Tue Jun 08 16:59:07 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
0.099644	106.815289	0.000000
-0.093680	93.237044	0.005005
-0.969985	77.174368	0.010010
-2.509756	28.119073	0.015014
-6.605550	4.442712	0.020019
-12.282685	15.298742	0.025024
-17.046639	5.545901	0.030029
-21.594088	4.185768	0.035034
-25.789761	7.552366	0.040038
-29.107453	3.254331	0.045043
-32.698876	10.378381	0.050048
-36.342442	10.691970	0.055053
-40.091575	13.296009	0.060058
-44.174094	9.595279	0.065062
-47.481725	10.913045	0.070067
-51.228091	6.174223	0.075072
-55.461783	10.964770	0.080077
-59.151116	5.515566	0.085082
-62.949403	12.634849	0.090086
-66.238188	-1.092996	0.095091
-70.420255	9.873419	0.100096
-74.171747	1.663629	0.105101
-77.836064	0.199090	0.110106
-81.691450	5.831437	0.115110
-84.907324	-5.036981	0.120115
-88.737695	6.287530	0.125120
-92.483899	-1.006632	0.130125
-96.718249	6.486245	0.135130
-100.908973	10.101912	0.140134
-104.266229	-10.261455	0.145139
-108.272606	5.435053	0.150144
-112.100290	4.843235	0.155149
-115.295579	10.037963	0.160154
-118.728313	11.379206	0.165158
-122.777709	2.560986	0.170163
-126.600197	4.186557	0.175168
-130.850001	-2.008779	0.180173
-134.665638	3.263527	0.185178
-138.237379	7.749985	0.190182
-141.665979	-0.951662	0.195187
-145.425956	13.904919	0.200192
-148.958915	4.747125	0.205197
-153.242171	0.190460	0.210202
-157.381875	7.918982	0.215206
-160.612028	2.140087	0.220211
-164.588762	12.817962	0.225216
-168.499557	7.193688	0.230221
-171.991719	10.179259	0.235226
-175.968724	13.195486	0.240230
-179.389930	16.026799	0.245235
-183.667268	23.647911	0.250240
-187.265045	10.622056	0.255245
-190.864663	5.777670	0.260250
-194.574991	14.353839	0.265254
-198.222615	9.580054	0.270259
-201.951589	16.438496	0.275264
-205.793133	10.779486	0.280269
-208.979523	11.702784	0.285274
-213.487020	19.735209	0.290278
-216.832676	4.511823	0.295283
-220.875843	8.496999	0.300288
-224.969471	10.760033	0.305293
-227.954829	-0.498307	0.310298
-232.393873	6.875461	0.315302
-235.941823	9.426205	0.320307
-239.995752	12.825127	0.325312
-243.343793	3.285595	0.330317
-247.194514	7.836560	0.335322
-251.052429	14.470064	0.340326
-254.392535	9.220061	0.345331
-258.465051	11.084795	0.350336
-262.395291	3.039248	0.355341
-265.662307	1.167271	0.360346
-269.294803	9.184261	0.365350
-272.961961	8.477026	0.370355
-277.212245	8.712516	0.375360
-281.122870	6.441371	0.380365
-285.020047	7.578604	0.385370
-288.928214	15.596318	0.390374
-292.337406	4.308492	0.395379
-296.054597	7.626021	0.400384
-299.817414	5.742407	0.405389
-303.614587	5.234723	0.410394
-307.416111	11.446917	0.415398
-310.990134	4.436422	0.420403
-314.590209	6.337793	0.425408
-318.760523	10.959423	0.430413
-322.608053	12.629713	0.435418
-326.204407	14.699784	0.440422
-329.590897	-0.132043	0.445427
-333.919450	8.069910	0.450432
-338.037274	7.361486	0.455437
-341.706468	3.686843	0.460442
-345.138030	16.407112	0.465446
-348.548562	6.633273	0.470451
-352.534775	16.928079	0.475456
-356.433069	3.083608	0.480461
-360.100412	3.918209	0.485466
-363.711005	11.521804	0.490470
-367.144677	11.185882	0.495475
-371.304846	12.300017	0.500480
-375.261040	6.350985	0.505485
-378.959169	11.651879	0.510490
-382.710383	9.676746	0.515494
-386.264907	4.919521	0.520499
-390.334840	13.104396	0.525504
-393.849302	14.319349	0.530509
-397.614008	16.361913	0.535514
-401.551377	24.341707	0.540518
-405.042211	15.337948	0.545523
-409.283068	13.345395	0.550528
-412.866178	12.194415	0.555533
-416.450739	4.736642	0.560538
-420.139327	16.108520	0.565542
-423.620534	6.194908	0.570547
-427.974685	12.447531	0.575552
-431.733876	12.396828	0.580557
-434.911249	1.309739	0.585562
-439.240785	18.920223	0.590566
-442.746791	7.910040	0.595571
-446.566023	16.640464	0.600576
-450.434946	9.484116	0.605581
-453.786498	12.227502	0.610586
-457.732705	11.002282	0.615590
-461.423113	3.513371	0.620595
-465.543321	6.345217	0.625600
-469.600241	14.312019	0.630605
-473.120756	8.050326	0.635610
-476.857627	11.781083	0.640614
-480.559030	4.670232	0.645619
-484.069843	8.955062	0.650624
-487.698394	6.292709	0.655629
-491.725701	-0.115289	0.660634
-495.525238	15.567335	0.665638
-499.383608	6.257671	0.670643
-502.922127	13.860449	0.675648
-506.649549	0.448232	0.680653
-510.455773	4.750609	0.685658
-514.158807	13.043151	0.690662
-518.066064	2.183984	0.695667
-521.925561	7.495700	0.700672
-525.371416	12.637775	0.705677
-529.312935	3.029405	0.710682
-533.282312	7.050738	0.715686
-536.892757	1.543031	0.720691
-541.051871	7.095630	0.725696
-544.596771	7.827669	0.730701
-548.054828	2.808129	0.735706
-552.106284	6.471352	0.740710
-555.470574	4.468663	0.745715
-559.135914	1.501654	0.750720
-563.043885	11.500193	0.755725
-566.832366	2.663701	0.760730
-570.851972	7.888070	0.765734
-574.392951	5.867559	0.770739
-578.307509	7.882699	0.775744
-581.719190	5.748436	0.780749
-585.520462	3.853906	0.785754
-589.878070	11.172191	0.790758
-593.408234	7.729681	0.795763
-597.099942	9.291761	0.800768
-601.441707	14.753398	0.805773
-604.832855	-0.234468	0.810778
-608.265162	6.100514	0.815782
-611.506116	2.334073	0.820787
-615.972213	10.479357	0.825792
-619.632146	8.984915	0.830797
-623.041483	8.722774	0.835802
-627.299487	15.544039	0.840806
-630.643760	9.104619	0.845811
-634.674437	5.681325	0.850816
-638.255158	4.376581	0.855821
-642.024879	-4.148471	0.860826
-646.032818	4.312136	0.865830
-649.612899	-3.968367	0.870835
-653.768496	6.239693	0.875840
-657.872020	11.682207	0.880845
-660.641840	-2.977258	0.885850
-664.500328	8.336713	0.890854
-668.242897	12.819731	0.895859
-672.395384	3.713068	0.900864
-676.280282	8.904543	0.905869
-679.695431	2.624160	0.910874
-683.830705	13.143738	0.915878
-687.395534	7.213496	0.920883
-691.609455	8.388466	0.925888
-695.093488	15.461019	0.930893
-698.612513	11.586849	0.935898
-702.476096	14.735238	0.940902
-705.964321	3.958283	0.945907
-709.886358	1.259652	0.950912
-713.524745	3.395265	0.955917
-717.651679	0.955209	0.960922
-721.397937	11.878546	0.965926
-724.840222	6.044535	0.970931
-728.706941	16.143881	0.975936
-732.862005	20.243042	0.980941
-736.271934	19.287985	0.985946
-740.138122	18.785813	0.990950
-743.560320	9.239305	0.995955
-747.265030	10.997148	1.000960
-751.122879	16.094052	1.005965
-754.930902	12.117172	1.010970
-759.139013	15.366579	1.015974
-762.749356	6.279849	1.020979
-766.288798	3.646649	1.025984
-769.952747	14.835744	1.030989
-773.423637	1.292535	1.035994
-777.954478	15.650322	1.040998
-781.256486	2.656379	1.046003
-785.100120	13.537666	1.051008
-789.167368	4.924484	1.056013
-793.152600	3.460367	1.061018
-796.856061	12.333019	1.066022
-800.104798	4.579154	1.071027
-803.487831	14.347269	1.076032
-807.300068	9.339398	1.081037
-811.117467	11.968018	1.086042
-815.236340	11.185624	1.091046
-819.067537	8.874892	1.096051
-822.962578	14.239535	1.101056
-826.194736	13.997665	1.106061
-830.140839	9.703529	1.111066
-834.243594	15.157909	1.116070
-837.784089	4.330447	1.121075
-841.649241	11.578250	1.126080
-845.858497	4.927905	1.131085
-848.942778	-1.159274	1.136090
-852.703924	7.824759	1.141094
-856.346077	2.256862	1.146099
-860.444432	4.576934	1.151104
-863.953624	10.547959	1.156109
-867.961880	-0.752163	1.161114
-871.898538	8.268327	1.166118
-875.151615	6.460337	1.171123
-879.294266	4.317193	1.176128
-882.767854	13.628442	1.181133
-886.429319	-0.521764	1.186138
-890.592618	11.535045	1.191142
-894.131133	5.590603	1.196147
-898.091592	14.046431	1.201152
-901.826577	10.237531	1.206157
-905.390063	6.833767	1.211162
-909.278228	18.230389	1.216166
-913.086699	11.533811	1.221171
-917.070101	17.554705	1.226176
-921.092540	13.783720	1.231181
-924.156934	6.119489	1.236186
-928.054998	10.900969	1.241190
-931.823256	8.556642	1.246195
-935.317084	13.282944	1.251200
-939.336297	17.077152	1.256205
-942.524187	8.282382	1.261210
-946.675320	15.506346	1.266214
-950.627174	9.332144	1.271219
-954.420172	12.153656	1.276224
-958.404601	15.513654	1.281229
-961.635885	8.097559	1.286234
-965.480379	10.396252	1.291238
-969.230087	10.842503	1.296243
-973.289657	9.248433	1.301248
-977.249158	7.038420	1.306253
-980.973819	1.764647	1.311258
-984.652486	9.673260	1.316262
-988.019600	3.268852	1.321267
-991.692700	5.844434	1.326272
-995.794949	10.250926	1.331277
-999.261780	5.721922	1.336282
-1003.641989	8.999129	1.341286
-1006.924515	3.252005	1.346291
-1010.868316	1.391011	1.351296
-1014.785881	4.466047	1.356301
-1018.080036	-0.503474	1.361306
-1022.249216	6.090544	1.366310
-1025.970922	1.705973	1.371315
-1029.753442	-3.307970	1.376320
-1033.521033	4.505822	1.381325
-1037.193067	2.236249	1.386330
-1040.897144	12.693146	1.391334
-1044.715954	0.198670	1.396339
-1048.520196	3.622539	1.401344
-1052.467279	2.205402	1.406349
-1055.957431	-7.161001	1.411354
-1059.844158	4.578086	1.416358
-1063.715782	1.207238	1.421363
-1067.294013	-4.753909	1.426368
-1070.993244	-2.201010	1.431373
-1074.864804	-3.359930	1.436378
-1078.654787	4.962572	1.441382
-1082.495282	5.034147	1.446387
-1086.043321	0.701121	1.451392
-1089.893894	6.129006	1.456397
-1093.535673	1.594205	1.461402
-1097.329973	6.619307	1.466406
-1101.067687	-2.726653	1.471411
-1104.852155	-5.021067	1.476416
-1108.858544	6.298116	1.481421
-1112.123604	0.815296	1.486426
-1116.153338	2.303232	1.491430
-1119.835561	3.653743	1.496435
-1123.874280	3.462575	1.501440
-1127.626169	4.752035	1.506445
-1131.150289	-4.132059	1.511450
-1135.098143	-4.220802	1.516454
-1138.501170	2.375566	1.521459
-1142.319138	8.597175	1.526464
-1146.283405	8.667957	1.531469
-1150.029359	3.016319	1.536474
-1154.027767	8.050467	1.541478
-1157.260191	2.809560	1.546483
-1161.315219	12.837379	1.551488
-1164.878066	3.973382	1.556493
-1168.580620	-6.392149	1.561498
-1172.649264	9.116912	1.566502
-1176.427779	2.858702	1.571507
-1179.722576	2.524839	1.576512
-1184.155489	6.197298	1.581517
-1187.585999	-2.181414	1.586522
-1191.451826	13.455060	1.591526
-1194.933347	0.599686	1.596531
-1198.891155	7.443333	1.601536
-1202.695113	9.830791	1.606541
-1205.904647	-1.297081	1.611546
-1210.303260	7.100049	1.616550
-1213.720122	-2.690868	1.621555
-1217.620194	6.344147	1.626560
-1221.641721	15.869727	1.631565
-1225.187309	8.595850	1.636570
-1229.288939	8.537155	1.641574
-1232.769785	3.198063	1.646579
-1236.560412	5.016466	1.651584
-1240.562911	10.567668	1.656589
-1244.098595	7.660306	1.661594
-1247.905515	18.997061	1.666598
-1251.618300	8.570996	1.671603
-1255.185031	5.730945	1.676608
-1258.991580	9.908488	1.681613
-1262.806448	-1.765450	1.686618
-1266.438481	9.251564	1.691622
-1270.336074	3.417679	1.696627
-1273.593228	2.617199	1.701632
-1277.906432	4.453947	1.706637
-1281.534258	2.619463	1.711642
-1285.606141	8.563511	1.716646
-1289.718928	9.298174	1.721651
-1293.223993	9.582308	1.726656
-1296.563673	10.006974	1.731661
-1299.720264	-0.388259	1.736666
-1303.704567	7.582568	1.741670
-1307.653429	1.704636	1.746675
-1311.934686	4.467038	1.751680
-1316.126360	14.900139	1.756685
-1319.686364	-3.923772	1.761690
-1323.515551	6.359841	1.766694
-1326.898647	3.329641	1.771699
-1329.992910	8.317985	1.776704
-1334.061477	8.858795	1.781709
-1337.849357	1.842940	1.786714
-1341.810158	11.821967	1.791718
-1345.439055	2.982117	1.796723
-1349.361151	3.180047	1.801728
-1353.429781	5.822687	1.806733
-1356.457362	3.578088	1.811738
-1360.471229	6.067260	1.816742
-1364.739346	6.591460	1.821747
-1368.277677	1.958227	1.826752
-1372.151311	4.175449	1.831757
-1375.653928	-0.989657	1.836762
-1379.602414	3.478005	1.841766
-1383.601360	7.404517	1.846771
-1386.776182	8.481011	1.851776
-1390.597294	1.311456	1.856781
-1394.018392	-0.104529	1.861786
-1397.788548	-0.418533	1.866790
-1401.854849	1.176602	1.871795
-1405.731735	6.050770	1.876800
-1409.667369	13.741775	1.881805
-1413.400282	-3.089866	1.886810
-1417.144831	5.775321	1.891814
-1420.520696	0.154702	1.896819
-1424.610022	2.909902	1.901824
-1428.694004	8.516713	1.906829
-1431.883915	-1.112875	1.911834
-1435.777043	3.756215	1.916838
-1439.523141	1.791412	1.921843
-1443.032147	1.224578	1.926848
-1447.043185	9.669031	1.931853
-1450.890034	-0.129901	1.936858
-1454.645048	8.138350	1.941862
-1458.325169	2.700678	1.946867
-1462.395671	-0.669961	1.951872
-1466.258557	2.645143	1.956877
-1469.234881	0.508261	1.961882
-1473.509869	8.188544	1.966886
-1477.380776	4.709030	1.971891
-1480.919893	5.962643	1.976896
-1484.981565	5.624595	1.981901
-1488.243710	1.491082	1.986906
-1492.078583	9.303386	1.991910
-1495.921708	9.453548	1.996915
-1500.062379	8.839090	2.006912
-1500.806009	6.369676	2.016909
-1498.418361	4.988197	2.026906
-1495.418325	12.525714	2.036902
-1493.442664	8.453296	2.046899
-1491.570700	11.604540	2.056896
-1489.677697	4.510330	2.066893
-1487.771942	3.860183	2.076890
-1486.215816	5.032734	2.086886
-1483.990447	-1.098537	2.096883
-1482.155129	5.647108	2.106880
-1480.226108	5.141566	2.116877
-1478.103401	2.518024	2.126874
-1476.425762	10.011228	2.136870
-1474.553037	10.721934	2.146867
-1472.719443	9.758934	2.156864
-1470.673351	4.869386	2.166861
-1468.622908	4.863876	2.176858
-1466.908519	8.611303	2.186854
-1464.803627	3.065095	2.196851
-1463.617501	9.195092	2.206848
-1461.237962	6.641256	2.216845
-1458.875733	-5.851085	2.226842
-1457.352284	5.858223	2.236838
-1455.831281	4.140333	2.246835
-1453.734773	7.703164	2.256832
-1451.840918	4.759703	2.266829
-1449.569176	0.576371	2.276826
-1448.142650	4.219521	2.286822
-1446.381441	7.261765	2.296819
-1444.523315	11.557564	2.306816
-1442.406739	4.002881	2.316813
-1440.442442	1.612079	2.326810
-1438.456885	8.037112	2.336806
-1436.584437	5.389000	2.346803
-1435.153827	5.242978	2.356800
-1433.005697	-1.633407	2.366797
-1431.103987	4.863338	2.376794
-1429.069425	5.532827	2.386790
-1426.978700	4.405532	2.396787
-1425.402037	6.179249	2.406784
-1423.724031	6.961368	2.416781
-1421.724840	0.985960	2.426778
-1419.917531	3.261890	2.436774
-1417.998366	5.792882	2.446771
-1416.092103	6.614045	2.456768
-1414.287577	4.938758	2.466765
-1412.111197	4.940493	2.476762
-1410.426152	6.073144	2.486758
-1408.947412	6.769749	2.496755
-1406.710875	9.490469	2.506752
-1404.537130	3.468880	2.516749
-1402.727477	7.571073	2.526746
-1401.146511	10.175977	2.536742
-1399.006423	12.673377	2.546739
-1397.330207	6.414367	2.556736
-1395.526180	1.683417	2.566733
-1393.503723	8.662148	2.576730
-1391.807536	6.557708	2.586726
-1389.906774	6.966439	2.596723
-1387.381080	4.571706	2.606720
-1385.867444	1.984064	2.616717
-1384.174473	2.331269	2.626714
-1382.306693	5.168697	2.636710
-1380.259381	3.348967	2.646707
-1378.542200	-2.379980	2.656704
-1376.542794	5.517628	2.666701
-1374.416413	4.801576	2.676698
-1372.878194	-2.740676	2.686694
-1371.178993	-0.500298	2.696691
-1369.163860	0.237766	2.706688
-1366.925334	-8.119946	2.716685
-1365.267793	-3.700736	2.726682
-1363.977188	-9.156427	2.736678
-1361.819870	-0.862274	2.746675
-1359.511173	5.419955	2.756672
-1357.702324	4.194884	2.766669
-1355.717208	-4.966231	2.776666
-1353.911978	-0.962455	2.786662
-1352.036674	3.405527	2.796659
-1350.436018	3.320830	2.806656
-1348.736777	3.632984	2.816653
-1346.549716	-0.080865	2.826650
-1344.627235	0.658108	2.836646
-1342.676695	-3.565640	2.846643
-1341.071172	4.376325	2.856640
-1339.197082	4.769505	2.866637
-1337.155588	4.644663	2.876634
-1335.204561	-2.723848	2.886630
-1333.321040	5.103186	2.896627
-1331.479685	1.176423	2.906624
-1329.705503	3.349402	2.916621
-1327.818206	0.148258	2.926618
-1326.119160	-1.108526	2.936614
-1324.293757	8.764616	2.946611
-1322.134514	7.633508	2.956608
-1319.932066	2.775268	2.966605
-1318.409552	3.912160	2.976602
-1316.278930	1.109887	2.986598
-1314.685369	2.134590	2.996595
-1312.873340	-1.557906	3.006592
-1310.916752	1.217272	3.016589
-1308.757959	2.947962	3.026586
-1307.073604	-0.234125	3.036582
-1305.141848	-4.250703	3.046579
-1303.308187	-1.122827	3.056576
-1301.577502	0.957252	3.066573
-1299.854834	-1.326778	3.076570
-1297.751470	3.830026	3.086566
-1295.796940	3.640702	3.096563
-1294.044312	6.306669	3.106560
-1291.931912	5.202987	3.116557
-1290.269665	3.660081	3.126554
-1288.393187	2.917041	3.136550
-1286.348470	2.697215	3.146547
-1284.734910	2.811488	3.156544
-1282.312001	3.426997	3.166541
-1280.994802	1.617309	3.176538
-1279.176610	7.605617	3.186534
-1276.937042	3.369009	3.196531
-1275.223225	3.443145	3.206528
-1273.451908	-0.240368	3.216525
-1271.456330	0.165175	3.226522
-1269.585756	2.971746	3.236518
-1267.747121	-1.144621	3.246515
-1265.773079	4.960388	3.256512
-1263.981100	2.572779	3.266509
-1261.809154	4.727272	3.276506
-1259.915261	1.319514	3.286502
-1258.510038	6.701762	3.296499
-1256.469769	-3.703820	3.306496
-1254.467561	-1.257359	3.316493
-1252.871446	-2.862007	3.326490
-1250.778876	-1.739207	3.336486
-1248.918105	1.967369	3.346483
-1247.042021	1.910499	3.356480
-1245.197205	-1.958333	3.366477
-1243.453922	-4.345078	3.376474
-1241.845399	5.003366	3.386470
-1239.263910	11.289411	3.396467
-1237.067050	7.376324	3.406464
-1235.917894	4.938669	3.416461
-1233.906775	0.632633	3.426458
-1232.319919	0.955441	3.436454
-1230.628508	2.920966	3.446451
-1228.127814	3.356370	3.456448
-1226.126851	5.037539	3.466445
-1224.591556	-0.718216	3.476442
-1222.878462	3.198298	3.486438
-1220.973391	0.723704	3.496435
-1218.916962	1.864583	3.506432
-1216.849294	-0.618962	3.516429
-1215.186050	3.540080	3.526426
-1213.306435	2.542414	3.536422
-1211.299917	6.902951	3.546419
-1209.733145	2.034969	3.556416
-1207.469585	-4.326420	3.566413
-1205.593992	0.268435	3.576410
-1204.067805	1.286571	3.586406
-1201.610289	2.845874	3.596403
-1200.410164	7.254791	3.606400
-1198.421650	-1.596611	3.616397
-1196.265321	5.500725	3.626394
-1194.602270	6.134535	3.636390
-1192.542362	6.648817	3.646387
-1190.577416	-1.036617	3.656384
-1189.062346	6.855349	3.666381
-1186.961875	6.483326	3.676378
-1185.074868	3.054650	3.686374
-1182.963139	2.887785	3.696371
-1181.372080	9.692130	3.706368
-1179.541091	3.395549	3.716365
-1177.390004	2.584454	3.726362
-1175.892862	4.728406	3.736358
-1174.162467	1.351922	3.746355
-1172.206832	5.245383	3.756352
-1169.799601	3.516102	3.766349
-1168.273398	-0.073113	3.776346
-1166.289972	3.834945	3.786342
-1164.233433	1.083406	3.796339
-1162.536510	7.549460	3.806336
-1160.717682	2.175815	3.816333
-1158.872594	7.018197	3.826330
-1156.803769	5.209895	3.836326
-1155.260467	1.999126	3.846323
-1153.250325	3.548730	3.856320
-1151.352806	0.700013	3.866317
-1149.532392	9.983269	3.876314
-1147.859603	6.772793	3.886310
-1145.614764	10.024188	3.896307
-1143.934886	7.912368	3.906304
-1141.817497	7.938600	3.916301
-1140.008700	2.513332	3.926298
-1138.240204	5.337099	3.936294
-1136.571698	10.383312	3.946291
-1134.555341	11.142228	3.956288
-1132.287967	5.996278	3.966285
-1130.516214	9.422581	3.976282
-1128.910182	9.918005	3.986278
-1127.084679	7.733365	3.996275
-1125.025277	13.491423	4.006272
-1123.020678	7.449207	4.016269
-1121.449507	7.387444	4.026266
-1119.602326	-0.772150	4.036262
-1117.581658	6.189257	4.046259
-1115.698544	6.056148	4.056256
-1113.706071	2.320098	4.066253
-1112.002444	-0.252256	4.076250
-1110.103201	-8.488363	4.086246
-1108.069461	-2.687560	4.096243
-1106.390660	3.468228	4.106240
-1104.390232	0.588423	4.116237
-1102.350645	1.779282	4.126234
-1100.640777	-0.837216	4.136230
-1098.724235	-4.833312	4.146227
-1097.105637	1.616183	4.156224
-1095.270960	-1.512990	4.166221
-1092.927056	2.720515	4.176218
-1091.374057	-4.077247	4.186214
-1089.396782	-10.447123	4.196211
-1087.244989	-2.564851	4.206208
-1086.084831	-4.149122	4.216205
-1083.694279	-2.247065	4.226202
-1081.964690	-0.371817	4.236198
-1079.988946	-0.429916	4.246195
-1077.882968	-2.875711	4.256192
-1076.208729	-0.482717	4.266189
-1074.233903	0.638653	4.276186
-1072.332070	-4.806515	4.286182
-1070.957309	0.146699	4.296179
-1069.110428	-0.645703	4.306176
-1066.958646	1.290642	4.316173
-1064.882229	-7.706614	4.326170
-1063.376381	-1.581185	4.336166
-1061.296133	3.112975	4.346163
-1059.042171	-1.830263	4.356160
-1057.465075	-1.653522	4.366157
-1055.486316	4.042931	4.376154
-1053.737686	3.637718	4.386150
-1052.159592	3.334899	4.396147
-1050.417249	1.362175	4.406144
-1048.037253	3.167263	4.416141
-1045.991487	0.838528	4.426138
-1044.226678	2.829470	4.436134
-1042.782592	-0.380826	4.446131
-1040.689910	5.939480	4.456128
-1038.938665	2.448807	4.466125
-1036.742491	7.167736	4.476122
-1035.013370	7.000240	4.486118
-1033.068704	3.605200	4.496115
-1031.127717	7.729285	4.506112
-1029.357795	15.276420	4.516109
-1027.484593	6.536169	4.526106
-1025.739167	10.800540	4.536102
-1023.681944	11.925177	4.546099
-1021.537700	8.665816	4.556096
-1020.095764	7.741006	4.566093
-1018.313280	4.720811	4.576090
-1016.262033	6.438899	4.586086
-1013.920280	10.232163	4.596083
-1012.641308	0.497624	4.606080
-1010.760816	-1.159316	4.616077
-1008.762658	3.082221	4.626074
-1006.677368	2.783635	4.636070
-1005.068595	5.113995	4.646067
-1003.066973	6.761567	4.656064
-1001.333222	5.534519	4.666061
-999.034427	11.971225	4.676058
-997.452142	8.029393	4.686054
-995.505607	5.663572	4.696051
-993.842312	4.568766	4.706048
-991.902428	1.830220	4.716045
-990.354802	2.072908	4.726042
-988.155643	2.938044	4.736038
-985.514167	3.775065	4.746035
-984.428267	9.369141	4.756032
-982.615086	5.989581	4.766029
-980.550041	4.366969	4.776026
-978.538395	9.444846	4.786022
-976.793693	11.136934	4.796019
-975.247086	10.910687	4.806016
-973.100809	5.530691	4.816013
-971.051842	-2.780475	4.826010
-969.269773	2.964018	4.836006
-967.627939	1.008580	4.846003
-965.622027	5.454714	4.856000
-963.872609	6.264281	4.865997
-961.843864	4.866066	4.875994
-959.740291	8.681676	4.885990
-957.956635	8.702454	4.895987
-956.334634	10.198249	4.905984
-954.399315	5.486815	4.915981
-952.283099	4.314272	4.925978
-950.721793	3.838503	4.935974
-948.542387	4.522883	4.945971
-946.835753	9.238957	4.955968
-944.973927	10.233164	4.965965
-942.919375	6.421714	4.975962
-941.090295	8.333297	4.985958
-939.414532	9.581161	4.995955
-937.487190	13.750715	5.005952
-935.654366	8.488174	5.015949
-933.616208	4.191852	5.025946
-931.737179	3.573020	5.035942
-930.108482	2.647796	5.045939
-928.018206	15.114514	5.055936
-925.971018	5.887170	5.065933
-923.744778	13.885212	5.075930
-922.344999	8.646427	5.085926
-920.916316	9.359705	5.095923
-918.705057	3.182107	5.105920
-916.727196	5.770056	5.115917
-914.864305	7.579810	5.125914
-913.301188	8.086635	5.135910
-911.046616	7.528628	5.145907
-909.394609	7.298539	5.155904
-907.294322	8.185828	5.165901
-905.440294	5.735146	5.175898
-903.628355	3.644614	5.185894
-901.748028	6.040641	5.195891
-899.861402	3.707673	5.205888
-897.924790	5.374359	5.215885
-896.075805	0.841388	5.225882
-894.467035	1.629678	5.235878
-892.230045	3.552279	5.245875
-890.612776	6.824202	5.255872
-888.665553	4.056379	5.265869
-886.770812	-3.649296	5.275866
-884.991124	0.712405	5.285862
-882.858516	4.752293	5.295859
-881.140635	9.085482	5.305856
-879.454207	4.028705	5.315853
-877.243093	3.696331	5.325850
-875.406068	1.373073	5.335846
-873.511968	10.173525	5.345843
-871.820535	8.492974	5.355840
-869.880978	3.645685	5.365837
-867.987305	4.581106	5.375834
-866.040512	5.100341	5.385830
-864.151697	6.128682	5.395827
-862.615123	4.532022	5.405824
-860.638739	5.276590	5.415821
-858.745738	5.158496	5.425818
-856.469802	5.569465	5.435814
-854.750765	3.784985	5.445811
-853.015418	6.334759	5.455808
-851.179762	5.856594	5.465805
-849.079730	6.341630	5.475802
-847.160708	-2.385475	5.485798
-845.549054	1.135622	5.495795
-843.568553	3.605380	5.505792
-841.687671	3.647458	5.515789
-839.746425	-1.308000	5.525786
-837.933224	7.902753	5.535782
-836.291908	4.570928	5.545779
-834.418935	5.241173	5.555776
-832.413613	10.172799	5.565773
-830.312441	-2.189106	5.575770
-828.706270	-4.145486	5.585766
-826.879733	-0.922895	5.595763
-824.868900	2.496892	5.605760
-822.673000	4.635651	5.615757
-821.029262	5.836892	5.625754
-819.399407	5.133223	5.635750
-817.217325	6.628186	5.645747
-815.353881	4.202799	5.655744
-813.546168	8.418635	5.665741
-811.607908	1.470250	5.675738
-809.909938	2.647563	5.685734
-808.317763	8.800180	5.695731
-805.901605	6.425368	5.705728
-803.863797	-1.609938	5.715725
-802.190435	5.072952	5.725722
-800.527709	1.737860	5.735718
-798.664861	7.836910	5.745715
-796.829196	12.406809	5.755712
-794.776876	7.434673	5.765709
-792.465196	10.212791	5.775706
-790.994567	0.439471	5.785702
-788.949559	1.869842	5.795699
-787.211712	5.508815	5.805696
-785.442475	0.535474	5.815693
-783.830209	4.363177	5.825690
-781.818959	4.433888	5.835686
-779.860760	2.930091	5.845683
-777.869851	1.672826	5.855680
-776.069323	0.806694	5.865677
-774.079778	0.088339	5.875674
-772.148869	1.785309	5.885670
-770.609780	4.693666	5.895667
-768.806079	2.969383	5.905664
-766.806093	2.835734	5.915661
-764.633531	4.810564	5.925658
-762.918187	4.324234	5.935654
-760.913705	3.549967	5.945651
-759.282843	6.365117	5.955648
-757.308124	4.484623	5.965645
-755.268688	6.373228	5.975642
-753.426049	5.892719	5.985638
-751.720852	3.088635	5.995635
-749.887756	5.320920	6.005632
-748.155933	5.306813	6.015629
-745.759150	3.941964	6.025626
-744.056785	0.440423	6.035622
-742.338945	8.622653	6.045619
-740.512538	7.424858	6.055616
-738.410048	5.995513	6.065613
-736.642175	-0.269525	6.075610
-734.795002	-0.284849	6.085606
-732.473959	6.171516	6.095603
-731.199825	6.744207	6.105600
-729.471610	6.110638	6.115597
-727.396158	6.605485	6.125594
-725.420214	12.700181	6.135590
-723.655731	10.503252	6.145587
-721.416073	9.974382	6.155584
-719.776645	6.783221	6.165581
-717.771581	8.469862	6.175578
-716.097653	7.637732	6.185574
-714.246341	2.335742	6.195571
-712.015078	4.823786	6.205568
-710.263178	3.715462	6.215565
-708.450095	2.495069	6.225562
-706.445605	5.896640	6.235558
-704.763284	1.776884	6.245555
-703.063406	3.319485	6.255552
-701.051201	2.153055	6.265549
-698.868361	1.991218	6.275546
-697.228317	-0.520274	6.285542
-695.423479	3.306429	6.295539
-693.587569	3.814736	6.305536
-691.730268	7.694092	6.315533
-689.603261	9.317531	6.325530
-687.766117	11.883896	6.335526
-685.734102	6.840200	6.345523
-684.195957	2.180039	6.355520
-682.335656	2.311084	6.365517
-680.321665	0.415191	6.375514
-678.524370	1.264085	6.385510
-676.871148	3.033650	6.395507
-674.671292	6.302512	6.405504
-672.821623	0.676349	6.415501
-670.820019	-1.432410	6.425498
-669.195472	6.229955	6.435494
-667.065842	1.442609	6.445491
-665.153818	3.950288	6.455488
-663.363409	5.263559	6.465485
-661.792131	5.948107	6.475482
-659.615815	4.958254	6.485478
-658.026246	11.186474	6.495475
-655.770906	4.520455	6.505472
-654.200583	4.844735	6.515469
-651.972193	1.094480	6.525466
-650.673509	2.444317	6.535462
-648.471289	6.805945	6.545459
-646.411462	4.411346	6.555456
-644.725141	2.175694	6.565453
-642.494145	0.097140	6.575450
-640.914201	6.789021	6.585446
-638.883205	9.263256	6.595443
-637.360189	6.148220	6.605440
-635.240003	4.151523	6.615437
-633.338873	4.881049	6.625434
-631.728942	5.866056	6.635430
-629.547544	6.711898	6.645427
-627.990671	7.672418	6.655424
-626.171808	9.590636	6.665421
-623.971640	4.460805	6.675418
-622.422326	2.582625	6.685414
-620.327493	8.630890	6.695411
-618.195711	5.361602	6.705408
-616.478486	10.384668	6.715405
-614.645657	11.132246	6.725402
-612.883483	8.783994	6.735398
-610.888308	6.329761	6.745395
-609.080762	8.431727	6.755392
-607.339000	12.829313	6.765389
-605.306118	5.720513	6.775386
-603.409574	4.332498	6.785382
-601.381354	5.957124	6.795379
-599.551318	7.675831	6.805376
-597.845941	8.584005	6.815373
-595.884102	6.127990	6.825370
-594.112086	0.346820	6.835366
-592.060181	7.139141	6.845363
-590.474953	10.065737	6.855360
-588.355140	6.343625	6.865357
-586.545489	7.542573	6.875354
-584.645025	9.802105	6.885350
-582.610015	8.831792	6.895347
-581.162633	10.252965	6.905344
-579.161905	7.944021	6.915341
-576.820561	3.866548	6.925338
-574.933640	3.175771	6.935334
-573.641471	12.432197	6.945331
-571.660499	8.248594	6.955328
-569.744711	15.657502	6.965325
-567.877029	8.779805	6.975322
-565.643378	9.346784	6.985318
-563.977674	9.555929	6.995315
-562.270448	16.200716	7.005312
-560.246429	6.100108	7.015309
-558.145865	6.886347	7.025306
-556.539547	9.014959	7.035302
-554.679782	6.048470	7.045299
-552.604882	6.530454	7.055296
-550.779082	12.601601	7.065293
-549.127607	9.036535	7.075290
-546.947447	12.116772	7.085286
-545.243103	12.210611	7.095283
-543.482208	9.075735	7.105280
-541.807441	5.473083	7.115277
-539.556339	7.922247	7.125274
-537.675010	9.951908	7.135270
-536.101964	7.516385	7.145267
-534.174118	7.498371	7.155264
-532.066563	8.094116	7.165261
-530.029774	-0.035369	7.175258
-528.032183	2.058528	7.185254
-526.512514	3.948290	7.195251
-524.541352	8.444086	7.205248
-522.995052	8.695470	7.215245
-520.686661	11.321752	7.225242
-519.040978	6.117555	7.235238
-517.078189	5.539859	7.245235
-515.327313	3.974919	7.255232
-513.271319	6.039437	7.265229
-511.460259	-2.930264	7.275226
-509.867091	0.309588	7.285222
-507.752456	6.618518	7.295219
-505.480175	5.475530	7.305216
-503.864330	0.647960	7.315213
-502.170634	6.673816	7.325210
-500.415309	-2.036545	7.335206
-497.983576	4.010893	7.345203
-496.456997	7.668851	7.355200
-494.628891	6.383523	7.365197
-492.658626	10.890556	7.375194
-490.773689	7.612297	7.385190
-489.155581	3.085495	7.395187
-487.386582	9.019792	7.405184
-485.002601	4.607416	7.415181
-483.124575	4.260458	7.425178
-481.350423	-1.991343	7.435174
-479.518046	2.646058	7.445171
-477.851065	1.900180	7.455168
-475.696866	6.728590	7.465165
-473.681954	5.613965	7.475162
-472.138924	6.097917	7.485158
-470.194832	6.553771	7.495155
-468.199119	14.172314	7.505152
-466.700969	11.133130	7.515149
-464.651421	10.125598	7.525146
-462.663060	6.288955	7.535142
-460.779847	11.567377	7.545139
-458.777906	10.878653	7.555136
-457.219824	11.778955	7.565133
-455.203288	8.859514	7.575130
-453.103609	8.507346	7.585126
-451.354779	1.145000	7.595123
-449.724615	8.335012	7.605120
-447.599654	1.110489	7.615117
-445.812959	4.553504	7.625114
-443.808431	8.847196	7.635110
-442.089852	7.504006	7.645107
-440.245684	13.148387	7.655104
-438.388383	3.721018	7.665101
-436.272301	4.731111	7.675098
-434.827839	-1.890946	7.685094
-432.469828	2.524696	7.695091
-430.739256	7.482320	7.705088
-429.043515	7.375725	7.715085
-426.983602	3.827975	7.725082
-424.786540	-0.624233	7.735078
-423.107856	0.583814	7.745075
-421.794494	3.492298	7.755072
-419.525976	4.379026	7.765069
-417.432495	2.582641	7.775066
-415.736047	-0.309931	7.785062
-413.891059	5.171095	7.795059
-412.130349	2.486053	7.805056
-410.141984	1.183147	7.815053
-408.181942	3.499328	7.825050
-406.466704	-0.543769	7.835046
-404.689464	1.900995	7.845043
-402.380047	5.761023	7.855040
-400.776297	10.527002	7.865037
-398.667161	5.509713	7.875034
-396.971765	8.015158	7.885030
-395.302652	3.360280	7.895027
-393.350202	8.807865	7.905024
-391.501253	9.619959	7.915021
-389.281278	2.491399	7.925018
-387.533236	5.958065	7.935014
-385.688804	5.077445	7.945011
-383.577141	7.710280	7.955008
-382.139069	6.655916	7.965005
-380.280332	8.814805	7.975002
-378.482358	10.325692	7.984998
-376.275315	6.738892	7.994995
-374.236176	3.983970	8.004992
-372.610737	8.276330	8.014989
-370.755173	8.685760	8.024986
-368.776212	4.780024	8.034982
-367.041364	6.812755	8.044979
-365.050225	4.352601	8.054976
-363.192967	9.996353	8.064973
-361.480417	6.881297	8.074970
-359.462369	3.729252	8.084966
-357.520737	6.048616	8.094963
-355.590691	0.047554	8.104960
-354.098556	3.482250	8.114957
-352.142642	10.802971	8.124954
-350.049935	6.012212	8.134950
-348.092173	7.405594	8.144947
-346.490955	11.994579	8.154944
-344.549774	12.343489	8.164941
-342.389782	7.787805	8.174938
-340.619595	5.630750	8.184934
-338.731587	9.875714	8.194931
-337.064980	5.094026	8.204928
-335.063382	9.073684	8.214925
-333.185587	2.657527	8.224922
-331.234389	4.376117	8.234918
-329.423170	6.765289	8.244915
-327.794471	11.253135	8.254912
-325.783367	16.991454	8.264909
-323.925710	4.773846	8.274906
-321.992921	3.516079	8.284902
-319.816414	3.485937	8.294899
-318.248867	3.832946	8.304896
-316.326904	3.400270	8.314893
-314.459365	2.599105	8.324890
-312.445399	9.042393	8.334886
-310.845466	8.412809	8.344883
-308.832300	8.135225	8.354880
-307.001926	13.220435	8.364877
-305.004455	7.997067	8.374874
-302.991975	8.223896	8.384870
-301.012956	2.554337	8.394867
-299.334611	11.585361	8.404864
-297.947173	8.987702	8.414861
-295.786363	6.972731	8.424858
-293.364281	10.374414	8.434854
-291.899973	10.409927	8.444851
-290.014759	13.315222	8.454848
-287.996686	16.857739	8.464845
-286.278991	3.262323	8.474842
-284.492858	0.552812	8.484838
-282.577401	8.959441	8.494835
-280.643482	9.586275	8.504832
-278.756798	5.974634	8.514829
-276.971578	10.209196	8.524826
-275.042047	3.181089	8.534822
-273.156746	8.160460	8.544819
-271.448130	13.188318	8.554816
-269.605534	12.529379	8.564813
-267.661882	6.313783	8.574810
-265.686908	5.478798	8.584807
-263.677303	5.009375	8.594803
-261.873527	5.692922	8.604800
-259.980546	10.778877	8.614797
-258.191548	3.508899	8.624794
-256.234788	7.714444	8.634791
-254.389049	11.186149	8.644787
-252.595362	-0.858820	8.654784
-250.570080	9.720058	8.664781
-248.765241	2.603081	8.674778
-246.797216	3.988029	8.684775
-244.520199	0.363995	8.694771
-243.142230	0.952219	8.704768
-241.405404	-0.295222	8.714765
-239.181074	2.082417	8.724762
-237.365471	-4.836420	8.734759
-235.281152	-4.532564	8.744755
-234.057743	-1.386481	8.754752
-231.788582	-3.091582	8.764749
-230.032067	-1.026152	8.774746
-227.872988	-5.346079	8.784743
-226.539687	-0.893688	8.794739
-224.477736	0.053863	8.804736
-222.395855	-0.349685	8.814733
-220.681108	2.088486	8.824730
-218.659024	1.446605	8.834727
-216.916801	3.124811	8.844723
-215.566071	0.507783	8.854720
-213.004216	0.987431	8.864717
-211.399929	-1.773466	8.874714
-209.343759	-0.591741	8.884711
-207.704413	8.085973	8.894707
-205.480485	4.701866	8.904704
-203.601112	7.031978	8.914701
-201.979663	8.494961	8.924698
-199.754224	9.336232	8.934695
-198.164244	5.872334	8.944691
-196.200893	7.225699	8.954688
-194.398875	-0.985124	8.964685
-192.412760	3.401167	8.974682
-190.877953	7.117508	8.984679
-188.678240	5.056393	8.994675
-186.865942	5.243305	9.004672
-185.050024	4.295331	9.014669
-182.997420	5.920717	9.024666
-181.016829	4.791950	9.034663
-179.062601	4.579071	9.044659
-177.345659	3.714470	9.054656
-175.568512	2.430498	9.064653
-173.994831	3.670482	9.074650
-171.677077	3.522126	9.084647
-170.012378	-1.005451	9.094643
-168.260019	-2.560239	9.104640
-166.091231	2.012500	9.114637
-164.131864	4.199676	9.124634
-162.611387	-3.125394	9.134631
-160.623830	1.720299	9.144627
-158.863023	4.483763	9.154624
-156.987618	-1.122127	9.164621
-155.090750	0.171124	9.174618
-153.137179	-8.361294	9.184615
-151.153987	-4.259038	9.194611
-149.299445	-1.022766	9.204608
-147.276514	4.103795	9.214605
-145.677826	8.204018	9.224602
-143.650639	5.186054	9.234599
-141.757480	4.958370	9.244595
-140.228501	2.507216	9.254592
-137.824693	11.664475	9.264589
-136.007740	10.261845	9.274586
-134.601262	3.738459	9.284583
-132.657332	12.250550	9.294579
-130.282338	7.257735	9.304576
-128.592501	11.374743	9.314573
-126.987768	10.745585	9.324570
-125.271314	6.130892	9.334567
-122.877198	10.596644	9.344563
-121.192632	9.199333	9.354560
-119.297927	11.011098	9.364557
-117.499450	13.720300	9.374554
-115.323295	11.315865	9.384551
-113.590512	13.528087	9.394547
-111.627638	9.237110	9.404544
-109.729995	13.645334	9.414541
-108.136753	6.512517	9.424538
-106.574956	7.325360	9.434535
-104.277158	7.892639	9.444531
-102.507546	6.528968	9.454528
-100.718654	4.167629	9.464525
-98.608277	11.896731	9.474522
-96.347015	5.838569	9.484519
-94.827272	7.427321	9.494515
-93.358816	9.218918	9.504512
-91.192978	8.656385	9.514509
-88.798402	9.465942	9.524506
-87.478605	6.883894	9.534503
-85.615758	9.640563	9.544499
-84.064242	9.844569	9.554496
-81.975897	7.058015	9.564493
-80.038468	4.226992	9.574490
-77.862447	8.675233	9.584487
-76.142850	12.862251	9.594483
-74.194422	8.844488	9.604480
-72.207330	3.306422	9.614477
-70.622939	3.384651	9.624474
-68.686226	0.391322	9.634471
-66.712553	7.272431	9.644467
-64.706103	4.575413	9.654464
-63.141043	4.731655	9.664461
-61.149652	11.938549	9.674458
-59.156093	6.603310	9.684455
-57.325792	6.593927	9.694451
-55.565057	9.162606	9.704448
-53.640780	12.132844	9.714445
-51.730370	3.944578	9.724442
-50.110085	6.962198	9.734439
-48.145345	10.560611	9.744435
-45.958760	5.066205	9.754432
-44.518646	3.656298	9.764429
-42.212640	5.228814	9.774426
-40.495912	6.297694	9.784423
-38.779945	5.340436	9.794419
-36.733378	8.689669	9.804416
-34.740743	12.876524	9.814413
-32.802962	10.001984	9.824410
-31.126298	7.983991	9.834407
-29.194621	6.888574	9.844403
-27.448570	-0.701204	9.854400
-25.908652	0.250187	9.864397
-23.725598	3.420309	9.874394
-21.555244	4.403511	9.884391
-19.340049	6.071444	9.894387
-18.009605	13.006749	9.904384
-16.463251	7.861235	9.914381
-14.398538	9.762066	9.924378
-12.003706	7.648211	9.934375
-10.430145	8.154755	9.944371
-8.595713	13.573760	9.954368
-6.687544	18.674623	9.964365
-4.986167	9.888680	9.974362
-3.695923	25.177844	9.984359
-2.308809	65.345904	9.994355
-1.016841	103.376050	10.004352
0.000000	150.440832	10.009357
0.570356	180.021866	10.014362
1.520587	210.879066	10.019367
1.596126	235.523084	10.024371
2.443302	257.514968	10.029376
2.764218	266.984725	10.034381
2.972632	290.696226	10.039386
3.261208	298.268615	10.044391
2.874914	300.641057	10.049395
3.074073	307.483555	10.054400
3.420128	317.600317	10.059405
3.526737	329.582529	10.064410
3.862484	329.068937	10.069415
3.675191	336.753329	10.074419
3.901032	326.860338	10.079424
3.895171	325.825871	10.084429
3.800413	337.038178	10.089434
3.857504	321.610566	10.094439
3.830484	341.910308	10.099443
4.090177	351.632182	10.104448
4.268328	355.896842	10.109453
3.910028	343.379250	10.114458
4.242694	341.612560	10.119463
4.030588	348.638085	10.124467
4.180737	346.671383	10.129472
4.320547	349.645175	10.134477
4.397603	361.749315	10.139482
4.640010	355.568167	10.144487
4.279264	347.396058	10.149491
4.102307	336.698609	10.154496
4.334890	351.483450	10.159501
4.318846	363.316199	10.164506
4.584737	362.367761	10.169511
4.431514	376.371707	10.174515
4.501273	366.079944	10.179520
4.913030	379.250872	10.184525
4.801424	377.414699	10.189530
4.849370	375.685376	10.194535
4.536381	380.143984	10.199539
4.559414	383.348585	10.204544
4.492612	378.292503	10.209549
4.152255	387.565859	10.214554
4.683888	377.244632	10.219559
4.646616	399.153108	10.224563
5.312662	408.940735	10.229568
5.257747	409.241329	10.234573
5.343168	411.233315	10.239578
5.145813	417.354406	10.244583
5.022925	424.611369	10.249587
5.356420	417.109632	10.254592
5.479657	424.388339	10.259597
5.427569	430.329798	10.264602
5.763382	419.479246	10.269607
5.526403	419.210291	10.274611
5.127694	411.254253	10.279616
5.574674	418.276143	10.284621
5.305503	426.930237	10.289626
5.781304	427.899278	10.294631
5.181143	431.141664	10.299635
5.315365	435.862281	10.304640
5.394831	427.988847	10.309645
5.482764	433.538420	10.314650
5.735598	431.727383	10.319655
5.370038	454.854679	10.324659
5.734320	455.769425	10.329664
5.869189	459.670102	10.334669
5.703065	471.769840	10.339674
6.129841	462.349528	10.344679
6.028511	475.675218	10.349683
5.909319	467.565836	10.354688
6.135125	471.815647	10.359693
5.921476	475.892527	10.364698
6.126422	471.093362	10.369703
6.253143	482.696863	10.374707
6.346366	480.231897	10.379712
6.259554	485.165289	10.384717
6.297651	500.118217	10.389722
6.614072	500.724999	10.394727
6.260266	514.683331	10.399731
6.791943	513.428403	10.404736
6.811469	522.746709	10.409741
6.778770	517.076861	10.414746
6.937910	518.298353	10.419751
6.795534	512.342585	10.424755
6.751637	504.271983	10.429760
6.885813	511.143870	10.434765
7.080340	516.690195	10.439770
6.913837	499.913293	10.444775
6.610901	517.786054	10.449779
7.073897	514.153248	10.454784
7.514137	520.831747	10.459789
6.822234	525.894555	10.464794
7.090773	525.262617	10.469799
7.111386	529.893009	10.474803
7.067463	522.502510	10.479808
7.385832	529.123753	10.484813
6.996457	528.305813	10.489818
7.519702	532.306097	10.494823
6.847572	538.301803	10.499827
6.988560	536.453486	10.504832
7.422639	536.941811	10.509837
7.245343	541.797974	10.514842
7.504122	550.992384	10.519847
7.598667	565.092171	10.524851
7.857186	559.955384	10.529856
8.078598	562.223274	10.534861
7.807421	565.906238	10.539866
8.041558	539.931024	10.544871
7.617137	545.792291	10.549875
7.855265	556.825711	10.554880
8.013947	565.463364	10.559885
7.723769	571.207284	10.564890
8.320677	565.400258	10.569895
8.226797	569.037035	10.574899
8.102306	568.153151	10.579904
8.163023	576.526168	10.584909
8.024451	574.889589	10.589914
8.473900	566.818049	10.594919
7.912221	575.924601	10.599923
7.952406	582.113973	10.604928
8.190651	579.044671	10.609933
8.159639	575.781542	10.614938
8.306060	575.626053	10.619943
8.093330	583.590050	10.624947
8.514085	583.620807	10.629952
8.491084	593.510114	10.634957
8.803098	612.004235	10.639962
9.262309	603.871794	10.644967
9.027212	593.061772	10.649971
8.882700	584.736809	10.654976
8.871395	588.108387	10.659981
8.626658	588.224431	10.664986
9.017244	581.306888	10.669991
8.715285	587.130201	10.674995
8.707813	588.375528	10.680000
8.474820	603.510031	10.685005
8.766937	620.938659	10.690010
9.052954	627.282472	10.695015
8.798265	629.030440	10.700019
8.814529	627.766772	10.705024
8.970199	625.603304	10.710029
9.027381	632.770675	10.715034
8.957907	632.079454	10.720039
9.027444	653.179733	10.725043
8.916778	646.393893	10.730048
9.019326	654.772016	10.735053
9.214257	662.911283	10.740058
10.205888	662.011287	10.745063
9.719966	661.968952	10.750067
9.343156	663.392871	10.755072
9.648186	671.823127	10.760077
9.810380	664.579190	10.765082
9.968645	659.926521	10.770087
9.471639	653.789139	10.775091
9.440489	660.658650	10.780096
9.798967	677.743603	10.785101
9.766155	695.774327	10.790106
10.228547	690.990165	10.795111
9.987072	699.604134	10.800115
9.913645	699.460680	10.805120
9.896133	693.029892	10.810125
9.877631	695.300253	10.815130
10.111770	689.493804	10.820135
9.852447	697.781235	10.825139
10.223680	693.139804	10.830144
10.576494	693.519307	10.835149
10.182417	697.093508	10.840154
10.519804	688.032590	10.845159
10.010907	703.591460	10.850163
10.446043	711.612991	10.855168
10.607985	717.076161	10.860173
10.588002	720.311891	10.865178
11.199922	721.067355	10.870183
11.064017	728.031828	10.875187
10.774219	701.656320	10.880192
10.756521	701.909486	10.885197
10.451374	705.514624	10.890202
11.066011	706.155151	10.895207
10.767716	720.347301	10.900211
10.950576	724.529941	10.905216
10.745920	719.774877	10.910221
10.875473	718.130601	10.915226
11.181806	718.188477	10.920231
10.972780	728.216736	10.925235
11.007249	723.378830	10.930240
11.156913	722.475168	10.935245
10.864750	721.293188	10.940250
10.959849	714.708481	10.945255
10.814149	735.072502	10.950259
11.160054	750.884718	10.955264
11.326341	763.691489	10.960269
11.287643	760.707529	10.965274
11.348348	758.535458	10.970279
11.446201	771.308574	10.975283
11.666106	760.980940	10.980288
12.010658	768.920139	10.985293
11.416919	771.361374	10.990298
11.884331	765.860684	10.995303
11.627709	762.528832	11.000307
11.899287	765.466296	11.005312
11.974830	770.745355	11.010317
11.530462	770.479188	11.015322
11.941628	767.605987	11.020327
11.679925	769.891610	11.025331
12.216948	793.375828	11.030336
12.456316	788.935395	11.035341
11.946175	790.202978	11.040346
12.106560	779.779749	11.045351
12.224169	788.710746	11.050355
12.081465	791.088862	11.055360
12.558323	796.729773	11.060365
12.264304	797.714385	11.065370
12.438732	793.067589	11.070375
12.592655	793.396724	11.075379
12.688945	801.015749	11.080384
12.455170	796.518676	11.085389
12.340227	807.573732	11.090394
12.848154	797.835759	11.095399
12.490219	806.986062	11.100403
12.661186	800.858829	11.105408
12.393759	798.048682	11.110413
12.511737	810.423255	11.115418
12.487703	802.827506	11.120423
12.340740	811.497173	11.125427
12.563218	832.168057	11.130432
12.733057	835.274950	11.135437
12.816204	834.635709	11.140442
13.208020	839.475307	11.145447
13.011100	829.237647	11.150451
13.316440	832.406174	11.155456
13.334091	834.323388	11.160461
13.133770	839.001225	11.165466
13.328469	828.612343	11.170471
13.111578	844.470228	11.175475
13.293309	839.003099	11.180480
13.114803	836.079411	11.185485
13.231908	840.493222	11.190490
13.586042	842.082750	11.195495
13.268029	843.725942	11.200499
13.846259	851.843405	11.205504
13.796968	843.460530	11.210509
13.772805	847.745014	11.215514
14.245794	842.447812	11.220519
13.854229	848.606316	11.225523
13.984040	846.574356	11.230528
13.793997	846.563788	11.235533
13.469326	855.091451	11.240538
13.743348	844.887112	11.245543
14.003578	858.301924	11.250547
14.298360	854.260520	11.255552
13.978197	851.475983	11.260557
13.854815	861.551616	11.265562
14.177981	870.046764	11.270567
14.331126	872.198907	11.275571
14.528636	876.119738	11.280576
14.872539	867.925221	11.285581
14.336969	854.727092	11.290586
14.455307	845.428118	11.295591
14.394611	846.641540	11.300595
14.338994	842.239827	11.305600
14.542854	850.305821	11.310605
14.193337	860.462856	11.315610
14.753596	861.399685	11.320615
14.707807	872.679769	11.325619
14.727461	875.724000	11.330624
15.187130	876.687154	11.335629
15.203803	868.079801	11.340634
14.988745	851.545315	11.345639
14.754192	844.220505	11.350643
14.731867	843.318693	11.355648
14.593083	845.997325	11.360653
14.538746	856.462164	11.365658
14.948447	864.624319	11.370663
14.769963	877.511611	11.375667
14.779944	878.083320	11.380672
14.791391	870.832371	11.385677
14.376034	877.661668	11.390682
15.060443	884.017017	11.395687
15.179361	909.536495	11.400691
15.538735	900.313003	11.405696
15.791793	901.227900	11.410701
15.353773	911.336985	11.415706
15.542446	897.276495	11.420711
15.576171	912.774904	11.425715
15.473826	909.862617	11.430720
15.232076	904.156234	11.435725
15.244544	909.765099	11.440730
15.423404	907.851036	11.445735
15.465885	910.243603	11.450739
15.593051	913.501116	11.455744
15.990891	906.502847	11.460749
15.696535	916.954405	11.465754
15.658673	929.989734	11.470759
15.924061	941.036122	11.475763
16.168424	940.560681	11.480768
16.037241	936.522421	11.485773
16.126646	942.891390	11.490778
16.230490	936.827323	11.495783
16.079178	935.273811	11.500787
15.958080	940.285461	11.505792
16.373854	933.488576	11.510797
16.030822	938.775907	11.515802
16.475802	926.624587	11.520807
16.392923	927.031036	11.525811
16.617001	938.242793	11.530816
16.509017	925.785233	11.535821
16.626113	934.698639	11.540826
16.536552	929.862988	11.545831
16.340496	937.677860	11.550835
16.740232	937.574856	11.555840
16.757398	936.064299	11.560845
16.509727	938.366883	11.565850
16.496159	935.402660	11.570855
16.174066	940.497323	11.575859
16.270535	954.890025	11.580864
16.930801	961.343098	11.585869
16.987996	967.054051	11.590874
17.056745	966.622930	11.595879
16.926569	973.863239	11.600883
17.073411	978.844751	11.605888
17.313145	973.379867	11.610893
17.170961	971.762418	11.615898
17.626546	967.076840	11.620903
17.265658	968.361872	11.625907
17.207258	970.735429	11.630912
17.208071	974.315406	11.635917
17.157044	977.522959	11.640922
17.436909	974.002763	11.645927
17.586333	978.434757	11.650931
17.524677	977.258629	11.655936
17.240757	973.974833	11.660941
17.294157	981.913929	11.665946
17.679241	992.488649	11.670951
17.798928	1003.239143	11.675955
17.938320	1000.301576	11.680960
17.928047	999.868213	11.685965
17.740211	1003.070412	11.690970
17.784743	995.472287	11.695975
18.016564	1006.160925	11.700979
18.213106	1003.552242	11.705984
18.219048	996.797967	11.710989
17.964331	1006.410292	11.715994
18.316452	1000.982577	11.720999
18.252637	1002.436150	11.726003
18.555778	1003.669307	11.731008
18.387777	998.266823	11.736013
17.843262	987.559709	11.741018
18.088682	992.530640	11.746023
18.111191	1004.213976	11.751027
18.415721	1003.183483	11.756032
18.527025	1008.388597	11.761037
18.395179	1000.549132	11.766042
18.438034	1006.056901	11.771047
18.505847	1008.166456	11.776051
18.540342	1013.695793	11.781056
18.742543	1010.678377	11.786061
18.687278	1015.985868	11.791066
18.464756	1008.031288	11.796071
18.475180	1009.373844	11.801075
18.371498	1013.926217	11.806080
18.890092	1036.394360	11.811085
18.657428	1044.606746	11.816090
19.445672	1036.930825	11.821095
19.493295	1038.256348	11.826099
19.292974	1030.438871	11.831104
19.160432	1013.248225	11.836109
18.993306	1015.482536	11.841114
19.206583	1015.211765	11.846119
19.178768	1032.233472	11.851123
19.007623	1035.754920	11.856128
19.213961	1038.314412	11.861133
19.297286	1039.171183	11.866138
19.191304	1035.203182	11.871143
19.442858	1041.927679	11.876147
19.158742	1040.215742	11.881152
19.483944	1043.242750	11.886157
19.496741	1045.311612	11.891162
19.737096	1037.950286	11.896167
19.556514	1040.083092	11.901171
19.879975	1046.387500	11.906176
19.816122	1044.378061	11.911181
19.664837	1049.662553	11.916186
19.801106	1046.016172	11.921191
19.932339	1047.919465	11.926195
19.749156	1044.068119	11.931200
20.045706	1060.094375	11.936205
20.001202	1072.948199	11.941210
20.333518	1069.360174	11.946215
20.296791	1073.791742	11.951219
20.253875	1063.908838	11.956224
20.271966	1042.269702	11.961229
20.424627	1044.202478	11.966234
20.264317	1043.951549	11.971239
20.264979	1055.922880	11.976243
20.284544	1063.743872	11.981248
20.540670	1060.823385	11.986253
20.501183	1064.313582	11.991258
20.682882	1064.029672	11.996263
20.803821	1072.087498	12.001267
20.379660	1066.781014	12.006272
20.471704	1062.111159	12.011277
20.331681	1063.137278	12.016282
20.511982	1062.728870	12.021287
20.271572	1079.793000	12.026291
20.610563	1076.497118	12.031296
20.698385	1064.619297	12.036301
20.555402	1072.530926	12.041306
20.682757	1064.943435	12.046311
20.824267	1068.084837	12.051315
20.810138	1058.606343	12.056320
21.175206	1060.142310	12.061325
20.972630	1061.340600	12.066330
21.124750	1047.767031	12.071335
20.901652	1032.036230	12.076339
20.909256	1026.125997	12.081344
20.960581	1021.202610	12.086349
20.731067	1029.281422	12.091354
21.049773	1021.344960	12.096359
20.886401	1024.131654	12.101363
20.974872	1018.313348	12.106368
20.932773	1021.758984	12.111373
21.052810	1018.538154	12.116378
21.169427	1004.170580	12.121383
20.629038	1003.685608	12.126387
20.697144	995.266733	12.131392
21.146730	993.283743	12.136397
20.916345	1002.360581	12.141402
21.024047	996.217277	12.146407
20.990114	992.253512	12.151411
20.657433	994.329101	12.156416
20.613817	989.508448	12.161421
20.715410	999.025731	12.166426
20.985109	992.827812	12.171431
20.990054	993.506967	12.176435
20.594044	976.441664	12.181440
20.520668	966.609833	12.186445
20.719459	965.559578	12.191450
20.359779	963.721658	12.196455
20.526246	975.150555	12.201459
20.757784	984.993706	12.206464
20.825644	984.151029	12.211469
20.735151	998.812668	12.216474
20.993161	992.557937	12.221479
20.612295	979.438570	12.226483
20.263848	971.947702	12.231488
20.626264	973.977532	12.236493
20.707049	997.733704	12.241498
20.936660	991.126212	12.246503
20.781998	979.275819	12.251507
20.584853	978.488052	12.256512
20.669095	971.554573	12.261517
20.518056	971.982973	12.266522
20.828452	971.514763	12.271527
20.760896	972.392662	12.276531
20.485341	970.031900	12.281536
20.770732	968.551536	12.286541
20.486949	970.975183	12.291546
20.603169	973.694983	12.296551
20.926728	970.411638	12.301555
20.726778	968.111729	12.306560
20.792298	976.096903	12.311565
20.653841	980.352861	12.316570
20.613536	973.237053	12.321575
20.240374	973.418538	12.326579
20.389252	977.242339	12.331584
20.597435	977.649412	12.336589
20.599132	986.931580	12.341594
20.580280	992.453082	12.346599
20.823077	994.680265	12.351603
20.714304	994.620236	12.356608
20.946725	986.156615	12.361613
20.536265	988.423564	12.366618
21.000878	984.161168	12.371623
20.711883	982.954544	12.376627
20.694707	982.894206	12.381632
20.937910	971.060472	12.386637
20.813309	972.251308	12.391642
20.916004	979.456825	12.396647
20.922442	979.155597	12.401651
20.723583	978.083914	12.406656
20.728289	975.764310	12.411661
20.723922	980.307934	12.416666
20.809020	979.600459	12.421671
20.922080	988.070906	12.426675
20.628122	981.737922	12.431680
20.794752	971.150469	12.436685
20.584161	984.972955	12.441690
20.719881	981.999706	12.446695
20.578632	981.041302	12.451699
20.641459	995.989282	12.456704
21.128350	983.904943	12.461709
20.421022	974.634561	12.466714
20.565273	974.103653	12.471719
20.875080	973.406203	12.476723
20.804989	972.523626	12.481728
20.840885	952.400894	12.486733
20.703570	958.446376	12.491738
20.777864	950.256989	12.496743
20.539989	950.034360	12.501747
20.432458	957.055254	12.506752
20.826372	941.936382	12.511757
20.434428	955.208493	12.516762
20.712262	961.815951	12.521767
20.779277	953.290707	12.526771
20.565856	962.115931	12.531776
20.731009	947.843507	12.536781
20.665734	956.151093	12.541786
20.733099	946.454223	12.546791
20.573079	947.683892	12.551795
20.659009	953.559650	12.556800
20.709642	957.368712	12.561805
20.865856	958.241402	12.566810
20.929377	951.487141	12.571815
21.006739	958.018839	12.576819
20.457350	956.925152	12.581824
20.671385	948.305231	12.586829
20.624947	956.565773	12.591834
20.661130	962.579141	12.596839
20.613356	961.497739	12.601843
20.681210	963.866622	12.606848
20.962664	949.622809	12.611853
20.642680	962.235224	12.616858
20.786731	953.362433	12.621863
20.905860	956.158310	12.626867
20.497337	963.815019	12.631872
20.496982	957.637363	12.636877
20.712011	969.442795	12.641882
21.028495	959.269786	12.646887
20.733768	966.588435	12.651891
20.771117	967.635058	12.656896
20.617626	957.210657	12.661901
20.577178	969.521731	12.666906
20.598461	968.497962	12.671911
20.688157	965.305634	12.676915
20.717230	963.203695	12.681920
20.795545	962.528172	12.686925
20.764216	967.584439	12.691930
21.029561	954.698902	12.696935
20.636763	938.848081	12.701939
20.620163	936.155954	12.706944
20.604809	926.771697	12.711949
20.393636	941.796997	12.716954
20.911296	950.644499	12.721959
20.883522	937.828573	12.726963
20.555586	933.674838	12.731968
20.696032	925.301229	12.736973
20.446994	937.990276	12.741978
20.724918	943.821269	12.746983
20.751229	937.260499	12.751987
20.390067	935.426784	12.756992
20.819235	944.849581	12.761997
20.485008	939.023252	12.767002
20.757807	949.097331	12.772007
20.756042	933.211446	12.777011
20.469494	938.223041	12.782016
20.869582	942.404023	12.787021
20.986243	945.736764	12.792026
20.980171	929.974383	12.797031
20.837947	931.932837	12.802035
20.975786	934.074192	12.807040
21.237794	924.802248	12.812045
20.793291	933.188263	12.817050
20.925860	932.588307	12.822055
20.748384	932.734267	12.827059
20.588972	941.846664	12.832064
20.775492	930.255573	12.837069
20.328251	935.588005	12.842074
20.325625	942.457092	12.847079
20.577523	925.931280	12.852083
20.110033	936.973847	12.857088
20.391015	935.608714	12.862093
20.242234	934.057531	12.867098
20.338680	933.444032	12.872103
20.534222	933.474327	12.877107
20.470170	938.008041	12.882112
20.495023	945.662280	12.887117
20.415142	964.734405	12.892122
20.860796	971.749670	12.897127
21.212008	964.344503	12.902131
20.915364	955.197929	12.907136
20.865594	952.178331	12.912141
20.887445	948.373170	12.917146
20.613258	938.978020	12.922151
20.771144	940.196999	12.927155
20.568489	941.675555	12.932160
20.643434	935.542233	12.937165
20.341514	947.836147	12.942170
20.508563	944.457273	12.947175
20.381147	948.151993	12.952179
20.189537	947.622618	12.957184
20.643770	955.404557	12.962189
20.573712	969.518327	12.967194
20.531980	974.169014	12.972199
20.829238	975.358968	12.977203
20.497702	978.900798	12.982208
20.760465	978.889962	12.987213
20.693487	977.612511	12.992218
20.813287	977.950264	12.997223
20.663580	978.121068	13.002227
20.622634	969.896562	13.007232
21.148389	967.439466	13.012237
20.587709	961.041300	13.017242
20.582347	954.127139	13.022247
20.474824	946.409056	13.027251
20.536825	946.600404	13.032256
20.451354	942.608383	13.037261
20.542681	964.638105	13.042266
20.599726	974.419983	13.047271
20.546958	983.786882	13.052275
20.639144	984.024370	13.057280
20.864284	974.748060	13.062285
20.543357	982.224761	13.067290
20.515415	976.706692	13.072295
20.604297	979.069209	13.077299
20.806219	980.159062	13.082304
20.920565	977.877501	13.087309
20.856462	984.088071	13.092314
20.768995	964.071343	13.097319
20.601382	955.835798	13.102323
20.411067	951.262939	13.107328
20.525004	956.483769	13.112333
20.846461	970.790544	13.117338
20.853012	968.877201	13.122343
20.943097	952.449762	13.127347
20.720092	948.903291	13.132352
20.973437	943.153849	13.137357
20.603496	946.777256	13.142362
20.703566	956.040565	13.147367
20.474805	944.888556	13.152371
20.510608	957.081153	13.157376
20.573485	946.822161	13.162381
20.441980	951.588890	13.167386
20.705879	949.216166	13.172391
20.418734	954.971548	13.177395
20.427468	946.549063	13.182400
20.746053	957.684631	13.187405
20.616067	964.152803	13.192410
20.772737	956.169946	13.197415
20.987006	951.198907	13.202419
20.474415	956.297816	13.207424
20.828500	946.300341	13.212429
20.743484	954.905388	13.217434
20.757959	957.152765	13.222439
20.681645	949.050385	13.227443
20.606023	952.705041	13.232448
20.635267	940.900909	13.237453
20.695080	952.730968	13.242458
20.538398	959.948973	13.247463
20.843464	945.626510	13.252467
20.707387	950.757968	13.257472
21.107158	948.856155	13.262477
21.027585	951.134656	13.267482
20.996291	947.012952	13.272487
21.061110	952.379963	13.277491
21.159179	945.786360	13.282496
20.857154	928.304736	13.287501
20.231342	933.350813	13.292506
20.119683	933.501673	13.297511
20.403155	940.689993	13.302515
20.694226	954.775780	13.307520
20.627336	950.962544	13.312525
20.518151	955.207161	13.317530
20.656606	955.454479	13.322535
20.688571	948.970892	13.327539
20.232485	958.099427	13.332544
20.681903	947.885870	13.337549
20.361024	955.449786	13.342554
19.933908	960.224965	13.347559
20.228470	961.015909	13.352563
20.282777	972.224036	13.357568
20.569016	978.102958	13.362573
20.861980	985.638222	13.367578
20.773072	992.136073	13.372583
21.186605	988.432694	13.377587
20.720270	978.351652	13.382592
20.859031	962.287303	13.387597
20.588508	963.667761	13.392602
20.743288	962.069660	13.397607
20.720801	957.250921	13.402611
20.380169	962.730084	13.407616
20.477370	953.768220	13.412621
20.644870	962.512344	13.417626
20.381459	959.038719	13.422631
20.671700	964.457085	13.427635
20.591869	966.806290	13.432640
20.623074	955.711938	13.437645
20.710654	972.373534	13.442650
20.635751	972.537039	13.447655
21.005182	972.105286	13.452659
20.604108	978.239024	13.457664
20.813201	960.299075	13.462669
20.763372	958.970527	13.467674
20.804016	955.985163	13.472679
20.798732	959.517631	13.477683
20.850896	957.324891	13.482688
20.761743	957.790837	13.487693
20.925252	961.856861	13.492698
20.472886	963.747310	13.497703
20.664317	961.203458	13.502707
20.759886	969.602289	13.507712
20.733966	959.900088	13.512717
20.823319	961.549632	13.517722
20.866525	968.929553	13.522727
20.609821	963.138081	13.527731
20.770407	962.668714	13.532736
21.785449	952.176993	13.537741
21.137352	943.441208	13.542746
20.610197	938.430319	13.547751
20.864768	927.301243	13.552755
20.629676	936.147141	13.557760
20.675320	927.506761	13.562765
20.654353	925.826692	13.567770
20.576426	916.487116	13.572775
20.661916	919.988221	13.577779
20.470483	928.794261	13.582784
20.749591	928.830755	13.587789
20.475069	932.107011	13.592794
20.719849	932.930963	13.597799
20.797500	920.616840	13.602803
20.572690	932.771207	13.607808
20.787430	931.409142	13.612813
20.474187	930.764834	13.617818
20.624530	923.244522	13.622823
20.864576	931.240408	13.627827
20.736825	935.602676	13.632832
20.948496	926.083574	13.637837
20.410392	932.702627	13.642842
20.774647	933.388068	13.647847
20.866025	929.407966	13.652851
20.494390	931.436147	13.657856
20.608793	925.865664	13.662861
20.416722	928.435816	13.667866
20.778751	921.929202	13.672871
21.048515	925.398320	13.677875
20.370039	927.800027	13.682880
20.671775	932.448260	13.687885
20.598116	930.888539	13.692890
20.647491	920.756220	13.697895
20.608070	925.107683	13.702899
20.530951	930.391261	13.707904
20.682269	920.113175	13.712909
20.282455	927.059038	13.717914
20.559271	928.327098	13.722919
20.526888	922.814151	13.727923
20.523219	933.664693	13.732928
20.728098	929.634737	13.737933
20.543374	931.957711	13.742938
20.191303	933.797802	13.747943
20.827376	947.157726	13.752947
20.727677	945.832598	13.757952
20.590102	941.549119	13.762957
21.065825	938.221928	13.767962
21.077274	937.851158	13.772967
21.361069	927.426012	13.777971
21.225895	940.632771	13.782976
20.957137	936.135734	13.787981
20.892939	937.208843	13.792986
20.926455	925.173466	13.797991
