
541.868890	34866.886266	31.178420
542.474222	34908.393181	31.183437
542.655838	34972.798314	31.188455
543.073737	35022.556315	31.193472
543.688764	35070.481643	31.198490
544.215869	35129.658279	31.203508
544.789322	35181.596260	31.208525
545.042612	35242.590819	31.213543
546.411359	35289.241877	31.218560
546.849956	35339.467483	31.223578
547.656326	35388.437151	31.228596
548.658133	35425.360719	31.233613
549.236527	35475.111404	31.238631
549.931678	35515.171375	31.243648
550.624279	35548.550011	31.248666
550.886833	35597.442978	31.253684
551.542700	35638.207493	31.258701
551.850095	35679.268526	31.263719
552.604401	35720.997974	31.268736
552.859751	35762.266960	31.273754
552.977577	35815.118088	31.278772
553.732741	35856.835076	31.283789
554.008221	35913.008354	31.288807
554.208801	35968.525491	31.293824
554.937778	36021.313542	31.298842
555.020424	36095.978875	31.303860
555.694211	36146.706159	31.308877
556.373586	36221.424432	31.313895
556.934009	36276.707253	31.318912
557.305068	36333.869193	31.323930
557.923204	36404.826785	31.328948
558.730464	36457.650037	31.333965
559.203692	36522.922910	31.338983
559.834415	36582.013924	31.344000
560.349834	36640.597754	31.349018
560.889740	36705.727285	31.354036
561.581159	36763.031385	31.359053
561.784813	36839.967488	31.364071
562.148585	36895.879302	31.369088
562.700391	36966.809409	31.374106
562.901795	37033.727884	31.379124
564.096480	37096.382374	31.384141
564.744575	37165.955222	31.389159
564.977502	37226.682132	31.394176
565.768684	37294.810495	31.399194
566.089265	37356.226737	31.404212
566.720316	37415.664460	31.409229
567.674816	37468.332834	31.414247
567.907512	37529.259653	31.419264
568.760502	37582.100421	31.424282
569.214179	37649.066307	31.429300
570.128269	37702.550380	31.434317
570.942079	37750.183547	31.439335
571.205809	37804.066598	31.444352
571.833174	37856.331260	31.449370
572.230163	37913.433717	31.454388
572.767517	37970.982651	31.459405
573.096038	38031.263379	31.464423
573.539407	38087.806006	31.469440
574.271962	38153.857856	31.474458
574.707344	38203.002819	31.479476
575.920320	38261.582811	31.484493
576.755523	38314.741257	31.489511
577.596374	38363.823497	31.494528
578.779574	38406.476834	31.499546
579.085295	38453.198177	31.504564
579.918863	38483.754811	31.509581
581.095441	38519.518269	31.514599
581.523449	38545.488211	31.519616
582.301419	38575.723060	31.524634
582.020489	38626.014682	31.529652
582.894176	38666.799151	31.534669
583.645016	38701.695171	31.539687
583.850704	38751.458653	31.544704
584.393795	38793.022957	31.549722
584.894582	38838.247082	31.554740
585.526118	38880.917115	31.559757
585.508573	38935.221021	31.564775
585.789959	39000.927032	31.569792
586.457998	39047.136374	31.574810
586.712549	39110.492334	31.579828
586.911776	39179.805609	31.584845
587.202035	39249.179314	31.589863
587.892697	39331.314470	31.594880
588.382806	39405.048978	31.599898
588.478941	39482.822736	31.604916
589.278733	39553.758223	31.609933
589.974678	39642.615057	31.614951
590.209037	39713.389154	31.619968
591.084148	39782.307918	31.624986
591.582846	39872.146750	31.630004
592.328052	39943.784473	31.635021
593.212076	40023.682802	31.640039
593.943887	40094.521511	31.645056
594.776667	40167.647861	31.650074
595.337663	40235.229853	31.655092
596.240809	40290.497604	31.660109
597.695492	40342.251882	31.665127
598.633051	40389.213996	31.670144
599.841709	40416.236748	31.675162
600.210275	40454.794380	31.680180
601.001400	40485.705735	31.685197
601.809282	40518.896883	31.690215
601.646961	40559.894597	31.695232
602.284246	40592.199530	31.700250
602.661594	40633.928967	31.705268
603.310086	40669.408217	31.710285
603.631353	40708.482783	31.715303
604.177685	40750.998084	31.720320
604.707330	40803.928743	31.725338
605.217354	40855.887340	31.730356
605.692518	40899.580179	31.735373
606.275249	40962.914657	31.740391
606.470826	41020.212761	31.745408
607.072423	41067.281507	31.750426
607.610490	41131.132523	31.755444
608.293729	41188.196050	31.760461
608.767072	41250.814607	31.765479
609.038942	41323.653258	31.770496
609.867821	41381.702755	31.775514
610.279836	41463.528837	31.780532
611.070880	41534.457605	31.785549
611.686630	41597.049769	31.790567
611.700142	41670.669689	31.795584
612.407571	41740.044367	31.800602
612.962425	41812.233388	31.805620
613.605642	41887.754363	31.810637
614.030721	41969.952991	31.815655
614.722456	42059.924017	31.820672
615.619754	42127.101627	31.825690
616.075472	42218.218942	31.830708
616.286433	42294.769152	31.835725
617.054040	42370.551775	31.840743
617.581044	42458.418498	31.845760
618.321675	42540.859214	31.850778
618.732173	42620.063583	31.855796
619.737251	42690.135956	31.860813
621.173385	42768.243252	31.865831
621.900753	42839.301543	31.870848
623.243500	42898.363377	31.875866
624.013772	42945.692133	31.880884
624.727608	42998.250119	31.885901
625.539719	43041.211363	31.890919
626.093167	43090.655308	31.895936
626.967637	43140.701164	31.900954
627.079929	43200.445225	31.905972
627.711766	43253.156905	31.910989
628.594940	43306.182486	31.916007
628.793481	43364.475579	31.921024
629.557623	43407.218529	31.926042
630.221193	43473.919995	31.931060
630.737160	43534.596930	31.936077
631.382932	43586.849299	31.941095
631.719052	43651.011895	31.946112
632.104393	43702.336638	31.951130
632.464297	43767.411281	31.956148
633.139736	43825.106237	31.961165
633.602754	43880.295807	31.966183
633.930380	43950.779444	31.971200
634.737948	44007.574478	31.976218
635.066578	44084.857028	31.981236
635.389226	44153.772879	31.986253
636.016486	44224.026211	31.991271
637.022451	44303.640885	31.996288
637.549663	44366.828999	32.001306
638.055639	44437.084953	32.006324
638.775483	44506.069827	32.011341
639.600812	44587.974476	32.016359
639.893286	44667.435021	32.021376
640.675933	44740.922539	32.026394
641.458652	44815.108217	32.031412
641.979866	44890.766341	32.036429
642.929734	44957.547152	32.041447
643.512435	45034.742681	32.046464
644.370884	45098.814385	32.051482
645.139593	45182.098673	32.056500
645.761655	45248.933508	32.061517
646.733089	45321.781454	32.066535
647.221807	45391.200725	32.071552
648.729496	45440.449449	32.076570
648.906564	45495.013745	32.081588
649.410412	45566.793229	32.086605
650.533241	45622.070633	32.091623
650.788767	45696.444805	32.096640
651.333412	45762.085189	32.101658
652.323227	45818.813375	32.106676
652.723635	45881.459805	32.111693
653.356357	45947.546813	32.116711
653.862446	46002.037246	32.121728
654.951241	46062.380969	32.126746
656.232801	46114.600869	32.131764
656.279426	46168.627299	32.136781
657.057015	46235.028401	32.141799
657.486218	46302.054716	32.146816
658.092367	46354.845746	32.151834
658.637043	46426.078273	32.156852
658.649965	46506.216527	32.161869
659.651399	46572.924694	32.166887
659.831047	46653.035001	32.171904
660.630314	46731.409877	32.176922
661.229831	46811.063620	32.181940
661.573612	46889.321362	32.186957
662.094162	46970.252575	32.191975
662.214496	47061.693801	32.196992
662.816891	47148.675551	32.202010
663.389448	47239.759071	32.207028
664.403810	47338.596707	32.212045
665.413351	47429.391506	32.217063
666.220002	47513.260583	32.222080
666.997040	47586.014658	32.227098
667.737197	47646.505219	32.232116
668.640443	47727.374063	32.237133
670.112625	47773.618688	32.242151
671.452864	47829.585343	32.247168
672.120126	47887.129769	32.252186
672.573849	47919.311298	32.257204
673.249873	47965.348509	32.262221
674.141196	48013.616671	32.267239
674.706685	48075.319741	32.272256
675.510827	48124.348498	32.277274
675.771344	48178.593454	32.282292
676.236372	48238.457107	32.287309
676.688327	48287.413956	32.292327
677.246588	48362.321436	32.297344
677.604174	48428.359894	32.302362
678.380192	48483.708137	32.307380
679.305879	48554.665352	32.312397
680.369258	48605.151202	32.317415
680.827724	48678.658844	32.322432
681.497074	48734.221906	32.327450
682.709616	48789.426762	32.332468
683.133396	48853.743420	32.337485
683.676869	48909.176938	32.342503
683.887374	48980.024497	32.347520
684.647882	49045.320111	32.352538
685.103102	49123.125635	32.357556
685.585547	49201.760673	32.362573
686.049053	49272.616498	32.367591
686.437044	49362.216054	32.372608
686.910696	49449.861954	32.377626
687.949584	49537.853635	32.382644
688.274658	49628.873949	32.387661
688.872645	49706.695259	32.392679
689.540585	49812.446569	32.397696
690.139156	49909.391254	32.402714
690.607748	50008.721404	32.407732
690.842860	50109.500848	32.412749
691.714605	50213.665330	32.417767
692.270420	50318.446748	32.422784
692.686798	50425.381631	32.427802
693.829023	50531.422016	32.432820
694.560919	50638.386146	32.437837
694.965119	50736.903423	32.442855
696.018434	50838.481485	32.447872
696.720517	50953.671769	32.452890
697.588805	51043.607429	32.457908
698.507135	51151.009942	32.462925
699.470210	51232.388577	32.467943
700.631455	51317.688576	32.472960
701.317553	51405.610126	32.477978
702.583161	51479.533416	32.482996
703.252879	51570.844908	32.488013
704.119113	51645.386896	32.493031
704.730297	51723.953183	32.498048
705.639302	51787.785732	32.503066
706.066996	51864.836104	32.508084
706.365882	51943.437810	32.513101
707.021867	52008.059946	32.518119
707.871108	52079.580139	32.523136
708.480044	52157.093421	32.528154
709.394855	52230.725819	32.533172
709.908946	52315.300701	32.538189
710.411451	52391.670595	32.543207
711.191608	52479.561884	32.548224
711.602922	52557.931965	32.553242
712.544637	52640.274150	32.558260
713.092143	52728.004215	32.563277
713.723731	52801.472440	32.568295
714.354348	52889.858729	32.573312
715.145153	52992.371153	32.578330
715.901508	53069.957547	32.583348
716.669496	53161.929336	32.588365
717.436962	53240.133702	32.593383
718.183013	53336.709903	32.598400
719.251089	53421.927575	32.603418
719.932421	53498.637592	32.608436
720.757598	53592.004300	32.613453
721.231334	53674.254037	32.618471
722.210780	53752.007088	32.623488
722.465115	53848.714243	32.628506
723.741105	53922.689160	32.633524
724.707513	54005.658352	32.638541
725.262725	54091.383789	32.643559
726.076250	54169.640804	32.648576
725.967351	54270.690031	32.653594
726.957459	54345.296822	32.658612
727.649023	54451.846240	32.663629
728.255972	54533.293177	32.668647
728.941271	54630.941333	32.673664
729.271202	54732.676002	32.678682
730.133547	54822.617261	32.683700
730.869946	54929.433267	32.688717
731.400931	55037.978532	32.693735
732.234972	55136.734792	32.698752
732.663110	55243.478899	32.703770
733.619874	55333.785434	32.708788
733.959665	55450.845962	32.713805
734.727438	55554.007454	32.718823
735.641889	55657.871065	32.723840
736.441587	55763.246217	32.728858
737.289277	55854.490079	32.733876
738.315240	55962.747037	32.738893
739.026715	56065.617479	32.743911
740.023453	56154.796025	32.748928
740.548485	56262.969783	32.753946
741.423320	56365.933850	32.758964
742.079190	56466.812604	32.763981
743.112386	56552.637346	32.768999
744.314120	56646.712182	32.774016
744.717907	56748.476027	32.779034
745.440081	56822.859895	32.784052
746.018084	56912.265196	32.789069
746.595722	57001.746792	32.794087
747.501443	57091.419056	32.799104
748.102101	57179.962187	32.804122
748.992199	57258.907009	32.809140
749.841209	57359.940424	32.814157
750.225994	57435.781011	32.819175
750.908386	57524.065179	32.824192
751.592230	57627.118962	32.829210
752.014806	57726.217537	32.834228
753.034345	57828.993652	32.839245
753.174905	57939.403659	32.844263
754.387200	58043.367595	32.849280
754.615777	58147.987202	32.854298
755.569544	58259.852304	32.859316
756.380063	58369.644292	32.864333
756.864495	58478.443589	32.869351
758.294093	58581.974898	32.874368
758.885591	58702.550448	32.879386
759.528935	58796.117873	32.884404
760.773410	58896.699354	32.889421
761.527716	59013.753768	32.894439
762.268031	59117.437468	32.899456
763.116330	59221.425536	32.904474
763.967194	59317.051841	32.909492
764.670776	59416.704637	32.914509
765.369487	59522.622303	32.919527
766.338201	59615.625802	32.924544
766.889732	59718.693883	32.929562
767.836296	59828.306095	32.934580
768.823022	59927.818076	32.939597
769.824280	60016.526164	32.944615
771.373295	60098.580017	32.949632
772.424792	60182.267973	32.954650
773.556675	60257.984787	32.959668
774.373809	60338.211876	32.964685
774.888286	60412.467481	32.969703
776.204558	60485.132253	32.974720
776.521019	60560.389381	32.979738
777.404509	60639.032413	32.984756
777.712837	60715.890661	32.989773
778.086156	60808.097681	32.994791
778.876528	60890.170873	32.999808
779.432064	60986.923783	33.004826
780.087751	61076.492077	33.009844
780.779846	61172.533490	33.014861
781.217370	61276.330542	33.019879
781.986636	61366.715011	33.024896
782.936774	61468.332977	33.029914
783.329291	61572.935679	33.034932
784.312632	61673.246827	33.039949
784.729368	61783.263626	33.044967
785.481391	61894.519421	33.049984
785.908878	62011.785969	33.055002
786.585826	62109.528414	33.060020
787.482059	62213.460203	33.065037
788.180973	62313.791566	33.070055
789.303715	62414.581814	33.075072
790.082177	62511.107715	33.080090
790.698323	62615.032598	33.085108
791.542815	62721.991098	33.090125
792.359189	62824.011592	33.095143
793.259074	62920.859958	33.100160
793.958746	63030.651587	33.105178
794.683134	63129.737191	33.110196
795.387964	63239.408928	33.115213
796.216376	63348.516416	33.120231
797.103151	63457.740913	33.125248
797.838152	63575.191188	33.130266
798.138860	63683.676463	33.135284
798.999388	63791.219304	33.140301
799.771519	63903.019748	33.145319
800.945888	64019.859919	33.150336
801.750751	64145.323808	33.155354
802.051997	64262.934420	33.160372
802.923533	64372.406538	33.165389
803.883557	64503.276521	33.170407
804.926126	64610.438362	33.175424
805.580456	64743.385237	33.180442
806.315636	64858.067305	33.185460
807.584082	64969.339565	33.190477
807.941893	65095.094330	33.195495
809.028731	65209.357723	33.200512
809.780348	65336.468967	33.205530
810.697730	65456.762499	33.210548
811.469034	65575.033320	33.215565
812.033350	65702.867980	33.220583
813.143000	65814.955873	33.225600
813.802031	65935.713659	33.230618
814.625372	66061.950821	33.235636
815.899043	66175.820750	33.240653
816.427214	66300.162571	33.245671
817.314805	66416.180018	33.250688
818.350333	66547.441756	33.255706
819.093969	66661.740174	33.260724
820.310928	66770.963260	33.265741
820.886953	66901.926533	33.270759
821.657764	67009.336779	33.275776
822.829588	67129.811213	33.280794
823.600068	67246.226295	33.285812
824.395772	67335.797388	33.290829
825.624350	67440.450542	33.295847
827.348400	67530.527355	33.300864
828.454097	67633.242418	33.305882
829.075977	67725.683900	33.310900
829.960334	67810.044368	33.315917
830.776375	67915.130918	33.320935
831.802064	67990.501921	33.325952
832.600180	68094.738820	33.330970
833.298121	68169.806176	33.335988
834.092184	68250.250913	33.341005
834.773847	68330.936511	33.346023
835.562898	68409.858841	33.351040
836.005757	68500.070656	33.356058
836.322129	68597.607778	33.361076
837.496025	68684.046693	33.366093
837.964467	68779.863982	33.371111
838.884191	68881.820169	33.376128
839.671689	68974.017363	33.381146
839.987544	69087.244872	33.386164
841.308523	69188.849246	33.391181
841.728064	69298.082721	33.396199
842.249836	69409.847575	33.401216
842.689679	69533.167332	33.406234
843.625289	69659.621538	33.411252
844.762077	69762.493246	33.416269
846.387635	69864.870706	33.421287
847.910999	69960.999492	33.426304
848.999257	70049.361961	33.431322
849.842556	70152.064468	33.436340
850.833707	70243.599854	33.441357
851.541216	70341.134793	33.446375
852.679788	70427.776475	33.451392
853.125218	70522.340706	33.456410
853.656166	70624.909239	33.461428
854.391185	70727.708906	33.466445
854.684403	70844.218901	33.471463
855.273793	70955.626029	33.476480
855.822168	71073.124342	33.481498
856.001689	71204.630735	33.486516
856.663415	71329.288685	33.491533
857.343386	71480.283736	33.496551
858.077909	71618.299847	33.501568
858.785539	71770.000461	33.506586
859.274726	71916.977460	33.511604
860.392574	72061.216920	33.516621
860.842785	72219.529244	33.521639
861.280268	72383.195229	33.526656
862.249207	72542.458229	33.531674
862.909875	72709.288533	33.536692
863.687524	72881.311392	33.541709
864.318823	73052.449938	33.546727
865.655990	73212.818440	33.551744
866.985489	73371.367952	33.556762
868.514765	73523.724227	33.561780
870.058138	73664.353246	33.566797
870.782601	73806.660309	33.571815
872.356545	73946.975988	33.576832
873.697558	74063.823307	33.581850
874.591443	74181.076708	33.586868
875.791586	74305.880726	33.591885
876.893689	74421.626059	33.596903
877.955571	74527.524703	33.601920
878.748311	74640.927031	33.606938
879.440262	74751.026597	33.611956
880.514170	74859.714075	33.616973
881.158794	74954.073543	33.621991
881.943088	75060.275271	33.627008
882.934213	75164.987319	33.632026
883.220792	75283.008363	33.637044
884.187639	75393.601670	33.642061
884.968253	75511.330588	33.647079
885.778112	75636.177301	33.652096
886.807351	75753.662513	33.657114
887.032289	75874.423422	33.662132
888.088170	75986.478213	33.667149
888.931669	76123.017382	33.672167
889.813701	76248.437091	33.677184
890.781220	76370.091891	33.682202
891.561410	76496.207248	33.687220
892.441795	76622.704662	33.692237
893.583597	76754.098254	33.697255
894.437684	76889.381503	33.702272
895.078942	77017.288414	33.707290
895.644007	77151.389246	33.712308
896.827873	77277.560049	33.717325
897.557659	77411.368542	33.722343
898.494440	77548.273626	33.727360
899.980099	77674.920010	33.732378
900.947144	77802.680704	33.737396
902.043667	77920.431429	33.742413
902.865558	78054.265918	33.747431
903.963443	78176.382607	33.752448
904.881866	78308.962193	33.757466
905.432992	78437.006457	33.762484
906.397540	78564.278455	33.767501
907.593822	78693.554803	33.772519
908.386052	78820.149228	33.777536
909.090784	78961.885141	33.782554
909.419262	79096.620029	33.787572
910.467534	79239.987933	33.792589
911.133679	79393.664393	33.797607
912.035771	79531.030237	33.802624
912.798264	79667.630023	33.807642
913.560886	79823.266673	33.812660
914.425430	79962.431909	33.817677
915.815769	80119.342238	33.822695
916.635365	80259.016768	33.827712
917.543037	80400.157477	33.832730
918.585440	80558.756324	33.837748
919.303144	80691.972522	33.842765
920.333122	80850.189587	33.847783
921.375028	81001.560204	33.852800
922.012846	81135.988404	33.857818
922.876312	81293.686610	33.862836
923.858123	81445.450045	33.867853
925.221829	81588.690060	33.872871
925.752314	81744.607254	33.877888
926.281846	81893.319268	33.882906
927.091940	82033.702164	33.887924
927.995904	82177.676241	33.892941
928.924640	82331.555159	33.897959
929.694101	82481.931847	33.902976
930.804568	82622.140329	33.907994
931.744698	82779.614089	33.913012
932.787333	82923.436179	33.918029
934.235694	83067.847715	33.923047
934.519193	83219.717051	33.928064
935.977253	83352.182733	33.933082
936.942758	83496.578380	33.938100
938.210660	83634.209740	33.943117
939.238196	83778.223189	33.948135
940.379438	83910.531165	33.953152
941.784266	84036.562133	33.958170
942.878546	84163.134183	33.963188
944.346215	84285.808453	33.968205
945.616334	84398.538522	33.973223
946.605396	84522.719708	33.978240
947.957484	84629.229415	33.983258
948.584201	84737.869708	33.988276
949.564018	84851.569187	33.993293
950.503058	84961.998409	33.998311
951.197497	85080.386128	34.003328
952.396957	85193.049852	34.008346
953.035920	85321.787981	34.013364
954.103709	85443.587596	34.018381
955.110748	85565.296997	34.023399
955.458099	85687.803412	34.028416
956.279792	85814.064008	34.033434
957.149432	85939.962697	34.038452
957.966834	86077.546304	34.043469
959.249997	86199.692621	34.048487
959.922830	86345.111429	34.053504
960.600775	86468.204411	34.058522
961.029618	86624.000633	34.063540
962.073054	86767.080401	34.068557
962.945620	86928.504400	34.073575
963.579477	87085.084884	34.078592
964.361316	87235.420250	34.083610
964.764033	87396.041896	34.088628
965.315106	87571.966780	34.093645
966.068295	87741.846252	34.098663
966.480027	87924.879206	34.103680
967.888008	88100.192921	34.108698
968.366622	88293.127846	34.113716
969.296827	88482.999836	34.118733
970.636695	88674.847366	34.123751
971.354988	88861.100600	34.128768
972.551676	89042.805176	34.133786
973.838132	89232.761309	34.138804
975.498979	89409.724760	34.143821
976.589933	89576.173354	34.148839
977.373915	89751.903410	34.153856
979.101882	89914.182001	34.158874
980.260233	90075.046556	34.163892
980.873123	90231.942251	34.168909
982.000597	90390.966068	34.173927
982.897452	90541.422628	34.178944
984.228754	90696.027366	34.183962
984.672939	90856.348476	34.188980
985.745158	91016.265617	34.193997
986.808260	91164.121498	34.199015
987.425241	91327.846658	34.204032
988.358774	91490.746509	34.209050
988.996225	91657.850324	34.214068
989.700107	91832.184951	34.219085
991.041873	92001.645374	34.224103
992.057506	92176.840533	34.229120
992.933472	92351.029111	34.234138
994.494397	92514.923372	34.239156
995.372405	92692.291556	34.244173
996.511063	92854.899476	34.249191
997.360040	93028.502456	34.254208
998.608903	93189.669484	34.259226
1000.476252	93345.041008	34.264244
1001.763388	93491.138109	34.269261
1003.209419	93633.195612	34.274279
1004.462589	93788.390235	34.279296
1005.685333	93932.228461	34.284314
1006.597991	94080.045316	34.289332
1007.527100	94233.804293	34.294349
1008.564003	94368.529723	34.299367
1009.087609	94517.415970	34.304384
1009.836953	94670.796956	34.309402
1010.830895	94821.503575	34.314420
1011.717393	94973.495579	34.319437
1012.556405	95134.200978	34.324455
1013.197603	95303.253189	34.329472
1013.993654	95463.974389	34.334490
1014.904731	95630.779577	34.339508
1016.165339	95797.380420	34.344525
1017.399698	95960.802551	34.349543
1018.134102	96140.574870	34.354560
1019.093488	96308.053660	34.359578
1020.411468	96464.336343	34.364596
1020.958004	96640.276293	34.369613
1022.244166	96811.285706	34.374631
1023.188235	96992.794498	34.379648
1024.222041	97157.955399	34.384666
1025.334726	97338.209590	34.389684
1026.504789	97517.397956	34.394701
1028.376221	97675.359705	34.399719
1028.794549	97840.858350	34.404736
1030.008049	98002.214298	34.409754
1031.149130	98162.279443	34.414772
1031.903130	98334.276594	34.419789
1032.966350	98487.513050	34.424807
1034.203829	98658.125354	34.429824
1035.591938	98803.438257	34.434842
1036.691833	98947.003221	34.439860
1038.305312	99086.314979	34.444877
1040.117255	99216.856113	34.449895
1040.810098	99350.666627	34.454912
1041.554894	99465.575709	34.459930
1042.627949	99600.886306	34.464948
1043.248344	99743.144882	34.469965
1044.212700	99884.344953	34.474983
1044.649303	100031.613235	34.480000
1045.714986	100188.791371	34.485018
1046.880642	100327.439386	34.490036
1047.510600	100492.279374	34.495053
1048.464862	100642.001531	34.500071
1049.174191	100801.245247	34.505088
1050.307134	100976.671338	34.510106
1051.412232	101133.766140	34.515124
1051.932097	101304.126235	34.520141
1053.262544	101481.890067	34.525159
1054.308723	101655.005408	34.530176
1055.300617	101825.471715	34.535194
1056.681046	101997.708926	34.540212
1057.051191	102175.654567	34.545229
1058.560221	102354.242269	34.550247
1059.493683	102539.198670	34.555264
1060.303826	102713.843173	34.560282
1061.828242	102887.290041	34.565300
1062.466805	103070.869565	34.570317
1063.668963	103257.608737	34.575335
1064.726974	103443.702670	34.580352
1065.621224	103617.971479	34.585370
1066.596892	103811.858433	34.590388
1067.191578	104014.563704	34.595405
1068.422175	104201.013367	34.600423
1069.476269	104407.771873	34.605440
1070.585708	104605.340019	34.610458
1071.570825	104800.359801	34.615476
1072.576181	104999.848533	34.620493
1073.714948	105189.183287	34.625511
1074.697593	105387.741535	34.630528
1075.816084	105597.398720	34.635546
1077.196011	105802.845646	34.640564
1077.440752	106014.441604	34.645581
1079.224295	106203.799793	34.650599
1080.416880	106410.068745	34.655616
1081.501827	106615.445721	34.660634
1082.888920	106815.731242	34.665652
1083.246570	107013.053176	34.670669
1084.604213	107217.488707	34.675687
1085.618023	107428.609401	34.680704
1086.954021	107636.763182	34.685722
1088.355775	107837.611093	34.690740
1089.056577	108040.721241	34.695757
1090.546703	108243.077068	34.700775
1092.289516	108435.117951	34.705792
1092.985116	108624.248638	34.710810
1094.620190	108804.415889	34.715828
1095.694035	108978.498650	34.720845
1096.765845	109149.821321	34.725863
1098.101002	109325.077636	34.730880
1099.067673	109498.852686	34.735898
1100.155770	109668.313636	34.740916
1100.929095	109855.792675	34.745933
1102.591835	110015.428388	34.750951
1103.636776	110180.858776	34.755968
1104.905378	110360.883613	34.760986
1105.763669	110526.981437	34.766004
1106.536587	110701.569992	34.771021
1107.994656	110881.299737	34.776039
1108.772905	111060.500943	34.781056
1109.797866	111241.675368	34.786074
1110.964472	111428.578299	34.791092
1111.994303	111609.855633	34.796109
1113.551939	111784.709364	34.801127
1114.484564	111970.363760	34.806144
1115.263909	112164.964607	34.811162
1116.078267	112342.457540	34.816180
1117.419255	112537.699623	34.821197
1118.211116	112729.324984	34.826215
1119.516256	112929.339566	34.831232
1120.568866	113121.999850	34.836250
1121.822988	113311.674952	34.841268
1122.803092	113505.528532	34.846285
1123.953311	113695.920828	34.851303
1125.657933	113894.518194	34.856320
1126.293095	114098.874790	34.861338
1127.404613	114296.689620	34.866356
1128.535400	114504.549876	34.871373
1129.415590	114712.365861	34.876391
1130.317589	114922.523617	34.881408
1131.523729	115122.697311	34.886426
1132.494468	115326.992579	34.891444
1133.718325	115548.161102	34.896461
1134.775425	115759.527483	34.901479
1135.659263	115976.639567	34.906496
1136.683451	116203.802546	34.911514
1137.698400	116431.336350	34.916532
1138.669666	116653.671642	34.921549
1139.397190	116881.194836	34.926567
1140.787972	117113.472005	34.931584
1141.575037	117348.832145	34.936602
1143.029665	117578.909968	34.941620
1144.610100	117817.432636	34.946637
1146.153241	118035.068160	34.951655
1147.393097	118258.890329	34.956672
1148.466658	118481.336110	34.961690
1150.082044	118696.835326	34.966708
1151.402855	118919.356144	34.971725
1152.470562	119139.805739	34.976743
1153.466762	119358.457104	34.981760
1154.321922	119579.009729	34.986778
1155.338944	119783.784549	34.991796
1156.118602	119997.522819	34.996813
1157.194996	120217.383355	35.001831
1157.956858	120433.472230	35.006848
1158.758674	120661.480866	35.011866
1159.594063	120885.645633	35.016884
1160.969819	121124.382143	35.021901
1161.926958	121358.503205	35.026919
1162.793832	121602.070352	35.031936
1164.098945	121846.071380	35.036954
1165.172276	122092.813486	35.041972
1166.499657	122342.745848	35.046989
1167.707853	122592.827418	35.052007
1169.112694	122834.956363	35.057024
1170.225544	123081.497000	35.062042
1171.579122	123327.276018	35.067060
1172.671801	123574.077581	35.072077
1174.202609	123814.950726	35.077095
1175.414258	124046.742350	35.082112
1176.651330	124295.717656	35.087130
1178.419719	124525.655878	35.092148
1179.944914	124765.333405	35.097165
1181.009253	125003.177840	35.102183
1182.705953	125221.447616	35.107200
1183.737072	125458.540774	35.112218
1185.119481	125683.699303	35.117236
1185.771403	125915.423378	35.122253
1186.704342	126157.507261	35.127271
1188.191290	126390.029881	35.132288
1189.081760	126628.677071	35.137306
1190.218780	126864.039002	35.142324
1191.295756	127112.950311	35.147341
1192.540901	127352.074675	35.152359
1193.985908	127585.640088	35.157376
1195.059536	127835.014022	35.162394
1196.754869	128073.420349	35.167412
1198.511667	128304.034965	35.172429
1200.169240	128535.428810	35.177447
1201.755908	128751.815350	35.182464
1202.692013	128978.113400	35.187482
1203.960191	129192.440549	35.192500
1205.062465	129413.617406	35.197517
1206.156625	129639.715634	35.202535
1207.654745	129854.489577	35.207552
1208.679729	130080.856298	35.212570
1209.985828	130292.864529	35.217588
1211.055464	130509.389534	35.222605
1211.746350	130734.525027	35.227623
1213.135443	130959.998940	35.232640
1214.107328	131200.023012	35.237658
1215.441379	131431.315717	35.242676
1216.727348	131666.294696	35.247693
1217.052118	131900.577861	35.252711
1218.268144	132141.467195	35.257728
1219.411266	132389.051828	35.262746
1220.858816	132606.172705	35.267764
1222.281459	132819.153694	35.272781
1222.996934	133042.120407	35.277799
1224.733164	133281.420439	35.282816
1225.791582	133505.802221	35.287834
1226.796696	133721.624323	35.292852
1228.041204	133962.991251	35.297869
1229.069475	134201.544363	35.302887
1230.249449	134426.659604	35.307904
1231.222190	134682.189217	35.312922
1232.384230	134917.085877	35.317940
1233.828569	135149.704445	35.322957
1235.068215	135397.409222	35.327975
1236.819890	135628.697972	35.332992
1238.022390	135873.242944	35.338010
1240.006090	136097.724719	35.343028
1241.272684	136326.273915	35.348045
1242.351395	136559.193067	35.353063
1243.734949	136785.962962	35.358080
1244.907745	137019.972271	35.363098
1246.172200	137247.894098	35.368116
1247.407312	137480.716737	35.373133
1248.684835	137718.897143	35.378151
1250.125627	137955.529711	35.383168
1251.376420	138194.909895	35.388186
1252.256555	138434.355199	35.393204
1253.377244	138667.142106	35.398221
1254.655792	138917.579423	35.403239
1255.844133	139157.154520	35.408256
1257.296308	139397.041161	35.413274
1258.712839	139636.605880	35.418292
1259.771988	139878.655369	35.423309
1260.910349	140128.833800	35.428327
1262.051984	140375.348806	35.433344
1263.027941	140624.747043	35.438362
1264.422782	140875.102490	35.443380
1266.331714	141116.178176	35.448397
1267.439721	141361.044698	35.453415
1269.144359	141593.294717	35.458432
1270.531417	141829.037181	35.463450
1271.978341	142071.885068	35.468468
1273.202808	142308.089713	35.473485
1274.683459	142536.973030	35.478503
1276.333346	142757.078723	35.483520
1277.571974	143001.591833	35.488538
1278.990530	143231.162355	35.493556
1280.278314	143456.153316	35.498573
1281.315655	143694.478954	35.503591
1282.816171	143920.045130	35.508608
1283.867693	144152.892858	35.513626
1285.018586	144378.838797	35.518644
1286.198737	144619.568353	35.523661
1286.790895	144858.789528	35.528679
1288.129926	145102.678298	35.533696
1288.576667	145357.323801	35.538714
1289.871700	145594.590573	35.543732
1291.444600	145837.011117	35.548749
1291.946286	146085.273023	35.553767
1293.057797	146335.740457	35.558784
1294.042660	146601.691469	35.563802
1295.130946	146859.750689	35.568820
1296.760442	147123.071242	35.573837
1297.653746	147390.070906	35.578855
1299.338270	147650.202359	35.583872
1300.333530	147923.758221	35.588890
1301.387610	148199.030937	35.593908
1303.077198	148461.272592	35.598925
1303.812683	148750.872632	35.603943
1305.439512	149024.087434	35.608960
1306.350450	149313.928123	35.613978
1307.395930	149601.820078	35.618996
1308.600494	149899.491569	35.624013
1309.841771	150204.756764	35.629031
1311.311791	150495.056174	35.634048
1312.485766	150783.873684	35.639066
1314.209426	151090.344474	35.644084
1315.878784	151378.891404	35.649101
1317.527977	151663.968422	35.654119
1319.621205	151943.377684	35.659136
1321.176938	152216.323037	35.664154
1323.708823	152476.431258	35.669172
1325.783776	152718.924221	35.674189
1326.907929	152981.813708	35.679207
1328.675605	153214.861414	35.684224
1330.312885	153458.930692	35.689242
1331.762709	153700.712206	35.694260
1333.379256	153933.193840	35.699277
1334.386846	154171.502094	35.704295
1336.093449	154398.262708	35.709312
1337.892316	154621.406188	35.714330
1338.960748	154839.627145	35.719348
1340.447149	155060.898387	35.724365
1341.507517	155295.703147	35.729383
1342.575224	155527.514217	35.734400
1344.255717	155743.935473	35.739418
1345.342956	155991.488832	35.744436
1346.376684	156213.617737	35.749453
1347.799069	156452.794647	35.754471
1348.616743	156688.866910	35.759488
1349.980469	156929.477501	35.764506
1350.845987	157179.270750	35.769524
1352.056561	157428.968411	35.774541
1352.920691	157691.730352	35.779559
1354.366728	157943.128868	35.784576
1355.481067	158210.151983	35.789594
1356.653831	158476.469065	35.794612
1357.779714	158739.446616	35.799629
1359.069324	159016.251699	35.804647
1359.842260	159295.874714	35.809664
1361.312855	159563.111983	35.814682
1362.514066	159841.193669	35.819700
1363.568107	160112.032708	35.824717
1364.856980	160390.521698	35.829735
1366.082889	160657.820495	35.834752
1367.730976	160922.067211	35.839770
1368.835020	161206.543543	35.844788
1370.125142	161490.444367	35.849805
1371.176406	161784.461868	35.854823
1372.482540	162072.093951	35.859840
1373.614954	162370.846756	35.864858
1374.710456	162680.912783	35.869876
1375.884198	162974.080053	35.874893
1377.167274	163297.440681	35.879911
1378.301106	163611.541579	35.884928
1379.627627	163923.746596	35.889946
1380.866268	164253.707068	35.894964
1382.950996	164556.892351	35.899981
1384.175829	164876.163570	35.904999
1385.850954	165196.984158	35.910016
1387.519937	165520.713810	35.915034
1388.936482	165833.728983	35.920052
1390.699678	166151.762542	35.925069
1391.969351	166468.284017	35.930087
1393.563215	166773.281390	35.935104
1395.599190	167072.507767	35.940122
1396.964952	167391.036819	35.945140
1398.377275	167694.523381	35.950157
1400.117202	168005.201496	35.955175
1401.398346	168311.988450	35.960192
1403.118010	168617.585725	35.965210
1404.252820	168920.011206	35.970228
1405.801301	169228.890350	35.975245
1407.332363	169537.228870	35.980263
1408.361165	169844.069156	35.985280
1409.834657	170147.142584	35.990298
1410.911627	170464.727042	35.995316
1412.604069	170785.748838	36.000333
1413.675042	171099.836128	36.005351
1414.573676	171421.797563	36.010368
1415.762967	171743.241884	36.015386
1417.629383	172075.359341	36.020404
1419.807616	172392.336715	36.025421
1420.714574	172711.957641	36.030439
1422.107382	173041.523162	36.035456
1423.910933	173347.263520	36.040474
1424.962552	173689.366832	36.045492
1426.662456	174009.469729	36.050509
1427.971242	174323.016937	36.055527
1429.324216	174654.059590	36.060544
1431.208570	174980.406619	36.065562
1432.553054	175301.416320	36.070580
1433.865000	175625.251130	36.075597
1435.560567	175945.214953	36.080615
1436.637925	176260.641517	36.085632
1438.760506	176575.853099	36.090650
1440.249229	176872.454922	36.095668
1441.884786	177156.506611	36.100685
1444.044362	177440.736729	36.105703
1445.018882	177736.175074	36.110720
1446.731269	178016.347357	36.115738
1448.330253	178298.571288	36.120756
1449.745613	178576.106728	36.125773
1451.163471	178865.028072	36.130791
1452.463995	179159.695282	36.135808
1453.897588	179432.053725	36.140826
1455.223027	179733.662570	36.145844
1456.642857	180022.374171	36.150861
1457.738235	180315.737551	36.155879
1458.870469	180623.768843	36.160896
1460.294438	180918.082015	36.165914
1462.030427	181228.767769	36.170932
1463.532250	181527.919571	36.175949
1465.239408	181828.446796	36.180967
1466.376524	182137.577491	36.185984
1467.783516	182439.682608	36.191002
1468.939473	182759.006066	36.196020
1470.095634	183085.794909	36.201037
1471.451838	183406.344469	36.206055
1472.666421	183745.338078	36.211072
1474.263634	184082.745066	36.216090
1475.517541	184435.394196	36.221108
1477.019499	184776.045786	36.226125
1477.869943	185107.582673	36.231143
1478.589572	185525.384751	36.236160
1480.284884	185869.830608	36.241178
1481.701797	186237.962113	36.246196
1482.839076	186607.159332	36.251213
1484.596283	186964.752042	36.256231
1485.593432	187343.422253	36.261248
1487.281087	187712.062598	36.266266
1488.863584	188086.461045	36.271284
1490.099896	188466.265409	36.276301
1491.811050	188849.113760	36.281319
1493.425528	189234.393054	36.286336
1495.037579	189602.715278	36.291354
1496.755350	189980.656886	36.296372
1498.343840	190364.475230	36.301389
1500.481251	190723.371005	36.306407
1502.412404	191093.704167	36.311424
1504.443170	191454.323551	36.316442
1505.599173	191818.370029	36.321460
1507.234626	192175.049590	36.326477
1508.902296	192530.468835	36.331495
1510.208066	192889.709792	36.336512
1512.148751	193253.401745	36.341530
1513.196372	193610.812021	36.346548
1515.129132	193963.375497	36.351565
1516.811733	194313.000251	36.356583
1518.637969	194665.001768	36.361600
1520.454726	194994.129227	36.366618
1521.728514	195334.929735	36.371636
1523.385449	195655.289704	36.376653
1524.626972	195975.417597	36.381671
1525.919113	196312.677826	36.386688
1527.369267	196637.648403	36.391706
1528.528586	196975.988437	36.396724
1529.676402	197316.173053	36.401741
1531.703039	197653.987152	36.406759
1532.918460	197992.830455	36.411776
1534.511805	198341.018689	36.416794
1536.152302	198690.013161	36.421812
1537.793905	199025.538296	36.426829
1539.388820	199372.157030	36.431847
1540.713540	199723.445228	36.436864
1542.417891	200059.485074	36.441882
1543.661968	200408.784372	36.446900
1545.558977	200764.474351	36.451917
1547.622271	201101.016280	36.456935
1548.923055	201464.683693	36.461952
1550.380484	201810.245721	36.466970
1551.736318	202163.698856	36.471988
1552.677321	202513.948817	36.477005
1554.315633	202867.102999	36.482023
1555.969554	203249.281808	36.487040
1557.209798	203605.465975	36.492058
1559.193236	203973.091830	36.497076
1560.537306	204336.702211	36.502093
1562.771195	204694.537104	36.507111
1563.793024	205071.258951	36.512128
1565.915300	205434.868256	36.517146
1567.416437	205792.046273	36.522164
1569.209858	206155.511980	36.527181
1571.065119	206521.584468	36.532199
1572.218200	206897.467119	36.537216
1573.501030	207262.840932	36.542234
1575.335750	207630.420245	36.547252
1576.868452	208008.427044	36.552269
1578.325205	208379.337697	36.557287
1579.743611	208760.770496	36.562304
1581.188521	209141.387798	36.567322
1582.667253	209529.670672	36.572340
1583.926223	209903.796336	36.577357
1585.841914	210290.915818	36.582375
1587.061226	210688.390983	36.587392
1588.763729	211082.839245	36.592410
1590.729935	211461.523514	36.597428
1592.127283	211860.903603	36.602445
1594.009037	212237.040487	36.607463
1595.741000	212637.306419	36.612480
1597.623205	213014.563886	36.617498
1599.355026	213397.131259	36.622516
1600.863585	213781.617801	36.627533
1602.783834	214147.419070	36.632551
1604.280897	214533.028108	36.637568
1605.994618	214904.607467	36.642586
1607.288325	215259.548338	36.647604
1608.770561	215623.144325	36.652621
1610.270691	215980.211298	36.657639
1611.643207	216348.730528	36.662656
1613.270327	216711.797730	36.667674
1614.685858	217078.255004	36.672692
1616.030391	217460.879104	36.677709
1617.572403	217834.149590	36.682727
1618.779197	218226.603881	36.687744
1620.559427	218607.684514	36.692762
1622.822423	218984.645510	36.697780
1624.604205	219358.743893	36.702797
1626.940550	219716.823560	36.707815
1628.474151	220091.373297	36.712832
1630.257797	220453.461364	36.717850
1632.033556	220832.442398	36.722868
1633.090036	221211.344569	36.727885
1634.935224	221575.076645	36.732903
1636.671518	221963.465932	36.737920
1637.951629	222343.781317	36.742938
1639.649988	222730.376263	36.747956
1640.709302	223120.612347	36.752973
