Tue Jun 08 17:05:23 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-1.299358	98.172908	0.000000
-1.309401	92.766290	0.005005
-2.083187	56.006361	0.010010
-3.396564	10.672758	0.015014
-7.718520	-8.760637	0.020019
-12.759094	-11.267567	0.025024
-18.126897	-14.449388	0.030029
-23.065969	-16.731752	0.035034
-26.998162	-12.088679	0.040038
-30.792001	-6.873311	0.045043
-34.449367	-11.215970	0.050048
-37.959265	-13.611937	0.055053
-41.547967	-21.696768	0.060058
-45.024522	-14.836174	0.065062
-49.526941	-8.196353	0.070067
-52.904642	-14.954818	0.075072
-56.603409	-10.765008	0.080077
-60.215536	-12.382031	0.085082
-63.944270	-7.533042	0.090086
-67.847780	-5.554411	0.095091
-71.589860	-14.328135	0.100096
-75.607246	-9.219653	0.105101
-78.938094	-16.399787	0.110106
-82.902711	-13.834783	0.115110
-87.142191	-10.502297	0.120115
-90.399507	-17.197695	0.125120
-94.536215	-13.090642	0.130125
-97.927741	-13.242407	0.135130
-101.810601	-5.851470	0.140134
-105.368176	-4.500118	0.145139
-109.153062	-14.709132	0.150144
-113.220183	-6.689392	0.155149
-117.014690	-7.819599	0.160154
-120.623717	-11.245668	0.165158
-124.597452	-10.048710	0.170163
-127.994759	-16.862562	0.175168
-131.630777	-10.886340	0.180173
-135.331091	-19.064048	0.185178
-139.082381	-23.168285	0.190182
-143.373468	-24.981019	0.195187
-146.739061	-28.719580	0.200192
-150.919580	-17.930425	0.205197
-154.919134	-16.866372	0.210202
-158.765930	-7.926024	0.215206
-162.637993	-8.887771	0.220211
-165.857564	-11.559989	0.225216
-169.630041	-14.864439	0.230221
-173.320962	-16.349444	0.235226
-177.023404	-20.254409	0.240230
-180.643482	-11.255830	0.245235
-184.159087	-14.545509	0.250240
-188.586514	-7.703304	0.255245
-192.228910	-20.345588	0.260250
-196.022363	-19.937723	0.265254
-200.055172	-13.913532	0.270259
-203.338683	-20.364757	0.275264
-207.236271	-17.429066	0.280269
-210.751389	-13.909275	0.285274
-214.564304	-17.455416	0.290278
-218.598758	-14.353751	0.295283
-222.143014	-19.427702	0.300288
-226.074852	-10.645603	0.305293
-229.918691	-9.678448	0.310298
-233.613935	-19.589711	0.315302
-237.260319	-17.694115	0.320307
-240.775656	-20.900509	0.325312
-244.526446	-15.375408	0.330317
-248.828290	-16.383357	0.335322
-252.005479	-19.562482	0.340326
-256.109743	-10.243189	0.345331
-259.919754	-11.215493	0.350336
-263.634017	-5.073394	0.355341
-267.287925	-13.348148	0.360346
-271.099168	-8.238153	0.365350
-274.925359	-13.603944	0.370355
-278.091345	-25.824602	0.375360
-282.767836	-10.588730	0.380365
-286.131974	-12.843721	0.385370
-289.714138	-16.061901	0.390374
-294.127018	-11.764024	0.395379
-297.313685	-12.089321	0.400384
-301.231742	-7.494627	0.405389
-305.204336	-21.798730	0.410394
-308.699545	-11.812208	0.415398
-312.483349	-5.310799	0.420403
-316.108611	-17.353580	0.425408
-320.290715	-6.195745	0.430413
-324.105893	-11.226299	0.435418
-327.441595	-10.572393	0.440422
-331.629588	-7.331010	0.445427
-334.925939	-14.611978	0.450432
-338.882571	-9.072018	0.455437
-342.329606	-12.535950	0.460442
-346.032461	-14.719372	0.465446
-349.987284	-10.248587	0.470451
-353.974972	-21.363956	0.475456
-357.791157	-19.565445	0.480461
-361.567456	-18.623185	0.485466
-365.057049	-18.267697	0.490470
-368.865223	-12.248348	0.495475
-372.554704	-15.281877	0.500480
-376.881636	-10.438968	0.505485
-380.231040	-8.223571	0.510490
-384.059740	-11.811457	0.515494
-387.949355	-11.487981	0.520499
-391.319180	-15.388640	0.525504
-394.968237	-8.630435	0.530509
-399.064589	-16.457352	0.535514
-402.762359	-18.715408	0.540518
-406.756393	-7.785543	0.545523
-410.324206	-24.254877	0.550528
-414.040076	-9.577998	0.555533
-417.716323	-14.876229	0.560538
-421.747307	-18.674097	0.565542
-425.536470	-13.970371	0.570547
-429.046513	-19.928243	0.575552
-433.086991	-12.764990	0.580557
-437.047021	-7.867741	0.585562
-440.336250	-20.911010	0.590566
-443.937897	-8.997325	0.595571
-447.524708	-16.251261	0.600576
-451.797960	-6.146158	0.605581
-455.570811	-17.153032	0.610586
-459.468131	-21.509018	0.615590
-463.592395	-5.433844	0.620595
-466.320735	-12.162858	0.625600
-470.167265	-11.332001	0.630605
-474.100335	-14.987551	0.635610
-478.008420	-12.283498	0.640614
-481.462085	-4.598818	0.645619
-485.268070	-19.965454	0.650624
-489.409155	-16.413448	0.655629
-493.154807	-13.382803	0.660634
-496.539546	-15.134788	0.665638
-500.693966	-11.076836	0.670643
-504.340893	-19.937131	0.675648
-508.693430	-18.448282	0.680653
-512.056523	-13.566949	0.685658
-515.842624	-10.753539	0.690662
-519.099068	-11.107754	0.695667
-522.767840	-12.446275	0.700672
-527.067604	-9.735368	0.705677
-530.404649	-10.559657	0.710682
-534.675914	-16.889294	0.715686
-538.675727	-6.849190	0.720691
-541.974859	-17.199155	0.725696
-545.592104	-17.318166	0.730701
-549.455074	-17.567895	0.735706
-553.090885	-13.894516	0.740710
-557.418202	-10.399698	0.745715
-561.148024	-16.292907	0.750720
-565.003896	-14.943693	0.755725
-568.110553	-16.401915	0.760730
-571.561783	-13.119377	0.765734
-576.077860	-3.158013	0.770739
-579.252406	-8.371280	0.775744
-583.332675	-13.666349	0.780749
-587.162571	-11.326514	0.785754
-590.959630	-7.222044	0.790758
-594.972105	-5.332812	0.795763
-598.475016	-11.315447	0.800768
-602.280460	-3.053647	0.805773
-605.764342	-7.319404	0.810778
-609.506599	-14.764007	0.815782
-613.827392	-13.207087	0.820787
-617.221095	-14.608912	0.825792
-620.896197	-1.195631	0.830797
-624.703324	-14.824031	0.835802
-628.187286	-20.494517	0.840806
-632.436303	-13.046647	0.845811
-636.096599	-21.561918	0.850816
-639.632849	-21.993544	0.855821
-643.836399	-12.162327	0.860826
-647.271460	-12.515398	0.865830
-651.000195	-7.773309	0.870835
-654.584073	-14.368401	0.875840
-658.724727	-6.745299	0.880845
-662.520937	-14.871727	0.885850
-665.942732	-12.091106	0.890854
-670.353053	-10.815588	0.895859
-673.705025	-19.477282	0.900864
-677.310490	-8.577969	0.905869
-680.909900	-13.432475	0.910874
-684.953267	-9.321577	0.915878
-689.105113	-8.802845	0.920883
-692.222876	-17.377622	0.925888
-696.344231	-13.662643	0.930893
-700.024444	-7.422243	0.935898
-703.827556	-18.339607	0.940902
-707.471607	-12.419201	0.945907
-711.106938	-23.098920	0.950912
-714.970645	-10.392105	0.955917
-718.798177	-9.944002	0.960922
-722.481572	-20.456396	0.965926
-726.731187	-5.924523	0.970931
-729.785395	-15.015010	0.975936
-733.941663	-11.528066	0.980941
-737.487688	-13.146794	0.985946
-741.081222	-14.414759	0.990950
-745.217167	-6.854754	0.995955
-748.770604	-18.881423	1.000960
-752.790521	-5.084819	1.005965
-756.386793	-18.284699	1.010970
-759.664897	-20.505533	1.015974
-763.665872	-13.331020	1.020979
-767.533501	-17.709577	1.025984
-771.625065	-8.810821	1.030989
-775.335172	-12.786177	1.035994
-779.327715	-17.498520	1.040998
-782.795307	-8.331878	1.046003
-786.487528	-17.352283	1.051008
-790.336448	-8.788030	1.056013
-793.882419	-17.274229	1.061018
-797.450770	-18.195574	1.066022
-801.668687	-6.404400	1.071027
-805.419912	-10.497400	1.076032
-809.174085	-17.962660	1.081037
-812.769537	-7.286005	1.086042
-816.499255	-17.449727	1.091046
-820.558365	-4.266822	1.096051
-823.990774	-9.181049	1.101056
-827.662659	-7.147978	1.106061
-831.673644	-14.520194	1.111066
-835.204116	-13.283042	1.116070
-839.558439	-11.032962	1.121075
-843.059124	-15.474038	1.126080
-847.111763	-8.885409	1.131085
-850.493422	-14.015545	1.136090
-854.376558	-13.824205	1.141094
-858.117380	-12.753807	1.146099
-861.609226	-16.292112	1.151104
-865.561252	-2.777051	1.156109
-868.995854	-11.240859	1.161114
-872.482104	-16.857062	1.166118
-876.545763	-11.280912	1.171123
-880.460807	-9.610632	1.176128
-884.351993	-6.352985	1.181133
-888.231068	-13.980665	1.186138
-891.718093	-17.807907	1.191142
-895.905510	-8.465124	1.196147
-899.556576	-10.715767	1.201152
-903.321360	-3.334196	1.206157
-906.784833	-12.100489	1.211162
-910.444030	-11.862285	1.216166
-914.782821	-11.995272	1.221171
-918.020909	-14.045235	1.226176
-921.973039	-6.939361	1.231181
-925.704449	-13.038787	1.236186
-929.196358	-16.232445	1.241190
-933.110550	-11.101082	1.246195
-936.671880	-23.854446	1.251200
-941.025425	-7.916375	1.256205
-944.751351	-5.748806	1.261210
-948.374253	-11.458319	1.266214
-952.159897	-0.088564	1.271219
-955.438060	-4.958114	1.276224
-959.185334	-9.441621	1.281229
-963.374725	-5.670905	1.286234
-966.920682	-5.378678	1.291238
-971.050438	-7.915339	1.296243
-974.590892	-10.298187	1.301248
-978.517429	-7.441727	1.306253
-982.082913	-6.682355	1.311258
-985.635972	-14.124743	1.316262
-989.778146	-0.958622	1.321267
-993.544721	-11.951046	1.326272
-997.124937	-14.486508	1.331277
-1000.551918	-13.794318	1.336282
-1004.299868	-21.113233	1.341286
-1008.463176	-6.097826	1.346291
-1012.228223	-16.528428	1.351296
-1016.117891	-15.648243	1.356301
-1019.932920	-14.706665	1.361306
-1023.381514	-16.840393	1.366310
-1027.298209	-19.495676	1.371315
-1031.137883	-18.382501	1.376320
-1035.044000	-13.866601	1.381325
-1038.590891	-9.186996	1.386330
-1042.487760	-12.050917	1.391334
-1045.974137	-14.150116	1.396339
-1049.412689	-15.074589	1.401344
-1053.167095	-15.063055	1.406349
-1057.261228	-10.054625	1.411354
-1061.080938	-12.669297	1.416358
-1064.991603	-11.963081	1.421363
-1068.393304	-14.654254	1.426368
-1072.434919	-13.856868	1.431373
-1076.159064	-18.801699	1.436378
-1079.820495	-20.623725	1.441382
-1083.832587	-8.762267	1.446387
-1087.623445	-19.790286	1.451392
-1090.926258	-13.133631	1.456397
-1094.544293	-14.978489	1.461402
-1098.881858	-6.129573	1.466406
-1102.711503	-5.906145	1.471411
-1106.314942	-14.836891	1.476416
-1109.992712	-16.337558	1.481421
-1113.709495	-13.325957	1.486426
-1117.373876	-21.817969	1.491430
-1121.161671	-17.220083	1.496435
-1124.957799	-15.772882	1.501440
-1128.770096	-9.735631	1.506445
-1132.707152	-7.636640	1.511450
-1136.432709	-19.500758	1.516454
-1140.285140	-13.964988	1.521459
-1143.544284	-19.382337	1.526464
-1147.296391	-22.137210	1.531469
-1151.148564	-17.876374	1.536474
-1155.513453	-22.933715	1.541478
-1159.310975	-13.078624	1.546483
-1162.723278	-20.279380	1.551488
-1166.837404	-26.005377	1.556493
-1170.195446	-26.761617	1.561498
-1173.527369	-20.234896	1.566502
-1177.558657	-6.354303	1.571507
-1181.137995	-19.406683	1.576512
-1185.038249	-19.961254	1.581517
-1189.080090	-10.331792	1.586522
-1192.666115	-14.142169	1.591526
-1196.657976	-11.903456	1.596531
-1200.498296	-23.525184	1.601536
-1203.859345	-21.221915	1.606541
-1207.774940	-19.015237	1.611546
-1211.025582	-16.832756	1.616550
-1215.101903	-13.448692	1.621555
-1219.067209	-10.551809	1.626560
-1222.769141	-17.388588	1.631565
-1226.975475	-14.331894	1.636570
-1230.496344	-23.401424	1.641574
-1234.302011	-17.010386	1.646579
-1237.840106	-20.403855	1.651584
-1241.466101	-14.486527	1.656589
-1245.234018	-17.220044	1.661594
-1248.993557	-8.671560	1.666598
-1253.082451	-8.326504	1.671603
-1256.720319	-16.012214	1.676608
-1260.799038	-12.352190	1.681613
-1263.784367	-15.765579	1.686618
-1267.470207	-24.149163	1.691622
-1271.828073	-11.932928	1.696627
-1275.402777	-20.921335	1.701632
-1278.967212	-15.156248	1.706637
-1283.207499	-9.948446	1.711642
-1287.364943	-24.257236	1.716646
-1290.888160	-16.030342	1.721651
-1294.283788	-19.851619	1.726656
-1297.981578	-13.847710	1.731661
-1301.792187	-23.008319	1.736666
-1305.432730	-19.588501	1.741670
-1309.410474	-7.865378	1.746675
-1313.036444	-20.229539	1.751680
-1316.832033	-20.471202	1.756685
-1320.606194	-15.548278	1.761690
-1324.279988	-22.119418	1.766694
-1328.104109	-6.058020	1.771699
-1331.789203	-16.539136	1.776704
-1335.691005	-14.687970	1.781709
-1339.764414	-7.180413	1.786714
-1343.123123	-17.736523	1.791718
-1346.731087	-18.114588	1.796723
-1350.404760	-13.806087	1.801728
-1354.128182	-12.781664	1.806733
-1358.387050	-12.352445	1.811738
-1362.342375	-15.164179	1.816742
-1366.236297	-9.846070	1.821747
-1369.838625	-6.868119	1.826752
-1373.128419	-14.798230	1.831757
-1377.076387	-15.188912	1.836762
-1380.404936	-16.268180	1.841766
-1384.508876	-6.542625	1.846771
-1388.075391	-13.378826	1.851776
-1392.097493	-13.013531	1.856781
-1396.089736	-17.084708	1.861786
-1399.648022	-16.310830	1.866790
-1403.456507	-16.492967	1.871795
-1406.903057	-15.814454	1.876800
-1410.542874	-15.006826	1.881805
-1414.825170	-9.227648	1.886810
-1418.236327	-16.712562	1.891814
-1422.369645	-7.705815	1.896819
-1426.193544	-15.480580	1.901824
-1429.721082	-17.422787	1.906829
-1433.251668	-16.854938	1.911834
-1436.879074	-15.219751	1.916838
-1441.079523	-9.514209	1.921843
-1444.579216	-10.608231	1.926848
-1448.690372	-21.462838	1.931853
-1452.398247	-14.220462	1.936858
-1455.797236	-18.937791	1.941862
-1460.054817	-8.788704	1.946867
-1463.878989	-17.654345	1.951872
-1467.337755	-7.309352	1.956877
-1471.462596	-10.835087	1.961882
-1474.746825	-19.618228	1.966886
-1478.590245	-11.489720	1.971891
-1481.806187	-12.095661	1.976896
-1485.952493	-18.408643	1.981901
-1489.892249	-9.612313	1.986906
-1493.310530	-13.104293	1.991910
-1497.333489	-12.237870	1.996915
-1501.471036	-15.890125	2.006912
-1502.253314	-14.392210	2.016909
-1499.584668	-13.244913	2.026906
-1496.902189	-12.650516	2.036902
-1494.721591	-10.845523	2.046899
-1492.866458	-11.361008	2.056896
-1490.973121	-23.962234	2.066893
-1489.531527	-14.755265	2.076890
-1487.372146	-13.390048	2.086886
-1485.157304	-20.683911	2.096883
-1483.089883	-17.842596	2.106880
-1481.268785	-9.179811	2.116877
-1479.546560	-16.916647	2.126874
-1478.143654	-18.866110	2.136870
-1476.066736	-13.430686	2.146867
-1473.841079	-16.532835	2.156864
-1471.870763	-10.019537	2.166861
-1470.136336	-16.701280	2.176858
-1468.400945	-10.512794	2.186854
-1466.420720	-13.507962	2.196851
-1464.549227	-12.253335	2.206848
-1462.235812	-18.383236	2.216845
-1460.687456	-14.463526	2.226842
-1459.027742	-19.979998	2.236838
-1457.087555	-19.359624	2.246835
-1455.146380	-21.155335	2.256832
-1452.982439	-23.139888	2.266829
-1450.976728	-18.049883	2.276826
-1449.262415	-19.350942	2.286822
-1447.496113	-13.240081	2.296819
-1445.926830	-13.473265	2.306816
-1443.691232	-15.748352	2.316813
-1441.475439	-15.311664	2.326810
-1439.831749	-15.644574	2.336806
-1438.382971	-16.947043	2.346803
-1436.409619	-16.604260	2.356800
-1434.386715	-16.266828	2.366797
-1432.400893	-8.671716	2.376794
-1430.655206	-15.877057	2.386790
-1428.777951	-13.186421	2.396787
-1426.596173	-19.088578	2.406784
-1424.929205	-11.220138	2.416781
-1422.947947	-11.476659	2.426778
-1421.020011	-11.989601	2.436774
-1419.402158	-16.104570	2.446771
-1417.577153	-17.359026	2.456768
-1415.565035	-17.177025	2.466765
-1413.896971	-13.976195	2.476762
-1411.742535	-17.259731	2.486758
-1409.494780	-14.980120	2.496755
-1407.803755	-22.942372	2.506752
-1406.084367	-17.248284	2.516749
-1404.448602	-18.704191	2.526746
-1402.310741	-13.538452	2.536742
-1400.363703	-12.092053	2.546739
-1398.662962	-18.412691	2.556736
-1396.593713	-14.119642	2.566733
-1394.871647	-19.617558	2.576730
-1393.204270	-17.277763	2.586726
-1390.912084	-8.464655	2.596723
-1389.445811	-17.484214	2.606720
-1387.371858	-21.094189	2.616717
-1385.454071	-25.623467	2.626714
-1383.546974	-20.918416	2.636710
-1381.279437	-22.894250	2.646707
-1379.740630	-21.140988	2.656704
-1377.905588	-22.932265	2.666701
-1376.430413	-24.588216	2.676698
-1374.267109	-22.425290	2.686694
-1372.178879	-22.246067	2.696691
-1370.367157	-13.383220	2.706688
-1368.385538	-18.266105	2.716685
-1366.794424	-20.515813	2.726682
-1365.126065	-17.000821	2.736678
-1363.171934	-17.990117	2.746675
-1360.869537	-17.958729	2.756672
-1359.089662	-22.997051	2.766669
-1357.144815	-18.079524	2.776666
-1355.185279	-20.115469	2.786662
-1353.445761	-19.261787	2.796659
-1351.711154	-16.665175	2.806656
-1349.939964	-17.617508	2.816653
-1347.601680	-24.278043	2.826650
-1345.975130	-20.103371	2.836646
-1344.121936	-21.779189	2.846643
-1342.223241	-18.240913	2.856640
-1340.786169	-21.481818	2.866637
-1338.746790	-19.166772	2.876634
-1336.319943	-19.154771	2.886630
-1334.939532	-16.955757	2.896627
-1332.753086	-19.112080	2.906624
-1330.944401	-19.614378	2.916621
-1329.085765	-17.186473	2.926618
-1327.188688	-13.792953	2.936614
-1325.297300	-10.337591	2.946611
-1323.528069	-16.475920	2.956608
-1321.596226	-20.480773	2.966605
-1319.559988	-17.813440	2.976602
-1318.060747	-12.497652	2.986598
-1315.881939	-18.964399	2.996595
-1313.910193	-17.428143	3.006592
-1312.103885	-21.965910	3.016589
-1310.485515	-17.904032	3.026586
-1308.303848	-17.095052	3.036582
-1306.399368	-21.049749	3.046579
-1304.776871	-21.882860	3.056576
-1303.112261	-23.176509	3.066573
-1301.029464	-18.788910	3.076570
-1298.934953	-24.153155	3.086566
-1297.350950	-19.689764	3.096563
-1295.169923	-24.645991	3.106560
-1293.410372	-28.987203	3.116557
-1291.870543	-24.339566	3.126554
-1289.825507	-24.255637	3.136550
-1287.653199	-20.621262	3.146547
-1286.044824	-20.776526	3.156544
-1283.913552	-26.174742	3.166541
-1282.195037	-24.166966	3.176538
-1280.371456	-25.383179	3.186534
-1278.656522	-25.850383	3.196531
-1276.507835	-25.027027	3.206528
-1274.265465	-23.207232	3.216525
-1272.797778	-21.005797	3.226522
-1271.259730	-19.091117	3.236518
-1268.842928	-23.021154	3.246515
-1267.106229	-19.361354	3.256512
-1265.268578	-26.043363	3.266509
-1263.570905	-28.761874	3.276506
-1261.762806	-21.163814	3.286502
-1259.466233	-28.274795	3.296499
-1257.750556	-27.305529	3.306496
-1255.828949	-19.395378	3.316493
-1254.030974	-16.698947	3.326490
-1252.174803	-14.295876	3.336486
-1250.385382	-16.720692	3.346483
-1248.289849	-25.195395	3.356480
-1246.499250	-15.016758	3.366477
-1244.679717	-19.044578	3.376474
-1242.791614	-19.660861	3.386470
-1241.010964	-16.597855	3.396467
-1238.846425	-22.807600	3.406464
-1236.967487	-16.438939	3.416461
-1235.342702	-15.234315	3.426458
-1233.649236	-20.655729	3.436454
-1231.439439	-19.524305	3.446451
-1229.407598	-18.991493	3.456448
-1227.647674	-22.507152	3.466445
-1226.029972	-18.706752	3.476442
-1223.783594	-19.996738	3.486438
-1222.008336	-19.593354	3.496435
-1220.173551	-12.887890	3.506432
-1218.382481	-21.737518	3.516429
-1216.777090	-24.932597	3.526426
-1214.757793	-22.946806	3.536422
-1212.808487	-21.213390	3.546419
-1210.640495	-11.393183	3.556416
-1208.971205	-14.183473	3.566413
-1206.804019	-12.615519	3.576410
-1205.612498	-12.292097	3.586406
-1203.455140	-10.412212	3.596403
-1201.454484	-9.543634	3.606400
-1199.305077	-11.773364	3.616397
-1197.715874	-6.714447	3.626394
-1196.155318	-11.083897	3.636390
-1193.880544	-9.880221	3.646387
-1191.980350	-13.279657	3.656384
-1190.174924	-13.800700	3.666381
-1188.592953	-9.113222	3.676378
-1186.343470	-10.508847	3.686374
-1184.335168	-11.035878	3.696371
-1182.638422	-14.258886	3.706368
-1180.911956	-12.491138	3.716365
-1179.183254	-12.172616	3.726362
-1177.083760	-14.760124	3.736358
-1175.271248	-9.845067	3.746355
-1173.201731	-13.430866	3.756352
-1171.312092	-17.671860	3.766349
-1169.716975	-26.256227	3.776346
-1167.772659	-15.511523	3.786342
-1166.001151	-17.421431	3.796339
-1164.139744	-23.346704	3.806336
-1162.106308	-20.459072	3.816333
-1160.119585	-15.867173	3.826330
-1158.154688	-17.023422	3.836326
-1156.398148	-21.256966	3.846323
-1154.352731	-21.726332	3.856320
-1152.531665	-20.471992	3.866317
-1150.793035	-21.365694	3.876314
-1149.373094	-14.252632	3.886310
-1146.995227	-27.486295	3.896307
-1144.848972	-24.812472	3.906304
-1142.960789	-26.670872	3.916301
-1141.636043	-20.782030	3.926298
-1140.002455	-27.655802	3.936294
-1137.818616	-23.181131	3.946291
-1135.652646	-22.165436	3.956288
-1133.856146	-21.598884	3.966285
-1131.962931	-23.882600	3.976282
-1130.139732	-14.652866	3.986278
-1128.406395	-23.411927	3.996275
-1126.671979	-14.664911	4.006272
-1124.252325	-18.085541	4.016269
-1122.543727	-19.530136	4.026266
-1120.710265	-19.001937	4.036262
-1118.981976	-21.873462	4.046259
-1116.916544	-21.061811	4.056256
-1115.197462	-24.577133	4.066253
-1113.433444	-26.701122	4.076250
-1111.595157	-23.135368	4.086246
-1109.513373	-27.523543	4.096243
-1107.230454	-27.598541	4.106240
-1105.511523	-26.590249	4.116237
-1103.913473	-26.544880	4.126234
-1102.304067	-27.434553	4.136230
-1100.244877	-19.076851	4.146227
-1098.387045	-17.818524	4.156224
-1096.339807	-20.269368	4.166221
-1094.412809	-22.425683	4.176218
-1092.629527	-21.219763	4.186214
-1090.599060	-20.773989	4.196211
-1088.852294	-29.494635	4.206208
-1086.985103	-20.873550	4.216205
-1085.306114	-26.892356	4.226202
-1083.243951	-19.529901	4.236198
-1081.366630	-22.974763	4.246195
-1079.448753	-22.833725	4.256192
-1077.299032	-24.071469	4.266189
-1075.841400	-23.071652	4.276186
-1074.076847	-30.465461	4.286182
-1072.059418	-27.761181	4.296179
-1070.105172	-33.487360	4.306176
-1067.984844	-35.574102	4.316173
-1066.545136	-29.278937	4.326170
-1064.456408	-34.721521	4.336166
-1062.639391	-29.007283	4.346163
-1060.929549	-32.641536	4.356160
-1058.482421	-29.057779	4.366157
-1057.048078	-30.124863	4.376154
-1055.471601	-28.228160	4.386150
-1053.164598	-29.237986	4.396147
-1051.178962	-30.558203	4.406144
-1049.527238	-27.857911	4.416141
-1047.436710	-25.183558	4.426138
-1045.715156	-24.013260	4.436134
-1043.703960	-23.766898	4.446131
-1042.065491	-33.377523	4.456128
-1039.895768	-31.992110	4.466125
-1037.937140	-31.669139	4.476122
-1036.295669	-27.574358	4.486118
-1034.680749	-24.342111	4.496115
-1032.980224	-31.904733	4.506112
-1030.938742	-27.588939	4.516109
-1028.899659	-23.743032	4.526106
-1026.768288	-32.193761	4.536102
-1025.049045	-25.601156	4.546099
-1023.026094	-30.671207	4.556096
-1021.468853	-27.504537	4.566093
-1019.443367	-23.598590	4.576090
-1017.411907	-26.793242	4.586086
-1015.601833	-25.390727	4.596083
-1013.614331	-27.895300	4.606080
-1011.676232	-17.031272	4.616077
-1010.270973	-26.648883	4.626074
-1008.567411	-18.986110	4.636070
-1006.390866	-25.672856	4.646067
-1004.203366	-28.514099	4.656064
-1002.527099	-24.030065	4.666061
-1000.615610	-22.701865	4.676058
-998.816002	-22.693827	4.686054
-996.925004	-23.725472	4.696051
-995.248049	-23.361235	4.706048
-993.144946	-25.306267	4.716045
-991.233243	-27.961830	4.726042
-989.357733	-27.074037	4.736038
-987.465861	-20.657673	4.746035
-985.808970	-33.426418	4.756032
-984.148665	-24.240970	4.766029
-981.910954	-23.962329	4.776026
-979.915114	-18.398496	4.786022
-978.209668	-21.723701	4.796019
-976.174651	-27.945870	4.806016
-974.043562	-21.866582	4.816013
-972.611912	-24.115254	4.826010
-970.998085	-25.933199	4.836006
-968.722009	-18.784852	4.846003
-966.522268	-18.689781	4.856000
-964.830781	-17.555389	4.865997
-963.165699	-25.811037	4.875994
-961.706718	-18.628327	4.885990
-959.347716	-20.545346	4.895987
-957.475986	-17.207367	4.905984
-955.876633	-26.206188	4.915981
-953.844633	-22.657806	4.925978
-951.757106	-28.583086	4.935974
-950.322271	-28.032224	4.945971
-947.928352	-29.033597	4.955968
-946.300218	-25.693713	4.965965
-944.497620	-23.899019	4.975962
-942.288057	-25.122467	4.985958
-940.605879	-26.090178	4.995955
-938.742403	-28.421271	5.005952
-936.901335	-21.325486	5.015949
-935.009663	-21.986511	5.025946
-933.150229	-20.011076	5.035942
-931.518392	-17.597405	5.045939
-929.525968	-19.328172	5.055936
-927.353819	-22.562351	5.065933
-925.377282	-20.559591	5.075930
-923.764958	-19.400131	5.085926
-921.846269	-21.537952	5.095923
-920.133832	-22.108919	5.105920
-918.164340	-18.550973	5.115917
-915.948563	-22.596101	5.125914
-914.566484	-23.292549	5.135910
-912.491271	-20.336476	5.145907
-910.481742	-18.931399	5.155904
-908.487368	-20.044381	5.165901
-906.859767	-20.411869	5.175898
-905.355041	-23.731046	5.185894
-903.383389	-19.988900	5.195891
-901.091167	-25.683716	5.205888
-899.108749	-23.821857	5.215885
-897.446048	-17.261770	5.225882
-895.562273	-18.352203	5.235878
-893.775609	-22.837435	5.245875
-891.910919	-21.425270	5.255872
-889.636255	-15.908461	5.265869
-888.395714	-21.296273	5.275866
-886.411358	-15.441519	5.285862
-884.218263	-14.463942	5.295859
-882.315991	-20.383479	5.305856
-880.807615	-22.196332	5.315853
-879.105521	-15.386505	5.325850
-876.696405	-15.202047	5.335846
-874.713900	-22.281468	5.345843
-872.969728	-20.747433	5.355840
-871.193174	-18.160578	5.365837
-869.486640	-16.971819	5.375834
-867.308464	-19.850128	5.385830
-865.686749	-14.515260	5.395827
-863.514509	-15.982037	5.405824
-861.717762	-16.079367	5.415821
-860.062313	-12.956756	5.425818
-857.905393	-14.710196	5.435814
-856.014261	-14.142775	5.445811
-854.345418	-17.189352	5.455808
-852.977241	-18.379385	5.465805
-850.730829	-20.936235	5.475802
-848.510952	-20.576606	5.485798
-846.581337	-19.123397	5.495795
-844.859139	-22.775109	5.505792
-842.884301	-19.577291	5.515789
-841.124033	-16.077848	5.525786
-839.633700	-16.151424	5.535782
-837.729225	-15.381565	5.545779
-835.206716	-19.839344	5.555776
-833.652247	-24.148349	5.565773
-831.798537	-21.987323	5.575770
-830.169177	-19.412729	5.585766
-828.025140	-17.333941	5.595763
-826.230202	-17.617881	5.605760
-824.366446	-22.256225	5.615757
-822.277165	-17.201177	5.625754
-820.541360	-18.750316	5.635750
-818.738708	-14.325041	5.645747
-816.707298	-18.179998	5.655744
-814.515115	-15.701608	5.665741
-813.146422	-16.856938	5.675738
-811.387027	-21.768636	5.685734
-809.461583	-10.469558	5.695731
-807.216253	-12.411252	5.705728
-805.544211	-21.158509	5.715725
-803.668870	-20.657121	5.725722
-801.721033	-22.403892	5.735718
-799.909637	-17.192452	5.745715
-798.122623	-20.011889	5.755712
-796.225884	-18.929257	5.765709
-794.197012	-12.778175	5.775706
-792.586502	-19.066132	5.785702
-790.248511	-20.932426	5.795699
-788.526334	-19.520653	5.805696
-786.780299	-20.075994	5.815693
-784.950092	-17.263553	5.825690
-782.747529	-17.428132	5.835686
-781.129290	-16.106804	5.845683
-779.277497	-12.068954	5.855680
-777.472858	-24.339357	5.865677
-775.722403	-18.328603	5.875674
-773.909531	-12.687807	5.885670
-771.615304	-16.481937	5.895667
-769.640761	-14.710353	5.905664
-767.893597	-20.506003	5.915661
-766.149481	-15.911387	5.925658
-764.269348	-20.719299	5.935654
-762.355483	-14.352437	5.945651
-760.533817	-18.623100	5.955648
-758.572162	-17.875271	5.965645
-756.518538	-17.562941	5.975642
-754.806232	-19.822170	5.985638
-753.299126	-13.169310	5.995635
-751.131294	-16.907353	6.005632
-749.038651	-20.659759	6.015629
-747.575119	-16.232371	6.025626
-745.582638	-14.386787	6.035622
-743.604521	-15.008027	6.045619
-741.511487	-14.100940	6.055616
-740.073135	-19.634118	6.065613
-738.038502	-16.703794	6.075610
-736.024596	-17.133961	6.085606
-734.224502	-19.576214	6.095603
-732.506971	-19.506158	6.105600
-730.211337	-17.226089	6.115597
-728.545955	-19.185193	6.125594
-726.720113	-16.771537	6.135590
-724.988046	-6.677422	6.145587
-722.763015	-13.499236	6.155584
-721.042376	-21.473473	6.165581
-719.397920	-14.580169	6.175578
-717.449747	-17.898328	6.185574
-715.421404	-17.792288	6.195571
-713.630252	-15.610591	6.205568
-711.654796	-12.902086	6.215565
-709.820064	-17.930620	6.225562
-707.986704	-17.974097	6.235558
-706.144325	-15.685786	6.245555
-704.320428	-18.894083	6.255552
-702.173770	-15.775874	6.265549
-700.153741	-20.994684	6.275546
-698.545763	-8.020686	6.285542
-696.794989	-15.287522	6.295539
-694.985440	-14.168934	6.305536
-693.217904	-19.947504	6.315533
-690.744984	-19.096102	6.325530
-689.322437	-21.420191	6.335526
-687.330063	-18.359678	6.345523
-685.572820	-17.682653	6.355520
-683.354260	-23.806574	6.365517
-681.503870	-20.467176	6.375514
-679.573825	-23.758494	6.385510
-677.871823	-13.043853	6.395507
-675.949090	-14.136532	6.405504
-674.357235	-16.626812	6.415501
-672.002560	-20.178725	6.425498
-670.391445	-13.463846	6.435494
-668.702396	-15.560967	6.445491
-666.709000	-21.341533	6.455488
-664.817737	-22.473861	6.465485
-663.001364	-20.628449	6.475482
-660.936762	-20.473276	6.485478
-659.226484	-16.258534	6.495475
-657.220299	-20.161657	6.505472
-655.378540	-18.641511	6.515469
-653.663130	-21.476665	6.525466
-651.746850	-20.996860	6.535462
-649.926701	-19.865449	6.545459
-647.770102	-23.721661	6.555456
-646.020075	-24.579969	6.565453
-644.308638	-20.292305	6.575450
-642.024452	-24.386985	6.585446
-640.652650	-19.164850	6.595443
-638.653274	-16.568704	6.605440
-636.622564	-21.155794	6.615437
-634.539212	-23.996379	6.625434
-632.879543	-24.802027	6.635430
-631.278440	-18.638713	6.645427
-629.109374	-20.252641	6.655424
-627.275529	-18.093250	6.665421
-625.343868	-16.815370	6.675418
-623.400116	-12.417379	6.685414
-621.329285	-12.972269	6.695411
-619.761051	-19.784876	6.705408
-617.979418	-20.158928	6.715405
-616.122588	-20.369223	6.725402
-614.078517	-19.225239	6.735398
-612.459387	-21.250269	6.745395
-610.495177	-15.347649	6.755392
-608.344508	-19.995229	6.765389
-606.589379	-16.776193	6.775386
-604.965815	-13.905684	6.785382
-602.900139	-16.212057	6.795379
-600.957715	-18.353817	6.805376
-599.067174	-16.628601	6.815373
-597.220585	-16.661656	6.825370
-595.368497	-20.203961	6.835366
-593.770555	-22.767977	6.845363
-591.473148	-17.091674	6.855360
-589.573129	-19.017875	6.865357
-587.827288	-16.129215	6.875354
-586.162693	-22.101129	6.885350
-584.067505	-10.606173	6.895347
-581.932536	-11.406807	6.905344
-580.216197	-19.946606	6.915341
-578.818872	-23.543268	6.925338
-576.842872	-20.206800	6.935334
-574.589895	-17.173163	6.945331
-572.837471	-11.237345	6.955328
-570.683925	-15.997643	6.965325
-569.055883	-15.230424	6.975322
-567.364057	-19.032146	6.985318
-565.391508	-21.768322	6.995315
-563.384757	-20.355094	7.005312
-561.854721	-14.820195	7.015309
-559.835498	-13.382625	7.025306
-557.892271	-14.707598	7.035302
-555.949525	-14.311729	7.045299
-554.026037	-18.265436	7.055296
-552.077567	-20.402680	7.065293
-550.343244	-23.444181	7.075290
-548.579647	-15.194320	7.085286
-546.822023	-21.840214	7.095283
-544.634748	-16.146172	7.105280
-542.607222	-13.867423	7.115277
-540.702235	-19.608267	7.125274
-539.166971	-21.041871	7.135270
-537.158296	-18.233856	7.145267
-535.355810	-18.826449	7.155264
-533.365112	-22.277901	7.165261
-531.908525	-19.810683	7.175258
-529.745947	-14.125436	7.185254
-527.569257	-11.556892	7.195251
-525.906153	-18.843804	7.205248
-524.217796	-22.804975	7.215245
-522.219023	-14.955096	7.225242
-520.322902	-15.224260	7.235238
-518.378877	-17.067874	7.245235
-516.608352	-18.486109	7.255232
-514.633280	-27.340603	7.265229
-512.725830	-20.668597	7.275226
-510.938503	-16.759862	7.285222
-509.209625	-19.544317	7.295219
-507.011685	-12.320234	7.305216
-504.957447	-12.099581	7.315213
-503.339341	-8.423043	7.325210
-501.720846	-10.747499	7.335206
-499.884090	-13.768224	7.345203
-497.655232	-14.196036	7.355200
-495.586046	-15.345382	7.365197
-494.042587	-17.701620	7.375194
-492.208219	-18.256982	7.385190
-490.845834	-11.616332	7.395187
-488.399055	-12.043193	7.405184
-486.243456	-17.320746	7.415181
-484.382076	-16.783231	7.425178
-482.865591	-15.847844	7.435174
-480.804575	-11.060855	7.445171
-479.252143	-13.696069	7.455168
-477.323921	-9.745885	7.465165
-475.343854	-7.243963	7.475162
-473.340501	-11.847241	7.485158
-471.507768	-9.584439	7.495155
-469.407749	-18.589197	7.505152
-467.902223	-20.033089	7.515149
-465.673157	-19.816327	7.525146
-463.940893	-19.031775	7.535142
-462.289995	-19.668680	7.545139
-460.120707	-16.397327	7.555136
-458.370609	-10.245269	7.565133
-456.686045	-13.515331	7.575130
-454.478572	-19.375225	7.585126
-452.823048	-16.647278	7.595123
-451.300405	-20.773651	7.605120
-449.127092	-18.270489	7.615117
-446.879505	-13.753805	7.625114
-445.256621	-14.872801	7.635110
-443.499853	-11.555961	7.645107
-441.362360	-7.404137	7.655104
-439.487580	-15.224123	7.665101
-437.674590	-17.355467	7.675098
-436.018904	-11.422354	7.685094
-433.774604	-15.415639	7.695091
-431.907872	-9.635318	7.705088
-430.390107	-8.325864	7.715085
-428.359785	-2.443578	7.725082
-426.305568	-7.457103	7.735078
-424.925593	-2.987587	7.745075
-422.981967	-6.400490	7.755072
-420.782276	-10.362009	7.765069
-418.921485	-6.878832	7.775066
-417.102836	-9.890886	7.785062
-415.048469	-8.207129	7.795059
-413.230796	-12.558395	7.805056
-411.438731	-8.790728	7.815053
-409.757743	-9.772660	7.825050
-407.662533	-13.850621	7.835046
-405.800153	-12.555618	7.845043
-404.253859	-16.044998	7.855040
-401.971020	-12.527509	7.865037
-399.876318	-12.490409	7.875034
-398.307325	-15.095634	7.885030
-396.844476	-8.189603	7.895027
-394.710181	-14.614328	7.905024
-392.597862	-8.818021	7.915021
-390.703715	-8.691577	7.925018
-389.094390	-15.325815	7.935014
-387.277117	-14.488629	7.945011
-384.948693	-13.459316	7.955008
-383.282256	-14.072773	7.965005
-381.472063	-4.334931	7.975002
-379.666568	-11.126917	7.984998
-377.563749	-11.131510	7.994995
-375.737100	-10.874126	8.004992
-373.892924	-11.863883	8.014989
-372.021972	-13.074414	8.024986
-370.064611	-10.459074	8.034982
-368.503442	-13.273202	8.044979
-366.789731	-12.309163	8.054976
-364.356588	-9.196051	8.064973
-362.558909	-14.590001	8.074970
-361.003473	-12.453083	8.084966
-358.787138	-10.652830	8.094963
-357.013657	-20.415673	8.104960
-355.089207	-12.156553	8.114957
-353.451408	-9.898201	8.124954
-351.163614	-14.448652	8.134950
-349.576493	-18.557205	8.144947
-347.747288	-14.035094	8.154944
-345.545133	-13.848829	8.164941
-343.496316	-12.681422	8.174938
-342.314788	-7.674729	8.184934
-340.678144	-2.839373	8.194931
-338.452751	-11.798406	8.204928
-336.348888	-14.529744	8.214925
-334.555065	-13.792850	8.224922
-332.689507	-8.415003	8.234918
-330.554208	-5.536521	8.244915
-329.082606	-12.284654	8.254912
-326.983158	-10.390824	8.264909
-325.100425	-7.863441	8.274906
-323.248555	-6.393495	8.284902
-321.511115	-5.320081	8.294899
-319.357583	-12.411246	8.304896
-317.669858	-10.854256	8.314893
-315.833716	-5.916366	8.324890
-313.960276	-7.686925	8.334886
-312.006201	-11.401938	8.344883
-310.358350	-6.937624	8.354880
-307.922049	-8.181473	8.364877
-306.464522	-7.392416	8.374874
-304.500014	-1.494429	8.384870
-302.673244	-4.709394	8.394867
-300.840018	-2.152561	8.404864
-299.028389	-5.095785	8.414861
-296.958953	-1.985458	8.424858
-295.291268	-7.504110	8.434854
-293.228431	-2.969876	8.444851
-291.353835	-3.872733	8.454848
-289.230108	-3.322432	8.464845
-287.553874	-3.590536	8.474842
-285.954271	-4.261657	8.484838
-283.914744	-1.535481	8.494835
-282.043137	-1.116222	8.504832
-280.131014	-4.744590	8.514829
-277.914148	-7.109951	8.524826
-276.431965	-8.709049	8.534822
-274.421941	-2.090473	8.544819
-272.715557	-5.716353	8.554816
-270.759747	-6.859194	8.564813
-269.056729	-5.168852	8.574810
-266.799826	-7.303551	8.584807
-265.406455	-8.192625	8.594803
-263.146575	-7.560142	8.604800
-261.075266	-1.021233	8.614797
-259.840829	-17.192488	8.624794
-257.839017	-10.642451	8.634791
-255.618707	-9.300881	8.644787
-253.800604	-5.794894	8.654784
-251.823764	-13.496765	8.664781
-250.162833	-9.392734	8.674778
-248.112972	-10.305872	8.684775
-246.409257	-6.126182	8.694771
-244.437809	-6.008191	8.704768
-242.620683	-12.050823	8.714765
-240.773940	-8.336327	8.724762
-239.051027	-7.674574	8.734759
-237.000517	-4.724986	8.744755
-234.923818	-8.912337	8.754752
-232.878163	-17.106979	8.764749
-230.943111	-9.004535	8.774746
-229.506489	-15.732808	8.784743
-227.526575	-14.055163	8.794739
-225.767328	-16.678341	8.804736
-223.751556	-18.983102	8.814733
-222.005668	-14.278282	8.824730
-220.138451	-7.937922	8.834727
-218.048211	-17.439673	8.844723
-216.312135	-13.151700	8.854720
-214.724979	-12.047331	8.864717
-212.781295	-8.863228	8.874714
-210.578187	-9.235499	8.884711
-208.648729	-12.450649	8.894707
-206.927328	-12.529653	8.904704
-205.125599	-9.532246	8.914701
-203.284763	-13.708376	8.924698
-201.292854	-17.732173	8.934695
-199.445105	-19.347702	8.944691
-197.721602	-15.584388	8.954688
-195.863427	-17.081954	8.964685
-193.591596	-19.546019	8.974682
-191.667121	-14.121301	8.984679
-190.060833	-11.864595	8.994675
-188.219411	-13.001221	9.004672
-186.455972	-17.037602	9.014669
-184.732697	-22.659414	9.024666
-182.533046	-15.965424	9.034663
-180.386891	-12.104644	9.044659
-178.820980	-13.702262	9.054656
-177.052193	-25.215049	9.064653
-174.862926	-23.780773	9.074650
-173.102613	-16.626097	9.084647
-171.338028	-19.440268	9.094643
-169.492038	-21.904801	9.104640
-167.405467	-16.902296	9.114637
-165.804673	-20.072920	9.124634
-163.861028	-23.514966	9.134631
-162.183438	-19.163982	9.144627
-160.114407	-10.517345	9.154624
-158.060871	-20.006850	9.164621
-156.150225	-19.614390	9.174618
-154.065851	-14.558936	9.184615
-152.686052	-21.206306	9.194611
-150.920353	-14.495974	9.204608
-148.913338	-23.820990	9.214605
-147.002820	-23.240381	9.224602
-145.092554	-20.642551	9.234599
-143.198812	-22.615316	9.244595
-141.387716	-19.014020	9.254592
-139.493866	-27.335933	9.264589
-137.340515	-22.985114	9.274586
-135.529850	-15.111859	9.284583
-133.742687	-16.780998	9.294579
-131.887260	-17.869415	9.304576
-130.128035	-12.881892	9.314573
-128.264552	-11.215456	9.324570
-125.957841	-10.051070	9.334567
-124.427807	-12.455081	9.344563
-122.760686	-11.363206	9.354560
-120.451199	-16.055597	9.364557
-118.341512	-16.005521	9.374554
-117.076495	-15.109879	9.384551
-115.115734	-14.804248	9.394547
-113.279211	-14.186432	9.404544
-111.134273	-20.784389	9.414541
-109.067202	-16.562221	9.424538
-107.749063	-15.768561	9.434535
-105.957700	-11.825559	9.444531
-103.843614	-8.236285	9.454528
-102.036611	-14.947813	9.464525
-99.367806	-9.650688	9.474522
-98.359168	-9.021320	9.484519
-96.506648	-12.175017	9.494515
-94.504026	-8.594684	9.504512
-92.612091	-12.912330	9.514509
-90.642263	-10.856647	9.524506
-88.678516	-9.970154	9.534503
-86.910925	-4.323637	9.544499
-85.167069	-11.087173	9.554496
-82.962016	-11.435608	9.564493
-81.037877	-11.947707	9.574490
-79.439774	-8.376648	9.584487
-77.632504	-1.962703	9.594483
-75.471152	-9.196205	9.604480
-73.693843	-8.289987	9.614477
-71.742075	-18.770998	9.624474
-69.996220	-12.784026	9.634471
-68.269513	-9.651968	9.644467
-66.299861	-12.036494	9.654464
-64.371852	-7.710226	9.664461
-62.362377	-13.141974	9.674458
-60.619144	-14.737947	9.684455
-58.773162	-2.560480	9.694451
-56.775242	-8.499679	9.704448
-54.928145	-8.689498	9.714445
-53.051602	-10.183834	9.724442
-51.272139	-11.068305	9.734439
-49.472138	-5.052269	9.744435
-47.437884	-7.048696	9.754432
-45.644381	-7.316664	9.764429
-43.706156	-11.545006	9.774426
-41.921970	-11.424064	9.784423
-39.864445	-9.267596	9.794419
-38.276596	-7.214764	9.804416
-36.304166	-5.911597	9.814413
-34.245835	-8.563068	9.824410
-32.357488	-8.845317	9.834407
-30.675373	-6.992816	9.844403
-28.865197	-7.088555	9.854400
-26.775659	-7.831738	9.864397
-25.082544	-13.745138	9.874394
-23.249130	-7.917806	9.884391
-21.185434	-6.437812	9.894387
-19.078940	-10.123515	9.904384
-17.448149	-12.558997	9.914381
-15.490655	-7.504242	9.924378
-13.424812	-8.013340	9.934375
-12.198882	-10.855242	9.944371
-9.921376	-11.978831	9.954368
-7.649077	-8.053432	9.964365
-6.284050	-11.223104	9.974362
-4.957899	6.686821	9.984359
-3.871618	34.821059	9.994355
-2.464780	87.962361	10.004352
-1.019770	162.975109	10.014349
0.000000	216.314867	10.019354
0.611510	260.743983	10.024359
1.508185	300.041145	10.029363
1.760024	323.497179	10.034368
2.388723	359.347174	10.039373
2.839210	384.170100	10.044378
3.288647	404.500923	10.049383
3.007537	421.137311	10.054387
3.018737	447.120352	10.059392
2.767668	455.874945	10.064397
3.219691	471.166780	10.069402
3.707258	480.968647	10.074407
3.664841	498.509947	10.079411
4.135732	497.867933	10.084416
4.286662	511.197554	10.089421
4.327541	520.237641	10.094426
4.520561	521.520973	10.099431
4.270341	540.194888	10.104435
4.697042	533.646292	10.109440
4.591124	523.769525	10.114445
4.419631	516.203276	10.119450
4.387638	526.758970	10.124455
4.624337	533.606348	10.129459
4.789196	535.439624	10.134464
4.576833	545.918103	10.139469
4.659070	543.380944	10.144474
4.859881	554.799871	10.149479
4.877705	552.810976	10.154483
5.099696	551.196405	10.159488
4.820562	557.147399	10.164493
4.912085	555.754138	10.169498
4.699444	556.085084	10.174503
4.819399	565.581362	10.179507
5.053410	555.203015	10.184512
5.117759	572.882404	10.189517
5.372735	568.053057	10.194522
5.571678	561.805204	10.199527
5.370468	568.995305	10.204531
5.635518	565.717871	10.209536
5.222022	577.949491	10.214541
5.440500	570.128067	10.219546
5.481288	574.662806	10.224551
5.449552	577.462137	10.229555
5.644558	574.136713	10.234560
5.504819	586.356532	10.239565
5.494191	584.399353	10.244570
5.421033	576.452276	10.249575
5.186157	581.004678	10.254579
5.510168	579.994699	10.259584
5.363536	585.043536	10.264589
5.621315	614.723026	10.269594
5.886498	625.817950	10.274599
5.834715	621.516435	10.279603
6.184668	619.317036	10.284608
5.823702	627.863205	10.289613
6.152591	625.069800	10.294618
6.022414	623.442184	10.299623
5.947830	631.909254	10.304627
6.252923	625.613965	10.309632
6.106615	634.816473	10.314637
6.443562	631.504199	10.319642
6.247332	632.749678	10.324647
6.007488	634.096580	10.329651
6.244784	630.433901	10.334656
5.966799	642.968777	10.339661
6.240740	650.564145	10.344666
6.640895	661.502534	10.349671
6.721970	666.332754	10.354675
6.964874	665.705747	10.359680
6.791069	665.962538	10.364685
6.873691	658.839742	10.369690
6.422021	646.110275	10.374695
6.609486	670.386269	10.379699
7.026085	667.141644	10.384704
7.015742	683.327684	10.389709
6.929227	675.440477	10.394714
6.959972	682.220209	10.399719
6.463271	688.875648	10.404723
6.625882	682.107803	10.409728
6.543111	684.242102	10.414733
6.819165	680.789867	10.419738
6.893476	688.020806	10.424743
6.948169	703.036398	10.429747
7.519330	706.626835	10.434752
7.370698	713.103001	10.439757
7.789340	719.736506	10.444762
7.657608	713.417002	10.449767
7.440618	705.438075	10.454771
7.608167	693.591588	10.459776
7.378672	702.156308	10.464781
7.644962	705.493497	10.469786
7.825612	721.200390	10.474791
7.693021	720.987098	10.479795
8.063200	711.849223	10.484800
7.487211	710.195407	10.489805
7.823775	713.394236	10.494810
7.898448	725.362274	10.499815
8.110647	722.095449	10.504819
8.254758	720.778813	10.509824
7.933813	718.646670	10.514829
7.818449	705.624627	10.519834
8.103434	713.946012	10.524839
7.952222	729.775340	10.529843
8.283844	733.256067	10.534848
8.048120	732.681123	10.539853
7.833129	735.924790	10.544858
7.871266	743.196298	10.549863
8.272458	737.195140	10.554867
8.771877	739.311729	10.559872
8.432317	741.041257	10.564877
8.221399	740.515348	10.569882
8.045254	739.510591	10.574887
7.975831	743.198239	10.579891
8.437766	761.751497	10.584896
8.463872	774.599070	10.589901
8.474379	776.650678	10.594906
8.874338	780.529036	10.599911
8.610971	775.873762	10.604915
8.770033	777.848190	10.609920
8.498796	779.351669	10.614925
8.719750	778.674738	10.619930
8.726872	775.606482	10.624935
8.480630	782.799665	10.629939
8.923846	797.365843	10.634944
8.847022	811.146475	10.639949
9.259162	810.821625	10.644954
9.070869	818.773825	10.649959
9.073524	819.110493	10.654963
9.584422	815.688619	10.659968
9.107722	817.171278	10.664973
9.235769	819.535893	10.669978
9.493862	814.957776	10.674983
9.147480	817.251369	10.679987
9.377171	812.307074	10.684992
9.722492	825.623765	10.689997
9.712145	819.716427	10.695002
9.552221	820.717672	10.700007
9.431682	831.227571	10.705011
9.719324	821.435503	10.710016
9.635414	822.250033	10.715021
9.691863	824.677056	10.720026
9.829735	823.207141	10.725031
9.605568	826.417663	10.730035
9.761253	813.333268	10.735040
9.738950	834.188031	10.740045
9.939223	848.513283	10.745050
10.483907	841.949857	10.750055
10.187452	844.345024	10.755059
10.086459	828.121505	10.760064
9.931492	834.584202	10.765069
10.120984	842.182696	10.770074
10.630736	854.916620	10.775079
10.151528	862.115442	10.780083
10.407357	852.321704	10.785088
10.375301	863.131844	10.790093
10.255665	864.905782	10.795098
10.734197	868.089775	10.800103
10.627118	863.810701	10.805107
10.805433	853.273155	10.810112
10.955753	858.087220	10.815117
10.810562	852.778509	10.820122
10.740874	838.449854	10.825127
10.600658	840.818232	10.830131
10.810465	850.148885	10.835136
11.069181	864.328738	10.840141
10.933636	854.494341	10.845146
10.803521	851.646177	10.850151
10.749365	869.356089	10.855155
10.966567	859.474234	10.860160
10.861126	867.446200	10.865165
10.769988	865.920022	10.870170
10.784517	863.158766	10.875175
10.588354	870.540374	10.880179
10.754309	869.441031	10.885184
11.042617	872.896849	10.890189
11.795653	879.281248	10.895194
11.914259	877.857263	10.900199
11.467797	870.509301	10.905203
11.571611	856.585482	10.910208
11.515648	865.661320	10.915213
11.471114	857.580904	10.920218
11.777921	860.234609	10.925223
11.687533	855.649125	10.930227
11.691725	852.055178	10.935232
11.853555	858.488831	10.940237
11.688536	850.230526	10.945242
11.520449	857.511000	10.950247
11.758455	863.514756	10.955251
11.820188	871.389377	10.960256
11.597135	884.278971	10.965261
11.875142	887.329194	10.970266
12.181550	892.350584	10.975271
12.067543	897.285376	10.980275
12.120888	891.924848	10.985280
12.116852	902.559292	10.990285
12.332239	905.841306	10.995290
12.544798	899.953744	11.000295
12.082299	904.891054	11.005299
12.430612	897.188521	11.010304
12.306745	899.605419	11.015309
12.280859	903.469192	11.020314
12.344109	898.955641	11.025319
12.333536	901.878900	11.030323
12.604598	896.715909	11.035328
12.649237	909.190943	11.040333
12.835177	899.115083	11.045338
12.862086	895.853938	11.050343
12.632648	915.853412	11.055347
12.864418	902.800896	11.060352
12.755134	904.102540	11.065357
12.391293	906.253482	11.070362
12.475422	912.065748	11.075367
12.195353	920.057024	11.080371
12.754875	922.571490	11.085376
12.991032	932.820563	11.090381
12.927714	930.619349	11.095386
12.784537	939.232160	11.100391
12.700876	937.905218	11.105395
12.982677	936.811666	11.110400
12.842504	937.830453	11.115405
13.055592	948.760462	11.120410
13.533595	954.678894	11.125415
13.457135	962.460414	11.130419
13.908232	961.102966	11.135424
13.643246	958.247513	11.140429
13.389117	946.790502	11.145434
13.785362	944.780884	11.150439
13.408265	942.670968	11.155443
13.715185	954.769097	11.160448
13.853174	963.216477	11.165453
13.855264	957.201166	11.170458
13.763071	942.216277	11.175463
13.688877	945.922948	11.180467
13.775823	957.076695	11.185472
13.888036	963.739950	11.190477
14.061148	966.857122	11.195482
14.455424	966.392044	11.200487
14.041112	969.257040	11.205491
13.749115	953.837057	11.210496
14.126765	964.789388	11.215501
13.813403	973.732186	11.220506
14.102953	967.626531	11.225511
13.932636	977.481907	11.230515
14.093505	963.914919	11.235520
14.070654	982.236958	11.240525
14.146541	976.675958	11.245530
14.157092	973.055630	11.250535
13.993441	990.427611	11.255539
14.216821	993.613142	11.260544
14.418569	998.504880	11.265549
14.335272	1003.993387	11.270554
14.613527	1000.908204	11.275559
14.622755	1003.137694	11.280563
15.054007	1006.388244	11.285568
14.444844	1012.360075	11.290573
14.462497	1007.750100	11.295578
15.023210	1009.913061	11.300583
14.883959	1008.892091	11.305587
15.086011	1005.797078	11.310592
15.149482	1009.279635	11.315597
15.371994	1013.302556	11.320602
15.251825	1006.911082	11.325607
14.892751	1017.846477	11.330611
14.880761	1013.466584	11.335616
14.944218	1020.973486	11.340621
15.005624	1022.459821	11.345626
15.271030	1032.599340	11.350631
15.333084	1040.630308	11.355635
15.606439	1034.563324	11.360640
15.432311	1036.576756	11.365645
15.249841	1025.926480	11.370650
15.770674	1035.507864	11.375655
15.614962	1037.165243	11.380659
15.885540	1028.738210	11.385664
15.859309	1029.120493	11.390669
15.708090	1033.258023	11.395674
16.213642	1035.404787	11.400679
15.758173	1033.038296	11.405683
15.946972	1014.470684	11.410688
16.052507	1018.281952	11.415693
15.861245	1018.388583	11.420698
16.215855	1008.524521	11.425703
15.874997	1014.118376	11.430707
16.247968	1011.827741	11.435712
15.872212	1009.759427	11.440717
15.756634	1027.962024	11.445722
16.322420	1030.453723	11.450727
16.243018	1035.323020	11.455731
16.439107	1038.382976	11.460736
16.229450	1041.376317	11.465741
16.382825	1040.448462	11.470746
16.687226	1038.593133	11.475751
16.665227	1047.135490	11.480755
16.585832	1034.058453	11.485760
16.414678	1039.892036	11.490765
16.101399	1040.054719	11.495770
16.370010	1040.056054	11.500775
16.262329	1046.772837	11.505779
16.264544	1034.963519	11.510784
16.357705	1042.149154	11.515789
16.251767	1046.064582	11.520794
16.570394	1060.610921	11.525799
16.352228	1069.450610	11.530803
16.744000	1067.662797	11.535808
16.561534	1071.578721	11.540813
16.840897	1072.426505	11.545818
16.959219	1067.113198	11.550823
16.961242	1083.943324	11.555827
17.258267	1095.026807	11.560832
17.536465	1096.200847	11.565837
17.623376	1093.157533	11.570842
17.681483	1078.342138	11.575847
17.475241	1073.917376	11.580851
18.141161	1066.756753	11.585856
17.753968	1068.398166	11.590861
17.573609	1070.400433	11.595866
17.621023	1065.221259	11.600871
17.426441	1071.636372	11.605875
17.594183	1066.719198	11.610880
17.608848	1070.640007	11.615885
17.417791	1067.071198	11.620890
17.730486	1076.675267	11.625895
17.410182	1082.352859	11.630899
17.902243	1067.150833	11.635904
17.677664	1073.852539	11.640909
17.494657	1071.059193	11.645914
17.673342	1076.307411	11.650919
17.344387	1099.097217	11.655923
17.827876	1099.765924	11.660928
17.411586	1112.021334	11.665933
17.686081	1110.316782	11.670938
17.923171	1104.109147	11.675943
17.581189	1116.206555	11.680947
17.889428	1123.433904	11.685952
17.902175	1129.459806	11.690957
17.952997	1132.569162	11.695962
18.150139	1132.114985	11.700967
18.256472	1141.766714	11.705971
18.156010	1135.141676	11.710976
18.295950	1145.603572	11.715981
18.693313	1147.043370	11.720986
18.913201	1152.486261	11.725991
19.164400	1158.856163	11.730995
19.042061	1139.572400	11.736000
19.200561	1137.129045	11.741005
18.866503	1122.961904	11.746010
19.029643	1114.929827	11.751015
19.087505	1121.306809	11.756019
18.999103	1120.592510	11.761024
19.143497	1123.345555	11.766029
18.958147	1125.060921	11.771034
19.243120	1116.452950	11.776039
18.931571	1124.716572	11.781043
19.272453	1132.619254	11.786048
19.117316	1129.235325	11.791053
19.111905	1130.102728	11.796058
19.187313	1124.149387	11.801063
19.189281	1126.647772	11.806067
19.456685	1122.078233	11.811072
19.048448	1125.649588	11.816077
18.856754	1123.524042	11.821082
19.251121	1128.543849	11.826087
19.180091	1150.355948	11.831091
19.319401	1148.801283	11.836096
20.070596	1150.504496	11.841101
19.744134	1160.701368	11.846106
19.792598	1164.501140	11.851111
19.556978	1166.146575	11.856115
19.498679	1154.895047	11.861120
19.794678	1153.767467	11.866125
19.890638	1162.479533	11.871130
19.978706	1157.685334	11.876135
19.538086	1158.109064	11.881139
19.716827	1154.788675	11.886144
19.871179	1165.357062	11.891149
19.547899	1163.525653	11.896154
20.079717	1179.865569	11.901159
20.113674	1191.553179	11.906163
20.550251	1196.367217	11.911168
20.374586	1196.217750	11.916173
20.374441	1200.156525	11.921178
20.805026	1183.779125	11.926183
20.508902	1176.835901	11.931187
20.588928	1167.249743	11.936192
20.821874	1168.606417	11.941197
20.736624	1159.431500	11.946202
20.868701	1156.184638	11.951207
20.591155	1154.885393	11.956211
20.361209	1148.573079	11.961216
20.402099	1148.955698	11.966221
20.367958	1149.948424	11.971226
20.781537	1167.506635	11.976231
20.420586	1190.238507	11.981235
20.628090	1187.701082	11.986240
20.539591	1189.374585	11.991245
20.777536	1199.174312	11.996250
21.115646	1184.695287	12.001255
21.033710	1192.119830	12.006259
20.959794	1184.829028	12.011264
20.874598	1191.428727	12.016269
21.204066	1200.613151	12.021274
21.180405	1191.333706	12.026279
21.389388	1195.687024	12.031283
21.057225	1195.939394	12.036288
21.008860	1189.174740	12.041293
21.093733	1188.581520	12.046298
21.329593	1191.130999	12.051303
20.943179	1198.948017	12.056307
21.157217	1196.441839	12.061312
21.400174	1204.574508	12.066317
21.154587	1202.738458	12.071322
21.405965	1181.776470	12.076327
21.475742	1193.325308	12.081331
21.230356	1191.185669	12.086336
21.284277	1199.530748	12.091341
21.284527	1194.542777	12.096346
21.206650	1193.094820	12.101351
21.165732	1207.399388	12.106355
21.478867	1196.968760	12.111360
21.343686	1195.217203	12.116365
21.115606	1201.129686	12.121370
21.612355	1185.087522	12.126375
21.272802	1191.891492	12.131379
21.328637	1189.329545	12.136384
21.297801	1192.683048	12.141389
21.425422	1194.427261	12.146394
21.735081	1190.223882	12.151399
21.372052	1185.191225	12.156403
21.075192	1173.435449	12.161408
21.367607	1170.534913	12.166413
21.276253	1171.568240	12.171418
21.491125	1162.193045	12.176423
21.244206	1162.056586	12.181427
21.322068	1167.281463	12.186432
21.250647	1166.140299	12.191437
20.940973	1166.913423	12.196442
21.340591	1160.782111	12.201447
20.893797	1164.789168	12.206451
21.341387	1163.810072	12.211456
21.481631	1164.045788	12.216461
21.324061	1167.388646	12.221466
21.618820	1166.862467	12.226471
21.355570	1168.886459	12.231475
21.310174	1168.355049	12.236480
21.362879	1166.531413	12.241485
21.457712	1171.507458	12.246490
21.475318	1158.160262	12.251495
21.174920	1153.846357	12.256499
21.134573	1138.618309	12.261504
21.274239	1139.088994	12.266509
21.012064	1143.487947	12.271514
21.264538	1134.797512	12.276519
20.920185	1139.906481	12.281523
21.031853	1141.317499	12.286528
21.166972	1158.766732	12.291533
21.426063	1169.360980	12.296538
21.335640	1156.010992	12.301543
21.121417	1152.459161	12.306547
21.202952	1145.232119	12.311552
20.944447	1138.626676	12.316557
20.901478	1158.279881	12.321562
21.458333	1161.517219	12.326567
21.396191	1163.935812	12.331571
20.934894	1152.279693	12.336576
21.371546	1155.700668	12.341581
20.933949	1161.788797	12.346586
21.070875	1169.933706	12.351591
20.698351	1180.730204	12.356595
20.952581	1179.788996	12.361600
21.091542	1171.397874	12.366605
20.975615	1186.280552	12.371610
21.360868	1178.530889	12.376615
21.278774	1176.744574	12.381619
21.333029	1179.300714	12.386624
21.484454	1183.895215	12.391629
21.472058	1179.969691	12.396634
21.446949	1173.204610	12.401639
20.871794	1176.303669	12.406643
21.206510	1171.130858	12.411648
21.132725	1175.495547	12.416653
21.194270	1180.457961	12.421658
21.367256	1177.530136	12.426663
21.354352	1183.504010	12.431667
21.273887	1157.307055	12.436672
21.391828	1154.018407	12.441677
21.079887	1149.417928	12.446682
21.517287	1147.061753	12.451687
20.990013	1148.403110	12.456691
21.469183	1149.706118	12.461696
21.098783	1146.552911	12.466701
21.517549	1147.925882	12.471706
21.409504	1143.978082	12.476711
21.378471	1141.863277	12.481715
21.386875	1147.423349	12.486720
21.440761	1150.536920	12.491725
20.846850	1149.702843	12.496730
21.579924	1143.157125	12.501735
21.188358	1150.450788	12.506739
21.356288	1147.176070	12.511744
21.508314	1149.900575	12.516749
21.536839	1148.517669	12.521754
21.486155	1130.371114	12.526759
21.154467	1123.016773	12.531763
21.212007	1116.910576	12.536768
21.131319	1118.441415	12.541773
20.943021	1116.450289	12.546778
21.040210	1111.610330	12.551783
21.016507	1123.535540	12.556787
21.397301	1132.312043	12.561792
21.421725	1128.814432	12.566797
21.363536	1127.485475	12.571802
21.337407	1113.775944	12.576807
20.869869	1121.987757	12.581811
20.932639	1118.046597	12.586816
21.122060	1119.846916	12.591821
21.177904	1122.076325	12.596826
21.104982	1128.975474	12.601831
20.831950	1147.423892	12.606835
21.046001	1151.464483	12.611840
21.330816	1152.551734	12.616845