20.770033	917.910224	13.802995
20.548845	911.452688	13.808000
20.857408	897.113881	13.813005
20.922544	909.524041	13.818010
20.468359	907.286282	13.823015
20.774863	904.391134	13.828019
20.657623	913.798255	13.833024
20.581504	906.680722	13.838029
20.736741	905.670701	13.843034
20.658703	908.344455	13.848039
20.639673	903.891057	13.853043
20.283196	911.447635	13.858048
20.250650	906.341691	13.863053
20.234165	912.919065	13.868058
20.554914	927.018291	13.873063
20.432529	928.211902	13.878067
20.708349	938.832556	13.883072
20.697817	936.390045	13.888077
20.866029	941.813931	13.893082
20.734113	940.319855	13.898087
20.798323	939.246097	13.903091
20.709554	929.684953	13.908096
20.544543	925.671048	13.913101
20.487269	925.537848	13.918106
20.275446	935.785797	13.923111
20.603679	939.985808	13.928115
20.569821	934.948370	13.933120
20.898848	940.346656	13.938125
20.633536	941.515431	13.943130
20.689137	943.399311	13.948135
20.898939	945.197147	13.953139
20.344190	955.104828	13.958144
20.612061	947.353961	13.963149
20.806837	939.742734	13.968154
20.492995	941.446405	13.973159
20.696414	944.430327	13.978163
20.431256	943.604485	13.983168
20.551455	937.095512	13.988173
20.738641	940.984577	13.993178
20.168422	942.636679	13.998183
20.837957	942.593206	14.003187
20.758807	948.072531	14.008192
20.764915	946.473213	14.013210
20.612061	947.194222	14.018227
20.805744	949.920128	14.023245
21.166873	945.146748	14.028263
21.257753	949.715991	14.033280
20.729831	933.223785	14.038298
20.841956	921.889129	14.043315
20.682658	916.248232	14.048333
20.928973	915.708598	14.053351
20.543177	926.248525	14.058368
20.744238	928.013256	14.063386
20.534780	932.430432	14.068403
20.665600	948.173485	14.073421
21.392268	939.447411	14.078439
21.004444	942.520277	14.083456
21.104367	942.968404	14.088474
21.098737	941.442764	14.093491
20.997446	936.207296	14.098509
21.015306	913.459713	14.103527
20.184180	923.511782	14.108544
20.639967	931.150943	14.113562
20.759043	937.865095	14.118579
20.647248	950.461349	14.123597
20.886169	947.872845	14.128615
20.598487	951.060441	14.133632
20.772185	945.585683	14.138650
20.972530	948.756145	14.143667
20.853720	966.232680	14.148685
21.175539	981.103592	14.153703
21.072705	985.711177	14.158720
20.987638	974.414623	14.163738
21.402086	978.110626	14.168755
21.296087	980.167396	14.173773
21.241927	982.397574	14.178791
21.158910	980.130423	14.183808
21.301581	982.230390	14.188826
21.122957	974.734784	14.193843
20.840821	985.165633	14.198861
21.174737	980.429981	14.203879
20.966614	990.328029	14.208896
20.979088	982.766975	14.213914
21.134506	986.629053	14.218931
21.157186	1005.438159	14.223949
21.362471	1013.418362	14.228967
21.644207	1021.162611	14.233984
21.618685	1022.633501	14.239002
21.664641	1017.031790	14.244019
21.579954	1019.529825	14.249037
21.581934	1012.222935	14.254055
21.073503	1008.666811	14.259072
21.178092	1020.885052	14.264090
21.284765	1023.241216	14.269107
21.160887	1021.890971	14.274125
21.321415	1011.305880	14.279143
21.694785	1014.013588	14.284160
21.501115	1014.146280	14.289178
21.344880	1024.300039	14.294195
21.353501	1026.089114	14.299213
21.797401	1033.381520	14.304231
21.699921	1047.439282	14.309248
21.766733	1050.315707	14.314266
21.990550	1039.318929	14.319283
21.523586	1042.388846	14.324301
21.888551	1048.571482	14.329319
22.107018	1048.236239	14.334336
21.772922	1038.557254	14.339354
21.378175	1039.982781	14.344371
21.765617	1050.748511	14.349389
22.086889	1047.928533	14.354407
21.831380	1063.838735	14.359424
21.938499	1061.846081	14.364442
21.613857	1052.532817	14.369459
21.924486	1064.562999	14.374477
22.100762	1059.815766	14.379495
22.241987	1057.560160	14.384512
22.147532	1060.009085	14.389530
22.066131	1064.713025	14.394547
22.687675	1065.985176	14.399565
22.484008	1036.715462	14.404583
22.105411	1035.384084	14.409600
22.012906	1028.810367	14.414618
22.223981	1021.953091	14.419635
22.076884	1026.404092	14.424653
22.180078	1014.711032	14.429671
22.272112	1025.676617	14.434688
22.065403	1022.890470	14.439706
21.744284	1029.474608	14.444723
21.421754	1039.157246	14.449741
22.060737	1050.885434	14.454759
21.873853	1056.702420	14.459776
22.121060	1065.352677	14.464794
22.227451	1051.850640	14.469811
21.948728	1058.862986	14.474829
21.908052	1055.511319	14.479847
21.843891	1077.045049	14.484864
22.514487	1084.627375	14.489882
22.672267	1083.954086	14.494899
22.394203	1093.002315	14.499917
22.681459	1083.923515	14.504935
22.388426	1087.869200	14.509952
22.359404	1086.339288	14.514970
22.928083	1079.573836	14.519987
22.665130	1087.440642	14.525005
22.572822	1085.518401	14.530023
23.062959	1085.190127	14.535040
22.783453	1079.655219	14.540058
22.720083	1064.065583	14.545075
22.312437	1059.644466	14.550093
22.637865	1064.261724	14.555111
22.302268	1055.098379	14.560128
22.424710	1084.177455	14.565146
22.733232	1078.325965	14.570163
22.549800	1094.079734	14.575181
22.897041	1079.218562	14.580199
22.636419	1083.074430	14.585216
22.581959	1087.992673	14.590234
22.737570	1086.136201	14.595251
22.775231	1094.860594	14.600269
22.949272	1085.997282	14.605287
22.715853	1085.679275	14.610304
22.926137	1089.919402	14.615322
22.973812	1082.673942	14.620339
22.786310	1086.869663	14.625357
22.843887	1087.293950	14.630375
23.030159	1092.789864	14.635392
22.640830	1096.061064	14.640410
22.570948	1088.580225	14.645427
22.751882	1094.340461	14.650445
23.042018	1103.891716	14.655463
23.002085	1110.591076	14.660480
23.082069	1118.098683	14.665498
23.335684	1107.942877	14.670515
23.027664	1120.382738	14.675533
23.260710	1122.710163	14.680551
23.220120	1114.915604	14.685568
23.421445	1109.420303	14.690586
23.341323	1087.118434	14.695603
23.236039	1085.055887	14.700621
23.375564	1078.513633	14.705639
23.132686	1072.248772	14.710656
23.056978	1083.015581	14.715674
23.590349	1093.026345	14.720691
23.183229	1095.629284	14.725709
23.429680	1094.250974	14.730727
23.238705	1094.926947	14.735744
23.267105	1106.666943	14.740762
23.600839	1109.719285	14.745779
23.476241	1111.533573	14.750797
23.710524	1106.876782	14.755815
23.559588	1095.107932	14.760832
23.560065	1084.488417	14.765850
23.938797	1080.358090	14.770867
23.717451	1082.661439	14.775885
23.449442	1084.134930	14.780903
23.756382	1076.850927	14.785920
23.403767	1084.048801	14.790938
23.759799	1082.855657	14.795955
23.749061	1088.590875	14.800973
23.537376	1080.408314	14.805991
23.699577	1087.249005	14.811008
23.388195	1087.697965	14.816026
23.655974	1089.292997	14.821043
23.625412	1091.213610	14.826061
23.660479	1103.389108	14.831079
23.809254	1113.966651	14.836096
23.906138	1121.417421	14.841114
23.945113	1106.275980	14.846131
23.643075	1103.264412	14.851149
23.655988	1112.922263	14.856167
23.939426	1109.312636	14.861184
23.701178	1122.377200	14.866202
23.975856	1110.325114	14.871219
23.970963	1116.784199	14.876237
23.924415	1122.807481	14.881255
23.984370	1110.527228	14.886272
23.653106	1116.510340	14.891290
23.820077	1105.585078	14.896307
23.906430	1111.747392	14.901325
23.935697	1109.080626	14.906343
24.328224	1109.276607	14.911360
24.401159	1110.859767	14.916378
24.649449	1119.472859	14.921395
24.353083	1117.285183	14.926413
24.506833	1116.973240	14.931431
24.535159	1112.060005	14.936448
24.197626	1099.118721	14.941466
24.080443	1089.058393	14.946483
24.090276	1094.600702	14.951501
24.003233	1114.398117	14.956519
24.166779	1110.900392	14.961536
23.874274	1118.991195	14.966554
23.911868	1115.841073	14.971571
23.847496	1118.693936	14.976589
23.890138	1111.727693	14.981607
24.205971	1124.501182	14.986624
24.210717	1142.221317	14.991642
24.327218	1145.656608	14.996659
24.452369	1145.565728	15.001677
24.578673	1144.525362	15.006695
24.847736	1138.908192	15.011712
24.433067	1139.372894	15.016730
24.384479	1140.822156	15.021747
24.815860	1139.472772	15.026765
24.982013	1138.571255	15.031783
24.682372	1129.370202	15.036800
24.459150	1140.741521	15.041818
25.011849	1145.426933	15.046835
24.503815	1140.134351	15.051853
24.764009	1136.459013	15.056871
25.062168	1133.701255	15.061888
25.182992	1136.654269	15.066906
24.746747	1124.141733	15.071923
24.613484	1113.056901	15.076941
24.451296	1124.722099	15.081959
24.914431	1129.867778	15.086976
24.792094	1147.894770	15.091994
24.878900	1141.555638	15.097011
24.855136	1146.906860	15.102029
25.035958	1143.579801	15.107047
24.934881	1137.856000	15.112064
24.776951	1138.917679	15.117082
25.039963	1131.611258	15.122099
24.801382	1141.985134	15.127117
24.864434	1146.887578	15.132135
24.947716	1144.290291	15.137152
24.693013	1150.668589	15.142170
24.675268	1145.942783	15.147187
24.860845	1144.831620	15.152205
24.789192	1151.689599	15.157223
25.409230	1147.754515	15.162240
25.277882	1155.961812	15.167258
25.512377	1156.736507	15.172275
25.325069	1154.886061	15.177293
25.215029	1148.054257	15.182311
25.256335	1145.827187	15.187328
25.217696	1150.406096	15.192346
25.115380	1145.281765	15.197363
25.356177	1151.995615	15.202381
25.140770	1171.165059	15.207399
25.585340	1170.433539	15.212416
25.478449	1176.073061	15.217434
25.831098	1172.029866	15.222451
25.805367	1155.292648	15.227469
25.468715	1150.912093	15.232487
25.909335	1138.282672	15.237504
25.844198	1151.872742	15.242522
25.655962	1137.856532	15.247539
25.362981	1139.319742	15.252557
24.951372	1145.204032	15.257575
25.620466	1142.148405	15.262592
25.569733	1144.772144	15.267610
25.816458	1146.497573	15.272627
25.395109	1143.826558	15.277645
25.252863	1154.494579	15.282663
25.491466	1161.020211	15.287680
25.747265	1174.065472	15.292698
25.922480	1165.662187	15.297715
25.925441	1177.944437	15.302733
25.261026	1173.275948	15.307751
25.749097	1177.527533	15.312768
25.727182	1175.288462	15.317786
25.746923	1171.885463	15.322803
25.910326	1167.329397	15.327821
25.718599	1175.846293	15.332839
26.272052	1175.243361	15.337856
25.822485	1173.969811	15.342874
25.745000	1172.098959	15.347891
26.002698	1171.888495	15.352909
25.665245	1185.485910	15.357927
25.985287	1190.769144	15.362944
25.829112	1195.876921	15.367962
26.227444	1197.983089	15.372979
26.647898	1201.539916	15.377997
26.263173	1197.504231	15.383015
26.301389	1182.236458	15.388032
26.098232	1184.279989	15.393050
26.044571	1180.162349	15.398067
26.384475	1177.547438	15.403085
26.065459	1190.194769	15.408103
26.452786	1192.848143	15.413120
26.284158	1201.813493	15.418138
26.286111	1205.084169	15.423155
26.415966	1203.297853	15.428173
26.298548	1202.053187	15.433191
26.616232	1204.046401	15.438208
26.632152	1203.080867	15.443226
26.419646	1192.463146	15.448243
26.558606	1193.327851	15.453261
26.499858	1187.656622	15.458279
26.574333	1182.757894	15.463296
26.390376	1189.401266	15.468314
26.679528	1191.352122	15.473331
26.585649	1187.336265	15.478349
26.315567	1186.994224	15.483367
26.482174	1190.357150	15.488384
26.785431	1199.039607	15.493402
26.404968	1198.444028	15.498419
26.550959	1197.916861	15.503437
26.451432	1196.709682	15.508455
26.636434	1199.346168	15.513472
26.743470	1199.400531	15.518490
26.607132	1202.872885	15.523507
26.757196	1194.257344	15.528525
26.502951	1199.617782	15.533543
26.569369	1189.043588	15.538560
27.039161	1209.179940	15.543578
26.962610	1224.415474	15.548595
27.285941	1223.920899	15.553613
27.250767	1215.584765	15.558631
26.945718	1200.838464	15.563648
27.205465	1199.602760	15.568666
27.186810	1200.566148	15.573683
27.188679	1193.425348	15.578701
26.836551	1196.521672	15.583719
26.961459	1189.138501	15.588736
27.064411	1209.113321	15.593754
26.868704	1226.213928	15.598771
27.335348	1226.052686	15.603789
27.114130	1232.626867	15.608807
27.202081	1223.597121	15.613824
27.272091	1227.378618	15.618842
27.073665	1224.168932	15.623859
27.147888	1221.407423	15.628877
26.983718	1228.886860	15.633895
27.202930	1227.434070	15.638912
27.356756	1226.372443	15.643930
26.874631	1224.127223	15.648947
27.275796	1217.153799	15.653965
27.008151	1239.782966	15.658983
27.403040	1241.362520	15.664000
28.028335	1246.402083	15.669018
27.669508	1254.854751	15.674035
28.044141	1237.468043	15.679053
27.723366	1230.740449	15.684071
27.822570	1218.871921	15.689088
28.027426	1225.918370	15.694106
27.597605	1222.662523	15.699123
27.526958	1223.202507	15.704141
27.932460	1224.351857	15.709159
27.854133	1218.485532	15.714176
27.861900	1223.006895	15.719194
27.717921	1226.238811	15.724211
27.972240	1230.513951	15.729229
27.871259	1223.046648	15.734247
27.759470	1220.777700	15.739264
27.772697	1223.092824	15.744282
27.748988	1224.209455	15.749299
27.990245	1217.778451	15.754317
27.753133	1221.768129	15.759335
27.715197	1220.169648	15.764352
27.855739	1216.402985	15.769370
27.806971	1228.503183	15.774387
28.123925	1239.110643	15.779405
27.579465	1254.345715	15.784423
28.245443	1252.993504	15.789440
28.044834	1247.660382	15.794458
27.883640	1253.823459	15.799475
28.202790	1249.447377	15.804493
28.087872	1252.716052	15.809511
28.212170	1248.015078	15.814528
28.324236	1243.802860	15.819546
28.479921	1255.095517	15.824563
28.425175	1255.174862	15.829581
28.475246	1260.746161	15.834599
28.108720	1251.323805	15.839616
28.242316	1246.904334	15.844634
28.329991	1254.579207	15.849651
28.459184	1246.612940	15.854669
28.202813	1247.526923	15.859687
28.447033	1253.213763	15.864704
28.524857	1254.098797	15.869722
28.348387	1258.656089	15.874739
28.337244	1250.154385	15.879757
28.400234	1261.699180	15.884775
28.607732	1277.837723	15.889792
28.970928	1274.110045	15.894810
28.975621	1278.977651	15.899827
29.143489	1254.248170	15.904845
29.248941	1248.242835	15.909863
29.129298	1248.930208	15.914880
28.872086	1247.124416	15.919898
28.874739	1257.798376	15.924915
28.703098	1245.138003	15.929933
28.647298	1250.648310	15.934951
28.380332	1247.015687	15.939968
28.652829	1250.257312	15.944986
28.956820	1244.260856	15.950003
28.976487	1237.938314	15.955021
28.958005	1245.345533	15.960039
28.565868	1249.337779	15.965056
29.010048	1263.102062	15.970074
29.037436	1275.736924	15.975091
29.425813	1274.895733	15.980109
29.393455	1263.089496	15.985127
29.024193	1255.412640	15.990144
29.148601	1238.888588	15.995162
29.019197	1237.919225	16.000179
29.313928	1241.484230	16.005197
29.272600	1243.429150	16.010215
29.082249	1246.502078	16.015232
29.660214	1251.250913	16.020250
29.073288	1244.757149	16.025267
29.440144	1246.184411	16.030285
29.525396	1255.295255	16.035303
29.187011	1250.495641	16.040320
29.499428	1250.896320	16.045338
29.317103	1271.189839	16.050355
29.303508	1272.948890	16.055373
29.742373	1281.037228	16.060391
30.069634	1276.672347	16.065408
29.669682	1254.818021	16.070426
29.650684	1254.544750	16.075443
29.668791	1241.962093	16.080461
29.569970	1232.975388	16.085479
29.218967	1235.478169	16.090496
29.628143	1245.435910	16.095514
29.754257	1261.297419	16.100531
29.850691	1267.837628	16.105549
29.780015	1268.581967	16.110567
29.969098	1269.670780	16.115584
29.996298	1273.968728	16.120602
29.762717	1262.863584	16.125619
29.800248	1265.560014	16.130637
29.723506	1263.998499	16.135655
29.795505	1265.567268	16.140672
30.135763	1266.578976	16.145690
30.149719	1272.580918	16.150707
29.924485	1264.796680	16.155725
30.112806	1262.889693	16.160743
30.021468	1268.591942	16.165760
29.939511	1265.351254	16.170778
29.952220	1276.755850	16.175795
29.935287	1266.646326	16.180813
30.127272	1277.550854	16.185831
29.821604	1271.718761	16.190848
30.151736	1263.482581	16.195866
29.845985	1265.441735	16.200883
29.550434	1265.517480	16.205901
29.747574	1279.787560	16.210919
30.015983	1286.991266	16.215936
30.304128	1286.485398	16.220954
30.286898	1293.592791	16.225971
30.237206	1279.147941	16.230989
30.115481	1284.266771	16.236007
30.037237	1283.542987	16.241024
30.004807	1292.124375	16.246042
30.573740	1310.243291	16.251059
30.771125	1313.765942	16.256077
30.756828	1311.478297	16.261095
30.817910	1314.100218	16.266112
30.647103	1296.661673	16.271130
30.918997	1288.366167	16.276147
30.813905	1282.653633	16.281165
31.009551	1277.632517	16.286183
30.406318	1280.669537	16.291200
30.771538	1278.352659	16.296218
30.662068	1282.946113	16.301235
30.855656	1275.135735	16.306253
30.995855	1285.465238	16.311271
30.947319	1284.278840	16.316288
30.786756	1280.697657	16.321306
30.716136	1296.525210	16.326323
30.866265	1307.777122	16.331341
31.232120	1295.716349	16.336359
31.088106	1311.772268	16.341376
31.527499	1302.300297	16.346394
31.546102	1292.480753	16.351411
31.394636	1276.872147	16.356429
31.715128	1276.061888	16.361447
31.322853	1278.336298	16.366464
31.668533	1270.020276	16.371482
31.068923	1279.061531	16.376499
31.182778	1279.328130	16.381517
31.434447	1275.969998	16.386535
31.225119	1276.176642	16.391552
31.383612	1272.361215	16.396570
31.157029	1284.021823	16.401587
31.055340	1277.624001	16.406605
31.481295	1277.814253	16.411623
31.241617	1277.540232	16.416640
31.513650	1269.036033	16.421658
30.969224	1281.011392	16.426675
31.269298	1286.385886	16.431693
31.343030	1281.178566	16.436711
31.374621	1303.733292	16.441728
31.131457	1308.261872	16.446746
31.032644	1312.197149	16.451763
31.173687	1313.902131	16.456781
31.161681	1309.900160	16.461799
31.127204	1340.745357	16.466816
31.398571	1329.257109	16.471834
31.862485	1341.556922	16.476851
31.755188	1335.510857	16.481869
32.021109	1333.714191	16.486887
32.126225	1343.068949	16.491904
32.313858	1331.510795	16.496922
31.878721	1334.854075	16.501939
32.247596	1330.677732	16.506957
32.023997	1335.419914	16.511975
32.130130	1340.360707	16.516992
32.204112	1336.372336	16.522010
32.215038	1334.031146	16.527027
32.238875	1334.643918	16.532045
32.539139	1324.244913	16.537063
32.296215	1313.877622	16.542080
32.359524	1294.283788	16.547098
32.107784	1300.945522	16.552115
32.105141	1312.936687	16.557133
32.200682	1306.462121	16.562151
32.026356	1321.019175	16.567168
32.447587	1325.018851	16.572186
32.464070	1333.099705	16.577203
32.354750	1332.354473	16.582221
32.448731	1331.596827	16.587239
32.593617	1340.734509	16.592256
32.725954	1332.160124	16.597274
32.321936	1327.634361	16.602291
32.470748	1335.614175	16.607309
32.484723	1330.729317	16.612327
32.299672	1335.986592	16.617344
32.272463	1334.741017	16.622362
32.639779	1331.968612	16.627379
32.290298	1343.810585	16.632397
32.555332	1328.988077	16.637415
32.373534	1339.376759	16.642432
32.400787	1334.333704	16.647450
32.461741	1346.092710	16.652467
32.847402	1358.000404	16.657485
33.012082	1365.091998	16.662503
33.120896	1374.594579	16.667520
33.131911	1370.523285	16.672538
33.055423	1372.724273	16.677555
33.423798	1368.829922	16.682573
33.479914	1345.125456	16.687591
33.422034	1342.925208	16.692608
32.862711	1331.953823	16.697626
33.210516	1337.189037	16.702643
33.123261	1332.231763	16.707661
33.065101	1332.532974	16.712679
33.096893	1332.588820	16.717696
33.069924	1333.055564	16.722714
33.097107	1337.700022	16.727731
33.362444	1361.221145	16.732749
33.529616	1353.679062	16.737767
32.990558	1353.199257	16.742784
33.329053	1368.868543	16.747802
33.566119	1363.689891	16.752819
33.286234	1367.643627	16.757837
33.410768	1365.783396	16.762855
33.278864	1364.445127	16.767872
33.453225	1360.382842	16.772890
33.616859	1354.848244	16.777907
33.387592	1357.158109	16.782925
33.691423	1359.882133	16.787943
33.745364	1368.374732	16.792960
33.518758	1362.340844	16.797978
33.757226	1355.836633	16.802995
33.548566	1363.969491	16.808013
33.860880	1360.865929	16.813031
33.526799	1361.825527	16.818048
33.918916	1360.442302	16.823066
34.261052	1352.394586	16.828083
33.663760	1361.580780	16.833101
34.179023	1359.640958	16.838119
34.139004	1359.759909	16.843136
34.142311	1360.500623	16.848154
33.874700	1363.261986	16.853171
33.980593	1359.787083	16.858189
34.228377	1357.690347	16.863207
34.227995	1363.700688	16.868224
34.338829	1348.747103	16.873242
34.546570	1353.671267	16.878259
34.565803	1358.065889	16.883277
34.466387	1354.128898	16.888295
34.399596	1354.252832	16.893312
34.503866	1356.110593	16.898330
34.427259	1354.180114	16.903347
34.274175	1352.517101	16.908365
34.325517	1341.156339	16.913383
34.060631	1349.847305	16.918400
34.186357	1355.602930	16.923418
34.346487	1351.227703	16.928435
34.353267	1359.001544	16.933453
34.149609	1357.158602	16.938471
34.625362	1354.246724	16.943488
34.358179	1352.046529	16.948506
34.792551	1359.776984	16.953523
33.963862	1365.711996	16.958541
34.174993	1374.920632	16.963559
34.381677	1386.714138	16.968576
34.191876	1394.215373	16.973594
34.309262	1389.613583	16.978611
34.241120	1395.457584	16.983629
34.492633	1405.916521	16.988647
34.792535	1419.225713	16.993664
34.665087	1412.730666	16.998682
35.011281	1410.991496	17.003699
34.873920	1407.541358	17.008717
35.355836	1406.470717	17.013735
35.283617	1409.229300	17.018752
34.935239	1411.089076	17.023770
35.275300	1408.902489	17.028787
35.530093	1416.149933	17.033805
35.335191	1409.821192	17.038823
35.791876	1409.137591	17.043840
35.663895	1406.802094	17.048858
35.860454	1413.980773	17.053875
35.401623	1399.238206	17.058893
35.424189	1378.462949	17.063911
35.261497	1380.657063	17.068928
35.288385	1381.598085	17.073946
35.601848	1372.606367	17.078963
35.186303	1383.777744	17.083981
35.618531	1388.052743	17.088999
35.670719	1405.750475	17.094016
35.461751	1405.564502	17.099034
35.849891	1409.574993	17.104051
35.428553	1409.402987	17.109069
35.232416	1412.608841	17.114087
35.346593	1405.046682	17.119104
35.265437	1406.655111	17.124122
35.507369	1407.041893	17.129139
35.270697	1403.481999	17.134157
35.643643	1409.913437	17.139175
35.957514	1428.410112	17.144192
35.719282	1438.549848	17.149210
36.017433	1434.076912	17.154227
35.744660	1443.377609	17.159245
35.779986	1442.869802	17.164263
35.829075	1439.554636	17.169280
35.693862	1429.653100	17.174298
36.010872	1421.677380	17.179315
35.818439	1433.323187	17.184333
35.841356	1430.219617	17.189351
36.075142	1439.597258	17.194368
36.065855	1453.511512	17.199386
36.544278	1452.469423	17.204403
36.499905	1458.226293	17.209421
36.560229	1453.376762	17.214439
36.031127	1436.998801	17.219456
36.579371	1455.199393	17.224474
36.598352	1445.764373	17.229491
36.190092	1439.665526	17.234509
36.511335	1445.237254	17.239527
36.737211	1456.860184	17.244544
36.776117	1456.676991	17.249562
36.966396	1445.428173	17.254579
36.379248	1439.709637	17.259597
36.568852	1439.861668	17.264615
36.764881	1454.551825	17.269632
36.765836	1454.862983	17.274650
37.157928	1451.933145	17.279667
36.877948	1465.124058	17.284685
36.778665	1446.293417	17.289703
37.098682	1451.008186	17.294720
36.864616	1444.773162	17.299738
37.097964	1443.159252	17.304755
36.887559	1448.660698	17.309773
37.078282	1443.445866	17.314791
37.137142	1437.620905	17.319808
36.938668	1455.544365	17.324826
37.784307	1448.387144	17.329843
37.155287	1439.998357	17.334861
36.835626	1420.056993	17.339879
37.144642	1420.842944	17.344896
37.457851	1442.101434	17.349914
37.379068	1431.650799	17.354931
37.299366	1430.416972	17.359949
37.234118	1417.501186	17.364967
37.455448	1436.173595	17.369984
37.282107	1450.826673	17.375002
37.564587	1451.419518	17.380019
37.226083	1453.320130	17.385037
37.103317	1453.621789	17.390055
37.176149	1453.613113	17.395072
37.154611	1457.027253	17.400090
37.003707	1449.501859	17.405107
37.014696	1460.958464	17.410125
37.121478	1473.704691	17.415143
37.612883	1477.748681	17.420160
37.430787	1489.378583	17.425178
37.412351	1487.613722	17.430195
37.406267	1488.530873	17.435213
37.550947	1494.155727	17.440231
37.876073	1501.353747	17.445248
37.849489	1514.009474	17.450266
38.024733	1512.288577	17.455283
38.140263	1513.536884	17.460301
38.322236	1515.194709	17.465319
38.685899	1508.875292	17.470336
38.459598	1503.327566	17.475354
38.089215	1487.738169	17.480371
37.970634	1483.135072	17.485389
37.965174	1475.920589	17.490407
38.336569	1490.140905	17.495424
37.948845	1510.088021	17.500442
38.315300	1510.236506	17.505459
38.157104	1521.902496	17.510477
38.390594	1518.319846	17.515495
38.501495	1511.092091	17.520512
38.492058	1507.508963	17.525530
38.520347	1516.068252	17.530547
38.312131	1516.333375	17.535565
38.597242	1512.622179	17.540583
38.563747	1512.914833	17.545600
38.624144	1517.537506	17.550618
38.610144	1508.252999	17.555635
38.467105	1510.844983	17.560653
38.567883	1511.291406	17.565671
38.806497	1514.477079	17.570688
38.460382	1517.368082	17.575706
38.855268	1524.102136	17.580723
38.978842	1531.048081	17.585741
38.584257	1537.117019	17.590759
39.169209	1535.959406	17.595776
38.923982	1536.252137	17.600794
39.331611	1532.622698	17.605811
39.154232	1532.632509	17.610829
39.276882	1537.625262	17.615847
39.318817	1537.965227	17.620864
39.186236	1540.678270	17.625882
39.279061	1528.264088	17.630899
39.404744	1527.545097	17.635917
39.337725	1523.379650	17.640935
39.334608	1504.472603	17.645952
39.047059	1512.998236	17.650970
39.686130	1519.109655	17.655987
39.470463	1530.661870	17.661005
39.183535	1532.498918	17.666023
39.723574	1530.570579	17.671040
39.473449	1532.054825	17.676058
39.832499	1539.117505	17.681075
39.893674	1538.249320	17.686093
39.282950	1532.786393	17.691111
39.313465	1534.141019	17.696128
39.724802	1537.830210	17.701146
39.646557	1531.351878	17.706163
39.380632	1541.445636	17.711181
39.521967	1537.449997	17.716199
39.961132	1527.879888	17.721216
40.073634	1543.139232	17.726234
40.044349	1526.035258	17.731251
40.062378	1530.018674	17.736269
39.968446	1534.535121	17.741287
40.271600	1532.553291	17.746304
39.699951	1534.791554	17.751322
40.118481	1530.138880	17.756339
40.138711	1533.183240	17.761357
39.927486	1539.282165	17.766375
40.379918	1542.507571	17.771392
40.312751	1556.451921	17.776410
40.303667	1568.301458	17.781427
40.900781	1564.057179	17.786445
40.413128	1542.023370	17.791463
40.841084	1525.166628	17.796480
40.756692	1530.237007	17.801498
40.728120	1520.993971	17.806515
40.848362	1510.474904	17.811533
40.330591	1526.409278	17.816551
40.807272	1514.134041	17.821568
40.538850	1519.065872	17.826586
40.496342	1522.793496	17.831603
40.594129	1519.630217	17.836621
40.529994	1522.751644	17.841639
40.700246	1522.690041	17.846656
41.054386	1547.894036	17.851674
41.110367	1537.651745	17.856691
41.043990	1523.251265	17.861709
40.808944	1534.142958	17.866727
40.548650	1521.648756	17.871744
40.712697	1537.057540	17.876762
40.817526	1544.781196	17.881779
41.174894	1544.655226	17.886797
41.058038	1543.661642	17.891815
41.123027	1548.992667	17.896832
41.133302	1555.943873	17.901850
41.218353	1549.400919	17.906867
41.264279	1553.913867	17.911885
41.107116	1558.420686	17.916903
41.189121	1550.745063	17.921920
41.008768	1550.785701	17.926938
41.260444	1560.215079	17.931955
41.363140	1569.416040	17.936973
41.501739	1576.913820	17.941991
41.373598	1572.258392	17.947008
41.596536	1571.736528	17.952026
41.514493	1574.525173	17.957043
41.947068	1570.954053	17.962061
41.254430	1575.575127	17.967079
41.556613	1576.187043	17.972096
41.363775	1575.821511	17.977114
41.257278	1575.420701	17.982131
41.964334	1579.620285	17.987149
41.946692	1595.335504	17.992167
42.435687	1584.210194	17.997184
42.269043	1578.647094	18.002202
42.258630	1573.988413	18.007219
42.626145	1565.518871	18.012237
42.114848	1566.047397	18.017255
42.365598	1566.980368	18.022272
42.215077	1560.304157	18.027290
42.139034	1568.853407	18.032307
42.306878	1563.658995	18.037325
41.891775	1563.437093	18.042343
41.995028	1560.137027	18.047360
42.052211	1568.511844	18.052378
42.142249	1587.470358	18.057395
42.118841	1591.960555	18.062413
42.239635	1600.886355	18.067431
42.597988	1591.767512	18.072448
42.776368	1590.253572	18.077466
42.655398	1594.533307	18.082483
42.757880	1594.956603	18.087501
42.568475	1601.684163	18.092519
43.082723	1597.810420	18.097536
43.283470	1590.353028	18.102554
43.139201	1592.087269	18.107571
43.345710	1590.272018	18.112589
43.335887	1592.223393	18.117607
43.342129	1578.776264	18.122624
43.086256	1568.041691	18.127642
43.007775	1554.892603	18.132659
43.302408	1554.172994	18.137677
42.901964	1553.294179	18.142695
42.862357	1551.189992	18.147712
42.903057	1563.940535	18.152730
42.688880	1584.408049	18.157747
42.877857	1589.832803	18.162765
42.949723	1586.980680	18.167783
43.002657	1582.471782	18.172800
43.129931	1589.566742	18.177818
42.952062	1595.261895	18.182835
43.127385	1608.599302	18.187853
43.272167	1619.347972	18.192871
43.200423	1617.707996	18.197888
43.272280	1621.897192	18.202906
43.221404	1627.604447	18.207923
43.374518	1619.020830	18.212941
43.454700	1637.103438	18.217959
43.960540	1647.251582	18.222976
44.352474	1641.072556	18.227994
43.987452	1629.476242	18.233011
44.152897	1614.347275	18.238029
43.992523	1620.680453	18.243047
44.255234	1610.203436	18.248064
44.109400	1612.712048	18.253082
43.842724	1617.705035	18.258099
44.027592	1610.673629	18.263117
43.838196	1616.746398	18.268135
44.028060	1613.004654	18.273152
43.999558	1626.810140	18.278170
44.117741	1640.333768	18.283187
44.244456	1642.846056	18.288205
44.112771	1649.307019	18.293223
44.121735	1647.545317	18.298240
44.257089	1648.145677	18.303258
44.464161	1649.311757	18.308275
45.043104	1642.121032	18.313293
44.812636	1653.093133	18.318311
45.104417	1648.555473	18.323328
45.110962	1642.794135	18.328346
44.830967	1644.331155	18.333363
44.967810	1614.731078	18.338381
44.633913	1617.295559	18.343399
44.443449	1611.570765	18.348416
44.823109	1611.055892	18.353434
44.565980	1634.958376	18.358451
45.137561	1632.374940	18.363469
44.881002	1645.191869	18.368487
44.874786	1643.594994	18.373504
45.179715	1639.416933	18.378522
44.848516	1644.438708	18.383539
45.367345	1639.224258	18.388557
45.096301	1647.160849	18.393575
45.109695	1643.476914	18.398592
45.360547	1639.152990	18.403610
44.764101	1652.109309	18.408627
45.183009	1640.355353	18.413645
45.207031	1641.169310	18.418663
45.015389	1642.337993	18.423680
45.248261	1640.984016	18.428698
45.000435	1662.287415	18.433715
45.462436	1662.851459	18.438733
44.848345	1669.964493	18.443751
45.036387	1658.764336	18.448768
45.539123	1662.125254	18.453786
45.077245	1677.827338	18.458803
45.319070	1684.306571	18.463821
45.692415	1689.850555	18.468839
45.647358	1696.000588	18.473856
45.810522	1689.759179	18.478874
45.518213	1690.150940	18.483891
45.968626	1683.682706	18.488909
45.807735	1691.275987	18.493927
45.513205	1689.124925	18.498944
46.454934	1698.530578	18.503962
46.133920	1715.742977	18.508979
46.562769	1710.650636	18.513997
46.563275	1705.096239	18.519015
46.419588	1688.699182	18.524032
46.519836	1677.818035	18.529050
46.300915	1696.524498	18.534067
46.556170	1684.094550	18.539085
46.320850	1682.453475	18.544103
46.485841	1685.582901	18.549120
46.625252	1675.089181	18.554138
46.261402	1682.309728	18.559155
46.580762	1690.604225	18.564173
46.656033	1698.405473	18.569191
46.942730	1711.955791	18.574208
47.014008	1707.122022	18.579226
46.841012	1694.889517	18.584243
46.930946	1684.945674	18.589261
46.765787	1687.824976	18.594279
46.986373	1692.634434	18.599296
46.929026	1706.867032	18.604314
46.905608	1712.328637	18.609331
47.037599	1715.793686	18.614349
47.107625	1709.503664	18.619367
47.050171	1715.115216	18.624384
47.222474	1705.729351	18.629402
47.102810	1719.044978	18.634419
47.449862	1712.371199	18.639437
47.084704	1720.772833	18.644455
47.068241	1710.586949	18.649472
47.352189	1707.384627	18.654490
47.074398	1719.629207	18.659507
47.063088	1707.544189	18.664525
47.514607	1724.479645	18.669543
47.335066	1732.860487	18.674560
47.841559	1737.086233	18.679578
47.529155	1745.242587	18.684595
47.856230	1746.003017	18.689613
47.789275	1745.250107	18.694631
48.118522	1748.948305	18.699648
48.467048	1737.011439	18.704666
48.266015	1734.998689	18.709683
48.329575	1712.317313	18.714701
48.186577	1704.773902	18.719719
47.651993	1705.426517	18.724736
47.724341	1704.403634	18.729754
47.190650	1706.739361	18.734771
47.844372	1727.430353	18.739789
48.176827	1729.302588	18.744807
48.274823	1742.756135	18.749824
48.071028	1733.748550	18.754842
48.244557	1740.871480	18.759859
48.406623	1729.750144	18.764877
48.460034	1734.741444	18.769895
48.437457	1738.610602	18.774912
48.536714	1734.184281	18.779930
48.130682	1737.122214	18.784947
48.366699	1750.970658	18.789965
48.687692	1749.450759	18.794983
48.829950	1760.198383	18.800000
48.848100	1761.285826	18.805018
48.432121	1755.339376	18.810035
48.684043	1754.353427	18.815053
48.776539	1758.893494	18.820071
48.408107	1762.509712	18.825088
48.701915	1763.214421	18.830106
48.863863	1759.458134	18.835123
48.787663	1757.860251	18.840141
49.098657	1779.636179	18.845159
49.417925	1785.682835	18.850176
49.359702	1791.339828	18.855194
49.440143	1790.831363	18.860211
49.415880	1786.395492	18.865229
49.482335	1776.734389	18.870247
49.474929	1781.091566	18.875264
49.964747	1764.920108	18.880282
49.424550	1769.756863	18.885299
49.573715	1761.096671	18.890317
49.745692	1751.569085	18.895335
49.619764	1753.292719	18.900352
49.585135	1750.989202	18.905370
49.408648	1770.231455	18.910387
49.346481	1785.058328	18.915405
49.855585	1781.505148	18.920423
49.697364	1789.837871	18.925440
50.180433	1781.018047	18.930458
49.791986	1787.328576	18.935475
49.698724	1788.585534	18.940493
50.274124	1783.595224	18.945511
49.961691	1788.275992	18.950528
50.315731	1787.951355	18.955546
50.192630	1787.627805	18.960563
49.890834	1785.134232	18.965581
49.765172	1788.212317	18.970599
49.928660	1802.565427	18.975616
50.362976	1796.870474	18.980634
49.689314	1806.222003	18.985651
49.876960	1821.182480	18.990669
50.101294	1808.660873	18.995687
50.082181	1834.587672	19.000704
50.557315	1834.918735	19.005722
50.385294	1840.365306	19.010739
50.184428	1843.525202	19.015757
50.219738	1846.239831	19.020775
50.392144	1851.235181	19.025792
51.016580	1859.944845	19.030810
51.058979	1864.217119	19.035827
51.895776	1842.458630	19.040845
52.028001	1823.217324	19.045863
51.494886	1818.911603	19.050880
51.921843	1812.553257	19.055898
51.877228	1802.382376	19.060915
51.550697	1782.587018	19.065933
51.990746	1781.784982	19.070951
51.628273	1781.791876	19.075968
51.792138	1775.454632	19.080986
51.364162	1785.278262	19.086003
51.642735	1774.579886	19.091021
51.765406	1774.924914	19.096039
51.641123	1772.396972	19.101056
51.683593	1777.359450	19.106074
52.139350	1774.158766	19.111091
51.560053	1756.781863	19.116109
51.901373	1744.276080	19.121127
51.486776	1747.721842	19.126144
51.540857	1750.423394	19.131162
51.782039	1774.658817	19.136179
51.721655	1768.897882	19.141197
51.937195	1767.148394	19.146215
51.475117	1774.186194	19.151232
51.562479	1775.328708	19.156250
51.722842	1779.088943	19.161267
51.810671	1792.459227	19.166285
52.285975	1804.038079	19.171303
52.173004	1805.290148	19.176320
52.071239	1816.712796	19.181338
51.787987	1814.703895	19.186355
52.110497	1813.770415	19.191373
52.260201	1815.316469	19.196391
52.070163	1828.576135	19.201408
52.071866	1840.052330	19.206426
52.017790	1841.022224	19.211443
51.661378	1844.941161	19.216461
52.190711	1857.219539	19.221479
52.389951	1875.856886	19.226496
52.721356	1875.180966	19.231514
52.635493	1874.806536	19.236531
52.760290	1875.443758	19.241549
53.140774	1871.155033	19.246567
53.004532	1879.239517	19.251584
52.852537	1865.839351	19.256602
52.804699	1873.325925	19.261619
53.316020	1891.343180	19.266637
53.637414	1902.645304	19.271655
53.432866	1894.769002	19.276672
53.343022	1880.143447	19.281690
53.321400	1872.503939	19.286707
53.055117	1873.047166	19.291725
53.718796	1882.359641	19.296743
53.587383	1896.700791	19.301760
53.594173	1904.621377	19.306778
53.960794	1893.871600	19.311795
53.725058	1895.879463	19.316813
53.728011	1872.404600	19.321831
53.730090	1886.025522	19.326848
54.059995	1893.217393	19.331866
53.863823	1893.569838	19.336883
54.223551	1897.736135	19.341901
54.494596	1883.916924	19.346919
53.728791	1875.393062	19.351936
53.615649	1871.633906	19.356954
53.933831	1885.726683	19.361971
53.723376	1895.583177	19.366989
53.743640	1888.359762	19.372007
54.081939	1904.232798	19.377024
54.020691	1897.382454	19.382042
54.031047	1889.839042	19.387059
54.003486	1916.909304	19.392077
54.750266	1911.788379	19.397095
54.575053	1918.711304	19.402112
54.262636	1917.605930	19.407130
54.592770	1922.216734	19.412147
54.282241	1928.630511	19.417165
54.646860	1924.270073	19.422183
54.681704	1928.811017	19.427200
54.422546	1933.727213	19.432218
54.903926	1935.311702	19.437235
54.475808	1952.046595	19.442253
55.196766	1942.453911	19.447271
54.726770	1947.899630	19.452288
55.065306	1946.008941	19.457306
55.399765	1948.699864	19.462323
54.941678	1953.508027	19.467341
55.272419	1949.694406	19.472359
55.446967	1957.361032	19.477376
55.183217	1948.470703	19.482394
55.632831	1943.572391	19.487411
55.105806	1957.649883	19.492429
55.462893	1940.748146	19.497447
55.628779	1955.789265	19.502464
55.644047	1963.800566	19.507482
55.966338	1965.605666	19.512499
55.993146	1959.805693	19.517517
55.710345	1950.555195	19.522535
55.605492	1961.223261	19.527552
55.748881	1969.787478	19.532570
56.112027	1975.807786	19.537587
55.987942	1973.454210	19.542605
56.539346	1972.276334	19.547623
56.541271	1980.382069	19.552640
56.200002	1953.835370	19.557658
56.369745	1939.717295	19.562675
56.332380	1943.474063	19.567693
56.331220	1930.381884	19.572711
56.018772	1939.699520	19.577728
56.004931	1947.577990	19.582746
56.261593	1976.637295	19.587763
56.241770	1969.944012	19.592781
56.373169	1977.830278	19.597799
56.490721	1970.764578	19.602816
56.537626	1972.362922	19.607834
56.861604	1967.622775	19.612851
56.760595	1965.439282	19.617869
56.692949	1961.095850	19.622887
56.451138	1975.337479	19.627904
56.696395	1981.752460	19.632922
56.352046	1987.500710	19.637939
56.193312	1997.559845	19.642957
56.427668	2000.528998	19.647975
56.578932	2017.444193	19.652992
56.850714	2023.595948	19.658010
57.309840	2026.968756	19.663027
57.396560	2034.039764	19.668045
57.223326	2028.059860	19.673063
57.026517	2034.961732	19.678080
57.491626	2029.430730	19.683098
57.966240	2041.440645	19.688115
57.540373	2049.322473	19.693133
57.630896	2051.909153	19.698151
58.119192	2046.382833	19.703168
57.836043	2050.909818	19.708186
58.150221	2030.677088	19.713203
57.961104	2030.554640	19.718221
57.769063	2024.801613	19.723239
58.153965	2035.714155	19.728256
58.030101	2042.126294	19.733274
58.380328	2040.738776	19.738291
58.474338	2049.541850	19.743309
58.234046	2038.321538	19.748327
58.215257	2039.003466	19.753344
58.419748	2049.535867	19.758362
58.228503	2048.964116	19.763379
58.190974	2046.578757	19.768397
58.333864	2039.452769	19.773415
58.307442	2043.396294	19.778432
58.184802	2041.087741	19.783450
58.499595	2044.518374	19.788467
58.176838	2047.410585	19.793485
58.533804	2061.845346	19.798503
58.680433	2073.009816	19.803520
58.496977	2073.092331	19.808538
58.863206	2071.576066	19.813555
58.681469	2064.421852	19.818573
59.396532	2071.455240	19.823591
58.989382	2069.019059	19.828608
59.056669	2072.635852	19.833626
59.388895	2061.794993	19.838643
59.449578	2071.106224	19.843661
59.321811	2068.577650	19.848679
59.159230	2060.507823	19.853696
58.937109	2068.866612	19.858714
59.313807	2080.395637	19.863731
59.634176	2092.150893	19.868749
59.792434	2097.355863	19.873767
59.710576	2094.101203	19.878784
59.251875	2102.856526	19.883802
59.812499	2097.945435	19.888819
59.796185	2093.920376	19.893837
59.705270	2097.361120	19.898855
59.919369	2096.213896	19.903872
60.051057	2095.522201	19.908890
60.088569	2092.031298	19.913907
59.973101	2095.782199	19.918925
59.941814	2092.242846	19.923943
60.265544	2099.387833	19.928960
59.984175	2107.599298	19.933978
60.387554	2111.765257	19.938995
60.099351	2122.027403	19.944013
60.416656	2123.095477	19.949031
60.771740	2126.653097	19.954048
60.571419	2125.613934	19.959066
60.920619	2123.714703	19.964083
60.384794	2123.790690	19.969101
60.753092	2120.104467	19.974119
60.972024	2120.739343	19.979136
60.956619	2112.462341	19.984154
60.869568	2107.971386	19.989171
60.896123	2114.853505	19.994189
60.942133	2117.171016	19.999207
61.358339	2114.043196	20.004224
61.082810	2113.723327	20.009242
61.258428	2113.230035	20.014259
60.980927	2117.495797	20.019277
61.309422	2120.456709	20.024295
61.528487	2132.710535	20.029312
61.469343	2135.924154	20.034330
61.911508	2133.714059	20.039347
61.800358	2131.079068	20.044365
62.026669	2128.203518	20.049383
62.038915	2109.970760	20.054400
61.771945	2110.095942	20.059418
61.747787	2094.638337	20.064435
61.362155	2105.746032	20.069453
61.694849	2125.823209	20.074471
61.915465	2131.575059	20.079488
61.666189	2133.320275	20.084506
61.869719	2126.948920	20.089523
61.834810	2136.723886	20.094541
61.735051	2131.844102	20.099559
62.001926	2140.171857	20.104576
61.799301	2162.586062	20.109594
62.246456	2161.439040	20.114611
62.189139	2157.413514	20.119629
62.265875	2163.325495	20.124647
62.609345	2164.204414	20.129664
62.321650	2163.947268	20.134682
62.565440	2163.815569	20.139699
62.573652	2173.575290	20.144717
62.524954	2194.818889	20.149735
62.913027	2191.841569	20.154752
62.966262	2188.803527	20.159770
63.285236	2183.997628	20.164787
63.130280	2184.490278	20.169805
62.904050	2185.811802	20.174823
62.900577	2186.284781	20.179840
63.197644	2188.319068	20.184858
62.979759	2179.870809	20.189875
63.167886	2179.911668	20.194893
63.405205	2186.550568	20.199911
63.345553	2191.171578	20.204928
63.241192	2216.100878	20.209946
63.550300	2211.391953	20.214963
63.562907	2219.123878	20.219981
63.369970	2224.140244	20.224999
63.997175	2215.314763	20.230016
64.191675	2222.789488	20.235034
64.455970	2211.077760	20.240051
64.379198	2221.194650	20.245069
64.327284	2218.404585	20.250087
64.439839	2213.487588	20.255104
64.454065	2214.934056	20.260122
64.616818	2192.253880	20.265139
64.319965	2176.162925	20.270157
64.326435	2184.729865	20.275175
64.430823	2166.793493	20.280192
64.286029	2179.837402	20.285210
64.234926	2196.739841	20.290227
64.539679	2211.726685	20.295245
64.242839	2217.815350	20.300263
64.196547	2212.735007	20.305280
64.252740	2220.868183	20.310298
64.649999	2228.573543	20.315315
64.551008	2231.789289	20.320333
64.417541	2248.913022	20.325351
64.583257	2246.657380	20.330368
64.543573	2254.721958	20.335386
64.526745	2266.009093	20.340403
65.034090	2273.813730	20.345421
65.089093	2275.125634	20.350439
65.290182	2276.612523	20.355456
65.054839	2279.279127	20.360474
65.525007	2279.051915	20.365491
65.671801	2272.728030	20.370509
65.445035	2279.807218	20.375527
65.490271	2270.523129	20.380544
65.611717	2283.599443	20.385562
65.845435	2273.501028	20.390579
65.980117	2270.675026	20.395597
65.908812	2278.257562	20.400615
65.634660	2283.347723	20.405632
65.696602	2298.899980	20.410650
65.528252	2308.184466	20.415667
66.057751	2307.183185	20.420685
65.879272	2309.614814	20.425703
66.139954	2296.514452	20.430720
66.233596	2298.693883	20.435738
66.240525	2305.447147	20.440755
66.421302	2309.763152	20.445773
66.346951	2327.869902	20.450791
66.565227	2328.871886	20.455808
66.780646	2330.049189	20.460826
66.894962	2328.696186	20.465843
67.457710	2324.918697	20.470861
67.218224	2315.332158	20.475879
67.190417	2293.900441	20.480896
67.142784	2296.122205	20.485914
67.241884	2291.629602	20.490931
67.474326	2288.738797	20.495949
67.345086	2293.065422	20.500967
67.451452	2286.509056	20.505984
67.329182	2290.815584	20.511002
67.379270	2297.978045	20.516019
67.363296	2288.963533	20.521037
67.184607	2291.392045	20.526055
67.495455	2292.522271	20.531072
67.411390	2306.979713	20.536090
67.515902	2317.286880	20.541107
67.845352	2319.459749	20.546125
67.688512	2322.163304	20.551143
67.710166	2323.855003	20.556160
67.727928	2327.450813	20.561178
67.523584	2319.238776	20.566195
67.938128	2311.147447	20.571213
67.844545	2337.471370	20.576231
67.792751	2347.433642	20.581248
67.542366	2357.552822	20.586266
67.730054	2352.676452	20.591283
67.981891	2352.182687	20.596301
68.035778	2370.198986	20.601319
68.307449	2374.311995	20.606336
68.473481	2384.040852	20.611354
68.707201	2383.369060	20.616371
69.056628	2364.860447	20.621389
68.722938	2385.723176	20.626407
68.566284	2371.213751	20.631424
68.965062	2379.348128	20.636442
68.736233	2379.004495	20.641459
68.858440	2380.390726	20.646477
68.999322	2393.251168	20.651495
68.866914	2408.284797	20.656512
69.202663	2412.737281	20.661530
69.345158	2413.730211	20.666547
69.907404	2401.301799	20.671565
69.210117	2407.202455	20.676583
69.506527	2408.013067	20.681600
69.940381	2399.260009	20.686618
69.659051	2395.570511	20.691635
69.972733	2391.775067	20.696653
69.819839	2401.592476	20.701671
70.033177	2395.069702	20.706688
69.964989	2394.732392	20.711706
70.014164	2398.009397	20.716723
70.176692	2391.807984	20.721741
70.037540	2395.817387	20.726759
70.058725	2390.075709	20.731776
70.263444	2392.779504	20.736794
70.198081	2391.836101	20.741811
70.182020	2393.175161	20.746829
70.099947	2386.883380	20.751847
70.725696	2380.940404	20.756864
70.803220	2384.227510	20.761882
70.565344	2382.893932	20.766899
71.037151	2376.215024	20.771917
71.029713	2380.141203	20.776935
71.121989	2369.861432	20.781952
70.796882	2371.964609	20.786970
70.826131	2378.121859	20.791987
70.874589	2383.122879	20.797005
71.160948	2406.195449	20.802023
71.409673	2398.924755	20.807040
71.654562	2399.541805	20.812058
71.511452	2406.033388	20.817075
71.585356	2403.625721	20.822093
71.551965	2414.611029	20.827111
71.448042	2412.037753	20.832128
71.795228	2394.537525	20.837146
72.141054	2400.979933	20.842163
72.333098	2398.135411	20.847181
71.941307	2374.457743	20.852199
71.671085	2366.070332	20.857216
72.195190	2382.215198	20.862234
72.280428	2389.786701	20.867251
72.057529	2379.334938	20.872269
72.275003	2389.228235	20.877287
72.245714	2403.262923	20.882304
72.459064	2398.962548	20.887322
72.101548	2400.654683	20.892339
72.083152	2397.066587	20.897357
72.073293	2400.189121	20.902375
72.212708	2398.984591	20.907392
72.129076	2403.199472	20.912410
71.779856	2407.176379	20.917427
72.421631	2411.938659	20.922445
72.281621	2427.627259	20.927463
72.343304	2417.543283	20.932480
72.514252	2433.884991	20.937498
72.598450	2453.894151	20.942515
72.967701	2442.894297	20.947533
72.805868	2455.871266	20.952551
72.864888	2455.891735	20.957568
73.140015	2467.555803	20.962586
73.516527	2477.340774	20.967603
73.630980	2470.994791	20.972621
73.406372	2481.816046	20.977639
73.676265	2476.177391	20.982656
73.950564	2476.961871	20.987674
74.000598	2481.972103	20.992691
73.921591	2476.464141	20.997709
73.586464	2482.242096	21.002727
73.782153	2473.078573	21.007744
74.045769	2476.792137	21.012762
73.736427	2476.083502	21.017779
74.105294	2463.912641	21.022797
73.916157	2478.167745	21.027815
74.212896	2503.728853	21.032832
75.007561	2501.737062	21.037850
74.868521	2503.494919	21.042867
75.036387	2490.811162	21.047885
74.444411	2480.543885	21.052903
74.303300	2476.974447	21.057920
74.611131	2487.646935	21.062938
74.297400	2499.975066	21.067955
74.993723	2501.962211	21.072973
74.930052	2499.730896	21.077991
75.073325	2494.760506	21.083008
75.259389	2491.079846	21.088026
74.980488	2497.751466	21.093043
75.138478	2496.995786	21.098061
74.940562	2507.939276	21.103079
75.342810	2518.026999	21.108096
75.421203	2529.105053	21.113114
75.354749	2534.603068	21.118131
75.557442	2528.408103	21.123149
75.141460	2531.787722	21.128167
75.127076	2531.223037	21.133184
75.527985	2546.056687	21.138202
75.495562	2556.053573	21.143219
75.509617	2562.073318	21.148237
75.569871	2556.872218	21.153255
75.801736	2574.996846	21.158272
76.427806	2576.265212	21.163290
76.240459	2574.706382	21.168307
76.467511	2576.486538	21.173325
76.685609	2578.417073	21.178343
76.603010	2577.550643	21.183360
76.735293	2576.774953	21.188378
76.775327	2578.732079	21.193395
76.783293	2574.970102	21.198413
77.198762	2575.734323	21.203431
77.084512	2574.429149	21.208448
76.904702	2577.581642	21.213466
77.102128	2581.605056	21.218483
77.201944	2573.322626	21.223501
76.965900	2581.018605	21.228519
77.217310	2576.080840	21.233536
77.154178	2569.676270	21.238554
77.230581	2573.549535	21.243571
77.408326	2571.615462	21.248589
77.245344	2573.708196	21.253607
77.273936	2576.390241	21.258624
77.807400	2595.631891	21.263642
77.600936	2604.508054	21.268659
77.531928	2605.888498	21.273677
77.893408	2603.645709	21.278695
77.785961	2608.961768	21.283712
78.259282	2602.414813	21.288730
77.932576	2607.718847	21.293747
78.005729	2606.453207	21.298765
77.733149	2613.922355	21.303783
78.113048	2628.814026	21.308800
78.299583	2633.527629	21.313818
78.208024	2631.221535	21.318835
78.151802	2635.112039	21.323853
78.179225	2645.474378	21.328871
78.703218	2661.502209	21.333888
78.746966	2661.823774	21.338906
78.818843	2662.492548	21.343923
78.861908	2655.864976	21.348941
78.957258	2662.815084	21.353959
78.803263	2669.976476	21.358976
79.229594	2659.401407	21.363994
79.082287	2664.734557	21.369011
79.002984	2677.719611	21.374029
79.027626	2674.247717	21.379047
78.851232	2684.840334	21.384064
79.257965	2685.591096	21.389082
79.550053	2696.332579	21.394099
79.992678	2704.995925	21.399117
80.383129	2715.567775	21.404135
80.183662	2702.817665	21.409152
80.245894	2679.127064	21.414170
79.927186	2675.662056	21.419187
79.756861	2680.411652	21.424205
80.292087	2693.961562	21.429223
80.424814	2712.643600	21.434240
80.644921	2712.177315	21.439258
80.360296	2715.528153	21.444275
80.531730	2719.647413	21.449293
80.510117	2711.188055	21.454311
80.714412	2713.276908	21.459328
80.977373	2716.881174	21.464346
80.784315	2715.342997	21.469363
80.641879	2708.662151	21.474381
81.304595	2703.469547	21.479399
81.343992	2711.663348	21.484416
81.388117	2701.992510	21.489434
81.109209	2702.270162	21.494451
81.166234	2703.561279	21.499469
81.300553	2709.609291	21.504487
80.978843	2710.529828	21.509504
81.296324	2703.884329	21.514522
81.040220	2717.528973	21.519539
81.437900	2728.809956	21.524557
81.421151	2734.544445	21.529575
81.301122	2740.392723	21.534592
81.464698	2737.891665	21.539610
81.319292	2758.229605	21.544627
81.403098	2759.673645	21.549645
81.640780	2768.678517	21.554663
81.575686	2781.057172	21.559680
82.160387	2782.745323	21.564698
82.304722	2786.079338	21.569715
82.738107	2792.462795	21.574733
82.782332	2786.793414	21.579751
82.639939	2791.864298	21.584768
82.920284	2792.773767	21.589786
82.961922	2789.425729	21.594803
82.936034	2784.410219	21.599821
83.061888	2780.924100	21.604839
82.967731	2787.822485	21.609856
83.498127	2781.552339	21.614874
83.168242	2787.346044	21.619891
83.400060	2787.668446	21.624909
83.429446	2781.961446	21.629927
83.226694	2779.772836	21.634944
83.349128	2784.504562	21.639962
83.503947	2810.449622	21.644979
83.487495	2816.371526	21.649997
83.644114	2815.949200	21.655015
83.783927	2825.337094	21.660032
83.957173	2810.744714	21.665050
83.496990	2810.464360	21.670067
83.629706	2828.049483	21.675085
83.932335	2829.858452	21.680103
84.038963	2835.379664	21.685120
84.151906	2834.526161	21.690138
84.244048	2836.918563	21.695155
84.282202	2837.893182	21.700173
84.302385	2832.872121	21.705191
84.261943	2861.566996	21.710208
84.599837	2864.094470	21.715226
84.957541	2866.316916	21.720243
84.895218	2870.661365	21.725261
85.218230	2861.397822	21.730279
84.956945	2876.334286	21.735296
85.279544	2864.660905	21.740314
85.022116	2872.794632	21.745331
84.869236	2865.479956	21.750349
85.137300	2857.370146	21.755367
85.181591	2871.568261	21.760384
85.648658	2879.161171	21.765402
85.930877	2888.100986	21.770419
85.911836	2887.722949	21.775437
85.993941	2882.642428	21.780455
85.880656	2884.497506	21.785472
85.849321	2883.739615	21.790490
86.113069	2889.678876	21.795507
86.251217	2880.347783	21.800525
86.266382	2873.347666	21.805543
86.307888	2881.541981	21.810560
86.088603	2882.515059	21.815578
86.227742	2878.232002	21.820595
86.363868	2880.272711	21.825613
86.507080	2879.242330	21.830631
86.301831	2901.117776	21.835648
86.644502	2907.754674	21.840666
86.483509	2911.612017	21.845683
86.460994	2916.816750	21.850701
86.751655	2916.961319	21.855719
87.030952	2930.011111	21.860736
87.665460	2940.282955	21.865754
87.780801	2939.154179	21.870771
87.720607	2932.925369	21.875789
87.683437	2920.241765	21.880807
87.176846	2914.229677	21.885824
87.369948	2921.948331	21.890842
87.026416	2922.531610	21.895859
87.291126	2938.036351	21.900877
87.724419	2931.960781	21.905895
87.714627	2952.070958	21.910912
87.783784	2963.096560	21.915930
87.905773	2952.375797	21.920947
88.078676	2961.788027	21.925965
88.447026	2957.954724	21.930983
88.643691	2955.166015	21.936000
88.826400	2946.688040	21.941018
88.817834	2940.821315	21.946035
89.122315	2948.464184	21.951053
89.315531	2944.193102	21.956071
89.173083	2951.095899	21.961088
89.045988	2949.114022	21.966106
89.319977	2943.696590	21.971123
89.267921	2943.503774	21.976141
89.347901	2939.090658	21.981159
89.360949	2941.367477	21.986176
89.689376	2941.162986	21.991194
89.706620	2939.796647	21.996211
89.395107	2947.286014	22.001229
89.459159	2947.199302	22.006247
89.341517	2940.955924	22.011264
89.039425	2952.381451	22.016282
89.425807	2970.587155	22.021299
88.915604	2982.818612	22.026317
89.129689	2984.304917	22.031335
89.616388	3004.977416	22.036352
89.525463	3012.244709	22.041370
89.720307	3021.001903	22.046387
89.709830	3042.150314	22.051405
90.041192	3038.617881	22.056423
90.300975	3042.906369	22.061440
90.432067	3057.689892	22.066458
90.705435	3065.996553	22.071475
90.633203	3073.372503	22.076493
90.632789	3075.280708	22.081511
90.619507	3069.052465	22.086528
90.816119	3071.618370	22.091546
91.609355	3074.627772	22.096563
90.973377	3070.401154	22.101581
91.382266	3085.819894	22.106599
91.353177	3092.200066	22.111616
91.339095	3094.851713	22.116634
91.353787	3103.262594	22.121651
91.462952	3110.059320	22.126669
91.546114	3093.957401	22.131687
91.507189	3108.691363	22.136704
91.809891	3120.634714	22.141722
92.011357	3130.703701	22.146739
91.950225	3124.136324	22.151757
92.080157	3124.864471	22.156775
92.389863	3133.705206	22.161792
92.239021	3125.688339	22.166810
92.414475	3130.125982	22.171827
92.390358	3153.571055	22.176845
92.580712	3156.996493	22.181863
92.612550	3159.077957	22.186880
92.821586	3162.471053	22.191898
93.222204	3157.364191	22.196915
92.758755	3161.036390	22.201933
93.055439	3153.189295	22.206951
93.464569	3150.360189	22.211968
93.126705	3160.865822	22.216986
93.846250	3157.818110	22.222003
93.822526	3154.152786	22.227021
94.369708	3146.621879	22.232039
94.257249	3131.083489	22.237056
94.438153	3130.460101	22.242074
94.521039	3124.042086	22.247091
94.377014	3124.543914	22.252109
94.319230	3117.054517	22.257127
94.676465	3120.497804	22.262144
94.319641	3121.709480	22.267162
94.778476	3116.576112	22.272179
94.523815	3121.612795	22.277197
94.481593	3117.061491	22.282215
94.756069	3119.546326	22.287232
94.614184	3119.678420	22.292250
94.951870	3116.961589	22.297267
94.804619	3124.905656	22.302285
95.014736	3123.310920	22.307303
95.039179	3122.859267	22.312320
95.142654	3125.501791	22.317338
95.088658	3122.016503	22.322355
95.126701	3131.308618	22.327373
94.942529	3129.061644	22.332391
94.879840	3152.006924	22.337408
95.089369	3158.010713	22.342426
95.253021	3160.048314	22.347443
95.084482	3175.804768	22.352461
95.629470	3187.579836	22.357479
95.455177	3186.336882	22.362496
95.381119	3200.947792	22.367514
95.727071	3205.996520	22.372531
96.020173	3218.121157	22.377549
95.709054	3224.676532	22.382567
96.092456	3227.293923	22.387584
95.999859	3247.313139	22.392602
96.449721	3249.551345	22.397619
96.378294	3252.030132	22.402637
96.285273	3251.604914	22.407655
96.465786	3263.718173	22.412672
96.823261	3277.666859	22.417690
96.912062	3281.458628	22.422707
97.094531	3281.983246	22.427725
97.098218	3287.901875	22.432743
97.225084	3299.832191	22.437760
97.327798	3307.462572	22.442778
97.643600	3311.394999	22.447795
97.636291	3302.665096	22.452813
98.126236	3298.330448	22.457831
98.056201	3298.859763	22.462848
98.204497	3297.809583	22.467866
98.471507	3288.771185	22.472883
98.270687	3293.212739	22.477901
98.334602	3294.296380	22.482919
98.510509	3293.904602	22.487936
98.155359	3290.809561	22.492954
98.813602	3287.866843	22.497971
98.485451	3300.092535	22.502989
98.321952	3297.665576	22.508007
98.994822	3315.692618	22.513024
98.806106	3321.441051	22.518042
99.388859	3309.719592	22.523059
99.499122	3310.547204	22.528077
99.173677	3309.725515	22.533095
99.333625	3313.066417	22.538112
99.198574	3319.772000	22.543130
99.757616	3305.001189	22.548147
99.419431	3311.180842	22.553165
99.583481	3309.106478	22.558183
99.814946	3305.845499	22.563200
99.682151	3324.467463	22.568218
99.956691	3332.937880	22.573235
100.295057	3338.312431	22.578253
100.113458	3339.505897	22.583271
100.197378	3341.430392	22.588288
100.148839	3345.968715	22.593306
100.527354	3340.672629	22.598323
100.070663	3343.179675	22.603341
100.139766	3340.715984	22.608359
100.624083	3356.901759	22.613376
100.310870	3372.206727	22.618394
100.399713	3371.625103	22.623411
100.339641	3374.628064	22.628429
100.831496	3392.491696	22.633447
100.958934	3400.204516	22.638464
100.885645	3407.419350	22.643482
101.127136	3409.736619	22.648499
100.990450	3421.313695	22.653517
101.367333	3438.619795	22.658535
101.760908	3433.511690	22.663552
101.526621	3434.660640	22.668570
102.020638	3442.546123	22.673587
101.925807	3440.384598	22.678605
101.768084	3445.815093	22.683623
102.144853	3450.358504	22.688640
101.778650	3466.714616	22.693658
101.903953	3459.292903	22.698675
102.198391	3485.385259	22.703693
102.506507	3490.274386	22.708711
102.942987	3481.824290	22.713728
102.765480	3489.912341	22.718746
103.260884	3487.235354	22.723763
103.211670	3487.523256	22.728781
103.249034	3484.269526	22.733799
103.265262	3485.723644	22.738816
103.432376	3490.354201	22.743834
103.659350	3480.806692	22.748851
103.478191	3481.807136	22.753869
103.288543	3476.980146	22.758887
103.790871	3493.845808	22.763904
103.864924	3502.894906	22.768922
104.217171	3505.301889	22.773939
104.115034	3510.855191	22.778957
104.387262	3508.142428	22.783975
104.506365	3503.409777	22.788992
104.457149	3515.201901	22.794010
104.577653	3506.108163	22.799027
104.414138	3504.016684	22.804045
104.145849	3505.080108	22.809063
104.428455	3511.564532	22.814080
104.632066	3528.312899	22.819098
105.096901	3523.716292	22.824115
105.179264	3540.623285	22.829133
105.031959	3535.215657	22.834151
105.354006	3529.388906	22.839168
105.163206	3531.256560	22.844186
105.549499	3528.568344	22.849203
105.302877	3533.383255	22.854221
104.959636	3551.999822	22.859239
105.844104	3548.194463	22.864256
105.493111	3565.615247	22.869274
105.955692	3562.040514	22.874291
106.031982	3556.040874	22.879309
106.245091	3555.045723	22.884327
106.373260	3555.428443	22.889344
106.316711	3585.040209	22.894362
106.480808	3588.655327	22.899379
106.610724	3589.426028	22.904397
106.196901	3592.773207	22.909415
106.538055	3591.066963	22.914432
106.345669	3583.353905	22.919450
106.741259	3605.403765	22.924467
106.618817	3615.041076	22.929485
106.634555	3621.232633	22.934503
106.757616	3618.651748	22.939520
106.995220	3645.403085	22.944538
107.148215	3646.350191	22.949555
107.553220	3641.677961	22.954573
107.170474	3645.380538	22.959591
107.982331	3650.326698	22.964608
108.040795	3666.544844	22.969626
108.410700	3659.782848	22.974643
108.142354	3661.402331	22.979661
108.213106	3667.469486	22.984679
108.233645	3656.002462	22.989696
108.144515	3663.090963	22.994714
108.315884	3666.074779	22.999731
108.605850	3675.476820	23.004749
108.893739	3690.422292	23.009767
108.803323	3687.637778	23.014784
108.830503	3691.189756	23.019802
109.165906	3689.579000	23.024819
108.877938	3692.651806	23.029837
109.065640	3707.951560	23.034855
109.184275	3713.356822	23.039872
109.280055	3723.678223	23.044890
109.256555	3711.681570	23.049907
109.415382	3721.529057	23.054925
109.546534	3747.269432	23.059943
109.742772	3748.199680	23.064960
109.821156	3758.839125	23.069978
110.166497	3748.085045	23.074995
110.267248	3750.715540	23.080013
110.305302	3759.199164	23.085031
110.474215	3769.421422	23.090048
110.858705	3775.556124	23.095066
110.960526	3776.245016	23.100083
111.379501	3771.827109	23.105101
111.075347	3764.430833	23.110119
110.901029	3770.550280	23.115136
110.970109	3765.892285	23.120154
111.090418	3768.125632	23.125171
111.189451	3763.455415	23.130189
110.763527	3780.806583	23.135207
111.098317	3785.881040	23.140224
111.218238	3794.612918	23.145242
111.139283	3804.014486	23.150259
111.818432	3813.405810	23.155277
111.464329	3824.338393	23.160295
111.944480	3828.355404	23.165312
111.969405	3829.253593	23.170330
111.873537	3834.885481	23.175347
112.258692	3854.714876	23.180365
112.157381	3864.440865	23.185383
112.270089	3861.896371	23.190400
112.363936	3870.195642	23.195418
112.616654	3879.970425	23.200435
112.977396	3888.065643	23.205453
112.839140	3890.985230	23.210471
112.937169	3890.712328	23.215488
112.932324	3898.215728	23.220506
112.923437	3912.963406	23.225523