1642.067446	223514.760924	36.757991
1643.404499	223923.443083	36.763008
1644.770370	224329.327668	36.768026
1646.343779	224745.820658	36.773044
1647.866981	225171.366033	36.778061
1649.489730	225590.621942	36.783079
1650.772404	226016.160440	36.788096
1652.578036	226437.851587	36.793114
1654.220389	226872.119797	36.798132
1655.749936	227305.037066	36.803149
1657.313775	227739.448458	36.808167
1659.018680	228176.478731	36.813184
1661.237186	228609.205955	36.818202
1662.927810	229034.887165	36.823220
1664.602262	229466.592385	36.828237
1666.862169	229894.515556	36.833255
1668.876104	230319.484700	36.838272
1670.641584	230748.866513	36.843290
1672.569218	231166.410227	36.848308
1674.174649	231587.744141	36.853325
1676.266581	232007.751261	36.858343
1677.541804	232426.527507	36.863360
1679.245081	232853.893453	36.868378
1681.187034	233275.097884	36.873396
1682.468507	233703.960594	36.878413
1684.498326	234111.003353	36.883431
1685.981961	234534.549948	36.888448
1687.343276	234968.253736	36.893466
1689.271778	235390.100477	36.898484
1690.682141	235824.661507	36.903501
1692.282815	236250.224086	36.908519
1694.243360	236689.316052	36.913536
1695.795728	237100.231784	36.918554
1697.286513	237512.987816	36.923572
1698.676893	237943.924330	36.928589
1700.320409	238357.392528	36.933607
1702.031344	238773.695013	36.938624
1703.454215	239198.100056	36.943642
1705.589754	239609.860634	36.948660
1707.471906	240035.890580	36.953677
1708.583833	240456.489922	36.958695
1710.200249	240891.889483	36.963712
1711.647656	241323.762356	36.968730
1713.552117	241753.982794	36.973748
1714.942901	242192.979462	36.978765
1717.068664	242626.719768	36.983783
1718.667405	243063.421384	36.988800
1720.232355	243510.442904	36.993818
1722.085217	243949.159950	36.998836
1723.671298	244414.545299	37.003853
1724.882661	244871.510890	37.008871
1726.279279	245340.384716	37.013888
1727.958812	245803.342711	37.018906
1729.967064	246268.734533	37.023924
1731.466951	246750.928985	37.028941
1733.215167	247221.192965	37.033959
1735.248680	247695.244508	37.038976
1736.507366	248176.618147	37.043994
1738.068120	248668.940102	37.049012
1739.901103	249156.719640	37.054029
1741.991153	249656.699919	37.059047
1743.313714	250148.809967	37.064064
1744.752721	250639.325502	37.069082
1746.725581	251139.784306	37.074100
1748.184699	251653.744195	37.079117
1750.354775	252154.398572	37.084135
1752.210241	252659.552610	37.089152
1753.956648	253169.729991	37.094170
1755.699664	253673.836829	37.099188
1757.602314	254185.131064	37.104205
1759.461330	254683.147066	37.109223
1761.362038	255195.966134	37.114240
1763.000113	255701.133066	37.119258
1765.715291	256195.040023	37.124276
1767.087423	256708.737235	37.129293
1769.018261	257201.381239	37.134311
1770.974132	257698.110857	37.139328
1772.691560	258197.573954	37.144346
1774.825000	258685.686788	37.149364
1776.737349	259190.552636	37.154381
1778.685121	259677.452231	37.159399
1780.842649	260160.683128	37.164416
1783.292676	260642.746065	37.169434
1785.459251	261109.920223	37.174452
1787.104495	261590.392964	37.179469
1789.225945	262059.632009	37.184487
1791.116679	262516.538928	37.189504
1793.114774	262984.121895	37.194522
1794.491537	263412.004202	37.199540
1795.982558	263856.785108	37.204557
1797.534621	264298.100420	37.209575
1799.782487	264744.605589	37.214592
1801.358526	265185.408008	37.219610
1803.589879	265609.433590	37.224628
1805.004429	266061.516342	37.229645
1806.191385	266507.896506	37.234663
1807.881739	266954.723553	37.239680
1809.208152	267433.873994	37.244698
1811.197665	267885.983418	37.249716
1812.477615	268351.194494	37.254733
1814.396265	268829.835384	37.259751
1816.339729	269296.963924	37.264768
1817.932299	269783.457865	37.269786
1819.888118	270255.993676	37.274804
1821.742883	270739.799396	37.279821
1823.329143	271222.659550	37.284839
1825.270130	271699.234592	37.289856
1826.959266	272199.781022	37.294874
1828.613400	272687.021627	37.299892
1830.692297	273178.049820	37.304909
1832.657907	273662.822053	37.309927
1834.766346	274162.505429	37.314944
1836.308845	274659.312492	37.319962
1838.435791	275147.559590	37.324980
1840.289500	275635.953967	37.329997
1842.409486	276127.527764	37.335015
1844.521115	276619.482882	37.340032
1846.247153	277117.573845	37.345050
1847.697272	277626.328754	37.350068
1849.339017	278128.826131	37.355085
1851.290173	278625.655488	37.360103
1852.922342	279130.946043	37.365120
1854.623686	279644.097870	37.370138
1856.700824	280157.133150	37.375156
1858.936748	280674.966045	37.380173
1860.423373	281187.540450	37.385191
1862.423697	281689.560094	37.390208
1864.170497	282206.862299	37.395226
1866.401678	282727.534549	37.400244
1868.292406	283241.405032	37.405261
1869.982416	283750.735968	37.410279
1872.084162	284264.058915	37.415296
1873.933381	284794.340210	37.420314
1875.907372	285300.696190	37.425332
1877.786278	285831.273423	37.430349
1879.527012	286344.676150	37.435367
1881.546767	286855.870218	37.440384
1883.130550	287382.758129	37.445402
1884.720534	287910.658915	37.450420
1886.389853	288452.006071	37.455437
1888.142369	288984.167332	37.460455
1890.086654	289510.019794	37.465472
1892.308857	290046.998419	37.470490
1894.285368	290549.346163	37.475508
1895.674623	291062.764883	37.480525
1896.996677	291588.029040	37.485543
1898.915622	292108.743879	37.490560
1900.762808	292626.014356	37.495578
1902.954855	293145.915815	37.500596
1904.860993	293666.574945	37.505613
1906.563926	294203.216881	37.510631
1908.917759	294720.619602	37.515648
1910.340413	295262.764974	37.520666
1912.081942	295801.221061	37.525684
1914.109282	296327.408888	37.530701
1915.378156	296888.925713	37.535719
1917.591097	297439.204419	37.540736
1919.382001	297997.806630	37.545754
1920.887269	298556.454552	37.550772
1922.618879	299127.530829	37.555789
1924.262799	299702.428354	37.560807
1926.101190	300270.939816	37.565824
1927.943429	300872.641317	37.570842
1929.442573	301456.289517	37.575860
1931.620073	302047.564025	37.580877
1933.310633	302646.714731	37.585895
1935.685132	303251.357073	37.590912
1937.296621	303858.843165	37.595930
1939.377990	304457.889311	37.600948
1941.838929	305064.205801	37.605965
1943.818627	305675.450853	37.610983
1946.138002	306272.538779	37.616000
1947.834734	306876.864995	37.621018
1949.896566	307481.454436	37.626036
1952.305992	308084.024482	37.631053
1954.280458	308688.924502	37.636071
1956.276250	309296.838197	37.641088
1958.058113	309900.847591	37.646106
1959.635163	310516.035355	37.651124
1961.740633	311133.540213	37.656141
1963.705865	311757.209296	37.661159
1965.844319	312370.482925	37.666176
1967.371629	312988.122052	37.671194
1969.919126	313604.845063	37.676212
1972.328704	314218.259894	37.681229
1974.182529	314827.777816	37.686247
1976.294972	315445.397243	37.691264
1978.701198	316060.193192	37.696282
1980.664809	316661.144488	37.701300
1982.752365	317271.946734	37.706317
1984.521090	317895.417625	37.711335
1986.848809	318491.872228	37.716352
1988.817990	319108.162496	37.721370
1990.979116	319703.796711	37.726388
1993.179002	320306.858311	37.731405
1995.001866	320911.959188	37.736423
1997.434831	321510.348530	37.741440
1999.393211	322099.850697	37.746458
2001.542223	322680.504468	37.751476
2003.708055	323257.062216	37.756493
2005.072326	323823.697479	37.761511
2007.177601	324398.604527	37.766528
2008.958057	324961.298865	37.771546
2010.615947	325539.648228	37.776564
2012.802272	326121.481347	37.781581
2014.210736	326709.890304	37.786599
2016.204469	327292.074793	37.791616
2017.996373	327890.739067	37.796634
2019.891470	328488.947873	37.801652
2021.811249	329102.886111	37.806669
2023.378270	329720.508300	37.811687
2025.859028	330324.436457	37.816704
2027.516877	330953.529513	37.821722
2028.963346	331583.971594	37.826740
2031.279657	332200.549449	37.831757
2033.165744	332842.198343	37.836775
2034.819424	333479.614639	37.841792
2036.686709	334126.759871	37.846810
2038.703938	334782.070673	37.851828
2040.923361	335428.073530	37.856845
2043.070704	336093.423054	37.861863
2045.056454	336750.389718	37.866880
2047.216823	337419.425779	37.871898
2048.983265	338089.814880	37.876916
2051.529177	338744.020090	37.881933
2053.648955	339405.853420	37.886951
2055.585028	340079.232583	37.891968
2058.115871	340738.667964	37.896986
2060.424380	341398.792324	37.902004
2063.027362	342055.583193	37.907021
2065.087665	342723.929738	37.912039
2066.863167	343375.285641	37.917056
2069.118689	344038.859562	37.922074
2071.245403	344698.004730	37.927092
2073.587799	345354.870319	37.932109
2075.780345	346020.786912	37.937127
2077.978924	346668.014472	37.942144
2080.130638	347324.326060	37.947162
2082.539727	347990.785793	37.952180
2084.815485	348638.352518	37.957197
2086.826843	349293.618760	37.962215
2088.783221	349954.594328	37.967232
2090.688350	350600.368528	37.972250
2092.709316	351259.942982	37.977268
2095.508816	351910.619826	37.982285
2097.097875	352563.752118	37.987303
2099.277792	353223.497565	37.992320
2101.591269	353871.664740	37.997338
2103.707955	354534.825957	38.002356
2105.932787	355185.449182	38.007373
2108.183206	355839.736866	38.012391
2110.388435	356481.995387	38.017408
2113.118702	357110.986004	38.022426
2115.094361	357735.123085	38.027444
2117.493442	358330.128117	38.032461
2119.441709	358941.540215	38.037479
2121.286337	359544.943616	38.042496
2123.741312	360156.174301	38.047514
2125.501268	360764.850537	38.052532
2127.430452	361374.198728	38.057549
2129.154689	361995.901693	38.062567
2131.305368	362623.255033	38.067584
2133.378608	363245.766105	38.072602
2135.007551	363882.320568	38.077620
2136.860589	364516.999634	38.082637
2139.079316	365158.429180	38.087655
2140.936385	365804.450190	38.092672
2142.911913	366463.909052	38.097690
2144.670707	367121.338670	38.102708
2146.717456	367782.055527	38.107725
2148.788019	368469.313030	38.112743
2150.481470	369148.607045	38.117760
2152.377204	369831.658279	38.122778
2154.036223	370535.585451	38.127796
2156.302696	371238.836957	38.132813
2158.720835	371940.780535	38.137831
2160.302822	372657.714991	38.142848
2162.806668	373375.339490	38.147866
2165.048731	374106.282885	38.152884
2166.988779	374829.603832	38.157901
2168.907889	375574.037564	38.162919
2170.858591	376309.574144	38.167936
2172.985402	377046.586235	38.172954
2174.778324	377799.209013	38.177972
2177.283330	378549.664643	38.182989
2178.853395	379322.272780	38.188007
2181.064455	380090.696412	38.193024
2183.063382	380856.831091	38.198042
2185.089065	381650.478600	38.203060
2187.364572	382432.147628	38.208077
2189.335921	383223.509498	38.213095
2191.598376	384018.934673	38.218112
2193.761679	384815.320410	38.223130
2196.092897	385614.826445	38.228148
2199.071809	386403.858305	38.233165
2201.552703	387193.107579	38.238183
2203.553499	387988.097306	38.243200
2206.373087	388773.724961	38.248218
2208.661140	389562.009004	38.253236
2211.177698	390350.005572	38.258253
2213.557988	391128.956131	38.263271
2215.733666	391916.539429	38.268288
2218.296870	392691.261588	38.273306
2220.331342	393469.729131	38.278324
2222.850771	394241.123668	38.283341
2225.508688	395010.446911	38.288359
2227.395048	395792.325429	38.293376
2229.432731	396548.383881	38.298394
2231.980664	397306.185407	38.303412
2234.396090	398038.065715	38.308429
2236.811907	398771.118351	38.313447
2238.641334	399505.823538	38.318464
2241.036431	400237.752452	38.323482
2242.883470	400992.079434	38.328500
2244.959577	401731.752448	38.333517
2247.575267	402465.562156	38.338535
2249.542454	403213.803915	38.343552
2251.618323	403963.780433	38.348570
2253.884044	404720.088588	38.353588
2256.138996	405472.172238	38.358605
2258.473379	406223.385594	38.363623
2260.602407	406987.254500	38.368640
2263.474579	407735.800712	38.373658
2265.728094	408496.135080	38.378676
2268.270885	409234.689797	38.383693
2271.283953	409979.045587	38.388711
2273.276999	410729.076681	38.393728
2275.903207	411474.874949	38.398746
2278.165407	412228.439314	38.403764
2280.171380	412973.515757	38.408781
2282.387462	413730.970295	38.413799
2284.514042	414492.774003	38.418816
2286.978459	415244.443346	38.423834
2289.393632	416009.698234	38.428852
2291.453551	416772.230607	38.433869
2293.836501	417535.039362	38.438887
2295.581195	418304.214049	38.443904
2297.891749	419081.143382	38.448922
2299.327451	419862.274725	38.453940
2301.519813	420662.166007	38.458957
2304.047099	421460.758890	38.463975
2306.100030	422260.926056	38.468992
2308.510146	423067.132811	38.474010
2310.373886	423884.596149	38.479028
2312.341476	424702.368627	38.484045
2314.851908	425509.692256	38.489063
2316.709032	426356.893689	38.494080
2319.119254	427180.632111	38.499098
2321.556481	428017.195892	38.504116
2323.742481	428852.305019	38.509133
2326.232425	429699.987684	38.514151
2328.218529	430549.193761	38.519168
2330.745173	431391.848214	38.524186
2332.813417	432247.507829	38.529204
2335.347088	433093.237281	38.534221
2337.806743	433954.182199	38.539239
2340.141408	434815.976429	38.544256
2342.167335	435672.780686	38.549274
2344.317380	436548.052856	38.554292
2346.579778	437408.293246	38.559309
2349.164729	438284.435540	38.564327
2351.321908	439170.432831	38.569344
2353.767749	440028.618082	38.574362
2356.078545	440874.650188	38.579380
2358.505866	441731.203874	38.584397
2360.996570	442571.675705	38.589415
2363.475493	443397.648509	38.594432
2365.961216	444233.200355	38.599450
2368.347047	445078.196465	38.604468
2370.926098	445910.025154	38.609485
2373.430937	446749.016794	38.614503
2375.563831	447595.727081	38.619520
2377.801075	448434.141563	38.624538
2380.672874	449277.471854	38.629556
2383.163218	450124.727669	38.634573
2385.512738	450959.330343	38.639591
2388.122118	451816.409183	38.644608
2390.465888	452656.709600	38.649626
2392.513517	453522.511387	38.654644
2394.462831	454375.349323	38.659661
2396.775161	455235.572719	38.664679
2398.684186	456110.743620	38.669696
2400.936513	456997.547248	38.674714
2403.625148	457878.828016	38.679732
2405.727462	458771.544616	38.684749
2408.285685	459666.013813	38.689767
2410.645465	460557.292247	38.694784
2413.022082	461465.106646	38.699802
2415.493855	462364.371786	38.704820
2417.806301	463269.182488	38.709837
2420.192543	464168.935421	38.714855
2422.375308	465091.372262	38.719872
2425.082695	466001.395868	38.724890
2427.755528	466928.108314	38.729908
2430.068651	467856.353401	38.734925
2432.555801	468780.885797	38.739943
2434.993618	469712.050884	38.744960
2437.066902	470642.878882	38.749978
2439.374643	471580.440945	38.754996
2441.676434	472520.937700	38.760013
2444.271647	473451.335274	38.765031
2446.441799	474418.632212	38.770048
2448.252425	475375.282811	38.775066
2451.036089	476334.899389	38.780084
2453.424370	477302.613932	38.785101
2455.644269	478267.932510	38.790119
2457.939385	479243.943102	38.795136
2460.666866	480207.304424	38.800154
2463.841499	481176.748453	38.805172
2466.619129	482133.737019	38.810189
2469.499358	483088.283934	38.815207
2472.209582	484053.410438	38.820224
2475.025849	485014.276293	38.825242
2477.663777	485960.632870	38.830260
2479.649190	486914.722380	38.835277
2481.828900	487863.830751	38.840295
2484.462524	488824.216220	38.845312
2486.969020	489777.757096	38.850330
2489.680767	490691.797008	38.855348
2492.472385	491629.592992	38.860365
2495.127888	492522.855437	38.865383
2497.323652	493435.928890	38.870400
2499.998320	494343.523300	38.875418
2502.864081	495256.888797	38.880436
2505.035839	496163.815521	38.885453
2507.626019	497080.055223	38.890471
2509.890935	497995.039261	38.895488
2512.797875	498899.926545	38.900506
2515.820845	499811.856424	38.905524
2518.605283	500717.371519	38.910541
2521.144452	501626.661185	38.915559
2523.480280	502544.003952	38.920576
2526.112040	503455.445608	38.925594
2528.483333	504369.704506	38.930612
2530.746100	505292.249905	38.935629
2533.316149	506222.958707	38.940647
2536.255669	507159.902877	38.945664
2538.514678	508084.960899	38.950682
2540.980697	509013.257002	38.955700
2542.992229	509961.940792	38.960717
2545.846574	510904.425800	38.965735
2548.391867	511846.403368	38.970752
2550.602273	512802.543391	38.975770
2552.735010	513760.502941	38.980788
2554.960381	514747.362707	38.985805
2557.313220	515718.769793	38.990823
2559.640276	516699.844594	38.995840
2562.414185	517688.035569	39.000858
2565.148867	518688.310820	39.005876
2567.386672	519702.509042	39.010893
2570.337585	520690.274425	39.015911
2572.475830	521713.623954	39.020928
2574.844205	522734.397057	39.025946
2577.747841	523751.635322	39.030964
2579.887547	524783.992146	39.035981
2582.158268	525830.203411	39.040999
2584.509275	526882.772314	39.046016
2587.462072	527940.852869	39.051034
2590.495266	528990.587512	39.056052
2592.660969	530051.772255	39.061069
2595.170675	531110.858213	39.066087
2597.398435	532172.734071	39.071104
2599.764467	533253.532986	39.076122
2602.379731	534330.585174	39.081140
2604.812562	535418.356775	39.086157
2607.692765	536522.876120	39.091175
2610.068309	537623.270623	39.096192
2613.145490	538717.674556	39.101210
2615.980662	539811.029219	39.106228
2618.499233	540919.795945	39.111245
2621.716524	542010.047434	39.116263
2624.703679	543105.383328	39.121280
2627.459408	544191.218220	39.126298
2630.399064	545249.229166	39.131316
2632.968010	546301.892631	39.136333
2635.654233	547342.992177	39.141351
2638.566946	548405.994396	39.146368
2640.750065	549460.794282	39.151386
2643.265003	550515.757447	39.156404
2645.500612	551588.529703	39.161421
2647.664326	552654.142666	39.166439
2650.170461	553735.794934	39.171456
2652.433618	554827.954226	39.176474
2655.355435	555925.087183	39.181492
2657.911345	557017.117794	39.186509
2660.622309	558117.170652	39.191527
2663.477101	559235.141428	39.196544
2665.898240	560351.785394	39.201562
2669.062558	561465.344459	39.206580
2671.442414	562594.159666	39.211597
2674.526104	563710.353149	39.216615
2677.119423	564842.903585	39.221632
2680.151271	565969.154385	39.226650
2683.102871	567095.571304	39.231668
2686.259958	568220.749711	39.236685
2688.795044	569347.441054	39.241703
2691.444584	570481.491394	39.246720
2693.926331	571615.920562	39.251738
2696.952979	572760.241110	39.256756
2699.085126	573911.133298	39.261773
2701.862601	575061.408107	39.266791
2704.889644	576208.674675	39.271808
2707.688041	577377.695204	39.276826
2710.601328	578531.086890	39.281844
2713.594346	579689.873954	39.286861
2716.655227	580838.660847	39.291879
2719.715370	582002.132487	39.296896
2722.334212	583150.025380	39.301914
2725.762918	584307.848719	39.306932
2728.628376	585468.063721	39.311949
2731.297634	586601.784848	39.316967
2734.280953	587748.476776	39.321984
2737.046172	588897.150821	39.327002
2739.815086	590028.976707	39.332020
2742.173721	591176.898882	39.337037
2745.229544	592312.867065	39.342055
2748.376704	593459.380663	39.347072
2751.041396	594605.714553	39.352090
2754.624050	595739.959070	39.357108
2757.668149	596893.015853	39.362125
2760.224615	598035.024802	39.367143
2763.129814	599164.794399	39.372160
2765.661302	600305.431748	39.377178
2768.400113	601435.057232	39.382196
2771.209744	602564.809570	39.387213
2774.097708	603706.499206	39.392231
2776.761407	604846.611232	39.397248
2779.466885	605969.237107	39.402266
2782.356603	607064.299919	39.407284
2784.982041	608161.803012	39.412301
2787.749273	609258.924459	39.417319
2790.643323	610354.365981	39.422336
2793.462495	611464.117604	39.427354
2796.045215	612561.195772	39.432372
2798.595994	613662.321344	39.437389
2801.533719	614774.521474	39.442407
2804.104352	615880.122287	39.447424
2806.748302	617000.246775	39.452442
2809.627156	618111.768582	39.457460
2812.497755	619229.576054	39.462477
2815.301647	620353.676845	39.467495
2818.363573	621474.218744	39.472512
2821.452360	622602.184523	39.477530
2824.395012	623722.013207	39.482548
2826.849251	624858.893116	39.487565
2829.916859	625996.396382	39.492583
2832.333082	627138.983733	39.497600
2834.593826	628308.142260	39.502618
2837.352131	629470.944653	39.507636
2839.941535	630636.543424	39.512653
2842.509130	631816.943459	39.517671
2845.546781	632997.030235	39.522688
2848.319317	634198.191203	39.527706
2851.217018	635391.656240	39.532724
2854.192353	636600.788746	39.537741
2856.915769	637800.592274	39.542759
2860.278425	638997.552496	39.547776
2863.118737	640205.236757	39.552794
2866.781451	641409.545452	39.557812
2869.671647	642609.205688	39.562829
2872.377106	643821.171937	39.567847
2875.259490	645013.567741	39.572864
2878.323194	646230.368880	39.577882
2881.243485	647448.941288	39.582900
2884.254366	648669.094310	39.587917
2886.877191	649880.692552	39.592935
2889.606122	651101.991054	39.597952
2892.495116	652332.378623	39.602970
2895.013332	653548.927057	39.607988
2897.744609	654791.787521	39.613005
2900.493799	656042.655208	39.618023
2903.835168	657281.609215	39.623040
2906.099435	658532.290428	39.628058
2909.372882	659783.185815	39.633076
2912.630231	661041.886663	39.638093
2915.243238	662287.343909	39.643111
2918.420991	663540.455902	39.648128
2921.169605	664800.393635	39.653146
2924.475847	666065.343503	39.658164
2927.438437	667321.677477	39.663181
2930.394626	668575.160203	39.668199
2933.678669	669833.543031	39.673216
2936.718647	671088.368362	39.678234
2939.424403	672310.815685	39.683252
2942.457705	673513.808728	39.688269
2945.213074	674736.278136	39.693287
2948.150787	675958.356850	39.698304
2950.812313	677167.053625	39.703322
2953.702882	678395.675999	39.708340
2956.811634	679609.888827	39.713357
2959.129722	680845.087676	39.718375
2962.265772	682067.017202	39.723392
2964.927992	683313.296357	39.728410
2967.986806	684552.633808	39.733428
2970.736666	685799.450299	39.738445
2973.338559	687059.174957	39.743463
2976.209262	688318.727062	39.748480
2979.113092	689598.492504	39.753498
2982.116025	690872.550325	39.758516
2985.169361	692155.595392	39.763533
2987.622502	693450.412879	39.768551
2990.758601	694756.033925	39.773568
2993.291353	696065.184845	39.778586
2996.268219	697385.617522	39.783604
2999.355201	698711.930084	39.788621
3002.052088	700041.428881	39.793639
3004.961586	701383.078035	39.798656
3008.243146	702735.803378	39.803674
3011.330716	704083.296910	39.808692
3014.240701	705435.761805	39.813709
3017.261086	706802.952209	39.818727
3020.129719	708166.979063	39.823744
3023.108261	709543.394537	39.828762
3026.212230	710923.476586	39.833780
3029.449099	712294.451542	39.838797
3032.293888	713677.197353	39.843815
3035.908411	715047.610628	39.848832
3039.404117	716432.859496	39.853850
3042.390621	717815.492654	39.858868
3045.794327	719197.478961	39.863885
3048.842426	720600.409553	39.868903
3052.208631	721970.616734	39.873920
3055.396924	723355.010722	39.878938
3057.859536	724745.324908	39.883956
3060.628741	726156.252487	39.888973
3063.480304	727557.189576	39.893991
3066.694411	728958.663316	39.899008
3069.420449	730376.029066	39.904026
3072.328415	731792.078279	39.909044
3075.747676	733196.633680	39.914061
3079.053946	734623.224511	39.919079
3082.150036	736041.848560	39.924096
3084.988098	737472.501483	39.929114
3087.629987	738898.292929	39.934132
3090.577106	740339.559819	39.939149
3093.510814	741778.839768	39.944167
3096.878280	743218.275402	39.949184
3100.244791	744650.200023	39.954202
3103.450289	746056.653458	39.959220
3106.965937	747445.699491	39.964237
3109.638484	748835.084366	39.969255
3112.752187	750220.942336	39.974272
3115.946733	751618.013719	39.979290
3119.015935	752999.882028	39.984308
3122.228791	754384.578505	39.989325
3125.520642	755779.889737	39.994343
3129.151410	757160.269487	39.999360
3132.283120	758563.168931	40.004378
3135.422076	759948.390061	40.009396
3138.867120	761336.747856	40.014413
3142.034114	762732.569108	40.019431
3145.139117	764126.223177	40.024448
3148.425949	765519.192849	40.029466
3151.670570	766913.187129	40.034484
3154.675317	768309.909262	40.039501
3157.417451	769722.332629	40.044519
3160.801193	771132.509145	40.049536
3163.806432	772540.220381	40.054554
3166.373399	773978.772029	40.059572
3169.755807	775401.435337	40.064589
3172.749413	776844.356827	40.069607
3176.406680	778263.762171	40.074624
3179.682735	779697.772875	40.079642
3182.980110	781137.332788	40.084660
3186.253028	782577.344305	40.089677
3189.218681	784028.790213	40.094695
3192.956845	785468.140290	40.099712
3196.432974	786911.214635	40.104730
3199.080499	788366.389327	40.109748
3202.537919	789820.195427	40.114765
3205.172296	791280.553796	40.119783
3208.001310	792752.771259	40.124800
3211.599616	794235.467968	40.129818
3214.042243	795720.005481	40.134836
3216.944641	797209.189503	40.139853
3219.442384	798723.912711	40.144871
3222.664464	800234.364258	40.149888
3225.717014	801763.737425	40.154906
3228.602809	803293.825573	40.159924
3232.041729	804839.758816	40.164941
3235.094242	806394.939794	40.169959
3237.891391	807954.646974	40.174976
3240.868514	809516.309808	40.179994
3244.396633	811094.516731	40.185012
3247.548812	812669.976025	40.190029
3250.745667	814264.734300	40.195047
3254.049443	815848.891978	40.200064
3257.623208	817443.119371	40.205082
3260.759813	819047.284606	40.210100
3264.393948	820649.902998	40.215117
3267.563507	822252.894047	40.220135
3271.039010	823836.232750	40.225152
3273.933340	825420.555342	40.230170
3276.984551	826986.582536	40.235188
3280.785566	828538.512226	40.240205
3283.918860	830093.350597	40.245223
3287.351713	831637.927354	40.250240
3291.357369	833184.519025	40.255258
3294.240546	834728.934358	40.260276
3297.983278	836269.764830	40.265293
3301.546738	837799.940279	40.270311
3304.702379	839333.805579	40.275328
3308.385594	840873.531161	40.280346
3312.050558	842410.162433	40.285364
3315.697783	843936.409989	40.290381
3319.241042	845474.549131	40.295399
3322.471770	846999.830604	40.300416
3325.850182	848530.930626	40.305434
3328.945036	850072.287118	40.310452
3331.978982	851608.416767	40.315469
3335.352255	853160.412947	40.320487
3338.328247	854706.166958	40.325504
3341.591289	856271.176307	40.330522
3344.645146	857836.888277	40.335540
3348.179536	859402.795374	40.340557
3351.168600	860991.754138	40.345575
3354.690450	862566.541337	40.350592
3358.084033	864153.535299	40.355610
3361.080527	865746.281275	40.360628
3364.539927	867341.915120	40.365645
3367.751906	868944.716979	40.370663
3371.082537	870572.328115	40.375680
3374.496153	872180.806065	40.380698
3377.256943	873813.915093	40.385716
3380.582376	875443.962263	40.390733
3383.663391	877097.092041	40.395751
3387.056595	878750.089672	40.400768
3390.815394	880399.562733	40.405786
3394.083913	882066.619156	40.410804
3397.899024	883720.647364	40.415821
3401.331974	885391.548702	40.420839
3405.079090	887051.586463	40.425856
3408.460459	888715.645963	40.430874
3411.824812	890386.748994	40.435892
3415.096303	892050.533294	40.440909
3418.863968	893724.061586	40.445927
3421.847041	895390.388548	40.450944
3425.650009	897065.141051	40.455962
3428.695516	898756.669068	40.460980
3432.252903	900448.852623	40.465997
3435.638696	902126.309180	40.471015
3438.524645	903836.255859	40.476032
3442.481003	905523.370129	40.481050
3445.959249	907220.150356	40.486068
3449.475878	908919.191422	40.491085
3453.414377	910612.735438	40.496103
3456.629721	912316.160964	40.501120
3460.406876	913973.973082	40.506125
3463.854413	915605.292863	40.511130
3467.264998	917169.631425	40.516135
3470.640089	918661.176099	40.521140
3474.150901	920083.419082	40.526144
3477.267335	921441.312412	40.531149
3479.923966	922719.629242	40.536154
3483.271200	923905.734205	40.541159
3486.358919	925025.603546	40.546164
3489.085214	926066.709705	40.551168
3491.626993	927013.794706	40.556173
3494.340852	927900.462822	40.561178
3496.573067	928701.984109	40.566183
3499.338969	929432.530013	40.571188
3501.301076	930095.622108	40.576192
3503.693579	930683.203578	40.581197
3505.530565	931218.119895	40.586202
3507.780961	931675.172217	40.591207
3509.458775	932075.661967	40.596212
3510.673367	932419.487403	40.601216
3512.832375	932700.853883	40.606221
3514.011659	932948.597591	40.611226
3515.464064	933136.987238	40.616231
3516.829577	933265.610919	40.621236
3518.069384	933366.812937	40.626240
3519.486178	933416.461508	40.631245
3519.987999	933436.235737	40.636250
3521.359649	933408.273704	40.641255
3522.378193	933350.149375	40.646260
3522.913727	933242.406835	40.651264
3524.011344	933116.431873	40.656269
3524.792095	932964.505199	40.661274
3525.429748	932780.453798	40.666279
3526.263954	932574.004114	40.671284
3526.979509	932336.282779	40.676288
3527.703604	932076.476759	40.681293
3527.991736	931806.175390	40.686298
3528.898238	931496.403709	40.691303
3529.486696	931168.335208	40.696308
3529.913722	930839.505975	40.701312
3530.512776	930472.516336	40.706317
3530.615109	930095.601659	40.711322
3531.167006	929703.029688	40.716327
3531.110798	929303.331085	40.721332
3531.503777	928888.545711	40.726336
3532.160261	928465.904259	40.731341
3532.348246	928035.337755	40.736346
3532.921590	927586.421303	40.741351
3533.363650	927119.814836	40.746356
3532.960272	926656.097695	40.751360
3533.515435	926173.634218	40.756365
3533.517674	925692.566649	40.761370
3533.751411	925195.945398	40.766375
3534.161708	924687.619615	40.771380
3534.052827	924186.734639	40.776384
3534.632320	923674.919929	40.781389
3534.489649	923159.238341	40.786394
3534.690157	922615.280105	40.791399
3535.053281	922089.891724	40.796404
3535.023896	921559.711130	40.801408
3535.045578	921006.389498	40.806413
3535.398145	920468.246675	40.811418
3535.404780	919916.162154	40.816423
3535.451618	919359.685458	40.821428
3535.340828	918806.160755	40.826432
3536.195928	918230.573409	40.831437
3536.188015	917662.962814	40.836442
3536.363569	917070.239851	40.841447
3536.676989	916490.133315	40.846452
3536.360149	915902.179288	40.851456
3536.768074	915304.988762	40.856461
3536.813326	914716.941166	40.861466
3536.947578	914112.638340	40.866471
3536.788102	913508.415054	40.871476
3536.762635	912906.317232	40.876480
3537.223041	912291.355782	40.881485
3537.087861	911682.014248	40.886490
3536.918996	911059.026379	40.891495
3537.141034	910445.536508	40.896500
3537.002978	909840.230645	40.901504
3536.656536	909206.655777	40.906509
3536.372891	908599.792790	40.911514
3536.579971	907983.814366	40.916519
3536.385581	907364.557925	40.921524
3536.448616	906754.155128	40.926528
3536.646755	906136.044083	40.931533
3536.678667	905518.567586	40.936538
3536.378634	904899.632301	40.941543
3536.701234	904275.891648	40.946548
3536.473350	903663.944663	40.951552
3536.541764	903036.249654	40.956557
3536.537048	902417.759896	40.961562
3536.599161	901790.794349	40.966567
3536.591435	901161.840120	40.971572
3536.602781	900529.143980	40.976576
3536.713427	899897.904072	40.981581
3536.481845	899282.099241	40.986586
3536.734861	898644.225429	40.991591
3536.746605	898006.030782	40.996596
3536.422705	897368.400612	41.001600
3536.807840	896735.503483	41.006605
3536.608549	896100.509951	41.011610
3536.449983	895466.211057	41.016615
3536.563408	894830.441935	41.021620
3536.652258	894194.992247	41.026624
3537.182490	893552.630893	41.031629
3536.933803	892915.066076	41.036634
3536.990410	892258.237549	41.041639
3537.317671	891607.184509	41.046644
3537.156620	890967.839973	41.051648
3537.069005	890317.194094	41.056653
3537.435449	889664.269042	41.061658
3537.354804	889002.737568	41.066663
3537.169520	888343.275784	41.071668
3536.592229	887680.612587	41.076672
3536.883018	887022.756135	41.081677
3536.799020	886373.500758	41.086682
3536.782570	885717.289497	41.091687
3536.823079	885064.284735	41.096692
3536.863732	884420.208545	41.101696
3536.791131	883747.811302	41.106701
3536.650339	883088.902753	41.111706
3536.560430	882425.746878	41.116711
3536.866830	881766.127733	41.121716
3536.711197	881114.357920	41.126720
3536.856016	880445.415527	41.131725
3536.910885	879787.649499	41.136730
3536.639453	879123.179844	41.141735
3536.857931	878459.907649	41.146740
3536.710707	877800.305336	41.151744
3536.898718	877132.236430	41.156749
3536.778143	876470.153963	41.161754
3536.882911	875797.876445	41.166759
3536.894176	875132.034030	41.171764
3536.844307	874470.296330	41.176768
3537.067298	873797.576625	41.181773
3536.633341	873122.952780	41.186778
3536.548792	872459.541113	41.191783
3536.594973	871785.555970	41.196788
3536.681425	871128.950914	41.201792
3536.573771	870456.781643	41.206797
3536.203141	869794.673614	41.211802
3536.418966	869128.898044	41.216807
3536.623236	868459.070606	41.221812
3536.352516	867792.258452	41.226816
3536.499700	867110.932147	41.231821
3536.315256	866443.081258	41.236826
3536.007826	865784.207889	41.241831
3536.526067	865100.550745	41.246836
3536.139788	864439.309757	41.251840
3536.334977	863778.674034	41.256845
3536.164240	863114.239620	41.261850
3536.202375	862439.397521	41.266855
3536.344908	861755.328259	41.271860
3536.076926	861086.023451	41.276864
3536.532942	860416.618393	41.281869
3536.243325	859746.780838	41.286874
3536.043931	859082.006433	41.291879
3536.043054	858404.875304	41.296884
3536.000273	857732.440678	41.301888
3536.116376	857050.861019	41.306893
3535.970644	856388.409675	41.311898
3535.934072	855711.472493	41.316903
3536.079716	855030.538362	41.321908
3536.055053	854370.183015	41.326912
3535.903183	853685.356376	41.331917
3536.022229	853010.430274	41.336922
3535.657605	852336.680717	41.341927
3536.046227	851665.843663	41.346932
3535.719728	850990.188828	41.351936
3535.845659	850315.940672	41.356941
3536.004622	849640.639942	41.361946
3535.755091	848964.653892	41.366951
3535.776650	848275.109040	41.371956
3535.587866	847608.995936	41.376960
3535.675738	846930.686187	41.381965
3535.744599	846257.663883	41.386970
3535.659176	845582.257248	41.391975
3535.727428	844910.161821	41.396980
3535.424294	844236.693493	41.401984
3535.527242	843557.431056	41.406989
3535.251672	842895.119334	41.411994
3535.432473	842219.402969	41.416999
3536.028147	841537.304087	41.422004
3535.777243	840858.201043	41.427008
3536.090297	840176.442289	41.432013
3535.985681	839488.976487	41.437018
3535.808930	838806.617624	41.442023
3535.568705	838109.711326	41.447028
3535.439561	837431.000762	41.452032
3535.431228	836755.416811	41.457037
3535.312903	836078.609199	41.462042
3535.372647	835404.724547	41.467047
3535.617831	834708.876265	41.472052
3535.299894	834038.279210	41.477056
3535.413806	833346.014347	41.482061
3535.653226	832665.758956	41.487066
3535.328678	831981.671314	41.492071
3535.543286	831288.386757	41.497076
3535.161825	830608.557171	41.502080
3535.115105	829931.382385	41.507085
3535.161503	829260.420955	41.512090
3535.128040	828567.082271	41.517095
3535.365814	827881.487822	41.522100
3535.037765	827203.050267	41.527104
3535.120544	826523.348087	41.532109
3535.683890	825834.697482	41.537114
3535.053810	825152.726393	41.542119
3535.147268	824461.421144	41.547124
3534.958964	823774.734512	41.552128
3534.997688	823091.896816	41.557133
3535.141812	822407.112294	41.562138
3534.979497	821733.310023	41.567143
3535.390401	821042.763975	41.572148
3535.181603	820358.071053	41.577152
3535.067617	819668.204313	41.582157
3535.492937	818979.005084	41.587162
3535.198955	818290.786398	41.592167
3534.943455	817594.563841	41.597172
3534.648566	816912.954068	41.602176
3535.009343	816216.384075	41.607181
3534.879286	815541.407703	41.612186
3534.384726	814859.915534	41.617191
3534.703085	814171.117274	41.622196
3534.536444	813490.506423	41.627200
3534.391538	812811.585280	41.632205
3534.447505	812132.365283	41.637210
3534.326868	811450.315477	41.642215
3534.534010	810765.104128	41.647220
3534.305283	810091.701702	41.652224
3534.347908	809397.759035	41.657229
3534.691601	808724.465473	41.662234
3534.377174	808043.427117	41.667239
3534.514445	807348.474282	41.672244
3534.399027	806673.879429	41.677248
3534.517388	805984.719894	41.682253
3534.419051	805301.556393	41.687258
3534.104881	804621.449513	41.692263
3534.261060	803936.390213	41.697268
3533.907945	803255.859924	41.702272
3534.195818	802571.131789	41.707277
3534.221744	801894.667618	41.712282
3533.745461	801219.841004	41.717287
3534.041417	800530.052712	41.722292
3533.952263	799862.384252	41.727296
3533.758584	799182.944103	41.732301
3534.020039	798499.385337	41.737306
3533.833124	797809.702097	41.742311
3534.048263	797130.677617	41.747316
3533.737286	796451.970991	41.752320
3533.821970	795774.014031	41.757325
3533.687024	795094.752276	41.762330
3533.620071	794419.585546	41.767335
3534.047468	793746.183912	41.772340
3533.570924	793057.748501	41.777344
3533.646111	792384.717904	41.782349
3533.644823	791702.157365	41.787354
3533.366494	791031.807603	41.792359
3533.524800	790353.018072	41.797364
3532.933602	789678.957973	41.802368
3533.189918	789001.888386	41.807373
3533.708031	788337.336800	41.812378
3533.245181	787661.490008	41.817383
3533.302978	786981.509225	41.822388
3533.269793	786309.735778	41.827392
3532.952524	785632.442185	41.832397
3533.143172	784964.091635	41.837402
3533.053796	784286.680355	41.842407
3532.721995	783612.147043	41.847412
3532.575845	782956.105285	41.852416
3532.793151	782279.041514	41.857421
3532.751334	781610.564713	41.862426
3532.460257	780945.855521	41.867431
3532.754844	780280.689784	41.872436
3532.503889	779627.362422	41.877440
3532.403568	778954.467421	41.882445
3532.843098	778287.174408	41.887450
3532.693859	777627.990490	41.892455
3532.964394	776957.798995	41.897460
3532.473177	776288.413912	41.902464
3532.558235	775613.848197	41.907469
3532.959700	774948.715835	41.912474
3532.446648	774285.648140	41.917479
3532.546058	773607.300492	41.922484
3532.012762	772945.197773	41.927488
3532.402273	772286.423225	41.932493
3532.502521	771619.217408	41.937498
3532.198557	770950.887174	41.942503
3532.339323	770283.356190	41.947508
3532.167863	769619.660457	41.952512
3531.998286	768956.052500	41.957517
3532.284684	768293.834503	41.962522
3531.855357	767624.435994	41.967527
3532.220859	766959.917137	41.972532
3532.075337	766301.340118	41.977536
3532.076953	765636.321445	41.982541
3531.838452	764980.502105	41.987546
3531.643552	764314.462445	41.992551
3531.674203	763643.986346	41.997556
3532.135287	763000.199050	42.002560
3532.264572	762334.075621	42.007565
3532.203730	761670.637804	42.012570
3531.964674	761003.916783	42.017575
3532.160429	760330.798407	42.022580
3531.727694	759672.476166	42.027584
3531.884764	759001.810831	42.032589
3531.730395	758343.275894	42.037594
3531.237569	757687.849903	42.042599
3531.444249	757026.918599	42.047604
3531.110009	756374.806253	42.052608
3531.321272	755726.197007	42.057613
3531.634291	755070.999980	42.062618
3531.195185	754420.070827	42.067623
3531.431584	753760.479951	42.072628
3531.429681	753110.944420	42.077632
3531.517481	752451.858646	42.082637
3531.693111	751793.244447	42.087642
3531.325786	751131.851685	42.092647
3531.318747	750473.451976	42.097652
3531.252887	749814.709738	42.102656
3531.058648	749165.021990	42.107661
3531.224391	748508.005862	42.112666
3531.236499	747861.088017	42.117671
3531.080643	747208.759434	42.122676
3531.049358	746549.881827	42.127680
3531.006270	745899.746539	42.132685
3531.209058	745250.602288	42.137690
3530.694925	744595.200103	42.142695
3531.030557	743942.316468	42.147700