21.176441	1153.295862	12.621850
21.160133	1148.890618	12.626855
21.161575	1164.518158	12.631859
21.297958	1152.185216	12.636864
21.365775	1150.688204	12.641869
21.391966	1156.684969	12.646874
21.234614	1139.678940	12.651879
21.122069	1140.627870	12.656883
21.136457	1128.952974	12.661888
21.267646	1130.415908	12.666893
20.698123	1128.506327	12.671898
21.146907	1143.974647	12.676903
21.237783	1150.942432	12.681907
21.385881	1151.611015	12.686912
21.752361	1151.485833	12.691917
21.225565	1142.492421	12.696922
21.361854	1132.705584	12.701927
21.091740	1129.273473	12.706931
21.276474	1122.479146	12.711936
21.197866	1128.705844	12.716941
21.415516	1124.731812	12.721946
21.418476	1125.567780	12.726951
21.233563	1134.144038	12.731955
21.285319	1130.394239	12.736960
21.461989	1134.056759	12.741965
20.928889	1133.977657	12.746970
21.496995	1128.495237	12.751975
21.495594	1126.168904	12.756979
21.298844	1119.366564	12.761984
21.478364	1130.562985	12.766989
21.472917	1129.721172	12.771994
21.569885	1122.654127	12.776999
21.134067	1108.909449	12.782003
20.983076	1105.329024	12.787008
21.388128	1102.013660	12.792013
21.064577	1106.035098	12.797018
21.264191	1098.637832	12.802023
21.284169	1105.399068	12.807027
21.405151	1100.225821	12.812032
21.117604	1104.469639	12.817037
21.002733	1102.055792	12.822042
21.401062	1091.631153	12.827047
21.220432	1100.604161	12.832051
21.086910	1099.703782	12.837056
21.349522	1096.794948	12.842061
21.092706	1106.207734	12.847066
21.226371	1098.472826	12.852071
21.377519	1102.527742	12.857075
21.416820	1103.235108	12.862080
21.047614	1094.589707	12.867085
21.424815	1102.722990	12.872090
21.560591	1103.002102	12.877095
21.559826	1103.395415	12.882099
21.263931	1107.474086	12.887104
21.202000	1098.682050	12.892109
20.730660	1108.810570	12.897114
21.052333	1092.328384	12.902119
20.969821	1109.113821	12.907123
21.066485	1107.313049	12.912128
20.977678	1109.451993	12.917133
20.925386	1100.469618	12.922138
21.000440	1095.854908	12.927143
20.997348	1105.378928	12.932147
21.008168	1105.998020	12.937152
21.009997	1095.413202	12.942157
20.790088	1110.247715	12.947162
21.516363	1122.651445	12.952167
21.223735	1128.666547	12.957171
21.069482	1129.546839	12.962176
21.050886	1123.004085	12.967181
21.264728	1135.529633	12.972186
21.635286	1130.507007	12.977191
21.240688	1124.296354	12.982195
21.006346	1116.314663	12.987200
21.165967	1113.777171	12.992205
20.699235	1115.322489	12.997210
21.330046	1122.939402	13.002215
21.306454	1141.741758	13.007219
21.484168	1131.650974	13.012224
21.229827	1115.212262	13.017229
21.192839	1123.401966	13.022234
21.576107	1111.773968	13.027239
21.491089	1116.980965	13.032243
20.972150	1108.418071	13.037248
20.982100	1114.357605	13.042253
21.030606	1106.724136	13.047258
21.221886	1104.906747	13.052263
20.859143	1107.289634	13.057267
20.849212	1108.757814	13.062272
20.811998	1119.692964	13.067277
20.939946	1134.554306	13.072282
21.710313	1125.957054	13.077287
21.648049	1137.849019	13.082291
21.572276	1123.443776	13.087296
21.454500	1115.341441	13.092301
21.053514	1116.248246	13.097306
21.012475	1114.400030	13.102311
21.241572	1116.624601	13.107315
21.141069	1111.821301	13.112320
21.055521	1110.784406	13.117325
21.006865	1119.196767	13.122330
21.022735	1107.357816	13.127335
20.944276	1118.963594	13.132339
21.233945	1126.308997	13.137344
21.166371	1126.868109	13.142349
21.342345	1125.337949	13.147354
21.138224	1124.099540	13.152359
20.929452	1127.024850	13.157363
21.249215	1124.008711	13.162368
21.416205	1135.450049	13.167373
21.208818	1132.592582	13.172378
21.587132	1109.892992	13.177383
21.391200	1112.260700	13.182387
21.329742	1116.365099	13.187392
21.671944	1110.902470	13.192397
21.719970	1122.094983	13.197402
21.738118	1111.289460	13.202407
21.370395	1107.121718	13.207411
20.926262	1092.202552	13.212416
21.045184	1096.235361	13.217421
21.256379	1111.171223	13.222426
21.848310	1104.826958	13.227431
21.586940	1098.236629	13.232435
21.318703	1100.768312	13.237440
21.712220	1088.346333	13.242445
21.415963	1083.524104	13.247450
21.459123	1079.345921	13.252455
21.316770	1084.939714	13.257459
21.416796	1079.804408	13.262464
21.586967	1080.502362	13.267469
20.930956	1072.378253	13.272474
21.469112	1076.718520	13.277479
21.374587	1060.454570	13.282483
21.218214	1063.586411	13.287488
21.083379	1060.350201	13.292493
21.084894	1055.367189	13.297498
21.050810	1048.586727	13.302503
20.985939	1051.456560	13.307507
21.079927	1058.834299	13.312512
21.080130	1072.975772	13.317517
20.657406	1086.320952	13.322522
21.216172	1078.812774	13.327527
21.266948	1081.032783	13.332531
21.087431	1088.480324	13.337536
21.521249	1090.750712	13.342541
21.371884	1094.634913	13.347546
21.643699	1086.589744	13.352551
21.211414	1078.864249	13.357555
21.417130	1060.619735	13.362560
21.512126	1060.863996	13.367565
21.243869	1067.432661	13.372570
21.200635	1060.900868	13.377575
21.361972	1062.169942	13.382579
21.125436	1067.442770	13.387584
21.371010	1070.328854	13.392589
20.962677	1076.602197	13.397594
21.125678	1065.099236	13.402599
21.197821	1068.739004	13.407603
21.337837	1064.674877	13.412608
21.345678	1062.278680	13.417613
21.140732	1065.172138	13.422618
21.519137	1054.024228	13.427623
21.092129	1056.881548	13.432627
20.730874	1060.533649	13.437632
20.837354	1058.594226	13.442637
20.865757	1062.359914	13.447642
20.838117	1061.190330	13.452647
20.912452	1067.435386	13.457651
20.808195	1076.807392	13.462656
21.074154	1085.163029	13.467661
20.771791	1090.554915	13.472666
21.137019	1097.288532	13.477671
21.134558	1090.802236	13.482675
21.185178	1095.661890	13.487680
21.097268	1091.476571	13.492685
20.897225	1090.625493	13.497690
21.240759	1090.030560	13.502695
21.273817	1094.912962	13.507699
21.159585	1092.651375	13.512704
21.134547	1092.184767	13.517709
20.940191	1096.972345	13.522714
21.376362	1095.676261	13.527719
21.105402	1099.612891	13.532723
20.979561	1097.645401	13.537728
21.272748	1092.932896	13.542733
21.264568	1097.514473	13.547738
21.382584	1091.068310	13.552743
21.266522	1093.982850	13.557747
20.999972	1096.363058	13.562752
21.029058	1095.731643	13.567757
20.893117	1102.019477	13.572762
20.957283	1092.279767	13.577767
21.116184	1095.477954	13.582771
20.995538	1094.767211	13.587776
21.280291	1096.268944	13.592781
20.993381	1099.067514	13.597786
21.110065	1090.474596	13.602791
21.358421	1101.157085	13.607795
21.285450	1094.517876	13.612800
21.510972	1083.742344	13.617805
21.394717	1097.358278	13.622810
20.738294	1089.859893	13.627815
20.965587	1097.219530	13.632819
20.734872	1092.872774	13.637824
20.896597	1111.171212	13.642829
20.966402	1129.243851	13.647834
21.312436	1127.903219	13.652839
21.565774	1129.115866	13.657843
21.398906	1132.131888	13.662848
21.460764	1122.047158	13.667853
21.068044	1118.117384	13.672858
21.292851	1105.221026	13.677863
21.624867	1102.537924	13.682867
21.325602	1102.594389	13.687872
21.574900	1096.314795	13.692877
20.992442	1100.709835	13.697882
21.263098	1101.146217	13.702887
21.110431	1105.870597	13.707891
21.021713	1107.874525	13.712896
21.421786	1108.100822	13.717901
21.257021	1111.774904	13.722906
21.278589	1098.511553	13.727911
21.502105	1101.824584	13.732915
21.070485	1109.427861	13.737920
21.185871	1112.091535	13.742925
20.948259	1114.830734	13.747930
21.077037	1096.883187	13.752935
21.015669	1104.374426	13.757939
20.692751	1110.800901	13.762944
21.221645	1105.950478	13.767949
21.235436	1111.357244	13.772954
21.188471	1109.518730	13.777959
21.146519	1106.490796	13.782963
21.201896	1106.704351	13.787968
21.667263	1096.728481	13.792973
21.289858	1111.876974	13.797978
21.559726	1107.903072	13.802983
21.566659	1105.280444	13.807987
21.369346	1114.226320	13.812992
21.533254	1100.710403	13.817997
21.407898	1113.221459	13.823002
20.959021	1092.036625	13.828007
21.128547	1093.551404	13.833011
21.249787	1108.005315	13.838016
21.296071	1090.765081	13.843021
21.085474	1097.417031	13.848026
20.933146	1085.610882	13.853031
21.226089	1101.769829	13.858035
21.383771	1105.854416	13.863040
21.209929	1094.932611	13.868045
21.235828	1103.614814	13.873050
21.289653	1094.488721	13.878055
20.915529	1090.090764	13.883059
20.725200	1094.862650	13.888064
21.161324	1101.966220	13.893069
21.181350	1117.463816	13.898074
21.304680	1107.290003	13.903079
21.031086	1107.211012	13.908083
21.183827	1109.330647	13.913088
21.469716	1110.392053	13.918093
21.312725	1112.698610	13.923098
21.351034	1111.705611	13.928103
21.221442	1105.330712	13.933107
21.113622	1107.769760	13.938112
21.321610	1107.223724	13.943117
21.095074	1103.591120	13.948122
21.178314	1111.237569	13.953127
21.064417	1100.141666	13.958131
21.007406	1115.766153	13.963136
21.345846	1113.600241	13.968141
20.850701	1114.311214	13.973146
20.987990	1112.938085	13.978151
20.907888	1118.865033	13.983155
21.147077	1118.451411	13.988160
21.283661	1117.825248	13.993165
20.913417	1127.728814	13.998170
20.995038	1120.692033	14.003175
20.824989	1117.478428	14.008179
20.819698	1119.123051	14.013184
21.484577	1114.681550	14.018189
21.369740	1121.077286	14.023207
21.317947	1117.155559	14.028224
21.616033	1110.771685	14.033242
20.918445	1111.807921	14.038259
21.344559	1110.490296	14.043277
21.258337	1124.706630	14.048295
20.932214	1121.725710	14.053312
20.990321	1119.665605	14.058330
21.215816	1118.311899	14.063347
21.370782	1118.063680	14.068365
21.098148	1131.645786	14.073383
21.270454	1116.308343	14.078400
21.163778	1123.815444	14.083418
21.065403	1138.553994	14.088435
21.449689	1141.185592	14.093453
21.302144	1151.985414	14.098471
21.427018	1156.436441	14.103488
21.165682	1148.905845	14.108506
21.027176	1159.750977	14.113523
21.445326	1153.086636	14.118541
21.291114	1156.737019	14.123559
21.470645	1154.415520	14.128576
21.457315	1148.767757	14.133594
21.369761	1158.933232	14.138611
21.481580	1145.462584	14.143629
21.693516	1150.755051	14.148647
21.671567	1156.888474	14.153664
21.915747	1156.938764	14.158682
21.748152	1156.422200	14.163699
21.779393	1152.896104	14.168717
21.567845	1155.075093	14.173735
21.665226	1156.612090	14.178752
21.496628	1156.657950	14.183770
21.232376	1168.241636	14.188787
21.690764	1174.577772	14.193805
21.754352	1183.064454	14.198823
22.073904	1183.455788	14.203840
21.769525	1181.713358	14.208858
22.131849	1189.026288	14.213875
22.156198	1183.960292	14.218893
22.106745	1186.078419	14.223911
22.152522	1177.141890	14.228928
21.857233	1167.536618	14.233946
21.814026	1167.540111	14.238963
21.866752	1164.208377	14.243981
21.915160	1183.874576	14.248999
21.889415	1185.056670	14.254016
22.485675	1186.980222	14.259034
21.951356	1180.259866	14.264051
22.123208	1175.675711	14.269069
22.026260	1189.210420	14.274087
22.173033	1185.721993	14.279104
22.299338	1186.248831	14.284122
22.070021	1181.481861	14.289139
22.033752	1171.771934	14.294157
21.898716	1186.943623	14.299175
22.017555	1185.521577	14.304192
22.139858	1184.762378	14.309210
21.723146	1187.718737	14.314227
22.274065	1184.854776	14.319245
22.188149	1190.938545	14.324263
22.270407	1185.675201	14.329280
22.064092	1187.274509	14.334298
21.824172	1195.218697	14.339315
22.134188	1190.569507	14.344333
22.233393	1185.828105	14.349351
22.376709	1194.927161	14.354368
22.094699	1196.513067	14.359386
22.359013	1210.627641	14.364403
22.587841	1217.006698	14.369421
22.441115	1221.453125	14.374439
22.411129	1217.558739	14.379456
22.503975	1216.541969	14.384474
22.243561	1221.989469	14.389491
22.700469	1215.235773	14.394509
22.758432	1220.105018	14.399527
22.901789	1220.355287	14.404544
22.731107	1217.805611	14.409562
22.452600	1200.824366	14.414579
22.516183	1191.586325	14.419597
22.475326	1208.797179	14.424615
22.685692	1216.628345	14.429632
22.632583	1207.672136	14.434650
22.545310	1227.314798	14.439667
22.737035	1222.014562	14.444685
22.738568	1225.159870	14.449703
22.565001	1215.639219	14.454720
22.846483	1211.891449	14.459738
22.770220	1219.963902	14.464755
22.994442	1218.944293	14.469773
22.831026	1225.354382	14.474791
22.727206	1224.537881	14.479808
22.919928	1211.977400	14.484826
22.751701	1227.274908	14.489843
22.604685	1216.824427	14.494861
22.939738	1217.215073	14.499879
22.539193	1210.850934	14.504896
22.683660	1215.969148	14.509914
22.411221	1219.346877	14.514931
22.847548	1228.760706	14.519949
23.035695	1246.615469	14.524967
23.307225	1240.692435	14.529984
23.451871	1236.595646	14.535002
22.901371	1231.063185	14.540019
23.005593	1226.390209	14.545037
22.987101	1241.664420	14.550055
23.360211	1250.211858	14.555072
23.425685	1241.623915	14.560090
23.487554	1228.913401	14.565107
23.393411	1225.256804	14.570125
23.380619	1224.227040	14.575143
23.294340	1214.246504	14.580160
23.764876	1210.171412	14.585178
23.237350	1220.631279	14.590195
23.282447	1217.356751	14.595213
23.436084	1219.286506	14.600231
23.542573	1219.804143	14.605248
23.391443	1211.911678	14.610266
23.218950	1216.418826	14.615283
23.261732	1217.451366	14.620301
23.358153	1217.409264	14.625319
23.252040	1215.754107	14.630336
23.296519	1209.422731	14.635354
23.147854	1219.203019	14.640371
23.302633	1222.117703	14.645389
23.378564	1223.246144	14.650407
23.417201	1247.492448	14.655424
23.924959	1245.810390	14.660442
23.421895	1244.446538	14.665459
23.493225	1242.322333	14.670477
23.613329	1245.856013	14.675495
23.719079	1247.173848	14.680512
23.818458	1247.123363	14.685530
23.481725	1259.410549	14.690547
23.801663	1252.513377	14.695565
24.062227	1248.191181	14.700583
23.497419	1241.970557	14.705600
23.732686	1243.068137	14.710618
23.611204	1246.646781	14.715635
23.628861	1248.045868	14.720653
23.505321	1250.749198	14.725671
23.394780	1251.489891	14.730688
23.694758	1248.954402	14.735706
23.546445	1251.011529	14.740723
23.596384	1252.223175	14.745741
23.887123	1239.402933	14.750759
23.784289	1250.352257	14.755776
23.931602	1254.515581	14.760794
24.093922	1256.389123	14.765811
24.594215	1250.204795	14.770829
24.810728	1243.775793	14.775847
24.361721	1251.721998	14.780864
24.501952	1242.972010	14.785882
24.417817	1243.480990	14.790899
24.070404	1247.506675	14.795917
24.214071	1242.496980	14.800935
23.956703	1252.590834	14.805952
24.458136	1248.193478	14.810970
24.229791	1250.417096	14.815987
24.174582	1241.446266	14.821005
24.318180	1242.453254	14.826023
24.344833	1244.759146	14.831040
24.293754	1247.422490	14.836058
24.487208	1243.819738	14.841075
24.204950	1240.185548	14.846093
24.272834	1235.295551	14.851111
24.519814	1248.201215	14.856128
24.115264	1245.343176	14.861146
24.380576	1237.342286	14.866163
24.465131	1242.339274	14.871181
24.696335	1239.371445	14.876199
24.535644	1245.962981	14.881216
24.614535	1230.945800	14.886234
24.572236	1224.780097	14.891251
23.996402	1221.684084	14.896269
24.804152	1229.714432	14.901287
24.664772	1239.643155	14.906304
24.335304	1235.328810	14.911322
24.216500	1237.086362	14.916339
24.234776	1241.701766	14.921357
24.054249	1243.682518	14.926375
24.055806	1248.868557	14.931392
24.088048	1247.019581	14.936410
24.460960	1264.178453	14.941427
24.283682	1274.496406	14.946445
24.511186	1279.688995	14.951463
24.549649	1288.544642	14.956480
24.487167	1280.688917	14.961498
24.489111	1284.488949	14.966515
24.553645	1280.041285	14.971533
24.924242	1276.107339	14.976551
24.585337	1287.848807	14.981568
24.951334	1294.399671	14.986586
25.120646	1301.656369	14.991603
25.308727	1306.994716	14.996621
25.009130	1287.932548	15.001639
25.018440	1284.407032	15.006656
24.832337	1273.428127	15.011674
25.292261	1278.888374	15.016691
25.378162	1277.532996	15.021709
25.273304	1272.377303	15.026727
25.029159	1273.776000	15.031744
24.990479	1277.143586	15.036762
25.223813	1277.018949	15.041779
25.045324	1284.218725	15.046797
24.883504	1278.941288	15.051815
25.005284	1277.860886	15.056832
25.397700	1291.989401	15.061850
25.145034	1286.969291	15.066867
25.038669	1299.753281	15.071885
25.644675	1292.996036	15.076903
25.401492	1310.989793	15.081920
25.386121	1291.022117	15.086938
25.450897	1285.091598	15.091955
24.982412	1281.809435	15.096973
25.486295	1289.361158	15.101991
25.428609	1297.881295	15.107008
25.679281	1303.118349	15.112026
25.721086	1300.680272	15.117043
25.613797	1293.136975	15.122061
25.596321	1272.203848	15.127079
25.524360	1284.779546	15.132096
25.574340	1278.741320	15.137114
25.219553	1268.376432	15.142131
25.381271	1277.074314	15.147149
26.174614	1285.857230	15.152167
25.963460	1289.348493	15.157184
25.783890	1278.055444	15.162202
25.651686	1276.948897	15.167219
25.702878	1272.270431	15.172237
25.892010	1272.342760	15.177255
25.786512	1283.011830	15.182272
25.840458	1276.556351	15.187290
26.316303	1271.317237	15.192307
26.073192	1281.052728	15.197325
25.990002	1268.467455	15.202343
26.156865	1279.915490	15.207360
25.925146	1276.064734	15.212378
26.040313	1275.578826	15.217395
25.659274	1278.947233	15.222413
25.833874	1270.204331	15.227431
25.976450	1280.430042	15.232448
25.838637	1279.195312	15.237466
26.243984	1267.824820	15.242483
25.502137	1284.610228	15.247501
25.774964	1277.847118	15.252519
25.937988	1276.100924	15.257536
25.792758	1276.998759	15.262554
25.987996	1270.056418	15.267571
25.638388	1276.445298	15.272589
25.705295	1295.720636	15.277607
25.665087	1303.000658	15.282624
25.732990	1303.194569	15.287642
26.117129	1313.253283	15.292659
25.709808	1322.255466	15.297677
25.840782	1328.491883	15.302695
25.998430	1346.394119	15.307712
26.137588	1350.454920	15.312730
26.475487	1350.858075	15.317747
26.282051	1356.099237	15.322765
26.136746	1342.571708	15.327783
26.365297	1345.063885	15.332800
26.642719	1351.949676	15.337818
26.785856	1347.267235	15.342835
26.706092	1355.848674	15.347853
26.589251	1350.317022	15.352871
26.639128	1340.919810	15.357888
26.494657	1358.399011	15.362906
26.751935	1351.873203	15.367923
26.606693	1364.610363	15.372941
26.637574	1350.446655	15.377959
27.206626	1354.798746	15.382976
26.752627	1350.489971	15.387994
26.821775	1350.395846	15.393011
26.671315	1354.903587	15.398029
26.997768	1354.278686	15.403047
26.580822	1342.714054	15.408064
26.682355	1347.390025	15.413082
27.303154	1345.227115	15.418099
26.902654	1336.062258	15.423117
26.607942	1320.299129	15.428135
26.689584	1325.397046	15.433152
26.810581	1346.271984	15.438170
26.703271	1349.303682	15.443187
26.775898	1349.849573	15.448205
27.107510	1353.389930	15.453223
27.008958	1350.019520	15.458240
26.722398	1348.742564	15.463258
26.966054	1349.756816	15.468275
26.743211	1356.739012	15.473293
26.641483	1345.401856	15.478311
27.060201	1357.548569	15.483328
27.059478	1354.845308	15.488346
27.556026	1350.833838	15.493363
27.284406	1349.604719	15.498381
27.372058	1355.343408	15.503399
26.939266	1356.604756	15.508416
27.043204	1360.671598	15.513434
27.054471	1348.748083	15.518451
26.869146	1361.030257	15.523469
27.357644	1375.286088	15.528487
27.581272	1374.216960	15.533504
27.461367	1371.248277	15.538522
27.622170	1356.094873	15.543539
27.541403	1354.054610	15.548557
27.454523	1349.455311	15.553575
27.824315	1352.821390	15.558592
27.312445	1352.161072	15.563610
27.372759	1345.642263	15.568627
27.188954	1352.744941	15.573645
27.447333	1363.722579	15.578663
27.561550	1378.735959	15.583680
27.147415	1387.514129	15.588698
27.493289	1379.510379	15.593715
27.564819	1383.955261	15.598733
27.097755	1383.144726	15.603751
27.424025	1383.756983	15.608768
27.386262	1385.414427	15.613786
27.564269	1375.187274	15.618803
27.774818	1402.721594	15.623821
27.865617	1403.532113	15.628839
27.899409	1399.336955	15.633856
27.972183	1409.406592	15.638874
28.273187	1388.552970	15.643891
28.095581	1378.754144	15.648909
28.196946	1375.378195	15.653927
27.772545	1367.276969	15.658944
27.971252	1371.057461	15.663962
28.007336	1361.311387	15.668979
28.071703	1367.983690	15.673997
27.966396	1364.623097	15.679015
28.136929	1368.117447	15.684032
27.835077	1367.322291	15.689050
28.265891	1364.660799	15.694067
28.318857	1367.837872	15.699085
27.950291	1366.998244	15.704103
28.413255	1367.705972	15.709120
28.104149	1365.120156	15.714138
28.366014	1363.949976	15.719155
28.248214	1371.848904	15.724173
28.333644	1365.459257	15.729191
28.411246	1364.857729	15.734208
28.393774	1372.675670	15.739226
28.404737	1372.715549	15.744243
28.549084	1370.994202	15.749261
28.562538	1371.093896	15.754279
28.293141	1370.647540	15.759296
28.256284	1367.418138	15.764314
28.155180	1355.772176	15.769331
28.254936	1370.490362	15.774349
28.347797	1390.703584	15.779367
28.471046	1394.589548	15.784384
28.176517	1404.424491	15.789402
28.433720	1395.618927	15.794419
28.558417	1405.617842	15.799437
28.136951	1399.778523	15.804455
28.593615	1404.601122	15.809472
28.642342	1407.490713	15.814490
28.760978	1400.793755	15.819507
28.790756	1406.034068	15.824525
28.505324	1403.043753	15.829543
28.903322	1418.794027	15.834560
28.901869	1440.681522	15.839578
29.081048	1430.278524	15.844595
28.748268	1423.141185	15.849613
29.025381	1429.063187	15.854631
29.323460	1420.313206	15.859648
28.966438	1413.003238	15.864666
29.049825	1402.199713	15.869683
28.835357	1405.914820	15.874701
28.833836	1404.581114	15.879719
29.222084	1412.259033	15.884736
29.166147	1432.186372	15.889754
29.186950	1432.334418	15.894771
29.228446	1427.009471	15.899789
29.282584	1424.578317	15.904807
29.283928	1409.477794	15.909824
29.321847	1408.774790	15.914842
29.494282	1403.797516	15.919859
29.614284	1403.656479	15.924877
29.207213	1398.368290	15.929895
29.510210	1387.919285	15.934912
29.186674	1400.644519	15.939930
29.338231	1393.910026	15.944947
29.345352	1390.826244	15.949965
29.151840	1395.538247	15.954983
29.530191	1400.639259	15.960000
29.417591	1410.884789	15.965018
29.554132	1409.488824	15.970035
29.959916	1408.652269	15.975053
29.508633	1408.205204	15.980071
29.562799	1399.500991	15.985088
29.538777	1396.153229	15.990106
29.555985	1399.512834	15.995123
29.581565	1396.256972	16.000141
29.628017	1409.624358	16.005159
29.746151	1418.705025	16.010176
29.743392	1436.980571	16.015194
29.710301	1430.280084	16.020211
29.719911	1432.050682	16.025229
29.674501	1435.068634	16.030247
29.977042	1431.701098	16.035264
29.850877	1435.659760	16.040282
29.811258	1431.022016	16.045299
29.987009	1430.126857	16.050317
29.720974	1436.885369	16.055335
29.738658	1426.263581	16.060352
29.378325	1437.067796	16.065370
29.772743	1427.091329	16.070387
29.859740	1433.664889	16.075405
29.835052	1432.924581	16.080423
30.175112	1435.975271	16.085440
29.619714	1444.861560	16.090458
29.740481	1454.905673	16.095475
30.012326	1455.871000	16.100493
29.979733	1461.197230	16.105511
30.586543	1458.201973	16.110528
30.635227	1464.673442	16.115546
30.195341	1464.207885	16.120563
30.418220	1458.847891	16.125581
30.241496	1467.677536	16.130599
30.553712	1453.966731	16.135616
30.158560	1456.975747	16.140634
30.290620	1454.702899	16.145651
30.407235	1456.020858	16.150669
30.077833	1457.341659	16.155687
30.598743	1459.725455	16.160704
30.309434	1466.439146	16.165722
30.278156	1457.311316	16.170739
30.531623	1453.853361	16.175757
30.636455	1467.113533	16.180775
30.855351	1468.108020	16.185792
30.827538	1465.392060	16.190810
30.547873	1461.646338	16.195827
30.610180	1467.127182	16.200845
30.550834	1479.279177	16.205863
31.078891	1477.866478	16.210880
30.935403	1487.779524	16.215898
30.781595	1486.970004	16.220915
31.125321	1481.594008	16.225933
30.735390	1484.039084	16.230951
30.930855	1486.987003	16.235968
31.047262	1482.708753	16.240986
31.242194	1481.032664	16.246003
30.940491	1467.062896	16.251021
30.628144	1466.025808	16.256039
30.932503	1475.402566	16.261056
31.131935	1492.628052	16.266074
31.258748	1482.489929	16.271091
31.164088	1488.556020	16.276109
31.245800	1490.039038	16.281127
31.273204	1490.569850	16.286144
31.306297	1488.392319	16.291162
31.113020	1492.266823	16.296179
31.288310	1488.878568	16.301197
30.626166	1493.344538	16.306215
31.375006	1492.749191	16.311232
31.109612	1492.622257	16.316250
31.192760	1496.240290	16.321267
31.242875	1489.041603	16.326285
31.146197	1492.893245	16.331303
31.147804	1487.299104	16.336320
31.287967	1494.797135	16.341338
31.729477	1506.297077	16.346355
31.281298	1505.612837	16.351373
31.310821	1519.228914	16.356391
31.446041	1526.706940	16.361408
31.397460	1526.382185	16.366426
31.155350	1523.567116	16.371443
31.814080	1523.069117	16.376461
31.264108	1522.446822	16.381479
31.507125	1523.641530	16.386496
31.696131	1526.310613	16.391514
31.788043	1518.409397	16.396531
32.071109	1521.709272	16.401549
31.575161	1523.105882	16.406567
31.781295	1526.983968	16.411584
32.056658	1544.830812	16.416602
32.110121	1545.340621	16.421619
32.109417	1528.549209	16.426637
32.063371	1530.453784	16.431655
32.244217	1520.405596	16.436672
31.950441	1524.616270	16.441690
31.907839	1523.219904	16.446707
32.089172	1529.208766	16.451725
32.338988	1548.219566	16.456743
32.318834	1533.739999	16.461760
32.224603	1519.984244	16.466778
31.858279	1533.467788	16.471795
32.521507	1540.856866	16.476813
32.374571	1547.206381	16.481831
32.490978	1543.250196	16.486848
32.033864	1541.881980	16.491866
32.285726	1542.616068	16.496883
32.648122	1545.862185	16.501901
32.216354	1549.703963	16.506919
32.416677	1542.576752	16.511936
32.427060	1546.371464	16.516954
32.350429	1551.801348	16.521971
32.429929	1556.955226	16.526989
32.454109	1552.786086	16.532007
32.419672	1552.756970	16.537024
32.606051	1548.544666	16.542042
32.635952	1549.766465	16.547059
32.871527	1543.866806	16.552077
32.484304	1549.392073	16.557095
32.777287	1542.621062	16.562112
32.786695	1541.183885	16.567130
32.543282	1547.208565	16.572147
32.356310	1545.522350	16.577165
32.543021	1549.912882	16.582183
33.010659	1560.652397	16.587200
33.206305	1570.038795	16.592218
32.904238	1562.047215	16.597235
33.365466	1553.582212	16.602253
32.959288	1550.920872	16.607271
33.038323	1540.164459	16.612288
33.361839	1537.458337	16.617306
32.979390	1542.139779	16.622323
33.147542	1541.260092	16.627341
32.776311	1555.466227	16.632359
33.095112	1561.020857	16.637376
33.452975	1567.942170	16.642394
33.695693	1564.640381	16.647411
33.667319	1539.449248	16.652429
33.553877	1545.693402	16.657447
33.427156	1541.702516	16.662464
33.313439	1535.263472	16.667482
33.102098	1544.775545	16.672499
33.613428	1541.720257	16.677517
33.685898	1542.027967	16.682535
33.474700	1539.981300	16.687552
33.583457	1536.593418	16.692570
33.518557	1545.814608	16.697587
33.488627	1532.886883	16.702605
33.485643	1539.839734	16.707623
33.487519	1540.707637	16.712640
33.829793	1539.935907	16.717658
33.957204	1545.349312	16.722675
33.709949	1535.626509	16.727693
33.495968	1548.179913	16.732711
33.757079	1559.187145	16.737728
34.037640	1564.051407	16.742746
33.947079	1578.763045	16.747763
33.653782	1553.327516	16.752781
34.009796	1573.756515	16.757799
33.731677	1570.535361	16.762816
33.909896	1566.227197	16.767834
33.649518	1577.825876	16.772851
33.842444	1567.050311	16.777869
33.785436	1574.538875	16.782887
33.961092	1575.552595	16.787904
33.638682	1569.783638	16.792922
33.707376	1571.820137	16.797939
34.114013	1577.534536	16.802957
33.974153	1589.457480	16.807975
34.052850	1593.590923	16.812992
34.280634	1591.030747	16.818010
33.943397	1601.815365	16.823027
34.220955	1604.519679	16.828045
34.332655	1589.963904	16.833063
34.127245	1600.234132	16.838080
34.350860	1594.884204	16.843098
34.646758	1592.968327	16.848115
35.180849	1592.816929	16.853133
34.708122	1594.005210	16.858151
34.642356	1593.355018	16.863168
34.562416	1592.452897	16.868186
34.308709	1593.781992	16.873203
34.983995	1596.335821	16.878221
34.931883	1592.892034	16.883239
34.739433	1598.701675	16.888256
34.950478	1584.280463	16.893274
34.561598	1590.712427	16.898291
35.036890	1586.508458	16.903309
34.694266	1588.835977	16.908327
34.694557	1592.585969	16.913344
34.757098	1594.518790	16.918362
34.655801	1596.260779	16.923379
34.685381	1583.590950	16.928397
34.749695	1600.091607	16.933415
34.594927	1596.258683	16.938432
34.834238	1605.630528	16.943450
34.514800	1616.923579	16.948467
34.896377	1615.558034	16.953485
35.260237	1626.658733	16.958503
35.154958	1622.290093	16.963520
35.561171	1620.345849	16.968538
35.324682	1625.619288	16.973555
35.331749	1621.977533	16.978573
35.665871	1610.876515	16.983591
35.337615	1608.368358	16.988608
35.669102	1609.406943	16.993626
35.389504	1624.719603	16.998643
35.510365	1621.048099	17.003661
35.545863	1615.388647	17.008679
35.614611	1619.420248	17.013696
35.507161	1611.152727	17.018714
35.622590	1610.758508	17.023731
35.698704	1609.222082	17.028749
35.800596	1612.882997	17.033767
35.810114	1608.722262	17.038784
35.789497	1604.049315	17.043802
35.970176	1616.785924	17.048819
35.871915	1597.469935	17.053837
35.865351	1586.042657	17.058855
35.233313	1587.365351	17.063872
35.566324	1599.835644	17.068890
35.512296	1607.920628	17.073907
35.531785	1614.534188	17.078925
35.738600	1607.481434	17.083943
35.749075	1612.894436	17.088960
35.970479	1603.708630	17.093978
35.527805	1613.039123	17.098995
35.940148	1628.488691	17.104013
36.010106	1636.119707	17.109031
35.884442	1644.584357	17.114048
36.349670	1633.265940	17.119066
36.613516	1636.303751	17.124083
36.597059	1629.799561	17.129101
36.742463	1610.830405	17.134119
36.409936	1601.689961	17.139136
36.821635	1594.792656	17.144154
36.598040	1601.616805	17.149171
36.555357	1598.104857	17.154189
36.711541	1592.997619	17.159207
36.536451	1600.779699	17.164224
36.580097	1587.727097	17.169242
36.597698	1599.598640	17.174259
36.426289	1599.887135	17.179277
36.420626	1593.165731	17.184295
36.479974	1605.209668	17.189312
36.890460	1591.362984	17.194330
36.951458	1595.955024	17.199347
36.622542	1597.479712	17.204365
36.976129	1595.232649	17.209383
36.585451	1597.671569	17.214400
36.797732	1592.244837	17.219418
36.547240	1591.732627	17.224435
36.338306	1596.954871	17.229453
36.702142	1599.468388	17.234471
36.596112	1616.527067	17.239488
37.268306	1618.827859	17.244506
37.266355	1633.002643	17.249523
37.358168	1632.125803	17.254541
37.254425	1631.019469	17.259559
36.915803	1629.514775	17.264576
37.137473	1618.011331	17.269594
37.240608	1626.020554	17.274611
37.304292	1622.549427	17.279629
37.236445	1620.257280	17.284647
36.792364	1631.395708	17.289664
37.241262	1633.640681	17.294682
37.124999	1631.215873	17.299699
37.229679	1634.487688	17.304717
37.163636	1628.024682	17.309735
37.066622	1637.973167	17.314752
37.306964	1626.297205	17.319770
37.371133	1642.699890	17.324787
37.220702	1649.066582	17.329805
37.819631	1660.447905	17.334823
37.941362	1668.082266	17.339840
37.766213	1660.134630	17.344858
37.510174	1666.747415	17.349875
37.822781	1660.771900	17.354893
37.938830	1662.315591	17.359911
37.487610	1667.811708	17.364928
37.664523	1663.251350	17.369946
37.883291	1659.980423	17.374963
37.817377	1665.624676	17.379981
37.989238	1663.765888	17.384999
37.629682	1665.219843	17.390016
37.704646	1667.343478	17.395034
38.065336	1664.723885	17.400051
37.700559	1666.419314	17.405069
37.903209	1655.295524	17.410087
37.987492	1662.153930	17.415104
38.689266	1680.675545	17.420122
38.350428	1682.368497	17.425139
38.347662	1673.175410	17.430157
38.692045	1661.553639	17.435175
38.071071	1660.315486	17.440192
38.090964	1650.820068	17.445210
38.000686	1661.745083	17.450227
38.184044	1681.770706	17.455245
38.390534	1687.517493	17.460263
38.250251	1698.636956	17.465280
38.308127	1695.499130	17.470298
38.486428	1690.275457	17.475315
38.320159	1690.122075	17.480333
38.560332	1681.739792	17.485351
38.005407	1687.791555	17.490368
38.565123	1699.955705	17.495386
38.829146	1705.285893	17.500403
39.174081	1716.315090	17.505421
39.267425	1703.054241	17.510439
38.974791	1691.458192	17.515456
38.946765	1681.234271	17.520474
39.177727	1667.957339	17.525491
38.757128	1674.503448	17.530509
39.085021	1673.968063	17.535527
38.848622	1684.372021	17.540544
39.017098	1671.028625	17.545562
38.837858	1677.106139	17.550579
38.786389	1704.799315	17.555597
39.461431	1699.282179	17.560615
39.322557	1708.905564	17.565632
39.146119	1706.105976	17.570650
39.542435	1701.435147	17.575667
39.506620	1712.598920	17.580685
39.322419	1699.193512	17.585703
39.337778	1707.911216	17.590720
39.365499	1708.923534	17.595738
39.611094	1705.429468	17.600755
39.113677	1703.747242	17.605773
39.563994	1707.206693	17.610791
39.531784	1709.553458	17.615808
39.430504	1703.915062	17.620826
39.713322	1703.935106	17.625843
39.457599	1709.105559	17.630861
39.629948	1701.239284	17.635879
39.652650	1711.292896	17.640896
39.645573	1706.394736	17.645914
39.817249	1710.571330	17.650931
39.435930	1705.530618	17.655949
39.729578	1700.166678	17.660967
39.676251	1722.684795	17.665984
39.767384	1734.663533	17.671002
39.876660	1737.045106	17.676019
39.880984	1742.831694	17.681037
40.075644	1732.475453	17.686055
39.894218	1742.983031	17.691072
39.878826	1735.344620	17.696090
39.884903	1738.156535	17.701107
39.973147	1743.006970	17.706125
40.237124	1741.220580	17.711143
40.187245	1742.699015	17.716160
39.940586	1745.798387	17.721178
40.732257	1764.567319	17.726195
40.250389	1775.428040	17.731213
40.698589	1769.956466	17.736231
40.199018	1776.964638	17.741248
40.335686	1772.673778	17.746266
40.847756	1774.919754	17.751283
40.706441	1766.032685	17.756301
40.769170	1772.637717	17.761319
41.133257	1768.234630	17.766336
40.630845	1752.384612	17.771354
40.821736	1738.632936	17.776371
40.551579	1751.611931	17.781389
40.550634	1756.754468	17.786407
40.606582	1772.514526	17.791424
40.724208	1774.708037	17.796442
40.911772	1762.483081	17.801459
40.707741	1770.652930	17.806477
40.865235	1768.998192	17.811495
40.752340	1770.891027	17.816512
40.549471	1773.625766	17.821530
40.979462	1771.301792	17.826547
40.878130	1787.468405	17.831565
41.380369	1797.103198	17.836583
41.276287	1795.709868	17.841600
41.170468	1790.396668	17.846618
41.627519	1793.247035	17.851635
41.379421	1795.647364	17.856653
41.669422	1795.334641	17.861671
41.376740	1791.952925	17.866688
41.112117	1796.704802	17.871706
41.519420	1793.449560	17.876723
41.541377	1789.295307	17.881741
41.632863	1788.437021	17.886759
41.368717	1797.259002	17.891776
41.317686	1796.007775	17.896794
41.536588	1790.783407	17.901811
41.589501	1793.248284	17.906829
41.576891	1787.147356	17.911847
41.911644	1784.534553	17.916864
41.544817	1791.719996	17.921882
41.679509	1794.417732	17.926899
41.633364	1791.994658	17.931917
42.085611	1799.890565	17.936935
42.365133	1810.343176	17.941952
41.815666	1797.082997	17.946970
42.132849	1791.853590	17.951987
41.872022	1801.077810	17.957005
41.825210	1814.522957	17.962023
42.187324	1810.557654	17.967040
42.363986	1807.823508	17.972058
42.511901	1806.785840	17.977075
42.900343	1811.980546	17.982093
42.642388	1800.074889	17.987111
42.860666	1784.933660	17.992128
42.723723	1778.686315	17.997146
43.056999	1774.001466	18.002163
43.041098	1776.080452	18.007181
43.086344	1777.062208	18.012199
42.686296	1770.989913	18.017216
42.354451	1761.915800	18.022234
42.471229	1767.153525	18.027251
42.422802	1779.052275	18.032269
42.615563	1777.649002	18.037287
42.690818	1775.501609	18.042304
42.265577	1777.564546	18.047322
42.702748	1771.077415	18.052339
42.406483	1772.323260	18.057357
42.583681	1778.841731	18.062375
42.476949	1795.362472	18.067392
42.377153	1810.639366	18.072410
42.670943	1807.304751	18.077427
42.596384	1810.864847	18.082445
42.594634	1814.191567	18.087463
42.789878	1827.719257	18.092480
42.816123	1847.105409	18.097498
43.090218	1843.895833	18.102515
43.091300	1839.735302	18.107533
42.993552	1842.961937	18.112551
43.185759	1839.203732	18.117568
43.156122	1851.870673	18.122586
43.468588	1857.307190	18.127603
43.278566	1877.957387	18.132621
43.477816	1873.593164	18.137639
43.169976	1873.841267	18.142656
43.773175	1874.949836	18.147674
43.881823	1868.862343	18.152691
43.572524	1874.992945	18.157709
43.549985	1874.029778	18.162727
44.030460	1865.685342	18.167744
43.866420	1880.679186	18.172762
44.118818	1867.047972	18.177779
44.011522	1864.129007	18.182797
44.401042	1865.619531	18.187815
44.834348	1849.020720	18.192832
44.347151	1831.509534	18.197850
44.496914	1819.845808	18.202867
44.628032	1821.891324	18.207885
44.431439	1820.542203	18.212903
44.591991	1818.733373	18.217920
44.230795	1814.662525	18.222938
44.341198	1806.234700	18.227955
44.322174	1806.335239	18.232973
44.374967	1805.948211	18.237991
44.476479	1796.612747	18.243008
44.347266	1800.857885	18.248026
44.827521	1797.483429	18.253043
44.646008	1787.984658	18.258061
44.713184	1796.480903	18.263079
44.656918	1781.112305	18.268096
44.566625	1786.142595	18.273114
44.088017	1786.775136	18.278131
44.086549	1802.935669	18.283149
44.460641	1811.345438	18.288167
44.579550	1814.156134	18.293184
44.647573	1820.410629	18.298202
44.411811	1810.504952	18.303219
44.601130	1820.390680	18.308237
44.387061	1838.650162	18.313255
44.785470	1846.645493	18.318272
44.672627	1850.532675	18.323290
44.557995	1851.539090	18.328307
44.377489	1859.047782	18.333325
44.623985	1856.117773	18.338343
45.211592	1872.550262	18.343360
44.756575	1881.373515	18.348378
45.013644	1877.283667	18.353395
45.330320	1879.382034	18.358413
45.316700	1875.129514	18.363431
45.310159	1868.939313	18.368448
45.281012	1875.271127	18.373466
45.274275	1880.721824	18.378483
45.385592	1882.412823	18.383501
45.230395	1894.073634	18.388519
45.783487	1888.989994	18.393536
46.118550	1887.517032	18.398554
46.231119	1867.501484	18.403571
46.648979	1859.452074	18.408589
46.439473	1855.934808	18.413607
46.461388	1855.040408	18.418624
46.159789	1867.074769	18.423642
46.527810	1847.301707	18.428659
46.448916	1839.055551	18.433677
46.291112	1829.579465	18.438695
46.405238	1828.773995	18.443712
45.977061	1827.762646	18.448730
46.579670	1827.862526	18.453747
46.606945	1819.645033	18.458765
46.433437	1819.903572	18.463783
46.555904	1814.288987	18.468800
46.450254	1803.601463	18.473818
46.385308	1799.145926	18.478835
46.227538	1790.897962	18.483853
46.050489	1795.881705	18.488871
46.393384	1801.557504	18.493888
46.103590	1820.628473	18.498906
46.256350	1818.965486	18.503923
46.579492	1813.827189	18.508941
46.345135	1822.878358	18.513959
46.464886	1822.337705	18.518976
46.326149	1818.324002	18.523994
46.644847	1823.275520	18.529011
46.876258	1816.362568	18.534029
46.680791	1823.528489	18.539047
46.723375	1835.415222	18.544064
46.560770	1839.925183	18.549082
46.526233	1857.617619	18.554099
46.815914	1854.608150	18.559117
46.799955	1849.105486	18.564135
47.028016	1854.939199	18.569152
46.787371	1857.379604	18.574170
46.679262	1859.046009	18.579187
46.850862	1867.662595	18.584205
46.677379	1887.854007	18.589223
47.142733	1880.385103	18.594240
47.131657	1882.342787	18.599258
47.206763	1890.171496	18.604275
47.385839	1889.858495	18.609293
47.274776	1899.035439	18.614311
47.654094	1905.448829	18.619328
47.363920	1916.624464	18.624346
47.536491	1911.149698	18.629363
48.076006	1905.717941	18.634381
47.641093	1920.977586	18.639399
47.950543	1917.254780	18.644416
48.042494	1914.420558	18.649434
48.165595	1907.527317	18.654451
48.558765	1898.867473	18.659469
47.899916	1887.056470	18.664487
48.031107	1873.817338	18.669504
48.062947	1883.450936	18.674522
47.687979	1881.540582	18.679539
47.766567	1882.175639	18.684557
47.924695	1903.376496	18.689575
47.810305	1905.451122	18.694592
47.933624	1916.282994	18.699610
47.717489	1910.983154	18.704627
48.101506	1909.480140	18.709645
48.520352	1931.420295	18.714663
48.237863	1925.518754	18.719680
48.539166	1935.260535	18.724698
48.279064	1940.656254	18.729715
48.661063	1937.897512	18.734733
48.338479	1938.261937	18.739751
48.617927	1934.144612	18.744768
48.721152	1937.075751	18.749786
48.622715	1936.228363	18.754803
48.833901	1941.909470	18.759821
48.575378	1938.040305	18.764839
48.659125	1933.096971	18.769856
48.947814	1936.387702	18.774874
48.902659	1934.219982	18.779891
48.968446	1923.573859	18.784909
49.101870	1931.238632	18.789927
48.900288	1936.642035	18.794944
49.131324	1931.899856	18.799962
49.331678	1933.862642	18.804979
49.304554	1934.412662	18.809997
49.477481	1941.181967	18.815015
49.540610	1932.646810	18.820032
49.364478	1937.674541	18.825050
49.334266	1935.232962	18.830067
49.523185	1925.442221	18.835085
48.974061	1939.746140	18.840103
49.732563	1939.493266	18.845120
49.637209	1958.259376	18.850138
49.692296	1967.661450	18.855155
50.065313	1956.947274	18.860173
50.104009	1953.955617	18.865191
50.035715	1941.309366	18.870208
49.975906	1930.506007	18.875226
49.886308	1932.881545	18.880243
50.178858	1919.141813	18.885261
49.959041	1929.003649	18.890279
50.258083	1923.163449	18.895296
50.203983	1922.404142	18.900314
49.664685	1921.338207	18.905331
49.691129	1925.086157	18.910349
49.805228	1944.777096	18.915367
49.890160	1949.541932	18.920384
49.970155	1962.585888	18.925402
50.050277	1941.404785	18.930419
50.049078	1943.418273	18.935437
49.866453	1965.313546	18.940455
50.166008	1975.791578	18.945472
50.335542	1986.266315	18.950490
50.283387	1988.471640	18.955507
50.267761	1986.298062	18.960525
49.963114	1996.388686	18.965543
50.579131	2009.749104	18.970560
50.782963	2010.599734	18.975578
50.625079	2015.937789	18.980595
50.570557	2008.628046	18.985613
50.646281	2018.238058	18.990631
51.104123	2010.502628	18.995648
51.240747	2012.841360	19.000666
51.277462	2013.172142	19.005683
51.189756	2006.767818	19.010701
50.918956	2017.181832	19.015719
51.175630	2005.874493	19.020736
51.425316	2008.031220	19.025754
50.861402	2019.810236	19.030771
51.208147	1989.947130	19.035789
51.109084	2008.420589	19.040807
50.956258	2022.073093	19.045824
51.260341	2029.848045	19.050842
51.220836	2038.611171	19.055859
51.750604	2036.941012	19.060877
51.300824	2040.678499	19.065895
51.367842	2041.271445	19.070912
51.789868	2043.865230	19.075930
51.947001	2045.169993	19.080947
52.304372	2032.924376	19.085965
51.874744	2044.953654	19.090983
51.524479	2036.440491	19.096000
51.868988	2029.939610	19.101018
51.923027	2036.456468	19.106035
52.075946	2032.162752	19.111053
52.121511	2038.097124	19.116071
52.084651	2044.609488	19.121088
52.255157	2054.413932	19.126106
52.216821	2062.683101	19.131123
52.587584	2052.995374	19.136141
52.869540	2061.706549	19.141159
52.801095	2044.652930	19.146176
53.205516	2027.589920	19.151194
52.813351	2036.060309	19.156211
52.701828	2028.035032	19.161229
52.766737	2031.024734	19.166247
52.930156	2025.362889	19.171264
53.030010	2028.932113	19.176282
52.949168	2030.502116	19.181299
52.899992	2026.435203	19.186317
52.949149	2026.927654	19.191335
52.683300	2030.474527	19.196352
52.879369	2029.987327	19.201370
52.912712	2026.957987	19.206387
52.953113	2026.338005	19.211405
52.995833	2022.362046	19.216423
53.117737	2028.792845	19.221440
53.234126	2028.879226	19.226458
52.778712	2038.911857	19.231475
53.000420	2027.858956	19.236493
53.321572	2047.644859	19.241511
53.165869	2061.979483	19.246528
53.464001	2053.531545	19.251546
53.055504	2065.654868	19.256563
53.115677	2067.512158	19.261581
53.201426	2065.929148	19.266599
53.474385	2055.836475	19.271616
53.546575	2051.469969	19.276634
53.336248	2070.914285	19.281651
53.543503	2083.838872	19.286669
53.582880	2089.243540	19.291687
53.509292	2091.965225	19.296704
53.674603	2082.479658	19.301722
53.876619	2091.677850	19.306739
53.725934	2084.987399	19.311757
53.855894	2085.923544	19.316775
53.803092	2101.250940	19.321792
54.158350	2115.700006	19.326810
54.210965	2119.422253	19.331827
54.356724	2109.522638	19.336845
54.444385	2104.084807	19.341863
54.519284	2114.947562	19.346880
54.756390	2106.133234	19.351898
54.654036	2109.459153	19.356915
54.491266	2108.613728	19.361933
54.637278	2113.669760	19.366951
54.297771	2111.696203	19.371968
54.802173	2108.366761	19.376986
55.009126	2107.212244	19.382003
55.211680	2111.125348	19.387021
54.796291	2115.309777	19.392039
54.906759	2109.828658	19.397056
54.921048	2104.034063	19.402074
54.849540	2111.593095	19.407091
54.952582	2109.853944	19.412109
55.244847	2105.985988	19.417127
55.431570	2104.484495	19.422144
55.181092	2103.111511	19.427162
54.922697	2106.383855	19.432179
54.982767	2106.959489	19.437197
55.552734	2104.477198	19.442215
55.316524	2108.168635	19.447232
55.421287	2110.693579	19.452250
55.420833	2129.471974	19.457267
55.567458	2132.642595	19.462285
55.545828	2142.283157	19.467303
55.510464	2148.605123	19.472320
55.950979	2130.711283	19.477338
55.703111	2137.526437	19.482355
55.741223	2134.302135	19.487373
56.011603	2135.474088	19.492391
56.065976	2139.889052	19.497408
55.954649	2138.752875	19.502426
56.117783	2131.130914	19.507443
55.903889	2130.248577	19.512461
56.309712	2135.999550	19.517479
56.358006	2134.286321	19.522496
56.518347	2124.505474	19.527514
56.296791	2141.942852	19.532531
55.788595	2136.864686	19.537549
56.137757	2126.363176	19.542567
56.117074	2151.505828	19.547584
56.408608	2157.696937	19.552602
56.417663	2159.031823	19.557619
56.632482	2159.863646	19.562637
56.565091	2159.585416	19.567655
56.455235	2163.728499	19.572672
56.534665	2162.454876	19.577690
56.814527	2170.034021	19.582707
56.689269	2165.717873	19.587725
56.730110	2155.963007	19.592743
56.379075	2172.886319	19.597760
56.610817	2177.316560	19.602778
56.648922	2195.035511	19.607795
56.617792	2194.463619	19.612813
56.689696	2199.479621	19.617831
56.983469	2210.268691	19.622848
57.448739	2213.672930	19.627866
57.485052	2215.733178	19.632883
57.424483	2220.457679	19.637901
57.669242	2214.115579	19.642919
57.645394	2218.966086	19.647936
57.524800	2211.896744	19.652954
57.675858	2215.064259	19.657971
57.546472	2213.644516	19.662989
58.103107	2212.361525	19.668007
57.866848	2218.358065	19.673024
58.080214	2214.682377	19.678042
57.637958	2217.061718	19.683059
57.781243	2220.023450	19.688077
58.073389	2210.590086	19.693095
58.151168	2215.653912	19.698112
58.356312	2206.540238	19.703130
58.206106	2213.338680	19.708147
58.314955	2218.781490	19.713165
58.299479	2211.268865	19.718183
58.007490	2222.452115	19.723200
58.302274	2213.177377	19.728218
58.708072	2232.875369	19.733235
58.376779	2241.772112	19.738253
58.842565	2239.447842	19.743271
58.408893	2251.508289	19.748288
58.694951	2244.910240	19.753306
58.652975	2245.271056	19.758323
58.655532	2238.237289	19.763341
58.769486	2235.466963	19.768359
58.415475	2243.472979	19.773376
58.873604	2244.920672	19.778394
58.987498	2235.850976	19.783411
58.530620	2243.444641	19.788429
58.708044	2248.527620	19.793447
58.803460	2261.382538	19.798464
58.595941	2265.378588	19.803482
58.765193	2269.102136	19.808499
59.066305	2275.967345	19.813517
59.371129	2289.833002	19.818535
59.546193	2296.896235	19.823552
59.565914	2295.333579	19.828570
59.946276	2294.615532	19.833587
59.981689	2302.992675	19.838605
59.972053	2288.228279	19.843623
60.028162	2280.586793	19.848640
60.065082	2264.470923	19.853658
60.168584	2255.488050	19.858675
59.906447	2251.156757	19.863693
60.243150	2248.838865	19.868711
59.958134	2248.015179	19.873728
59.700996	2247.294603	19.878746
60.052087	2255.293140	19.883763
60.016096	2281.100142	19.888781
60.454984	2274.476665	19.893799
60.272136	2274.483623	19.898816
60.341184	2284.948225	19.903834
60.590554	2287.604336	19.908851
60.158275	2286.203440	19.913869
60.469435	2276.888843	19.918887
60.239366	2289.162482	19.923904
60.480407	2289.097552	19.928922
60.705302	2282.339868	19.933939
60.490984	2291.359913	19.938957
60.805052	2281.156489	19.943975
60.208986	2289.992338	19.948992
60.766405	2310.702389	19.954010
61.066636	2316.830644	19.959027
61.142791	2317.007403	19.964045
60.818816	2305.381618	19.969063
60.977617	2314.717293	19.974080
61.021667	2315.282293	19.979098
61.398761	2314.565593	19.984115
61.119071	2322.925106	19.989133
61.023109	2317.677763	19.994151
61.377967	2334.515664	19.999168
61.149781	2338.180577	20.004186
61.396102	2349.772492	20.009203
61.343514	2344.320823	20.014221
61.670206	2340.238214	20.019239
61.825723	2350.876254	20.024256
62.029526	2349.233993	20.029274
62.327587	2345.711497	20.034291
62.178019	2343.227316	20.039309
62.067679	2345.702550	20.044327
61.900667	2348.238690	20.049344
62.034504	2348.103150	20.054362
61.939091	2347.136697	20.059379
62.249773	2347.019664	20.064397
61.975529	2338.337765	20.069415
61.911360	2347.076153	20.074432
61.873144	2354.202755	20.079450
62.349923	2356.168604	20.084467
62.512817	2355.311433	20.089485
62.440974	2364.012558	20.094503
62.349911	2361.887694	20.099520
62.235309	2360.114165	20.104538
62.679537	2364.744288	20.109555
62.739392	2379.071775	20.114573
63.098310	2386.247646	20.119591
63.048354	2385.754577	20.124608
63.248786	2386.665270	20.129626
63.701733	2375.690610	20.134643
63.546569	2362.190663	20.139661
63.538117	2342.114930	20.144679
63.697886	2351.906439	20.149696
63.791899	2340.046735	20.154714
64.029130	2339.212258	20.159731
63.791644	2337.788198	20.164749
64.125437	2324.552539	20.169767
64.043426	2309.509146	20.174784
63.608222	2320.995017	20.179802
63.402182	2306.761991	20.184819
63.360956	2314.772693	20.189837
63.576658	2303.412707	20.194855
63.715048	2325.623189	20.199872
63.531976	2325.964883	20.204890
63.573683	2333.435310	20.209907
63.778043	2332.708847	20.214925
64.054731	2341.280116	20.219943
63.904804	2341.256228	20.224960
63.879264	2337.164706	20.229978
63.775646	2346.231168	20.234995
63.916613	2359.264214	20.240013
64.172273	2361.026991	20.245031
64.290268	2371.315517	20.250048
64.130229	2374.148150	20.255066
64.059256	2371.463058	20.260083
63.976299	2385.177927	20.265101
64.455300	2389.219324	20.270119
64.509078	2399.493677	20.275136
64.126863	2401.958042	20.280154
64.589593	2399.653173	20.285171
64.495716	2425.279755	20.290189
64.454429	2430.347526	20.295207
64.539245	2438.016156	20.300224
64.684614	2434.312699	20.305242
65.023101	2440.491934	20.310259
65.044576	2453.370712	20.315277
65.366355	2457.222512	20.320295
65.459054	2455.985179	20.325312
65.454128	2452.778429	20.330330
65.331208	2450.821246	20.335347
65.465531	2455.387186	20.340365
65.493480	2454.142054	20.345383
65.427445	2447.969699	20.350400
65.672897	2448.423784	20.355418
65.593708	2443.005780	20.360435
65.563700	2456.870714	20.365453
66.148907	2474.653689	20.370471
66.468327	2470.418724	20.375488
66.143683	2457.393495	20.380506
66.652736	2446.113055	20.385523
66.250149	2447.157850	20.390541
66.280967	2445.241250	20.395559
66.117765	2436.405590	20.400576
66.239381	2442.807865	20.405594
66.367634	2437.236167	20.410611
66.264975	2444.207689	20.415629
66.619517	2462.659435	20.420647
66.661529	2470.148775	20.425664
66.794015	2473.184072	20.430682
67.324319	2454.794864	20.435699
66.910508	2449.673636	20.440717
66.708402	2444.653932	20.445735
66.919694	2443.976678	20.450752
66.836415	2455.781113	20.455770
67.008769	2469.360142	20.460787
66.779120	2472.353571	20.465805
66.882909	2472.690976	20.470823
66.895653	2472.272996	20.475840
67.265813	2465.943947	20.480858
67.706280	2471.018915	20.485875
67.365355	2472.272075	20.490893
67.602802	2472.236113	20.495911
67.682127	2465.216646	20.500928
67.550704	2473.424025	20.505946
67.415985	2474.481175	20.510963
67.409399	2477.625370	20.515981
67.434818	2487.884954	20.520999
67.765014	2501.680297	20.526016
67.499106	2503.204110	20.531034
67.771485	2502.015509	20.536051
67.614217	2501.284099	20.541069
68.011786	2511.274348	20.546087
68.155596	2518.087092	20.551104
68.233994	2529.091291	20.556122
68.469181	2531.042669	20.561139
68.419875	2530.201393	20.566157
68.425048	2526.395157	20.571175
68.772751	2520.540095	20.576192
68.651112	2528.463101	20.581210
68.850495	2519.628233	20.586227
68.600642	2517.437642	20.591245
68.604574	2520.303618	20.596263
68.699449	2517.848378	20.601280
68.408756	2528.320479	20.606298
68.520818	2522.514479	20.611315
68.481945	2539.902864	20.616333
68.744588	2549.311443	20.621351
68.814812	2555.283917	20.626368
68.804721	2558.145215	20.631386
68.995667	2572.479544	20.636403
69.247335	2586.534137	20.641421
69.144677	2574.966286	20.646439
69.430141	2584.476504	20.651456
69.454612	2589.142433	20.656474
69.607038	2585.777947	20.661491
69.758610	2579.235105	20.666509
69.568367	2582.762050	20.671527
69.719965	2582.890439	20.676544
69.940830	2583.693685	20.681562
70.140891	2581.983527	20.686579
70.250453	2583.643009	20.691597
70.003825	2581.516434	20.696615
71.223349	2554.834303	20.701632
71.831092	2536.264765	20.706650
71.628187	2519.503018	20.711667
71.506878	2508.067570	20.716685
71.444144	2498.806707	20.721703
71.551340	2482.320235	20.726720
71.358788	2471.764102	20.731738
71.200877	2463.692213	20.736755
71.488883	2467.278107	20.741773
71.634647	2447.325430	20.746791
71.307869	2435.281061	20.751808
71.453443	2429.038570	20.756826
71.560976	2423.706689	20.761843
71.723902	2425.051444	20.766861
71.115420	2423.718544	20.771879
71.135991	2407.607691	20.776896
70.929982	2410.411199	20.781914
70.964794	2419.861911	20.786931
70.987956	2425.552593	20.791949
71.116381	2425.318752	20.796967
71.322053	2417.344421	20.801984
70.999823	2428.932280	20.807002
71.758569	2444.597727	20.812019
72.084357	2446.868262	20.817037
71.774198	2456.463193	20.822055
72.022970	2454.139085	20.827072
71.230711	2459.120620	20.832090
71.164110	2457.636537	20.837107
71.156067	2460.589608	20.842125
71.398393	2491.041357	20.847143
71.773199	2487.435583	20.852160
71.693849	2494.721295	20.857178
71.860284	2510.245008	20.862195
72.152318	2523.549980	20.867213
71.862259	2531.933431	20.872231
71.875007	2525.756989	20.877248
72.029934	2556.319928	20.882266
72.272817	2557.964426	20.887283
72.290891	2565.932013	20.892301
72.355493	2559.011108	20.897319
72.733595	2575.022308	20.902336
72.672518	2596.170331	20.907354
73.101411	2596.430739	20.912371
73.007974	2594.696869	20.917389
72.911520	2593.061959	20.922407
72.983339	2594.063230	20.927424
73.035959	2600.343517	20.932442
72.965842	2603.865622	20.937459
73.309159	2611.701868	20.942477
73.356306	2621.959390	20.947495
73.405670	2617.993560	20.952512
73.266775	2622.653643	20.957530
73.586533	2624.477916	20.962547
73.587887	2613.992397	20.967565
73.447687	2623.028276	20.972583
73.636001	2643.276762	20.977600
73.878865	2643.196557	20.982618
73.671631	2656.799087	20.987635
73.801391	2646.715230	20.992653
73.845506	2651.341584	20.997671
74.075909	2655.599720	21.002688
74.208466	2671.960258	21.007706
74.430850	2669.671357	21.012723
74.585526	2666.422237	21.017741
74.752867	2686.649960	21.022759
74.936393	2671.648112	21.027776
74.788767	2676.592436	21.032794
74.767332	2674.588687	21.037811
74.628679	2666.256653	21.042829
74.609534	2673.247035	21.047847
74.913799	2671.383544	21.052864
74.615212	2670.788185	21.057882
74.817186	2672.260149	21.062899
75.101015	2681.224939	21.067917
75.027173	2703.015567	21.072935
75.334024	2703.146479	21.077952
75.031341	2705.879983	21.082970
75.280350	2702.565067	21.087987
75.339298	2700.696379	21.093005
75.340866	2709.063003	21.098023
75.769200	2714.175572	21.103040
75.608055	2724.900446	21.108058
75.930206	2727.581170	21.113075
76.126529	2719.717758	21.118093
75.895711	2727.342201	21.123111
76.228983	2726.916515	21.128128
76.114196	2726.686564	21.133146
76.331032	2730.252432	21.138163
75.997614	2722.822423	21.143181
75.836648	2729.280349	21.148199
76.349157	2738.213842	21.153216
76.462351	2752.593955	21.158234
76.572517	2760.375742	21.163251
76.692571	2751.258228	21.168269
76.507687	2761.035840	21.173287
76.671764	2759.364909	21.178304
76.641713	2758.589624	21.183322
76.372782	2753.327687	21.188339
77.001906	2768.548667	21.193357
76.616926	2786.185674	21.198375
76.779497	2782.483124	21.203392
77.094382	2783.070225	21.208410
77.210144	2784.451449	21.213427