113.233740	3913.930030	23.230541
113.160419	3926.934776	23.235559
113.633520	3929.659776	23.240576
113.706149	3949.979988	23.245594
113.734386	3952.411083	23.250611
114.100218	3940.337273	23.255629
114.226011	3949.440766	23.260647
114.761891	3937.728459	23.265664
114.556648	3939.575007	23.270682
114.840557	3936.604986	23.275699
114.869071	3932.066524	23.280717
114.656846	3943.853045	23.285735
115.141742	3951.398530	23.290752
115.468454	3961.377270	23.295770
115.309139	3966.167106	23.300787
115.450761	3951.127797	23.305805
115.384584	3962.734137	23.310823
115.484406	3961.345677	23.315840
115.835546	3953.484127	23.320858
115.634770	3965.337223	23.325875
115.733448	3953.859737	23.330893
115.583939	3962.481164	23.335911
115.822211	3964.915634	23.340928
116.549564	3983.257024	23.345946
116.189226	3994.514499	23.350963
116.341591	3992.755518	23.355981
116.220122	3988.446741	23.360999
116.368612	3993.677646	23.366016
116.163543	3996.217266	23.371034
116.572793	4017.895975	23.376051
116.860303	4019.379246	23.381069
116.360025	4026.353306	23.386087
116.563691	4036.330347	23.391104
116.916036	4041.186074	23.396122
117.090596	4057.081489	23.401139
117.431897	4045.441839	23.406157
117.727322	4041.165544	23.411175
117.721869	4031.857602	23.416192
118.205724	4044.987458	23.421210
117.908744	4040.602428	23.426227
118.724214	4049.260102	23.431245
118.371413	4045.257179	23.436263
118.287065	4040.938874	23.441280
118.517494	4052.546415	23.446298
118.472542	4075.287580	23.451315
118.743361	4064.201876	23.456333
118.755706	4073.139014	23.461351
119.191775	4069.209565	23.466368
119.690960	4050.173175	23.471386
119.875689	4053.062626	23.476403
120.297573	4040.275795	23.481421
119.768097	4020.378504	23.486439
119.647828	4009.935624	23.491456
120.221575	3999.984958	23.496474
120.000140	4005.907007	23.501491
119.960261	4003.226401	23.506509
119.886492	4009.877665	23.511527
119.982625	4005.135413	23.516544
120.049394	4027.470643	23.521562
119.812099	4042.723863	23.526579
120.418067	4048.979014	23.531597
120.156348	4043.245064	23.536615
120.255998	4042.919112	23.541632
120.467879	4054.996099	23.546650
120.379286	4061.420731	23.551667
120.713477	4048.741078	23.556685
120.769291	4074.732761	23.561703
120.903062	4081.982504	23.566720
121.341977	4088.447459	23.571738
121.421570	4097.264392	23.576755
121.720259	4082.780865	23.581773
121.595481	4096.100952	23.586791
121.818825	4109.345620	23.591808
121.953400	4122.566136	23.596826
121.943083	4125.580399	23.601843
121.740342	4119.629168	23.606861
122.022046	4121.615942	23.611879
122.137660	4136.405495	23.616896
122.491368	4144.805284	23.621914
122.391560	4154.161802	23.626931
122.099109	4146.737348	23.631949
122.786984	4160.230859	23.636967
122.165994	4177.208702	23.641984
122.412471	4176.492123	23.647002
122.560110	4199.797465	23.652019
122.721837	4212.460494	23.657037
123.182652	4217.704879	23.662055
123.315562	4243.355186	23.667072
123.551555	4245.426211	23.672090
123.657106	4249.263388	23.677107
123.721448	4252.591739	23.682125
123.620593	4254.426729	23.687143
123.687858	4268.503234	23.692160
123.917695	4268.398334	23.697178
124.074344	4279.331097	23.702195
124.334570	4284.469696	23.707213
124.424647	4303.124703	23.712231
124.617945	4306.779088	23.717248
124.941680	4305.321496	23.722266
124.694432	4307.687242	23.727283
125.229456	4308.024650	23.732301
125.384721	4327.926345	23.737319
125.339910	4331.918488	23.742336
125.897515	4331.278524	23.747354
125.732344	4338.533162	23.752371
126.116681	4325.781682	23.757389
126.065104	4335.550629	23.762407
125.933934	4332.030258	23.767424
126.025799	4326.411229	23.772442
125.719009	4342.618648	23.777459
126.155345	4355.727769	23.782477
126.271475	4361.432981	23.787495
126.146733	4364.789045	23.792512
126.291559	4373.828086	23.797530
126.346352	4402.010081	23.802547
126.734743	4397.656320	23.807565
127.055418	4412.344816	23.812583
126.818061	4425.441102	23.817600
127.587724	4417.294917	23.822618
127.157426	4423.797177	23.827635
127.347355	4430.163972	23.832653
128.105040	4443.206263	23.837671
128.375949	4455.174196	23.842688
128.351449	4454.912839	23.847706
128.501134	4454.993382	23.852723
128.249622	4460.935721	23.857741
128.686528	4456.256211	23.862759
128.556548	4458.758614	23.867776
128.769643	4450.957503	23.872794
128.703121	4460.842508	23.877811
129.073667	4456.533534	23.882829
129.152565	4450.910383	23.887847
128.799098	4471.369685	23.892864
129.071618	4475.945446	23.897882
128.750011	4488.393041	23.902899
128.756291	4496.135833	23.907917
129.069661	4507.519980	23.912935
129.073044	4526.523281	23.917952
129.404322	4526.430920	23.922970
129.560145	4541.019413	23.927987
129.675998	4549.705148	23.933005
130.010953	4553.310890	23.938023
130.049663	4573.110790	23.943040
130.399257	4578.822529	23.948058
130.482050	4580.559912	23.953075
130.454722	4594.648985	23.958093
130.519764	4606.665714	23.963111
130.284336	4611.401054	23.968128
131.081731	4614.784184	23.973146
130.833307	4635.374552	23.978163
131.030132	4642.484570	23.983181
131.255090	4642.916888	23.988199
131.684594	4652.979264	23.993216
132.152650	4651.284238	23.998234
132.738010	4657.835383	24.003251
132.699096	4652.411151	24.008269
132.977749	4634.921774	24.013287
132.863382	4620.952795	24.018304
132.751627	4620.121965	24.023322
132.493952	4626.764057	24.028339
132.515949	4618.524616	24.033357
132.889742	4631.197309	24.038375
132.858840	4646.066803	24.043392
133.125734	4638.725810	24.048410
133.188778	4643.385576	24.053427
133.085449	4645.126518	24.058445
133.583123	4653.844523	24.063463
133.456708	4669.952829	24.068480
133.918223	4669.228509	24.073498
133.354068	4674.967752	24.078515
133.557944	4675.552549	24.083533
133.898666	4693.599523	24.088551
133.984966	4704.406803	24.093568
134.233400	4703.466964	24.098586
134.165936	4716.055478	24.103603
134.635168	4727.768292	24.108621
134.818358	4734.931886	24.113639
134.953287	4736.609152	24.118656
135.298290	4723.089844	24.123674
135.182249	4736.259318	24.128691
135.147470	4755.246593	24.133709
135.717058	4753.914585	24.138727
135.642156	4757.318897	24.143744
135.699254	4750.539965	24.148762
135.825013	4758.443561	24.153779
136.029535	4776.587229	24.158797
136.228511	4779.009660	24.163815
135.867461	4792.081769	24.168832
136.252669	4781.239818	24.173850
135.871336	4795.485061	24.178867
136.433585	4804.637888	24.183885
136.786011	4810.073550	24.188903
136.731684	4823.367204	24.193920
137.068894	4831.245615	24.198938
136.949331	4838.407596	24.203955
137.125515	4845.644905	24.208973
137.220736	4847.252588	24.213991
137.288996	4870.377188	24.219008
137.681139	4868.684915	24.224026
137.639405	4886.863048	24.229043
137.567552	4887.725115	24.234061
138.263913	4894.050966	24.239079
138.278612	4901.022977	24.244096
138.417727	4907.067074	24.249114
138.204079	4914.894244	24.254131
138.348283	4916.104436	24.259149
138.775947	4910.767115	24.264167
138.729343	4933.290039	24.269184
138.972030	4929.404561	24.274202
139.137854	4942.437670	24.279219
139.121082	4935.737485	24.284237
139.526661	4933.506510	24.289255
139.708219	4955.295642	24.294272
139.629201	4967.969828	24.299290
139.749118	4965.714567	24.304307
139.684059	4963.311431	24.309325
140.030955	4970.905483	24.314343
139.928076	4989.373045	24.319360
140.290546	4988.230905	24.324378
140.412121	4995.768289	24.329395
140.171253	5011.919404	24.334413
140.892283	5014.119264	24.339431
140.978768	5021.456310	24.344448
141.028545	5018.102468	24.349466
141.289295	5027.919121	24.354483
141.246230	5042.201114	24.359501
141.794628	5044.886627	24.364519
141.834646	5053.283178	24.369536
141.666121	5044.186121	24.374554
141.980942	5045.259954	24.379571
142.219219	5073.469976	24.384589
142.234347	5081.549443	24.389607
142.345070	5074.692653	24.394624
142.490085	5087.463219	24.399642
142.510021	5079.789432	24.404659
142.716567	5093.442663	24.409677
143.559586	5098.413884	24.414695
143.445108	5096.586315	24.419712
144.280466	5085.847366	24.424730
144.339421	5082.969259	24.429747
144.059290	5088.615850	24.434765
144.546195	5074.552850	24.439783
144.691867	5057.408746	24.444800
144.933785	5041.759678	24.449818
145.202778	5039.096049	24.454835
145.108654	5040.460530	24.459853
145.256056	5032.679848	24.464871
144.704560	5040.751670	24.469888
144.553453	5038.175022	24.474906
144.625737	5034.595986	24.479923
144.497508	5031.390017	24.484941
144.725664	5043.143606	24.489959
144.935189	5067.947197	24.494976
144.994723	5068.665451	24.499994
144.895108	5082.505058	24.505011
144.847877	5098.783750	24.510029
145.366427	5097.177695	24.515047
144.941453	5115.677777	24.520064
145.207492	5130.273125	24.525082
145.561377	5141.196303	24.530099
145.461227	5164.473077	24.535117
145.673948	5180.919960	24.540135
146.449109	5194.294639	24.545152
146.165595	5203.784876	24.550170
146.623808	5217.862946	24.555187
146.642197	5228.513664	24.560205
146.676831	5228.451676	24.565223
147.153346	5257.146560	24.570240
147.334760	5269.100521	24.575258
147.621335	5266.329868	24.580275
147.146007	5276.106659	24.585293
147.732915	5290.141465	24.590311
147.969316	5292.284238	24.595328
147.970682	5291.177200	24.600346
148.420617	5311.574685	24.605363
148.280065	5325.917755	24.610381
148.791103	5318.292783	24.615399
148.621350	5319.993198	24.620416
148.686265	5330.936900	24.625434
148.764687	5345.543341	24.630451
149.312419	5348.955258	24.635469
149.646093	5352.165992	24.640487
149.711963	5346.802328	24.645504
149.414319	5370.182573	24.650522
149.823868	5382.747344	24.655539
149.794070	5382.518386	24.660557
150.255516	5374.138631	24.665575
150.243314	5388.634619	24.670592
150.188836	5410.620011	24.675610
150.504541	5414.212712	24.680627
150.108057	5420.686734	24.685645
150.507730	5421.693274	24.690663
150.862736	5429.016773	24.695680
151.143921	5443.848479	24.700698
151.417266	5450.106078	24.705715
151.367427	5472.732720	24.710733
151.635483	5466.871200	24.715751
151.619196	5469.660678	24.720768
151.638718	5473.482180	24.725786
152.154449	5479.373716	24.730803
152.120138	5492.054833	24.735821
152.678514	5483.829332	24.740839
153.046112	5492.855243	24.745856
152.522841	5487.045874	24.750874
153.024120	5499.338228	24.755891
153.042025	5517.435967	24.760909
153.306164	5518.470474	24.765927
153.262075	5519.920153	24.770944
153.554749	5517.509958	24.775962
153.723295	5519.889673	24.780979
153.463743	5526.451328	24.785997
153.567734	5537.316007	24.791015
153.726715	5546.996829	24.796032
153.719424	5548.619795	24.801050
154.414681	5553.205323	24.806067
154.338217	5580.057882	24.811085
154.827286	5576.023675	24.816103
154.866640	5577.121925	24.821120
154.678122	5582.318970	24.826138
155.092204	5584.680234	24.831155
155.325333	5605.699727	24.836173
155.498451	5612.499172	24.841191
155.458438	5607.293779	24.846208
155.206477	5622.324172	24.851226
155.720413	5631.911904	24.856243
155.511704	5655.872814	24.861261
156.198003	5650.392453	24.866279
156.356889	5647.278924	24.871296
156.089355	5664.968902	24.876314
156.421532	5676.540502	24.881331
156.234614	5679.789346	24.886349
156.579182	5699.431093	24.891367
156.667764	5718.466113	24.896384
156.649903	5712.294329	24.901402
156.699835	5727.088749	24.906419
156.928299	5746.711073	24.911437
157.054684	5754.170012	24.916455
157.528123	5763.283485	24.921472
157.743020	5763.834141	24.926490
158.199116	5783.566363	24.931507
158.240829	5796.912109	24.936525
158.512083	5784.304883	24.941543
159.133548	5786.150134	24.946560
159.082138	5784.946557	24.951578
159.299942	5787.007516	24.956595
159.549665	5812.138574	24.961613
159.373820	5812.987009	24.966631
159.858854	5810.454787	24.971648
159.860117	5807.425749	24.976666
160.487360	5807.235392	24.981683
160.485117	5808.560556	24.986701
160.321578	5807.860633	24.991719
160.446770	5809.460914	24.996736
160.450997	5800.503163	25.001754
160.718343	5798.774688	25.006771
160.764601	5816.581185	25.011789
160.955461	5835.820156	25.016807
160.977952	5824.118860	25.021824
160.782316	5842.645847	25.026842
161.133895	5849.443946	25.031859
161.596871	5866.597742	25.036877
161.503445	5871.524153	25.041895
161.751976	5865.547680	25.046912
161.478358	5879.340612	25.051930
162.115333	5885.667596	25.056947
162.045940	5893.173552	25.061965
162.158739	5892.459337	25.066983
162.867347	5889.653255	25.072000
163.260216	5908.525276	25.077018
163.081531	5904.241537	25.082035
163.310920	5908.733737	25.087053
163.377214	5914.242463	25.092071
163.208282	5907.485242	25.097088
163.292683	5909.689604	25.102106
163.923613	5897.380613	25.107123
163.734412	5913.185071	25.112141
163.715412	5925.835552	25.117159
164.549607	5925.001612	25.122176
164.351592	5930.667505	25.127194
164.286779	5926.598189	25.132211
164.770689	5946.244714	25.137229
164.606049	5962.068641	25.142247
164.604040	5962.400483	25.147264
164.794222	5971.806034	25.152282
164.874667	5991.989675	25.157299
165.297541	5993.372740	25.162317
165.294204	6005.144670	25.167335
165.915101	6016.358245	25.172352
165.802641	6020.557760	25.177370
165.920363	6022.935235	25.182387
166.253441	6048.992902	25.187405
166.938544	6057.696100	25.192423
166.982747	6051.612009	25.197440
166.962221	6057.306600	25.202458
167.143227	6050.095477	25.207475
167.336266	6045.908672	25.212493
167.530562	6067.304868	25.217511
167.819149	6074.959863	25.222528
167.723242	6083.960801	25.227546
167.554893	6081.589380	25.232563
167.842314	6086.377314	25.237581
168.038258	6100.162413	25.242599
168.051183	6104.873737	25.247616
168.009555	6113.135966	25.252634
168.127119	6118.153106	25.257651
168.371944	6134.744352	25.262669
168.477007	6155.826700	25.267687
168.850399	6173.546797	25.272704
168.665045	6183.194084	25.277722
168.770558	6199.439052	25.282739
169.259591	6213.261444	25.287757
169.293560	6228.757771	25.292775
169.483384	6233.760198	25.297792
169.858776	6246.215716	25.302810
170.308742	6259.308328	25.307827
170.822944	6269.361945	25.312845
170.883190	6277.006554	25.317863
171.419026	6260.358283	25.322880
171.102258	6270.308577	25.327898
171.282445	6266.264132	25.332915
171.455081	6263.912215	25.337933
171.188455	6263.092878	25.342951
171.599019	6271.805447	25.347968
171.644267	6294.823419	25.352986
172.150824	6293.294930	25.358003
172.152810	6288.850930	25.363021
172.043655	6296.666376	25.368039
171.883938	6320.682903	25.373056
171.657196	6322.238011	25.378074
171.961746	6335.602958	25.383091
172.450594	6352.437756	25.388109
172.494763	6375.812081	25.393127
172.964477	6389.677325	25.398144
172.705852	6405.977046	25.403162
172.615326	6417.849300	25.408179
173.192570	6433.877366	25.413197
173.168461	6463.698473	25.418215
173.534526	6467.764874	25.423232
173.794837	6489.352766	25.428250
174.014043	6503.702181	25.433267
174.272948	6512.719736	25.438285
174.738982	6528.332921	25.443303
175.318637	6530.012919	25.448320
175.539400	6547.599687	25.453338
175.837971	6535.195938	25.458355
176.248271	6535.854919	25.463373
176.207296	6540.728431	25.468391
175.989362	6536.440221	25.473408
176.159403	6532.593594	25.478426
176.091853	6537.298359	25.483443
176.376513	6547.251284	25.488461
176.310935	6563.351862	25.493479
176.602637	6559.918415	25.498496
176.512874	6587.890380	25.503514
176.532919	6597.317588	25.508531
176.977227	6608.942332	25.513549
177.077596	6636.665163	25.518567
177.822336	6630.352059	25.523584
177.873358	6638.071681	25.528602
177.946405	6645.503158	25.533619
178.541505	6651.287002	25.538637
178.551185	6655.163254	25.543655
179.029395	6646.592484	25.548672
179.092968	6648.402711	25.553690
179.421924	6646.385515	25.558707
179.541204	6647.697008	25.563725
179.558365	6655.900600	25.568743
179.785808	6670.088054	25.573760
179.767280	6681.863087	25.578778
179.721791	6680.628492	25.583795
179.587441	6687.615807	25.588813
179.593644	6695.321082	25.593831
179.445904	6717.481022	25.598848
179.683377	6727.019919	25.603866
179.880622	6739.496909	25.608883
180.110381	6758.965074	25.613901
180.102776	6781.679284	25.618919
180.523208	6796.731011	25.623936
180.552903	6820.624440	25.628954
180.929100	6828.063905	25.633971
181.531699	6838.484001	25.638989
181.472055	6850.864894	25.644007
181.981697	6850.140906	25.649024
182.191578	6864.572594	25.654042
182.489648	6863.651699	25.659059
182.552701	6860.817472	25.664077
182.691268	6875.262970	25.669095
182.864883	6883.431983	25.674112
183.243139	6890.955414	25.679130
183.196119	6888.683599	25.684148
183.740656	6905.099019	25.689165
183.743848	6926.477922	25.694183
184.188746	6925.889494	25.699200
184.091406	6927.458713	25.704218
184.007729	6932.301064	25.709236
184.366887	6931.526456	25.714253
184.327463	6948.110556	25.719271
184.795373	6954.052596	25.724288
184.819655	6969.048715	25.729306
184.990752	6986.471175	25.734324
185.283542	6973.740372	25.739341
185.092465	6989.155487	25.744359
185.362310	6994.728163	25.749376
185.719885	7011.060729	25.754394
185.845961	7028.452352	25.759412
186.143839	7047.812298	25.764429
186.123183	7053.540352	25.769447
186.274263	7063.894622	25.774464
186.397794	7079.708068	25.779482
186.704857	7079.879030	25.784500
187.134345	7092.262918	25.789517
187.169287	7115.720257	25.794535
187.574986	7106.931647	25.799552
187.565760	7130.824334	25.804570
187.500963	7146.854465	25.809588
187.945822	7143.463177	25.814605
187.797685	7163.338501	25.819623
188.536158	7182.894865	25.824640
188.498405	7186.079053	25.829658
188.430707	7203.946806	25.834676
188.860866	7210.046665	25.839693
189.027995	7216.066358	25.844711
188.954402	7238.389979	25.849728
189.248198	7240.608262	25.854746
189.207336	7264.324596	25.859764
189.995621	7266.916601	25.864781
189.930035	7277.427103	25.869799
190.036813	7297.213205	25.874816
190.539745	7300.941253	25.879834
190.631161	7315.872620	25.884852
190.850178	7311.684185	25.889869
191.001659	7329.587770	25.894887
191.011177	7329.875913	25.899904
191.040842	7329.365740	25.904922
190.855921	7356.540801	25.909940
191.571915	7350.241803	25.914957
191.693362	7369.858473	25.919975
191.750279	7388.793774	25.924992
191.947125	7394.225488	25.930010
192.397629	7402.437897	25.935028
192.813167	7406.571688	25.940045
192.942918	7415.686732	25.945063
193.228741	7411.775146	25.950080
193.457813	7419.687566	25.955098
193.515209	7439.497277	25.960116
193.793590	7438.550578	25.965133
193.810983	7446.405550	25.970151
193.798249	7463.625283	25.975168
193.986900	7472.367098	25.980186
194.164495	7480.278130	25.985204
194.747431	7497.387915	25.990221
194.996807	7507.625576	25.995239
194.986984	7509.247598	26.000256
194.913272	7518.802498	26.005274
195.139575	7542.103189	26.010292
195.234717	7554.748783	26.015309
195.393176	7579.669811	26.020327
195.637760	7586.301081	26.025344
195.870494	7595.863368	26.030362
195.881619	7616.252373	26.035380
196.087013	7626.161264	26.040397
196.406867	7646.298864	26.045415
196.632991	7662.200862	26.050432
196.826734	7672.662443	26.055450
196.834598	7690.799814	26.060468
197.378996	7697.585350	26.065485
197.535277	7707.907635	26.070503
197.437759	7728.755780	26.075520
197.910606	7733.507702	26.080538
197.863752	7756.552228	26.085556
198.561281	7757.336134	26.090573
198.605591	7774.438494	26.095591
198.888250	7794.035139	26.100608
199.460428	7795.663780	26.105626
199.424643	7805.771682	26.110644
199.788877	7796.876364	26.115661
200.290074	7806.475478	26.120679
200.323042	7815.669576	26.125696
200.278398	7815.703100	26.130714
200.640562	7826.411641	26.135732
200.950815	7819.230354	26.140749
200.752950	7832.118615	26.145767
200.821833	7858.023632	26.150784
201.310458	7848.153728	26.155802
200.913714	7859.636008	26.160820
201.255997	7857.312292	26.165837
201.423939	7880.180735	26.170855
201.485090	7889.669409	26.175872
201.874733	7903.982200	26.180890
201.995662	7918.643581	26.185908
202.293223	7916.790749	26.190925
202.686449	7940.061830	26.195943
202.745754	7952.188417	26.200960
202.940718	7957.774267	26.205978
202.873439	7978.996486	26.210996
203.660932	7989.599141	26.216013
203.601099	7996.181923	26.221031
203.670411	8002.897768	26.226048
203.780678	8011.177480	26.231066
203.463759	8022.384640	26.236084
203.753282	8044.383223	26.241101
204.045878	8065.242926	26.246119
204.319907	8092.016770	26.251136
204.698936	8092.050938	26.256154
204.688218	8117.245232	26.261172
205.314449	8122.999861	26.266189
205.517506	8140.625291	26.271207
205.589968	8160.790975	26.276224
206.179085	8170.196405	26.281242
206.333785	8190.119563	26.286260
206.608419	8187.530874	26.291277
207.005566	8194.647536	26.296295
206.907945	8205.734513	26.301312
207.198550	8201.646236	26.306330
207.265357	8222.709500	26.311348
207.476515	8237.334434	26.316365
207.943501	8238.222487	26.321383
207.901514	8242.061498	26.326400
208.472575	8250.543598	26.331418
208.902976	8268.503625	26.336436
208.643500	8263.792708	26.341453
209.013141	8267.357122	26.346471
208.924268	8281.812148	26.351488
208.915440	8294.711705	26.356506
209.288079	8301.087339	26.361524
209.330462	8319.994717	26.366541
209.760544	8323.736284	26.371559
209.275725	8341.876119	26.376576
209.619051	8346.949800	26.381594
209.905556	8379.611741	26.386612
210.216787	8391.594635	26.391629
210.469006	8411.628192	26.396647
210.867465	8427.801571	26.401664
210.941091	8437.417633	26.406682
211.498955	8450.404528	26.411700
212.671525	8433.580276	26.416717
213.642200	8412.077878	26.421735
213.607429	8415.371305	26.426752
213.900781	8401.064420	26.431770
213.890224	8386.052541	26.436788
213.789945	8372.706545	26.441805
214.028063	8372.233088	26.446823
214.019676	8368.639564	26.451840
214.115406	8365.866437	26.456858
214.077804	8368.813699	26.461876
214.104247	8366.637013	26.466893
214.521848	8363.251724	26.471911
214.560382	8368.172035	26.476928
214.389794	8364.804846	26.481946
214.570666	8379.773866	26.486964
214.141367	8394.017910	26.491981
214.757873	8400.334452	26.496999
214.594872	8427.513078	26.502016
214.951915	8440.112903	26.507034
215.157210	8462.677187	26.512052
215.036582	8479.044376	26.517069
215.477142	8498.583304	26.522087
215.626211	8533.605818	26.527104
215.894713	8546.084607	26.532122
215.884746	8575.258039	26.537140
216.168400	8594.833432	26.542157
216.395129	8610.022490	26.547175
216.783357	8632.446934	26.552192
216.980185	8649.620985	26.557210
217.451773	8669.153226	26.562228
217.550763	8687.499058	26.567245
218.184821	8702.251250	26.572263
218.386215	8722.579104	26.577280
218.850140	8717.121662	26.582298
218.660891	8749.055215	26.587316
218.818906	8751.345833	26.592333
219.246664	8766.958316	26.597351
219.138332	8790.266967	26.602368
219.530564	8783.936256	26.607386
219.825744	8802.202895	26.612404
219.668101	8815.341094	26.617421
220.189883	8835.885192	26.622439
219.964203	8852.038351	26.627456
220.691213	8867.281348	26.632474
220.810137	8875.411905	26.637492
220.877181	8896.606005	26.642509
221.542113	8908.238730	26.647527
221.434927	8933.646221	26.652544
221.870442	8936.877265	26.657562
221.983411	8958.186478	26.662580
221.889286	8970.359039	26.667597
221.996438	8991.371485	26.672615
222.620892	9012.867270	26.677632
222.746403	9034.517938	26.682650
222.954796	9045.370255	26.687668
222.969656	9070.337902	26.692685
223.337690	9085.815967	26.697703
223.539864	9100.818247	26.702720
223.762646	9116.567050	26.707738
223.990317	9132.423755	26.712756
223.819636	9150.603615	26.717773
224.371291	9161.234872	26.722791
224.555552	9175.723455	26.727808
226.225023	9157.355743	26.732826
226.591875	9155.932888	26.737844
226.819954	9147.197258	26.742861
227.269566	9128.129480	26.747879
227.089515	9142.916837	26.752896
227.525029	9138.177927	26.757914
227.777590	9141.268619	26.762932
227.368712	9140.188301	26.767949
227.795080	9136.678446	26.772967
227.584043	9138.624266	26.777984
227.602686	9142.194680	26.783002
227.846821	9146.860962	26.788020
227.841412	9165.452136	26.793037
228.030586	9167.386087	26.798055
228.359517	9182.018481	26.803072
228.421743	9194.531556	26.808090
228.534271	9214.120490	26.813108
228.623435	9237.774109	26.818125
228.820307	9245.152475	26.823143
228.882319	9274.295922	26.828160
229.282045	9286.059471	26.833178
229.565595	9295.915816	26.838196
229.169363	9317.873746	26.843213
229.833098	9330.252308	26.848231
230.219548	9362.134089	26.853248
230.270541	9380.797781	26.858266
230.597055	9399.579722	26.863284
230.640225	9413.309557	26.868301
230.973612	9437.345482	26.873319
231.067020	9467.681466	26.878336
231.460601	9478.852149	26.883354
232.064574	9496.902768	26.888372
232.243974	9513.013940	26.893389
232.927266	9529.831364	26.898407
233.213610	9534.826162	26.903424
233.188659	9549.773244	26.908442
233.858360	9561.769629	26.913460
233.173227	9582.754767	26.918477
233.622972	9591.649954	26.923495
233.646596	9605.419544	26.928512
233.922443	9625.841351	26.933530
234.274361	9645.151833	26.938548
234.010294	9671.797564	26.943565
234.825645	9687.418567	26.948583
234.963246	9708.352664	26.953600
235.295644	9725.109103	26.958618
235.911519	9739.536817	26.963636
235.772923	9750.332477	26.968653
236.245658	9759.097754	26.973671
236.312291	9775.809980	26.978688
236.731723	9788.599504	26.983706
236.640334	9800.770644	26.988724
236.866579	9816.257957	26.993741
237.378713	9821.447359	26.998759
237.487696	9844.178207	27.003776
237.398853	9841.941506	27.008794
237.766835	9862.664553	27.013812
237.884144	9875.978670	27.018829
238.644415	9897.383023	27.023847
238.524789	9909.330594	27.028864
238.477403	9923.575910	27.033882
239.101989	9935.055567	27.038900
238.778555	9957.632201	27.043917
239.213866	9968.595946	27.048935
239.438936	9984.269565	27.053952
239.474088	10003.437795	27.058970
239.952563	10026.863528	27.063988
239.819068	10050.230306	27.069005
240.445484	10058.304414	27.074023
240.754518	10080.741295	27.079040
240.662625	10108.541666	27.084058
241.270780	10122.706310	27.089076
241.252506	10145.921107	27.094093
241.703577	10164.832291	27.099111
241.799657	10189.850775	27.104128
241.994800	10212.983388	27.109146
242.760266	10227.505663	27.114164
242.789036	10251.547735	27.119181
242.868028	10268.883954	27.124199
243.214444	10294.483720	27.129216
243.636008	10308.387405	27.134234
244.148010	10312.369900	27.139252
244.191105	10337.091981	27.144269
244.627947	10342.559199	27.149287
244.826331	10356.628822	27.154304
245.464634	10353.756843	27.159322
246.174763	10349.022519	27.164340
246.434739	10358.349346	27.169357
246.623522	10346.200239	27.174375
246.497741	10353.234152	27.179392
246.675409	10353.449404	27.184410
247.301251	10364.511556	27.189428
247.151361	10379.135708	27.194445
247.170080	10375.240046	27.199463
247.200928	10379.826634	27.204480
247.351496	10394.561612	27.209498
247.425779	10408.004880	27.214516
247.334772	10436.538427	27.219533
247.719218	10446.899788	27.224551
247.732859	10474.361222	27.229568
248.097435	10510.034206	27.234586
248.266035	10521.912338	27.239604
248.231955	10558.042995	27.244621
248.478112	10577.440479	27.249639
249.058823	10604.931005	27.254656
249.218734	10622.620908	27.259674
249.845977	10644.685704	27.264692
249.996698	10655.355156	27.269709
250.319300	10671.491787	27.274727
250.663629	10689.566183	27.279744
250.635803	10705.829098	27.284762
250.957922	10721.100707	27.289780
251.489343	10746.858581	27.294797
251.280760	10769.662491	27.299815
251.558816	10783.745619	27.304832
251.792496	10801.910020	27.309850
252.194138	10813.575074	27.314868
252.508576	10835.692170	27.319885
252.834582	10858.510158	27.324903
253.466918	10870.321667	27.329920
253.610275	10882.081470	27.334938
253.863639	10892.170892	27.339956
253.899798	10901.504876	27.344973
254.116510	10923.158194	27.349991
254.620525	10930.338128	27.355008
254.672304	10957.098870	27.360026
254.974685	10968.231061	27.365044
254.913725	10987.368071	27.370061
254.971357	11007.179750	27.375079
255.318206	11019.530407	27.380096
255.457498	11047.685155	27.385114
255.693002	11071.568508	27.390132
255.681801	11100.855430	27.395149
255.971649	11123.465664	27.400167
256.529949	11151.536166	27.405184
256.627684	11185.254955	27.410202
257.333296	11205.664975	27.415220
257.451339	11233.399763	27.420237
257.927702	11238.841602	27.425255
258.212112	11273.535593	27.430272
258.522732	11287.544236	27.435290
259.234482	11295.148897	27.440308
259.440076	11304.398914	27.445325
259.858080	11317.204076	27.450343
260.207450	11318.396934	27.455360
260.390836	11333.634589	27.460378
260.757722	11333.552667	27.465396
260.968356	11348.279790	27.470413
261.135529	11365.539026	27.475431
261.337721	11374.030064	27.480448
261.048357	11376.583699	27.485466
261.809503	11400.185176	27.490484
261.920827	11412.040680	27.495501
261.962040	11424.913662	27.500519
262.142339	11427.722481	27.505536
262.223428	11453.410525	27.510554
262.639950	11465.754307	27.515572
262.743796	11486.863531	27.520589
263.110949	11506.213018	27.525607
263.570388	11524.848563	27.530624
263.600252	11541.167037	27.535642
263.864644	11561.913163	27.540660
264.378316	11582.009845	27.545677
264.379509	11597.635140	27.550695
264.835382	11582.824820	27.555712
265.153030	11601.075007	27.560730
265.365941	11613.001500	27.565748
266.090196	11627.927667	27.570765
266.187120	11639.541532	27.575783
266.482270	11638.316725	27.580800
266.524644	11659.506051	27.585818
267.194514	11653.703454	27.590836
267.812589	11666.258694	27.595853
268.033076	11671.987236	27.600871
268.451249	11666.180496	27.605888
268.273891	11671.546989	27.610906
268.539897	11669.072706	27.615924
268.696123	11690.136969	27.620941
268.847882	11705.498590	27.625959
269.091898	11707.081464	27.630976
268.585476	11732.752448	27.635994
268.662400	11731.336522	27.641012
268.758143	11761.211473	27.646029
269.051896	11794.092600	27.651047
269.825400	11818.534140	27.656064
269.657241	11849.935906	27.661082
270.201310	11879.171603	27.666100
270.427484	11916.266139	27.671117
270.596044	11925.201354	27.676135
271.237198	11949.341121	27.681152
271.115694	11965.700146	27.686170
271.775680	11994.090361	27.691188
272.256757	12013.239685	27.696205
272.548213	12031.061443	27.701223
272.551665	12044.225065	27.706240
273.112272	12065.207893	27.711258
273.327286	12077.161157	27.716276
273.297436	12099.047418	27.721293
273.200569	12120.770258	27.726311
273.852870	12147.705825	27.731328
274.191017	12176.821325	27.736346
274.599816	12187.959753	27.741364
274.885134	12216.846401	27.746381
274.726060	12237.514668	27.751399
275.182353	12261.127094	27.756416
275.309972	12285.408961	27.761434
275.568804	12307.573834	27.766452
276.282417	12332.776601	27.771469
276.644874	12358.488762	27.776487
277.079590	12361.230497	27.781504
276.872500	12390.843294	27.786522
277.469775	12411.941638	27.791540
277.646110	12425.099575	27.796557
277.674540	12451.430203	27.801575
278.158377	12470.423562	27.806592
278.336543	12493.122607	27.811610
278.837421	12500.369972	27.816628
279.070718	12525.571830	27.821645
279.423144	12539.946332	27.826663
279.842296	12547.251856	27.831680
279.904124	12569.517044	27.836698
280.218468	12566.912988	27.841716
280.639614	12592.629642	27.846733
280.490682	12596.804795	27.851751
280.869539	12623.269492	27.856768
281.088461	12633.794586	27.861786
281.228573	12657.545308	27.866804
282.053587	12671.195893	27.871821
281.913018	12703.155641	27.876839
282.671712	12708.871106	27.881856
282.481629	12738.773187	27.886874
282.696865	12748.810405	27.891892
283.079587	12768.306872	27.896909
283.246091	12792.373208	27.901927
283.383286	12813.029246	27.906944
283.648995	12839.668141	27.911962
284.161505	12865.137881	27.916980
284.357784	12880.713626	27.921997
284.717238	12905.085914	27.927015
285.124748	12919.497016	27.932032
285.351361	12933.571907	27.937050
285.766298	12956.402805	27.942068
286.347140	12967.425595	27.947085
286.163907	12995.098375	27.952103
286.576727	13010.585119	27.957120
286.801878	13032.474625	27.962138
286.994924	13048.795002	27.967156
287.583323	13069.965067	27.972173
287.660613	13089.758561	27.977191
287.902490	13089.825729	27.982208
288.800669	13121.409666	27.987226
289.185167	13131.041419	27.992244
289.718622	13133.758484	27.997261
289.790946	13151.002763	28.002279
290.054761	13164.054886	28.007296
289.940348	13173.168524	28.012314
290.047826	13193.762362	28.017332
290.493977	13208.818030	28.022349
290.370681	13231.391664	28.027367
291.196583	13254.639562	28.032384
291.021895	13269.517993	28.037402
291.146540	13297.846191	28.042420
291.638579	13308.151535	28.047437
291.406052	13338.377204	28.052455
291.940322	13362.899889	28.057472
292.551991	13397.138805	28.062490
292.856160	13413.985841	28.067508
293.310828	13432.941186	28.072525
293.649691	13461.195124	28.077543
294.182461	13468.651811	28.082560
294.663882	13483.383308	28.087578
294.307109	13504.340808	28.092596
294.690550	13515.434053	28.097613
294.994134	13539.411792	28.102631
294.914944	13544.571354	28.107648
294.943785	13570.446621	28.112666
295.356694	13605.503383	28.117684
295.897010	13613.690178	28.122701
295.632690	13646.817253	28.127719
296.247465	13676.690268	28.132736
296.490861	13697.346554	28.137754
296.661305	13721.062090	28.142772
297.250065	13742.697931	28.147789
297.724427	13777.574301	28.152807
297.769712	13792.130214	28.157824
297.890676	13817.569243	28.162842
297.799705	13856.730563	28.167860
298.812065	13877.088205	28.172877
298.949375	13910.388128	28.177895
299.649685	13915.598619	28.182912
300.026061	13946.052038	28.187930
299.944712	13964.395311	28.192948
300.453704	13987.277724	28.197965
300.616703	14016.522655	28.202983
301.158134	14032.163278	28.208000
301.518715	14058.884037	28.213018
301.295687	14080.776094	28.218036
301.935773	14095.362732	28.223053
302.273482	14117.875904	28.228071
302.594119	14138.908826	28.233088
302.950505	14160.635483	28.238106
303.468631	14189.045938	28.243124
303.756395	14195.435301	28.248141
303.838389	14222.027536	28.253159
303.903757	14237.346438	28.258176
304.419213	14257.171843	28.263194
304.702914	14294.990101	28.268212
305.335379	14303.070029	28.273229
305.616105	14342.039544	28.278247
305.765721	14357.022568	28.283264
305.964270	14376.877213	28.288282
306.134524	14401.055594	28.293300
306.230765	14422.699508	28.298317
306.397693	14456.876569	28.303335
306.739247	14476.618554	28.308352
307.141236	14512.434133	28.313370
307.417159	14539.173332	28.318388
307.987967	14560.078797	28.323405
308.203390	14591.955969	28.328423
308.615529	14608.560320	28.333440
309.594896	14614.071561	28.338458
310.268526	14638.662112	28.343476
310.689327	14637.670911	28.348493
310.743365	14648.408401	28.353511
311.207942	14649.868649	28.358528
311.739054	14672.398296	28.363546
311.313600	14674.528099	28.368564
311.617090	14675.342897	28.373581
312.064716	14690.174269	28.378599
312.152832	14706.060311	28.383616
312.818692	14714.289193	28.388634
312.908588	14727.477975	28.393652
312.906802	14747.463552	28.398669
312.811023	14759.191462	28.403687
313.206620	14783.921304	28.408704
313.642953	14797.476358	28.413722
313.472531	14823.452365	28.418740
313.701086	14850.479186	28.423757
313.789879	14880.535957	28.428775
314.233051	14912.682087	28.433792
314.519155	14944.007161	28.438810
315.002970	14975.035169	28.443828
315.014649	15002.610123	28.448845
315.202649	15041.984946	28.453863
315.417798	15082.450732	28.458880
316.041936	15110.888741	28.463898
316.697862	15146.189283	28.468916
317.169286	15174.729238	28.473933
317.549675	15206.204160	28.478951
317.703779	15225.602431	28.483968
318.456918	15249.261279	28.488986
318.454503	15276.757136	28.494004
318.871767	15292.833233	28.499021
319.107804	15321.814168	28.504039
319.133331	15340.884668	28.509056
319.664886	15368.221379	28.514074
319.847000	15404.207408	28.519092
320.365877	15425.803843	28.524109
320.405145	15455.086709	28.529127
321.026343	15486.088977	28.534144
321.780543	15499.046295	28.539162
321.705612	15531.164196	28.544180
322.079465	15550.165781	28.549197
322.432102	15577.158333	28.554215
322.965521	15603.768421	28.559232
323.328427	15617.763922	28.564250
323.399759	15646.294443	28.569268
324.229943	15664.749775	28.574285
324.626153	15684.434970	28.579303
324.538048	15701.003199	28.584320
324.936844	15722.369962	28.589338
325.414811	15729.036289	28.594356
326.169751	15751.300475	28.599373
326.200593	15769.197747	28.604391
326.767743	15782.948727	28.609408
326.909428	15796.224064	28.614426
327.413725	15807.313907	28.619444
327.690803	15817.640331	28.624461
327.665604	15820.953308	28.629479
328.068509	15845.224762	28.634496
328.428201	15863.469325	28.639514
328.283400	15894.113389	28.644532
328.847144	15909.676307	28.649549
328.812778	15929.438740	28.654567
328.916134	15947.043181	28.659584
329.723008	15963.426759	28.664602
330.044031	15993.556090	28.669620
330.319516	16013.981195	28.674637
330.485971	16037.719652	28.679655
330.807590	16060.389559	28.684672
331.201640	16076.334828	28.689690
331.258562	16116.626898	28.694708
331.459712	16135.148002	28.699725
331.522061	16164.978322	28.704743
332.011289	16197.481622	28.709760
332.156333	16220.870896	28.714778
332.636741	16262.422798	28.719796
332.884105	16289.149220	28.724813
333.545530	16323.581152	28.729831
333.790388	16354.908075	28.734848
334.430061	16375.912809	28.739866
334.214548	16405.070758	28.744884
334.901641	16430.694222	28.749901
335.081836	16461.777048	28.754919
335.419844	16504.581993	28.759936
335.777965	16523.311513	28.764954
335.682767	16561.816259	28.769972
336.213296	16597.029454	28.774989
336.996244	16634.042321	28.780007
337.204774	16665.710259	28.785024
337.491188	16690.390716	28.790042
337.432226	16720.703142	28.795060
337.683261	16757.397567	28.800077
338.117562	16795.886198	28.805095
338.448358	16838.429967	28.810112
339.110771	16863.561743	28.815130
339.587088	16904.625668	28.820148
339.882526	16930.037989	28.825165
340.629912	16950.091721	28.830183
340.978180	16980.249696	28.835200
341.648574	17004.022975	28.840218
341.717878	17023.482016	28.845236
342.283282	17051.958643	28.850253
342.516124	17068.556778	28.855271
342.911696	17096.636938	28.860288
342.967847	17119.068439	28.865306
343.418553	17148.722029	28.870324
343.565245	17166.432261	28.875341
344.034307	17188.912904	28.880359
344.010243	17227.938269	28.885376
344.520976	17251.114971	28.890394
345.084148	17283.787437	28.895412
345.295369	17315.553889	28.900429
345.510961	17337.018760	28.905447
346.092157	17366.065489	28.910464
346.720632	17379.793098	28.915482
346.613435	17400.315440	28.920500
347.109922	17416.452537	28.925517
347.804318	17434.934694	28.930535
347.823697	17462.370509	28.935552
347.685539	17485.647709	28.940570
348.362805	17503.049807	28.945588
348.472302	17526.089131	28.950605
349.019328	17557.171034	28.955623
349.117104	17591.410527	28.960640
349.827169	17598.961681	28.965658
350.651294	17610.642721	28.970676
351.032021	17629.248217	28.975693
351.751264	17631.705612	28.980711
351.679151	17662.900127	28.985728
352.320120	17673.729740	28.990746
352.511059	17687.765916	28.995764
352.659111	17710.627043	29.000781
352.797234	17728.854868	29.005799
353.115997	17754.001163	29.010816
353.488246	17775.862264	29.015834
353.832532	17804.896756	29.020852
354.260205	17835.257077	29.025869
354.683981	17850.246714	29.030887
354.732063	17877.872207	29.035904
355.236749	17905.621292	29.040922
355.384515	17935.640355	29.045940
355.636743	17974.891276	29.050957
355.778203	17992.707332	29.055975
356.025149	18034.202753	29.060992
356.330525	18057.884010	29.066010
356.581863	18090.326135	29.071028
356.813298	18122.688175	29.076045
357.402529	18159.941005	29.081063
357.620208	18195.707809	29.086080
358.240467	18227.550934	29.091098
358.779162	18268.585445	29.096116
358.923893	18305.928966	29.101133
359.262834	18334.279470	29.106151
359.456903	18373.184978	29.111168
359.825849	18411.433116	29.116186
359.898835	18444.526096	29.121204
360.082037	18487.578637	29.126221
360.926073	18522.767386	29.131239
360.907283	18571.401297	29.136256
361.266339	18609.601129	29.141274
361.936317	18645.171551	29.146292
362.126200	18684.344945	29.151309
362.462942	18722.917790	29.156327
362.833236	18769.215237	29.161344
363.588753	18793.908269	29.166362
363.910829	18841.268951	29.171380
363.929283	18881.951078	29.176397
364.516351	18916.763725	29.181415
364.802982	18955.911710	29.186432
365.436616	18994.412223	29.191450
365.910442	19018.092768	29.196468
366.094808	19047.232493	29.201485
366.529644	19076.392410	29.206503
366.629216	19104.569231	29.211520
367.503787	19133.385853	29.216538
368.077444	19164.537122	29.221556
368.130813	19199.039764	29.226573
369.180678	19221.794120	29.231591
369.486227	19232.772102	29.236608
370.296166	19252.177749	29.241626
370.565027	19268.185361	29.246644
370.803366	19278.917892	29.251661
371.597626	19293.607249	29.256679
371.393692	19312.675871	29.261696
371.660772	19333.145885	29.266714
372.173836	19358.363768	29.271732
372.126872	19388.404602	29.276749
372.410733	19404.091280	29.281767
372.563530	19441.713434	29.286784
372.780049	19468.071802	29.291802
373.034285	19501.444828	29.296820
373.093544	19535.187174	29.301837
373.678217	19572.079693	29.306855
373.733202	19622.378459	29.311872
374.360329	19661.832375	29.316890
374.711527	19699.184592	29.321908
374.945747	19745.769775	29.326925
375.308108	19779.009717	29.331943
376.528510	19816.260536	29.336960
377.582879	19822.992138	29.341978
378.074483	19845.070410	29.346996
378.585379	19858.083870	29.352013
379.435120	19872.294358	29.357031
379.495092	19893.921610	29.362048
380.026290	19897.461695	29.367066
380.400716	19908.918683	29.372084
380.399217	19942.717980	29.377101
381.146553	19946.487505	29.382119
381.404431	19966.843186	29.387136
381.396591	19982.086869	29.392154
381.336969	20000.103490	29.397172
381.110305	20027.191456	29.402189
381.666267	20061.865163	29.407207
381.687141	20091.687486	29.412224
382.052436	20130.588199	29.417242
382.871733	20169.510534	29.422260
382.740463	20208.075525	29.427277
383.148257	20252.353919	29.432295
383.350494	20295.092449	29.437312
383.577989	20333.165780	29.442330
384.213213	20377.370835	29.447348
384.372546	20421.432079	29.452365
384.986967	20448.677746	29.457383
385.450253	20483.773435	29.462400
385.899077	20517.581850	29.467418
386.818386	20548.539258	29.472436
386.913684	20574.573226	29.477453
387.587322	20606.201987	29.482471
387.594935	20639.797701	29.487488
387.895027	20667.898610	29.492506
388.348470	20697.598986	29.497524
388.494937	20735.396970	29.502541
389.042667	20761.779434	29.507559
389.550220	20799.432109	29.512576
389.304501	20837.294375	29.517594
390.219879	20863.836327	29.522612
390.318520	20908.972022	29.527629
390.872690	20945.929531	29.532647
391.479573	20980.791921	29.537664
391.731556	21010.905813	29.542682
392.343319	21042.060321	29.547700
392.589780	21080.702897	29.552717
393.075219	21117.153773	29.557735
393.596578	21150.711337	29.562752
393.757739	21193.618429	29.567770
393.884706	21222.885268	29.572788
394.207257	21284.346755	29.577805
394.707442	21314.465956	29.582823
395.389209	21352.870556	29.587840
395.402081	21389.382499	29.592858
395.573457	21428.497604	29.597876
396.213507	21467.705941	29.602893
396.823713	21515.647594	29.607911
397.414134	21551.483766	29.612928
397.693245	21589.319259	29.617946
398.445240	21615.754775	29.622964
398.733521	21657.141614	29.627981
399.370057	21673.526873	29.632999
399.648957	21714.887075	29.638016
399.918245	21753.047882	29.643034
400.822889	21781.220490	29.648052
400.960820	21814.688956	29.653069
401.146364	21840.349856	29.658087
401.744070	21874.133879	29.663104
401.982133	21905.360318	29.668122
402.631786	21929.896313	29.673140
402.964978	21969.981552	29.678157
403.907046	22001.330371	29.683175
404.230332	22024.582033	29.688192
404.632338	22061.713121	29.693210
405.142228	22077.656853	29.698228
405.227229	22102.668328	29.703245
405.484014	22126.820924	29.708263
405.851874	22163.680542	29.713280
405.628469	22195.387139	29.718298
406.239448	22226.209636	29.723316
406.538449	22262.418944	29.728333
406.895852	22305.843985	29.733351
407.193894	22339.987793	29.738368
408.059812	22380.326483	29.743386
408.627627	22405.504824	29.748404
409.726947	22420.619305	29.753421
410.099410	22446.039344	29.758439
410.641523	22462.958797	29.763456
410.586549	22478.561302	29.768474
410.972784	22495.280414	29.773492
410.820778	22527.145703	29.778509
411.238335	22547.300486	29.783527
411.783535	22580.834705	29.788544
412.251488	22604.179063	29.793562
412.857309	22620.128941	29.798580
413.372652	22641.613835	29.803597
414.205437	22676.026234	29.808615
414.558059	22695.514210	29.813632
414.567384	22722.841985	29.818650
415.094502	22741.057430	29.823668
415.526857	22761.695650	29.828685
415.349705	22794.524567	29.833703
415.927207	22822.190390	29.838720
416.354346	22862.258468	29.843738
416.436775	22886.375782	29.848756
416.759807	22927.975794	29.853773
417.077769	22977.260063	29.858791
417.601217	23009.051500	29.863808
417.788469	23049.280978	29.868826
418.437499	23086.699983	29.873844
418.719982	23133.568448	29.878861
418.993059	23177.082694	29.883879
419.607096	23220.314680	29.888896
419.711887	23267.371666	29.893914
420.220519	23304.979221	29.898932
420.857614	23350.415468	29.903949
421.043997	23391.166325	29.908967
421.527107	23420.076249	29.913984
421.962514	23465.405426	29.919002
422.736781	23500.520270	29.924020
423.643559	23541.337283	29.929037
424.350053	23576.075935	29.934055
424.635495	23602.632333	29.939072
425.104315	23641.685753	29.944090
425.853758	23643.850290	29.949108
426.311692	23678.275320	29.954125
426.621444	23704.975958	29.959143
426.480700	23736.245414	29.964160
427.100882	23762.527058	29.969178
427.482424	23793.940529	29.974196
427.703606	23831.115901	29.979213
428.359887	23860.492104	29.984231
428.895233	23893.519597	29.989248
429.035460	23929.311731	29.994266
429.475610	23942.518664	29.999284
430.039535	23979.468449	30.004301
430.144218	24014.856800	30.009319
430.875502	24048.731050	30.014336
430.797036	24086.153885	30.019354
431.268131	24122.107365	30.024372
431.426706	24156.833839	30.029389
432.043665	24198.273003	30.034407
432.178365	24236.041302	30.039424
432.141442	24281.267464	30.044442
432.484400	24323.939899	30.049460
433.082466	24384.087792	30.054477
433.265612	24424.485210	30.059495
433.772204	24475.974709	30.064512
434.180811	24529.310670	30.069530
434.738736	24574.255867	30.074548
435.143879	24619.397697	30.079565
435.849406	24667.204082	30.084583
436.516838	24697.182287	30.089600
436.928853	24754.328843	30.094618
437.349442	24798.326607	30.099636
437.809111	24836.255029	30.104653
438.398979	24894.289501	30.109671
439.341588	24922.249437	30.114688
439.967982	24954.881677	30.119706
440.270159	24991.020481	30.124724
440.768131	25023.431966	30.129741
440.857170	25053.241776	30.134759
441.637018	25087.563986	30.139776
441.987352	25136.060270	30.144794
442.782368	25162.935521	30.149812
442.666957	25190.698660	30.154829
443.223804	25235.563745	30.159847
443.934663	25264.939300	30.164864
443.797023	25304.933190	30.169882
444.191481	25348.851660	30.174900
444.938654	25387.403931	30.179917
445.742325	25421.035041	30.184935
446.472983	25436.278469	30.189952
446.873349	25474.937682	30.194970
447.127205	25498.508775	30.199988
447.866971	25534.378148	30.205005
448.059426	25565.981817	30.210023
448.547882	25583.553916	30.215040
448.625015	25630.931221	30.220058
449.111209	25667.781221	30.225076
449.392952	25712.495947	30.230093
449.973460	25748.919865	30.235111
450.126936	25778.757735	30.240128
450.381283	25825.445898	30.245146
451.051833	25868.719004	30.250164
451.471406	25905.028871	30.255181
451.913779	25953.540060	30.260199
452.474122	25984.671352	30.265216
453.262326	26017.943493	30.270234
453.978723	26046.839927	30.275252
454.679034	26076.581450	30.280269
455.049608	26111.906439	30.285287
455.621215	26136.553309	30.290304
455.703701	26178.069875	30.295322
455.985055	26202.902225	30.300340
456.620116	26229.705597	30.305357
456.569230	26261.027299	30.310375
457.625588	26279.127412	30.315392
457.884435	26318.856948	30.320410
457.956258	26346.914778	30.325428
458.384752	26379.981105	30.330445
458.736015	26415.281628	30.335463
459.138614	26444.522727	30.340480
459.397083	26483.867831	30.345498
459.585989	26525.515260	30.350516
460.314563	26569.142960	30.355533
460.363109	26625.906837	30.360551
461.167370	26664.524725	30.365568
461.262727	26718.242876	30.370586
461.853400	26761.263739	30.375604
462.700403	26804.291261	30.380621
462.918616	26855.812001	30.385639
463.624471	26897.863881	30.390656
464.092936	26945.155619	30.395674
464.838372	26983.759057	30.400692
464.907784	27033.245741	30.405709
465.243646	27080.377589	30.410727
465.696610	27121.706725	30.415744
466.574257	27168.925799	30.420762
466.935719	27203.210316	30.425780
467.357596	27246.980603	30.430797
467.576583	27299.581472	30.435815
468.239941	27345.377050	30.440832
468.316461	27401.548693	30.445850
468.730824	27445.181949	30.450868
469.735278	27486.010468	30.455885
470.235549	27535.730766	30.460903
470.911469	27565.712477	30.465920
471.466206	27608.321985	30.470938
471.840021	27648.243068	30.475956
473.137272	27679.184866	30.480973
473.558350	27720.508262	30.485991
474.328252	27755.730295	30.491008
474.792462	27786.783480	30.496026
474.909961	27815.454207	30.501044
475.686900	27844.665057	30.506061
475.465945	27891.903968	30.511079
475.639967	27908.743560	30.516096
475.731271	27954.850139	30.521114
476.347371	27996.412095	30.526132
476.861949	28049.623954	30.531149
477.078914	28101.145417	30.536167
477.703851	28146.296592	30.541184
478.120522	28197.519098	30.546202
478.311473	28243.950101	30.551220
478.771965	28299.547713	30.556237
479.295044	28361.186134	30.561255
479.421588	28407.858924	30.566272
480.143258	28453.760990	30.571290
480.582477	28501.569907	30.576308
481.525115	28553.873854	30.581325
481.785002	28602.818049	30.586343
482.129929	28639.313610	30.591360
482.870974	28696.546064	30.596378
483.049214	28741.270495	30.601396
483.719616	28783.058487	30.606413
483.982930	28832.898786	30.611431
484.492962	28875.746201	30.616448
484.816550	28922.487555	30.621466
485.855893	28973.211233	30.626484
486.549044	29013.531887	30.631501
487.072787	29064.757502	30.636519
487.514750	29102.354323	30.641536
487.742341	29146.288844	30.646554
488.283694	29184.288448	30.651572
489.277646	29234.648346	30.656589
489.686440	29283.603624	30.661607
489.564094	29319.111047	30.666624
490.333907	29368.354928	30.671642
490.725580	29410.589726	30.676660
491.348108	29455.470171	30.681677
492.013606	29502.018801	30.686695
492.427703	29542.628280	30.691712
493.657814	29580.274077	30.696730
494.593735	29607.965034	30.701748
494.952932	29636.013587	30.706765
495.869627	29664.023454	30.711783
496.078332	29686.632948	30.716800
496.625771	29717.536452	30.721818
496.786863	29745.515000	30.726836
497.328013	29766.095580	30.731853
497.520808	29803.847027	30.736871
497.956027	29846.583410	30.741888
498.378335	29877.978775	30.746906
498.635931	29925.955198	30.751924
499.358246	29955.797366	30.756941
499.528669	30008.234797	30.761959
499.855476	30053.990977	30.766976
500.010174	30099.669483	30.771994
500.303127	30140.837504	30.777012
501.232911	30183.969573	30.782029
501.685035	30232.333158	30.787047
502.141959	30286.877440	30.792064
503.252065	30331.114909	30.797082
503.236165	30386.917475	30.802100
503.880803	30425.274390	30.807117
504.359561	30472.848371	30.812135
505.031444	30521.014162	30.817152
505.752768	30561.690089	30.822170
505.691953	30605.478858	30.827188
506.226823	30648.430448	30.832205
506.804132	30707.470837	30.837223
507.242432	30751.502612	30.842240
507.792795	30802.854920	30.847258
508.098222	30855.571491	30.852276
509.072217	30889.755075	30.857293
509.266390	30937.773501	30.862311
509.351915	30983.226314	30.867328
509.955205	31027.419832	30.872346
510.308128	31085.045233	30.877364
510.605578	31129.357674	30.882381
510.892435	31198.367293	30.887399
511.505093	31255.440698	30.892416
512.075581	31303.067452	30.897434
512.492906	31361.607291	30.902452
513.184826	31415.499436	30.907469
513.474760	31465.762271	30.912487
514.203797	31521.715289	30.917504
515.015894	31577.695274	30.922522
515.476179	31637.137472	30.927540
516.171585	31672.954421	30.932557
516.816593	31733.731677	30.937575
517.148688	31791.391330	30.942592
518.072377	31837.340147	30.947610
518.453190	31891.012495	30.952628
518.739077	31930.608035	30.957645
519.041273	31988.093573	30.962663
519.652893	32052.554004	30.967680
520.083271	32107.843692	30.972698
520.741789	32173.959580	30.977716
521.458812	32223.182565	30.982733
521.608156	32285.018587	30.987751
522.236789	32332.524520	30.992768
523.008854	32393.329586	30.997786
523.385359	32449.544728	31.002804
524.438031	32499.029695	31.007821
524.907893	32543.041551	31.012839
525.202984	32598.340155	31.017856
525.478359	32641.710239	31.022874
525.903255	32706.293381	31.027892
526.414005	32759.469542	31.032909
527.014509	32824.000928	31.037927
527.307390	32879.449102	31.042944
528.614299	32928.942190	31.047962
528.965022	32985.804069	31.052980
529.961773	33019.814276	31.057997
531.113373	33055.287586	31.063015
531.340211	33090.695349	31.068032
532.336234	33122.787105	31.073050
532.767064	33167.517256	31.078068
533.480320	33191.297638	31.083085
533.823398	33241.180803	31.088103
534.329714	33276.771428	31.093120
534.757172	33298.909354	31.098138
534.847561	33345.989473	31.103156
535.622755	33389.013783	31.108173
536.419006	33431.371842	31.113191
537.011354	33465.714131	31.118208
537.686579	33487.724628	31.123226
537.902181	33523.034178	31.128244
538.298437	33554.983309	31.133261
538.634367	33601.939973	31.138279
538.890346	33628.769048	31.143296
539.848528	33675.180607	31.148314
540.500715	33707.288141	31.153332
541.026936	33741.901079	31.158349
541.372354	33772.407552	31.163367
541.802620	33805.377000	31.168384
542.249744	33844.198012	31.173402
542.386615	33890.851842	31.178420
543.420749	33915.275687	31.183437
543.891031	33969.469136	31.188455
544.321826	34012.538169	31.193472
544.888935	34049.126684	31.198490
545.217887	34096.265726	31.203508
546.005630	34135.568690	31.208525
545.997732	34194.632486	31.213543
546.548128	34245.821086	31.218560
547.009722	34291.890095	31.223578
547.715185	34345.353195	31.228596
548.209782	34398.284484	31.233613
548.771579	34448.868891	31.238631
548.932317	34511.748975	31.243648
549.514009	34558.142103	31.248666
550.065026	34625.708849	31.253684
550.515650	34690.496695	31.258701
551.083185	34746.335950	31.263719
551.350320	34811.714308	31.268736
551.559054	34876.361205	31.273754
552.037685	34954.303345	31.278772
552.841490	35022.822465	31.283789
553.409913	35087.900857	31.288807
553.605934	35164.124834	31.293824
554.407299	35220.174829	31.298842
555.506573	35289.540708	31.303860
555.664378	35362.483244	31.308877
556.368872	35431.570116	31.313895
556.808518	35504.051458	31.318912
557.582983	35555.871351	31.323930
558.325864	35628.960905	31.328948
558.964093	35682.972893	31.333965
560.146768	35742.958240	31.338983
560.102206	35801.992516	31.344000
560.903915	35853.726527	31.349018
561.339436	35912.934574	31.354036
561.936359	35977.329496	31.359053
562.625810	36039.297312	31.364071
562.918761	36111.888276	31.369088
563.731613	36160.856244	31.374106
563.914475	36226.926447	31.379124
564.149507	36291.324511	31.384141
564.792491	36353.547559	31.389159
565.297760	36436.368194	31.394176
565.976256	36480.675859	31.399194
566.512922	36559.505058	31.404212
567.140030	36616.160538	31.409229
568.121550	36676.489609	31.414247
568.264631	36729.314311	31.419264
568.964255	36793.211573	31.424282
569.417317	36849.105309	31.429300
570.331872	36912.237005	31.434317
571.195438	36969.007738	31.439335
571.266781	37019.194066	31.444352
572.441547	37054.936430	31.449370
573.434524	37102.600817	31.454388
574.009384	37146.669018	31.459405
574.814228	37190.394889	31.464423
575.220627	37236.755443	31.469440
576.013061	37280.710932	31.474458
576.275632	37321.676457	31.479476
576.780567	37366.773597	31.484493
577.337900	37412.423751	31.489511
578.035741	37454.091527	31.494528
579.144307	37491.683252	31.499546
579.774110	37540.487419	31.504564
580.211932	37582.032733	31.509581
580.766029	37614.981571	31.514599
580.980783	37662.244119	31.519616
581.766752	37711.871131	31.524634
581.925233	37750.036534	31.529652
581.942549	37797.661552	31.534669
582.941996	37854.995744	31.539687
583.194922	37924.371451	31.544704
583.849277	37980.218369	31.549722
584.347982	38033.030094	31.554740
584.656757	38107.185686	31.559757
585.517235	38170.195248	31.564775
585.787411	38236.993266	31.569792
586.452137	38293.164505	31.574810
586.666466	38360.629149	31.579828
586.755559	38425.912049	31.584845
587.809582	38509.547725	31.589863
587.825546	38589.664982	31.594880
588.653760	38664.576696	31.599898
588.771097	38747.789917	31.604916
589.238189	38836.187150	31.609933
590.067947	38912.217138	31.614951
590.495661	39008.214246	31.619968
591.209890	39091.471968	31.624986
591.947927	39171.824769	31.630004
592.486521	39255.403758	31.635021
593.539913	39332.044333	31.640039
594.126073	39411.335048	31.645056
594.888440	39483.846287	31.650074
595.922822	39540.286320	31.655092
596.893136	39602.161228	31.660109
597.481613	39664.982568	31.665127
598.016579	39732.457268	31.670144
598.613156	39787.498733	31.675162
599.091715	39851.040397	31.680180
599.375584	39907.543834	31.685197
600.470256	39963.687539	31.690215
600.802655	40032.707113	31.695232
601.313778	40087.937750	31.700250
601.581943	40145.650609	31.705268
601.719240	40219.310501	31.710285
602.709792	40285.506303	31.715303
603.046516	40354.870458	31.720320
603.605812	40425.570097	31.725338
604.051904	40497.789046	31.730356
604.671253	40575.244744	31.735373
605.328462	40649.177181	31.740391
605.816561	40729.541669	31.745408
606.332243	40804.970224	31.750426
606.847549	40881.450501	31.755444
607.312499	40964.850899	31.760461
607.922073	41039.831777	31.765479
608.726585	41128.226323	31.770496
609.729937	41196.087050	31.775514
610.877072	41265.467303	31.780532
611.392332	41342.202061	31.785549
613.008472	41395.618101	31.790567
613.371391	41463.305365	31.795584
613.836208	41522.100172	31.800602
614.891719	41570.589458	31.805620
614.841343	41632.822808	31.810637
615.786524	41685.524249	31.815655
616.369809	41747.668365	31.820672
616.913029	41811.230899	31.825690
617.515630	41876.965228	31.830708
617.822477	41944.698572	31.835725
618.393221	42011.755467	31.840743
619.594799	42075.177691	31.845760
619.965159	42148.120103	31.850778
620.463344	42207.186042	31.855796
620.525513	42276.768559	31.860813
621.307006	42334.921222	31.865831
621.591222	42421.412345	31.870848
622.695678	42493.090484	31.875866
623.288250	42564.600835	31.880884
623.751688	42637.229239	31.885901
624.635054	42698.898836	31.890919
625.499926	42775.775338	31.895936
626.008339	42839.884103	31.900954
626.591299	42909.471310	31.905972
626.873017	42980.373411	31.910989
627.417421	43055.499828	31.916007
627.914518	43135.001606	31.921024
628.281013	43209.827570	31.926042
628.821029	43283.758915	31.931060
629.318374	43380.038136	31.936077
630.007619	43461.361905	31.941095
630.961482	43545.277341	31.946112
631.232187	43625.186259	31.951130
632.293181	43688.300147	31.956148
632.708448	43766.170289	31.961165
633.248387	43839.920680	31.966183
633.829949	43916.316718	31.971200
634.497118	43990.573240	31.976218
635.429533	44061.835272	31.981236
635.679846	44144.288709	31.986253
636.354081	44214.903998	31.991271
636.686933	44290.254721	31.996288
637.495182	44377.223962	32.001306
638.243697	44453.097790	32.006324
638.997423	44537.910847	32.011341
639.761644	44612.276336	32.016359
640.583133	44688.024921	32.021376
641.112816	44761.812238	32.026394
641.971530	44839.345561	32.031412
642.389931	44913.149372	32.036429
643.270447	44994.361698	32.041447
643.825844	45072.797415	32.046464
644.151486	45153.328630	32.051482
645.006172	45220.323020	32.056500
645.818608	45310.630611	32.061517
646.063647	45383.155392	32.066535
646.900858	45470.070991	32.071552
647.708688	45550.063371	32.076570
648.320546	45622.472535	32.081588
648.555070	45704.843862	32.086605
649.586998	45770.663464	32.091623
650.312880	45854.154472	32.096640
651.118608	45932.550844	32.101658
652.242927	46006.664297	32.106676
652.809553	46082.241030	32.111693
653.686974	46144.832407	32.116711
654.212645	46225.248611	32.121728
654.920598	46295.066848	32.126746
655.840241	46340.986232	32.131764
656.226762	46423.081966	32.136781
657.049108	46491.251720	32.141799
657.792050	46563.692528	32.146816
657.830705	46641.531580	32.151834
658.898596	46702.080392	32.156852
659.232022	46782.490815	32.161869
660.274660	46856.150986	32.166887
660.660263	46927.154233	32.171904
661.038764	47008.919078	32.176922
661.894347	47069.003262	32.181940
662.531535	47144.392079	32.186957
662.876872	47221.836694	32.191975
663.819542	47301.298502	32.196992
663.981080	47378.408873	32.202010
664.721524	47466.948225	32.207028
665.188261	47555.692789	32.212045
665.783955	47639.873973	32.217063