3530.801364	743297.285185	42.152704
3530.564573	742649.730290	42.157709
3530.690123	741995.830589	42.162714
3530.325495	741353.579766	42.167719
3530.625421	740705.822635	42.172724
3530.291598	740059.999725	42.177728
3530.212646	739418.185445	42.182733
3530.465741	738773.146375	42.187738
3530.338551	738132.917841	42.192743
3530.194319	737492.393225	42.197748
3530.224154	736844.762105	42.202752
3530.140063	736204.865652	42.207757
3530.397471	735564.067850	42.212762
3529.676646	734932.936225	42.217767
3530.064253	734293.053473	42.222772
3529.821383	733656.048332	42.227776
3529.918285	733019.776045	42.232781
3530.214382	732379.459314	42.237786
3529.707886	731749.773121	42.242791
3529.931224	731102.486143	42.247796
3529.883666	730479.405077	42.252800
3529.799354	729836.921414	42.257805
3529.985008	729199.391734	42.262810
3529.803343	728573.166115	42.267815
3529.778932	727925.469309	42.272820
3529.556179	727306.978540	42.277824
3529.870262	726673.042686	42.282829
3530.135186	726034.904656	42.287834
3529.774727	725400.440209	42.292839
3529.820540	724757.681927	42.297844
3529.809260	724125.685102	42.302848
3529.941710	723492.376208	42.307853
3529.803893	722847.071472	42.312858
3529.676777	722210.040836	42.317863
3530.020585	721566.982198	42.322868
3529.821025	720942.753356	42.327872
3529.940245	720295.866844	42.332877
3529.569555	719655.706466	42.337882
3529.115688	719021.758176	42.342887
3529.014488	718386.610432	42.347892
3528.855563	717774.284652	42.352896
3528.993589	717149.514610	42.357901
3529.181610	716524.738879	42.362906
3529.271716	715898.792381	42.367911
3529.470262	715266.232871	42.372916
3529.674606	714633.376633	42.377920
3529.330011	713996.795965	42.382925
3529.710036	713364.161482	42.387930
3529.293899	712736.081122	42.392935
3529.385423	712097.545857	42.397940
3529.341619	711472.086803	42.402944
3529.191900	710841.586999	42.407949
3529.586706	710200.921352	42.412954
3529.251299	709571.004084	42.417959
3529.079061	708935.452505	42.422964
3528.890384	708306.856227	42.427968
3528.723932	707684.415891	42.432973
3528.843211	707056.072157	42.437978
3528.799040	706438.038571	42.442983
3528.964240	705802.146686	42.447988
3528.665902	705184.314473	42.452992
3528.378788	704564.498958	42.457997
3528.751983	703937.969670	42.463002
3528.433905	703321.000553	42.468007
3528.842116	702700.833080	42.473012
3528.568733	702080.787207	42.478016
3528.471322	701463.449244	42.483021
3528.405807	700835.329366	42.488026
3528.359948	700223.459517	42.493031
3528.402358	699602.884703	42.498036
3528.548792	698986.621429	42.503040
3527.957836	698364.277526	42.508045
3528.220350	697746.465654	42.513050
3528.111283	697131.457358	42.518055
3528.473339	696520.501372	42.523060
3528.012687	695909.345077	42.528064
3528.020877	695298.513778	42.533069
3527.808072	694679.423915	42.538074
3527.865311	694082.422413	42.543079
3527.629714	693464.245830	42.548084
3527.233533	692861.520477	42.553088
3527.442745	692258.203191	42.558093
3527.401979	691657.573563	42.563098
3527.071997	691056.405594	42.568103
3527.161701	690458.209700	42.573108
3527.041446	689866.377523	42.578112
3526.853500	689262.527246	42.583117
3527.563305	688662.662519	42.588122
3527.088917	688081.171868	42.593127
3527.153676	687485.518395	42.598132
3527.106210	686888.849312	42.603136
3526.859373	686297.848464	42.608141
3526.986754	685708.188424	42.613146
3526.896356	685122.708264	42.618151
3526.807020	684527.134653	42.623156
3526.770623	683938.183716	42.628160
3526.706457	683349.199309	42.633165
3526.643620	682762.118284	42.638170
3526.816814	682177.149964	42.643175
3526.829550	681588.187897	42.648180
3526.601626	680995.643443	42.653184
3526.300561	680404.567140	42.658189
3526.514003	679825.865894	42.663194
3526.467224	679252.003953	42.668199
3526.513476	678657.966592	42.673204
3526.768694	678076.358626	42.678208
3526.461578	677500.987332	42.683213
3526.566957	676905.830615	42.688218
3526.415417	676328.466552	42.693223
3526.395331	675743.221227	42.698228
3526.471189	675165.048286	42.703232
3526.307929	674579.006545	42.708237
3526.586256	674003.517459	42.713242
3526.374486	673417.859435	42.718247
3526.322283	672828.399223	42.723252
3526.218946	672259.945406	42.728256
3525.882051	671677.489479	42.733261
3526.340190	671093.964303	42.738266
3525.848495	670529.310422	42.743271
3526.140239	669948.185390	42.748276
3526.135138	669375.501671	42.753280
3525.823325	668795.854598	42.758285
3525.993868	668221.774440	42.763290
3526.051864	667647.828278	42.768295
3525.844594	667072.346578	42.773300
3525.409792	666497.567086	42.778304
3525.728401	665930.904125	42.783309
3525.742750	665356.178505	42.788314
3525.309010	664791.222305	42.793319
3525.442917	664230.875115	42.798324
3525.428124	663661.789591	42.803329
3525.377709	663101.307959	42.808333
3525.573220	662537.059242	42.813338
3525.162766	661971.433750	42.818343
3525.462824	661408.398345	42.823348
3525.201030	660850.266795	42.828353
3524.967143	660297.837652	42.833357
3525.318323	659733.398200	42.838362
3525.054578	659163.540272	42.843367
3525.132335	658601.776939	42.848372
3524.839670	658053.872147	42.853377
3524.748167	657490.376190	42.858381
3525.058177	656935.765691	42.863386
3524.809322	656385.462986	42.868391
3524.799349	655823.454528	42.873396
3525.014363	655274.707777	42.878401
3524.763657	654721.665304	42.883405
3524.935401	654166.671776	42.888410
3524.704148	653618.757602	42.893415
3524.608242	653067.493436	42.898420
3524.866593	652512.491762	42.903425
3524.522727	651970.049414	42.908429
3524.780319	651413.587534	42.913434
3524.391109	650868.045351	42.918439
3524.480420	650309.352133	42.923444
3524.634502	649775.247663	42.928449
3524.261242	649227.414332	42.933453
3524.206401	648684.443281	42.938458
3524.372678	648146.551853	42.943463
3524.493806	647601.343171	42.948468
3524.458089	647049.634762	42.953473
3524.246667	646506.622196	42.958477
3524.356969	645967.373863	42.963482
3523.864607	645426.699994	42.968487
3523.995637	644883.791243	42.973492
3524.332772	644348.466392	42.978497
3524.013317	643805.626551	42.983501
3523.923378	643274.067088	42.988506
3523.753591	642723.144576	42.993511
3524.192679	642184.138112	42.998516
3524.017963	641645.907888	43.003521
3523.806996	641110.055624	43.008525
3524.131566	640567.332751	43.013530
3523.737037	640038.706637	43.018535
3523.913710	639492.251166	43.023540
3524.077702	638955.871819	43.028545
3523.346582	638426.119575	43.033549
3523.718555	637887.948307	43.038554
3523.473183	637369.313294	43.043559
3523.367807	636840.923294	43.048564
3523.343195	636307.989905	43.053569
3522.946773	635794.654546	43.058573
3523.740290	635267.931830	43.063578
3523.045275	634747.140563	43.068583
3523.088911	634212.636667	43.073588
3523.548656	633693.897221	43.078593
3523.371740	633182.196653	43.083597
3523.510363	632651.950196	43.088602
3523.262733	632130.551276	43.093607
3523.324613	631599.413700	43.098612
3523.480757	631076.892344	43.103617
3523.287168	630553.253386	43.108621
3523.370196	630021.081234	43.113626
3523.056620	629499.412614	43.118631
3522.837757	628979.804659	43.123636
3522.743023	628463.053748	43.128641
3522.525153	627949.452896	43.133645
3522.809471	627437.694148	43.138650
3522.728036	626924.621171	43.143655
3522.613147	626413.281755	43.148660
3522.791619	625899.363773	43.153665
3522.400528	625403.446974	43.158669
3522.702731	624885.152066	43.163674
3522.146283	624383.256252	43.168679
3522.366281	623868.432038	43.173684
3522.584313	623368.660457	43.178689
3522.124405	622862.469364	43.183693
3522.318868	622359.899791	43.188698
3522.196565	621864.374382	43.193703
3521.969722	621351.660035	43.198708
3521.957407	620860.177840	43.203713
3521.814501	620373.355238	43.208717
3522.033880	619869.262537	43.213722
3521.711366	619375.861879	43.218727
3521.932471	618888.409366	43.223732
3521.966959	618393.900955	43.228737
3521.643914	617902.287687	43.233741
3521.887585	617402.185900	43.238746
3521.538904	616910.582446	43.243751
3521.616060	616418.332851	43.248756
3521.821387	615923.783667	43.253761
3521.404690	615440.596821	43.258765
3521.620294	614952.017267	43.263770
3521.541217	614462.162927	43.268775
3521.508406	613974.986092	43.273780
3521.589834	613489.322436	43.278785
3521.319070	613007.608283	43.283789
3521.595629	612521.969106	43.288794
3521.158520	612051.773878	43.293799
3521.746146	611557.264548	43.298804
3521.558453	611067.830064	43.303809
3521.122496	610594.915250	43.308813
3520.907895	610111.009774	43.313818
3520.971406	609643.034529	43.318823
3521.041527	609154.926517	43.323828
3521.000884	608683.217453	43.328833
3520.834452	608210.205883	43.333837
3521.016738	607734.907763	43.338842
3520.867729	607254.429135	43.343847
3521.169811	606777.765894	43.348852
3521.361933	606305.516025	43.353857
3520.688155	605829.731859	43.358861
3520.987394	605352.808292	43.363866
3521.059043	604885.888090	43.368871
3520.655670	604415.517457	43.373876
3521.035730	603945.043770	43.378881
3520.966486	603468.706095	43.383885
3521.042032	603003.062757	43.388890
3520.646223	602535.272785	43.393895
3520.266980	602061.639227	43.398900
3520.554742	601588.072940	43.403905
3520.358563	601136.000975	43.408909
3520.433445	600668.757044	43.413914
3520.238848	600206.459170	43.418919
3520.483051	599749.940782	43.423924
3520.569238	599275.359884	43.428929
3520.033392	598818.737017	43.433933
3520.484090	598351.535786	43.438938
3520.117366	597900.068825	43.443943
3520.207929	597431.586665	43.448948
3520.281587	596974.033917	43.453953
3519.964676	596528.028003	43.458957
3520.027156	596076.316458	43.463962
3519.972849	595628.925770	43.468967
3520.334319	595167.034929	43.473972
3520.228257	594712.889035	43.478977
3519.954242	594256.393857	43.483981
3519.946678	593798.228309	43.488986
3519.832763	593355.984030	43.493991
3519.873160	592892.702373	43.498996
3519.734898	592442.642911	43.504001
3519.381574	592005.160411	43.509005
3519.467354	591551.763794	43.514010
3519.444096	591117.708299	43.519015
3519.237332	590674.525401	43.524020
3519.196253	590237.125165	43.529025
3519.032639	589801.990495	43.534029
3519.106227	589358.258461	43.539034
3519.077519	588935.729779	43.544039
3518.890378	588497.084700	43.549044
3519.314666	588057.816659	43.554049
3519.180922	587638.777267	43.559053
3518.837117	587206.141352	43.564058
3518.773673	586772.286171	43.569063
3518.696972	586333.392223	43.574068
3519.163055	585908.461095	43.579073
3518.662944	585486.192787	43.584077
3518.991893	585054.319475	43.589082
3518.648512	584632.798685	43.594087
3518.623280	584211.862293	43.599092
3518.711013	583785.212130	43.604097
3518.758958	583358.805080	43.609101
3518.658502	582936.329273	43.614106
3518.519087	582513.493550	43.619111
3518.475318	582090.626813	43.624116
3518.459029	581668.545085	43.629121
3517.904088	581262.477784	43.634125
3518.139719	580833.637680	43.639130
3518.292570	580433.957964	43.644135
3518.047151	580021.964416	43.649140
3518.167078	579609.844384	43.654145
3518.256570	579205.006773	43.659149
3518.363047	578791.403410	43.664154
3518.009542	578378.065846	43.669159
3518.159566	577976.144435	43.674164
3518.482853	577562.312007	43.679169
3517.991555	577154.136867	43.684173
3518.152508	576738.594723	43.689178
3518.007074	576334.356991	43.694183
3517.882968	575919.992898	43.699188
3517.739226	575516.784520	43.704193
3517.650451	575112.195617	43.709197
3517.932453	574705.115831	43.714202
3517.818815	574309.810904	43.719207
3517.953917	573907.659914	43.724212
3517.853787	573497.436891	43.729217
3517.694216	573101.900461	43.734221
3517.791139	572687.441782	43.739226
3517.408588	572297.250889	43.744231
3517.498363	571900.476951	43.749236
3517.678388	571495.524236	43.754241
3517.329239	571111.177688	43.759245
3517.417126	570708.781590	43.764250
3517.575124	570325.129656	43.769255
3517.359415	569935.692758	43.774260
3517.660558	569532.568758	43.779265
3517.256033	569148.272790	43.784269
3517.642153	568744.958355	43.789274
3517.400481	568356.685344	43.794279
3517.414176	567960.002452	43.799284
3517.375120	567567.543947	43.804289
3517.378397	567179.143008	43.809293
3517.627887	566776.947416	43.814298
3517.444409	566389.259094	43.819303
3517.293343	565994.556857	43.824308
3517.366416	565607.757549	43.829313
3517.259810	565226.615257	43.834317
3517.566639	564829.231859	43.839322
3517.574649	564438.230339	43.844327
3517.209926	564048.136473	43.849332
3516.819261	563652.648372	43.854337
3516.531928	563279.736130	43.859341
3516.715399	562900.237920	43.864346
3516.518199	562524.217384	43.869351
3516.834256	562145.480116	43.874356
3516.929235	561754.533985	43.879361
3516.637778	561383.632576	43.884365
3516.819582	561003.072354	43.889370
3516.342514	560634.749510	43.894375
3516.187272	560268.577120	43.899380
3516.602211	559890.764846	43.904385
3516.397928	559524.177193	43.909389
3516.353224	559144.206062	43.914394
3516.260174	558784.629549	43.919399
3515.850952	558414.016885	43.924404
3516.178392	558047.398105	43.929409
3516.065044	557691.169840	43.934413
3516.115815	557313.698501	43.939418
3516.166129	556958.782574	43.944423
3516.215913	556599.122277	43.949428
3515.955049	556226.911929	43.954433
3515.933264	555872.583787	43.959437
3515.733813	555507.496060	43.964442
3516.012122	555159.848147	43.969447
3516.015143	554797.628333	43.974452
3515.934176	554435.413048	43.979457
3515.449661	554087.212549	43.984461
3515.435566	553720.583331	43.989466
3515.528233	553369.041145	43.994471
3515.257398	553022.388837	43.999476
3515.382742	552672.888684	44.004481
3515.409419	552336.497220	44.009485
3515.365089	551983.380224	44.014490
3515.314183	551638.922319	44.019495
3515.317493	551293.236978	44.024500
3515.369539	550951.364380	44.029505
3515.149973	550611.545314	44.034509
3515.363910	550261.262198	44.039514
3514.822603	549931.912983	44.044519
3515.113739	549592.888401	44.049524
3515.485878	549252.833566	44.054529
3515.225231	548910.005447	44.059533
3515.328386	548564.435300	44.064538
3515.210293	548227.160340	44.069543
3514.978168	547887.779549	44.074548
3515.243357	547537.821037	44.079553
3514.770855	547213.535939	44.084557
3515.263093	546871.939671	44.089562
3514.999856	546535.000764	44.094567
3514.724006	546208.692432	44.099572
3514.740793	545864.127707	44.104577
3514.879784	545547.462421	44.109581
3514.801401	545199.620521	44.114586
3514.802690	544881.148575	44.119591
3514.467245	544543.669272	44.124596
3515.106878	544209.090782	44.129601
3514.721284	543893.435209	44.134605
3514.431533	543554.915698	44.139610
3514.955292	543233.745348	44.144615
3514.536365	542902.038933	44.149620
3514.558318	542582.603218	44.154625
3514.385874	542267.983768	44.159629
3514.482722	541936.216792	44.164634
3514.649586	541614.515483	44.169639
3514.470586	541303.304545	44.174644
3514.382281	540963.326322	44.179649
3514.162633	540643.232071	44.184653
3514.453890	540328.489967	44.189658
3514.426985	540012.937793	44.194663
3514.052917	539684.728398	44.199668
3514.200156	539366.660766	44.204673
3513.978659	539068.621794	44.209677
3513.938751	538743.410122	44.214682
3514.518108	538431.955923	44.219687
3514.081587	538126.922873	44.224692
3514.622042	537804.263906	44.229697
3514.421825	537495.192118	44.234701
3514.412054	537171.301252	44.239706
3514.473083	536865.096899	44.244711
3514.095001	536539.388127	44.249716
3514.237827	536227.354909	44.254721
3513.979862	535915.736448	44.259725
3514.128232	535598.240226	44.264730
3514.173825	535288.019305	44.269735
3514.259289	534974.808269	44.274740
3514.266258	534650.352998	44.279745
3513.987675	534353.991134	44.284749
3514.280507	534030.986697	44.289754
3514.083013	533717.796632	44.294759
3513.694228	533408.315753	44.299764
3513.958187	533098.716805	44.304769
3513.773951	532793.173987	44.309773
3513.716502	532481.497463	44.314778
3513.462514	532186.701679	44.319783
3513.468222	531889.282025	44.324788
3513.827994	531576.757932	44.329793
3513.399770	531280.711959	44.334797
3513.282445	530987.331993	44.339802
3513.345087	530690.433257	44.344807
3513.108133	530392.671235	44.349812
3513.094965	530099.709863	44.354817
3513.074161	529817.342402	44.359821
3513.200329	529525.657954	44.364826
3513.513443	529224.447261	44.369831
3513.040124	528935.074153	44.374836
3513.428789	528637.169676	44.379841
3513.216294	528358.794272	44.384845
3513.099835	528066.062351	44.389850
3513.167697	527770.718883	44.394855
3512.924331	527484.962780	44.399860
3512.867750	527192.859533	44.404865
3512.987976	526913.441005	44.409869
3512.969125	526620.613330	44.414874
3512.491954	526340.023998	44.419879
3512.077463	526061.690340	44.424884
3512.283004	525784.810574	44.429889
3512.443897	525519.140637	44.434893
3512.114071	525234.870485	44.439898
3512.430479	524970.426335	44.444903
3512.126242	524697.955171	44.449908
3512.592960	524422.722075	44.454913
3512.024701	524162.706098	44.459917
3512.434391	523895.904575	44.464922
3512.494508	523621.433029	44.469927
3512.246428	523349.028721	44.474932
3512.758222	523081.185475	44.479937
3512.608515	522812.087101	44.484941
3512.653902	522533.508306	44.489946
3512.426050	522259.818491	44.494951
3511.997291	521993.328365	44.499956
3512.464977	521719.560503	44.504961
3511.854284	521455.010807	44.509965
3512.051972	521188.399541	44.514970
3511.730671	520925.154630	44.519975
3511.818994	520673.197679	44.524980
3511.898990	520408.410796	44.529985
3511.682091	520157.608423	44.534989
3511.825121	519892.902809	44.539994
3511.696613	519631.168147	44.544999
3511.748432	519377.428363	44.550004
3511.950408	519129.113259	44.555009
3511.739760	518884.500985	44.560013
3511.616577	518615.677204	44.565018
3512.009361	518361.761338	44.570023
3511.442283	518116.945116	44.575028
3511.704425	517855.113365	44.580033
3511.574530	517602.334864	44.585037
3511.324660	517353.209467	44.590042
3511.098314	517100.742253	44.595047
3511.017520	516864.915148	44.600052
3511.420563	516617.636363	44.605057
3511.093928	516388.259121	44.610061
3511.180560	516140.824668	44.615066
3511.247670	515891.975154	44.620071
3511.054670	515662.715878	44.625076
3511.332620	515413.469063	44.630081
3511.579511	515176.701476	44.635085
3511.317022	514922.234662	44.640090
3511.282752	514685.406552	44.645095
3511.157465	514440.658690	44.650100
3511.218785	514201.887130	44.655105
3511.342436	513975.681204	44.660109
3511.378804	513728.065330	44.665114
3511.274480	513479.610653	44.670119
3511.026100	513246.182305	44.675124
3511.013951	513004.221953	44.680129
3510.907983	512770.004313	44.685133
3510.751698	512531.446489	44.690138
3511.305069	512299.433470	44.695143
3510.945340	512073.232052	44.700148
3511.255598	511826.903623	44.705153
3511.194872	511594.277645	44.710157
3511.258606	511352.177826	44.715162
3511.473939	511113.636109	44.720167
3511.008559	510880.159122	44.725172
3511.088930	510638.298170	44.730177
3511.189212	510404.111182	44.735181
3511.310701	510165.520645	44.740186
3511.254961	509929.584586	44.745191
3510.949978	509701.672185	44.750196
3511.408339	509452.451478	44.755201
3510.853200	509226.444809	44.760205
3510.888765	508988.205007	44.765210
3510.821852	508756.801839	44.770215
3510.575081	508527.144353	44.775220
3510.711362	508296.154659	44.780225
3510.766117	508065.377706	44.785229
3510.659668	507846.249473	44.790234
3510.909674	507610.631185	44.795239
3510.536214	507392.199370	44.800244
3510.961577	507162.306433	44.805249
3510.910301	506941.791729	44.810253
3510.781476	506710.571701	44.815258
3510.747189	506481.606762	44.820263
3510.750053	506264.207350	44.825268
3510.405927	506031.346284	44.830273
3510.422848	505812.876890	44.835277
3510.095704	505594.412732	44.840282
3510.582435	505371.358331	44.845287
3510.126698	505155.589299	44.850292
3510.376670	504928.828527	44.855297
3510.648136	504714.193214	44.860301
3510.521122	504507.306983	44.865306
3510.564870	504282.442796	44.870311
3510.214433	504061.434292	44.875316
3510.349766	503843.625850	44.880321
3510.339338	503629.732085	44.885325
3510.101899	503416.935929	44.890330
3510.188871	503199.329345	44.895335
3509.824179	502993.071097	44.900340
3510.375887	502771.385487	44.905345
3509.845790	502569.447495	44.910349
3509.771199	502356.862500	44.915354
3509.863167	502149.302227	44.920359
3509.813741	501936.758039	44.925364
3509.747060	501733.719416	44.930369
3509.721068	501532.643217	44.935373
3509.781475	501334.735193	44.940378
3509.837042	501131.112068	44.945383
3509.535834	500930.126048	44.950388
3509.997771	500720.815976	44.955393
3509.755833	500512.887529	44.960397
3509.591032	500311.718983	44.965402
3509.692223	500111.716141	44.970407
3509.632827	499919.171509	44.975412
3509.727892	499719.316664	44.980417
3509.603195	499519.041820	44.985421
3509.486453	499314.869468	44.990426
3509.571783	499124.869851	44.995431
3509.287192	498927.093009	45.000436
3509.545749	498723.203282	45.005441
3509.358067	498533.546930	45.010445
3509.436068	498333.122026	45.015450
3509.794170	498130.421740	45.020455
3509.409914	497944.686245	45.025460
3509.565705	497743.836395	45.030465
3509.348048	497548.054644	45.035469
3509.320482	497360.785123	45.040474
3509.370728	497167.835885	45.045479
3508.957493	496979.363579	45.050484
3509.540585	496783.183281	45.055489
3509.460803	496598.695806	45.060493
3509.330024	496414.164431	45.065498
3509.514224	496221.484886	45.070503
3509.495447	496024.488090	45.075508
3509.542222	495819.182924	45.080513
3509.076775	495630.552646	45.085517
3509.543042	495436.854953	45.090522
3509.020118	495252.782424	45.095527
3508.979786	495074.745758	45.100532
3509.243013	494886.286225	45.105537
3509.089486	494692.837559	45.110541
3509.005665	494511.211067	45.115546
3509.404150	494326.262969	45.120551
3509.014409	494150.805379	45.125556
3509.053263	493962.070363	45.130561
3508.896050	493784.647087	45.135565
3508.977773	493592.612645	45.140570
3509.237085	493410.409925	45.145575
3508.943851	493228.350178	45.150580
3508.924948	493044.268761	45.155585
3508.962590	492867.156750	45.160589
3508.739222	492688.519239	45.165594
3509.120130	492506.387264	45.170599
3508.890609	492333.160039	45.175604
3508.948406	492144.755762	45.180609
3508.861887	491966.239098	45.185613
3508.623641	491786.987619	45.190618
3508.715854	491615.266496	45.195623
3508.508344	491453.055438	45.200628
3508.468223	491277.963900	45.205633
3508.805305	491103.514469	45.210637
3508.719406	490931.563950	45.215642
3508.826250	490750.724933	45.220647
3508.256970	490580.472427	45.225652
3508.528955	490413.970383	45.230657
3508.472301	490244.031784	45.235661
3508.208784	490081.867945	45.240666
3508.795004	489906.048363	45.245671
3508.394743	489738.389674	45.250676
3508.253190	489562.690855	45.255681
3508.213365	489402.809912	45.260685
3508.501075	489239.228514	45.265690
3508.580802	489064.245824	45.270695
3508.484531	488895.616292	45.275700
3508.662845	488732.402984	45.280705
3508.620539	488560.623815	45.285709
3508.262318	488385.051250	45.290714
3508.332954	488204.596593	45.295719
3508.053742	488056.432944	45.300724
3508.049347	487897.999531	45.305729
3508.086839	487739.709333	45.310733
3507.833233	487583.086689	45.315738
3507.939501	487417.798637	45.320743
3507.702119	487275.086358	45.325748
3508.006076	487119.831868	45.330753
3507.666671	486958.815711	45.335757
3507.706602	486806.943428	45.340762
3507.498669	486655.820624	45.345767
3507.644738	486512.429387	45.350772
3507.734561	486354.117708	45.355777
3507.872827	486202.324609	45.360781
3507.701280	486055.441390	45.365786
3507.646778	485900.186693	45.370791
3507.531203	485755.265106	45.375796
3508.063928	485594.593600	45.380801
3507.994678	485459.074853	45.385805
3507.667012	485300.824970	45.390810
3507.449883	485146.350530	45.395815
3507.779282	485013.543835	45.400820
3507.525053	484853.303598	45.405825
3507.515524	484713.416405	45.410829
3507.600502	484564.401900	45.415834
3507.557091	484417.786821	45.420839
3507.642877	484281.574609	45.425844
3507.708606	484127.802156	45.430849
3507.537978	483987.683668	45.435853
3507.421086	483840.519612	45.440858
3507.580894	483698.166035	45.445863
3507.213242	483548.967201	45.450868
3507.467229	483409.075334	45.455873
3507.707002	483266.907109	45.460877
3507.686935	483123.415491	45.465882
3507.463954	482972.263722	45.470887
3507.265621	482841.504893	45.475892
3507.669818	482695.507801	45.480897
3507.632001	482557.380039	45.485901
3507.498052	482420.077503	45.490906
3507.575266	482272.715489	45.495911
3507.252379	482140.504865	45.500916
3506.968536	481995.783752	45.505921
3507.450455	481859.890325	45.510925
3507.321411	481717.114677	45.515930
3507.333043	481583.982292	45.520935
3507.002065	481457.184339	45.525940
3507.346046	481316.956998	45.530945
3507.373728	481186.906791	45.535949
3506.966799	481056.777981	45.540954
3506.960502	480914.278715	45.545959
3506.737800	480778.041806	45.550964
3506.776729	480651.175003	45.555969
3507.040992	480523.762605	45.560973
3506.994236	480401.464740	45.565978
3506.833026	480272.199520	45.570983
3506.851008	480156.520641	45.575988
3507.010867	480022.895776	45.580993
3506.887898	479899.949406	45.585997
3506.996918	479773.874461	45.591002
3507.199571	479635.430041	45.596007
3507.296888	479505.558314	45.601012
3507.127289	479372.693656	45.606017
3507.025804	479238.398849	45.611021
3506.835764	479106.497632	45.616026
3507.025985	478981.668980	45.621031
3506.848247	478859.180538	45.626036
3506.877512	478729.669264	45.631041
3506.725925	478601.808051	45.636045
3506.795841	478485.400833	45.641050
3507.155729	478357.602462	45.646055
3506.779117	478232.106005	45.651060
3506.981800	478106.661664	45.656065
3506.991654	477991.881695	45.661069
3506.908335	477848.004429	45.666074
3506.698408	477722.425370	45.671079
3506.771823	477611.480095	45.676084
3507.001226	477485.672504	45.681089
3506.897466	477359.718403	45.686093
3506.452662	477241.973437	45.691098
3506.874390	477120.940550	45.696103
3506.802837	477001.965764	45.701108
3507.068342	476865.818655	45.706113
3506.750872	476747.593068	45.711117
3507.046174	476619.793568	45.716122
3507.176163	476484.780712	45.721127
3506.460081	476377.507150	45.726132
3506.537237	476251.109461	45.731137
3506.731042	476138.463758	45.736141
3506.505146	476017.837981	45.741146
3506.851683	475897.214947	45.746151
3506.721520	475784.521120	45.751156
3506.741611	475657.167006	45.756161
3507.115798	475541.296752	45.761165
3506.322999	475421.422136	45.766170
3506.648166	475293.709601	45.771175
3506.817939	475190.075675	45.776180
3506.986396	475068.211681	45.781185
3506.793247	474947.877138	45.786189
3506.856966	474826.181346	45.791194
3507.010735	474707.001334	45.796199
3506.674897	474590.841236	45.801204
3506.682874	474462.923923	45.806209
3506.970322	474348.326998	45.811213
3506.887352	474229.690736	45.816218
3506.946902	474096.698050	45.821223
3507.144777	473980.493642	45.826228
3507.158308	473860.471235	45.831233
3506.806599	473732.154524	45.836237
3506.382191	473616.459220	45.841242
3506.587276	473502.377560	45.846247
3506.108683	473380.714238	45.851252
3506.272838	473275.804508	45.856257
3506.490626	473164.655904	45.861261
3506.319572	473048.356735	45.866266
3506.449037	472939.905985	45.871271
3506.314433	472827.093643	45.876276
3506.082145	472711.917005	45.881281
3506.043183	472605.214981	45.886285
3505.998869	472507.274865	45.891290
3506.190028	472407.116281	45.896295
3505.957506	472298.166511	45.901300
3505.874412	472182.657266	45.906305
3506.377156	472084.013779	45.911309
3505.987287	471974.379944	45.916314
3506.226510	471868.588508	45.921319
3505.927160	471774.132085	45.926324
3505.990026	471664.165901	45.931329
3505.858636	471560.512549	45.936333
3505.686504	471459.549921	45.941338
3506.015051	471358.349322	45.946343
3505.689723	471263.135040	45.951348
3506.029227	471157.727669	45.956353
3506.051921	471052.525746	45.961357
3506.063704	470968.749741	45.966362
3506.246425	470854.301224	45.971367
3506.168939	470762.587563	45.976372
3506.171003	470656.677856	45.981377
3506.325956	470549.728443	45.986381
3506.291851	470449.040734	45.991386
3506.071197	470337.443739	45.996391
3506.117528	470234.917721	46.001396
3505.845690	470135.636514	46.006401
3506.284727	470028.483693	46.011405
3505.661463	469935.542255	46.016410
3505.960029	469833.122949	46.021415
3505.720083	469726.945439	46.026420
3505.992909	469641.346138	46.031425
3505.932076	469535.491544	46.036429
3505.900765	469447.208029	46.041434
3505.914464	469348.785704	46.046439
3505.736847	469249.939649	46.051444
3505.896119	469146.881923	46.056449
3506.008986	469051.834953	46.061453
3505.935647	468957.427157	46.066458
3505.970298	468853.679954	46.071463
3505.932650	468756.732323	46.076468
3505.851973	468662.678903	46.081473
3505.816267	468565.071444	46.086477
3505.801498	468480.427824	46.091482
3506.196555	468372.715963	46.096487
3506.045092	468276.646477	46.101492
3505.933997	468173.882931	46.106497
3505.888665	468074.552277	46.111501
3505.713487	467983.753690	46.116506
3505.668116	467882.851673	46.121511
3505.741271	467787.957157	46.126516
3505.797443	467694.331520	46.131521
3505.811689	467599.648760	46.136525
3505.626182	467516.347134	46.141530
3505.660070	467418.975229	46.146535
3505.349212	467340.658793	46.151540
3505.549095	467246.195885	46.156545
3505.700183	467157.819973	46.161549
3505.330409	467078.094060	46.166554
3505.539811	466981.601841	46.171559
3505.547185	466897.656675	46.176564
3505.314443	466812.536293	46.181569
3505.106018	466716.012759	46.186573
3505.513302	466645.220613	46.191578
3505.718086	466551.158738	46.196583
3505.241876	466476.463938	46.201588
3505.636187	466388.144282	46.206593
3505.796279	466301.130754	46.211597
3505.495999	466213.638155	46.216602
3505.356131	466115.985345	46.221607
3505.200506	466024.920842	46.226612
3505.441800	465953.495886	46.231617
3505.462970	465864.629593	46.236621
3505.122315	465779.928373	46.241626
3505.051061	465700.956393	46.246631
3505.092868	465622.572748	46.251636
3505.051421	465547.040164	46.256641
3505.478906	465471.731202	46.261645
3505.079867	465380.249244	46.266650
3505.325054	465295.749861	46.271655
3505.233963	465219.109859	46.276660
3504.804493	465139.487445	46.281665
3505.183806	465055.622755	46.286669
3505.113030	464987.996723	46.291674
3505.568785	464899.862441	46.296679
3505.286105	464829.738770	46.301684
3505.092534	464747.895854	46.306689
3505.448707	464664.844079	46.311693
3505.009955	464592.111569	46.316698
3505.506278	464520.789787	46.321703
3505.250928	464434.700129	46.326708
3505.315627	464356.206123	46.331713
3505.161887	464274.354411	46.336717
3505.019224	464193.007135	46.341722
3504.981374	464107.132226	46.346727
3505.118568	464051.222256	46.351732
3505.026352	463969.764099	46.356737
3504.999633	463891.486500	46.361741
3504.905183	463820.263023	46.366746
3505.153234	463746.751401	46.371751
3505.195772	463666.282335	46.376756
3505.074764	463583.763443	46.381761
3505.019181	463510.404111	46.386765
3504.799988	463442.595373	46.391770
3505.291334	463362.504449	46.396775
3505.414728	463291.951221	46.401780
3504.877350	463212.744700	46.406785
3504.818981	463135.128179	46.411789
3504.974974	463073.891861	46.416794
3504.715083	463002.186948	46.421799
3504.512044	462933.714973	46.426804
3504.816663	462861.254445	46.431809
3505.083937	462791.232223	46.436813
3505.176507	462726.610705	46.441818
3505.181549	462636.414977	46.446823
3504.854113	462568.875049	46.451828
3504.785889	462501.949361	46.456833
3505.351796	462429.239940	46.461837
3504.884028	462358.074881	46.466842
3504.866191	462277.103696	46.471847
3504.920468	462213.095091	46.476852
3505.189504	462147.580109	46.481857
3505.231773	462060.669092	46.486861
3504.695782	461996.000472	46.491866
3505.113285	461918.196543	46.496871
3505.105315	461855.869615	46.501876
3504.984766	461787.987639	46.506881
3505.269292	461708.786733	46.511885
3504.981268	461647.419086	46.516890
3504.760435	461562.527069	46.521895
3505.150690	461493.391364	46.526900
3504.825867	461421.894466	46.531905
3504.847836	461350.084726	46.536909
3504.690746	461283.423440	46.541914
3505.177488	461216.499978	46.546919
3504.869362	461149.712004	46.551924
3504.921050	461081.798191	46.556929
3504.572898	461012.381477	46.561933
3504.363292	460951.251653	46.566938
3504.258802	460884.478689	46.571943
3504.434470	460826.373916	46.576948
3504.442542	460760.290777	46.581953
3505.132193	460695.459302	46.586957
3504.631886	460632.503108	46.591962
3504.843861	460560.810090	46.596967
3504.984324	460499.619101	46.601972
3504.692077	460441.390384	46.606977
3504.807265	460380.659435	46.611981
3504.828708	460311.278512	46.616986
3504.640040	460244.517765	46.621991
3504.643010	460173.771227	46.626996
3504.456857	460122.770344	46.632001
3504.452898	460050.453542	46.637005
3504.669543	459996.798993	46.642010
3504.410459	459927.464626	46.647015
3504.801869	459866.684944	46.652020
3504.671895	459810.149731	46.657025
3505.227575	459736.621311	46.662029
3504.762747	459673.402622	46.667034
3504.641384	459604.144971	46.672039
3504.372829	459547.531315	46.677044
3504.488157	459493.436597	46.682049
3504.260331	459418.165644	46.687053
3504.527587	459367.085409	46.692058
3504.416036	459294.378795	46.697063
3504.741342	459240.146179	46.702068
3504.631176	459183.605806	46.707073
3504.736068	459119.882646	46.712077
3504.341922	459062.427492	46.717082
3504.752057	459000.020202	46.722087
3504.426951	458947.874384	46.727092
3504.441052	458889.943584	46.732097
3504.622254	458826.713269	46.737101
3504.534734	458776.959124	46.742106
3504.618427	458713.390331	46.747111
3504.674461	458652.917624	46.752116
3504.487574	458600.747300	46.757121
3504.555707	458533.683568	46.762125
3504.382936	458470.563246	46.767130
3504.206686	458405.213311	46.772135
3504.137097	458361.232820	46.777140
3503.984258	458311.944811	46.782145
3504.152972	458259.155377	46.787149
3504.199115	458209.427683	46.792154
3504.281876	458157.058116	46.797159
3504.259233	458103.591388	46.802164
3504.055582	458054.970299	46.807169
3504.094502	457993.028719	46.812173
3504.307521	457949.759320	46.817178
3504.358710	457898.256082	46.822183
3504.675457	457841.334928	46.827188
3504.705446	457780.205152	46.832193
3505.023272	457712.842628	46.837197
3504.666222	457663.435842	46.842202
3504.375989	457597.595900	46.847207
3504.464049	457542.740309	46.852212
3504.237221	457490.421865	46.857217
3504.473730	457431.131087	46.862221
3504.315679	457383.869070	46.867226
3504.264480	457321.484648	46.872231
3504.362708	457266.879994	46.877236
3504.465798	457215.670257	46.882241
3504.266587	457164.562691	46.887245
3504.248560	457107.037715	46.892250
3503.886865	457059.454910	46.897255
3503.958138	457011.443268	46.902260
3504.360447	456970.673723	46.907265
3504.218159	456911.598152	46.912269
3504.065713	456865.955908	46.917274
3504.224899	456806.727184	46.922279
3504.167544	456751.387409	46.927284
3504.067951	456714.707251	46.932289
3504.307969	456658.252035	46.937293
3504.101669	456614.949994	46.942298
3504.326217	456568.887905	46.947303
3504.022187	456513.843030	46.952308
3504.073199	456472.068040	46.957313
3504.248035	456420.438544	46.962317
3504.033029	456363.908137	46.967322
3504.206450	456320.946130	46.972327
3504.261707	456273.391656	46.977332
3504.222246	456219.314555	46.982337
3504.311330	456167.800432	46.987341
3504.626773	456120.353238	46.992346
3504.658062	456073.562705	46.997351
3504.341527	456011.371607	47.002356
3504.093200	455962.601037	47.007361
3504.379418	455902.030087	47.012365
3504.106144	455856.811703	47.017370
3504.128288	455805.612221	47.022375
3503.739711	455769.081068	47.027380
3503.908547	455715.778078	47.032385
3503.982068	455663.707756	47.037389
3504.004216	455619.350803	47.042394
3503.766590	455580.461843	47.047399
3503.967170	455535.161837	47.052404
3503.875772	455494.220176	47.057409
3504.283679	455445.944592	47.062413
3504.174765	455411.646071	47.067418
3504.065269	455355.398977	47.072423
3504.195074	455306.765029	47.077428
3504.280270	455254.945117	47.082433
3504.564079	455205.524284	47.087437
3504.035176	455152.643092	47.092442
3503.889746	455111.050913	47.097447
3503.929070	455058.934193	47.102452
3503.789365	455023.018181	47.107457
3503.988130	454974.270285	47.112461
3503.806189	454936.789923	47.117466
3504.061454	454883.976907	47.122471
3503.973290	454842.374402	47.127476
3504.088908	454812.953558	47.132481
3504.011139	454759.842246	47.137485
3504.012226	454719.998443	47.142490
3504.277977	454664.344359	47.147495
3503.877125	454626.191125	47.152500
3504.115249	454575.864121	47.157505
3504.225367	454541.729506	47.162509
3503.850635	454490.746557	47.167514
3503.690603	454455.948237	47.172519
3503.867130	454411.866451	47.177524
3503.801499	454366.457228	47.182529
3504.075443	454323.828691	47.187533
3504.124393	454278.653171	47.192538
3503.722667	454240.195210	47.197543
3503.688041	454199.342642	47.202548
3503.574039	454165.904669	47.207553
3503.769210	454122.275309	47.212557
3503.611090	454081.646362	47.217562
3503.868157	454044.038714	47.222567
3503.907223	454013.514547	47.227572
3503.656363	453975.435873	47.232577
3503.781006	453923.859317	47.237581
3503.841328	453894.395900	47.242586
3504.417337	453844.516343	47.247591
3504.199124	453798.067351	47.252596
3504.112046	453760.365862	47.257601
3504.293552	453712.327618	47.262605
3504.327207	453681.195556	47.267610
3504.649267	453615.238161	47.272615
3504.596631	453560.902792	47.277620
3503.915792	453515.140477	47.282625
3503.884787	453462.930313	47.287629
3503.987784	453421.647144	47.292634
3504.167983	453380.806961	47.297639
3503.949550	453342.518798	47.302644
3503.913335	453306.683494	47.307649
3504.118909	453257.727573	47.312653
3503.953508	453216.388429	47.317658
3503.825237	453155.322470	47.322663
3504.136069	453126.271437	47.327668
3503.986454	453099.174704	47.332673
3504.188465	453058.228767	47.337677
3503.773562	453012.014361	47.342682
3503.793986	452966.029697	47.347687
3503.966104	452932.540864	47.352692
3503.682203	452897.558268	47.357697
3503.643430	452855.487037	47.362701
3503.700426	452813.450065	47.367706
3503.528141	452778.955170	47.372711
3503.834564	452752.996823	47.377716
3503.858158	452720.800407	47.382721
3503.610052	452674.962336	47.387725
3503.748961	452647.105997	47.392730
3503.680184	452599.614856	47.397735
3503.905667	452562.567557	47.402740
3503.626418	452528.039809	47.407745
3503.709549	452473.475604	47.412749
3503.601256	452455.851267	47.417754
3503.572716	452421.432626	47.422759
3504.039350	452372.886305	47.427764
3503.540403	452351.272817	47.432769
3503.703566	452309.825058	47.437773
3503.389139	452263.693213	47.442778
3503.453177	452248.168563	47.447783
3503.520033	452212.719339	47.452788
3503.312690	452178.178728	47.457793
3503.648110	452142.531437	47.462797
3503.665535	452123.922098	47.467802
3503.548611	452087.084503	47.472807
3503.697219	452040.619613	47.477812
3503.515823	452021.232963	47.482817
3503.763323	451983.116212	47.487821
3503.963795	451944.500439	47.492826
3503.867080	451916.835443	47.497831
3503.586551	451875.766760	47.502836
3503.409914	451843.298977	47.507841
3503.659828	451810.656916	47.512845
3503.521506	451774.278704	47.517850
3503.561611	451732.394514	47.522855
3503.718078	451704.026923	47.527860
3503.425608	451670.615372	47.532865