77.463014	2778.007715	21.218445
77.380342	2784.410501	21.223463
77.402918	2781.082411	21.228480
77.684140	2786.812462	21.233498
77.691637	2795.944400	21.238515
78.216240	2799.667795	21.243533
77.807221	2797.950992	21.248551
78.069183	2785.723512	21.253568
77.923902	2785.991794	21.258586
78.064390	2801.685629	21.263603
78.501338	2805.424053	21.268621
78.077604	2811.619919	21.273639
78.335850	2807.899385	21.278656
78.707621	2805.398991	21.283674
78.292570	2809.305537	21.288691
78.478630	2803.733250	21.293709
78.050678	2811.046584	21.298727
78.499942	2801.877325	21.303744
78.571451	2808.304878	21.308762
78.168806	2812.271514	21.313779
78.624358	2815.946898	21.318797
78.619028	2828.533673	21.323815
78.907716	2830.465679	21.328832
78.585450	2833.297855	21.333850
79.133818	2840.168964	21.338867
79.064886	2829.107839	21.343885
79.036323	2859.796545	21.348903
79.427441	2860.905328	21.353920
79.583375	2867.102643	21.358938
79.445854	2866.477298	21.363955
79.782417	2861.395036	21.368973
79.999322	2866.142251	21.373991
80.134972	2867.116846	21.379008
80.217083	2866.431796	21.384026
79.932982	2869.442510	21.389043
80.243707	2861.001040	21.394061
79.911781	2863.443465	21.399079
80.344546	2864.257651	21.404096
80.349217	2862.170647	21.409114
80.089443	2863.798973	21.414131
80.308896	2859.890552	21.419149
80.279070	2869.960607	21.424167
80.562925	2895.201086	21.429184
80.777952	2894.483796	21.434202
80.533636	2890.428850	21.439219
80.820486	2892.914042	21.444237
80.536565	2899.486837	21.449255
80.690215	2901.475868	21.454272
80.672311	2893.481349	21.459290
80.534210	2902.843075	21.464307
81.249841	2917.739862	21.469325
81.063193	2921.871895	21.474343
81.113758	2933.667918	21.479360
81.482557	2923.535027	21.484378
81.336854	2923.797870	21.489395
81.402368	2924.290696	21.494413
81.435403	2919.658955	21.499431
81.542428	2912.868444	21.504448
81.415665	2926.304624	21.509466
81.498432	2936.611374	21.514483
81.751119	2949.151648	21.519501
81.796575	2949.830627	21.524519
81.791310	2945.538581	21.529536
82.277777	2957.362271	21.534554
81.933085	2974.187698	21.539571
82.493539	2980.181820	21.544589
82.810011	2976.144117	21.549607
82.797049	2968.173127	21.554624
83.063663	2963.929759	21.559642
82.750862	2963.275395	21.564659
83.368840	2944.281494	21.569677
82.945798	2936.626543	21.574695
82.994839	2929.797925	21.579712
83.047815	2917.006054	21.584730
82.948170	2934.258810	21.589747
83.294971	2936.687265	21.594765
83.345663	2954.843585	21.599783
83.285992	2955.797330	21.604800
83.701381	2954.025014	21.609818
83.288404	2962.121831	21.614835
83.313478	2953.892309	21.619853
83.146173	2955.720582	21.624871
83.149322	2960.573778	21.629888
83.469365	2965.671131	21.634906
83.360677	2979.845350	21.639923
83.538643	2986.385460	21.644941
83.629833	2991.923711	21.649959
83.571893	3003.836833	21.654976
84.187773	3016.473195	21.659994
84.052483	3030.841822	21.665011
84.312241	3021.647434	21.670029
84.349087	3017.155197	21.675047
84.363249	3023.380029	21.680064
84.588905	3018.551423	21.685082
84.501359	3033.613583	21.690099
84.735311	3044.981318	21.695117
84.834282	3050.078010	21.700135
84.764812	3054.850753	21.705152
84.949008	3048.277708	21.710170
84.967665	3054.085162	21.715187
85.079471	3047.085069	21.720205
85.229615	3044.164275	21.725223
85.625923	3046.380281	21.730240
85.500423	3040.160396	21.735258
85.458064	3046.365000	21.740275
85.499386	3032.852840	21.745293
85.652945	3050.648258	21.750311
85.790659	3069.597042	21.755328
86.212841	3073.044302	21.760346
86.344871	3064.649899	21.765363
86.113595	3040.824088	21.770381
86.551564	3034.896658	21.775399
86.055954	3037.618402	21.780416
85.987515	3034.755560	21.785434
85.900973	3054.047558	21.790451
86.166712	3057.049098	21.795469
86.658284	3066.591217	21.800487
86.171171	3068.743678	21.805504
86.543445	3062.471522	21.810522
86.292490	3074.535923	21.815539
86.461438	3076.365629	21.820557
86.684258	3086.546083	21.825575
86.394583	3107.895435	21.830592
86.669073	3108.027175	21.835610
86.581276	3111.321668	21.840627
86.839554	3123.392523	21.845645
87.019186	3131.569756	21.850663
87.079827	3145.042512	21.855680
87.491956	3131.443069	21.860698
87.413915	3141.050599	21.865715
87.353287	3142.652686	21.870733
87.369770	3149.517462	21.875751
87.654238	3153.072620	21.880768
87.664551	3153.303993	21.885786
87.871762	3155.494155	21.890803
88.097769	3159.409804	21.895821
87.973160	3155.672132	21.900839
88.096974	3169.956299	21.905856
88.282184	3182.468162	21.910874
88.314360	3193.043651	21.915891
88.649982	3189.253058	21.920909
88.778445	3192.498679	21.925927
88.594344	3192.439693	21.930944
89.021172	3189.977056	21.935962
88.858489	3188.789750	21.940979
88.753406	3188.388014	21.945997
89.057658	3187.221465	21.951015
88.815207	3191.029994	21.956032
89.353813	3188.132358	21.961050
89.051626	3209.733652	21.966067
89.434918	3219.697664	21.971085
89.602029	3222.558631	21.976103
89.547200	3221.285889	21.981120
89.614616	3219.540124	21.986138
89.499702	3219.650418	21.991155
89.226620	3228.476303	21.996173
89.617274	3214.341773	22.001191
89.444251	3238.570347	22.006208
89.905664	3240.602742	22.011226
89.870691	3250.477817	22.016243
89.822678	3244.791929	22.021261
90.333048	3246.323700	22.026279
90.196884	3248.264802	22.031296
90.482361	3257.010696	22.036314
90.678910	3268.169998	22.041331
90.644031	3264.636649	22.046349
91.018680	3260.534559	22.051367
91.093466	3267.120040	22.056384
91.451669	3257.572344	22.061402
91.372609	3251.779941	22.066419
91.464710	3229.413691	22.071437
91.566735	3224.774759	22.076455
91.365920	3224.624130	22.081472
91.424007	3228.704047	22.086490
91.366114	3220.406702	22.091507
91.306766	3220.707512	22.096525
91.669988	3237.436268	22.101543
91.480685	3253.725006	22.106560
91.633131	3250.201286	22.111578
91.666870	3253.934915	22.116595
91.695899	3256.812473	22.121613
91.749623	3257.115951	22.126631
91.587382	3266.601743	22.131648
92.747335	3274.314857	22.136666
92.316716	3292.967558	22.141683
92.266362	3288.428763	22.146701
92.330392	3284.783156	22.151719
92.009373	3294.315875	22.156736
92.324746	3288.455048	22.161754
92.393511	3302.406966	22.166771
92.256907	3314.440132	22.171789
92.652003	3319.156937	22.176807
92.887081	3313.814702	22.181824
93.299428	3322.601888	22.186842
93.555620	3338.648159	22.191859
93.685037	3336.457797	22.196877
93.858913	3307.179042	22.201895
93.573011	3312.085839	22.206912
93.854175	3297.808553	22.211930
93.706107	3297.325187	22.216947
93.402538	3304.068483	22.221965
93.723513	3323.764278	22.226983
93.560132	3338.970469	22.232000
93.777822	3327.691313	22.237018
93.913127	3334.959515	22.242035
93.890281	3339.724350	22.247053
94.051832	3337.270942	22.252071
94.196132	3365.272141	22.257088
94.315050	3364.765841	22.262106
94.413739	3368.219798	22.267123
94.423996	3366.299523	22.272141
94.547542	3369.009683	22.277159
94.636288	3395.360246	22.282176
94.910699	3390.838989	22.287194
94.817363	3391.491376	22.292211
94.948012	3400.061485	22.297229
95.449573	3392.749483	22.302247
94.798566	3395.786969	22.307264
95.049858	3406.636130	22.312282
95.634124	3407.143209	22.317299
95.293854	3421.064547	22.322317
95.309284	3415.940291	22.327335
95.698419	3421.069265	22.332352
95.882586	3419.992595	22.337370
96.008638	3422.583410	22.342387
95.978212	3421.093034	22.347405
96.234711	3412.388853	22.352423
95.731198	3424.324339	22.357440
95.942985	3442.610331	22.362458
96.502917	3446.271122	22.367475
96.130788	3456.198614	22.372493
96.278611	3447.059399	22.377511
96.381337	3455.905254	22.382528
96.424177	3471.262874	22.387546
96.586448	3475.074542	22.392563
96.939320	3476.497875	22.397581
97.174650	3473.178845	22.402599
97.074760	3473.851261	22.407616
96.872672	3475.779278	22.412634
97.534898	3479.162637	22.417651
97.420158	3500.575463	22.422669
97.266185	3501.683235	22.427687
97.349362	3506.267702	22.432704
97.596158	3509.870355	22.437722
97.819344	3514.883683	22.442739
97.979899	3505.635926	22.447757
98.372354	3491.040104	22.452775
98.134960	3489.723818	22.457792
98.201793	3490.943376	22.462810
98.606783	3493.317051	22.467827
98.522805	3503.601566	22.472845
98.797156	3508.928243	22.477863
98.543503	3511.468394	22.482880
98.610454	3520.342471	22.487898
98.929852	3525.661430	22.492915
98.879945	3523.478946	22.497933
98.974020	3520.343215	22.502951
98.779005	3520.023044	22.507968
98.838051	3520.096428	22.512986
99.060702	3516.973308	22.518003
98.740979	3538.748964	22.523021
99.255209	3546.140533	22.528039
99.177028	3553.395817	22.533056
99.551420	3552.586597	22.538074
99.786926	3552.683284	22.543091
99.508929	3559.981491	22.548109
99.944475	3571.201634	22.553127
99.733238	3577.239290	22.558144
100.045704	3569.409889	22.563162
100.252433	3566.439919	22.568179
100.782723	3568.204585	22.573197
100.993704	3557.835292	22.578215
101.195671	3564.000576	22.583232
100.822240	3567.574108	22.588250
100.788626	3555.569188	22.593267
100.353104	3560.522977	22.598285
100.747050	3560.777584	22.603303
100.688373	3557.657795	22.608320
100.804437	3561.163159	22.613338
101.230226	3572.468461	22.618355
101.230723	3585.495892	22.623373
101.325931	3593.750847	22.628391
101.137200	3601.166871	22.633408
101.453241	3592.401191	22.638426
101.284271	3594.009296	22.643443
100.924736	3600.181859	22.648461
101.433123	3610.843744	22.653479
101.681801	3616.558414	22.658496
101.905120	3621.539463	22.663514
102.108283	3618.221979	22.668531
101.596440	3631.884658	22.673549
102.155850	3636.363891	22.678567
102.239716	3640.867157	22.683584
102.286668	3642.485506	22.688602
102.631678	3643.211609	22.693619
102.479694	3664.952380	22.698637
102.604273	3670.581233	22.703655
102.693314	3680.351044	22.708672
102.756981	3683.492887	22.713690
102.869282	3679.597123	22.718707
102.844368	3694.846075	22.723725
103.169168	3702.860102	22.728743
103.195432	3707.853695	22.733760
103.285698	3709.693815	22.738778
103.754709	3711.620222	22.743795
103.784664	3714.058228	22.748813
104.070308	3719.389340	22.753831
104.234236	3729.173121	22.758848
104.180172	3742.236814	22.763866
104.337975	3738.445861	22.768883
104.052067	3736.462901	22.773901
104.148983	3728.386841	22.778919
104.706487	3734.968522	22.783936
104.600689	3741.388262	22.788954
104.495889	3726.157609	22.793971
104.599358	3732.927391	22.798989
104.551730	3740.556357	22.804007
104.750471	3761.046288	22.809024
104.577478	3765.547157	22.814042
104.742066	3769.376614	22.819059
104.830254	3779.640457	22.824077
105.348587	3788.675943	22.829095
105.546267	3799.906313	22.834112
105.410270	3793.743849	22.839130
106.109567	3792.313421	22.844147
105.575713	3802.707547	22.849165
105.687535	3795.384206	22.854183
105.805838	3794.064408	22.859200
105.831881	3809.463042	22.864218
106.225025	3814.627690	22.869235
106.157218	3820.065112	22.874253
105.943463	3822.552792	22.879271
106.154359	3823.190057	22.884288
105.967209	3823.567132	22.889306
106.344090	3840.107527	22.894323
106.352593	3851.075016	22.899341
106.578261	3847.231447	22.904359
106.420885	3853.641960	22.909376
106.938424	3868.202656	22.914394
107.344419	3872.761028	22.919411
107.524163	3874.729171	22.924429
107.767248	3869.271964	22.929447
107.689007	3864.785039	22.934464
107.627823	3873.132323	22.939482
107.966131	3863.891689	22.944499
108.076767	3871.632204	22.949517
108.278843	3865.658272	22.954535
108.462687	3865.410186	22.959552
108.263036	3866.662856	22.964570
108.365780	3852.798433	22.969587
108.315297	3864.750306	22.974605
108.310035	3859.812965	22.979623
108.303364	3860.686794	22.984640
108.457691	3890.776716	22.989658
108.517832	3886.318831	22.994675
108.424176	3894.796922	22.999693
108.555562	3891.718518	23.004711
108.849648	3902.652835	23.009728
109.216421	3923.489857	23.014746
109.034136	3925.760291	23.019763
109.046163	3917.962536	23.024781
109.213269	3926.774778	23.029799
109.973900	3928.658307	23.034816
109.557992	3938.223431	23.039834
110.322768	3936.866040	23.044851
110.562303	3937.433816	23.049869
110.671304	3933.269195	23.054887
110.731253	3932.780075	23.059904
110.547281	3928.175003	23.064922
110.652815	3932.301313	23.069939
110.639847	3933.603895	23.074957
110.603682	3934.091345	23.079975
110.907852	3931.989871	23.084992
110.785324	3931.786431	23.090010
111.225239	3928.599206	23.095027
111.585835	3932.591215	23.100045
111.198840	3937.342262	23.105063
110.946983	3929.461360	23.110080
110.936144	3936.328799	23.115098
111.032908	3937.121104	23.120115
111.321485	3952.571745	23.125133
110.878945	3970.356981	23.130151
111.556613	3969.124787	23.135168
111.458035	3977.387174	23.140186
111.990552	3984.782118	23.145203
111.790541	3990.410812	23.150221
112.022195	3990.934261	23.155239
112.152559	3993.403928	23.160256
111.879849	4000.492713	23.165274
112.002314	4014.930674	23.170291
112.229844	4022.024285	23.175309
112.186739	4028.230190	23.180327
112.450496	4032.220711	23.185344
112.461999	4053.987547	23.190362
112.619243	4058.087698	23.195379
112.940543	4055.609944	23.200397
112.665116	4066.494726	23.205415
113.004956	4078.124659	23.210432
113.147829	4091.692030	23.215450
113.421796	4093.321914	23.220467
113.423266	4100.240084	23.225485
113.510063	4121.091498	23.230503
113.811641	4114.772767	23.235520
113.561496	4123.471562	23.240538
113.751794	4134.553789	23.245555
113.918129	4139.745614	23.250573
113.860905	4148.003363	23.255591
114.411582	4145.797380	23.260608
114.455878	4162.314007	23.265626
114.490397	4168.548402	23.270643
115.302811	4159.461817	23.275661
115.259543	4162.717389	23.280679
115.427428	4155.493749	23.285696
115.698025	4167.190752	23.290714
115.935806	4161.795788	23.295731
116.400886	4156.624923	23.300749
116.383633	4154.509214	23.305767
116.218704	4126.955984	23.310784
116.270569	4122.894046	23.315802
116.383919	4124.613691	23.320819
116.293663	4130.492195	23.325837
116.465411	4122.690585	23.330855
116.241240	4120.641858	23.335872
115.932421	4119.615002	23.340890
115.875076	4119.743785	23.345907
116.068013	4138.499298	23.350925
116.001115	4151.185110	23.355943
116.409239	4160.702037	23.360960
116.406513	4179.892828	23.365978
116.318857	4180.712823	23.370995
116.511835	4193.333638	23.376013
116.232108	4212.482955	23.381031
116.986293	4213.791089	23.386048
117.129519	4229.546526	23.391066
116.939450	4242.319686	23.396083
117.815100	4243.412458	23.401101
117.712869	4251.449566	23.406119
117.831245	4246.994198	23.411136
117.656617	4258.109144	23.416154
118.089002	4267.477842	23.421171
118.075152	4269.797424	23.426189
118.039838	4286.416042	23.431207
118.641583	4272.549981	23.436224
118.395036	4284.578315	23.441242
118.184092	4281.025302	23.446259
118.890965	4292.972894	23.451277
118.664563	4315.237696	23.456295
119.046825	4303.689408	23.461312
119.273618	4306.159921	23.466330
119.322693	4302.329190	23.471347
119.822775	4294.009660	23.476365
119.547563	4294.002517	23.481383
119.823507	4290.894528	23.486400
119.772751	4288.711295	23.491418
119.547449	4298.279401	23.496435
120.034749	4304.371643	23.501453
119.840509	4316.587153	23.506471
120.395237	4322.498503	23.511488
120.165473	4326.516997	23.516506
120.083765	4323.438023	23.521523
120.785327	4332.414059	23.526541
120.472189	4346.870291	23.531559
120.803745	4340.863746	23.536576
120.648570	4346.636890	23.541594
120.721533	4343.219496	23.546611
120.945087	4346.602642	23.551629
121.498745	4361.014256	23.556647
121.664687	4369.371697	23.561664
121.568685	4369.246404	23.566682
121.841101	4376.283648	23.571699
122.157770	4363.265822	23.576717
122.118411	4377.221474	23.581735
122.128085	4367.713960	23.586752
122.526598	4367.840208	23.591770
121.876059	4379.281778	23.596787
122.223204	4360.370425	23.601805
121.868572	4373.434182	23.606823
122.428203	4391.267830	23.611840
122.441397	4399.286014	23.616858
122.372103	4402.809953	23.621875
122.853862	4403.084969	23.626893
122.682818	4426.345451	23.631911
122.839804	4424.456603	23.636928
123.054228	4430.968224	23.641946
122.800967	4437.335550	23.646963
123.314944	4455.454344	23.651981
123.252803	4452.775257	23.656999
123.718734	4445.066405	23.662016
124.151440	4460.525130	23.667034
124.167277	4473.490802	23.672051
124.729161	4468.741166	23.677069
124.849195	4470.093454	23.682087
125.424658	4443.812366	23.687104
125.338527	4417.059532	23.692122
125.221114	4411.168522	23.697139
126.070025	4411.119104	23.702157
125.690931	4392.499190	23.707175
125.586720	4373.478530	23.712192
125.471175	4364.596595	23.717210
125.683127	4370.222535	23.722227
125.884429	4356.341562	23.727245
125.536631	4366.392257	23.732263
125.763461	4369.298332	23.737280
125.559077	4371.617512	23.742298
125.388106	4373.503282	23.747315
125.846788	4378.224475	23.752333
125.764645	4394.662205	23.757351
125.712343	4403.130328	23.762368
125.879800	4410.477004	23.767386
125.921916	4423.268790	23.772403
126.158647	4437.548139	23.777421
126.246530	4445.414919	23.782439
126.113795	4449.631045	23.787456
126.409277	4472.563514	23.792474
126.524428	4478.437652	23.797491
126.604142	4491.010387	23.802509
126.671419	4507.719556	23.807527
126.808644	4508.602620	23.812544
126.830307	4526.328588	23.817562
126.852495	4542.939193	23.822579
127.246619	4554.046634	23.827597
127.238731	4569.231287	23.832615
127.427634	4581.011127	23.837632
128.170196	4596.010444	23.842650
127.653237	4610.433333	23.847667
128.231725	4611.714915	23.852685
128.593503	4605.179309	23.857703
129.484304	4605.466910	23.862720
129.724510	4607.136505	23.867738
129.368355	4590.675283	23.872755
129.406150	4582.840490	23.877773
129.489025	4584.069985	23.882791
129.528411	4580.698465	23.887808
129.875561	4573.150902	23.892826
129.842894	4587.994836	23.897843
129.816966	4580.319044	23.902861
130.264535	4597.739725	23.907879
130.084082	4611.907230	23.912896
130.362498	4612.273821	23.917914
130.428842	4621.128143	23.922931
130.669578	4619.279262	23.927949
130.392347	4616.070707	23.932967
130.000710	4620.756588	23.937984
130.367492	4615.115667	23.943002
130.430419	4631.705204	23.948019
130.566270	4640.909148	23.953037
130.779756	4645.660642	23.958055
131.007257	4638.769186	23.963072
130.652337	4660.873772	23.968090
130.760355	4676.602610	23.973107
130.794332	4674.232304	23.978125
131.179043	4695.142098	23.983143
131.351924	4708.185798	23.988160
131.745019	4715.273393	23.993178
131.499388	4725.726614	23.998195
131.878497	4730.508027	24.003213
131.941190	4745.535034	24.008231
132.541451	4761.805749	24.013248
132.397512	4766.204251	24.018266
132.762198	4776.696230	24.023283
132.651999	4772.814713	24.028301
133.020267	4779.000011	24.033319
132.773993	4780.672683	24.038336
133.326213	4790.129059	24.043354
133.173883	4802.444877	24.048371
133.402470	4803.502907	24.053389
133.228555	4806.002023	24.058407
133.562693	4812.906796	24.063424
133.860374	4824.535845	24.068442
133.721089	4831.951055	24.073459
134.144740	4830.956899	24.078477
134.131451	4841.377454	24.083495
134.250350	4845.577327	24.088512
134.438162	4845.595562	24.093530
134.521893	4856.083774	24.098547
134.746938	4850.842778	24.103565
134.806205	4859.072263	24.108583
135.128531	4874.446346	24.113600
135.209327	4878.351877	24.118618
135.344406	4886.334447	24.123635
135.506863	4884.806140	24.128653
135.544980	4880.640820	24.133671
135.417901	4889.704097	24.138688
136.127180	4892.520474	24.143706
135.924656	4905.750778	24.148723
135.875143	4911.906930	24.153741
136.447851	4910.797424	24.158759
135.902551	4926.082424	24.163776
136.373640	4926.115897	24.168794
135.879081	4943.810316	24.173811
136.663947	4957.753570	24.178829
136.715578	4971.160115	24.183847
136.745560	4979.481325	24.188864
137.048839	4973.684181	24.193882
137.051842	4990.431658	24.198899
137.137173	5012.884232	24.203917
137.335975	5011.921523	24.208935
137.337614	5022.263235	24.213952
137.836695	5034.883446	24.218970
137.586350	5052.306910	24.223987
137.750619	5048.195536	24.229005
138.406508	5057.586253	24.234023
138.144383	5081.665148	24.239040
138.472981	5088.826195	24.244058
138.548552	5089.940408	24.249075
138.811685	5086.146832	24.254093
138.845119	5083.803339	24.259111
139.066728	5101.680774	24.264128
139.503310	5100.618222	24.269146
139.491068	5104.974549	24.274163
139.489945	5101.597261	24.279181
139.854561	5101.028309	24.284199
139.872323	5111.239713	24.289216
139.918562	5100.525092	24.294234
140.006490	5097.945408	24.299251
140.120604	5097.412310	24.304269
140.603205	5119.028172	24.309287
139.937525	5129.327606	24.314304
140.186982	5134.109314	24.319322
140.199460	5141.776697	24.324339
140.142638	5149.733222	24.329357
140.861644	5155.907378	24.334375
140.639091	5166.223815	24.339392
140.787069	5184.882729	24.344410
140.723418	5180.964776	24.349427
141.176312	5200.435508	24.354445
141.321175	5211.344329	24.359463
141.656513	5220.292289	24.364480
141.874418	5215.173700	24.369498
141.796759	5235.357686	24.374515
142.373648	5234.818505	24.379533
143.130130	5231.865046	24.384551
143.210649	5236.995540	24.389568
143.346046	5228.039382	24.394586
143.410603	5220.904651	24.399603
143.179929	5224.816402	24.404621
143.970839	5227.096623	24.409639
143.530069	5231.042029	24.414656
143.909271	5224.214110	24.419674
143.543408	5232.005471	24.424691
143.732664	5219.299439	24.429709
143.748195	5217.865603	24.434727
143.432884	5228.037298	24.439744
143.630999	5235.641396	24.444762
143.940148	5241.112355	24.449779
143.974814	5249.212355	24.454797
144.150076	5268.262889	24.459815
143.994769	5280.437806	24.464832
144.226823	5281.062843	24.469850
144.384134	5314.361576	24.474867
144.545595	5323.308683	24.479885
144.731366	5329.792506	24.484903
144.686905	5356.748113	24.489920
144.877076	5370.954368	24.494938
145.033008	5375.170088	24.499955
145.608429	5386.303750	24.504973
145.655566	5380.306190	24.509991
145.579553	5400.711441	24.515008
145.990802	5407.043216	24.520026
145.931097	5418.725304	24.525043
145.842496	5429.746764	24.530061
146.587244	5438.521478	24.535079
146.442563	5451.059399	24.540096
146.557323	5446.838258	24.545114
146.722694	5467.448759	24.550131
146.619828	5480.739648	24.555149
146.924670	5486.829761	24.560167
147.276596	5498.958851	24.565184
147.259773	5506.738557	24.570202
147.422913	5512.825404	24.575219
147.756188	5517.723615	24.580237
148.271460	5528.080791	24.585255
148.183652	5551.808350	24.590272
148.381351	5551.097071	24.595290
148.901548	5542.006243	24.600307
149.077352	5545.854692	24.605325
149.075765	5540.460915	24.610343
148.737678	5548.036567	24.615360
148.858150	5544.754917	24.620378
149.117076	5560.469789	24.625395
149.247098	5561.582578	24.630413
149.952766	5547.896096	24.635431
150.081827	5556.862280	24.640448
150.314778	5545.428489	24.645466
150.382496	5548.536927	24.650483
150.598618	5541.499736	24.655501
150.599682	5543.439645	24.660519
150.499347	5543.619919	24.665536
150.789057	5544.350873	24.670554
151.085747	5549.054506	24.675571
151.523871	5575.598504	24.680589
151.744116	5571.109550	24.685607
151.475962	5568.802720	24.690624
151.318347	5573.114779	24.695642
151.478901	5574.652412	24.700659
151.482575	5575.516685	24.705677
151.522889	5567.708543	24.710695
151.369707	5587.527046	24.715712
151.732328	5595.295312	24.720730
152.125313	5606.940894	24.725747
151.837833	5616.807955	24.730765
152.136446	5626.435128	24.735783
152.065331	5650.606593	24.740800
152.151924	5658.531697	24.745818
152.474337	5666.792109	24.750835
152.437121	5683.566115	24.755853
152.702117	5701.124073	24.760871
153.353391	5703.526767	24.765888
153.610636	5698.617108	24.770906
154.025177	5700.310500	24.775923
153.987454	5723.129395	24.780941
154.475378	5719.155351	24.785959
154.440798	5719.945057	24.790976
154.496622	5725.408411	24.795994
154.533910	5719.149322	24.801011
155.046275	5723.070876	24.806029
154.708478	5714.203441	24.811047
155.128245	5725.088333	24.816064
155.345160	5717.497968	24.821082
155.304529	5718.822768	24.826099
154.950824	5712.792973	24.831117
155.476858	5724.783687	24.836135
155.291107	5739.265817	24.841152
155.243984	5751.545428	24.846170
155.594118	5745.312256	24.851187
155.338011	5763.912727	24.856205
155.566880	5761.873553	24.861223
155.644752	5786.051979	24.866240
155.829228	5803.790846	24.871258
156.559778	5812.719443	24.876275
156.482088	5839.336551	24.881293
156.441784	5845.920781	24.886311
156.755663	5859.769919	24.891328
156.529438	5877.537525	24.896346
156.970035	5883.730552	24.901363
157.265311	5904.502886	24.906381
157.796438	5903.353973	24.911399
157.428686	5913.163295	24.916416
157.495595	5931.889760	24.921434
157.698154	5932.626221	24.926451
158.235131	5953.311498	24.931469
158.269266	5969.257509	24.936487
158.270863	5978.544322	24.941504
158.252478	5980.056743	24.946522
158.972476	6001.631538	24.951539
158.927938	6006.956227	24.956557
159.079886	6010.193678	24.961575
159.155329	6028.461922	24.966592
159.652268	6031.637087	24.971610
159.919890	6028.126097	24.976627
159.773515	6044.174808	24.981645
160.189724	6055.196024	24.986663
160.298478	6050.014746	24.991680
160.324905	6053.017718	24.996698
160.839519	6057.717229	25.001715
160.867338	6079.554938	25.006733
161.549992	6080.346168	25.011751
161.596739	6092.692660	25.016768
161.411256	6096.526769	25.021786
161.827121	6086.329454	25.026803
161.869712	6086.267035	25.031821
162.042980	6082.947080	25.036839
162.028914	6074.556440	25.041856
161.962461	6084.144071	25.046874
162.190400	6099.195232	25.051891
162.606490	6106.248005	25.056909
162.734787	6101.836895	25.061927
163.118849	6105.775814	25.066944
162.851775	6108.360420	25.071962
162.848041	6096.945541	25.076979
163.097081	6099.373140	25.081997
163.780604	6079.676603	25.087015
163.980261	6085.139056	25.092032
163.735837	6092.735930	25.097050
164.077601	6101.128739	25.102067
164.003710	6105.039034	25.107085
164.414061	6106.243232	25.112103
164.263214	6114.033607	25.117120
163.917609	6110.411887	25.122138
164.267016	6104.187366	25.127155
164.622158	6129.086015	25.132173
164.818937	6137.153164	25.137191
165.224283	6140.029754	25.142208
164.928638	6144.008793	25.147226
165.090202	6158.106437	25.152243
165.246434	6167.811913	25.157261
165.249907	6178.892939	25.162279
165.776424	6197.077751	25.167296
165.471884	6215.811509	25.172314
165.883441	6207.039839	25.177331
165.923232	6232.645727	25.182349
166.156896	6238.872005	25.187367
166.382186	6241.796811	25.192384
166.097339	6262.348456	25.197402
166.585260	6269.463823	25.202419
166.459294	6292.475108	25.207437
166.856596	6298.751343	25.212455
167.313296	6315.281436	25.217472
167.225746	6339.245651	25.222490
167.963907	6334.480223	25.227507
167.794994	6338.779458	25.232525
167.987749	6352.948336	25.237543
168.200129	6362.487548	25.242560
168.225179	6372.215635	25.247578
168.247217	6377.713363	25.252595
168.479469	6396.794865	25.257613
168.538286	6401.249647	25.262631
168.879395	6418.805591	25.267648
168.615375	6436.095843	25.272666
169.369228	6438.582688	25.277683
169.245517	6469.686193	25.282701
169.544357	6479.977116	25.287719
169.993796	6481.297530	25.292736
169.923673	6508.595056	25.297754
170.296189	6505.270005	25.302771
170.216045	6513.532909	25.307789
170.364947	6534.031817	25.312807
170.721695	6537.491859	25.317824
170.919474	6542.616065	25.322842
170.934081	6553.456759	25.327859
171.274226	6566.404779	25.332877
171.201821	6577.331301	25.337895
171.532389	6573.452559	25.342912
171.395588	6592.408502	25.347930
171.541140	6601.037659	25.352947
172.083594	6601.181014	25.357965
172.067485	6603.718738	25.362983
172.733378	6620.062042	25.368000
172.670189	6631.574675	25.373018
173.270694	6619.717114	25.378035
173.090390	6627.996460	25.383053
173.015323	6627.126294	25.388071
173.037408	6635.432393	25.393088
172.949668	6655.682923	25.398106
173.376524	6649.662332	25.403123
173.420642	6672.552842	25.408141
173.281392	6680.987452	25.413159
173.757839	6696.726027	25.418176
173.702596	6720.504094	25.423194
173.840783	6722.225280	25.428211
174.689637	6748.377063	25.433229
174.583272	6756.713122	25.438247
174.800827	6759.542457	25.443264
174.605093	6776.806402	25.448282
175.208287	6776.076765	25.453299
175.258645	6792.552546	25.458317
175.462682	6808.189832	25.463335
175.967127	6813.335605	25.468352
176.205957	6822.948545	25.473370
176.462964	6829.324664	25.478387
176.686699	6832.707528	25.483405
176.594736	6835.849104	25.488423
176.924890	6830.854131	25.493440
176.836491	6833.551592	25.498458
177.459755	6844.956158	25.503475
177.169631	6856.688249	25.508493
177.191536	6862.548532	25.513511
177.659264	6859.696281	25.518528
177.508478	6882.726061	25.523546
177.933227	6879.755133	25.528563
177.980481	6899.336086	25.533581
178.028395	6908.323244	25.538599
178.546087	6922.832380	25.543616
178.441080	6925.428720	25.548634
178.765942	6940.608221	25.553651
178.953875	6943.396189	25.558669
179.273839	6945.852725	25.563687
179.581833	6947.258084	25.568704
179.559394	6963.542492	25.573722
179.506744	6971.876544	25.578739
180.135432	6973.958758	25.583757
180.296981	6978.028208	25.588775
180.725476	6987.622127	25.593792
180.467051	7001.204845	25.598810
180.694025	6998.088978	25.603827
181.200073	6999.871601	25.608845
180.973023	7013.406412	25.613863
180.878820	7009.864279	25.618880
181.331270	7029.535059	25.623898
181.429666	7041.186504	25.628915
181.694962	7041.891784	25.633933
181.839337	7047.041063	25.638951
182.480614	7056.126680	25.643968
182.386810	7075.803715	25.648986
182.603756	7075.255292	25.654003
182.443349	7072.561096	25.659021
182.108934	7073.673256	25.664039
182.790960	7082.902365	25.669056
182.677876	7099.332430	25.674074
182.478552	7109.071068	25.679092
182.531479	7125.496335	25.684109
182.871697	7144.285294	25.689127
183.709912	7155.765888	25.694144
183.399771	7170.466787	25.699162
183.778686	7187.232482	25.704180
183.991955	7198.654016	25.709197
184.140339	7220.757000	25.714215
184.793224	7218.505526	25.719232
184.941608	7227.178652	25.724250
185.060984	7236.148229	25.729268
185.570430	7235.521300	25.734285
185.500230	7245.657767	25.739303
185.926799	7252.431962	25.744320
185.830835	7251.552740	25.749338
186.173880	7266.870445	25.754356
186.648303	7278.216546	25.759373
186.588983	7277.464174	25.764391
186.967718	7276.444495	25.769408
187.092098	7279.595551	25.774426
186.802337	7281.956565	25.779444
187.250219	7303.775931	25.784461
187.184831	7315.094852	25.789479
187.514014	7310.963297	25.794496
187.220180	7319.334146	25.799514
187.610202	7337.516087	25.804532
187.548233	7344.454419	25.809549
187.596691	7370.849992	25.814567
187.887105	7374.290078	25.819584
188.214979	7397.567048	25.824602
188.576669	7413.585970	25.829620
188.715408	7427.602780	25.834637
188.634489	7448.700791	25.839655
189.005374	7437.835207	25.844672
189.112604	7465.533301	25.849690
189.161849	7470.269683	25.854708
189.742297	7486.493028	25.859725
189.772388	7499.781708	25.864743
190.078642	7505.611602	25.869760
190.245527	7526.717656	25.874778
190.574915	7538.435429	25.879796
190.866093	7544.562553	25.884813
191.035630	7558.132251	25.889831
191.486578	7562.851795	25.894848
191.354519	7561.807794	25.899866
191.498732	7559.379563	25.904884
192.227708	7561.815714	25.909901
192.125734	7576.914582	25.914919
192.392894	7583.616195	25.919936
192.692334	7585.384674	25.924954
192.566261	7586.304383	25.929972
193.014182	7591.778367	25.934989
192.539626	7590.752109	25.940007
193.407689	7583.306852	25.945024
193.517706	7597.991263	25.950042
193.953634	7593.816129	25.955060
194.408927	7590.683069	25.960077
194.328020	7591.451660	25.965095
194.626241	7586.597428	25.970112
194.695758	7582.209381	25.975130
194.771559	7586.051835	25.980148
194.946923	7586.801705	25.985165
194.388153	7611.179467	25.990183
194.761035	7610.260821	25.995200
194.852481	7628.457250	26.000218
195.004402	7647.617039	26.005236
195.245352	7645.903282	26.010253
195.430618	7672.269597	26.015271
195.732180	7682.504898	26.020288
195.815591	7691.289463	26.025306
196.304506	7706.945757	26.030324
196.630310	7708.119675	26.035341
196.773715	7720.995219	26.040359
196.869705	7732.149694	26.045376
196.816087	7747.858063	26.050394
196.662814	7758.161926	26.055412
197.296116	7770.461948	26.060429
197.137854	7791.682384	26.065447
197.367551	7805.104902	26.070464
197.811060	7819.361297	26.075482
197.815031	7835.928821	26.080500
198.310089	7836.689289	26.085517
198.548799	7862.044675	26.090535
198.726489	7861.035791	26.095552
199.452220	7867.157089	26.100570
199.167099	7883.405527	26.105588
199.739660	7887.642671	26.110605
199.750682	7891.287535	26.115623
199.860311	7895.212499	26.120640
200.638767	7896.297022	26.125658
200.911876	7914.315315	26.130676
201.113580	7915.145769	26.135693
200.918544	7917.716735	26.140711
201.237834	7920.777785	26.145728
201.379041	7922.437137	26.150746
201.176496	7924.229467	26.155764
201.776738	7933.232814	26.160781
201.895625	7949.519994	26.165799
201.828587	7948.939078	26.170816
202.144727	7941.262906	26.175834
201.858656	7951.268232	26.180852
202.173723	7965.847716	26.185869
202.488190	7987.253654	26.190887
202.651819	7978.929245	26.195904
202.901986	8000.369857	26.200922
202.895173	8013.766128	26.205940
203.276592	8017.851726	26.210957
203.253198	8040.379977	26.215975
203.448908	8053.973970	26.220992
203.806896	8063.657830	26.226010
203.691466	8083.142065	26.231028
204.026713	8087.941474	26.236045
204.247088	8109.425940	26.241063
204.299742	8114.281676	26.246080
204.863805	8129.662375	26.251098
204.710545	8146.972505	26.256116
205.413029	8152.370747	26.261133
205.638235	8173.095806	26.266151
205.449007	8178.371962	26.271168
205.726587	8183.072567	26.276186
205.910195	8201.575275	26.281204
205.820013	8215.108116	26.286221
206.389418	8239.354888	26.291239
206.581694	8245.843512	26.296256
206.517840	8261.866113	26.301274
206.400747	8282.428611	26.306292
206.987248	8298.206625	26.311309
207.370806	8320.176273	26.316327
207.251403	8338.959548	26.321344
207.569325	8353.707490	26.326362
207.847827	8371.089597	26.331380
208.083875	8380.189502	26.336397
208.489381	8398.014685	26.341415
208.527280	8402.039518	26.346432
209.250496	8422.110720	26.351450
209.288574	8444.097215	26.356468
209.578946	8429.904376	26.361485
210.695212	8441.872390	26.366503
210.617584	8462.448835	26.371520
210.813909	8457.213169	26.376538
210.496858	8458.160936	26.381556
210.742882	8452.951417	26.386573
211.234010	8443.571664	26.391591
211.644350	8430.413950	26.396608
212.090795	8415.171770	26.401626
212.134109	8425.547142	26.406644
212.529446	8431.127334	26.411661
212.422606	8426.073636	26.416679
212.765614	8435.612966	26.421696
213.035282	8438.724378	26.426714
213.365189	8435.488964	26.431732
213.682356	8436.524973	26.436749
213.244627	8443.265054	26.441767
213.171676	8445.399203	26.446784
213.693792	8444.893753	26.451802
213.477921	8448.784048	26.456820
213.539382	8448.937403	26.461837
213.577614	8455.978000	26.466855
213.618945	8474.477049	26.471872
214.418709	8470.879832	26.476890
214.610681	8499.916312	26.481908
214.593156	8501.874735	26.486925
214.994640	8501.187490	26.491943
215.088603	8512.231771	26.496960
215.364415	8535.468109	26.501978
215.121541	8540.445536	26.506996
215.775846	8556.533620	26.512013
215.850000	8566.085237	26.517031
215.456478	8577.006710	26.522048
216.356962	8597.385730	26.527066
216.644728	8610.029253	26.532084
216.421034	8615.691984	26.537101
216.954624	8625.325602	26.542119
216.993020	8635.158344	26.547136
217.364653	8645.323951	26.552154
217.095094	8669.775847	26.557172
217.415853	8686.651564	26.562189
217.478254	8705.215020	26.567207
217.588939	8733.786847	26.572224
218.042680	8742.539233	26.577242
218.136369	8766.316069	26.582260
218.547627	8784.260448	26.587277
218.743439	8799.968055	26.592295
218.760613	8821.164499	26.597312
219.189688	8833.707555	26.602330
219.752512	8856.320029	26.607348
220.102794	8870.375108	26.612365
220.139288	8883.091067	26.617383
219.883285	8899.153540	26.622400
220.161767	8901.882213	26.627418
220.505782	8931.192790	26.632436
220.800775	8951.290789	26.637453
221.252630	8957.796659	26.642471
221.403029	8973.063142	26.647488
221.346166	8994.478922	26.652506
221.551938	9013.813891	26.657524
221.877681	9029.869743	26.662541
222.362756	9045.702910	26.667559
222.437037	9054.747414	26.672576
222.928629	9060.389325	26.677594
223.108858	9083.882347	26.682612
223.531253	9089.928484	26.687629
223.943074	9097.284284	26.692647
223.849745	9110.293699	26.697664
224.285919	9122.496983	26.702682
224.152191	9134.019557	26.707700
224.380781	9142.459369	26.712717
225.266138	9152.083431	26.717735
224.846249	9160.218417	26.722752
224.940090	9162.819636	26.727770
225.049981	9179.008755	26.732788
225.111781	9184.892985	26.737805
225.308238	9198.196307	26.742823
225.591575	9229.090405	26.747840
225.978838	9233.037439	26.752858
226.113456	9259.105404	26.757876
226.039570	9269.684981	26.762893
226.127726	9284.579524	26.767911
226.850157	9294.920197	26.772928
227.244054	9307.214383	26.777946
227.541404	9315.922982	26.782964
227.964145	9315.864724	26.787981
229.053382	9309.471194	26.792999
229.469553	9310.895258	26.798016
229.933889	9306.042769	26.803034
229.660475	9300.319296	26.808052
229.656128	9290.307813	26.813069
230.251448	9293.007456	26.818087
230.153060	9298.963306	26.823104
230.136470	9290.386270	26.828122
230.391181	9305.165617	26.833140
230.528257	9309.762216	26.838157
230.795693	9302.543625	26.843175
230.761536	9316.264752	26.848192
230.427913	9315.233123	26.853210
230.934812	9330.987196	26.858228
230.940180	9346.721677	26.863245
231.054286	9358.450897	26.868263
230.873871	9384.721185	26.873280
230.972670	9401.248063	26.878298
231.799077	9425.226454	26.883316
231.766353	9437.095929	26.888333
232.344901	9458.022075	26.893351
232.420329	9481.810973	26.898368
233.059320	9482.977830	26.903386
233.054081	9506.626167	26.908404
233.321608	9517.831265	26.913421
234.294495	9510.070933	26.918439
234.630645	9526.710104	26.923456
234.530003	9509.844669	26.928474
235.220387	9527.047123	26.933492
235.452395	9531.931635	26.938509
235.414560	9540.986175	26.943527
235.497507	9546.666790	26.948544
235.762981	9539.393279	26.953562
235.805151	9541.436141	26.958580
236.121494	9565.377686	26.963597
236.278910	9570.353783	26.968615
236.177181	9577.206919	26.973632
236.420145	9579.888221	26.978650
236.653159	9598.445520	26.983668
236.728300	9612.913988	26.988685
237.097963	9625.970519	26.993703
236.763994	9645.759614	26.998720
237.279549	9653.546985	27.003738
237.400555	9676.742169	27.008756
237.618903	9703.926331	27.013773
237.890170	9712.193671	27.018791
238.229202	9738.235250	27.023808
238.211281	9755.185896	27.028826
238.594498	9775.704717	27.033844
238.823164	9788.218263	27.038861
239.148149	9810.111741	27.043879
238.767323	9826.349379	27.048896
239.027246	9850.527930	27.053914
239.577562	9880.997747	27.058932
239.918075	9888.484319	27.063949
240.617710	9894.744823	27.068967
241.049304	9907.556172	27.073984
241.203042	9935.386845	27.079002
241.587778	9944.337662	27.084020
241.282743	9958.502865	27.089037
242.393923	9960.901469	27.094055
242.294001	9969.809310	27.099072
242.746859	9982.242032	27.104090
242.848465	9993.726453	27.109108
242.792750	10002.678736	27.114125
243.278731	10011.314408	27.119143
243.258587	10033.552568	27.124160
243.405179	10038.462905	27.129178
243.777698	10058.572632	27.134196
244.079654	10069.945552	27.139213
244.472069	10083.107284	27.144231
244.886855	10097.086193	27.149248
245.268376	10105.479811	27.154266
245.508550	10115.609002	27.159284
245.305267	10124.678043	27.164301
245.690924	10129.687679	27.169319
245.716651	10141.610684	27.174336
245.601268	10158.906228	27.179354
246.067520	10165.934874	27.184372
246.109129	10189.465869	27.189389
246.906753	10200.062132	27.194407
246.915554	10222.594996	27.199424
247.460940	10226.182675	27.204442
247.801738	10228.462814	27.209460
247.704838	10253.423284	27.214477
247.833348	10251.664711	27.219495
248.330591	10278.132305	27.224512
248.459167	10281.232018	27.229530
248.829475	10294.791671	27.234548
249.012004	10314.524564	27.239565
249.624921	10311.942310	27.244583
249.200470	10329.937107	27.249600
249.398968	10344.671887	27.254618
249.820201	10365.218032	27.259636
249.825898	10379.336643	27.264653
250.309881	10399.348896	27.269671
250.017986	10415.658548	27.274688
250.435273	10428.748537	27.279706
250.482172	10442.187252	27.284724
250.604572	10470.164465	27.289741
250.857678	10498.782757	27.294759
250.961298	10520.663136	27.299776
251.412124	10545.968260	27.304794
251.665119	10562.758275	27.309812
251.807262	10593.617721	27.314829
252.024471	10616.479433	27.319847
252.243990	10647.841028	27.324864
252.139503	10663.976976	27.329882
252.971521	10681.214694	27.334900
253.120923	10715.634603	27.339917
253.917842	10726.072171	27.344935
254.391381	10755.368581	27.349952
254.210744	10765.783051	27.354970
254.794780	10778.195478	27.359988
255.054384	10797.778645	27.365005
255.844055	10807.212094	27.370023
255.859072	10813.610794	27.375040
256.495601	10810.644629	27.380058
256.830520	10812.582318	27.385076
256.922364	10824.634744	27.390093
256.988300	10833.070227	27.395111
257.626232	10828.144989	27.400128
257.550683	10836.425074	27.405146
258.322574	10837.142195	27.410164
258.552644	10850.289830	27.415181
258.538180	10854.804107	27.420199
259.023756	10861.243514	27.425216
258.897075	10856.449325	27.430234
259.350693	10853.561782	27.435252
259.618882	10879.024802	27.440269
259.429800	10888.470048	27.445287
259.529192	10895.007179	27.450304
259.610639	10911.138293	27.455322
260.004999	10925.728141	27.460340
259.881219	10945.813724	27.465357
259.814740	10960.666972	27.470375
260.240407	10986.215057	27.475392
260.113117	11009.218318	27.480410
260.568565	11026.918079	27.485428
260.753595	11059.041239	27.490445
261.088233	11088.453461	27.495463
261.403562	11107.608258	27.500480
261.600742	11134.760623	27.505498
262.213447	11160.406148	27.510516
262.227102	11183.746382	27.515533
262.659777	11212.763803	27.520551
263.057945	11230.393233	27.525568
263.404881	11253.818275	27.530586
263.982618	11267.663102	27.535604
263.820426	11279.713706	27.540621
264.396337	11304.486395	27.545639
264.589439	11309.187427	27.550656
265.021033	11333.932891	27.555674
265.147383	11346.985238	27.560692
264.941794	11359.194628	27.565709
265.380576	11374.809506	27.570727
265.501353	11391.186504	27.575744
265.734182	11408.009216	27.580762
266.411788	11424.133211	27.585780
266.881832	11440.223457	27.590797
266.837509	11444.861211	27.595815
267.563379	11458.097710	27.600832
268.030794	11466.337055	27.605850
268.187427	11463.746160	27.610868
268.274850	11481.388149	27.615885
268.374847	11498.216387	27.620903
268.696446	11498.933503	27.625920
268.673220	11521.361761	27.630938
269.403456	11527.994318	27.635956
269.527039	11535.805661	27.640973
269.446571	11555.372384	27.645991
269.814032	11570.597805	27.651008
270.131170	11594.075724	27.656026
270.051960	11610.936370	27.661044
270.355377	11632.966809	27.666061
270.355329	11657.394333	27.671079
270.938336	11669.210330	27.676096
271.238714	11685.288925	27.681114
271.558477	11705.595700	27.686132
271.704638	11727.996784	27.691149
271.944533	11747.245637	27.696167
272.920661	11759.550639	27.701184
273.223717	11784.695479	27.706202
273.468664	11787.495010	27.711220
273.776804	11800.299076	27.716237
273.813213	11821.485105	27.721255
274.236702	11824.150027	27.726272
274.338092	11841.433839	27.731290
274.730173	11842.411537	27.736308
274.628183	11870.104960	27.741325
274.948454	11880.371243	27.746343
275.551710	11891.771023	27.751360
275.834911	11909.569038	27.756378
276.552813	11905.980404	27.761396
276.842852	11922.061005	27.766413
277.255821	11938.115823	27.771431
277.215327	11929.908699	27.776448
277.447640	11935.700085	27.781466
277.763562	11940.564640	27.786484
277.832757	11956.074793	27.791501
277.677911	11964.654295	27.796519
278.013121	11977.895140	27.801536
277.907391	12003.412975	27.806554
278.666609	12010.193638	27.811572
279.436871	12013.684868	27.816589
279.874048	12031.949914	27.821607
280.555762	12033.617129	27.826624
280.610795	12029.787483	27.831642
281.175573	12019.519173	27.836660
281.381530	12027.811499	27.841677
281.270157	12022.197972	27.846695
281.636754	12020.693117	27.851712
281.354178	12031.281888	27.856730
281.272146	12034.651284	27.861748
281.366841	12048.486589	27.866765
281.758298	12062.272617	27.871783
282.026095	12080.388661	27.876800
281.921579	12108.383938	27.881818
282.112575	12131.986693	27.886836
282.390501	12149.795331	27.891853
282.468666	12178.757036	27.896871
282.936294	12204.336089	27.901888
282.904958	12240.170788	27.906906
283.221053	12271.348743	27.911924
283.588457	12287.507854	27.916941
283.512096	12320.841408	27.921959
284.317613	12353.510090	27.926976
284.517377	12383.513562	27.931994
284.900724	12410.558915	27.937012
285.425305	12436.736922	27.942029
285.255835	12461.224630	27.947047
285.955395	12476.846303	27.952064
286.573150	12493.857903	27.957082
287.284325	12493.329411	27.962100
287.887570	12512.493249	27.967117
287.760520	12529.665642	27.972135
288.404301	12535.574267	27.977152
288.619230	12554.127008	27.982170
288.765032	12555.336091	27.987188
288.960658	12562.976397	27.992205
288.870466	12594.223027	27.997223
289.675531	12604.416132	28.002240
289.619021	12616.310910	28.007258
289.864385	12635.474766	28.012276
290.252287	12654.678833	28.017293
290.590611	12669.639193	28.022311
290.920232	12679.868129	28.027328
291.118406	12694.371832	28.032346
291.646405	12712.040505	28.037364
291.772889	12720.441368	28.042381
291.621076	12745.208589	28.047399
292.192274	12755.189702	28.052416
292.646236	12781.195964	28.057434
292.640488	12799.381754	28.062452
292.643576	12816.979748	28.067469
292.926691	12842.474795	28.072487
293.375008	12866.316623	28.077504
293.458585	12886.928555	28.082522
293.655453	12919.576603	28.087540
294.156937	12937.268977	28.092557
294.446763	12961.560501	28.097575
294.587703	12981.664674	28.102592
295.017743	13006.805391	28.107610
295.320461	13023.726539	28.112628
295.762180	13040.455238	28.117645
295.386886	13069.242483	28.122663
296.093473	13072.681819	28.127680
296.359660	13095.994105	28.132698
296.495606	13126.227377	28.137716
296.954475	13148.657189	28.142733
297.229991	13177.517482	28.147751
298.301943	13175.748205	28.152768
299.197200	13190.167546	28.157786
299.443440	13187.545263	28.162804
299.663334	13191.236686	28.167821
299.998184	13200.610797	28.172839
300.111133	13210.007185	28.177856
300.084895	13222.754622	28.182874
300.357014	13221.886846	28.187892
300.787499	13237.415094	28.192909
300.533175	13258.596070	28.197927
300.853898	13261.693367	28.202944
300.906228	13287.890633	28.207962
301.170610	13311.868660	28.212980
301.273813	13329.793639	28.217997
301.604493	13358.450932	28.223015
301.925150	13381.335036	28.228032
302.435925	13409.791329	28.233050
302.333385	13436.857032	28.238068
302.825595	13466.082608	28.243085
302.815398	13503.010280	28.248103
303.311495	13525.547710	28.253120
303.651540	13548.343611	28.258138
303.980365	13576.459406	28.263156
304.342583	13602.946086	28.268173
304.437492	13632.481204	28.273191
305.459238	13651.804769	28.278208
305.636775	13673.601041	28.283226
306.056832	13703.670043	28.288244
306.488233	13721.833941	28.293261
306.364622	13747.058074	28.298279
306.887239	13762.394497	28.303296
307.141307	13778.492545	28.308314
307.556346	13796.167564	28.313332
308.290684	13816.205729	28.318349
308.127068	13832.271389	28.323367
308.490680	13842.258800	28.328384
308.560769	13871.317866	28.333402
309.450317	13880.230046	28.338420
309.875773	13892.692527	28.343437
309.725748	13913.768200	28.348455
310.047938	13938.512715	28.353472
310.452961	13955.533928	28.358490
310.666495	13969.523864	28.363508
311.073053	13985.340636	28.368525
311.047232	14025.779183	28.373543
311.191751	14030.722605	28.378560
311.239923	14056.024949	28.383578
311.373808	14081.080939	28.388596
312.193144	14102.301223	28.393613
312.405871	14128.081435	28.398631
312.435754	14161.733085	28.403648
312.809020	14177.270453	28.408666
312.956953	14213.688716	28.413684
313.163453	14235.461852	28.418701
313.217806	14271.724474	28.423719
313.618173	14302.532462	28.428736
314.487395	14322.278594	28.433754
314.719782	14361.642857	28.438772
315.784563	14362.426613	28.443789
315.861217	14394.667878	28.448807
316.429178	14404.559135	28.453824
317.142977	14408.087372	28.458842
317.575424	14425.991791	28.463860
318.055932	14429.169110	28.468877
318.101178	14446.747432	28.473895
318.225517	14449.468794	28.478912
318.583709	14463.859941	28.483930
318.757335	14479.442845	28.488948
319.088042	14493.231876	28.493965
319.318992	14508.697798	28.498983
319.108443	14529.765714	28.504000
319.662747	14544.042931	28.509018
319.594489	14572.923606	28.514036
319.897097	14596.323197	28.519053
319.854663	14628.166045	28.524071
320.346037	14659.219184	28.529088
320.466443	14677.183661	28.534106
320.636966	14709.633281	28.539124
321.427766	14743.593902	28.544141
321.728249	14774.218128	28.549159
321.895432	14798.128281	28.554176
322.659802	14826.852508	28.559194
322.400212	14863.006300	28.564212
322.740145	14882.032039	28.569229
323.275369	14918.355526	28.574247
323.194021	14951.545504	28.579264
323.804844	14974.150374	28.584282
324.064947	15010.912137	28.589300
324.780291	15032.953778	28.594317
325.044409	15072.276462	28.599335
325.307943	15096.640268	28.604352
325.648964	15123.790339	28.609370
326.378445	15162.833290	28.614388
326.825621	15173.021566	28.619405
327.001211	15201.484805	28.624423
327.065024	15228.706203	28.629440
327.612180	15236.889655	28.634458
327.678317	15274.192817	28.639476
328.204661	15291.828296	28.644493
328.691717	15324.341516	28.649511
328.647022	15342.643970	28.654528
329.008357	15359.830177	28.659546
328.862606	15390.571430	28.664564
329.430817	15404.952623	28.669581
329.714222	15441.791740	28.674599
330.200256	15470.738187	28.679616
330.410391	15486.079332	28.684634
330.497180	15529.703783	28.689652
331.042142	15556.914190	28.694669
331.421367	15583.973345	28.699687
331.928312	15610.053811	28.704704
332.426695	15634.543674	28.709722
332.415450	15658.979046	28.714740
332.894255	15681.287511	28.719757
332.958248	15708.719319	28.724775
333.371010	15728.504386	28.729792
333.892885	15751.497585	28.734810
334.576513	15783.569739	28.739828
334.582447	15813.346264	28.744845
335.160586	15822.798402	28.749863
335.859541	15829.734451	28.754880
336.418879	15848.154629	28.759898
337.002536	15853.576641	28.764916
337.521530	15863.987915	28.769933
337.714402	15885.332054	28.774951
338.005456	15886.276885	28.779968
338.378704	15883.044429	28.784986
338.386947	15903.080318	28.790004
339.388850	15906.532713	28.795021
339.521472	15920.095206	28.800039
339.616665	15937.712262	28.805056
340.106418	15951.306579	28.810074
340.114340	15961.906394	28.815092
340.831488	15972.357866	28.820109
340.872347	15980.269047	28.825127
340.971718	15995.077913	28.830144
341.176271	16008.814164	28.835162
341.290118	16040.902497	28.840180
341.369224	16061.128209	28.845197
341.361620	16093.652049	28.850215
341.599960	16124.059265	28.855232
341.888178	16164.682509	28.860250
341.562862	16194.743488	28.865268
342.341684	16224.279514	28.870285
342.894689	16265.771938	28.875303
342.743424	16307.572760	28.880320
344.085844	16335.480119	28.885338
344.583392	16368.174875	28.890356
344.808496	16397.516047	28.895373
345.162157	16423.184242	28.900391
345.404288	16450.257269	28.905408
345.980275	16476.311501	28.910426
346.442408	16504.412577	28.915444
346.979884	16522.878239	28.920461
347.131305	16544.301267	28.925479
347.112720	16558.571215	28.930496
347.935066	16576.461586	28.935514
347.786093	16594.775404	28.940532
347.909014	16627.210127	28.945549
348.657223	16645.712326	28.950567
348.459551	16665.945219	28.955584
349.205670	16689.057354	28.960602
349.420196	16728.994660	28.965620
349.929419	16748.666672	28.970637
350.519595	16770.374227	28.975655
351.073457	16788.042842	28.980672
351.779465	16809.043261	28.985690
351.714345	16819.709738	28.990708
351.800945	16838.033896	28.995725
352.476852	16865.750546	29.000743
352.864198	16886.023748	29.005760
353.042346	16901.054811	29.010778
352.930071	16930.025942	29.015796
353.492143	16950.474219	29.020813
354.218833	16971.367251	29.025831
354.099022	17006.793896	29.030848
354.953878	17024.780074	29.035866
355.098938	17049.129211	29.040884
355.305168	17070.756347	29.045901
355.424048	17086.592282	29.050919
355.386436	17121.847435	29.055936
356.039084	17144.009835	29.060954
356.421820	17176.724278	29.065972
356.567559	17211.092159	29.070989
357.321363	17236.064006	29.076007
357.640065	17275.363622	29.081024
358.006522	17302.976384	29.086042
358.001071	17341.522961	29.091060
358.323885	17372.034636	29.096077
358.620783	17405.478398	29.101095
358.879062	17446.212364	29.106112
359.372584	17471.470378	29.111130
359.770518	17514.144922	29.116148
360.305913	17547.835022	29.121165
360.755479	17574.551133	29.126183
361.210510	17607.235109	29.131200
361.496099	17632.689810	29.136218
361.893610	17668.487965	29.141236
362.065062	17697.842193	29.146253
362.883130	17718.165558	29.151271
363.168393	17761.246295	29.156288
363.621991	17786.826938	29.161306
364.265718	17814.553834	29.166324
364.247713	17837.547849	29.171341
364.831533	17867.683042	29.176359
364.747593	17894.852129	29.181376
365.338517	17915.348671	29.186394
365.531014	17952.199452	29.191412
365.665133	17982.418228	29.196429
366.313911	18009.706295	29.201447
366.271957	18037.290937	29.206464
367.023581	18057.149978	29.211482
367.242164	18086.656042	29.216500
367.572547	18116.773631	29.221517
368.077031	18141.951951	29.226535
368.296262	18175.281279	29.231552
368.550021	18194.875805	29.236570
369.176934	18222.174272	29.241588
369.516130	18248.068472	29.246605
369.705560	18274.688388	29.251623
369.868886	18303.720288	29.256640
370.203071	18344.735098	29.261658
370.580698	18364.751620	29.266676
370.761087	18404.591560	29.271693
371.431299	18440.576390	29.276711
371.345274	18486.588900	29.281728
371.567794	18533.191919	29.286746
372.403587	18558.429178	29.291764
372.401104	18595.043604	29.296781
373.394226	18629.720081	29.301799
374.116845	18658.997296	29.306816
375.172113	18686.295633	29.311834
375.326706	18709.359011	29.316852
375.126563	18732.328703	29.321869
375.651818	18754.887160	29.326887
376.160374	18773.934170	29.331904
377.304598	18799.183577	29.336922
377.741600	18804.984869	29.341940
378.062124	18829.741674	29.346957
378.260157	18826.533963	29.351975
378.210520	18857.432228	29.356992
378.728380	18870.237366	29.362010
379.022868	18888.980635	29.367028
379.174463	18920.114137	29.372045
379.606252	18937.342412	29.377063
379.758459	18975.233475	29.382080
380.003622	19007.560403	29.387098
380.232502	19033.340702	29.392116
380.302717	19070.110828	29.397133
380.491076	19114.383106	29.402151
381.030837	19143.484382	29.407168
381.297370	19180.736678	29.412186
381.724682	19230.532421	29.417204
382.137590	19270.777610	29.422221
382.820240	19294.393004	29.427239
383.259875	19339.612973	29.432256
383.863553	19373.384907	29.437274
384.770837	19394.138075	29.442292
384.922091	19413.630182	29.447309
385.496853	19443.834402	29.452327
385.790069	19469.487666	29.457344
386.160082	19497.412463	29.462362
386.800251	19529.224910	29.467380
386.700797	19548.507863	29.472397
386.838374	19573.196203	29.477415
387.035136	19601.226545	29.482432
387.305423	19629.124502	29.487450
387.733945	19665.585395	29.492468
387.922338	19700.053537	29.497485
387.991766	19734.021815	29.502503
388.215339	19774.423636	29.507520
388.681820	19815.014129	29.512538
388.916894	19857.525434	29.517556
388.912125	19910.415119	29.522573