666.757069	47728.295711	32.222080
667.258179	47803.760958	32.227098
667.795748	47877.524204	32.232116
668.523413	47962.612755	32.237133
669.271075	48029.028905	32.242151
670.632109	48090.435185	32.247168
671.834169	48152.604810	32.252186
672.476488	48222.286536	32.257204
673.150462	48281.199097	32.262221
673.815852	48339.336328	32.267239
674.637551	48398.688235	32.272256
674.874673	48465.973492	32.277274
675.727889	48519.338214	32.282292
675.806676	48585.198105	32.287309
676.378826	48658.307761	32.292327
677.046899	48731.957160	32.297344
676.929739	48823.157518	32.302362
677.848813	48895.539029	32.307380
678.301520	48991.178230	32.312397
678.947937	49074.649461	32.317415
679.941754	49157.316112	32.322432
680.071614	49257.206538	32.327450
681.013073	49344.993585	32.332468
681.280618	49446.352267	32.337485
681.643305	49540.859852	32.342503
682.765000	49647.013392	32.347520
683.124482	49748.787478	32.352538
683.830957	49839.883097	32.357556
684.234616	49945.902259	32.362573
685.155487	50050.576218	32.367591
686.262307	50154.378658	32.372608
686.986165	50253.704945	32.377626
687.916113	50336.393869	32.382644
689.106916	50439.065231	32.387661
689.600610	50524.918992	32.392679
690.315550	50605.959086	32.397696
691.232748	50701.343906	32.402714
692.029078	50783.242633	32.407732
692.794138	50874.370954	32.412749
693.639829	50944.416146	32.417767
694.909299	51015.014456	32.422784
696.292130	51082.763225	32.427802
697.070765	51132.433034	32.432820
697.743910	51193.164622	32.437837
698.587953	51255.326549	32.442855
699.215792	51306.715819	32.447872
699.892621	51373.341915	32.452890
700.421487	51439.064850	32.457908
700.918873	51509.039054	32.462925
701.480613	51577.385085	32.467943
702.535075	51636.119429	32.472960
702.694232	51721.081728	32.477978
703.181874	51776.331277	32.482996
704.130564	51844.637226	32.488013
704.628549	51924.304698	32.493031
705.109687	51995.831348	32.498048
705.749057	52073.718774	32.503066
706.445734	52149.195795	32.508084
706.792057	52222.900853	32.513101
706.960969	52299.264945	32.518119
707.960766	52380.756398	32.523136
708.355792	52460.279401	32.528154
709.009666	52540.744034	32.533172
709.457287	52622.672262	32.538189
710.237802	52712.801858	32.543207
711.148981	52803.294902	32.548224
711.721861	52895.703917	32.553242
712.405053	52987.165661	32.558260
713.067576	53083.812494	32.563277
713.622055	53177.338023	32.568295
714.479114	53263.760712	32.573312
714.938236	53361.157731	32.578330
715.725606	53458.341037	32.583348
716.558543	53553.109628	32.588365
717.044108	53655.748000	32.593383
717.523440	53754.122875	32.598400
717.595705	53864.706175	32.603418
718.773261	53960.213833	32.608436
719.668556	54064.509143	32.613453
720.783209	54179.907456	32.618471
721.446532	54269.868327	32.623488
722.291020	54375.886374	32.628506
722.836875	54476.837840	32.633524
723.737473	54573.135196	32.638541
724.347397	54682.449298	32.643559
725.139883	54777.167464	32.648576
726.042773	54880.435753	32.653594
727.014509	54981.380010	32.658612
727.683217	55088.398771	32.663629
728.336360	55191.825194	32.668647
729.126073	55282.678935	32.673664
729.904119	55379.108598	32.678682
730.957513	55465.968521	32.683700
732.243715	55548.871021	32.688717
732.678719	55637.436381	32.693735
733.571892	55731.440385	32.698752
734.248975	55819.560648	32.703770
734.788538	55917.525112	32.708788
735.569218	55999.024705	32.713805
735.862016	56097.569463	32.718823
737.115380	56183.703111	32.723840
737.707074	56289.212175	32.728858
738.312063	56375.704168	32.733876
739.250055	56470.405419	32.738893
739.997883	56567.395767	32.743911
741.020801	56650.821890	32.748928
742.212867	56735.679212	32.753946
743.145381	56819.070961	32.758964
743.664652	56890.501227	32.763981
743.964403	56979.500122	32.768999
745.148749	57056.763871	32.774016
745.661451	57145.132968	32.779034
746.302233	57216.891160	32.784052
747.325006	57293.222889	32.789069
748.054486	57369.320755	32.794087
748.875450	57442.325484	32.799104
749.429026	57506.951927	32.804122
749.999401	57580.448788	32.809140
750.661167	57658.689136	32.814157
750.921958	57751.894511	32.819175
751.862045	57829.664412	32.824192
752.314527	57919.020475	32.829210
753.146842	58010.062510	32.834228
754.108289	58097.347699	32.839245
754.681908	58194.261937	32.844263
755.400010	58278.751885	32.849280
756.228379	58366.497113	32.854298
756.915351	58468.493571	32.859316
757.946918	58549.568638	32.864333
758.277157	58649.756341	32.869351
759.510416	58723.801098	32.874368
760.413143	58810.941407	32.879386
761.414453	58903.974661	32.884404
763.165293	58952.859080	32.889421
763.972755	59028.077613	32.894439
764.693328	59093.331495	32.899456
765.413869	59162.327243	32.904474
766.176729	59226.070063	32.909492
766.975179	59298.927319	32.914509
767.412336	59384.146261	32.919527
768.151220	59465.306712	32.924544
768.509278	59542.146307	32.929562
768.948909	59626.752751	32.934580
769.477319	59708.607551	32.939597
769.701216	59807.245339	32.944615
770.493574	59905.881040	32.949632
771.031729	60016.765870	32.954650
771.320674	60127.441160	32.959668
772.229298	60234.382829	32.964685
772.718987	60354.714573	32.969703
773.460880	60468.967497	32.974720
774.413171	60584.992765	32.979738
774.746056	60709.702151	32.984756
775.723150	60822.804288	32.989773
776.006923	60948.149295	32.994791
776.981084	61072.365460	32.999808
777.491854	61187.167633	33.004826
778.187424	61312.456960	33.009844
779.295933	61441.096009	33.014861
779.822478	61574.437299	33.019879
780.832988	61698.474014	33.024896
781.968166	61824.911130	33.029914
782.744622	61946.056396	33.034932
783.685173	62068.571260	33.039949
783.980651	62201.551606	33.044967
784.767970	62325.984302	33.049984
785.624883	62444.590169	33.055002
786.509697	62557.022252	33.060020
787.541723	62663.045085	33.065037
788.539910	62784.738841	33.070055
790.142800	62884.356203	33.075072
791.143623	62987.724689	33.080090
791.323660	63087.586735	33.085108
791.769766	63194.249966	33.090125
792.362320	63298.309438	33.095143
792.838697	63410.285072	33.100160
793.794651	63521.268841	33.105178
794.439551	63644.444188	33.110196
795.271028	63755.393627	33.115213
796.128864	63882.478683	33.120231
796.639640	63997.536608	33.125248
797.733400	64124.747093	33.130266
798.386957	64248.227961	33.135284
799.636548	64360.088886	33.140301
800.565428	64482.158434	33.145319
801.250791	64599.819705	33.150336
801.883167	64721.005769	33.155354
802.822148	64847.684487	33.160372
803.909062	64960.550078	33.165389
803.946937	65092.151490	33.170407
804.803931	65208.155648	33.175424
805.642343	65322.804349	33.180442
806.791243	65453.117649	33.185460
807.488177	65569.815051	33.190477
808.536963	65699.350410	33.195495
809.620454	65812.651071	33.200512
810.382623	65934.808173	33.205530
811.367830	66062.681209	33.210548
811.972314	66169.642216	33.215565
812.575701	66295.596797	33.220583
813.339393	66415.069337	33.225600
814.322577	66530.395272	33.230618
815.000711	66654.695308	33.235636
816.219256	66785.403213	33.240653
816.856514	66894.638422	33.245671
817.570305	67013.142856	33.250688
818.515758	67130.406945	33.255706
819.494560	67259.160830	33.260724
820.566246	67369.127064	33.265741
821.587544	67481.726489	33.270759
822.196194	67596.319349	33.275776
823.563632	67707.849018	33.280794
824.251729	67826.343405	33.285812
825.297459	67938.865183	33.290829
825.987432	68045.865240	33.295847
826.885915	68156.718809	33.300864
827.609722	68263.891207	33.305882
828.238060	68377.169674	33.310900
828.935288	68481.141881	33.315917
829.746265	68589.426501	33.320935
830.804230	68713.230846	33.325952
831.420027	68813.121151	33.330970
832.373582	68924.177924	33.335988
833.150534	69025.799494	33.341005
834.147424	69117.102096	33.346023
835.207897	69207.388779	33.351040
836.414824	69300.584819	33.356058
837.034911	69419.763615	33.361076
837.720601	69509.186207	33.366093
838.383472	69606.473187	33.371111
839.197439	69708.458402	33.376128
840.008489	69816.957866	33.381146
840.704774	69918.508933	33.386164
841.498882	70025.893072	33.391181
842.162631	70130.378544	33.396199
842.403385	70248.279941	33.401216
843.272470	70375.180525	33.406234
843.924020	70496.958921	33.411252
844.764392	70610.010446	33.416269
845.539325	70736.290566	33.421287
846.801544	70854.469303	33.426304
847.845341	70967.987437	33.431322
848.478840	71098.853418	33.436340
849.486563	71216.015289	33.441357
850.450471	71339.559890	33.446375
850.782176	71453.272080	33.451392
851.635312	71583.230637	33.456410
852.164823	71716.261996	33.461428
853.389591	71840.156852	33.466445
854.083769	71973.882531	33.471463
854.764646	72113.322083	33.476480
855.897316	72232.763710	33.481498
856.388709	72372.142499	33.486516
857.153704	72509.400930	33.491533
857.785679	72651.223909	33.496551
858.351815	72793.792712	33.501568
859.087568	72943.758314	33.506586
859.638947	73106.367591	33.511604
860.510712	73245.490715	33.516621
861.559516	73416.884120	33.521639
862.209653	73576.235430	33.526656
863.226900	73729.181351	33.531674
863.726494	73894.208689	33.536692
864.833218	74050.980631	33.541709
865.958121	74203.652081	33.546727
866.904001	74367.031631	33.551744
868.220321	74506.624177	33.556762
869.263907	74657.680857	33.561780
870.675774	74796.816120	33.566797
872.020970	74933.149034	33.571815
872.348471	75075.223146	33.576832
873.456955	75194.678633	33.581850
874.170923	75331.147394	33.586868
875.063667	75479.540981	33.591885
875.818836	75621.406177	33.596903
876.612435	75759.698240	33.601920
877.808462	75895.101151	33.606938
878.626298	76031.195863	33.611956
879.323489	76147.140421	33.616973
879.938766	76274.289265	33.621991
880.864912	76411.531617	33.627008
882.379703	76546.238683	33.632026
882.725621	76682.677520	33.637044
883.430298	76802.799039	33.642061
884.583560	76936.147110	33.647079
885.307092	77073.137231	33.652096
886.214270	77207.066734	33.657114
886.920333	77346.300799	33.662132
887.935651	77480.757422	33.667149
888.761442	77622.540945	33.672167
889.266079	77764.102022	33.677184
890.377941	77907.438778	33.682202
891.290416	78055.782759	33.687220
892.249824	78192.334420	33.692237
893.084158	78337.663500	33.697255
893.841272	78483.386299	33.702272
895.076338	78620.842240	33.707290
896.060841	78775.346519	33.712308
896.436772	78912.356705	33.717325
897.521278	79059.501125	33.722343
898.047270	79208.804501	33.727360
899.472808	79361.181203	33.732378
900.223858	79511.086971	33.737396
901.387147	79649.826688	33.742413
902.180596	79792.812337	33.747431
902.955179	79950.264352	33.752448
904.344022	80088.961783	33.757466
904.926258	80243.703066	33.762484
905.950268	80389.177239	33.767501
907.431704	80523.350608	33.772519
908.025132	80674.638559	33.777536
908.917887	80822.687596	33.782554
909.924210	80968.674606	33.787572
910.861167	81104.589565	33.792589
911.354140	81258.650701	33.797607
912.435376	81418.780796	33.802624
913.688104	81545.438720	33.807642
914.265595	81700.608191	33.812660
914.947201	81858.323294	33.817677
916.451494	81999.416730	33.822695
917.132135	82154.356461	33.827712
918.079456	82301.608436	33.832730
918.785360	82450.712248	33.837748
919.703508	82587.518621	33.842765
920.694731	82739.960463	33.847783
921.640247	82892.069460	33.852800
922.543316	83040.111948	33.857818
923.520420	83190.293990	33.862836
924.156832	83347.761201	33.867853
925.396009	83493.331953	33.872871
926.083329	83653.791703	33.877888
926.737637	83790.662982	33.882906
927.562515	83947.330004	33.887924
928.797895	84085.210815	33.892941
929.820734	84223.236405	33.897959
930.311596	84377.229976	33.902976
931.705576	84522.331358	33.907994
932.373212	84670.437141	33.913012
933.064788	84822.412351	33.918029
934.413333	84972.333398	33.923047
934.863063	85129.990088	33.928064
936.100001	85275.154649	33.933082
937.353154	85414.470320	33.938100
938.249761	85565.466020	33.943117
939.084292	85719.567712	33.948135
939.910787	85874.532398	33.953152
940.861487	86024.756072	33.958170
941.475050	86187.099854	33.963188
942.004232	86352.541018	33.968205
943.197166	86502.890770	33.973223
943.847179	86680.349798	33.978240
945.605099	86828.408950	33.983258
946.499876	86984.501953	33.988276
947.623339	87141.898434	33.993293
948.667883	87305.599930	33.998311
949.463682	87463.402707	34.003328
950.362186	87619.024586	34.008346
951.781899	87770.697804	34.013364
952.971273	87925.917470	34.018381
953.798263	88070.378233	34.023399
954.381498	88230.988081	34.028416
955.686118	88373.805696	34.033434
956.368878	88528.312267	34.038452
957.051323	88680.250394	34.043469
958.547885	88828.708442	34.048487
959.217197	88990.042761	34.053504
960.389579	89139.703766	34.058522
961.152575	89301.460818	34.063540
962.013364	89459.657967	34.068557
963.028011	89624.171501	34.073575
963.831955	89794.323474	34.078592
964.639924	89953.165799	34.083610
965.705446	90114.895465	34.088628
966.232763	90289.648953	34.093645
967.227082	90460.760351	34.098663
967.680219	90644.579930	34.103680
968.506708	90824.374785	34.108698
969.936297	90997.959819	34.113716
970.530025	91186.538099	34.118733
971.684915	91359.868931	34.123751
972.460443	91542.880520	34.128768
974.010485	91719.342647	34.133786
975.533259	91899.083134	34.138804
976.651712	92066.975395	34.143821
977.764082	92232.534180	34.148839
978.876961	92391.150247	34.153856
979.895333	92543.213190	34.158874
981.334038	92690.862828	34.163892
982.179876	92850.293488	34.168909
983.135222	92987.228906	34.173927
984.049835	93136.344544	34.178944
984.919189	93276.309343	34.183962
985.389229	93425.781372	34.188980
986.714134	93575.449738	34.193997
987.167272	93725.565803	34.199015
988.500039	93886.394664	34.204032
989.178036	94046.190925	34.209050
990.473611	94190.481039	34.214068
991.385267	94355.550327	34.219085
992.589449	94505.194322	34.224103
993.532841	94670.462829	34.229120
994.688446	94825.314270	34.234138
995.950777	94973.064660	34.239156
996.957335	95127.304121	34.244173
997.849682	95276.797229	34.249191
998.400829	95443.024273	34.254208
999.501168	95603.125337	34.259226
1000.620343	95771.643914	34.264244
1001.060747	95943.774374	34.269261
1001.803822	96105.528807	34.274279
1002.559117	96287.483585	34.279296
1003.368002	96477.635203	34.284314
1004.369348	96654.707437	34.289332
1004.957284	96837.916685	34.294349
1005.844065	97028.768164	34.299367
1006.287631	97227.939907	34.304384
1006.944117	97430.742417	34.309402
1008.027238	97629.320300	34.314420
1008.907740	97857.906011	34.319437
1010.118159	98060.080532	34.324455
1011.318740	98260.713519	34.329472
1012.457632	98473.869267	34.334490
1013.569690	98675.331069	34.339508
1014.444194	98882.216812	34.344525
1016.066161	99077.022475	34.349543
1017.692189	99270.360017	34.354560
1019.308369	99457.438814	34.359578
1020.821530	99641.117560	34.364596
1021.902578	99825.966978	34.369613
1022.724311	100010.475890	34.374631
1023.820253	100182.820271	34.379648
1024.701257	100363.085636	34.384666
1026.159568	100535.332326	34.389684
1026.840221	100719.978090	34.394701
1028.191085	100881.234408	34.399719
1029.978008	101043.043921	34.404736
1030.930603	101212.329712	34.409754
1032.494227	101366.796411	34.414772
1032.860403	101524.565429	34.419789
1033.965277	101680.676551	34.424807
1035.323500	101843.811863	34.429824
1035.895720	102004.207982	34.434842
1037.108420	102156.111597	34.439860
1037.807998	102321.401628	34.444877
1038.667679	102467.592502	34.449895
1039.558857	102621.896805	34.454912
1039.991438	102791.946745	34.459930
1041.245871	102947.343244	34.464948
1042.213134	103119.900024	34.469965
1043.269563	103286.540812	34.474983
1044.344450	103446.593693	34.480000
1045.477257	103607.828142	34.485018
1046.795671	103763.877078	34.490036
1047.789352	103938.638417	34.495053
1049.123785	104098.080861	34.500071
1050.227384	104265.948274	34.505088
1051.307934	104428.019910	34.510106
1052.378948	104599.492001	34.515124
1053.117327	104758.647835	34.520141
1054.169539	104933.722332	34.525159
1055.283250	105106.330285	34.530176
1055.593240	105284.979263	34.535194
1056.581579	105462.702662	34.540212
1056.871415	105650.603676	34.545229
1058.049514	105837.999262	34.550247
1058.885283	106036.107064	34.555264
1059.490824	106247.074061	34.560282
1060.563422	106445.562313	34.565300
1061.376695	106667.896811	34.570317
1062.212867	106882.097245	34.575335
1063.336187	107105.838918	34.580352
1064.071703	107329.598171	34.585370
1065.305125	107545.901861	34.590388
1066.647922	107775.666271	34.595405
1067.132591	108001.348724	34.600423
1068.398227	108223.517170	34.605440
1068.966027	108462.008453	34.610458
1070.403632	108689.344859	34.615476
1071.857633	108922.228740	34.620493
1072.523633	109143.683933	34.625511
1074.011501	109379.682144	34.630528
1074.937298	109608.735271	34.635546
1076.503044	109833.677645	34.640564
1077.304430	110064.567380	34.645581
1078.898553	110291.548188	34.650599
1080.601950	110505.451132	34.655616
1081.375159	110734.717068	34.660634
1082.817001	110936.493788	34.665652
1084.061500	111150.239570	34.670669
1085.017713	111363.681629	34.675687
1086.106015	111579.649129	34.680704
1087.059333	111800.632951	34.685722
1088.559355	112008.678565	34.690740
1089.625746	112225.744336	34.695757
1090.674095	112427.649877	34.700775
1092.185216	112635.647564	34.705792
1093.221039	112843.462111	34.710810
1094.443798	113027.123566	34.715828
1095.170414	113216.091006	34.720845
1096.771526	113411.118090	34.725863
1097.924566	113602.219613	34.730880
1098.828577	113786.092608	34.735898
1099.919238	113969.314016	34.740916
1100.711485	114168.133716	34.745933
1101.828331	114353.329627	34.750951
1103.168990	114544.658766	34.755968
1103.873603	114753.532286	34.760986
1104.898636	114947.768963	34.766004
1106.345988	115144.760146	34.771021
1107.117897	115351.789306	34.776039
1108.295493	115556.799233	34.781056
1109.134499	115760.348116	34.786074
1110.451074	115954.275606	34.791092
1111.454877	116167.086799	34.796109
1112.732619	116370.780280	34.801127
1114.214162	116576.999847	34.806144
1114.993335	116788.802382	34.811162
1116.228661	116984.879445	34.816180
1117.359569	117195.281580	34.821197
1118.349475	117407.926868	34.826215
1119.468655	117624.631787	34.831232
1120.468340	117829.916359	34.836250
1121.239856	118043.047171	34.841268
1122.356750	118268.956876	34.846285
1123.168593	118498.519353	34.851303
1124.090128	118714.315790	34.856320
1125.082029	118957.245260	34.861338
1126.327144	119185.078878	34.866356
1127.391284	119415.188225	34.871373
1128.908068	119643.549119	34.876391
1129.762203	119876.207128	34.881408
1130.946540	120106.491356	34.886426
1131.934296	120340.384706	34.891444
1133.377968	120571.768674	34.896461
1134.660303	120815.816874	34.901479
1135.764627	121034.931869	34.906496
1136.589448	121277.186570	34.911514
1137.948777	121515.663838	34.916532
1139.539040	121755.117322	34.921549
1140.670599	121994.195006	34.926567
1141.538662	122217.959504	34.931584
1142.333739	122460.963889	34.936602
1143.611966	122693.152948	34.941620
1144.559505	122948.770752	34.946637
1145.455949	123201.877362	34.951655
1146.751362	123441.027137	34.956672
1147.626110	123693.507852	34.961690
1148.926875	123930.366548	34.966708
1150.825965	124166.389539	34.971725
1151.965450	124411.441781	34.976743
1153.092065	124643.291421	34.981760
1154.164599	124885.912744	34.986778
1155.193157	125118.606597	34.991796
1156.559008	125352.537282	34.996813
1157.713517	125571.359513	35.001831
1158.840893	125782.228099	35.006848
1160.098584	126000.820226	35.011866
1161.946609	126221.657716	35.016884
1163.505290	126426.677004	35.021901
1164.384001	126642.727441	35.026919
1165.811413	126852.930833	35.031936
1166.319927	127090.912707	35.036954
1167.634992	127293.900625	35.041972
1168.922958	127512.840399	35.046989
1169.594018	127739.834970	35.052007
1170.739188	127960.183955	35.057024
1171.587449	128202.261055	35.062042
1172.174226	128432.887665	35.067060
1173.627795	128669.743623	35.072077
1174.646140	128927.135189	35.077095
1175.734912	129164.538985	35.082112
1176.725428	129408.122082	35.087130
1177.988651	129658.125346	35.092148
1179.361903	129906.856749	35.097165
1180.597073	130158.516678	35.102183
1182.128536	130392.291666	35.107200
1183.499720	130645.744903	35.112218
1184.649334	130891.530482	35.117236
1185.918319	131123.542910	35.122253
1186.930871	131378.432416	35.127271
1188.240375	131622.370669	35.132288
1189.215813	131869.879564	35.137306
1190.320105	132111.840926	35.142324
1191.647342	132363.895254	35.147341
1192.923732	132631.338185	35.152359
1194.373037	132867.312953	35.157376
1195.471057	133116.306276	35.162394
1196.647107	133361.586178	35.167412
1198.090006	133610.600268	35.172429
1199.191799	133859.750701	35.177447
1200.271068	134107.943325	35.182464
1201.229845	134377.166360	35.187482
1202.503161	134627.206036	35.192500
1203.720839	134880.426737	35.197517
1204.260499	135144.352048	35.202535
1205.786997	135400.706152	35.207552
1206.972788	135656.448570	35.212570
1207.924686	135922.819839	35.217588
1209.264123	136190.052440	35.222605
1210.573862	136452.524909	35.227623
1212.073837	136709.882501	35.232640
1213.304084	136973.780013	35.237658
1214.755416	137235.562312	35.242676
1216.364918	137480.113515	35.247693
1217.531124	137736.673823	35.252711
1218.884196	137984.429750	35.257728
1220.364021	138230.187734	35.262746
1221.580332	138463.236682	35.267764
1222.943095	138699.381398	35.272781
1223.693541	138936.799114	35.277799
1224.788066	139170.127294	35.282816
1225.726669	139410.990402	35.287834
1227.109376	139649.953203	35.292852
1228.092904	139884.015286	35.297869
1229.061509	140146.168665	35.302887
1230.471070	140375.012859	35.307904
1231.709227	140626.725676	35.312922
1232.445456	140883.306851	35.317940
1233.691042	141140.157770	35.322957
1235.058402	141407.476821	35.327975
1236.217493	141667.897048	35.332992
1237.265751	141925.269345	35.338010
1238.384141	142193.981160	35.343028
1239.595868	142459.546756	35.348045
1240.466722	142735.292420	35.353063
1242.077452	143003.228591	35.358080
1243.619087	143273.207649	35.363098
1245.219776	143537.547977	35.368116
1246.566858	143802.098527	35.373133
1247.701187	144069.375991	35.378151
1249.629698	144317.762906	35.383168
1251.512618	144566.932936	35.388186
1252.874431	144817.576233	35.393204
1254.456511	145066.585599	35.398221
1255.472539	145314.159008	35.403239
1256.688270	145566.278246	35.408256
1258.003069	145796.809417	35.413274
1259.798182	146033.423528	35.418292
1261.059447	146274.442634	35.423309
1262.180292	146514.383961	35.428327
1263.255459	146760.219475	35.433344
1264.578156	147006.889369	35.438362
1265.399210	147258.948246	35.443380
1266.811318	147494.622648	35.448397
1268.068453	147758.304015	35.453415
1269.209310	148014.726990	35.458432
1270.180808	148277.826757	35.463450
1271.075609	148535.449594	35.468468
1272.499121	148796.547748	35.473485
1273.589434	149063.742119	35.478503
1274.736224	149326.349917	35.483520
1276.047185	149585.874654	35.488538
1276.949706	149866.133026	35.493556
1278.407442	150133.830132	35.498573
1279.969340	150401.473235	35.503591
1281.494123	150661.577531	35.508608
1283.560621	150904.898494	35.513626
1285.138617	151150.181886	35.518644
1287.067630	151402.624143	35.523661
1287.936777	151644.074501	35.528679
1290.063862	151874.212114	35.533696
1292.170569	152085.124789	35.538714
1293.493153	152285.479692	35.543732
1295.607448	152468.994380	35.548749
1297.013494	152659.962945	35.553767
1297.804313	152853.473235	35.558784
1299.416766	153045.727575	35.563802
1300.478181	153240.956657	35.568820
1301.179216	153427.876300	35.573837
1301.807105	153627.608570	35.578855
1302.719412	153840.231991	35.583872
1304.342624	154049.094221	35.588890
1305.041499	154267.819994	35.593908
1306.491100	154480.836926	35.598925
1307.539513	154699.809695	35.603943
1308.560589	154928.327818	35.608960
1309.688450	155159.391450	35.613978
1310.935561	155393.911862	35.618996
1311.967209	155638.314623	35.624013
1312.911016	155884.662141	35.629031
1314.201399	156129.099707	35.634048
1315.031561	156385.034859	35.639066
1315.515174	156651.141694	35.644084
1317.254135	156918.963684	35.649101
1317.952947	157193.130955	35.654119
1319.012973	157471.627685	35.659136
1320.225591	157747.068148	35.664154
1321.131008	158042.658361	35.669172
1322.507350	158336.140241	35.674189
1324.107815	158644.378447	35.679207
1325.287252	158932.240018	35.684224
1327.000173	159218.832394	35.689242
1328.247036	159518.802373	35.694260
1329.538677	159823.613266	35.699277
1331.206963	160123.007957	35.704295
1332.353624	160425.995717	35.709312
1333.858427	160716.097532	35.714330
1335.182165	161010.241524	35.719348
1337.804549	161287.836556	35.724365
1339.029758	161575.150108	35.729383
1340.317328	161857.849319	35.734400
1341.793463	162140.644995	35.739418
1343.034190	162430.232711	35.744436
1344.331371	162710.398326	35.749453
1346.012964	162999.787522	35.754471
1347.362880	163278.805870	35.759488
1348.826746	163556.702639	35.764506
1350.100180	163847.575707	35.769524
1351.761148	164127.269462	35.774541
1353.557015	164395.725421	35.779559
1355.027666	164661.383786	35.784576
1357.089137	164918.923504	35.789594
1358.237444	165183.904246	35.794612
1359.937919	165434.644234	35.799629
1361.812369	165674.392821	35.804647
1363.113824	165928.376053	35.809664
1364.418725	166171.181267	35.814682
1365.870409	166397.847760	35.819700
1367.293988	166605.842049	35.824717
1368.655673	166841.268871	35.829735
1369.872144	167063.220577	35.834752
1371.356969	167283.985416	35.839770
1372.646291	167516.738027	35.844788
1373.376058	167755.386596	35.849805
1374.725545	167993.422769	35.854823
1375.514144	168243.611119	35.859840
1376.994356	168485.256640	35.864858
1378.310522	168735.674605	35.869876
1379.794511	168986.141340	35.874893
1380.903885	169237.346096	35.879911
1381.693170	169501.081026	35.884928
1383.460850	169748.571977	35.889946
1384.193052	170022.331892	35.894964
1385.614040	170298.107431	35.899981
1386.915066	170565.656585	35.904999
1388.210145	170854.210424	35.910016
1389.277108	171132.995536	35.915034
1390.240225	171437.612079	35.920052
1391.235282	171724.699711	35.925069
1392.774637	172036.099616	35.930087
1393.274033	172342.032243	35.935104
1394.527408	172651.188084	35.940122
1395.953148	172977.575729	35.945140
1397.322051	173282.515202	35.950157
1398.635129	173608.393342	35.955175
1400.040576	173930.310961	35.960192
1401.802017	174246.941061	35.965210
1403.274472	174585.819382	35.970228
1404.952161	174913.115915	35.975245
1406.340188	175240.045363	35.980263
1407.780386	175577.133794	35.985280
1409.215934	175895.848085	35.990298
1410.719198	176221.418913	35.995316
1412.249690	176546.314521	36.000333
1413.679043	176878.933365	36.005351
1414.815966	177200.486444	36.010368
1416.266913	177530.097883	36.015386
1417.728606	177867.883194	36.020404
1419.218503	178189.585117	36.025421
1420.831437	178523.490454	36.030439
1422.090362	178857.509287	36.035456
1423.969118	179183.415367	36.040474
1425.658444	179518.037439	36.045492
1426.974244	179850.694774	36.050509
1428.608768	180178.781127	36.055527
1429.966863	180497.067385	36.060544
1431.667574	180813.202618	36.065562
1433.092443	181136.761387	36.070580
1434.582001	181466.873197	36.075597
1436.000481	181785.778695	36.080615
1437.555780	182117.101727	36.085632
1439.341342	182419.244207	36.090650
1440.611855	182727.708799	36.095668
1442.192186	183011.814719	36.100685
1444.383360	183294.789413	36.105703
1445.903608	183591.652577	36.110720
1447.395679	183870.510292	36.115738
1448.981845	184152.488565	36.120756
1449.924994	184440.239587	36.125773
1451.838906	184720.565243	36.130791
1452.668951	185010.077538	36.135808
1454.532261	185302.194392	36.140826
1455.721295	185591.457803	36.145844
1456.770186	185883.805861	36.150861
1458.417774	186195.969611	36.155879
1459.914687	186547.321618	36.160896
1461.406343	186845.844189	36.165914
1462.594892	187162.610761	36.170932
1464.303777	187459.614087	36.175949
1466.058564	187749.933909	36.180967
1467.391192	188058.607142	36.185984
1468.588827	188347.095712	36.191002
1470.054524	188654.682943	36.196020
1471.473427	188964.526682	36.201037
1473.134763	189267.805546	36.206055
1474.418883	189584.784471	36.211072
1476.102284	189885.815714	36.216090
1476.681594	190200.506478	36.221108
1478.076986	190527.004989	36.226125
1479.452830	190850.703017	36.231143
1480.671339	191175.991137	36.236160
1482.091261	191509.587095	36.241178
1483.853722	191848.597782	36.246196
1485.379503	192189.821668	36.251213
1486.698696	192520.533050	36.256231
1487.897200	192870.792109	36.261248
1489.219460	193209.479167	36.266266
1490.870710	193549.330471	36.271284
1492.551523	193893.494962	36.276301
1494.375971	194245.038192	36.281319
1495.677291	194590.845561	36.286336
1497.503725	194929.531496	36.291354
1498.696148	195277.367023	36.296372
1499.993008	195623.269438	36.301389
1501.234357	195979.403310	36.306407
1502.807870	196336.409034	36.311424
1504.241205	196695.040330	36.316442
1505.544383	197050.242464	36.321460
1506.789589	197410.318982	36.326477
1508.629438	197779.652724	36.331495
1509.499872	198161.520488	36.336512
1511.370707	198527.970860	36.341530
1512.977245	198889.656443	36.346548
1514.423234	199267.508560	36.351565
1516.310323	199634.926838	36.356583
1517.639841	200001.820288	36.361600
1519.186966	200362.571281	36.366618
1520.431637	200719.262092	36.371636
1521.742087	201081.669643	36.376653
1523.501214	201437.260186	36.381671
1524.834648	201793.572830	36.386688
1526.307433	202157.062520	36.391706
1527.978690	202509.664057	36.396724
1529.895830	202874.731805	36.401741
1530.914494	203230.533775	36.406759
1532.016426	203595.934943	36.411776
1533.558467	203969.147545	36.416794
1535.328112	204340.189851	36.421812
1537.085314	204713.458099	36.426829
1538.470506	205081.116022	36.431847
1540.146408	205457.703053	36.436864
1541.927232	205824.763433	36.441882
1544.038475	206183.680569	36.446900
1545.933774	206554.165751	36.451917
1547.648425	206918.550526	36.456935
1548.738435	207287.157894	36.461952
1550.220799	207653.503044	36.466970
1551.706849	208017.169920	36.471988
1553.087543	208388.805330	36.477005
1555.038909	208758.236856	36.482023
1556.182838	209135.782544	36.487040
1557.605110	209507.491919	36.492058
1559.618063	209887.584211	36.497076
1560.961949	210268.148199	36.502093
1562.895493	210645.565349	36.507111
1564.385099	211035.783821	36.512128
1565.666163	211409.633342	36.517146
1567.416360	211781.981916	36.522164
1568.679541	212174.529793	36.527181
1570.984608	212541.072197	36.532199
1572.663936	212921.742398	36.537216
1574.206302	213294.081870	36.542234
1576.011719	213666.301616	36.547252
1577.216729	214042.028830	36.552269
1579.074616	214423.004709	36.557287
1580.213129	214815.178598	36.562304
1581.964658	215192.493033	36.567322
1583.556862	215580.579507	36.572340
1584.985155	215959.577653	36.577357
1587.074584	216334.730587	36.582375
1588.608769	216717.472397	36.587392
1589.915810	217097.714679	36.592410
1591.863248	217473.378671	36.597428
1593.172328	217858.601491	36.602445
1594.860470	218238.071581	36.607463
1597.139494	218613.708324	36.612480
1598.956216	218984.599722	36.617498
1600.768075	219354.147087	36.622516
1602.635935	219722.111389	36.627533
1604.178533	220075.680529	36.632551
1605.798544	220447.372508	36.637568
1606.951880	220810.687636	36.642586
1608.468899	221161.851649	36.647604
1609.923286	221517.446940	36.652621
1611.430449	221867.065429	36.657639
1612.640371	222221.104535	36.662656
1613.968728	222576.013423	36.667674
1615.342657	222941.786619	36.672692
1616.312794	223324.622429	36.677709
1618.145249	223703.171730	36.682727
1619.414702	224095.813859	36.687744
1620.823232	224479.467238	36.692762
1622.277706	224865.323723	36.697780
1623.458593	225261.693032	36.702797
1625.093512	225676.528016	36.707815
1626.990485	226079.279741	36.712832
1628.953351	226479.989385	36.717850
1630.577641	226882.002770	36.722868
1631.271312	227296.013200	36.727885
1633.776144	227701.358194	36.732903
1635.612714	228103.084799	36.737920
1637.205211	228511.179079	36.742938
1639.447147	228909.917507	36.747956
1641.010107	229321.346618	36.752973
1642.471825	229726.266148	36.757991
1644.314971	230136.303310	36.763008
1645.966039	230537.890476	36.768026
1648.088298	230942.624005	36.773044
1649.558236	231360.805807	36.778061
1651.374182	231766.152663	36.783079
1653.076419	232163.315353	36.788096
1654.719055	232570.014711	36.793114
1657.068705	232959.016286	36.798132
1658.734434	233354.181314	36.803149
1660.906284	233741.640179	36.808167
1663.155020	234136.275394	36.813184
1664.233657	234523.287950	36.818202
1666.432976	234903.403533	36.823220
1667.950083	235295.778656	36.828237
1669.543227	235678.615895	36.833255
1671.370870	236063.039493	36.838272
1672.304726	236460.444727	36.843290
1674.101326	236851.352650	36.848308
1675.420496	237250.928884	36.853325
1677.231791	237655.883130	36.858343
1678.459000	238062.817831	36.863360
1679.535423	238477.856976	36.868378
1681.411018	238887.374897	36.873396
1682.256387	239316.578744	36.878413
1683.419194	239748.015277	36.883431
1685.586213	240179.255379	36.888448
1686.569281	240630.258637	36.893466
1687.750068	241071.372725	36.898484
1689.050637	241530.477430	36.903501
1691.361365	241988.622622	36.908519
1692.407045	242453.437255	36.913536
1694.004183	242905.634815	36.918554
1695.974654	243352.460045	36.923572
1697.704816	243812.079192	36.928589
1699.184703	244255.941335	36.933607
1701.132460	244692.204824	36.938624
1702.816409	245143.095208	36.943642
1704.656679	245597.947670	36.948660
1706.527768	246038.366608	36.953677
1708.134634	246492.574217	36.958695
1709.981399	246946.487275	36.963712
1711.403169	247402.099325	36.968730
1713.678351	247843.391000	36.973748
1715.551179	248294.024024	36.978765
1717.509665	248739.587618	36.983783
1719.858855	249179.369082	36.988800
1721.780589	249622.501028	36.993818
1723.653108	250057.995414	36.998836
1725.791684	250498.499811	37.003853
1727.078997	250934.984028	37.008871
1729.525913	251362.709289	37.013888
1731.414361	251792.054521	37.018906
1733.225838	252225.960308	37.023924
1734.772536	252642.078589	37.028941
1736.851010	253061.916547	37.033959
1738.353587	253488.915268	37.038976
1740.131085	253921.150966	37.043994
1741.959713	254348.322815	37.049012
1743.282653	254784.599415	37.054029
1744.787018	255232.276511	37.059047
1746.156702	255678.376321	37.064064
1747.567733	256131.886847	37.069082
1749.133733	256583.033801	37.074100
1750.127200	257053.026274	37.079117
1751.303302	257528.271356	37.084135
1753.160489	258021.131318	37.089152
1754.532167	258511.229104	37.094170
1756.140266	259007.408513	37.099188
1757.841639	259508.220615	37.104205
1759.829545	260009.085145	37.109223
1762.020564	260512.023194	37.114240
1763.448355	261017.708100	37.119258
1765.494245	261521.178544	37.124276
1766.764608	262020.056380	37.129293
1768.590213	262527.323551	37.134311
1770.567945	263049.450544	37.139328
1771.869773	263562.064981	37.144346
1773.614428	264084.357997	37.149364
1775.140108	264617.687491	37.154381
1776.648537	265136.107835	37.159399
1778.322426	265672.916472	37.164416
1779.848166	266210.842151	37.169434
1782.305878	266740.783645	37.174452
1784.378581	267281.459517	37.179469
1786.123220	267821.301658	37.184487
1788.398505	268343.244883	37.189504
1790.160260	268877.087461	37.194522
1792.169312	269377.990381	37.199540
1793.685736	269887.181860	37.204557
1794.887782	270392.107838	37.209575
1796.772094	270901.006074	37.214592
1798.286810	271404.073249	37.219610
1800.348604	271919.925000	37.224628
1802.493293	272440.334025	37.229645
1804.204800	272958.504494	37.234663
1806.318276	273469.797313	37.239680
1808.232720	273986.635406	37.244698
1809.927018	274493.780976	37.249716
1812.057134	275010.910144	37.254733
1813.515065	275530.947331	37.259751
1815.391593	276055.585652	37.264768
1817.062994	276581.096027	37.269786
1818.764959	277097.785369	37.274804
1820.776384	277632.709785	37.279821
1822.246692	278166.353604	37.284839
1824.222793	278704.989757	37.289856
1825.589314	279243.296796	37.294874
1827.551770	279788.638144	37.299892
1829.199998	280332.786893	37.304909
1831.167044	280877.793852	37.309927
1833.375986	281418.566465	37.314944
1835.411140	281972.524880	37.319962
1837.532643	282516.229970	37.324980
1839.036631	283060.089625	37.329997
1840.716973	283619.259398	37.335015
1843.011692	284154.470606	37.340032
1844.891102	284700.241457	37.345050
1846.453660	285242.686176	37.350068
1848.658062	285805.085526	37.355085
1851.242878	286342.271077	37.360103
1854.027018	286873.832359	37.365120
1855.981357	287399.158020	37.370138
1857.989922	287913.499455	37.375156
1860.484292	288423.666363	37.380173
1861.868864	288950.073874	37.385191
1863.989959	289463.932681	37.390208
1865.804437	289979.416607	37.395226
1867.459640	290500.081749	37.400244
1869.290733	291015.736254	37.405261
1870.732642	291544.078624	37.410279
1872.607457	292062.921420	37.415296
1874.311867	292601.297637	37.420314
1875.885764	293139.211053	37.425332
1877.473634	293671.811117	37.430349
1878.981377	294217.477333	37.435367
1880.707718	294771.205624	37.440384
1882.487306	295329.163518	37.445402
1884.332261	295881.875213	37.450420
1886.249201	296440.311691	37.455437
1887.589827	297010.399882	37.460455
1889.321559	297570.106377	37.465472
1890.866409	298144.724870	37.470490
1892.983755	298688.460037	37.475508
1895.128975	299227.565038	37.480525
1896.445227	299793.704710	37.485543
1898.653144	300342.646908	37.490560
1900.828381	300888.823190	37.495578
1902.859255	301432.811401	37.500596
1905.004215	301979.087978	37.505613
1906.637957	302542.235904	37.510631
1908.605536	303091.151912	37.515648
1910.750572	303651.665692	37.520666
1912.357726	304197.944396	37.525684
1914.223154	304754.841803	37.530701
1915.942793	305324.280672	37.535719
1917.707059	305892.616038	37.540736
1919.751804	306476.797150	37.545754
1921.444958	307050.292008	37.550772
1923.448302	307631.297526	37.555789
1924.641606	308224.246047	37.560807
1926.235417	308808.131885	37.565824
1927.940917	309419.598204	37.570842
1930.019749	310012.559522	37.575860
1931.974335	310620.062985	37.580877
1933.963591	311228.799957	37.585895
1936.191902	311825.809961	37.590912
1938.529497	312442.044800	37.595930
1940.574877	313047.405292	37.600948
1943.191210	313645.349856	37.605965
1944.845197	314254.017487	37.610983
1946.989471	314862.697622	37.616000
1948.885167	315468.520253	37.621018
1950.689111	316080.828329	37.626036
1952.850430	316697.030999	37.631053
1954.223243	317312.931287	37.636071
1956.169855	317915.371843	37.641088
1958.578518	318550.736698	37.646106
1960.300361	319169.607124	37.651124
1962.223669	319785.923545	37.656141
1964.365705	320413.774818	37.661159
1966.652462	321027.630489	37.666176
1968.810119	321651.556797	37.671194
1970.838010	322279.282199	37.676212
1972.841565	322897.306606	37.681229
1974.785341	323520.463699	37.686247
1976.908788	324134.367470	37.691264
1979.120247	324750.560353	37.696282
1981.069656	325365.243023	37.701300
1983.067534	325985.318765	37.706317
1985.621850	326582.138920	37.711335
1987.702750	327195.637560	37.716352
1989.735295	327801.318617	37.721370
1991.783294	328398.663624	37.726388
1994.030823	329002.111896	37.731405
1995.428924	329611.512545	37.736423
1997.143914	330227.782869	37.741440
1999.165995	330825.055768	37.746458
2001.609318	331409.557209	37.751476
2003.598330	331990.119165	37.756493
2005.607202	332568.437599	37.761511
2007.541977	333141.558550	37.766528
2009.607177	333726.835752	37.771546
2011.627460	334310.388026	37.776564
2013.317052	334886.019728	37.781581
2015.076481	335485.189450	37.786599
2016.887113	336072.362404	37.791616
2019.079066	336666.012354	37.796634
2020.948394	337266.741682	37.801652
2022.935966	337859.625775	37.806669
2025.053685	338466.644038	37.811687
2026.971496	339077.217224	37.816704
2029.036400	339682.072202	37.821722
2031.005021	340290.921106	37.826740
2033.229212	340899.769477	37.831757
2035.182153	341509.595678	37.836775
2037.325048	342120.473032	37.841792
2039.511902	342748.948937	37.846810
2041.037973	343373.392589	37.851828
2043.054856	343997.744030	37.856845
2044.674152	344627.078689	37.861863
2046.579494	345258.843028	37.866880
2048.836314	345900.055544	37.871898
2050.287760	346548.172758	37.876916
2052.418278	347205.503626	37.881933
2054.238153	347860.873214	37.886951
2055.929894	348538.713790	37.891968
2058.108992	349205.447224	37.896986
2059.860864	349890.489160	37.902004
2061.884255	350564.689210	37.907021
2064.007299	351250.534471	37.912039
2066.072157	351934.526401	37.917056
2067.897430	352625.272656	37.922074
2069.633275	353320.742589	37.927092
2071.840094	354030.558221	37.932109
2073.994926	354738.670704	37.937127
2076.138172	355445.149247	37.942144
2078.203357	356154.496145	37.947162
2079.732919	356873.918950	37.952180
2082.442382	357573.337434	37.957197
2084.478209	358291.582922	37.962215
2086.520567	359010.169629	37.967232
2089.193579	359727.747584	37.972250
2091.201002	360455.472768	37.977268
2093.481201	361162.943861	37.982285
2095.612981	361883.568571	37.987303
2097.476342	362606.052303	37.992320
2099.149120	363335.201452	37.997338
2101.029249	364070.693825	38.002356
2103.072787	364796.555316	38.007373
2104.775725	365540.293667	38.012391
2107.114804	366278.125047	38.017408
2110.172313	366992.888607	38.022426
2112.501083	367702.487036	38.027444
2114.975188	368391.298776	38.032461
2117.384871	369071.839866	38.037479
2120.188723	369741.090111	38.042496
2122.712559	370414.611432	38.047514
2125.023603	371074.562138	38.052532
2127.840536	371728.834452	38.057549
2129.814546	372379.586727	38.062567
2132.162359	373023.238017	38.067584
2134.850208	373668.188811	38.072602
2137.139005	374301.656979	38.077620
2138.899741	374940.732280	38.082637
2141.146948	375594.775966	38.087655
2142.429978	376237.991657	38.092672
2145.200294	376887.559431	38.097690
2146.777407	377542.694626	38.102708
2149.025672	378193.315510	38.107725
2151.349834	378845.888619	38.112743
2153.257783	379512.415393	38.117760
2155.626265	380166.222819	38.122778
2157.080088	380846.086811	38.127796
2158.773122	381517.376600	38.132813
2160.946224	382198.788264	38.137831
2163.020705	382887.783237	38.142848
2164.968868	383578.914759	38.147866
2166.777409	384277.610348	38.152884
2168.944112	384988.499798	38.157901
2170.547131	385698.531689	38.162919
2172.180317	386417.744828	38.167936
2174.714976	387133.390407	38.172954
2176.978483	387875.480355	38.177972
2178.960027	388601.478712	38.182989
2181.505101	389326.298995	38.188007
2183.852654	390067.282551	38.193024
2185.782902	390801.095470	38.198042
2187.859934	391552.861694	38.203060
2189.909249	392284.210345	38.208077
2192.177998	393038.669380	38.213095
2194.359153	393793.529826	38.218112
2196.772733	394549.243715	38.223130
2198.619615	395312.410086	38.228148
2200.535589	396081.956528	38.233165
2202.720002	396846.343006	38.238183
2205.130280	397615.713682	38.243200
2207.835337	398380.350736	38.248218
2209.765138	399159.265080	38.253236
2212.050518	399918.839408	38.258253
2214.172569	400688.024718	38.263271
2216.254963	401454.712721	38.268288
2218.383256	402237.207791	38.273306
2220.577292	403022.279369	38.278324
2222.439520	403804.826555	38.283341
2224.955562	404591.749463	38.288359
2227.266964	405384.663749	38.293376
2229.395935	406158.484579	38.298394
2231.448484	406928.369828	38.303412
2233.739813	407686.159490	38.308429
2235.779073	408452.330328	38.313447
2237.571003	409223.410376	38.318464
2239.487636	409993.205606	38.323482
2241.486640	410776.971538	38.328500
2243.343269	411561.852965	38.333517
2245.625268	412358.390306	38.338535
2247.573358	413163.115727	38.343552
2249.663203	413980.885644	38.348570
2251.524762	414799.124541	38.353588
2253.886676	415622.291435	38.358605
2256.225331	416446.929882	38.363623
2258.271575	417283.873210	38.368640
2260.706198	418116.873463	38.373658
2262.683136	418961.800054	38.378676
2265.229125	419810.601452	38.383693
2267.986158	420641.993891	38.388711
2270.395881	421482.886979	38.393728
2272.900683	422314.823201	38.398746
2275.299818	423163.964793	38.403764
2277.544419	424002.824870	38.408781
2280.821416	424838.087189	38.413799
2283.265506	425690.423583	38.418816
2285.677781	426512.662744	38.423834
2287.503926	427369.854541	38.428852
2289.692793	428212.525760	38.433869
2292.878531	429039.151980	38.438887
2295.281249	429873.071008	38.443904
2298.024880	430699.815532	38.448922
2299.779278	431536.772435	38.453940
2302.303196	432378.021639	38.458957
2304.762867	433205.433938	38.463975
2306.383383	434057.860303	38.468992
2308.615682	434899.522454	38.474010
2310.979622	435744.066145	38.479028
2313.371970	436592.115804	38.484045
2315.838615	437434.554488	38.489063
2317.986558	438279.090631	38.494080
2320.630885	439113.693692	38.499098
2322.691980	439973.005971	38.504116
2325.430697	440823.466601	38.509133
2327.618844	441669.536234	38.514151
2329.749460	442537.236123	38.519168
2331.948302	443392.647160	38.524186
2334.770718	444240.987384	38.529204
2337.170406	445098.522476	38.534221
2339.926763	445950.904029	38.539239
2342.393107	446800.569779	38.544256
2344.522877	447643.532091	38.549274
2346.717762	448494.643269	38.554292
2349.228833	449352.392571	38.559309
2351.405322	450204.449253	38.564327
2353.560041	451068.814283	38.569344
2355.947592	451906.403155	38.574362
2358.009606	452751.295459	38.579380
2360.047786	453587.965710	38.584397
2362.569560	454420.019116	38.589415
2364.870537	455263.806516	38.594432
2367.171998	456089.913863	38.599450
2369.061182	456936.280685	38.604468
2371.241526	457780.438966	38.609485
2373.653512	458620.073586	38.614503
2375.874923	459488.974148	38.619520
2378.116670	460350.453334	38.624538
2380.388428	461222.908970	38.629556
2382.555169	462095.596740	38.634573
2384.921022	462961.388673	38.639591
2387.752045	463846.722512	38.644608
2389.964475	464724.591900	38.649626
2392.574105	465607.205005	38.654644
2394.733794	466498.192511	38.659661
2397.590831	467375.224936	38.664679
2399.744049	468278.258103	38.669696
2401.988307	469173.047909	38.674714
2404.465503	470064.017074	38.679732
2406.951197	470962.925019	38.684749
2409.922576	471865.798987	38.689767
2412.278719	472768.633600	38.694784
2415.011167	473655.297105	38.699802
2417.241760	474582.715598	38.704820
2419.278034	475507.393413	38.709837
2421.955477	476417.824234	38.714855
2424.678768	477333.908881	38.719872
2426.653480	478241.035973	38.724890
2429.878512	479164.972429	38.729908
2432.164907	480080.538981	38.734925
2435.001150	480978.494601	38.739943
2437.447032	481888.387755	38.744960
2440.229935	482783.535612	38.749978
2442.789419	483697.810546	38.754996
2444.961238	484617.304331	38.760013
2447.649323	485524.092555	38.765031
2450.065286	486425.227111	38.770048
2452.478143	487337.622201	38.775066
2454.588458	488240.986822	38.780084
2456.902896	489168.091178	38.785101
2459.322040	490087.860805	38.790119
2461.138172	491025.548677	38.795136
2463.409596	491964.520464	38.800154
2465.795356	492917.398131	38.805172
2467.781875	493873.973980	38.810189
2470.407044	494823.172009	38.815207
2472.302710	495790.098811	38.820224
2474.706697	496760.212661	38.825242
2477.393535	497723.361613	38.830260
2479.846098	498701.576858	38.835277
2482.196249	499678.743247	38.840295
2484.974247	500664.201449	38.845312
2487.407609	501632.664009	38.850330
2489.386715	502591.464657	38.855348
2491.734099	503544.246257	38.860365
2494.640356	504488.758432	38.865383
2496.922401	505446.481937	38.870400
2499.100414	506403.964748	38.875418
2501.516715	507367.248301	38.880436
2503.460599	508339.729497	38.885453
2506.293702	509327.222687	38.890471
2508.310820	510321.346589	38.895488
2510.175287	511313.468474	38.900506
2512.451498	512321.837065	38.905524
2514.619951	513351.325281	38.910541
2517.041733	514368.406797	38.915559
2519.469683	515410.111196	38.920576
2521.891933	516458.095095	38.925594
2524.679212	517499.446238	38.930612
2526.822949	518553.431378	38.935629
2529.699843	519598.000089	38.940647
2532.371796	520668.876427	38.945664
2534.880213	521730.236049	38.950682
2537.554706	522798.896310	38.955700
2539.846529	523883.510399	38.960717
2542.305546	524963.837834	38.965735
2545.188373	526043.108310	38.970752
2547.490676	527131.210805	38.975770
2550.117319	528231.109861	38.980788
2552.619430	529326.920771	38.985805
2555.460655	530416.551340	38.990823
2557.817607	531534.572094	38.995840
2560.260499	532638.601060	39.000858
2563.268194	533739.228514	39.005876
2566.079769	534854.852110	39.010893
2568.774913	535966.433821	39.015911
2571.844384	537072.079015	39.020928
2574.129020	538179.634085	39.025946
2577.384076	539273.756427	39.030964
2579.603489	540387.337867	39.035981
2582.436395	541492.628226	39.040999
2585.010021	542590.784127	39.046016
2587.749528	543690.786718	39.051034
2590.670790	544796.504620	39.056052
2593.613708	545913.645483	39.061069
2596.021503	547008.362757	39.066087
2598.999714	548121.547534	39.071104
2601.165832	549224.022517	39.076122
2604.072916	550324.120273	39.081140
2606.728787	551432.716579	39.086157
2609.356260	552539.970424	39.091175
2611.965338	553646.784652	39.096192
2613.938733	554755.877524	39.101210
2616.942476	555879.072845	39.106228
2619.490945	556990.343816	39.111245
2622.216036	558100.386284	39.116263
2624.713990	559214.041385	39.121280
2627.034596	560329.691988	39.126298
2630.101112	561411.167900	39.131316
2632.655781	562487.016950	39.136333
2635.241947	563564.077329	39.141351
2637.884206	564642.896535	39.146368
2640.385655	565722.704091	39.151386
2643.162774	566797.152689	39.156404
2645.458518	567881.884567	39.161421
2648.288026	568964.776687	39.166439
2651.334521	570051.404366	39.171456
2653.737783	571139.353717	39.176474
2656.380361	572234.043593	39.181492
2658.807855	573328.123074	39.186509
2661.833883	574430.082924	39.191527
2664.995458	575530.166499	39.196544
2667.508780	576637.637949	39.201562
2670.354462	577731.360156	39.206580
2672.827130	578822.842440	39.211597
2675.050231	579935.886162	39.216615
2677.956710	581048.311007	39.221632
2680.055096	582169.296996	39.226650
2683.121473	583287.206727	39.231668
2685.311425	584424.965984	39.236685
2688.035311	585555.960125	39.241703
2691.148803	586697.107096	39.246720
2693.368006	587846.467825	39.251738
2696.486081	588982.985823	39.256756
2698.754915	590143.192269	39.261773
2701.188668	591297.946090	39.266791
2704.203896	592460.052917	39.271808
2706.836059	593620.257097	39.276826
2709.992196	594784.865394	39.281844
2712.609102	595957.012696	39.286861
2715.675324	597116.645737	39.291879
2717.973530	598291.216491	39.296896
2720.523438	599479.243975	39.301914
2723.220491	600662.818361	39.306932
2725.315198	601859.989827	39.311949
2728.145051	603052.005183	39.316967
2731.138338	604252.426330	39.321984
2733.153512	605465.098322	39.327002
2735.854895	606684.128178	39.332020
2738.769242	607910.094478	39.337037
2741.288308	609132.392558	39.342055
2743.865501	610361.550241	39.347072
2746.463000	611599.171715	39.352090
2749.518033	612836.177050	39.357108
2752.055739	614093.284419	39.362125
2754.551729	615343.355712	39.367143
2757.455171	616592.065278	39.372160
2760.553514	617851.096446	39.377178
2763.401983	619095.280230	39.382196
2766.479505	620349.377531	39.387213
2769.631495	621600.568381	39.392231
2772.743964	622847.273841	39.397248
2775.271504	624084.492308	39.402266
2778.331332	625292.104410	39.407284
2780.326332	626499.461978	39.412301
2783.522748	627703.380749	39.417319
2786.467776	628913.697262	39.422336
2789.282104	630127.691975	39.427354
2792.076137	631336.307906	39.432372
2795.025390	632533.875595	39.437389
2797.774501	633732.937336	39.442407
2800.508787	634948.382767	39.447424
2802.693583	636164.478224	39.452442
2805.889647	637374.519833	39.457460
2808.718601	638597.104041	39.462477
2811.651970	639824.064168	39.467495
2814.567624	641047.588173	39.472512
2817.200970	642282.833089	39.477530
2820.106465	643509.603581	39.482548
2822.871413	644752.004977	39.487565
2826.018514	645986.161645	39.492583
2828.926356	647219.609449	39.497600
2831.082257	648473.817515	39.502618
2833.737159	649724.742836	39.507636
2836.556087	650986.594550	39.512653
2839.272052	652250.495369	39.517671
2842.306085	653514.578641	39.522688
2845.171215	654797.256665	39.527706
2848.018692	656073.146197	39.532724
2850.632279	657357.673236	39.537741
2853.505883	658642.285181	39.542759
2856.816231	659932.277945	39.547776
2859.505751	661222.652655	39.552794
2862.545254	662513.839969	39.557812
2865.405905	663812.497941	39.562829
2868.221893	665115.216572	39.567847
2871.194577	666408.178616	39.572864
2873.875263	667721.707480	39.577882
2876.892023	669029.376633	39.582900
2879.980523	670346.151564	39.587917
2882.924823	671664.357820	39.592935
2886.069423	672969.518046	39.597952
2889.049137	674285.012326	39.602970
2891.927307	675600.039780	39.607988
2895.057896	676916.378136	39.613005
2897.533267	678232.939023	39.618023
2900.691189	679554.908246	39.623040
2903.898088	680869.774237	39.628058
2906.449283	682183.271897	39.633076
2909.591158	683508.446931	39.638093
2912.400746	684828.967182	39.643111
2915.671684	686143.854516	39.648128
2918.630360	687468.282561	39.653146
2921.645980	688787.840672	39.658164
2924.838417	690110.498879	39.663181
2927.976759	691421.261475	39.668199
2930.921929	692725.960790	39.673216
2933.975488	694032.731259	39.678234
2936.680325	695299.495910	39.683252
2940.038553	696563.438008	39.688269
2942.760211	697831.917701	39.693287
2945.567470	699082.353449	39.698304
2948.385149	700347.675685	39.703322
2951.051838	701615.168845	39.708340
2953.836843	702879.780888	39.713357
2956.496145	704162.559970	39.718375
2959.587282	705439.724599	39.723392
2961.951382	706743.865351	39.728410
2964.548237	708036.972448	39.733428
2967.005126	709342.186530	39.738445
2969.502690	710673.034701	39.743463
2972.362963	712012.620405	39.748480
2974.768608	713371.668878	39.753498
2977.497599	714732.422071	39.758516
2980.075746	716101.588655	39.763533
2982.672256	717496.051585	39.768551
2985.804071	718895.135466	39.773568
2988.410382	720304.556377	39.778586
2991.283906	721719.130063	39.783604
2994.062459	723153.101371	39.788621
2996.721654	724597.864070	39.793639
3000.124640	726035.327220	39.798656
3003.323557	727492.877308	39.803674
3006.211255	728948.688223	39.808692
3009.501994	730412.811574	39.813709
3012.465582	731879.144999	39.818727
3015.607958	733339.898457	39.823744
3018.663502	734808.693203	39.828762
3021.814697	736288.552379	39.833780
3025.109103	737765.349152	39.838797
3028.450770	739243.244466	39.843815
3031.675686	740705.199047	39.848832
3035.385379	742191.357899	39.853850
3038.966412	743661.085842	39.858868
3042.343811	745112.432119	39.863885
3045.585234	746569.790981	39.868903
3049.293600	748017.582268	39.873920
3052.515631	749469.127533	39.878938
3055.439831	750911.190362	39.883956
3058.539687	752361.276155	39.888973
3061.318737	753806.071009	39.893991
3064.716907	755261.071687	39.899008
3067.571463	756707.569096	39.904026
3070.846325	758146.878890	39.909044
3074.444148	759585.909092	39.914061
3077.567091	761032.370810	39.919079
3080.608255	762459.632731	39.924096
3084.306744	763899.246709	39.929114
3087.167373	765332.384148	39.934132
3090.178235	766762.959029	39.939149
3093.074856	768200.059808	39.944167
3096.604281	769624.882503	39.949184
3099.992552	771032.898359	39.954202
3102.847202	772413.819383	39.959220
3106.181489	773788.308898	39.964237
3108.786436	775158.392753	39.969255
3112.073836	776530.262310	39.974272
3115.107163	777913.106362	39.979290
3117.859376	779274.290223	39.984308
3120.801280	780650.982841	39.989325
3123.514272	782042.166791	39.994343
3126.649099	783427.319928	39.999360
3129.260241	784843.430160	40.004378
3131.917597	786259.300206	40.009396
3134.981354	787681.484569	40.014413
3137.469743	789110.636147	40.019431
3140.643086	790552.952734	40.024448
3143.633361	792011.267495	40.029466
3146.408331	793465.691895	40.034484
3149.337958	794942.848945	40.039501
3152.198991	796434.488319	40.044519
3155.139547	797927.555815	40.049536
3157.945678	799447.236504	40.054554
3160.330685	800969.981141	40.059572
3163.629473	802502.308088	40.064589
3166.440942	804051.685813	40.069607
3169.804990	805602.328996	40.074624
3173.006141	807177.133781	40.079642
3175.860699	808747.576660	40.084660
3178.837732	810333.218223	40.089677
3182.126136	811935.821274	40.094695
3185.251562	813524.251085	40.099712
3189.083636	815130.490245	40.104730
3191.653791	816757.837736	40.109748
3195.142831	818373.651451	40.114765
3198.380382	819989.504390	40.119783
3201.557857	821612.141501	40.124800
3204.368966	823249.848751	40.129818
3207.171389	824900.505001	40.134836
3210.568465	826537.777211	40.139853
3213.385652	828203.774777	40.144871
3216.738096	829855.517511	40.149888
3220.532247	831523.368450	40.154906
3223.291029	833197.439478	40.159924
3226.768327	834869.637432	40.164941
3230.298093	836536.134458	40.169959
3233.952835	838202.758454	40.174976
3237.390641	839874.332048	40.179994
3240.990814	841549.666692	40.185012
3244.613956	843202.096340	40.190029
3247.826362	844871.850271	40.195047
3251.758524	846523.061523	40.200064
3255.219957	848176.247943	40.205082
3258.170961	849826.654755	40.210100
3261.738391	851475.643595	40.215117
3265.370409	853127.966965	40.220135
3268.828241	854757.559398	40.225152
3272.336687	856368.958406	40.230170
3275.651810	857954.653810	40.235188
3279.729162	859522.839415	40.240205
3282.599904	861091.117448	40.245223
3285.923424	862640.403167	40.250240
3289.351883	864198.380821	40.255258
3292.033144	865763.347483	40.260276
3295.614380	867310.807036	40.265293
3298.441652	868886.553503	40.270311
3301.215972	870461.796211	40.275328
3304.232516	872049.932799	40.280346
3307.079642	873641.252008	40.285364
3310.703216	875239.359759	40.290381
3313.664665	876847.781556	40.295399
3316.669619	878459.524836	40.300416
3320.153563	880072.385225	40.305434
3323.219792	881703.707529	40.310452
3326.708861	883327.353951	40.315469
3329.716027	884968.874454	40.320487
3332.818533	886613.772993	40.325504
3336.077174	888276.893637	40.330522
3339.141199	889955.577868	40.335540
3342.246518	891630.194626	40.340557
3345.723621	893323.054555	40.345575
3348.692676	895024.074180	40.350592
3352.009961	896724.908957	40.355610
3354.703657	898449.127510	40.360628
3357.979307	900174.836656	40.365645
3361.858002	901904.050726	40.370663
3365.417433	903631.244559	40.375680
3368.578521	905376.728820	40.380698
3371.946846	907129.610481	40.385716
3375.469583	908879.603075	40.390733
3378.906455	910646.353398	40.395751
3382.257380	912413.991278	40.400768
3385.596195	914162.620521	40.405786
3389.149728	915942.912241	40.410804
3392.865586	917706.084930	40.415821
3396.583584	919480.868854	40.420839
3399.925562	921247.843998	40.425856
3404.042893	923015.544884	40.430874
3408.079826	924775.104384	40.435892
3411.990666	926519.732836	40.440909
3415.649031	928274.848826	40.445927
3419.032541	930021.483515	40.450944
3422.617818	931757.168663	40.455962
3426.125905	933508.181138	40.460980
3430.051482	935249.642267	40.465997
3433.118016	936988.088974	40.471015
3436.465645	938729.828456	40.476032
3440.086391	940472.945242	40.481050
3443.658631	942220.547792	40.486068
3446.825866	943969.156650	40.491085
3450.241258	945720.757545	40.496103
3453.587875	947468.050561	40.501120
3456.962373	949201.959364	40.506125
3460.147343	950906.666521	40.511130
3463.593546	952575.595721	40.516135
3467.124141	954188.136682	40.521140
3469.998485	955731.130602	40.526144
3473.114035	957196.051368	40.531149
3475.789811	958588.267333	40.536154
3478.834994	959908.084658	40.541159
3481.607308	961152.920211	40.546164
3484.132084	962322.328553	40.551168
3486.974978	963413.615713	40.556173
3489.783290	964435.989180	40.561178
3491.989716	965369.715818	40.566183
3494.528386	966234.347386	40.571188
3496.907285	967034.499499	40.576192
3499.142598	967747.598825	40.581197
3500.900813	968406.404569	40.586202
3502.955897	968985.570022	40.591207
3505.005903	969504.729837	40.596212
3506.458696	969973.193354	40.601216
3508.484728	970382.461952	40.606221
3510.153986	970731.142657	40.611226
3511.741219	971029.367615	40.616231
3513.309343	971276.058563	40.621236
3514.532248	971474.406187	40.626240
3516.204758	971617.632260	40.631245
3517.494428	971720.742094	40.636250
3519.021758	971776.984543	40.641255
3520.265307	971784.397125	40.646260
3521.222432	971757.448446	40.651264
3522.231995	971693.929521	40.656269
3522.749067	971601.264080	40.661274
3523.398398	971470.545563	40.666279
3524.590773	971313.335172	40.671284
3525.116147	971136.094366	40.676288
3525.851534	970919.508563	40.681293
3526.338621	970698.166017	40.686298
3527.088539	970435.018614	40.691303
3527.581360	970156.551003	40.696308
3527.966588	969857.161471	40.701312
3528.736898	969541.847945	40.706317
3529.044660	969219.750066	40.711322
3529.627085	968863.453115	40.716327
3530.224903	968505.762043	40.721332