3503.565481	451627.598563	47.537869
3503.422813	451606.937441	47.542874
3503.520769	451586.336612	47.547879
3503.549356	451548.205740	47.552884
3503.338038	451511.535336	47.557889
3503.674657	451482.224099	47.562893
3503.331546	451468.137260	47.567898
3503.406548	451428.173070	47.572903
3503.642187	451397.915668	47.577908
3503.401294	451382.898729	47.582913
3503.634703	451351.779749	47.587917
3503.412457	451312.423783	47.592922
3503.381346	451278.966976	47.597927
3503.374550	451252.046236	47.602932
3503.280276	451235.685962	47.607937
3503.610666	451196.894518	47.612941
3503.363095	451172.752581	47.617946
3503.421222	451140.091513	47.622951
3504.069700	451109.560403	47.627956
3503.620719	451080.737635	47.632961
3503.635404	451043.774317	47.637965
3503.420973	451019.322341	47.642970
3503.559929	450977.369052	47.647975
3503.629578	450947.798442	47.652980
3503.427945	450933.636384	47.657985
3503.716620	450880.097606	47.662989
3503.447384	450859.102445	47.667994
3503.405044	450835.482783	47.672999
3503.378692	450810.795646	47.678004
3503.494550	450768.288170	47.683009
3503.734789	450741.172488	47.688013
3503.708907	450720.338441	47.693018
3503.617941	450675.483139	47.698023
3503.832292	450646.495811	47.703028
3503.681437	450619.649551	47.708033
3503.613934	450567.945332	47.713037
3503.357793	450547.657442	47.718042
3503.212992	450524.359131	47.723047
3503.687346	450497.051054	47.728052
3503.493385	450455.609873	47.733057
3503.197838	450426.861404	47.738061
3503.270911	450414.933669	47.743066
3503.472941	450393.198451	47.748071
3503.258324	450345.220035	47.753076
3503.455566	450326.172770	47.758081
3503.355818	450294.297864	47.763085
3503.642027	450279.392939	47.768090
3503.336866	450242.381406	47.773095
3503.530107	450210.152134	47.778100
3503.327343	450189.550567	47.783105
3503.166869	450164.885567	47.788109
3503.158467	450150.182959	47.793114
3502.882009	450107.842528	47.798119
3503.558500	450075.631943	47.803124
3503.234342	450063.163400	47.808129
3503.434925	450037.422548	47.813133
3503.377963	450030.739177	47.818138
3503.231651	449998.314040	47.823143
3503.244610	449959.726606	47.828148
3503.272128	449945.068424	47.833153
3503.359297	449915.696174	47.838157
3503.225812	449906.237163	47.843162
3503.227812	449881.645493	47.848167
3503.327967	449844.665459	47.853172
3502.827450	449823.810151	47.858177
3502.966703	449794.124618	47.863181
3503.209085	449780.392998	47.868186
3503.059157	449758.666512	47.873191
3503.308973	449742.804055	47.878196
3503.006859	449737.379330	47.883201
3503.218555	449709.151709	47.888205
3502.970282	449681.509620	47.893210
3503.161378	449655.465698	47.898215
3503.331875	449631.605521	47.903220
3502.963897	449624.214567	47.908225
3503.372496	449603.254520	47.913229
3503.650798	449591.849018	47.918234
3503.149430	449562.171129	47.923239
3503.228062	449536.602597	47.928244
3503.067092	449514.319999	47.933249
3502.776326	449493.986293	47.938253
3502.932322	449483.615696	47.943258
3503.057061	449476.901124	47.948263
3503.471038	449446.813266	47.953268
3503.216545	449430.225412	47.958273
3503.017202	449394.005579	47.963277
3503.229486	449366.842187	47.968282
3502.974669	449349.443055	47.973287
3502.714732	449330.016605	47.978292
3502.796979	449325.388122	47.983297
3502.820987	449305.608942	47.988301
3502.861931	449296.373395	47.993306
3502.694215	449282.356539	47.998311
3503.289358	449257.612159	48.003316
3502.993778	449248.484754	48.008321
3503.234420	449237.389718	48.013325
3503.161513	449230.404586	48.018330
3503.286944	449185.458439	48.023335
3503.122498	449153.440729	48.028340
3502.826649	449140.155523	48.033345
3503.131099	449124.029747	48.038349
3502.810620	449118.709406	48.043354
3502.569136	449098.721837	48.048359
3503.050849	449067.759886	48.053364
3502.699001	449063.002644	48.058369
3502.814378	449045.033001	48.063373
3502.994943	449040.489079	48.068378
3502.999968	449031.208844	48.073383
3502.895774	449015.203462	48.078388
3502.541179	449005.477564	48.083393
3502.877881	448997.560430	48.088397
3502.767464	448983.482885	48.093402
3502.955722	448967.934586	48.098407
3503.064984	448948.140513	48.103412
3502.828849	448942.552200	48.108417
3502.633515	448918.195917	48.113421
3503.049303	448911.127239	48.118426
3503.022245	448900.229849	48.123431
3503.122936	448872.222879	48.128436
3502.925190	448846.954225	48.133441
3502.765711	448815.239386	48.138445
3503.240556	448812.622691	48.143450
3503.075069	448797.185371	48.148455
3503.093046	448780.347659	48.153460
3502.754712	448770.770994	48.158465
3502.861490	448762.893028	48.163469
3502.882063	448739.513790	48.168474
3502.880388	448724.403388	48.173479
3502.656568	448719.725619	48.178484
3502.509567	448715.744616	48.183489
3502.952946	448698.834205	48.188493
3503.085555	448681.824724	48.193498
3502.708215	448670.682786	48.198503
3503.043313	448657.695195	48.203508
3502.645325	448646.201827	48.208513
3502.694450	448622.614760	48.213517
3502.633316	448613.447049	48.218522
3502.625046	448603.763245	48.223527
3503.021289	448592.387772	48.228532
3502.832621	448583.698179	48.233537
3502.927444	448563.601973	48.238541
3502.996492	448559.076989	48.243546
3502.764489	448549.837012	48.248551
3503.124963	448528.731995	48.253556
3503.041244	448521.494942	48.258561
3502.747002	448515.561492	48.263565
3502.808694	448504.243092	48.268570
3502.735108	448485.240401	48.273575
3502.893673	448474.564630	48.278580
3502.647590	448475.569735	48.283585
3502.969558	448457.361493	48.288589
3502.951177	448441.797382	48.293594
3502.862083	448414.329274	48.298599
3503.128423	448386.800443	48.303604
3502.582593	448374.267329	48.308609
3502.577342	448363.923712	48.313613
3502.850891	448349.932305	48.318618
3502.736708	448344.170890	48.323623
3503.108731	448324.483489	48.328628
3503.270818	448329.019096	48.333633
3503.316067	448303.150526	48.338637
3503.140133	448292.126120	48.343642
3503.072977	448284.581916	48.348647
3503.281062	448273.238397	48.353652
3503.130513	448250.496319	48.358657
3503.379483	448222.868827	48.363661
3503.385486	448194.167225	48.368666
3502.911181	448176.652476	48.373671
3503.372723	448165.164210	48.378676
3502.934184	448162.601975	48.383681
3503.035419	448144.532566	48.388685
3503.353983	448120.391861	48.393690
3503.361927	448098.535289	48.398695
3503.257371	448058.291089	48.403700
3503.053312	448060.201772	48.408705
3503.411175	448055.120293	48.413709
3502.806532	448036.461409	48.418714
3502.581466	448025.191714	48.423719
3502.849011	448010.186957	48.428724
3502.943917	448006.925130	48.433729
3502.557792	447999.638116	48.438733
3502.684732	447983.389655	48.443738
3502.627344	447985.833088	48.448743
3502.883036	447963.021337	48.453748
3502.971344	447958.340813	48.458753
3503.252596	447944.094285	48.463757
3503.008411	447912.544675	48.468762
3502.763497	447890.578938	48.473767
3502.866745	447868.807273	48.478772
3502.802068	447866.637539	48.483777
3503.125687	447849.189111	48.488781
3503.171743	447845.580644	48.493786
3502.968376	447831.112536	48.498791
3502.965342	447811.539405	48.503796
3502.937135	447811.188929	48.508801
3502.900117	447799.075677	48.513805
3503.097112	447786.922463	48.518810
3503.009617	447774.969940	48.523815
3502.887605	447761.502057	48.528820
3502.834396	447746.196921	48.533825
3502.828976	447743.611391	48.538829
3502.791141	447734.692862	48.543834
3502.857079	447731.943021	48.548839
3502.869060	447705.927276	48.553844
3502.922027	447684.671090	48.558849
3502.644683	447665.854577	48.563853
3502.786701	447655.789720	48.568858
3502.228419	447655.276205	48.573863
3502.727866	447653.212964	48.578868
3502.527697	447655.427270	48.583873
3502.827793	447641.329447	48.588877
3502.849604	447640.209801	48.593882
3502.680468	447625.735708	48.598887
3502.789498	447613.141036	48.603892
3502.581531	447615.103135	48.608897
3502.683717	447595.917508	48.613901
3502.721341	447585.515482	48.618906
3502.574034	447582.649906	48.623911
3502.816773	447565.113637	48.628916
3502.675614	447564.021813	48.633921
3502.828560	447544.573929	48.638925
3502.952221	447537.858926	48.643930
3502.824930	447531.085352	48.648935
3502.961180	447528.779859	48.653940
3502.994757	447519.291250	48.658945
3503.106215	447500.408205	48.663949
3502.985297	447496.371809	48.668954
3502.904493	447491.567930	48.673959
3502.932512	447471.583511	48.678964
3503.127402	447474.034637	48.683969
3503.145434	447447.003363	48.688973
3503.243323	447421.936071	48.693978
3502.872888	447408.814634	48.698983
3503.044862	447394.130014	48.703988
3502.803626	447381.595010	48.708993
3502.939736	447375.587758	48.713997
3503.366804	447368.060261	48.719002
3502.997615	447361.530771	48.724007
3503.171821	447340.202831	48.729012
3503.297348	447317.615448	48.734017
3502.812944	447297.464811	48.739021
3502.909322	447275.338745	48.744026
3502.751067	447265.578519	48.749031
3503.231475	447250.942557	48.754036
3502.744097	447246.715135	48.759041
3503.095269	447236.766497	48.764045
3502.646924	447220.362130	48.769050
3502.484687	447218.918920	48.774055
3503.326905	447204.018312	48.779060
3503.100496	447195.436010	48.784065
3502.520229	447189.094634	48.789069
3502.727444	447179.069130	48.794074
3502.545333	447175.448797	48.799079
3502.907986	447162.455587	48.804084
3502.923114	447164.937442	48.809089
3502.619865	447144.603599	48.814093
3503.018616	447139.210664	48.819098
3502.648628	447145.307954	48.824103
3502.659515	447109.859661	48.829108
3502.903850	447115.344973	48.834113
3502.739774	447109.186061	48.839117
3502.612097	447093.538201	48.844122
3502.373570	447082.118173	48.849127
3502.665071	447077.453471	48.854132
3502.572040	447075.846305	48.859137
3502.521610	447054.049334	48.864141
3502.598102	447050.638375	48.869146
3502.564408	447065.451082	48.874151
3503.070389	447074.035742	48.879156
3502.503530	447075.754909	48.884161
3502.670964	447063.707748	48.889165
3502.851788	447062.358082	48.894170
3502.335077	447051.695473	48.899175
3502.909696	447048.909402	48.904180
3502.836679	447041.112206	48.909185
3503.205921	447030.856127	48.914189
3503.321646	447008.117960	48.919194
3502.911711	446986.027331	48.924199
3503.065434	446957.248123	48.929204
3502.794943	446958.054624	48.934209
3503.086949	446942.842097	48.939213
3503.152418	446938.520220	48.944218
3502.889208	446937.753463	48.949223
3503.240306	446917.155548	48.954228
3503.082166	446907.547269	48.959233
3503.025561	446909.128616	48.964237
3503.091456	446888.832922	48.969242
3502.924830	446865.990681	48.974247
3502.914282	446838.557829	48.979252
3503.075310	446823.823975	48.984257
3503.026424	446813.385631	48.989261
3502.761059	446805.773322	48.994266
3502.952127	446810.101466	48.999271
3503.022238	446793.202562	49.004276
3502.716781	446797.412644	49.009281
3502.565338	446782.225007	49.014285
3503.082324	446767.937443	49.019290
3502.717605	446764.094665	49.024295
3502.812174	446754.493879	49.029300
3502.751348	446748.773629	49.034305
3502.591724	446735.869334	49.039309
3502.962213	446736.769244	49.044314
3502.698412	446725.809735	49.049319
3502.923626	446706.450167	49.054324
3502.642979	446707.968362	49.059329
3502.713336	446700.805800	49.064333
3503.086106	446680.964619	49.069338
3502.784085	446688.774601	49.074343
3502.749132	446667.988807	49.079348
3503.068907	446660.276538	49.084353
3502.932915	446659.183784	49.089357
3502.910206	446646.915299	49.094362
3503.077887	446642.322355	49.099367
3503.414953	446622.436505	49.104372
3503.420291	446601.593056	49.109377
3502.859091	446570.602687	49.114381
3503.022045	446564.692046	49.119386
3502.808464	446559.504938	49.124391
3503.059752	446543.690546	49.129396
3502.564486	446538.044416	49.134401
3502.618163	446536.260027	49.139405
3502.833659	446528.362670	49.144410
3502.535650	446526.181927	49.149415
3502.866367	446507.108432	49.154420
3502.864994	446505.891262	49.159425
3502.657179	446502.731604	49.164429
3503.009601	446484.364339	49.169434
3502.829928	446489.770075	49.174439
3502.756217	446477.155221	49.179444
3502.940623	446472.660808	49.184449
3502.806266	446453.108848	49.189453
3502.848099	446454.267731	49.194458
3502.839118	446449.248507	49.199463
3502.945420	446431.328911	49.204468
3502.896503	446427.787131	49.209473
3502.515077	446418.926714	49.214477
3503.046819	446411.634567	49.219482
3502.855799	446405.530763	49.224487
3502.885463	446394.470265	49.229492
3503.169705	446397.869778	49.234497
3503.057971	446390.028243	49.239501
3502.934200	446379.551761	49.244506
3502.703392	446375.026798	49.249511
3502.911896	446358.154632	49.254516
3502.826243	446360.045249	49.259521
3502.870969	446342.795342	49.264525
3502.936139	446312.509036	49.269530
3502.421070	446301.642922	49.274535
3502.902153	446308.812217	49.279540
3502.831131	446314.300869	49.284545
3502.917605	446304.244858	49.289549
3503.014163	446273.040326	49.294554
3502.726062	446272.480641	49.299559
3502.451060	446255.335966	49.304564
3502.844599	446261.100294	49.309569
3502.663568	446252.256304	49.314573
3502.814417	446243.812051	49.319578
3502.605905	446262.255704	49.324583
3502.761228	446255.839163	49.329588
3502.640742	446256.366518	49.334593
3502.653405	446237.144240	49.339597
3502.931237	446228.729012	49.344602
3502.619371	446233.193857	49.349607
3502.653272	446217.669900	49.354612
3502.828742	446219.211674	49.359617
3502.072177	446215.486412	49.364621
3502.616080	446209.662766	49.369626
3502.510041	446192.539903	49.374631
3502.218865	446177.071420	49.379636
3502.274521	446185.986891	49.384641
3502.816519	446208.815813	49.389645
3502.777678	446211.205569	49.394650
3502.553369	446210.533567	49.399655
3502.862406	446198.867436	49.404660
3502.811265	446198.368714	49.409665
3502.546546	446186.191996	49.414669
3502.825985	446177.624338	49.419674
3502.602692	446183.240446	49.424679
3502.592885	446168.383172	49.429684
3502.421085	446168.057186	49.434689
3502.605339	446152.051102	49.439693
3503.059791	446147.713362	49.444698
3502.809747	446146.893614	49.449703
3502.868622	446135.929419	49.454708
3502.857670	446128.679125	49.459713
3502.843005	446121.835159	49.464717
3502.608167	446111.022524	49.469722
3502.887982	446110.365867	49.474727
3502.712534	446101.216588	49.479732
3502.785189	446097.096162	49.484737
3502.797963	446095.318720	49.489741
3502.898799	446084.702319	49.494746
3502.469695	446092.635641	49.499751
3502.893036	446070.858196	49.504756
3502.891816	446071.365192	49.509761
3502.320533	446069.028211	49.514765
3502.756548	446053.486190	49.519770
3502.664393	446054.465123	49.524775
3502.970412	446041.176629	49.529780
3502.698824	446035.492173	49.534785
3502.388522	446038.891833	49.539789
3503.139365	446032.627107	49.544794
3502.502380	446024.165146	49.549799
3502.725951	446014.795564	49.554804
3502.781746	446008.497367	49.559809
3502.566693	446007.823777	49.564813
3502.640935	445999.341795	49.569818
3502.674075	446000.299338	49.574823
3502.507537	445981.563838	49.579828
3502.874093	446002.445150	49.584833
3502.643404	446009.482514	49.589837
3502.783216	446002.105010	49.594842
3502.669247	446006.130414	49.599847
3502.668258	445992.590034	49.604852
3502.841508	445989.669510	49.609857
3502.531593	445992.156287	49.614861
3502.725156	445990.094406	49.619866
3502.592033	445981.394261	49.624871
3502.750003	445963.465450	49.629876
3502.658021	445965.813595	49.634881
3502.518072	445959.954506	49.639885
3502.856612	445944.682612	49.644890
3502.400539	445946.839361	49.649895
3502.612501	445944.622197	49.654900
3502.705466	445929.950060	49.659905
3502.612129	445927.176469	49.664909
3502.704271	445930.710283	49.669914
3502.875620	445922.515966	49.674919
3503.011858	445910.118493	49.679924
3502.534862	445906.142591	49.684929
3502.458939	445902.098208	49.689933
3502.840053	445889.506776	49.694938
3502.329529	445894.259173	49.699943
3502.259702	445911.310208	49.704948
3502.765488	445916.599052	49.709953
3502.498720	445917.962793	49.714957
3502.420943	445904.334043	49.719962
3502.627048	445913.274652	49.724967
3502.665239	445895.163385	49.729972
3502.652012	445895.925999	49.734977
3502.554307	445892.595311	49.739981
3502.904549	445880.465558	49.744986
3502.517423	445879.263504	49.749991
3502.793108	445870.189237	49.754996
3502.767792	445856.652925	49.760001
3502.453802	445861.726762	49.765005
3502.940888	445867.627364	49.770010
3502.582800	445877.222159	49.775015
3502.647887	445875.435767	49.780020
3502.299263	445874.277852	49.785025
3502.532750	445877.280413	49.790029
3502.476041	445863.039487	49.795034
3502.616007	445871.737843	49.800039
3502.412166	445863.861128	49.805044
3502.506481	445852.687885	49.810049
3502.582855	445854.348031	49.815053
3503.154282	445836.500659	49.820058
3502.835932	445837.416797	49.825063
3502.813934	445832.551789	49.830068
3502.892857	445831.980138	49.835073
3502.342318	445830.501706	49.840077
3502.501825	445820.027295	49.845082
3502.138299	445832.970086	49.850087
3502.448203	445841.842289	49.855092
3502.535906	445847.861800	49.860097
3502.499128	445851.366926	49.865101
3502.599060	445839.837729	49.870106
3502.440865	445838.140169	49.875111
3502.905580	445822.491656	49.880116
3503.245660	445819.238347	49.885121
3502.905733	445819.904605	49.890125
3502.978138	445811.270724	49.895130
3502.976278	445813.400647	49.900135
3502.950503	445799.255822	49.905140
3503.079439	445798.574206	49.910145
3502.710678	445794.985505	49.915149
3502.469022	445778.849011	49.920154
3502.159710	445780.422877	49.925159
3502.433403	445769.472528	49.930164
3502.802333	445760.990850	49.935169
3502.456958	445759.477382	49.940173
3502.583608	445749.211399	49.945178
3502.527111	445756.827660	49.950183
3502.850280	445775.282378	49.955188
3502.426459	445769.015288	49.960193
3502.585053	445775.580559	49.965197
3502.662852	445774.755533	49.970202
3502.777133	445773.772140	49.975207
3502.530959	445766.764737	49.980212
3502.735002	445760.238303	49.985217
3502.581683	445759.959868	49.990221
3502.745185	445746.695526	49.995226
3502.686298	445745.538846	50.000231
3502.658477	445737.429178	50.005236
3502.736926	445735.944771	50.010241
3502.466343	445728.738670	50.015245
3502.710363	445726.871001	50.020250
3502.371930	445727.232729	50.025255
3502.505905	445716.306209	50.030260
3502.506377	445725.991990	50.035265
3502.536971	445740.591788	50.040269
3502.872137	445738.911410	50.045274
3502.731023	445741.014403	50.050279
3502.833113	445733.389682	50.055284
3503.013134	445735.539271	50.060289
3502.702801	445731.484167	50.065293
3502.915932	445716.081383	50.070298
3502.741305	445719.711493	50.075303
3503.194387	445707.665510	50.080308
3503.307390	445681.224338	50.085313
3502.911609	445664.759082	50.090317
3503.170949	445648.486235	50.095322
3502.838083	445643.674263	50.100327
3502.850692	445636.926911	50.105332
3503.205905	445638.793031	50.110337
3503.015500	445637.303808	50.115341
3503.092193	445619.236448	50.120346
3503.221116	445622.814745	50.125351
3503.236069	445598.165178	50.130356
3503.202412	445572.154620	50.135361
3502.930132	445573.062903	50.140365
3502.858652	445549.239451	50.145370
3502.791894	445558.378939	50.150375
3502.489089	445548.135471	50.155380
3502.473028	445542.102974	50.160385
3502.662861	445547.648710	50.165389
3502.810181	445525.309279	50.170394
3502.577474	445522.356578	50.175399
3502.424442	445519.035278	50.180404
3502.935577	445541.008054	50.185409
3502.823735	445539.201129	50.190413
3502.579363	445530.114086	50.195418
3502.396626	445540.490508	50.200423
3502.425229	445538.862458	50.205428
3502.834425	445541.125077	50.210433
3502.643086	445538.114602	50.215437
3502.737970	445523.796854	50.220442
3502.706286	445523.497648	50.225447
3502.827241	445520.230994	50.230452
3502.801201	445517.902282	50.235457
3502.592012	445509.975636	50.240461
3502.637066	445502.664853	50.245466
3502.656922	445508.746757	50.250471
3502.743462	445494.024705	50.255476
3502.940313	445495.461455	50.260481
3502.930341	445487.703640	50.265485
3502.745020	445479.164343	50.270490
3503.017094	445479.472549	50.275495
3503.055260	445472.162932	50.280500
3502.801411	445463.736757	50.285505
3502.718204	445468.771283	50.290509
3502.516631	445461.046172	50.295514
3502.752168	445455.072120	50.300519
3502.682531	445449.657308	50.305524
3502.546399	445442.580296	50.310529
3502.791165	445438.278216	50.315533
3502.850912	445432.841309	50.320538
3502.869256	445437.300652	50.325543
3502.667955	445428.510494	50.330548
3503.250637	445416.442221	50.335553
3502.811222	445421.081152	50.340557
3502.704383	445414.303412	50.345562
3502.576784	445416.150560	50.350567
3502.499610	445403.890661	50.355572
3502.731570	445402.684303	50.360577
3502.240209	445399.927889	50.365581
3502.613903	445387.489572	50.370586
3502.467206	445392.179958	50.375591
3502.280786	445405.853474	50.380596
3502.808033	445411.240208	50.385601
3502.574167	445417.872597	50.390605
3502.647763	445409.390492	50.395610
3502.612949	445406.657556	50.400615
3502.579233	445410.415800	50.405620
3502.796500	445407.335540	50.410625
3502.326675	445396.410523	50.415629
3502.791225	445390.143782	50.420634
3502.771295	445392.581114	50.425639
3502.627071	445394.177534	50.430644
3502.746885	445381.224708	50.435649
3502.645357	445375.206756	50.440653
3502.866438	445373.850113	50.445658
3502.648911	445371.706221	50.450663
3502.704615	445364.241431	50.455668
3503.127916	445352.961044	50.460673
3502.618980	445357.916143	50.465677
3502.841311	445343.576514	50.470682
3502.956338	445335.594446	50.475687
3502.517802	445333.031860	50.480692
3502.702410	445335.079278	50.485697
3502.483784	445333.949850	50.490701
3503.046702	445322.797750	50.495706
3502.949201	445330.573305	50.500711
3502.769921	445320.055068	50.505716
3502.880947	445310.957965	50.510721
3502.232460	445311.119067	50.515725
3502.677381	445307.847782	50.520730
3502.626846	445303.494667	50.525735
3502.506519	445288.452796	50.530740
3502.865439	445252.739142	50.535745
3502.789093	445207.261176	50.540749
3502.980481	445137.394480	50.545754
3502.353717	445076.593018	50.550759
3502.575180	445001.598570	50.555764
3502.698771	444901.060223	50.560769
3502.228061	444813.200255	50.565773
3502.548469	444696.246325	50.570778
3502.822595	444576.358149	50.575783
3502.702636	444440.408881	50.580788
3502.507847	444285.097854	50.585793
3502.336377	444131.962551	50.590797
3502.481593	443963.759802	50.595802
3502.541054	443784.919686	50.600807
3502.349811	443592.274866	50.605812
3502.955015	443377.784803	50.610817
3502.438212	443165.056485	50.615821
3502.439752	442929.819514	50.620826
3502.770394	442684.836251	50.625831
3502.471216	442431.994606	50.630836
3502.715013	442166.934907	50.635841
3502.373517	441892.436182	50.640845
3502.319444	441591.762741	50.645850
3502.240091	441304.277577	50.650855
3502.167717	440983.715335	50.655860
3502.188500	440653.444057	50.660865
3502.203181	440324.589186	50.665869
3502.102609	439977.284665	50.670874
3501.993587	439615.062310	50.675879
3502.125669	439229.001361	50.680884
3502.306647	438837.345152	50.685889
3501.984020	438440.339926	50.690893
3502.090329	438024.839075	50.695898
3501.925477	437595.882116	50.700903
3501.913702	437156.439832	50.705908
3501.855243	436688.585928	50.710913
3501.719110	436227.534051	50.715917
3501.281395	435740.090768	50.720922
3501.358745	435242.908978	50.725927
3501.423445	434739.782076	50.730932
3501.677735	434201.499970	50.735937
3501.489408	433668.862226	50.740941
3501.739141	433097.370478	50.745946
3501.586304	432537.705677	50.750951
3501.228026	431946.550059	50.755956
3501.805631	431337.154030	50.760961
3501.379054	430719.032712	50.765965
3501.453533	430068.685608	50.770970
3501.410648	429407.987457	50.775975
3501.393321	428732.700680	50.780980
3501.298050	428043.755325	50.785985
3501.545855	427340.824619	50.790989
3501.765909	426593.517118	50.795994
3501.674010	425854.462225	50.800999
3500.897804	425077.330461	50.806004
3501.364446	424289.707709	50.811009
3500.975855	423489.159377	50.816013
3501.035412	422661.196991	50.821018
3500.861776	421813.802984	50.826023
3500.523879	420962.549447	50.831028
3500.528024	420083.538743	50.836033
3500.076061	419192.821223	50.841037
3500.399101	418275.791372	50.846042
3500.314928	417356.131881	50.851047
3500.667650	416405.872715	50.856052
3500.629789	415427.462387	50.861057
3500.199843	414440.144131	50.866061
3499.925747	413435.190499	50.871066
3500.341005	412400.294817	50.876071
3500.124547	411348.782416	50.881076
3499.916244	410279.704298	50.886081
3499.649988	409200.282259	50.891085
3499.781617	408084.126633	50.896090
3499.543460	406947.466395	50.901095
3499.060191	405808.158753	50.906100
3499.128615	404640.058262	50.911105
3498.835016	403465.137060	50.916109
3498.744760	402258.658186	50.921114
3498.669082	401043.792464	50.926119
3498.641244	399801.124738	50.931124
3498.414553	398537.248533	50.936129
3497.976967	397257.371919	50.941133
3497.636097	395964.337227	50.946138
3497.569909	394658.824301	50.951143
3497.419524	393331.542474	50.956148
3497.434812	391983.463178	50.961153
3497.207222	390629.697989	50.966157
3496.816648	389234.959417	50.971162
3496.459839	387849.072181	50.976167
3496.382609	386435.448504	50.981172
3496.033656	385000.508239	50.986177
3495.789440	383555.902601	50.991181
3495.770849	382102.042512	50.996186
3495.626914	380621.269513	51.001191
3495.203602	379126.877018	51.006196
3494.960054	377619.675393	51.011201
3494.918387	376097.778632	51.016205
3494.915351	374552.899595	51.021210
3494.372942	372996.093377	51.026215
3494.091647	371416.034698	51.031220
3494.187163	369818.702723	51.036225
3493.806481	368212.531781	51.041229
3493.778574	366581.486114	51.046234
3493.497923	364948.657063	51.051239
3493.037354	363294.678745	51.056244
3493.028766	361628.852122	51.061249
3492.541013	359938.821833	51.066253
3492.458783	358231.684124	51.071258
3492.149471	356514.871931	51.076263
3491.598825	354778.034376	51.081268
3491.730303	353031.111901	51.086273
3491.138603	351271.418904	51.091277
3490.919109	349492.916599	51.096282
3490.855092	347706.097880	51.101287
3490.694405	345896.554391	51.106292
3490.482801	344078.754885	51.111297
3489.966268	342252.539678	51.116301
3489.732507	340402.490262	51.121306
3489.203774	338559.266273	51.126311
3489.258765	336690.019048	51.131316
3489.079507	334806.339090	51.136321
3488.524825	332897.841497	51.141325
3488.016706	330985.323008	51.146330
3487.801508	329069.760924	51.151335
3487.457976	327141.327503	51.156340
3487.154627	325190.169366	51.161345
3486.689904	323240.349401	51.166349
3486.720155	321263.960454	51.171354
3485.991694	319272.722063	51.176359
3485.954335	317284.385101	51.181364
3485.881893	315270.003359	51.186369
3485.208463	313260.655788	51.191373
3484.697723	311221.284808	51.196378
3484.551339	309185.996853	51.201383
3483.848246	307133.335871	51.206388
3483.932569	305060.807087	51.211393
3483.221582	302991.800484	51.216397
3482.704794	300910.541266	51.221402
3482.291017	298817.632004	51.226407
3482.238056	296714.252382	51.231412
3482.306070	294592.525764	51.236417
3481.281413	292477.717363	51.241421
3480.998991	290331.905291	51.246426
3480.640718	288188.589219	51.251431
3480.086255	286042.037032	51.256436
3479.701906	283863.641214	51.261441
3478.926175	281696.154651	51.266445
3478.945715	279509.810996	51.271450
3478.374984	277324.789220	51.276455
3477.993594	275115.287939	51.281460
3477.870845	272903.733917	51.286465
3477.521999	270689.295684	51.291469
3476.951641	268454.606040	51.296474
3476.694316	266204.542239	51.301479
3476.355490	263956.747093	51.306484
3475.636044	261692.198882	51.311489
3474.618711	259426.676400	51.316493
3474.238570	257151.949389	51.321498
3473.788475	254875.043329	51.326503
3473.035640	252601.425572	51.331508
3472.892633	250308.047354	51.336513
3472.373528	248012.602104	51.341517
3471.662068	245699.373255	51.346522
3471.301217	243389.562354	51.351527
3470.947533	241084.886372	51.356532
3470.421996	238757.925111	51.361537
3469.774607	236425.965783	51.366541
3469.315609	234085.749880	51.371546
3468.725842	231741.664603	51.376551
3467.974455	229394.839026	51.381556
3467.868467	227028.356878	51.386561
3467.152732	224687.866286	51.391565
3466.770798	222319.350400	51.396570
3465.921752	219938.814922	51.401575
3465.168854	217564.323151	51.406580
3464.958198	215186.966174	51.411585
3464.385553	212805.807016	51.416589
3463.848136	210408.127044	51.421594
3463.346781	208012.211683	51.426599
3462.453784	205619.817560	51.431604
3461.966933	203208.840093	51.436609
3461.230499	200793.704081	51.441613
3460.441947	198374.494220	51.446618
3460.359941	195961.280264	51.451623
3459.289824	193552.865253	51.456628
3458.879555	191132.730483	51.461633
3458.025719	188712.574331	51.466637
3457.357310	186282.900788	51.471642
3457.105480	183855.751911	51.476647
3455.839862	181428.741017	51.481652
3455.236387	178988.440779	51.486657
3454.297264	176565.946590	51.491661
3453.821199	174143.946314	51.496666
3453.138679	171704.618440	51.501671
3452.353093	169280.596714	51.506676
3451.781873	166842.275909	51.511681
3450.934870	164419.690481	51.516685
3450.140555	161990.779414	51.521690
3449.665212	159560.411523	51.526695
3448.793810	157127.364523	51.531700
3447.893912	154690.307887	51.536705
3447.011131	152260.263892	51.541709
3446.413684	149833.781004	51.546714
3445.644340	147404.264510	51.551719
3444.859940	144994.184064	51.556724
3444.105316	142581.701982	51.561729
3443.112145	140083.153140	51.566733
3442.274540	137660.990300	51.571738
3441.407082	135252.185196	51.576743
3440.536243	132846.756392	51.581748
3439.676990	130435.057694	51.586753
3438.713890	128042.161847	51.591757
3437.814950	125653.883320	51.596762
3437.125302	123262.512289	51.601767
3435.765438	120880.603546	51.606772
3435.231082	118490.967862	51.611777
3433.794996	116115.882239	51.616781
3432.973305	113748.075910	51.621786
3432.238194	111388.682009	51.626791
3431.202604	109051.458593	51.631796
3430.294059	106698.956848	51.636801
3429.074625	104367.155926	51.641805
3428.303120	102043.379534	51.646810
3426.904796	99717.325565	51.651815
3425.936268	97415.196718	51.656820
3424.686608	95118.832459	51.661825
3423.578350	92826.620003	51.666829
3422.474836	90555.603345	51.671834
3421.973808	88285.500491	51.676839
3420.487839	86033.975124	51.681844
3419.817841	83784.375814	51.686849
3418.257762	81550.012376	51.691853
3417.103815	79338.406159	51.696858
3416.064901	77124.482646	51.701863
3414.755136	74935.470977	51.706868
3413.478190	72747.911193	51.711873
3412.278694	70584.203649	51.716877
3410.617043	68439.161604	51.721882
3409.422971	66295.514830	51.726887
3407.911560	64185.388139	51.731892
3406.863962	62087.384412	51.736897
3405.662835	60010.910329	51.741901
3404.085566	57948.491260	51.746906
3403.037978	55900.920846	51.751911
3401.230583	53884.039042	51.756916
3399.428827	51878.223558	51.761921
3398.336794	49900.593171	51.766925
3396.405827	47954.281040	51.771930
3395.044026	46016.983334	51.776935
3393.083133	44112.902545	51.781940
3390.833753	42231.277813	51.786945
3389.476825	40390.954238	51.791949
3387.494331	38571.427819	51.796954
3385.639119	36786.660830	51.801959
3383.678868	35039.212637	51.806964
3381.437988	33300.225588	51.811969
3378.907324	31628.023975	51.816973
3375.265276	30025.078041	51.821978
3370.758671	28508.263885	51.826983
3364.533006	27099.796343	51.831988
3357.655812	25797.715738	51.836993
3350.920231	24603.719840	51.841997
3344.804720	23513.834464	51.847002
3338.975220	22534.086381	51.852007
3333.697838	21673.366266	51.857012
3329.267219	20898.743651	51.862017
3325.150008	20230.444344	51.867021
3321.118481	19650.816797	51.872026
3318.221542	19152.772858	51.877031
3315.413406	18735.170426	51.882036
3313.003788	18368.317752	51.887041
3310.882089	18074.155553	51.892045
3308.868448	17822.919163	51.897050
3307.297034	17618.128066	51.902055
3305.876093	17461.927844	51.907060
3305.140333	17337.210891	51.912065
3304.062740	17236.372384	51.917069
3303.324867	17159.930857	51.922074
3302.994290	17098.057610	51.927079
3302.150515	17056.658178	51.932084
3301.289619	17030.955023	51.937089
3301.497382	17018.372815	51.942093
3300.987853	17010.635814	51.947098
3300.977481	17005.321877	51.952103
3300.193467	17014.916613	51.957108
3300.367393	17019.275745	51.962113
3300.115994	17030.867412	51.967117
3299.924283	17038.402686	51.972122
3299.755762	17049.518688	51.977127
3299.477080	17059.664090	51.982132
3299.805708	17069.410195	51.987137
3299.379582	17066.100271	51.992141
3299.294613	17070.026315	51.997146
3299.305982	17059.752038	52.002151
3299.032832	17063.958371	52.007156
3298.872239	17042.403062	52.012161
3298.586040	17030.916775	52.017165
3298.548293	17007.869036	52.022170
3298.623733	16989.338154	52.027175
3298.491870	16949.304673	52.032180
3298.408379	16908.046011	52.037185
3298.052254	16869.280686	52.042189
3298.198258	16819.964999	52.047194
3297.892585	16758.115623	52.052199
3296.905008	16707.865412	52.057204
3296.980403	16646.619913	52.062209
3296.454203	16582.009773	52.067213
3295.780589	16527.167263	52.072218
3295.547426	16447.857935	52.077223
3294.864008	16395.189131	52.082228
3294.724664	16322.575123	52.087233
3294.128430	16245.663143	52.092237
3293.591334	16160.649431	52.097242
3293.332288	16088.191227	52.102247
3292.286096	16009.670848	52.107252
3292.131164	15931.886803	52.112257
3291.490331	15848.711491	52.117261
3290.849863	15781.418261	52.122266
3290.768901	15706.241404	52.127271
3289.958332	15626.165377	52.132276
3289.619212	15520.833332	52.137281
3288.893379	15447.065313	52.142285
3288.156850	15345.426116	52.147290
3287.527701	15268.971515	52.152295
3286.954858	15186.914706	52.157300
3286.379415	15087.164982	52.162305
3286.069863	15007.965628	52.167309
3285.468038	14920.216321	52.172314
3285.080144	14834.957897	52.177319
3284.355725	14734.028362	52.182324
3283.834673	14646.062843	52.187329
3283.272288	14550.783261	52.192333
3282.313864	14464.133966	52.197338
3281.510605	14359.868349	52.202343
3280.581178	14268.825065	52.207348
3280.013150	14179.183883	52.212353
3279.346983	14096.566865	52.217357
3278.800357	14012.403307	52.222362
3278.461104	13922.438408	52.227367
3277.761733	13839.553381	52.232372
3277.786750	13747.604049	52.237377
3276.681784	13654.667824	52.242381
3275.806171	13555.648609	52.247386
3275.751851	13456.061456	52.252391
3274.475261	13372.534677	52.257396
3274.118032	13267.855271	52.262401
3273.817945	13185.575321	52.267405
3272.676673	13088.645886	52.272410
3272.201608	12996.771935	52.277415
3271.648215	12914.114707	52.282420
3271.054268	12812.070087	52.287425
3270.421393	12724.280851	52.292429
3269.171639	12631.381454	52.297434
3268.600300	12540.149068	52.302439
3267.866802	12463.494567	52.307444
3266.959398	12368.798468	52.312449
3266.643673	12275.264339	52.317453
3266.014277	12202.560892	52.322458
3265.513440	12109.429069	52.327463
3264.540824	12021.826449	52.332468
3264.038703	11940.893953	52.337473
3263.423388	11860.207141	52.342477
3262.721232	11774.969225	52.347482
3262.483523	11678.881290	52.352487
3261.561549	11596.058231	52.357492
3261.216482	11501.459104	52.362497
3260.472912	11414.904498	52.367501
3259.739743	11328.372274	52.372506
3259.202506	11233.172362	52.377511
3258.507994	11151.342857	52.382516
3257.743341	11053.814438	52.387521
3256.856203	10975.984461	52.392525
3256.272520	10884.003438	52.397530
3255.785654	10795.934155	52.402535
3255.480908	10716.212682	52.407540
3254.531415	10623.913268	52.412545
3254.064900	10535.104086	52.417549
3253.544660	10441.340461	52.422554
3252.950163	10348.035595	52.427559
3252.290076	10263.852175	52.432564
3251.430932	10162.841006	52.437569
3250.815889	10087.504517	52.442573
3250.125628	9991.317387	52.447578
3249.425092	9896.879913	52.452583
3248.571677	9813.556539	52.457588
3248.230431	9722.646557	52.462593
3247.204926	9635.803574	52.467597
3246.327531	9558.907656	52.472602
3245.707452	9460.493595	52.477607
3245.171826	9387.317464	52.482612
3244.534910	9300.760612	52.487617
3244.071467	9215.959761	52.492621
3242.864909	9137.588088	52.497626
3242.462774	9044.630676	52.502631
3242.040322	8968.473430	52.507636
3241.456879	8878.972894	52.512641
3240.834943	8789.255103	52.517645
3239.920151	8708.737747	52.522650
3239.213344	8624.679815	52.527655
3238.591151	8549.187401	52.532660
3238.118432	8459.441210	52.537665
3237.041028	8386.764984	52.542669
3236.110784	8306.599021	52.547674
3235.997397	8221.255451	52.552679
3235.639221	8145.792487	52.557684
3234.902015	8065.378327	52.562689
3234.118377	7987.997587	52.567693
3233.223018	7902.644745	52.572698
3232.621442	7820.665298	52.577703
3231.559605	7752.586884	52.582708
3231.224316	7657.098583	52.587713
3230.897801	7578.887435	52.592717
3229.961717	7501.603000	52.597722
3229.261835	7424.190916	52.602727
3228.401870	7348.179239	52.607732
3227.874895	7267.672335	52.612737
3227.291279	7188.428923	52.617741
3226.537270	7112.714600	52.622746
3225.949391	7033.597468	52.627751
3225.364858	6958.680253	52.632756
3224.520263	6882.502299	52.637761
3224.022510	6795.136643	52.642765
3223.228490	6725.919035	52.647770
3222.877802	6648.586088	52.652775
3221.713350	6575.910018	52.657780
3221.447121	6505.900301	52.662785
3220.321833	6431.134793	52.667789
3219.853911	6363.306732	52.672794
3219.366775	6280.852003	52.677799
3218.660129	6208.063067	52.682804
3218.283956	6131.473018	52.687809
3217.716105	6051.647327	52.692813
3216.794450	5976.185773	52.697818
3216.637681	5896.762103	52.702823
3215.636642	5820.615139	52.707828
3214.626886	5738.823463	52.712833
3214.284496	5666.018992	52.717837
3213.172563	5586.046919	52.722842
3212.986575	5504.398436	52.727847
3212.065968	5437.957037	52.732852
3211.428623	5363.459856	52.737857
3210.905311	5284.800740	52.742861
3209.812399	5220.106509	52.747866
3209.489158	5142.367088	52.752871
3208.795763	5069.887482	52.757876
3208.265495	4992.024644	52.762881
3207.759194	4915.085186	52.767885
3207.062771	4850.616908	52.772890
3206.571189	4770.079409	52.777895
3205.736483	4689.788879	52.782900
3204.898417	4614.431629	52.787905
3204.594217	4536.473963	52.792909
3203.600994	4463.548480	52.797914
3203.186337	4370.854011	52.802919
3202.621118	4305.002576	52.807924
3201.793613	4224.886101	52.812929
3200.998482	4153.442760	52.817933
3200.102727	4074.155994	52.822938
3199.693757	3998.059535	52.827943
3198.953734	3931.743617	52.832948
3198.260468	3861.082517	52.837953
3197.567008	3789.095972	52.842957
3196.977480	3712.955132	52.847962
3196.340088	3648.370317	52.852967
3195.474732	3579.802374	52.857972
3195.367036	3499.223901	52.862977
3194.341880	3420.784507	52.867981
3193.348582	3356.351702	52.872986
3192.951221	3285.615772	52.877991
3192.090542	3208.197934	52.882996
3191.240462	3148.219355	52.888001
3191.184733	3074.750048	52.893005
3190.061994	3002.920958	52.898010
3189.658188	2932.370896	52.903015
3188.960509	2871.543001	52.908020
3188.210235	2796.765278	52.913025
3187.473298	2719.669006	52.918029
3186.524016	2660.787005	52.923034
3186.319547	2592.235199	52.928039
3185.478293	2532.581969	52.933044
3184.906701	2468.510275	52.938049
3184.311211	2394.642075	52.943053
3183.617684	2323.980001	52.948058
3183.235840	2258.056022	52.953063
3181.781302	2186.528946	52.958068
3181.428188	2123.575657	52.963073
3181.091773	2059.869698	52.968077
3179.917232	2000.299113	52.973082