389.409295	19947.416718	29.527591
389.633679	20002.284086	29.532608
390.194706	20046.920663	29.537626
391.001481	20081.367175	29.542644
391.187450	20134.243791	29.547661
391.835784	20179.491734	29.552679
392.649760	20218.409025	29.557696
393.546793	20234.436231	29.562714
394.365834	20259.127043	29.567732
394.835737	20294.878957	29.572749
395.501027	20308.214954	29.577767
395.886748	20327.584363	29.582784
396.233237	20349.081300	29.587802
397.009570	20366.452244	29.592820
397.247942	20375.968358	29.597837
397.775880	20394.249135	29.602855
397.910210	20408.820958	29.607872
398.220866	20434.822747	29.612890
398.670017	20445.676170	29.617908
398.650683	20479.809372	29.622925
398.867260	20492.410360	29.627943
399.008498	20522.134192	29.632960
399.207069	20569.383960	29.637978
399.683385	20582.791980	29.642996
399.556543	20616.023022	29.648013
400.439090	20642.045383	29.653031
400.970485	20674.477819	29.658048
401.769862	20696.837371	29.663066
402.860546	20722.620778	29.668084
402.583323	20753.296595	29.673101
402.914480	20768.103057	29.678119
403.525689	20800.183038	29.683136
403.369083	20836.557508	29.688154
404.056965	20861.025693	29.693172
404.179524	20897.924846	29.698189
404.783101	20914.036104	29.703207
405.504784	20950.865813	29.708224
405.652368	20992.280125	29.713242
405.892776	21011.698871	29.718260
406.367935	21046.904303	29.723277
406.747995	21072.008981	29.728295
407.092433	21104.814881	29.733312
407.444352	21134.771745	29.738330
407.770253	21170.206426	29.743348
408.200895	21201.778822	29.748365
408.786663	21221.838754	29.753383
409.106083	21254.767496	29.758400
409.573166	21273.242570	29.763418
410.095649	21296.006741	29.768436
410.259564	21336.862454	29.773453
410.820885	21354.104114	29.778471
410.948630	21388.117742	29.783488
411.220341	21420.805833	29.788506
411.615979	21450.345770	29.793524
412.080592	21480.101011	29.798541
412.512900	21503.721399	29.803559
412.909541	21547.759338	29.808576
413.117894	21582.937488	29.813594
413.690091	21603.891149	29.818612
413.775775	21657.122415	29.823629
413.950351	21691.119161	29.828647
414.560569	21726.846890	29.833664
414.500607	21770.977845	29.838682
415.294074	21817.602438	29.843700
415.880185	21862.160644	29.848717
416.319717	21905.435229	29.853735
416.815409	21932.155065	29.858752
416.819093	21977.529311	29.863770
417.536142	22017.299967	29.868788
417.760955	22069.180886	29.873805
418.625834	22095.702094	29.878823
419.099748	22134.451822	29.883840
419.429193	22175.443602	29.888858
420.065176	22204.350721	29.893876
420.528293	22242.172137	29.898893
421.223792	22283.713309	29.903911
421.746621	22304.569060	29.908928
422.124969	22338.727719	29.913946
422.519991	22362.677390	29.918964
423.158523	22402.632714	29.923981
423.204089	22423.302311	29.928999
423.855362	22452.443778	29.934016
424.117254	22491.076105	29.939034
424.560179	22517.395884	29.944052
424.879238	22559.248246	29.949069
425.361145	22587.838635	29.954087
425.642649	22624.783669	29.959104
425.746695	22658.374942	29.964122
426.630243	22686.776815	29.969140
427.078618	22729.030070	29.974157
427.028055	22767.243461	29.979175
427.718694	22799.056544	29.984192
427.491131	22843.627430	29.989210
428.082248	22880.829055	29.994228
428.816961	22926.099464	29.999245
428.961398	22963.992856	30.004263
430.096986	22995.357876	30.009280
430.115644	23036.304045	30.014298
430.967738	23070.442907	30.019316
431.179137	23102.966344	30.024333
431.824346	23132.056390	30.029351
432.266286	23159.579035	30.034368
432.513553	23191.087180	30.039386
432.984670	23217.964637	30.044404
433.590723	23256.908743	30.049421
433.824700	23288.056619	30.054439
433.961984	23317.098393	30.059456
434.182380	23358.575347	30.064474
434.488852	23384.137616	30.069492
434.718991	23437.437972	30.074509
435.320292	23478.146565	30.079527
436.216577	23497.580333	30.084544
436.572514	23536.280905	30.089562
437.028061	23572.034265	30.094580
437.342273	23604.935306	30.099597
437.551245	23649.957067	30.104615
438.125508	23681.201898	30.109632
438.675959	23717.781469	30.114650
440.251827	23729.639358	30.119668
440.694274	23749.062867	30.124685
441.069479	23787.092010	30.129703
441.414389	23794.312858	30.134720
442.142609	23830.133582	30.139738
442.701004	23850.373205	30.144756
443.035092	23866.468781	30.149773
443.202838	23893.569611	30.154791
443.610893	23916.427857	30.159808
443.424658	23945.276945	30.164826
444.000421	23966.753348	30.169844
444.607418	24014.098776	30.174861
444.509623	24049.881713	30.179879
444.983269	24079.065851	30.184896
445.417153	24122.693972	30.189914
445.597957	24165.088085	30.194932
446.130074	24205.942739	30.199949
446.641711	24233.786363	30.204967
447.390844	24276.234767	30.209984
447.568194	24320.181771	30.215002
448.369589	24367.053253	30.220020
448.469567	24395.784652	30.225037
448.579470	24448.875319	30.230055
449.202295	24482.996350	30.235072
449.804047	24533.514217	30.240090
449.874806	24568.720487	30.245108
450.560419	24616.943627	30.250125
450.774978	24665.540980	30.255143
451.188581	24705.167991	30.260160
451.210422	24760.198878	30.265178
451.874756	24806.558793	30.270196
452.524871	24855.246070	30.275213
452.794445	24910.982579	30.280231
453.420152	24957.418915	30.285248
453.781497	25010.089685	30.290266
454.062680	25056.086923	30.295284
454.490125	25109.030567	30.300301
455.072142	25155.045914	30.305319
455.837300	25208.190657	30.310336
455.887448	25253.647585	30.315354
456.486634	25290.796257	30.320372
457.554128	25318.152069	30.325389
457.991438	25353.439073	30.330407
459.078157	25375.545747	30.335424
459.954711	25406.010061	30.340442
460.554807	25411.689470	30.345460
461.214316	25437.708473	30.350477
461.096184	25454.961869	30.355495
461.686672	25468.317890	30.360512
462.274443	25495.563764	30.365530
462.225154	25521.748515	30.370548
462.861073	25551.806378	30.375565
462.911141	25594.828913	30.380583
463.516605	25625.065622	30.385600
463.879275	25652.858198	30.390618
464.009592	25692.498159	30.395636
464.277903	25736.565661	30.400653
464.402982	25783.660978	30.405671
464.722543	25819.593716	30.410688
464.713611	25882.494662	30.415706
465.336814	25930.874115	30.420724
465.686366	25983.676046	30.425741
465.921255	26043.308621	30.430759
466.911652	26089.064037	30.435776
467.569787	26136.106820	30.440794
468.061111	26177.692377	30.445812
468.611823	26233.413348	30.450829
468.827243	26287.794434	30.455847
469.903907	26330.049793	30.460864
470.287111	26377.850144	30.465882
470.798922	26411.795255	30.470900
471.790383	26458.065677	30.475917
471.850456	26500.350533	30.480935
472.488952	26524.160163	30.485952
473.348014	26570.504047	30.490970
473.279479	26611.429443	30.495988
474.059816	26646.672914	30.501005
474.322221	26695.551672	30.506023
474.911166	26741.431229	30.511040
474.686595	26780.904180	30.516058
475.251265	26831.690631	30.521076
476.108727	26880.001033	30.526093
476.019580	26930.691592	30.531111
476.564048	26979.737338	30.536128
476.998067	27038.992168	30.541146
477.140881	27095.117043	30.546164
477.767802	27151.553498	30.551181
477.864427	27203.976561	30.556199
478.487596	27259.054272	30.561216
478.921414	27318.142875	30.566234
479.356095	27375.124079	30.571252
480.066190	27427.294411	30.576269
480.436060	27497.259972	30.581287
480.999789	27546.941296	30.586304
482.179562	27582.550435	30.591322
482.925426	27617.069837	30.596340
484.026947	27648.556434	30.601357
484.245639	27674.468183	30.606375
485.026851	27703.820252	30.611392
485.414690	27739.849357	30.616410
485.958103	27754.499267	30.621428
486.464477	27776.894600	30.626445
486.680795	27816.338503	30.631463
487.246902	27834.417173	30.636480
487.457991	27871.372841	30.641498
487.622862	27904.828189	30.646516
488.077714	27947.623098	30.651533
488.297468	27997.724310	30.656551
488.671191	28046.824391	30.661568
489.314483	28080.608243	30.666586
490.116687	28119.040640	30.671604
490.732168	28159.407587	30.676621
491.116948	28207.622821	30.681639
491.552885	28249.295367	30.686656
491.995315	28299.554895	30.691674
492.137976	28340.075842	30.696692
492.903652	28375.404192	30.701709
493.207562	28437.541363	30.706727
493.546763	28480.171239	30.711744
494.092033	28532.420432	30.716762
494.105253	28587.559508	30.721780
494.935598	28644.909286	30.726797
494.725655	28707.037648	30.731815
495.430275	28767.608646	30.736832
496.368007	28821.823345	30.741850
496.561600	28876.657921	30.746868
497.593486	28928.723945	30.751885
498.075373	28997.247004	30.756903
498.582227	29037.555703	30.761920
499.516645	29083.363265	30.766938
499.971180	29136.144091	30.771956
500.607598	29173.042233	30.776973
501.231730	29218.786573	30.781991
502.458795	29242.719922	30.787008
503.123532	29265.724216	30.792026
503.800300	29298.378268	30.797044
504.635218	29318.595817	30.802061
504.852954	29343.595178	30.807079
505.646604	29361.141067	30.812096
506.020827	29389.038570	30.817114
506.120161	29412.237750	30.822132
506.789650	29436.875865	30.827149
507.103635	29477.221774	30.832167
507.268545	29498.955264	30.837184
507.592689	29532.563108	30.842202
507.993528	29568.685236	30.847220
508.296396	29608.257155	30.852237
508.724618	29650.316126	30.857255
509.003165	29685.885189	30.862272
509.530245	29729.325198	30.867290
509.553440	29775.767147	30.872308
509.967746	29813.922635	30.877325
511.027666	29855.204929	30.882343
511.332310	29898.983224	30.887360
511.814632	29953.613905	30.892378
511.925461	29997.375167	30.897396
512.799923	30033.041605	30.902413
513.346832	30087.554351	30.907431
513.735104	30125.437301	30.912448
514.675916	30172.903164	30.917466
514.926473	30214.526925	30.922484
515.544270	30254.891968	30.927501
515.971029	30306.409430	30.932519
516.208938	30347.972563	30.937536
516.946429	30391.248773	30.942554
517.280343	30440.526419	30.947572
517.581739	30489.084026	30.952589
518.135291	30553.265285	30.957607
518.446257	30612.001023	30.962624
519.299347	30663.919790	30.967642
519.580296	30723.437281	30.972660
520.227437	30764.072981	30.977677
521.326655	30813.690696	30.982695
521.488731	30871.146434	30.987712
522.282224	30917.412049	30.992730
522.840418	30968.495541	30.997748
523.714387	31013.330795	31.002765
524.086092	31062.253427	31.007783
524.537727	31101.591768	31.012800
525.139564	31147.449048	31.017818
525.268069	31196.009810	31.022836
525.456054	31250.748561	31.027853
526.117829	31297.769826	31.032871
526.715087	31353.139300	31.037888
527.071719	31401.516377	31.042906
527.316729	31462.471976	31.047924
528.412173	31502.338320	31.052941
529.372594	31557.718784	31.057959
529.799134	31601.451986	31.062976
530.745766	31648.254966	31.067994
531.307870	31688.172089	31.073012
532.004353	31719.656490	31.078029
532.450714	31769.262513	31.083047
533.442820	31793.656140	31.088064
534.302008	31815.466002	31.093082
534.683300	31844.773581	31.098100
535.475510	31868.564118	31.103117
536.322532	31886.548328	31.108135
536.459324	31924.812704	31.113152
536.839055	31951.365820	31.118170
536.965183	31988.963156	31.123188
537.240453	32019.478883	31.128205
537.658340	32067.541169	31.133223
537.733404	32100.145700	31.138240
538.174783	32136.493317	31.143258
538.058070	32189.658806	31.148276
538.297518	32236.795936	31.153293
539.094651	32298.183638	31.158311
538.955499	32360.669234	31.163328
539.539922	32421.456342	31.168346
539.564183	32492.898863	31.173364
539.847387	32561.075239	31.178381
540.637872	32642.163707	31.183399
541.212898	32708.065800	31.188416
541.581547	32783.316342	31.193434
542.752143	32851.439606	31.198452
543.978194	32889.077588	31.203469
544.650351	32951.413606	31.208487
545.415215	33017.833430	31.213504
545.990848	33057.842814	31.218522
546.643762	33112.169919	31.223540
547.367578	33165.800210	31.228557
547.786199	33224.011678	31.233575
548.289148	33274.644157	31.238592
549.198026	33312.627721	31.243610
549.485276	33364.929024	31.248628
550.555333	33407.909415	31.253645
551.199395	33454.200899	31.258663
551.567447	33496.900980	31.263680
552.161541	33535.254546	31.268698
552.469824	33588.868931	31.273716
552.866367	33627.827773	31.278733
553.315338	33681.743395	31.283751
553.612083	33737.938642	31.288768
554.474406	33784.966800	31.293786
554.632795	33854.157295	31.298804
554.913041	33898.656522	31.303821
555.687397	33968.559327	31.308839
555.660662	34032.019302	31.313856
556.276645	34091.720974	31.318874
556.526519	34164.453860	31.323892
556.707852	34234.462458	31.328909
557.439479	34314.953117	31.333927
558.050930	34389.543863	31.338944
558.935617	34464.425807	31.343962
559.018601	34544.987597	31.348980
559.507658	34614.960723	31.353997
560.202697	34690.968126	31.359015
560.922511	34774.316024	31.364032
562.302546	34831.272759	31.369050
563.481572	34900.478599	31.374068
563.983401	34959.135900	31.379085
564.848027	35027.761697	31.384103
565.189671	35075.744081	31.389120
565.549337	35126.712460	31.394138
566.166750	35180.300694	31.399156
566.858868	35241.545991	31.404173
567.278897	35281.517533	31.409191
567.804053	35340.910639	31.414208
568.229618	35375.383209	31.419226
569.036371	35427.554126	31.424244
569.472696	35479.867568	31.429261
569.743522	35532.269486	31.434279
570.239860	35580.365576	31.439296
570.929479	35641.577932	31.444314
571.336411	35698.846162	31.449332
571.784361	35754.712440	31.454349
572.220837	35807.127800	31.459367
572.588913	35874.389953	31.464384
573.316928	35921.519280	31.469402
573.942987	35988.497768	31.474420
574.323187	36060.477330	31.479437
575.144841	36127.943625	31.484455
575.617217	36189.611693	31.489472
576.307436	36256.201402	31.494490
576.591659	36321.503645	31.499508
577.448584	36385.713714	31.504525
578.290685	36443.222214	31.509543
578.619210	36506.399539	31.514560
579.429457	36569.384071	31.519578
580.230768	36625.798522	31.524596
580.564932	36689.736231	31.529613
581.339571	36746.499685	31.534631
581.643328	36817.482087	31.539648
581.826517	36882.888873	31.544666
582.378384	36945.644352	31.549684
583.287727	37018.720740	31.554701
584.081814	37085.630275	31.559719
584.154611	37164.586073	31.564736
584.533011	37231.157003	31.569754
585.655991	37297.531161	31.574772
586.084950	37375.183138	31.579789
587.356885	37423.299566	31.584807
587.974734	37484.050593	31.589824
589.158969	37522.409338	31.594842
590.020120	37568.377403	31.599860
590.793271	37620.093170	31.604877
591.947135	37643.665231	31.609895
592.599941	37691.471762	31.614912
593.319577	37724.424221	31.619930
593.976274	37750.152386	31.624948
594.348480	37788.957016	31.629965
594.768577	37814.511153	31.634983
595.330348	37853.592798	31.640000
595.543404	37890.205743	31.645018
596.218183	37928.946203	31.650036
596.414936	37977.036801	31.655053
597.449665	38020.555052	31.660071
597.527308	38065.332773	31.665088
597.990973	38127.239308	31.670106
598.463280	38166.756796	31.675124
598.849230	38218.736311	31.680141
599.536497	38276.488608	31.685159
599.539620	38331.024730	31.690176
599.982326	38383.657912	31.695194
600.582400	38450.896096	31.700212
600.885254	38512.487385	31.705229
601.434289	38569.617137	31.710247
601.950252	38636.542099	31.715264
602.485225	38704.003869	31.720282
602.817679	38777.820630	31.725300
602.919677	38856.879708	31.730317
603.653476	38926.473847	31.735335
604.311490	39007.660761	31.740352
604.987457	39075.598524	31.745370
606.271318	39138.412872	31.750388
606.654508	39209.353016	31.755405
607.758891	39275.762768	31.760423
608.236257	39343.088366	31.765440
608.581886	39410.269459	31.770458
609.518582	39475.073344	31.775476
609.936149	39551.653603	31.780493
611.323320	39611.095971	31.785511
611.892285	39680.809589	31.790528
612.608757	39737.923740	31.795546
613.656722	39790.482492	31.800564
613.754448	39856.549042	31.805581
614.355432	39900.367044	31.810599
614.712126	39966.275964	31.815616
614.984563	40031.593392	31.820634
616.069685	40089.358968	31.825652
616.595312	40163.599623	31.830669
617.391299	40227.483118	31.835687
617.762652	40286.261900	31.840704
618.388619	40359.103325	31.845722
619.111414	40419.107271	31.850740
619.475829	40491.211052	31.855757
619.714766	40558.641896	31.860775
619.954032	40631.828472	31.865792
620.618356	40702.760890	31.870810
621.401675	40779.776073	31.875828
621.996123	40869.774856	31.880845
622.639272	40944.986704	31.885863
623.127782	41019.546542	31.890880
623.675372	41106.482492	31.895898
624.398747	41174.542953	31.900916
624.831873	41264.167145	31.905933
625.778677	41347.310222	31.910951
626.261814	41426.100233	31.915968
626.816195	41501.080103	31.920986
627.984671	41586.109080	31.926004
628.955525	41659.297482	31.931021
629.782623	41726.562319	31.936039
630.843465	41779.983298	31.941056
631.582468	41840.288993	31.946074
632.583767	41889.666404	31.951092
632.670072	41945.566029	31.956109
633.903202	41994.509323	31.961127
634.492426	42038.864820	31.966144
634.782626	42098.651486	31.971162
635.483927	42145.880241	31.976180
635.786819	42190.929270	31.981197
636.694935	42245.725976	31.986215
636.877610	42288.134100	31.991232
637.847606	42338.812620	31.996250
638.933661	42385.698207	32.001268
638.909188	42437.084137	32.006285
640.271743	42476.316197	32.011303
640.986337	42523.243666	32.016320
641.478199	42569.565278	32.021338
641.949450	42612.483576	32.026356
642.384033	42672.237862	32.031373
643.046855	42730.115550	32.036391
643.189119	42782.294817	32.041408
643.429927	42849.758857	32.046426
644.037972	42919.446303	32.051444
644.186691	42992.793394	32.056461
644.875141	43069.979507	32.061479
645.424919	43142.333297	32.066496
645.813287	43217.288475	32.071514
646.210828	43303.199359	32.076532
646.676604	43389.471547	32.081549
647.536144	43483.005602	32.086567
648.253295	43569.563945	32.091584
648.583620	43662.722219	32.096602
649.729552	43739.659025	32.101620
650.229751	43837.932962	32.106637
650.887072	43918.468749	32.111655
651.406684	43993.988705	32.116672
652.265491	44090.920475	32.121690
653.242651	44170.253115	32.126708
653.898791	44258.211328	32.131725
654.635422	44340.554212	32.136743
655.422402	44421.344656	32.141760
655.707703	44506.336045	32.146778
656.426592	44581.899994	32.151796
656.864028	44677.163821	32.156813
657.689629	44761.353271	32.161831
658.459900	44845.192574	32.166848
658.893291	44926.952060	32.171866
659.856385	45013.146445	32.176884
660.624214	45094.208300	32.181901
661.372358	45170.944331	32.186919
662.463400	45251.168314	32.191936
663.728032	45313.343532	32.196954
664.811738	45368.624506	32.201972
665.754996	45428.079295	32.206989
666.601570	45488.899298	32.212007
667.320666	45548.910779	32.217024
667.914267	45597.486671	32.222042
668.663901	45647.400221	32.227060
669.452958	45697.566108	32.232077
670.006171	45740.714315	32.237095
670.505307	45773.267173	32.242112
670.213405	45821.947965	32.247130
671.200945	45860.060739	32.252148
671.449392	45921.316186	32.257165
672.112731	45977.956281	32.262183
672.958605	46033.554686	32.267200
673.796622	46100.261622	32.272218
674.468875	46159.288250	32.277236
675.042213	46218.799406	32.282253
675.553803	46273.963113	32.287271
676.092683	46338.618816	32.292288
676.493151	46405.948135	32.297306
676.993468	46466.571607	32.302324
677.362618	46542.222200	32.307341
677.914033	46615.321638	32.312359
678.298373	46706.852780	32.317376
680.583204	46737.048546	32.322394
682.468610	46777.539063	32.327412
683.186287	46831.228930	32.332429
683.839561	46875.445829	32.337447
684.468335	46920.541857	32.342464
684.626684	46973.355205	32.347482
685.350535	47016.101231	32.352500
685.821158	47082.944016	32.357517
686.180109	47131.339770	32.362535
686.921133	47186.567867	32.367552
687.190011	47263.820780	32.372570
687.788066	47313.780444	32.377588
688.803963	47385.754696	32.382605
689.128071	47460.086976	32.387623
689.885834	47517.400807	32.392640
690.095137	47592.302814	32.397658
690.527759	47660.610113	32.402676
691.114747	47747.806665	32.407693
691.711833	47821.632455	32.412711
692.154771	47899.979327	32.417728
692.683069	47995.351498	32.422746
693.746314	48084.012445	32.427764
694.641307	48171.701399	32.432781
694.860208	48257.415676	32.437799
696.124169	48344.729522	32.442816
696.664848	48417.755530	32.447834
697.515451	48497.582645	32.452852
698.344477	48573.377219	32.457869
698.846531	48659.625937	32.462887
699.533771	48740.536984	32.467904
700.055154	48823.731982	32.472922
700.679500	48905.949498	32.477940
701.316540	48997.811463	32.482957
701.640385	49091.193100	32.487975
702.700154	49179.357452	32.492992
703.462235	49268.805061	32.498010
704.748602	49342.085848	32.503028
705.807424	49410.061475	32.508045
706.726039	49496.552103	32.513063
707.486701	49558.666331	32.518080
707.873932	49622.998943	32.523098
708.584966	49695.830015	32.528116
709.154462	49755.659146	32.533133
709.338388	49826.306742	32.538151
710.315008	49894.961478	32.543168
710.701849	49971.285802	32.548186
711.321976	50050.097456	32.553204
712.395111	50116.986499	32.558221
712.520961	50199.200119	32.563239
713.505901	50281.184791	32.568256
714.562971	50364.736849	32.573274
715.024485	50437.177524	32.578292
715.780926	50506.067978	32.583309
716.721199	50579.564344	32.588327
717.811015	50655.562441	32.593344
718.313574	50734.567578	32.598362
718.867462	50807.271781	32.603380
719.954189	50884.844415	32.608397
720.374069	50965.608349	32.613415
721.511016	51035.926487	32.618432
721.791868	51117.277146	32.623450
722.683081	51187.113542	32.628468
723.243189	51263.571180	32.633485
723.464824	51344.812887	32.638503
724.556505	51417.654677	32.643520
724.842240	51517.283927	32.648538
725.607355	51604.947427	32.653556
726.212643	51699.354748	32.658573
726.445981	51794.957168	32.663591
727.080436	51884.242763	32.668608
728.115559	51982.254931	32.673626
729.303438	52075.755544	32.678644
729.951936	52162.872877	32.683661
730.748590	52256.611957	32.688679
731.535143	52348.817884	32.693696
731.774186	52441.004302	32.698714
732.814622	52526.122716	32.703732
734.209162	52613.941942	32.708749
734.685138	52706.916714	32.713767
735.211098	52793.950414	32.718784
736.387974	52872.595901	32.723802
737.204387	52957.546045	32.728820
738.130149	53027.231418	32.733837
738.376896	53125.491732	32.738855
739.055635	53210.245399	32.743872
739.393166	53299.145964	32.748890
740.308779	53396.743337	32.753908
741.011290	53492.501073	32.758925
741.369571	53591.041562	32.763943
742.268636	53696.080261	32.768960
742.722445	53793.562814	32.773978
743.340095	53889.962554	32.778996
744.427716	53998.926073	32.784013
744.806006	54098.451376	32.789031
745.671740	54185.192867	32.794048
746.322746	54286.744966	32.799066
746.833725	54385.629728	32.804084
747.860121	54462.569613	32.809101
749.026067	54564.098109	32.814119
749.767478	54647.267439	32.819136
750.491926	54747.880422	32.824154
751.158122	54835.354013	32.829172
751.840659	54930.566019	32.834189
752.506407	55019.771915	32.839207
753.198353	55113.491879	32.844224
754.180921	55206.840226	32.849242
754.376552	55319.135961	32.854260
755.208740	55416.030820	32.859277
755.824834	55526.498958	32.864295
756.244976	55625.557078	32.869312
757.006879	55742.314375	32.874330
757.766032	55850.326860	32.879348
758.830541	55956.436046	32.884365
759.625585	56069.852946	32.889383
760.418454	56177.425376	32.894400
761.340628	56283.965119	32.899418
761.600655	56402.606951	32.904436
762.585464	56504.195275	32.909453
763.326819	56623.090894	32.914471
763.863079	56740.644670	32.919488
764.899967	56839.887509	32.924506
765.622072	56956.437483	32.929524
766.755639	57068.234738	32.934541
767.204095	57182.930658	32.939559
768.171512	57294.397400	32.944576
768.938336	57404.673071	32.949594
769.762558	57518.573430	32.954612
771.267529	57602.445790	32.959629
771.992119	57707.333164	32.964647
773.019660	57809.426332	32.969664
774.155760	57900.858575	32.974682
774.918100	57991.818052	32.979700
776.599717	58064.633666	32.984717
777.672102	58137.421177	32.989735
778.590225	58207.328139	32.994752
779.446163	58278.225609	32.999770
780.114412	58354.356933	33.004788
780.907246	58420.260175	33.009805
781.419745	58503.863862	33.014823
781.753132	58583.712778	33.019840
782.392242	58668.622694	33.024858
783.074437	58760.876028	33.029876
783.445405	58840.839599	33.034893
783.752969	58944.654506	33.039911
784.237722	59037.897278	33.044928
784.950605	59139.994147	33.049946
785.430175	59254.013832	33.054964
786.484442	59369.029150	33.059981
786.982035	59471.316242	33.064999
787.281271	59577.170978	33.070016
788.204678	59686.661102	33.075034
788.893366	59791.584326	33.080052
789.659221	59897.790591	33.085069
790.268929	60002.987570	33.090087
791.385135	60111.031119	33.095104
792.240360	60206.548083	33.100122
792.775644	60326.145363	33.105140
793.716304	60434.903325	33.110157
794.128053	60550.136461	33.115175
794.929759	60665.297127	33.120192
795.937538	60789.620004	33.125210
796.539536	60906.940041	33.130228
797.482828	61018.968549	33.135245
798.200794	61136.491262	33.140263
798.973421	61251.609619	33.145280
800.232027	61355.444487	33.150298
801.165087	61485.738784	33.155316
802.010246	61596.510378	33.160333
802.910024	61715.857335	33.165351
803.912520	61825.553896	33.170368
804.896195	61931.113864	33.175386
805.382676	62041.506792	33.180404
806.241736	62154.605214	33.185421
806.692089	62268.703491	33.190439
807.211292	62384.339335	33.195456
808.155642	62495.907883	33.200474
808.839713	62621.207500	33.205492
809.757121	62731.479713	33.210509
810.660389	62855.561085	33.215527
811.754408	62981.955814	33.220544
812.939389	63088.675638	33.225562
813.206422	63217.969652	33.230580
814.415834	63318.428076	33.235597
815.409559	63430.935105	33.240615
816.122731	63550.236057	33.245632
817.142783	63659.547346	33.250650
817.763252	63780.875808	33.255668
818.458938	63876.607715	33.260685
819.356835	64001.360611	33.265703
820.187651	64118.849252	33.270720
820.701819	64229.988687	33.275738
821.840030	64348.203560	33.280756
822.632682	64462.299454	33.285773
823.665586	64582.221653	33.290791
824.225762	64711.234438	33.295808
825.436661	64806.920280	33.300826
826.107358	64923.391384	33.305844
827.064574	65039.080688	33.310861
828.032120	65149.881803	33.315879
829.023085	65267.987984	33.320896
829.505313	65369.377396	33.325914
830.044809	65485.292429	33.330932
831.258957	65592.418317	33.335949
831.935036	65706.553566	33.340967
832.181263	65815.825267	33.345984
833.127039	65925.869178	33.351002
833.479691	66034.181737	33.356020
834.437802	66146.178320	33.361037
835.094848	66269.828892	33.366055
835.682289	66392.676497	33.371072
836.615417	66513.088307	33.376090
837.475725	66641.340696	33.381108
838.299050	66763.429265	33.386125
838.986252	66884.119239	33.391143
839.772471	66995.498507	33.396160
841.038779	67123.564136	33.401178
841.933178	67253.983096	33.406196
842.786631	67375.089977	33.411213
843.503640	67502.746139	33.416231
844.374532	67631.799368	33.421248
845.700615	67749.463627	33.426266
846.410881	67874.353707	33.431284
847.349671	67995.436846	33.436301
847.978849	68122.631204	33.441319
848.620824	68253.959442	33.446336
849.643757	68374.967085	33.451354
850.871835	68494.454327	33.456372
851.773432	68616.704492	33.461389
852.781588	68730.754809	33.466407
853.672788	68848.385776	33.471424
855.280860	68953.779122	33.476442
855.756851	69074.625131	33.481460
856.394588	69187.299589	33.486477
857.342733	69303.133772	33.491495
858.031460	69421.567685	33.496512
858.805886	69534.669514	33.501530
859.516937	69661.915870	33.506548
860.426608	69774.180057	33.511565
861.801973	69897.741215	33.516583
862.473483	70019.172416	33.521600
863.399643	70129.519565	33.526618
863.897783	70253.296234	33.531636
865.035941	70362.122190	33.536653
866.608112	70481.624762	33.541671
867.097843	70595.761085	33.546688
867.939265	70698.303106	33.551706
869.113695	70817.002959	33.556724
869.953975	70914.468135	33.561741
871.145256	71020.746095	33.566759
871.726550	71132.093352	33.571776
872.760594	71243.325692	33.576794
873.241937	71365.385127	33.581812
873.971741	71471.630494	33.586829
875.370960	71586.286599	33.591847
875.573652	71706.650219	33.596864
876.696664	71819.286866	33.601882
877.396964	71941.115971	33.606900
877.871129	72056.894256	33.611917
878.792338	72167.657346	33.616935
879.558523	72290.356184	33.621952
880.610593	72397.398315	33.626970
881.262896	72516.829278	33.631988
881.762243	72629.077283	33.637005
882.799389	72749.360638	33.642023
883.348643	72877.931035	33.647040
884.208940	72995.608727	33.652058
884.796829	73136.064068	33.657076
885.495035	73270.278030	33.662093
886.341231	73407.332514	33.667111
886.675781	73543.039781	33.672128
887.703655	73686.737393	33.677146
888.387124	73843.542855	33.682164
888.995901	73998.464785	33.687181
890.247386	74147.035126	33.692199
890.856370	74302.699155	33.697216
892.168807	74453.607641	33.702234
893.115871	74595.427523	33.707252
894.275447	74740.621087	33.712269
895.723371	74888.795910	33.717287
896.555099	75035.413758	33.722304
896.819059	75178.069084	33.727322
897.835639	75325.333971	33.732340
898.350967	75481.629513	33.737357
899.470274	75630.004705	33.742375
900.713862	75775.576474	33.747392
901.631438	75919.920985	33.752410
902.863172	76066.856628	33.757428
903.705265	76210.279786	33.762445
904.749625	76356.237355	33.767463
905.962327	76484.911110	33.772480
907.580239	76621.979759	33.777498
908.455774	76755.083748	33.782516
909.690036	76878.999250	33.787533
910.689123	76995.725517	33.792551
911.906584	77122.719498	33.797568
913.050971	77228.428085	33.802586
914.069311	77348.619368	33.807604
915.118829	77467.755876	33.812621
915.906099	77573.166672	33.817639
916.735363	77692.531863	33.822656
917.900741	77795.399220	33.827674
918.565157	77906.766267	33.832692
919.423208	78023.332235	33.837709
920.853920	78133.696190	33.842727
921.578650	78243.321255	33.847744
922.253629	78349.792366	33.852762
923.550119	78457.808636	33.857780
923.833797	78575.253914	33.862797
924.919326	78692.290455	33.867815
925.360365	78821.318461	33.872832
926.923171	78939.223460	33.877850
927.499625	79056.393342	33.882868
928.298327	79176.062588	33.887885
929.100021	79294.979125	33.892903
929.469026	79407.321436	33.897920
930.309954	79531.774331	33.902938
931.215223	79652.313515	33.907956
931.719131	79780.001318	33.912973
932.269012	79904.132827	33.917991
933.563566	80034.647425	33.923008
934.666928	80167.656525	33.928026
935.468804	80293.739845	33.933044
936.216024	80424.654075	33.938061
937.485405	80551.032016	33.943079
937.979900	80685.786988	33.948096
938.968019	80814.030296	33.953114
939.616051	80960.806610	33.958132
940.471185	81104.302760	33.963149
941.647988	81247.795331	33.968167
942.476884	81390.665077	33.973184
943.737690	81527.141180	33.978202
945.065850	81656.760826	33.983220
945.717186	81809.014763	33.988237
946.757970	81945.809407	33.993255
947.625270	82095.915030	33.998272
948.222900	82229.237769	34.003290
949.285618	82386.803073	34.008308
949.379625	82535.006631	34.013325
951.252399	82673.112011	34.018343
952.074897	82827.443954	34.023360
953.515282	82976.134734	34.028378
954.284873	83114.419004	34.033396
955.243975	83265.743965	34.038413
956.197132	83409.939945	34.043431
956.889537	83566.956573	34.048448
957.933364	83721.269186	34.053466
959.177999	83860.912867	34.058484
959.881171	84012.159941	34.063501
961.145368	84158.015712	34.068519
961.751073	84308.749872	34.073536
962.579071	84464.236990	34.078554
963.776017	84618.358443	34.083572
964.517883	84783.790629	34.088589
965.544926	84933.330298	34.093607
966.440325	85093.163565	34.098624
967.554331	85245.272087	34.103642
968.542371	85399.314197	34.108660
969.562407	85547.220025	34.113677
971.022816	85691.608927	34.118695
971.945238	85842.602406	34.123712
973.698878	85975.248585	34.128730
975.711083	86099.998030	34.133748
976.544794	86228.468399	34.138765
978.004859	86332.183913	34.143783
979.251972	86450.162173	34.148800
980.487694	86554.727090	34.153818
981.455526	86677.652368	34.158836
981.937989	86788.536360	34.163853
983.092859	86895.129022	34.168871
983.790641	86991.251057	34.173888
984.128232	87096.782186	34.178906
985.076404	87210.727274	34.183924
985.076159	87335.176002	34.188941
985.962470	87449.265718	34.193959
987.123931	87573.231969	34.198976
987.889698	87713.157609	34.203994
988.977087	87835.131752	34.209012
989.844330	87969.871064	34.214029
990.209184	88109.317080	34.219047
991.524310	88249.246706	34.224064
992.002997	88390.446895	34.229082
993.091840	88531.473812	34.234100
993.834733	88681.680605	34.239117
995.125341	88826.788426	34.244135
996.355908	88973.780753	34.249152
997.090114	89125.523388	34.254170
998.010173	89272.868168	34.259188
998.948882	89425.748527	34.264205
999.656579	89586.662990	34.269223
1000.749760	89753.499827	34.274240
1001.605563	89914.112623	34.279258
1002.912051	90065.028970	34.284276
1003.481845	90239.712005	34.289293
1004.265628	90397.144075	34.294311
1005.330801	90565.934369	34.299328
1005.971147	90746.064809	34.304346
1007.062926	90919.637981	34.309364
1007.762748	91093.349128	34.314381
1008.710411	91281.773090	34.319399
1009.773534	91456.570242	34.324416
1010.486623	91647.284165	34.329434
1011.739118	91823.076895	34.334452
1012.551232	92013.624796	34.339469
1013.696585	92203.889241	34.344487
1014.591449	92398.325060	34.349504
1015.138754	92596.512213	34.354522
1016.152335	92791.684052	34.359540
1017.212592	92999.996690	34.364557
1018.108448	93180.791186	34.369575
1019.171722	93387.005014	34.374592
1020.208994	93604.422916	34.379610
1021.443152	93791.329431	34.384628
1022.289514	94002.516682	34.389645
1023.381651	94201.408311	34.394663
1024.780772	94413.118424	34.399680
1025.582235	94615.259920	34.404698
1026.872141	94811.027009	34.409716
1027.973019	95014.405530	34.414733
1029.365776	95209.506090	34.419751
1030.730723	95398.143126	34.424768
1031.942739	95593.176331	34.429786
1032.943672	95770.806312	34.434804
1034.224162	95955.581321	34.439821
1035.238864	96134.110463	34.444839
1036.535915	96297.601280	34.449856
1037.780843	96461.083090	34.454874
1039.121375	96609.596146	34.459892
1040.349963	96767.688865	34.464909
1041.539905	96926.086743	34.469927
1042.624847	97078.071340	34.474944
1043.372466	97242.320762	34.479962
1044.559825	97388.192933	34.484980
1045.539738	97554.240595	34.489997
1046.361182	97710.212020	34.495015
1047.594753	97860.403135	34.500032
1048.075218	98033.206139	34.505050
1049.022520	98202.245597	34.510068
1050.323730	98368.091593	34.515085
1051.099424	98537.726137	34.520103
1052.407677	98710.088069	34.525120
1053.406290	98886.942492	34.530138
1054.788698	99038.602922	34.535156
1056.217558	99207.186669	34.540173
1056.664417	99374.211162	34.545191
1057.983692	99540.232595	34.550208
1058.980675	99714.028508	34.555226
1060.410978	99862.481803	34.560244
1061.518846	100031.740078	34.565261
1062.379330	100193.038521	34.570279
1063.571225	100357.662384	34.575296
1064.213729	100531.999374	34.580314
1065.713414	100697.497138	34.585332
1066.949158	100857.855337	34.590349
1067.817085	101026.414029	34.595367
1068.707258	101199.212420	34.600384
1069.442358	101377.813303	34.605402
1070.628646	101545.712970	34.610420
1071.556717	101724.739092	34.615437
1072.735700	101897.340684	34.620455
1073.962822	102064.299534	34.625472
1074.788409	102232.645301	34.630490
1075.743927	102417.712397	34.635508
1076.567145	102605.539007	34.640525
1077.406309	102797.910856	34.645543
1078.824924	102982.421374	34.650560
1079.854285	103162.478470	34.655578
1080.964598	103355.745164	34.660596
1081.834707	103544.115023	34.665613
1082.692587	103733.336883	34.670631
1083.898021	103930.226385	34.675648
1084.458251	104130.850109	34.680666
1085.772485	104324.937534	34.685684
1087.060768	104526.326165	34.690701
1087.821811	104728.148566	34.695719
1089.101044	104920.485802	34.700736
1090.007603	105121.032351	34.705754
1091.098833	105318.369640	34.710772
1092.501324	105519.226903	34.715789
1093.355453	105720.863531	34.720807
1094.939042	105900.882254	34.725824
1095.782903	106099.407600	34.730842
1097.072398	106285.103077	34.735860
1098.327395	106446.752163	34.740877
1099.750519	106624.409245	34.745895
1101.346271	106790.599996	34.750912
1102.503825	106958.804800	34.755930
1103.946086	107116.207828	34.760948
1104.874281	107284.073920	34.765965
1105.862264	107451.728143	34.770983
1106.566161	107628.134263	34.776000
1107.631441	107811.953226	34.781018
1108.959023	107984.112735	34.786036
1110.562485	108136.515884	34.791053
1111.810494	108302.205407	34.796071
1113.278259	108466.122879	34.801088
1114.290015	108628.193958	34.806106
1115.453285	108791.506807	34.811124
1116.433638	108951.330353	34.816141
1117.212703	109119.815984	34.821159
1118.388483	109284.510404	34.826176
1119.269052	109462.722264	34.831194
1120.009140	109637.703674	34.836212
1121.469543	109810.764011	34.841229
1122.384801	109994.217919	34.846247
1123.651426	110180.475892	34.851264
1124.313213	110357.337487	34.856282
1125.579019	110540.418291	34.861300
1126.457847	110730.622868	34.866317
1127.272511	110922.486638	34.871335
1128.648365	111111.265861	34.876352
1129.260062	111312.073087	34.881370
1130.344302	111502.108409	34.886388
1131.533665	111714.006149	34.891405
1132.584180	111916.288189	34.896423
1133.407909	112114.011652	34.901440
1134.380390	112332.906512	34.906458
1135.284317	112554.602048	34.911476
1136.111740	112774.576728	34.916493
1136.980389	113007.443560	34.921511
1138.814433	113220.597915	34.926528
1139.641889	113438.183215	34.931546
1140.882592	113668.546552	34.936564
1142.008655	113887.946632	34.941581
1143.190851	114118.931794	34.946599
1144.660141	114339.505580	34.951616
1145.627696	114563.448543	34.956634
1146.869358	114781.137915	34.961652
1148.236481	114991.585375	34.966669
1149.057747	115217.750475	34.971687
1150.487796	115428.988612	34.976704
1151.877345	115658.303544	34.981722
1152.832442	115889.696660	34.986740
1154.050278	116105.943027	34.991757
1154.971881	116319.466801	34.996775
1156.885511	116515.070233	35.001792
1157.632655	116724.939607	35.006810
1158.801425	116925.070202	35.011828
1160.157007	117142.555179	35.016845
1160.697665	117346.141428	35.021863
1162.275714	117540.364691	35.026880
1163.101935	117751.266991	35.031898
1164.359388	117974.451828	35.036916
1165.481058	118183.013094	35.041933
1166.436558	118389.969630	35.046951
1168.042597	118608.068905	35.051968
1169.075012	118823.581541	35.056986
1170.058920	119045.402091	35.062004
1171.162983	119265.264894	35.067021
1171.853673	119501.914853	35.072039
1172.984818	119718.608316	35.077056
1174.438692	119954.624339	35.082074
1175.827170	120173.482084	35.087092
1177.469386	120392.500764	35.092109
1178.698730	120610.806028	35.097127
1180.037590	120830.538847	35.102144
1181.101773	121049.851409	35.107162
1182.108537	121270.227270	35.112180
1183.645237	121488.068110	35.117197
1184.541357	121710.734641	35.122215
1185.703299	121939.072981	35.127232
1186.991779	122165.857905	35.132250
1187.691809	122406.420003	35.137268
1189.408550	122628.192408	35.142285
1190.139203	122860.844540	35.147303
1191.560603	123091.200305	35.152320
1193.268339	123309.810786	35.157338
1194.569375	123533.942281	35.162356
1195.890397	123752.444708	35.167373
1196.952489	123977.799060	35.172391
1198.540727	124190.948397	35.177408
1199.660318	124414.141492	35.182426
1200.601165	124653.260574	35.187444
1202.057334	124869.098868	35.192461
1202.885936	125101.890705	35.197479
1203.988108	125321.582487	35.202496
1205.142972	125554.930270	35.207514
1206.248577	125781.050865	35.212532
1207.624068	126013.020786	35.217549
1208.763102	126259.698021	35.222567
1209.997017	126484.914514	35.227584
1210.984610	126719.262991	35.232602
1212.165832	126961.514875	35.237620
1213.552732	127187.927084	35.242637
1214.630654	127424.876530	35.247655
1216.238099	127655.792218	35.252672
1217.189418	127879.558710	35.257690
1218.398204	128121.979609	35.262708
1220.158734	128350.288304	35.267725
1221.059899	128585.337308	35.272743
1222.523306	128804.332542	35.277760
1223.882173	129011.799143	35.282778
1224.379235	129235.538893	35.287796
1225.829421	129447.099823	35.292813
1226.812052	129671.976442	35.297831
1227.922866	129898.163739	35.302848
1229.192566	130119.533655	35.307866
1230.177785	130352.996711	35.312884
1231.279331	130576.249367	35.317901
1232.171522	130811.810678	35.322919
1233.769678	131055.239381	35.327936
1234.541685	131295.946314	35.332954
1235.695590	131540.937944	35.337972
1237.154367	131774.533040	35.342989
1238.266223	132031.629722	35.348007
1239.546950	132284.287751	35.353024
1240.759806	132527.628638	35.358042
1241.748491	132794.970563	35.363060
1243.326771	133038.176620	35.368077
1244.428201	133300.482953	35.373095
1245.440973	133563.960249	35.378112
1246.765026	133828.400610	35.383130
1247.861153	134074.080333	35.388148
1249.238367	134342.420583	35.393165
1250.311485	134604.361754	35.398183
1251.768569	134861.345356	35.403200
1252.978147	135134.918876	35.408218
1254.381596	135399.434212	35.413236
1256.022601	135657.051741	35.418253
1257.598006	135914.745872	35.423271
1258.983989	136169.317335	35.428288
1259.984619	136429.865140	35.433306
1260.696319	136699.365202	35.438324
1262.179987	136959.060963	35.443341
1263.255420	137236.478299	35.448359
1264.383112	137505.951589	35.453376
1265.459764	137779.315699	35.458394
1266.291993	138055.285133	35.463412
1268.027890	138329.948237	35.468429
1270.035971	138611.883247	35.473447
1271.331319	138882.010694	35.478464
1272.514091	139154.987188	35.483482
1273.662070	139423.292801	35.488500
1275.446790	139682.120757	35.493517
1277.064928	139947.458835	35.498535
1277.755626	140214.073577	35.503552
1279.604854	140468.217239	35.508570
1280.770972	140730.937689	35.513588
1282.460230	140983.983901	35.518605
1283.780876	141255.837340	35.523623
1285.330509	141494.581759	35.528640
1286.963814	141742.557945	35.533658
1288.238915	141996.291011	35.538676
1289.378077	142235.288231	35.543693
1290.699043	142479.024105	35.548711
1291.670040	142723.062502	35.553728
1293.136633	142953.790962	35.558746
1294.321483	143194.435385	35.563764
1295.625555	143418.257852	35.568781
1297.041841	143649.100857	35.573799
1297.991133	143890.031218	35.578816
1299.586906	144123.788721	35.583834
1300.488799	144354.457975	35.588852
1301.773184	144594.587440	35.593869
1302.643375	144842.944003	35.598887
1303.747593	145102.600106	35.603904
1305.322271	145347.022171	35.608922
1305.953425	145612.254314	35.613940
1307.304759	145870.643385	35.618957
1308.093152	146141.622973	35.623975
1309.056361	146414.794101	35.628992
1310.447312	146676.948808	35.634010
1311.805502	146972.479584	35.639028
1313.145757	147246.683045	35.644045
1314.578639	147521.430728	35.649063
1316.084748	147797.550366	35.654080
1318.113061	148074.191456	35.659098
1319.731794	148343.700567	35.664116
1321.328954	148609.384914	35.669133
1322.825162	148859.119881	35.674151
1324.355305	149121.686488	35.679168
1325.648228	149379.222052	35.684186
1326.820849	149645.163926	35.689204
1327.777869	149911.385559	35.694221
1328.977522	150179.229118	35.699239
1330.158414	150461.664408	35.704256
1331.703273	150717.187183	35.709274
1332.873607	151006.515773	35.714292
1333.947258	151285.373160	35.719309
1335.068585	151568.714679	35.724327
1336.148402	151853.371881	35.729344
1337.508373	152140.494766	35.734362
1338.605094	152440.108505	35.739380
1340.058201	152731.989249	35.744397
1341.222510	153033.752383	35.749415
1342.360314	153327.442043	35.754432
1343.875075	153607.902273	35.759450
1345.437403	153915.604076	35.764468
1347.267494	154201.634076	35.769485
1349.244663	154490.863041	35.774503
1350.630435	154783.404750	35.779520
1352.553430	155044.307744	35.784538
1354.156600	155328.989271	35.789556
1355.354387	155598.671591	35.794573
1356.757489	155860.962824	35.799591
1357.932747	156138.898373	35.804608
1359.547430	156407.867765	35.809626
1360.723355	156674.414891	35.814644
1362.067634	156947.062342	35.819661
1363.411476	157214.028271	35.824679
1364.802174	157467.933738	35.829696
1366.222918	157725.108716	35.834714
1367.324676	157986.462993	35.839732
1368.316238	158239.261700	35.844749
1369.727800	158502.545315	35.849767
1370.559548	158769.824653	35.854784
1372.357413	159027.983498	35.859802
1373.383928	159308.046585	35.864820
1374.563436	159581.894141	35.869837
1375.882324	159861.682526	35.874855
1376.437507	160157.703413	35.879872
1377.936828	160445.127801	35.884890
1379.154085	160737.410897	35.889908
1380.257647	161034.029169	35.894925
1381.480023	161340.715698	35.899943
1382.718597	161658.351009	35.904960
1384.238613	161964.775381	35.909978
1385.160588	162277.127964	35.914996
1386.513361	162602.997736	35.920013
1387.858499	162933.921061	35.925031
1389.338565	163250.321411	35.930048
1390.740088	163580.110769	35.935066
1392.593787	163899.941111	35.940084
1394.220563	164217.731744	35.945101
1395.459307	164539.765564	35.950119
1396.388000	164873.883476	35.955136
1398.365916	165195.732115	35.960154
1399.845174	165525.230875	35.965172
1401.264654	165847.052908	35.970189
1403.246899	166163.768839	35.975207
1405.100304	166477.742864	35.980224
1406.749641	166773.164581	35.985242
1408.665659	167071.917886	35.990260
1410.210867	167369.175850	35.995277
1412.022197	167666.770886	36.000295
1413.596258	167962.987260	36.005312
1415.252209	168252.770678	36.010330
1416.731064	168529.274935	36.015348
1418.074428	168825.587102	36.020365
1419.819098	169102.188877	36.025383
1420.973426	169382.738325	36.030400
1422.321690	169671.707687	36.035418
1424.081642	169956.687198	36.040436
1425.075305	170241.850346	36.045453
1426.514659	170527.878005	36.050471
1427.985083	170827.049052	36.055488
1429.402229	171118.452006	36.060506
1430.447743	171410.948261	36.065524
1431.489574	171715.261666	36.070541
1432.436904	172011.940838	36.075559
1433.165421	172325.715353	36.080576
1434.326972	172639.760441	36.085594
1435.593470	172951.847927	36.090612
1436.950289	173293.224959	36.095629
1438.605505	173604.539415	36.100647
1439.950056	173929.018760	36.105664
1441.827167	174234.601001	36.110682
1443.639149	174536.921976	36.115700
1444.688511	174842.992298	36.120717
1446.301119	175150.757574	36.125735
1447.030105	175462.331075	36.130752
1448.378933	175773.787739	36.135770
1449.920183	176087.370952	36.140788
1451.079976	176405.082697	36.145805
1452.600407	176721.732072	36.150823
1454.118754	177051.012045	36.155840
1455.805335	177375.150545	36.160858
1457.444482	177698.753459	36.165876
1458.612571	178033.925256	36.170893
1460.582868	178356.929864	36.175911
1462.130905	178663.813585	36.180928
1464.248835	178980.196888	36.185946
1465.847615	179299.031712	36.190964
1467.092524	179615.619018	36.195981
1468.668588	179923.736464	36.200999
1470.209173	180248.146260	36.206016
1472.323439	180535.664055	36.211034
1473.851097	180838.058030	36.216052
1475.834103	181152.408484	36.221069
1477.974302	181442.795258	36.226087
1479.568117	181740.270863	36.231104
1480.901117	182029.618484	36.236122
1482.948597	182319.632334	36.241140
1484.010705	182601.388157	36.246157
1485.806047	182872.268866	36.251175
1486.747790	183169.470339	36.256192
1488.291415	183454.930687	36.261210
1489.684730	183742.449154	36.266228
1490.966070	184039.736786	36.271245
1492.732366	184323.868744	36.276263
1493.944617	184624.877785	36.281280
1495.485193	184916.223195	36.286298
1497.208411	185217.008311	36.291316
1498.240425	185516.377360	36.296333
1499.945154	185823.706101	36.301351
1500.800877	186130.458226	36.306368
1502.108537	186454.753807	36.311386
1503.129279	186765.073435	36.316404
1504.354762	187104.644886	36.321421
1505.639009	187488.383880	36.326439
1506.770821	187825.525556	36.331456
1508.062937	188165.218663	36.336474
1509.215401	188508.479336	36.341492
1510.643100	188860.580990	36.346509
1512.217704	189211.148920	36.351527
1513.935498	189564.588749	36.356544
1515.327129	189918.175313	36.361562
1516.946090	190253.482687	36.366580
1518.215739	190620.512519	36.371597
1519.739592	190968.750690	36.376615
1521.356392	191305.676405	36.381632
1522.324686	191650.408097	36.386650
1523.975188	191996.408709	36.391668
1524.773312	192343.801208	36.396685
1526.748387	192694.129929	36.401703
1528.158109	193056.313172	36.406720
1529.747562	193405.480340	36.411738
1531.640374	193756.209811	36.416756
1533.586929	194110.029691	36.421773
1535.720122	194443.011507	36.426791
1537.633902	194781.758297	36.431808
1539.496023	195116.948179	36.436826
1541.347484	195438.861811	36.441844
1542.775277	195769.330312	36.446861
1544.621524	196096.021640	36.451879
1545.928255	196432.328842	36.456896
1547.402502	196757.461948	36.461914
1549.414619	197083.609129	36.466932
1551.054503	197417.426547	36.471949
1552.963251	197734.631042	36.476967
1554.740340	198052.341981	36.481984
1556.355547	198364.343342	36.487002
1558.632441	198673.261921	36.492020
1560.236708	198979.770370	36.497037
1561.251372	199286.520702	36.502055
1562.626390	199596.029325	36.507072
1563.700766	199918.236534	36.512090
1565.409104	200232.998049	36.517108
1566.788995	200574.289759	36.522125
1568.272253	200905.446066	36.527143
1569.644832	201244.393266	36.532160
1570.658397	201581.460838	36.537178
1572.196064	201923.531735	36.542196
1573.175867	202274.854195	36.547213
1574.510115	202627.527024	36.552231
1575.927910	203003.689568	36.557248
1577.438958	203361.185863	36.562266
1579.396323	203713.261923	36.567284
1580.547227	204088.167656	36.572301
1582.587546	204447.508421	36.577319
1584.952162	204806.325548	36.582336
1586.374275	205159.375868	36.587354
1588.405337	205510.888745	36.592372
1589.684434	205871.826475	36.597389
1592.032757	206215.060130	36.602407
1593.780287	206558.525024	36.607424
1595.088831	206910.967604	36.612442
1597.216967	207235.577561	36.617460
1598.879086	207581.854879	36.622477
1600.276191	207924.420409	36.627495
1601.729844	208267.295115	36.632512
1602.975298	208612.822631	36.637530
1604.742119	208960.243242	36.642548
1606.344252	209312.620313	36.647565
1607.633140	209651.719356	36.652583
1609.254452	209994.038984	36.657600
1610.559075	210324.782537	36.662618
1612.336125	210651.967164	36.667636
1614.107901	210985.401492	36.672653
1615.583617	211319.421057	36.677671
1617.119812	211654.015643	36.682688
1618.695612	211995.893626	36.687706
1620.091461	212325.257522	36.692724
1622.079592	212667.194446	36.697741
1623.835324	213005.032644	36.702759
1625.322628	213351.248327	36.707776
1626.406553	213690.956363	36.712794
1628.038777	214031.663895	36.717812
1629.052745	214397.266518	36.722829
1630.917077	214757.416903	36.727847
1632.517791	215125.055290	36.732864
1633.670235	215502.473762	36.737882
1634.951874	215863.870814	36.742900
1636.243031	216259.707387	36.747917
1637.664152	216653.288233	36.752935
1638.990415	217045.743906	36.757952
1640.014778	217464.413096	36.762970
1641.624267	217874.094376	36.767988
1643.408033	218291.189229	36.773005
1644.833302	218716.957224	36.778023
1646.674152	219131.277132	36.783040
1648.562967	219560.321785	36.788058
1650.016242	219978.267068	36.793076
1651.714390	220410.979706	36.798093
1653.189298	220836.696626	36.803111
1654.995150	221261.494940	36.808128
1656.629474	221703.798952	36.813146
1658.695852	222134.956544	36.818164
1660.365339	222572.050920	36.823181
1661.934575	223001.213950	36.828199
1663.930326	223437.646059	36.833216
1665.335464	223874.764968	36.838234
1667.526435	224298.339796	36.843252
1669.809979	224727.208817	36.848269
1671.265996	225154.011054	36.853287
1673.211146	225584.896645	36.858304
1674.997156	226000.697718	36.863322
1677.304507	226408.155781	36.868340
1679.556217	226820.095074	36.873357
1681.083483	227229.670306	36.878375
1683.175217	227628.837543	36.883392
1684.098537	228035.775211	36.888410
1686.091641	228438.365297	36.893428
1687.715663	228861.213282	36.898445
1688.936654	229278.848061	36.903463
1690.932322	229681.771338	36.908480
1692.143306	230106.624002	36.913498
1693.646435	230519.540157	36.918516
1695.628569	230945.330037	36.923533
1696.699640	231357.509477	36.928551
1698.302907	231764.874286	36.933568
1699.878361	232171.559032	36.938586
1701.216614	232582.730598	36.943604
1703.208738	232999.278011	36.948621
1704.183367	233420.979209	36.953639
1706.068474	233834.549557	36.958656
1707.781123	234266.718967	36.963674
1709.236994	234696.545575	36.968692
1710.923836	235127.324334	36.973709
1712.038627	235566.101907	36.978727
1713.867003	236008.009835	36.983744
1715.157131	236470.967432	36.988762
1716.985857	236921.768003	36.993780
1718.514171	237378.336414	36.998797
1719.612205	237852.938711	37.003815
1721.268603	238322.416895	37.008832
1722.986286	238803.341985	37.013850
1724.427918	239283.045204	37.018868
1726.443445	239763.184673	37.023885
1728.041273	240243.650583	37.028903
1730.044857	240730.424014	37.033920
1732.037368	241223.525481	37.038938
1734.508449	241692.870864	37.043956
1736.895590	242166.372035	37.048973
1739.067530	242626.752282	37.053991
1741.355338	243074.589943	37.059008
1743.581513	243530.466062	37.064026
1745.533324	243973.891661	37.069044
1747.692279	244420.483182	37.074061
1749.327415	244861.830336	37.079079
1750.815150	245302.060147	37.084096
1752.516137	245765.497610	37.089114
1754.430462	246212.793738	37.094132
1755.730660	246647.138356	37.099149
1757.679967	247106.724508	37.104167
1760.586655	247532.005819	37.109184
1762.185696	247973.057856	37.114202
1763.875082	248397.938553	37.119220
1766.350798	248831.779379	37.124237
1767.902373	249267.836309	37.129255
1769.814858	249681.019904	37.134272
1771.741458	250120.163319	37.139290
1773.714558	250534.505676	37.144308
1775.696488	250959.084236	37.149325
1777.481572	251383.645918	37.154343
1779.155719	251791.689376	37.159360
1780.713794	252215.452035	37.164378
1782.250416	252650.675385	37.169396
1783.730328	253063.985694	37.174413
1785.139007	253501.847809	37.179431
1786.867030	253925.531277	37.184448
1788.674700	254367.440733	37.189466
1790.304974	254802.521787	37.194484
1792.162749	255248.919243	37.199501
1793.354610	255680.595216	37.204519
1795.487421	256104.921166	37.209536
1797.327796	256539.433049	37.214554
1798.497900	256953.762439	37.219572
1800.524824	257373.838792	37.224589
1801.993228	257807.067907	37.229607
1803.663139	258235.385087	37.234624
1805.198406	258670.634903	37.239642
1807.182496	259112.234858	37.244660
1809.014554	259547.713138	37.249677
1810.466770	260002.461062	37.254695
1812.209189	260447.124930	37.259712
1813.604158	260908.639536	37.264730
1815.426759	261369.801340	37.269748
1817.271702	261833.245361	37.274765
1818.744603	262300.639433	37.279783
1820.544606	262777.732040	37.284800
1822.157974	263272.358955	37.289818
1823.380450	263749.727461	37.294836
1825.319652	264242.773659	37.299853
1826.936900	264750.913064	37.304871
1828.781117	265244.203200	37.309888
1830.920524	265745.114027	37.314906
1832.820003	266252.314462	37.319924
1834.707253	266748.847173	37.324941
1836.325117	267263.334378	37.329959
1838.114777	267779.874546	37.334976
1840.250493	268306.465110	37.339994
1841.469770	268814.870861	37.345012
1843.634656	269332.640116	37.350029
1845.775426	269851.784413	37.355047
1847.554996	270368.296951	37.360064
1850.202495	270871.730222	37.365082
1852.291545	271385.952608	37.370100
1854.319583	271890.328316	37.375117
1856.448586	272390.392797	37.380135
1858.898452	272891.417532	37.385152
1860.751464	273391.984515	37.390170
1862.962883	273896.807559	37.395188
1864.585294	274389.333992	37.400205
1865.892797	274894.309505	37.405223
1868.186569	275399.445412	37.410240
1869.901422	275898.862104	37.415258
1871.480042	276410.773312	37.420276
1873.047345	276918.290658	37.425293
1874.491930	277437.283967	37.430311
1876.268331	277969.351888	37.435328
1878.006850	278497.538353	37.440346