3530.605621	968124.511558	40.726336
3531.237119	967718.736675	40.731341
3531.187769	967307.668544	40.736346
3531.573664	966882.896995	40.741351
3531.856524	966446.663522	40.746356
3532.186000	966007.551169	40.751360
3532.694278	965551.836032	40.756365
3532.564843	965084.057705	40.761370
3532.712615	964616.193961	40.766375
3532.923502	964140.744108	40.771380
3533.527556	963649.231014	40.776384
3534.304717	963138.946859	40.781389
3534.064742	962629.182689	40.786394
3534.035013	962111.797537	40.791399
3534.548208	961583.500905	40.796404
3534.677495	961060.509991	40.801408
3535.120002	960520.179284	40.806413
3535.205787	959975.058853	40.811418
3535.172438	959430.103075	40.816423
3535.510148	958866.906857	40.821428
3535.049751	958316.039989	40.826432
3535.245671	957745.115445	40.831437
3535.170398	957179.570893	40.836442
3535.106089	956609.852377	40.841447
3535.663090	956048.891696	40.846452
3535.619671	955468.470268	40.851456
3535.734755	954888.453602	40.856461
3535.801096	954307.994743	40.861466
3536.064348	953723.423301	40.866471
3536.198658	953129.007345	40.871476
3535.755502	952537.963616	40.876480
3536.497011	951929.490787	40.881485
3536.227457	951337.902275	40.886490
3536.061781	950727.697140	40.891495
3536.151780	950135.945793	40.896500
3536.270107	949551.676646	40.901504
3536.740717	948958.288947	40.906509
3536.707157	948358.030443	40.911514
3536.601378	947748.720156	40.916519
3536.741883	947154.413940	40.921524
3536.492607	946546.516043	40.926528
3536.756601	945939.224140	40.931533
3536.523674	945334.051099	40.936538
3536.571713	944721.770317	40.941543
3536.327686	944112.147374	40.946548
3536.884079	943495.804257	40.951552
3536.449066	942875.438729	40.956557
3536.148898	942271.353797	40.961562
3536.460094	941652.438051	40.966567
3536.478840	941042.982560	40.971572
3536.654034	940431.799866	40.976576
3536.923948	939803.759795	40.981581
3536.681145	939191.640021	40.986586
3536.865641	938569.311324	40.991591
3536.929522	937944.819943	40.996596
3536.721733	937321.546422	41.001600
3536.813652	936694.503802	41.006605
3536.795019	936063.473190	41.011610
3536.671599	935441.974787	41.016615
3536.754059	934813.557462	41.021620
3536.364593	934195.889233	41.026624
3536.784238	933560.261568	41.031629
3536.876602	932935.167446	41.036634
3536.531145	932295.007822	41.041639
3536.595304	931659.307215	41.046644
3536.670020	931035.430327	41.051648
3536.672550	930392.964795	41.056653
3536.679437	929763.861580	41.061658
3536.814886	929121.603040	41.066663
3536.716817	928487.565220	41.071668
3536.775816	927849.871276	41.076672
3536.859777	927197.592379	41.081677
3536.853671	926563.309278	41.086682
3536.942262	925922.016937	41.091687
3537.393852	925278.567672	41.096692
3537.200615	924636.880774	41.101696
3536.950551	923978.210843	41.106701
3536.694863	923333.302670	41.111706
3536.854524	922670.076397	41.116711
3537.148809	922029.339824	41.121716
3536.846694	921381.801408	41.126720
3536.913859	920720.946681	41.131725
3536.826565	920063.403641	41.136730
3536.982438	919422.284279	41.141735
3536.914374	918761.789799	41.146740
3536.674205	918115.965232	41.151744
3536.620200	917455.116441	41.156749
3536.411980	916804.414891	41.161754
3536.584503	916157.709173	41.166759
3536.769821	915507.651393	41.171764
3536.453842	914856.927622	41.176768
3536.663063	914204.688484	41.181773
3536.502477	913550.219664	41.186778
3536.652136	912890.707710	41.191783
3537.023916	912236.953908	41.196788
3536.931000	911576.169151	41.201792
3537.153517	910907.061688	41.206797
3537.215149	910254.280645	41.211802
3536.967728	909582.490524	41.216807
3536.689793	908910.141737	41.221812
3536.359374	908263.648983	41.226816
3536.427075	907598.406984	41.231821
3536.589373	906936.443249	41.236826
3536.854804	906267.440129	41.241831
3536.686674	905601.516239	41.246836
3536.328402	904953.387796	41.251840
3536.495391	904277.120808	41.256845
3536.175173	903623.043182	41.261850
3536.348601	902952.402443	41.266855
3536.668815	902294.972219	41.271860
3536.665267	901637.230366	41.276864
3536.882176	900961.903957	41.281869
3536.832082	900294.843148	41.286874
3536.455933	899620.807745	41.291879
3536.631487	898954.804126	41.296884
3536.329943	898286.195847	41.301888
3536.426363	897611.162863	41.306893
3536.568549	896948.597424	41.311898
3536.459627	896272.183639	41.316903
3536.388965	895601.285687	41.321908
3536.143065	894941.642691	41.326912
3536.408600	894241.733374	41.331917
3536.276265	893569.059224	41.336922
3536.134335	892903.072920	41.341927
3536.285500	892241.308603	41.346932
3536.253385	891563.063516	41.351936
3536.584794	890884.095600	41.356941
3536.681503	890219.108637	41.361946
3536.690902	889541.776870	41.366951
3536.762137	888849.942652	41.371956
3536.599983	888175.670604	41.376960
3536.432827	887490.000912	41.381965
3536.612267	886818.123433	41.386970
3536.675230	886127.704532	41.391975
3536.606636	885443.225840	41.396980
3536.146050	884772.187032	41.401984
3535.936510	884081.376370	41.406989
3535.957230	883407.192974	41.411994
3535.736683	882735.683497	41.416999
3535.981063	882059.659299	41.422004
3535.909368	881392.326818	41.427008
3535.944806	880712.210927	41.432013
3535.847995	880035.816228	41.437018
3535.650155	879356.744567	41.442023
3536.108880	878685.136514	41.447028
3535.516792	878012.467925	41.452032
3535.960801	877333.051897	41.457037
3535.952904	876660.031544	41.462042
3535.734867	875982.123083	41.467047
3535.855256	875300.588577	41.472052
3535.836317	874631.216038	41.477056
3535.934844	873949.432151	41.482061
3535.669176	873268.116679	41.487066
3535.576521	872587.081185	41.492071
3535.588937	871901.293233	41.497076
3535.591158	871233.569756	41.502080
3535.715055	870555.562641	41.507085
3535.488428	869880.546271	41.512090
3535.716093	869198.776530	41.517095
3535.828881	868521.898556	41.522100
3535.630193	867844.802916	41.527104
3535.502685	867159.657744	41.532109
3535.718850	866489.424976	41.537114
3535.573438	865798.690096	41.542119
3535.699886	865104.721683	41.547124
3535.325015	864428.241550	41.552128
3535.167491	863751.939741	41.557133
3535.518682	863072.463669	41.562138
3535.121034	862389.929906	41.567143
3535.163328	861703.065696	41.572148
3535.333864	861037.189983	41.577152
3535.121871	860344.287174	41.582157
3535.155589	859669.440303	41.587162
3535.105289	858989.380578	41.592167
3535.225151	858314.563213	41.597172
3535.397105	857638.689944	41.602176
3535.542344	856947.673320	41.607181
3535.644955	856255.807847	41.612186
3535.505773	855574.313171	41.617191
3535.737928	854884.118846	41.622196
3534.901711	854203.563729	41.627200
3535.072023	853511.863813	41.632205
3534.983974	852837.646363	41.637210
3534.829161	852160.544273	41.642215
3535.234647	851473.733710	41.647220
3534.879167	850799.339402	41.652224
3534.897900	850105.336966	41.657229
3534.978300	849427.506297	41.662234
3534.881481	848752.845298	41.667239
3535.548291	848060.743431	41.672244
3534.952938	847378.130242	41.677248
3535.294940	846691.970466	41.682253
3535.135855	845988.967480	41.687258
3535.011860	845309.359951	41.692263
3535.053133	844613.280590	41.697268
3535.159719	843939.623922	41.702272
3535.039408	843239.716734	41.707277
3535.192783	842556.352657	41.712282
3535.148428	841862.420109	41.717287
3535.297576	841172.375426	41.722292
3535.073656	840485.829204	41.727296
3534.950567	839787.196991	41.732301
3535.091256	839098.195238	41.737306
3534.860742	838408.889435	41.742311
3535.212854	837706.435729	41.747316
3534.267855	837024.612904	41.752320
3534.718407	836339.210372	41.757325
3534.873924	835644.758649	41.762330
3534.666344	834956.051184	41.767335
3534.622643	834268.998414	41.772340
3534.818044	833576.609077	41.777344
3534.650633	832885.280816	41.782349
3534.984646	832205.020109	41.787354
3534.630368	831508.596653	41.792359
3534.566352	830806.531096	41.797364
3534.486374	830127.342485	41.802368
3534.605024	829425.290992	41.807373
3534.606426	828741.889666	41.812378
3534.286483	828045.477991	41.817383
3534.684068	827362.791896	41.822388
3534.366097	826678.446310	41.827392
3534.568128	825983.874462	41.832397
3534.748981	825293.581457	41.837402
3534.295183	824603.372718	41.842407
3534.222697	823907.942780	41.847412
3534.263002	823219.263347	41.852416
3534.069279	822533.484844	41.857421
3534.144180	821849.642404	41.862426
3534.366030	821163.650094	41.867431
3534.566811	820473.922241	41.872436
3534.480205	819782.557392	41.877440
3534.296974	819087.761685	41.882445
3534.426895	818391.225269	41.887450
3534.306253	817699.746491	41.892455
3534.439695	817003.112649	41.897460
3534.049070	816320.930747	41.902464
3534.043597	815618.205686	41.907469
3533.987265	814933.328753	41.912474
3533.994472	814245.091146	41.917479
3534.094433	813552.409965	41.922484
3533.420592	812863.608046	41.927488
3533.838918	812177.633667	41.932493
3533.711386	811495.306139	41.937498
3533.401375	810807.798272	41.942503
3533.660363	810123.453677	41.947508
3533.210183	809451.063833	41.952512
3533.429089	808766.931482	41.957517
3533.430074	808090.753156	41.962522
3533.546693	807413.409647	41.967527
3533.906270	806723.216132	41.972532
3533.361676	806047.662421	41.977536
3533.510021	805353.004172	41.982541
3533.743271	804670.368197	41.987546
3533.319969	803981.157897	41.992551
3533.328072	803296.167977	41.997556
3533.162164	802618.690335	42.002560
3533.273527	801925.112034	42.007565
3533.392772	801251.324730	42.012570
3533.199510	800564.919503	42.017575
3532.988450	799879.969535	42.022580
3532.980799	799207.083071	42.027584
3532.833163	798521.889404	42.032589
3532.932377	797854.249875	42.037594
3532.532469	797175.099352	42.042599
3532.784764	796505.488169	42.047604
3532.579774	795834.908906	42.052608
3532.376988	795164.264643	42.057613
3532.331775	794487.785325	42.062618
3532.582354	793819.143416	42.067623
3532.393650	793145.160624	42.072628
3532.393066	792477.611773	42.077632
3532.505802	791802.908236	42.082637
3532.224419	791141.124193	42.087642
3531.967768	790468.369243	42.092647
3532.228348	789803.223240	42.097652
3532.273139	789147.729588	42.102656
3532.221971	788470.474807	42.107661
3532.279603	787806.649404	42.112666
3531.919844	787140.965645	42.117671
3532.484810	786472.260188	42.122676
3532.187484	785814.698034	42.127680
3532.168511	785135.448171	42.132685
3532.049027	784475.028350	42.137690
3531.893125	783807.965505	42.142695
3532.510656	783139.429948	42.147700
3532.098352	782472.581336	42.152704
3531.806464	781806.141900	42.157709
3531.990523	781140.493816	42.162714
3531.454109	780469.693173	42.167719
3531.841760	779804.034250	42.172724
3531.851835	779154.711728	42.177728
3531.598225	778481.316343	42.182733
3531.659331	777822.713942	42.187738
3531.393817	777158.202152	42.192743
3531.536964	776504.829933	42.197748
3531.407954	775851.346967	42.202752
3531.457826	775190.145071	42.207757
3531.536002	774528.582964	42.212762
3531.568216	773868.298002	42.217767
3531.508960	773197.776890	42.222772
3531.299200	772547.261389	42.227776
3531.340271	771885.663461	42.232781
3531.664964	771232.970314	42.237786
3530.798599	770575.103022	42.242791
3531.161691	769906.425552	42.247796
3530.848847	769261.646453	42.252800
3530.805200	768609.030019	42.257805
3530.997505	767953.802816	42.262810
3530.833941	767303.308952	42.267815
3530.989700	766650.140904	42.272820
3530.615118	766006.025158	42.277824
3530.648136	765350.102418	42.282829
3531.025267	764703.330433	42.287834
3530.664539	764056.874834	42.292839
3530.789897	763413.139849	42.297844
3530.955654	762759.875710	42.302848
3530.820876	762112.227377	42.307853
3530.882830	761461.530651	42.312858
3530.438002	760810.370907	42.317863
3530.533088	760150.036397	42.322868
3531.080156	759512.356447	42.327872
3530.790378	758862.432462	42.332877
3530.750400	758206.242896	42.337882
3530.711835	757554.782275	42.342887
3530.771706	756899.399975	42.347892
3530.600522	756257.867691	42.352896
3530.599224	755601.298220	42.357901
3530.539605	754953.615847	42.362906
3530.517992	754307.550299	42.367911
3530.606363	753652.821662	42.372916
3530.276016	753010.747255	42.377920
3530.594615	752363.373334	42.382925
3530.641781	751702.066407	42.387930
3530.451000	751062.767912	42.392935
3530.628430	750409.821475	42.397940
3530.211585	749766.354876	42.402944
3530.004208	749118.847274	42.407949
3529.947442	748471.111539	42.412954
3529.537251	747839.487448	42.417959
3529.656256	747190.033736	42.422964
3529.652010	746573.603018	42.427968
3529.816951	745930.756202	42.432973
3529.682026	745290.576189	42.437978
3529.619797	744656.360904	42.442983
3529.530140	744018.243479	42.447988
3529.450586	743391.639268	42.452992
3529.676494	742755.194027	42.457997
3529.786269	742112.537074	42.463002
3529.634725	741485.446902	42.468007
3529.804208	740840.302545	42.473012
3529.624822	740210.593830	42.478016
3529.574245	739568.547956	42.483021
3529.596431	738933.015643	42.488026
3529.043811	738302.031629	42.493031
3529.220113	737671.417112	42.498036
3529.381967	737047.977804	42.503040
3529.029317	736416.216185	42.508045
3529.138155	735791.994930	42.513050
3528.970927	735164.159724	42.518055
3529.084902	734532.812597	42.523060
3528.878659	733917.653772	42.528064
3529.100928	733288.367654	42.533069
3529.324449	732661.110926	42.538074
3528.648179	732031.087740	42.543079
3529.083810	731407.211703	42.548084
3529.173146	730789.980845	42.553088
3528.666135	730171.368721	42.558093
3528.676998	729545.490347	42.563098
3528.588760	728929.138127	42.568103
3528.886827	728302.421448	42.573108
3528.654814	727681.195091	42.578112
3528.683348	727063.542227	42.583117
3528.665558	726438.568606	42.588122
3528.681112	725824.886119	42.593127
3528.975132	725197.435906	42.598132
3528.407092	724589.556986	42.603136
3528.474301	723964.330224	42.608141
3528.605354	723342.117364	42.613146
3528.258797	722726.034688	42.618151
3528.370741	722097.783934	42.623156
3528.390458	721492.846790	42.628160
3528.056310	720870.724988	42.633165
3528.169684	720264.839285	42.638170
3528.429462	719650.356991	42.643175
3528.363854	719033.752754	42.648180
3528.231762	718421.080873	42.653184
3528.082128	717802.614632	42.658189
3528.306360	717193.262763	42.663194
3527.968198	716579.201245	42.668199
3528.298236	715972.073216	42.673204
3528.140173	715367.365417	42.678208
3527.762485	714742.560911	42.683213
3528.017777	714137.495473	42.688218
3527.804011	713528.894400	42.693223
3528.207989	712919.945412	42.698228
3528.291411	712314.976849	42.703232
3528.260490	711693.906197	42.708237
3527.940417	711075.022941	42.713242
3527.986762	710462.136605	42.718247
3528.095253	709848.947216	42.723252
3528.238813	709243.451240	42.728256
3528.034890	708634.992976	42.733261
3527.631414	708021.163593	42.738266
3527.769707	707418.418331	42.743271
3527.794716	706805.818654	42.748276
3527.579408	706197.288002	42.753280
3527.454244	705590.834152	42.758285
3527.593643	704985.434571	42.763290
3527.313269	704380.660049	42.768295
3527.598540	703770.729790	42.773300
3527.653039	703168.395923	42.778304
3527.460532	702564.571917	42.783309
3527.370959	701963.718733	42.788314
3527.295507	701350.301046	42.793319
3527.254255	700754.721766	42.798324
3526.936646	700159.943919	42.803329
3527.069641	699568.179261	42.808333
3527.411233	698971.021163	42.813338
3526.657388	698382.209954	42.818343
3526.811882	697779.783773	42.823348
3526.650966	697202.671378	42.828353
3526.924985	696602.927561	42.833357
3527.232229	696001.894268	42.838362
3527.230383	695415.290933	42.843367
3527.076861	694814.553570	42.848372
3527.103663	694215.285996	42.853377
3526.732660	693623.604381	42.858381
3526.518392	693023.352372	42.863386
3526.272664	692439.378105	42.868391
3526.171507	691847.929775	42.873396
3526.656840	691275.293426	42.878401
3526.438714	690686.125689	42.883405
3526.410276	690112.358212	42.888410
3526.038960	689523.786616	42.893415
3526.494072	688942.000802	42.898420
3526.312231	688368.495938	42.903425
3526.270160	687778.111443	42.908429
3526.328421	687202.152339	42.913434
3526.381800	686615.606577	42.918439
3526.338201	686030.482542	42.923444
3526.182841	685450.217467	42.928449
3525.964639	684878.188811	42.933453
3526.211704	684297.382877	42.938458
3525.767127	683724.025715	42.943463
3525.741312	683144.337574	42.948468
3526.053466	682575.110133	42.953473
3525.734351	682008.842853	42.958477
3525.988192	681427.254948	42.963482
3525.533663	680855.909898	42.968487
3525.770358	680280.028591	42.973492
3525.733922	679718.401936	42.978497
3525.788107	679146.016718	42.983501
3525.666106	678570.487827	42.988506
3525.635376	678009.702181	42.993511
3525.711963	677429.535003	42.998516
3525.681060	676868.032355	43.003521
3525.423316	676300.356230	43.008525
3525.966787	675726.927951	43.013530
3525.376262	675152.063269	43.018535
3525.684922	674589.766628	43.023540
3525.556151	674025.816265	43.028545
3525.418604	673453.908912	43.033549
3525.670849	672888.479050	43.038554
3525.384005	672331.879663	43.043559
3525.489823	671757.135279	43.048564
3525.319048	671190.129726	43.053569
3525.043114	670621.911376	43.058573
3525.210423	670062.557205	43.063578
3525.038043	669503.875965	43.068583
3524.952328	668944.349015	43.073588
3524.985600	668380.779344	43.078593
3524.912241	667825.422593	43.083597
3524.926683	667264.881522	43.088602
3525.043370	666713.566498	43.093607
3525.021536	666156.656869	43.098612
3525.112045	665610.020646	43.103617
3524.733084	665056.998296	43.108621
3525.069566	664484.266443	43.113626
3524.800198	663935.550387	43.118631
3524.819320	663379.369629	43.123636
3524.483516	662829.304333	43.128641
3524.762702	662276.358152	43.133645
3524.771996	661726.569965	43.138650
3524.696928	661177.413521	43.143655
3524.678980	660616.587927	43.148660
3524.602207	660069.364948	43.153665
3524.522209	659523.758637	43.158669
3524.398754	658968.794976	43.163674
3523.935560	658424.739558	43.168679
3524.259935	657884.412977	43.173684
3524.494271	657344.820605	43.178689
3523.970469	656795.492408	43.183693
3524.160636	656249.256740	43.188698
3524.166762	655713.108082	43.193703
3524.037451	655158.527499	43.198708
3524.152513	654633.885867	43.203713
3523.812861	654097.857677	43.208717
3524.019126	653553.716288	43.213722
3523.723984	653026.761556	43.218727
3523.937552	652484.307925	43.223732
3523.697474	651962.531448	43.228737
3523.609725	651417.573175	43.233741
3524.153195	650888.263174	43.238746
3523.299945	650358.813670	43.243751
3523.742886	649822.919462	43.248756
3524.045044	649289.118900	43.253761
3523.817403	648763.874479	43.258765
3523.948644	648234.343727	43.263770
3523.771393	647693.893762	43.268775
3523.904532	647149.063803	43.273780
3523.881625	646607.879198	43.278785
3523.895912	646071.806983	43.283789
3523.751274	645533.933936	43.288794
3523.323418	645001.128998	43.293799
3523.628219	644462.672150	43.298804
3523.409302	643944.822075	43.303809
3522.992680	643412.331276	43.308813
3523.344299	642889.580447	43.313818
3523.178891	642375.340634	43.318823
3522.930057	641845.938804	43.323828
3522.899601	641332.223175	43.328833
3522.635661	640814.271002	43.333837
3523.139737	640293.961037	43.338842
3522.983803	639789.240628	43.343847
3522.958432	639262.267094	43.348852
3522.812260	638739.488419	43.353857
3522.873812	638225.650969	43.358861
3522.762752	637711.467146	43.363866
3522.290206	637197.369365	43.368871
3522.610017	636689.463952	43.373876
3522.406305	636186.525706	43.378881
3522.145923	635684.122995	43.383885
3522.545935	635168.474437	43.388890
3522.080202	634678.065962	43.393895
3522.267156	634168.758610	43.398900
3522.257404	633660.961107	43.403905
3522.355527	633160.376647	43.408909
3522.759168	632657.864315	43.413914
3522.305601	632161.780165	43.418919
3522.399453	631659.823249	43.423924
3522.279503	631154.875618	43.428929
3522.243350	630650.139639	43.433933
3522.239218	630150.179437	43.438938
3522.035553	629655.035263	43.443943
3522.030452	629153.275777	43.448948
3522.199637	628652.914534	43.453953
3521.879625	628163.727935	43.458957
3522.317707	627657.415851	43.463962
3521.715941	627166.528911	43.468967
3521.774946	626670.298761	43.473972
3521.797501	626180.912087	43.478977
3521.278649	625688.640704	43.483981
3521.232458	625191.608362	43.488986
3521.617024	624723.878067	43.493991
3521.192751	624229.870478	43.498996
3521.471210	623750.946718	43.504001
3521.194668	623274.049808	43.509005
3521.210870	622789.718196	43.514010
3521.149688	622313.443138	43.519015
3521.094403	621833.138275	43.524020
3521.248126	621362.094672	43.529025
3521.239697	620875.526921	43.534029
3521.282302	620392.385666	43.539034
3521.317852	619923.203437	43.544039
3521.358740	619439.067943	43.549044
3521.243150	618956.641299	43.554049
3520.965800	618481.637427	43.559053
3521.444707	618006.634050	43.564058
3520.936567	617535.436982	43.569063
3520.873729	617056.124579	43.574068
3520.865537	616586.204515	43.579073
3520.302017	616121.120750	43.584077
3520.639202	615646.389853	43.589082
3520.479225	615185.458132	43.594087
3520.750917	614716.462840	43.599092
3520.840548	614255.249005	43.604097
3520.174107	613783.967866	43.609101
3520.564642	613317.650105	43.614106
3520.279491	612855.138220	43.619111
3520.419676	612397.097106	43.624116
3520.332672	611932.507271	43.629121
3520.051869	611482.372519	43.634125
3520.512077	611021.311649	43.639130
3520.143470	610567.895386	43.644135
3520.170487	610112.637877	43.649140
3520.447624	609647.489282	43.654145
3520.177899	609192.345225	43.659149
3520.264217	608730.601560	43.664154
3520.050311	608296.477160	43.669159
3520.167078	607834.691410	43.674164
3520.083169	607375.228413	43.679169
3519.751845	606918.949248	43.684173
3520.061128	606477.341302	43.689178
3519.986788	606029.861717	43.694183
3520.173825	605575.697311	43.699188
3519.965728	605128.857122	43.704193
3519.854384	604674.356302	43.709197
3520.145435	604223.431446	43.714202
3520.002125	603776.828008	43.719207
3520.345149	603334.439507	43.724212
3520.358532	602874.676897	43.729217
3519.662448	602423.849309	43.734221
3520.054611	601963.232568	43.739226
3520.096864	601515.956905	43.744231
3520.084765	601064.406901	43.749236
3520.053411	600616.205287	43.754241
3519.928711	600173.121920	43.759245
3519.923600	599719.811284	43.764250
3519.982816	599277.565585	43.769255
3519.849972	598821.982553	43.774260
3519.959960	598373.418566	43.779265
3519.377365	597929.473777	43.784269
3519.687769	597484.857455	43.789274
3519.484673	597051.708900	43.794279
3519.331073	596608.293009	43.799284
3519.390108	596168.941252	43.804289
3519.336583	595741.593118	43.809293
3519.803740	595294.506320	43.814298
3519.590645	594863.437365	43.819303
3519.485644	594429.421376	43.824308
3519.506847	593978.091810	43.829313
3518.910699	593551.760739	43.834317
3518.565370	593103.674379	43.839322
3518.796844	592682.544509	43.844327
3518.841295	592247.970365	43.849332
3518.714706	591819.537478	43.854337
3518.789652	591407.078594	43.859341
3518.645063	590982.385821	43.864346
3518.642762	590563.078945	43.869351
3518.546780	590144.175137	43.874356
3518.841554	589714.740142	43.879361
3518.797598	589305.594484	43.884365
3518.789772	588876.683319	43.889370
3518.504918	588457.601655	43.894375
3518.482209	588029.014270	43.899380
3518.770286	587612.015958	43.904385
3518.692650	587196.372052	43.909389
3518.696546	586771.604329	43.914394
3518.449759	586365.458008	43.919399
3518.357626	585939.420928	43.924404
3518.528094	585526.390639	43.929409
3518.390249	585122.545834	43.934413
3518.720962	584700.111865	43.939418
3518.360980	584287.330780	43.944423
3518.202447	583871.686468	43.949428
3518.060636	583451.300119	43.954433
3518.006025	583048.176117	43.959437
3518.170419	582633.892008	43.964442
3518.111030	582232.450907	43.969447
3518.125921	581825.353448	43.974452
3518.318557	581408.157345	43.979457
3518.199862	581007.339612	43.984461
3517.907588	580601.158751	43.989466
3517.512026	580195.233444	43.994471
3517.545720	579798.221570	43.999476
3517.694388	579402.534840	44.004481
3518.114474	579009.755764	44.009485
3518.184224	578599.625344	44.014490
3517.969747	578196.519666	44.019495
3517.934408	577795.582928	44.024500
3517.858433	577396.400274	44.029505
3517.596733	577003.070280	44.034509
3517.868577	576603.148887	44.039514
3518.073395	576197.894800	44.044519
3517.929509	575791.781698	44.049524
3517.831456	575391.733588	44.054529
3517.461375	575000.823323	44.059533
3517.972386	574593.503060	44.064538
3517.672412	574192.797064	44.069543
3517.816952	573800.755327	44.074548
3517.842254	573405.351171	44.079553
3517.784714	573009.948695	44.084557
3517.770203	572609.495496	44.089562
3517.193511	572216.873402	44.094567
3517.342409	571819.536750	44.099572
3517.479179	571432.403394	44.104577
3517.233676	571047.889527	44.109581
3517.064831	570643.324675	44.114586
3517.090592	570266.187667	44.119591
3517.272755	569873.363168	44.124596
3517.611990	569487.041522	44.129601
3517.180268	569103.909481	44.134605
3517.290858	568711.665178	44.139610
3516.605513	568331.371375	44.144615
3517.035257	567950.422901	44.149620
3517.081443	567561.626857	44.154625
3516.377915	567189.606495	44.159629
3516.942376	566805.883081	44.164634
3516.271075	566438.314976	44.169639
3516.485762	566070.736083	44.174644
3516.545692	565687.921107	44.179649
3516.661676	565326.730568	44.184653
3516.576120	564947.643451	44.189658
3516.612392	564585.640338	44.194663
3516.486904	564207.897531	44.199668
3516.680494	563835.022920	44.204673
3516.349055	563471.893519	44.209677
3517.155532	563095.721258	44.214682
3517.076350	562729.859655	44.219687
3516.918422	562351.262752	44.224692
3517.112639	561966.653289	44.229697
3516.719146	561590.994879	44.234701
3516.610770	561224.592470	44.239706
3516.556330	560848.049144	44.244711
3516.773431	560477.793592	44.249716
3516.631795	560100.991895	44.254721
3516.348769	559744.599200	44.259725
3516.645471	559370.421125	44.264730
3516.517653	559005.370143	44.269735
3516.372253	558639.506225	44.274740
3516.441961	558267.702693	44.279745
3516.076764	557904.424555	44.284749
3516.210196	557533.143513	44.289754
3515.675040	557173.097872	44.294759
3515.771097	556816.611752	44.299764
3515.630534	556466.301864	44.304769
3515.441137	556117.754153	44.309773
3515.768000	555765.532558	44.314778
3515.673392	555416.194679	44.319783
3515.488742	555055.225828	44.324788
3515.816575	554711.993827	44.329793
3515.464618	554368.869083	44.334797
3515.583857	554013.865849	44.339802
3515.552384	553671.827308	44.344807
3515.443790	553323.747139	44.349812
3515.470469	552976.944878	44.354817
3515.196357	552636.483358	44.359821
3515.281406	552282.951840	44.364826
3514.933388	551957.400595	44.369831
3515.164266	551618.893124	44.374836
3515.323143	551269.202525	44.379841
3515.159377	550946.870949	44.384845
3515.219346	550605.847687	44.389850
3515.352800	550267.222289	44.394855
3515.278724	549926.658415	44.399860
3515.642363	549588.329587	44.404865
3515.202907	549259.806109	44.409869
3515.686831	548903.951249	44.414874
3515.380104	548561.276158	44.419879
3515.201664	548217.713721	44.424884
3515.685678	547878.061896	44.429889
3515.184747	547553.136993	44.434893
3515.172961	547205.790730	44.439898
3515.048615	546870.149547	44.444903
3515.269726	546527.484726	44.449908
3515.163866	546199.133350	44.454913
3514.948205	545870.137551	44.459917
3514.902930	545530.719780	44.464922
3514.827625	545200.524572	44.469927
3514.618826	544876.494931	44.474932
3514.967512	544555.589179	44.479937
3514.522363	544233.097341	44.484941
3514.504695	543894.340608	44.489946
3514.502420	543581.287171	44.494951
3514.527460	543252.339393	44.499956
3514.625470	542924.278993	44.504961
3514.480314	542611.026466	44.509965
3514.174933	542285.288976	44.514970
3514.341990	541975.498621	44.519975
3514.461675	541657.086511	44.524980
3514.597558	541331.453198	44.529985
3514.367556	541021.911275	44.534989
3514.407341	540692.194786	44.539994
3514.145108	540390.309864	44.544999
3513.752220	540077.547356	44.550004
3514.277939	539764.570637	44.555009
3513.636943	539459.401826	44.560013
3514.170938	539144.342129	44.565018
3514.120720	538835.629350	44.570023
3513.696977	538530.403402	44.575028
3513.926296	538223.344451	44.580033
3513.885132	537924.445915	44.585037
3513.821587	537616.969898	44.590042
3513.760683	537311.050500	44.595047
3513.680931	537013.753576	44.600052
3513.930407	536703.278675	44.605057
3513.610114	536405.707484	44.610061
3513.837894	536095.424861	44.615066
3513.900345	535795.101943	44.620071
3513.657961	535511.523311	44.625076
3513.866392	535199.509332	44.630081
3513.539367	534902.664810	44.635085
3513.727103	534588.017640	44.640090
3513.733508	534300.386916	44.645095
3513.622518	534003.688774	44.650100
3513.914248	533695.210194	44.655105
3513.406251	533414.057413	44.660109
3513.375257	533117.731054	44.665114
3513.452474	532814.971967	44.670119
3513.384061	532522.070960	44.675124
3513.364618	532230.467643	44.680129
3513.183808	531950.340708	44.685133
3513.308754	531653.049496	44.690138
3513.410756	531375.487236	44.695143
3513.154275	531080.924011	44.700148
3513.510275	530787.814685	44.705153
3513.363309	530512.297112	44.710157
3513.202061	530209.070321	44.715162
3512.981163	529919.423379	44.720167
3513.345838	529640.622539	44.725172
3513.296744	529350.480796	44.730177
3513.141358	529065.499523	44.735181
3513.127935	528774.583246	44.740186
3512.974522	528493.476900	44.745191
3513.141810	528216.348357	44.750196
3513.011208	527927.807640	44.755201
3512.950736	527651.313069	44.760205
3512.967409	527369.701983	44.765210
3512.743494	527094.436348	44.770215
3512.552809	526823.400140	44.775220
3512.694404	526537.814557	44.780225
3512.621634	526269.171116	44.785229
3512.606843	525995.363794	44.790234
3512.911170	525720.083434	44.795239
3512.954723	525441.863983	44.800244
3512.980454	525159.603627	44.805249
3512.705835	524893.191131	44.810253
3512.865347	524617.713206	44.815258
3512.791222	524337.726246	44.820263
3512.734905	524064.092515	44.825268
3512.697568	523792.419618	44.830273
3512.340222	523535.993911	44.835277
3512.819403	523250.035333	44.840282
3512.732267	522982.900469	44.845287
3512.528392	522712.902711	44.850292
3512.554334	522438.821385	44.855297
3512.277304	522169.533290	44.860301
3512.529536	521895.403455	44.865306
3512.572361	521627.767932	44.870311
3512.109238	521373.444318	44.875316
3512.264123	521106.285411	44.880321
3512.127704	520849.119819	44.885325
3512.465100	520583.536507	44.890330
3512.370276	520324.132928	44.895335
3512.041151	520067.441507	44.900340
3512.146859	519803.550679	44.905345
3512.171375	519541.436756	44.910349
3512.383246	519273.882399	44.915354
3512.336289	519021.367528	44.920359
3512.036635	518764.144083	44.925364
3512.697240	518498.065211	44.930369
3512.287864	518240.094091	44.935373
3512.404891	517971.472492	44.940378
3512.307378	517717.126442	44.945383
3511.933163	517457.519862	44.950388
3512.192761	517196.083308	44.955393
3511.653924	516944.729466	44.960397
3511.966604	516684.891551	44.965402
3511.762251	516440.140040	44.970407
3511.584307	516183.155684	44.975412
3512.085410	515928.021206	44.980417
3511.742759	515684.645251	44.985421
3511.769699	515432.260904	44.990426
3511.508765	515181.740232	44.995431
3511.547776	514938.843094	45.000436
3511.717573	514686.018072	45.005441
3511.330361	514445.459357	45.010445
3511.557982	514194.889879	45.015450
3511.130625	513958.624759	45.020455
3511.299370	513721.445925	45.025460
3511.574235	513477.071090	45.030465
3510.982704	513245.117661	45.035469
3511.184278	513007.215046	45.040474
3511.205678	512763.226007	45.045479
3510.861319	512527.026122	45.050484
3511.231625	512296.208092	45.055489
3511.091529	512064.564318	45.060493
3511.087744	511832.590684	45.065498
3511.266115	511601.087820	45.070503
3510.799398	511374.795210	45.075508
3511.148849	511136.687427	45.080513
3510.732079	510911.188123	45.085517
3511.144498	510679.631769	45.090522
3511.116914	510448.753544	45.095527
3510.816613	510218.676514	45.100532
3511.075397	509985.266487	45.105537
3510.836215	509759.316162	45.110541
3510.879325	509518.709581	45.115546
3510.980489	509294.058987	45.120551
3510.913988	509079.339138	45.125556
3511.402030	508844.306547	45.130561
3510.930109	508620.350742	45.135565
3510.944299	508387.616018	45.140570
3511.040917	508170.834496	45.145575
3510.690555	507944.068733	45.150580
3510.817346	507711.961966	45.155585
3511.297188	507490.658134	45.160589
3510.926788	507264.189406	45.165594
3510.886899	507036.599629	45.170599
3510.342281	506820.515822	45.175604
3510.768102	506600.017633	45.180609
3510.707516	506376.010721	45.185613
3510.470951	506157.540297	45.190618
3510.354281	505935.508139	45.195623
3509.985804	505719.531102	45.200628
3510.419124	505515.444807	45.205633
3510.236290	505302.817240	45.210637
3510.683210	505087.602413	45.215642
3510.642320	504876.562597	45.220647
3510.075511	504664.699904	45.225652
3510.433843	504442.212264	45.230657
3510.405204	504244.962759	45.235661
3510.248087	504035.852830	45.240666
3510.461396	503816.768434	45.245671
3510.260524	503595.527408	45.250676
3510.360454	503387.780779	45.255681
3510.120043	503181.353502	45.260685
3510.079241	502973.777289	45.265690
3510.235782	502767.833122	45.270695
3510.099889	502557.284986	45.275700
3510.162376	502336.993071	45.280705
3510.025046	502152.477481	45.285709
3509.762337	501939.971253	45.290714
3510.040368	501739.807748	45.295719
3510.015710	501544.698999	45.300724
3510.226150	501335.188356	45.305729
3510.038177	501136.563342	45.310733
3510.071583	500927.330537	45.315738
3509.989370	500724.334097	45.320743
3509.844243	500521.244770	45.325748
3510.208241	500309.773427	45.330753
3509.932969	500111.403777	45.335757
3509.661535	499907.873377	45.340762
3509.944337	499709.302481	45.345767
3509.508956	499507.463834	45.350772
3509.695245	499309.056316	45.355777
3509.797513	499128.157365	45.360781
3509.843347	498927.544263	45.365786
3510.056027	498723.461530	45.370791
3509.416049	498529.029034	45.375796
3509.715637	498325.937981	45.380801
3509.588206	498147.343246	45.385805
3509.479260	497956.100509	45.390810
3509.661986	497763.743758	45.395815
3509.484799	497577.211551	45.400820
3509.825707	497370.005394	45.405825
3509.435015	497184.769594	45.410829
3509.622072	496994.021610	45.415834
3509.592451	496805.129157	45.420839
3509.241736	496631.866732	45.425844
3509.438427	496422.599864	45.430849
3509.171926	496243.300455	45.435853
3509.164727	496062.589265	45.440858
3509.441453	495867.665809	45.445863
3509.057255	495692.528015	45.450868
3509.436705	495501.426748	45.455873
3509.108174	495326.579117	45.460877
3509.171265	495137.399185	45.465882
3509.015126	494962.113697	45.470887
3508.574901	494788.544077	45.475892
3508.835701	494607.619779	45.480897
3508.888087	494436.946766	45.485901
3509.086397	494266.398866	45.490906
3509.074315	494078.383320	45.495911
3508.399944	493912.229860	45.500916
3508.996243	493744.492038	45.505921
3508.702085	493566.585273	45.510925
3508.491351	493392.658650	45.515930
3508.937388	493211.434902	45.520935
3508.562338	493048.914662	45.525940
3508.691608	492884.940914	45.530945
3508.623195	492716.598233	45.535949
3508.510669	492547.452013	45.540954
3508.716761	492383.409738	45.545959
3508.745609	492211.150151	45.550964
3509.137199	492038.573947	45.555969
3508.861725	491867.324055	45.560973
3508.603282	491694.450645	45.565978
3508.801260	491531.919303	45.570983
3508.347224	491371.116670	45.575988
3508.591023	491198.304276	45.580993
3508.563083	491038.892943	45.585997
3508.496715	490872.353093	45.591002
3508.537878	490709.537180	45.596007
3508.032458	490554.705691	45.601012
3508.601100	490386.383117	45.606017
3508.223382	490236.080447	45.611021
3508.187954	490067.756710	45.616026
3508.207904	489908.326728	45.621031
3508.130074	489750.986413	45.626036
3508.297391	489595.373691	45.631041
3507.937300	489433.069603	45.636045
3508.189595	489274.504851	45.641050
3508.508890	489126.502199	45.646055
3508.166350	488973.551437	45.651060
3508.401464	488821.411477	45.656065
3508.514731	488669.594583	45.661069
3508.179412	488497.208220	45.666074
3508.234760	488338.061333	45.671079
3508.169733	488184.196025	45.676084
3508.196976	488021.559586	45.681089
3508.450998	487875.733274	45.686093
3508.386607	487721.560157	45.691098
3508.501628	487560.877913	45.696103
3508.249476	487414.425729	45.701108
3508.435623	487242.696950	45.706113
3508.364101	487096.059444	45.711117
3507.835394	486938.618826	45.716122
3508.132636	486775.013789	45.721127
3508.292127	486640.731210	45.726132
3508.319005	486484.203747	45.731137
3508.128974	486338.389817	45.736141
3508.000108	486190.742395	45.741146
3508.073205	486035.417592	45.746151
3508.193264	485886.055075	45.751156
3508.312088	485730.719771	45.756161
3508.326772	485578.943458	45.761165
3508.205020	485421.824603	45.766170
3508.205871	485269.440678	45.771175
3508.089798	485122.996726	45.776180
3508.321442	484972.190334	45.781185
3508.251197	484821.332977	45.786189
3507.914391	484669.507626	45.791194
3507.995405	484519.178581	45.796199
3507.845502	484373.999476	45.801204
3507.847562	484216.190794	45.806209
3508.195779	484080.236876	45.811213
3507.756029	483939.962509	45.816218
3508.111696	483785.531300	45.821223
3508.130230	483640.013740	45.826228
3507.932504	483490.179081	45.831233
3508.047033	483344.946398	45.836237
3508.003604	483198.879041	45.841242
3508.041486	483057.048306	45.846247
3508.103916	482912.985149	45.851252
3508.001646	482766.215664	45.856257
3507.686016	482630.667702	45.861261
3507.700328	482484.685862	45.866266
3508.003361	482337.135004	45.871271
3507.938781	482195.669233	45.876276
3507.498090	482049.963998	45.881281
3507.831014	481911.363973	45.886285
3507.683008	481768.542360	45.891290
3507.769632	481625.072111	45.896295
3507.501375	481493.556999	45.901300
3507.425782	481356.034827	45.906305
3507.374911	481221.898969	45.911309
3507.227390	481086.513082	45.916314
3507.568759	480952.105751	45.921319
3507.458992	480814.737132	45.926324
3507.874870	480680.821272	45.931329
3507.619687	480550.410709	45.936333
3507.483697	480415.524026	45.941338
3507.582938	480282.671728	45.946343
3507.319255	480150.437278	45.951348
3507.543783	480019.232231	45.956353
3507.746269	479882.866297	45.961357
3507.427110	479746.790899	45.966362
3507.559138	479610.333688	45.971367
3507.484934	479483.124522	45.976372
3507.337851	479337.600298	45.981377
3507.382667	479207.483190	45.986381
3507.179226	479080.040126	45.991386
3507.558839	478946.826379	45.996391
3507.450909	478816.479409	46.001396
3507.457668	478686.516944	46.006401
3507.375154	478563.403596	46.011405
3507.405782	478431.258216	46.016410
3507.540419	478295.094433	46.021415
3507.205249	478172.173461	46.026420
3507.252653	478032.579817	46.031425
3507.666703	477905.023079	46.036429
3507.656170	477773.487513	46.041434
3507.446440	477640.871133	46.046439
3507.207140	477523.650688	46.051444
3507.146554	477392.475338	46.056449
3507.346128	477270.975928	46.061453
3507.027189	477141.108679	46.066458
3507.379392	477010.214531	46.071463
3507.505185	476889.737836	46.076468
3507.499362	476755.966297	46.081473
3507.283438	476625.875269	46.086477
3507.272001	476507.799271	46.091482
3507.289203	476375.084332	46.096487
3507.333975	476250.262724	46.101492
3507.285034	476127.582935	46.106497
3507.352010	476001.793784	46.111501
3507.148534	475881.923681	46.116506
3507.233913	475751.775015	46.121511
3506.912260	475632.885550	46.126516
3507.162782	475502.808200	46.131521
3506.889706	475384.162019	46.136525
3506.739565	475265.494083	46.141530
3507.092360	475136.966447	46.146535
3506.852555	475034.567015	46.151540
3506.920967	474904.313989	46.156545
3507.096968	474787.815381	46.161549
3506.969781	474668.025638	46.166554
3507.003151	474542.181632	46.171559
3507.055615	474437.399581	46.176564
3507.147102	474304.859616	46.181569
3507.217708	474184.678494	46.186573
3507.218158	474060.356044	46.191578
3507.226362	473931.473752	46.196583
3507.226532	473827.507441	46.201588
3507.152586	473701.220280	46.206593
3506.836988	473584.595483	46.211597
3506.672943	473471.640960	46.216602
3507.011779	473339.102511	46.221607
3506.677689	473228.606388	46.226612
3507.072385	473106.185315	46.231617
3507.478061	472991.307448	46.236621
3507.115900	472874.331647	46.241626
3507.451995	472743.004882	46.246631
3506.905106	472628.844513	46.251636
3507.001999	472515.231906	46.256641
3507.099802	472398.934263	46.261645
3506.448870	472276.433058	46.266650
3506.803787	472167.231081	46.271655
3506.856085	472050.939046	46.276660
3507.072103	471932.947004	46.281665
3506.927785	471821.143993	46.286669
3506.731599	471704.284473	46.291674
3506.869280	471589.646348	46.296679
3506.533580	471471.137835	46.301684
3506.459207	471366.410837	46.306689
3506.648514	471259.156474	46.311693
3506.668740	471154.209549	46.316698
3506.711602	471044.699785	46.321703
3506.386098	470938.189926	46.326708
3506.440744	470834.349620	46.331713
3506.530815	470716.371446	46.336717
3506.227735	470614.768944	46.341722
3506.443582	470505.530410	46.346727
3506.416079	470404.284924	46.351732
3506.512089	470296.585157	46.356737
3506.484294	470190.881307	46.361741
3506.343999	470092.591170	46.366746
3506.381466	469984.393107	46.371751
3506.377771	469889.877463	46.376756
3506.430528	469773.216719	46.381761
3506.524682	469678.784619	46.386765
3506.228707	469573.933551	46.391770
3506.308035	469465.370806	46.396775
3506.286010	469370.855703	46.401780
3506.265538	469261.245112	46.406785
3506.354967	469159.922352	46.411789
3506.142241	469055.712705	46.416794
3506.396756	468951.270744	46.421799
3506.224728	468863.161177	46.426804
3506.057803	468753.268734	46.431809
3506.085438	468654.739851	46.436813
3505.925721	468563.334207	46.441818
3506.013315	468474.266712	46.446823
3505.956615	468384.260977	46.451828
3506.144855	468279.927963	46.456833
3506.114587	468192.348304	46.461837
3506.075409	468095.398287	46.466842
3506.259806	467993.293256	46.471847
3506.280856	467908.337692	46.476852
3506.371785	467803.106860	46.481857
3506.151119	467705.375332	46.486861
3505.967783	467610.220486	46.491866
3506.198992	467512.664109	46.496871
3506.195390	467414.742061	46.501876
3506.526242	467316.509112	46.506881
3506.269989	467225.974749	46.511885
3505.880065	467126.901376	46.516890
3505.762490	467019.675471	46.521895
3505.742988	466939.636504	46.526900
3505.823067	466848.232376	46.531905
3505.724661	466755.743763	46.536909
3505.630201	466676.881684	46.541914
3505.849140	466575.371126	46.546919
3505.892690	466490.304115	46.551924
3505.754623	466400.404271	46.556929
3505.940403	466317.439978	46.561933
3505.774968	466223.592395	46.566938
3505.828061	466125.046153	46.571943
3505.689784	466043.959841	46.576948
3505.580636	465960.233775	46.581953
3505.772874	465886.436397	46.586957
3505.756740	465806.848107	46.591962
3506.032216	465712.466790	46.596967
3505.905429	465629.654234	46.601972
3505.909212	465532.633281	46.606977
3505.838427	465438.157756	46.611981
3505.656721	465347.399173	46.616986
3505.756458	465260.189262	46.621991
3505.528633	465175.922756	46.626996
3505.848251	465082.290793	46.632001
3505.651824	465005.668535	46.637005
3505.938471	464926.379578	46.642010
3506.013010	464829.647012	46.647015
3505.706714	464748.938613	46.652020
3505.942849	464646.857670	46.657025
3505.975097	464563.557410	46.662029
3505.178350	464485.262288	46.667034
3505.345648	464396.972972	46.672039
3505.340303	464326.851369	46.677044
3505.748044	464246.728298	46.682049
3505.676057	464157.668084	46.687053
3505.574510	464093.794107	46.692058
3505.694075	464000.393757	46.697063
3505.675885	463915.427309	46.702068
3505.687148	463838.764987	46.707073
3505.470050	463759.810626	46.712077
3505.269199	463683.031904	46.717082
3505.945903	463604.126975	46.722087
3505.823493	463523.179419	46.727092
3505.895579	463436.371399	46.732097
3506.210942	463345.265251	46.737101
3505.678274	463266.768128	46.742106
3505.927846	463171.770867	46.747111
3505.233081	463100.039802	46.752116
3505.116725	463022.990709	46.757121
3505.215134	462946.614026	46.762125
3504.952181	462884.537105	46.767130
3505.146846	462794.969112	46.772135
3505.198822	462731.115135	46.777140
3505.255892	462664.118486	46.782145
3505.335002	462582.676592	46.787149
3505.093388	462519.632120	46.792154
3505.381618	462433.694832	46.797159
3504.968362	462371.945979	46.802164
3505.294062	462296.541389	46.807169
3505.256909	462219.070239	46.812173
3504.942561	462154.162147	46.817178
3505.286079	462078.550990	46.822183
3504.966574	462010.349598	46.827188
3505.061560	461941.773162	46.832193
3505.304760	461872.765798	46.837197
3505.180675	461802.199364	46.842202
3505.369920	461728.032048	46.847207
3505.303150	461667.336633	46.852212
3505.156549	461588.412158	46.857217
3505.414374	461508.354163	46.862221
3505.083276	461449.223424	46.867226
3505.161682	461376.036515	46.872231
3505.291406	461307.755987	46.877236
3505.215044	461235.456448	46.882241
3504.814384	461161.489074	46.887245
3505.238065	461094.779210	46.892250
3505.154337	461032.007064	46.897255
3504.955453	460958.460554	46.902260
3505.180727	460885.246751	46.907265
3504.924898	460829.040478	46.912269
3504.837686	460763.379565	46.917274
3505.260690	460693.121160	46.922279
3505.365853	460626.768161	46.927284
3505.192783	460553.317089	46.932289
3505.221813	460484.696179	46.937293
3504.949239	460420.535397	46.942298
3505.160628	460353.656579	46.947303
3504.855173	460286.713753	46.952308
3505.500267	460218.442827	46.957313
3505.581950	460153.359181	46.962317
3505.147025	460093.735343	46.967322
3505.183843	460011.681933	46.972327
3505.171325	459957.002651	46.977332
3505.115045	459880.741867	46.982337
3505.501636	459804.557208	46.987341
3505.146902	459745.628127	46.992346
3505.010869	459673.890541	46.997351
3504.861525	459600.431892	47.002356
3504.978297	459541.320341	47.007361
3504.909541	459471.547015	47.012365
3504.693849	459417.914523	47.017370
3504.532770	459355.048921	47.022375
3504.858271	459304.769915	47.027380
3504.629463	459240.952607	47.032385
3505.162911	459175.535230	47.037389
3504.752345	459115.600221	47.042394
3504.622257	459043.352549	47.047399
3504.547016	458982.751724	47.052404
3504.589931	458933.280237	47.057409
3504.949995	458869.513237	47.062413
3504.597239	458825.886628	47.067418
3504.701840	458756.790733	47.072423
3504.634969	458709.972844	47.077428
3504.360000	458660.554958	47.082433
3504.517162	458605.589592	47.087437
3504.694441	458551.836994	47.092442
3504.671325	458494.266671	47.097447
3504.652261	458432.843683	47.102452
3504.678109	458376.886477	47.107457
3504.785706	458318.279693	47.112461
3504.589134	458269.658368	47.117466
3504.573703	458205.345182	47.122471
3504.739768	458151.593425	47.127476
3504.656228	458101.279873	47.132481
3504.793030	458044.491874	47.137485
3504.446693	457992.449026	47.142490
3504.927922	457929.367906	47.147495
3505.017093	457873.195751	47.152500
3504.430095	457812.019881	47.157505
3504.343846	457759.932022	47.162509
3504.399690	457709.492321	47.167514
3504.943083	457648.933884	47.172519
3504.726774	457593.624045	47.177524
3504.639864	457544.171298	47.182529
3504.527183	457483.775068	47.187533
3504.420411	457438.278810	47.192538
3504.416010	457371.629598	47.197543
3504.500496	457334.970213	47.202548
3504.440506	457286.221817	47.207553
3504.548444	457232.325475	47.212557
3504.199311	457182.561818	47.217562
3504.455457	457137.712503	47.222567
3504.418835	457096.359661	47.227572
3504.452523	457044.857692	47.232577
3504.663975	456991.601940	47.237581
3504.675243	456941.725467	47.242586
3504.753168	456888.542927	47.247591
3504.479025	456840.488931	47.252596
3504.626129	456789.980662	47.257601
3504.394857	456735.127193	47.262605
3504.637838	456692.255889	47.267610
3504.613569	456630.878973	47.272615
3504.567423	456577.818172	47.277620
3504.380522	456524.020967	47.282625
3504.392676	456476.069280	47.287629
3504.376285	456427.260679	47.292634
3504.658273	456374.295377	47.297639
3504.042241	456324.118993	47.302644
3504.158031	456281.521971	47.307649
3504.695461	456234.240331	47.312653
3504.271360	456194.168295	47.317658
3504.493394	456135.332875	47.322663
3504.656042	456091.004078	47.327668
3504.401385	456041.525604	47.332673
3504.520014	455980.578506	47.337677
3504.444390	455942.778114	47.342682
3504.656527	455891.749621	47.347687
3504.639891	455839.391480	47.352692
3504.462511	455789.138871	47.357697
3504.401720	455732.783615	47.362701
3504.333194	455698.276306	47.367706
3504.413806	455645.596929	47.372711
3504.634894	455598.976088	47.377716
3504.330756	455554.877888	47.382721
3504.533774	455515.052255	47.387725
3504.223501	455464.568088	47.392730
3504.492150	455421.030757	47.397735
3504.454623	455378.762155	47.402740
3504.384709	455325.448688	47.407745
3504.851398	455270.015874	47.412749
3504.815493	455231.497722	47.417754
3504.803695	455174.422897	47.422759
3504.872829	455121.490673	47.427764
3504.558391	455065.227565	47.432769
3504.668363	455013.149820	47.437773
3504.607613	454976.663038	47.442778
3504.661078	454910.553444	47.447783
3504.630738	454855.761965	47.452788
3504.565863	454806.248078	47.457793
3504.723961	454757.050836	47.462797
3504.610122	454715.402179	47.467802
3504.667050	454667.894800	47.472807
3504.616910	454608.797292	47.477812
3504.456151	454571.262345	47.482817
3504.730436	454510.689801	47.487821
3504.313236	454465.391949	47.492826
3504.610383	454428.336162	47.497831
3504.175658	454366.464882	47.502836
3503.884060	454335.389709	47.507841
3504.366373	454283.398603	47.512845
3504.156823	454240.396633	47.517850
3504.134097	454203.800594	47.522855
3504.533621	454153.749602	47.527860
3504.576414	454112.630588	47.532865
3504.434031	454070.123717	47.537869
3504.276757	454044.297196	47.542874
3504.570809	453982.198934	47.547879
3504.483936	453942.166267	47.552884
3504.429760	453896.044775	47.557889
3504.476591	453853.707919	47.562893
3504.516339	453805.441074	47.567898
3504.275018	453763.203925	47.572903
3503.959551	453704.909511	47.577908
3504.001479	453676.209677	47.582913
3504.301209	453630.990339	47.587917
3504.022286	453584.957215	47.592922
3504.040978	453540.495378	47.597927
3504.209459	453515.423673	47.602932
3504.222764	453482.064608	47.607937
3504.314025	453439.060288	47.612941
3504.076003	453397.379458	47.617946
3504.084206	453347.900261	47.622951
3504.357214	453322.911863	47.627956
3504.082374	453270.692612	47.632961
3504.456733	453232.303424	47.637965
3504.293184	453186.908739	47.642970
3504.222974	453145.807084	47.647975
3504.320597	453104.271129	47.652980
3503.938636	453065.047562	47.657985
3504.151345	453021.970938	47.662989
3504.120812	452978.580890	47.667994
3504.322319	452939.409545	47.672999
3504.176867	452906.127348	47.678004
3503.977791	452865.554091	47.683009
3504.107101	452826.648337	47.688013
3504.221788	452795.197284	47.693018
3504.456442	452752.521917	47.698023
3504.346351	452714.670745	47.703028
3504.126044	452667.713032	47.708033
3504.112382	452636.334348	47.713037
3503.997680	452592.400200	47.718042
3503.989677	452554.734089	47.723047
3503.997925	452523.807759	47.728052
3503.540443	452486.623841	47.733057
3503.901542	452449.046605	47.738061
3503.742323	452424.536492	47.743066
3503.957580	452400.469379	47.748071
3504.193004	452365.448285	47.753076
3503.922781	452327.471654	47.758081
3504.066169	452298.600486	47.763085
3504.124993	452259.655002	47.768090
3504.248920	452210.609590	47.773095
3504.285721	452179.221595	47.778100
3503.997220	452143.782611	47.783105
3504.228759	452100.599456	47.788109
3503.909088	452073.834938	47.793114
3504.062791	452028.028650	47.798119
3504.020443	451994.372495	47.803124
3503.755865	451970.386811	47.808129
3503.947504	451919.047746	47.813133
3503.803653	451896.410206	47.818138
3503.803087	451866.751848	47.823143
3504.296982	451840.659285	47.828148
3504.488365	451796.569787	47.833153
3504.266621	451748.849758	47.838157
3504.049492	451718.315595	47.843162
3503.672570	451674.728460	47.848167
3504.218832	451643.455460	47.853172
3503.977193	451605.624719	47.858177
3504.045202	451564.851208	47.863181
3503.907051	451540.437848	47.868186
3504.015664	451492.052435	47.873191
3504.261328	451456.216874	47.878196
3503.980960	451429.039218	47.883201
3504.002065	451380.921984	47.888205
3503.914073	451360.555785	47.893210
3503.893495	451331.812666	47.898215
3504.062078	451288.942768	47.903220
3503.388070	451253.770881	47.908225
3503.751939	451233.885100	47.913229
3503.818605	451219.322807	47.918234
3504.164755	451173.684574	47.923239
3503.915917	451144.473173	47.928244
3503.500996	451126.444057	47.933249
3503.996259	451093.049544	47.938253
3503.680466	451052.898260	47.943258
3503.698131	451011.625260	47.948263
3504.126645	450992.133812	47.953268
3503.718097	450958.893405	47.958273
3504.034724	450918.126876	47.963277
3503.993459	450901.453375	47.968282
3503.776275	450877.863937	47.973287
3504.047945	450834.316395	47.978292
3503.571556	450802.912542	47.983297
3503.901441	450773.094799	47.988301
3503.752300	450750.304810	47.993306
3503.691248	450721.466357	47.998311
3503.485907	450689.407643	48.003316
3503.381236	450670.463241	48.008321
3503.721651	450650.175302	48.013325
3503.624197	450631.077530	48.018330
3503.571730	450597.725046	48.023335
3503.827300	450555.700705	48.028340
3503.583900	450530.340806	48.033345
3503.494858	450499.478774	48.038349
3503.715226	450489.554252	48.043354
3503.422396	450475.052821	48.048359
3503.676184	450451.737395	48.053364
3503.374771	450412.342941	48.058369
3503.393560	450377.862505	48.063373
3503.563770	450360.949656	48.068378
3503.462832	450347.784318	48.073383
3503.916889	450325.854204	48.078388
3503.513938	450309.292687	48.083393
3503.809274	450269.745371	48.088397
3503.792239	450228.121831	48.093402
3503.862386	450208.285226	48.098407
3503.897326	450186.578635	48.103412
3503.616800	450161.275329	48.108417
3503.783398	450132.194383	48.113421
3503.816460	450111.045759	48.118426
3503.626116	450085.017129	48.123431
3504.006337	450059.955798	48.128436
3503.593026	450021.847274	48.133441
3503.558946	449987.425923	48.138445
3503.623750	449973.725023	48.143450
3503.478931	449952.555909	48.148455
3503.528899	449933.888651	48.153460
3503.446133	449910.832898	48.158465
3503.695915	449865.816694	48.163469
3503.339662	449846.458175	48.168474
3503.134828	449827.682220	48.173479
3503.415821	449813.133054	48.178484
3503.512586	449800.339239	48.183489
3503.468897	449781.130102	48.188493
3503.470388	449763.383626	48.193498
3503.279029	449749.675615	48.198503
3503.303754	449732.989913	48.203508
3503.425621	449713.853854	48.208513
3503.644717	449671.225526	48.213517
3503.302125	449647.503999	48.218522
3503.352250	449630.560361	48.223527
3503.654215	449600.897826	48.228532
3503.394693	449595.719547	48.233537
3503.643406	449569.311088	48.238541
3503.725075	449565.342135	48.243546
3503.579216	449531.699675	48.248551
3503.676723	449502.426837	48.253556
3503.103058	449489.037451	48.258561
3503.659356	449457.252430	48.263565
3503.589986	449447.224776	48.268570
3503.720538	449435.185528	48.273575
3503.683775	449394.374962	48.278580
3503.718942	449370.690029	48.283585
3503.468035	449332.856745	48.288589
3503.587005	449324.318000	48.293594
3503.095449	449306.097576	48.298599
3503.353590	449290.233639	48.303604
3503.555102	449285.027268	48.308609
3503.633839	449262.957312	48.313613
3503.810405	449237.067797	48.318618
3503.221178	449200.863879	48.323623
3503.734163	449183.739441	48.328628
3503.540312	449170.538521	48.333633
3503.487248	449146.259946	48.338637
3503.466611	449139.823853	48.343642
3503.744092	449112.953567	48.348647
3503.685652	449077.216558	48.353652
3503.257818	449058.173760	48.358657
3503.396199	449029.045398	48.363661
3503.513194	449020.557572	48.368666
3503.530499	449002.047178	48.373671
3504.063302	448982.992403	48.378676
3503.750327	448952.622671	48.383681
3503.853177	448923.094589	48.388685
3503.736887	448908.359106	48.393690
3504.079567	448880.716813	48.398695
3504.024124	448843.052093	48.403700
3503.736458	448822.362577	48.408705
3503.805640	448791.572423	48.413709
3503.780381	448761.102583	48.418714
3503.506904	448739.497861	48.423719
3504.089418	448721.245653	48.428724
3503.970832	448702.149729	48.433729
3504.074870	448659.386879	48.438733
3503.399936	448630.853188	48.443738
3503.223361	448613.693909	48.448743
3503.451538	448589.975142	48.453748
3503.442001	448580.443918	48.458753
3503.674918	448566.206336	48.463757
3503.692502	448551.194214	48.468762
3503.822752	448516.742394	48.473767
3503.729924	448501.089909	48.478772
3503.388416	448485.530579	48.483777
3503.426353	448470.717750	48.488781
3503.607658	448454.308536	48.493786
3503.438911	448428.882639	48.498791
3503.619423	448397.667250	48.503796
3503.309159	448374.952893	48.508801
3503.351603	448352.330409	48.513805
3503.720843	448338.677876	48.518810
3503.467911	448332.991092	48.523815
3503.655404	448310.800156	48.528820
3503.528429	448296.573136	48.533825
3503.597970	448258.378964	48.538829
3503.454457	448241.112323	48.543834
3503.481252	448216.717626	48.548839
3503.453980	448201.712915	48.553844
3502.928750	448192.370981	48.558849
3503.160158	448172.251386	48.563853
3503.372220	448152.692852	48.568858
3503.064542	448150.564859	48.573863
3503.390765	448140.012672	48.578868
3503.320262	448125.167409	48.583873
3503.166066	448119.514416	48.588877
3503.265486	448103.676689	48.593882
3502.923601	448081.829437	48.598887
3503.601037	448065.791574	48.603892
3503.285495	448063.817036	48.608897
3503.184880	448043.956839	48.613901
3503.205884	448028.335274	48.618906
3503.028866	448021.976249	48.623911
3503.037575	448009.956991	48.628916
3502.923360	448000.899745	48.633921
3503.176247	447987.114730	48.638925
3502.788154	447981.045269	48.643930
3502.981547	447959.714984	48.648935
3503.189300	447936.556754	48.653940
3502.869252	447939.450898	48.658945
3503.024196	447917.569352	48.663949
3503.266921	447905.459371	48.668954
3502.989491	447896.379240	48.673959
3503.230453	447884.979455	48.678964
3502.902003	447877.733504	48.683969
3503.300817	447855.860963	48.688973
3503.429843	447849.398922	48.693978
3503.356295	447836.227332	48.698983
3503.345884	447825.732468	48.703988
3502.930640	447827.476601	48.708993
3503.292547	447810.883928	48.713997
3502.892308	447799.694994	48.719002
3502.845635	447783.374893	48.724007
3503.370972	447769.746050	48.729012
3503.169135	447763.746140	48.734017
3503.031833	447748.506354	48.739021
3503.107604	447743.016826	48.744026
3502.994164	447732.133843	48.749031
3503.422804	447713.095713	48.754036
3503.056993	447709.202816	48.759041
3503.181767	447695.135238	48.764045
3503.366891	447681.108055	48.769050
3502.860728	447676.529202	48.774055
3503.136199	447658.582047	48.779060
3502.834777	447647.629702	48.784065
3503.049734	447635.118641	48.789069
3503.213731	447622.717691	48.794074
3503.027791	447610.275067	48.799079
3503.134316	447596.413373	48.804084
3503.320773	447589.840030	48.809089
3503.351923	447584.003121	48.814093
3503.326796	447573.916312	48.819098
3503.076892	447566.910385	48.824103
3503.100779	447549.208928	48.829108
3502.890883	447540.066404	48.834113
3502.939606	447524.591860	48.839117
3502.986101	447518.701605	48.844122
3503.461447	447509.594192	48.849127
3503.470249	447492.858726	48.854132
3503.255851	447496.089851	48.859137
3503.284583	447475.294280	48.864141
3503.531227	447459.532351	48.869146
3503.345627	447459.969586	48.874151
3503.457190	447449.910087	48.879156
3503.464366	447441.846049	48.884161
3503.398062	447420.965234	48.889165
3503.127254	447417.208188	48.894170
3503.017499	447405.969447	48.899175
3503.398420	447388.663274	48.904180
3503.118887	447376.236493	48.909185
3503.295879	447356.886049	48.914189
3503.460216	447337.436330	48.919194
3503.097336	447308.847567	48.924199
3503.058506	447287.505548	48.929204
3502.838960	447283.181925	48.934209
3503.434032	447284.449340	48.939213
3503.224046	447273.481188	48.944218
3502.846091	447258.586395	48.949223
3503.197044	447242.907914	48.954228
3503.144013	447247.328544	48.959233
3502.766634	447236.135408	48.964237
3503.068831	447240.748933	48.969242
3503.078904	447247.897087	48.974247
3502.875876	447235.862834	48.979252
3502.504593	447237.650217	48.984257
3503.013977	447225.646445	48.989261
3503.187046	447213.547963	48.994266
3502.590207	447209.795839	48.999271
3503.017748	447196.994676	49.004276
3503.206083	447186.921945	49.009281
3502.886104	447180.891332	49.014285
3503.366045	447171.681572	49.019290
3503.248682	447162.168120	49.024295
3503.621452	447148.717058	49.029300
3502.997347	447143.803260	49.034305
3503.305247	447128.994107	49.039309
3503.371578	447123.759578	49.044314
3502.918963	447110.905809	49.049319
3503.263282	447094.822675	49.054324
3502.930482	447088.287129	49.059329
3502.500979	447080.601771	49.064333
3502.858841	447071.767780	49.069338
3502.729087	447076.455094	49.074343
3503.113053	447080.344758	49.079348
3502.344644	447084.329764	49.084353
3502.713839	447072.045585	49.089357