3179.264142	1928.708141	52.978087
3178.562030	1876.773488	52.983092
3177.677759	1807.735659	52.988097
3177.145775	1753.756669	52.993101
3176.509617	1685.463363	52.998106
3176.179703	1631.592781	53.003111
3175.052572	1575.829510	53.008116
3174.514443	1506.138573	53.013121
3173.982434	1454.324293	53.018125
3173.247435	1408.197385	53.023130
3172.686751	1341.151958	53.028135
3172.068445	1275.095650	53.033140
3171.050538	1231.883504	53.038145
3170.407413	1164.750675	53.043149
3169.669704	1113.810720	53.048154
3169.283319	1062.944728	53.053159
3168.508245	1011.567003	53.058164
3167.674204	952.492511	53.063169
3167.152055	898.613078	53.068173
3166.082821	851.282918	53.073178
3165.729609	792.755314	53.078183
3165.139795	752.327708	53.083188
3163.963607	697.198853	53.088193
3163.494507	651.225727	53.093197
3162.671966	602.071147	53.098202
3162.351220	552.231786	53.103207
3161.463451	512.838201	53.108212
3160.554288	462.789786	53.113217
3160.049076	414.651705	53.118221
3159.078318	375.201595	53.123226
3158.734288	328.955027	53.128231
3158.178664	289.262109	53.133236
3157.434177	247.856073	53.138241
3156.467224	204.287159	53.143245
3155.388918	176.162081	53.148250
3154.213891	145.701413	53.153255
3151.913273	160.797640	53.158260
3150.767037	167.530577	53.163265
3150.056078	170.129793	53.168269
3150.069068	177.547686	53.173274
3149.442927	173.545625	53.178279
3148.708003	173.128496	53.183284
3148.024930	178.673918	53.188289
3147.926968	184.832648	53.193293
3147.256181	178.432755	53.198298
3146.818987	177.317409	53.203303
3146.145020	166.150567	53.208308
3145.241259	170.770166	53.213313
3144.694794	169.598098	53.218317
3143.830706	180.918888	53.223322
3142.765485	170.296507	53.228327
3142.702805	168.674691	53.233332
3141.733927	176.248096	53.238337
3141.589167	160.672547	53.243341
3140.507584	177.297709	53.248346
3139.795670	170.348677	53.253351
3139.255836	174.106783	53.258356
3138.724483	171.680063	53.263361
3138.069468	166.947960	53.268365
3137.447261	188.574372	53.273370
3136.710964	159.587240	53.278375
3135.447028	171.207252	53.283380
3135.080575	172.005293	53.288385
3135.283434	166.414539	53.293389
3134.563223	168.001682	53.298394
3133.923979	166.862439	53.303399
3132.744829	174.542425	53.308404
3131.875100	177.424157	53.313409
3131.518968	175.109602	53.318413
3131.320942	176.380960	53.323418
3130.761319	173.913677	53.328423
3129.639598	167.906218	53.333428
3128.876011	170.724027	53.338433
3128.749810	167.676658	53.343437
3127.741103	171.504212	53.348442
3126.789205	175.402191	53.353447
3126.503168	174.486016	53.358452
3125.708107	172.679073	53.363457
3125.482191	170.547135	53.368461
3124.879385	172.751702	53.373466
3124.178725	164.277114	53.378471
3123.186655	166.010965	53.383476
3122.134520	168.561503	53.388481
3122.341790	161.630694	53.393485
3121.397790	167.577920	53.398490
3120.328289	169.153691	53.403495
3119.837563	170.417821	53.408500
3118.914226	171.890464	53.413505
3118.572710	167.293481	53.418509
3117.978916	164.813092	53.423514
3117.834684	161.794068	53.428519
3117.116226	157.572927	53.433524
3116.217943	167.421700	53.438529
3115.131424	156.958497	53.443533
3114.156489	169.202534	53.448538
3113.868275	161.536930	53.453543
3113.374237	172.070171	53.458548
3113.232485	172.609566	53.463553
3113.181931	169.693742	53.468557
3112.100282	167.478674	53.473562
3111.056842	164.907746	53.478567
3110.604743	166.347639	53.483572
3109.627681	166.897516	53.488577
3108.880496	165.946845	53.493581
3107.550337	168.159240	53.498586
3107.554643	168.088303	53.503591
3107.154667	164.181816	53.508596
3106.379105	168.863986	53.513601
3105.430115	162.337959	53.518605
3104.497389	167.903535	53.523610
3104.714495	171.065751	53.528615
3103.710141	164.911145	53.533620
3102.739316	169.875355	53.538625
3102.232365	157.765415	53.543629
3101.278454	164.739042	53.548634
3100.936512	160.670277	53.553639
3100.853064	165.023019	53.558644
3099.868329	167.197713	53.563649
3098.664059	164.173491	53.568653
3098.420097	175.293988	53.573658
3098.181968	173.840698	53.578663
3098.018600	163.760939	53.583668
3096.716356	167.663911	53.588673
3096.209256	169.452666	53.593677
3095.308600	172.966905	53.598682
3094.213867	174.152660	53.603687
3093.609537	170.687261	53.608692
3092.414709	170.638839	53.613697
3092.453533	158.404470	53.618701
3092.055512	173.356831	53.623706
3091.597794	169.077722	53.628711
3090.595623	160.530319	53.633716
3089.420030	171.664334	53.638721
3089.011860	161.704559	53.643725
3088.813851	165.126770	53.648730
3088.503875	162.868281	53.653735
3088.172308	166.838691	53.658740
3086.989549	165.942312	53.663745
3085.981566	159.412555	53.668749
3085.272085	176.702408	53.673754
3084.807151	165.995246	53.678759
3084.278813	172.549202	53.683764
3083.027774	172.450783	53.688769
3082.565396	158.040272	53.693773
3081.867466	171.498130	53.698778
3081.632912	163.844676	53.703783
3081.235627	161.953200	53.708788
3080.058332	165.189845	53.713793
3079.814176	160.066248	53.718797
3078.866492	167.681426	53.723802
3078.115586	152.074467	53.728807
3078.060976	159.379163	53.733812
3076.678838	166.736607	53.738817
3076.251898	152.924767	53.743821
3075.215675	160.671119	53.748826
3074.338397	156.532382	53.753831
3074.028475	159.426625	53.758836
3073.632853	162.350115	53.763841
3073.435667	152.525611	53.768845
3072.318566	155.942624	53.773850
3071.478382	155.411257	53.778855
3070.929236	148.216156	53.783860
3070.158799	159.811844	53.788865
3069.386686	158.190064	53.793869
3068.505590	154.027114	53.798874
3068.003951	153.664476	53.803879
3067.644773	149.805499	53.808884
3067.388527	157.336085	53.813889
3066.222525	152.850774	53.818893
3065.889008	159.182364	53.823898
3065.401763	151.480122	53.828903
3064.687761	157.698306	53.833908
3063.377517	164.474274	53.838913
3063.244848	150.981228	53.843917
3062.684770	153.074290	53.848922
3061.784074	157.371274	53.853927
3061.053859	151.619042	53.858932
3060.238357	158.930588	53.863937
3059.903153	145.577149	53.868941
3058.846516	158.390517	53.873946
3058.468553	154.586852	53.878951
3057.882157	149.299902	53.883956
3056.860604	151.862589	53.888961
3056.260124	155.086336	53.893965
3055.370996	160.260004	53.898970
3055.378709	156.324128	53.903975
3055.223498	159.774156	53.908980
3053.477799	160.010912	53.913985
3052.858790	158.182980	53.918989
3052.887451	154.351680	53.923994
3052.294113	155.545717	53.928999
3051.426320	144.991092	53.934004
3050.313549	156.659480	53.939009
3050.058960	155.214532	53.944013
3049.251669	154.054673	53.949018
3048.809959	154.102969	53.954023
3048.125586	154.673501	53.959028
3047.330132	156.871517	53.964033
3046.777408	157.313374	53.969037
3045.739467	158.314176	53.974042
3045.325831	152.391410	53.979047
3044.667704	151.552239	53.984052
3043.795366	161.743542	53.989057
3043.326729	146.075739	53.994061
3042.370006	156.932752	53.999066
3042.014657	151.892896	54.004071
3041.335312	156.739412	54.009076
3040.384404	160.100798	54.014081
3039.732955	147.218620	54.019085
3039.213406	158.510132	54.024090
3038.526941	151.904139	54.029095
3037.829623	151.510203	54.034100
3037.624947	157.314136	54.039105
3037.419454	154.121643	54.044109
3035.988196	161.939444	54.049114
3035.602179	154.974623	54.054119
3034.780562	151.406236	54.059124
3033.507188	155.580196	54.064129
3033.760191	147.116367	54.069133
3033.199516	149.917274	54.074138
3032.065373	154.327173	54.079143
3031.518573	154.954724	54.084148
3030.600336	161.681083	54.089153
3029.966509	147.815795	54.094157
3029.537048	156.824221	54.099162
3029.250443	159.096736	54.104167
3028.324209	151.151360	54.109172
3027.129137	157.930151	54.114177
3027.152560	149.520943	54.119181
3026.221417	156.501340	54.124186
3025.387467	156.248774	54.129191
3025.117620	151.656928	54.134196
3024.087549	155.366172	54.139201
3023.549748	148.565839	54.144205
3022.938303	158.325338	54.149210
3022.400485	153.667966	54.154215
3021.614931	155.320757	54.159220
3020.604958	161.092163	54.164225
3020.774815	150.747861	54.169229
3019.801518	156.509447	54.174234
3018.812156	156.080943	54.179239
3018.146250	157.905127	54.184244
3017.620273	163.752515	54.189249
3016.742440	159.388496	54.194253
3016.578866	157.362358	54.199258
3016.089483	161.047111	54.204263
3014.940168	155.784115	54.209268
3013.941542	153.025558	54.214273
3013.564637	150.514047	54.219277
3013.435991	158.267953	54.224282
3012.590359	153.870014	54.229287
3011.796133	152.478988	54.234292
3010.885699	155.805040	54.239297
3010.659714	153.655361	54.244301
3009.957971	153.296526	54.249306
3009.269695	157.713136	54.254311
3009.057080	153.175062	54.259316
3007.989832	160.879354	54.264321
3007.682937	150.087980	54.269325
3006.489713	146.785984	54.274330
3005.268992	157.382987	54.279335
3005.475020	163.353973	54.284340
3004.394510	167.144076	54.289345
3003.537328	159.516104	54.294349
3003.590625	159.275748	54.299354
3002.541070	158.732405	54.304359
3001.573327	148.745905	54.309364
3000.809905	163.442142	54.314369
3000.733083	147.909102	54.319373
3000.229046	146.410074	54.324378
2999.416458	144.817721	54.329383
2998.617119	147.357051	54.334388
2997.718374	151.419636	54.339393
2997.102535	145.383409	54.344397
2996.425553	148.023013	54.349402
2995.821101	143.255064	54.354407
2995.749050	141.447362	54.359412
2994.639095	149.979580	54.364417
2994.292659	141.637524	54.369421
2993.305965	148.571361	54.374426
2992.711507	154.173482	54.379431
2992.509362	149.227845	54.384436
2991.242650	146.000381	54.389441
2990.719076	144.580874	54.394445
2989.348640	145.379165	54.399450
2988.942714	153.131501	54.404455
2989.032289	144.690470	54.409460
2988.304753	145.365091	54.414465
2987.470772	140.208484	54.419469
2986.093603	152.217305	54.424474
2986.080301	145.689713	54.429479
2985.850164	137.368840	54.434484
2984.336266	146.085734	54.439489
2984.020536	141.429500	54.444493
2983.445830	149.141597	54.449498
2982.510860	145.023003	54.454503
2981.982179	148.291325	54.459508
2981.170012	146.177867	54.464513
2981.033113	140.320324	54.469517
2980.057797	141.971992	54.474522
2979.073318	142.085802	54.479527
2978.815157	143.921628	54.484532
2977.819178	151.400195	54.489537
2977.451574	147.244256	54.494541
2977.133719	148.586219	54.499546
2976.519240	145.136787	54.504551
2976.081745	137.750134	54.509556
2975.466663	145.773856	54.514561
2974.538426	139.631942	54.519565
2973.231083	139.845921	54.524570
2972.086538	139.595518	54.529575
2971.950829	135.844022	54.534580
2971.899149	146.381387	54.539585
2971.600737	144.260666	54.544589
2970.269041	142.915699	54.549594
2969.205828	151.161652	54.554599
2968.908673	139.509707	54.559604
2968.082435	139.637531	54.564609
2967.509442	133.294791	54.569613
2966.932895	143.543696	54.574618
2966.444429	143.917345	54.579623
2965.762151	135.743997	54.584628
2965.337872	150.752916	54.589633
2964.861962	139.740576	54.594637
2963.155918	142.506684	54.599642
2962.908662	142.790960	54.604647
2962.402459	137.090865	54.609652
2961.119032	142.923603	54.614657
2961.106470	142.585952	54.619661
2960.274111	140.184247	54.624666
2959.637708	148.110565	54.629671
2958.885953	138.557291	54.634676
2957.894278	144.540696	54.639681
2957.320222	142.615494	54.644685
2957.817456	141.490884	54.649690
2956.842788	141.038566	54.654695
2956.208946	140.718266	54.659700
2955.479686	142.730511	54.664705
2954.551000	145.370498	54.669709
2953.475248	147.738390	54.674714
2952.279577	152.547617	54.679719
2952.541808	130.430297	54.684724
2952.061947	144.126381	54.689729
2951.222889	143.814307	54.694733
2950.714060	140.676815	54.699738
2949.734597	149.166607	54.704743
2949.576064	140.237862	54.709748
2948.618924	144.791203	54.714753
2948.089282	136.827426	54.719757
2947.185097	141.530002	54.724762
2946.143704	143.047708	54.729767
2945.662926	140.619873	54.734772
2945.135985	138.155719	54.739777
2944.195516	148.657465	54.744781
2943.829250	141.598502	54.749786
2942.849501	141.318759	54.754791
2942.489872	148.398861	54.759796
2941.693983	151.262072	54.764801
2941.240281	151.340845	54.769805
2940.826317	146.741267	54.774810
2940.017647	143.813297	54.779815
2939.858936	142.796827	54.784820
2939.015043	140.798531	54.789825
2938.230503	143.372443	54.794829
2936.779533	143.033492	54.799834
2936.009260	138.943606	54.804839
2936.253691	146.036531	54.809844
2935.172914	140.424361	54.814849
2934.167493	144.038616	54.819853
2933.915747	140.789697	54.824858
2933.434578	145.656429	54.829863
2933.039402	145.250743	54.834868
2932.179978	146.534469	54.839873
2931.557017	138.130734	54.844877
2931.430710	137.709892	54.849882
2929.913624	141.508684	54.854887
2929.061274	140.699954	54.859892
2928.178458	141.248359	54.864897
2927.568568	145.692234	54.869901
2927.918286	147.156956	54.874906
2927.159676	147.204152	54.879911
2926.535950	147.290271	54.884916
2925.637942	152.365205	54.889921
2924.948457	145.101352	54.894925
2923.968733	148.338994	54.899930
2922.738056	147.530180	54.904935
2922.667432	144.087684	54.909940
2922.183932	151.067379	54.914945
2921.609684	152.029619	54.919949
2921.089187	140.226380	54.924954
2920.480421	146.897095	54.929959
2919.633785	142.040680	54.934964
2918.884392	154.796021	54.939969
2918.476081	142.515730	54.944973
2917.100613	149.765081	54.949978
2916.128030	147.924169	54.954983
2916.335554	148.395592	54.959988
2915.371443	146.226006	54.964993
2914.743678	145.507185	54.969997
2914.053932	146.654157	54.975002
2913.357881	149.079535	54.980007
2913.223168	150.698484	54.985012
2912.434345	156.348033	54.990017
2911.857052	152.551606	54.995021
2911.283706	146.509316	55.000026
2910.565288	158.649913	55.005031
2909.721748	151.601853	55.010036
2908.555073	152.498365	55.015041
2907.924804	150.737505	55.020045
2907.719069	148.769893	55.025050
2906.790797	147.882169	55.030055
2906.610948	147.928751	55.035060
2905.721358	143.796892	55.040065
2905.076323	143.968757	55.045069
2903.694161	142.836503	55.050074
2903.300235	151.342682	55.055079
2902.992733	141.888365	55.060084
2902.094767	142.357655	55.065089
2901.189383	145.305895	55.070093
2901.245907	145.001436	55.075098
2900.534097	150.918472	55.080103
2899.864782	139.853146	55.085108
2898.882785	153.869905	55.090113
2898.447263	148.794426	55.095117
2898.314286	143.903293	55.100122
2897.406337	145.244656	55.105127
2896.556462	156.973914	55.110132
2895.459360	148.512658	55.115137
2894.750253	149.879645	55.120141
2894.455628	151.454082	55.125146
2893.673963	155.302073	55.130151
2893.391099	153.019231	55.135156
2892.890943	155.801516	55.140161
2891.629300	146.533145	55.145165
2890.683529	147.766107	55.150170
2889.908060	154.099405	55.155175
2889.770771	146.822112	55.160180
2888.819583	151.082349	55.165185
2888.046981	156.167041	55.170189
2887.991454	139.771077	55.175194
2887.009764	147.407071	55.180199
2886.540908	146.130588	55.185204
2886.178175	147.843370	55.190209
2885.381523	146.531328	55.195213
2885.151679	142.171470	55.200218
2883.905722	148.981471	55.205223
2883.202141	139.442481	55.210228
2882.216074	135.080414	55.215233
2882.022455	140.929418	55.220237
2881.467418	138.123110	55.225242
2880.709232	139.750714	55.230247
2880.393723	133.556612	55.235252
2878.963944	142.834258	55.240257
2878.405637	144.509017	55.245261
2877.540953	139.358863	55.250266
2876.938571	139.161481	55.255271
2876.599689	142.907750	55.260276
2876.164328	142.697219	55.265281
2875.631893	140.728995	55.270285
2875.446472	136.600355	55.275290
2873.656614	151.989865	55.280295
2872.932528	138.840685	55.285300
2872.257784	144.752176	55.290305
2872.144675	143.870411	55.295309
2871.534035	139.978642	55.300314
2870.550268	146.018730	55.305319
2870.112484	144.143274	55.310324
2869.642215	146.366655	55.315329
2868.956771	145.622170	55.320333
2867.819146	140.854572	55.325338
2867.084230	142.851609	55.330343
2866.487451	141.517255	55.335348
2865.972766	149.538033	55.340353
2865.243128	147.118789	55.345357
2864.835089	133.303784	55.350362
2864.140200	145.109176	55.355367
2863.948121	139.400411	55.360372
2862.387676	145.425370	55.365377
2861.934245	144.239013	55.370381
2861.363230	136.678230	55.375386
2860.665842	143.036865	55.380391
2860.429798	142.112164	55.385396
2859.795943	147.159328	55.390401
2859.148997	140.070584	55.395405
2858.130287	135.692390	55.400410
2856.636600	142.562096	55.405415
2856.537280	136.219738	55.410420
2856.125541	135.341642	55.415425
2855.306451	139.000245	55.420429
2854.966315	137.239152	55.425434
2854.184859	151.236637	55.430439
2853.804931	138.197195	55.435444
2853.071049	148.931264	55.440449
2852.457694	143.078580	55.445453
2851.355272	142.735741	55.450458
2850.371382	147.168538	55.455463
2850.251009	139.135624	55.460468
2849.429397	141.785352	55.465473
2849.035683	149.161004	55.470477
2848.545440	145.860879	55.475482
2847.826089	146.943446	55.480487
2846.956113	136.388465	55.485492
2845.887206	144.222518	55.490497
2845.243673	149.398833	55.495501
2844.855636	144.291565	55.500506
2844.162797	150.015105	55.505511
2843.859176	143.265964	55.510516
2843.187951	147.729800	55.515521
2842.792659	149.726034	55.520525
2841.738534	142.337811	55.525530
2840.361184	152.938700	55.530535
2840.255451	143.344519	55.535540
2839.728664	142.867782	55.540545
2839.070212	147.637319	55.545549
2838.551146	143.906741	55.550554
2838.015590	145.202628	55.555559
2837.103465	143.564550	55.560564
2835.877554	140.268578	55.565569
2835.218637	140.568345	55.570573
2834.672921	136.014588	55.575578
2833.959277	142.320741	55.580583
2833.514512	133.623294	55.585588
2833.112486	140.658532	55.590593
2832.580854	140.576954	55.595597
2832.183965	139.507643	55.600602
2831.750414	145.144240	55.605607
2830.937316	135.175181	55.610612
2829.772822	144.521967	55.615617
2829.060875	141.794979	55.620621
2828.910617	148.718117	55.625626
2827.455740	148.079083	55.630631
2826.553221	146.081351	55.635636
2825.981624	139.885231	55.640641
2825.950117	136.619208	55.645645
2825.307345	136.524651	55.650650
2824.981477	146.003634	55.655655
2824.408580	146.328174	55.660660
2823.220315	142.260401	55.665665
2822.050168	148.721940	55.670669
2821.287205	139.118905	55.675674
2820.488501	135.641772	55.680679
2820.803929	136.840382	55.685684
2820.006776	139.616981	55.690689
2819.305782	142.740292	55.695693
2818.940370	137.832050	55.700698
2818.092106	143.582546	55.705703
2817.289747	137.389552	55.710708
2816.269009	143.397280	55.715713
2815.711810	135.715333	55.720717
2815.111077	136.069498	55.725722
2814.497792	138.408503	55.730727
2813.896316	128.211845	55.735732
2813.783768	136.590191	55.740737
2812.898947	146.653763	55.745741
2811.937456	136.593231	55.750746
2811.030234	144.102033	55.755751
2810.745584	143.734307	55.760756
2810.233214	141.332807	55.765761
2809.416875	145.012656	55.770765
2808.493231	135.884704	55.775770
2807.275104	142.489042	55.780775
2806.905346	138.520986	55.785780
2806.190821	137.718719	55.790785
2805.705202	132.606821	55.795789
2805.421571	128.437344	55.800794
2804.753226	143.018231	55.805799
2804.524305	141.625358	55.810804
2803.987300	139.419115	55.815809
2802.706412	143.970963	55.820813
2802.186153	129.054535	55.825818
2800.712959	140.088628	55.830823
2800.689611	134.688917	55.835828
2799.963284	134.118003	55.840833
2799.455284	149.313312	55.845837
2799.187415	137.175621	55.850842
2797.592454	145.832981	55.855847
2797.170731	141.940514	55.860852
2796.256437	143.881770	55.865857
2795.741197	144.588814	55.870861
2795.861780	136.898397	55.875866
2794.901059	143.647818	55.880871
2794.487659	129.422841	55.885876
2793.924716	138.815630	55.890881
2792.998868	133.463588	55.895885
2792.250427	135.618069	55.900890
2791.601024	143.144387	55.905895
2791.328011	133.951031	55.910900
2790.022712	147.711604	55.915905
2788.877147	137.674642	55.920909
2788.511048	139.897985	55.925914
2787.670021	138.617227	55.930919
2787.358519	138.590790	55.935924
2786.987911	139.215091	55.940929
2786.144425	138.424604	55.945933
2786.223670	129.600112	55.950938
2785.122825	134.093953	55.955943
2784.206433	127.133776	55.960948
2783.438028	130.871746	55.965953
2782.833830	131.761751	55.970957
2782.715068	120.379749	55.975962
2782.006977	131.867267	55.980967
2780.923051	127.634050	55.985972
2779.987990	127.901679	55.990977
2779.326299	132.856104	55.995981
2778.562620	127.354382	56.000986
2778.088554	139.075845	56.005991
2777.388772	132.320217	56.010996
2777.171409	130.985764	56.016001
2776.834788	129.460122	56.021005
2775.765195	130.809391	56.026010
2774.414136	142.844554	56.031015
2773.940093	133.620034	56.036020
2773.347501	130.435305	56.041025
2772.853456	137.730997	56.046029
2772.661234	131.080853	56.051034
2772.218062	141.599844	56.056039
2771.570699	133.969629	56.061044
2770.364801	132.294540	56.066049
2769.523727	136.235188	56.071053
2768.948792	124.161441	56.076058
2768.242818	141.924696	56.081063
2767.743542	129.264086	56.086068
2767.145719	131.926099	56.091073
2766.051861	143.517055	56.096077
2765.422917	140.618002	56.101082
2764.642364	133.515009	56.106087
2764.080622	126.456725	56.111092
2763.911098	130.525746	56.116097
2763.074121	133.653355	56.121101
2762.909325	135.750323	56.126106
2762.311294	133.559253	56.131111
2761.221324	127.134388	56.136116
2760.481621	136.026088	56.141121
2759.791213	138.362885	56.146125
2759.546853	128.973594	56.151130
2758.576835	133.861116	56.156135
2757.609385	127.079403	56.161140
2757.220439	131.405393	56.166145
2756.432600	133.283200	56.171149
2756.158024	122.804116	56.176154
2755.569688	128.988591	56.181159
2754.681571	123.360122	56.186164
2753.843793	125.979464	56.191169
2753.005682	136.244646	56.196173
2752.762091	128.785420	56.201178
2751.805401	134.780626	56.206183
2750.984876	132.850209	56.211188
2750.038562	130.922738	56.216193
2749.302988	131.352849	56.221197
2749.340280	131.245091	56.226202
2748.340127	134.183098	56.231207
2747.987953	140.240771	56.236212
2747.193208	140.798622	56.241217
2746.967999	131.289615	56.246221
2746.419997	124.740152	56.251226
2745.238522	135.610316	56.256231
2744.498087	135.160237	56.261236
2743.867681	127.283984	56.266241
2743.622646	131.114473	56.271245
2742.697688	126.404901	56.276250
2741.095313	126.728961	56.281255
2741.189447	133.434271	56.286260
2740.706717	133.443023	56.291265
2739.664389	134.416205	56.296269
2738.928722	127.909474	56.301274
2738.642082	135.666278	56.306279
2738.405102	128.275789	56.311284
2738.099179	127.783813	56.316289
2736.954837	132.341935	56.321293
2735.696820	135.192970	56.326298
2735.001171	131.899154	56.331303
2734.978319	131.275904	56.336308
2734.203447	131.648394	56.341313
2733.283567	134.155067	56.346317
2732.421804	127.436214	56.351322
2731.603652	140.607095	56.356327
2731.098341	132.777353	56.361332
2730.764843	134.103842	56.366337
2730.401013	138.407778	56.371341
2730.055765	137.994758	56.376346
2729.402519	142.091592	56.381351
2728.298584	136.755791	56.386356
2727.492503	138.800925	56.391361
2726.900766	140.376019	56.396365
2726.465940	137.920619	56.401370
2724.886360	138.133817	56.406375
2724.148101	140.019733	56.411380
2723.582026	132.571813	56.416385
2722.822147	140.220826	56.421389
2722.780518	138.775026	56.426394
2722.285813	140.535238	56.431399
2722.067717	136.351013	56.436404
2721.454829	126.453158	56.441409
2720.370117	138.039787	56.446413
2720.001345	132.590573	56.451418
2719.015924	136.061311	56.456423
2718.101421	129.557520	56.461428
2717.067290	137.516687	56.466433
2716.453823	142.143546	56.471437
2716.422420	126.016653	56.476442
2715.144042	137.055352	56.481447
2714.820757	139.166779	56.486452
2714.292410	136.872623	56.491457
2713.668518	137.604164	56.496461
2713.491366	135.537340	56.501466
2712.188791	137.048806	56.506471
2711.197787	126.497976	56.511476
2710.493688	138.331776	56.516481
2709.854728	145.370409	56.521485
2709.454444	133.045771	56.526490
2708.875191	145.304670	56.531495
2708.507688	142.750530	56.536500
2708.298731	138.526061	56.541505
2707.220824	146.077861	56.546509
2706.119546	134.074348	56.551514
2705.571568	141.369786	56.556519
2705.183223	134.482390	56.561524
2704.647173	134.818801	56.566529
2703.612404	143.690680	56.571533
2702.773530	126.576054	56.576538
2701.587096	136.931958	56.581543
2701.097534	132.359940	56.586548
2700.821518	131.969035	56.591553
2700.313391	133.960876	56.596557
2700.173159	132.246151	56.601562
2699.766608	140.553958	56.606567
2698.582485	133.166287	56.611572
2697.783066	132.684061	56.616577
2697.064847	132.661623	56.621581
2696.512614	133.065140	56.626586
2696.084262	131.931747	56.631591
2694.936836	127.028113	56.636596
2694.367566	131.769386	56.641601
2693.454999	138.402429	56.646605
2692.939540	128.750417	56.651610
2692.667644	134.945544	56.656615
2691.928870	132.042381	56.661620
2690.908838	136.364535	56.666625
2690.091322	141.621909	56.671629
2689.618460	121.683252	56.676634
2689.835331	134.941681	56.681639
2689.341867	131.382006	56.686644
2688.016733	126.946101	56.691649
2686.767743	130.388869	56.696653
2686.293784	127.368605	56.701658
2685.758577	134.209111	56.706663
2685.527952	141.936605	56.711668
2685.047326	126.562662	56.716673
2683.559372	135.212010	56.721677
2682.868335	134.136939	56.726682
2682.123941	141.023466	56.731687
2681.855781	131.526940	56.736692
2681.572399	133.581417	56.741697
2680.967906	136.295101	56.746701
2680.132646	126.506314	56.751706
2679.161038	135.302266	56.756711
2678.231431	126.759957	56.761716
2678.027051	130.650204	56.766721
2677.188259	131.337958	56.771725
2677.111462	127.091694	56.776730
2675.566762	130.526195	56.781735
2674.719556	128.901129	56.786740
2674.556290	134.062067	56.791745
2673.872926	131.138384	56.796749
2673.979358	131.884435	56.801754
2672.959081	129.264647	56.806759
2671.869881	128.932215	56.811764
2671.271368	133.496520	56.816769
2670.360296	135.355535	56.821773
2670.176802	129.015743	56.826778
2669.218061	134.444092	56.831783
2669.011232	130.384653	56.836788
2667.830017	127.473440	56.841793
2667.060591	122.843086	56.846797
2666.656098	124.976683	56.851802
2665.977325	138.811344	56.856807
2665.168851	130.204912	56.861812
2665.249373	131.046176	56.866817
2663.973161	134.373607	56.871821
2663.227243	125.115850	56.876826
2662.499605	130.237864	56.881831
2661.940777	126.273724	56.886836
2661.542429	128.842044	56.891841
2660.977255	135.794249	56.896845
2660.357254	121.976847	56.901850
2659.390307	130.832788	56.906855
2658.767794	135.988544	56.911860
2657.997524	127.098884	56.916865
2657.263180	138.439715	56.921869
2657.441476	120.591924	56.926874
2656.051160	129.082089	56.931879
2655.108102	129.419787	56.936884
2655.055494	131.173907	56.941889
2654.263267	132.554731	56.946893
2653.739530	130.094012	56.951898
2652.629956	138.019503	56.956903
2651.682367	134.546535	56.961908
2651.283988	124.873337	56.966913
2650.356502	132.453502	56.971917
2650.077110	127.155988	56.976922
2649.900287	124.274801	56.981927
2649.619614	128.538865	56.986932
2648.503054	127.793104	56.991937
2647.370177	137.027925	56.996941
2646.813128	129.867809	57.001946
2646.137654	131.838524	57.006951
2645.743826	132.065764	57.011956
2644.853684	135.143660	57.016961
2643.876480	137.045561	57.021965
2643.125317	125.721938	57.026970
2642.369781	129.621136	57.031975
2641.997665	129.547834	57.036980
2641.827914	130.148073	57.041985
2641.151139	139.870176	57.046989
2641.389734	127.178203	57.051994
2639.810071	133.850281	57.056999
2638.616545	135.032476	57.062004
2638.479858	124.934035	57.067009
2637.413423	141.390789	57.072013
2637.453567	125.094188	57.077018
2636.090840	133.583590	57.082023
2635.307626	130.747241	57.087028
2634.766667	140.113773	57.092033
2634.327094	135.036658	57.097037
2634.084619	121.579058	57.102042
2633.387991	136.541332	57.107047
2632.044700	135.808673	57.112052
2631.326642	125.783557	57.117057
2630.581671	132.792941	57.122061
2630.251436	125.062763	57.127066
2629.730683	133.094834	57.132071
2629.531326	139.015466	57.137076
2629.294997	130.926614	57.142081
2628.057291	128.308872	57.147085
2627.407647	129.580462	57.152090
2626.215741	136.693481	57.157095
2625.029804	132.664835	57.162100
2624.624531	129.712571	57.167105
2624.262439	125.768489	57.172109
2623.917380	126.331592	57.177114
2623.172627	128.352834	57.182119
2622.770803	129.664165	57.187124
2622.454635	135.084914	57.192129
2620.973553	136.003646	57.197133
2620.530240	127.969520	57.202138
2619.747233	127.752911	57.207143
2619.405712	128.721578	57.212148
2619.119683	128.604747	57.217153
2617.640782	128.202761	57.222157
2617.136595	124.721901	57.227162
2616.576939	119.944783	57.232167
2615.576320	125.528315	57.237172
2615.442015	123.679560	57.242177
2614.181376	133.900923	57.247181
2613.432161	130.420895	57.252186
2612.662554	123.805129	57.257191
2612.426687	132.391637	57.262196
2612.002103	131.021959	57.267201
2611.334070	131.791450	57.272205
2611.612918	132.532499	57.277210
2610.228766	130.810551	57.282215
2609.165017	133.791027	57.287220
2608.484990	130.217860	57.292225
2607.994835	129.664230	57.297229
2606.851263	115.268082	57.302234
2606.335857	127.694069	57.307239
2605.847798	129.159874	57.312244
2605.268162	130.068592	57.317249
2604.227444	134.340215	57.322253
2604.142247	129.006747	57.327258
2603.917230	130.489954	57.332263
2602.940348	125.088656	57.337268
2602.081835	116.609611	57.342273
2601.270928	130.011341	57.347277
2600.667620	121.831682	57.352282
2600.009510	116.946270	57.357287
2599.267120	122.659733	57.362292
2598.383770	120.151946	57.367297
2597.528409	125.081462	57.372301
2597.003314	124.995630	57.377306
2596.666196	126.485763	57.382311
2596.084874	126.183762	57.387316
2596.182942	121.788802	57.392321
2594.822806	132.470052	57.397325
2593.882581	131.565874	57.402330
2593.133660	128.248821	57.407335
2592.323112	135.976760	57.412340
2592.361800	122.442685	57.417345
2591.764458	132.251465	57.422349
2590.651113	126.985992	57.427354
2589.919632	125.383394	57.432359
2589.205095	122.340323	57.437364
2588.894724	120.358647	57.442369
2588.108243	132.167052	57.447373
2588.004813	127.243661	57.452378
2586.857237	124.931826	57.457383
2585.887227	123.837750	57.462388
2585.801662	122.397491	57.467393
2584.588744	138.158520	57.472397
2584.354424	120.142073	57.477402
2583.268875	140.570628	57.482407
2582.302771	135.692470	57.487412
2582.286329	128.055888	57.492417
2581.053791	128.929774	57.497421
2581.041039	118.539775	57.502426
2580.673013	117.636862	57.507431
2580.038951	121.390961	57.512436
2578.981623	118.139264	57.517441
2578.218009	128.745777	57.522445
2577.929891	111.469170	57.527450
2577.099057	122.642938	57.532455
2575.994952	121.983481	57.537460
2575.383246	116.278988	57.542465
2574.933898	125.814975	57.547469
2574.699176	117.907829	57.552474
2573.570097	127.314891	57.557479
2572.365460	121.084937	57.562484
2571.836950	118.825564	57.567489
2571.036634	124.070134	57.572493
2570.532440	121.353858	57.577498
2570.219450	126.628013	57.582503
2570.088520	129.516136	57.587508
2569.862438	123.436653	57.592513
2568.638842	128.384518	57.597517
2568.277521	127.405462	57.602522
2567.476182	130.415688	57.607527
2565.915085	137.512882	57.612532
2565.376187	142.349626	57.617537
2564.439362	146.804807	57.622541
2564.078306	142.032817	57.627546
2563.797350	141.160807	57.632551
2563.247137	133.495870	57.637556
2562.940394	127.863185	57.642561
2561.824238	135.539557	57.647565
2561.142510	136.746378	57.652570
2560.577002	138.735802	57.657575
2559.448734	146.960151	57.662580
2559.300673	136.439726	57.667585
2557.891261	141.482516	57.672589
2557.383064	133.135423	57.677594
2557.069836	121.058040	57.682599
2556.403677	136.456006	57.687604
2556.113351	134.728262	57.692609
2555.305472	137.516591	57.697613
2554.475403	134.231177	57.702618
2553.658290	136.519393	57.707623
2553.080125	138.112707	57.712628
2552.722506	126.789724	57.717633
2552.167826	134.773123	57.722637
2550.895768	134.166065	57.727642
2549.735154	133.558903	57.732647
2549.136285	131.136302	57.737652
2548.943010	126.021438	57.742657
2548.329182	135.169511	57.747661
2548.406657	128.883799	57.752666
2547.772337	135.135354	57.757671
2546.588639	136.153261	57.762676
2546.020386	128.920476	57.767681
2545.437885	136.551804	57.772685
2544.838048	131.241583	57.777690
2543.888785	129.094006	57.782695
2542.624231	134.619647	57.787700
2542.436247	130.005175	57.792705
2541.664861	135.919386	57.797709
2541.354007	132.437455	57.802714
2540.738436	125.304337	57.807719
2540.212769	131.832568	57.812724
2539.398992	130.048264	57.817729
2538.090519	134.760391	57.822733
2538.049830	129.358532	57.827738
2537.599793	130.025240	57.832743
2536.703737	131.647636	57.837748
2535.728493	131.013525	57.842753
2535.014625	130.183552	57.847757
2534.590804	120.060007	57.852762
2534.020722	130.314503	57.857767
2533.670398	132.458188	57.862772
2533.020094	124.604721	57.867777
2532.172506	126.219226	57.872781
2531.598706	125.591485	57.877786
2530.906307	124.173654	57.882791
2529.469719	130.529990	57.887796
2528.918997	123.139088	57.892801
2528.262410	130.094684	57.897805
2527.810480	127.751568	57.902810
2527.239729	125.684545	57.907815
2526.560227	129.294845	57.912820
2526.361024	120.235360	57.917825
2525.687770	130.019223	57.922829
2524.533028	126.823266	57.927834
2524.114231	129.374957	57.932839
2523.391095	133.743479	57.937844
2523.316384	124.809151	57.942849
2522.227593	124.830744	57.947853
2521.345130	125.895050	57.952858
2520.609792	124.869416	57.957863
2519.920543	135.184549	57.962868
2519.493348	130.954381	57.967873
2518.966190	133.509598	57.972877
2517.854790	134.208059	57.977882
2517.289037	124.451002	57.982887
2516.527687	131.189649	57.987892
2516.289027	125.876898	57.992897
2515.536950	120.272197	57.997901
2515.297893	126.416705	58.002906
2514.142634	120.697385	58.007911
2513.256373	127.250156	58.012916
2512.721728	123.679783	58.017921
2511.907307	136.416618	58.022925
2511.599893	121.235341	58.027930
2511.151258	124.488027	58.032935
2510.106523	131.412484	58.037940
2509.258326	129.811299	58.042945
2508.778438	128.181490	58.047949
2508.435941	124.367882	58.052954
2507.823818	129.264509	58.057959
2506.834143	127.635013	58.062964
2505.951092	121.032349	58.067969
2505.436659	131.500745	58.072973
2504.775366	131.210056	58.077978
2504.365294	124.819811	58.082983
2503.951408	134.173298	58.087988
2503.400642	124.693539	58.092993
2502.413393	128.982086	58.097997
2501.530240	126.614803	58.103002
2501.292072	124.067389	58.108007
2500.275297	123.861157	58.113012
2499.466868	121.362289	58.118017
2498.905041	131.901943	58.123021
2498.066705	132.122293	58.128026
2497.548113	125.758890	58.133031
2496.801100	127.172660	58.138036
2496.502666	123.693744	58.143041
2495.078686	126.162291	58.148045
2494.781183	125.245749	58.153050
2494.299674	117.784999	58.158055
2493.415764	126.745960	58.163060
2493.611222	122.928803	58.168065
2492.924343	122.509864	58.173069
2491.832118	121.518011	58.178074
2491.272757	118.961170	58.183079
2490.205104	121.249594	58.188084
2490.268427	119.687967	58.193089
2488.414316	119.448843	58.198093
2487.746449	120.623302	58.203098
2487.361800	125.659849	58.208103
2486.795502	134.929660	58.213108
2486.453439	119.017763	58.218113
2485.947812	124.482345	58.223117
2485.591535	126.789674	58.228122
2484.869031	123.617723	58.233127
2483.708867	126.341158	58.238132
2483.454172	123.924066	58.243137
2482.724088	126.095178	58.248141
2481.743671	127.076372	58.253146
2481.022459	112.817267	58.258151
2480.190971	125.052557	58.263156
2479.600268	127.679427	58.268161
2479.265217	126.027228	58.273165
2479.197885	126.107481	58.278170
2478.272891	122.671345	58.283175
2477.323666	125.263196	58.288180
2476.659108	122.859731	58.293185
2475.275583	129.857506	58.298189
2474.364787	125.751863	58.303194
2474.378300	124.011259	58.308199
2473.822532	127.344629	58.313204
2473.217255	126.653988	58.318209
2472.466050	130.110373	58.323213
2472.219116	125.756635	58.328218
2471.670246	128.447404	58.333223
2470.224684	118.465790	58.338228
2469.828321	120.088420	58.343233
2468.841887	122.918730	58.348237
2468.526769	117.817207	58.353242
2468.322360	117.955630	58.358247
2467.745286	121.367639	58.363252
2466.458065	119.084049	58.368257
2465.864415	128.101569	58.373261
2465.173768	123.745141	58.378266
2464.869869	129.837185	58.383271
2464.091325	123.747958	58.388276
2463.008913	119.396144	58.393281
2461.951594	120.440618	58.398285
2461.687403	120.713993	58.403290
2461.523567	118.504388	58.408295
2460.698472	127.902910	58.413300
2460.557821	120.366917	58.418305
2459.580713	123.635353	58.423309
2458.480090	122.297193	58.428314
2458.144612	121.024792	58.433319
2457.810936	129.249868	58.438324
2457.015483	121.536493	58.443329
2455.690972	129.300598	58.448333
2455.485876	130.015827	58.453338
2455.252926	119.730985	58.458343
2454.234050	126.807730	58.463348
2452.994065	129.292197	58.468353
2451.870330	129.182415	58.473357
2451.719432	125.441841	58.478362
2451.532584	124.911367	58.483367
2450.712200	135.902185	58.488372
2450.713532	123.462763	58.493377
2450.173036	129.431052	58.498381
2448.585120	128.498297	58.503386
2448.479791	126.163430	58.508391
2447.548680	122.022190	58.513396
2446.428605	122.409132	58.518401
2445.563963	123.889597	58.523405
2444.596219	125.394398	58.528410
2445.076077	122.338587	58.533415
2444.418646	128.660803	58.538420
2444.106651	120.186643	58.543425
2443.203790	127.849452	58.548429
2442.102819	123.539103	58.553434
2441.441498	122.411618	58.558439
2440.544532	127.559045	58.563444
2440.418754	119.858676	58.568449
2439.736020	131.426327	58.573453
2438.554610	128.136665	58.578458
2438.385559	124.385775	58.583463
2437.564376	127.440459	58.588468
2437.471854	108.707477	58.593473
2436.092127	128.195162	58.598477
2435.076210	122.766632	58.603482
2434.432729	116.020795	58.608487
2433.885795	126.145414	58.613492
2433.396361	111.172908	58.618497
2432.910700	128.783200	58.623501
2432.585132	131.347771	58.628506
2432.543519	117.503386	58.633511
2431.226545	131.353993	58.638516
2430.572273	119.845712	58.643521
2429.599127	123.254391	58.648525
2428.487072	127.276928	58.653530
2427.882739	120.274538	58.658535
2427.001874	127.842012	58.663540
2426.980912	124.164485	58.668545
2426.347868	127.636591	58.673549
2425.995942	136.959354	58.678554
2425.709703	122.460105	58.683559
2424.377145	126.960062	58.688564
2423.704634	124.501124	58.693569
2423.416214	121.974150	58.698573
2422.632126	113.695180	58.703578
2421.267428	118.510092	58.708583
2420.422139	122.174400	58.713588
2420.400583	120.450056	58.718593
2419.800974	115.881897	58.723597
2419.559305	123.896247	58.728602
2419.014348	117.568945	58.733607
2417.520546	125.590542	58.738612
2417.302538	126.662439	58.743617
2416.844678	125.446489	58.748621
2415.485359	134.722022	58.753626
2414.854903	117.248593	58.758631
2413.728567	123.042712	58.763636
2413.275922	116.692129	58.768641
2412.458259	122.837274	58.773645
2412.294541	120.594099	58.778650
2411.891086	117.518001	58.783655
2411.441213	125.593606	58.788660
2411.507495	126.064682	58.793665
2410.747574	120.833960	58.798669
2409.402882	122.262300	58.803674
2407.936261	128.560637	58.808679
2406.788866	117.022207	58.813684
2407.249450	121.732274	58.818689
2406.707010	123.141867	58.823693
2406.121397	120.748992	58.828698
2405.581245	113.516172	58.833703
2404.323433	125.116619	58.838708
2403.790420	118.488473	58.843713