1879.277304	279012.086493	37.445364
1882.043070	279528.765173	37.450381
1884.236791	280061.568566	37.455399
1886.516910	280564.178650	37.460416
1889.138716	281076.609948	37.465434
1891.000033	281584.851539	37.470452
1893.683938	282076.109859	37.475469
1895.466658	282563.837658	37.480487
1897.641109	283030.896696	37.485504
1899.343031	283502.480323	37.490522
1900.939936	283962.573846	37.495540
1903.536032	284421.682230	37.500557
1905.511153	284889.404645	37.505575
1907.082215	285333.495845	37.510592
1908.941341	285797.831459	37.515610
1910.665137	286261.452071	37.520628
1912.595870	286719.981053	37.525645
1914.218001	287195.579491	37.530663
1915.731615	287669.010382	37.535680
1917.163049	288157.414313	37.540698
1918.485293	288645.149283	37.545716
1920.728141	289133.715536	37.550733
1921.922771	289651.389596	37.555751
1923.845138	290153.544790	37.560768
1925.723435	290666.754296	37.565786
1927.164434	291197.562073	37.570804
1928.597528	291722.755558	37.575821
1930.324803	292270.298531	37.580839
1931.929477	292813.567408	37.585856
1934.002068	293364.220964	37.590874
1935.928653	293915.684138	37.595892
1938.071742	294466.853526	37.600909
1939.628892	295028.127390	37.605927
1941.536580	295601.961407	37.610944
1943.619948	296172.714438	37.615962
1945.142723	296740.512415	37.620980
1947.815904	297306.865972	37.625997
1949.726745	297877.232610	37.631015
1951.798274	298459.810226	37.636032
1953.839599	299032.027300	37.641050
1956.238058	299600.979819	37.646068
1958.735297	300156.756221	37.651085
1961.060689	300724.596998	37.656103
1962.876005	301287.137366	37.661120
1964.675584	301848.584906	37.666138
1966.750186	302424.102503	37.671156
1968.677595	302986.181394	37.676173
1970.949649	303547.308889	37.681191
1973.039137	304110.927432	37.686208
1974.639685	304684.682748	37.691226
1976.540474	305253.963966	37.696244
1978.741170	305814.199958	37.701261
1980.854267	306390.649514	37.706279
1982.895698	306964.339190	37.711296
1985.017055	307531.281424	37.716314
1987.058963	308093.916095	37.721332
1989.118239	308653.724988	37.726349
1990.837462	309222.831701	37.731367
1992.678183	309783.228567	37.736384
1994.717558	310362.328348	37.741402
1996.305438	310940.891481	37.746420
1998.437903	311511.129419	37.751437
2000.251097	312089.061092	37.756455
2002.041319	312651.146632	37.761472
2004.236680	313207.800573	37.766490
2006.009295	313775.543126	37.771508
2008.239119	314328.424322	37.776525
2009.927745	314886.624653	37.781543
2012.009572	315438.506748	37.786560
2014.356434	316003.238418	37.791578
2015.635509	316575.283238	37.796596
2018.247122	317136.938632	37.801613
2020.736419	317697.620000	37.806631
2022.652052	318263.676194	37.811648
2025.027253	318816.953355	37.816666
2026.342283	319390.719965	37.821684
2028.327620	319963.198915	37.826701
2030.887485	320520.974967	37.831719
2033.370187	321088.509238	37.836736
2035.931432	321650.312223	37.841754
2037.505817	322221.622424	37.846772
2039.933184	322777.268447	37.851789
2041.780021	323348.750184	37.856807
2043.616245	323915.810689	37.861824
2045.368337	324483.743511	37.866842
2047.523713	325061.427435	37.871860
2049.371117	325636.416485	37.876877
2051.565909	326229.848539	37.881895
2053.727089	326813.607538	37.886912
2055.795422	327400.042267	37.891930
2057.434114	327995.353946	37.896948
2059.084619	328584.285239	37.901965
2061.017894	329182.834474	37.906983
2062.763769	329780.597021	37.912000
2065.132218	330384.288656	37.917018
2066.939740	331009.241604	37.922036
2068.754971	331615.273726	37.927053
2070.976231	332236.537121	37.932071
2072.777540	332863.424541	37.937088
2074.855785	333484.469514	37.942106
2076.703847	334122.376574	37.947124
2078.800428	334745.256692	37.952141
2081.241191	335378.122588	37.957159
2083.362507	336006.745546	37.962176
2085.737195	336634.530612	37.967194
2087.765121	337283.587470	37.972212
2089.530287	337918.593537	37.977229
2091.954618	338565.484729	37.982247
2093.716274	339208.242037	37.987264
2095.731452	339852.292870	37.992282
2097.348092	340499.347638	37.997300
2099.585957	341147.785061	38.002317
2101.512739	341810.708592	38.007335
2103.573387	342467.432639	38.012352
2105.838796	343119.112744	38.017370
2107.761310	343786.704762	38.022388
2109.689052	344451.596167	38.027405
2112.419397	345120.959782	38.032423
2114.239332	345763.060522	38.037440
2116.539916	346397.964174	38.042458
2118.246645	347039.025809	38.047476
2120.522445	347678.737537	38.052493
2122.926225	348314.408665	38.057511
2124.526660	348957.744976	38.062528
2126.483924	349602.558869	38.067546
2128.462528	350261.849338	38.072564
2130.811961	350912.438715	38.077581
2133.136136	351562.032993	38.082599
2135.112570	352230.428927	38.087616
2137.569043	352884.725614	38.092634
2139.556354	353552.439174	38.097652
2141.696583	354217.502508	38.102669
2143.828456	354881.846239	38.107687
2145.971738	355551.937022	38.112704
2148.526586	356215.273594	38.117722
2150.713384	356877.647472	38.122740
2153.132662	357541.467739	38.127757
2155.473164	358208.664938	38.132775
2157.449336	358882.661963	38.137792
2159.566421	359551.828513	38.142810
2161.579356	360229.297523	38.147828
2163.199512	360914.229912	38.152845
2165.899528	361593.612806	38.157863
2167.702138	362290.945981	38.162880
2170.104078	362974.541415	38.167898
2171.904597	363672.382633	38.172916
2173.667551	364368.746192	38.177933
2175.742767	365068.569518	38.182951
2177.600832	365790.713850	38.187968
2179.960043	366491.248397	38.192986
2181.674174	367224.043136	38.198004
2183.538438	367951.014481	38.203021
2185.886795	368691.306293	38.208039
2188.360161	369420.325543	38.213056
2190.048850	370157.529737	38.218074
2192.463176	370906.997066	38.223092
2194.824857	371634.468676	38.228109
2197.562559	372389.657375	38.233127
2199.342302	373136.091926	38.238144
2202.376980	373864.492899	38.243162
2204.184654	374613.072053	38.248180
2206.765346	375352.905968	38.253197
2209.237477	376087.138174	38.258215
2211.320661	376820.279942	38.263232
2213.913452	377557.046315	38.268250
2216.273514	378297.589228	38.273268
2218.362022	379029.312706	38.278285
2221.077940	379759.619662	38.283303
2223.219848	380491.834224	38.288320
2225.912271	381207.204062	38.293338
2228.870166	381923.450964	38.298356
2231.248146	382629.310066	38.303373
2233.914192	383309.421558	38.308391
2235.724887	383993.062167	38.313408
2238.262705	384656.104551	38.318426
2240.286317	385326.370211	38.323444
2242.520017	385989.614164	38.328461
2244.834782	386666.925250	38.333479
2246.939292	387329.427799	38.338496
2249.385638	387997.612165	38.343514
2251.609931	388652.663925	38.348532
2253.234700	389326.232620	38.353549
2255.603161	389998.746850	38.358567
2257.971401	390678.622378	38.363584
2259.681147	391360.901811	38.368602
2261.728659	392055.705156	38.373620
2263.644314	392749.349074	38.378637
2266.202205	393442.208124	38.383655
2267.931111	394152.477658	38.388672
2269.992646	394863.484272	38.393690
2272.240267	395582.678434	38.398708
2274.055539	396307.504204	38.403725
2276.581199	397032.494586	38.408743
2278.756976	397769.361021	38.413760
2281.055401	398499.599071	38.418778
2283.512092	399236.633258	38.423796
2285.709651	399963.835682	38.428813
2288.374314	400698.034442	38.433831
2291.330870	401435.027389	38.438848
2293.425283	402165.788691	38.443866
2295.840014	402902.430237	38.448884
2297.382576	403655.745774	38.453901
2299.663773	404402.048640	38.458919
2301.634912	405169.462668	38.463936
2303.814554	405930.106040	38.468954
2305.464910	406704.777227	38.473972
2307.767707	407485.318509	38.478989
2310.109330	408261.042835	38.484007
2312.148469	409060.632861	38.489024
2314.258584	409853.828882	38.494042
2316.621898	410652.277071	38.499060
2319.188032	411450.995684	38.504077
2321.553005	412258.082570	38.509095
2323.728484	413063.302681	38.514112
2326.002307	413864.909990	38.519130
2328.709330	414681.487055	38.524148
2330.960586	415499.432956	38.529165
2333.262254	416317.698594	38.534183
2335.356175	417131.592512	38.539200
2337.396305	417952.990150	38.544218
2339.929572	418781.873107	38.549236
2342.070287	419620.316257	38.554253
2344.562542	420447.631677	38.559271
2347.191196	421270.262790	38.564288
2349.881772	422099.944908	38.569306
2352.605090	422916.884120	38.574324
2354.803423	423747.759071	38.579341
2357.253753	424551.778727	38.584359
2359.328327	425353.456275	38.589376
2361.437064	426151.557316	38.594394
2364.172455	426946.841438	38.599412
2366.562441	427737.703102	38.604429
2369.440868	428519.494684	38.609447
2371.611119	429316.213319	38.614464
2373.923465	430106.603855	38.619482
2376.278886	430903.591177	38.624500
2378.183518	431706.499666	38.629517
2380.438939	432505.524307	38.634535
2382.900081	433325.338280	38.639552
2384.888650	434141.914057	38.644570
2387.005493	434961.120952	38.649588
2389.266779	435787.965835	38.654605
2391.352188	436620.225263	38.659623
2394.122640	437463.823681	38.664640
2395.872341	438296.685593	38.669658
2398.638792	439150.543619	38.674676
2400.697823	440014.254946	38.679693
2403.277477	440866.965556	38.684711
2405.539039	441732.902263	38.689728
2407.632967	442587.197386	38.694746
2410.723536	443449.484077	38.699764
2413.039882	444317.888652	38.704781
2415.426680	445187.257920	38.709799
2418.205617	446057.030781	38.714816
2420.874145	446932.705071	38.719834
2423.497195	447800.359611	38.724852
2425.943918	448683.636943	38.729869
2428.387122	449551.402000	38.734887
2430.544463	450435.363225	38.739904
2432.670880	451320.354280	38.744922
2435.733833	452205.906086	38.749940
2437.671075	453098.944448	38.754957
2440.088070	453999.143262	38.759975
2442.498236	454880.899260	38.764992
2445.067419	455796.464757	38.770010
2447.366615	456687.919361	38.775028
2449.873788	457592.190586	38.780045
2452.239585	458508.375725	38.785063
2454.548700	459420.838456	38.790080
2456.179387	460334.992899	38.795098
2458.981921	461264.877334	38.800116
2460.971169	462197.586306	38.805133
2463.312993	463126.096952	38.810151
2466.296642	464078.408999	38.815168
2468.538852	465010.586839	38.820186
2471.088069	465946.507913	38.825204
2473.825651	466902.159519	38.830221
2476.358936	467833.999579	38.835239
2478.951182	468785.893471	38.840256
2481.298518	469730.405176	38.845274
2484.341330	470666.364440	38.850292
2486.699366	471604.061378	38.855309
2489.199976	472533.250950	38.860327
2491.919264	473462.710537	38.865344
2494.212762	474378.710052	38.870362
2496.511660	475274.914553	38.875380
2498.925266	476186.510739	38.880397
2501.785440	477093.086523	38.885415
2504.337886	478001.285988	38.890432
2506.529317	478912.178279	38.895450
2509.215619	479818.042144	38.900468
2511.541663	480736.797940	38.905485
2513.794564	481651.429552	38.910503
2516.338323	482572.023323	38.915520
2519.051377	483500.769777	38.920538
2521.935927	484421.209634	38.925556
2524.575017	485332.254197	38.930573
2527.755305	486238.919011	38.935591
2531.083886	487157.221813	38.940608
2532.914210	488072.300261	38.945626
2535.818855	488980.434506	38.950644
2538.452133	489901.032891	38.955661
2540.628334	490816.765231	38.960679
2543.052720	491737.149767	38.965696
2545.544510	492657.372376	38.970714
2548.233143	493577.965779	38.975732
2550.304370	494514.608528	38.980749
2552.999456	495447.157639	38.985767
2555.657158	496391.163607	38.990784
2557.525581	497344.180092	38.995802
2560.238515	498283.832510	39.000820
2562.601082	499240.691511	39.005837
2565.086304	500202.770108	39.010855
2567.786341	501163.343775	39.015872
2570.117673	502129.774232	39.020890
2573.265191	503098.781656	39.025908
2575.424487	504078.388617	39.030925
2578.131360	505040.296284	39.035943
2580.734195	506018.247948	39.040960
2582.829545	507010.393621	39.045978
2585.570880	507990.923995	39.050996
2588.216768	508979.022243	39.056013
2590.942560	509963.315432	39.061031
2593.269750	510966.062968	39.066048
2595.299002	511972.023268	39.071066
2598.495058	512976.510283	39.076084
2600.674708	513991.537851	39.081101
2603.084958	515012.204343	39.086119
2606.068483	516028.170997	39.091136
2608.358396	517042.879452	39.096154
2611.234577	518057.571997	39.101172
2613.902017	519087.043707	39.106189
2616.545611	520108.743046	39.111207
2619.127464	521135.119047	39.116224
2621.693838	522170.745883	39.121242
2624.452180	523195.289785	39.126260
2626.651717	524235.772825	39.131277
2629.147802	525263.040397	39.136295
2631.837923	526271.070177	39.141312
2634.328842	527274.181727	39.146330
2636.754019	528283.630359	39.151348
2639.903308	529284.227282	39.156365
2642.541855	530282.427008	39.161383
2645.223205	531290.215618	39.166400
2647.455960	532301.081385	39.171418
2650.194508	533319.943459	39.176436
2652.652331	534336.416433	39.181453
2655.017466	535366.269185	39.186471
2657.752927	536392.009657	39.191488
2659.971281	537432.355817	39.196506
2662.443909	538476.707915	39.201524
2664.736223	539541.035770	39.206541
2667.121462	540599.734287	39.211559
2670.114782	541661.921027	39.216576
2672.380000	542748.041647	39.221594
2674.920158	543832.874093	39.226612
2677.865809	544923.235012	39.231629
2680.373540	546032.038684	39.236647
2683.122540	547130.354570	39.241664
2685.574757	548251.659160	39.246682
2687.591911	549361.685596	39.251700
2690.264204	550493.325313	39.256717
2692.688593	551625.516182	39.261735
2695.120732	552770.728227	39.266752
2697.995915	553936.923922	39.271770
2700.653479	555093.508011	39.276788
2703.025635	556262.451159	39.281805
2705.890140	557433.418012	39.286823
2708.507523	558606.483694	39.291840
2711.512304	559789.575831	39.296858
2714.370328	560960.431563	39.301876
2717.805770	562128.271380	39.306893
2721.028860	563294.586460	39.311911
2724.174592	564467.940217	39.316928
2727.051001	565653.936278	39.321946
2730.181814	566813.573013	39.326964
2732.993249	567966.482861	39.331981
2735.712341	569130.096359	39.336999
2738.751030	570292.695572	39.342016
2741.376812	571458.821851	39.347034
2743.907281	572623.401419	39.352052
2746.811688	573782.139266	39.357069
2749.656441	574949.158804	39.362087
2752.573946	576110.839338	39.367104
2755.275905	577282.881907	39.372122
2758.679994	578429.865419	39.377140
2761.469675	579587.479675	39.382157
2764.296178	580741.718906	39.387175
2766.959177	581892.918730	39.392192
2769.914870	583044.962631	39.397210
2773.036011	584194.713220	39.402228
2775.872437	585353.977921	39.407245
2778.157679	586501.395913	39.412263
2780.850517	587612.397976	39.417280
2782.953600	588743.794583	39.422298
2785.965586	589852.078180	39.427316
2788.161448	590971.421122	39.432333
2790.553472	592109.362542	39.437351
2793.512811	593238.380547	39.442368
2795.313317	594390.129384	39.447386
2798.437439	595533.575122	39.452404
2801.607525	596692.977109	39.457421
2804.367589	597839.914570	39.462439
2807.548458	598994.577895	39.467456
2809.933143	600166.985255	39.472474
2812.528615	601327.923260	39.477492
2815.634882	602497.115909	39.482509
2817.986948	603687.339119	39.487527
2820.742699	604861.854676	39.492544
2823.416202	606060.632352	39.497562
2826.104869	607265.134326	39.502580
2829.000524	608476.326098	39.507597
2831.541700	609692.850211	39.512615
2834.433664	610907.881425	39.517632
2837.112642	612145.322387	39.522650
2839.838900	613373.965831	39.527668
2843.008421	614610.597254	39.532685
2845.080283	615863.376104	39.537703
2848.026952	617111.763151	39.542720
2850.390486	618374.052958	39.547738
2852.871440	619650.670257	39.552756
2856.237257	620928.885058	39.557773
2858.663359	622226.696251	39.562791
2861.531453	623515.632124	39.567808
2864.442442	624816.095170	39.572826
2867.484124	626116.677189	39.577844
2869.970311	627417.794388	39.582861
2873.066702	628733.578679	39.587879
2875.886247	630047.498679	39.592896
2879.227039	631364.909780	39.597914
2882.206320	632675.727613	39.602932
2885.260896	634005.583909	39.607949
2887.573450	635340.437267	39.612967
2890.805603	636674.312827	39.617984
2893.994672	638008.222849	39.623002
2896.827416	639347.458156	39.628020
2899.673634	640676.141114	39.633037
2902.962289	642018.240548	39.638055
2906.192065	643341.373235	39.643072
2909.318023	644662.555768	39.648090
2912.180114	645998.865349	39.653108
2915.432819	647326.007988	39.658125
2918.146441	648652.967088	39.663143
2921.497287	649969.574501	39.668160
2924.512593	651306.443853	39.673178
2927.050946	652653.028663	39.678196
2929.983373	653979.387348	39.683213
2932.596782	655299.296127	39.688231
2935.664453	656585.235024	39.693248
2939.121411	657873.875752	39.698266
2941.883412	659155.693408	39.703284
2945.143924	660434.468668	39.708301
2947.815232	661715.315462	39.713319
2950.773861	662988.427906	39.718336
2953.637633	664273.280215	39.723354
2956.001482	665560.532840	39.728372
2958.965228	666852.881665	39.733389
2961.818960	668147.062887	39.738407
2964.955723	669445.594108	39.743424
2968.149504	670741.151999	39.748442
2970.806262	672057.853028	39.753460
2973.469033	673377.251114	39.758477
2976.353334	674702.439048	39.763495
2978.943069	676034.744258	39.768512
2981.996437	677376.021126	39.773530
2984.805071	678723.752768	39.778548
2988.061945	680065.745955	39.783565
2990.958284	681435.716782	39.788583
2993.773903	682797.599706	39.793600
2996.413668	684161.443955	39.798618
2999.147846	685549.939792	39.803636
3002.042832	686925.636177	39.808653
3004.889620	688333.787818	39.813671
3007.619685	689730.126505	39.818688
3010.942032	691141.477060	39.823706
3013.851951	692557.486293	39.828724
3017.162612	693969.877937	39.833741
3019.676466	695403.256455	39.838759
3022.934464	696836.770499	39.843776
3025.941717	698267.862335	39.848794
3028.957571	699711.754686	39.853812
3032.351303	701150.932484	39.858829
3035.370818	702597.665517	39.863847
3039.009661	704038.799315	39.868864
3041.997945	705480.694845	39.873882
3044.732248	706927.938553	39.878900
3048.034957	708382.317550	39.883917
3050.829146	709836.386772	39.888935
3053.939103	711291.687713	39.893952
3057.640981	712750.151279	39.898970
3060.471782	714212.915394	39.903988
3063.202887	715669.257620	39.909005
3066.182891	717139.946014	39.914023
3069.254269	718598.638217	39.919040
3072.674618	720068.239720	39.924058
3075.389461	721555.202647	39.929076
3078.548644	723022.543843	39.934093
3081.477007	724524.208595	39.939111
3084.138324	726007.608140	39.944128
3087.505664	727494.026525	39.949146
3090.393690	728990.726902	39.954164
3093.702125	730483.622197	39.959181
3096.717193	731963.601926	39.964199
3099.268252	733421.815191	39.969216
3102.555911	734885.017698	39.974234
3105.414096	736348.371156	39.979252
3108.400082	737802.207313	39.984269
3111.335270	739274.827823	39.989287
3113.811686	740748.288329	39.994304
3116.687730	742220.517595	39.999322
3119.550086	743723.041535	40.004340
3122.594236	745219.922312	40.009357
3125.618807	746732.585964	40.014375
3128.522109	748258.428005	40.019392
3131.777568	749776.223996	40.024410
3134.814217	751315.578994	40.029428
3138.320597	752844.351874	40.034445
3141.187577	754390.210642	40.039463
3143.937708	755928.195712	40.044480
3147.398030	757491.980550	40.049498
3150.444281	759055.857982	40.054516
3153.654021	760619.088598	40.059533
3156.752979	762193.276823	40.064551
3159.899570	763775.240315	40.069568
3162.987082	765356.928198	40.074586
3166.351590	766953.028022	40.079604
3169.570289	768550.922526	40.084621
3172.940505	770152.671147	40.089639
3175.977969	771756.633471	40.094656
3178.763813	773359.109587	40.099674
3182.185487	774979.096551	40.104692
3185.489251	776592.803705	40.109709
3188.385798	778217.558707	40.114727
3191.904068	779849.987722	40.119744
3195.070394	781474.552495	40.124762
3198.231981	783106.107251	40.129780
3201.547107	784749.571124	40.134797
3204.735907	786394.589553	40.139815
3207.957794	788023.832028	40.144832
3211.602533	789655.861210	40.149850
3214.885306	791309.814998	40.154868
3218.186908	792948.095624	40.159885
3222.076542	794595.440635	40.164903
3225.319798	796232.471523	40.169920
3228.771919	797867.710837	40.174938
3232.006943	799504.460483	40.179956
3235.284602	801143.896553	40.184973
3238.245424	802793.168520	40.189991
3241.514519	804433.140903	40.195008
3244.714824	806080.014756	40.200026
3247.683154	807737.525665	40.205044
3251.285066	809376.640596	40.210061
3255.109582	811023.868126	40.215079
3258.247987	812674.472361	40.220096
3261.802982	814315.713410	40.225114
3264.932655	815961.895728	40.230132
3268.642473	817589.906698	40.235149
3271.742548	819210.792161	40.240167
3274.609176	820799.811095	40.245184
3278.608083	822377.281751	40.250202
3281.388867	823959.359343	40.255220
3284.913342	825535.078865	40.260237
3287.982461	827116.148242	40.265255
3291.247876	828701.866392	40.270272
3294.421192	830270.750046	40.275290
3297.782711	831851.345298	40.280308
3300.777346	833440.134498	40.285325
3304.044755	835033.156135	40.290343
3307.133611	836635.640303	40.295360
3310.316695	838235.711215	40.300378
3313.378184	839862.634165	40.305396
3316.803734	841474.880056	40.310413
3320.079017	843099.377722	40.315431
3322.552272	844743.905430	40.320448
3326.026819	846378.211673	40.325466
3329.483403	848037.932288	40.330484
3332.801341	849692.281472	40.335501
3335.677249	851357.332940	40.340519
3339.241114	853022.595204	40.345536
3342.529426	854699.098605	40.350554
3346.240725	856390.496305	40.355572
3349.440185	858069.488471	40.360589
3352.800755	859751.772205	40.365607
3355.847398	861460.007946	40.370624
3359.077264	863158.912978	40.375642
3362.008892	864876.280781	40.380660
3365.517026	866601.097982	40.385677
3369.111427	868325.210593	40.390695
3371.794955	870065.241424	40.395712
3375.304524	871807.912544	40.400730
3378.368988	873558.273090	40.405748
3382.014983	875310.530379	40.410765
3385.431282	877068.396030	40.415783
3388.771267	878845.463582	40.420800
3392.223125	880597.722003	40.425818
3395.719085	882375.330923	40.430836
3399.207337	884146.507236	40.435853
3402.981029	885919.023301	40.440871
3406.430973	887689.505896	40.445888
3410.228250	889462.856541	40.450906
3413.692980	891240.633034	40.455924
3417.340238	893004.713281	40.460941
3420.979509	894766.705606	40.465959
3424.582667	896545.402209	40.470976
3427.961455	898316.642109	40.475994
3431.126041	900095.352767	40.481012
3434.427341	901868.759437	40.486029
3438.282050	903641.316408	40.491047
3441.404596	905422.476304	40.496064
3444.821338	907193.109565	40.501082
3448.021180	908988.976231	40.506100
3451.306197	910772.134518	40.511117
3454.889009	912535.163877	40.516122
3457.508538	914274.083876	40.521127
3460.826197	915943.027240	40.526132
3463.716166	917563.033443	40.531136
3467.202670	919117.808497	40.536141
3470.220424	920601.722392	40.541146
3473.065107	922001.705881	40.546151
3476.285643	923334.070666	40.551156
3479.151675	924596.203873	40.556160
3481.477266	925784.054746	40.561165
3484.430386	926885.945747	40.566170
3486.630604	927943.462702	40.571175
3489.286523	928906.973859	40.576180
3491.879969	929804.172414	40.581184
3494.098416	930626.409890	40.586189
3496.575252	931375.052604	40.591194
3498.710268	932061.941927	40.596199
3500.889338	932679.839452	40.601204
3503.084800	933244.796748	40.606208
3504.871623	933733.974934	40.611213
3506.897863	934175.678973	40.616218
3508.299435	934558.557922	40.621223
3510.373888	934885.376508	40.626228
3511.671407	935154.570391	40.631232
3513.225728	935381.700433	40.636237
3514.445184	935548.555885	40.641242
3515.504589	935690.787295	40.646247
3516.677861	935790.800732	40.651252
3517.277988	935855.332728	40.656256
3518.036816	935880.423851	40.661261
3519.175173	935876.873211	40.666266
3519.793019	935858.259854	40.671271
3520.880180	935787.590194	40.676276
3521.713119	935700.084784	40.681280
3522.201911	935591.538486	40.686285
3522.996400	935450.330650	40.691290
3523.510052	935294.301479	40.696295
3524.143302	935100.458860	40.701300
3524.872802	934907.455872	40.706304
3525.312088	934676.512048	40.711309
3525.673909	934433.293262	40.716314
3525.851639	934183.187911	40.721319
3526.571260	933907.268499	40.726324
3527.130996	933618.890098	40.731328
3527.451579	933319.311445	40.736333
3527.719097	933001.590594	40.741338
3528.074267	932674.815909	40.746343
3528.501187	932320.851896	40.751348
3528.698243	931991.374913	40.756352
3529.205011	931614.317781	40.761357
3529.870667	931240.757866	40.766362
3530.026729	930860.443429	40.771367
3529.825405	930458.179914	40.776372
3530.053149	930052.740491	40.781376
3530.307753	929642.945004	40.786381
3530.447004	929226.224291	40.791386
3530.669767	928808.688366	40.796391
3530.632606	928377.047222	40.801396
3530.852827	927941.101281	40.806400
3530.985033	927508.208136	40.811405
3531.788722	927061.044915	40.816410
3531.994249	926612.985608	40.821415
3531.924699	926145.625023	40.826420
3532.131468	925677.023330	40.831424
3531.784496	925207.994566	40.836429
3531.862383	924729.722777	40.841434
3531.947850	924252.079655	40.846439
3532.049629	923763.145627	40.851444
3532.277742	923296.253916	40.856448
3532.194048	922805.149420	40.861453
3532.366668	922316.263615	40.866458
3532.520717	921823.105881	40.871463
3532.375557	921324.953720	40.876468
3532.673954	920828.506917	40.881472
3532.908787	920335.391404	40.886477
3532.668551	919824.806100	40.891482
3532.709025	919321.050597	40.896487
3532.908970	918809.428390	40.901492
3533.006466	918300.469235	40.906496
3533.053384	917780.405321	40.911501
3533.207989	917258.252249	40.916506
3533.000363	916745.734809	40.921511
3533.179949	916225.017912	40.926516
3533.027072	915700.265001	40.931520
3533.310031	915175.483343	40.936525
3533.244588	914642.334436	40.941530
3533.163252	914120.497973	40.946535
3533.550039	913582.450216	40.951540
3533.649237	913052.584565	40.956544
3533.494991	912511.249327	40.961549
3533.693791	911974.520203	40.966554
3533.587208	911435.285954	40.971559
3533.625296	910886.050591	40.976564
3533.276317	910345.787237	40.981568
3533.341372	909804.147384	40.986573
3533.893905	909259.190726	40.991578
3533.419931	908716.475800	40.996583
3533.541106	908164.448676	41.001588
3533.715692	907628.070602	41.006592
3533.442981	907074.073734	41.011597
3534.018286	906521.130091	41.016602
3533.805565	905971.833677	41.021607
3533.720349	905411.370549	41.026612
3533.481615	904866.791120	41.031616
3533.176997	904312.041422	41.036621
3533.597498	903756.630274	41.041626
3533.379871	903213.139421	41.046631
3533.450561	902656.424117	41.051636
3533.713411	902110.717600	41.056640
3533.617229	901552.473274	41.061645
3533.791855	900985.923142	41.066650
3533.520539	900428.851328	41.071655
3533.582795	899864.620125	41.076660
3533.461192	899305.287369	41.081664
3533.499749	898744.230151	41.086669
3533.776232	898187.035477	41.091674
3533.595621	897615.957063	41.096679
3533.784912	897055.671588	41.101684
3533.584891	896484.868281	41.106688
3533.460649	895922.012400	41.111693
3533.793337	895357.573310	41.116698
3533.700712	894786.097134	41.121703
3533.965425	894214.985498	41.126708
3533.936863	893643.673167	41.131712
3533.729965	893074.460150	41.136717
3533.636807	892498.887765	41.141722
3533.555458	891932.922263	41.146727
3533.776617	891354.473821	41.151732
3533.900934	890785.265552	41.156736
3533.782950	890215.558435	41.161741
3533.719629	889639.305694	41.166746
3533.431286	889065.838229	41.171751
3533.524464	888491.764615	41.176756
3533.565311	887914.159920	41.181760
3533.272047	887342.262345	41.186765
3533.742473	886771.435393	41.191770
3533.381912	886190.533125	41.196775
3533.512163	885613.649960	41.201780
3533.507913	885033.344555	41.206784
3533.446091	884465.961457	41.211789
3533.481145	883895.505185	41.216794
3533.290928	883312.832397	41.221799
3533.529374	882741.259634	41.226804
3533.646809	882162.194965	41.231808
3533.302856	881578.405972	41.236813
3533.725120	880999.367179	41.241818
3533.866283	880417.412906	41.246823
3533.918927	879834.059445	41.251828
3534.098597	879241.228324	41.256832
3533.562492	878659.214426	41.261837
3533.842084	878068.185230	41.266842
3533.585244	877478.447863	41.271847
3533.524038	876891.816250	41.276852
3533.544958	876295.321875	41.281856
3533.756046	875704.647997	41.286861
3533.905647	875102.388098	41.291866
3533.447546	874517.429577	41.296871
3533.793739	873927.621153	41.301876
3533.897615	873328.194115	41.306880
3533.781357	872747.075159	41.311885
3534.092457	872152.828209	41.316890
3533.769821	871568.524905	41.321895
3533.642829	870951.629110	41.326900
3533.367292	870361.765941	41.331904
3533.215728	869771.629056	41.336909
3533.229032	869177.523623	41.341914
3533.374345	868594.207027	41.346919
3533.423108	867995.804424	41.351924
3533.685114	867416.041508	41.356928
3533.690695	866816.945922	41.361933
3533.344500	866209.111785	41.366938
3532.895461	865624.539213	41.371943
3533.279912	865033.066478	41.376948
3533.601590	864435.233156	41.381952
3533.107692	863854.478367	41.386957
3533.417917	863248.467081	41.391962
3533.290932	862656.459836	41.396967
3533.559534	862059.177401	41.401972
3533.408297	861463.656817	41.406976
3533.480448	860869.108581	41.411981
3533.476613	860265.962114	41.416986
3533.602233	859671.579054	41.421991
3533.531587	859068.519575	41.426996
3533.275128	858468.445946	41.432000
3533.235332	857865.456566	41.437005
3533.350092	857264.617767	41.442010
3533.286274	856669.877135	41.447015
3533.218766	856062.727374	41.452020
3533.420615	855459.556768	41.457024
3533.324465	854861.436218	41.462029
3533.114132	854256.953181	41.467034
3532.990046	853663.196033	41.472039
3533.127732	853066.904261	41.477044
3533.076201	852471.560278	41.482048
3532.991635	851873.244732	41.487053
3533.248543	851261.283355	41.492058
3533.200616	850663.428512	41.497063
3532.940461	850062.436863	41.502068
3533.248792	849464.210842	41.507072
3532.775594	848869.176549	41.512077
3533.045264	848259.156365	41.517082
3533.079166	847666.939384	41.522087
3533.149126	847059.368005	41.527092
3533.326761	846455.907762	41.532096
3533.274171	845856.617610	41.537101
3533.354900	845232.402769	41.542106
3533.083795	844633.617429	41.547111
3532.955718	844027.929119	41.552116
3532.892098	843416.226460	41.557120
3533.018727	842809.207719	41.562125
3532.997111	842208.491749	41.567130
3532.863424	841607.055267	41.572135
3532.855643	840991.598155	41.577140
3532.918598	840386.794563	41.582144
3532.523376	839794.103109	41.587149
3533.014375	839176.043945	41.592154
3532.678488	838572.988244	41.597159
3532.643333	837965.629640	41.602164
3532.585861	837364.265020	41.607168
3532.552453	836763.424862	41.612173
3532.633176	836154.946958	41.617178
3532.716059	835565.780085	41.622183
3532.750654	834956.171304	41.627188
3532.728696	834357.298600	41.632192
3532.190148	833757.921277	41.637197
3532.516879	833148.188239	41.642202
3532.448514	832549.593997	41.647207
3532.354185	831948.117106	41.652212
3532.407220	831337.087527	41.657216
3532.358754	830731.583554	41.662221
3532.651160	830129.675738	41.667226
3532.521512	829528.369963	41.672231
3532.565246	828916.380516	41.677236
3532.215322	828312.704023	41.682240
3532.117647	827718.600371	41.687245
3532.297227	827105.342284	41.692250
3532.319109	826509.446737	41.697255
3532.088829	825902.545702	41.702260
3532.177683	825303.694490	41.707264
3531.907499	824702.601580	41.712269
3532.546984	824092.256089	41.717274
3532.239758	823493.942162	41.722279
3532.149756	822883.315322	41.727284
3532.315297	822270.388034	41.732288
3532.087992	821674.045724	41.737293
3532.199685	821055.978398	41.742298
3532.030767	820456.924292	41.747303
3532.094932	819846.722929	41.752308
3532.003120	819241.138479	41.757312
3531.790691	818657.286961	41.762317
3531.943096	818046.268561	41.767322
3531.861748	817452.651160	41.772327
3531.904675	816839.289783	41.777332
3531.966257	816244.463612	41.782336
3531.918206	815632.474552	41.787341
3532.178979	815019.593507	41.792346
3531.925923	814420.400264	41.797351
3531.908241	813815.092045	41.802356
3532.066679	813209.992756	41.807360
3531.772238	812599.873193	41.812365
3532.168925	812000.009744	41.817370
3531.958034	811391.920624	41.822375
3531.996264	810768.013352	41.827380
3532.018307	810164.377154	41.832384
3532.016119	809562.111579	41.837389
3532.162643	808943.650111	41.842394
3531.700988	808343.411842	41.847399
3531.523706	807732.194694	41.852404
3531.692959	807121.843303	41.857408
3531.549100	806514.969849	41.862413
3531.852327	805915.660345	41.867418
3531.635829	805320.013807	41.872423
3531.559011	804712.036925	41.877428
3531.698583	804092.007522	41.882432
3531.491984	803488.895165	41.887437
3531.436342	802885.164542	41.892442
3531.158392	802283.478157	41.897447
3531.185673	801675.851190	41.902452
3531.364293	801078.149600	41.907456
3531.456087	800478.154696	41.912461
3531.321264	799880.844099	41.917466
3531.222202	799276.803968	41.922471
3531.119330	798671.337949	41.927476
3531.351673	798069.147195	41.932480
3531.336911	797471.558792	41.937485
3531.801245	796864.758466	41.942490
3531.442690	796255.297225	41.947495
3531.089185	795635.572550	41.952500
3531.332050	795036.749087	41.957504
3531.178429	794436.518238	41.962509
3531.208594	793822.899618	41.967514
3530.833232	793234.337040	41.972519
3531.078742	792630.200475	41.977524
3530.909224	792026.573760	41.982528
3530.965502	791425.754175	41.987533
3531.217962	790821.558943	41.992538
3531.424112	790219.137192	41.997543
3531.212528	789611.184165	42.002548
3531.651326	789001.839491	42.007552
3531.095757	788394.429938	42.012557
3531.480159	787782.090566	42.017562
3531.466390	787182.690461	42.022567
3531.144525	786567.418235	42.027572
3531.137338	785956.413327	42.032576
3531.018571	785351.175164	42.037581
3530.991808	784729.254318	42.042586
3531.034732	784129.046389	42.047591
3530.720018	783530.766563	42.052596
3530.976018	782923.832687	42.057600
3530.413372	782325.543568	42.062605
3530.840671	781712.675210	42.067610
3530.678780	781120.758023	42.072615
3530.454945	780517.981459	42.077620
3530.713875	779913.153532	42.082624
3530.737727	779313.382136	42.087629
3530.572587	778716.249943	42.092634
3530.766031	778117.383473	42.097639
3530.828093	777506.187926	42.102644
3530.801023	776896.530833	42.107648
3530.808319	776299.268321	42.112653
3530.772771	775685.770608	42.117658
3530.699629	775084.730556	42.122663
3530.608393	774475.767478	42.127668
3530.563667	773880.432246	42.132672
3530.198861	773278.899356	42.137677
3530.199729	772665.535329	42.142682
3530.189157	772079.649624	42.147687
3530.393982	771480.235524	42.152692
3530.371057	770868.892276	42.157696
3530.093400	770272.762007	42.162701
3530.468913	769668.984370	42.167706
3530.072986	769079.280161	42.172711
3530.528821	768486.328806	42.177716
3530.159695	767876.964458	42.182720
3530.052920	767281.746106	42.187725
3529.784837	766680.938817	42.192730
3529.640695	766094.896376	42.197735
3529.469360	765496.391726	42.202740
3529.741185	764911.959491	42.207744
3529.200655	764330.972264	42.212749
3529.353131	763739.222019	42.217754
3529.493253	763154.083069	42.222759
3529.382251	762566.919640	42.227764
3529.579266	761980.002814	42.232768
3529.410939	761396.258654	42.237773
3529.395306	760801.050339	42.242778
3529.351742	760206.934154	42.247783
3528.939042	759631.233123	42.252788
3529.727673	759037.622668	42.257792
3529.466760	758456.083761	42.262797
3529.704251	757861.833767	42.267802
3529.348822	757276.914751	42.272807
3529.698397	756690.843360	42.277812
3529.572340	756108.509210	42.282816
3529.586866	755519.641151	42.287821
3529.746599	754920.831278	42.292826
3529.536281	754321.543966	42.297831
3529.109505	753734.143621	42.302836
3529.492435	753144.980126	42.307840
3529.470240	752555.149267	42.312845
3529.382711	751964.839818	42.317850
3529.406941	751379.601486	42.322855
3528.766153	750793.197548	42.327860
3528.852979	750202.772478	42.332864
3528.714160	749615.254844	42.337869
3528.612839	749046.505759	42.342874
3528.478067	748481.326680	42.347879
3528.266918	747904.262765	42.352884
3528.691066	747322.996130	42.357888
3528.659020	746757.920932	42.362893
3528.750574	746175.389990	42.367898
3528.830241	745593.855257	42.372903
3528.425229	745016.708937	42.377908
3528.825518	744441.161750	42.382912
3528.650455	743862.111584	42.387917
3528.824788	743276.532784	42.392922
3528.621619	742695.572202	42.397927
3528.420488	742110.217611	42.402932
3528.439642	741534.324308	42.407936
3528.285305	740975.576417	42.412941
3528.201862	740393.832006	42.417946
3528.492790	739824.640943	42.422951
3528.403987	739252.654657	42.427956
3528.531752	738672.527942	42.432960
3528.299612	738098.504327	42.437965
3528.503693	737520.209401	42.442970
3528.523461	736954.519111	42.447975
3528.337307	736368.736860	42.452980
3528.930834	735793.564810	42.457984
3528.798776	735219.068967	42.462989
3528.894575	734635.684425	42.467994
3528.922011	734057.069500	42.472999
3528.529178	733470.021215	42.478004
3528.861009	732874.193818	42.483008
3528.754050	732301.266331	42.488013
3528.746702	731697.489589	42.493018
3528.693137	731116.300496	42.498023
3528.500524	730534.103050	42.503028
3528.563187	729946.621020	42.508032
3528.426936	729376.857845	42.513037
3528.459225	728800.389912	42.518042
3528.537928	728215.107117	42.523047
3528.299615	727630.182982	42.528052
3528.338612	727056.314246	42.533056
3528.067533	726476.216502	42.538061
3528.160563	725902.604089	42.543066
3528.065259	725320.214464	42.548071
3527.933172	724752.009479	42.553076
3527.820209	724167.261720	42.558080
3527.838051	723598.951226	42.563085
3527.814062	723021.391001	42.568090
3527.741263	722455.296541	42.573095
3527.452984	721884.590550	42.578100
3527.595711	721318.133395	42.583104
3527.548010	720760.146455	42.588109
3527.608700	720181.232804	42.593114
3527.450063	719619.569032	42.598119
3527.157562	719056.253924	42.603124
3527.308245	718493.122454	42.608128
3527.072092	717944.547970	42.613133
3527.275197	717382.472926	42.618138
3526.840295	716828.155979	42.623143
3526.985797	716268.297061	42.628148
3526.966169	715703.121608	42.633152
3526.743520	715153.071840	42.638157
3526.670554	714606.879393	42.643162
3526.867335	714050.137608	42.648167
3526.782472	713498.418020	42.653172
3527.149643	712937.058685	42.658176
3527.278065	712393.268262	42.663181
3527.379191	711827.365113	42.668186
3527.204220	711273.133491	42.673191
3527.186962	710704.048953	42.678196
3527.181405	710141.773613	42.683200
3526.987425	709591.157782	42.688205
3526.761648	709032.122611	42.693210
3526.959389	708473.276288	42.698215
3526.557024	707922.042012	42.703220
3526.507567	707364.456067	42.708224
3526.691336	706819.256750	42.713229
3526.566264	706270.897475	42.718234
3526.383056	705716.404999	42.723239
3526.650115	705163.438689	42.728244
3526.721142	704613.052883	42.733248
3526.597134	704070.612145	42.738253
3526.586884	703514.805856	42.743258
3526.441055	702971.405634	42.748263
3526.205994	702423.515471	42.753268
3526.551595	701877.826506	42.758272
3526.320124	701328.425714	42.763277
3526.399225	700775.955880	42.768282
3526.339814	700231.176610	42.773287
3526.366865	699691.814775	42.778292
3526.413957	699136.811385	42.783296
3526.339559	698595.113004	42.788301
3526.240951	698051.496472	42.793306
3526.368751	697499.506619	42.798311
3526.282201	696950.053764	42.803316
3526.124348	696398.391344	42.808321
3525.933826	695866.784863	42.813325
3525.946511	695319.102278	42.818330
3526.215522	694777.905128	42.823335
3526.047646	694244.705290	42.828340
3526.317704	693696.032730	42.833345
3526.203092	693156.393060	42.838349
3526.171097	692600.841404	42.843354
3526.245731	692051.553332	42.848359
3525.804186	691516.893178	42.853364
3526.087432	690972.775269	42.858369
3525.926460	690439.594299	42.863373
3525.763123	689889.716045	42.868378
3525.952200	689349.246385	42.873383
3525.634496	688818.333765	42.878388
3525.957104	688272.154020	42.883393
3525.761895	687739.166281	42.888397
3525.797973	687193.019582	42.893402
3526.324734	686651.234976	42.898407
3526.112444	686121.886863	42.903412
3526.380027	685575.005347	42.908417
3525.989031	685028.551602	42.913421
3525.736738	684482.290063	42.918426
3525.853087	683944.395539	42.923431
3525.905321	683401.252695	42.928436
3526.058571	682861.097186	42.933441
3525.824167	682320.776636	42.938445
3525.725262	681776.666401	42.943450
3525.977604	681229.326580	42.948455
3525.597033	680688.685360	42.953460
3525.968459	680145.742311	42.958465
3525.610612	679613.201303	42.963469
3525.541858	679072.809956	42.968474
3525.336331	678537.490918	42.973479
3525.451804	678006.818265	42.978484
3525.675499	677457.415250	42.983489
3525.301421	676927.561149	42.988493
3524.984617	676390.093841	42.993498
3525.147923	675856.300095	42.998503
3525.410702	675326.843528	43.003508
3525.426512	674793.761246	43.008513
3525.173976	674259.348680	43.013517
3525.399908	673729.458579	43.018522
3525.533501	673205.684416	43.023527
3525.226038	672671.738430	43.028532
3525.110907	672133.591927	43.033537
3525.013530	671610.415792	43.038541
3524.938415	671071.503560	43.043546
3525.250188	670554.828897	43.048551
3524.684461	670026.210340	43.053556
3524.958504	669501.606914	43.058561
3524.777592	668987.572890	43.063565
3524.568316	668449.131754	43.068570
3524.761764	667927.247036	43.073575
3524.454102	667407.364048	43.078580
3524.695787	666879.778021	43.083585
3524.534653	666370.785314	43.088589
3524.409640	665846.645951	43.093594
3524.464903	665336.563384	43.098599
3524.364310	664815.006795	43.103604
3524.357875	664293.405632	43.108609
3524.044333	663786.695505	43.113613
3524.117097	663268.417409	43.118618
3524.184276	662760.889525	43.123623
3523.964366	662254.281972	43.128628
3524.363132	661742.202783	43.133633
3524.192867	661235.283581	43.138637
3524.101875	660722.086012	43.143642
3523.953793	660204.129636	43.148647
3523.892461	659704.547726	43.153652
3523.996937	659196.775866	43.158657
3523.625230	658691.205080	43.163661
3523.896640	658173.867154	43.168666
3523.963244	657673.759440	43.173671
3524.039589	657174.922379	43.178676
3524.146296	656657.232416	43.183681
3523.624639	656163.638048	43.188685
3523.642412	655649.205129	43.193690
3523.670264	655146.977280	43.198695
3523.792332	654643.958559	43.203700
3523.954437	654139.808560	43.208705
3523.976387	653639.002718	43.213709
3523.841853	653130.956193	43.218714
3523.925439	652627.041765	43.223719
3523.513151	652125.084336	43.228724
3523.571512	651624.719414	43.233729
3523.708897	651128.262094	43.238733
3523.292750	650623.981217	43.243738
3523.542932	650119.510988	43.248743
3523.539321	649630.946370	43.253748
3523.612670	649128.154744	43.258753
3523.361788	648633.187937	43.263757
3523.450654	648134.690683	43.268762
3523.187392	647641.475721	43.273767
3523.049263	647150.014153	43.278772
3523.220811	646653.477929	43.283777
3522.955217	646165.438253	43.288781
3523.104389	645671.406220	43.293786
3523.358160	645189.628156	43.298791
3522.546255	644696.911997	43.303796
3523.107821	644201.787750	43.308801
3522.877990	643715.172906	43.313805
3522.962296	643222.281792	43.318810
3522.969592	642744.678674	43.323815
3522.867612	642263.871821	43.328820
3522.802551	641771.285692	43.333825
3522.837806	641288.609242	43.338829
3522.989960	640793.988604	43.343834
3523.199292	640311.186146	43.348839
3522.652350	639830.790465	43.353844
3522.878699	639331.035258	43.358849
3523.139585	638854.506875	43.363853
3523.025801	638367.716701	43.368858
3523.262630	637881.193734	43.373863
3523.100522	637391.414389	43.378868
3522.887259	636891.815634	43.383873
3522.290102	636416.871558	43.388877
3522.462184	635932.618925	43.393882
3522.338502	635450.695574	43.398887
3522.376257	634977.978529	43.403892
3522.060659	634477.430008	43.408897
3522.060269	634010.179394	43.413901
3522.071145	633531.746730	43.418906
3522.380273	633046.885666	43.423911
3521.882109	632581.907894	43.428916
3522.141543	632105.619409	43.433921
3522.186650	631639.756239	43.438925
3522.078332	631171.195711	43.443930
3522.089499	630698.539424	43.448935
3521.959780	630237.549138	43.453940
3521.977824	629761.345540	43.458945
3521.721769	629294.228281	43.463949
3521.792894	628831.139663	43.468954
3522.507164	628359.409770	43.473959
3521.991063	627893.826968	43.478964
3522.056294	627418.410834	43.483969
3521.834447	626958.995456	43.488973
3521.970552	626484.126211	43.493978
3521.888242	626008.221427	43.498983
3521.772825	625550.429595	43.503988
3522.127724	625084.524827	43.508993
3521.977258	624615.080007	43.513997
3521.936407	624145.044907	43.519002
3521.975457	623678.231219	43.524007
3521.215692	623212.284923	43.529012
3521.664492	622749.317938	43.534017
3521.742465	622295.812024	43.539021
3521.768679	621827.517430	43.544026
3521.719101	621365.477732	43.549031
3521.416206	620914.082817	43.554036
3521.648871	620443.688888	43.559041
3521.787417	619982.459774	43.564045
3521.503210	619524.339726	43.569050
3521.685344	619064.116347	43.574055
3521.289751	618611.238232	43.579060
3521.012656	618151.505617	43.584065
3521.226077	617702.093853	43.589069
3521.228020	617241.473367	43.594074
3521.075693	616788.277492	43.599079
3520.767253	616342.357126	43.604084
3521.168587	615880.007220	43.609089
3521.172457	615444.923984	43.614093
3520.922776	614986.507263	43.619098
3521.235317	614535.394663	43.624103
3520.902747	614096.605904	43.629108
3520.694094	613640.131391	43.634113
3520.959739	613201.204886	43.639117
3520.744535	612751.713809	43.644122
3520.716885	612307.487296	43.649127
3520.790612	611857.810338	43.654132
3521.145712	611412.529944	43.659137
3520.540491	610977.073848	43.664141
3520.696145	610531.140323	43.669146
3520.587942	610089.597054	43.674151
3520.174811	609649.592932	43.679156
3520.581451	609207.325056	43.684161
3520.313707	608774.333370	43.689165
3520.594429	608337.419315	43.694170
3520.917684	607898.524756	43.699175
3520.555115	607460.733380	43.704180
3520.632658	607017.381978	43.709185
3520.288888	606584.469351	43.714189
3520.264629	606149.177846	43.719194
3520.392310	605717.505998	43.724199
3520.108041	605276.204922	43.729204
3520.215125	604846.309535	43.734209
3520.126119	604420.495524	43.739213
3520.001631	603989.904775	43.744218
3520.106322	603559.057874	43.749223
3520.131839	603140.903957	43.754228
3520.237997	602701.292893	43.759233
3520.316502	602271.204719	43.764237
3520.044394	601836.342310	43.769242
3519.978127	601417.287792	43.774247
3519.858696	600984.274122	43.779252
3520.253609	600568.271837	43.784257
3520.043479	600141.214728	43.789261
3519.945601	599708.249681	43.794266
3520.124795	599280.291035	43.799271
3520.026598	598852.062678	43.804276
3520.196770	598428.290761	43.809281
3520.117206	597998.320747	43.814285
3519.693356	597571.004222	43.819290
3519.929165	597147.525681	43.824295
3519.885884	596730.606500	43.829300
3519.720757	596293.257434	43.834305
3519.496476	595891.904415	43.839309
3519.539299	595470.757792	43.844314
3519.607134	595045.072262	43.849319
3519.208594	594637.629727	43.854324
3519.509763	594213.229974	43.859329
3519.662540	593811.238947	43.864333
3519.264465	593391.649660	43.869338
3519.470090	592969.431071	43.874343
3519.349902	592569.302493	43.879348
3519.501862	592145.004215	43.884353
3519.329045	591733.052546	43.889357
3519.000139	591319.204344	43.894362
3519.017902	590914.123610	43.899367
3518.966850	590509.643598	43.904372
3519.186456	590101.235322	43.909377
3519.151223	589689.791940	43.914381
3519.084658	589284.619750	43.919386
3519.255022	588871.354548	43.924391
3518.767148	588473.059646	43.929396
3519.252633	588064.033666	43.934401
3519.152377	587652.028605	43.939405
3518.987582	587250.170715	43.944410
3519.149522	586854.575171	43.949415
3518.799960	586455.033718	43.954420
3518.912047	586047.661015	43.959425
3518.796853	585646.193263	43.964429
3518.704527	585236.566502	43.969434
3518.856997	584839.298073	43.974439
3518.850888	584439.982958	43.979444
3518.951734	584038.525371	43.984449
3518.431038	583642.890714	43.989453
3518.495811	583252.923754	43.994458
3518.663946	582851.214307	43.999463
3518.201760	582457.189840	44.004468
3518.117967	582057.859854	44.009473
3518.423547	581666.996610	44.014477
3518.296028	581283.886710	44.019482
3518.427781	580890.212945	44.024487
3518.127896	580500.119610	44.029492
3518.164992	580107.945167	44.034497
3518.182675	579728.180747	44.039501
3518.234404	579349.153000	44.044506
3518.567237	578955.583944	44.049511
3518.329477	578569.793345	44.054516
3518.208116	578175.070063	44.059521
3518.264043	577788.702028	44.064525
3517.900305	577398.571540	44.069530
3517.869298	577019.335466	44.074535
3517.896760	576643.397135	44.079540
3518.331247	576257.671095	44.084545
3517.934622	575883.693356	44.089549
3517.631614	575498.673232	44.094554
3517.979371	575113.228302	44.099559
3517.833301	574743.197457	44.104564
3517.641130	574361.594037	44.109569
3517.618987	573987.243963	44.114573
3517.913411	573616.551224	44.119578
3517.718890	573232.951896	44.124583
3517.515927	572859.856686	44.129588
3517.534991	572486.511249	44.134593
3517.771964	572112.614418	44.139597
3517.664310	571739.972832	44.144602
3517.738005	571355.465455	44.149607
3517.676607	570983.699295	44.154612
3517.710834	570615.176488	44.159617
3517.691555	570251.532988	44.164621
3517.641321	569874.297940	44.169626
3517.399610	569503.022308	44.174631
3517.277350	569128.645730	44.179636
3517.569441	568767.372394	44.184641
3517.297967	568398.686483	44.189645
3516.873071	568032.582800	44.194650
3517.238502	567670.712283	44.199655
3517.035802	567308.676876	44.204660
3516.948833	566942.635274	44.209665
3517.282668	566591.359609	44.214669
3517.292839	566227.898340	44.219674
3517.436904	565862.994526	44.224679
3517.440810	565507.718706	44.229684
3517.209503	565130.173225	44.234689
3517.169111	564773.022184	44.239693
3516.989630	564409.491644	44.244698
3517.056760	564042.787514	44.249703
3516.666302	563688.284107	44.254708
3516.658561	563333.655312	44.259713
3516.883867	562971.223589	44.264717
3516.894318	562620.096498	44.269722
3516.819176	562260.666823	44.274727
3516.562138	561910.019395	44.279732
3516.999647	561555.668923	44.284737
3516.837091	561203.123323	44.289741
3516.714738	560850.158508	44.294746
3516.817855	560497.598888	44.299751
3516.942344	560147.644751	44.304756
3516.629058	559781.187798	44.309761
3516.649296	559430.275510	44.314765
3516.259172	559086.071715	44.319770
3516.725815	558734.007045	44.324775
3516.472797	558403.108291	44.329780
3516.386593	558047.694902	44.334785
3516.685235	557699.056209	44.339789
3516.147479	557359.466385	44.344794
3516.456502	557017.658111	44.349799
3516.150496	556676.802349	44.354804
3516.387025	556320.582328	44.359809
3516.762224	555981.506585	44.364813
3516.486547	555629.032794	44.369818
3516.798724	555283.753905	44.374823
3516.678500	554938.036135	44.379828
3516.465968	554582.098218	44.384833
3516.379608	554239.026684	44.389837
3516.151597	553901.965969	44.394842
3516.329228	553554.549397	44.399847
3516.346823	553219.747230	44.404852
3516.194604	552866.272683	44.409857
3516.123764	552538.270704	44.414861
3515.914615	552197.485790	44.419866
3516.339778	551851.041139	44.424871
3515.940457	551532.241647	44.429876
3515.663576	551189.124890	44.434881
3515.819754	550855.903329	44.439885
3515.878887	550518.658604	44.444890
3515.844554	550197.144869	44.449895
3515.481463	549871.849507	44.454900
3515.713520	549535.810783	44.459905
3515.813448	549212.285330	44.464909
3515.508209	548892.198202	44.469914
3515.591221	548550.818219	44.474919
3515.487054	548233.755828	44.479924
3515.626164	547912.662643	44.484929
3515.498292	547589.339286	44.489933
3515.438577	547265.089356	44.494938
3515.578368	546930.867420	44.499943
3515.427502	546619.169287	44.504948
3515.678627	546278.762639	44.509953
3515.369996	545962.186807	44.514957
3515.072928	545644.442254	44.519962
3515.470343	545328.588353	44.524967
3515.039860	545009.944548	44.529972
3514.839573	544696.295677	44.534977
3514.882378	544378.564853	44.539981
3514.871180	544062.550188	44.544986
3514.850729	543742.899734	44.549991
3514.507172	543442.305556	44.554996
3515.042830	543144.882583	44.560001
3514.768940	542835.187565	44.565005
3514.681788	542514.915254	44.570010
3514.999754	542213.173167	44.575015
3514.741012	541918.128815	44.580020
3514.515821	541616.063185	44.585025
3514.798297	541309.567562	44.590029
3514.896664	541004.760840	44.595034
3515.083455	540690.552397	44.600039
3514.670163	540393.939049	44.605044
3514.974544	540083.025429	44.610049
3514.772863	539786.211857	44.615053
3514.769769	539472.311268	44.620058
3514.788051	539163.947979	44.625063
3514.617229	538867.462885	44.630068
3514.592924	538567.718550	44.635073
3514.581564	538253.590590	44.640077
3514.592756	537947.471787	44.645082
3514.809302	537654.224233	44.650087
3514.694366	537357.748498	44.655092
3514.744475	537047.265660	44.660097
3514.845752	536746.553508	44.665101
3514.311469	536449.525151	44.670106
3514.275661	536158.711297	44.675111
3514.600812	535860.464589	44.680116
3514.297800	535552.733723	44.685121
3514.566366	535254.887662	44.690125
3514.327853	534958.635515	44.695130
3514.484051	534662.007157	44.700135
3514.197665	534368.324047	44.705140
3514.422695	534073.992639	44.710145
3514.118467	533782.823321	44.715149
3514.294244	533490.859792	44.720154
3514.681334	533193.253593	44.725159
3513.994220	532909.397807	44.730164
3514.181752	532622.510972	44.735169
3514.286276	532323.421382	44.740173
3513.962716	532032.775205	44.745178
3514.146006	531747.738851	44.750183
3513.963597	531463.919992	44.755188
3513.936177	531172.499580	44.760193
3514.073487	530882.912411	44.765197
3513.631030	530596.194099	44.770202
3514.147036	530317.734449	44.775207
3514.410694	530033.205999	44.780212
3514.173919	529736.947796	44.785217
3514.227242	529450.374722	44.790221
3513.907777	529166.282291	44.795226
3514.191513	528885.008728	44.800231
3513.688117	528603.006145	44.805236
3513.679020	528316.522562	44.810241
3513.523637	528031.976418	44.815245
3513.537639	527759.863309	44.820250
3513.676426	527475.559065	44.825255
3513.432896	527202.621565	44.830260
3513.401228	526921.566327	44.835265
3513.410271	526653.371017	44.840269
3513.295223	526380.951712	44.845274
3513.500709	526104.787559	44.850279
3513.129060	525838.308400	44.855284
3513.295517	525565.371742	44.860289
3513.652868	525298.102164	44.865293
3513.067629	525026.344137	44.870298
3513.303217	524754.592468	44.875303
3513.186125	524492.791443	44.880308
3513.394069	524225.326230	44.885313
3513.487029	523956.512687	44.890317
3513.257898	523686.941486	44.895322
3513.459464	523417.695826	44.900327
3512.905984	523155.693497	44.905332
3512.700728	522889.183851	44.910337
3513.238864	522617.392287	44.915341
3512.977721	522363.960535	44.920346
3513.002519	522104.264867	44.925351
3512.892142	521845.698712	44.930356
3512.995002	521579.214295	44.935361
3512.963948	521320.120644	44.940365
3512.797953	521061.803069	44.945370
3513.104599	520797.795010	44.950375
3512.768420	520541.669087	44.955380
3512.924647	520281.616718	44.960385
3512.678952	520023.093071	44.965389
3512.879902	519777.013358	44.970394
3512.672452	519502.717605	44.975399
3513.006718	519245.899863	44.980404
3512.899430	518993.446114	44.985409
3513.106708	518743.661795	44.990413
3512.647574	518484.542447	44.995418
3512.897264	518225.095658	45.000423
3512.926294	517983.511583	45.005428
3512.501390	517715.685964	45.010433
3512.343063	517462.104489	45.015437
3512.369277	517215.306280	45.020442
3512.569199	516967.514735	45.025447
3512.660931	516717.565643	45.030452
3512.641804	516470.157090	45.035457
3512.863026	516206.438003	45.040461
3512.667572	515962.031747	45.045466
3512.940230	515703.094208	45.050471
3512.817512	515462.254256	45.055476
3512.628654	515207.529587	45.060481
3512.734465	514957.499132	45.065485
3512.564052	514703.924965	45.070490
3512.627727	514457.581546	45.075495