3502.859969	447065.478967	49.094362
3502.665377	447057.652071	49.099367
3503.213527	447063.034994	49.104372
3502.827318	447072.735643	49.109377
3502.869124	447068.722319	49.114381
3503.035635	447068.845891	49.119386
3502.905768	447061.616462	49.124391
3503.506501	447044.830284	49.129396
3502.905194	447053.401345	49.134401
3503.065956	447038.059445	49.139405
3503.229795	447032.757535	49.144410
3502.941287	447023.476082	49.149415
3503.036278	447013.368497	49.154420
3502.675287	447010.995940	49.159425
3502.801641	447002.049319	49.164429
3502.984131	446990.050521	49.169434
3502.634127	446989.653769	49.174439
3503.073266	446993.584738	49.179444
3502.671427	446995.275939	49.184449
3502.572848	446987.686173	49.189453
3503.286674	446974.988125	49.194458
3502.852039	446968.216380	49.199463
3503.280934	446953.690705	49.204468
3503.206933	446961.461829	49.209473
3502.879515	446948.079485	49.214477
3503.142877	446947.172323	49.219482
3502.712475	446928.432298	49.224487
3502.917790	446922.362630	49.229492
3502.414455	446919.710107	49.234497
3502.856168	446931.500695	49.239501
3503.009309	446934.567729	49.244506
3503.106517	446936.782244	49.249511
3502.872706	446932.511695	49.254516
3502.974043	446929.451669	49.259521
3502.854691	446916.743718	49.264525
3503.209159	446909.786509	49.269530
3503.034314	446900.789854	49.274535
3503.270014	446892.788008	49.279540
3503.243993	446890.916053	49.284545
3503.213175	446875.403908	49.289549
3503.358007	446869.496682	49.294554
3502.986023	446857.643193	49.299559
3503.420048	446851.027351	49.304564
3503.198429	446841.024455	49.309569
3503.381684	446840.283097	49.314573
3503.255253	446826.866358	49.319578
3503.047304	446825.228302	49.324583
3503.048142	446811.739114	49.329588
3502.870497	446805.024857	49.334593
3502.558427	446796.812242	49.339597
3503.085822	446782.675315	49.344602
3503.201436	446780.525616	49.349607
3502.997676	446771.888816	49.354612
3502.919587	446766.577437	49.359617
3502.932787	446755.266647	49.364621
3503.221994	446748.523370	49.369626
3503.041452	446746.525656	49.374631
3503.319179	446728.425200	49.379636
3503.031296	446720.157716	49.384641
3503.011691	446727.513953	49.389645
3503.429074	446715.728446	49.394650
3503.030304	446708.849073	49.399655
3503.285196	446686.797063	49.404660
3503.105771	446692.253601	49.409665
3502.980467	446682.031341	49.414669
3503.272942	446678.177986	49.419674
3502.948829	446666.975453	49.424679
3503.482229	446658.770557	49.429684
3503.330714	446654.283058	49.434689
3503.267525	446645.672915	49.439693
3503.424496	446640.321370	49.444698
3502.967747	446631.119181	49.449703
3502.879665	446618.405712	49.454708
3502.473618	446622.227509	49.459713
3502.560080	446626.675161	49.464717
3502.779120	446630.846623	49.469722
3502.231952	446635.148909	49.474727
3503.083544	446622.477841	49.479732
3502.938152	446623.415333	49.484737
3502.777799	446607.164449	49.489741
3503.368181	446624.355871	49.494746
3502.729606	446623.399855	49.499751
3503.059994	446620.909204	49.504756
3502.997436	446631.923978	49.509761
3502.955630	446620.318244	49.514765
3503.153140	446618.560231	49.519770
3502.901573	446620.935752	49.524775
3502.782865	446611.827968	49.529780
3502.938793	446600.543436	49.534785
3503.153378	446589.248883	49.539789
3503.017843	446586.685650	49.544794
3503.103683	446581.295525	49.549799
3503.065157	446570.601998	49.554804
3502.846276	446571.805594	49.559809
3502.733242	446559.654169	49.564813
3502.982633	446564.885389	49.569818
3502.716139	446581.056804	49.574823
3503.005801	446587.346069	49.579828
3502.654609	446580.255687	49.584833
3502.655669	446571.330279	49.589837
3502.792557	446553.608699	49.594842
3502.527836	446555.986472	49.599847
3502.791466	446568.720465	49.604852
3502.742470	446589.570843	49.609857
3502.737128	446577.603884	49.614861
3503.024706	446571.367937	49.619866
3502.310981	446574.177350	49.624871
3502.604772	446563.427078	49.629876
3502.735892	446576.335824	49.634881
3502.369562	446576.499669	49.639885
3502.433940	446579.125513	49.644890
3502.498443	446582.866973	49.649895
3502.564286	446598.626654	49.654900
3502.415627	446616.603510	49.659905
3502.480840	446603.914569	49.664909
3502.721428	446599.613662	49.669914
3502.394479	446611.332831	49.674919
3502.604802	446622.503860	49.679924
3502.495513	446628.201992	49.684929
3502.380366	446622.846195	49.689933
3502.546949	446633.314737	49.694938
3502.215843	446646.758759	49.699943
3502.639905	446638.572524	49.704948
3502.606317	446642.939249	49.709953
3502.602869	446661.753354	49.714957
3503.100390	446664.457362	49.719962
3502.604542	446669.410117	49.724967
3502.641492	446661.644962	49.729972
3502.948302	446665.801430	49.734977
3502.770369	446651.683426	49.739981
3503.016389	446648.953631	49.744986
3502.388261	446654.385371	49.749991
3502.604150	446669.865827	49.754996
3502.928277	446679.800341	49.760001
3502.921403	446671.789120	49.765005
3503.500157	446660.533846	49.770010
3503.377898	446668.566869	49.775015
3502.915470	446660.126321	49.780020
3502.708508	446651.439308	49.785025
3502.671459	446651.901904	49.790029
3502.697760	446649.818152	49.795034
3502.817936	446667.546220	49.800039
3503.072451	446673.182223	49.805044
3503.058161	446670.851851	49.810049
3502.659004	446670.767748	49.815053
3502.801067	446655.986582	49.820058
3502.364110	446663.515524	49.825063
3502.588147	446649.988123	49.830068
3502.680118	446665.692583	49.835073
3502.564287	446675.093692	49.840077
3502.760249	446676.987109	49.845082
3502.546005	446679.660514	49.850087
3502.884098	446673.010288	49.855092
3502.504402	446686.564002	49.860097
3502.442313	446682.821897	49.865101
3502.603418	446679.700920	49.870106
3502.692095	446691.247658	49.875111
3502.663619	446681.008865	49.880116
3502.720739	446702.145278	49.885121
3502.831297	446713.536136	49.890125
3502.859445	446719.109356	49.895130
3502.921495	446719.707161	49.900135
3503.070242	446710.807305	49.905140
3502.690633	446703.975370	49.910145
3502.851325	446700.499493	49.915149
3503.077948	446678.807275	49.920154
3502.902040	446687.103004	49.925159
3502.823580	446702.937958	49.930164
3502.775050	446697.925779	49.935169
3503.125154	446702.480531	49.940173
3503.016447	446696.515127	49.945178
3502.849467	446698.470512	49.950183
3502.937804	446686.031225	49.955188
3503.084478	446691.381372	49.960193
3503.040006	446678.914046	49.965197
3503.137687	446662.771278	49.970202
3502.591777	446670.065268	49.975207
3502.928082	446659.916312	49.980212
3503.055024	446646.811172	49.985217
3502.799582	446650.810092	49.990221
3502.820698	446678.798608	49.995226
3503.051432	446680.280403	50.000231
3503.039285	446674.704190	50.005236
3502.983407	446675.271422	50.010241
3502.641342	446670.360066	50.015245
3502.923141	446653.932301	50.020250
3502.543943	446653.337684	50.025255
3502.666454	446648.904816	50.030260
3502.578772	446667.276903	50.035265
3502.526901	446677.782723	50.040269
3502.756623	446679.163269	50.045274
3502.537851	446681.837447	50.050279
3502.984856	446670.908937	50.055284
3502.893147	446685.579823	50.060289
3502.510007	446692.592460	50.065293
3503.066403	446697.568385	50.070298
3502.840328	446700.852334	50.075303
3503.134417	446693.246127	50.080308
3503.203945	446691.662104	50.085313
3502.886382	446686.543726	50.090317
3503.248294	446680.396541	50.095322
3502.802586	446675.046487	50.100327
3503.138783	446666.368160	50.105332
3503.200723	446663.213402	50.110337
3502.855984	446661.700110	50.115341
3503.133810	446652.271084	50.120346
3502.850873	446660.686520	50.125351
3502.620532	446647.236700	50.130356
3502.834665	446665.050148	50.135361
3502.590905	446677.160762	50.140365
3502.889030	446677.160443	50.145370
3502.635687	446677.000733	50.150375
3502.589262	446669.452659	50.155380
3502.800548	446680.471362	50.160385
3502.870478	446698.207983	50.165389
3502.990215	446700.266545	50.170394
3502.552884	446697.906987	50.175399
3502.557066	446694.052148	50.180404
3502.394248	446693.623428	50.185409
3502.701919	446703.662162	50.190413
3503.051952	446711.918790	50.195418
3502.794491	446720.938379	50.200423
3502.976296	446715.531902	50.205428
3502.931919	446709.454096	50.210433
3502.889379	446710.069760	50.215437
3502.835376	446704.855675	50.220442
3502.401875	446702.901147	50.225447
3502.548436	446716.263566	50.230452
3502.794257	446722.002461	50.235457
3502.395732	446741.543188	50.240461
3502.622580	446726.696885	50.245466
3502.469546	446735.292953	50.250471
3502.484107	446740.868487	50.255476
3502.617022	446755.957365	50.260481
3502.564885	446755.104065	50.265485
3502.815014	446750.395876	50.270490
3502.487590	446758.261056	50.275495
3502.649364	446776.996137	50.280500
3502.616039	446784.557539	50.285505
3502.532544	446778.942825	50.290509
3503.072119	446769.874841	50.295514
3502.544922	446782.794445	50.300519
3502.600816	446800.888350	50.305524
3502.723609	446802.236436	50.310529
3502.706400	446799.754445	50.315533
3502.786505	446802.073315	50.320538
3502.578657	446803.224305	50.325543
3502.888708	446814.885307	50.330548
3502.718131	446824.904221	50.335553
3502.762914	446831.083094	50.340557
3502.844035	446826.961592	50.345562
3502.731141	446822.112562	50.350567
3502.956697	446818.372078	50.355572
3502.996338	446815.677542	50.360577
3502.768631	446814.245699	50.365581
3502.746166	446828.549692	50.370586
3502.654718	446844.133207	50.375591
3502.604795	446836.332239	50.380596
3502.902765	446831.666610	50.385601
3502.649685	446834.701598	50.390605
3503.134968	446825.237226	50.395610
3502.818850	446828.384399	50.400615
3503.029021	446823.125236	50.405620
3503.100501	446839.492300	50.410625
3502.733949	446852.080171	50.415629
3502.634172	446850.880039	50.420634
3502.607210	446854.028546	50.425639
3502.756906	446844.672193	50.430644
3503.169179	446838.668584	50.435649
3502.757119	446840.817933	50.440653
3502.618464	446827.301862	50.445658
3502.422735	446852.233852	50.450663
3502.718718	446858.420537	50.455668
3502.392104	446863.750032	50.460673
3502.545588	446859.109079	50.465677
3502.806499	446877.269333	50.470682
3502.610060	446904.584758	50.475687
3502.794367	446896.693109	50.480692
3502.845311	446898.763396	50.485697
3502.880684	446896.982380	50.490701
3502.942290	446891.393631	50.495706
3502.416369	446895.844368	50.500711
3502.854594	446897.240009	50.505716
3502.834214	446909.363059	50.510721
3502.729250	446910.141506	50.515725
3502.784608	446906.176548	50.520730
3502.433875	446911.459440	50.525735
3502.444938	446876.923884	50.530740
3502.462607	446861.454159	50.535745
3502.689968	446829.822782	50.540749
3502.644943	446772.781293	50.545754
3502.367434	446720.698261	50.550759
3502.597843	446652.757380	50.555764
3502.673854	446560.653588	50.560769
3502.621259	446467.709269	50.565773
3502.818147	446356.465876	50.570778
3502.704431	446239.493816	50.575783
3503.032347	446109.412750	50.580788
3502.773435	445963.811720	50.585793
3502.567197	445823.018401	50.590797
3502.994387	445646.414071	50.595802
3502.922462	445467.104267	50.600807
3502.588830	445277.897730	50.605812
3502.705719	445069.949717	50.610817
3502.747612	444862.266071	50.615821
3502.765331	444630.444025	50.620826
3502.577057	444398.401076	50.625831
3502.640062	444136.187100	50.630836
3502.637984	443875.553285	50.635841
3502.477109	443597.750101	50.640845
3502.638015	443309.389681	50.645850
3502.604990	443015.276553	50.650855
3502.565655	442708.835584	50.655860
3502.832820	442386.563844	50.660865
3502.488687	442048.617352	50.665869
3502.792785	441698.483051	50.670874
3502.875710	441327.026488	50.675879
3502.925809	440955.975028	50.680884
3503.185613	440561.548059	50.685889
3503.021969	440162.164473	50.690893
3502.874500	439730.762308	50.695898
3502.920382	439292.267550	50.700903
3502.801513	438835.174772	50.705908
3502.683702	438374.521321	50.710913
3502.135657	437896.987665	50.715917
3502.387221	437410.175498	50.720922
3502.695004	436915.936110	50.725927
3502.415431	436394.592531	50.730932
3502.692593	435851.680680	50.735937
3502.413052	435311.996530	50.740941
3502.587229	434740.865947	50.745946
3502.438052	434159.171711	50.750951
3502.285609	433554.985078	50.755956
3502.208011	432941.940607	50.760961
3501.986896	432320.277905	50.765965
3502.573343	431673.341864	50.770970
3502.021145	431012.322463	50.775975
3502.090926	430326.260897	50.780980
3502.036451	429623.960600	50.785985
3502.043912	428921.577927	50.790989
3502.033875	428174.819671	50.795994
3501.588477	427426.488027	50.800999
3501.357744	426661.955831	50.806004
3501.732568	425879.276873	50.811009
3501.501226	425086.270254	50.816013
3501.391643	424241.745321	50.821018
3500.803737	423420.572594	50.826023
3501.276581	422559.290291	50.831028
3500.810392	421679.151459	50.836033
3500.749722	420795.485027	50.841037
3500.590249	419876.950397	50.846042
3500.426270	418948.913663	50.851047
3500.454351	417994.813579	50.856052
3500.513828	417022.875089	50.861057
3500.028489	416038.831063	50.866061
3500.790804	415029.044620	50.871066
3500.188671	414005.714951	50.876071
3500.130254	412956.961581	50.881076
3500.205054	411884.400778	50.886081
3499.801448	410800.069499	50.891085
3500.165228	409684.606052	50.896090
3499.757712	408561.786365	50.901095
3499.456387	407405.478725	50.906100
3499.405759	406245.319700	50.911105
3499.251664	405062.599542	50.916109
3498.892016	403848.341392	50.921114
3498.888073	402636.737846	50.926119
3498.768039	401387.403750	50.931124
3498.674314	400120.099836	50.936129
3498.242880	398848.376408	50.941133
3498.289294	397538.939097	50.946138
3498.249895	396230.828995	50.951143
3498.134418	394890.023249	50.956148
3497.933123	393535.856369	50.961153
3497.775141	392168.660837	50.966157
3497.328223	390763.995090	50.971162
3497.008047	389357.412867	50.976167
3496.913455	387933.725369	50.981172
3497.099334	386493.709458	50.986177
3496.891929	385030.285742	50.991181
3496.676520	383542.089632	50.996186
3496.437066	382038.729621	51.001191
3496.241100	380524.361822	51.006196
3496.238088	378983.198767	51.011201
3495.758892	377433.529043	51.016205
3495.863375	375857.222222	51.021210
3495.478037	374267.603585	51.026215
3495.010690	372662.136301	51.031220
3494.848469	371041.185364	51.036225
3494.631027	369412.134632	51.041229
3494.315067	367766.447117	51.046234
3494.098938	366099.179661	51.051239
3494.130393	364417.044712	51.056244
3494.189963	362709.956584	51.061249
3493.549593	361000.953652	51.066253
3493.506167	359260.514002	51.071258
3493.049929	357520.450077	51.076263
3492.869364	355743.201681	51.081268
3492.822997	353953.693890	51.086273
3492.441262	352163.174732	51.091277
3492.121255	350349.037191	51.096282
3491.568351	348522.015625	51.101287
3491.431189	346687.571148	51.106292
3491.472263	344834.880402	51.111297
3491.159512	342964.746052	51.116301
3490.855052	341072.271052	51.121306
3490.309043	339187.219046	51.126311
3489.918954	337275.933508	51.131316
3490.099626	335351.244862	51.136321
3489.337944	333419.112483	51.141325
3489.341323	331463.288177	51.146330
3488.868190	329510.376515	51.151335
3488.312411	327541.961150	51.156340
3488.213799	325546.088914	51.161345
3487.842928	323556.839384	51.166349
3487.370500	321553.312901	51.171354
3487.146598	319537.028532	51.176359
3486.564761	317496.533352	51.181364
3486.371282	315449.214415	51.186369
3486.098868	313400.040969	51.191373
3486.111253	311321.991965	51.196378
3485.649327	309247.173931	51.201383
3485.254485	307151.717052	51.206388
3485.201813	305037.433609	51.211393
3484.371453	302926.641722	51.216397
3484.230199	300793.147624	51.221402
3483.911893	298648.430874	51.226407
3483.102581	296500.287547	51.231412
3482.807193	294335.918233	51.236417
3482.637981	292171.076586	51.241421
3482.406570	289984.585150	51.246426
3481.962193	287800.815690	51.251431
3481.509585	285591.341853	51.256436
3481.082569	283368.586620	51.261441
3480.343481	281155.070998	51.266445
3480.146672	278912.681410	51.271450
3479.685368	276675.682933	51.276455
3479.172294	274429.653210	51.281460
3478.777897	272161.857380	51.286465
3478.702721	269895.897393	51.291469
3478.496655	267605.290091	51.296474
3477.862516	265318.510874	51.301479
3477.161703	263015.584997	51.306484
3477.245352	260701.361643	51.311489
3476.297838	258385.424202	51.316493
3475.935945	256052.575250	51.321498
3475.435087	253720.718380	51.326503
3474.894079	251384.109491	51.331508
3474.471099	249030.296330	51.336513
3473.788921	246682.395123	51.341517
3473.372233	244314.214931	51.346522
3472.578390	241942.321149	51.351527
3471.917138	239567.394096	51.356532
3471.568725	237185.306157	51.361537
3470.954122	234803.748825	51.366541
3470.478024	232421.612151	51.371546
3470.022843	230019.565381	51.376551
3469.411311	227619.747192	51.381556
3469.161346	225198.975528	51.386561
3468.324381	222803.278798	51.391565
3468.031153	220377.285065	51.396570
3467.439151	217957.480076	51.401575
3466.631643	215520.859616	51.406580
3466.405736	213085.981641	51.411585
3465.335236	210649.706705	51.416589
3464.979612	208196.011837	51.421594
3464.600735	205756.687899	51.426599
3463.959658	203300.157423	51.431604
3463.041386	200842.950814	51.436609
3462.419424	198379.080387	51.441613
3461.627361	195916.445368	51.446618
3461.198148	193445.857822	51.451623
3460.336904	190981.076413	51.456628
3460.007507	188514.672478	51.461633
3459.440322	186045.343246	51.466637
3458.787747	183562.809749	51.471642
3457.933238	181092.560591	51.476647
3457.038750	178615.050546	51.481652
3456.611342	176129.574294	51.486657
3455.455887	173650.400225	51.491661
3455.360865	171160.355349	51.496666
3454.258577	168687.850446	51.501671
3453.428824	166206.792596	51.506676
3453.019255	163708.829674	51.511681
3452.051933	161234.953725	51.516685
3451.129500	158750.872183	51.521690
3450.674983	156269.567516	51.526695
3449.743333	153790.403168	51.531700
3449.156292	151310.266436	51.536705
3448.301559	148836.692007	51.541709
3447.426191	146367.020840	51.546714
3446.802465	143813.048166	51.551719
3445.844738	141341.327089	51.556724
3445.055979	138870.105641	51.561729
3444.018265	136405.801933	51.566733
3443.249034	133938.364633	51.571738
3442.592463	131482.987498	51.576743
3441.478322	129034.138899	51.581748
3440.673998	126579.223600	51.586753
3439.446199	124137.927686	51.591757
3438.874454	121692.863577	51.596762
3438.270288	119259.437191	51.601767
3437.159525	116836.066084	51.606772
3436.791018	114409.428926	51.611777
3435.221239	111980.865434	51.616781
3434.395572	109557.629649	51.621786
3433.538155	107146.332880	51.626791
3432.008809	104738.907187	51.631796
3430.973394	102350.455896	51.636801
3429.996476	99982.054631	51.641805
3429.116714	97599.266524	51.646810
3427.962145	95241.442676	51.651815
3426.475808	92895.084484	51.656820
3425.847332	90553.167303	51.661825
3424.664961	88218.383338	51.666829
3423.831292	85903.655328	51.671834
3422.193842	83598.932267	51.676839
3421.056994	81309.510088	51.681844
3419.988517	79027.450549	51.686849
3418.703159	76763.527256	51.691853
3417.623027	74509.016216	51.696858
3416.222976	72266.987245	51.701863
3414.530538	70048.586661	51.706868
3413.579272	67840.023082	51.711873
3412.320962	65662.608228	51.716877
3411.003701	63489.768355	51.721882
3409.656818	61329.579745	51.726887
3408.161530	59197.643200	51.731892
3407.129175	57068.484951	51.736897
3405.676614	54980.529258	51.741901
3404.375191	52893.556772	51.746906
3402.857723	50829.706307	51.751911
3400.916326	48797.089772	51.756916
3399.909624	46765.314325	51.761921
3398.365813	44769.934343	51.766925
3397.284167	42806.473999	51.771930
3395.618952	40849.059259	51.776935
3394.379887	38909.636663	51.781940
3392.871792	36997.986217	51.786945
3390.627522	35113.329686	51.791949
3388.933347	33254.513726	51.796954
3387.169064	31409.707503	51.801959
3385.398875	29611.739953	51.806964
3383.651056	27843.854445	51.811969
3381.259163	26121.648583	51.816973
3378.837064	24421.827570	51.821978
3376.822941	22775.294330	51.826983
3374.121481	21169.294497	51.831988
3371.357432	19600.851432	51.836993
3368.074008	18095.006602	51.841997
3365.279427	16643.805328	51.847002
3361.479951	15257.976872	51.852007
3356.305924	13981.964899	51.857012
3349.741352	12818.991533	51.862017
3342.919249	11763.671493	51.867021
3337.136174	10809.340358	51.872026
3331.424855	9959.781220	51.877031
3326.416098	9221.420026	51.882036
3322.323538	8562.191633	51.887041
3318.053351	8009.281284	51.892045
3314.947710	7530.980699	51.897050
3312.425079	7129.929711	51.902055
3309.305854	6794.592568	51.907060
3307.182948	6507.330699	51.912065
3304.971891	6296.961163	51.917069
3303.918652	6118.039635	51.922074
3302.182979	5975.831918	51.927079
3300.942785	5873.251351	51.932084
3300.280663	5793.992347	51.937089
3299.166005	5749.889469	51.942093
3299.096011	5716.971736	51.947098
3298.441643	5705.821003	51.952103
3298.208779	5704.905080	51.957108
3298.122638	5706.230627	51.962113
3297.897020	5724.319196	51.967117
3297.981658	5737.061984	51.972122
3297.876911	5760.711003	51.977127
3297.478499	5774.021235	51.982132
3297.670260	5785.451383	51.987137
3297.482663	5815.351192	51.992141
3297.354581	5827.426731	51.997146
3297.481433	5840.737320	52.002151
3297.673116	5850.982128	52.007156
3297.599934	5849.944150	52.012161
3297.270737	5849.636189	52.017165
3297.130861	5845.362982	52.022170
3296.971094	5829.184689	52.027175
3296.538075	5815.086669	52.032180
3297.080613	5788.776142	52.037185
3296.678197	5773.283783	52.042189
3296.325528	5729.673899	52.047194
3296.172806	5704.452863	52.052199
3295.645512	5669.271788	52.057204
3295.715184	5618.650692	52.062209
3295.597879	5588.326879	52.067213
3295.136865	5533.546394	52.072218
3294.382466	5486.588661	52.077223
3294.029465	5440.882119	52.082228
3293.532158	5370.377176	52.087233
3293.028689	5323.224643	52.092237
3292.701936	5262.031788	52.097242
3292.349335	5201.059963	52.102247
3291.605416	5129.277821	52.107252
3291.409384	5086.419216	52.112257
3290.758594	5023.611618	52.117261
3290.264214	4962.049751	52.122266
3290.080837	4881.931697	52.127271
3289.374795	4814.206683	52.132276
3288.880969	4736.167159	52.137281
3288.058005	4667.669108	52.142285
3287.123260	4595.335239	52.147290
3286.848241	4526.003477	52.152295
3286.279121	4475.371939	52.157300
3285.873722	4400.726390	52.162305
3285.014657	4323.238510	52.167309
3284.172531	4249.096277	52.172314
3283.986423	4177.853289	52.177319
3282.869453	4112.313009	52.182324
3282.906053	4037.496534	52.187329
3282.253656	3980.106390	52.192333
3281.394177	3909.139146	52.197338
3281.008739	3832.780908	52.202343
3280.045586	3746.681279	52.207348
3279.842488	3676.747920	52.212353
3279.176382	3612.120521	52.217357
3278.272622	3534.459357	52.222362
3277.632273	3458.189109	52.227367
3276.587931	3398.185685	52.232372
3276.763940	3321.675566	52.237377
3276.297153	3247.043563	52.242381
3275.258672	3182.571547	52.247386
3274.406888	3097.226295	52.252391
3273.930656	3030.886189	52.257396
3273.882229	2961.397799	52.262401
3273.007615	2891.104128	52.267405
3271.991582	2817.250191	52.272410
3271.736600	2730.959315	52.277415
3270.724624	2676.225172	52.282420
3270.402541	2583.910202	52.287425
3269.661647	2522.350967	52.292429
3268.585377	2445.462093	52.297434
3268.279417	2379.882838	52.302439
3267.678743	2317.197424	52.307444
3266.779938	2242.219187	52.312449
3265.858075	2174.160980	52.317453
3265.125075	2102.952066	52.322458
3264.354499	2030.680052	52.327463
3263.658875	1981.376924	52.332468
3263.314753	1912.376338	52.337473
3262.373435	1849.058552	52.342477
3261.790864	1791.720494	52.347482
3261.089689	1745.304819	52.352487
3260.650638	1667.815063	52.357492
3260.391058	1603.506213	52.362497
3259.385113	1558.139937	52.367501
3258.594026	1489.450869	52.372506
3258.185033	1423.448304	52.377511
3256.993397	1376.464575	52.382516
3256.352584	1304.926539	52.387521
3255.767884	1256.221772	52.392525
3254.979382	1198.301691	52.397530
3254.816345	1152.436921	52.402535
3253.702049	1086.052955	52.407540
3253.252962	1032.756467	52.412545
3252.394041	978.099999	52.417549
3251.870685	928.840229	52.422554
3251.352147	874.888625	52.427559
3250.229489	830.166520	52.432564
3249.704358	767.639788	52.437569
3249.017988	737.146166	52.442573
3248.120384	683.136032	52.447578
3247.515076	620.732928	52.452583
3246.636642	578.250632	52.457588
3246.484182	528.590864	52.462593
3245.798523	494.921537	52.467597
3245.073017	464.450134	52.472602
3244.416034	409.820368	52.477607
3243.353512	371.137037	52.482612
3242.739887	320.382776	52.487617
3242.164104	283.484384	52.492621
3241.072700	241.014128	52.497626
3240.404200	208.092083	52.502631
3239.227653	188.105320	52.507636
3238.718298	169.979825	52.512641
3237.923242	150.934891	52.517645
3235.899386	153.940980	52.522650
3234.947407	155.371353	52.527655
3233.597396	153.752163	52.532660
3233.509215	149.741272	52.537665
3232.992632	153.992199	52.542669
3232.821050	163.460914	52.547674
3232.087915	150.976447	52.552679
3231.680342	159.640363	52.557684
3231.004569	157.660073	52.562689
3230.324576	157.842825	52.567693
3229.418120	159.079900	52.572698
3229.110884	154.184346	52.577703
3228.614776	162.777339	52.582708
3227.990216	157.823102	52.587713
3226.993535	159.441899	52.592717
3226.335963	156.948117	52.597722
3225.943476	146.681461	52.602727
3225.178626	162.253365	52.607732
3224.731090	154.279611	52.612737
3223.804833	157.540288	52.617741
3222.842278	154.884667	52.622746
3222.536664	153.085083	52.627751
3221.549863	163.068455	52.632756
3221.625081	153.213724	52.637761
3220.974580	159.906819	52.642765
3220.150370	154.033425	52.647770
3219.244907	151.392919	52.652775
3218.588926	160.537027	52.657780
3218.211029	149.199744	52.662785
3217.558030	154.969206	52.667789
3216.731970	159.575762	52.672794
3216.617635	154.809882	52.677799
3215.527062	156.254857	52.682804
3215.126754	155.264854	52.687809
3214.033602	151.833406	52.692813
3213.664301	155.662866	52.697818
3213.069790	152.160836	52.702823
3212.244393	155.302048	52.707828
3211.239981	159.307509	52.712833
3210.804690	156.608785	52.717837
3210.078613	162.383630	52.722842
3210.208872	158.220948	52.727847
3209.217314	161.171080	52.732852
3208.498607	153.996008	52.737857
3208.239441	150.262218	52.742861
3207.035434	155.071497	52.747866
3206.692341	159.117134	52.752871
3206.172446	163.605467	52.757876
3205.109004	155.789831	52.762881
3204.597960	158.601820	52.767885
3203.859249	157.981861	52.772890
3203.520594	154.333887	52.777895
3202.851859	160.402085	52.782900
3202.225387	159.608613	52.787905
3201.184933	156.408553	52.792909
3200.557609	153.330542	52.797914
3200.033770	153.720693	52.802919
3199.211261	156.967201	52.807924
3198.886984	152.392712	52.812929
3198.274429	151.703045	52.817933
3197.143595	153.064508	52.822938
3196.707730	152.584254	52.827943
3195.904318	159.978064	52.832948
3195.845083	155.456582	52.837953
3195.905923	154.996467	52.842957
3194.280414	157.527550	52.847962
3193.655329	151.251467	52.852967
3192.313484	153.645274	52.857972
3192.080032	151.536134	52.862977
3191.530608	144.473461	52.867981
3191.336594	151.500267	52.872986
3190.974285	151.151128	52.877991
3190.082283	151.769569	52.882996
3189.090181	144.459639	52.888001
3188.180547	149.169286	52.893005
3187.018631	155.530947	52.898010
3186.941260	145.921367	52.903015
3186.128109	151.356620	52.908020
3185.734106	150.511987	52.913025
3185.322686	151.954619	52.918029
3184.400573	157.195336	52.923034
3183.862320	151.316121	52.928039
3183.160840	150.100476	52.933044
3182.615728	142.404715	52.938049
3181.964460	144.751987	52.943053
3180.670666	145.791565	52.948058
3180.745644	147.841872	52.953063
3179.885177	153.675595	52.958068
3179.648939	151.249176	52.963073
3178.434149	149.534663	52.968077
3177.628567	148.602851	52.973082
3177.570730	152.395282	52.978087
3176.839260	151.054107	52.983092
3176.006587	147.045679	52.988097
3175.398148	146.416099	52.993101
3174.277233	158.188394	52.998106
3174.390611	146.672849	53.003111
3173.854922	152.258063	53.008116
3172.835665	143.712147	53.013121
3172.133750	148.424991	53.018125
3170.628765	148.256077	53.023130
3170.729648	143.293569	53.028135
3170.295208	138.951851	53.033140
3169.714177	142.253417	53.038145
3169.094493	142.406925	53.043149
3167.644053	145.445721	53.048154
3167.303855	146.183833	53.053159
3167.069851	147.071956	53.058164
3166.768407	146.249405	53.063169
3166.139721	146.050775	53.068173
3164.666651	147.587159	53.073178
3163.839807	151.923069	53.078183
3163.102804	147.644094	53.083188
3162.363937	146.031033	53.088193
3162.569408	141.686958	53.093197
3161.647363	152.684370	53.098202
3161.052565	150.015667	53.103207
3159.955080	150.019892	53.108212
3159.276496	151.693692	53.113217
3159.218467	148.620658	53.118221
3158.318538	154.463888	53.123226
3158.191867	149.551309	53.128231
3157.003110	147.835117	53.133236
3156.309332	139.326755	53.138241
3155.602489	142.639948	53.143245
3154.957298	151.056699	53.148250
3154.185071	139.298528	53.153255
3153.629027	148.451607	53.158260
3153.315369	144.673451	53.163265
3152.599463	148.870015	53.168269
3151.891097	142.786983	53.173274
3151.044323	147.277478	53.178279
3150.121681	149.979400	53.183284
3149.167794	143.037942	53.188289
3149.009353	145.889950	53.193293
3148.438928	143.962725	53.198298
3147.820248	136.834135	53.203303
3147.161803	139.969326	53.208308
3146.561436	143.526033	53.213313
3145.990006	143.458541	53.218317
3145.091015	145.692223	53.223322
3145.290781	139.546404	53.228327
3143.944717	144.758109	53.233332
3143.395232	143.201903	53.238337
3142.923668	139.189813	53.243341
3141.811527	150.807846	53.248346
3141.548699	136.471918	53.253351
3140.742803	142.430525	53.258356
3139.890309	146.217410	53.263361
3139.272353	138.682916	53.268365
3138.155105	152.207961	53.273370
3137.645456	139.163120	53.278375
3137.326213	139.489900	53.283380
3137.104958	147.165550	53.288385
3136.583310	141.234958	53.293389
3134.904405	145.137380	53.298394
3134.714652	140.907015	53.303399
3134.103327	154.935741	53.308404
3133.709770	144.454554	53.313409
3133.019968	139.490959	53.318413
3132.135822	139.022566	53.323418
3131.371638	131.007416	53.328423
3130.470468	135.178001	53.333428
3129.824782	140.235309	53.338433
3128.999335	138.116401	53.343437
3128.289353	145.680556	53.348442
3128.790925	140.861166	53.353447
3127.920852	146.450617	53.358452
3126.726942	139.955165	53.363457
3126.481819	138.388801	53.368461
3125.450630	142.432396	53.373466
3125.045194	132.555997	53.378471
3124.730200	140.476206	53.383476
3123.280194	140.747110	53.388481
3122.941400	136.216166	53.393485
3122.277810	139.783281	53.398490
3121.926651	135.756938	53.403495
3120.955080	148.001463	53.408500
3119.862356	141.781217	53.413505
3119.396784	139.032417	53.418509
3118.304995	154.200706	53.423514
3117.976666	133.338501	53.428519
3117.203765	141.220502	53.433524
3117.158494	140.650231	53.438529
3116.735024	135.820737	53.443533
3115.840693	145.521864	53.448538
3114.591717	132.382305	53.453543
3114.306194	144.350932	53.458548
3114.106811	138.623040	53.463553
3113.525294	135.259724	53.468557
3112.072758	149.254149	53.473562
3111.845765	144.013724	53.478567
3110.979262	138.933880	53.483572
3110.685657	145.575074	53.488577
3109.721974	140.905377	53.493581
3109.181324	150.525552	53.498586
3108.599718	142.434996	53.503591
3107.824308	144.730461	53.508596
3106.801559	149.971010	53.513601
3106.792822	139.795125	53.518605
3106.090464	144.882250	53.523610
3104.746766	147.401124	53.528615
3104.346446	143.513045	53.533620
3103.672922	142.041589	53.538625
3103.221642	138.369845	53.543629
3102.162903	143.480361	53.548634
3101.793693	137.066636	53.553639
3100.978945	144.309226	53.558644
3100.180629	146.520976	53.563649
3099.637758	134.639164	53.568653
3098.710448	140.054847	53.573658
3099.128938	144.123906	53.578663
3097.959834	145.237721	53.583668
3096.880536	140.845537	53.588673
3096.668332	143.989356	53.593677
3096.115173	142.013793	53.598682
3095.345694	134.747167	53.603687
3094.416515	138.955305	53.608692
3094.045261	139.567677	53.613697
3093.157601	134.921706	53.618701
3093.088314	145.517236	53.623706
3092.039967	133.661398	53.628711
3091.224456	135.120578	53.633716
3090.069319	141.351617	53.638721
3090.222076	136.353015	53.643725
3089.809044	140.050212	53.648730
3088.623592	137.369153	53.653735
3087.706220	148.640102	53.658740
3087.231918	138.235090	53.663745
3087.047862	140.743720	53.668749
3085.854281	145.520050	53.673754
3085.579693	144.400817	53.678759
3084.696444	138.174395	53.683764
3083.735944	141.570012	53.688769
3083.950048	139.324806	53.693773
3082.689531	139.096382	53.698778
3082.153801	139.583309	53.703783
3081.758374	143.325261	53.708788
3080.613206	140.882840	53.713793
3080.199385	140.760400	53.718797
3079.179507	142.844223	53.723802
3078.828810	137.582704	53.728807
3078.227285	134.904900	53.733812
3077.200450	140.545611	53.738817
3077.176168	140.253984	53.743821
3076.396484	139.119610	53.748826
3075.563557	148.347628	53.753831
3074.593787	142.093754	53.758836
3073.779020	140.907349	53.763841
3073.600174	137.167745	53.768845
3072.818843	150.433690	53.773850
3072.134038	137.245507	53.778855
3071.258738	139.738038	53.783860
3071.005247	130.120286	53.788865
3070.403784	134.222300	53.793869
3069.523570	135.708327	53.798874
3068.990919	133.862683	53.803879
3068.520532	136.312080	53.808884
3067.508300	136.993317	53.813889
3066.974601	141.138228	53.818893
3066.426314	145.742726	53.823898
3066.327728	136.453362	53.828903
3065.520724	135.276290	53.833908
3064.316586	139.644304	53.838913
3063.701104	138.977257	53.843917
3062.538268	139.862645	53.848922
3062.616377	141.330584	53.853927
3061.720577	134.747900	53.858932
3060.611048	140.817206	53.863937
3060.550823	139.976735	53.868941
3059.631943	142.825257	53.873946
3058.896673	141.230939	53.878951
3058.401362	139.164973	53.883956
3057.817506	143.500818	53.888961
3057.024001	128.921650	53.893965
3055.884130	140.968356	53.898970
3056.147950	140.492506	53.903975
3055.421801	138.119018	53.908980
3054.486320	134.746720	53.913985
3053.863256	129.501351	53.918989
3052.896708	136.266207	53.923994
3052.380087	134.777027	53.928999
3051.415880	134.100884	53.934004
3050.893906	136.007269	53.939009
3050.720618	127.947225	53.944013
3050.457645	138.758993	53.949018
3049.620244	136.052419	53.954023
3049.072644	146.360209	53.959028
3047.627472	142.100419	53.964033
3046.650735	140.102899	53.969037
3046.116633	136.480839	53.974042
3046.078662	132.523751	53.979047
3045.735710	129.612697	53.984052
3044.176254	141.993591	53.989057
3043.720871	133.354525	53.994061
3043.235081	140.029737	53.999066
3042.142553	137.585831	54.004071
3042.230105	128.475849	54.009076
3041.606908	126.746335	54.014081
3040.526955	139.436865	54.019085
3039.710539	144.544272	54.024090
3039.210285	140.601831	54.029095
3038.311701	139.700536	54.034100
3037.479483	129.544192	54.039105
3037.312743	128.669029	54.044109
3036.732896	139.229422	54.049114
3036.408590	127.620144	54.054119
3035.410212	137.828904	54.059124
3035.019684	136.242787	54.064129
3034.892901	135.689998	54.069133
3033.470601	137.943244	54.074138
3032.061483	136.348810	54.079143
3031.422262	142.998532	54.084148
3031.675690	145.038077	54.089153
3031.260231	136.161668	54.094157
3029.775664	140.368795	54.099162
3029.304612	133.389472	54.104167
3028.639832	127.846112	54.109172
3027.794660	137.380158	54.114177
3027.228606	145.471946	54.119181
3026.606221	134.122409	54.124186
3026.257564	141.046945	54.129191
3025.605653	142.055822	54.134196
3024.789724	141.636182	54.139201
3024.592551	133.187466	54.144205
3023.858984	140.602499	54.149210
3023.200575	142.681801	54.154215
3021.601927	134.817154	54.159220
3021.139736	139.665091	54.164225
3021.026212	129.613704	54.169229
3019.870882	136.756601	54.174234
3019.528980	128.908525	54.179239
3018.463925	131.086520	54.184244
3018.271082	135.451865	54.189249
3017.413729	126.409400	54.194253
3016.516340	137.841924	54.199258
3015.924751	138.135117	54.204263
3015.598092	134.538404	54.209268
3014.711084	131.880575	54.214273
3014.511508	131.646138	54.219277
3013.423285	139.680310	54.224282
3013.334487	132.687777	54.229287
3012.903286	130.963748	54.234292
3012.208772	143.381189	54.239297
3010.687474	128.286149	54.244301
3009.838735	137.808569	54.249306
3009.574090	130.408333	54.254311
3009.099563	129.907860	54.259316
3007.674772	135.565658	54.264321
3007.574920	124.011584	54.269325
3006.909859	135.438355	54.274330
3006.180268	133.024017	54.279335
3005.894190	127.190957	54.284340
3005.115605	133.280688	54.289345
3004.743457	119.232688	54.294349
3004.117759	133.348710	54.299354
3003.510940	130.417618	54.304359
3002.284139	119.909120	54.309364
3001.601191	134.709908	54.314369
3001.140616	119.769936	54.319373
3000.540180	131.748146	54.324378
2999.770170	129.271245	54.329383
2999.394269	129.711921	54.334388
2998.699058	138.701279	54.339393
2998.186213	126.499373	54.344397
2996.598402	133.275263	54.349402
2995.714126	135.070275	54.354407
2995.656095	129.632841	54.359412
2995.531454	133.358127	54.364417
2994.497301	134.305220	54.369421
2993.655043	138.993504	54.374426
2992.988085	133.841299	54.379431
2992.389980	136.956324	54.384436
2991.740182	137.863003	54.389441
2991.269074	129.969115	54.394445
2990.637556	136.535810	54.399450
2989.967899	135.977895	54.404455
2989.775341	134.582158	54.409460
2988.086307	135.063673	54.414465
2987.255583	132.893982	54.419469
2986.766718	137.767398	54.424474
2987.022798	134.560966	54.429479
2986.193540	132.942062	54.434484
2985.027482	139.566944	54.439489
2984.484967	128.448897	54.444493
2984.063295	126.373515	54.449498
2983.842139	129.923061	54.454503
2982.701431	127.119122	54.459508
2982.064173	131.524092	54.464513
2980.836033	125.527154	54.469517
2980.171319	140.304699	54.474522
2979.875408	134.460688	54.479527
2979.349728	120.469321	54.484532
2978.166841	133.620716	54.489537
2978.419610	124.514087	54.494541
2977.446949	126.297758	54.499546
2977.043682	120.436177	54.504551
2976.709463	118.142569	54.509556
2975.225613	133.763089	54.514561
2974.264441	125.808084	54.519565
2973.319220	129.158077	54.524570
2973.585165	127.246636	54.529575
2972.825707	123.908618	54.534580
2971.702406	128.665056	54.539585
2970.851128	118.535677	54.544589
2970.251466	124.436548	54.549594
2969.761057	130.413092	54.554599
2969.876377	128.639492	54.559604
2969.048005	136.523081	54.564609
2968.620627	128.666725	54.569613
2967.925104	132.111414	54.574618
2966.926693	125.324455	54.579623
2965.912538	123.854780	54.584628
2964.752881	131.699059	54.589633
2964.417109	127.398928	54.594637
2963.794654	133.052257	54.599642
2963.652101	129.296988	54.604647
2963.399261	128.995077	54.609652
2962.242222	122.159044	54.614657
2962.074256	119.007314	54.619661
2961.395742	128.274859	54.624666
2960.091176	120.823396	54.629671
2959.444780	115.272175	54.634676
2958.797504	126.186308	54.639681
2958.159570	121.159414	54.644685
2957.475240	118.274733	54.649690
2957.088104	133.419694	54.654695
2956.770995	127.213794	54.659700
2954.874583	124.160063	54.664705
2954.529529	122.073960	54.669709
2953.688825	121.251603	54.674714
2953.539344	115.642309	54.679719
2952.672192	112.931762	54.684724
2951.883962	122.241736	54.689729
2951.580026	116.909881	54.694733
2950.945631	122.173284	54.699738
2950.437379	116.541617	54.704743
2950.068053	118.874277	54.709748
2949.251870	122.731548	54.714753
2948.828607	120.253033	54.719757
2947.731390	129.614233	54.724762
2946.854981	110.876237	54.729767
2946.608988	113.569521	54.734772
2946.069609	125.189142	54.739777
2945.233160	120.251830	54.744781
2943.559163	123.253876	54.749786
2943.045220	117.654365	54.754791
2943.285948	116.314849	54.759796
2942.086110	129.777420	54.764801
2941.380695	118.099481	54.769805
2940.711282	124.420024	54.774810
2939.834229	125.409751	54.779815
2939.933194	122.039912	54.784820
2939.028937	126.193675	54.789825
2938.574505	121.854222	54.794829
2937.922327	124.033514	54.799834
2937.539303	120.156715	54.804839
2936.602849	120.411351	54.809844
2935.224204	115.012897	54.814849
2934.578467	111.028630	54.819853
2934.393890	117.955115	54.824858
2934.286360	117.931129	54.829863
2934.028485	120.760652	54.834868
2932.910203	123.777864	54.839873
2931.632106	119.125232	54.844877
2930.338202	127.210343	54.849882
2930.180959	125.744629	54.854887
2930.051204	120.690108	54.859892
2929.073981	119.339257	54.864897
2928.446672	120.480907	54.869901
2927.841194	123.353253	54.874906
2927.281844	120.420377	54.879911
2927.190943	119.766725	54.884916
2926.020595	123.175325	54.889921
2924.913376	121.859716	54.894925
2924.205417	121.774526	54.899930
2923.518939	121.348569	54.904935
2923.212024	118.809912	54.909940
2922.156116	124.997957	54.914945
2922.206233	126.341598	54.919949
2921.435503	126.072930	54.924954
2921.099153	119.834406	54.929959
2920.119015	115.485718	54.934964
2918.865066	124.625814	54.939969
2918.137164	122.750793	54.944973
2917.377541	119.989508	54.949978
2916.814543	123.767990	54.954983
2916.875904	121.734804	54.959988
2916.269204	126.676512	54.964993
2915.792498	119.085960	54.969997
2915.371717	113.445666	54.975002
2913.705387	114.162525	54.980007
2912.898061	119.791394	54.985012
2912.146283	130.869042	54.990017
2911.672563	124.787014	54.995021
2911.290813	125.237379	55.000026
2911.223954	124.758824	55.005031
2910.532694	118.312144	55.010036
2909.629339	128.623085	55.015041
2909.059247	118.787897	55.020045
2907.901661	126.604986	55.025050
2907.238578	122.693156	55.030055
2906.957531	122.955790	55.035060
2906.354992	115.784233	55.040065
2905.987304	117.060724	55.045069
2904.341351	123.290001	55.050074
2903.414666	123.619945	55.055079
2903.052056	119.487431	55.060084
2902.183533	118.217085	55.065089
2902.580289	110.668318	55.070093
2901.421026	117.670187	55.075098
2900.956844	116.689548	55.080103
2901.007970	120.400186	55.085108
2899.780634	118.185793	55.090113
2898.545722	114.288796	55.095117
2897.682150	120.509103	55.100122
2897.030221	125.607353	55.105127
2896.595489	114.821827	55.110132
2895.952655	118.015549	55.115137
2895.836730	109.604292	55.120141
2895.523276	119.314695	55.125146
2894.341341	124.629437	55.130151
2893.530333	122.784016	55.135156
2892.318502	128.696353	55.140161
2892.182751	117.153567	55.145165
2891.540042	116.602901	55.150170
2890.975260	118.966203	55.155175
2890.871624	117.145157	55.160180
2889.828689	117.111295	55.165185
2888.933658	117.392412	55.170189
2887.715761	114.162359	55.175194
2887.176018	119.583663	55.180199
2886.997476	106.700606	55.185204
2885.828252	121.289619	55.190209
2886.067849	111.151468	55.195213
2885.577218	120.219142	55.200218
2884.547638	129.912200	55.205223
2883.491857	116.385258	55.210228
2882.615982	120.533386	55.215233
2882.236704	110.980591	55.220237
2881.663143	110.427977	55.225242
2880.773610	120.159463	55.230247
2880.526162	106.807406	55.235252
2879.817779	130.535694	55.240257
2878.881497	121.680039	55.245261
2878.061137	127.111014	55.250266
2877.316652	120.023323	55.255271
2876.997741	114.306021	55.260276
2876.355530	120.555998	55.265281
2876.074066	112.899722	55.270285
2875.441083	121.270166	55.275290
2874.356097	119.222499	55.280295
2873.579160	111.571558	55.285300
2872.707326	121.208049	55.290305
2872.421284	116.105245	55.295309
2871.667382	120.230555	55.300314
2871.290896	129.406619	55.305319
2870.863947	118.624502	55.310324
2869.917170	122.810012	55.315329
2868.972591	124.159042	55.320333
2868.118194	118.625225	55.325338
2867.138662	124.005247	55.330343
2867.200094	112.574819	55.335348
2866.227044	117.409404	55.340353
2866.279992	121.108281	55.345357
2865.607654	118.427611	55.350362
2864.465446	124.956455	55.355367
2863.790050	113.747868	55.360372
2863.073352	117.646959	55.365377
2862.453608	117.402231	55.370381
2861.848351	113.744600	55.375386
2861.247127	122.027514	55.380391
2861.172469	113.393291	55.385396
2859.629981	118.697815	55.390401
2858.687021	117.344280	55.395405
2858.096783	120.702696	55.400410
2857.692038	125.584631	55.405415
2857.407378	115.822251	55.410420
2856.430859	122.247386	55.415425
2856.191274	116.703234	55.420429
2855.807479	117.326841	55.425434
2854.583815	117.619917	55.430439
2853.800760	108.139686	55.435444
2852.911896	118.512487	55.440449
2852.594802	112.867508	55.445453
2851.978066	118.682881	55.450458
2851.224090	124.175931	55.455463
2851.468993	117.639927	55.460468
2849.830178	112.285567	55.465473
2848.662274	107.163748	55.470477
2848.130444	115.389406	55.475482
2847.889465	115.550461	55.480487
2847.691721	105.318117	55.485492
2846.828783	116.768821	55.490497
2846.579303	105.750341	55.495501
2845.701571	103.370429	55.500506
2844.318524	111.631038	55.505511
2844.077500	116.256444	55.510516
2843.095425	119.820375	55.515521
2842.796688	115.649321	55.520525
2842.254943	117.787249	55.525530
2841.201361	125.338287	55.530535
2840.428721	110.889447	55.535540
2839.498424	123.654262	55.540545
2839.133799	117.390977	55.545549
2838.575497	117.318904	55.550554
2837.831228	124.439327	55.555559
2837.880824	109.795099	55.560564
2837.356673	121.224222	55.565569
2836.442115	117.154073	55.570573
2835.544266	118.175000	55.575578
2834.784358	119.259192	55.580583
2834.660361	107.853751	55.585588
2833.732267	118.622061	55.590593
2832.318256	119.630153	55.595597
2831.556505	111.007576	55.600602
2831.061684	126.466176	55.605607
2831.113645	114.577514	55.610612
2830.097755	115.666377	55.615617
2829.648792	111.554947	55.620621
2829.186701	115.955642	55.625626
2828.352595	118.958250	55.630631
2827.583944	118.700291	55.635636
2826.866589	119.731424	55.640641
2826.461728	113.020690	55.645645
2825.830800	119.818987	55.650650
2825.058371	112.134524	55.655655
2824.428288	109.692949	55.660660
2822.729480	122.594633	55.665665
2822.344080	120.710431	55.670669
2822.098689	120.612906	55.675674
2821.351642	117.083721	55.680679
2820.932951	107.611487	55.685684
2820.465347	115.683673	55.690689
2820.179986	116.493743	55.695693
2819.306898	120.423513	55.700698
2817.996142	120.542013	55.705703
2817.347531	119.713294	55.710708
2816.690034	115.120414	55.715713
2816.640701	113.494952	55.720717
2815.908255	111.118634	55.725722
2814.972867	119.905883	55.730727
2814.111139	110.885935	55.735732
2813.193035	114.466961	55.740737
2812.622098	114.309026	55.745741
2812.177741	113.357375	55.750746
2811.783377	116.471534	55.755751
2811.444113	107.134539	55.760756
2810.660879	111.844322	55.765761
2809.955359	114.054451	55.770765
2809.394461	119.018334	55.775770
2808.444315	124.694515	55.780775
2808.266365	113.790912	55.785780
2806.661962	117.638836	55.790785
2805.887252	111.088418	55.795789
2805.205126	112.988243	55.800794
2804.443065	114.588712	55.805799
2804.854411	109.666717	55.810804
2804.153435	110.550583	55.815809
2803.602042	105.527086	55.820813
2803.232815	108.125778	55.825818
2801.452324	110.324242	55.830823
2801.026393	112.213437	55.835828
2800.206359	113.093968	55.840833
2799.775870	118.803303	55.845837
2799.115704	116.070433	55.850842
2798.526844	120.700027	55.855847
2797.752203	113.769478	55.860852
2796.479411	118.349784	55.865857
2796.121581	122.555036	55.870861
2795.591590	115.043873	55.875866
2794.929671	112.224859	55.880871
2794.417932	118.510959	55.885876
2794.098434	128.680276	55.890881
2793.954194	115.481506	55.895885
2792.947420	114.104548	55.900890
2791.838127	117.401684	55.905895
2791.172183	106.560178	55.910900
2790.828857	111.883573	55.915905
2790.288209	115.503903	55.920909
2788.809540	109.637472	55.925914
2787.651234	121.084586	55.930919
2788.171800	107.951010	55.935924
2786.896233	111.954307	55.940929
2786.792640	116.326889	55.945933
2786.028366	121.389084	55.950938
2785.435878	126.699412	55.955943
2785.168671	115.521338	55.960948
2783.649602	127.370764	55.965953
2783.114240	108.222051	55.970957
2782.657856	117.144531	55.975962
2782.329937	121.087310	55.980967
2782.050262	113.204957	55.985972
2780.547451	117.197360	55.990977
2779.553166	118.779893	55.995981
2778.835020	115.914440	56.000986
2778.013243	124.613988	56.005991
2777.703373	108.697826	56.010996
2777.269927	108.236930	56.016001
2776.899932	111.913354	56.021005
2776.755612	117.545753	56.026010
2775.846806	123.882352	56.031015
2774.883396	113.337600	56.036020
2774.116419	116.551760	56.041025
2773.703614	111.318663	56.046029
2772.881508	114.050418	56.051034
2771.547350	114.184375	56.056039
2771.243114	110.873981	56.061044
2770.475293	112.626618	56.066049
2769.831703	110.930625	56.071053
2769.549178	110.807477	56.076058
2768.913402	114.826951	56.081063
2768.810703	111.521583	56.086068
2767.366136	111.763226	56.091073
2766.887065	106.687112	56.096077
2765.952406	108.875620	56.101082
2765.646437	118.604867	56.106087
2765.334827	111.369404	56.111092
2764.080496	116.573777	56.116097
2763.079019	117.480588	56.121101
2762.421627	116.421278	56.126106
2761.732017	117.215182	56.131111
2761.857891	113.078535	56.136116
2760.858555	117.096202	56.141121
2760.424680	107.104354	56.146125
2759.395068	107.604671	56.151130
2758.406112	113.790366	56.156135
2757.867269	104.085268	56.161140
2757.498902	117.050474	56.166145
2756.922423	111.886406	56.171149
2756.695707	110.758224	56.176154
2755.516382	116.802385	56.181159
2754.808426	103.505381	56.186164
2753.726427	113.227134	56.191169
2753.577049	109.810144	56.196173
2753.209382	110.027197	56.201178
2752.471698	108.473996	56.206183
2752.515251	110.108482	56.211188
2751.344398	114.730185	56.216193
2750.481752	115.817342	56.221197
2749.699741	112.544401	56.226202
2748.073620	116.230660	56.231207
2747.742518	110.622825	56.236212
2747.745526	113.564859	56.241217
2746.864406	104.807580	56.246221
2745.982550	109.682246	56.251226
2745.428521	114.102210	56.256231
2745.348392	102.129964	56.261236
2744.948837	111.363243	56.266241
2743.976839	106.589666	56.271245
2743.063500	107.025508	56.276250
2742.361246	111.646064	56.281255
2742.087401	107.368534	56.286260
2741.387715	120.288927	56.291265
2739.922759	107.696424	56.296269
2739.409218	108.805621	56.301274
2738.569547	115.134745	56.306279
2738.383022	96.363398	56.311284
2737.328314	107.930163	56.316289
2736.819891	107.956150	56.321293
2736.490307	107.713946	56.326298
2735.799593	118.444844	56.331303
2735.414900	106.812801	56.336308
2734.117117	109.255611	56.341313
2733.051065	108.799032	56.346317
2732.922346	109.200238	56.351322
2732.121087	113.915083	56.356327
2732.386907	108.933096	56.361332
2731.525885	105.574588	56.366337
2730.968164	107.365132	56.371341
2730.198350	105.717166	56.376346
2729.152874	114.087063	56.381351
2728.664545	109.696199	56.386356
2727.968803	110.214453	56.391361
2726.648484	112.107713	56.396365
2726.413885	106.727326	56.401370
2725.362977	117.185063	56.406375
2725.378143	102.030049	56.411380
2724.999735	104.304270	56.416385
2724.135012	112.290388	56.421389
2722.934290	107.184473	56.426394
2722.097909	105.061586	56.431399
2721.663159	107.901605	56.436404
2721.066309	115.568789	56.441409
2720.675714	115.198860	56.446413
2720.592038	108.131281	56.451418
2719.479245	111.993877	56.456423
2718.593861	122.239384	56.461428
2717.516773	115.887504	56.466433
2717.218584	109.231184	56.471437
2716.591357	103.968434	56.476442
2716.421641	108.178240	56.481447
2715.267057	107.648379	56.486452
2714.341099	103.690335	56.491457
2713.384513	106.666127	56.496461
2713.105739	106.669442	56.501466
2712.722306	105.545550	56.506471
2712.630426	103.602111	56.511476
2711.902803	110.109051	56.516481
2710.391008	109.689983	56.521485
2709.896246	101.958879	56.526490
2709.254356	113.750343	56.531495
2708.722241	107.870170	56.536500
2708.355549	110.637375	56.541505
2707.193410	106.355766	56.546509
2706.778370	104.564666	56.551514
2705.670946	109.510654	56.556519
2705.451946	114.813589	56.561524
2704.999551	115.690107	56.566529
2703.845549	109.508481	56.571533
2703.331678	105.251852	56.576538
2702.348278	106.210844	56.581543
2702.163881	102.953393	56.586548
2701.407630	108.221055	56.591553
2700.858584	108.044785	56.596557
2700.656231	100.805265	56.601562
2699.382613	111.334224	56.606567
2698.773508	102.745193	56.611572
2698.150053	102.580063	56.616577
2697.536312	106.055790	56.621581
2697.038467	107.433483	56.626586
2695.942018	112.079580	56.631591
2695.237351	103.392415	56.636596
2694.726742	112.746119	56.641601
2694.133368	108.772282	56.646605
2693.872021	102.070198	56.651610
2692.922772	109.513414	56.656615
2691.851842	105.257270	56.661620
2691.217580	102.494333	56.666625
2690.459785	103.017277	56.671629
2690.276442	95.906744	56.676634
2689.590116	104.946675	56.681639
2689.204147	102.862064	56.686644
2688.567867	105.768899	56.691649
2687.487099	104.272772	56.696653
2686.999104	99.860150	56.701658
2686.042019	106.394865	56.706663
2685.328952	106.105716	56.711668
2685.241270	105.129819	56.716673
2684.279163	108.078928	56.721677
2683.426620	105.193439	56.726682
2682.584704	112.689361	56.731687
2682.366844	108.345033	56.736692
2681.608879	104.467224	56.741697
2681.599868	108.236678	56.746701
2680.513867	96.047577	56.751706
2679.396853	112.664444	56.756711
2679.027963	107.149916	56.761716
2678.216286	117.589658	56.766721
2677.660860	109.311180	56.771725
2676.623441	106.711891	56.776730
2675.539070	102.817248	56.781735
2675.352684	95.951965	56.786740
2675.038705	111.533174	56.791745
2674.286824	105.628601	56.796749
2674.054636	103.677569	56.801754
2673.422397	105.897289	56.806759
2672.913720	105.911878	56.811764
2672.137133	106.753027	56.816769
2671.300555	107.048264	56.821773
2670.845219	97.071159	56.826778
2669.005432	104.052011	56.831783
2668.473996	100.722045	56.836788
2667.910899	107.357964	56.841793
2667.295924	95.794120	56.846797
2667.018147	90.489018	56.851802
2666.524531	103.281806	56.856807
2666.700316	96.195543	56.861812
2665.261287	97.807142	56.866817
2664.377811	108.944393	56.871821
2664.297887	99.152978	56.876826
2663.296938	105.887029	56.881831
2662.687594	105.629493	56.886836
2661.583928	99.740848	56.891841
2660.309005	109.710314	56.896845
2660.088583	101.490629	56.901850
2659.432195	105.122854	56.906855
2659.182297	97.061757	56.911860
2658.821974	100.877839	56.916865
2658.127637	108.418006	56.921869
2657.498661	103.172538	56.926874
2656.144451	101.108968	56.931879
2655.617360	101.319332	56.936884
2655.234248	97.607974	56.941889
2654.778815	107.325652	56.946893
2654.389310	99.986686	56.951898
2653.116751	108.232777	56.956903
2652.276019	99.678615	56.961908
2652.058747	105.377553	56.966913
2651.518230	106.457421	56.971917
2650.778574	104.257620	56.976922
2649.831569	106.996132	56.981927
2649.423650	98.824683	56.986932
2648.772950	104.449293	56.991937
2648.233531	109.239777	56.996941
2647.193444	102.315957	57.001946
2646.152377	111.014306	57.006951
2645.627359	103.415486	57.011956
2644.937399	104.069336	57.016961
2644.437252	99.232495	57.021965
2644.242885	107.592300	57.026970
2643.772093	104.889845	57.031975
2642.868671	104.334434	57.036980
2642.130295	106.903473	57.041985
2641.062221	104.917307	57.046989
2640.819388	97.231966	57.051994
2640.149137	105.078268	57.056999
2639.134062	98.325039	57.062004
2638.205898	101.510317	57.067009
2637.350432	95.565831	57.072013
2637.306133	98.562523	57.077018
2636.467851	109.462715	57.082023
2635.787630	103.205254	57.087028
2635.543798	101.265689	57.092033
2635.450813	101.540002	57.097037
2634.674352	99.982791	57.102042
2633.701067	98.811318	57.107047
2633.217313	92.727508	57.112052
2631.668305	102.202263	57.117057
2630.624142	99.478616	57.122061
2630.297615	90.329740	57.127066
2629.645940	101.753010	57.132071
2629.241352	97.043516	57.137076
2628.749656	99.924455	57.142081
2628.133150	102.888307	57.147085
2627.987048	92.058248	57.152090
2627.460572	103.308149	57.157095
2626.244632	98.463014	57.162100
2625.420591	96.302510	57.167105
2624.954439	109.049554	57.172109
2624.543748	93.628293	57.177114
2623.101348	97.736317	57.182119
2622.301583	98.761428	57.187124
2622.030662	96.969384	57.192129
2621.562082	109.186334	57.197133
2621.277382	94.822317	57.202138
2620.604277	110.342149	57.207143
2619.522793	104.822735	57.212148
2618.668551	104.132609	57.217153
2618.171377	110.483323	57.222157
2617.968843	103.001482	57.227162
2617.372086	101.751043	57.232167
2615.809088	103.062540	57.237172
2615.240379	104.791815	57.242177
2614.204201	116.571735	57.247181
2613.918508	100.481754	57.252186
2613.495550	109.529561	57.257191
2613.265494	98.126106	57.262196
2612.881676	102.432506	57.267201
2611.732486	106.683432	57.272205
2611.073333	100.463822	57.277210
2610.120206	110.337234	57.282215
2610.019401	108.838205	57.287220
2608.641262	94.010602	57.292225
2607.943022	102.538639	57.297229
2607.360604	103.316210	57.302234
2606.655319	102.229583	57.307239
2606.567014	104.687894	57.312244
2606.010708	102.604384	57.317249
2605.343152	109.634334	57.322253
2604.530890	110.220678	57.327258
2603.783954	109.580103	57.332263
2603.630090	107.130571	57.337268
2602.665382	103.267593	57.342273
2601.140191	107.715029	57.347277
2600.779551	101.944900	57.352282
2600.037422	105.896908	57.357287
2599.573445	100.664297	57.362292
2599.090601	103.722930	57.367297
2598.775444	105.845033	57.372301
2598.246935	95.289550	57.377306
2596.774335	105.672932	57.382311
2596.274447	105.502479	57.387316
2595.886152	106.251998	57.392321
2595.241518	110.102476	57.397325
2594.574436	100.719720	57.402330
2593.424953	107.690743	57.407335
2593.119669	100.874607	57.412340
2592.558172	97.135725	57.417345
2591.722302	98.178065	57.422349
2591.806904	99.419883	57.427354
2590.024203	104.984990	57.432359
2589.286830	104.715403	57.437364
2588.774140	103.190078	57.442369
2588.346909	97.201212	57.447373
2588.021409	95.374292	57.452378
2587.686320	101.908473	57.457383
2586.790433	100.562336	57.462388
2585.679524	103.870041	57.467393
2584.923360	107.257232	57.472397
2584.355074	97.768779	57.477402
2583.873263	101.592605	57.482407
2583.401433	104.908690	57.487412
2582.752873	107.790397	57.492417
2581.620517	104.338965	57.497421
2581.458005	109.987096	57.502426
2580.590673	104.544763	57.507431
2580.394217	101.390826	57.512436
2579.071514	103.875820	57.517441
2577.996205	105.101983	57.522445
2577.731162	104.889412	57.527450
2577.253187	101.466243	57.532455
2577.055744	102.896008	57.537460
2576.577266	92.932748	57.542465
2575.500414	106.096412	57.547469
2574.941675	92.574227	57.552474
2574.151699	105.369913	57.557479
2573.108832	99.855358	57.562484
2572.184616	106.304731	57.567489
2571.306318	101.957267	57.572493
2571.120344	97.222249	57.577498
2570.695844	106.635437	57.582503
2569.866154	103.652907	57.587508
2569.428075	101.500640	57.592513
2569.088549	108.312677	57.597517
2568.435951	102.449178	57.602522
2567.569838	104.340216	57.607527
2566.786527	105.297392	57.612532
2566.564316	104.498045	57.617537
2565.134288	117.951429	57.622541
2564.790479	103.502787	57.627546
2564.111374	107.303503	57.632551
2563.666736	112.187127	57.637556
2562.754185	102.168205	57.642561
2561.737095	104.443857	57.647565
2561.310648	100.118621	57.652570
2560.319525	115.333622	57.657575
2559.767042	112.205812	57.662580
2559.609889	107.650597	57.667585
2559.096865	112.595252	57.672589
2558.434071	106.647052	57.677594
2557.110636	112.416280	57.682599
2556.504999	109.322425	57.687604
2556.362601	106.439897	57.692609
2555.534916	113.824056	57.697613
2555.360026	102.545383	57.702618
2553.810520	108.199710	57.707623
2553.240298	109.576761	57.712628
2552.931962	98.228539	57.717633
2552.252648	113.447863	57.722637
2551.684439	108.209786	57.727642
2550.652032	113.978999	57.732647
2549.930689	106.693616	57.737652
2549.368155	103.582922	57.742657
2548.804090	101.331409	57.747661
2548.722911	104.232565	57.752666
2547.946070	105.403368	57.757671
2547.067046	101.837981	57.762676
2546.376181	101.312167	57.767681
2546.018115	106.407167	57.772685
2545.121704	97.221125	57.777690
2543.604471	101.174991	57.782695
2543.070085	102.677753	57.787700
2543.120794	94.856589	57.792705
2542.238346	102.679171	57.797709
2542.384450	97.219908	57.802714
2540.689310	100.663813	57.807719
2540.206362	99.720758	57.812724
2539.918511	98.920791	57.817729
2539.031211	106.651050	57.822733
2538.495515	89.868072	57.827738
2537.502209	97.530399	57.832743
2536.294435	101.951214	57.837748
2535.954551	99.002979	57.842753
2535.138248	94.955179	57.847757
2535.055996	92.836029	57.852762
2534.615369	99.535087	57.857767
2534.090420	102.845255	57.862772
2533.324061	99.911510	57.867777
2532.422716	109.490294	57.872781
2531.774952	96.166094	57.877786
2531.083271	100.045142	57.882791
2530.365147	108.608952	57.887796
2529.346391	103.766841	57.892801
2528.386576	109.286415	57.897805
2528.211473	102.589343	57.902810
2527.764853	103.134503	57.907815
2527.180531	104.566859	57.912820
2526.775512	108.630184	57.917825
2526.218775	113.067595	57.922829
2525.428862	103.343890	57.927834
2524.438074	107.455649	57.932839
2523.861000	105.549772	57.937844
2523.254386	97.439944	57.942849
2521.949152	104.562728	57.947853
2521.183981	96.168570	57.952858
2520.831113	108.389811	57.957863
2519.963581	106.264389	57.962868