2403.257350	120.369339	58.848717
2402.392462	120.497142	58.853722
2402.127575	125.106651	58.858727
2401.328197	124.587753	58.863732
2400.697353	120.726750	58.868737
2399.871199	127.352936	58.873741
2399.072130	128.645360	58.878746
2398.754638	125.294838	58.883751
2398.163600	126.708399	58.888756
2397.473903	127.763842	58.893761
2396.667922	122.787303	58.898765
2395.891324	133.363282	58.903770
2395.642387	124.263765	58.908775
2394.319445	138.152505	58.913780
2393.487368	121.737063	58.918785
2392.851733	129.060514	58.923789
2392.062234	127.070775	58.928794
2391.853652	115.279866	58.933799
2391.254821	125.294546	58.938804
2391.189439	112.348674	58.943809
2390.604297	119.434549	58.948813
2388.861269	121.631630	58.953818
2388.672343	120.944020	58.958823
2387.909333	125.148059	58.963828
2387.710605	126.684800	58.968833
2387.217515	128.282922	58.973837
2385.948592	121.852047	58.978842
2385.220887	121.148403	58.983847
2384.464542	131.544083	58.988852
2384.580821	120.276683	58.993857
2383.552958	129.240555	58.998861
2382.326139	128.424100	59.003866
2381.994155	132.503525	59.008871
2381.471721	140.621937	59.013876
2381.176167	123.423606	59.018881
2379.959505	132.172666	59.023885
2378.635007	136.765989	59.028890
2378.457079	128.739025	59.033895
2377.967711	131.937106	59.038900
2377.612045	129.335188	59.043905
2377.212351	130.710509	59.048909
2376.576888	134.618412	59.053914
2375.918617	132.695840	59.058919
2374.567942	137.575470	59.063924
2374.537279	128.855459	59.068929
2373.775942	126.402243	59.073933
2372.473851	129.002339	59.078938
2371.898878	124.410237	59.083943
2371.050926	130.338339	59.088948
2370.551935	126.211253	59.093953
2370.692188	126.118650	59.098957
2370.093762	130.036008	59.103962
2369.404945	130.479093	59.108967
2367.925303	130.751879	59.113972
2367.862747	122.116665	59.118977
2366.766449	123.858582	59.123981
2365.604784	127.443576	59.128986
2365.212241	117.859826	59.133991
2364.396475	131.238309	59.138996
2364.120760	119.797156	59.144001
2363.904875	125.433244	59.149005
2363.318790	124.686048	59.154010
2362.894803	116.214078	59.159015
2361.732822	124.764715	59.164020
2361.215851	126.308504	59.169025
2360.429458	127.663500	59.174029
2358.997739	130.296027	59.179034
2358.889946	112.994164	59.184039
2357.659072	122.449438	59.189044
2357.823432	116.491503	59.194049
2357.405365	123.591445	59.199053
2356.552949	126.588717	59.204058
2355.675485	116.878286	59.209063
2354.604774	128.601086	59.214068
2354.410185	124.809175	59.219073
2353.753556	124.564285	59.224077
2353.009352	122.499706	59.229082
2352.574091	115.040153	59.234087
2350.912598	121.053673	59.239092
2350.745562	119.467095	59.244097
2350.534053	123.028177	59.249101
2349.796132	125.789172	59.254106
2349.976308	122.645260	59.259111
2348.558437	121.817665	59.264116
2348.077773	115.992125	59.269121
2347.221773	124.563468	59.274125
2346.100060	126.796426	59.279130
2345.505622	122.359625	59.284135
2344.812724	130.822166	59.289140
2344.085032	126.453936	59.294145
2343.584932	123.550678	59.299149
2343.170187	134.080576	59.304154
2343.222246	119.970328	59.309159
2341.771909	138.062132	59.314164
2341.271966	127.726248	59.319169
2340.718382	140.236916	59.324173
2340.188424	131.439260	59.329178
2339.303989	124.233736	59.334183
2338.254928	132.345484	59.339188
2337.862863	127.223973	59.344193
2337.256819	123.580573	59.349197
2336.765803	125.067033	59.354202
2335.522432	124.947338	59.359207
2334.777366	125.188868	59.364212
2334.361306	121.474301	59.369217
2334.310697	123.888442	59.374221
2333.638749	133.445912	59.379226
2332.908667	122.406124	59.384231
2331.770218	131.673505	59.389236
2330.950230	121.076179	59.394241
2330.350269	132.120488	59.399245
2329.988453	127.400764	59.404250
2329.012896	123.432537	59.409255
2327.980569	135.732177	59.414260
2327.480656	134.065549	59.419265
2327.465268	135.392529	59.424269
2326.874069	128.241862	59.429274
2326.491955	120.380080	59.434279
2325.008266	136.277019	59.439284
2323.827223	125.752481	59.444289
2323.740092	130.099501	59.449293
2322.770811	127.190816	59.454298
2322.913545	126.926479	59.459303
2322.092348	134.565863	59.464308
2322.114679	122.682584	59.469313
2320.748583	134.113280	59.474317
2319.895996	136.568241	59.479322
2319.539299	125.982878	59.484327
2319.021446	134.944023	59.489332
2317.725403	126.850106	59.494337
2317.334752	119.326878	59.499341
2316.372098	129.813886	59.504346
2316.643478	120.976714	59.509351
2315.670140	121.357934	59.514356
2314.437292	123.225047	59.519361
2313.726785	124.716672	59.524365
2313.245616	125.294382	59.529370
2313.275182	124.700857	59.534375
2312.306780	121.837023	59.539380
2311.350213	114.967121	59.544385
2310.318439	123.984952	59.549389
2309.816722	125.528505	59.554394
2309.184467	118.202111	59.559399
2308.670544	135.574082	59.564404
2308.596967	123.601023	59.569409
2307.526347	120.134168	59.574413
2306.094387	132.157155	59.579418
2305.884245	126.438117	59.584423
2305.138981	132.821542	59.589428
2305.324520	125.694768	59.594433
2304.731581	124.442718	59.599437
2303.638558	127.928358	59.604442
2303.004315	121.300170	59.609447
2302.329818	130.354805	59.614452
2301.727302	126.150302	59.619457
2300.281636	125.914817	59.624461
2299.532895	124.006148	59.629466
2299.221870	117.584788	59.634471
2298.600680	123.000059	59.639476
2298.326946	129.742574	59.644481
2297.928468	123.622733	59.649485
2297.375812	126.584150	59.654490
2296.527029	126.428174	59.659495
2295.605492	127.691029	59.664500
2295.203088	121.217007	59.669505
2294.010734	124.799367	59.674509
2293.073447	126.399244	59.679514
2292.452365	128.687916	59.684519
2292.044365	130.540695	59.689524
2291.614808	120.074375	59.694529
2291.523979	125.595134	59.699533
2290.710270	133.988735	59.704538
2289.927943	121.619000	59.709543
2288.874805	125.966207	59.714548
2288.377832	125.666788	59.719553
2287.862741	125.636115	59.724557
2286.569090	123.872333	59.729562
2286.444884	125.195815	59.734567
2285.568189	127.763450	59.739572
2285.632773	124.952317	59.744577
2284.423548	121.746790	59.749581
2283.396609	125.885447	59.754586
2283.182665	117.189293	59.759591
2282.560941	120.014105	59.764596
2281.939597	118.018131	59.769601
2281.062110	122.950277	59.774605
2279.927300	126.044793	59.779610
2280.073943	118.837046	59.784615
2279.003740	127.079512	59.789620
2278.299389	118.798386	59.794625
2277.304750	118.626304	59.799629
2276.143591	116.696981	59.804634
2276.516173	128.251535	59.809639
2275.964770	130.096469	59.814644
2275.456376	124.501064	59.819649
2275.007366	121.441059	59.824653
2273.765680	126.019449	59.829658
2272.943938	123.724204	59.834663
2272.627032	116.048248	59.839668
2271.989677	120.846573	59.844673
2271.204785	124.697536	59.849677
2269.791442	128.709253	59.854682
2269.308373	118.421423	59.859687
2268.643842	126.027307	59.864692
2268.310081	119.913378	59.869697
2268.292812	120.658860	59.874701
2267.629629	122.627904	59.879706
2266.801088	125.700049	59.884711
2265.852632	123.516470	59.889716
2265.236860	122.142809	59.894721
2264.977920	118.756631	59.899725
2263.821298	125.318946	59.904730
2263.284412	118.451101	59.909735
2262.381712	121.591583	59.914740
2261.733129	120.158009	59.919745
2261.587993	119.040961	59.924750
2260.361526	127.389489	59.929754
2259.900064	119.589442	59.934759
2258.862804	119.145190	59.939764
2258.491759	126.229591	59.944769
2258.347265	114.962592	59.949774
2257.379896	122.571710	59.954778
2256.585802	118.131172	59.959783
2255.647491	123.182664	59.964788
2255.023255	123.075531	59.969793
2254.963582	120.446299	59.974798
2254.064174	127.517635	59.979802
2253.017286	117.117811	59.984807
2252.035887	128.432598	59.989812
2251.594447	122.803643	59.994817
2251.509684	120.820123	59.999822
2250.795933	126.898962	60.004826
2250.539996	123.240704	60.009831
2249.296878	123.157694	60.014836
2248.342269	125.820364	60.019841
2248.180370	112.787602	60.024846
2247.383660	121.752215	60.029850
2247.109006	121.183477	60.034855
2245.812831	119.867356	60.039860
2245.250815	116.533797	60.044865
2244.614645	123.763005	60.049870
2244.064638	125.495207	60.054874
2243.987054	114.459127	60.059879
2242.732408	122.321836	60.064884
2242.003161	134.418474	60.069889
2241.925644	129.106219	60.074894
2240.516677	129.044861	60.079898
2239.718641	115.520905	60.084903
2238.980777	125.888162	60.089908
2238.590318	120.104446	60.094913
2238.475024	129.042140	60.099918
2237.979233	123.716153	60.104922
2237.374492	115.716018	60.109927
2236.372063	119.787729	60.114932
2235.302293	126.334012	60.119937
2234.688916	115.213905	60.124942
2233.677585	121.312449	60.129946
2232.991501	119.422284	60.134951
2232.357467	126.428901	60.139956
2232.195015	122.423882	60.144961
2231.723937	112.314006	60.149966
2231.068750	121.209026	60.154970
2230.787127	113.967156	60.159975
2229.481240	124.423259	60.164980
2228.526940	120.866665	60.169985
2228.165815	119.239471	60.174990
2227.335453	127.354879	60.179994
2227.122454	116.435900	60.184999
2226.099743	116.139949	60.190004
2225.474841	114.642333	60.195009
2225.287954	114.631327	60.200014
2224.630467	129.713590	60.205018
2223.847620	124.658132	60.210023
2222.586717	125.302482	60.215028
2222.326064	128.929992	60.220033
2221.957974	119.959033	60.225038
2220.710742	123.443820	60.230042
2220.087385	120.199303	60.235047
2219.425068	120.992333	60.240052
2218.892053	122.485194	60.245057
2218.836789	120.915822	60.250062
2217.502383	123.272803	60.255066
2216.515540	123.865945	60.260071
2215.494944	120.493974	60.265076
2215.162997	124.877328	60.270081
2214.783146	117.047151	60.275086
2214.397139	127.644753	60.280090
2214.177908	123.238936	60.285095
2213.726883	127.012681	60.290100
2212.489519	126.142017	60.295105
2211.881961	116.994127	60.300110
2211.200806	123.649211	60.305114
2210.220571	113.958369	60.310119
2209.070383	118.922551	60.315124
2208.425764	121.870885	60.320129
2207.990239	118.314787	60.325134
2207.593457	129.974452	60.330138
2207.442382	121.338998	60.335143
2207.155029	119.841684	60.340148
2206.688076	125.493863	60.345153
2205.692544	122.438515	60.350158
2204.535799	123.065451	60.355162
2203.221964	113.049176	60.360167
2202.602808	117.396780	60.365172
2201.858028	123.986959	60.370177
2201.712426	114.668497	60.375182
2201.363782	124.817621	60.380186
2200.941723	118.269610	60.385191
2199.975607	122.566422	60.390196
2198.515766	120.492414	60.395201
2198.408281	114.277435	60.400206
2197.811226	121.148258	60.405210
2197.654557	114.693411	60.410215
2196.651921	122.756967	60.415220
2195.665138	114.370615	60.420225
2195.481760	116.889560	60.425230
2194.902251	123.349243	60.430234
2193.914859	124.389306	60.435239
2192.573434	128.877009	60.440244
2192.323745	122.261233	60.445249
2192.166766	118.386724	60.450254
2191.831873	122.039560	60.455258
2190.901539	116.828946	60.460263
2189.710871	114.532074	60.465268
2188.921390	121.610666	60.470273
2188.533049	123.815337	60.475278
2188.032199	130.357488	60.480282
2186.950933	121.869271	60.485287
2186.340408	120.255127	60.490292
2185.166510	120.975391	60.495297
2184.797653	114.613672	60.500302
2184.238356	124.016090	60.505306
2184.329263	121.376108	60.510311
2183.694890	118.995550	60.515316
2183.083527	122.104376	60.520321
2182.390629	115.213098	60.525326
2181.242744	123.901075	60.530330
2180.617208	121.489796	60.535335
2180.108326	118.927126	60.540340
2179.049475	118.107256	60.545345
2178.735991	120.891599	60.550350
2178.046093	127.511472	60.555354
2177.800479	124.333013	60.560359
2176.667109	116.731175	60.565364
2175.412118	119.369834	60.570369
2175.200714	113.929307	60.575374
2174.739405	127.643863	60.580378
2174.717594	118.909338	60.585383
2173.388475	121.209768	60.590388
2172.146249	125.401442	60.595393
2172.186913	121.297747	60.600398
2171.206219	129.027966	60.605402
2171.265920	116.617683	60.610407
2170.487580	123.507274	60.615412
2169.197091	124.933110	60.620417
2168.963117	122.812090	60.625422
2168.142637	126.943087	60.630426
2167.214811	121.507847	60.635431
2166.257988	125.328227	60.640436
2165.659023	128.252969	60.645441
2165.327622	124.260270	60.650446
2164.908143	131.957273	60.655450
2164.426626	125.674817	60.660455
2164.182584	127.903756	60.665460
2162.925394	120.660187	60.670465
2161.956493	123.126375	60.675470
2161.439310	127.679956	60.680474
2161.099985	123.092585	60.685479
2159.983234	124.138199	60.690484
2159.338599	129.226714	60.695489
2158.885256	122.117634	60.700494
2158.162301	125.532509	60.705498
2157.787554	121.586696	60.710503
2156.927558	122.480641	60.715508
2155.875952	127.658097	60.720513
2155.656891	116.146902	60.725518
2154.575728	120.317349	60.730522
2154.587174	122.277604	60.735527
2154.079376	120.000529	60.740532
2152.625264	116.864152	60.745537
2152.336599	120.310144	60.750542
2151.427623	128.230985	60.755546
2151.092999	121.884728	60.760551
2150.356457	121.598269	60.765556
2149.316683	118.402480	60.770561
2148.930939	111.784324	60.775566
2148.082222	117.760727	60.780570
2148.014966	113.009600	60.785575
2147.154434	115.027011	60.790580
2145.827189	123.273582	60.795585
2145.439510	112.280681	60.800590
2144.591267	119.181043	60.805594
2144.282176	125.866444	60.810599
2144.111882	123.107720	60.815604
2143.240739	126.071512	60.820609
2142.472466	123.704385	60.825614
2141.666947	122.035968	60.830618
2141.323608	116.916415	60.835623
2140.222665	116.298743	60.840628
2138.946573	118.902729	60.845633
2138.640475	116.944831	60.850638
2138.341268	120.470385	60.855642
2137.881392	112.706801	60.860647
2137.411451	120.641366	60.865652
2137.029779	119.005062	60.870657
2136.131795	117.052078	60.875662
2135.259808	114.277973	60.880666
2134.415362	115.494116	60.885671
2133.315681	110.601810	60.890676
2132.374409	111.575182	60.895681
2131.958980	114.539586	60.900686
2131.331669	120.361289	60.905690
2130.934034	112.374307	60.910695
2130.796768	121.917299	60.915700
2130.484322	125.029479	60.920705
2129.655689	113.798587	60.925710
2128.727691	112.026783	60.930714
2128.227948	119.394890	60.935719
2127.324291	117.009080	60.940724
2126.174538	120.388007	60.945729
2125.747617	116.776371	60.950734
2125.128939	130.203643	60.955738
2124.825420	118.389541	60.960743
2123.749767	114.764914	60.965748
2122.784650	115.120288	60.970753
2122.701473	116.600956	60.975758
2121.970495	118.925410	60.980762
2121.246710	117.104866	60.985767
2120.640712	119.505441	60.990772
2119.404906	123.190785	60.995777
2119.084163	117.521868	61.000782
2118.305487	118.420068	61.005786
2118.133270	120.913422	61.010791
2117.560923	120.924135	61.015796
2116.383884	119.622407	61.020801
2115.874987	112.094174	61.025806
2115.246003	121.543638	61.030810
2115.344772	111.386456	61.035815
2114.173656	104.971309	61.040820
2113.101401	118.075504	61.045825
2112.522878	124.475025	61.050830
2111.877290	124.219987	61.055834
2111.412315	116.805815	61.060839
2110.771600	117.702920	61.065844
2109.761896	121.415909	61.070849
2108.899931	120.818157	61.075854
2108.552867	123.374177	61.080858
2107.958381	115.306001	61.085863
2107.797827	118.652718	61.090868
2106.562041	112.575064	61.095873
2105.923690	107.165726	61.100878
2105.076957	112.615236	61.105882
2104.573536	109.405882	61.110887
2104.707277	115.883310	61.115892
2103.447250	120.984711	61.120897
2102.555997	123.505125	61.125902
2101.852281	120.610276	61.130906
2101.695025	110.603458	61.135911
2101.010460	113.086941	61.140916
2099.706207	117.786582	61.145921
2099.045906	113.302273	61.150926
2098.533745	119.035208	61.155930
2098.371406	115.440690	61.160935
2097.876766	122.756612	61.165940
2096.638185	116.406686	61.170945
2095.980019	114.926619	61.175950
2095.373987	109.137560	61.180954
2094.816142	114.396749	61.185959
2094.739536	110.788359	61.190964
2093.391557	116.220578	61.195969
2092.583190	115.066976	61.200974
2091.866852	116.361080	61.205978
2091.899106	125.095507	61.210983
2091.013484	115.814024	61.215988
2089.737468	120.670673	61.220993
2089.325589	116.581621	61.225998
2088.616443	118.796560	61.231002
2088.043991	112.435336	61.236007
2088.011332	115.708864	61.241012
2086.852896	118.265502	61.246017
2086.084356	111.766508	61.251022
2085.150542	121.519939	61.256026
2084.971763	113.677104	61.261031
2084.672772	112.358624	61.266036
2083.697600	114.838921	61.271041
2082.459592	112.047694	61.276046
2081.756489	112.621145	61.281050
2081.569253	113.555952	61.286055
2081.428820	110.978829	61.291060
2080.266440	119.047612	61.296065
2079.660884	110.433466	61.301070
2078.561303	117.356295	61.306074
2078.127386	114.571615	61.311079
2077.928836	115.036272	61.316084
2077.123959	126.515867	61.321089
2075.860656	113.952552	61.326094
2075.164137	118.569174	61.331098
2074.703254	110.670385	61.336103
2074.531498	112.890908	61.341108
2074.094856	123.987008	61.346113
2073.613055	118.653919	61.351118
2072.390575	117.933106	61.356122
2071.754142	108.381259	61.361127
2071.521321	104.820904	61.366132
2070.429760	119.908317	61.371137
2069.763623	107.775349	61.376142
2068.925414	113.122752	61.381146
2068.311712	113.595655	61.386151
2067.553340	115.282196	61.391156
2066.124518	116.954336	61.396161
2066.211660	111.445786	61.401166
2065.939868	114.376546	61.406170
2065.182597	116.411042	61.411175
2064.541518	116.259840	61.416180
2063.994851	113.165645	61.421185
2063.349259	110.263231	61.426190
2062.375356	109.150184	61.431194
2061.983475	116.004074	61.436199
2061.375352	108.662948	61.441204
2060.214550	109.420076	61.446209
2059.576830	107.538639	61.451214
2059.573084	115.737660	61.456218
2058.702202	111.024520	61.461223
2057.540680	116.795497	61.466228
2056.544129	112.995126	61.471233
2056.327392	103.214009	61.476238
2055.834388	113.006511	61.481242
2055.315427	112.312999	61.486247
2054.852166	114.356417	61.491252
2053.771596	117.341040	61.496257
2053.118368	110.163149	61.501262
2052.334040	120.384018	61.506266
2052.090371	115.318874	61.511271
2051.514254	113.429270	61.516276
2050.119141	112.592733	61.521281
2049.491800	111.380940	61.526286
2049.393302	111.236801	61.531290
2048.577957	110.966598	61.536295
2048.405425	109.468998	61.541300
2047.440262	121.170207	61.546305
2046.872897	105.799836	61.551310
2046.346389	119.163965	61.556314
2044.858687	116.668865	61.561319
2043.930795	106.347440	61.566324
2043.111406	119.330630	61.571329
2043.003132	111.035234	61.576334
2042.475838	112.357401	61.581338
2041.914363	117.374067	61.586343
2041.849166	114.389752	61.591348
2041.119778	120.804815	61.596353
2039.999852	114.579474	61.601358
2039.216197	118.127103	61.606362
2038.778797	118.375258	61.611367
2038.535661	110.124640	61.616372
2037.229391	116.907176	61.621377
2036.444661	112.526657	61.626382
2035.819161	121.281215	61.631386
2035.401062	117.342832	61.636391
2035.311242	120.623768	61.641396
2033.633200	122.721027	61.646401
2033.103484	119.471968	61.651406
2032.279729	121.852168	61.656410
2031.738940	115.084502	61.661415
2031.353001	111.253510	61.666420
2030.884078	116.411049	61.671425
2030.537904	118.118272	61.676430
2029.350028	116.881968	61.681434
2028.675424	123.418314	61.686439
2028.216091	115.630181	61.691444
2027.272341	124.454175	61.696449
2026.325248	108.214851	61.701454
2025.439522	113.201718	61.706458
2025.365886	114.245379	61.711463
2025.099936	111.525130	61.716468
2024.561181	119.684218	61.721473
2024.362378	108.197216	61.726478
2023.190842	115.063677	61.731482
2022.274422	122.811333	61.736487
2021.286841	106.696564	61.741492
2020.148115	122.474123	61.746497
2019.993777	116.454269	61.751502
2019.594315	119.475550	61.756506
2019.205913	112.891813	61.761511
2018.896012	116.083686	61.766516
2017.083939	120.099711	61.771521
2016.803492	110.337782	61.776526
2016.201171	116.668745	61.781530
2015.780596	119.539302	61.786535
2014.728593	123.290723	61.791540
2013.691471	133.261959	61.796545
2013.485510	107.494048	61.801550
2012.821707	114.476155	61.806554
2012.498749	118.381152	61.811559
2011.812334	116.630414	61.816564
2010.479991	118.506713	61.821569
2010.060447	108.848311	61.826574
2009.345547	115.390758	61.831578
2008.742366	115.467939	61.836583
2008.855111	115.316482	61.841588
2007.675549	120.980032	61.846593
2006.655642	126.780480	61.851598
2005.914905	119.355074	61.856602
2005.563174	118.607305	61.861607
2005.579065	110.178576	61.866612
2004.640352	116.027497	61.871617
2003.890391	106.677051	61.876622
2002.942754	104.692720	61.881626
2002.242233	111.786103	61.886631
2002.006599	110.559813	61.891636
2000.342784	123.061814	61.896641
2000.245671	111.163885	61.901646
1999.553722	110.151825	61.906650
1998.826696	112.288125	61.911655
1998.653657	113.223662	61.916660
1997.840901	122.070248	61.921665
1997.038346	105.653064	61.926670
1996.570169	113.847048	61.931674
1995.658202	106.825922	61.936679
1995.418887	108.403557	61.941684
1993.985377	110.485445	61.946689
1993.389656	108.603544	61.951694
1992.869680	118.638283	61.956698
1993.048265	113.971029	61.961703
1992.343129	106.000356	61.966708
1990.673745	117.640847	61.971713
1990.025305	111.664858	61.976718
1989.774668	106.659728	61.981722
1988.835146	118.620619	61.986727
1988.948853	112.832409	61.991732
1987.617254	119.525344	61.996737
1987.040609	120.475843	62.001742
1986.263875	113.854723	62.006746
1985.782270	117.516080	62.011751
1985.839732	111.163174	62.016756
1984.429896	120.743047	62.021761
1983.758345	108.077762	62.026766
1983.212651	110.776308	62.031770
1982.715400	103.222428	62.036775
1982.006225	116.798183	62.041780
1980.893105	115.927639	62.046785
1980.533206	118.863210	62.051790
1979.801926	123.055148	62.056794
1979.012493	119.444751	62.061799
1978.955176	121.234403	62.066804
1977.791063	127.262407	62.071809
1976.952053	116.456469	62.076814
1976.183470	115.965130	62.081818
1976.112046	113.324894	62.086823
1975.950749	112.413113	62.091828
1974.417053	119.600072	62.096833
1973.390219	112.487287	62.101838
1973.043061	124.933410	62.106842
1972.552278	119.999354	62.111847
1972.564523	120.544399	62.116852
1971.641924	122.341541	62.121857
1970.578537	114.783844	62.126862
1969.833026	115.618762	62.131866
1969.091923	119.512789	62.136871
1968.801905	107.848381	62.141876
1967.869674	116.554358	62.146881
1967.675185	108.156488	62.151886
1966.688814	107.938051	62.156890
1966.261538	110.126496	62.161895
1965.262682	109.794937	62.166900
1964.074334	111.623722	62.171905
1963.753427	103.504837	62.176910
1963.226602	109.845384	62.181914
1962.551273	116.369224	62.186919
1962.767558	114.423031	62.191924
1961.861566	112.392506	62.196929
1961.044493	112.092613	62.201934
1960.507161	113.024153	62.206938
1959.008531	111.734053	62.211943
1958.332975	103.259405	62.216948
1957.664433	115.334988	62.221953
1957.321165	111.311582	62.226958
1956.892993	109.155510	62.231962
1955.805885	111.097631	62.236967
1955.780214	107.448169	62.241972
1954.588855	117.464335	62.246977
1953.943719	116.548480	62.251982
1953.382406	117.220846	62.256986
1952.741671	114.791675	62.261991
1952.761313	109.791233	62.266996
1951.491316	117.088607	62.272001
1950.472840	110.658842	62.277006
1949.956390	107.757249	62.282010
1949.084443	115.393094	62.287015
1948.999503	115.540309	62.292020
1947.749682	112.849818	62.297025
1947.151360	114.528732	62.302030
1946.531127	117.963947	62.307034
1945.799599	111.519044	62.312039
1945.509537	111.868707	62.317044
1944.985753	122.261714	62.322049
1944.797317	115.934294	62.327054
1943.803820	119.267182	62.332058
1942.989540	128.686379	62.337063
1942.489316	112.396691	62.342068
1941.709501	111.878069	62.347073
1940.995096	106.964906	62.352078
1940.061074	111.871232	62.357082
1939.632942	114.470333	62.362087
1939.296862	113.495298	62.367092
1937.824609	113.836801	62.372097
1937.288176	109.723289	62.377102
1936.619210	111.379947	62.382106
1936.346368	110.452908	62.387111
1935.909696	111.962862	62.392116
1935.175429	113.314522	62.397121
1934.288175	106.959416	62.402126
1933.653271	109.190090	62.407130
1932.978238	113.660554	62.412135
1932.870019	116.274401	62.417140
1931.441916	116.861764	62.422145
1930.519686	112.293217	62.427150
1930.161572	115.003100	62.432154
1929.411835	112.908748	62.437159
1929.308034	109.891571	62.442164
1928.615102	110.437645	62.447169
1927.760097	105.817340	62.452174
1927.173678	111.561401	62.457178
1926.728837	122.049845	62.462183
1926.348352	109.328862	62.467188
1924.748425	122.155063	62.472193
1923.845095	110.851749	62.477198
1923.438439	120.756187	62.482202
1922.943816	117.591136	62.487207
1922.857665	111.787383	62.492212
1921.663423	114.955676	62.497217
1920.575017	100.777320	62.502222
1920.391544	104.378599	62.507226
1919.871937	102.341195	62.512231
1919.675710	108.039428	62.517236
1918.288723	112.797463	62.522241
1917.485769	108.160361	62.527246
1916.975257	102.457229	62.532250
1916.446548	111.127729	62.537255
1916.161496	105.480366	62.542260
1915.066314	115.910327	62.547265
1914.584845	110.127228	62.552270
1913.954140	110.003083	62.557274
1913.588318	110.229925	62.562279
1912.654287	102.479998	62.567284
1911.380748	111.423564	62.572289
1911.370324	105.019518	62.577294
1910.809449	108.050256	62.582298
1909.924937	109.062110	62.587303
1908.909856	103.467792	62.592308
1907.911376	116.894888	62.597313
1907.643178	111.546995	62.602318
1907.121310	108.710279	62.607322
1906.488417	112.111742	62.612327
1906.269616	108.818200	62.617332
1905.111277	115.498087	62.622337
1904.409696	114.812542	62.627342
1904.123730	114.100897	62.632346
1903.414769	118.437437	62.637351
1903.078608	109.330029	62.642356
1901.713345	116.753045	62.647361
1901.332113	113.428081	62.652366
1900.928058	114.861803	62.657370
1899.752218	116.166643	62.662375
1899.070234	108.749767	62.667380
1898.188699	112.169687	62.672385
1897.958713	120.135437	62.677390
1897.553517	118.727379	62.682394
1896.956886	118.578856	62.687399
1896.178767	108.517232	62.692404
1895.191092	111.916628	62.697409
1894.826553	110.522142	62.702414
1894.115573	107.683043	62.707418
1892.986418	108.268614	62.712423
1892.433967	108.943812	62.717428
1891.549594	103.965792	62.722433
1891.090310	104.049947	62.727438
1890.840103	102.784712	62.732442
1890.321630	113.732172	62.737447
1889.880686	103.386699	62.742452
1888.838550	116.821658	62.747457
1888.088556	111.748416	62.752462
1887.578494	115.620293	62.757466
1886.689937	108.341780	62.762471
1886.116369	101.306213	62.767476
1885.030074	113.272082	62.772481
1884.581544	104.050882	62.777486
1884.538796	102.672398	62.782490
1883.676026	108.895952	62.787495
1882.550261	98.741843	62.792500
1881.831298	110.451065	62.797505
1881.002077	97.206106	62.802510
1880.910764	104.880110	62.807514
1880.631935	99.080512	62.812519
1879.766374	89.161752	62.817524
1878.577358	98.995155	62.822529
1877.958524	100.874153	62.827534
1877.673527	95.976358	62.832538
1876.918502	104.740832	62.837543
1876.179667	100.613011	62.842548
1874.823975	108.058863	62.847553
1874.531395	97.896427	62.852558
1874.502445	104.415475	62.857562
1873.794414	110.727422	62.862567
1873.538646	103.090410	62.867572
1872.243188	106.394047	62.872577
1871.799909	105.211577	62.877582
1871.044978	106.603093	62.882586
1869.858391	106.842459	62.887591
1869.402834	104.761736	62.892596
1868.636039	107.980066	62.897601
1868.329135	105.203287	62.902606
1867.886208	109.924954	62.907610
1866.709819	107.562566	62.912615
1865.911423	98.927779	62.917620
1865.284310	107.023429	62.922625
1864.659736	106.780221	62.927630
1864.435324	106.619733	62.932634
1863.828968	105.939613	62.937639
1863.805209	95.584752	62.942644
1862.319608	107.169741	62.947649
1862.157998	103.051720	62.952654
1861.224015	101.419144	62.957658
1859.996499	101.729064	62.962663
1859.399088	96.205802	62.967668
1858.729327	104.873194	62.972673
1858.441333	100.701799	62.977678
1858.052233	102.410057	62.982682
1856.866385	112.937238	62.987687
1856.398936	96.142270	62.992692
1855.704880	100.408368	62.997697
1855.343227	106.468436	63.002702
1854.021263	94.063669	63.007706
1853.027034	102.765649	63.012711
1852.453706	97.165245	63.017716
1851.847704	98.547468	63.022721
1851.332173	97.436569	63.027726
1851.311417	99.196674	63.032730
1850.929632	105.656483	63.037735
1850.536105	109.152783	63.042740
1849.123170	115.005090	63.047745
1848.653618	104.534656	63.052750
1848.069521	98.049952	63.057754
1847.009376	106.205475	63.062759
1846.222612	98.201831	63.067764
1845.612908	104.174077	63.072769
1845.241003	105.871105	63.077774
1844.813900	109.610770	63.082778
1843.684813	109.275462	63.087783
1842.881349	106.187733	63.092788
1842.238427	112.657089	63.097793
1841.706075	115.261789	63.102798
1841.236389	110.622948	63.107802
1840.740272	110.711434	63.112807
1839.877652	108.985340	63.117812
1839.220375	114.752186	63.122817
1838.646396	108.407848	63.127822
1838.343257	106.700903	63.132826
1837.189359	119.069117	63.137831
1836.397860	102.485499	63.142836
1835.370632	101.908173	63.147841
1835.027134	114.024062	63.152846
1834.886466	106.213817	63.157850
1833.659985	107.849029	63.162855
1832.651131	111.637697	63.167860
1832.466591	115.664272	63.172865
1832.140017	118.518756	63.177870
1831.638469	103.347967	63.182874
1830.761766	111.443296	63.187879
1830.047910	109.679517	63.192884
1828.822660	115.955224	63.197889
1828.603402	113.413704	63.202894
1828.256173	107.928164	63.207898
1827.589413	104.408912	63.212903
1826.713998	101.824525	63.217908
1825.638067	114.199528	63.222913
1825.602880	102.056180	63.227918
1825.089380	103.831114	63.232922
1823.735701	109.364222	63.237927
1822.992190	100.600456	63.242932
1822.304423	111.104793	63.247937
1822.169500	112.359457	63.252942
1821.750819	107.112316	63.257946
1820.701489	114.230649	63.262951
1819.685939	110.022682	63.267956
1818.820108	115.975202	63.272961
1818.690545	104.432577	63.277966
1818.671309	102.240506	63.282970
1817.832646	110.392087	63.287975
1816.598325	104.872798	63.292980
1815.962325	109.608158	63.297985
1815.425106	104.691152	63.302990
1815.244016	107.509692	63.307994
1814.098302	115.403165	63.312999
1813.675417	105.497095	63.318004
1813.066107	113.546285	63.323009
1812.062427	110.340848	63.328014
1811.196048	113.445964	63.333018
1810.573460	117.476039	63.338023
1810.315347	105.164786	63.343028
1809.481119	104.617996	63.348033
1809.050718	111.926479	63.353038
1807.647728	102.415845	63.358042
1807.233482	109.926817	63.363047
1806.612324	103.357674	63.368052
1806.377457	113.067720	63.373057
1805.994551	104.004247	63.378062
1805.041192	108.092883	63.383066
1803.571175	109.262554	63.388071
1803.477938	105.335725	63.393076
1803.300571	109.551720	63.398081
1802.324001	112.538328	63.403086
1801.483716	105.607614	63.408090
1800.737414	114.141273	63.413095
1800.466298	103.075611	63.418100
1799.662246	112.410164	63.423105
1798.499881	107.772606	63.428110
1798.057116	114.608755	63.433114
1797.038997	109.883757	63.438119
1797.016753	105.535066	63.443124
1796.449442	116.016824	63.448129
1795.700257	108.555417	63.453134
1795.504622	108.648549	63.458138
1794.124618	110.099257	63.463143
1793.848850	107.769898	63.468148
1793.421626	114.031441	63.473153
1792.261820	117.054137	63.478158
1791.635516	109.806959	63.483162
1791.044593	111.892366	63.488167
1790.458836	103.025041	63.493172
1788.940724	110.130425	63.498177
1788.144306	109.589405	63.503182
1788.185901	105.422020	63.508186
1787.265022	105.804225	63.513191
1786.669194	106.870914	63.518196
1786.320466	113.257573	63.523201
1786.365122	108.123393	63.528206
1785.963575	104.795209	63.533210
1784.107301	117.359380	63.538215
1783.906476	109.943887	63.543220
1783.201750	111.708518	63.548225
1781.842715	113.698773	63.553230
1781.248004	114.530809	63.558234
1780.732415	118.084706	63.563239
1780.248474	110.076629	63.568244
1779.842554	119.244786	63.573249
1779.518652	115.025068	63.578254
1779.358168	111.867998	63.583258
1777.990211	120.542361	63.588263
1777.337918	107.624768	63.593268
1775.981551	110.600573	63.598273
1775.270071	108.725876	63.603278
1775.026368	100.516841	63.608282
1774.117593	110.312974	63.613287
1774.046742	108.959431	63.618292
1773.344370	106.124406	63.623297
1772.807436	107.944405	63.628302
1772.026258	108.661904	63.633306
1771.031741	112.164326	63.638311
1770.611083	111.159171	63.643316
1769.953818	101.598329	63.648321
1768.933765	104.983151	63.653326
1768.374941	107.172010	63.658330
1767.477812	116.859975	63.663335
1767.151475	108.798885	63.668340
1766.925331	113.252163	63.673345
1765.967477	107.374154	63.678350
1765.494228	106.218136	63.683354
1764.765132	115.101731	63.688359
1763.967039	108.907455	63.693364
1762.392648	105.488636	63.698369
1762.109312	113.165492	63.703374
1761.930377	105.274570	63.708378
1761.137894	111.110340	63.713383
1760.646656	103.104702	63.718388
1760.051429	108.311487	63.723393
1759.785463	115.854721	63.728398
1758.892300	114.009531	63.733402
1758.017851	109.651523	63.738407
1757.548654	106.966859	63.743412
1756.760985	110.478496	63.748417
1755.691482	119.275473	63.753422
1755.450789	113.544750	63.758426
1754.712897	109.112855	63.763431
1754.104824	112.010766	63.768436
1753.018896	105.562991	63.773441
1751.845045	114.320586	63.778446
1751.530934	106.230172	63.783450
1750.809185	114.854760	63.788455
1750.676810	106.741936	63.793460
1750.660166	110.232965	63.798465
1749.958834	116.000249	63.803470
1748.923678	108.271612	63.808474
1747.968502	108.481279	63.813479
1747.588098	109.205602	63.818484
1746.786580	106.458199	63.823489
1745.549668	117.447664	63.828494
1745.024080	110.125239	63.833498
1744.707249	108.434064	63.838503
1744.268465	107.455301	63.843508
1743.584197	113.865424	63.848513
1742.551478	104.414613	63.853518
1741.961957	101.084651	63.858522
1741.434345	106.564459	63.863527
1741.074415	107.707233	63.868532
1740.484375	104.988777	63.873537
1739.118201	111.157167	63.878542
1738.692765	104.232064	63.883546
1737.915894	113.646835	63.888551
1737.758070	109.339500	63.893556
1737.321723	109.715386	63.898561
1736.145631	108.548185	63.903566
1735.524248	104.300824	63.908570
1734.972921	113.857786	63.913575
1734.329503	103.717899	63.918580
1733.212018	107.874492	63.923585
1732.589429	114.866140	63.928590
1732.084093	102.324059	63.933594
1731.445019	107.296780	63.938599
1731.220211	103.377468	63.943604
1730.215950	109.314998	63.948609
1729.111707	106.957273	63.953614
1728.875990	92.026024	63.958618
1728.021902	108.679703	63.963623
1727.725461	106.143107	63.968628
1727.230714	106.515567	63.973633
1726.142773	111.486541	63.978638
1725.498302	101.477490	63.983642
1724.735619	105.290365	63.988647
1724.420892	100.866597	63.993652
1723.651873	103.759285	63.998657
1722.602094	112.906950	64.003662
1722.040812	100.038935	64.008666
1721.012718	106.874578	64.013671
1721.110248	100.306426	64.018676
1720.739013	100.227905	64.023681
1720.053259	109.081979	64.028686
1719.203028	103.216752	64.033690
1718.234697	111.655777	64.038695
1718.067282	103.355542	64.043700
1716.910620	115.402146	64.048705
1715.678279	106.500605	64.053710
1715.465920	96.413282	64.058714
1714.812971	99.568729	64.063719
1714.513203	102.430468	64.068724
1714.075789	105.150372	64.073729
1713.100399	109.485936	64.078734
1712.402084	100.717621	64.083738
1711.661710	108.232685	64.088743
1711.539668	98.722774	64.093748
1710.350348	102.785482	64.098753
1709.130337	109.830404	64.103758
1708.994231	98.989148	64.108762
1708.166255	105.091112	64.113767
1708.044281	105.661883	64.118772
1707.592981	110.372357	64.123777
1706.526842	105.048129	64.128782
1706.097136	107.370025	64.133786
1705.487670	107.702118	64.138791
1704.197169	105.321007	64.143796
1703.705981	109.166770	64.148801
1702.539232	116.429545	64.153806
1702.387815	104.034534	64.158810
1702.119949	102.099733	64.163815
1701.570633	103.900936	64.168820
1700.528041	103.599806	64.173825
1699.415558	99.805147	64.178830
1699.320737	94.628529	64.183834
1698.893090	108.070053	64.188839
1697.425282	108.814658	64.193844
1696.768239	110.890467	64.198849
1696.275188	103.899575	64.203854
1696.380336	107.464890	64.208858
1695.769217	102.667911	64.213863
1694.924969	106.538560	64.218868
1694.257954	106.601436	64.223873
1693.434812	101.003146	64.228878
1692.204864	102.225317	64.233882
1691.359742	99.259213	64.238887
1690.701333	100.979615	64.243892
1690.288466	101.916723	64.248897
1689.431015	109.176308	64.253902
1689.328322	96.279572	64.258906
1688.931880	102.776227	64.263911
1688.082919	102.586039	64.268916
1687.329406	102.214923	64.273921
1686.481983	113.172087	64.278926
1686.341662	106.443721	64.283930
1685.335183	108.935356	64.288935
1684.271977	104.083110	64.293940
1683.884699	97.518972	64.298945
1683.068602	103.049722	64.303950
1683.228410	95.273739	64.308954
1682.238792	100.910755	64.313959
1680.949640	105.060811	64.318964
1680.721453	104.541784	64.323969
1680.117586	102.223973	64.328974
1679.705141	100.057346	64.333978
1678.701928	101.727411	64.338983
1677.462035	103.371266	64.343988
1676.968052	108.354690	64.348993
1676.468376	114.183390	64.353998
1676.380202	104.015612	64.359002
1675.748043	104.346854	64.364007
1675.187587	103.127219	64.369012
1674.003919	101.303730	64.374017
1673.398250	101.427161	64.379022
1673.047753	100.694996	64.384026
1671.793711	97.749527	64.389031
1670.942715	102.657465	64.394036
1670.499669	99.110223	64.399041
1670.135706	108.791429	64.404046
1670.116567	97.766753	64.409050
1669.086927	106.819004	64.414055
1667.898605	95.415733	64.419060
1667.816443	94.608839	64.424065
1666.654515	107.049087	64.429070
1666.144300	102.762980	64.434074
1665.371025	98.282688	64.439079
1664.566231	96.045837	64.444084
1664.109200	97.021292	64.449089
1663.505772	106.578875	64.454094
1663.082658	103.337286	64.459098
1662.038265	101.300504	64.464103
1661.153566	96.949800	64.469108
1660.937699	97.918329	64.474113
1660.161183	102.494592	64.479118
1660.269528	104.286286	64.484122
1659.084020	111.041116	64.489127
1658.127563	103.198782	64.494132
1658.227098	95.195495	64.499137
1656.568785	101.825971	64.504142
1656.005102	97.886499	64.509146
1655.099102	96.262596	64.514151
1654.752657	103.715781	64.519156
1654.509234	96.013929	64.524161
1653.762546	103.975710	64.529166
1653.019825	100.004509	64.534170
1652.055563	107.058963	64.539175
1651.409289	106.853045	64.544180
1651.014585	102.617040	64.549185
1650.370059	110.249122	64.554190
1649.538951	100.371889	64.559194
1648.697032	102.204218	64.564199
1647.926083	102.213440	64.569204
1647.800054	102.216118	64.574209
1647.131934	99.053560	64.579214
1646.919888	90.388364	64.584218
1645.290048	107.286092	64.589223
1644.860568	100.491955	64.594228
1644.532402	100.595929	64.599233
1643.730698	106.634985	64.604238
1642.948698	102.740766	64.609242
1641.924213	98.972905	64.614247
1641.149669	111.162931	64.619252
1640.713590	101.442699	64.624257
1640.387245	104.361880	64.629262
1640.543898	101.874071	64.634266
1639.236327	115.268808	64.639271
1638.302192	102.382906	64.644276
1637.724496	100.249692	64.649281
1637.001177	103.381664	64.654286
1636.767313	98.888808	64.659290
1635.039664	105.539444	64.664295
1634.491552	101.042733	64.669300
1634.311833	98.039749	64.674305
1633.781632	100.230035	64.679310
1633.792798	99.971617	64.684314
1632.960187	100.951740	64.689319
1631.894586	96.562923	64.694324
1631.021572	92.061813	64.699329
1630.268007	97.406217	64.704334
1630.343446	91.869697	64.709338
1629.340723	101.954660	64.714343
1628.526302	98.743722	64.719348
1628.033314	91.534953	64.724353
1626.832794	107.847272	64.729358