3512.837030	514218.787450	45.080500
3512.757050	513957.658114	45.085505
3512.882267	513706.341207	45.090509
3512.540736	513460.303819	45.095514
3512.588152	513199.038993	45.100519
3512.587548	512970.972703	45.105524
3512.459402	512712.862258	45.110529
3512.505129	512463.964180	45.115533
3512.536569	512214.155105	45.120538
3512.465504	511960.772081	45.125543
3512.544249	511724.943361	45.130548
3512.719546	511481.767861	45.135553
3512.329486	511225.900996	45.140557
3512.020302	510980.880337	45.145562
3512.769624	510736.281524	45.150567
3512.668477	510505.265795	45.155572
3512.682991	510255.276956	45.160577
3512.606802	510001.812801	45.165581
3512.230449	509758.199617	45.170586
3512.209700	509512.601616	45.175591
3512.363008	509285.415900	45.180596
3512.292180	509035.927776	45.185601
3512.439331	508783.416778	45.190605
3512.227637	508541.727809	45.195610
3512.206878	508292.876496	45.200615
3511.948736	508069.584692	45.205620
3511.964865	507831.535503	45.210625
3512.176846	507590.315739	45.215629
3511.837840	507361.720964	45.220634
3511.925918	507128.753828	45.225639
3511.886066	506885.949072	45.230644
3511.730002	506654.128696	45.235649
3511.917104	506415.624925	45.240653
3511.808924	506186.771816	45.245658
3511.965402	505954.129791	45.250663
3511.604771	505729.862515	45.255668
3511.654621	505491.722328	45.260673
3511.700317	505255.298008	45.265677
3511.255935	505035.989201	45.270682
3511.447386	504811.817108	45.275687
3511.278496	504590.281548	45.280692
3511.344347	504375.628487	45.285697
3511.612823	504141.980774	45.290701
3511.331816	503924.246703	45.295706
3511.568461	503699.596542	45.300711
3511.023712	503492.770823	45.305716
3511.291649	503268.766582	45.310721
3511.371518	503050.200865	45.315725
3511.094235	502838.922802	45.320730
3511.407984	502606.964255	45.325735
3511.125527	502400.585467	45.330740
3511.217861	502189.286450	45.335745
3511.494384	501966.981884	45.340749
3510.962798	501746.430200	45.345754
3511.349262	501528.196272	45.350759
3511.341021	501314.981851	45.355764
3511.108835	501099.780418	45.360769
3511.106126	500881.452662	45.365773
3511.436418	500675.099228	45.370778
3511.618807	500452.234042	45.375783
3511.339191	500232.074091	45.380788
3511.378530	500015.092926	45.385793
3511.412894	499806.958809	45.390797
3511.455074	499585.673411	45.395802
3511.587350	499360.931092	45.400807
3511.576494	499146.121494	45.405812
3511.371394	498928.459864	45.410817
3511.494290	498710.739377	45.415821
3511.477767	498499.613937	45.420826
3511.270756	498270.464623	45.425831
3511.165306	498053.179077	45.430836
3510.689286	497837.369984	45.435841
3510.776736	497628.896064	45.440845
3510.588121	497433.008835	45.445850
3510.514706	497218.185026	45.450855
3510.627386	497024.770259	45.455860
3510.967016	496818.974196	45.460865
3510.945639	496605.398011	45.465869
3510.614340	496412.557737	45.470874
3510.801938	496205.009924	45.475879
3510.833242	496002.493409	45.480884
3510.834802	495791.431824	45.485889
3510.919460	495588.496587	45.490893
3510.670010	495379.849899	45.495898
3510.475687	495184.443175	45.500903
3510.583175	494989.741363	45.505908
3510.667140	494787.201241	45.510913
3510.476916	494584.604343	45.515917
3510.455528	494388.046075	45.520922
3510.661802	494183.909790	45.525927
3510.131959	493995.071801	45.530932
3510.274736	493798.225739	45.535937
3510.529584	493606.467314	45.540941
3510.269816	493414.440495	45.545946
3510.559885	493210.834633	45.550951
3510.230290	493023.266873	45.555956
3510.374723	492833.390281	45.560961
3510.271919	492645.122001	45.565965
3510.266111	492454.052733	45.570970
3510.208906	492257.172402	45.575975
3510.237300	492068.875363	45.580980
3510.109895	491878.326309	45.585985
3510.259505	491686.817207	45.590989
3510.056946	491509.126830	45.595994
3510.087694	491310.399312	45.600999
3509.729174	491134.300014	45.606004
3509.923273	490951.223965	45.611009
3510.011278	490759.563251	45.616013
3509.876897	490577.298202	45.621018
3509.859333	490391.621464	45.626023
3509.648570	490205.115600	45.631028
3509.433184	490033.787092	45.636033
3510.027750	489843.800528	45.641037
3509.676463	489671.783288	45.646042
3509.607222	489485.296075	45.651047
3509.827223	489311.356216	45.656052
3509.526677	489132.089514	45.661057
3509.453555	488958.347950	45.666061
3509.573860	488782.800655	45.671066
3509.570011	488599.227470	45.676071
3509.811039	488435.597519	45.681076
3509.374883	488254.877503	45.686081
3509.822322	488075.978178	45.691085
3509.360560	487903.000824	45.696090
3509.425311	487733.170379	45.701095
3509.651900	487566.245589	45.706100
3509.606448	487391.117369	45.711105
3509.981430	487215.105950	45.716109
3509.707020	487045.276114	45.721114
3509.719957	486855.558604	45.726119
3509.493716	486690.220896	45.731124
3509.383850	486524.102673	45.736129
3509.588711	486346.947641	45.741133
3509.251320	486181.016832	45.746138
3509.608753	486007.729022	45.751143
3509.288979	485840.931670	45.756148
3508.972023	485671.500641	45.761153
3509.310193	485509.091907	45.766157
3509.101146	485350.722600	45.771162
3509.271905	485173.915828	45.776167
3509.199627	485015.570765	45.781172
3509.075425	484855.158124	45.786177
3509.374714	484683.992847	45.791181
3509.227711	484522.821919	45.796186
3509.394975	484349.347826	45.801191
3509.187648	484198.509032	45.806196
3508.873976	484032.604550	45.811201
3509.316906	483873.604549	45.816205
3509.004318	483707.038863	45.821210
3509.060806	483543.192367	45.826215
3509.028432	483382.902547	45.831220
3509.258586	483230.513001	45.836225
3509.692581	483058.246113	45.841229
3509.302336	482907.680655	45.846234
3509.445460	482738.092358	45.851239
3509.057280	482574.920264	45.856244
3509.062310	482406.010404	45.861249
3509.170034	482248.217313	45.866253
3508.660745	482088.756543	45.871258
3508.782396	481931.110127	45.876263
3508.380888	481785.194028	45.881268
3508.701605	481637.128646	45.886273
3509.048726	481486.324059	45.891277
3508.504495	481336.986524	45.896282
3508.681277	481177.856077	45.901287
3508.855539	481022.217512	45.906292
3508.604807	480869.484975	45.911297
3508.736591	480715.116543	45.916301
3508.490296	480576.909282	45.921306
3508.839683	480428.879666	45.926311
3509.081773	480271.805587	45.931316
3508.657574	480124.968649	45.936321
3508.712545	479964.076437	45.941325
3508.374596	479819.601620	45.946330
3508.499068	479661.276696	45.951335
3508.863031	479513.388957	45.956340
3508.658500	479368.128369	45.961345
3508.620888	479227.546352	45.966349
3508.706672	479088.612854	45.971354
3508.370001	478937.954328	45.976359
3508.371584	478792.248911	45.981364
3508.388255	478654.083296	45.986369
3508.690455	478504.324642	45.991373
3508.248271	478362.843065	45.996378
3508.432902	478211.431328	46.001383
3508.551932	478073.446337	46.006388
3508.306954	477933.902300	46.011393
3508.116227	477788.322933	46.016397
3508.292125	477657.008268	46.021402
3508.144687	477511.216775	46.026407
3508.443376	477379.524731	46.031412
3507.998829	477233.781752	46.036417
3508.213917	477098.658998	46.041421
3508.283110	476964.269012	46.046426
3508.390521	476820.352530	46.051431
3508.292665	476692.925782	46.056436
3508.441633	476553.709002	46.061441
3508.428735	476416.544165	46.066445
3508.037237	476275.088386	46.071450
3508.408427	476136.184936	46.076455
3508.295591	475993.210997	46.081460
3508.347602	475857.398050	46.086465
3508.315768	475720.484426	46.091469
3508.284719	475582.708833	46.096474
3508.320218	475446.743767	46.101479
3508.503797	475311.309422	46.106484
3508.244689	475169.316164	46.111489
3508.408494	475024.616434	46.116493
3508.448253	474893.963541	46.121498
3508.487023	474758.600506	46.126503
3508.602604	474608.841896	46.131508
3508.512368	474468.890619	46.136513
3508.707487	474329.699798	46.141517
3508.477277	474203.088663	46.146522
3508.612638	474047.549166	46.151527
3508.672857	473908.125011	46.156532
3508.047396	473761.271331	46.161537
3508.153690	473625.584644	46.166541
3508.057267	473496.970823	46.171546
3507.976036	473360.048166	46.176551
3507.970436	473227.517510	46.181556
3508.072888	473097.651546	46.186561
3508.409630	472970.732638	46.191565
3508.168590	472836.669454	46.196570
3508.211272	472708.127723	46.201575
3507.953499	472564.443045	46.206580
3507.999789	472434.683347	46.211585
3507.984199	472295.715873	46.216589
3507.793761	472177.491286	46.221594
3507.820328	472045.909016	46.226599
3507.807139	471922.587958	46.231604
3507.872523	471792.010203	46.236609
3507.812394	471662.668498	46.241613
3507.732047	471551.866274	46.246618
3507.709559	471426.618946	46.251623
3507.630208	471301.886971	46.256628
3507.931294	471173.746422	46.261633
3508.148884	471044.960825	46.266637
3507.889321	470924.258360	46.271642
3507.866631	470782.647147	46.276647
3508.282195	470653.318576	46.281652
3507.982334	470540.066037	46.286657
3508.346430	470411.251095	46.291661
3508.188913	470285.968585	46.296666
3508.466016	470152.000356	46.301671
3507.938101	470010.013751	46.306676
3507.700534	469882.462918	46.311681
3507.985344	469750.871166	46.316685
3507.541200	469632.977828	46.321690
3507.825128	469508.931760	46.326695
3507.964477	469382.326258	46.331700
3507.655990	469262.533287	46.336705
3507.974627	469141.467444	46.341709
3507.594141	469025.838880	46.346714
3507.775383	468899.172350	46.351719
3507.552010	468775.613347	46.356724
3507.347986	468656.406573	46.361729
3507.792429	468528.426259	46.366733
3507.411336	468415.681445	46.371738
3507.368030	468298.116625	46.376743
3507.482445	468180.524149	46.381748
3507.409632	468062.557664	46.386753
3507.356471	467955.022423	46.391757
3507.083836	467840.077440	46.396762
3507.138261	467731.661399	46.401767
3507.022848	467620.386248	46.406772
3506.999033	467509.246784	46.411777
3507.162973	467398.986467	46.416781
3507.103905	467302.036164	46.421786
3506.845038	467182.576259	46.426791
3506.942074	467066.145056	46.431796
3506.788093	466965.257832	46.436801
3507.444268	466867.524635	46.441805
3507.152915	466760.023354	46.446810
3507.287623	466641.100797	46.451815
3507.373155	466532.622005	46.456820
3506.950394	466424.178729	46.461825
3507.195229	466317.849948	46.466829
3507.184082	466216.934408	46.471834
3507.180624	466105.023418	46.476839
3507.410633	465996.314289	46.481844
3507.256209	465884.985081	46.486849
3507.378564	465767.781764	46.491853
3507.145430	465665.229371	46.496858
3506.960307	465549.749109	46.501863
3507.507407	465449.595513	46.506868
3507.450938	465341.843559	46.511873
3507.142825	465228.358265	46.516877
3507.154050	465131.790347	46.521882
3506.960156	465018.486977	46.526887
3507.234461	464913.918701	46.531892
3506.907326	464808.337920	46.536897
3506.965620	464695.040265	46.541901
3507.060329	464588.018288	46.546906
3506.685370	464494.755746	46.551911
3507.219166	464386.644367	46.556916
3507.382448	464277.379653	46.561921
3507.539878	464170.446002	46.566925
3507.317430	464072.950045	46.571930
3507.025367	463963.913321	46.576935
3507.366258	463863.381416	46.581940
3506.802298	463757.075346	46.586945
3507.129539	463654.669982	46.591949
3506.649563	463550.881857	46.596954
3506.643832	463444.377428	46.601959
3507.007538	463344.903001	46.606964
3506.674511	463244.330971	46.611969
3506.623956	463143.963539	46.616973
3506.249175	463056.318396	46.621978
3506.502012	462954.530106	46.626983
3506.560698	462867.114123	46.631988
3506.270821	462767.190983	46.636993
3506.681938	462682.500879	46.641997
3506.537655	462600.590800	46.647002
3506.591133	462499.492909	46.652007
3507.304791	462414.344620	46.657012
3506.977999	462315.438910	46.662017
3507.011137	462206.590216	46.667021
3507.100623	462113.693046	46.672026
3506.941853	462015.162511	46.677031
3506.871166	461919.150079	46.682036
3506.681347	461807.195535	46.687041
3506.731648	461707.969016	46.692045
3506.851251	461619.776982	46.697050
3506.813907	461517.372039	46.702055
3507.072379	461418.159190	46.707060
3506.922648	461331.430726	46.712065
3507.285164	461228.854663	46.717069
3507.184703	461129.904350	46.722074
3507.239163	461019.474541	46.727079
3507.299591	460923.536223	46.732084
3506.517464	460821.913620	46.737089
3507.012281	460717.285293	46.742093
3507.044128	460625.100416	46.747098
3507.008131	460522.943470	46.752103
3506.887337	460418.520031	46.757108
3506.508662	460325.339646	46.762113
3506.699404	460236.571852	46.767117
3506.756032	460147.370466	46.772122
3506.915566	460047.052740	46.777127
3507.030373	459956.320237	46.782132
3506.670307	459862.729081	46.787137
3506.889126	459758.548250	46.792141
3506.744924	459669.328331	46.797146
3506.438597	459569.493167	46.802151
3506.493097	459481.556124	46.807156
3506.358937	459388.887065	46.812161
3506.621639	459294.376032	46.817165
3506.480969	459206.014984	46.822170
3506.424690	459127.724424	46.827175
3506.596397	459026.284521	46.832180
3506.679363	458938.036141	46.837185
3506.736980	458854.200906	46.842189
3506.426123	458777.574218	46.847194
3506.232752	458681.465694	46.852199
3506.770464	458585.383922	46.857204
3506.499653	458502.667596	46.862209
3506.592180	458407.775977	46.867213
3506.139982	458316.828742	46.872218
3506.222316	458232.479863	46.877223
3506.536951	458140.995439	46.882228
3506.281265	458063.799092	46.887233
3506.376343	457970.273394	46.892237
3506.336570	457894.103865	46.897242
3506.149725	457810.660785	46.902247
3506.434305	457719.280938	46.907252
3506.313661	457639.475047	46.912257
3506.721380	457549.137757	46.917261
3506.170504	457477.615463	46.922266
3506.302997	457382.965596	46.927271
3506.403100	457293.592000	46.932276
3506.191416	457216.080775	46.937281
3506.318609	457129.134689	46.942285
3506.323932	457049.355634	46.947290
3506.390902	456964.750636	46.952295
3506.444616	456882.580450	46.957300
3506.155289	456796.869817	46.962305
3506.089294	456711.728918	46.967309
3506.101777	456634.177181	46.972314
3506.019321	456545.541049	46.977319
3506.256098	456458.928170	46.982324
3505.998573	456398.249564	46.987329
3506.300520	456315.527821	46.992333
3506.448978	456237.545851	46.997338
3506.038370	456154.843743	47.002343
3506.066183	456078.250317	47.007348
3506.284502	456005.222901	47.012353
3506.217195	455926.972450	47.017357
3506.324286	455847.931599	47.022362
3506.039071	455766.777827	47.027367
3506.154598	455677.242390	47.032372
3506.375649	455608.572293	47.037377
3506.205280	455524.356621	47.042381
3506.099248	455444.640945	47.047386
3506.042530	455357.211761	47.052391
3506.177200	455278.873637	47.057396
3506.064246	455208.991983	47.062401
3506.180994	455127.412197	47.067405
3506.148556	455049.608623	47.072410
3505.873711	454975.952054	47.077415
3506.086587	454887.308944	47.082420
3505.974312	454818.034119	47.087425
3505.978955	454742.554812	47.092429
3506.137347	454663.247146	47.097434
3505.724920	454599.649534	47.102439
3505.933579	454523.931819	47.107444
3505.949190	454461.578667	47.112449
3506.345449	454380.100242	47.117453
3506.132290	454300.905302	47.122458
3506.036209	454213.630013	47.127463
3506.206239	454124.534680	47.132468
3505.845525	454061.027946	47.137473
3505.997792	453979.234739	47.142477
3506.230986	453905.893107	47.147482
3506.005861	453823.910254	47.152487
3506.123653	453752.514117	47.157492
3506.061442	453684.849090	47.162497
3506.164463	453604.127358	47.167501
3505.826950	453531.946403	47.172506
3505.694253	453464.850318	47.177511
3505.966040	453390.232904	47.182516
3505.521494	453328.563205	47.187521
3505.720305	453251.423030	47.192525
3505.679144	453189.126396	47.197530
3505.661861	453118.105981	47.202535
3505.803499	453050.454753	47.207540
3505.611373	452983.519330	47.212545
3505.757296	452915.258583	47.217549
3505.642331	452850.388062	47.222554
3505.707564	452779.200302	47.227559
3505.607785	452720.410262	47.232564
3505.449153	452656.002847	47.237569
3505.750279	452582.036544	47.242573
3505.803259	452518.302314	47.247578
3505.567661	452449.902386	47.252583
3505.766982	452380.160553	47.257588
3505.727079	452315.630410	47.262593
3505.842233	452244.635070	47.267597
3505.733941	452185.997053	47.272602
3505.961445	452109.506772	47.277607
3506.096995	452051.080223	47.282612
3505.722766	451993.348925	47.287617
3505.809725	451912.775406	47.292621
3505.598875	451837.930602	47.297626
3505.800258	451767.679373	47.302631
3505.827027	451705.417361	47.307636
3505.761576	451648.544948	47.312641
3506.003714	451566.878920	47.317645
3505.716285	451502.489904	47.322650
3505.681462	451438.108256	47.327655
3505.524971	451368.170275	47.332660
3505.595803	451314.974716	47.337665
3505.819069	451237.062361	47.342669
3505.701240	451174.569949	47.347674
3505.525841	451112.036479	47.352679
3505.414811	451044.472536	47.357684
3505.361082	450983.895204	47.362689
3505.588521	450916.982856	47.367693
3505.484082	450861.331750	47.372698
3505.534679	450806.110329	47.377703
3505.689736	450731.199058	47.382708
3505.538025	450683.109952	47.387713
3505.294497	450618.558599	47.392717
3505.655060	450565.007447	47.397722
3505.534524	450494.198470	47.402727
3505.944666	450427.304055	47.407732
3505.338984	450368.897939	47.412737
3505.570940	450304.619338	47.417741
3505.544195	450241.398750	47.422746
3505.785318	450185.129115	47.427751
3505.978396	450107.521905	47.432756
3505.556304	450054.001675	47.437761
3505.632395	449983.360202	47.442765
3505.281736	449919.991139	47.447770
3505.316496	449865.885394	47.452775
3505.498853	449803.540429	47.457780
3505.194522	449747.768376	47.462785
3505.561171	449686.304251	47.467789
3505.236549	449629.571986	47.472794
3505.257371	449572.070735	47.477799
3505.607679	449512.484921	47.482804
3505.267166	449454.335192	47.487809
3504.927964	449393.548473	47.492813
3505.479633	449344.930557	47.497818
3505.786206	449289.509312	47.502823
3505.954723	449224.274848	47.507828
3505.911098	449168.000399	47.512833
3505.609279	449093.059866	47.517837
3505.764470	449033.962353	47.522842
3505.385212	448965.879739	47.527847
3505.818174	448908.204888	47.532852
3505.366366	448857.221930	47.537857
3505.521270	448795.943472	47.542861
3505.662787	448733.703715	47.547866
3504.882598	448671.367626	47.552871
3505.029453	448613.132351	47.557876
3504.821470	448574.479296	47.562881
3504.835668	448511.652152	47.567885
3505.067249	448470.489959	47.572890
3504.975958	448412.244086	47.577895
3505.220576	448363.422803	47.582900
3505.058774	448310.360745	47.587905
3505.070092	448258.435247	47.592909
3504.812469	448211.321983	47.597914
3504.698370	448166.060263	47.602919
3505.184568	448111.720802	47.607924
3505.110698	448066.299877	47.612929
3505.279561	448016.882243	47.617933
3504.763235	447965.603899	47.622938
3504.639953	447915.627422	47.627943
3504.664001	447866.639824	47.632948
3504.805645	447832.641520	47.637953
3504.787947	447791.013491	47.642957
3504.791095	447752.120048	47.647962
3504.620707	447703.570935	47.652967
3504.680659	447662.284351	47.657972
3504.552564	447618.291550	47.662977
3504.514631	447571.697139	47.667981
3504.569709	447550.542369	47.672986
3504.735733	447498.233631	47.677991
3504.747042	447448.283778	47.682996
3504.789106	447412.527001	47.688001
3504.793187	447364.048737	47.693005
3504.600070	447329.346154	47.698010
3504.626868	447284.362743	47.703015
3505.118388	447227.839620	47.708020
3504.615149	447187.459622	47.713025
3504.497806	447141.232788	47.718029
3504.783001	447110.352797	47.723034
3504.622423	447064.589563	47.728039
3504.743203	447022.327866	47.733044
3504.702851	446987.243671	47.738049
3504.429887	446938.862451	47.743053
3504.530087	446911.766287	47.748058
3504.338088	446876.352833	47.753063
3504.856705	446817.339203	47.758068
3504.733989	446791.345861	47.763073
3504.516203	446746.301654	47.768077
3504.630600	446691.159966	47.773082
3504.669746	446669.956330	47.778087
3504.669164	446621.680010	47.783092
3504.270790	446591.068116	47.788097
3504.659536	446552.005213	47.793101
3504.607575	446518.494261	47.798106
3505.018871	446474.356281	47.803111
3504.993736	446436.479477	47.808116
3504.904935	446393.745208	47.813121
3505.139073	446349.687930	47.818125
3505.354508	446296.708554	47.823130
3504.973097	446247.583608	47.828135
3504.950262	446205.243389	47.833140
3504.575124	446165.245267	47.838145
3505.127874	446113.019227	47.843149
3504.835534	446081.577105	47.848154
3504.665640	446031.299883	47.853159
3504.973733	445989.257715	47.858164
3504.807408	445959.720957	47.863169
3505.027980	445902.226342	47.868173
3504.831655	445857.024453	47.873178
3504.854739	445823.550309	47.878183
3504.801380	445779.084532	47.883188
3504.303733	445736.773745	47.888193
3504.587139	445705.334188	47.893197
3504.679540	445675.347157	47.898202
3504.574136	445628.354311	47.903207
3504.703893	445592.427369	47.908212
3504.530400	445553.813636	47.913217
3504.585891	445515.363588	47.918221
3504.426954	445482.477836	47.923226
3504.491167	445439.309824	47.928231
3504.502096	445395.491548	47.933236
3504.434946	445377.804011	47.938241
3504.678150	445338.966601	47.943245
3504.310045	445300.081358	47.948250
3504.618391	445277.917528	47.953255
3504.451703	445239.454208	47.958260
3504.427942	445193.612887	47.963265
3504.453048	445163.940917	47.968269
3504.479890	445132.290757	47.973274
3504.874093	445096.723544	47.978279
3504.592054	445054.577450	47.983284
3504.394817	445033.311125	47.988289
3504.596316	444982.815883	47.993293
3504.470712	444951.394345	47.998298
3504.664169	444923.214733	48.003303
3504.674365	444876.910506	48.008308
3504.813419	444849.450093	48.013313
3504.748836	444809.244264	48.018317
3504.747747	444771.867559	48.023322
3504.398920	444746.265343	48.028327
3504.709542	444691.237145	48.033332
3504.484701	444665.055795	48.038337
3504.877871	444630.400863	48.043341
3505.001361	444584.685246	48.048346
3504.753805	444560.891273	48.053351
3504.814898	444511.991081	48.058356
3504.587339	444479.470518	48.063361
3504.399413	444446.385266	48.068365
3504.407527	444404.543364	48.073370
3504.569308	444378.599946	48.078375
3504.696935	444340.997651	48.083380
3504.281865	444302.676497	48.088385
3504.535204	444273.319340	48.093389
3504.544130	444243.648863	48.098394
3504.322623	444203.265833	48.103399
3504.724686	444171.803775	48.108404
3504.851134	444137.295026	48.113409
3504.681450	444100.757408	48.118413
3504.647495	444070.688282	48.123418
3504.587447	444044.528756	48.128423
3504.569625	443990.670619	48.133428
3504.781413	443963.805261	48.138433
3504.075766	443918.635542	48.143437
3504.745509	443878.708329	48.148442
3505.109788	443846.643645	48.153447
3504.928718	443813.302665	48.158452
3504.617252	443778.158075	48.163457
3504.578968	443747.784935	48.168461
3505.002218	443699.581826	48.173466
3504.639786	443667.793114	48.178471
3504.665320	443627.011800	48.183476
3504.619185	443588.271359	48.188481
3504.789164	443568.208829	48.193485
3505.115324	443515.457284	48.198490
3504.690752	443484.997580	48.203495
3504.973433	443437.984405	48.208500
3504.917991	443404.519908	48.213505
3504.987310	443359.825314	48.218509
3504.829176	443329.319897	48.223514
3504.536659	443286.056329	48.228519
3504.873119	443252.017495	48.233524
3504.595544	443216.511176	48.238529
3503.995712	443171.169669	48.243533
3504.216613	443143.895989	48.248538
3504.312258	443127.294623	48.253543
3504.668435	443089.854005	48.258548
3504.602225	443061.919181	48.263553
3504.771100	443022.938140	48.268557
3505.023961	442993.325736	48.273562
3504.719501	442958.026460	48.278567
3504.972626	442922.784078	48.283572
3504.532024	442889.485991	48.288577
3504.582741	442853.365108	48.293581
3504.449072	442819.456590	48.298586
3504.466774	442778.776458	48.303591
3504.748387	442747.434342	48.308596
3504.776813	442717.961324	48.313601
3504.726922	442671.510476	48.318605
3504.163817	442655.173389	48.323610
3504.341084	442620.146349	48.328615
3504.160222	442577.014464	48.333620
3504.075674	442563.790963	48.338625
3504.188854	442536.636356	48.343629
3504.182512	442521.928590	48.348634
3504.083190	442494.810215	48.353639
3504.320265	442448.259170	48.358644
3503.896991	442426.623110	48.363649
3503.812150	442400.770157	48.368653
3503.902030	442388.328296	48.373658
3504.026663	442375.525449	48.378663
3503.994143	442338.707836	48.383668
3504.175466	442334.467080	48.388673
3504.207231	442307.123205	48.393677
3504.357490	442261.702443	48.398682
3504.161886	442242.867694	48.403687
3504.376561	442213.260750	48.408692
3504.411082	442197.429926	48.413697
3504.235201	442153.941305	48.418701
3504.457092	442121.898391	48.423706
3504.367441	442113.138953	48.428711
3504.387692	442076.768379	48.433716
3504.177277	442050.632124	48.438721
3504.290149	442022.310338	48.443725
3503.975343	442006.285416	48.448730
3503.999163	441989.999776	48.453735
3504.214138	441971.703344	48.458740
3504.078202	441934.040440	48.463745
3504.437246	441900.097083	48.468749
3503.952600	441873.398780	48.473754
3503.888470	441859.309096	48.478759
3504.367846	441836.858939	48.483764
3504.168388	441830.400620	48.488769
3504.435551	441792.516478	48.493773
3504.440674	441754.879902	48.498778
3504.120449	441737.587656	48.503783
3503.925999	441714.390154	48.508788
3504.094702	441696.912948	48.513793
3503.908813	441653.881539	48.518797
3504.002175	441633.221642	48.523802
3503.948390	441615.224415	48.528807
3504.239126	441596.204621	48.533812
3504.007784	441590.664678	48.538817
3504.105271	441568.330176	48.543821
3503.946262	441546.343783	48.548826
3504.031152	441512.700249	48.553831
3504.057347	441487.588095	48.558836
3504.072430	441463.948768	48.563841
3504.255398	441444.795075	48.568845
3503.959652	441430.288158	48.573850
3503.841650	441422.649185	48.578855
3503.886327	441401.236541	48.583860
3503.908566	441391.595420	48.588865
3503.824062	441353.466228	48.593869
3503.832954	441318.618021	48.598874
3503.951661	441305.967730	48.603879
3503.955928	441281.721376	48.608884
3504.010997	441268.422528	48.613889
3503.745856	441250.359643	48.618893
3503.990692	441230.941585	48.623898
3503.787292	441232.092249	48.628903
3503.925453	441209.902606	48.633908
3503.664556	441201.425659	48.638913
3503.614007	441186.369479	48.643917
3503.962753	441165.411919	48.648922
3503.862386	441161.776993	48.653927
3503.801434	441140.585024	48.658932
3503.968611	441131.629169	48.663937
3503.769953	441098.794268	48.668941
3503.895669	441067.679258	48.673946
3503.704872	441055.943972	48.678951
3503.602078	441032.780820	48.683956
3503.622399	441019.183413	48.688961
3503.642741	441007.513496	48.693965
3503.979740	440997.818457	48.698970
3503.456619	440984.313820	48.703975
3503.774723	440967.622105	48.708980
3503.575907	440956.598269	48.713985
3503.528750	440943.265955	48.718989
3503.874416	440926.975294	48.723994
3503.620738	440921.286823	48.728999
3503.566098	440901.970333	48.734004
3503.772949	440888.138098	48.739009
3503.967105	440868.373304	48.744013
3503.625526	440865.134584	48.749018
3503.680397	440857.364448	48.754023
3503.641666	440836.168391	48.759028
3503.889963	440823.597143	48.764033
3503.826618	440811.586343	48.769037
3503.996642	440795.376300	48.774042
3504.023938	440795.067315	48.779047
3504.246327	440771.746915	48.784052
3503.738114	440763.109130	48.789057
3503.665425	440754.143353	48.794061
3504.034112	440737.290654	48.799066
3504.065561	440724.807101	48.804071
3504.102371	440703.547293	48.809076
3504.066666	440669.923059	48.814081
3504.223708	440648.541219	48.819085
3504.034887	440627.928559	48.824090
3503.352870	440623.124743	48.829095
3503.992725	440605.261873	48.834100
3503.798774	440593.729776	48.839105
3503.686454	440582.386635	48.844109
3503.695782	440572.696634	48.849114
3503.952822	440555.051262	48.854119
3503.936169	440547.141055	48.859124
3503.842397	440536.454145	48.864129
3503.694202	440521.617082	48.869133
3503.853143	440513.372531	48.874138
3503.549930	440496.127124	48.879143
3503.856235	440485.219702	48.884148
3503.585103	440470.352871	48.889153
3503.615887	440455.282303	48.894157
3503.722731	440453.742330	48.899162
3503.529333	440452.811598	48.904167
3503.747426	440423.252380	48.909172
3503.630194	440429.156533	48.914177
3503.526302	440415.174160	48.919181
3503.645182	440386.899963	48.924186
3503.535460	440391.230362	48.929191
3503.544369	440373.677938	48.934196
3503.624348	440360.222112	48.939201
3503.644821	440346.066285	48.944205
3503.413599	440342.960819	48.949210
3503.333166	440338.865825	48.954215
3503.781169	440317.535433	48.959220
3503.501329	440313.575933	48.964225
3503.180835	440303.231975	48.969229
3503.501192	440284.104539	48.974234
3503.447495	440279.700616	48.979239
3503.816322	440270.152000	48.984244
3503.737221	440256.520372	48.989249
3503.606404	440244.114978	48.994253
3503.671224	440237.611063	48.999258
3503.621879	440232.496230	49.004263
3503.698244	440206.866790	49.009268
3503.731730	440206.658192	49.014273
3503.502272	440199.900159	49.019277
3503.827833	440187.924065	49.024282
3503.549781	440193.348483	49.029287
3503.645507	440162.896749	49.034292
3503.656240	440165.786304	49.039297
3503.434537	440161.005239	49.044301
3503.725808	440164.049795	49.049306
3503.907550	440164.728945	49.054311
3503.914772	440134.698090	49.059316
3503.764138	440111.136330	49.064321
3503.602543	440106.142085	49.069325
3503.721535	440075.736984	49.074330
3503.752087	440069.188145	49.079335
3503.422303	440052.657090	49.084340
3503.964862	440051.803581	49.089345
3503.804869	440033.924645	49.094349
3503.798396	440030.527129	49.099354
3503.622749	440027.868663	49.104359
3503.892915	440001.445003	49.109364
3503.730090	439994.066817	49.114369
3503.791596	439989.643165	49.119373
3504.104861	439971.784823	49.124378
3503.951643	439967.499282	49.129383
3504.133892	439954.989545	49.134388
3504.239970	439948.072690	49.139393
3503.931957	439923.066541	49.144397
3504.016207	439899.870259	49.149402
3503.876221	439888.937295	49.154407
3503.870497	439873.618932	49.159412
3504.017707	439859.288973	49.164417
3503.767746	439859.737486	49.169421
3504.084254	439846.443867	49.174426
3503.912825	439837.393124	49.179431
3503.606663	439825.271067	49.184436
3503.466725	439811.649552	49.189441
3503.802763	439807.331167	49.194445
3503.993184	439790.609638	49.199450
3503.662452	439791.528484	49.204455
3503.720903	439770.162628	49.209460
3503.566930	439770.290394	49.214465
3503.796455	439749.554753	49.219469
3503.969449	439741.916235	49.224474
3503.859397	439740.210341	49.229479
3503.789189	439709.837042	49.234484
3503.838673	439683.755045	49.239489
3504.076200	439656.778551	49.244493
3504.454683	439650.575994	49.249498
3503.552909	439649.614001	49.254503
3503.482611	439632.125240	49.259508
3503.617422	439626.775914	49.264513
3503.895739	439620.032455	49.269517
3504.353306	439600.881000	49.274522
3503.761396	439596.822475	49.279527
3503.753984	439580.794019	49.284532
3503.707023	439579.584610	49.289537
3503.596073	439563.878182	49.294541
3504.052137	439557.459444	49.299546
3503.990250	439557.622215	49.304551
3503.669650	439531.095957	49.309556
3503.691297	439503.395231	49.314561
3503.679948	439502.484101	49.319565
3504.015510	439488.426104	49.324570
3503.836164	439474.050201	49.329575
3503.952704	439454.551032	49.334580
3503.936025	439442.430063	49.339585
3504.133425	439424.286699	49.344589
3504.106394	439420.334598	49.349594
3503.920601	439410.170129	49.354599
3503.817539	439399.179890	49.359604
3503.871833	439399.475007	49.364609
3504.018785	439392.398817	49.369613
3503.834340	439350.123568	49.374618
3504.107237	439328.061210	49.379623
3504.389919	439306.859531	49.384628
3504.255865	439303.280776	49.389633
3504.220515	439288.727982	49.394637
3504.270927	439277.254928	49.399642
3503.894955	439247.034658	49.404647
3503.916757	439224.000515	49.409652
3504.239483	439214.357862	49.414657
3504.127413	439200.021021	49.419661
3504.029815	439188.268825	49.424666
3504.159595	439183.681171	49.429671
3503.826082	439154.823181	49.434676
3504.265638	439133.543822	49.439681
3504.198550	439111.843670	49.444685
3504.293023	439105.841641	49.449690
3503.734968	439093.305639	49.454695
3504.025065	439081.132091	49.459700
3503.906713	439068.470268	49.464705
3503.823821	439067.774248	49.469709
3504.105642	439037.745745	49.474714
3503.932304	439020.477008	49.479719
3503.890694	439003.642320	49.484724
3503.896156	438985.429914	49.489729
3503.619310	438986.085948	49.494733
3504.020278	438968.364009	49.499738
3503.746423	438968.410792	49.504743
3503.690961	438956.549822	49.509748
3504.095201	438949.886116	49.514753
3503.730992	438937.469112	49.519757
3504.077471	438923.865452	49.524762
3503.894363	438920.092097	49.529767
3503.998675	438908.660377	49.534772
3503.622560	438874.736437	49.539777
3503.664021	438850.024503	49.544781
3503.932289	438833.339689	49.549786
3503.554131	438828.331404	49.554791
3503.713012	438824.753283	49.559796
3503.942755	438815.126334	49.564801
3503.472099	438809.728008	49.569805
3503.773808	438798.262526	49.574810
3503.614767	438793.977752	49.579815
3503.790651	438782.939577	49.584820
3503.779455	438772.643546	49.589825
3503.722171	438760.275493	49.594829
3504.010746	438753.022732	49.599834
3503.403619	438749.473935	49.604839
3503.770759	438741.497550	49.609844
3503.852917	438727.025780	49.614849
3504.009842	438723.143603	49.619853
3503.558989	438713.886466	49.624858
3503.421689	438706.402033	49.629863
3503.797274	438690.206079	49.634868
3504.054649	438686.103827	49.639873
3503.443812	438686.867627	49.644877
3504.192419	438665.027759	49.649882
3504.069821	438663.374653	49.654887
3504.122107	438652.002414	49.659892
3503.819999	438650.735062	49.664897
3503.748711	438635.071933	49.669901
3503.930678	438616.778358	49.674906
3503.908891	438595.729448	49.679911
3503.696067	438576.843769	49.684916
3504.203390	438567.930258	49.689921
3504.002533	438560.000063	49.694925
3504.194167	438546.016778	49.699930
3504.148784	438541.763277	49.704935
3503.666732	438529.772001	49.709940
3503.813561	438523.862334	49.714945
3503.648841	438514.454798	49.719949
3503.782277	438505.960209	49.724954
3503.502182	438500.427810	49.729959
3503.788160	438494.494376	49.734964
3503.846700	438480.838152	49.739969
3503.541359	438481.854172	49.744973
3504.128500	438453.649743	49.749978
3503.726165	438431.346684	49.754983
3503.598813	438411.076569	49.759988
3503.985646	438392.544911	49.764993
3503.716402	438384.626331	49.769997
3504.233080	438376.573553	49.775002
3503.553068	438370.044080	49.780007
3503.797920	438359.095379	49.785012
3504.024932	438353.932924	49.790017
3503.671175	438350.848098	49.795021
3503.865274	438338.031048	49.800026
3503.886063	438329.606357	49.805031
3503.949880	438318.739278	49.810036
3503.559862	438310.131074	49.815041
3503.450067	438307.055315	49.820045
3503.779323	438298.628671	49.825050
3503.601538	438292.672911	49.830055
3503.798754	438283.304937	49.835060
3503.729327	438281.490533	49.840065
3503.392235	438272.112326	49.845069
3503.576916	438257.876397	49.850074
3503.857664	438252.349633	49.855079
3504.031543	438246.638194	49.860084
3503.833591	438238.555198	49.865089
3503.612567	438234.382360	49.870093
3503.781365	438223.294388	49.875098
3503.596833	438222.006935	49.880103
3503.769667	438207.417885	49.885108
3504.052071	438199.709427	49.890113
3503.938956	438188.263733	49.895117
3503.870768	438167.577452	49.900122
3503.717180	438141.629779	49.905127
3503.608611	438127.545300	49.910132
3503.507097	438121.728661	49.915137
3503.585931	438125.367810	49.920141
3503.699979	438123.369874	49.925146
3503.510638	438118.582839	49.930151
3503.705700	438122.607985	49.935156
3503.810140	438126.344222	49.940161
3503.468024	438127.518728	49.945165
3503.527089	438112.086626	49.950170
3503.614691	438108.977135	49.955175
3503.696072	438099.933245	49.960180
3503.490216	438095.656330	49.965185
3503.332357	438093.501897	49.970189
3503.656060	438078.126045	49.975194
3503.568393	438076.822043	49.980199
3503.782678	438062.834588	49.985204
3503.780148	438060.653629	49.990209
3503.688492	438063.104366	49.995213
3504.061547	438048.125912	50.000218
3503.841298	438039.184231	50.005223
3503.977732	438028.761187	50.010228
3504.094020	438024.023407	50.015233
3503.930288	438001.679176	50.020237
3503.938182	437967.688282	50.025242
3503.450479	437968.836925	50.030247
3503.677570	437958.652022	50.035252
3503.872108	437947.458057	50.040257
3503.522010	437948.633935	50.045261
3503.799260	437931.084491	50.050266
3503.503641	437927.177985	50.055271
3503.720227	437916.893396	50.060276
3503.759974	437913.081817	50.065281
3503.478745	437911.557202	50.070285
3503.741134	437901.163322	50.075290
3503.651589	437894.532887	50.080295
3503.569517	437887.038747	50.085300
3504.047284	437878.130009	50.090305
3503.317023	437871.913354	50.095309
3503.497854	437860.569494	50.100314
3503.531040	437871.927586	50.105319
3503.432370	437873.567846	50.110324
3503.666880	437882.862319	50.115329
3503.298885	437882.722252	50.120333
3503.493671	437857.424997	50.125338
3503.274171	437859.441007	50.130343
3503.731544	437861.493634	50.135348
3503.748588	437849.264577	50.140353
3503.499548	437845.705220	50.145357
3503.508540	437831.296094	50.150362
3503.462964	437826.027869	50.155367
3503.336100	437824.629083	50.160372
3503.675782	437812.497109	50.165377
3503.558594	437819.315105	50.170381
3503.740468	437802.796467	50.175386
3503.821698	437799.535828	50.180391
3503.603950	437799.877417	50.185396
3503.747921	437786.206181	50.190401
3503.677561	437782.210456	50.195405
3503.866786	437774.162643	50.200410
3503.499971	437770.927772	50.205415
3503.540625	437768.029175	50.210420
3503.756055	437756.882279	50.215425
3503.323157	437756.702562	50.220429
3503.886719	437741.995761	50.225434
3503.697489	437743.905150	50.230439
3503.870124	437737.787945	50.235444
3504.018922	437730.203601	50.240449
3503.824968	437731.099172	50.245453
3504.189441	437719.318033	50.250458
3504.065652	437719.795773	50.255463
3503.158251	437700.571368	50.260468
3503.484648	437698.435673	50.265473
3503.505142	437695.033195	50.270477
3503.725311	437682.262050	50.275482
3503.531031	437676.461135	50.280487
3503.334746	437673.044937	50.285492
3503.776429	437662.265213	50.290497
3503.443687	437666.887879	50.295501
3503.703819	437650.761617	50.300506
3503.363835	437653.609921	50.305511
3503.520938	437664.490377	50.310516
3503.842488	437665.450123	50.315521
3503.456268	437677.235047	50.320525
3503.667692	437667.255613	50.325530
3503.683469	437667.405136	50.330535
3503.471005	437658.106853	50.335540
3503.307928	437654.380593	50.340545
3503.379767	437650.969341	50.345549
3503.608621	437637.131326	50.350554
3503.553666	437640.844130	50.355559
3503.759567	437627.466612	50.360564
3503.984827	437623.978428	50.365569
3503.871843	437627.041633	50.370573
3503.862390	437611.164301	50.375578
3503.933865	437604.709211	50.380583
3503.831420	437601.936489	50.385588
3503.750818	437592.869322	50.390593
3503.607540	437588.886013	50.395597
3503.439306	437578.920634	50.400602
3503.380421	437573.553158	50.405607
3503.379375	437573.046042	50.410612
3503.305287	437556.723123	50.415617
3503.310221	437557.939862	50.420621
3503.382500	437550.267060	50.425626
3503.435432	437547.721459	50.430631
3503.431782	437543.967959	50.435636
3503.640049	437548.904126	50.440641
3503.444403	437566.744369	50.445645
3503.256964	437574.436874	50.450650
3503.382186	437571.523811	50.455655
3503.229961	437556.583988	50.460660
3503.424707	437543.766373	50.465665
3503.321609	437550.480582	50.470669
3503.392300	437539.003170	50.475674
3503.715829	437542.194779	50.480679
3503.294136	437532.881437	50.485684
3503.799088	437540.303533	50.490689
3503.225921	437550.344835	50.495693
3503.290797	437545.717196	50.500698
3503.082467	437550.420106	50.505703
3503.274518	437544.299532	50.510708
3503.767239	437537.569569	50.515713
3503.228345	437538.168924	50.520717
3503.316394	437532.421227	50.525722
3503.259897	437530.300164	50.530727
3503.105292	437516.679745	50.535732
3503.710700	437514.394928	50.540737
3503.388110	437491.214871	50.545741
3503.508675	437436.200949	50.550746
3503.269091	437382.364492	50.555751
3503.193099	437314.345688	50.560756
3503.588433	437229.656707	50.565761
3503.225775	437154.431629	50.570765
3503.602256	437050.263871	50.575770
3503.141924	436937.715361	50.580775
3503.204350	436816.198693	50.585780
3503.052345	436679.345690	50.590785
3502.965776	436539.436643	50.595789
3503.369018	436380.011852	50.600794
3503.333395	436217.819728	50.605799
3503.227548	436040.773051	50.610804
3503.264300	435838.535821	50.615809
3503.084262	435647.089827	50.620813
3503.077156	435419.792756	50.625818
3503.074253	435197.566385	50.630823
3503.233471	434963.386845	50.635828
3503.056575	434707.698611	50.640833
3503.057087	434450.556528	50.645837
3503.601624	434171.500776	50.650842
3503.363605	433878.672500	50.655847
3503.107507	433571.078049	50.660852
3503.109696	433257.143442	50.665857
3502.845792	432924.120235	50.670861
3502.885121	432583.327523	50.675866
3503.030692	432237.132812	50.680871
3502.771808	431868.725206	50.685876
3503.234479	431494.403575	50.690881
3503.002198	431107.914028	50.695885
3503.186989	430686.280724	50.700890
3503.010481	430271.501690	50.705895
3502.969445	429842.330252	50.710900
3502.866302	429391.237663	50.715905
3502.724579	428927.353801	50.720909
3502.657678	428451.419846	50.725914
3502.838324	427958.939353	50.730919
3502.922853	427449.005677	50.735924
3503.086032	426928.084527	50.740929
3502.818832	426385.349556	50.745933
3502.929637	425821.879453	50.750938
3502.531400	425259.701227	50.755943
3502.368863	424662.648382	50.760948
3502.780052	424061.726478	50.765953
3502.513974	423459.128629	50.770957
3502.593227	422806.860766	50.775962
3502.449274	422156.491891	50.780967
3502.119627	421485.830884	50.785972
3502.295079	420796.966604	50.790977
3502.154878	420097.780080	50.795981
3501.703517	419366.108306	50.800986
3502.268794	418628.783438	50.805991
3501.589081	417890.151623	50.810996
3501.957784	417106.535258	50.816001
3501.883705	416327.438586	50.821005
3501.877163	415510.070262	50.826010
3501.839011	414680.138469	50.831015
3501.645167	413832.178874	50.836020
3501.817775	412956.781899	50.841025
3501.585334	412072.537144	50.846029
3501.707711	411161.157747	50.851034
3501.269004	410240.421205	50.856039
3500.990699	409299.537490	50.861044
3501.692472	408337.094896	50.866049
3501.395689	407355.257782	50.871053
3501.496080	406357.595635	50.876058
3501.023814	405331.852416	50.881063
3500.651635	404286.495551	50.886068
3500.781456	403221.378253	50.891073
3500.404194	402144.520073	50.896077
3500.569795	401041.210152	50.901082
3500.181078	399924.208048	50.906087
3499.972886	398793.488617	50.911092
3499.884703	397637.145491	50.916097
3499.774955	396480.149879	50.921101
3499.382094	395275.999132	50.926106
3499.479777	394073.341340	50.931111
3499.412972	392853.587086	50.936116
3499.256149	391607.167370	50.941121
3498.780706	390348.120565	50.946125
3498.928679	389068.304931	50.951130
3498.754119	387778.198181	50.956135
3498.635747	386458.190364	50.961140
3498.477567	385110.277141	50.966145
3498.111976	383763.587402	50.971149
3498.062634	382391.622413	50.976154
3498.116160	381004.965260	50.981159
3497.683542	379606.282818	50.986164
3497.795861	378171.730274	50.991169
3497.662985	376728.997309	50.996173
3497.326674	375258.601550	51.001178
3497.102254	373774.877077	51.006183
3496.883048	372292.410514	51.011188
3496.982241	370769.626325	51.016193
3496.384008	369244.887348	51.021197
3496.461793	367692.148608	51.026202
3495.902595	366133.781815	51.031207
3495.762838	364549.617417	51.036212
3495.980622	362954.363891	51.041217
3495.570494	361346.942865	51.046221
3495.374124	359708.744329	51.051226
3495.134012	358080.634299	51.056231
3494.776824	356417.222486	51.061236
3494.688621	354735.737657	51.066241
3494.318434	353047.288000	51.071245
3494.155891	351335.355918	51.076250
3494.230054	349618.634110	51.081255
3493.661676	347877.657509	51.086260
3493.688228	346105.674341	51.091265
3493.527120	344334.443030	51.096269
3493.136333	342541.707748	51.101274
3492.891148	340741.398694	51.106279
3492.702517	338918.797851	51.111284
3492.401273	337087.802233	51.116289
3492.412450	335246.074902	51.121293
3492.146048	333378.981588	51.126298
3491.922142	331508.608582	51.131303
3491.508522	329620.234931	51.136308
3491.027773	327696.379177	51.141313
3490.834362	325784.754620	51.146317
3490.689762	323846.562070	51.151322
3490.301260	321906.160094	51.156327
3489.786294	319954.518928	51.161332
3489.684701	317974.084089	51.166337
3489.052397	316001.648919	51.171341
3488.899975	314006.137581	51.176346
3488.588507	312000.082941	51.181351
3488.170876	309985.030083	51.186356
3488.084140	307945.909758	51.191361
3487.637341	305902.572091	51.196365
3487.389508	303844.280610	51.201370
3487.107004	301774.513599	51.206375
3486.597265	299693.330767	51.211380
3486.680423	297608.232368	51.216385
3486.149002	295499.514169	51.221389
3485.690457	293379.053114	51.226394
3485.276349	291246.168161	51.231399
3485.010547	289100.919643	51.236404
3484.844272	286954.496913	51.241409
3484.336294	284795.034275	51.246413
3483.857343	282619.057824	51.251418
3483.697134	280438.030696	51.256423
3483.112905	278251.114332	51.261428
3482.598201	276032.377799	51.266433
3482.468894	273827.788064	51.271437
3482.242659	271595.332817	51.276442
3482.066050	269354.013355	51.281447
3480.835840	267101.473839	51.286452
3480.778683	264840.239943	51.291457
3480.481778	262581.048466	51.296461
3479.905589	260294.646114	51.301466
3479.355446	258008.005171	51.306471
3479.247642	255720.064207	51.311476
3478.609298	253411.330874	51.316481
3478.153543	251107.180025	51.321485
3477.699621	248785.259112	51.326490
3477.669279	246459.404825	51.331495
3476.501621	244130.447146	51.336500
3476.018579	241775.666675	51.341505
3475.509562	239431.861437	51.346509
3475.418311	237073.313215	51.351514
3474.607762	234714.863217	51.356519
3474.034600	232347.183380	51.361524
3473.684753	229955.662232	51.366529
3473.145943	227577.146888	51.371533
3472.670616	225183.788963	51.376538
3472.181162	222784.111041	51.381543
3471.287198	220393.894907	51.386548
3471.084886	217975.244561	51.391553
3470.552614	215567.068997	51.396557
3470.069400	213138.802279	51.401562
3469.282339	210725.544949	51.406567
3468.894554	208282.393343	51.411572
3468.518031	205845.064102	51.416577
3467.506651	203413.925196	51.421581
3467.753534	200955.190942	51.426586
3466.874831	198501.058749	51.431591
3465.516361	196039.558616	51.436596
3465.499236	193576.684320	51.441601
3464.790961	191111.628566	51.446605
3464.394508	188626.037216	51.451610
3463.911960	186158.609109	51.456615
3463.146618	183675.324870	51.461620
3462.513899	181192.585900	51.466625
3461.634882	178708.908184	51.471629
3460.959967	176221.622997	51.476634
3460.115186	173725.340148	51.481639
3459.788994	171241.932220	51.486644
3459.302669	168744.240679	51.491649
3458.511075	166244.216398	51.496653
3457.738652	163749.796817	51.501658
3456.999850	161245.285893	51.506663
3455.998250	158749.856875	51.511668
3455.527769	156243.370267	51.516673
3454.878160	153750.752710	51.521677
3453.996718	151247.076690	51.526682
3453.273380	148746.447269	51.531687
3452.147086	146243.343427	51.536692
3451.809052	143732.887246	51.541697
3450.636662	141182.535234	51.546701
3450.146791	138690.028787	51.551706
3449.554194	136200.109109	51.556711
3448.408321	133707.988247	51.561716
3447.617943	131215.231155	51.566721
3446.961927	128737.638347	51.571725
3445.926277	126255.257856	51.576730
3445.130353	123769.081627	51.581735
3444.384087	121295.511704	51.586740
3443.595158	118813.513054	51.591745
3442.569122	116349.078065	51.596749
3441.273644	113885.609504	51.601754
3440.523240	111426.655137	51.606759
3439.476091	108973.478874	51.611764
3438.901127	106523.932413	51.616769
3438.074861	104091.601790	51.621773
3437.069169	101651.803893	51.626778
3436.293516	99230.671785	51.631783
3435.153969	96799.596942	51.636788
3433.873584	94380.608398	51.641793
3432.482825	91981.405035	51.646797
3431.823621	89581.472266	51.651802
3430.403216	87190.427154	51.656807
3429.300752	84826.154165	51.661812
3428.732171	82458.740477	51.666817
3427.260427	80105.846779	51.671821
3425.827499	77760.125445	51.676826
3424.994798	75428.850450	51.681831
3423.853834	73121.870788	51.686836
3422.510222	70822.432283	51.691841
3421.524294	68529.958156	51.696845
3420.408186	66255.308567	51.701850
3418.786055	63981.913734	51.706855
3417.759682	61735.539983	51.711860
3416.679353	59497.877750	51.716865
3414.974678	57289.705486	51.721869
3413.653719	55084.590313	51.726874
3412.765083	52899.236597	51.731879
3411.044540	50754.784029	51.736884
3409.908581	48592.542285	51.741889
3408.428890	46470.571164	51.746893
3406.638876	44360.781553	51.751898
3405.110656	42273.973346	51.756903
3403.581532	40227.095008	51.761908
3401.898702	38185.122890	51.766913
3400.440013	36182.376147	51.771917
3398.869431	34198.175688	51.776922
3396.938588	32241.836432	51.781927
3394.608469	30320.953638	51.786932
3392.846210	28432.632191	51.791937
3389.658775	26584.336147	51.796941
3385.614557	24795.423073	51.801946
3380.384435	23136.042715	51.806951
3373.001458	21590.248811	51.811956
3365.547273	20152.227580	51.816961
3358.372205	18839.119548	51.821965
3351.732644	17650.492144	51.826970
3345.370167	16587.743447	51.831975
3339.642193	15642.799755	51.836980
3334.609575	14813.364693	51.841985
3329.810867	14097.382397	51.846989
3325.832713	13471.412378	51.851994
3322.386475	12947.477819	51.856999
3318.721706	12507.917589	51.862004
3316.390709	12138.076173	51.867009
3314.198710	11838.429476	51.872013
3312.241350	11589.593886	51.877018
3310.431671	11388.971750	51.882023
3309.254691	11244.776655	51.887028
3308.537714	11129.434006	51.892033
3307.279603	11054.384289	51.897037
3306.756192	10990.743303	51.902042
3306.246576	10942.067359	51.907047
3305.673257	10927.637402	51.912052
3305.426369	10911.288901	51.917057
3304.991455	10921.593578	51.922061
3304.850239	10932.292063	51.927066
3304.638257	10935.442438	51.932071
3304.180412	10953.104282	51.937076
3304.268298	10971.753627	51.942081
3304.186167	11007.050332	51.947085
3303.923835	11031.385907	51.952090
3304.314991	11047.991166	51.957095
3303.794510	11066.978384	51.962100
3303.889125	11076.737662	51.967105
3303.980133	11098.808885	51.972109
3303.863434	11107.575702	51.977114
3303.532435	11115.312634	51.982119
3303.732212	11113.110772	51.987124
3303.520055	11105.768451	51.992129
3303.255516	11093.017276	51.997133
3303.439841	11080.317412	52.002138
3303.579248	11052.533146	52.007143
3303.173441	11026.891310	52.012148
3303.535627	10989.246307	52.017153
3303.523952	10951.376118	52.022157
3303.340071	10890.429852	52.027162
3303.449767	10833.972916	52.032167
3303.001289	10759.193885	52.037172
3303.089524	10675.911828	52.042177
3302.187417	10610.264116	52.047181
3301.558563	10546.315826	52.052186
3301.102512	10464.434439	52.057191
3299.845210	10392.149362	52.062196
3299.439048	10305.436733	52.067201
3298.795924	10226.282262	52.072205
3298.124323	10164.846932	52.077210
3297.552057	10098.323389	52.082215
3296.942217	10030.371993	52.087220
3296.703721	9942.638900	52.092225
3296.138279	9882.410912	52.097229
3295.673789	9806.490416	52.102234
3295.451174	9721.108231	52.107239
3294.520604	9640.936144	52.112244
3294.281502	9549.238260	52.117249
3293.619610	9480.291693	52.122253
3292.795774	9401.759806	52.127258
3292.412358	9305.714976	52.132263
3291.763453	9237.642443	52.137268
3291.401205	9137.568041	52.142273
3290.590107	9053.119294	52.147277
3290.009159	8959.036033	52.152282
3289.720791	8872.874905	52.157287
3288.678885	8777.236372	52.162292
3288.127156	8697.901542	52.167297
3287.180200	8611.644201	52.172301
3286.748561	8533.588221	52.177306
3285.825718	8439.171449	52.182311
3285.200467	8362.356290	52.187316
3285.063715	8272.420597	52.192321
3284.290539	8186.635030	52.197325
3283.707025	8103.318982	52.202330
3283.259652	8018.796124	52.207335
3282.456448	7935.812294	52.212340
3281.764042	7836.555849	52.217345
3280.926254	7765.882136	52.222349
3280.286387	7672.118936	52.227354
3279.565127	7594.425795	52.232359
3278.945037	7511.456309	52.237364
3278.576544	7421.215054	52.242369
3277.949620	7337.847981	52.247373
3277.196405	7258.380098	52.252378
3276.951193	7167.180910	52.257383
3276.012642	7080.669689	52.262388
3275.517048	6994.912551	52.267393
3274.735313	6917.597107	52.272397
3274.020726	6823.632842	52.277402
3273.436323	6741.718760	52.282407
3272.775832	6661.969459	52.287412
3272.762738	6564.318639	52.292417
3271.997483	6494.326023	52.297421
3271.235510	6398.828333	52.302426
3270.491281	6309.376986	52.307431
3269.978592	6217.924820	52.312436
3269.599670	6127.217966	52.317441
3268.648742	6037.354079	52.322445
3267.978162	5944.884024	52.327450
3267.236731	5861.319895	52.332455
3266.294707	5772.654014	52.337460
3265.669798	5682.065151	52.342465
3265.038937	5594.305050	52.347469
3264.316091	5506.724617	52.352474
3263.657333	5423.425059	52.357479
3262.937762	5337.737165	52.362484
3262.531745	5256.814202	52.367489
3261.813775	5176.203966	52.372493
3260.883781	5094.129920	52.377498
3260.327752	5011.018710	52.382503
3259.577354	4931.636917	52.387508
3259.203921	4847.645651	52.392513
3258.216447	4772.819824	52.397517
3257.608513	4694.696540	52.402522
3257.363644	4602.373963	52.407527
3256.781435	4524.718557	52.412532
3256.120934	4433.675378	52.417537
3255.522858	4352.360237	52.422541
3254.915570	4271.969413	52.427546
3254.083503	4184.022449	52.432551
3253.409492	4098.796181	52.437556
3252.927801	4016.850102	52.442561
3252.216974	3927.434837	52.447565
3251.516844	3847.566607	52.452570
3250.695880	3760.751651	52.457575
3249.802935	3682.608598	52.462580
3249.202391	3597.571460	52.467585
3248.278234	3519.141594	52.472589
3247.584085	3446.208077	52.477594
3247.450838	3361.127120	52.482599
3246.523274	3293.739404	52.487604
3245.721679	3214.771331	52.492609
3245.284377	3138.942486	52.497613
3244.428631	3063.802171	52.502618
3243.928385	2977.413641	52.507623
3243.274329	2912.209077	52.512628
3242.571199	2826.510609	52.517633
3242.025821	2760.273480	52.522637
3241.016583	2684.997746	52.527642
3240.833606	2602.917151	52.532647
3239.846530	2527.644698	52.537652
3239.204846	2442.740026	52.542657
3238.455095	2371.970976	52.547661
3237.381222	2305.676815	52.552666
3236.972335	2231.154997	52.557671
3236.529433	2166.778065	52.562676
3235.792169	2092.751205	52.567681
3234.905056	2024.465070	52.572685
3234.343989	1953.680666	52.577690
3233.841074	1877.900673	52.582695
3232.659840	1815.590435	52.587700
3232.385232	1741.989125	52.592705
3231.654999	1683.410304	52.597709
3230.908783	1618.089464	52.602714
3230.560105	1543.949457	52.607719
3229.680804	1488.310978	52.612724
3229.014380	1415.851886	52.617729
3228.291633	1356.706919	52.622733
3227.247782	1291.949893	52.627738
3227.116683	1228.741361	52.632743
3225.904304	1180.118455	52.637748
3225.025508	1119.838490	52.642753
3224.089592	1063.327341	52.647757
3223.547000	1007.949242	52.652762
3222.956046	963.926665	52.657767
3222.174574	906.777046	52.662772
3221.545362	859.783321	52.667777
3220.968680	810.440711	52.672781
3219.893521	766.459175	52.677786
3219.523833	713.758945	52.682791
3218.740800	676.922342	52.687796
3217.999777	620.109892	52.692801
3217.367330	570.543881	52.697805
3216.833527	544.898507	52.702810
3216.293115	490.813057	52.707815
3214.909327	449.111858	52.712820
3214.042065	405.003852	52.717825
3213.611918	370.436623	52.722829
3212.808528	334.989429	52.727834
3212.265041	298.616476	52.732839
3211.347665	270.981713	52.737844
3210.939881	242.464161	52.742849
3210.597404	212.438686	52.747853
3209.572677	193.324501	52.752858