2519.939162	96.706259	57.967873
2519.339122	113.874990	57.972877
2519.125715	95.761954	57.977882
2518.095327	107.985736	57.982887
2517.252232	100.663943	57.987892
2516.787388	103.703320	57.992897
2516.059712	107.020517	57.997901
2515.202973	91.009248	58.002906
2514.204284	99.867326	58.007911
2513.642285	93.993483	58.012916
2513.517337	102.697451	58.017921
2512.819966	101.175288	58.022925
2512.062622	94.123435	58.027930
2510.907261	108.957575	58.032935
2510.471668	102.106492	58.037940
2509.858693	95.585333	58.042945
2509.610533	101.906105	58.047949
2509.182031	97.624647	58.052954
2507.827134	97.532484	58.057959
2507.129466	99.089216	58.062964
2506.590618	99.716458	58.067969
2505.918487	101.698283	58.072973
2505.378770	100.238770	58.077978
2504.619322	101.938297	58.082983
2503.893199	110.272957	58.087988
2503.377149	110.127775	58.092993
2502.463326	109.124576	58.097997
2502.266694	97.758056	58.103002
2501.041655	102.218933	58.108007
2500.336803	103.500982	58.113012
2499.852991	102.721099	58.118017
2499.482456	104.118882	58.123021
2498.792794	100.082593	58.128026
2498.431134	106.213173	58.133031
2497.296308	108.556331	58.138036
2497.017255	92.252099	58.143041
2496.115000	97.786305	58.148045
2495.570940	89.641319	58.153050
2494.696379	98.664092	58.158055
2493.737099	95.358350	58.163060
2493.308117	95.264597	58.168065
2492.500037	102.563697	58.173069
2492.323308	98.704575	58.178074
2491.850228	97.761417	58.183079
2490.648565	102.605918	58.188084
2490.164461	95.166708	58.193089
2489.226127	103.648563	58.198093
2489.118917	96.047421	58.203098
2488.011595	90.716009	58.208103
2486.805793	92.942622	58.213108
2486.263221	90.860333	58.218113
2485.742795	96.443335	58.223117
2485.522395	94.177285	58.228122
2484.868832	104.488549	58.233127
2484.007001	91.860545	58.238132
2484.128468	100.622642	58.243137
2482.984175	107.052414	58.248141
2482.094955	100.886765	58.253146
2481.503772	109.517687	58.258151
2480.806617	104.924147	58.263156
2480.766500	97.903619	58.268161
2479.599069	108.915745	58.273165
2478.721461	98.972977	58.278170
2478.277396	104.095311	58.283175
2477.702299	98.918029	58.288180
2476.897848	92.542110	58.293185
2475.846333	106.449842	58.298189
2475.231664	97.633661	58.303194
2474.439253	98.505566	58.308199
2474.152734	111.414122	58.313204
2473.883030	104.687835	58.318209
2473.464251	107.701576	58.323213
2472.559055	90.760348	58.328218
2471.203215	94.760450	58.333223
2470.774103	97.698985	58.338228
2470.375125	96.031868	58.343233
2469.823703	105.969235	58.348237
2469.103857	100.286983	58.353242
2468.244922	99.119675	58.358247
2467.415179	94.941163	58.363252
2467.034865	97.945564	58.368257
2466.509580	108.047009	58.373261
2465.873557	92.202486	58.378266
2464.880733	102.945555	58.383271
2464.123786	106.289472	58.388276
2464.010579	96.276808	58.393281
2463.356015	98.152610	58.398285
2462.525376	97.799121	58.403290
2461.890637	98.688280	58.408295
2460.996122	96.475907	58.413300
2460.791154	99.265599	58.418305
2459.024597	103.624073	58.423309
2458.536323	96.458730	58.428314
2457.800065	100.943806	58.433319
2456.993709	95.795410	58.438324
2457.160228	93.867012	58.443329
2456.522649	96.003192	58.448333
2456.440812	90.224892	58.453338
2455.821043	100.263542	58.458343
2454.582222	98.634624	58.463348
2454.242958	97.888452	58.468353
2453.356187	98.599262	58.473357
2451.987905	102.672546	58.478362
2451.398551	100.883643	58.483367
2450.574296	108.618920	58.488372
2450.447176	95.200200	58.493377
2450.084991	100.963380	58.498381
2449.521275	98.140261	58.503386
2448.578100	99.330830	58.508391
2447.350044	99.632638	58.513396
2447.066056	95.787912	58.518401
2446.697699	105.720031	58.523405
2446.393973	102.092618	58.528410
2445.227422	104.948034	58.533415
2444.394509	95.826949	58.538420
2444.017381	101.373613	58.543425
2442.999912	103.065947	58.548429
2442.964073	105.636861	58.553434
2441.588085	99.435241	58.558439
2440.560724	99.424457	58.563444
2440.460633	90.002827	58.568449
2440.212026	102.001764	58.573453
2439.927186	103.519499	58.578458
2438.988022	98.541438	58.583463
2437.901133	99.193705	58.588468
2437.320130	94.389271	58.593473
2436.643542	94.082866	58.598477
2436.220580	96.418003	58.603482
2434.546387	101.500008	58.608487
2433.717551	97.467001	58.613492
2433.946157	88.878089	58.618497
2433.394174	103.227368	58.623501
2432.575189	93.848915	58.628506
2432.524482	95.751340	58.633511
2431.548209	99.198282	58.638516
2430.509309	91.931305	58.643521
2429.566523	91.700019	58.648525
2429.112254	92.340437	58.653530
2428.780070	93.912843	58.658535
2428.150627	93.436937	58.663540
2427.935805	85.416457	58.668545
2426.486273	89.581396	58.673549
2426.120009	92.184329	58.678554
2425.385616	95.490840	58.683559
2424.854487	95.799807	58.688564
2423.947150	92.189552	58.693569
2422.928076	101.503871	58.698573
2422.611368	91.973231	58.703578
2422.117638	99.704885	58.708583
2421.582603	98.484573	58.713588
2421.057786	87.624565	58.718593
2419.746566	106.489029	58.723597
2419.035487	97.705528	58.728602
2418.693842	88.982414	58.733607
2418.018145	97.319896	58.738612
2417.824765	99.978927	58.743617
2417.253967	108.678204	58.748621
2416.239970	92.835164	58.753626
2415.735745	93.135584	58.758631
2415.082132	92.846963	58.763636
2414.364005	84.548211	58.768641
2412.905678	100.573318	58.773645
2412.100897	94.787974	58.778650
2411.696963	91.893727	58.783655
2411.082740	100.073469	58.788660
2411.156365	87.004110	58.793665
2410.166953	96.573478	58.798669
2410.405027	92.575155	58.803674
2409.319296	93.016053	58.808679
2408.207724	93.852539	58.813684
2407.656162	97.132133	58.818689
2407.154226	101.459522	58.823693
2406.202735	96.587785	58.828698
2405.710903	93.721593	58.833703
2405.041915	99.587755	58.838708
2405.244680	97.983542	58.843713
2403.798562	93.993717	58.848717
2403.045145	97.867937	58.853722
2401.637177	106.331813	58.858727
2400.932483	95.437824	58.863732
2401.105033	92.894206	58.868737
2399.928853	98.591701	58.873741
2399.257262	98.861531	58.878746
2398.892566	96.408981	58.883751
2398.329239	98.090776	58.888756
2398.139323	90.178930	58.893761
2396.904979	97.741568	58.898765
2395.957801	87.142459	58.903770
2395.165156	98.434307	58.908775
2394.827037	96.436671	58.913780
2394.259496	95.520331	58.918785
2393.875497	106.921124	58.923789
2393.418522	104.003184	58.928794
2392.405490	95.892217	58.933799
2391.433581	108.120218	58.938804
2391.310009	100.904367	58.943809
2390.772625	104.347719	58.948813
2389.841931	96.959227	58.953818
2389.171433	94.491863	58.958823
2388.164991	98.326455	58.963828
2387.723151	96.338265	58.968833
2387.517628	100.493399	58.973837
2386.290794	94.023540	58.978842
2385.486665	90.743793	58.983847
2384.822707	102.961370	58.988852
2384.847486	93.012359	58.993857
2384.197762	94.128290	58.998861
2382.780135	91.163038	59.003866
2382.196907	94.849481	59.008871
2381.260956	96.138296	59.013876
2381.154269	94.490287	59.018881
2380.564364	97.921697	59.023885
2380.127238	98.549715	59.028890
2379.118013	97.671399	59.033895
2377.991656	99.930238	59.038900
2377.951177	93.816461	59.043905
2377.200256	96.090444	59.048909
2376.953752	96.427720	59.053914
2376.153229	93.745362	59.058919
2374.872489	101.515272	59.063924
2374.471122	84.635169	59.068929
2373.622605	90.057964	59.073933
2373.474397	90.996568	59.078938
2372.994351	92.782147	59.083943
2371.791632	100.920808	59.088948
2371.422917	91.744451	59.093953
2370.987679	96.599233	59.098957
2369.897164	96.843989	59.103962
2368.741557	92.660823	59.108967
2367.796574	94.516822	59.113972
2367.816728	92.384510	59.118977
2367.054224	89.483293	59.123981
2366.666695	91.799744	59.128986
2365.963177	96.591454	59.133991
2365.464033	95.555663	59.138996
2364.606165	90.882263	59.144001
2363.839559	91.945157	59.149005
2363.243861	89.071469	59.154010
2362.831260	90.142910	59.159015
2362.452730	96.594516	59.164020
2361.508467	89.218224	59.169025
2360.347726	95.567534	59.174029
2359.891930	94.714588	59.179034
2359.457323	95.976101	59.184039
2358.347859	92.842116	59.189044
2357.612643	90.246486	59.194049
2357.078020	96.135461	59.199053
2356.978240	92.637786	59.204058
2356.389898	94.217286	59.209063
2355.622428	92.748184	59.214068
2354.608572	96.245376	59.219073
2353.750201	95.895067	59.224077
2353.163729	88.981790	59.229082
2352.992462	85.233060	59.234087
2352.255629	96.958638	59.239092
2351.780964	86.779256	59.244097
2350.588090	97.716791	59.249101
2350.055474	94.349967	59.254106
2349.639636	82.775052	59.259111
2349.024166	95.088539	59.264116
2348.009714	93.137082	59.269121
2346.839914	90.877070	59.274125
2346.649907	92.262938	59.279130
2346.220643	89.285007	59.284135
2345.506530	96.703435	59.289140
2345.211980	96.281981	59.294145
2344.140078	90.115239	59.299149
2343.494065	86.872013	59.304154
2343.255535	83.706344	59.309159
2342.106843	96.694013	59.314164
2341.075148	98.952461	59.319169
2340.144899	90.285402	59.324173
2339.998424	89.772315	59.329178
2339.713666	83.446114	59.334183
2339.347523	89.600742	59.339188
2338.631004	87.408482	59.344193
2337.451314	85.546071	59.349197
2336.695573	92.931749	59.354202
2336.368821	83.355084	59.359207
2335.734859	91.321890	59.364212
2334.829174	86.985872	59.369217
2333.688738	91.918606	59.374221
2333.163809	88.814540	59.379226
2332.910740	87.753649	59.384231
2332.413769	90.204863	59.389236
2332.247651	86.466307	59.394241
2330.828581	94.948270	59.399245
2330.250205	89.170808	59.404250
2329.589591	86.475983	59.409255
2329.269027	94.133027	59.414260
2328.717366	87.367744	59.419265
2327.362066	97.279542	59.424269
2326.555632	95.600009	59.429274
2326.184800	85.631027	59.434279
2325.430218	91.085131	59.439284
2325.585166	78.221745	59.444289
2324.683644	87.755955	59.449293
2323.476944	94.684292	59.454298
2322.779794	89.825530	59.459303
2322.293348	86.908300	59.464308
2322.005597	85.804789	59.469313
2321.025315	87.586701	59.474317
2319.601578	86.808881	59.479322
2319.301423	83.833744	59.484327
2319.172030	88.429787	59.489332
2318.940814	91.089760	59.494337
2318.550976	84.810738	59.499341
2317.248044	82.284958	59.504346
2316.742516	74.172897	59.509351
2315.466170	91.208556	59.514356
2314.648996	78.478639	59.519361
2313.898838	86.052433	59.524365
2313.489025	85.086238	59.529370
2313.009987	75.197345	59.534375
2311.873924	93.400290	59.539380
2311.989491	85.471745	59.544385
2311.261173	91.018066	59.549389
2311.074292	89.017076	59.554394
2310.197025	85.574988	59.559399
2309.015938	87.069935	59.564404
2308.825361	83.295696	59.569409
2307.726446	89.672333	59.574413
2306.799443	91.980381	59.579418
2306.335604	81.621929	59.584423
2305.670349	90.867855	59.589428
2305.317997	88.142031	59.594433
2304.970967	89.836186	59.599437
2304.074508	91.115891	59.604442
2303.455969	86.982217	59.609447
2302.412154	94.626361	59.614452
2302.205423	85.022072	59.619457
2300.929559	91.910135	59.624461
2300.346288	86.311931	59.629466
2299.658555	78.660880	59.634471
2298.981966	85.579487	59.639476
2298.877095	86.275032	59.644481
2298.413371	85.660676	59.649485
2297.025222	95.981105	59.654490
2296.336504	89.517939	59.659495
2295.927580	97.394164	59.664500
2295.700601	94.326386	59.669505
2294.699339	90.814716	59.674509
2293.376575	89.566101	59.679514
2292.950279	92.730337	59.684519
2292.252530	100.538326	59.689524
2292.248741	93.009122	59.694529
2291.665972	95.608033	59.699533
2290.878439	90.726838	59.704538
2290.139095	90.810116	59.709543
2288.978284	96.949457	59.714548
2288.837609	89.976538	59.719553
2288.318753	87.179718	59.724557
2287.546336	93.703020	59.729562
2286.466846	85.342146	59.734567
2285.887229	92.998488	59.739572
2285.451324	79.379596	59.744577
2285.084009	87.467377	59.749581
2284.123280	83.251700	59.754586
2283.276211	86.358815	59.759591
2282.839590	101.068079	59.764596
2282.055379	84.644242	59.769601
2281.523841	92.904972	59.774605
2280.167432	91.548827	59.779610
2279.640770	88.863075	59.784615
2278.971285	93.959223	59.789620
2278.875142	99.521389	59.794625
2278.444072	99.106705	59.799629
2277.748669	91.689456	59.804634
2276.909312	89.151910	59.809639
2275.710311	94.516232	59.814644
2275.300288	92.292096	59.819649
2275.079149	93.784732	59.824653
2274.354348	90.404995	59.829658
2273.608886	85.106495	59.834663
2272.477107	95.793204	59.839668
2272.343972	93.381987	59.844673
2271.885736	93.059973	59.849677
2270.713052	87.613485	59.854682
2269.829996	88.442499	59.859687
2269.077023	88.147598	59.864692
2268.685582	83.320251	59.869697
2268.335613	93.133162	59.874701
2267.948724	86.921929	59.879706
2267.335595	86.276285	59.884711
2265.870895	97.520828	59.889716
2265.173439	92.716600	59.894721
2264.693766	90.297541	59.899725
2264.177135	95.656094	59.904730
2263.977462	93.170996	59.909735
2263.055550	94.813467	59.914740
2262.493142	92.225800	59.919745
2261.820531	96.880791	59.924750
2261.091016	99.505983	59.929754
2259.923211	85.064522	59.934759
2258.855442	100.352222	59.939764
2258.626063	92.802785	59.944769
2257.934924	92.486654	59.949774
2257.453689	94.812424	59.954778
2257.501527	86.454165	59.959783
2256.778832	98.705860	59.964788
2255.771247	92.768527	59.969793
2254.821360	97.311072	59.974798
2254.046310	97.493220	59.979802
2254.244618	96.158967	59.984807
2253.073828	99.433942	59.989812
2252.355565	90.084495	59.994817
2252.058266	88.617109	59.999822
2251.209900	96.740975	60.004826
2250.355312	91.607975	60.009831
2249.237180	93.820037	60.014836
2248.994611	91.929622	60.019841
2248.632439	97.516753	60.024846
2248.199695	93.421179	60.029850
2247.187257	93.609583	60.034855
2245.971144	94.878042	60.039860
2245.406160	91.163096	60.044865
2244.879884	84.310992	60.049870
2244.441537	94.877935	60.054874
2244.040539	92.613970	60.059879
2242.882456	86.212134	60.064884
2242.699503	85.249386	60.069889
2241.930514	92.124591	60.074894
2241.154711	85.423312	60.079898
2240.979916	91.389698	60.084903
2239.477099	89.871898	60.089908
2238.978359	82.324717	60.094913
2238.328718	83.825108	60.099918
2237.808261	87.310174	60.104922
2237.547788	80.236966	60.109927
2236.413162	87.216143	60.114932
2235.590549	84.380094	60.119937
2234.962170	92.009646	60.124942
2234.251268	88.385575	60.129946
2234.361336	82.805784	60.134951
2232.987812	94.603137	60.139956
2232.330078	82.872252	60.144961
2231.814485	85.980316	60.149966
2231.201138	96.619818	60.154970
2231.119669	89.948610	60.159975
2229.492906	98.328746	60.164980
2229.011961	90.924568	60.169985
2228.296221	87.209355	60.174990
2227.646036	92.262733	60.179994
2227.196467	90.235621	60.184999
2226.959302	100.131476	60.190004
2226.120514	89.456644	60.195009
2224.993950	93.721127	60.200014
2224.789804	89.487784	60.205018
2224.235450	95.692363	60.210023
2223.298280	90.846640	60.215028
2222.273252	94.755089	60.220033
2221.689055	90.927384	60.225038
2220.959953	92.510837	60.230042
2220.565799	85.949156	60.235047
2220.274877	87.938445	60.240052
2219.965216	85.751229	60.245057
2218.717445	92.713446	60.250062
2217.699999	90.357544	60.255066
2217.595008	83.035914	60.260071
2216.783964	97.555000	60.265076
2216.233124	81.050228	60.270081
2215.068778	82.126294	60.275086
2214.455656	83.430975	60.280090
2214.645444	79.551040	60.285095
2213.330582	90.832723	60.290100
2212.477758	81.422622	60.295105
2211.873718	85.264995	60.300110
2211.143863	87.478159	60.305114
2210.967442	86.063917	60.310119
2210.156682	90.552674	60.315124
2209.506643	82.840328	60.320129
2208.318123	83.176084	60.325134
2207.519141	81.098208	60.330138
2207.533647	77.613761	60.335143
2206.699741	85.274906	60.340148
2206.392037	79.668277	60.345153
2205.959849	86.462990	60.350158
2204.535298	89.846498	60.355162
2204.438466	85.326000	60.360167
2203.636785	92.385212	60.365172
2202.845236	94.387095	60.370177
2201.874775	91.049382	60.375182
2201.147848	94.394505	60.380186
2201.035420	82.234858	60.385191
2200.397522	82.745255	60.390196
2199.695360	85.195254	60.395201
2198.716449	85.285963	60.400206
2197.534382	88.342225	60.405210
2197.592152	84.683806	60.410215
2196.997632	83.246729	60.415220
2196.691988	86.533224	60.420225
2195.628663	84.035969	60.425230
2194.605326	84.231773	60.430234
2194.266202	85.837347	60.435239
2193.517102	86.527415	60.440244
2193.292790	87.625479	60.445249
2192.060448	90.756259	60.450254
2191.098654	89.357125	60.455258
2190.877895	82.158319	60.460263
2190.334244	84.851595	60.465268
2190.096976	80.308538	60.470273
2189.246293	87.743616	60.475278
2188.327762	87.566642	60.480282
2188.019259	80.544285	60.485287
2187.199307	91.414503	60.490292
2186.069087	85.365536	60.495297
2185.394466	85.213163	60.500302
2184.529297	80.766043	60.505306
2184.517352	73.531531	60.510311
2184.080719	74.174478	60.515316
2182.928177	79.375739	60.520321
2182.108354	81.981251	60.525326
2181.457264	80.705818	60.530330
2181.135513	74.169659	60.535335
2180.463466	79.378743	60.540340
2179.582157	73.579702	60.545345
2178.510673	73.544936	60.550350
2177.799223	90.676222	60.555354
2177.339063	83.408627	60.560359
2176.924427	90.278890	60.565364
2176.551880	82.873159	60.570369
2176.638592	75.855054	60.575374
2175.670108	86.492918	60.580378
2174.677990	82.401051	60.585383
2173.829581	87.385310	60.590388
2172.480561	83.777623	60.595393
2171.771502	72.694987	60.600398
2171.189214	75.526707	60.605402
2170.871423	72.900378	60.610407
2170.427988	78.793494	60.615412
2170.113174	82.432070	60.620417
2169.450948	79.380323	60.625422
2168.863408	82.486090	60.630426
2168.183348	80.864311	60.635431
2166.799283	84.814038	60.640436
2166.953775	81.042767	60.645441
2165.992626	77.075865	60.650446
2164.846249	85.739363	60.655450
2164.678565	68.721476	60.660455
2163.804318	76.796082	60.665460
2163.303888	83.860218	60.670465
2162.315098	75.067443	60.675470
2161.468252	74.607830	60.680474
2161.299192	81.468851	60.685479
2160.697555	79.324865	60.690484
2160.267921	77.302641	60.695489
2159.613053	78.220140	60.700494
2158.124749	87.442625	60.705498
2157.857721	73.056756	60.710503
2157.264684	83.815927	60.715508
2156.494209	79.046710	60.720513
2155.496342	79.120143	60.725518
2154.361885	77.026233	60.730522
2154.745540	71.466762	60.735527
2153.898378	76.559354	60.740532
2153.529970	72.023338	60.745537
2153.195886	77.928935	60.750542
2152.006012	84.092603	60.755546
2151.090277	77.523433	60.760551
2150.488747	87.981308	60.765556
2149.840641	80.891121	60.770561
2149.858342	71.506626	60.775566
2148.464255	81.449939	60.780570
2148.321500	68.719599	60.785575
2147.202283	82.395754	60.790580
2146.595228	80.185199	60.795585
2146.384087	73.396452	60.800590
2144.886083	81.113549	60.805594
2144.649216	77.022385	60.810599
2144.151587	77.003556	60.815604
2143.806162	81.245765	60.820609
2142.933713	79.370720	60.825614
2141.341266	78.369181	60.830618
2141.203162	75.446081	60.835623
2140.315698	77.956591	60.840628
2139.891171	78.228011	60.845633
2139.370772	80.980073	60.850638
2139.452994	85.194536	60.855642
2138.191567	74.127829	60.860647
2137.079138	81.819640	60.865652
2136.739862	80.005377	60.870657
2136.917046	73.075614	60.875662
2135.643399	79.415446	60.880666
2135.060781	75.222371	60.885671
2134.312517	82.290210	60.890676
2133.204677	76.746625	60.895681
2132.335084	76.125913	60.900686
2131.460343	87.604688	60.905690
2131.302829	87.459009	60.910695
2130.816197	84.921161	60.915700
2130.511452	81.256853	60.920705
2130.179154	81.602102	60.925710
2128.764744	79.391085	60.930714
2128.241501	75.725860	60.935719
2127.714402	78.879317	60.940724
2126.901854	74.549127	60.945729
2125.996987	69.757906	60.950734
2125.030066	76.878930	60.955738
2124.529557	76.362062	60.960743
2124.044956	81.220551	60.965748
2123.486676	84.665120	60.970753
2123.587919	88.716862	60.975758
2122.353747	83.484609	60.980762
2121.588923	81.706420	60.985767
2120.385989	83.178300	60.990772
2120.209332	84.517285	60.995777
2120.038342	75.163879	61.000782
2118.999502	84.080952	61.005786
2118.165117	79.937254	61.010791
2117.654171	78.578258	61.015796
2116.876912	82.876562	61.020801
2116.655592	76.580592	61.025806
2115.630988	80.719498	61.030810
2115.100341	74.238416	61.035815
2114.454479	85.554497	61.040820
2113.765629	80.463049	61.045825
2112.628851	74.249446	61.050830
2111.604753	81.703135	61.055834
2111.358842	71.053650	61.060839
2110.892888	76.699181	61.065844
2110.675611	76.920946	61.070849
2110.447372	76.667369	61.075854
2109.161588	77.778436	61.080858
2108.787920	68.954285	61.085863
2107.774522	81.605015	61.090868
2106.923510	76.006063	61.095873
2106.236281	78.703375	61.100878
2105.590504	73.903369	61.105882
2105.206741	76.904421	61.110887
2104.121089	73.145136	61.115892
2103.721372	75.465260	61.120897
2103.317753	82.484023	61.125902
2102.258018	83.441566	61.130906
2101.639568	81.468615	61.135911
2101.098383	79.922169	61.140916
2100.653703	77.420570	61.145921
2099.721583	75.166545	61.150926
2098.544954	84.522828	61.155930
2098.214320	79.839834	61.160935
2097.729278	78.666666	61.165940
2097.348787	78.435971	61.170945
2097.005947	77.351766	61.175950
2095.926310	85.684133	61.180954
2094.984262	77.941234	61.185959
2094.145473	78.768229	61.190964
2093.801955	86.088544	61.195969
2093.508926	77.395462	61.200974
2092.652893	85.168947	61.205978
2092.089560	83.050391	61.210983
2091.393246	79.352407	61.215988
2090.792034	77.952802	61.220993
2089.585762	81.054274	61.225998
2088.541956	85.360673	61.231002
2088.468472	77.134495	61.236007
2087.813517	79.935626	61.241012
2087.517613	70.026116	61.246017
2087.144938	69.076483	61.251022
2085.686711	74.395171	61.256026
2085.145647	78.482559	61.261031
2084.605309	83.982532	61.266036
2084.015261	85.376829	61.271041
2083.719730	77.421121	61.276046
2082.628213	86.136822	61.281050
2081.992614	81.178767	61.286055
2081.341205	80.666793	61.291060
2080.505207	79.299847	61.296065
2079.236686	68.974875	61.301070
2078.403708	81.909735	61.306074
2078.884312	76.253945	61.311079
2078.388965	81.054671	61.316084
2077.698729	90.407502	61.321089
2077.077266	80.168816	61.326094
2075.555580	88.244439	61.331098
2075.040280	72.203751	61.336103
2074.677334	81.080614	61.341108
2074.117388	74.558763	61.346113
2073.575411	77.570694	61.351118
2072.391848	78.329562	61.356122
2071.978878	77.676942	61.361127
2071.135648	84.254208	61.366132
2070.704459	79.067779	61.371137
2070.394790	81.232378	61.376142
2069.421966	93.516983	61.381146
2068.740455	79.174390	61.386151
2068.092906	83.730765	61.391156
2067.412026	86.089115	61.396161
2067.285319	76.102113	61.401166
2065.817135	82.248662	61.406170
2065.322705	77.372645	61.411175
2064.356792	88.696497	61.416180
2064.229153	78.343353	61.421185
2064.214104	69.998638	61.426190
2062.533025	82.292670	61.431194
2061.988709	74.649903	61.436199
2061.454711	77.281932	61.441204
2060.751615	80.632068	61.446209
2060.658271	71.668402	61.451214
2059.078394	86.998689	61.456218
2059.004463	79.952805	61.461223
2057.951834	87.763473	61.466228
2057.544244	77.388348	61.471233
2057.329710	70.876103	61.476238
2055.958993	78.820908	61.481242
2055.569346	75.589930	61.486247
2054.954709	76.086497	61.491252
2054.469250	77.736448	61.496257
2053.249074	77.971868	61.501262
2052.570796	73.391763	61.506266
2051.871908	73.410919	61.511271
2051.209985	75.468406	61.516276
2050.877008	75.515367	61.521281
2050.663509	81.693223	61.526286
2049.688216	78.361898	61.531290
2048.552383	75.999048	61.536295
2048.076798	74.533358	61.541300
2047.538050	79.889776	61.546305
2047.571198	76.880154	61.551310
2046.066932	76.326569	61.556314
2045.288048	81.994445	61.561319
2044.491409	85.830697	61.566324
2044.169168	75.861749	61.571329
2043.861021	67.124294	61.576334
2042.814211	84.458974	61.581338
2042.804512	74.729057	61.586343
2041.738033	78.568832	61.591348
2041.183744	75.929679	61.596353
2040.704073	82.221349	61.601358
2039.648887	81.270439	61.606362
2039.132778	78.588045	61.611367
2038.680639	76.763886	61.616372
2038.091465	76.807302	61.621377
2036.818759	76.901716	61.626382
2035.586960	81.563949	61.631386
2035.299170	75.029499	61.636391
2034.642877	80.704037	61.641396
2034.251263	73.315804	61.646401
2033.963095	82.492494	61.651406
2033.332466	86.039441	61.656410
2032.929896	80.846937	61.661415
2031.813461	82.838493	61.666420
2031.112748	84.282117	61.671425
2030.989739	82.651519	61.676430
2029.657034	93.997855	61.681434
2028.642110	82.970724	61.686439
2028.451056	77.033124	61.691444
2027.827410	80.952676	61.696449
2027.739807	81.286469	61.701454
2026.364967	88.438205	61.706458
2025.846786	80.936229	61.711463
2025.023687	81.119523	61.716468
2024.709292	89.586259	61.721473
2023.948230	80.604967	61.726478
2023.034112	81.355651	61.731482
2022.257612	81.287827	61.736487
2021.868260	79.901332	61.741492
2021.285425	85.718039	61.746497
2020.952209	76.655673	61.751502
2020.002220	77.388020	61.756506
2019.071079	76.523260	61.761511
2018.793363	72.811318	61.766516
2017.739750	80.833331	61.771521
2016.752756	78.332534	61.776526
2015.902897	79.544708	61.781530
2015.704701	79.834658	61.786535
2015.031317	80.509824	61.791540
2015.227479	77.030627	61.796545
2014.680374	68.642722	61.801550
2013.217171	70.209272	61.806554
2012.470396	76.882141	61.811559
2012.168175	75.431799	61.816564
2011.061823	78.276203	61.821569
2010.213499	75.825896	61.826574
2009.255133	78.648934	61.831578
2009.220984	79.422777	61.836583
2008.499462	77.155640	61.841588
2007.884200	75.838578	61.846593
2007.867829	78.973362	61.851598
2006.882866	85.127658	61.856602
2005.875732	66.288478	61.861607
2005.271591	80.101129	61.866612
2004.651962	83.069509	61.871617
2004.377413	72.082717	61.876622
2003.435047	73.289006	61.881626
2002.589765	74.697759	61.886631
2002.012061	74.529226	61.891636
2001.886741	81.042903	61.896641
2001.253032	72.584552	61.901646
1999.940674	81.016338	61.906650
1999.440089	76.667152	61.911655
1998.919880	82.062241	61.916660
1997.699681	86.194756	61.921665
1996.847611	73.730236	61.926670
1996.178746	81.095148	61.931674
1995.763141	78.295704	61.936679
1995.589269	81.497296	61.941684
1995.206840	79.011112	61.946689
1994.619514	74.762419	61.951694
1993.687794	82.005721	61.956698
1993.021245	81.023078	61.961703
1992.223115	79.684800	61.966708
1990.842404	79.210355	61.971713
1990.211094	79.555840	61.976718
1989.433698	79.029114	61.981722
1989.386774	77.314059	61.986727
1988.646715	85.769923	61.991732
1988.556144	81.887817	61.996737
1988.364027	81.750035	62.001742
1986.885544	84.606391	62.006746
1986.012618	85.286090	62.011751
1985.192767	76.361049	62.016756
1984.801402	82.915103	62.021761
1984.616929	77.594120	62.026766
1983.469676	80.102909	62.031770
1982.679436	73.587706	62.036775
1982.597933	73.207986	62.041780
1982.009801	79.869905	62.046785
1980.519561	76.015654	62.051790
1979.663100	89.744769	62.056794
1979.023658	77.624785	62.061799
1979.124743	73.459250	62.066804
1978.427372	79.199631	62.071809
1978.548258	81.365580	62.076814
1977.354052	86.371511	62.081818
1976.572219	69.828967	62.086823
1975.740272	77.917666	62.091828
1974.502901	88.796532	62.096833
1974.153177	82.460568	62.101838
1973.343428	85.255033	62.106842
1972.780565	78.110434	62.111847
1972.855397	79.084704	62.116852
1971.645228	86.484190	62.121857
1971.057015	83.772693	62.126862
1970.048163	87.411973	62.131866
1969.667216	79.684435	62.136871
1969.239675	77.742396	62.141876
1968.190515	76.038922	62.146881
1967.586173	72.779157	62.151886
1966.619557	75.405463	62.156890
1966.137465	75.777923	62.161895
1965.709786	76.565795	62.166900
1965.210862	83.836116	62.171905
1964.542882	74.089740	62.176910
1963.384971	88.158960	62.181914
1962.808878	81.605153	62.186919
1962.229636	87.593741	62.191924
1961.594846	86.965259	62.196929
1961.460909	75.180767	62.201934
1960.093270	75.390908	62.206938
1959.210895	74.959115	62.211943
1959.146977	76.107903	62.216948
1958.111482	80.809197	62.221953
1958.266424	66.146333	62.226958
1957.848336	81.314205	62.231962
1956.515408	74.281208	62.236967
1955.917393	80.909689	62.241972
1955.421559	91.790389	62.246977
1954.646615	85.986226	62.251982
1953.605784	93.227282	62.256986
1952.855786	78.684473	62.261991
1952.629909	76.111910	62.266996
1951.786945	83.092545	62.272001
1951.356579	74.812568	62.277006
1950.227038	92.379295	62.282010
1949.824902	81.461303	62.287015
1949.258401	77.914814	62.292020
1948.633339	86.480871	62.297025
1948.328161	79.795858	62.302030
1946.734437	85.326829	62.307034
1946.350120	84.762077	62.312039
1945.987476	77.733621	62.317044
1945.233262	80.789762	62.322049
1944.447859	77.304798	62.327054
1943.218358	88.867556	62.332058
1942.650819	78.024834	62.337063
1942.252883	73.228641	62.342068
1941.914106	76.813295	62.347073
1941.762381	76.871886	62.352078
1941.084106	77.795388	62.357082
1940.097746	75.067930	62.362087
1939.520966	76.379052	62.367092
1938.679087	78.246293	62.372097
1938.121715	78.554268	62.377102
1937.124293	83.266421	62.382106
1936.482452	78.443665	62.387111
1936.107189	77.458567	62.392116
1935.326297	74.640306	62.397121
1935.090057	72.388847	62.402126
1933.634553	69.582179	62.407130
1933.026971	62.500900	62.412135
1932.560034	66.538115	62.417140
1932.076723	65.332301	62.422145
1931.941113	65.700754	62.427150
1930.412677	77.123993	62.432154
1929.965490	72.037819	62.437159
1929.430161	73.936300	62.442164
1928.834744	69.315597	62.447169
1928.516866	76.057596	62.452174
1927.030699	75.577525	62.457178
1926.415688	71.452785	62.462183
1925.946012	71.291437	62.467188
1925.411042	73.836014	62.472193
1925.472816	67.385461	62.477198
1924.042052	78.090574	62.482202
1923.296306	73.666502	62.487207
1922.948179	67.686711	62.492212
1922.323972	76.060782	62.497217
1921.401421	65.705498	62.502222
1920.628833	75.636862	62.507226
1920.027823	76.095193	62.512231
1919.631179	77.422473	62.517236
1918.807526	76.036471	62.522241
1918.221245	73.439911	62.527246
1917.213808	77.955234	62.532250
1916.479191	71.312116	62.537255
1916.429536	68.223116	62.542260
1915.590279	84.758112	62.547265
1914.874543	79.487362	62.552270
1914.123059	82.155818	62.557274
1913.440976	76.502749	62.562279
1913.196724	70.539134	62.567284
1912.019124	77.585304	62.572289
1911.365137	76.048309	62.577294
1910.691939	88.737563	62.582298
1910.171073	74.468192	62.587303
1909.827270	72.124219	62.592308
1909.304508	83.784354	62.597313
1908.436992	77.340015	62.602318
1907.537980	83.071873	62.607322
1906.823617	75.969782	62.612327
1906.296702	77.231721	62.617332
1905.386799	79.622160	62.622337
1904.659233	76.117837	62.627342
1903.651489	80.358885	62.632346
1903.292309	83.336004	62.637351
1903.128599	76.122345	62.642356
1902.444553	74.395108	62.647361
1902.131543	68.327999	62.652366
1901.152284	74.322256	62.657370
1900.404660	75.107632	62.662375
1899.741151	71.558406	62.667380
1898.979650	82.417839	62.672385
1898.015362	69.191398	62.677390
1896.890908	76.742404	62.682394
1896.587061	78.038417	62.687399
1896.678370	72.078184	62.692404
1896.243477	78.253253	62.697409
1895.851151	66.240229	62.702414
1894.085032	75.310551	62.707418
1893.814654	70.469255	62.712423
1893.330125	71.826571	62.717428
1892.285855	73.146229	62.722433
1891.349652	68.050565	62.727438
1890.654150	70.804573	62.732442
1890.290308	68.629418	62.737447
1890.004037	62.277883	62.742452
1889.313509	69.189808	62.747457
1888.411888	58.428343	62.752462
1887.412112	69.048674	62.757466
1886.518679	66.843730	62.762471
1886.383885	64.571368	62.767476
1885.748156	64.987091	62.772481
1885.349180	64.499060	62.777486
1884.876831	65.915474	62.782490
1883.972532	65.998213	62.787495
1883.181361	62.462937	62.792500
1882.844665	73.449024	62.797505
1881.773573	70.447929	62.802510
1880.709358	68.964542	62.807514
1880.102934	68.520290	62.812519
1880.046322	61.388577	62.817524
1879.196083	80.086143	62.822529
1878.906263	68.584509	62.827534
1877.660077	78.334409	62.832538
1876.930943	68.313136	62.837543
1877.092668	62.888733	62.842548
1876.313687	76.675237	62.847553
1875.161220	73.167035	62.852558
1874.157261	74.460063	62.857562
1873.760915	66.910832	62.862567
1873.114623	69.971014	62.867572
1872.523178	71.009137	62.872577
1872.240228	56.311475	62.877582
1871.205561	69.300173	62.882586
1870.633697	72.541825	62.887591
1870.125890	64.253802	62.892596
1869.356723	78.540318	62.897601
1868.254497	66.987022	62.902606
1867.701590	72.980182	62.907610
1866.945895	63.835790	62.912615
1866.974173	59.868630	62.917620
1865.934219	76.788463	62.922625
1866.116679	64.234632	62.927630
1865.010111	70.732230	62.932634
1864.351694	69.647166	62.937639
1863.303773	65.340326	62.942644
1862.560508	69.252721	62.947649
1861.808337	61.797130	62.952654
1861.325628	75.159148	62.957658
1860.905632	73.482265	62.962663
1859.950262	61.843460	62.967668
1858.403824	75.228388	62.972673
1858.262678	62.150473	62.977678
1857.537201	66.798345	62.982682
1856.833588	70.306475	62.987687
1856.989883	67.342105	62.992692
1856.136349	78.331750	62.997697
1856.434097	72.187392	63.002702
1855.115357	76.780060	63.007706
1853.896038	74.850733	63.012711
1853.743759	71.530618	63.017716
1852.544789	77.315770	63.022721
1851.743059	71.140444	63.027726
1850.932467	75.406187	63.032730
1850.361651	77.599287	63.037735
1850.356329	76.828394	63.042740
1849.521112	81.459127	63.047745
1849.264771	67.982512	63.052750
1848.093031	70.316311	63.057754
1847.443821	70.653034	63.062759
1846.992777	71.795028	63.067764
1846.434619	70.675840	63.072769
1845.466151	69.695926	63.077774
1844.861815	72.891427	63.082778
1844.317735	67.028851	63.087783
1843.792925	65.894486	63.092788
1842.804405	67.338029	63.097793
1841.947212	74.104402	63.102798
1841.125047	72.843680	63.107802
1840.887634	67.173365	63.112807
1840.627326	60.129792	63.117812
1839.295880	72.499430	63.122817
1838.720058	66.281117	63.127822
1838.356040	66.708779	63.132826
1837.657273	70.745401	63.137831
1837.506796	73.085262	63.142836
1835.829205	69.899401	63.147841
1835.540928	65.139329	63.152846
1834.639013	70.178559	63.157850
1834.087776	68.980035	63.162855
1834.134000	68.662540	63.167860
1832.891213	79.616550	63.172865
1832.305140	68.422967	63.177870
1831.396488	73.384801	63.182874
1830.903107	69.154798	63.187879
1830.827579	69.645206	63.192884
1829.580338	69.511506	63.197889
1828.777442	66.628744	63.202894
1828.067080	68.438368	63.207898
1827.638578	65.653782	63.212903
1827.347109	55.723039	63.217908
1826.242924	67.285274	63.222913
1825.577182	62.750040	63.227918
1824.822583	72.782533	63.232922
1824.077477	68.517443	63.237927
1823.894929	68.286850	63.242932
1823.197894	78.836450	63.247937
1822.329060	74.229385	63.252942
1821.557255	72.714929	63.257946
1820.772625	73.902946	63.262951
1820.744932	67.451916	63.267956
1820.123315	74.918876	63.272961
1819.103345	71.046192	63.277966
1818.033621	75.137204	63.282970
1817.573497	77.450309	63.287975
1817.586873	76.890551	63.292980
1816.411429	80.569802	63.297985
1815.597232	77.875676	63.302990
1815.116012	75.415096	63.307994
1814.652755	78.160166	63.312999
1814.027395	65.095629	63.318004
1813.007073	73.852854	63.323009
1812.187900	69.343476	63.328014
1811.563986	70.915690	63.333018
1811.147323	72.241665	63.338023
1810.802019	71.560517	63.343028
1809.908952	74.653454	63.348033
1809.213297	67.830806	63.353038
1808.564150	74.421857	63.358042
1808.241550	73.061065	63.363047
1807.676682	75.292622	63.368052
1806.383079	77.365054	63.373057
1805.633545	77.456063	63.378062
1805.315607	72.152012	63.383066
1804.708938	73.299321	63.388071
1803.746868	71.805973	63.393076
1802.551688	77.830870	63.398081
1802.153397	67.237903	63.403086
1801.822775	76.107251	63.408090
1801.112974	72.372154	63.413095
1801.246257	73.727191	63.418100
1800.004512	75.995612	63.423105
1798.973884	63.458688	63.428110
1798.511785	69.602884	63.433114
1798.319056	71.293556	63.438119
1797.647200	77.790208	63.443124
1796.470230	80.051101	63.448129
1795.988909	65.450542	63.453134
1795.160155	67.567781	63.458138
1794.475439	68.869358	63.463143
1794.401430	64.898780	63.468148
1792.934501	66.392606	63.473153
1792.871488	61.565580	63.478158
1792.365602	67.303996	63.483162
1791.541573	61.033822	63.488167
1790.402072	68.219929	63.493172
1789.324489	69.432415	63.498177
1789.137389	66.772708	63.503182
1788.842294	70.756057	63.508186
1788.263743	63.250646	63.513191
1787.693762	57.921044	63.518196
1786.364420	70.178225	63.523201
1785.808419	66.834431	63.528206
1785.326524	58.278715	63.533210
1784.818338	62.278390	63.538215
1784.647494	63.327450	63.543220
1783.124064	68.095276	63.548225
1782.854431	61.037912	63.553230
1781.938837	68.313600	63.558234
1781.505745	70.907858	63.563239
1780.834499	62.425984	63.568244
1779.834695	61.669329	63.573249
1779.231851	66.886332	63.578254
1778.623704	71.815309	63.583258
1778.503934	70.621518	63.588263
1778.165009	66.268785	63.593268
1776.777218	66.914244	63.598273
1775.810230	65.857514	63.603278
1775.467497	70.839366	63.608282
1774.881814	73.840242	63.613287
1774.124492	70.403795	63.618292
1773.026796	74.993394	63.623297
1772.831912	68.390192	63.628302
1772.315439	70.770569	63.633306
1771.871623	70.045098	63.638311
1770.988944	66.047100	63.643316
1769.846687	71.295610	63.648321
1769.373562	64.428582	63.653326
1768.784825	65.094031	63.658330
1768.303114	68.775377	63.663335
1767.700888	64.260863	63.668340
1766.839300	73.195792	63.673345
1766.122494	68.153011	63.678350
1765.957380	69.840537	63.683354
1765.098889	67.305968	63.688359
1764.035893	68.745295	63.693364
1763.456680	69.959749	63.698369
1763.050187	73.133642	63.703374
1762.615963	73.629767	63.708378
1761.644040	85.051369	63.713383
1760.895410	77.458219	63.718388
1759.895023	84.980914	63.723393
1759.380896	71.737887	63.728398
1759.244696	74.605414	63.733402
1758.530168	74.963981	63.738407
1757.656951	69.940857	63.743412
1756.535838	72.655205	63.748417
1756.613160	67.581547	63.753422
1755.927896	75.424909	63.758426
1755.118197	72.823969	63.763431
1754.720242	76.871101	63.768436
1753.933129	75.093234	63.773441
1753.262385	70.407294	63.778446
1751.377893	76.720264	63.783450
1751.129675	81.859624	63.788455
1751.018662	74.133698	63.793460
1750.040593	83.886293	63.798465
1749.894339	76.295865	63.803470
1749.246961	77.124501	63.808474
1748.552128	76.230806	63.813479
1747.968116	76.909659	63.818484
1746.760227	78.850208	63.823489
1746.527478	76.642768	63.828494
1745.937675	68.446555	63.833498
1745.446285	77.789442	63.838503
1744.472569	74.202137	63.843508
1743.835651	75.091350	63.848513
1742.988910	71.113259	63.853518
1742.884508	70.592204	63.858522
1741.694942	73.673121	63.863527
1740.788557	71.786986	63.868532
1740.119520	80.062950	63.873537
1739.870855	74.385490	63.878542
1739.448170	72.349096	63.883546
1738.411611	65.795574	63.888551
1737.828884	62.797003	63.893556
1736.559583	68.627756	63.898561
1736.536603	81.321005	63.903566
1736.357880	71.383607	63.908570
1735.338963	74.250598	63.913575
1734.789537	72.004979	63.918580
1733.777651	71.990499	63.923585
1733.436830	72.977464	63.928590
1732.678036	69.442596	63.933594
1731.251476	81.220264	63.938599
1730.868343	74.602698	63.943604
1730.422874	78.754668	63.948609
1730.086991	75.947139	63.953614
1729.554907	66.117178	63.958618
1728.580949	73.125766	63.963623
1727.826984	75.112592	63.968628
1726.955633	78.793904	63.973633
1726.560300	73.906508	63.978638
1726.234697	73.836574	63.983642
1725.495417	77.063070	63.988647
1724.501015	76.129062	63.993652
1723.854587	77.066086	63.998657
1723.765978	76.633115	64.003662
1722.754212	75.616819	64.008666
1721.486876	75.351590	64.013671
1721.131985	66.823490	64.018676
1720.272542	86.570611	64.023681
1719.660799	73.401529	64.028686
1719.598669	71.718293	64.033690
1718.996695	76.599248	64.038695
1718.672513	65.407460	64.043700
1717.277198	74.228069	64.048705
1716.968879	75.225657	64.053710
1716.423991	72.310214	64.058714
1715.149694	74.758295	64.063719
1714.764608	76.403727	64.068724
1714.076701	86.746123	64.073729
1713.587981	83.099521	64.078734
1712.583938	77.619206	64.083738
1711.313830	80.265509	64.088743
1711.241409	76.544519	64.093748
1710.642193	77.690562	64.098753
1710.495434	73.762828	64.103758
1710.245223	75.134930	64.108762
1708.690906	80.898809	64.113767
1708.364256	74.868397	64.118772
1707.606999	80.956924	64.123777
1706.581110	81.979010	64.128782
1705.883523	78.733264	64.133786
1704.917389	81.003097	64.138791
1704.675354	67.453015	64.143796
1704.281445	77.186572	64.148801
1703.764727	75.197059	64.153806
1702.951797	79.068895	64.158810
1702.032697	77.968854	64.163815
1701.552752	72.165981	64.168820
1700.727324	70.264028	64.173825
1700.393437	76.694566	64.178830
1699.370912	72.014752	64.183834
1698.442161	81.646416	64.188839
1698.207643	71.626996	64.193844
1697.641563	77.229277	64.198849
1697.024614	68.447614	64.203854
1696.619819	64.662716	64.208858
1695.697292	73.872145	64.213863
1694.992986	71.497118	64.218868
1694.564366	76.408014	64.223873
1693.855747	68.958821	64.228878
1692.518747	76.863577	64.233882
1691.734406	70.316642	64.238887
1691.582914	75.743777	64.243892
1691.056014	78.590136	64.248897
1690.751204	78.054824	64.253902
1689.469986	77.904868	64.258906
1688.815212	74.019065	64.263911
1688.523671	66.877832	64.268916
1687.872482	68.835234	64.273921
1686.495564	70.632620	64.278926
1686.245109	78.260671	64.283930
1685.326759	72.938193	64.288935
1684.993899	67.249887	64.293940
1684.356635	68.347182	64.298945
1683.773541	69.211797	64.303950
1682.763724	66.018695	64.308954
1681.948674	76.089959	64.313959
1681.657649	63.214159	64.318964
1681.320917	69.502688	64.323969
1680.989523	72.894251	64.328974
1679.774719	67.129105	64.333978
1678.647080	69.820112	64.338983
1678.364710	61.671963	64.343988
1677.706444	68.468253	64.348993
1677.237356	70.405944	64.353998
1676.439819	70.602680	64.359002
1675.387833	68.225575	64.364007
1675.454776	67.739936	64.369012
1674.576692	68.989357	64.374017
1673.721508	63.761467	64.379022
1672.927359	71.732010	64.384026
1672.042077	65.202750	64.389031
1671.684666	61.931171	64.394036
1671.273718	66.967324	64.399041
1670.775465	72.423795	64.404046
1669.581023	73.715509	64.409050
1668.735160	76.615659	64.414055
1668.309368	65.376533	64.419060
1667.784302	68.311784	64.424065
1667.756916	67.029166	64.429070
1667.095127	65.566960	64.434074
1665.675727	62.915638	64.439079
1665.513042	61.804981	64.444084
1664.437924	75.951617	64.449089
1663.516781	62.161323	64.454094
1662.966744	63.508156	64.459098
1662.234384	66.971093	64.464103
1662.095175	66.930055	64.469108
1662.030122	72.473443	64.474113
1660.564711	69.052004	64.479118
1659.640882	69.841907	64.484122
1658.850606	71.712986	64.489127
1658.933729	60.496513	64.494132
1658.263365	66.137163	64.499137
1657.046206	71.052734	64.504142
1656.317904	66.585074	64.509146
1655.604728	71.535188	64.514151
1655.036582	65.036134	64.519156
1654.633488	70.747888	64.524161
1654.103828	72.037949	64.529166
1653.351565	68.814990	64.534170
1652.369682	65.977493	64.539175
1652.128572	72.581225	64.544180
1651.492849	74.199684	64.549185
1650.928507	72.395951	64.554190
1650.205676	67.206992	64.559194
1649.030219	73.739698	64.564199
1648.642546	71.859157	64.569204
1648.259747	71.560605	64.574209
1647.371364	67.162969	64.579214
1646.880560	70.819431	64.584218
1646.099567	73.649275	64.589223
1645.492961	69.630901	64.594228
1644.165468	65.314722	64.599233
1643.519630	65.661550	64.604238
1643.239087	65.208138	64.609242
1642.425300	75.706668	64.614247
1642.377801	56.319765	64.619252
1641.472409	75.554491	64.624257
1641.082092	63.084489	64.629262
1640.324008	67.205090	64.634266
1639.622695	74.225056	64.639271
1639.126769	59.199956	64.644276
1637.605187	72.566451	64.649281
1636.650627	73.083735	64.654286
1636.541229	69.338684	64.659290
1635.866451	76.116885	64.664295
1635.716865	66.203333	64.669300
1635.568612	71.395448	64.674305
1634.314801	69.350901	64.679310
1633.431914	66.643303	64.684314
1632.720559	71.046817	64.689319
1632.087846	66.286895	64.694324
1631.824422	71.362146	64.699329
1630.681332	75.027999	64.704334
1630.074491	70.090367	64.709338
1629.104426	70.838058	64.714343
1629.102621	73.167083	64.719348
1628.501188	71.794023	64.724353
1627.074911	67.169899	64.729358
1626.652041	62.857206	64.734362
1625.821362	72.569583	64.739367
1625.548209	69.118201	64.744372
1624.928535	75.451203	64.749377
1624.585723	71.398348	64.754382
1623.919229	58.664575	64.759386
1623.231215	66.606695	64.764391
1622.832980	67.705328	64.769396
1621.312098	58.003553	64.774401
1620.305341	63.735715	64.779406
1620.002787	60.543566	64.784410
1619.205829	67.909094	64.789415
1618.800910	57.686366	64.794420
1618.655841	67.461011	64.799425
1617.807433	68.634312	64.804430
1617.172268	60.520494	64.809434
1616.034102	69.745514	64.814439
1615.803721	62.504225	64.819444
1615.125543	65.299504	64.824449
1614.018307	66.767350	64.829454
1613.288810	75.796524	64.834458
1612.840689	73.569898	64.839463
1612.738516	64.714768	64.844468
1612.124039	75.454311	64.849473
1610.682456	74.375807	64.854478
1610.536671	65.611425	64.859482
1609.941904	67.394188	64.864487
1609.451281	68.361007	64.869492
1608.353625	73.506389	64.874497
1607.406763	71.806015	64.879502
1607.203347	72.150159	64.884506
1606.590470	75.506213	64.889511
1605.862134	63.568909	64.894516
1604.484781	76.509302	64.899521
1603.947063	66.220090	64.904526
1603.787413	70.425778	64.909530
1603.263791	70.793141	64.914535
1602.596812	61.666000	64.919540
1602.425437	73.977665	64.924545
1601.376409	65.761784	64.929550
1600.803725	67.300780	64.934554
1599.694142	67.336596	64.939559
1598.942476	61.646555	64.944564
1598.203822	73.040475	64.949569
1597.380592	64.663198	64.954574
1597.483369	65.116383	64.959578
1596.831594	67.407038	64.964583
1595.850981	66.595033	64.969588
1594.710541	69.328112	64.974593
1593.931765	67.185311	64.979598
1593.889233	62.976079	64.984602
1593.510247	68.417667	64.989607
1592.990234	68.144969	64.994612
1591.715651	61.402496	64.999617
1590.870985	66.965615	65.004622
1590.721515	63.868844	65.009626
1589.771954	69.916868	65.014631
1589.767464	69.925800	65.019636
1588.782425	71.494708	65.024641
1587.926330	67.535223	65.029646
1587.379577	64.409339	65.034650
1586.066582	63.559484	65.039655
1585.508916	57.859142	65.044660
1584.788758	66.180167	65.049665
1584.014380	71.376803	65.054670
1583.971582	68.764648	65.059674
1583.520597	65.596324	65.064679
1583.429112	60.477356	65.069684
1582.523035	60.501243	65.074689
1581.300828	70.912964	65.079694
1580.969876	64.386357	65.084698
1579.755181	67.701726	65.089703
1579.084548	64.544545	65.094708
1578.418108	64.889380	65.099713
1577.727506	69.699460	65.104718
1577.522077	64.563676	65.109722
1576.855740	65.407023	65.114727
1576.327250	60.184429	65.119732
1575.528908	62.865677	65.124737
1574.474481	61.891448	65.129742
1574.296928	59.356827	65.134746
1573.108453	75.715923	65.139751
1572.456230	62.234095	65.144756
1571.899207	71.013104	65.149761
1571.382743	63.477374	65.154766
1571.286436	60.223882	65.159770
1570.319164	60.527047	65.164775
1569.214086	58.183920	65.169780
1568.875962	64.898586	65.174785
1568.383491	61.948933	65.179790
1567.120106	54.576163	65.184794
1566.370031	61.523556	65.189799
1565.451255	58.218196	65.194804
1564.942218	69.047843	65.199809
1564.491366	69.987729	65.204814
1564.215632	58.200737	65.209818
1563.793066	66.968970	65.214823
1563.402926	54.746449	65.219828
1562.341924	52.708004	65.224833
1561.332897	58.620158	65.229838
1561.037532	55.804925	65.234842
1560.260958	61.936235	65.239847
1559.545442	63.886501	65.244852
1558.937186	61.740181	65.249857
1558.653713	65.185515	65.254862
1557.485962	59.872203	65.259866
1556.128604	65.164662	65.264871
1555.733398	55.837875	65.269876
1555.175509	59.961325	65.274881
1554.774599	67.913916	65.279886
1554.813282	55.800369	65.284890
1554.118088	66.339387	65.289895
1553.611542	63.582004	65.294900
1552.394291	64.452534	65.299905
1551.473833	65.409634	65.304910
1551.010131	69.379606	65.309914
1549.592113	68.919954	65.314919
1549.109121	58.930458	65.319924
1548.631251	53.581581	65.324929
1548.479104	62.706144	65.329934
1548.190802	63.617424	65.334938
1546.888986	59.937115	65.339943
1546.014747	64.929011	65.344948
1545.256750	63.857086	65.349953
1544.994066	56.495817	65.354958
1544.823083	56.534426	65.359962
1543.955477	63.635745	65.364967
1543.060957	60.985418	65.369972
1542.165496	74.504104	65.374977
1541.808736	69.427378	65.379982
1541.032216	55.178979	65.384986
1539.838394	66.399752	65.389991
1539.687146	59.461495	65.394996
1538.906648	65.073241	65.400001
1538.405619	55.140912	65.405006
1538.140182	53.564711	65.410010
1536.581622	58.865161	65.415015
1536.087590	53.446819	65.420020
1535.567082	58.529353	65.425025
1535.177883	58.610440	65.430030
1534.903096	61.471288	65.435034
1534.017150	69.776483	65.440039
1533.208513	65.371935	65.445044
1532.473578	62.277475	65.450049
1531.657908	63.421898	65.455054
1530.675958	57.432221	65.460058
1529.704277	59.901178	65.465063
1529.695726	61.665327	65.470068
1529.034531	61.310619	65.475073
1529.034734	66.193125	65.480078
1528.725671	55.165757	65.485082
1527.379269	71.446094	65.490087
1526.529096	56.853872	65.495092
1525.674294	51.395439	65.500097
1525.026200	59.778732	65.505102
1524.221863	50.305668	65.510106
1523.262523	57.788590	65.515111
1522.945320	53.157448	65.520116
1522.695362	56.602571	65.525121
1522.222277	57.002738	65.530126
1521.723836	52.131838	65.535130
1520.241978	65.338000	65.540135
1519.797589	50.067684	65.545140
1519.282862	57.573192	65.550145
1518.629073	61.713847	65.555150
1517.589067	53.166470	65.560154
1516.620201	61.267968	65.565159
1516.156457	55.847603	65.570164
1515.749607	65.909398	65.575169
1515.321324	64.094239	65.580174
1515.087124	57.849098	65.585178
1514.165260	63.042165	65.590183
1513.409908	64.992545	65.595188
1512.754879	61.544956	65.600193
1512.182894	69.070927	65.605198
1510.933670	62.278746	65.610202
1510.068779	61.269330	65.615207
1509.861983	52.166479	65.620212
1509.394722	60.313966	65.625217
1508.880009	75.445437	65.630222
1508.260862	64.217333	65.635226
1507.152094	75.183176	65.640231
1506.950968	70.510455	65.645236
1506.307841	70.110028	65.650241
1505.597566	74.151807	65.655246
1504.816559	60.343504	65.660250
1503.759253	74.414076	65.665255
1503.603736	60.459250	65.670260
1503.093971	64.818404	65.675265
1502.076919	70.234993	65.680270
1501.553824	65.942232	65.685274
1500.865858	72.348898	65.690279
1499.962230	66.363583	65.695284
1499.128232	70.017214	65.700289
1498.126554	69.776438	65.705294
1497.585080	59.360008	65.710298
1496.947266	73.084455	65.715303
1496.523879	67.518635	65.720308
1496.026551	64.483379	65.725313
1495.872656	76.623498	65.730318
1495.322862	60.048122	65.735322
1494.103293	63.572357	65.740327
1493.382203	59.032446	65.745332
1492.917738	66.344628	65.750337
1491.997296	59.210014	65.755342
1490.914937	54.511683	65.760346
1490.453854	63.479522	65.765351
1490.374925	65.890423	65.770356
1489.841017	64.675949	65.775361
1489.104335	67.341129	65.780366
1488.643217	56.222561	65.785370
1487.344090	63.433659	65.790375
1487.195221	59.606170	65.795380
1486.318223	52.041381	65.800385
1485.117516	59.116034	65.805390
1484.513088	64.123729	65.810394
1483.891474	70.721135	65.815399
1483.362810	61.277074	65.820404
1483.288929	61.622340	65.825409
1482.655930	70.141998	65.830414
1481.848382	62.933591	65.835418
1481.070948	70.144216	65.840423
1480.191302	67.998173	65.845428
1478.869298	66.897269	65.850433
1478.303676	62.973353	65.855438
1478.532250	58.902061	65.860442
1477.469575	60.594006	65.865447
1477.108794	54.346458	65.870452
1476.732637	60.725016	65.875457
1475.590253	57.130331	65.880462
1474.814182	60.238021	65.885466
1474.047319	67.597619	65.890471
1473.630158	59.144956	65.895476
1473.303530	59.730050	65.900481
1472.316439	57.666344	65.905486
1471.384459	56.499874	65.910490
1470.772987	64.441529	65.915495
1470.372289	58.110422	65.920500
1470.050315	56.675738	65.925505
1468.915190	63.369320	65.930510
1468.305722	62.294880	65.935514
1467.382532	67.146750	65.940519
1467.155160	63.764124	65.945524
1466.791201	59.942661	65.950529
1465.764100	71.063072	65.955534
1465.078404	59.676643	65.960538
1464.115313	68.322268	65.965543
1463.685911	66.265737	65.970548
1463.667854	66.791704	65.975553
1462.235473	64.739874	65.980558
1461.595452	57.884098	65.985562
1460.883038	60.395529	65.990567
1460.370437	61.472696	65.995572
1460.292316	70.293680	66.000577
1459.155735	67.382840	66.005582
1459.041733	64.220404	66.010586
1457.870350	73.078911	66.015591
1456.898498	73.287359	66.020596
1456.056443	67.839779	66.025601
1455.526469	70.064998	66.030606
1455.287841	71.372761	66.035610
1454.820474	75.975310	66.040615
1453.919915	66.874759	66.045620
1452.740815	66.555418	66.050625
1451.645654	73.638858	66.055630
1451.104258	70.959291	66.060634
1450.788256	64.239100	66.065639
1450.516638	65.352781	66.070644
1450.122576	66.020074	66.075649
1449.836416	67.665167	66.080654
1449.178285	62.978704	66.085658
1447.825674	65.504190	66.090663
1447.826800	57.702667	66.095668
1446.843217	68.747343	66.100673
1445.796829	68.854083	66.105678
1445.330791	67.606287	66.110682
1444.347071	71.959730	66.115687
1443.681898	68.355605	66.120692
1442.607632	66.595364	66.125697
1442.023408	72.285626	66.130702
1441.944664	70.100793	66.135706
1440.932639	74.180806	66.140711
1440.635602	69.877385	66.145716
1440.540979	69.844905	66.150721
1439.647462	74.225145	66.155726
1438.569798	68.249107	66.160730
1437.833016	69.592795	66.165735
1437.128288	69.573561	66.170740
1437.271088	71.031554	66.175745
1436.045890	83.719363	66.180750
1435.462225	67.355047	66.185754
1434.475389	66.263495	66.190759
1434.175963	73.381257	66.195764
1433.164490	67.935049	66.200769
1431.750529	70.850760	66.205774
1431.755593	57.810656	66.210778
1431.304770	69.527135	66.215783
1430.784425	65.762836	66.220788
1430.606462	63.911550	66.225793
1429.636561	74.694955	66.230798
1429.034725	63.285101	66.235802
1427.962465	63.515477	66.240807
1427.425031	61.797164	66.245812
1426.998980	58.022254	66.250817
1425.989358	66.008772	66.255822
1425.460965	62.782668	66.260826
1424.723860	65.743571	66.265831
1424.184741	65.322589	66.270836
1423.515091	66.046133	66.275841
1422.279655	70.323064	66.280846
1421.899584	66.240691	66.285850
1421.110237	74.498180	66.290855
1420.915305	70.296095	66.295860
1420.603100	70.972667	66.300865
1419.598810	71.559289	66.305870
1418.742191	64.618230	66.310874
1417.852568	67.897726	66.315879
1417.592890	68.722011	66.320884
1417.172418	68.146912	66.325889
1415.712474	80.152961	66.330894
1415.212829	68.064067	66.335898
1414.500955	67.144524	66.340903
1414.238521	67.533906	66.345908
1414.087048	63.325964	66.350913
1412.971031	67.526800	66.355918
1412.161926	61.510331	66.360922
1411.423114	69.277217	66.365927
1410.929843	64.309134	66.370932
1410.683137	60.719438	66.375937
1409.205761	67.574239	66.380942
1408.818483	54.465514	66.385946
1408.138966	63.973611	66.390951
1407.769000	69.168933	66.395956
1407.335552	62.210706	66.400961
1406.170047	63.207406	66.405966
1405.721011	61.016092	66.410970
1405.197411	63.746251	66.415975
1404.388840	63.225347	66.420980
1403.217999	64.348482	66.425985
1402.481877	67.851562	66.430990
1402.503631	53.865233	66.435994
1401.914915	66.374221	66.440999
1401.399817	55.613448	66.446004
1400.191586	61.487883	66.451009
1399.486934	68.429884	66.456014
1399.024273	61.094177	66.461018
1398.694363	67.578895	66.466023
1397.667383	69.490920	66.471028
1396.600596	65.842658	66.476033
1396.116837	64.167659	66.481038
1395.541205	65.110759	66.486042
1394.714163	73.019456	66.491047
1394.414183	67.541074	66.496052
1394.184671	62.054975	66.501057
1392.960275	77.107004	66.506062
1392.638743	65.185384	66.511066
1391.909515	71.012963	66.516071
1391.357456	58.682408	66.521076
1390.163627	62.840911	66.526081
1389.443554	65.579440	66.531086
1389.116881	64.200037	66.536090
1388.619606	73.354857	66.541095
1387.928241	66.645242	66.546100
1386.804502	61.372206	66.551105
1385.753942	64.005471	66.556110
1385.557801	59.980037	66.561114
1385.000506	65.675164	66.566119
1384.779560	65.113281	66.571124
1384.471806	67.346650	66.576129
1383.112987	65.160679	66.581134
1382.439249	65.046942	66.586138
1381.897108	69.049294	66.591143
1381.351867	61.095389	66.596148
1380.413494	71.406842	66.601153
1379.599914	67.509199	66.606158
1379.322254	65.757872	66.611162
1378.729653	72.488864	66.616167
1378.193960	71.880599	66.621172
1377.085720	73.561812	66.626177
1376.186235	72.390586	66.631182
1375.944885	66.686655	66.636186
1375.542126	77.526531	66.641191
1374.548077	70.774392	66.646196
1373.727777	65.162458	66.651201
1373.033159	72.521540	66.656206
1372.589240	71.109315	66.661210
1372.079871	74.398331	66.666215
1371.274392	67.378270	66.671220
1370.400812	68.656965	66.676225
1369.396852	68.072017	66.681230
1369.092228	76.811775	66.686234
1368.994254	70.117427	66.691239
1368.310355	70.133714	66.696244
1367.370787	67.232198	66.701249
1366.365277	71.259003	66.706254
1366.185924	62.413956	66.711258
1365.567789	69.264575	66.716263
1364.510960	68.918404	66.721268
1363.844309	67.163404	66.726273
1362.972985	73.465287	66.731278
1363.016411	62.065386	66.736282
1362.485403	63.380570	66.741287
1361.194887	70.358126	66.746292
1360.407196	62.166660	66.751297
1359.737658	75.555105	66.756302
1359.045113	62.774546	66.761306
1358.715088	72.182169	66.766311
1358.339596	66.787767	66.771316
1358.094354	68.649664	66.776321
1356.616778	72.154544	66.781326
1356.214675	67.950824	66.786330
1355.377815	69.611639	66.791335
1354.342610	74.535197	66.796340
1353.909059	67.402529	66.801345
1353.465369	65.876589	66.806350
1353.025516	60.351109	66.811354
1352.068176	67.561750	66.816359
1351.394197	67.945403	66.821364
1351.023126	66.843195	66.826369
1350.121648	66.364650	66.831374
1349.487023	64.955074	66.836378
1349.267175	68.762529	66.841383
1348.472420	66.513959	66.846388
1347.712446	58.022110	66.851393
1346.710278	72.390735	66.856398
1345.452184	62.933413	66.861402
1344.835640	62.337018	66.866407
1344.955661	70.780277	66.871412
1344.389696	67.984147	66.876417
1343.494161	68.269548	66.881422
1343.388674	62.999843	66.886426
1342.087689	67.517736	66.891431
1341.213753	69.003329	66.896436
1340.858454	61.654385	66.901441
1340.237212	69.289051	66.906446
1340.050524	64.078639	66.911450
1339.199321	64.519076	66.916455
1338.305020	70.310972	66.921460
1337.289245	65.416948	66.926465
1336.729095	55.781740	66.931470
1336.587624	58.632402	66.936474
1335.484397	65.258969	66.941479
1334.903970	62.365453	66.946484
1334.084752	58.408395	66.951489
1333.410795	60.755765	66.956494
1333.017743	62.007469	66.961498
1332.195670	73.114505	66.966503
1331.580766	69.778886	66.971508
1331.262104	63.839129	66.976513
1330.569326	64.801105	66.981518
1329.858844	64.974308	66.986522
1328.711477	65.968710	66.991527
1328.192008	61.946131	66.996532
1328.221374	63.390776	67.001537
1327.093847	66.875606	67.006542
1326.040303	72.050190	67.011546
1325.462047	70.267827	67.016551
1325.037106	64.909920	67.021556
1324.916976	71.643715	67.026561
1323.713131	70.125540	67.031566
1322.681799	62.559183	67.036570
1321.842400	65.194599	67.041575
1321.209863	66.576507	67.046580
1320.733868	56.061281	67.051585
1320.469754	66.637821	67.056590
1320.243976	56.301200	67.061594
1319.546087	61.806459	67.066599
1318.420601	64.900565	67.071604
1318.169824	54.951890	67.076609
1316.753565	57.656451	67.081614
1316.091078	58.323126	67.086618
1315.504423	56.695355	67.091623
1314.567103	60.839565	67.096628
1314.318002	60.413552	67.101633
1314.100013	60.985585	67.106638
1313.739498	57.024215	67.111642
1312.609455	61.029715	67.116647
1311.745505	63.563946	67.121652
1311.515085	58.664562	67.126657
1310.641460	61.795683	67.131662
1309.732365	50.706478	67.136666
1308.748197	55.248688	67.141671
1308.274855	66.120372	67.146676
1307.987274	57.010062	67.151681
1307.443735	65.480462	67.156686
1306.669530	57.164735	67.161690
1305.809109	65.883188	67.166695
1304.899019	61.055156	67.171700
1304.864798	52.129229	67.176705
1304.059192	65.244525	67.181710
1302.908895	52.904307	67.186714
1302.384438	57.479526	67.191719
1301.408949	55.864639	67.196724
1301.131702	54.535201	67.201729
1300.644107	65.183547	67.206734
1300.599014	53.262786	67.211738
1299.475378	58.245695	67.216743
1298.756527	66.244027	67.221748
1298.528763	63.513949	67.226753
1297.073019	69.598136	67.231758
1296.342975	58.209871	67.236762
1295.655589	64.507111	67.241767
1295.332016	67.675513	67.246772
1295.185903	67.893022	67.251777
1293.851256	77.938787	67.256782
1293.761316	59.679037	67.261786
1293.018993	64.094591	67.266791
1292.102800	66.313706	67.271796
1291.558273	56.439003	67.276801
1290.733761	70.877474	67.281806
1290.172702	61.630436	67.286810
1288.842431	71.832547	67.291815
1287.660534	61.849069	67.296820
1288.175642	60.606214	67.301825
1287.654999	68.252869	67.306830
1286.612032	66.170348	67.311834
1286.312220	66.696787	67.316839
1285.467276	69.602355	67.321844
1284.437115	65.872460	67.326849
1283.098234	74.149432	67.331854
1282.729576	67.746945	67.336858
1282.752337	69.312320	67.341863
1282.409889	65.522324	67.346868
1281.917085	58.582964	67.351873
1281.381018	66.933276	67.356878
1280.397549	65.367914	67.361882