1625.876177	103.607954	64.734362
1625.129153	107.337638	64.739367
1624.687710	105.036644	64.744372
1624.368843	100.417420	64.749377
1623.957029	107.562861	64.754382
1623.720560	100.795301	64.759386
1623.258884	100.901202	64.764391
1622.230683	106.276816	64.769396
1621.860153	105.130472	64.774401
1620.278353	106.046965	64.779406
1619.572608	103.171098	64.784410
1618.653572	103.960365	64.789415
1618.224734	107.615866	64.794420
1618.079204	97.937890	64.799425
1617.596344	105.695457	64.804430
1616.934254	91.850827	64.809434
1615.935632	104.378783	64.814439
1615.214418	101.630295	64.819444
1615.248216	104.280622	64.824449
1613.725483	107.723068	64.829454
1612.697566	95.500960	64.834458
1612.279161	106.261952	64.839463
1611.713793	103.107077	64.844468
1611.637574	103.733569	64.849473
1611.048123	98.257933	64.854478
1610.708365	97.477753	64.859482
1609.203917	94.392397	64.864487
1608.901326	97.195413	64.869492
1608.428800	98.561925	64.874497
1606.689557	98.235954	64.879502
1606.339743	88.925690	64.884506
1605.872109	103.927652	64.889511
1605.467892	98.496104	64.894516
1605.196869	94.426433	64.899521
1604.042913	107.477528	64.904526
1603.397528	90.705979	64.909530
1602.811457	103.322804	64.914535
1602.474097	104.292784	64.919540
1601.480030	100.363814	64.924545
1600.374410	105.423485	64.929550
1599.759853	98.184603	64.934554
1599.915930	101.593571	64.939559
1599.259246	97.248465	64.944564
1598.186915	105.007830	64.949569
1597.321232	109.754484	64.954574
1596.782200	103.241192	64.959578
1596.034906	109.049901	64.964583
1595.443902	107.373289	64.969588
1594.651082	101.527081	64.974593
1593.930594	105.503267	64.979598
1593.509301	104.463501	64.984602
1592.517226	103.677719	64.989607
1592.053121	108.993911	64.994612
1591.757922	96.044084	64.999617
1590.749736	105.417523	65.004622
1590.245402	105.963337	65.009626
1589.244436	98.040619	65.014631
1588.688182	98.434669	65.019636
1588.675287	101.299817	65.024641
1587.536868	108.375792	65.029646
1586.779021	101.659960	65.034650
1585.755785	104.820366	65.039655
1585.672188	112.571583	65.044660
1585.319007	104.474066	65.049665
1584.147619	110.034050	65.054670
1583.335861	107.244615	65.059674
1582.627124	107.306751	65.064679
1582.454575	103.470873	65.069684
1582.069335	103.982098	65.074689
1580.777083	106.564099	65.079694
1580.091726	100.713714	65.084698
1579.493938	111.934069	65.089703
1578.828341	104.603269	65.094708
1578.726940	101.091516	65.099713
1577.867196	104.313152	65.104718
1576.979521	104.042770	65.109722
1576.845993	99.645244	65.114727
1575.705769	101.388507	65.119732
1574.516100	102.018841	65.124737
1574.145087	107.271736	65.129742
1573.636433	93.157714	65.134746
1573.255753	103.026107	65.139751
1572.370900	108.991378	65.144756
1571.434035	97.704574	65.149761
1570.862351	102.740373	65.154766
1570.424238	99.461891	65.159770
1569.411151	110.555166	65.164775
1569.361266	112.488798	65.169780
1568.719293	99.319251	65.174785
1567.319647	102.695647	65.179790
1566.852687	100.789401	65.184794
1566.486960	106.034286	65.189799
1565.919335	102.969800	65.194804
1565.604707	101.955202	65.199809
1564.215190	106.663220	65.204814
1564.026119	97.586752	65.209818
1563.227238	101.010331	65.214823
1562.166906	105.415712	65.219828
1561.360763	99.346408	65.224833
1560.865662	101.177027	65.229838
1560.516486	107.875981	65.234842
1559.979909	109.291351	65.239847
1559.379794	109.227933	65.244852
1558.233319	99.735467	65.249857
1557.222960	105.588012	65.254862
1557.130573	98.147679	65.259866
1556.558169	96.767086	65.264871
1556.222654	102.282312	65.269876
1555.336860	102.949459	65.274881
1554.029251	104.226792	65.279886
1553.704821	95.652677	65.284890
1553.450353	98.407199	65.289895
1552.844830	106.046028	65.294900
1552.083761	98.587898	65.299905
1551.073625	104.638554	65.304910
1550.858584	96.129794	65.309914
1550.201280	98.150005	65.314919
1548.890228	104.217817	65.319924
1548.500561	97.360833	65.324929
1547.605613	101.920272	65.329934
1547.024534	99.587528	65.334938
1546.779949	98.663177	65.339943
1546.242837	103.891604	65.344948
1545.033124	102.467716	65.349953
1544.101412	108.607974	65.354958
1543.764150	96.618991	65.359962
1543.451865	107.060651	65.364967
1542.927371	105.716463	65.369972
1542.210504	99.115595	65.374977
1540.946381	113.171555	65.379982
1540.356720	111.867333	65.384986
1540.174303	101.086918	65.389991
1539.362897	112.003189	65.394996
1538.621257	112.621591	65.400001
1537.614510	108.855849	65.405006
1537.314816	109.380462	65.410010
1536.966389	105.908616	65.415015
1536.354443	106.762969	65.420020
1535.389804	103.192116	65.425025
1534.234648	102.652928	65.430030
1534.091062	104.274979	65.435034
1533.778102	108.432469	65.440039
1533.337746	103.612215	65.445044
1532.139204	104.409069	65.450049
1531.446343	114.075511	65.455054
1530.935732	104.842107	65.460058
1529.953935	112.446261	65.465063
1528.975332	110.989140	65.470068
1528.321821	106.294570	65.475073
1527.485454	107.612441	65.480078
1527.528930	109.591275	65.485082
1527.070263	105.183477	65.490087
1526.617313	100.174337	65.495092
1525.726902	95.203357	65.500097
1524.662179	112.754354	65.505102
1524.530519	99.582350	65.510106
1523.202994	102.123428	65.515111
1522.240631	105.282506	65.520116
1521.926442	102.992902	65.525121
1521.364434	102.786789	65.530126
1521.020052	106.404947	65.535130
1520.798562	106.877100	65.540135
1519.553470	106.301203	65.545140
1518.803351	106.313590	65.550145
1517.932589	106.153608	65.555150
1517.792890	105.451296	65.560154
1516.677774	104.396469	65.565159
1515.800611	107.665698	65.570164
1515.455066	104.923193	65.575169
1514.559867	112.285171	65.580174
1514.443377	101.638733	65.585178
1514.160609	101.633108	65.590183
1512.714303	99.160696	65.595188
1512.239662	99.033180	65.600193
1511.453136	110.184391	65.605198
1511.136646	101.659839	65.610202
1510.586856	103.295753	65.615207
1509.573054	110.978803	65.620212
1509.006045	106.404031	65.625217
1508.095535	104.624620	65.630222
1508.060195	102.509914	65.635226
1506.983802	98.946748	65.640231
1506.331688	100.916737	65.645236
1505.924211	97.942083	65.650241
1505.261133	97.556306	65.655246
1503.836014	102.928026	65.660250
1503.148159	106.701672	65.665255
1502.523316	107.934795	65.670260
1502.390797	105.031893	65.675265
1501.796379	103.552053	65.680270
1501.496822	100.655634	65.685274
1500.348043	108.867417	65.690279
1499.405400	105.652000	65.695284
1499.208716	94.156443	65.700289
1498.774565	99.517242	65.705294
1497.944082	108.520033	65.710298
1497.005457	102.378684	65.715303
1496.299759	109.259832	65.720308
1496.162947	102.234849	65.725313
1494.639596	107.881135	65.730318
1493.996838	105.248311	65.735322
1493.557202	97.550062	65.740327
1492.395710	104.678154	65.745332
1492.298361	91.111888	65.750337
1491.945021	101.135063	65.755342
1491.436968	100.238439	65.760346
1491.087355	95.233330	65.765351
1489.793984	111.042103	65.770356
1489.431353	98.618151	65.775361
1488.351446	115.408764	65.780366
1487.171294	107.199779	65.785370
1486.365584	102.550608	65.790375
1486.105085	108.702307	65.795380
1486.059485	99.987327	65.800385
1485.668987	106.034964	65.805390
1485.095959	97.522352	65.810394
1484.021741	103.919887	65.815399
1482.493336	101.671918	65.820404
1482.696703	94.290313	65.825409
1481.877608	100.567609	65.830414
1481.387497	104.065453	65.835418
1480.325005	100.261111	65.840423
1479.583201	113.173395	65.845428
1479.432598	92.345957	65.850433
1478.716258	96.203027	65.855438
1478.245838	94.728809	65.860442
1477.012531	93.050833	65.865447
1476.386072	107.098311	65.870452
1476.194481	101.738542	65.875457
1475.260990	106.877716	65.880462
1474.569807	95.439164	65.885466
1474.009431	99.749518	65.890471
1473.186114	107.447334	65.895476
1473.091130	95.954110	65.900481
1471.684558	99.945892	65.905486
1470.784490	103.331145	65.910490
1470.081219	96.822699	65.915495
1469.503544	103.239064	65.920500
1469.429631	93.009276	65.925505
1468.660319	95.956119	65.930510
1468.804843	93.134878	65.935514
1467.838129	95.790654	65.940519
1466.743664	95.646468	65.945524
1466.703160	92.911365	65.950529
1465.540604	102.272947	65.955534
1464.420478	99.389873	65.960538
1463.498510	98.880261	65.965543
1462.885812	108.377069	65.970548
1462.908281	100.357378	65.975553
1462.260841	102.410252	65.980558
1461.189064	100.079007	65.985562
1460.245674	100.238159	65.990567
1459.832373	99.439000	65.995572
1459.495800	92.164808	66.000577
1459.031765	95.749762	66.005582
1458.144193	97.533092	66.010586
1457.261195	94.163802	66.015591
1456.510665	101.268927	66.020596
1456.356156	99.398818	66.025601
1455.822645	104.123765	66.030606
1454.502473	102.164228	66.035610
1453.835523	108.212210	66.040615
1453.080415	99.161980	66.045620
1452.912666	97.784770	66.050625
1452.388545	94.016181	66.055630
1451.774554	103.674647	66.060634
1450.890706	92.056721	66.065639
1450.092006	101.877055	66.070644
1449.928741	85.173825	66.075649
1448.938205	93.713372	66.080654
1448.084425	94.787536	66.085658
1447.775305	93.548201	66.090663
1446.784577	103.605470	66.095668
1446.359367	92.224822	66.100673
1445.359410	99.686831	66.105678
1444.748192	98.657087	66.110682
1444.412694	97.368190	66.115687
1444.121271	107.659045	66.120692
1442.803463	100.154525	66.125697
1441.591685	101.375221	66.130702
1440.918539	103.191719	66.135706
1440.971991	104.921356	66.140711
1440.201405	100.881151	66.145716
1440.227293	96.295307	66.150721
1439.082942	106.756616	66.155726
1437.943777	95.521846	66.160730
1437.339686	103.057807	66.165735
1437.019526	106.173294	66.170740
1436.468907	95.914184	66.175745
1435.319973	101.035764	66.180750
1434.410357	96.289132	66.185754
1434.279380	98.815689	66.190759
1433.566915	102.748677	66.195764
1433.596413	98.570351	66.200769
1432.250687	102.316872	66.205774
1431.068934	96.002429	66.210778
1430.880329	92.271939	66.215783
1430.281801	104.381314	66.220788
1430.295597	92.345297	66.225793
1429.449634	99.262294	66.230798
1428.252422	96.507681	66.235802
1427.936298	100.697684	66.240807
1426.950913	105.076838	66.245812
1426.810550	97.997211	66.250817
1425.760029	100.499190	66.255822
1425.355752	106.841277	66.260826
1424.476758	94.990038	66.265831
1423.481271	96.987623	66.270836
1422.533147	91.653538	66.275841
1422.076040	96.800779	66.280846
1421.601337	98.978425	66.285850
1421.351743	100.785191	66.290855
1420.631481	97.847110	66.295860
1420.003234	92.226183	66.300865
1418.956110	99.303525	66.305870
1418.110950	99.206279	66.310874
1417.715555	92.679491	66.315879
1417.313684	93.874064	66.320884
1416.802050	94.774019	66.325889
1415.645263	91.771715	66.330894
1415.160446	91.583585	66.335898
1415.047469	96.973093	66.340903
1413.747437	99.494097	66.345908
1413.023222	101.625245	66.350913
1412.415491	99.262741	66.355918
1411.692511	98.644084	66.360922
1411.711208	99.149732	66.365927
1410.403656	99.734362	66.370932
1409.688853	103.728538	66.375937
1409.026006	103.003673	66.380942
1408.658281	98.868470	66.385946
1408.484316	99.242892	66.390951
1406.771428	104.159836	66.395956
1405.927826	98.809442	66.400961
1405.236019	105.831499	66.405966
1404.893973	95.812998	66.410970
1404.771008	102.577830	66.415975
1404.098362	103.038396	66.420980
1403.923853	104.403255	66.425985
1402.645618	102.523787	66.430990
1401.869923	117.099289	66.435994
1401.539948	102.006611	66.440999
1400.491653	105.946955	66.446004
1399.659371	93.715117	66.451009
1398.792527	99.476015	66.456014
1398.301579	95.521765	66.461018
1398.015614	83.966517	66.466023
1397.509591	93.838985	66.471028
1397.092481	97.980750	66.476033
1395.914571	94.484328	66.481038
1395.244127	99.388232	66.486042
1395.347760	93.419814	66.491047
1394.389676	96.959078	66.496052
1393.656316	95.027007	66.501057
1392.402751	109.579301	66.506062
1392.138248	98.370090	66.511066
1391.648026	95.114364	66.516071
1390.254641	105.203062	66.521076
1390.139479	98.307010	66.526081
1389.270288	100.204830	66.531086
1388.471422	105.936334	66.536090
1388.472454	95.603732	66.541095
1387.318782	102.084744	66.546100
1386.603027	95.180184	66.551105
1385.938722	104.842921	66.556110
1385.701485	102.088996	66.561114
1384.968465	100.501849	66.566119
1383.568810	115.660178	66.571124
1383.268223	97.955375	66.576129
1382.533958	101.973411	66.581134
1382.187913	109.753745	66.586138
1381.933597	105.351250	66.591143
1381.004590	99.961798	66.596148
1379.848465	99.283082	66.601153
1379.156764	102.430588	66.606158
1379.154526	107.035394	66.611162
1378.753600	97.830222	66.616167
1377.091687	104.834787	66.621172
1376.489303	103.408429	66.626177
1376.209416	101.214407	66.631182
1375.631760	110.548123	66.636186
1375.019314	96.199296	66.641191
1374.141401	102.325231	66.646196
1373.226302	100.961478	66.651201
1372.663610	103.897834	66.656206
1372.147219	96.901524	66.661210
1371.805330	97.047730	66.666215
1370.702068	102.337547	66.671220
1370.366791	91.422680	66.676225
1369.670916	97.084451	66.681230
1369.206083	97.717862	66.686234
1368.294278	105.809759	66.691239
1367.011428	97.941274	66.696244
1366.571461	92.303524	66.701249
1366.087269	100.223546	66.706254
1365.541562	90.983560	66.711258
1365.558718	95.990417	66.716263
1364.654236	105.732947	66.721268
1363.528693	96.308408	66.726273
1362.912462	100.556886	66.731278
1362.318243	105.266178	66.736282
1362.256762	95.548195	66.741287
1360.783776	107.530950	66.746292
1360.403228	98.180590	66.751297
1359.551867	93.565313	66.756302
1359.021100	96.655669	66.761306
1358.205650	96.724655	66.766311
1357.252277	99.862482	66.771316
1356.753957	97.429551	66.776321
1356.279285	98.531201	66.781326
1355.902355	100.055044	66.786330
1355.518827	103.206247	66.791335
1354.369817	103.665469	66.796340
1353.671403	99.423070	66.801345
1353.120764	102.542091	66.806350
1352.699276	103.732527	66.811354
1351.451407	105.654911	66.816359
1350.739977	97.806641	66.821364
1350.542577	101.171892	66.826369
1349.876013	94.816260	66.831374
1349.297064	101.325210	66.836378
1348.913719	89.892814	66.841383
1347.893466	103.240365	66.846388
1347.170176	96.158691	66.851393
1346.759745	103.878205	66.856398
1345.730911	101.672656	66.861402
1344.953551	96.599869	66.866407
1344.220670	106.481572	66.871412
1344.279754	96.653747	66.876417
1343.272512	95.237488	66.881422
1342.026876	98.544154	66.886426
1341.252953	95.693821	66.891431
1340.718391	95.681572	66.896436
1340.455232	100.339327	66.901441
1340.627603	101.813748	66.906446
1339.517046	100.980407	66.911450
1338.415313	98.698527	66.916455
1337.648173	99.841162	66.921460
1337.389195	93.905607	66.926465
1336.613094	99.778077	66.931470
1335.303485	101.004492	66.936474
1334.927607	106.151649	66.941479
1333.827347	106.993300	66.946484
1333.613571	98.819071	66.951489
1333.555421	101.293689	66.956494
1333.092098	101.631597	66.961498
1332.674782	100.271455	66.966503
1331.367749	109.229127	66.971508
1330.774146	99.237119	66.976513
1330.386507	109.823108	66.981518
1328.815833	101.193551	66.986522
1328.352930	99.624514	66.991527
1327.512952	103.828405	66.996532
1327.378240	103.114194	67.001537
1327.028891	103.101426	67.006542
1325.939978	109.117047	67.011546
1325.147686	98.871698	67.016551
1324.587393	104.677626	67.021556
1324.236579	101.821575	67.026561
1323.665702	106.365435	67.031566
1322.462573	104.465238	67.036570
1321.974624	99.421858	67.041575
1321.044964	107.726017	67.046580
1320.672539	94.727494	67.051585
1320.440585	97.701575	67.056590
1319.239927	109.554832	67.061594
1318.800788	97.286506	67.066599
1317.967803	96.595514	67.071604
1317.567828	105.712901	67.076609
1316.991073	100.524468	67.081614
1315.531356	107.766397	67.086618
1315.261959	101.329757	67.091623
1314.463163	98.435135	67.096628
1314.367688	93.734685	67.101633
1313.704900	100.613627	67.106638
1312.726130	104.199864	67.111642
1312.635255	88.508162	67.116647
1311.900165	101.531783	67.121652
1310.652285	100.922076	67.126657
1309.795523	94.788078	67.131662
1308.904846	102.544802	67.136666
1309.002329	98.256954	67.141671
1308.379214	99.212316	67.146676
1307.922898	91.766812	67.151681
1306.812758	104.850689	67.156686
1305.754908	97.785244	67.161690
1305.495992	95.689476	67.166695
1304.930736	103.796262	67.171700
1304.223811	91.334192	67.176705
1303.068446	95.480762	67.181710
1302.276736	105.349248	67.186714
1302.195971	96.477290	67.191719
1301.396879	97.821179	67.196724
1301.058060	93.838139	67.201729
1300.915846	88.345998	67.206734
1299.706101	100.242646	67.211738
1298.924786	95.107787	67.216743
1298.263355	104.843451	67.221748
1297.796610	93.040492	67.226753
1296.847470	107.227276	67.231758
1295.686691	103.634794	67.236762
1295.465485	92.383457	67.241767
1294.809256	105.763824	67.246772
1294.637647	98.627589	67.251777
1293.993443	98.620694	67.256782
1292.996901	103.548064	67.261786
1292.579716	104.062803	67.266791
1292.004927	108.166438	67.271796
1290.968296	93.545664	67.276801
1290.353449	97.437481	67.281806
1289.795171	101.722225	67.286810
1289.216788	91.169104	67.291815
1287.438311	99.332791	67.296820
1286.946347	97.137189	67.301825
1286.664762	96.357732	67.306830
1286.132155	101.514351	67.311834
1285.946557	96.999846	67.316839
1285.731002	109.068136	67.321844
1284.871151	97.575615	67.326849
1283.942386	98.213454	67.331854
1282.994885	101.578039	67.336858
1282.714635	100.717042	67.341863
1281.185535	97.317873	67.346868
1280.571349	106.294307	67.351873
1280.193615	102.113465	67.356878
1279.446856	93.269473	67.361882
1279.454682	91.072785	67.366887
1278.711239	98.289202	67.371892
1277.548385	97.294705	67.376897
1277.087830	98.241584	67.381902
1275.950343	97.367475	67.386906
1276.282311	91.313004	67.391911
1275.336784	91.587023	67.396916
1274.426596	94.888381	67.401921
1273.688302	93.529512	67.406926
1272.959607	100.561836	67.411930
1272.383606	89.218091	67.416935
1272.148912	98.528220	67.421940
1271.248556	93.151654	67.426945
1270.547646	93.904823	67.431950
1269.656160	92.962553	67.436954
1269.474203	90.197991	67.441959
1268.356520	102.517018	67.446964
1267.548694	93.586777	67.451969
1266.964191	93.060088	67.456974
1266.422483	99.540562	67.461978
1266.313352	97.066674	67.466983
1265.639534	107.083919	67.471988
1264.614277	88.979029	67.476993
1263.834465	91.533767	67.481998
1263.254259	95.375448	67.487002
1262.768925	88.625278	67.492007
1261.600314	98.360135	67.497012
1260.731167	95.176400	67.502017
1260.475023	88.253977	67.507022
1259.595385	97.111647	67.512026
1259.712863	92.656967	67.517031
1259.156340	101.183025	67.522036
1258.102636	95.986652	67.527041
1257.678241	91.456587	67.532046
1256.657578	90.434596	67.537050
1255.695721	89.783834	67.542055
1255.048147	96.702802	67.547060
1254.374060	94.400626	67.552065
1253.971373	96.091507	67.557070
1253.375886	94.332819	67.562074
1253.410992	87.406719	67.567079
1251.911084	93.655327	67.572084
1251.519729	95.482023	67.577089
1251.100163	95.566934	67.582094
1249.720024	101.625709	67.587098
1248.977554	94.036974	67.592103
1248.212531	98.180281	67.597108
1247.661234	90.717102	67.602113
1247.454552	90.857143	67.607118
1246.888308	93.815824	67.612122
1246.398853	84.930954	67.617127
1245.147428	98.827659	67.622132
1244.394957	90.172144	67.627137
1244.083493	98.161276	67.632142
1243.626075	99.311689	67.637146
1243.337628	94.148911	67.642151
1242.239069	90.929063	67.647156
1241.531021	95.831521	67.652161
1241.185336	96.310342	67.657166
1239.644421	102.018505	67.662170
1239.027086	91.684815	67.667175
1238.449201	96.795899	67.672180
1238.161532	94.649798	67.677185
1237.512474	96.511534	67.682190
1237.078900	98.965953	67.687194
1236.279209	92.082901	67.692199
1235.006515	101.389159	67.697204
1234.543862	98.198994	67.702209
1234.204476	89.959054	67.707214
1233.906788	99.223915	67.712218
1233.532973	91.667200	67.717223
1232.181250	93.970527	67.722228
1231.652904	91.143301	67.727233
1231.040254	94.506222	67.732238
1229.765190	103.197527	67.737242
1229.417939	93.615716	67.742247
1228.701628	93.174750	67.747252
1228.858991	88.425497	67.752257
1228.013977	99.029778	67.757262
1226.063632	97.119771	67.762266
1225.744757	94.264579	67.767271
1225.390979	100.134229	67.772276
1224.839817	95.549294	67.777281
1224.457942	90.583294	67.782286
1223.896587	96.297437	67.787290
1223.524084	92.819092	67.792295
1222.647155	85.538766	67.797300
1221.695383	92.324690	67.802305
1220.573052	94.598617	67.807310
1219.298331	107.788438	67.812314
1219.486086	87.784547	67.817319
1219.099010	95.943718	67.822324
1218.588395	92.370209	67.827329
1218.243768	91.795354	67.832334
1217.323909	97.960457	67.837338
1216.113628	90.040132	67.842343
1215.794405	102.218521	67.847348
1215.345939	98.358860	67.852353
1213.900746	97.712303	67.857358
1212.937320	96.969849	67.862362
1212.348129	83.466526	67.867367
1212.151145	91.171595	67.872372
1211.500059	90.136866	67.877377
1211.421552	82.975631	67.882382
1210.923862	93.311644	67.887386
1210.440034	86.747926	67.892391
1209.126446	92.580192	67.897396
1208.346080	94.409546	67.902401
1207.737439	95.438227	67.907406
1206.737519	96.555210	67.912410
1206.193098	92.218585	67.917415
1205.822075	92.264401	67.922420
1205.211342	98.486314	67.927425
1204.744798	96.239793	67.932430
1203.768743	104.735052	67.937434
1203.193078	98.369017	67.942439
1202.483859	95.867217	67.947444
1201.901766	94.984879	67.952449
1201.492713	95.240879	67.957454
1199.981764	98.526685	67.962458
1199.777832	91.928074	67.967463
1198.719799	97.760801	67.972468
1198.371579	101.481855	67.977473
1198.127214	89.556775	67.982478
1197.215790	99.504175	67.987482
1196.472215	100.917518	67.992487
1195.856643	95.378141	67.997492
1195.143281	99.922719	68.002497
1195.012080	99.104496	68.007502
1193.405700	98.443306	68.012506
1193.060850	99.003693	68.017511
1192.504158	97.962279	68.022516
1192.088092	95.847636	68.027521
1192.057794	93.987064	68.032526
1190.598935	103.153106	68.037530
1190.334495	93.995652	68.042535
1189.311682	99.869323	68.047540
1187.911629	99.344513	68.052545
1187.325890	95.453492	68.057550
1186.788317	103.831448	68.062554
1186.612663	98.802119	68.067559
1185.960831	99.600579	68.072564
1185.583922	94.875297	68.077569
1185.264638	93.392209	68.082574
1184.229032	97.140950	68.087578
1183.710387	98.968919	68.092583
1182.981103	96.586603	68.097588
1181.717214	93.767292	68.102593
1181.035597	95.331073	68.107598
1180.006130	99.543738	68.112602
1179.942151	93.714151	68.117607
1179.213580	96.306704	68.122612
1179.079349	95.191385	68.127617
1178.301526	92.158602	68.132622
1177.296879	107.522856	68.137626
1176.783264	93.717662	68.142631
1176.277269	96.917863	68.147636
1175.070049	99.979975	68.152641
1174.664811	90.768082	68.157646
1173.361816	97.353239	68.162650
1173.340819	98.532355	68.167655
1172.861209	107.444701	68.172660
1172.562834	105.196232	68.177665
1171.756392	92.817152	68.182670
1170.540289	97.643977	68.187674
1170.435991	97.263231	68.192679
1169.395237	97.441474	68.197684
1168.817227	95.359691	68.202689
1168.243255	89.495849	68.207694
1167.208081	93.541739	68.212698
1167.213883	88.695678	68.217703
1166.382371	98.658608	68.222708
1165.565638	92.024398	68.227713
1165.172994	92.227858	68.232718
1164.334704	96.715277	68.237722
1163.416939	88.868040	68.242727
1162.287640	92.843998	68.247732
1161.527145	91.327904	68.252737
1160.857880	98.093890	68.257742
1160.443573	99.938337	68.262746
1160.467012	93.777617	68.267751
1160.309560	94.819051	68.272756
1159.117116	92.140269	68.277761
1158.268231	93.907943	68.282766
1157.341326	108.801808	68.287770
1156.825202	93.017158	68.292775
1156.206084	100.215061	68.297780
1155.289695	97.422704	68.302785
1154.451330	92.443293	68.307790
1153.930709	94.581453	68.312794
1153.665039	95.412480	68.317799
1153.630875	95.721135	68.322804
1152.877213	94.601350	68.327809
1152.113458	96.155909	68.332814
1150.939235	103.661210	68.337818
1150.110343	99.154624	68.342823
1148.963299	100.556530	68.347828
1148.281679	103.921006	68.352833
1148.038466	102.577650	68.357838
1147.722954	106.818078	68.362842
1147.570020	93.956084	68.367847
1147.238189	97.195543	68.372852
1145.722454	99.662754	68.377857
1145.003016	97.552297	68.382862
1144.032256	105.429322	68.387866
1143.733206	95.673096	68.392871
1142.447954	103.853424	68.397876
1141.571861	102.101744	68.402881
1141.679256	89.492404	68.407886
1141.048543	98.739677	68.412890
1140.539696	93.870422	68.417895
1140.153327	99.685261	68.422900
1139.200933	99.954955	68.427905
1138.516921	90.116232	68.432910
1137.912997	101.883911	68.437914
1137.572485	93.700622	68.442919
1136.414850	102.347363	68.447924
1135.346803	99.637814	68.452929
1134.989533	94.664848	68.457934
1134.426052	103.138025	68.462938
1134.238042	101.392082	68.467943
1133.207873	101.931264	68.472948
1132.162672	100.494708	68.477953
1132.023093	101.506241	68.482958
1131.574859	109.190784	68.487962
1130.599322	92.177503	68.492967
1129.785309	100.243204	68.497972
1128.899159	98.707973	68.502977
1128.802228	99.179339	68.507982
1127.687865	108.914011	68.512986
1126.467034	99.009310	68.517991
1125.881946	99.743063	68.522996
1125.688286	98.290967	68.528001
1125.517423	94.214851	68.533006
1124.810020	102.210197	68.538010
1124.399428	95.980115	68.543015
1123.173446	102.515784	68.548020
1122.257138	107.897574	68.553025
1121.828188	106.256433	68.558030
1121.498221	107.467530	68.563034
1120.219812	98.608423	68.568039
1119.655168	94.844847	68.573044
1119.000696	98.243753	68.578049
1118.601237	95.583937	68.583054
1117.896675	100.202011	68.588058
1117.808819	93.925752	68.593063
1116.899538	96.739900	68.598068
1115.892005	103.890632	68.603073
1115.661229	95.667636	68.608078
1114.452146	109.085822	68.613082
1113.652743	98.822407	68.618087
1113.284845	107.365120	68.623092
1112.435764	103.808919	68.628097
1112.266772	101.499621	68.633102
1111.526157	104.991827	68.638106
1110.191847	98.143500	68.643111
1109.533835	103.179897	68.648116
1108.895094	99.921613	68.653121
1108.644890	94.943739	68.658126
1108.334442	100.377310	68.663130
1107.919510	98.449183	68.668135
1106.786011	103.450946	68.673140
1105.787116	101.860028	68.678145
1104.927868	100.097576	68.683150
1104.713883	106.808509	68.688154
1104.144088	99.831652	68.693159
1103.062421	97.716121	68.698164
1102.082142	102.594946	68.703169
1101.655010	84.047078	68.708174
1101.053539	103.859806	68.713178
1100.933703	93.884230	68.718183
1100.983756	94.813166	68.723188
1100.010846	101.485102	68.728193
1099.042213	94.451019	68.733198
1098.256401	109.195603	68.738202
1097.180603	92.374360	68.743207
1096.513155	104.064107	68.748212
1095.436684	102.827507	68.753217
1095.468145	96.155446	68.758222
1094.732067	106.222037	68.763226
1094.495818	102.072648	68.768231
1094.069063	95.762054	68.773236
1093.074853	101.005218	68.778241
1092.321174	94.914013	68.783246
1091.466823	109.461924	68.788250
1090.902764	102.460403	68.793255
1090.017068	100.369738	68.798260
1089.527573	104.580749	68.803265
1088.990255	99.107724	68.808270
1088.282359	105.818361	68.813274
1087.520927	106.440215	68.818279
1087.025345	101.959856	68.823284
1086.272488	102.378148	68.828289
1086.109477	93.454383	68.833294
1084.941157	102.878575	68.838298
1084.329913	93.296598	68.843303
1083.891943	96.137809	68.848308
1082.519515	98.653128	68.853313
1081.724273	93.314264	68.858318
1080.988407	99.689050	68.863322
1080.312493	98.979098	68.868327
1079.956685	92.199675	68.873332
1079.456771	92.947663	68.878337
1079.426871	87.056596	68.883342
1079.114579	99.942299	68.888346
1078.379435	92.219332	68.893351
1077.358665	89.453549	68.898356
1076.221745	95.673201	68.903361
1075.234997	97.476730	68.908366
1074.441559	100.546561	68.913370
1074.063835	99.503726	68.918375
1073.745689	102.867549	68.923380
1073.148085	104.101581	68.928385
1072.855109	96.092913	68.933390
1071.558157	99.304614	68.938394
1070.727405	89.658392	68.943399
1070.544873	95.868567	68.948404
1069.538414	103.634875	68.953409
1069.181431	92.560763	68.958414
1068.200533	106.373672	68.963418
1067.489338	98.114922	68.968423
1066.716716	95.976087	68.973428
1066.277980	103.580058	68.978433
1066.240826	100.968731	68.983438
1065.303463	102.126736	68.988442
1064.466255	97.644881	68.993447
1063.971648	97.249658	68.998452
1063.259228	106.784466	69.003457
1062.337158	88.331219	69.008462
1061.508138	96.377388	69.013466
1060.879614	92.687519	69.018471
1060.772751	85.679565	69.023476
1060.113721	99.685630	69.028481
1059.320491	92.095369	69.033486
1058.176065	108.012873	69.038490
1057.757471	102.327298	69.043495
1057.351927	96.961182	69.048500
1056.605029	106.942395	69.053505
1055.857559	101.562988	69.058510
1054.915776	102.267830	69.063514
1054.815924	98.785841	69.068519
1054.604170	100.677712	69.073524
1052.933193	105.706390	69.078529
1052.367229	93.500104	69.083534
1051.384747	106.959226	69.088538
1051.216814	98.149588	69.093543
1050.773724	102.523170	69.098548
1049.585107	98.451997	69.103553
1048.958238	91.755701	69.108558
1048.417386	92.386762	69.113562
1047.897596	96.063385	69.118567
1047.748716	95.595938	69.123572
1046.556449	105.362902	69.128577
1045.604807	103.562207	69.133582
1045.055852	95.592639	69.138586
1044.696905	95.364441	69.143591
1044.334803	93.970006	69.148596
1043.558844	92.460133	69.153601
1042.727813	93.078517	69.158606
1041.967638	105.189120	69.163610
1041.400376	95.725534	69.168615
1041.001820	94.291556	69.173620
1039.590802	91.815224	69.178625
1039.106936	90.677285	69.183630
1038.407770	92.173828	69.188634
1038.131430	97.296444	69.193639
1037.796463	94.904657	69.198644
1036.687542	98.777681	69.203649
1035.999962	99.847133	69.208654
1035.513527	97.636011	69.213658
1035.228812	98.098089	69.218663
1033.701220	93.376453	69.223668
1032.802117	96.925802	69.228673
1032.765738	94.035281	69.233678
1032.139022	93.463747	69.238682
1031.621484	95.246146	69.243687
1030.504112	89.323806	69.248692
1029.868482	91.825860	69.253697
1029.412944	94.008145	69.258702
1028.931590	85.410467	69.263706
1028.365295	93.508749	69.268711
1027.272748	92.425699	69.273716
1026.306149	91.349898	69.278721
1026.091648	89.499558	69.283726
1025.655913	100.820433	69.288730
1025.212391	97.186122	69.293735
1024.035059	97.888675	69.298740
1023.238639	99.796194	69.303745
1023.038644	91.318088	69.308750
1022.174323	106.365044	69.313754
1021.680798	91.652950	69.318759
1020.825693	93.228300	69.323764
1019.803747	104.235108	69.328769
1019.687890	89.442163	69.333774
1019.250213	92.400951	69.338778
1018.287291	85.498144	69.343783
1017.141571	89.310370	69.348788
1016.440486	94.326122	69.353793
1016.107926	92.608492	69.358798
1015.728477	88.180494	69.363802
1014.800336	96.095227	69.368807
1014.090455	90.189952	69.373812
1013.085503	99.608676	69.378817
1012.879259	98.528983	69.383822
1012.512953	92.515140	69.388826
1012.075201	95.774714	69.393831
1010.946555	89.525908	69.398836
1009.909621	93.441474	69.403841
1010.032701	87.804068	69.408846
1009.300143	102.305856	69.413850
1008.289701	103.695452	69.418855
1007.582569	100.090889	69.423860
1006.550180	94.257418	69.428865
1006.677458	100.410988	69.433870
1005.583160	95.034145	69.438874
1004.540630	93.979245	69.443879
1003.700284	87.055452	69.448884
1003.134300	90.221727	69.453889
1003.265773	90.659115	69.458894
1002.809241	97.182245	69.463898
1002.417647	92.239647	69.468903
1001.375562	93.912936	69.473908
1000.243579	88.806613	69.478913
999.803508	92.412354	69.483918
998.568216	94.747903	69.488922
997.899462	96.838420	69.493927
997.570687	95.062515	69.498932
996.730845	96.904451	69.503937
996.507831	88.002421	69.508942
996.092953	92.653393	69.513946
995.484445	96.503098	69.518951
994.723935	93.517908	69.523956
993.427245	94.945472	69.528961
993.383040	90.187321	69.533966
992.483129	92.939886	69.538970
991.410550	89.973797	69.543975
990.906309	88.818827	69.548980
990.216275	93.794402	69.553985
990.113926	89.412898	69.558990
989.399538	93.697946	69.563994
988.518958	100.931552	69.568999
988.223648	91.533116	69.574004
987.223223	95.278628	69.579009
986.827425	93.223297	69.584014
985.602733	94.255266	69.589018
984.722347	95.759560	69.594023
984.640831	92.752041	69.599028
983.719776	102.707424	69.604033
983.183251	91.057004	69.609038
982.048095	97.039146	69.614042
981.427691	95.851573	69.619047
980.977807	88.850657	69.624052
980.276844	91.005109	69.629057
980.395946	90.239157	69.634062
979.430313	100.456368	69.639066
978.393148	98.252725	69.644071
977.905899	89.881445	69.649076
977.341026	99.843723	69.654081
977.144628	86.317798	69.659086
975.809229	99.199100	69.664090
974.790559	104.988809	69.669095
974.704758	94.023003	69.674100
974.000889	95.316293	69.679105
974.022569	96.766371	69.684110
972.598822	101.210791	69.689114
971.587372	97.536777	69.694119
971.381545	90.755369	69.699124
970.837149	99.442766	69.704129
970.029698	99.789113	69.709134
968.803355	96.589637	69.714138
968.500737	99.439648	69.719143
968.133998	93.580218	69.724148
967.609514	100.224323	69.729153
966.616699	92.775230	69.734158
965.878121	97.550317	69.739162
965.228740	96.980699	69.744167
964.955170	87.312114	69.749172
964.012290	100.128174	69.754177
962.979954	94.117478	69.759182
962.432089	95.730613	69.764186
961.968932	105.541273	69.769191
961.801589	97.334275	69.774196
960.929174	100.273574	69.779201
960.248022	96.304197	69.784206
959.307616	104.445633	69.789210
958.616736	102.052832	69.794215
958.127871	98.944949	69.799220
957.540999	102.817004	69.804225
956.550522	92.553990	69.809230
955.593711	103.735166	69.814234
955.389110	106.691543	69.819239
955.001283	91.221671	69.824244
954.486299	98.629894	69.829249
953.564822	96.447101	69.834254
952.852323	96.326032	69.839258
952.225682	100.888937	69.844263
951.804748	100.253753	69.849268
950.720288	95.584542	69.854273
950.106560	97.297373	69.859278
949.664089	99.104422	69.864282
949.100603	102.922739	69.869287
948.238256	93.431950	69.874292
946.915795	102.699015	69.879297
946.488385	93.743972	69.884302
945.807135	100.288220	69.889306
945.418760	98.851323	69.894311
945.336148	92.552472	69.899316
944.663341	99.161587	69.904321
943.814510	102.633266	69.909326
943.123202	100.178176	69.914330
942.611977	92.306374	69.919335
941.654232	89.274845	69.924340
940.468150	99.256669	69.929345
940.301686	90.069846	69.934350
939.788649	95.395619	69.939354
938.841119	98.110561	69.944359
937.986346	91.033341	69.949364
937.127610	102.976492	69.954369
936.834632	91.623829	69.959374
936.263020	91.915188	69.964378
935.874008	94.367123	69.969383
935.344730	98.138137	69.974388
934.175196	92.908402	69.979393
933.789305	92.084466	69.984398
933.201281	91.881692	69.989402
931.973620	92.832871	69.994407
931.394708	88.952171	69.999412
930.475136	92.418202	70.004417
930.525684	94.929459	70.009422
929.618084	95.038372	70.014426
929.592874	93.003656	70.019431
928.844805	91.834401	70.024436
927.574425	93.316287	70.029441
926.968660	89.349008	70.034446
926.669793	101.237327	70.039450
925.495452	90.047842	70.044455
924.518654	90.168607	70.049460
923.965290	96.276899	70.054465
923.705044	94.302960	70.059470
923.224137	96.790369	70.064474
922.606639	91.671744	70.069479
922.106477	93.948122	70.074484
920.885061	102.417142	70.079489
920.487079	92.172270	70.084494
920.053875	89.846263	70.089498
918.845053	93.066192	70.094503
917.913239	85.629563	70.099508
917.843029	97.497667	70.104513
917.143511	89.488390	70.109518
916.818391	84.970975	70.114522
916.190713	94.668100	70.119527
915.308563	88.447763	70.124532
914.264532	96.894692	70.129537
913.998132	95.113243	70.134542
913.282841	94.646888	70.139546
912.400968	93.166228	70.144551
911.510492	87.704774	70.149556
910.640761	92.090639	70.154561
910.436868	83.131670	70.159566
909.835385	84.168630	70.164570
909.399084	88.340538	70.169575
908.427408	92.878460	70.174580
907.887270	97.812978	70.179585
907.645195	93.715130	70.184590
907.347622	93.413671	70.189594
906.008439	98.368198	70.194599
905.264577	84.070835	70.199604
904.225706	93.301176	70.204609
904.024096	92.616594	70.209614
902.642918	96.683102	70.214618
901.682723	92.714555	70.219623
902.206802	95.704023	70.224628
901.030443	97.294149	70.229633
900.562276	91.008047	70.234638
900.272888	94.862313	70.239642
899.524595	94.381877	70.244647
898.809970	90.744674	70.249652
897.778502	89.940125	70.254657
897.432416	89.944195	70.259662
897.070570	85.245188	70.264666
896.112611	95.759492	70.269671
895.213611	94.024020	70.274676
894.348278	97.326830	70.279681
894.529933	92.259230	70.284686
893.273365	87.156514	70.289690
892.171943	101.667396	70.294695
891.905009	93.841786	70.299700
891.001064	87.588084	70.304705
890.547519	88.894167	70.309710
890.463475	88.659161	70.314714
889.597314	87.953401	70.319719
888.520148	83.569523	70.324724
887.788779	93.970419	70.329729
887.670816	90.374708	70.334734
887.129189	84.494327	70.339738
885.975761	95.166443	70.344743
885.321054	90.906780	70.349748
884.572461	95.150331	70.354753
884.432254	86.887388	70.359758
883.931276	97.465132	70.364762
882.711586	107.089193	70.369767
882.269720	95.228778	70.374772
881.513987	102.763100	70.379777
881.174255	96.560785	70.384782
880.176121	95.499888	70.389786
878.998556	87.740247	70.394791
878.912332	90.173088	70.399796
878.478360	91.735148	70.404801
877.522374	86.886465	70.409806
876.673945	89.434452	70.414810
876.033943	94.737370	70.419815
875.509949	91.253827	70.424820
874.765042	96.879431	70.429825
874.328464	95.178838	70.434830
873.373656	90.025630	70.439834
872.567863	97.201834	70.444839
872.475681	85.708620	70.449844
871.529975	91.022448	70.454849
871.209077	97.094087	70.459854
870.264199	98.914955	70.464858
868.952714	105.034285	70.469863
869.097266	91.120397	70.474868
868.104897	97.485054	70.479873
867.736901	90.315404	70.484878
866.893683	96.757930	70.489882
866.094683	98.504475	70.494887
865.744193	94.678605	70.499892
865.113034	100.450114	70.504897
864.528949	87.881477	70.509902
863.375282	90.949874	70.514906
862.547772	95.459166	70.519911
862.335969	90.062661	70.524916
861.994120	93.063463	70.529921
861.502827	90.026665	70.534926
860.504627	87.307591	70.539930
859.618597	96.218884	70.544935
859.413264	82.951079	70.549940
858.032011	87.658229	70.554945
857.064675	84.443242	70.559950
857.051323	88.215891	70.564954
856.288530	91.840202	70.569959
856.257895	83.752697	70.574964
855.418971	91.960830	70.579969
854.568582	81.262572	70.584974
853.628550	83.262600	70.589978
853.008474	90.929201	70.594983
852.713223	86.606402	70.599988
851.309912	81.791317	70.604993
850.701628	84.125293	70.609998
850.336971	89.931283	70.615002
849.633848	96.300872	70.620007
849.378224	87.971652	70.625012
848.239879	92.536945	70.630017
847.237991	92.309938	70.635022
846.465842	85.934603	70.640026
846.211463	87.445774	70.645031
846.305330	80.309127	70.650036
845.554361	77.324703	70.655041
844.509677	81.605152	70.660046
844.112592	90.171795	70.665050
842.940814	97.446603	70.670055
842.792623	90.575607	70.675060
842.083761	93.966487	70.680065
840.933932	78.762158	70.685070
840.748629	96.178712	70.690074
839.807861	97.316815	70.695079
839.328874	88.409705	70.700084
837.959996	92.906333	70.705089
837.235338	92.971694	70.710094
836.701459	83.291272	70.715098
836.373606	89.560667	70.720103
836.096636	82.301624	70.725108
835.597202	94.598867	70.730113
835.039008	82.278424	70.735118
834.212482	83.089480	70.740122
833.422679	84.929183	70.745127
832.888021	76.607898	70.750132
831.597908	87.844183	70.755137
830.668880	86.518449	70.760142