3208.968698	172.037708	52.757863
3207.569486	160.305037	52.762868
3206.322963	143.402185	52.767873
3204.826516	137.753518	52.772877
3203.628831	143.502909	52.777882
3203.277823	139.947581	52.782887
3202.654971	145.493768	52.787892
3201.608041	139.389759	52.792897
3201.679159	138.880273	52.797901
3201.179321	146.079093	52.802906
3200.940806	142.682173	52.807911
3200.135105	138.841377	52.812916
3199.757646	137.571309	52.817921
3198.857963	138.942380	52.822925
3197.860298	138.716147	52.827930
3197.583558	139.961450	52.832935
3197.125712	142.369380	52.837940
3196.203479	141.918686	52.842945
3195.974571	144.176980	52.847949
3194.639640	146.307661	52.852954
3194.332628	136.726787	52.857959
3193.190722	146.529591	52.862964
3192.575562	141.121143	52.867969
3192.279322	132.330651	52.872973
3192.023520	137.057038	52.877978
3191.059401	134.281840	52.882983
3190.417960	140.027382	52.887988
3190.161847	137.896206	52.892993
3189.214451	138.470974	52.897997
3188.892650	137.788228	52.903002
3188.112203	132.741568	52.908007
3187.029473	134.400882	52.913012
3186.353066	140.520284	52.918017
3185.808999	140.496025	52.923021
3184.798005	138.569213	52.928026
3184.519501	135.346887	52.933031
3184.002288	140.423851	52.938036
3183.257470	136.002669	52.943041
3182.801312	137.860060	52.948045
3182.041263	138.275719	52.953050
3181.617958	140.539199	52.958055
3180.725320	145.046371	52.963060
3180.250416	144.848062	52.968065
3179.640146	137.630926	52.973069
3178.596678	143.410419	52.978074
3178.688724	142.621837	52.983079
3177.756304	142.094729	52.988084
3176.863620	136.434101	52.993089
3176.349515	138.462837	52.998093
3175.738279	138.102693	53.003098
3174.753371	143.486927	53.008103
3173.743130	142.458785	53.013108
3173.362128	144.678329	53.018113
3172.705601	140.948232	53.023117
3172.263980	143.134713	53.028122
3171.956221	141.744188	53.033127
3170.723837	149.700915	53.038132
3170.582545	142.741541	53.043137
3170.092930	140.757626	53.048141
3169.002403	145.582814	53.053146
3168.266805	134.282707	53.058151
3167.569994	139.645745	53.063156
3167.660585	135.842477	53.068161
3166.601858	133.394889	53.073165
3165.550274	132.025267	53.078170
3165.287350	132.606251	53.083175
3164.230713	138.089579	53.088180
3163.609276	132.066041	53.093185
3163.271214	127.085118	53.098189
3162.745739	133.361886	53.103194
3162.203055	133.457784	53.108199
3161.224623	139.557738	53.113204
3160.109088	138.036021	53.118209
3159.867313	130.204498	53.123213
3159.263583	140.704809	53.128218
3158.812824	125.994144	53.133223
3157.684848	130.311791	53.138228
3157.693086	131.057231	53.143233
3157.431796	128.362878	53.148237
3156.621114	136.899642	53.153242
3155.865858	128.249949	53.158247
3154.477565	131.657226	53.163252
3153.864985	128.386590	53.168257
3152.946121	127.696517	53.173261
3152.432304	130.033486	53.178266
3152.250312	129.048572	53.183271
3151.518621	137.661839	53.188276
3150.649215	129.489929	53.193281
3150.464255	128.444339	53.198285
3149.628676	138.419800	53.203290
3149.339384	131.094149	53.208295
3148.545003	129.967159	53.213300
3147.644583	136.879950	53.218305
3146.824122	130.157410	53.223309
3145.898643	135.955428	53.228314
3145.460732	125.607082	53.233319
3145.217219	133.467481	53.238324
3144.310352	132.090901	53.243329
3143.869495	124.418131	53.248333
3142.776658	134.263862	53.253338
3142.033279	127.573153	53.258343
3141.340039	132.388487	53.263348
3141.218132	127.526158	53.268353
3140.779634	131.765874	53.273357
3140.192413	130.044162	53.278362
3139.103919	126.498796	53.283367
3138.143142	129.963292	53.288372
3137.310137	130.417474	53.293377
3136.512633	125.461764	53.298381
3136.184145	132.435122	53.303386
3136.283837	128.013737	53.308391
3135.400985	136.245471	53.313396
3134.664362	130.109780	53.318401
3134.166642	129.629195	53.323405
3132.672202	136.752425	53.328410
3132.177637	124.983661	53.333415
3131.587468	130.373871	53.338420
3131.381961	128.235634	53.343425
3131.068664	122.791021	53.348429
3130.095193	135.450506	53.353434
3129.448291	119.797204	53.358439
3128.553960	125.107147	53.363444
3127.426748	126.736571	53.368449
3126.963627	125.003131	53.373453
3126.001490	127.524066	53.378458
3126.021836	118.228722	53.383463
3125.762561	126.226806	53.388468
3125.043678	123.887343	53.393473
3124.103961	123.561224	53.398477
3123.393416	129.446464	53.403482
3123.086400	123.788021	53.408487
3122.364121	118.628810	53.413492
3121.645488	121.140903	53.418497
3120.026797	129.201919	53.423501
3119.245629	132.339290	53.428506
3119.071655	121.369158	53.433511
3118.207243	122.787501	53.438516
3118.409115	121.843578	53.443521
3118.234891	122.817557	53.448525
3116.506279	131.830886	53.453530
3116.357270	128.643283	53.458535
3115.518920	135.704547	53.463540
3115.205577	123.364442	53.468545
3114.577090	124.837605	53.473549
3112.911852	132.501981	53.478554
3112.748744	128.367072	53.483559
3111.956972	125.627179	53.488564
3111.151998	129.704517	53.493569
3110.668633	116.194681	53.498573
3109.652517	121.633193	53.503578
3109.713818	110.215907	53.508583
3109.577915	118.610923	53.513588
3108.097417	129.807729	53.518593
3107.143932	123.753703	53.523597
3106.776417	126.251989	53.528602
3106.663489	115.636950	53.533607
3106.006743	120.554597	53.538612
3105.092108	110.373773	53.543617
3104.834785	114.153067	53.548621
3103.052337	127.229445	53.553626
3103.068171	110.436238	53.558631
3102.413150	114.712946	53.563636
3101.561786	118.620187	53.568641
3101.183038	111.608644	53.573645
3100.277517	122.991014	53.578650
3099.800206	115.985258	53.583655
3099.003397	115.092765	53.588660
3098.371119	120.922000	53.593665
3097.995442	112.034977	53.598669
3096.953800	119.443199	53.603674
3096.531277	111.024038	53.608679
3095.691294	113.195297	53.613684
3094.950325	116.964862	53.618689
3094.050155	115.235840	53.623693
3092.981150	126.515491	53.628698
3092.502852	112.400073	53.633703
3092.605786	121.274138	53.638708
3092.194951	120.239909	53.643713
3091.975611	115.022797	53.648717
3090.178339	124.191539	53.653722
3089.346124	114.959374	53.658727
3088.881933	120.032012	53.663732
3088.451338	122.730150	53.668737
3088.350281	118.572012	53.673741
3087.550968	115.193166	53.678746
3087.006024	114.792496	53.683751
3085.310197	117.861155	53.688756
3084.750848	123.337281	53.693761
3084.653985	119.340659	53.698765
3083.952279	119.700177	53.703770
3083.335746	113.957657	53.708775
3082.848766	120.686123	53.713780
3081.816179	118.077382	53.718785
3081.718724	120.678730	53.723789
3080.764486	125.892732	53.728794
3079.643685	119.034822	53.733799
3079.190600	120.016582	53.738804
3078.318070	117.551410	53.743809
3077.952369	116.404868	53.748813
3077.142570	122.302725	53.753818
3076.782139	109.266885	53.758823
3075.696812	118.550817	53.763828
3074.993307	117.612385	53.768833
3074.465373	107.938246	53.773837
3073.964113	116.958567	53.778842
3073.298919	114.650202	53.783847
3072.788973	119.575135	53.788852
3071.704495	116.044496	53.793857
3071.336045	114.849478	53.798861
3070.550974	111.489912	53.803866
3069.955315	110.331744	53.808871
3069.337013	112.872880	53.813876
3068.797591	116.231835	53.818881
3068.335368	107.322503	53.823885
3067.476641	115.116303	53.828890
3066.905446	112.076238	53.833895
3066.582961	112.079258	53.838900
3065.500987	118.159407	53.843905
3065.204472	106.986026	53.848909
3064.815936	112.957949	53.853914
3063.950583	101.342966	53.858919
3062.644265	109.663232	53.863924
3062.082616	113.022432	53.868929
3062.083086	111.691353	53.873933
3060.039913	114.638585	53.878938
3060.195615	111.429712	53.883943
3059.935507	113.329790	53.888948
3058.643127	120.110218	53.893953
3058.240514	112.586456	53.898957
3057.474685	120.204916	53.903962
3056.767462	109.857220	53.908967
3056.365190	119.734160	53.913972
3055.118495	106.663057	53.918977
3054.992257	106.004140	53.923981
3054.752547	113.315599	53.928986
3053.705463	116.775904	53.933991
3052.466425	111.504880	53.938996
3051.974789	108.307937	53.944001
3052.357783	111.899268	53.949005
3050.944188	115.014445	53.954010
3050.194386	109.464437	53.959015
3049.368161	117.790699	53.964020
3048.493135	112.306297	53.969025
3048.536587	115.697495	53.974029
3047.431508	114.114413	53.979034
3047.443274	112.437992	53.984039
3046.309947	121.589212	53.989044
3045.528409	112.051565	53.994049
3045.031779	110.748587	53.999053
3044.381065	113.023691	54.004058
3043.916475	108.602421	54.009063
3043.106998	108.848915	54.014068
3042.496765	114.921087	54.019073
3042.157793	108.706422	54.024077
3041.175946	113.874617	54.029082
3040.320155	111.537642	54.034087
3039.936217	122.013014	54.039092
3039.014326	118.572228	54.044097
3038.766064	112.006939	54.049101
3038.012805	116.648982	54.054106
3036.792314	118.428568	54.059111
3036.691243	113.680714	54.064116
3035.595842	114.954594	54.069121
3034.993928	109.596024	54.074125
3034.681561	114.372725	54.079130
3034.149851	114.328605	54.084135
3033.039428	122.918164	54.089140
3031.666415	122.224005	54.094145
3031.679502	112.847415	54.099149
3031.523492	112.061352	54.104154
3030.870004	122.512916	54.109159
3029.843373	117.317310	54.114164
3028.895940	120.739671	54.119169
3028.637860	113.767912	54.124173
3027.652993	117.753234	54.129178
3027.118444	111.783562	54.134183
3026.456344	110.235314	54.139188
3026.139339	114.246643	54.144193
3025.894353	106.324121	54.149197
3025.048573	121.966439	54.154202
3024.614008	105.333107	54.159207
3022.843187	104.979288	54.164212
3022.389521	111.107204	54.169217
3022.561511	104.175248	54.174221
3021.118212	113.063651	54.179226
3020.206601	104.924654	54.184231
3019.874237	109.267018	54.189236
3019.251843	114.013408	54.194241
3018.526390	109.845132	54.199245
3017.598182	109.290491	54.204250
3017.723705	109.107226	54.209255
3017.018161	118.084298	54.214260
3016.046280	117.458570	54.219265
3015.681409	113.114207	54.224269
3014.787865	118.497443	54.229274
3014.327098	110.507585	54.234279
3013.891101	114.962788	54.239284
3012.865223	115.432971	54.244289
3012.146108	113.093171	54.249293
3011.258213	121.662469	54.254298
3010.300540	111.759807	54.259303
3010.030426	111.827695	54.264308
3009.207238	109.131085	54.269313
3008.788127	107.226721	54.274317
3007.825363	116.288403	54.279322
3007.657491	110.877773	54.284327
3006.685740	111.264104	54.289332
3005.752937	114.826857	54.294337
3006.095255	104.871793	54.299341
3005.167745	118.160502	54.304346
3004.746146	111.573522	54.309351
3004.469641	108.965465	54.314356
3002.377242	120.012240	54.319361
3001.502081	114.888650	54.324365
3001.190000	119.799511	54.329370
3001.268422	115.276771	54.334375
3000.139683	122.273187	54.339380
2999.081212	115.428727	54.344385
2999.137598	106.692888	54.349389
2998.009867	112.018249	54.354394
2997.464689	119.019942	54.359399
2996.799742	114.775804	54.364404
2996.100980	117.659109	54.369409
2995.890187	113.002637	54.374413
2995.174646	108.923458	54.379418
2994.540033	111.140554	54.384423
2994.004743	110.500223	54.389428
2993.576455	111.806557	54.394433
2992.185476	113.196873	54.399437
2991.168427	113.644630	54.404442
2990.506293	113.471226	54.409447
2990.680260	110.665012	54.414452
2989.618572	116.910646	54.419457
2989.121458	109.067921	54.424461
2988.033918	113.642751	54.429466
2987.679684	111.653488	54.434471
2987.153681	105.596709	54.439476
2986.719716	117.317698	54.444481
2986.256980	110.945771	54.449485
2985.395549	116.865482	54.454490
2984.588185	120.135232	54.459495
2983.470461	108.308004	54.464500
2982.618686	114.588818	54.469505
2981.987126	113.055488	54.474509
2981.390067	115.889836	54.479514
2981.364994	111.269523	54.484519
2980.461074	107.545030	54.489524
2979.395841	117.943796	54.494529
2979.352310	104.995534	54.499533
2978.553561	109.246285	54.504538
2978.015134	110.333026	54.509543
2977.445364	110.736720	54.514548
2976.926716	106.923892	54.519553
2976.193841	105.939574	54.524557
2974.918349	113.513289	54.529562
2974.269185	105.814969	54.534567
2973.545777	109.705486	54.539572
2972.785947	113.775514	54.544577
2972.300937	99.375896	54.549581
2971.920945	108.789557	54.554586
2971.191503	119.882898	54.559591
2970.701427	110.724532	54.564596
2970.171698	110.382850	54.569601
2969.883494	104.742137	54.574605
2969.112005	111.201069	54.579610
2967.754014	108.765193	54.584615
2967.374304	109.627450	54.589620
2966.390585	107.129196	54.594625
2966.076005	105.820774	54.599629
2965.309892	110.340284	54.604634
2964.676170	110.376759	54.609639
2964.444327	109.024594	54.614644
2963.063003	113.347270	54.619649
2962.445932	106.555681	54.624653
2961.338721	111.540049	54.629658
2961.699544	114.930297	54.634663
2960.836110	109.076048	54.639668
2959.697078	120.950681	54.644673
2959.541618	107.051308	54.649677
2958.777973	115.845289	54.654682
2958.247777	111.214587	54.659687
2957.617293	114.516874	54.664692
2956.936839	109.725145	54.669697
2955.982630	104.253901	54.674701
2954.669618	118.915429	54.679706
2954.394257	111.100733	54.684711
2954.503045	114.569181	54.689716
2953.572037	115.622751	54.694721
2952.939659	109.774412	54.699725
2951.902118	115.217391	54.704730
2951.530500	107.771638	54.709735
2951.512428	108.171843	54.714740
2950.014702	116.667728	54.719745
2949.425911	111.841783	54.724749
2948.276667	113.090144	54.729754
2947.721179	112.977466	54.734759
2947.256211	109.964657	54.739764
2946.541631	113.160529	54.744769
2946.178676	105.295677	54.749773
2945.436579	113.901242	54.754778
2945.007064	109.904242	54.759783
2944.655397	111.790760	54.764788
2943.803199	119.617796	54.769793
2943.402287	104.995787	54.774797
2942.275637	110.467809	54.779802
2941.326020	104.819736	54.784807
2940.925925	105.076415	54.789812
2940.002994	110.262577	54.794817
2939.729941	102.562754	54.799821
2939.239065	110.683293	54.804826
2938.672946	102.470277	54.809831
2937.601632	98.341385	54.814836
2936.547719	102.351935	54.819841
2936.137593	94.391338	54.824845
2935.513443	103.824614	54.829850
2935.059556	112.379742	54.834855
2934.577009	102.203680	54.839860
2933.898969	110.309231	54.844865
2933.556040	114.771032	54.849869
2931.905818	105.900142	54.854874
2931.376757	101.776082	54.859879
2930.552419	107.180258	54.864884
2930.019207	109.839098	54.869889
2929.845688	105.440731	54.874893
2928.972843	108.038008	54.879898
2928.686946	101.272726	54.884903
2928.239358	92.173037	54.889908
2926.857752	106.582995	54.894913
2926.142020	98.130689	54.899917
2925.161797	106.269327	54.904922
2924.559650	103.731927	54.909927
2924.854903	98.816885	54.914932
2923.993772	105.340477	54.919937
2923.624196	99.599206	54.924941
2922.760582	104.359190	54.929946
2921.743762	107.121990	54.934951
2920.593106	107.989686	54.939956
2919.821124	112.069294	54.944961
2920.063908	106.591653	54.949965
2919.410549	110.081793	54.954970
2918.304416	105.013484	54.959975
2917.975439	104.972229	54.964980
2917.050909	112.580709	54.969985
2916.866925	98.999639	54.974989
2916.259492	104.835683	54.979994
2914.638781	108.416929	54.984999
2914.264938	107.541389	54.990004
2913.613323	112.160940	54.995009
2913.535612	107.260687	55.000013
2912.642321	108.569521	55.005018
2911.854122	106.681664	55.010023
2911.686893	101.563823	55.015028
2910.329380	111.697547	55.020033
2909.632189	98.510491	55.025037
2909.081122	104.229142	55.030042
2908.765636	111.591043	55.035047
2908.424768	102.420616	55.040052
2907.177753	106.396278	55.045057
2907.088343	101.981566	55.050061
2905.593983	104.424935	55.055066
2904.542534	106.915373	55.060071
2904.294274	109.883534	55.065076
2903.873879	102.780459	55.070081
2903.325051	105.294340	55.075085
2902.517034	97.697394	55.080090
2902.150755	103.130657	55.085095
2901.754716	102.406539	55.090100
2901.109637	100.438964	55.095105
2900.025201	104.626836	55.100109
2898.996566	110.175269	55.105114
2898.176921	95.497343	55.110119
2897.622444	99.761221	55.115124
2897.024838	110.807158	55.120129
2896.457636	100.681492	55.125133
2895.866604	102.259979	55.130138
2895.703899	109.505772	55.135143
2894.874069	110.768238	55.140148
2894.524028	118.298280	55.145153
2893.796970	103.597815	55.150157
2892.941756	101.685889	55.155162
2891.962992	106.726075	55.160167
2891.312020	102.674169	55.165172
2890.549382	109.202642	55.170177
2890.581706	102.880336	55.175181
2889.331031	109.646552	55.180186
2888.214990	99.187591	55.185191
2887.847089	105.814782	55.190196
2887.207356	100.697170	55.195201
2886.749710	99.010978	55.200205
2885.945161	107.901549	55.205210
2885.610731	103.027410	55.210215
2885.369103	99.724606	55.215220
2884.495950	115.776187	55.220225
2883.406974	102.905952	55.225229
2882.502072	103.632185	55.230234
2881.608413	106.201842	55.235239
2881.352595	104.884961	55.240244
2880.561423	108.831671	55.245249
2880.356226	96.212631	55.250253
2879.586529	105.368422	55.255258
2879.023734	97.587867	55.260263
2878.643049	95.633135	55.265268
2877.503635	109.293570	55.270273
2876.713408	102.559222	55.275277
2876.103675	113.044353	55.280282
2875.578579	106.394953	55.285287
2875.118224	107.715064	55.290292
2874.480898	107.635326	55.295297
2874.217238	100.972432	55.300301
2872.930487	106.598530	55.305306
2871.936222	109.899442	55.310311
2871.667809	104.587322	55.315316
2870.871036	111.061238	55.320321
2870.497936	100.402287	55.325325
2870.066825	99.887845	55.330330
2868.965185	101.610834	55.335335
2868.291029	89.696404	55.340340
2867.135984	106.473106	55.345345
2866.556561	90.759825	55.350349
2865.788392	104.350889	55.355354
2865.259103	99.217563	55.360359
2865.491848	99.576876	55.365364
2864.900325	107.898162	55.370369
2864.325699	100.541592	55.375373
2862.960944	105.875900	55.380378
2862.286688	100.327230	55.385383
2862.002898	97.351362	55.390388
2861.229583	93.878515	55.395393
2860.558258	91.866486	55.400397
2859.216057	94.298859	55.405402
2858.389452	99.529352	55.410407
2858.464604	104.432053	55.415412
2857.609769	109.012918	55.420417
2857.120184	93.852294	55.425421
2856.342262	96.901895	55.430426
2856.093509	106.076021	55.435431
2855.598499	110.690126	55.440436
2854.632408	115.351584	55.445441
2853.843640	106.060742	55.450445
2852.840804	117.452247	55.455450
2852.302486	104.257391	55.460455
2851.527738	105.129143	55.465460
2851.383321	110.905796	55.470465
2850.837614	98.016148	55.475469
2850.012284	102.507103	55.480474
2848.703688	100.648196	55.485479
2848.206048	95.612884	55.490484
2847.323507	105.643727	55.495489
2847.128638	100.040366	55.500493
2846.746998	101.251897	55.505498
2846.147162	96.881400	55.510503
2845.899853	95.916743	55.515508
2844.895878	107.795528	55.520513
2843.935996	101.340834	55.525517
2843.386951	102.484662	55.530522
2842.494291	97.141477	55.535527
2842.264396	89.805734	55.540532
2840.657123	100.789360	55.545537
2839.860840	96.626513	55.550541
2839.751955	110.219770	55.555546
2838.940872	102.790724	55.560551
2838.645001	100.606374	55.565556
2838.270008	103.645140	55.570561
2838.005705	95.592927	55.575565
2837.244017	103.109632	55.580570
2835.761801	108.940455	55.585575
2835.047418	103.018525	55.590580
2834.060697	109.492145	55.595585
2834.417119	94.149043	55.600589
2833.464089	96.093737	55.605594
2832.964887	99.826738	55.610599
2831.780456	99.966428	55.615604
2831.007578	108.374366	55.620609
2830.431973	106.394136	55.625613
2829.738825	103.618887	55.630618
2829.496508	98.863220	55.635623
2828.910478	104.553113	55.640628
2828.153119	104.587840	55.645633
2827.978528	102.278555	55.650637
2826.559229	108.024812	55.655642
2825.357223	107.043722	55.660647
2825.210316	104.262350	55.665652
2824.623357	109.102954	55.670657
2824.354506	101.463611	55.675661
2823.985081	111.231899	55.680666
2823.167318	103.615713	55.685671
2822.394746	95.672475	55.690676
2821.107252	106.030681	55.695681
2820.899824	87.946269	55.700685
2820.279224	97.431434	55.705690
2819.517964	104.240719	55.710695
2818.589147	101.482461	55.715700
2817.748828	108.562227	55.720705
2817.254619	103.489620	55.725709
2816.993507	100.240677	55.730714
2816.277820	107.295193	55.735719
2815.948635	99.047629	55.740724
2814.912486	101.038110	55.745729
2814.353255	99.037717	55.750733
2812.904197	108.556721	55.755738
2811.900199	100.072000	55.760743
2812.080689	100.317482	55.765748
2811.368027	104.766686	55.770753
2811.141154	101.038220	55.775757
2810.547655	103.655660	55.780762
2810.145851	102.516889	55.785767
2809.094568	95.936910	55.790772
2808.110080	101.177419	55.795777
2807.475624	105.861539	55.800781
2806.969562	102.038294	55.805786
2806.297188	102.875187	55.810791
2806.067528	100.614788	55.815796
2805.151915	98.924378	55.820801
2804.017145	89.119159	55.825805
2803.486997	85.706207	55.830810
2802.439559	95.143932	55.835815
2802.316361	95.655259	55.840820
2801.617804	100.901371	55.845825
2801.430611	90.079617	55.850829
2800.319457	92.982104	55.855834
2799.251471	94.879742	55.860839
2799.042384	99.672734	55.865844
2798.426602	98.871316	55.870849
2798.245488	95.915799	55.875853
2797.866385	94.241849	55.880858
2796.290225	96.848825	55.885863
2795.919926	91.760178	55.890868
2795.064107	98.894299	55.895873
2793.903977	93.294085	55.900877
2792.991462	104.557255	55.905882
2793.091090	99.002642	55.910887
2792.590904	91.049173	55.915892
2791.150317	97.569970	55.920897
2790.769208	90.176001	55.925901
2790.385211	94.801523	55.930906
2789.503882	93.795632	55.935911
2789.511284	81.313174	55.940916
2788.685997	94.747416	55.945921
2788.135914	97.213362	55.950925
2786.954441	101.412309	55.955930
2786.472875	102.667763	55.960935
2786.200539	86.733474	55.965940
2785.571988	104.527788	55.970945
2784.622410	99.977478	55.975949
2783.579404	94.724343	55.980954
2782.617867	104.730402	55.985959
2782.472961	90.838352	55.990964
2781.524615	99.077335	55.995969
2781.588797	91.613575	56.000973
2781.071419	96.421364	56.005978
2779.900018	99.408361	56.010983
2778.890622	98.386072	56.015988
2778.411171	99.718926	56.020993
2777.862736	97.130130	56.025997
2777.107391	100.917571	56.031002
2776.909697	94.336572	56.036007
2775.967066	98.021816	56.041012
2774.795842	95.745513	56.046017
2774.187196	94.329081	56.051021
2773.805264	93.435594	56.056026
2773.113199	98.918618	56.061031
2772.998331	105.044284	56.066036
2772.328998	100.476077	56.071041
2771.314763	95.951822	56.076045
2770.237399	99.292606	56.081050
2769.426395	102.101957	56.086055
2769.210214	94.117316	56.091060
2768.634748	99.031348	56.096065
2768.270704	91.862221	56.101069
2767.882395	96.908469	56.106074
2766.669033	93.197439	56.111079
2766.075416	95.385046	56.116084
2765.070274	103.471114	56.121089
2764.989129	95.576284	56.126093
2764.376629	104.597055	56.131098
2762.795877	102.053655	56.136103
2762.471291	94.942519	56.141108
2761.491902	98.990090	56.146113
2761.410210	94.853537	56.151117
2760.848120	94.655561	56.156122
2760.044364	93.370372	56.161127
2760.160395	93.013466	56.166132
2758.774257	99.657591	56.171137
2758.139684	91.918934	56.176141
2757.692280	92.080687	56.181146
2756.888470	94.473558	56.186151
2756.378299	93.175688	56.191156
2755.103749	96.282554	56.196161
2754.556570	94.816540	56.201165
2753.715050	86.086183	56.206170
2753.274364	93.316712	56.211175
2753.230108	94.727942	56.216180
2752.669886	90.923043	56.221185
2751.483685	89.443889	56.226189
2750.576118	88.956816	56.231194
2749.747004	96.569913	56.236199
2749.440885	97.114875	56.241204
2749.162978	97.830273	56.246209
2748.380271	95.286261	56.251213
2747.157190	90.878628	56.256218
2746.400135	91.422905	56.261223
2746.124354	89.573804	56.266228
2745.112600	99.217008	56.271233
2744.974220	92.712320	56.276237
2744.523208	94.160311	56.281242
2744.004423	92.959439	56.286247
2743.279977	89.954693	56.291252
2742.345412	94.994838	56.296257
2741.575551	90.909992	56.301261
2741.146011	90.560287	56.306266
2740.116606	91.712415	56.311271
2739.104750	78.963273	56.316276
2738.251972	84.141799	56.321281
2738.157317	84.056161	56.326285
2737.587251	84.666764	56.331290
2736.731464	88.562555	56.336295
2736.626059	86.721833	56.341300
2736.221976	89.267823	56.346305
2734.820760	86.668485	56.351309
2734.175018	97.760137	56.356314
2733.127368	93.613434	56.361319
2733.123009	88.223044	56.366324
2732.180676	86.250251	56.371329
2732.157127	90.753375	56.376333
2731.079910	86.885668	56.381338
2729.892100	98.122077	56.386343
2729.731601	94.100046	56.391348
2728.709330	96.888277	56.396353
2728.358421	98.214557	56.401357
2727.860019	100.003799	56.406362
2727.058541	93.523639	56.411367
2726.792957	90.083633	56.416372
2725.898327	91.138124	56.421377
2724.909999	92.915978	56.426381
2724.630494	85.540179	56.431386
2724.042617	89.627803	56.436391
2722.980961	84.355770	56.441396
2721.910435	93.670345	56.446401
2721.497191	86.573977	56.451405
2720.727477	86.456493	56.456410
2720.597816	90.823812	56.461415
2720.710042	82.055571	56.466420
2719.402370	98.155744	56.471425
2718.463686	85.554749	56.476429
2717.591343	82.968830	56.481434
2716.975476	87.075053	56.486439
2716.675516	87.467784	56.491444
2715.869761	87.862894	56.496449
2714.969255	92.370261	56.501453
2714.053063	90.581681	56.506458
2713.195453	90.244755	56.511463
2713.141976	85.649451	56.516468
2712.333075	85.144336	56.521473
2712.189318	91.049149	56.526477
2711.928346	85.526971	56.531482
2710.302596	90.859336	56.536487
2710.004045	85.394107	56.541492
2708.973686	89.541971	56.546497
2709.020544	82.938918	56.551501
2708.230514	82.960694	56.556506
2707.142193	85.390754	56.561511
2706.380048	80.716853	56.566516
2705.995893	82.257231	56.571521
2705.331377	81.954799	56.576525
2705.000000	84.956111	56.581530
2703.441384	96.086566	56.586535
2702.880706	89.289340	56.591540
2702.039814	87.425525	56.596545
2701.650669	89.063465	56.601549
2701.180309	79.997320	56.606554
2700.607321	86.335884	56.611559
2700.422674	89.036203	56.616564
2699.956617	91.983172	56.621569
2698.655426	93.435177	56.626573
2698.011874	89.361906	56.631578
2697.211513	100.716035	56.636583
2696.830160	87.148226	56.641588
2696.193771	84.418955	56.646593
2694.960471	87.217604	56.651597
2694.776522	87.893260	56.656602
2693.745396	90.075527	56.661607
2693.350533	91.462610	56.666612
2692.937098	90.762404	56.671617
2692.451626	81.873706	56.676621
2691.125319	84.403657	56.681626
2690.097387	95.426034	56.686631
2689.948983	90.519334	56.691636
2688.996353	88.702252	56.696641
2688.572595	89.680602	56.701645
2688.399878	75.460582	56.706650
2687.944892	85.078873	56.711655
2687.243178	85.001479	56.716660
2686.051518	89.311519	56.721665
2685.312918	83.705598	56.726669
2685.200210	88.584343	56.731674
2684.069140	90.165162	56.736679
2683.332432	80.729298	56.741684
2682.584100	90.694963	56.746689
2681.952776	88.813092	56.751693
2681.286781	80.964566	56.756698
2681.010658	90.824647	56.761703
2680.794384	84.270916	56.766708
2679.694174	92.271792	56.771713
2678.518366	87.747944	56.776717
2678.415317	76.698683	56.781722
2677.311319	91.596441	56.786727
2677.068992	84.223373	56.791732
2676.156002	88.580514	56.796737
2675.128265	78.464160	56.801741
2674.863818	74.871998	56.806746
2674.333081	83.286301	56.811751
2674.026426	76.209619	56.816756
2673.120094	85.937824	56.821761
2671.885878	90.995250	56.826765
2671.271391	77.305864	56.831770
2670.735112	89.906777	56.836775
2670.591577	84.308085	56.841780
2669.960689	88.487140	56.846785
2669.098907	85.667721	56.851789
2668.260809	81.581529	56.856794
2666.851562	91.730825	56.861799
2667.064845	91.159143	56.866804
2666.468882	88.587170	56.871809
2665.899563	85.946699	56.876813
2665.106887	79.681363	56.881818
2663.815302	82.206173	56.886823
2663.709972	68.289241	56.891828
2662.632685	71.115303	56.896833
2662.317884	77.872347	56.901837
2662.206393	74.753367	56.906842
2661.303159	80.032495	56.911847
2660.413450	79.938689	56.916852
2659.559272	91.335562	56.921857
2658.978711	74.074439	56.926861
2658.641340	78.152005	56.931866
2657.625156	89.182635	56.936871
2657.308511	73.396484	56.941876
2656.266608	87.984819	56.946881
2655.884886	85.823845	56.951885
2655.642728	81.973276	56.956890
2654.326433	90.186743	56.961895
2653.397648	81.915395	56.966900
2653.057154	89.440629	56.971905
2652.414708	83.595258	56.976909
2651.966354	81.179236	56.981914
2651.091479	86.133397	56.986919
2650.342363	78.302641	56.991924
2649.741181	79.816569	56.996929
2649.151894	88.982571	57.001933
2649.066737	85.132400	57.006938
2647.790876	87.230197	57.011943
2646.951491	87.995395	57.016948
2646.541995	90.412845	57.021953
2646.022108	84.942039	57.026957
2645.618314	91.233132	57.031962
2643.902984	97.628821	57.036967
2643.080113	89.645673	57.041972
2643.073514	88.465807	57.046977
2642.686110	88.456660	57.051981
2642.114590	82.920079	57.056986
2641.423836	88.423408	57.061991
2641.058733	81.437243	57.066996
2639.725619	84.576639	57.072001
2638.999413	83.205978	57.077005
2638.277403	87.179171	57.082010
2637.608019	84.367920	57.087015
2637.503968	81.047148	57.092020
2636.519377	84.668135	57.097025
2635.602655	83.108601	57.102029
2634.767588	85.046974	57.107034
2634.248884	91.152848	57.112039
2633.768800	85.374854	57.117044
2633.535733	80.951566	57.122049
2632.815565	81.840067	57.127053
2632.594078	73.519661	57.132058
2631.377685	82.831147	57.137063
2630.726902	81.117604	57.142068
2630.096563	83.686486	57.147073
2629.404578	81.859202	57.152077
2628.824063	77.663462	57.157082
2627.382773	85.134112	57.162087
2627.386814	82.456026	57.167092
2626.630069	89.249150	57.172097
2626.196189	84.487570	57.177101
2625.977710	82.507108	57.182106
2624.558736	88.688327	57.187111
2623.744627	80.388701	57.192116
2623.061409	81.883104	57.197121
2622.714088	86.021977	57.202125
2622.879632	85.089780	57.207130
2621.416400	87.045540	57.212135
2620.717083	80.616232	57.217140
2620.216787	87.155129	57.222145
2619.473230	89.603634	57.227149
2619.088880	77.565921	57.232154
2618.104286	84.094845	57.237159
2617.088722	80.372543	57.242164
2616.037104	80.762328	57.247169
2615.476663	89.425257	57.252173
2615.439168	77.390618	57.257178
2614.903296	92.203891	57.262183
2614.443136	84.090856	57.267188
2613.670116	92.225670	57.272193
2612.159558	94.191496	57.277197
2611.980804	80.128829	57.282202
2611.204509	89.342588	57.287207
2610.923075	86.279896	57.292212
2610.462390	88.722282	57.297217
2609.995613	88.050147	57.302221
2609.086962	86.311218	57.307226
2608.038810	91.425266	57.312231
2607.653343	82.088844	57.317236
2607.387860	85.730189	57.322241
2606.133011	84.997781	57.327245
2605.379551	83.201139	57.332250
2604.625255	90.311600	57.337255
2603.996285	84.761556	57.342260
2603.600685	81.855746	57.347265
2603.073671	88.009223	57.352269
2602.415298	82.345395	57.357274
2601.092851	93.442596	57.362279
2600.909185	86.513442	57.367284
2600.558290	87.681046	57.372289
2600.025664	87.731069	57.377293
2599.393948	86.364391	57.382298
2598.053751	95.146411	57.387303
2597.340904	83.031438	57.392308
2596.798874	84.834066	57.397313
2596.469017	93.446921	57.402317
2595.658546	85.499955	57.407322
2594.356254	84.483169	57.412327
2593.922203	81.554329	57.417332
2593.346959	88.702862	57.422337
2592.698568	90.380388	57.427341
2592.607637	81.837539	57.432346
2592.195125	87.211203	57.437351
2591.830167	86.482587	57.442356
2590.777263	85.294488	57.447361
2589.727370	86.536588	57.452365
2588.754193	72.094625	57.457370
2587.735321	79.627667	57.462375
2587.020599	76.746415	57.467380
2587.218785	82.671709	57.472385
2586.796982	85.737034	57.477389
2586.245953	76.692598	57.482394
2585.358171	87.845355	57.487399
2584.157089	83.339668	57.492404
2583.366633	79.419028	57.497409
2582.782313	90.783585	57.502413
2582.582846	85.895492	57.507418
2582.158627	91.336289	57.512423
2581.588658	78.038381	57.517428
2580.173321	81.475651	57.522433
2579.212133	82.564041	57.527437
2578.509891	78.036629	57.532442
2578.490845	87.437504	57.537447
2578.110414	75.434261	57.542452
2577.573937	82.061050	57.547457
2576.255313	86.159530	57.552461
2575.829506	88.179521	57.557466
2574.792541	81.814259	57.562471
2574.271887	78.286036	57.567476
2574.323835	82.117054	57.572481
2573.649719	86.975327	57.577485
2572.623548	83.275767	57.582490
2571.602814	93.433263	57.587495
2571.029121	80.629399	57.592500
2570.547205	85.499023	57.597505
2570.155364	78.303105	57.602509
2569.123925	76.277685	57.607514
2568.130030	88.188296	57.612519
2567.767763	73.707820	57.617524
2567.570791	76.757996	57.622529
2567.022277	85.750058	57.627533
2566.524445	80.319704	57.632538
2565.158113	86.819950	57.637543
2564.492930	76.079562	57.642548
2563.901402	82.859047	57.647553
2563.298076	82.182236	57.652557
2562.651698	83.399172	57.657562
2561.683042	89.437500	57.662567
2561.056057	73.622718	57.667572
2560.241264	81.547572	57.672577
2559.870313	87.067679	57.677581
2560.177545	77.303778	57.682586
2558.864663	84.573677	57.687591
2557.903116	85.229119	57.692596
2557.296424	83.833696	57.697601
2556.421065	85.621077	57.702605
2556.448711	80.629822	57.707610
2555.173017	83.725077	57.712615
2554.489820	89.451324	57.717620
2553.874833	84.400988	57.722625
2553.650058	78.603834	57.727629
2553.273848	80.093916	57.732634
2551.885418	87.250816	57.737639
2551.358111	77.332358	57.742644
2550.279834	76.109924	57.747649
2550.142940	89.981458	57.752653
2550.194830	84.471336	57.757658
2548.851338	82.197303	57.762663
2548.157036	72.303846	57.767668
2547.768318	89.513587	57.772673
2546.534517	82.973174	57.777677
2545.695516	76.677496	57.782682
2545.008841	79.117072	57.787687
2544.414732	75.931795	57.792692
2544.223565	84.675666	57.797697
2543.401575	83.473362	57.802701
2543.118527	76.024779	57.807706
2542.385001	73.142013	57.812711
2541.948241	79.691361	57.817716
2540.935824	76.032484	57.822721
2540.336692	77.390945	57.827725
2539.666781	77.518521	57.832730
2538.678290	77.735297	57.837735
2537.568318	74.627555	57.842740
2537.160612	77.931647	57.847745
2536.215832	79.002633	57.852749
2535.715444	81.949951	57.857754
2535.546152	84.194107	57.862759
2535.013753	83.520963	57.867764
2534.801545	82.912679	57.872769
2534.021295	74.064938	57.877773
2533.409814	73.220188	57.882778
2533.166963	76.499254	57.887783
2531.545807	73.730740	57.892788
2530.719746	74.883664	57.897793
2530.158914	82.399588	57.902797
2529.828229	62.234837	57.907802
2528.810031	82.531558	57.912807
2527.929779	75.039818	57.917812
2527.310558	75.721606	57.922817
2526.369758	81.551889	57.927821
2526.236682	70.828304	57.932826
2525.312807	79.438101	57.937831
2524.797316	71.863872	57.942836
2524.693342	82.321724	57.947841
2524.030027	82.928947	57.952845
2523.152115	77.284906	57.957850
2521.623358	85.326694	57.962855
2521.703596	82.318621	57.967860
2521.092854	78.627391	57.972865
2520.643247	85.392484	57.977869
2520.102071	85.578182	57.982874
2518.808966	84.403532	57.987879
2518.502519	73.495251	57.992884
2517.895290	84.466627	57.997889
2517.094813	85.426106	58.002893
2516.164471	82.467652	58.007898
2515.120706	79.262152	58.012903
2514.705232	77.521027	58.017908
2514.595851	79.779413	58.022913
2514.226090	76.322503	58.027917
2513.751053	78.939051	58.032922
2512.255612	81.104020	58.037927
2511.710225	78.126332	58.042932
2511.356505	71.317054	58.047937
2510.448443	79.943096	58.052941
2509.590775	70.671244	58.057946
2508.425106	67.131732	58.062951
2507.994498	75.678118	58.067956
2507.714240	79.344094	58.072961
2507.103065	82.708236	58.077965
2506.917095	75.837910	58.082970
2506.491825	79.225135	58.087975
2505.561889	75.567164	58.092980
2504.639059	75.438389	58.097985
2503.931600	81.827973	58.102989
2503.476030	66.190350	58.107994
2501.755227	76.455291	58.112999
2501.116626	76.592123	58.118004
2500.933362	69.690550	58.123009
2500.099901	74.947896	58.128013
2500.087165	74.470506	58.133018
2499.507558	74.200160	58.138023
2499.144083	77.660501	58.143028
2498.154112	78.648038	58.148033
2497.052137	80.664428	58.153037
2496.680325	74.033502	58.158042
2496.096977	77.823530	58.163047
2495.628072	78.199368	58.168052
2494.472310	78.284491	58.173057
2493.800574	73.464127	58.178061
2493.199303	65.785366	58.183066
2492.952381	74.497708	58.188071
2492.128352	70.711902	58.193076
2491.147522	69.592815	58.198081
2490.429082	70.940495	58.203085
2490.538024	73.611539	58.208090
2488.708346	76.116674	58.213095
2488.385138	76.067747	58.218100
2487.685888	72.706251	58.223105
2487.069432	77.187575	58.228109
2486.621266	73.283430	58.233114
2486.243598	71.985831	58.238119
2485.499399	73.266076	58.243124
2485.270709	80.341937	58.248129
2484.159962	75.143884	58.253133
2483.707208	72.195756	58.258138
2482.875762	71.752949	58.263143
2481.619193	74.854421	58.268148
2481.049818	68.093861	58.273153
2480.320464	78.081146	58.278157
2479.633018	71.326956	58.283162
2479.411773	79.147966	58.288167
2479.087386	79.122136	58.293172
2478.727377	76.576558	58.298177
2477.437458	78.302200	58.303181
2476.988653	75.888643	58.308186
2476.130789	73.959483	58.313191
2475.683798	68.477430	58.318196
2474.619381	76.442202	58.323201
2473.529143	85.227682	58.328205
2473.297193	74.700605	58.333210
2472.502159	71.265096	58.338215
2472.271344	76.877684	58.343220
2471.796925	73.844843	58.348225
2471.111646	79.113962	58.353229
2470.227166	69.989989	58.358234
2469.443585	72.919809	58.363239
2468.662665	73.283865	58.368244
2468.413032	72.676063	58.373249
2467.705698	80.862014	58.378253
2466.518387	75.923362	58.383258
2466.010215	78.440187	58.388263
2465.561877	76.820340	58.393268
2465.221406	69.708419	58.398273
2464.494955	75.712447	58.403277
2463.546750	78.293059	58.408282
2462.430997	73.888867	58.413287
2462.061289	75.860983	58.418292
2461.854107	75.551044	58.423297
2460.975147	79.555427	58.428301
2460.045710	71.417663	58.433306
2458.848056	76.054804	58.438311
2458.480930	71.851027	58.443316
2458.151260	68.358850	58.448321
2457.606631	75.180447	58.453325
2457.942236	74.288644	58.458330
2456.883179	75.254448	58.463335
2455.739817	66.156981	58.468340
2455.686941	63.847833	58.473345
2454.541797	73.855681	58.478349
2453.658973	68.993655	58.483354
2452.781245	69.727148	58.488359
2452.234323	77.446739	58.493364
2451.987947	72.424977	58.498369
2450.701298	77.421139	58.503373
2449.940337	63.077942	58.508378
2449.406008	80.946878	58.513383
2448.857637	62.960349	58.518388
2448.651833	74.055313	58.523393
2448.081480	74.120485	58.528397
2447.395350	69.119834	58.533402
2446.074986	75.093570	58.538407
2445.400772	73.636289	58.543412
2444.897357	68.867284	58.548417
2444.422260	79.624229	58.553421
2444.056927	67.878166	58.558426
2443.057277	81.526545	58.563431
2442.095418	76.227259	58.568436
2441.638386	73.907477	58.573441
2441.070246	86.231598	58.578445
2440.939547	73.622415	58.583450
2439.272198	79.861527	58.588455
2438.652557	73.496395	58.593460
2437.953583	75.348763	58.598465
2437.389124	81.463645	58.603469
2437.142679	66.350396	58.608474
2436.764418	74.699942	58.613479
2436.337390	80.010563	58.618484
2435.982793	73.444989	58.623489
2434.571205	78.989473	58.628493
2434.114152	79.000143	58.633498
2433.224250	76.403859	58.638503
2432.315927	77.217979	58.643508
2431.447132	75.275301	58.648513
2431.064003	75.437143	58.653517
2430.665804	65.000476	58.658522
2430.115018	75.424581	58.663527
2429.428928	76.953047	58.668532
2429.166132	66.181397	58.673537
2428.193937	71.130506	58.678541
2426.796443	66.118073	58.683546
2426.151425	75.056762	58.688551
2425.576483	70.815894	58.693556
2425.131134	64.162030	58.698561
2424.352073	73.992028	58.703565
2424.174354	69.837580	58.708570
2423.868420	72.666789	58.713575
2422.577579	77.971163	58.718580
2421.475636	75.075622	58.723585
2420.790342	73.011180	58.728589
2420.482796	78.290714	58.733594
2420.202120	68.499851	58.738599
2420.150867	78.028575	58.743604
2419.342304	69.460037	58.748609
2417.943502	81.133577	58.753613
2417.562812	72.772528	58.758618
2416.065346	67.616538	58.763623
2415.423330	76.604450	58.768628
2414.797219	63.284224	58.773633
2414.148020	71.639831	58.778637
2414.524641	61.717246	58.783642
2413.687220	72.079046	58.788647
2413.276405	75.945760	58.793652
2412.633272	66.843299	58.798657
2411.089693	78.872765	58.803661
2410.820291	76.038947	58.808666
2410.380219	76.209343	58.813671
2408.939300	75.361958	58.818676
2408.259550	68.859881	58.823681
2407.584535	68.980056	58.828685
2407.304656	67.910471	58.833690
2406.581407	79.940986	58.838695
2406.349632	73.494148	58.843700
2405.945573	67.472283	58.848705
2404.808723	77.854891	58.853709
2403.977960	77.382376	58.858714
2403.699583	69.014495	58.863719
2402.739142	66.736190	58.868724
2402.485895	74.168337	58.873729
2401.350462	71.563913	58.878733
2400.698492	65.038536	58.883738
2400.164299	61.648045	58.888743
2399.887182	71.500372	58.893748
2398.752968	79.079601	58.898753
2397.490322	77.292690	58.903757
2397.410273	68.636302	58.908762
2396.751478	72.960271	58.913767
2396.252795	72.574655	58.918772
2396.111021	68.682870	58.923777
2394.885306	72.302090	58.928781
2394.377805	72.628484	58.933786
2393.895572	64.366514	58.938791
2392.938276	76.057716	58.943796
2392.517039	68.521079	58.948801
2391.417460	66.364458	58.953805
2390.778957	67.232708	58.958810
2389.950804	77.339121	58.963815
2389.329548	75.774900	58.968820
2389.087888	64.866622	58.973825
2388.017236	75.862758	58.978829
2387.145639	67.760912	58.983834
2386.610415	69.233981	58.988839
2386.113601	64.597275	58.993844
2385.820825	69.973751	58.998849
2385.197542	81.559690	59.003853
2384.700631	65.068670	59.008858
2383.845018	67.819768	59.013863
2382.626467	79.848924	59.018868
2382.225419	69.504721	59.023873
2381.729602	74.732370	59.028877
2381.363177	65.150382	59.033882
2380.204779	76.113366	59.038887
2379.047193	73.200902	59.043892
2378.999254	73.341353	59.048897
2378.272625	73.454963	59.053901
2378.251967	67.956866	59.058906
2377.009231	70.281545	59.063911
2375.904426	78.123371	59.068916
2375.463978	65.680454	59.073921
2375.122332	76.658515	59.078925
2374.818306	66.331277	59.083930
2374.269911	74.021515	59.088935
2373.468481	79.114323	59.093940
2373.036113	78.288702	59.098945
2371.513683	68.165061	59.103949
2370.628654	75.987068	59.108954
2370.222915	65.812614	59.113959
2369.460186	74.270922	59.118964
2369.424805	63.176198	59.123969
2368.769022	74.926367	59.128973
2368.181896	62.800630	59.133978
2367.277379	64.803803	59.138983
2366.509769	71.265253	59.143988
2365.903030	62.584461	59.148993
2364.845451	68.083422	59.153997
2364.131933	62.527360	59.159002
2363.177628	63.581844	59.164007
2362.636537	66.907563	59.169012
2362.224767	67.032466	59.174017
2361.560848	66.973124	59.179021
2361.646739	65.845735	59.184026
2361.063622	67.958553	59.189031
2360.582769	69.578243	59.194036
2359.491090	68.383797	59.199041
2358.836578	82.150789	59.204045
2358.067944	69.936089	59.209050
2356.800202	71.412052	59.214055
2356.234554	71.737735	59.219060
2355.978549	60.241807	59.224065
2355.171954	63.706080	59.229069
2354.827757	62.378691	59.234074
2353.942225	71.403504	59.239079
2352.976423	71.624328	59.244084
2352.590611	62.624719	59.249089
2351.731324	65.805514	59.254093
2351.902801	60.235885	59.259098
2350.897455	72.530150	59.264103
2349.639880	73.921484	59.269108
2349.064013	63.969934	59.274113
2348.596800	71.572476	59.279117
2348.220979	66.428787	59.284122
2347.350914	61.798675	59.289127
2346.363774	68.119643	59.294132
2345.861181	60.554693	59.299137
2345.155803	64.673478	59.304141
2345.223032	65.531184	59.309146
2344.493655	67.569147	59.314151
2343.225999	69.212460	59.319156
2342.557498	61.919029	59.324161
2341.981011	67.864262	59.329165
2341.749219	68.053519	59.334170
2340.638629	71.828715	59.339175
2339.211534	68.676568	59.344180
2339.186991	72.315790	59.349185
2338.258359	76.513411	59.354189
2337.901141	69.979878	59.359194
2337.593043	64.616196	59.364199
2337.112034	73.536710	59.369204
2336.429032	65.051326	59.374209
2335.057961	77.146826	59.379213
2335.036374	73.876312	59.384218
2334.435855	72.956293	59.389223
2333.362832	70.811328	59.394228
2332.763817	62.915905	59.399233
2331.785985	79.579395	59.404237
2331.424624	60.525172	59.409242
2331.165192	61.248479	59.414247
2330.630386	70.923032	59.419252
2329.378010	61.719910	59.424257
2328.705813	70.968367	59.429261
2328.046938	62.632013	59.434266
2327.488567	69.903971	59.439271
2326.782114	69.590205	59.444276
2325.965921	58.910838	59.449281
2325.182105	65.197434	59.454285
2324.590899	68.866451	59.459290
2324.241528	65.893165	59.464295
2324.268008	63.273225	59.469300
2323.619706	65.867307	59.474305
2321.956823	63.477828	59.479309
2321.532296	53.218580	59.484314
2321.047620	71.810422	59.489319
2320.087991	66.821828	59.494324
2319.626893	66.400583	59.499329
2319.054173	74.203136	59.504333
2318.469141	66.600181	59.509338
2317.958089	62.396167	59.514343
2316.849390	73.247634	59.519348
2316.226966	61.161893	59.524353
2315.705989	68.597976	59.529357
2315.368694	66.977314	59.534362
2314.137228	58.685196	59.539367
2313.264806	63.619230	59.544372
2312.589036	69.852617	59.549377
2311.703955	69.891887	59.554381
2311.504990	61.191113	59.559386
2311.237423	66.577487	59.564391
2310.571507	71.109908	59.569396
2310.208494	57.621966	59.574401
2309.094433	70.178365	59.579405
2308.967162	66.064640	59.584410
2307.731662	69.459768	59.589415
2306.364119	70.845048	59.594420
2305.802946	64.537445	59.599425
2305.687997	70.220210	59.604429
2305.041565	68.210322	59.609434
2304.955847	62.610467	59.614439
2303.803190	78.790712	59.619444
2303.229704	57.901392	59.624449
2302.504859	70.182427	59.629453
2302.177175	60.604882	59.634458
2301.153730	68.033339	59.639463
2300.282329	62.591126	59.644468
2299.708608	57.481682	59.649473
2299.152399	67.036344	59.654477
2298.687869	61.675340	59.659482
2297.578067	63.905857	59.664487
2296.297356	69.827444	59.669492
2296.150345	58.658272	59.674497
2295.341871	71.026632	59.679501
2295.023620	67.609095	59.684506
2294.638109	66.362193	59.689511
2294.233047	67.898272	59.694516
2293.748967	68.741309	59.699521
2292.635074	66.104807	59.704525
2292.126007	62.241498	59.709530
2291.473153	68.571621	59.714535
2290.227561	72.428725	59.719540
2289.445573	67.652910	59.724545
2288.585460	60.676456	59.729549
2288.464146	68.397077	59.734554
2288.209885	65.915144	59.739559
2287.410205	70.037035	59.744564
2286.698628	58.575606	59.749569
2285.265063	61.865270	59.754573
2284.727517	58.531419	59.759578
2284.830458	61.114664	59.764583
2283.934091	63.937083	59.769588
2283.985743	66.388973	59.774593
2282.719253	71.009888	59.779597
2282.027783	67.299345	59.784602
2281.445896	67.269010	59.789607
2280.536464	76.124240	59.794612
2279.852476	62.712503	59.799617
2278.749595	73.028523	59.804621
2278.577992	65.249092	59.809626
2278.120178	66.166978	59.814631
2277.454088	76.569749	59.819636
2277.127877	66.852615	59.824641
2275.817719	69.192002	59.829645
2275.248331	71.251954	59.834650
2274.892712	68.800775	59.839655
2274.276953	72.285712	59.844660
2273.467024	67.621252	59.849665
2272.077233	80.951894	59.854669
2271.681380	65.850415	59.859674
2271.366010	64.777040	59.864679
2270.982110	71.214719	59.869684
2270.503538	64.288281	59.874689
2268.994267	69.607533	59.879693
2268.514095	64.950630	59.884698
2268.275038	62.905424	59.889703
2267.701578	67.600846	59.894708
2267.360152	68.315284	59.899713
2266.313845	72.640005	59.904718
2265.584619	70.770987	59.909722
2265.129667	64.642982	59.914727
2263.655176	66.622461	59.919732
2263.292531	61.148911	59.924737
2262.551837	73.104644	59.929742
2262.456537	67.865231	59.934746
2261.886440	64.168673	59.939751
2260.655893	64.736749	59.944756
2259.576730	56.716619	59.949761
2258.725285	64.620515	59.954766
2258.605753	55.237903	59.959770
2258.140327	60.951784	59.964775
2257.407021	63.689481	59.969780
2257.088496	67.755934	59.974785
2256.198782	67.747849	59.979790
2255.435434	70.047412	59.984794
2254.848504	62.781495	59.989799
2254.456587	65.688567	59.994804
2253.811904	65.102546	59.999809
2252.595617	65.385169	60.004814
2252.051295	66.133911	60.009818
2251.431227	71.963449	60.014823
2250.910841	66.528321	60.019828
2250.850121	61.357205	60.024833
2249.639469	61.400059	60.029838
2248.835661	60.753623	60.034842
2248.181317	63.159672	60.039847
2247.238180	71.195695	60.044852
2247.066416	71.973880	60.049857
2245.929214	64.532866	60.054862
2245.316630	66.916775	60.059866
2244.593025	67.596706	60.064871
2244.243112	69.963326	60.069876
2244.179571	62.178841	60.074881
2243.309242	68.318403	60.079886
2242.293731	60.067925	60.084890
2241.506005	61.530110	60.089895
2241.311439	69.300360	60.094900
2240.717943	64.430743	60.099905
2239.987442	71.531621	60.104910
2239.493739	62.924679	60.109914
2238.960101	59.217153	60.114919
2237.015960	71.312378	60.119924
2236.228721	58.773283	60.124929
2235.405002	66.656257	60.129934
2235.620881	69.775561	60.134938
2235.516358	65.318490	60.139943
2234.506328	68.445739	60.144948
2234.023466	55.432241	60.149953
2233.476949	65.262734	60.154958
2232.228893	62.887603	60.159962
2231.693955	61.910989	60.164967
2231.054569	60.873688	60.169972
2230.634322	57.410841	60.174977
2229.412653	68.019141	60.179982
2228.612884	62.193260	60.184986
2228.394660	63.190567	60.189991
2227.434176	70.421167	60.194996
2227.301273	64.547949	60.200001
2226.957169	65.782301	60.205006
2225.691697	62.057832	60.210010
2225.321251	60.164173	60.215015
2224.347271	60.307474	60.220020
2224.349547	54.621134	60.225025
2223.087418	62.395141	60.230030
2222.431527	65.901548	60.235034
2221.686079	62.764306	60.240039
2221.169145	63.814671	60.245044
2221.094995	64.173151	60.250049
2219.596362	64.098293	60.255054
2218.684551	67.844250	60.260058
2218.424208	59.481211	60.265063
2217.734610	70.637576	60.270068
2217.853574	59.263066	60.275073
2216.508213	61.330995	60.280078
2215.454972	59.807520	60.285082
2215.202171	58.180311	60.290087
2214.285335	67.140224	60.295092
2214.177239	59.280076	60.300097
2214.085897	66.155992	60.305102
2213.170040	65.373203	60.310106
2212.612489	61.130185	60.315111
2211.239238	66.443160	60.320116
2210.613515	64.424219	60.325121
2210.041440	61.042600	60.330126
2209.232297	59.735923	60.335130
2208.680659	62.761493	60.340135
2207.394966	66.191275	60.345140
2207.066347	64.686371	60.350145
2206.331102	66.040904	60.355150
2206.235648	69.508308	60.360154
2205.780037	63.136092	60.365159
2204.715911	66.605348	60.370164
2204.259400	62.332024	60.375169
2203.373342	60.157877	60.380174
2202.778082	65.354380	60.385178
2201.305684	67.245889	60.390183
2200.825683	60.888898	60.395188
2200.771926	67.968378	60.400193
2199.584150	63.741172	60.405198
2198.730117	68.027888	60.410202
2198.701124	62.550177	60.415207
2198.109423	69.832179	60.420212
2198.196051	68.775319	60.425217
2196.763966	71.074788	60.430222
2195.985593	72.590641	60.435226
2195.508285	60.715367	60.440231
2194.972085	66.912654	60.445236
2194.309672	63.427675	60.450241
2193.170781	65.834496	60.455246
2192.316949	70.590109	60.460250
2191.950090	57.769930	60.465255
2191.280667	65.570467	60.470260
2191.565513	57.726802	60.475265
2190.170289	68.602016	60.480270
2189.113333	62.635793	60.485274
2189.083971	57.475504	60.490279
2188.437150	69.623988	60.495284
2188.175252	60.114156	60.500289
2186.949269	68.107771	60.505294
2186.259419	66.686356	60.510298
2185.807743	65.854186	60.515303
2184.309399	59.604256	60.520308
2184.088094	62.592279	60.525313
2182.970326	63.477782	60.530318
2182.662256	58.051750	60.535322
2182.373380	47.613417	60.540327
2181.741333	57.914042	60.545332
2181.030208	59.257743	60.550337
2179.745905	68.241427	60.555342
2178.903961	61.801872	60.560346
2178.772841	58.305372	60.565351
2178.248796	66.497873	60.570356
2177.913452	58.889745	60.575361
2177.634610	61.379996	60.580366
2176.348886	61.366234	60.585370
2175.709278	51.223928	60.590375
2174.827276	57.937440	60.595380
2174.534900	57.115131	60.600385
2173.025448	60.860676	60.605390
2172.562836	61.655053	60.610394
2172.133930	56.031013	60.615399
2172.036998	74.323641	60.620404
2171.386163	54.473088	60.625409
2170.371715	61.243594	60.630414
2169.225913	60.726316	60.635418
2169.031213	61.110545	60.640423
2168.057381	55.956662	60.645428
2168.107568	54.420132	60.650433
2166.865259	63.034673	60.655438
2165.616752	57.875268	60.660442
2165.228891	52.483807	60.665447
2164.713318	68.560219	60.670452
2164.591803	58.629291	60.675457
2164.333953	56.003909	60.680462
2163.589187	51.936992	60.685466
2162.427608	54.074550	60.690471
2161.901226	54.369459	60.695476
2161.342934	59.498852	60.700481
2160.265802	60.036765	60.705486
2159.383910	62.558710	60.710490
2158.984085	67.291544	60.715495
2158.130649	67.953035	60.720500
2158.328978	67.709934	60.725505
2157.510807	64.615535	60.730510
2156.539402	57.898928	60.735514
2156.012617	63.204507	60.740519
2155.184322	65.577949	60.745524
2154.750072	52.473662	60.750529
2153.365390	58.317923	60.755534
2152.505227	55.678717	60.760538
2152.870433	51.666692	60.765543
2151.587375	58.807207	60.770548
2151.507353	60.486641	60.775553
2150.458974	59.436804	60.780558
2149.542010	57.637018	60.785562
2148.837699	55.078127	60.790567
2148.393601	63.076171	60.795572
2147.999601	59.260699	60.800577
2147.296849	59.211578	60.805582
2146.519625	60.832236	60.810586
2146.311368	58.134427	60.815591
2145.210512	67.441991	60.820596
2144.701711	60.454827	60.825601
2143.675228	59.343221	60.830606
2142.640297	59.291310	60.835610
2142.145073	58.563299	60.840615
2141.432067	56.419959	60.845620
2141.170927	57.854855	60.850625
2140.645852	55.367148	60.855630
2140.502873	56.672496	60.860634
2139.753764	50.903893	60.865639
2138.622828	62.090736	60.870644
2137.922234	58.742556	60.875649
2137.839365	53.645895	60.880654
2136.579820	57.966051	60.885658
2135.916259	56.126875	60.890663
2135.221346	64.035980	60.895668
2134.713124	64.964077	60.900673
2134.340909	63.185988	60.905678
2133.176164	61.883698	60.910682
2132.588538	60.058770	60.915687
2131.794297	53.527390	60.920692
2131.401744	61.263995	60.925697
2131.058904	53.635053	60.930702
2129.874075	56.706558	60.935706
2129.225716	61.278617	60.940711
2128.129498	57.065377	60.945716
2128.341203	51.576505	60.950721
2127.596373	55.277334	60.955726
2126.925107	56.813953	60.960730
2126.297547	54.598767	60.965735
2125.297528	58.910852	60.970740
2124.747959	44.586480	60.975745
2124.439643	52.155127	60.980750
2123.051609	52.071642	60.985754
2122.598971	47.820960	60.990759
2121.913441	61.193773	60.995764
2121.475064	55.432813	61.000769
2121.302911	50.327741	61.005774
2119.931197	58.120504	61.010778
2119.328935	54.876689	61.015783
2118.904811	63.256170	61.020788
2118.806254	56.340157	61.025793
2117.379967	50.358577	61.030798
2116.436334	56.317270	61.035802
2116.053628	50.073914	61.040807
2115.316312	62.229975	61.045812
2115.140000	51.202420	61.050817
2114.398367	57.509445	61.055822
2113.050969	60.939141	61.060826
2112.553030	49.211101	61.065831
2112.092781	59.852592	61.070836
2111.594450	57.391892	61.075841
2111.253148	52.187072	61.080846
2110.193567	57.752325	61.085850
2109.745616	56.331389	61.090855
2108.991708	65.065291	61.095860
2108.469564	57.948974	61.100865
2107.693388	67.541259	61.105870
2106.693950	59.700160	61.110874
2106.601970	55.952638	61.115879
2105.828501	67.611617	61.120884
2104.896771	56.271178	61.125889
2104.172596	53.602801	61.130894
2103.353588	54.643660	61.135898
2103.120234	49.296436	61.140903
2102.317393	53.553088	61.145908
2102.119648	51.284522	61.150913
2100.597424	58.000969	61.155918
2099.926643	54.736510	61.160922
2099.559600	46.279249	61.165927
2099.162490	57.052432	61.170932
2098.586854	48.480854	61.175937
2097.601443	55.102721	61.180942
2096.708415	55.334431	61.185946
2096.619950	49.023383	61.190951
2095.636857	53.850451	61.195956
2095.222057	53.690113	61.200961
2094.353049	55.051355	61.205966
2093.263348	61.359103	61.210970
2093.004657	54.322856	61.215975
2092.579584	62.203570	61.220980
2091.827000	57.614602	61.225985
2091.140809	51.337898	61.230990
2090.085023	55.212700	61.235994
2089.904333	54.582469	61.240999