1279.630946	60.058637	67.366887
1278.873630	64.744772	67.371892
1277.962812	55.663006	67.376897
1276.836359	60.288393	67.381902
1276.444615	52.246264	67.386906
1276.053632	55.285291	67.391911
1275.335222	56.747821	67.396916
1275.342010	52.123213	67.401921
1274.450730	67.957779	67.406926
1273.519793	57.429660	67.411930
1273.096778	56.231358	67.416935
1272.538314	67.076958	67.421940
1271.377584	64.842899	67.426945
1270.374483	63.157748	67.431950
1270.259325	58.098117	67.436954
1269.791900	57.939207	67.441959
1269.172122	61.099504	67.446964
1268.319513	62.519882	67.451969
1267.426896	69.630247	67.456974
1267.010543	59.891097	67.461978
1266.606089	62.594949	67.466983
1265.326202	67.089114	67.471988
1265.011298	57.202342	67.476993
1264.149394	67.093362	67.481998
1264.041017	67.403880	67.487002
1262.893950	63.493489	67.492007
1261.890758	66.732452	67.497012
1261.441496	62.098288	67.502017
1260.675292	74.280840	67.507022
1260.431775	65.989526	67.512026
1259.992288	58.237399	67.517031
1258.831545	70.614195	67.522036
1257.904636	64.421752	67.527041
1257.041311	69.222746	67.532046
1256.861114	67.607893	67.537050
1256.470243	64.555627	67.542055
1255.772318	68.709783	67.547060
1255.458546	69.789639	67.552065
1254.230161	61.092226	67.557070
1253.279831	61.204270	67.562074
1253.014553	62.968157	67.567079
1252.621285	59.732760	67.572084
1252.280923	56.696717	67.577089
1251.043831	63.965129	67.582094
1250.278243	55.733595	67.587098
1249.582899	63.267269	67.592103
1248.906364	73.700872	67.597108
1248.345829	66.154983	67.602113
1247.349828	68.937214	67.607118
1247.363021	59.522406	67.612122
1247.355833	65.553209	67.617127
1246.203715	60.751232	67.622132
1245.027953	70.222720	67.627137
1244.196940	68.190366	67.632142
1243.942403	67.965014	67.637146
1243.207879	65.746807	67.642151
1242.126665	68.082203	67.647156
1241.524551	62.312163	67.652161
1241.017479	70.431736	67.657166
1240.671714	60.543934	67.662170
1240.132529	60.179034	67.667175
1238.951983	73.050647	67.672180
1238.291386	66.608942	67.677185
1237.617611	72.157448	67.682190
1237.153332	66.752607	67.687194
1236.991894	68.621080	67.692199
1235.891861	72.889472	67.697204
1235.103538	65.233380	67.702209
1234.431494	79.540367	67.707214
1233.717434	67.690319	67.712218
1233.662205	70.834492	67.717223
1231.921696	61.998589	67.722228
1231.353844	66.182186	67.727233
1230.449382	74.508340	67.732238
1230.398551	70.668029	67.737242
1229.985440	69.766835	67.742247
1229.574455	68.104262	67.747252
1229.619553	66.883055	67.752257
1228.039901	71.789321	67.757262
1227.471081	68.069664	67.762266
1226.665094	69.018668	67.767271
1225.633647	69.918645	67.772276
1225.307416	62.312913	67.777281
1224.819195	64.824276	67.782286
1224.339712	61.433124	67.787290
1223.171857	68.124454	67.792295
1222.027786	65.867424	67.797300
1221.623300	58.294434	67.802305
1220.751996	63.114557	67.807310
1220.700239	57.296482	67.812314
1220.369769	60.557245	67.817319
1220.029645	65.151437	67.822324
1218.956306	58.745272	67.827329
1217.722023	66.129256	67.832334
1217.385531	66.918939	67.837338
1216.912286	69.700094	67.842343
1215.543560	71.526194	67.847348
1215.195760	59.075453	67.852353
1214.335103	72.388461	67.857358
1213.950761	65.666186	67.862362
1213.997485	69.227882	67.867367
1213.241212	73.433478	67.872372
1212.749550	70.530702	67.877377
1211.444437	72.842861	67.882382
1210.658840	64.077943	67.887386
1209.571413	63.871247	67.892391
1208.921394	71.218755	67.897396
1208.582703	67.548513	67.902401
1207.894713	68.692834	67.907406
1207.318359	66.411635	67.912410
1207.223732	69.550711	67.917415
1206.525251	68.587460	67.922420
1205.609958	57.410927	67.927425
1204.616098	62.057834	67.932430
1204.073398	63.072681	67.937434
1203.738130	60.233523	67.942439
1202.541877	71.191083	67.947444
1202.006583	55.877198	67.952449
1201.413853	69.693778	67.957454
1200.894969	70.495348	67.962458
1200.527589	67.449329	67.967463
1199.492340	66.960953	67.972468
1198.996483	58.385239	67.977473
1198.165487	65.146393	67.982478
1197.775666	66.699511	67.987482
1196.649863	69.278196	67.992487
1195.843989	74.978001	67.997492
1195.931751	61.515631	68.002497
1195.525663	64.475148	68.007502
1194.821244	71.692241	68.012506
1193.620276	71.914704	68.017511
1192.373726	67.689406	68.022516
1192.339499	64.048745	68.027521
1191.701833	66.549383	68.032526
1190.697916	64.916491	68.037530
1189.887100	63.438425	68.042535
1188.989245	69.960777	68.047540
1188.763444	55.804900	68.052545
1188.136848	64.677133	68.057550
1188.093591	67.265862	68.062554
1187.710080	69.805088	68.067559
1186.245196	65.459286	68.072564
1185.644555	63.621963	68.077569
1184.829033	67.495879	68.082574
1184.471810	63.450280	68.087578
1183.651780	66.831177	68.092583
1182.767141	72.552757	68.097588
1182.476814	68.876210	68.102593
1181.710109	70.392414	68.107598
1181.234456	65.561079	68.112602
1180.058423	65.161149	68.117607
1179.135269	75.606980	68.122612
1178.602220	66.544632	68.127617
1178.293120	70.254875	68.132622
1177.654774	69.148313	68.137626
1177.843916	70.899925	68.142631
1176.509058	68.910033	68.147636
1175.933910	58.506940	68.152641
1175.294097	63.101129	68.157646
1174.580775	63.178135	68.162650
1173.944346	59.872280	68.167655
1172.720659	56.217389	68.172660
1172.885075	48.534771	68.177665
1172.120099	60.061875	68.182670
1170.939757	62.131638	68.187674
1170.290577	66.885319	68.192679
1169.425798	65.858183	68.197684
1169.264835	59.079516	68.202689
1168.596294	72.270426	68.207694
1167.647509	67.096962	68.212698
1166.884712	57.671346	68.217703
1166.158892	65.376814	68.222708
1165.827678	59.281343	68.227713
1165.330798	68.950802	68.232718
1164.786998	66.212084	68.237722
1163.735050	54.800028	68.242727
1162.945754	61.986653	68.247732
1162.751103	57.520085	68.252737
1162.118389	63.632719	68.257742
1161.460298	59.378518	68.262746
1160.806954	59.818659	68.267751
1159.457986	64.413879	68.272756
1159.472382	60.541486	68.277761
1158.843934	71.284603	68.282766
1157.651787	67.003819	68.287770
1157.135148	57.625266	68.292775
1156.514867	64.343240	68.297780
1156.157925	54.077654	68.302785
1155.559115	62.224772	68.307790
1154.694453	58.950497	68.312794
1153.373971	64.156994	68.317799
1152.698405	61.899500	68.322804
1152.784695	52.773358	68.327809
1152.170025	66.924069	68.332814
1151.654272	62.711416	68.337818
1150.646375	56.489056	68.342823
1150.047109	58.588406	68.347828
1149.765285	51.050478	68.352833
1148.702135	60.853990	68.357838
1147.864425	55.017735	68.362842
1147.354148	57.389202	68.367847
1146.730775	62.802773	68.372852
1146.127319	60.676610	68.377857
1145.378862	63.253455	68.382862
1144.749704	59.155743	68.387866
1144.068758	61.472752	68.392871
1143.579695	70.867730	68.397876
1142.737134	59.004980	68.402881
1141.668297	58.678280	68.407886
1141.016733	71.310127	68.412890
1140.561086	64.039575	68.417895
1139.633149	59.801977	68.422900
1139.738968	52.816593	68.427905
1139.210679	59.314747	68.432910
1138.199991	62.864076	68.437914
1137.601855	52.479536	68.442919
1136.767038	60.541149	68.447924
1136.350243	49.356260	68.452929
1135.099874	58.523573	68.457934
1134.462890	65.451240	68.462938
1133.957588	51.400862	68.467943
1133.355631	68.495955	68.472948
1133.225477	49.722900	68.477953
1132.114411	58.612165	68.482958
1131.408153	54.406873	68.487962
1130.871615	48.954035	68.492967
1130.415436	59.565022	68.497972
1129.841760	55.573465	68.502977
1128.465032	50.626439	68.507982
1127.637124	55.935695	68.512986
1127.555809	55.840550	68.517991
1126.608986	57.927573	68.522996
1126.340090	57.156820	68.528001
1125.910824	54.512967	68.533006
1124.989600	59.629002	68.538010
1124.129994	54.193192	68.543015
1123.471899	62.397433	68.548020
1123.309429	58.973330	68.553025
1122.320095	58.814591	68.558030
1121.828744	56.985011	68.563034
1121.084983	47.524182	68.568039
1120.022058	57.966703	68.573044
1119.846373	53.225722	68.578049
1118.658953	58.602457	68.583054
1117.714942	60.848860	68.588058
1117.757771	53.479152	68.593063
1117.068438	52.751574	68.598068
1116.624739	49.779027	68.603073
1115.335305	62.044057	68.608078
1114.696226	58.559464	68.613082
1114.330332	57.875974	68.618087
1113.645619	62.974409	68.623092
1113.100060	67.685090	68.628097
1112.604739	60.471468	68.633102
1111.697299	61.638771	68.638106
1111.386638	56.610260	68.643111
1110.246374	69.792337	68.648116
1109.931816	53.355608	68.653121
1108.565651	58.083249	68.658126
1108.079765	55.438435	68.663130
1107.443423	54.127868	68.668135
1106.973161	62.125089	68.673140
1106.844254	50.875912	68.678145
1106.031158	66.268427	68.683150
1105.060973	65.589334	68.688154
1104.493103	58.480500	68.693159
1103.944925	65.510588	68.698164
1103.237480	57.996991	68.703169
1102.163641	57.912723	68.708174
1101.484908	61.025895	68.713178
1101.271132	51.370116	68.718183
1100.476023	54.042975	68.723188
1100.135784	52.624869	68.728193
1098.762262	55.325325	68.733198
1098.173014	64.450494	68.738202
1098.035864	54.507660	68.743207
1097.310548	55.422740	68.748212
1096.766276	47.709508	68.753217
1095.338110	59.071894	68.758222
1094.616676	53.396917	68.763226
1094.598597	52.055483	68.768231
1093.990052	57.260475	68.773236
1094.210470	53.406097	68.778241
1093.275944	57.097909	68.783246
1092.272894	58.563414	68.788250
1091.270265	56.096684	68.793255
1089.879327	62.095216	68.798260
1089.724504	51.318218	68.803265
1089.054082	64.295901	68.808270
1088.687113	59.038624	68.813274
1088.143677	52.997266	68.818279
1086.870457	54.852831	68.823284
1086.303055	57.430653	68.828289
1085.433014	61.400752	68.833294
1085.492882	65.005188	68.838298
1084.841415	54.842937	68.843303
1084.005974	68.083736	68.848308
1083.435729	52.836263	68.853313
1082.646878	53.151993	68.858318
1082.161245	56.512350	68.863322
1081.525529	53.586501	68.868327
1080.038056	59.326842	68.873332
1079.653027	57.143552	68.878337
1079.215184	60.819395	68.883342
1078.944183	61.894699	68.888346
1078.463498	55.113950	68.893351
1076.845238	61.691382	68.898356
1076.289436	62.765324	68.903361
1075.877319	69.748434	68.908366
1075.162680	70.645111	68.913370
1074.874467	64.392294	68.918375
1074.244011	71.653174	68.923380
1073.260313	69.966716	68.928385
1072.441425	68.110730	68.933390
1072.041790	66.663324	68.938394
1071.824893	63.965743	68.943399
1071.152639	69.834905	68.948404
1070.339205	60.050897	68.953409
1069.213988	62.984355	68.958414
1069.206031	64.587351	68.963418
1068.029482	61.324265	68.968423
1066.878382	61.866623	68.973428
1066.335981	62.249096	68.978433
1066.005608	66.028505	68.983438
1065.960554	61.196873	68.988442
1065.475365	57.669754	68.993447
1063.919244	64.560217	68.998452
1063.446370	63.559146	69.003457
1062.959794	68.264862	69.008462
1062.099306	63.324977	69.013466
1061.360066	60.032403	69.018471
1060.454635	65.470201	69.023476
1060.037736	60.107405	69.028481
1059.613697	57.916192	69.033486
1059.212081	57.822214	69.038490
1058.008634	59.181916	69.043495
1057.206661	63.846907	69.048500
1056.904913	51.736458	69.053505
1056.588402	59.096330	69.058510
1055.752588	60.296770	69.063514
1054.503654	57.021216	69.068519
1053.888831	58.577347	69.073524
1053.449890	59.099202	69.078529
1053.016289	66.507942	69.083534
1052.215311	69.699683	69.088538
1052.040165	59.171678	69.093543
1050.510237	65.437166	69.098548
1050.254606	63.499338	69.103553
1049.462541	65.039243	69.108558
1049.103840	62.192272	69.113562
1048.927608	54.924418	69.118567
1047.692285	67.731218	69.123572
1047.226215	53.908999	69.128577
1046.225679	57.668566	69.133582
1045.292758	64.860849	69.138586
1044.742695	60.928020	69.143591
1044.173519	63.575226	69.148596
1044.038743	66.685649	69.153601
1043.381528	68.118785	69.158606
1042.218937	62.963019	69.163610
1041.825930	60.350858	69.168615
1040.876019	69.085446	69.173620
1040.285706	61.511937	69.178625
1039.597882	51.941684	69.183630
1038.136582	59.446670	69.188634
1037.961331	59.163150	69.193639
1037.062722	69.174543	69.198644
1036.973059	60.857313	69.203649
1036.605204	61.049645	69.208654
1035.972641	64.297017	69.213658
1035.803865	61.773952	69.218663
1034.697092	62.123605	69.223668
1033.945375	56.411590	69.228673
1033.355212	67.402347	69.233678
1032.318538	62.114107	69.238682
1031.450184	64.484536	69.243687
1030.724377	62.203298	69.248692
1030.302336	59.584269	69.253697
1029.812887	64.590856	69.258702
1029.314516	63.313512	69.263706
1028.319160	61.871812	69.268711
1027.502890	61.510571	69.273716
1027.433230	65.237047	69.278721
1026.546364	69.289375	69.283726
1025.988887	66.614595	69.288730
1025.121281	58.802010	69.293735
1024.025822	69.560366	69.298740
1023.640217	56.839050	69.303745
1023.416595	66.835114	69.308750
1022.740237	68.809923	69.313754
1021.655688	62.333499	69.318759
1020.879789	75.312675	69.323764
1020.446930	69.398037	69.328769
1020.148984	76.255026	69.333774
1019.500608	70.305061	69.338778
1018.860196	54.705692	69.343783
1017.596337	68.717320	69.348788
1017.198186	64.963733	69.353793
1016.847644	69.493796	69.358798
1016.112724	69.677544	69.363802
1015.014816	67.244513	69.368807
1013.943733	70.784470	69.373812
1013.837892	70.012247	69.378817
1013.671953	67.648558	69.383822
1012.864640	69.192659	69.388826
1012.359197	56.324507	69.393831
1011.338158	75.665459	69.398836
1010.874842	65.302456	69.403841
1009.548375	70.503300	69.408846
1008.488974	69.350846	69.413850
1008.424138	65.295852	69.418855
1007.364374	71.062439	69.423860
1007.399191	62.273523	69.428865
1007.212874	70.027529	69.433870
1006.282130	67.142344	69.438874
1005.738882	61.919211	69.443879
1004.380674	73.332797	69.448884
1003.813968	64.704517	69.453889
1003.690842	67.593483	69.458894
1002.634660	63.629312	69.463898
1001.832224	61.400673	69.468903
1001.190823	71.382234	69.473908
1000.662311	68.324753	69.478913
1000.418639	67.289570	69.483918
999.784941	77.761238	69.488922
998.659372	68.614876	69.493927
998.234514	70.216637	69.498932
997.679955	53.194621	69.503937
996.631823	65.578995	69.508942
995.507613	68.969772	69.513946
995.074302	59.729342	69.518951
994.576294	73.421546	69.523956
994.124314	62.689126	69.528961
993.966844	65.551212	69.533966
992.953372	70.524784	69.538970
992.182749	58.068344	69.543975
991.311426	69.819713	69.548980
990.918286	68.946303	69.553985
990.389535	65.329947	69.558990
989.403615	59.414903	69.563994
989.189261	54.948173	69.568999
988.314004	58.998515	69.574004
987.872364	53.550368	69.579009
986.453866	64.443777	69.584014
985.982402	60.086204	69.589018
985.557842	61.123075	69.594023
985.004781	61.286341	69.599028
984.232708	65.405459	69.604033
983.339966	66.127001	69.609038
982.630014	66.192011	69.614042
982.449883	57.448593	69.619047
981.720538	65.896742	69.624052
980.848582	63.070176	69.629057
980.183419	61.604307	69.634062
979.216070	64.817837	69.639066
979.226079	59.244978	69.644071
978.129142	63.407493	69.649076
977.897810	64.001164	69.654081
976.928171	68.450548	69.659086
976.159961	65.561218	69.664090
975.986523	64.070349	69.669095
975.105787	69.036191	69.674100
973.989562	70.028495	69.679105
973.408636	73.757268	69.684110
972.585278	73.971562	69.689114
972.173546	68.977344	69.694119
971.828792	75.009497	69.699124
971.419388	70.515776	69.704129
970.638922	73.598231	69.709134
969.815322	66.633471	69.714138
969.650753	68.211578	69.719143
968.059397	71.395797	69.724148
967.489856	69.250431	69.729153
966.839247	71.720548	69.734158
966.176558	65.135975	69.739162
965.943318	69.770680	69.744167
965.112663	70.069510	69.749172
964.260524	66.872862	69.754177
963.529752	72.765474	69.759182
962.717515	71.811084	69.764186
962.915314	61.186857	69.769191
961.932564	67.355107	69.774196
961.021238	61.718990	69.779201
959.857851	55.762903	69.784206
959.741506	67.977052	69.789210
959.537607	64.380459	69.794215
958.642516	59.270876	69.799220
957.281673	59.603666	69.804225
956.592062	49.766913	69.809230
956.165534	60.648724	69.814234
955.957059	52.806567	69.819239
955.376599	55.755695	69.824244
954.844998	64.182215	69.829249
953.895026	62.678288	69.834254
952.934150	59.436717	69.839258
952.949872	54.057872	69.844263
951.874411	61.249313	69.849268
950.787934	61.081588	69.854273
950.149871	58.474697	69.859278
949.645624	69.172861	69.864282
949.502719	59.356944	69.869287
948.921159	67.303364	69.874292
947.911983	62.853550	69.879297
946.744794	54.982564	69.884302
946.287576	70.316109	69.889306
946.097871	64.871000	69.894311
945.606429	57.470833	69.899316
944.752899	57.889630	69.904321
943.790504	51.955967	69.909326
943.328520	65.027420	69.914330
943.015576	60.118917	69.919335
941.971304	62.790261	69.924340
940.921963	56.575846	69.929345
940.305706	56.789017	69.934350
939.641766	66.168943	69.939354
939.598205	60.011212	69.944359
938.852979	58.185266	69.949364
937.753548	60.626465	69.954369
937.426521	57.680928	69.959374
936.549245	61.389801	69.964378
936.257767	56.965097	69.969383
935.247498	65.142429	69.974388
934.444014	61.418404	69.979393
934.126249	58.607853	69.984398
933.602457	61.332159	69.989402
933.223715	64.984073	69.994407
931.626062	80.209797	69.999412
931.187457	70.215977	70.004417
930.549043	66.073702	70.009422
930.108190	68.260412	70.014426
929.910050	60.977375	70.019431
928.628166	69.207937	70.024436
928.047918	63.520652	70.029441
927.567241	59.034409	70.034446
926.810986	69.007616	70.039450
926.134600	60.874561	70.044455
925.124234	55.204103	70.049460
924.541679	62.604406	70.054465
924.531661	62.349826	70.059470
923.502770	66.740685	70.064474
922.133178	62.711005	70.069479
921.279103	61.311050	70.074484
921.655169	54.301893	70.079489
921.132709	55.222516	70.084494
920.377870	61.401076	70.089498
919.835235	50.658155	70.094503
918.699045	61.505593	70.099508
918.143909	54.665785	70.104513
917.698478	63.753696	70.109518
917.333751	68.426709	70.114522
916.054446	50.278779	70.119527
915.022064	59.709171	70.124532
914.581627	65.183791	70.129537
913.968595	66.600691	70.134542
913.397399	77.520315	70.139546
913.472111	64.334938	70.144551
912.300436	65.130315	70.149556
911.679625	61.369483	70.154561
911.435353	60.219942	70.159566
910.191103	70.196204	70.164570
909.288732	64.101879	70.169575
908.814183	70.440060	70.174580
908.091927	61.437806	70.179585
907.675217	63.166459	70.184590
906.716023	67.890366	70.189594
906.486430	62.689711	70.194599
906.011120	68.663305	70.199604
905.258254	54.088177	70.204609
904.385551	57.786007	70.209614
903.006578	57.010792	70.214618
902.903590	54.106227	70.219623
901.978637	62.655771	70.224628
901.605613	52.435616	70.229633
901.274481	51.626987	70.234638
900.285836	65.387025	70.239642
899.213623	58.321189	70.244647
898.407120	68.507465	70.249652
898.186753	64.307414	70.254657
898.167874	60.025096	70.259662
897.833586	66.259521	70.264666
897.125532	64.364455	70.269671
895.585888	64.179624	70.274676
895.022354	66.071969	70.279681
893.925882	63.874368	70.284686
892.595232	63.929651	70.289690
892.677839	55.099013	70.294695
892.456550	55.846485	70.299700
891.774272	61.262267	70.304705
891.752484	61.308107	70.309710
890.501566	60.679902	70.314714
889.810595	51.848738	70.319719
888.979314	57.410426	70.324724
888.215021	53.101443	70.329729
888.040341	58.446866	70.334734
887.183847	60.555167	70.339738
886.576419	52.980283	70.344743
885.918279	56.365462	70.349748
885.333941	54.914579	70.354753
884.311100	53.535247	70.359758
882.948700	61.909859	70.364762
882.992020	58.304088	70.369767
882.457395	62.705426	70.374772
881.953316	54.690891	70.379777
881.710333	57.601961	70.384782
880.685444	63.539030	70.389786
879.658288	56.270100	70.394791
879.065309	63.197742	70.399796
878.314292	62.324851	70.404801
878.260450	57.128046	70.409806
877.351579	64.185972	70.414810
876.553625	58.429807	70.419815
875.729154	54.007982	70.424820
875.496786	55.245220	70.429825
874.967315	59.190568	70.434830
873.735155	64.019647	70.439834
872.978970	64.817289	70.444839
872.395729	67.078124	70.449844
872.320176	67.111858	70.454849
871.106656	64.396708	70.459854
870.159417	61.517141	70.464858
869.828730	60.362667	70.469863
869.003679	69.575201	70.474868
868.823419	59.997391	70.479873
868.160425	59.173370	70.484878
867.260910	62.266358	70.489882
866.691638	58.671566	70.494887
866.166559	58.896760	70.499892
865.601252	63.455319	70.504897
864.787076	64.503276	70.509902
863.681198	62.522414	70.514906
863.142562	59.496686	70.519911
862.909206	64.909394	70.524916
862.487927	62.862591	70.529921
861.814787	51.549961	70.534926
860.622745	68.516772	70.539930
860.292853	57.820707	70.544935
859.052573	57.412124	70.549940
858.098695	57.691026	70.554945
857.562843	55.458990	70.559950
856.985384	58.283672	70.564954
856.586822	51.273384	70.569959
856.003606	57.034548	70.574964
855.692268	60.462958	70.579969
855.166500	52.451354	70.584974
854.143932	63.708395	70.589978
853.846581	56.403679	70.594983
852.749145	60.794841	70.599988
851.755037	59.510852	70.604993
851.131740	46.407159	70.609998
850.315198	60.147981	70.615002
849.925514	52.978286	70.620007
849.690776	60.270073	70.625012
849.311323	56.097671	70.630017
848.553041	53.715455	70.635022
847.487493	60.907975	70.640026
847.252594	59.280016	70.645031
846.364444	64.372267	70.650036
845.105116	65.145965	70.655041
844.476152	56.964547	70.660046
844.090199	62.416415	70.665050
843.616533	53.361341	70.670055
843.151442	65.573237	70.675060
842.110063	62.813611	70.680065
841.635121	61.007700	70.685070
840.759635	68.987889	70.690074
840.402351	49.831855	70.695079
839.578420	62.697677	70.700084
838.558279	66.389984	70.705089
838.045761	50.524045	70.710094
837.267744	67.822551	70.715098
837.026464	49.989076	70.720103
836.452482	69.761051	70.725108
835.861874	62.535773	70.730113
835.193231	61.771537	70.735118
834.282211	67.188611	70.740122
834.188752	52.883437	70.745127
832.943647	54.752008	70.750132
831.967022	58.104905	70.755137
831.782278	60.286042	70.760142
830.829033	69.316468	70.765146
830.422477	61.240633	70.770151
829.500357	62.524177	70.775156
828.293429	63.207986	70.780161
828.185542	57.662040	70.785166
827.969941	64.225064	70.790170
827.460614	56.596679	70.795175
826.308993	58.820667	70.800180
825.386655	59.583225	70.805185
824.856971	63.270470	70.810190
824.355865	60.649218	70.815194
824.087211	58.991123	70.820199
823.297345	65.225032	70.825204
822.309162	58.590854	70.830209
822.015154	57.558778	70.835214
821.032849	64.703890	70.840218
820.511817	55.624960	70.845223
819.344054	60.341578	70.850228
818.657696	65.285196	70.855233
818.437928	60.650470	70.860238
817.821035	60.133937	70.865242
817.601387	55.478666	70.870247
816.015658	57.171519	70.875252
815.616519	62.592491	70.880257
815.279105	59.885180	70.885262
814.266876	67.961421	70.890266
813.936464	57.060202	70.895271
812.712949	58.673647	70.900276
812.182441	51.204809	70.905281
811.561880	59.816294	70.910286
811.240046	66.961957	70.915290
810.707100	58.610555	70.920295
810.270909	66.157495	70.925300
808.891964	66.924849	70.930305
808.385523	63.128656	70.935310
807.748013	64.153861	70.940314
807.448573	53.621136	70.945319
806.462457	59.425659	70.950324
805.819046	60.477925	70.955329
804.937145	60.994758	70.960334
804.317492	71.003386	70.965338
804.206616	60.681503	70.970343
803.721764	59.812373	70.975348
802.669048	58.981304	70.980353
802.047960	60.401964	70.985358
801.402440	65.075709	70.990362
800.676889	68.161804	70.995367
799.836788	64.156725	71.000372
799.123954	68.324530	71.005377
798.610167	58.977929	71.010382
797.753092	68.325024	71.015386
797.548476	61.995954	71.020391
796.589518	68.460925	71.025396
796.017473	62.255578	71.030401
795.729665	61.221652	71.035406
794.673220	67.721083	71.040410
793.687475	64.305790	71.045415
793.343368	68.344914	71.050420
792.429772	70.027246	71.055425
792.086499	65.651294	71.060430
791.325665	62.279974	71.065434
790.513164	56.801042	71.070439
789.653532	72.492439	71.075444
788.948909	69.748164	71.080449
789.031300	66.803165	71.085454
788.312710	76.462053	71.090458
787.685541	63.937678	71.095463
786.070943	73.678204	71.100468
785.221888	64.612439	71.105473
785.293231	63.693827	71.110478
784.494407	63.018603	71.115482
784.441795	65.169214	71.120487
784.064717	67.256988	71.125492
782.744412	69.843415	71.130497
782.671984	55.390574	71.135502
781.823761	69.287218	71.140506
780.888665	62.556330	71.145511
780.310795	65.493979	71.150516
779.634262	65.103318	71.155521
778.830933	67.352917	71.160526
777.361919	69.341168	71.165530
776.602361	62.764939	71.170535
776.533349	72.321636	71.175540
775.901391	68.886796	71.180545
775.816014	62.884653	71.185550
775.353704	65.519892	71.190554
774.535297	60.499449	71.195559
773.280698	59.940981	71.200564
773.059451	68.243691	71.205569
772.363260	60.380496	71.210574
771.740538	71.831544	71.215578
770.637773	65.125431	71.220583
769.902259	72.885085	71.225588
769.501464	66.422262	71.230593
769.121545	66.110655	71.235598
768.250528	62.067856	71.240602
767.588918	60.760087	71.245607
766.856036	57.316488	71.250612
766.370383	71.400093	71.255617
765.995014	57.050458	71.260622
764.376907	62.276835	71.265626
763.894151	62.414663	71.270631
763.194609	66.194952	71.275636
762.517091	64.017588	71.280641
762.542090	67.471278	71.285646
761.698292	65.884866	71.290650
761.554959	61.536245	71.295655
760.310117	62.329981	71.300660
759.555516	63.063029	71.305665
759.322695	58.864336	71.310670
758.307902	73.476321	71.315674
757.459382	62.757011	71.320679
756.902972	64.079365	71.325684
755.971619	60.798442	71.330689
755.636074	69.015342	71.335694
755.413703	64.343963	71.340698
753.866512	62.980272	71.345703
753.417127	68.302097	71.350708
752.889109	60.223399	71.355713
752.965885	63.029175	71.360718
751.744425	64.977397	71.365722
751.103188	64.884230	71.370727
750.524697	65.531852	71.375732
750.044067	65.320389	71.380737
749.508809	64.690808	71.385742
748.071407	58.693306	71.390746
747.451579	57.126160	71.395751
746.776467	55.977014	71.400756
746.139980	56.027105	71.405761
746.528630	53.028859	71.410766
745.102134	68.078053	71.415770
744.129260	63.181966	71.420775
743.842497	63.264513	71.425780
743.027262	63.141551	71.430785
742.742731	59.444321	71.435790
741.651709	60.777733	71.440794
740.777232	56.717772	71.445799
740.061155	51.769806	71.450804
739.768452	59.496626	71.455809
739.582330	49.602889	71.460814
738.811868	58.185978	71.465818
737.888266	54.477440	71.470823
737.317483	56.371436	71.475828
736.817207	51.742142	71.480833
736.019307	55.141408	71.485838
734.869690	59.804804	71.490842
734.563224	51.828285	71.495847
734.048175	61.075742	71.500852
733.426060	57.904474	71.505857
732.578937	54.733858	71.510862
731.694529	58.233992	71.515866
731.471303	50.001651	71.520871
731.001926	55.722796	71.525876
730.026818	57.703816	71.530881
729.081672	51.666208	71.535886
727.945410	61.718330	71.540890
728.310966	55.395409	71.545895
727.539147	61.286385	71.550900
726.497313	60.081253	71.555905
725.945634	57.999964	71.560910
725.258177	62.017383	71.565914
724.953898	61.442179	71.570919
724.045848	65.700270	71.575924
722.854219	54.495441	71.580929
722.247739	54.776039	71.585934
721.544199	57.146306	71.590938
721.705338	55.225130	71.595943
720.870634	56.708838	71.600948
720.271339	64.356740	71.605953
719.415932	55.992705	71.610958
718.699821	56.773242	71.615962
718.032959	57.995711	71.620967
717.249854	56.301811	71.625972
715.983723	47.149242	71.630977
715.525623	51.596290	71.635982
714.654345	63.296347	71.640986
714.370855	50.296310	71.645991
714.006713	58.884792	71.650996
713.780511	65.722771	71.656001
713.807971	50.729049	71.661006
712.702638	63.648607	71.666010
711.929735	60.195296	71.671015
710.331264	55.136403	71.676020
709.710441	56.000085	71.681025
709.177064	53.026767	71.686030
708.296759	53.058239	71.691034
708.187815	49.788016	71.696039
708.084750	54.968016	71.701044
707.130462	53.639740	71.706049
706.149158	56.527301	71.711054
705.663367	58.130046	71.716058
704.880923	43.866750	71.721063
703.578817	59.303951	71.726068
702.510999	54.208628	71.731073
702.905336	52.172903	71.736078
702.339276	57.206047	71.741082
701.780109	60.396273	71.746087
701.148996	57.450355	71.751092
700.357897	53.517429	71.756097
699.596211	47.774436	71.761102
698.548065	55.980779	71.766106
698.280544	52.732589	71.771111
697.966428	54.275137	71.776116
697.082644	59.099436	71.781121
696.633043	44.555716	71.786126
695.671162	57.716339	71.791130
694.488456	50.315832	71.796135
693.594408	53.764730	71.801140
693.149542	54.397361	71.806145
693.143164	51.217325	71.811150
692.506602	52.395924	71.816154
692.174265	56.331984	71.821159
691.533183	48.454637	71.826164
690.071722	53.028970	71.831169
689.919882	44.625732	71.836174
688.708141	51.787660	71.841178
687.543048	45.170017	71.846183
687.381257	49.518150	71.851188
686.395670	48.456147	71.856193
685.879388	44.915463	71.861198
685.491479	51.839161	71.866202
685.083942	50.900356	71.871207
684.832576	44.981134	71.876212
684.084625	49.782951	71.881217
683.545758	51.468207	71.886222
682.292191	52.089387	71.891226
681.966502	50.077542	71.896231
681.113686	49.399351	71.901236
680.028938	54.897121	71.906241
679.604618	52.169582	71.911246
679.489976	52.981288	71.916250
678.608241	57.170143	71.921255
677.443741	53.852210	71.926260
676.558722	56.605262	71.931265
676.383874	54.638230	71.936270
675.900998	56.768605	71.941274
675.569125	57.315569	71.946279
674.295326	49.147561	71.951284
673.561053	59.886701	71.956289
673.133549	56.543164	71.961294
672.533382	61.254936	71.966298
672.055432	54.651411	71.971303
670.879239	52.726457	71.976308
670.227386	59.761294	71.981313
669.590366	48.662780	71.986318
669.239545	56.406658	71.991322
668.820060	51.694063	71.996327
667.738558	55.440327	72.001332
666.888302	51.549515	72.006337
666.272948	47.168092	72.011342
665.973344	56.533760	72.016346
665.832479	53.707139	72.021351
664.708168	49.236866	72.026356
663.660000	47.342085	72.031361
663.460584	41.166086	72.036366
662.348018	54.110168	72.041370
661.542522	52.170656	72.046375
660.980266	46.578233	72.051380
660.263396	61.720586	72.056385
659.938529	49.929160	72.061390
659.500816	58.892198	72.066394
659.088619	52.170444	72.071399
658.426535	54.687554	72.076404
657.450240	56.258683	72.081409
656.997021	50.484957	72.086414
655.712703	51.709799	72.091418
655.074420	50.477784	72.096423
654.533079	51.305752	72.101428
653.694153	57.817274	72.106433
653.693392	42.434873	72.111438
652.024821	52.487803	72.116442
651.670825	48.384089	72.121447
650.989077	50.372494	72.126452
650.234679	62.989186	72.131457
650.181578	50.916347	72.136462
649.875298	55.495670	72.141466
648.541668	58.092306	72.146471
647.841967	47.938431	72.151476
647.220089	53.864510	72.156481
647.072628	48.041957	72.161486
646.501502	50.334681	72.166490
645.338330	56.894254	72.171495
644.703947	56.878080	72.176500
643.918388	63.572689	72.181505
643.718632	51.037503	72.186510
642.365999	53.900275	72.191514
641.860271	57.858937	72.196519
641.507430	54.125267	72.201524
641.046610	62.020222	72.206529
640.455414	52.338781	72.211534
638.924000	57.349035	72.216538
638.395104	43.732284	72.221543
638.048477	50.515890	72.226548
637.357095	63.163232	72.231553
637.239546	52.836995	72.236558
635.927060	60.812334	72.241562
635.319430	60.956569	72.246567
634.514404	53.672945	72.251572
634.391124	65.527869	72.256577
633.859729	59.574521	72.261582
632.921834	58.271477	72.266586
631.863151	56.047733	72.271591
631.354709	51.473535	72.276596
630.930100	60.446960	72.281601
630.567949	51.735171	72.286606
629.582743	60.936868	72.291610
628.410505	63.730057	72.296615
628.119367	69.037406	72.301620
627.784713	63.653870	72.306625
627.126087	52.433942	72.311630
626.096992	57.802194	72.316634
625.323825	55.161268	72.321639
624.810737	60.707944	72.326644
624.125577	64.647616	72.331649
623.802027	56.265904	72.336654
622.566959	62.429271	72.341658
621.839749	60.539112	72.346663
621.484628	54.859104	72.351668
620.845024	59.832226	72.356673
620.678099	56.387214	72.361678
619.968974	59.715631	72.366682
618.967573	61.578421	72.371687
618.402879	57.798158	72.376692
617.487409	58.141180	72.381697
617.217374	54.633312	72.386702
615.967480	72.727884	72.391706
615.427259	65.131669	72.396711
614.945668	69.098436	72.401716
614.319572	69.382804	72.406721
614.205428	57.455811	72.411726
612.803692	63.579054	72.416730
612.066920	65.636099	72.421735
611.936311	57.776301	72.426740
611.409906	66.050368	72.431745
610.563373	69.136292	72.436750
609.408318	64.716689	72.441754
608.694885	61.630951	72.446759
608.347509	59.195352	72.451764
607.704078	62.649482	72.456769
607.319181	59.723760	72.461774
606.272216	67.526125	72.466778
605.563840	64.186508	72.471783
604.903104	61.591056	72.476788
604.395846	65.459989	72.481793
604.272640	59.403162	72.486798
602.941035	65.877136	72.491802
602.518358	66.080866	72.496807
602.040973	64.209878	72.501812
601.055794	66.864847	72.506817
600.341492	63.058905	72.511822
599.198245	58.678729	72.516826
598.659890	63.753711	72.521831
598.522018	63.862070	72.526836
597.785892	71.134367	72.531841
597.693554	57.183887	72.536846
596.249239	70.197852	72.541850
595.679523	64.661578	72.546855
595.239979	59.931903	72.551860
594.462857	64.291521	72.556865
594.375321	59.451014	72.561870
593.044168	60.693765	72.566874
592.467298	64.728169	72.571879
591.918495	62.535096	72.576884
591.523642	67.681014	72.581889
590.848585	56.668764	72.586894
589.878052	66.617516	72.591898
589.285295	61.170845	72.596903
588.691359	63.456432	72.601908
587.261959	68.597638	72.606913
586.658129	64.202014	72.611918
586.170175	69.576240	72.616922
585.959841	55.184954	72.621927
585.651409	62.548566	72.626932
585.074327	60.033121	72.631937
584.497720	49.735416	72.636942
583.123798	60.165359	72.641946
582.386457	63.592558	72.646951
582.443241	49.839551	72.651956
581.144035	71.390003	72.656961
580.377988	56.815260	72.661966
579.727840	63.856521	72.666970
579.048456	50.798032	72.671975
578.859516	53.145669	72.676980
578.310468	56.688624	72.681985
577.660142	60.959417	72.686990
576.594325	62.981664	72.691994
575.958327	56.955466	72.696999
575.561842	52.903247	72.702004
574.600920	56.125214	72.707009
573.793064	59.814348	72.712014
573.084575	56.521335	72.717018
572.820514	57.876507	72.722023
572.596050	56.246384	72.727028
571.386270	52.256937	72.732033
570.494130	49.738638	72.737038
569.642329	61.104593	72.742042
569.399149	58.450236	72.747047
569.391859	60.192837	72.752052
567.979731	61.401708	72.757057
567.218819	53.266643	72.762062
566.914260	48.869485	72.767066
566.538171	57.142661	72.772071
565.465988	47.234590	72.777076
564.438492	52.971633	72.782081
563.716050	47.752442	72.787086
563.461735	64.873187	72.792090
563.115543	55.318723	72.797095
562.721005	56.229699	72.802100
561.715426	58.811594	72.807105
560.923975	52.989262	72.812110
560.305316	60.119069	72.817114
558.920013	65.274434	72.822119
558.444646	58.919549	72.827124
557.729952	58.539012	72.832129
557.664456	62.565533	72.837134
557.045559	56.583774	72.842138
556.662578	59.915920	72.847143
555.665328	53.623616	72.852148
554.367210	64.509894	72.857153
554.069567	56.412685	72.862158
553.579635	55.928115	72.867162
552.931497	55.895759	72.872167
552.560433	51.623280	72.877172
551.245076	57.993825	72.882177
550.996773	56.717504	72.887182
550.304677	56.344148	72.892186
549.795654	54.935272	72.897191
548.786170	48.291405	72.902196
547.737469	61.415997	72.907201
547.315131	54.241287	72.912206
546.978817	55.781330	72.917210
546.337106	54.558601	72.922215
546.021875	43.265259	72.927220
544.800545	57.212801	72.932225
544.181413	54.226174	72.937230
543.649829	51.382434	72.942234
542.934136	51.803339	72.947239
542.707406	58.641795	72.952244
541.816520	60.386591	72.957249
540.870294	48.362199	72.962254
540.363483	57.291682	72.967258
539.656237	57.458919	72.972263
539.018357	53.361228	72.977268
537.874729	57.228286	72.982273
537.552062	60.275378	72.987278
537.169281	65.294499	72.992282
536.706457	55.277287	72.997287
536.665969	50.324126	73.002292
535.249966	69.040810	73.007297
534.266667	54.961571	73.012302
533.714723	65.188716	73.017306
532.468485	63.539074	73.022311
531.867864	57.617737	73.027316
531.095794	57.635038	73.032321
530.757714	51.943440	73.037326
530.426868	60.338330	73.042330
529.972938	59.351439	73.047335
529.881289	55.814593	73.052340
528.899642	71.547815	73.057345
527.938393	58.470924	73.062350
527.324262	61.002331	73.067354
526.800520	64.334915	73.072359
525.921432	59.241642	73.077364
524.864963	62.024490	73.082369
524.885631	51.270399	73.087374
523.843281	60.123102	73.092378
522.406702	67.304645	73.097383
521.921971	57.629064	73.102388
521.215138	66.915702	73.107393
521.417632	58.891476	73.112398
520.993389	60.159235	73.117402
520.329224	57.460970	73.122407
519.828282	58.708321	73.127412
518.527610	57.808099	73.132417
517.937708	58.514935	73.137422
517.541100	59.504424	73.142426
516.149036	68.027472	73.147431
515.726753	51.575010	73.152436
514.867631	59.659784	73.157441
514.675213	52.129914	73.162446
513.979775	52.382362	73.167450
513.420137	62.001781	73.172455
512.590954	53.638836	73.177460
511.646750	67.368389	73.182465
511.110933	49.735454	73.187470
511.017738	58.188695	73.192474
509.822309	62.795645	73.197479
508.957828	48.542518	73.202484
507.965656	59.690964	73.207489
507.627908	52.920953	73.212494
506.954752	59.587629	73.217498
506.861555	58.575637	73.222503
506.869067	49.934733	73.227508
505.662663	59.495246	73.232513
504.935158	55.894864	73.237518
504.427630	59.161910	73.242522
503.419727	54.050061	73.247527
502.331550	57.242137	73.252532
501.673510	52.754379	73.257537
501.407225	52.984607	73.262542
501.037505	53.422810	73.267546
500.173324	54.192435	73.272551
499.625695	52.423887	73.277556
498.785908	63.597932	73.282561
498.321632	50.959686	73.287566
497.413929	57.977585	73.292570
496.128426	60.990724	73.297575
495.745650	51.851466	73.302580
494.936365	63.068834	73.307585
494.695304	50.618512	73.312590
494.214178	55.982884	73.317594
493.736960	60.084688	73.322599
493.647902	50.724980	73.327604
492.137612	58.080594	73.332609
491.780206	55.139913	73.337614
490.561627	59.868063	73.342618
489.249872	57.789160	73.347623
488.856644	53.112352	73.352628
488.483930	56.682332	73.357633
488.384620	49.377683	73.362638
488.233439	55.014709	73.367642
487.384445	66.255856	73.372647
486.693698	57.476850	73.377652
485.655817	65.998420	73.382657
485.089342	59.305890	73.387662
483.904691	52.184453	73.392666
483.161662	56.030244	73.397671
482.891133	65.300932	73.402676
482.363784	60.975901	73.407681
481.761604	57.196953	73.412686
481.012300	55.155482	73.417690
479.962074	59.640852	73.422695
479.824701	52.071556	73.427700
478.938316	59.996804	73.432705
478.167919	53.818798	73.437710
477.020680	59.260605	73.442714
476.139810	57.407459	73.447719
476.109348	52.372062	73.452724
475.330381	58.876881	73.457729
475.136486	52.849943	73.462734
474.794926	62.385813	73.467738
474.184364	65.406455	73.472743
473.543441	57.133620	73.477748
472.816447	60.504588	73.482753
471.702190	53.903165	73.487758
470.963284	64.581139	73.492762
470.038163	55.187863	73.497767
469.820895	55.534028	73.502772
468.914218	54.157384	73.507777
468.087029	52.401615	73.512782
467.428222	51.518123	73.517786
467.081361	63.170565	73.522791
466.994463	49.918220	73.527796
465.735706	60.893679	73.532801
464.737254	61.860387	73.537806
463.866059	52.984817	73.542810
463.417920	52.952147	73.547815
463.152420	41.328610	73.552820
462.705814	51.334024	73.557825
462.146982	54.679728	73.562830
461.128454	51.913520	73.567834
460.424276	56.902061	73.572839
460.031390	47.952822	73.577844
458.653500	57.676139	73.582849
458.009834	51.880609	73.587854
457.259235	52.114098	73.592858
456.712979	53.926160	73.597863
456.324717	46.490645	73.602868
456.096987	53.083362	73.607873
455.874352	43.290659	73.612878
455.122837	46.692273	73.617882
454.014379	55.709460	73.622887
453.372778	50.822997	73.627892
452.007857	54.615499	73.632897
451.363662	47.893669	73.637902
450.914046	54.480596	73.642906
450.186512	58.168613	73.647911
450.464539	50.804043	73.652916
449.822144	55.324919	73.657921
448.921341	47.130969	73.662926
448.133895	52.381264	73.667930
447.202899	57.049485	73.672935
446.134424	48.088130	73.677940
445.202282	54.829186	73.682945
444.571130	49.404914	73.687950
444.497075	59.076508	73.692954
444.188117	60.868434	73.697959
443.836613	51.539495	73.702964
443.255309	56.289100	73.707969
442.243313	53.258897	73.712974
441.432330	46.717616	73.717978
440.608317	50.455716	73.722983
439.587960	50.971078	73.727988
438.253112	57.982054	73.732993
437.824111	56.330940	73.737998
437.801388	51.937602	73.743002
437.528300	48.662367	73.748007
436.891481	54.434319	73.753012
436.666444	53.614255	73.758017
435.637941	46.768428	73.763022
434.434147	50.865670	73.768026
433.957563	54.411612	73.773031
433.705554	48.570681	73.778036
432.197720	54.429134	73.783041
431.264163	52.515163	73.788046
431.014467	53.446325	73.793050
430.223472	55.369799	73.798055
430.348427	49.462691	73.803060
429.626639	57.251191	73.808065
429.119664	47.493005	73.813070
428.119954	44.744896	73.818074
427.220592	51.224561	73.823079
427.211993	43.404669	73.828084
426.385721	45.533912	73.833089
425.370896	48.221619	73.838094
424.753943	48.830477	73.843098
423.864981	60.920002	73.848103
423.920405	48.357707	73.853108
423.124764	58.813309	73.858113
422.176299	51.159606	73.863118
421.792311	57.583718	73.868122
421.041600	59.345957	73.873127
420.042782	57.563559	73.878132
419.227947	61.988471	73.883137
418.752659	59.140231	73.888142
418.254104	50.790914	73.893146
417.559242	55.723391	73.898151
416.882297	52.123836	73.903156
415.858254	63.407219	73.908161
415.606047	54.537686	73.913166
414.998596	52.835845	73.918170
414.323304	60.545725	73.923175
413.631645	51.181537	73.928180
412.673293	53.932591	73.933185
411.867467	50.856804	73.938190
411.622057	52.234837	73.943194
410.681282	61.262769	73.948199
409.786466	56.497463	73.953204
408.740964	57.839329	73.958209
408.251080	55.649211	73.963214
408.422662	57.047359	73.968218
407.655091	61.498119	73.973223
407.703015	52.432690	73.978228
406.645464	54.721959	73.983233
405.539356	60.639464	73.988238
404.816934	47.401704	73.993242
403.810985	57.526264	73.998247
404.031742	50.188877	74.003252
402.997483	66.313592	74.008257
401.921422	48.560522	74.013262
401.580285	59.271770	74.018266
400.929683	63.181464	74.023271
400.844680	53.049407	74.028276
400.019827	61.076217	74.033281
399.142670	60.600789	74.038286
398.254185	60.932518	74.043290
397.842110	61.379172	74.048295
397.094057	59.109752	74.053300
395.863575	73.401897	74.058305
395.311584	57.720067	74.063310
394.744812	58.340854	74.068314
394.479057	69.564159	74.073319
394.346394	58.493348	74.078324
392.812351	60.617977	74.083329
392.107779	55.227214	74.088334
391.730508	55.742505	74.093338
391.004522	64.355101	74.098343
390.772513	54.616109	74.103348
389.784221	56.559191	74.108353
388.883719	58.806155	74.113358
388.633708	52.766345	74.118362
388.031940	57.514725	74.123367
387.231003	46.401353	74.128372
386.317804	59.884816	74.133377
385.855357	51.191837	74.138382
385.620108	58.404753	74.143386
384.562776	60.242043	74.148391
383.739207	48.472983	74.153396
382.551174	63.880804	74.158401
382.346526	54.732353	74.163406
382.049866	58.427848	74.168410
381.164327	61.003809	74.173415
380.131373	54.981735	74.178420
379.378546	48.030263	74.183425
379.279136	49.636683	74.188430
378.902655	60.867904	74.193434
378.375899	59.488533	74.198439
377.256011	52.709301	74.203444
376.320580	61.939203	74.208449
375.904378	58.770992	74.213454
375.539768	56.358501	74.218458
374.276957	48.800523	74.223463
373.543499	51.518174	74.228468
373.039511	62.026424	74.233473
372.655445	55.574220	74.238478
372.450132	52.746426	74.243482
371.606628	54.104599	74.248487
370.906819	54.941203	74.253492
370.206609	55.267117	74.258497
369.007070	54.881285	74.263502
368.267390	59.842369	74.268506
367.475136	67.311395	74.273511
367.429277	57.885482	74.278516
366.655834	64.287531	74.283521
366.141451	55.767260	74.288526
365.729953	59.464279	74.293530
364.549189	66.448473	74.298535
364.094990	53.686958	74.303540
363.294108	59.500059	74.308545
362.792536	53.237327	74.313550
361.997208	61.551563	74.318554
360.999244	53.051805	74.323559
360.946248	57.811528	74.328564
360.306269	68.309537	74.333569
359.270308	59.653272	74.338574
358.595300	58.755994	74.343578
357.651598	54.041315	74.348583
357.634314	53.293407	74.353588
356.904716	59.893586	74.358593
356.038468	59.096185	74.363598
354.944566	55.344691	74.368602
354.347768	62.039736	74.373607
353.872420	58.587209	74.378612
353.791515	60.406761	74.383617
353.460892	59.817547	74.388622
352.432301	49.840106	74.393626
351.516610	58.231807	74.398631
350.827922	59.179791	74.403636
349.959040	53.598132	74.408641
349.160462	54.895323	74.413646
348.719709	54.541286	74.418650
347.998320	59.344115	74.423655
347.224768	50.162521	74.428660
347.152848	54.250921	74.433665
346.042082	51.757507	74.438670
345.322870	55.524631	74.443674
344.784660	60.748408	74.448679
344.478208	59.487592	74.453684
343.956067	52.397519	74.458689
343.112913	56.000764	74.463694
342.081977	56.083380	74.468698
341.427995	50.051630	74.473703
341.142752	53.392690	74.478708
339.840255	60.314858	74.483713
338.890126	57.634056	74.488718
338.388914	58.792659	74.493722
337.775063	59.977672	74.498727
337.846324	53.535460	74.503732
337.201053	57.584368	74.508737
337.125340	57.642215	74.513742
336.015664	60.168971	74.518746
335.209552	61.270494	74.523751
334.440657	63.082438	74.528756
333.322727	67.074206	74.533761
332.558072	62.795001	74.538766
332.299652	59.355427	74.543770
331.816630	62.971160	74.548775
331.012958	54.791775	74.553780
329.561896	60.003065	74.558785
328.985634	63.618595	74.563790
328.794792	57.064996	74.568794
327.875806	60.691503	74.573799
327.965595	49.905459	74.578804
327.171827	60.264042	74.583809
326.965860	62.036347	74.588814
326.094137	55.647203	74.593818
325.203906	55.819386	74.598823
324.748979	48.327822	74.603828
323.469295	50.215862	74.608833
322.715934	55.349415	74.613838
322.322850	58.561336	74.618842
321.598611	52.452425	74.623847
321.429717	53.227647	74.628852
320.416105	56.923264	74.633857
319.368222	62.040196	74.638862
319.165953	51.167241	74.643866
318.365901	58.919823	74.648871
318.454114	59.013520	74.653876
317.204063	64.822299	74.658881
316.386808	65.138678	74.663886
315.891386	55.377347	74.668890
314.987802	53.249856	74.673895
314.450464	64.669294	74.678900
313.547699	62.113792	74.683905
312.776525	63.834162	74.688910
312.535737	55.531074	74.693914
312.044848	59.925345	74.698919
311.899590	58.254429	74.703924
310.569428	62.845435	74.708929
310.157858	62.198654	74.713934
309.215169	58.273238	74.718938
307.817377	54.882506	74.723943
307.382636	58.566539	74.728948
306.726734	54.360670	74.733953
306.246061	59.653530	74.738958
305.769527	62.046122	74.743962
305.570793	57.867681	74.748967
305.140753	55.400099	74.753972
303.639364	58.781844	74.758977
302.917137	56.797735	74.763982
302.490900	53.066816	74.768986
301.865141	60.298505	74.773991
301.814828	54.925093	74.778996
300.653516	52.972032	74.784001
299.547309	50.752964	74.789006
299.283919	50.429320	74.794010
298.938955	56.013111	74.799015
298.100937	53.605192	74.804020
297.263048	54.536520	74.809025
296.130395	52.817745	74.814030
295.940108	52.051334	74.819034
295.201565	56.880001	74.824039
295.065049	61.386027	74.829044
293.740024	56.785268	74.834049
292.878404	47.366563	74.839054
292.636731	52.312951	74.844058
291.985592	59.252167	74.849063
291.846815	45.221689	74.854068
290.856345	59.169161	74.859073
289.910742	57.089927	74.864078
289.597245	58.473714	74.869082
288.891220	53.835151	74.874087
287.947555	51.723219	74.879092
287.050830	55.776153	74.884097
286.623778	51.575273	74.889102
286.284460	48.321271	74.894106
285.598786	49.261247	74.899111
284.695794	52.086514	74.904116
284.078178	50.603526	74.909121
283.655107	50.482898	74.914126
283.058290	47.473940	74.919130
281.542435	64.243666	74.924135
281.224375	50.439692	74.929140
280.528549	48.675259	74.934145
280.300512	45.331532	74.939150
279.947745	49.967771	74.944154
278.522074	58.074674	74.949159
277.793738	42.898352	74.954164
277.169707	50.692602	74.959169
276.575762	47.693415	74.964174
276.498879	46.196691	74.969178
275.619942	50.642868	74.974183
275.100380	48.295233	74.979188
273.981800	55.613363	74.984193
273.290897	49.799916	74.989198
273.555911	46.021177	74.994202
272.113365	53.482855	74.999207
271.036942	50.018897	75.004212
270.574147	59.794998	75.009217
270.305195	54.658393	75.014222
270.572695	49.830870	75.019226
268.978894	62.225543	75.024231
268.096215	48.350595	75.029236
267.777278	51.783478	75.034241
266.436488	54.711811	75.039246
265.754930	49.214508	75.044250
264.850809	55.828423	75.049255
265.292973	51.339624	75.054260
264.331100	51.038602	75.059265
263.612616	52.608245	75.064270
263.427473	52.919704	75.069274
262.287317	54.085203	75.074279
261.415677	54.956800	75.079284
260.751058	48.029709	75.084289
260.071146	48.727926	75.089294
260.012624	45.393038	75.094298
258.756984	53.411199	75.099303
257.853855	50.561713	75.104308
257.576444	54.906765	75.109313
256.782154	55.156063	75.114318
256.657278	55.696783	75.119322
256.202299	64.909082	75.124327
255.469409	48.601110	75.129332
254.830014	54.466274	75.134337
253.642976	54.456069	75.139342
252.616310	52.879786	75.144346
251.820403	53.530391	75.149351
251.437594	54.079797	75.154356
250.864856	56.912407	75.159361
250.492122	59.031043	75.164366
250.021324	49.916785	75.169370
249.017111	56.990726	75.174375
248.172921	50.034814	75.179380
247.642548	54.575583	75.184385
247.166027	53.664038	75.189390
247.072961	44.968562	75.194394
245.754378	50.876723	75.199399
245.166587	45.610443	75.204404
244.376541	50.895940	75.209409
243.881642	54.441085	75.214414
243.030438	55.905988	75.219418
242.027224	56.879478	75.224423
241.363401	53.507428	75.229428
241.165204	59.207372	75.234433
240.585639	56.407028	75.239438
240.377694	56.360839	75.244442
239.052774	62.811638	75.249447
238.135828	54.926807	75.254452
237.944266	56.990707	75.259457
237.367146	54.508082	75.264462
237.118922	46.735989	75.269466
235.657533	59.962127	75.274471
235.111804	51.442917	75.279476
234.990393	59.098129	75.284481
233.716728	50.781844	75.289486
233.319737	51.882333	75.294490
232.320382	57.511585	75.299495
232.035604	55.287912	75.304500
231.364390	49.709900	75.309505
230.417440	54.650870	75.314510
229.626925	49.690112	75.319514
228.838775	53.332494	75.324519
228.386957	47.925680	75.329524
228.249459	59.286841	75.334529
227.811540	62.956030	75.339534
226.737567	52.029624	75.344538
225.500339	47.257931	75.349543
225.232801	48.580162	75.354548
225.205613	55.003903	75.359553
224.058373	53.820508	75.364558
223.446905	54.889870	75.369562
222.376022	59.996550	75.374567
222.184794	53.245675	75.379572
221.429647	49.085649	75.384577
220.103597	48.972182	75.389582
219.680468	46.610394	75.394586
218.754653	51.198816	75.399591
218.725107	52.222113	75.404596
218.071603	54.827006	75.409601
217.695613	57.656289	75.414606
217.153551	63.059934	75.419610
215.958967	64.776320	75.424615
215.241735	47.122868	75.429620
214.635202	58.870720	75.434625
214.481850	54.523467	75.439630
213.487513	52.714298	75.444634
212.361945	56.633585	75.449639
211.955737	52.380988	75.454644
211.819765	53.916706	75.459649
210.730661	59.816331	75.464654
210.305499	54.158648	75.469658
209.289064	65.193263	75.474663
209.083328	54.005544	75.479668
208.101383	63.594335	75.484673
206.983860	57.139992	75.489678
206.509653	57.218387	75.494682
205.866428	55.215623	75.499687
205.624715	61.524173	75.504692
205.089828	50.664834	75.509697
204.317194	55.805255	75.514702
203.392861	52.501155	75.519706
202.630776	64.105159	75.524711
202.137878	55.984240	75.529716
202.122086	56.524025	75.534721
200.850342	59.446461	75.539726
200.266815	55.961976	75.544730
199.236827	60.057108	75.549735
199.117547	56.507649	75.554740
198.510285	57.106586	75.559745
197.004015	63.987929	75.564750
196.487613	53.204364	75.569754
195.820643	60.955854	75.574759
195.589170	54.653958	75.579764
195.077216	54.765665	75.584769
194.680694	58.813393	75.589774
193.958922	58.108882	75.594778
193.232451	55.875273	75.599783
192.460803	53.352189	75.604788
191.363375	60.508824	75.609793
190.470483	66.558362	75.614798
190.007212	58.307242	75.619802
189.615634	64.176906	75.624807
189.104039	50.950434	75.629812
188.740440	56.253623	75.634817
187.293979	62.857496	75.639822
186.891738	52.684720	75.644826
186.203915	66.447704	75.649831
185.832641	55.668077	75.654836
185.797548	51.964856	75.659841
184.566016	53.907831	75.664846
184.072804	52.749301	75.669850
182.632240	55.606738	75.674855
181.639472	56.503059	75.679860
181.114901	56.565224	75.684865
180.356224	60.587801	75.689870
180.682709	55.110731	75.694874
179.926051	63.609000	75.699879
179.321081	55.708205	75.704884
178.977788	50.462784	75.709889
178.052553	56.582992	75.714894
177.325898	55.209495	75.719898
176.378887	63.092670	75.724903
175.391222	49.261406	75.729908
174.401288	57.463759	75.734913
173.733596	59.545334	75.739918
173.297964	53.068056	75.744922
172.982648	57.844712	75.749927
172.873059	63.673932	75.754932
172.375735	59.665100	75.759937
171.535844	57.336470	75.764942
170.636432	44.738558	75.769946
169.936056	58.232124	75.774951
169.339181	48.213895	75.779956
167.941074	52.456207	75.784961
167.383814	56.767922	75.789966
167.112690	47.636427	75.794970
166.308470	58.432176	75.799975
166.534479	53.263234	75.804980
165.713868	51.727040	75.809985
164.591096	58.928283	75.814990
164.223252	49.109991	75.819994
163.018505	52.198176	75.824999
162.102281	52.644039	75.830004
161.414614	51.418194	75.835009
160.732096	51.527172	75.840014
160.374985	49.171046	75.845018
159.838305	52.136817	75.850023
159.809380	50.471623	75.855028
159.258112	41.897333	75.860033
157.901445	57.333285	75.865038
157.743375	44.190690	75.870042
156.314955	52.528995	75.875047
155.487586	47.046842	75.880052
154.802187	57.965899	75.885057
154.131764	51.803592	75.890062
154.009214	50.212470	75.895066
153.575477	54.716550	75.900071
153.358926	53.770713	75.905076
152.260532	48.186214	75.910081
150.849635	54.714132	75.915086
150.712862	52.889410	75.920090
150.272053	57.066697	75.925095
149.279090	61.423500	75.930100
148.472243	49.730193	75.935105
147.442723	56.145369	75.940110
147.215782	53.330773	75.945114
146.691702	52.485020	75.950119
146.279224	50.919521	75.955124
145.688571	54.346491	75.960129
144.417386	49.679322	75.965134
143.976708	41.827742	75.970138
143.552949	54.479331	75.975143
142.878223	52.661571	75.980148
141.920440	47.192700	75.985153
140.713782	54.210969	75.990158
140.680197	45.674246	75.995162
140.468229	61.035939	76.000167
139.973303	51.932943	76.005172
138.898226	56.004632	76.010177
138.032396	58.301744	76.015182
137.900283	50.392923	76.020186
136.990617	46.710559	76.025191
135.796331	49.613811	76.030196
135.170496	44.568007	76.035201
134.462747	53.427339	76.040206
134.169203	45.187401	76.045210
133.630009	54.806868	76.050215
132.999246	59.803381	76.055220
132.522087	60.175166	76.060225
131.190694	56.374452	76.065230
131.173764	49.357277	76.070234
130.686707	54.001542	76.075239
129.627576	47.614580	76.080244
128.547854	49.689823	76.085249
127.825027	56.607392	76.090254
127.679983	54.207020	76.095258
126.638476	53.181172	76.100263
125.773893	49.359249	76.105268
125.639238	51.722848	76.110273
124.838950	57.330622	76.115278
124.572471	53.437742	76.120282
123.793892	54.993234	76.125287
122.695519	51.264281	76.130292
122.250920	54.084015	76.135297
121.531141	61.388670	76.140302
121.251201	53.872668	76.145306
119.678686	47.617137	76.150311
118.922246	51.540658	76.155316
118.907360	49.597154	76.160321
118.295776	50.923111	76.165326
117.994129	43.788969	76.170330
117.751896	51.868674	76.175335
116.785114	45.831784	76.180340
115.988903	44.041960	76.185345
114.821932	45.339582	76.190350
113.860969	42.202827	76.195354
113.124047	50.228397	76.200359
112.664256	53.998439	76.205364
112.193273	49.584076	76.210369
112.086974	51.123787	76.215374
111.770796	40.877074	76.220378
110.371270	47.653690	76.225383
109.419403	47.109817	76.230388
109.353242	46.617775	76.235393
108.786960	55.113011	76.240398
107.647941	43.282862	76.245402
106.477612	52.157158	76.250407
106.092073	43.873395	76.255412
105.803776	42.651722	76.260417
105.353553	53.097460	76.265422
104.891335	41.678623	76.270426
103.668958	47.278235	76.275431
102.892682	48.849518	76.280436
102.539545	47.221355	76.285441
101.917284	58.084197	76.290446
100.990531	55.274320	76.295450
100.068978	47.796086	76.300455
99.766726	53.479523	76.305460
99.426025	55.278484	76.310465
98.916214	55.295104	76.315470
97.635077	55.338568	76.320474
96.609609	55.589633	76.325479
95.919163	57.049104	76.330484
95.660497	54.999771	76.335489
95.204750	62.322319	76.340494
95.344130	52.460894	76.345498
94.029350	59.636649	76.350503
93.184047	62.242467	76.355508
92.874787	54.060485	76.360513
91.900879	59.670793	76.365518
90.939182	57.999732	76.370522
90.089372	58.328441	76.375527
89.733468	61.892793	76.380532
89.388793	55.329675	76.385537
88.617190	57.765763	76.390542
88.389302	44.332012	76.395546
87.040083	53.802207	76.400551
86.688813	47.952678	76.405556
86.426743	50.922294	76.410561
85.120517	56.289593	76.415566
84.409146	56.051840	76.420570
83.842922	57.215693	76.425575
83.458761	50.444624	76.430580
83.028699	57.173067	76.435585
81.643399	56.999934	76.440590
81.456519	46.943410	76.445594
80.563108	52.553732	76.450599
80.430052	55.910548	76.455604
79.345710	51.998817	76.460609
78.010999	52.566570	76.465614
77.922108	49.701078	76.470618
77.184373	56.306226	76.475623
76.552071	46.008324	76.480628
76.449676	45.830765	76.485633
75.239551	58.473098	76.490638
74.619410	48.496379	76.495642
73.539673	52.877542	76.500647
73.216371	50.170256	76.505652
73.145411	56.011003	76.510657
71.945036	57.758414	76.515662
71.340627	50.704995	76.520666
70.585025	60.083690	76.525671
70.163087	51.348304	76.530676
69.657170	52.321435	76.535681
68.745573	60.116845	76.540686
68.017486	50.081269	76.545690
67.261161	53.211801	76.550695
66.723867	51.939271	76.555700
66.688916	49.981447	76.560705
65.280057	53.836838	76.565710
64.837206	48.945979	76.570714
64.175369	55.447333	76.575719
63.573023	52.515536	76.580724
63.290894	56.147366	76.585729
62.125605	56.075853	76.590734
61.785856	48.540118	76.595738
61.152050	48.933635	76.600743
59.782833	51.557835	76.605748
59.311272	50.480866	76.610753
58.553150	50.787151	76.615758
58.073078	51.401401	76.620762
57.499862	58.965126	76.625767
56.870539	54.032030	76.630772
55.965749	53.697977	76.635777
55.246933	53.394799	76.640782
54.799318	49.677052	76.645786
54.091733	62.785830	76.650791
53.688015	48.762529	76.655796
53.786583	47.212050	76.660801
52.316218	53.954252	76.665806
51.744515	47.886747	76.670810
51.252857	56.157626	76.675815
49.780561	59.293681	76.680820
49.134063	62.334339	76.685825
48.633567	67.514962	76.690830
48.595704	51.722201	76.695834
47.723512	52.656689	76.700839
47.404582	63.092160	76.705844
46.347775	55.563315	76.710849
44.964508	66.204157	76.715854
44.938836	57.558324	76.720858
44.482561	49.231042	76.725863
43.528292	59.921085	76.730868
42.730463	53.091084	76.735873
41.937705	61.958685	76.740878
41.478556	61.200489	76.745882
41.024930	60.721988	76.750887
40.641566	64.417753	76.755892
40.275132	59.593130	76.760897
39.063947	57.413442	76.765902
38.565781	57.986983	76.770906
37.917410	54.963219	76.775911
36.813136	60.366165	76.780916
36.234486	52.895863	76.785921
35.413316	58.908649	76.790926
35.372525	57.163786	76.795930
34.590804	61.847132	76.800935
33.749867	58.277341	76.805940
33.037725	56.006964	76.810945
32.032589	66.378123	76.815950
31.909502	56.288560	76.820954
31.695473	50.949948	76.825959
30.336849	53.728251	76.830964
29.472113	50.389107	76.835969
28.959924	50.799670	76.840974
28.586638	47.590597	76.845978
27.982449	46.039824	76.850983
26.987713	58.308546	76.855988
26.090861	55.628946	76.860993
25.693480	54.198626	76.865998
25.112376	49.383579	76.871002
24.754128	53.497771	76.876007
24.020956	49.849512	76.881012
23.266490	48.054522	76.886017
22.227473	47.894269	76.891022
22.104458	50.030887	76.896026
21.628659	49.287390	76.901031
20.407795	45.481974	76.906036
19.504973	39.734917	76.911041
18.950691	47.459197	76.916046
18.618683	50.255291	76.921050
18.096319	44.841265	76.926055
17.269963	49.397271	76.931060
16.741182	47.309394	76.936065
15.730533	49.207829	76.941070
15.810455	47.542134	76.946074
14.513982	50.466485	76.951079
13.419115	47.605327	76.956084
12.964999	38.856924	76.961089
12.569350	43.331583	76.966094
12.155925	36.962234	76.971098
11.579731	52.630676	76.976103
10.411038	49.124587	76.981108
9.839991	46.276639	76.986113
8.980755	53.329307	76.991118
9.145601	52.485049	76.996122
8.346685	54.907674	77.001127
7.067364	51.458445	77.006132
6.458494	39.987017	77.011137
6.017255	50.012423	77.016142
5.779125	42.983453	77.021147
4.849724	50.732579	77.026151
3.674027	50.703916	77.031156
3.478527	45.518832	77.036161