830.240592	82.855901	70.765146
829.844817	97.671425	70.770151
829.754504	91.247596	70.775156
829.009897	103.611704	70.780161
828.027104	88.423364	70.785166
827.272085	91.854912	70.790170
826.702790	98.964169	70.795175
826.355189	86.224784	70.800180
825.526892	94.435442	70.805185
824.340457	87.669648	70.810190
823.800049	85.693573	70.815194
823.615637	87.340779	70.820199
823.143373	84.044164	70.825204
821.936504	85.309157	70.830209
821.329077	92.115092	70.835214
820.666220	84.999508	70.840218
819.949446	92.328221	70.845223
819.145141	85.901166	70.850228
818.171500	89.512256	70.855233
817.836769	88.919554	70.860238
817.096973	87.167882	70.865242
816.366405	90.539194	70.870247
816.393298	93.046208	70.875252
815.938842	91.848786	70.880257
815.132011	84.944167	70.885262
814.403001	86.769909	70.890266
813.699058	91.868268	70.895271
812.709283	89.315516	70.900276
811.990126	99.339349	70.905281
810.973274	95.937073	70.910286
810.876467	90.698893	70.915290
810.167088	95.549120	70.920295
809.764037	85.343825	70.925300
808.853067	95.351564	70.930305
808.149062	85.971849	70.935310
807.614412	88.508731	70.940314
806.701939	96.637104	70.945319
805.888856	90.121560	70.950324
805.045099	92.851115	70.955329
804.695380	90.931981	70.960334
804.482730	79.380867	70.965338
803.899022	93.030224	70.970343
803.530714	87.180562	70.975348
802.327197	89.027977	70.980353
801.597090	98.372805	70.985358
800.991288	99.291710	70.990362
799.854513	99.704753	70.995367
799.277940	91.010537	71.000372
798.591008	93.055639	71.005377
798.124708	90.132588	71.010382
798.045833	95.772006	71.015386
796.694542	92.884096	71.020391
796.076131	91.266364	71.025396
795.724286	90.669490	71.030401
795.042736	95.813356	71.035406
794.468745	93.503188	71.040410
793.573237	94.003979	71.045415
793.088849	90.424065	71.050420
792.177215	94.505695	71.055425
791.407259	100.580835	71.060430
791.396998	87.801043	71.065434
790.023345	98.329720	71.070439
789.525484	88.538536	71.075444
788.412851	90.678265	71.080449
788.235819	91.789766	71.085454
787.906113	89.767738	71.090458
787.285561	90.477998	71.095463
786.497369	81.850035	71.100468
785.205779	90.060316	71.105473
784.522910	92.771395	71.110478
784.165788	93.143263	71.115482
783.522999	93.385650	71.120487
783.645080	91.754368	71.125492
782.506701	95.729583	71.130497
781.723633	92.688696	71.135502
781.141572	91.438928	71.140506
780.653218	97.289396	71.145511
779.882692	82.641004	71.150516
778.877826	93.613718	71.155521
778.321172	96.887750	71.160526
778.594484	91.892868	71.165530
776.842176	94.756340	71.170535
776.332266	97.019794	71.175540
775.950806	97.544243	71.180545
775.543899	99.398894	71.185550
774.402139	94.616395	71.190554
773.497402	100.911585	71.195559
773.031963	94.699635	71.200564
772.268318	102.088881	71.205569
771.704233	99.163634	71.210574
771.713710	89.376338	71.215578
770.542148	94.322312	71.220583
769.718092	89.923924	71.225588
768.952882	98.904526	71.230593
768.717225	102.383693	71.235598
768.218166	95.944227	71.240602
766.978829	98.514587	71.245607
766.418480	88.349661	71.250612
766.020738	92.719038	71.255617
765.110275	86.252551	71.260622
764.513506	86.190234	71.265626
763.684420	86.247442	71.270631
762.998164	95.019135	71.275636
762.393744	92.439858	71.280641
761.972234	91.116016	71.285646
761.915316	89.022398	71.290650
760.431171	97.390794	71.295655
759.857902	90.306846	71.300660
758.928926	100.066639	71.305665
759.120800	89.413677	71.310670
758.341472	85.839687	71.315674
756.969324	94.637687	71.320679
756.310621	96.038130	71.325684
755.884683	86.202664	71.330689
755.659365	89.606246	71.335694
755.057789	85.805242	71.340698
753.720244	88.902789	71.345703
753.466404	77.924759	71.350708
752.972394	87.165592	71.355713
751.680282	92.848229	71.360718
751.030446	86.138562	71.365722
750.083806	94.333973	71.370727
749.890548	86.074213	71.375732
749.793875	90.472540	71.380737
748.977443	94.083554	71.385742
748.198440	84.951160	71.390746
746.974027	92.398804	71.395751
746.432953	90.189183	71.400756
746.010403	81.513598	71.405761
745.614249	85.470621	71.410766
745.180204	73.359060	71.415770
743.845375	93.473795	71.420775
743.550156	86.172497	71.425780
742.994108	89.178417	71.430785
742.151832	93.329879	71.435790
741.610651	88.095985	71.440794
740.514649	92.930738	71.445799
740.121880	83.434180	71.450804
739.571824	88.609599	71.455809
738.719200	89.050952	71.460814
737.793327	81.282983	71.465818
736.978906	87.386658	71.470823
736.645968	89.122462	71.475828
736.572449	94.708068	71.480833
735.791412	90.665849	71.485838
734.943658	80.549772	71.490842
733.707346	94.293943	71.495847
733.865407	80.286984	71.500852
733.198662	88.868633	71.505857
732.394546	78.588776	71.510862
731.288378	79.662472	71.515866
730.712795	88.743606	71.520871
730.245862	80.635725	71.525876
730.040678	79.892557	71.530881
728.486822	82.475354	71.535886
728.243906	84.198894	71.540890
727.900537	92.461485	71.545895
727.363285	82.463921	71.550900
726.180373	89.654210	71.555905
725.192409	87.993614	71.560910
724.885448	86.018219	71.565914
724.282456	88.211573	71.570919
723.615377	84.200756	71.575924
722.431388	87.286611	71.580929
721.598635	80.847876	71.585934
721.239339	90.001297	71.590938
720.609982	97.991978	71.595943
720.765420	86.818715	71.600948
720.069670	93.223758	71.605953
719.575017	90.264917	71.610958
718.836523	76.900590	71.615962
717.820413	88.592424	71.620967
717.047670	83.338996	71.625972
715.826528	86.961316	71.630977
715.039688	94.418873	71.635982
715.165983	81.837534	71.640986
714.383914	89.129282	71.645991
714.483980	79.715272	71.650996
713.047076	79.832400	71.656001
711.777471	82.335327	71.661006
711.826295	79.015383	71.666010
710.955964	85.959903	71.671015
710.952917	76.696972	71.676020
709.623979	82.181460	71.681025
708.653938	89.115827	71.686030
708.375731	83.236534	71.691034
707.599539	87.924935	71.696039
707.343045	84.280735	71.701044
706.735642	88.116457	71.706049
705.604941	86.826479	71.711054
705.224447	85.479040	71.716058
704.516842	93.577459	71.721063
704.314209	77.303881	71.726068
702.782836	84.182044	71.731073
702.238057	81.857019	71.736078
701.823323	84.761370	71.741082
701.146282	96.935491	71.746087
700.900282	84.622387	71.751092
699.500939	88.147745	71.756097
698.884024	83.820463	71.761102
698.453338	84.600440	71.766106
698.120965	94.895102	71.771111
697.369280	87.060199	71.776116
696.226958	85.184882	71.781121
695.317277	88.028765	71.786126
695.511989	85.324054	71.791130
694.770674	90.183313	71.796135
694.285250	83.774685	71.801140
693.181347	87.234830	71.806145
692.377585	93.378921	71.811150
692.014515	84.440144	71.816154
691.322400	92.726556	71.821159
690.627518	84.839296	71.826164
689.629714	90.210623	71.831169
689.024078	96.754565	71.836174
689.067466	80.169649	71.841178
688.219955	91.040813	71.846183
687.225795	83.373759	71.851188
686.652581	80.740995	71.856193
685.794676	87.650629	71.861198
685.774154	85.941940	71.866202
684.611767	99.347029	71.871207
683.985657	88.341991	71.876212
683.276232	87.778357	71.881217
682.399788	89.764364	71.886222
681.957901	87.689725	71.891226
681.301049	87.512981	71.896231
680.903240	86.016940	71.901236
679.956615	80.966586	71.906241
679.444246	93.153546	71.911246
679.067795	82.559270	71.916250
678.082973	88.246512	71.921255
677.467976	84.176653	71.926260
677.020639	77.547967	71.931265
675.519025	92.941702	71.936270
674.862856	91.446897	71.941274
673.804705	92.164638	71.946279
674.248647	91.566837	71.951284
673.967106	94.512317	71.956289
672.866261	88.239905	71.961294
672.518755	84.487754	71.966298
671.469291	100.129678	71.971303
670.564188	86.450893	71.976308
670.076791	92.275148	71.981313
669.440173	98.873739	71.986318
668.735916	94.098029	71.991322
667.382669	95.042761	71.996327
667.070150	92.019965	72.001332
666.713974	88.112598	72.006337
665.984770	90.360735	72.011342
665.774965	86.307512	72.016346
665.431883	92.873972	72.021351
664.924873	93.637424	72.026356
664.269300	96.590142	72.031361
662.369393	102.233639	72.036366
662.031300	89.223858	72.041370
660.910613	96.610725	72.046375
660.564548	91.354471	72.051380
660.403189	95.691252	72.056385
660.052158	89.461303	72.061390
659.504686	86.127070	72.066394
658.200379	88.717661	72.071399
657.579093	91.073225	72.076404
656.804950	86.743281	72.081409
655.373370	96.027900	72.086414
655.050412	90.734927	72.091418
654.359149	90.892878	72.096423
653.897061	92.273071	72.101428
654.326106	91.560590	72.106433
653.471821	89.374640	72.111438
653.169858	82.743549	72.116442
651.777766	96.062866	72.121447
650.997978	91.826647	72.126452
649.792167	90.715329	72.131457
648.897852	94.053532	72.136462
648.768653	93.616673	72.141466
647.959212	93.117938	72.146471
647.298041	92.143040	72.151476
647.198668	94.300650	72.156481
646.178380	92.581665	72.161486
646.336857	84.564013	72.166490
645.197367	94.938919	72.171495
644.289980	90.219329	72.176500
643.957332	90.178091	72.181505
642.974339	86.176805	72.186510
642.085304	79.965219	72.191514
641.141206	94.655594	72.196519
640.766280	82.517738	72.201524
640.542868	83.735076	72.206529
639.921123	92.814649	72.211534
639.810943	90.187430	72.216538
638.319182	96.584777	72.221543
637.627270	94.460218	72.226548
637.322948	86.795385	72.231553
636.638492	96.308441	72.236558
635.366357	89.854212	72.241562
634.514137	97.508098	72.246567
634.295285	94.232826	72.251572
633.792725	97.047630	72.256577
633.418004	99.054265	72.261582
633.231018	81.330212	72.266586
631.723303	86.973232	72.271591
631.098400	88.217514	72.276596
630.552681	83.166380	72.281601
629.759503	91.665097	72.286606
628.945297	91.786880	72.291610
628.113275	97.904243	72.296615
628.006057	90.960334	72.301620
627.458705	85.993948	72.306625
626.901663	93.947770	72.311630
626.114961	88.651358	72.316634
625.046830	95.957784	72.321639
624.688944	95.573524	72.326644
623.770884	94.520279	72.331649
622.648493	97.004719	72.336654
622.061645	92.745714	72.341658
621.385165	102.928813	72.346663
621.028565	95.154521	72.351668
620.725475	91.760663	72.356673
620.246945	93.176042	72.361678
619.923518	91.577269	72.366682
619.100020	97.028872	72.371687
618.363948	92.349407	72.376692
617.427900	96.317225	72.381697
616.340423	96.623582	72.386702
615.779691	88.898869	72.391706
615.325761	94.585166	72.396711
614.753031	91.899041	72.401716
613.760215	92.930451	72.406721
612.757002	97.861430	72.411726
612.416009	87.148596	72.416730
611.966615	93.991017	72.421735
611.662148	93.988372	72.426740
611.145919	87.634374	72.431745
610.086588	95.853843	72.436750
609.351999	83.855368	72.441754
608.983880	90.205472	72.446759
607.731190	93.711650	72.451764
606.963694	86.378789	72.456769
605.870575	97.737670	72.461774
605.805217	93.921003	72.466778
605.277478	99.420616	72.471783
604.886361	93.658960	72.476788
604.646030	95.730200	72.481793
603.371964	100.733240	72.486798
602.774698	95.845666	72.491802
602.351249	95.956163	72.496807
601.617069	99.898873	72.501812
600.738400	89.363414	72.506817
599.395297	98.018320	72.511822
599.176289	94.404809	72.516826
598.519173	103.435189	72.521831
598.332149	101.858835	72.526836
597.845720	87.441675	72.531841
596.931349	98.488109	72.536846
596.356467	90.816742	72.541850
595.512964	88.595801	72.546855
594.862325	98.893675	72.551860
594.022750	90.249297	72.556865
592.909421	94.200521	72.561870
592.645517	89.536084	72.566874
592.103007	92.949408	72.571879
591.610776	83.984228	72.576884
591.420576	86.911297	72.581889
590.245672	96.179979	72.586894
589.454136	95.092828	72.591898
588.904951	93.246963	72.596903
588.359667	91.744620	72.601908
587.413748	83.341481	72.606913
586.456462	89.443203	72.611918
586.132243	90.101534	72.616922
585.433320	98.754625	72.621927
585.235476	89.067206	72.626932
584.983249	83.398202	72.631937
583.548505	91.473187	72.636942
583.294058	85.002901	72.641946
581.908443	95.439324	72.646951
581.287457	98.551905	72.651956
580.356503	89.973710	72.656961
579.635836	93.457819	72.661966
579.651638	86.739930	72.666970
579.029603	86.966947	72.671975
578.766434	89.554435	72.676980
578.250144	81.036248	72.681985
577.094630	92.634751	72.686990
576.571465	84.123266	72.691994
576.128599	87.944230	72.696999
574.999905	92.749089	72.702004
574.277274	80.969222	72.707009
573.690130	96.318794	72.712014
572.895253	89.027734	72.717018
572.309947	95.188881	72.722023
571.411518	84.845096	72.727028
570.981881	89.478874	72.732033
570.246051	89.228051	72.737038
570.132502	88.726939	72.742042
569.455550	90.310124	72.747047
568.138049	88.587608	72.752052
568.004748	90.606960	72.757057
567.367279	88.957792	72.762062
566.198862	83.353397	72.767066
565.515361	87.991987	72.772071
564.742889	91.205122	72.777076
564.224730	81.736396	72.782081
563.761697	90.197104	72.787086
563.517835	79.272262	72.792090
562.530182	84.783962	72.797095
561.470353	83.305837	72.802100
561.433435	83.061974	72.807105
560.328997	80.427881	72.812110
560.043169	76.359670	72.817114
558.811733	78.487432	72.822119
558.162700	74.857610	72.827124
557.882351	78.201151	72.832129
557.124929	85.267254	72.837134
557.045382	79.577748	72.842138
555.820487	79.517686	72.847143
555.115699	82.013084	72.852148
554.721053	76.641627	72.857153
553.573503	87.788793	72.862158
553.532061	79.176230	72.867162
552.025049	76.943461	72.872167
551.387616	74.365929	72.877172
551.039689	70.178895	72.882177
550.290646	77.735370	72.887182
550.257075	80.917033	72.892186
549.508341	79.838345	72.897191
548.798309	75.733875	72.902196
548.014975	69.556703	72.907201
547.133965	76.761207	72.912206
546.830773	73.556446	72.917210
545.670506	80.011480	72.922215
545.076175	91.169252	72.927220
544.570748	82.369359	72.932225
544.029477	84.773984	72.937230
543.686580	74.268328	72.942234
542.370723	76.439767	72.947239
541.839863	77.982925	72.952244
541.300602	72.866365	72.957249
540.599915	78.371529	72.962254
540.385339	83.057664	72.967258
539.502477	86.557330	72.972263
538.638061	76.858219	72.977268
538.183298	83.146986	72.982273
537.293790	81.509035	72.987278
536.502357	76.624354	72.992282
535.866707	76.240721	72.997287
535.077433	84.919550	73.002292
534.754207	74.281849	73.007297
534.177142	87.218390	73.012302
533.654712	78.270240	73.017306
532.812087	81.748801	73.022311
532.132183	78.089933	73.027316
531.883174	79.359815	73.032321
530.720950	74.348414	73.037326
529.785851	78.551328	73.042330
529.286342	82.805128	73.047335
528.461221	76.779977	73.052340
528.513789	75.242310	73.057345
527.473519	80.496205	73.062350
526.772204	76.781405	73.067354
526.100314	80.083486	73.072359
525.410265	87.188572	73.077364
525.110319	82.808987	73.082369
524.274641	80.790786	73.087374
523.367444	79.944898	73.092378
522.877201	84.127642	73.097383
522.361247	82.404770	73.102388
521.600765	82.002268	73.107393
520.510664	81.903331	73.112398
520.078821	73.564494	73.117402
519.381926	82.746541	73.122407
518.768226	92.140902	73.127412
518.673935	80.776386	73.132417
517.468659	85.048883	73.137422
516.762616	81.669214	73.142426
516.352851	84.917307	73.147431
515.423230	92.633804	73.152436
514.568050	85.145868	73.157441
513.571108	89.448588	73.162446
512.975272	78.056727	73.167450
512.673174	76.648113	73.172455
512.530649	77.806205	73.177460
512.495820	70.565720	73.182465
511.342473	88.992762	73.187470
510.525396	78.119569	73.192474
509.834046	76.875144	73.197479
508.877361	79.665534	73.202484
507.920741	78.680495	73.207489
507.131279	82.388357	73.212494
506.753492	84.803261	73.217498
506.365955	83.567566	73.222503
505.777998	86.871848	73.227508
505.546163	74.513338	73.232513
504.078701	82.682751	73.237518
503.458834	79.873283	73.242522
503.170838	79.873349	73.247527
502.450340	77.174276	73.252532
502.331581	74.218952	73.257537
501.289476	79.286071	73.262542
500.744054	76.006378	73.267546
499.730094	76.095308	73.272551
498.428146	75.317458	73.277556
498.020117	78.082915	73.282561
497.496763	81.275476	73.287566
497.172938	79.343252	73.292570
496.545351	75.290977	73.297575
495.704077	75.231511	73.302580
494.910382	77.746886	73.307585
494.307851	85.568379	73.312590
494.183162	73.342293	73.317594
493.412746	80.809284	73.322599
492.289529	84.693933	73.327604
491.879416	67.889552	73.332609
491.133333	77.433291	73.337614
490.487496	71.266912	73.342618
489.233587	73.104481	73.347623
488.025695	82.291985	73.352628
488.780416	75.004235	73.357633
487.935620	84.825008	73.362638
486.911959	68.485733	73.367642
486.943327	80.785944	73.372647
485.862089	85.049430	73.377652
485.083196	73.374755	73.382657
484.194054	82.489486	73.387662
483.769396	69.488672	73.392666
483.384409	72.637393	73.397671
482.898442	72.754271	73.402676
482.182038	79.679937	73.407681
481.249562	88.153191	73.412686
480.616323	84.741713	73.417690
479.944559	86.840303	73.422695
478.527011	83.145215	73.427700
478.577473	79.328054	73.432705
478.100381	79.315525	73.437710
477.678075	79.754632	73.442714
476.950559	68.786771	73.447719
475.609765	82.754507	73.452724
474.957237	79.285946	73.457729
474.390928	74.138902	73.462734
474.352012	73.583165	73.467738
473.324917	77.146629	73.472743
472.315513	83.870677	73.477748
471.934769	73.740180	73.482753
471.144692	82.150746	73.487758
470.758890	79.847852	73.492762
470.307481	85.966321	73.497767
469.306160	81.589692	73.502772
468.933256	70.643565	73.507777
468.471282	81.243028	73.512782
467.041649	76.136949	73.517786
466.329930	78.785903	73.522791
465.734375	82.112804	73.527796
465.621164	71.910812	73.532801
465.097195	84.510246	73.537806
463.967264	79.143221	73.542810
462.783387	77.517439	73.547815
462.269621	86.844942	73.552820
461.940032	74.364251	73.557825
461.522120	87.106161	73.562830
461.180856	79.182837	73.567834
460.369120	83.804332	73.572839
459.145695	86.715433	73.577844
458.867488	81.765324	73.582849
458.019367	86.752243	73.587854
457.398199	90.327466	73.592858
456.381729	90.917725	73.597863
455.639321	88.075185	73.602868
455.536394	81.521721	73.607873
454.811038	87.125063	73.612878
454.706031	85.645579	73.617882
453.869168	88.501100	73.622887
452.895442	90.668803	73.627892
452.399273	78.503216	73.632897
450.940067	88.936874	73.637902
449.955176	92.190369	73.642906
449.898238	89.159325	73.647911
449.299147	94.564993	73.652916
449.013973	83.698953	73.657921
448.599702	87.607780	73.662926
448.186572	82.421071	73.667930
447.160074	85.313824	73.672935
446.149151	87.841563	73.677940
445.747145	83.748667	73.682945
444.398484	90.138511	73.687950
443.727978	78.691571	73.692954
443.538918	78.689686	73.697959
442.615964	77.531929	73.702964
442.679987	80.219660	73.707969
441.934672	87.154628	73.712974
440.810274	85.646150	73.717978
439.950483	93.071628	73.722983
439.354848	97.618208	73.727988
439.044993	86.054204	73.732993
438.674060	86.315575	73.737998
437.636162	87.989835	73.743002
436.884602	92.728516	73.748007
436.446432	93.974373	73.753012
435.988194	83.345610	73.758017
434.627828	92.691089	73.763022
433.778290	89.113011	73.768026
433.513657	92.486626	73.773031
432.873264	87.046773	73.778036
432.811000	93.856016	73.783041
431.810070	95.621832	73.788046
430.586679	94.461877	73.793050
430.269890	91.508516	73.798055
429.623976	91.569129	73.803060
429.452891	92.061106	73.808065
428.521272	94.057399	73.813070
427.430873	94.975312	73.818074
426.640665	89.316805	73.823079
426.180527	93.778591	73.828084
426.192516	84.333119	73.833089
425.308672	91.799033	73.838094
424.475673	88.053923	73.843098
423.594211	89.041817	73.848103
423.030913	91.276949	73.853108
422.756330	84.128073	73.858113
421.364786	86.102131	73.863118
420.995218	90.117372	73.868122
420.561538	86.222131	73.873127
419.875694	89.509249	73.878132
419.608143	83.403576	73.883137
418.214693	90.705779	73.888142
417.628665	86.412725	73.893146
416.977628	85.979643	73.898151
416.286613	99.684880	73.903156
416.258431	84.967022	73.908161
414.720033	84.697051	73.913166
414.313980	92.452121	73.918170
413.796985	90.232893	73.923175
412.873112	95.031893	73.928180
413.155952	90.108399	73.933185
412.096481	93.473360	73.938190
410.995626	86.371344	73.943194
410.259236	87.356089	73.948199
409.971244	93.509714	73.953204
409.636268	91.746764	73.958209
408.456222	92.084029	73.963214
407.959153	88.363851	73.968218
407.492540	85.736938	73.973223
406.408903	91.342870	73.978228
405.703087	84.303023	73.983233
404.605483	95.554145	73.988238
404.282705	93.740951	73.993242
404.422517	90.457128	73.998247
403.956229	92.157777	74.003252
403.254614	90.456077	74.008257
402.342462	83.505665	74.013262
400.961054	84.780931	74.018266
400.157789	79.234007	74.023271
399.002609	93.393361	74.028276
399.502099	85.063091	74.033281
398.616031	92.580306	74.038286
397.899143	88.755309	74.043290
397.418855	86.233760	74.048295
396.718073	91.957627	74.053300
396.259104	89.003373	74.058305
395.201496	92.263813	74.063310
394.692867	92.347086	74.068314
394.299126	87.279420	74.073319
393.423261	91.227880	74.078324
392.563772	84.941823	74.083329
391.512640	96.196826	74.088334
390.972692	93.794046	74.093338
390.700683	94.990907	74.098343
390.221078	100.111648	74.103348
389.921571	82.612183	74.108353
388.651006	89.494675	74.113358
387.925880	92.128572	74.118362
387.634883	83.837060	74.123367
386.582929	85.495188	74.128372
385.906839	86.694983	74.133377
384.994761	95.461973	74.138382
384.729437	87.985482	74.143386
384.565644	78.776970	74.148391
383.794512	93.344165	74.153396
382.791764	86.927537	74.158401
382.055587	90.171973	74.163406
381.292317	96.526643	74.168410
381.154180	97.121917	74.173415
380.252382	91.791997	74.178420
379.571136	83.709459	74.183425
378.610117	87.910129	74.188430
378.116805	86.793619	74.193434
377.866932	82.978984	74.198439
376.428656	92.587677	74.203444
375.981009	85.848966	74.208449
375.404351	93.351448	74.213454
374.861420	92.183445	74.218458
374.647527	88.614469	74.223463
373.662710	87.288918	74.228468
373.173353	86.924840	74.233473
372.105083	87.181383	74.238478
371.832141	93.840817	74.243482
370.900551	89.857630	74.248487
370.128909	89.600344	74.253492
369.646391	85.293507	74.258497
369.390754	92.952936	74.263502
368.269543	93.893510	74.268506
367.525303	91.037880	74.273511
366.418676	87.830695	74.278516
366.428399	88.859284	74.283521
365.683263	91.855800	74.288526
365.020015	88.288047	74.293530
364.144041	79.819307	74.298535
363.185861	90.094099	74.303540
362.762621	95.733700	74.308545
362.501193	94.254184	74.313550
361.885936	100.596518	74.318554
361.126002	98.669176	74.323559
360.176220	96.245061	74.328564
359.913513	86.942979	74.333569
359.284832	88.985256	74.338574
358.353429	98.589982	74.343578
357.634408	89.925404	74.348583
356.939283	99.165976	74.353588
357.047933	92.294434	74.358593
355.639734	97.733380	74.363598
354.759693	95.658476	74.368602
354.149827	91.153214	74.373607
353.735155	96.170466	74.378612
353.359953	89.890627	74.383617
352.235659	91.177894	74.388622
351.339191	86.646361	74.393626
351.292733	93.716556	74.398631
350.175521	92.938665	74.403636
350.046743	93.156175	74.408641
349.414513	95.668769	74.413646
348.058860	90.737537	74.418650
347.929173	77.128470	74.423655
346.978036	90.954062	74.428660
346.644054	96.834534	74.433665
345.853321	85.648599	74.438670
344.754936	84.091086	74.443674
344.528485	81.038180	74.448679
343.876506	86.933280	74.453684
343.438704	89.096390	74.458689
342.059255	83.315874	74.463694
341.262935	92.472344	74.468698
340.688855	84.238826	74.473703
340.156597	93.635815	74.478708
340.102378	86.538388	74.483713
339.498321	88.195946	74.488718
338.786837	88.400036	74.493722
338.180121	86.890886	74.498727
337.417949	82.590536	74.503732
337.008262	86.358460	74.508737
335.829805	90.161429	74.513742
334.888914	96.085126	74.518746
334.381971	84.438086	74.523751
333.836321	95.267014	74.528756
333.728497	90.964646	74.533761
332.392509	91.157350	74.538766
331.779852	92.282338	74.543770
331.036044	82.608006	74.548775
330.568322	89.180826	74.553780
330.355188	85.505547	74.558785
329.781031	86.248172	74.563790
328.847371	94.229838	74.568794
328.462126	89.163883	74.573799
327.140414	101.878729	74.578804
326.341329	89.081831	74.583809
325.693128	96.876823	74.588814
324.894768	90.033234	74.593818
324.860069	84.098442	74.598823
324.132507	95.789413	74.603828
323.647387	95.299490	74.608833
322.480332	88.367521	74.613838
321.715450	91.480708	74.618842
321.444253	88.090099	74.623847
320.907348	83.490242	74.628852
320.093121	83.755755	74.633857
319.372307	90.373924	74.638862
318.759236	96.196050	74.643866
318.538322	88.007002	74.648871
317.345699	92.020022	74.653876
316.189466	79.638400	74.658881
315.712345	92.349799	74.663886
315.456821	92.274447	74.668890
314.893945	89.282751	74.673895
313.978225	94.529943	74.678900
314.014654	91.737097	74.683905
312.655986	89.876853	74.688910
311.625687	89.983623	74.693914
311.499108	92.194048	74.698919
310.878525	95.037392	74.703924
310.046715	91.608660	74.708929
308.840061	94.083529	74.713934
308.214590	96.986128	74.718938
308.132574	88.492637	74.723943
307.418217	96.606053	74.728948
307.252258	94.313257	74.733953
306.819514	97.754368	74.738958
305.936657	95.683509	74.743962
305.365957	88.430275	74.748967
304.057738	90.410610	74.753972
303.038111	86.908288	74.758977
302.371879	87.589333	74.763982
301.906687	100.686300	74.768986
301.489815	97.862991	74.773991
300.955840	94.839503	74.778996
300.837449	94.576844	74.784001
299.736758	94.707127	74.789006
298.698598	94.038455	74.794010
298.496647	91.883267	74.799015
297.641206	100.667007	74.804020
296.641687	94.920067	74.809025
295.974698	92.303431	74.814030
295.036081	95.110499	74.819034
294.813149	93.385985	74.824039
294.324134	102.283757	74.829044
294.266012	95.522899	74.834049
293.275729	91.814641	74.839054
292.618544	92.446377	74.844058
292.099576	86.887458	74.849063
290.695847	92.917325	74.854068
289.527933	92.586267	74.859073
289.018844	89.035919	74.864078
288.365836	92.485177	74.869082
288.507836	88.466028	74.874087
287.869449	94.566028	74.879092
287.710572	92.612656	74.884097
286.861630	96.910179	74.889102
285.860767	93.614630	74.894106
285.303026	85.229912	74.899111
284.016135	90.648872	74.904116
283.553741	94.139272	74.909121
282.738218	85.755317	74.914126
282.183718	91.675555	74.919130
281.970484	84.883659	74.924135
281.355795	98.479110	74.929140
280.327267	87.065939	74.934145
280.050215	97.766339	74.939150
279.136939	91.590572	74.944154
278.970256	86.116137	74.949159
277.273234	101.631450	74.954164
277.063870	93.625939	74.959169
276.353669	90.515430	74.964174
275.700280	92.853248	74.969178
275.388610	87.374849	74.974183
274.320838	90.355624	74.979188
273.563439	91.253996	74.984193
273.443422	90.122068	74.989198
272.925994	93.679135	74.994202
271.629685	85.508629	74.999207
270.809890	89.602617	75.004212
270.355560	84.449045	75.009217
269.861965	87.749411	75.014222
269.200241	96.833087	75.019226
268.874370	86.649403	75.024231
268.019932	90.454875	75.029236
267.165555	94.973186	75.034241
266.625592	92.222686	75.039246
265.955606	91.604596	75.044250
264.950726	87.061666	75.049255
264.236770	100.276263	75.054260
263.872502	97.565118	75.059265
263.674050	88.569780	75.064270
262.946963	96.249620	75.069274
262.095362	91.320836	75.074279
261.122317	96.013424	75.079284
261.048137	82.401565	75.084289
259.675687	91.018537	75.089294
258.971600	95.072961	75.094298
258.207721	87.333012	75.099303
257.589705	93.615432	75.104308
257.145657	82.214194	75.109313
257.141126	81.949784	75.114318
256.261842	97.729125	75.119322
255.455873	85.626151	75.124327
254.446301	86.844438	75.129332
254.309413	91.938415	75.134337
253.648483	88.550273	75.139342
252.570113	95.634311	75.144346
252.003588	85.524639	75.149351
251.344989	97.656921	75.154356
250.985469	96.591699	75.159361
249.831848	92.133077	75.164366
248.618613	92.260557	75.169370
248.371097	94.280146	75.174375
247.726924	93.214375	75.179380
247.434604	90.490902	75.184385
247.402066	90.905063	75.189390
246.547100	97.591231	75.194394
245.649940	87.105231	75.199399
244.645092	93.571182	75.204404
244.123968	94.540370	75.209409
243.353866	90.250475	75.214414
242.296251	93.659356	75.219418
241.931464	84.768317	75.224423
241.153912	89.060319	75.229428
241.185493	90.870634	75.234433
240.311557	90.832206	75.239438
238.893186	90.409887	75.244442
238.607919	86.300561	75.249447
237.849794	91.096437	75.254452
237.401096	94.177546	75.259457
237.159074	87.097714	75.264462
236.099403	95.281371	75.269466
235.345246	90.241162	75.274471
234.733098	102.793748	75.279476
234.356536	89.852227	75.284481
234.187958	84.275892	75.289486
232.673287	82.991850	75.294490
232.159376	80.924477	75.299495
231.656426	89.605961	75.304500
231.411901	83.291509	75.309505
230.487921	86.369612	75.314510
229.017247	94.453991	75.319514
228.957455	86.100770	75.324519
228.217581	96.259219	75.329524
227.588440	87.248107	75.334529
226.290386	85.281192	75.339534
225.797490	84.832873	75.344538
225.421323	81.241203	75.349543
225.068782	89.360100	75.354548
224.577885	87.328254	75.359553
224.292065	89.531239	75.364558
222.890692	91.227977	75.369562
222.426137	89.442652	75.374567
221.596846	91.964958	75.379572
221.084288	86.138919	75.384577
219.927031	88.293124	75.389582
218.958514	90.324986	75.394586
218.985910	81.993927	75.399591
218.263254	92.840956	75.404596
217.978548	90.652988	75.409601
217.376069	93.926235	75.414606
216.179855	98.682344	75.419610
215.658880	89.160095	75.424615
215.108514	92.341126	75.429620
214.423752	88.503947	75.434625
213.748704	92.504059	75.439630
212.695449	94.383090	75.444634
212.416848	89.037573	75.449639
211.948904	88.271579	75.454644
211.613602	90.783816	75.459649
210.450151	84.827386	75.464654
209.419938	94.208681	75.469658
209.415538	80.630262	75.474663
208.427259	97.179026	75.479668
207.413413	92.817634	75.484673
206.774841	96.773209	75.489678
206.200500	97.296816	75.494682
206.177369	89.387282	75.499687
205.247293	104.626690	75.504692
204.742886	99.159227	75.509697
204.209936	93.118803	75.514702
203.389303	98.489046	75.519706
202.994647	98.834232	75.524711
201.559363	101.314765	75.529716
201.051003	98.495307	75.534721
199.868571	97.256557	75.539726
199.319535	95.300596	75.544730
199.334812	82.455730	75.549735
198.601458	93.162892	75.554740
197.574459	91.385167	75.559745
196.830605	88.586342	75.564750
196.266568	94.820042	75.569754
196.001556	83.798233	75.574759
195.156177	88.819450	75.579764
195.056970	90.624552	75.584769
194.425497	93.969873	75.589774
193.044022	94.035026	75.594778
192.903151	91.160081	75.599783
191.773544	89.932015	75.604788
190.980569	88.029710	75.609793
190.602975	91.033506	75.614798
189.673692	93.361786	75.619802
189.336864	86.259134	75.624807
188.739035	97.511058	75.629812
187.614334	93.688507	75.634817
187.043103	90.396704	75.639822
186.153681	96.968003	75.644826
186.206937	85.590871	75.649831
185.689593	92.613883	75.654836
184.711646	85.078793	75.659841
183.632843	91.394018	75.664846
182.943914	97.579264	75.669850
182.718599	84.813531	75.674855
182.325681	92.670947	75.679860
181.519638	92.725885	75.684865
180.509459	90.245064	75.689870
179.505682	92.625981	75.694874
179.504770	87.997424	75.699879
179.205834	97.074178	75.704884
178.164336	91.694838	75.709889
177.272167	92.422522	75.714894
176.677744	93.939509	75.719898
176.474097	92.012763	75.724903
175.428836	96.037657	75.729908
174.568725	92.189886	75.734913
173.992370	91.451557	75.739918
173.419605	97.269547	75.744922
172.939402	93.971220	75.749927
171.776785	98.023731	75.754932
171.009027	105.226637	75.759937
170.799245	90.537575	75.764942
169.972070	93.429371	75.769946
169.949072	93.322063	75.774951
168.958017	84.996251	75.779956
167.857371	96.412516	75.784961
167.694612	90.755851	75.789966
166.853201	92.532266	75.794970
166.504571	87.389010	75.799975
165.622900	97.087853	75.804980
164.579760	90.324154	75.809985
164.372584	92.167895	75.814990
163.799642	102.939931	75.819994
163.052630	88.197707	75.824999
161.854570	91.207548	75.830004
161.466678	88.483098	75.835009
160.940848	92.327384	75.840014
160.204712	94.544408	75.845018
159.338822	90.614348	75.850023
158.611325	91.266049	75.855028
158.103285	94.230238	75.860033
157.849616	86.901376	75.865038
156.852689	89.498214	75.870042
156.065146	92.722668	75.875047
154.773514	86.803621	75.880052
154.237129	95.638067	75.885057
154.488337	87.954259	75.890062
153.797896	93.409945	75.895066
153.839945	86.846260	75.900071
152.698145	85.455699	75.905076
151.847926	89.017718	75.910081
151.480267	88.770951	75.915086
149.813781	93.336518	75.920090
149.132447	88.378181	75.925095
148.620621	84.491242	75.930100
148.232347	83.031512	75.935105
148.138556	84.186782	75.940110
147.356467	86.562859	75.945114
146.026459	83.089705	75.950119
145.394762	76.973862	75.955124
145.258374	88.630990	75.960129
144.799628	80.602336	75.965134
143.609530	83.413065	75.970138
142.839627	85.582987	75.975143
142.496887	93.174057	75.980148
141.992832	86.016794	75.985153
141.192431	85.323980	75.990158
140.285715	90.477683	75.995162
139.699432	84.972170	76.000167
139.084523	86.231374	76.005172
138.474286	91.125455	76.010177
138.052657	81.243983	76.015182
136.702219	92.527422	76.020186
136.587970	88.877442	76.025191
135.694781	88.121198	76.030196
134.897859	91.633822	76.035201
134.128397	75.449645	76.040206
133.326049	87.834704	76.045210
132.876178	78.717500	76.050215
132.599662	85.758434	76.055220
132.047574	82.679266	76.060225
131.333564	84.013481	76.065230
130.706954	86.259494	76.070234
129.769350	84.262396	76.075239
129.050038	82.453653	76.080244
128.632417	89.395627	76.085249
128.160565	88.024037	76.090254
126.781748	91.106316	76.095258
126.120513	88.928825	76.100263
125.851641	83.764009	76.105268
125.488873	86.580542	76.110273
124.865798	83.823786	76.115278
123.572676	89.473175	76.120282
123.278228	75.106525	76.125287
122.675541	82.395200	76.130292
122.109281	81.813032	76.135297
121.122360	81.073648	76.140302
120.174433	89.361707	76.145306
119.620553	82.183783	76.150311
119.282754	85.875055	76.155316
119.166246	82.307960	76.160321
118.260428	85.318235	76.165326
117.316983	87.159514	76.170330
116.704822	84.534695	76.175335
115.914088	86.159546	76.180340
115.002379	85.014533	76.185345
114.415275	87.277853	76.190350
113.639242	91.902350	76.195354
113.169806	89.168992	76.200359
112.714417	89.133833	76.205364
112.268050	87.898393	76.210369
111.402857	88.236228	76.215374
110.760768	89.429046	76.220378
110.238093	86.808624	76.225383
109.914791	81.670114	76.230388
108.459592	79.540712	76.235393
107.764471	79.260091	76.240398
106.984351	81.809113	76.245402
106.833256	79.188542	76.250407
106.445473	72.653158	76.255412
105.446093	78.459415	76.260417
104.655026	79.708165	76.265422
103.921394	88.568133	76.270426
103.511902	83.286119	76.275431
102.594065	86.410555	76.280436
101.716528	84.108318	76.285441
101.387509	74.228350	76.290446
100.826472	85.979582	76.295450
100.210745	79.578003	76.300455
99.886570	81.865719	76.305460
98.750498	79.374924	76.310465
98.015554	74.277776	76.315470
97.222573	90.305984	76.320474
97.210671	79.475659	76.325479
96.214785	85.824047	76.330484
95.087470	83.849216	76.335489
94.632290	86.126235	76.340494
94.097119	80.777748	76.345498
94.179137	76.609819	76.350503
92.971850	82.343175	76.355508
92.209221	78.631863	76.360513
91.776466	78.910568	76.365518
90.590944	89.093314	76.370522
89.987406	75.787353	76.375527
89.193768	78.163048	76.380532
88.549253	92.426715	76.385537
88.187783	87.642883	76.390542
87.657204	79.522745	76.395546
87.239232	83.631550	76.400551
86.250140	76.258657	76.405556
85.239016	80.859513	76.410561
84.930883	79.978906	76.415566
84.251213	87.119740	76.420570
83.629463	86.417625	76.425575
82.675092	86.563135	76.430580
81.988452	82.540791	76.435585
81.370726	80.869368	76.440590
81.071264	92.114347	76.445594
80.797181	83.446587	76.450599
79.461579	91.634544	76.455604
78.375416	77.660188	76.460609
78.038932	79.800420	76.465614
77.427124	80.690835	76.470618
77.333849	82.559257	76.475623
76.815329	84.026929	76.480628
75.833082	86.832434	76.485633
74.999436	85.040143	76.490638
74.424677	81.593054	76.495642
73.993559	87.450311	76.500647
72.715550	86.445861	76.505652
71.972024	91.643435	76.510657
71.443391	84.806563	76.515662
71.072196	90.338175	76.520666
70.817406	84.426133	76.525671
69.598174	84.215632	76.530676
68.890864	84.742709	76.535681
68.497352	79.029307	76.540686
67.824440	84.018998	76.545690
67.556568	80.994530	76.550695
66.347516	84.253364	76.555700
65.446463	87.819767	76.560705
65.275818	82.914021	76.565710
64.511250	88.401368	76.570714
63.990548	93.555218	76.575719
63.141667	84.250261	76.580724
62.732271	84.405367	76.585729
62.308331	81.348449	76.590734
60.700672	85.512799	76.595738
60.047583	79.369853	76.600743
59.638248	78.484888	76.605748
59.176711	89.898956	76.610753
59.116882	74.025751	76.615758
57.787827	83.415661	76.620762
57.021888	79.845835	76.625767
56.415064	79.690996	76.630772
56.111277	79.974829	76.635777
55.512888	79.828806	76.640782
54.076753	74.448878	76.645786
53.686192	76.459838	76.650791
53.072566	76.082365	76.655796
52.357967	89.036555	76.660801
52.188461	73.795140	76.665806
51.043941	81.072504	76.670810
50.297691	84.150165	76.675815
49.849470	79.899072	76.680820
49.302138	95.745839	76.685825
49.302466	89.082345	76.690830
48.049778	80.992861	76.695834
47.128937	84.326622	76.700839
46.670266	86.653187	76.705844
45.813750	87.770677	76.710849
44.814522	79.504330	76.715854
43.893187	88.086239	76.720858
43.233442	87.653125	76.725863
43.569468	85.913716	76.730868
43.230418	90.447123	76.735873
42.561534	79.256969	76.740878
41.585266	86.403657	76.745882
40.587376	78.062877	76.750887
39.733142	87.913326	76.755892
39.368125	86.424753	76.760897
38.986963	79.677466	76.765902
37.701145	91.222192	76.770906
37.266584	89.333859	76.775911
36.685929	92.137623	76.780916
36.318753	91.372134	76.785921
35.477966	90.466804	76.790926
34.365127	97.525999	76.795930
33.596729	80.266083	76.800935
33.607072	81.755582	76.805940
32.986835	90.226666	76.810945
32.287415	83.503549	76.815950
30.995615	85.014988	76.820954
30.703411	75.806436	76.825959
29.953980	83.519326	76.830964
29.791658	90.342538	76.835969
29.095755	79.268723	76.840974
27.985570	87.163059	76.845978
27.502621	78.740710	76.850983
27.234860	75.966079	76.855988
25.957895	87.332456	76.860993
25.198501	81.091697	76.865998
24.409144	87.024187	76.871002
24.178218	87.240272	76.876007
23.724069	79.933172	76.881012
22.884220	86.649134	76.886017
21.830167	81.770119	76.891022
21.158797	83.103748	76.896026
20.491109	84.293467	76.901031
20.132928	86.248751	76.906036
19.648253	84.310201	76.911041
19.313162	82.915967	76.916046
17.988650	84.294474	76.921050
17.616697	81.561389	76.926055
17.053157	85.375045	76.931060
16.332793	89.396760	76.936065
15.390792	80.635906	76.941070
14.519763	88.005329	76.946074
14.134521	81.456100	76.951079
13.983190	83.470256	76.956084
13.090696	82.794833	76.961089
12.132786	79.634482	76.966094
10.860477	91.146502	76.971098
10.759069	81.108321	76.976103
10.400849	77.721612	76.981108
9.969725	88.304731	76.986113
9.544464	85.211731	76.991118
8.221711	83.401869	76.996122
7.748874	79.233155	77.001127
7.254037	84.757151	77.006132
6.180840	83.472491	77.011137
5.313787	75.623204	77.016142
4.733721	86.006477	77.021147
4.040264	82.565540	77.026151
3.626480	87.027292	77.031156
3.325580	87.233270	77.036161