2089.175632	54.566609	61.246004
2088.540007	57.957458	61.251009
2087.411536	67.733154	61.256014
2086.651764	64.022486	61.261018
2086.476648	54.869657	61.266023
2085.781839	49.773856	61.271028
2085.473204	57.757806	61.276033
2084.873011	50.573533	61.281038
2083.461593	61.412845	61.286042
2082.735968	55.559316	61.291047
2082.242727	56.115001	61.296052
2082.038371	55.065677	61.301057
2081.864528	49.661699	61.306062
2080.658112	59.825708	61.311066
2079.661214	59.450737	61.316071
2079.085423	58.413235	61.321076
2078.713518	59.246971	61.326081
2077.567095	56.866734	61.331086
2076.671340	53.599313	61.336090
2076.385467	45.018440	61.341095
2075.650029	65.089133	61.346100
2075.310381	58.774075	61.351105
2075.200984	54.062467	61.356110
2073.739432	67.832877	61.361114
2072.912155	60.866252	61.366119
2072.489332	64.110579	61.371124
2072.293187	60.031151	61.376129
2071.615961	53.725681	61.381134
2070.102216	56.228612	61.386138
2070.016915	52.836779	61.391143
2069.403251	63.628454	61.396148
2069.107255	56.065716	61.401153
2067.899401	58.731056	61.406158
2066.926420	61.907253	61.411162
2066.773320	55.548448	61.416167
2065.997427	57.841493	61.421172
2065.496918	53.844127	61.426177
2064.559365	53.088760	61.431182
2063.461468	61.626115	61.436186
2063.334682	57.679294	61.441191
2062.481371	66.013770	61.446196
2061.962018	50.571915	61.451201
2061.449310	54.949465	61.456206
2060.564821	57.001754	61.461210
2060.023883	55.725408	61.466215
2059.521133	59.035114	61.471220
2058.800591	56.391385	61.476225
2058.247603	56.374288	61.481230
2057.090308	56.805542	61.486234
2056.985559	48.146324	61.491239
2056.201442	57.616415	61.496244
2055.646027	58.696664	61.501249
2054.622942	50.577403	61.506254
2053.572657	58.818073	61.511258
2053.614672	47.105054	61.516263
2053.201337	57.093937	61.521268
2052.409587	56.771904	61.526273
2051.261997	50.894248	61.531278
2050.668618	53.556324	61.536282
2050.312322	53.825308	61.541287
2049.472802	59.088859	61.546292
2048.706031	63.703678	61.551297
2047.544539	61.026431	61.556302
2047.188601	63.677498	61.561306
2047.471744	55.094817	61.566311
2046.539619	56.536728	61.571316
2045.767098	57.976601	61.576321
2045.046703	56.647667	61.581326
2044.154022	62.399899	61.586330
2043.799814	56.690471	61.591335
2042.202399	65.802728	61.596340
2041.418077	65.389429	61.601345
2041.149289	55.542130	61.606350
2040.098610	58.012439	61.611354
2039.994993	56.966411	61.616359
2039.116280	66.129017	61.621364
2039.142242	59.865895	61.626369
2039.364378	58.183906	61.631374
2038.066306	62.594747	61.636378
2037.326880	60.750405	61.641383
2036.272052	67.352975	61.646388
2035.183324	64.351849	61.651393
2034.521026	64.540155	61.656398
2033.431297	59.993867	61.661402
2033.524462	56.692687	61.666407
2033.015097	65.354765	61.671412
2032.340926	59.735592	61.676417
2032.294734	60.196655	61.681422
2030.995157	64.451447	61.686426
2030.597766	56.025829	61.691431
2029.686615	67.031412	61.696436
2029.303497	60.709980	61.701441
2028.348889	62.017193	61.706446
2027.187253	62.421565	61.711450
2026.951441	58.191039	61.716455
2026.350860	62.162851	61.721460
2025.910946	64.089365	61.726465
2024.931233	55.039832	61.731470
2023.889890	71.113805	61.736474
2023.730446	58.875921	61.741479
2023.031592	59.207450	61.746484
2022.712001	59.815144	61.751489
2021.969808	60.472626	61.756494
2021.064554	62.928721	61.761498
2020.566876	52.718358	61.766503
2019.942124	67.918995	61.771508
2019.006293	63.197575	61.776513
2017.872772	55.990072	61.781518
2017.414256	71.152014	61.786522
2016.913127	55.900067	61.791527
2016.317799	58.926413	61.796532
2016.092579	52.432324	61.801537
2015.580431	49.510598	61.806542
2014.198659	56.940772	61.811546
2013.790958	52.611760	61.816551
2013.099325	61.734470	61.821556
2012.692021	59.722799	61.826561
2011.635792	55.702871	61.831566
2010.709120	58.785106	61.836570
2010.294304	53.669843	61.841575
2009.700126	60.894247	61.846580
2009.553568	64.614325	61.851585
2009.078832	61.955398	61.856590
2007.958279	66.037471	61.861594
2007.769816	55.847634	61.866599
2006.788564	73.077337	61.871604
2005.741437	63.980128	61.876609
2004.876944	58.961915	61.881614
2004.430254	62.730570	61.886618
2004.039259	57.896220	61.891623
2003.256670	63.843170	61.896628
2002.361369	61.476834	61.901633
2001.739331	60.997099	61.906638
2001.471939	69.281484	61.911642
2001.443775	52.560801	61.916647
2000.160411	61.394352	61.921652
1998.655642	60.394984	61.926657
1998.011643	59.770591	61.931662
1997.514986	63.165703	61.936666
1997.099370	50.885995	61.941671
1996.914576	64.301438	61.946676
1996.406954	60.915535	61.951681
1995.782580	57.769859	61.956686
1994.908202	59.622278	61.961690
1993.921487	52.925703	61.966695
1992.930721	57.232671	61.971700
1992.026924	50.084562	61.976705
1991.572998	55.794111	61.981710
1991.112116	60.306085	61.986714
1991.018291	59.117467	61.991719
1991.032199	53.785192	61.996724
1989.228347	57.295757	62.001729
1988.512650	58.163440	62.006734
1987.954247	63.101027	62.011738
1987.933845	55.915483	62.016743
1986.361173	61.446159	62.021748
1985.442190	61.405628	62.026753
1984.951991	56.441415	62.031758
1984.569252	71.220538	62.036762
1985.011349	55.625285	62.041767
1983.736940	55.188466	62.046772
1982.958421	63.030961	62.051777
1981.972768	64.453224	62.056782
1981.598077	62.675177	62.061786
1981.013271	57.618205	62.066791
1979.859333	60.239604	62.071796
1978.932204	60.770445	62.076801
1978.826852	55.281340	62.081806
1978.117870	67.972143	62.086810
1977.270254	59.595918	62.091815
1977.291468	60.678584	62.096820
1975.674666	54.196765	62.101825
1975.113064	54.081286	62.106830
1974.381835	57.921508	62.111834
1974.029190	53.606372	62.116839
1973.793513	63.196986	62.121844
1972.965939	63.988681	62.126849
1972.323109	51.606931	62.131854
1971.336353	59.400576	62.136858
1971.006150	61.242407	62.141863
1970.391500	61.381914	62.146868
1969.913305	63.709701	62.151873
1968.710947	55.852830	62.156878
1967.800045	60.535730	62.161882
1967.733051	56.112916	62.166887
1967.179723	59.524038	62.171892
1966.070722	57.733850	62.176897
1965.266784	57.086692	62.181902
1964.641347	58.219189	62.186906
1964.449032	54.581599	62.191911
1963.847688	63.573213	62.196916
1962.753758	62.856851	62.201921
1962.173583	53.947403	62.206926
1961.536327	65.394404	62.211930
1961.373649	52.959728	62.216935
1960.893675	57.693643	62.221940
1959.349018	57.383583	62.226945
1959.003399	55.659774	62.231950
1958.269346	61.605529	62.236954
1957.701809	55.587224	62.241959
1956.562247	64.894322	62.246964
1955.947437	61.543734	62.251969
1955.791615	62.283278	62.256974
1955.152231	69.863565	62.261978
1954.697927	63.004472	62.266983
1953.751079	62.437419	62.271988
1952.679960	62.458048	62.276993
1952.248489	63.023308	62.281998
1951.794651	64.373153	62.287002
1951.500502	68.139005	62.292007
1950.471934	65.871657	62.297012
1949.879837	63.429779	62.302017
1949.472625	63.266971	62.307022
1948.425520	68.058830	62.312026
1947.635500	68.940416	62.317031
1946.832061	67.009542	62.322036
1946.388961	66.517755	62.327041
1945.883940	67.736230	62.332046
1945.263279	71.198742	62.337050
1944.511070	58.761497	62.342055
1943.854343	60.948912	62.347060
1942.600958	71.089006	62.352065
1942.658454	58.874416	62.357070
1941.947133	74.991408	62.362074
1940.878702	64.648570	62.367079
1939.620693	67.659213	62.372084
1939.222750	67.489689	62.377089
1939.205820	61.446269	62.382094
1938.587613	63.572230	62.387098
1938.197496	55.109070	62.392103
1937.597786	63.370565	62.397108
1936.498168	60.415930	62.402113
1936.172248	62.902399	62.407118
1935.142065	68.552646	62.412122
1934.557519	64.372706	62.417127
1933.610731	65.325321	62.422132
1932.909936	63.197292	62.427137
1932.842861	62.315535	62.432142
1932.322232	70.565480	62.437146
1931.460365	60.220862	62.442151
1930.307125	61.275503	62.447156
1929.603812	58.125579	62.452161
1929.315990	51.142889	62.457166
1928.786383	63.460384	62.462170
1928.252886	53.023282	62.467175
1926.804352	52.509691	62.472180
1926.054836	51.968488	62.477185
1926.153535	50.886274	62.482190
1925.469642	56.617009	62.487194
1925.304029	43.338146	62.492199
1923.972553	61.189041	62.497204
1923.194676	64.061105	62.502209
1923.073588	47.986707	62.507214
1921.649917	59.311275	62.512218
1920.985356	48.966464	62.517223
1920.313687	55.383501	62.522228
1919.865536	54.952184	62.527233
1919.000943	48.177503	62.532238
1918.662907	55.309933	62.537242
1918.576878	52.562416	62.542247
1917.555054	56.213551	62.547252
1916.428585	55.357114	62.552257
1916.257424	51.224482	62.557262
1915.476945	52.180227	62.562266
1914.903326	42.706012	62.567271
1913.658096	53.973210	62.572276
1913.073803	51.373300	62.577281
1912.755555	49.014839	62.582286
1911.809821	58.409958	62.587290
1911.808690	48.503079	62.592295
1910.686040	56.964161	62.597300
1909.644926	59.076423	62.602305
1909.631331	53.002440	62.607310
1908.979447	63.653817	62.612314
1908.518852	55.411526	62.617319
1907.426374	47.562722	62.622324
1906.386869	53.333373	62.627329
1906.108297	52.216232	62.632334
1905.375366	57.098024	62.637338
1905.158265	56.068652	62.642343
1904.026955	55.863151	62.647348
1902.967358	57.144926	62.652353
1902.787628	50.640306	62.657358
1902.234802	65.395226	62.662362
1902.158090	57.525007	62.667367
1901.038802	59.442232	62.672372
1900.040344	59.231767	62.677377
1899.612648	55.150917	62.682382
1898.962892	58.261185	62.687386
1898.312055	59.856305	62.692391
1897.280447	62.557446	62.697396
1896.834873	63.402217	62.702401
1896.821536	52.083930	62.707406
1895.822514	58.912616	62.712410
1894.860930	53.367903	62.717415
1894.113339	56.981994	62.722420
1893.572292	58.135192	62.727425
1893.312207	47.405416	62.732430
1892.143681	58.462926	62.737434
1891.553964	59.004739	62.742439
1890.826313	56.054372	62.747444
1889.694863	62.259162	62.752449
1889.922871	47.853926	62.757454
1889.035252	54.817887	62.762458
1888.439639	58.967271	62.767463
1887.707974	57.908698	62.772468
1887.184507	55.920860	62.777473
1886.634024	54.086058	62.782478
1885.094181	64.320161	62.787482
1884.745715	55.790675	62.792487
1883.986720	48.910309	62.797492
1883.657971	54.365166	62.802497
1883.576032	53.940671	62.807502
1882.635793	53.937345	62.812506
1881.369036	47.412654	62.817511
1880.735185	56.133521	62.822516
1879.998936	54.379447	62.827521
1879.798137	41.640670	62.832526
1879.592700	56.803893	62.837530
1878.287050	53.328755	62.842535
1877.532430	45.765566	62.847540
1876.781977	50.341291	62.852545
1876.733340	51.571688	62.857550
1875.920987	54.464653	62.862554
1874.804583	56.860975	62.867559
1874.329836	45.594399	62.872564
1873.771684	56.165396	62.877569
1873.290047	53.723975	62.882574
1872.497737	56.855475	62.887578
1871.624945	58.145164	62.892583
1871.017714	53.120468	62.897588
1870.173443	56.676105	62.902593
1870.168067	49.078677	62.907598
1869.432284	58.898914	62.912602
1868.233421	51.905917	62.917607
1867.742614	46.874332	62.922612
1866.950248	52.310219	62.927617
1866.648846	47.200442	62.932622
1866.132399	64.276407	62.937626
1865.008258	54.294037	62.942631
1864.359885	50.392652	62.947636
1863.356400	58.419686	62.952641
1863.510168	45.047114	62.957646
1863.147975	55.031187	62.962650
1861.791574	50.188741	62.967655
1861.269149	59.028700	62.972660
1860.508092	60.676233	62.977665
1860.365836	46.644597	62.982670
1858.954426	59.245181	62.987674
1858.231347	57.608851	62.992679
1857.766279	56.861500	62.997684
1857.262067	62.353088	63.002689
1856.907191	43.186993	63.007694
1856.005989	64.819120	63.012698
1855.057533	52.679548	63.017703
1854.764091	54.670219	63.022708
1853.930794	60.519675	63.027713
1853.627465	56.380450	63.032718
1852.821902	61.394669	63.037722
1852.033152	60.273634	63.042727
1851.219118	61.185789	63.047732
1850.874002	59.892937	63.052737
1849.967572	42.122207	63.057742
1849.228321	59.824417	63.062746
1848.670766	50.915072	63.067751
1848.041090	45.993692	63.072756
1847.189398	60.789869	63.077761
1846.496122	51.563494	63.082766
1845.555887	46.011197	63.087770
1845.271400	48.816222	63.092775
1844.718466	53.107905	63.097780
1844.248380	59.772685	63.102785
1843.887151	49.584409	63.107790
1842.578275	51.940247	63.112794
1842.016081	55.390393	63.117799
1841.401590	50.469572	63.122804
1840.920136	58.879381	63.127809
1840.357270	53.808418	63.132814
1839.108516	60.928115	63.137818
1839.291655	49.984759	63.142823
1838.670193	45.367094	63.147828
1837.297173	54.407049	63.152833
1836.776737	52.609743	63.157838
1836.079553	54.460683	63.162842
1835.462738	54.426110	63.167847
1834.534127	53.915561	63.172852
1833.719875	58.629702	63.177857
1833.119631	44.379206	63.182862
1832.801058	54.488835	63.187866
1832.464961	56.165897	63.192871
1832.258974	54.482549	63.197876
1830.599460	58.236878	63.202881
1829.978179	51.731629	63.207886
1829.279795	55.963334	63.212890
1828.844483	51.938663	63.217895
1828.489094	55.516841	63.222900
1826.959803	61.486167	63.227905
1826.420819	50.183223	63.232910
1825.604459	60.409600	63.237914
1825.135731	52.751324	63.242919
1824.829907	61.360813	63.247924
1824.631376	65.298982	63.252929
1824.411085	52.501965	63.257934
1823.188312	57.869397	63.262938
1822.614260	53.974644	63.267943
1821.750818	51.561053	63.272948
1820.419515	56.546019	63.277953
1819.925320	56.477047	63.282958
1819.162935	53.110285	63.287962
1818.867373	53.182190	63.292967
1818.298238	52.737636	63.297972
1817.979332	53.562319	63.302977
1817.569084	51.963654	63.307982
1816.139137	62.926961	63.312986
1815.525688	63.877430	63.317991
1815.059077	61.343053	63.322996
1814.224331	62.698869	63.328001
1813.494760	56.642789	63.333006
1812.652073	59.810547	63.338010
1812.408613	54.275220	63.343015
1811.964962	62.218319	63.348020
1811.389448	66.090730	63.353025
1810.689610	49.620394	63.358030
1809.479883	51.491927	63.363034
1808.944850	59.190934	63.368039
1808.222044	61.439403	63.373044
1807.579459	63.141670	63.378049
1806.826408	53.839087	63.383054
1806.270398	57.342649	63.388058
1805.457956	54.201549	63.393063
1805.322697	51.151027	63.398068
1804.957490	58.914526	63.403073
1804.032474	54.966933	63.408078
1802.895363	55.499389	63.413082
1802.411694	62.560820	63.418087
1802.102387	52.804964	63.423092
1800.506577	60.327848	63.428097
1799.982636	51.987474	63.433102
1799.127556	54.937099	63.438106
1798.613526	59.125029	63.443111
1798.911545	52.558809	63.448116
1798.123565	55.511164	63.453121
1797.959132	48.387780	63.458126
1796.851608	59.224082	63.463130
1796.246699	60.513736	63.468135
1795.217680	56.182509	63.473140
1794.244542	62.299045	63.478145
1793.842127	54.614429	63.483150
1793.176263	57.574705	63.488154
1792.641940	53.430800	63.493159
1792.228284	53.401734	63.498164
1790.782517	56.762280	63.503169
1790.401847	47.924522	63.508174
1790.081545	57.567888	63.513178
1789.409153	59.117762	63.518183
1788.292444	55.076660	63.523188
1787.645527	61.747619	63.528193
1787.225360	57.933115	63.533198
1786.736562	60.858360	63.538202
1786.040433	54.113699	63.543207
1785.801398	56.889635	63.548212
1784.574786	59.802178	63.553217
1783.963962	52.726751	63.558222
1783.067220	59.027576	63.563226
1782.595131	53.716100	63.568231
1781.734493	52.348440	63.573236
1780.835316	56.532403	63.578241
1780.724518	53.726765	63.583246
1780.211158	56.288728	63.588250
1779.579341	58.966087	63.593255
1778.722993	56.903776	63.598260
1777.585063	56.444446	63.603265
1777.351497	51.353465	63.608270
1776.806878	60.331821	63.613274
1776.235956	58.382509	63.618279
1775.312920	46.435188	63.623284
1774.154566	61.264889	63.628289
1774.135440	47.377194	63.633294
1773.973077	62.380677	63.638298
1772.746938	61.864206	63.643303
1771.673852	53.215576	63.648308
1770.975520	54.141102	63.653313
1770.790633	52.451779	63.658318
1770.053118	52.748114	63.663322
1770.173778	57.042966	63.668327
1769.292052	49.750222	63.673332
1767.863042	59.729336	63.678337
1767.191062	59.885781	63.683342
1766.842993	56.714968	63.688346
1766.331293	57.627508	63.693351
1765.150511	52.708860	63.698356
1764.302237	66.249248	63.703361
1763.922484	59.257833	63.708366
1763.695857	66.200683	63.713370
1763.151361	62.559816	63.718375
1762.374126	56.010607	63.723380
1761.649739	56.843491	63.728385
1761.233407	47.710668	63.733390
1759.603089	62.847694	63.738394
1758.915021	60.903429	63.743399
1758.873832	54.087761	63.748404
1758.050037	54.555565	63.753409
1757.807352	49.048139	63.758414
1757.358246	55.100275	63.763418
1756.011000	56.354720	63.768423
1755.430572	51.437953	63.773428
1754.707239	56.214305	63.778433
1754.295720	56.753272	63.783438
1753.678473	59.319988	63.788442
1752.909007	58.321585	63.793447
1752.083669	56.396466	63.798452
1750.877084	54.164755	63.803457
1751.023989	55.141835	63.808462
1750.637152	58.723818	63.813466
1750.027125	60.516437	63.818471
1749.221305	62.634255	63.823476
1748.165181	63.743762	63.828481
1748.188641	50.669010	63.833486
1746.855571	52.901516	63.838490
1745.667840	57.284850	63.843495
1745.447602	55.307905	63.848500
1744.836807	60.835891	63.853505
1744.587652	53.475176	63.858510
1743.993922	56.882174	63.863514
1742.895645	59.771188	63.868519
1742.346444	58.540895	63.873524
1741.872761	68.495498	63.878529
1741.025522	56.451135	63.883534
1739.737262	56.558698	63.888538
1738.839679	59.562970	63.893543
1739.124169	54.069152	63.898548
1738.144004	60.886735	63.903553
1737.590207	59.041467	63.908558
1737.474520	61.459603	63.913562
1736.763319	58.994321	63.918567
1735.992495	65.253083	63.923572
1735.013049	61.547701	63.928577
1734.421817	58.022595	63.933582
1734.039940	59.841700	63.938586
1732.642594	61.587466	63.943591
1732.347463	52.563770	63.948596
1731.332656	67.415493	63.953601
1731.155778	52.721933	63.958606
1730.815609	50.255533	63.963610
1729.977027	57.953983	63.968615
1729.234778	56.250694	63.973620
1728.617268	57.118187	63.978625
1727.985756	59.557482	63.983630
1726.792047	55.354316	63.988634
1725.488280	55.743207	63.993639
1725.430536	56.076385	63.998644
1724.940146	68.651630	64.003649
1724.178061	62.228908	64.008654
1723.952415	53.607779	64.013658
1723.503454	57.098555	64.018663
1723.174426	49.494154	64.023668
1721.971303	58.632553	64.028673
1721.309982	50.085186	64.033678
1720.930669	51.779515	64.038682
1719.650554	49.053180	64.043687
1718.956121	52.006904	64.048692
1718.273737	58.615252	64.053697
1718.381051	48.195650	64.058702
1717.777273	51.917381	64.063706
1716.400879	56.985869	64.068711
1715.879028	54.693841	64.073716
1715.301794	52.606281	64.078721
1714.837932	53.200390	64.083726
1713.437555	56.078735	64.088730
1712.592076	56.965502	64.093735
1712.280269	52.077380	64.098740
1711.631355	50.977045	64.103745
1711.409418	53.049428	64.108750
1711.146969	49.692664	64.113754
1710.179127	62.312497	64.118759
1709.538081	48.614120	64.123764
1708.648838	62.969112	64.128769
1708.090840	64.551920	64.133774
1707.557865	58.495772	64.138778
1706.318901	59.724596	64.143783
1705.534496	43.745986	64.148788
1705.270563	55.503293	64.153793
1705.053107	49.423552	64.158798
1704.517942	51.791892	64.163802
1703.553535	61.037861	64.168807
1703.002829	50.542968	64.173812
1702.275235	60.870604	64.178817
1701.278309	50.412199	64.183822
1700.038055	51.517697	64.188826
1699.311272	50.811198	64.193831
1699.312626	48.510562	64.198836
1698.515662	63.085806	64.203841
1698.422493	50.337716	64.208846
1698.244440	53.803451	64.213850
1696.909270	53.697219	64.218855
1696.242075	52.003197	64.223860
1695.449634	53.965975	64.228865
1694.801794	48.538146	64.233870
1693.535026	51.769800	64.238874
1692.661754	54.328227	64.243879
1692.885672	50.255503	64.248884
1692.149900	54.765579	64.253889
1691.939631	51.521461	64.258894
1691.771775	54.338901	64.263898
1690.457537	55.607449	64.268903
1689.940890	47.399265	64.273908
1688.501046	57.174991	64.278913
1688.038938	51.939186	64.283918
1687.412623	53.139755	64.288922
1686.666610	61.882981	64.293927
1686.785626	48.336777	64.298932
1685.302314	62.216738	64.303937
1684.461729	52.489052	64.308942
1683.964936	50.314314	64.313946
1683.466064	57.717805	64.318951
1683.202888	46.347964	64.323956
1682.140578	56.833527	64.328961
1681.312027	54.676482	64.333966
1680.823073	56.762980	64.338970
1680.277770	54.148536	64.343975
1679.839510	46.877821	64.348980
1679.346330	55.131352	64.353985
1678.014471	59.346739	64.358990
1677.473623	54.844378	64.363994
1676.844660	57.807035	64.368999
1676.849902	51.191053	64.374004
1675.554658	60.938486	64.379009
1674.408485	56.065650	64.384014
1674.059287	55.272042	64.389018
1673.366133	61.191872	64.394023
1673.193819	50.219359	64.399028
1672.622896	60.150334	64.404033
1671.366919	58.979022	64.409038
1670.585780	56.585717	64.414042
1670.113708	62.554950	64.419047
1670.277018	54.621579	64.424052
1669.439171	51.637610	64.429057
1668.596508	47.349919	64.434062
1667.680177	52.569811	64.439066
1666.860792	62.808950	64.444071
1666.861666	53.273579	64.449076
1665.506856	57.081597	64.454081
1664.344639	54.588511	64.459086
1663.747315	46.696099	64.464090
1663.537432	51.967595	64.469095
1663.172711	54.279141	64.474100
1662.829497	62.151766	64.479105
1662.300645	52.754409	64.484110
1661.166176	47.040797	64.489114
1660.205950	58.818179	64.494119
1659.829144	50.274635	64.499124
1659.269926	47.704022	64.504129
1658.056888	54.346734	64.509134
1657.638490	43.570279	64.514138
1656.400314	55.544821	64.519143
1656.625626	49.336031	64.524148
1656.253254	57.846378	64.529153
1655.668339	50.142097	64.534158
1654.659007	57.773855	64.539162
1653.903159	59.433154	64.544167
1653.119197	51.044545	64.549172
1652.469088	56.876881	64.554177
1651.412493	62.927588	64.559182
1650.932940	60.545437	64.564186
1650.218700	55.472383	64.569191
1649.930004	50.355719	64.574196
1649.720549	54.840862	64.579201
1648.746960	52.770218	64.584206
1647.899392	51.167462	64.589210
1647.034406	53.658954	64.594215
1646.499548	48.137987	64.599220
1646.063656	55.301368	64.604225
1644.826322	54.562250	64.609230
1644.375071	57.203590	64.614234
1643.911568	52.794968	64.619239
1643.696001	49.944901	64.624244
1643.144775	59.380684	64.629249
1641.682702	61.707130	64.634254
1641.050642	54.959428	64.639258
1640.561852	60.554170	64.644263
1640.115641	56.585464	64.649268
1639.327057	58.441016	64.654273
1638.628539	58.522285	64.659278
1638.043838	59.063266	64.664282
1637.480033	62.694879	64.669287
1636.959359	51.320557	64.674292
1635.554119	60.132782	64.679297
1635.233927	50.230403	64.684302
1634.851910	57.478114	64.689306
1634.169462	53.862849	64.694311
1634.020659	51.323448	64.699316
1632.688371	51.187924	64.704321
1631.937136	54.598595	64.709326
1631.557790	56.679761	64.714330
1630.388034	55.043331	64.719335
1629.756212	49.428438	64.724340
1628.927427	54.104036	64.729345
1628.393449	53.914001	64.734350
1628.181831	48.784939	64.739354
1627.675756	60.177120	64.744359
1627.084602	46.954551	64.749364
1626.028588	53.757493	64.754369
1625.267614	54.855592	64.759374
1625.040473	53.941237	64.764378
1623.956047	61.046269	64.769383
1623.278860	46.167181	64.774388
1622.521378	54.617514	64.779393
1621.737084	52.812101	64.784398
1621.678616	56.129088	64.789402
1620.762304	56.844051	64.794407
1620.607439	51.405290	64.799412
1619.582120	56.883830	64.804417
1618.895297	53.801398	64.809422
1618.384375	48.051744	64.814426
1617.536419	50.642558	64.819431
1616.549909	50.670092	64.824436
1615.612498	53.031094	64.829441
1615.231856	47.734783	64.834446
1615.024100	46.269636	64.839450
1614.546996	48.824616	64.844455
1614.364332	54.873394	64.849460
1613.289970	55.672640	64.854465
1612.333751	53.105632	64.859470
1610.930721	43.642769	64.864474
1610.166959	59.300568	64.869479
1609.927670	45.531495	64.874484
1609.093865	56.734242	64.879489
1608.789433	58.188800	64.884494
1608.714204	45.843429	64.889498
1608.047975	53.065963	64.894503
1607.616437	46.699201	64.899508
1606.308718	48.811353	64.904513
1605.749217	44.955985	64.909518
1604.983288	51.223387	64.914522
1603.713155	48.949697	64.919527
1603.347203	39.691449	64.924532
1603.015377	50.995384	64.929537
1602.301943	47.586735	64.934542
1602.114584	48.445362	64.939546
1601.017686	47.647091	64.944551
1600.258176	43.107959	64.949556
1599.722428	39.809029	64.954561
1599.079387	50.888736	64.959566
1598.632467	42.774424	64.964570
1597.472027	53.393623	64.969575
1596.898087	45.988254	64.974580
1596.363744	54.894590	64.979585
1595.543256	56.210499	64.984590
1595.292209	46.815353	64.989594
1594.068949	54.227948	64.994599
1593.599339	50.802045	64.999604
1592.825090	45.899925	65.004609
1592.594118	49.436292	65.009614
1592.431828	41.470236	65.014618
1590.981044	48.688093	65.019623
1590.578742	41.911351	65.024628
1589.918409	60.213435	65.029633
1589.408086	43.600221	65.034638
1588.211803	42.149518	65.039642
1587.500555	53.409050	65.044647
1587.265929	49.667025	65.049652
1586.670229	54.880607	65.054657
1585.596337	52.889113	65.059662
1584.873742	41.429766	65.064666
1584.083548	51.371419	65.069671
1583.687441	38.524418	65.074676
1583.568444	48.182264	65.079681
1583.170590	47.414753	65.084686
1582.290664	36.605596	65.089690
1581.378260	40.802896	65.094695
1580.541610	44.110168	65.099700
1579.205702	49.699888	65.104705
1578.310578	45.428298	65.109710
1578.417830	48.215628	65.114714
1577.519333	59.118411	65.119719
1577.003795	49.148426	65.124724
1576.609962	53.032782	65.129729
1576.019785	50.677468	65.134734
1575.854879	47.506119	65.139738
1574.437306	58.601152	65.144743
1573.803332	48.238955	65.149748
1573.360317	50.680346	65.154753
1572.674331	52.003634	65.159758
1571.911230	43.368331	65.164762
1570.877960	56.717357	65.169767
1570.709718	47.137919	65.174772
1570.177426	58.906409	65.179777
1569.530659	54.298250	65.184782
1568.521222	50.518703	65.189786
1567.692091	48.477432	65.194791
1567.639328	39.542153	65.199796
1566.965931	54.091899	65.204801
1565.642574	49.698213	65.209806
1565.078274	46.375753	65.214810
1564.420869	53.632699	65.219815
1564.400773	39.809944	65.224820
1563.688572	38.535337	65.229825
1562.486486	41.908703	65.234830
1561.783540	46.292782	65.239834
1560.980530	47.288351	65.244839
1560.934502	42.264768	65.249844
1560.173586	55.453898	65.254849
1559.608191	51.876637	65.259854
1558.712566	45.562072	65.264858
1557.736125	51.689461	65.269863
1557.322262	53.796668	65.274868
1556.772933	55.494447	65.279873
1556.245302	50.708804	65.284878
1554.909721	56.836872	65.289882
1554.294179	63.699439	65.294887
1554.116449	53.413891	65.299892
1553.973983	52.458207	65.304897
1552.934976	55.185539	65.309902
1552.341927	52.995712	65.314906
1551.497985	52.566247	65.319911
1550.680883	52.810316	65.324916
1550.628562	55.671533	65.329921
1549.134038	52.120662	65.334926
1548.579209	48.435810	65.339930
1547.912790	50.519139	65.344935
1547.515943	47.312095	65.349940
1547.489140	49.067283	65.354945
1546.078637	55.330932	65.359950
1545.347011	56.742952	65.364954
1544.437687	52.650633	65.369959
1544.297943	52.851405	65.374964
1543.794359	49.728153	65.379969
1542.781850	49.181098	65.384974
1542.184935	45.872908	65.389978
1541.204975	49.347600	65.394983
1541.300195	53.694549	65.399988
1540.646478	49.271920	65.404993
1539.396986	52.537359	65.409998
1538.866178	49.270747	65.415002
1538.179961	42.757329	65.420007
1537.946570	49.172794	65.425012
1536.636489	51.046956	65.430017
1536.021597	49.848458	65.435022
1535.817495	52.111205	65.440026
1534.818709	58.095193	65.445031
1534.683144	47.109703	65.450036
1533.505174	43.868593	65.455041
1532.534187	44.175316	65.460046
1532.299601	54.935263	65.465050
1531.667300	49.204818	65.470055
1531.418306	43.255623	65.475060
1530.287900	36.341806	65.480065
1529.401863	46.323151	65.485070
1529.279579	38.944704	65.490074
1528.472977	47.231742	65.495079
1527.646172	45.534670	65.500084
1526.708054	41.543597	65.505089
1525.856725	49.527647	65.510094
1525.477543	41.543460	65.515098
1524.872781	49.755299	65.520103
1524.999370	41.195494	65.525108
1523.833567	41.236759	65.530113
1522.812957	44.187514	65.535118
1522.707375	45.537782	65.540122
1522.066602	44.831193	65.545127
1521.107558	44.677210	65.550132
1520.266663	42.857425	65.555137
1519.390345	44.606039	65.560142
1519.089326	41.274052	65.565146
1518.588568	53.313837	65.570151
1518.265112	36.050539	65.575156
1517.546916	45.100436	65.580161
1516.517717	42.140566	65.585166
1515.510630	40.490140	65.590170
1514.255984	51.832016	65.595175
1513.720223	53.938379	65.600180
1513.941961	48.566220	65.605185
1513.058117	47.672691	65.610190
1512.633584	45.566919	65.615194
1512.386392	51.905408	65.620199
1511.608080	41.878183	65.625204
1510.886630	45.983999	65.630209
1510.099316	49.767551	65.635214
1509.463518	42.801452	65.640218
1507.771440	43.465268	65.645223
1507.224785	44.241320	65.650228
1506.842032	46.157686	65.655233
1506.396600	43.279081	65.660238
1506.116910	36.813721	65.665242
1505.449243	40.907963	65.670247
1504.709438	46.315150	65.675252
1503.443807	46.837694	65.680257
1502.918563	52.375916	65.685262
1502.786193	49.868446	65.690266
1502.333264	49.038135	65.695271
1501.447633	46.070668	65.700276
1500.351551	40.541972	65.705281
1499.937966	41.494582	65.710286
1499.706060	41.331410	65.715290
1498.413816	49.214093	65.720295
1497.584742	45.295147	65.725300
1496.935178	47.392174	65.730305
1496.503565	55.969496	65.735310
1496.216399	49.853159	65.740314
1495.605963	55.844101	65.745319
1494.710669	48.179161	65.750324
1493.742059	43.770570	65.755329
1493.096512	42.284443	65.760334
1493.080296	44.158996	65.765338
1492.173713	45.229931	65.770343
1491.060146	42.620412	65.775348
1490.540895	36.538277	65.780353
1489.922925	42.325645	65.785358
1489.511494	42.038866	65.790362
1489.105474	48.522558	65.795367
1488.090163	43.543698	65.800372
1487.415819	44.622646	65.805377
1486.509516	49.225871	65.810382
1486.311342	43.385609	65.815386
1485.126601	50.430459	65.820391
1484.594706	41.085375	65.825396
1484.437072	45.923996	65.830401
1483.887639	50.115632	65.835406
1482.763711	43.359394	65.840410
1481.834863	53.222158	65.845415
1481.242813	44.548522	65.850420
1481.025909	45.578781	65.855425
1480.199809	48.808869	65.860430
1479.188069	42.025537	65.865434
1478.033312	47.145344	65.870439
1477.305840	41.298971	65.875444
1477.461767	42.929333	65.880449
1476.819223	49.091156	65.885454
1476.974881	34.536923	65.890458
1476.224357	42.986856	65.895463
1475.362528	49.994201	65.900468
1474.702410	47.476802	65.905473
1473.602457	55.075539	65.910478
1472.931997	44.128325	65.915482
1472.317425	45.175730	65.920487
1471.364490	38.268658	65.925492
1470.579413	41.108847	65.930497
1469.571099	45.872421	65.935502
1469.099208	41.006205	65.940506
1468.830425	43.890652	65.945511
1468.539510	41.335720	65.950516
1467.991603	43.554685	65.955521
1466.936365	46.499929	65.960526
1466.078260	38.909948	65.965530
1465.092079	52.907728	65.970535
1464.848100	40.763758	65.975540
1464.668532	42.618114	65.980545
1463.773649	44.908310	65.985550
1462.800515	40.518264	65.990554
1462.301079	55.793330	65.995559
1461.623087	47.239007	66.000564
1461.556313	50.445311	66.005569
1460.324846	56.093361	66.010574
1459.393071	44.986018	66.015578
1458.983133	52.136667	66.020583
1458.487168	49.403683	66.025588
1457.656422	47.277054	66.030593
1456.809821	51.913879	66.035598
1456.144502	37.962775	66.040602
1455.504973	47.161440	66.045607
1455.363852	49.888649	66.050612
1454.776184	53.030959	66.055617
1453.531082	52.690700	66.060622
1453.008387	46.060498	66.065626
1452.534640	57.860409	66.070631
1451.738270	47.004220	66.075636
1450.650837	44.418262	66.080641
1449.380877	52.749094	66.085646
1449.125533	47.100585	66.090650
1448.962876	49.611227	66.095655
1448.433328	45.553002	66.100660
1448.244481	45.992697	66.105665
1447.436890	55.738794	66.110670
1446.778380	48.313587	66.115674
1445.621455	48.575577	66.120679
1445.407467	57.733384	66.125684
1444.719733	47.607383	66.130689
1443.290965	55.805538	66.135694
1443.020643	42.226541	66.140698
1442.120057	50.581776	66.145703
1441.936119	54.096279	66.150708
1441.758775	49.678967	66.155713
1440.234521	54.208374	66.160718
1439.640116	39.535825	66.165722
1439.190864	54.675200	66.170727
1438.825659	55.770316	66.175732
1438.248349	42.309783	66.180737
1437.065670	53.275422	66.185742
1436.606777	40.456565	66.190746
1435.786974	50.692622	66.195751
1435.326652	46.985295	66.200756
1434.419931	54.325578	66.205761
1433.151279	61.642555	66.210766
1433.297862	45.872163	66.215770
1432.733232	52.789960	66.220775
1432.287279	49.681725	66.225780
1431.184625	45.749229	66.230785
1430.311046	49.862541	66.235790
1429.926407	49.460659	66.240794
1429.580270	51.755219	66.245799
1428.922899	47.429152	66.250804
1427.695430	53.323617	66.255809
1426.764199	53.100947	66.260814
1426.733089	40.330839	66.265818
1426.358175	47.926654	66.270823
1425.589167	50.269518	66.275828
1424.495638	47.947492	66.280833
1423.564402	47.112221	66.285838
1423.110048	43.782410	66.290842
1422.773636	52.234491	66.295847
1422.224491	49.054715	66.300852
1421.399605	49.473023	66.305857
1420.229351	52.632165	66.310862
1419.917763	56.432190	66.315866
1419.604964	53.511154	66.320871
1418.663419	46.288736	66.325876
1417.904500	45.358053	66.330881
1417.020332	47.734050	66.335886
1416.750091	47.903876	66.340890
1415.936074	53.228649	66.345895
1415.802862	46.949004	66.350900
1414.939512	39.144022	66.355905
1413.798879	42.501373	66.360910
1413.551326	45.398371	66.365914
1412.988812	41.784721	66.370919
1411.895636	44.924355	66.375924
1411.339400	41.853158	66.380929
1410.470171	41.868946	66.385934
1410.353427	38.608449	66.390938
1409.925392	40.062067	66.395943
1409.141294	37.871019	66.400948
1408.402349	41.450521	66.405953
1407.347656	51.766652	66.410958
1406.719457	42.837523	66.415962
1405.647494	46.244698	66.420967
1405.088493	44.183270	66.425972
1404.316053	37.212164	66.430977
1403.517766	45.127540	66.435982
1403.576487	46.780459	66.440986
1402.688730	45.436852	66.445991
1402.657122	52.182890	66.450996
1402.377810	42.381317	66.456001
1400.971971	49.495603	66.461006
1400.721600	46.670853	66.466010
1399.306286	42.516766	66.471015
1398.482972	41.193313	66.476020
1398.038478	41.750976	66.481025
1397.382847	42.819626	66.486030
1396.854015	42.429009	66.491034
1396.643980	46.023762	66.496039
1395.651943	43.348466	66.501044
1395.365530	40.973155	66.506049
1394.275097	47.862540	66.511054
1393.792324	41.975877	66.516058
1392.447987	52.239357	66.521063
1391.668948	44.706512	66.526068
1391.590214	34.774300	66.531073
1390.419826	50.227360	66.536078
1390.267556	40.129715	66.541082
1390.042813	41.347230	66.546087
1389.643457	46.416296	66.551092
1388.357126	39.466450	66.556097
1387.402554	42.876822	66.561102
1387.265845	37.732202	66.566106
1386.093241	38.447262	66.571111
1385.204681	38.086250	66.576116
1384.751169	37.327494	66.581121
1384.228640	45.074096	66.586126
1384.063500	43.609957	66.591130
1383.688450	43.786278	66.596135
1382.684791	43.292608	66.601140
1382.193249	46.642668	66.606145
1380.973930	55.388770	66.611150
1379.962553	48.414751	66.616154
1378.985064	50.603843	66.621159
1378.601151	50.264996	66.626164
1378.444400	51.348905	66.631169
1377.666934	47.615746	66.636174
1377.304969	47.774829	66.641178
1377.113769	49.716437	66.646183
1376.286636	51.768482	66.651188
1375.506622	39.140788	66.656193
1374.060881	44.307658	66.661198
1373.105813	43.860538	66.666202
1372.569866	50.966838	66.671207
1372.259411	44.446762	66.676212
1371.805331	41.147700	66.681217
1371.370140	51.128457	66.686222
1370.562312	41.076324	66.691226
1370.242070	46.061983	66.696231
1369.167845	55.448349	66.701236
1368.477023	49.760320	66.706241
1368.026309	50.391679	66.711246
1367.187875	46.571858	66.716250
1366.216002	50.199527	66.721255
1365.367017	53.624592	66.726260
1365.546163	44.317281	66.731265
1364.931675	61.389456	66.736270
1364.154032	48.794112	66.741274
1363.027920	62.927169	66.746279
1362.226245	50.910649	66.751284
1362.050045	50.703212	66.756289
1361.349477	55.968705	66.761294
1360.697715	51.697344	66.766298
1359.956359	49.643848	66.771303
1358.891940	54.026274	66.776308
1358.925965	49.062416	66.781313
1358.066594	55.991200	66.786318
1357.163467	49.830328	66.791322
1356.392941	48.810067	66.796327
1355.717635	43.829089	66.801332
1355.484572	47.510676	66.806337
1354.732912	51.822985	66.811342
1353.705568	51.674017	66.816346
1352.906866	56.637376	66.821351
1352.442159	50.774465	66.826356
1352.256719	49.956402	66.831361
1351.486277	57.171529	66.836366
1350.935942	48.535776	66.841370
1349.724844	49.918587	66.846375
1349.310830	49.735282	66.851380
1349.405661	44.290908	66.856385
1347.981535	51.187294	66.861390
1347.335718	41.065988	66.866394
1347.001642	40.651905	66.871399
1346.014799	43.020226	66.876404
1344.906856	44.612736	66.881409
1344.221390	48.676095	66.886414
1344.094254	47.209398	66.891418
1343.526466	53.515532	66.896423
1342.672904	50.621156	66.901428
1342.482352	38.949621	66.906433
1341.122926	49.164771	66.911438
1340.822807	48.002805	66.916442
1339.882926	47.417703	66.921447
1339.617161	38.457731	66.926452
1338.946146	48.871995	66.931457
1338.003781	52.569614	66.936462
1337.256400	50.144540	66.941466
1336.719157	51.304637	66.946471
1336.168347	57.050524	66.951476
1335.806178	47.297878	66.956481
1334.519222	41.991762	66.961486
1334.121156	41.113788	66.966490
1333.610991	46.921395	66.971495
1332.857431	44.729079	66.976500
1332.760692	44.472517	66.981505
1331.330381	52.001909	66.986510
1330.640605	48.494920	66.991514
1330.128969	40.431997	66.996519
1329.727138	47.430869	67.001524
1328.525151	40.204117	67.006529
1327.353906	49.132248	67.011534
1326.884310	47.307749	67.016538
1326.598521	48.326122	67.021543
1325.985817	47.905661	67.026548
1325.871536	40.592967	67.031553
1325.615968	55.883905	67.036558
1324.449624	40.292503	67.041562
1323.245469	41.465325	67.046567
1322.572752	45.070603	67.051572
1322.713083	46.372854	67.056577
1321.812424	51.964693	67.061582
1320.975526	44.749255	67.066586
1319.957126	50.677023	67.071591
1319.690741	51.754835	67.076596
1319.344138	46.558916	67.081601
1318.672051	48.063399	67.086606
1317.565377	49.213614	67.091610
1316.987088	46.325013	67.096615
1316.368532	53.167576	67.101620
1315.771442	52.131052	67.106625
1314.154259	59.423638	67.111630
1313.891626	49.586063	67.116634
1313.748191	50.786505	67.121639
1312.861495	52.510481	67.126644
1312.663797	49.272925	67.131649
1312.080135	49.870603	67.136654
1311.048026	45.467794	67.141658
1310.351976	51.826674	67.146663
1309.944036	51.851928	67.151668
1309.388316	46.646022	67.156673
1308.039757	50.710405	67.161678
1307.731131	52.698563	67.166682
1307.030788	51.626034	67.171687
1306.622390	65.444793	67.176692
1306.161051	51.029347	67.181697
1305.242352	56.390209	67.186702
1304.529460	46.517618	67.191706
1303.928837	45.852736	67.196711
1302.817536	49.975182	67.201716
1301.727526	41.873520	67.206721
1301.286180	43.624279	67.211726
1300.870613	50.175525	67.216730
1300.752201	42.533162	67.221735
1300.302340	47.347994	67.226740
1299.303683	40.090784	67.231745
1298.347497	43.362505	67.236750
1297.815253	45.349078	67.241754
1297.386206	42.210731	67.246759
1296.190331	50.245101	67.251764
1295.450189	44.350409	67.256769
1294.770259	49.099634	67.261774
1294.223466	49.411542	67.266778
1294.096876	45.355800	67.271783
1293.249039	52.528918	67.276788
1293.122650	41.133364	67.281793
1291.839433	50.602486	67.286798
1291.225325	42.283573	67.291802
1290.599939	35.792953	67.296807
1290.174192	39.677253	67.301812
1289.418221	37.579301	67.306817
1288.139281	48.692873	67.311822
1287.883606	43.797167	67.316826
1287.514447	38.915365	67.321831
1286.305372	50.069870	67.326836
1285.693494	45.055152	67.331841
1284.878931	45.100286	67.336846
1284.358644	48.748943	67.341850
1283.959922	39.070066	67.346855
1283.320953	50.353540	67.351860
1283.045434	39.665592	67.356865
1282.237521	48.405218	67.361870
1281.232041	37.603039	67.366874
1280.817526	42.649044	67.371879
1280.069956	39.796929	67.376884
1279.466608	37.051961	67.381889
1278.720499	45.040120	67.386894
1278.403329	48.797682	67.391898
1277.912602	39.341389	67.396903
1276.202963	47.745543	67.401908
1275.973105	42.772001	67.406913
1275.334576	49.559961	67.411918
1275.080597	52.988958	67.416922
1273.866160	36.807026	67.421927
1272.890955	39.217575	67.426932
1272.404400	39.791923	67.431937
1271.788689	49.083617	67.436942
1271.670763	36.260111	67.441946
1271.367306	37.041128	67.446951
1269.811383	46.748375	67.451956
1269.305338	43.277046	67.456961
1268.592511	53.924251	67.461966
1268.394980	45.065889	67.466970
1267.431062	41.487825	67.471975
1266.729019	51.370588	67.476980
1266.374003	45.084327	67.481985
1265.544672	51.185778	67.486990
1265.057159	43.121894	67.491994
1263.957079	45.884202	67.496999
1262.804304	49.385760	67.502004
1262.589937	44.232734	67.507009
1261.832465	51.437354	67.512014
1261.562192	54.341009	67.517018
1261.631283	45.130306	67.522023
1260.232509	53.820704	67.527028
1259.263421	49.069240	67.532033
1258.674195	52.772727	67.537038
1258.390557	48.717822	67.542042
1257.706409	43.070514	67.547047
1256.544235	40.795806	67.552052
1256.111785	31.509931	67.557057
1255.762317	43.421172	67.562062
1255.103496	47.716807	67.567066
1254.290488	41.864204	67.572071
1253.393586	43.342844	67.577076
1253.113315	47.222372	67.582081
1252.458299	47.300193	67.587086
1251.622987	50.261901	67.592090
1250.789049	47.398130	67.597095
1249.863839	52.281715	67.602100
1249.625227	49.695742	67.607105
1249.024196	49.600513	67.612110
1248.208413	47.752796	67.617114
1247.336210	49.953489	67.622119
1246.825285	42.924224	67.627124
1246.181741	47.749324	67.632129
1245.866316	50.117182	67.637134
1245.409662	53.917967	67.642138
1245.028033	40.808047	67.647143
1244.199270	51.476678	67.652148
1243.362083	42.258907	67.657153
1242.057169	48.967939	67.662158
1241.421039	51.010195	67.667162
1241.195842	47.144225	67.672167
1240.324557	47.561822	67.677172
1239.523250	48.270582	67.682177
1238.498469	49.374427	67.687182
1238.027603	51.717190	67.692186
1237.603673	46.401501	67.697191
1237.086303	50.914488	67.702196
1236.918751	45.710030	67.707201
1235.838211	42.948479	67.712206
1234.918240	53.473657	67.717210
1234.503911	46.161026	67.722215
1233.678254	52.035283	67.727220
1233.315672	36.831288	67.732225
1231.928883	48.977361	67.737230
1231.267599	38.953465	67.742234
1230.897801	46.745365	67.747239
1230.621532	40.824558	67.752244
1230.744807	47.302103	67.757249
1229.456706	43.185105	67.762254
1228.825826	44.032049	67.767258
1228.113643	44.669897	67.772263
1226.954718	43.723653	67.777268
1226.120548	49.083867	67.782273
1225.576441	42.959454	67.787278
1224.859714	42.759700	67.792282
1224.688818	40.340944	67.797287
1223.973542	52.018385	67.802292
1223.245578	37.733485	67.807297
1222.533714	45.137524	67.812302
1221.895699	39.656791	67.817306
1221.589437	33.931377	67.822311
1220.287136	40.181695	67.827316
1219.676878	41.515742	67.832321
1219.317552	42.867615	67.837326
1218.386602	48.708191	67.842330
1218.376654	46.925399	67.847335
1216.815878	51.245203	67.852340
1216.198840	41.060584	67.857345
1214.998634	46.504780	67.862350
1214.607422	50.914858	67.867354
1214.504922	36.989432	67.872359
1213.868675	38.145965	67.877364
1213.816422	35.803208	67.882369
1213.618928	37.422227	67.887374
1212.483176	50.724475	67.892378
1211.719830	33.363686	67.897383
1210.215548	39.805684	67.902388
1209.338012	44.920703	67.907393
1208.758607	27.820520	67.912398
1208.193417	49.607414	67.917402
1208.058835	42.173477	67.922407
1207.405036	40.170146	67.927412
1207.193312	47.839461	67.932417
1206.316559	48.082746	67.937422
1205.589887	45.251143	67.942426
1204.921970	41.595575	67.947431
1203.970983	50.134319	67.952436
1203.103078	39.009019	67.957441
1202.411336	38.574871	67.962446
1201.956936	41.503734	67.967450
1201.622706	35.195771	67.972455
1200.999883	48.810047	67.977460
1200.100356	38.822212	67.982465
1199.365525	40.088384	67.987470
1198.594174	51.184929	67.992474
1198.353423	46.823887	67.997479
1197.266986	46.131279	68.002484
1196.534880	42.236846	68.007489
1195.540322	43.440519	68.012494
1195.042538	45.988014	68.017498
1194.653502	43.094264	68.022503
1194.206344	45.277452	68.027508
1193.780908	52.033275	68.032513
1193.132978	51.654386	68.037518
1192.453173	47.338518	68.042522
1191.806974	32.252567	68.047527
1190.905349	47.559757	68.052532
1190.075809	42.324573	68.057537
1189.276037	46.041613	68.062542
1188.780588	38.506052	68.067546
1188.779490	48.667469	68.072551
1187.420521	43.597928	68.077556
1186.207152	40.134037	68.082561
1185.607288	42.337054	68.087566
1184.993254	38.403857	68.092570
1184.656709	35.531515	68.097575
1184.454959	46.386067	68.102580
1184.177125	34.561751	68.107585
1183.184212	47.702575	68.112590
1182.453040	54.249048	68.117594
1181.927585	43.035120	68.122599
1180.405823	44.576549	68.127604
1179.921458	49.020339	68.132609
1179.094013	50.764190	68.137614
1178.833493	45.847221	68.142618
1178.717309	42.772947	68.147623
1177.937193	55.191325	68.152628
1177.348960	37.435053	68.157633
1176.840196	50.163397	68.162638
1175.889102	46.109497	68.167642
1174.870608	48.064077	68.172647
1173.825255	48.084405	68.177652
1173.572126	36.333223	68.182657
1173.038509	38.011372	68.187662
1172.998678	52.612489	68.192666
1172.191713	41.709646	68.197671
1170.968044	46.146997	68.202676
1170.480059	37.817570	68.207681
1169.080971	39.821131	68.212686
1168.138163	49.145938	68.217690
1168.430614	37.484493	68.222695
1167.305985	45.360635	68.227700
1167.128339	37.977891	68.232705
1166.918041	46.055492	68.237710
1166.259969	47.647588	68.242714
1164.947740	49.632727	68.247719
1164.334550	50.573751	68.252724
1163.728990	43.179802	68.257729
1163.000028	45.929900	68.262734
1162.060213	48.875172	68.267738
1161.277441	43.059253	68.272743
1160.504129	50.840906	68.277748
1160.338071	39.210994	68.282753
1159.912198	44.773659	68.287758
1159.466480	47.160671	68.292762
1159.311774	41.986389	68.297767
1157.897866	50.939514	68.302772
1156.976853	48.848528	68.307777
1156.480888	48.959521	68.312782
1155.797802	58.083951	68.317786
1154.786062	48.687282	68.322791
1153.978612	49.483945	68.327796
1153.583080	46.815510	68.332801
1153.301528	40.496163	68.337806
1152.562454	41.788330	68.342810
1152.568053	40.551534	68.347815
1151.399246	50.838283	68.352820
1150.634379	48.346371	68.357825
1150.071074	49.451740	68.362830
1148.747997	51.529526	68.367834
1147.906085	39.464706	68.372839
1147.160910	46.568153	68.377844
1147.134484	43.323783	68.382849
1146.792966	43.297417	68.387854
1146.388283	47.951764	68.392858
1145.875389	37.571709	68.397863
1144.821078	37.314906	68.402868
1144.012868	35.784055	68.407873
1143.435399	43.915443	68.412878
1141.998004	39.161700	68.417882
1141.209952	41.194849	68.422887
1140.587471	41.384740	68.427892
1140.024261	46.100570	68.432897
1140.390360	47.452968	68.437902
1139.472286	49.142873	68.442906
1139.775911	40.064517	68.447911
1138.166874	53.173483	68.452916
1137.623206	47.149267	68.457921
1137.028087	44.541060	68.462926
1135.775605	52.378315	68.467930
1134.992381	42.626754	68.472935
1134.220235	53.122285	68.477940
1134.011066	51.205061	68.482945
1133.705268	46.091780	68.487950
1132.916873	52.245442	68.492954
1132.004985	49.334255	68.497959
1131.188307	41.380045	68.502964
1130.705019	49.427025	68.507969
1130.156393	43.977184	68.512974
1129.123116	44.021505	68.517978
1128.480634	42.749238	68.522983
1128.131166	45.353838	68.527988
1127.632660	44.559393	68.532993
1127.522612	43.763563	68.537998
1126.301842	51.516840	68.543002
1125.677992	40.321354	68.548007
1124.679540	50.249348	68.553012
1123.726593	46.034733	68.558017
1122.647210	43.067759	68.563022
1122.307333	42.679947	68.568026
1122.792357	36.510386	68.573031
1121.492864	46.105075	68.578036
1121.292488	43.216133	68.583041
1120.484223	42.854840	68.588046
1119.173191	43.326045	68.593050
1118.730821	36.642682	68.598055
1118.036934	55.619517	68.603060
1117.757100	51.172415	68.608065
1116.821914	45.242873	68.613070
1115.790365	51.325677	68.618074
1115.471865	43.869559	68.623079
1114.977306	50.038827	68.628084
1114.511461	43.888401	68.633089
1113.402010	44.019186	68.638094
1112.618824	48.698873	68.643098
1112.540393	39.775933	68.648103
1111.780134	52.105652	68.653108
1110.889281	52.615828	68.658113
1110.255298	45.171101	68.663118
1109.301100	50.660822	68.668122
1109.375966	48.614442	68.673127
1108.515096	49.398944	68.678132
1107.480655	45.512087	68.683137
1106.775422	47.822362	68.688142
1105.991938	54.165440	68.693146
1105.581282	38.314870	68.698151
1105.120299	50.376643	68.703156
1104.111649	43.618146	68.708161
1103.382458	42.606639	68.713166
1102.734226	46.842450	68.718170
1102.515050	45.358368	68.723175
1102.077680	41.151393	68.728180
1100.769404	47.438284	68.733185
1100.123744	51.376435	68.738190
1099.512395	51.510743	68.743194
1099.403947	45.214258	68.748199
1098.703417	53.135814	68.753204
1097.178934	55.146263	68.758209
1096.571220	47.733749	68.763214
1096.266798	44.458829	68.768218
1096.192290	43.016288	68.773223
1095.439657	54.208707	68.778228
1094.330212	43.791078	68.783233
1093.785451	44.740128	68.788238
1092.975244	48.393049	68.793242
1092.662465	38.856194	68.798247
1091.176269	45.170000	68.803252
1090.326356	45.032938	68.808257
1090.286698	44.086510	68.813262
1089.284399	47.368133	68.818266
1089.239980	50.132070	68.823271
1088.457590	54.287046	68.828276
1088.484094	48.886748	68.833281
1087.503537	46.110481	68.838286
1086.411123	55.037781	68.843290
1086.288761	40.793291	68.848295
1085.048848	44.537950	68.853300
1084.356391	46.031738	68.858305
1083.578235	47.550464	68.863310
1082.846486	58.677735	68.868314
1082.628001	43.494882	68.873319
1082.100475	50.163587	68.878324
1081.113337	52.415958	68.883329
1080.776878	46.283643	68.888334
1079.623964	55.705620	68.893338
1079.502739	49.331590	68.898343
1078.594523	52.624737	68.903348
1077.713387	46.393463	68.908353
1077.269091	38.512864	68.913358
1076.388852	51.917416	68.918362
1076.146596	47.146533	68.923367
1075.087245	49.462978	68.928372
1074.581734	47.703077	68.933377
1074.812969	48.654242	68.938382
1072.816558	52.595547	68.943386
1072.047529	43.421411	68.948391
1071.532781	59.657448	68.953396
1071.249881	50.300200	68.958401
1070.805302	43.517751	68.963406
1070.329352	44.432916	68.968410
1070.001302	39.084257	68.973415
1068.537139	57.085021	68.978420
1067.657697	51.180283	68.983425
1067.551020	53.347807	68.988430
1066.857728	45.091049	68.993434
1066.061236	39.585381	68.998439
1065.257961	48.067661	69.003444
1064.706036	50.297612	69.008449
1064.335982	45.249419	69.013454
1062.842087	45.415653	69.018458
1062.134577	34.564496	69.023463
1061.804580	45.116936	69.028468
1061.263109	43.605551	69.033473
1060.972062	35.500567	69.038478
1060.282560	44.901209	69.043482
1059.342473	44.512371	69.048487
1058.393651	55.957456	69.053492
1057.947121	53.186849	69.058497
1057.862021	44.900943	69.063502
1057.074859	49.001084	69.068506
1056.109253	44.048164	69.073511
1055.295092	42.348619	69.078516
1054.936005	45.725357	69.083521
1053.930429	44.161215	69.088526
1052.842697	48.637283	69.093530
1052.210676	54.923247	69.098535
1051.891729	49.162523	69.103540
1051.295323	47.240961	69.108545
1051.283652	47.520467	69.113550
1050.529046	45.913351	69.118554
1049.637895	44.149625	69.123559
1048.930857	43.899293	69.128564
1047.899873	43.064994	69.133569
1048.003744	40.086460	69.138574
1046.821849	41.176984	69.143578
1045.770050	36.298827	69.148583
1045.120808	50.591406	69.153588
1044.716219	42.397317	69.158593
1044.378124	42.673513	69.163598
1043.525845	51.932307	69.168602
1042.864808	43.433203	69.173607
1041.949200	48.137548	69.178612
1041.610204	36.335571	69.183617
1041.629695	37.604821	69.188622
1040.075226	49.654511	69.193626
1039.436892	33.435604	69.198631
1038.794572	45.409219	69.203636
1038.464629	35.444678	69.208641
1038.002426	32.737153	69.213646
1036.468469	36.628484	69.218650
1035.822836	34.629308	69.223655
1035.540227	36.396320	69.228660
1035.505231	35.652374	69.233665
1034.843795	29.010883	69.238670
1033.316465	41.830354	69.243674
1032.967510	26.216342	69.248679
1032.418141	37.446966	69.253684
1031.539434	38.349398	69.258689
1030.633160	28.514345	69.263694
1030.149753	46.285180	69.268698
1029.779524	29.652098	69.273703
1029.338456	36.994378	69.278708
1028.632326	31.742838	69.283713
1027.878547	28.544089	69.288718
1026.719328	36.672079	69.293722
1026.364192	30.202335	69.298727
1025.762079	30.291257	69.303732
1024.886616	33.576036	69.308737
1024.590210	27.601079	69.313742
1023.208266	39.324393	69.318746
1023.015553	36.347310	69.323751
1022.935161	35.613901	69.328756
1021.644638	35.358498	69.333761
1021.279272	35.222941	69.338766
1020.209243	34.717423	69.343770
1019.611674	45.186610	69.348775
1019.023187	36.101568	69.353780
1018.033834	30.071996	69.358785
1017.172133	30.518777	69.363790
1016.328820	36.292659	69.368794
1016.656327	29.015262	69.373799
1015.709248	27.405590	69.378804
1015.075767	33.199586	69.383809
1014.777572	30.605286	69.388814
1013.887179	32.029957	69.393818
1013.124743	34.309381	69.398823
1012.350245	35.300543	69.403828
1012.292752	34.425456	69.408833
1011.832326	24.214077	69.413838
1010.362319	39.377030	69.418842
1010.039152	39.681066	69.423847
1009.571814	33.590125	69.428852
1008.456181	34.723781	69.433857
1007.599207	39.997136	69.438862
1006.968541	40.361725	69.443866
1006.659002	32.023877	69.448871
1006.181256	35.756838	69.453876
1004.916822	38.351561	69.458881
1004.220078	27.076629	69.463886
1003.394133	40.206232	69.468890
1003.139583	32.066983	69.473895
1002.564867	31.993330	69.478900
1002.005931	35.311533	69.483905
1002.012294	37.381147	69.488910
1000.456159	33.143948	69.493914
1000.164156	33.525932	69.498919
999.470197	35.936123	69.503924
998.052081	34.310414	69.508929
997.542324	35.364788	69.513934
996.758958	38.541436	69.518938
996.591457	35.172426	69.523943
996.341472	42.115688	69.528948
995.658502	30.878264	69.533953
995.161613	38.213526	69.538958
993.966729	40.386231	69.543962
993.719416	36.925499	69.548967
992.377010	44.094920	69.553972
991.339521	32.954916	69.558977
991.012803	36.517154	69.563982
990.561556	42.838865	69.568986
990.297053	36.441625	69.573991
989.678819	43.586892	69.578996
988.928883	36.503877	69.584001
988.202002	37.329397	69.589006
987.536581	43.351883	69.594010
987.083309	40.111544	69.599015
985.823986	37.098058	69.604020
984.774046	34.332909	69.609025
984.106927	42.947393	69.614030
984.135437	35.132282	69.619034
983.528071	34.779632	69.624039
983.254640	36.452317	69.629044
982.450957	37.411378	69.634049
981.525844	37.012886	69.639054
981.003205	52.424119	69.644058
980.016843	36.866771	69.649063
979.216390	33.759703	69.654068
978.091663	46.542212	69.659073
978.053274	41.214611	69.664078
977.499585	39.676910	69.669082
977.265319	34.516271	69.674087
976.705274	38.989606	69.679092
975.448828	43.401032	69.684097
975.120777	37.351764	69.689102
974.232109	34.768199	69.694106
973.683013	39.172163	69.699111
972.749173	34.914449	69.704116
972.217110	44.031961	69.709121
972.223504	41.542597	69.714126
970.811204	44.072261	69.719130
970.125440	43.576337	69.724135
969.511490	40.469301	69.729140
968.679832	42.768086	69.734145
968.427165	36.764722	69.739150
967.168058	36.922748	69.744154
966.439993	38.790524	69.749159
966.439665	47.854867	69.754164
965.338660	47.518473	69.759169
965.259255	38.322574	69.764174
964.512172	47.521910	69.769178
963.340916	38.919163	69.774183
962.714328	47.267775	69.779188
962.262721	43.531784	69.784193
961.924309	38.162810	69.789198
960.972932	46.643620	69.794202
960.088355	41.026750	69.799207
959.595749	51.922811	69.804212
958.946019	48.017472	69.809217
958.828782	40.759793	69.814222
957.769613	46.742748	69.819226
957.005465	48.113048	69.824231
956.790788	38.672699	69.829236
955.611747	47.013692	69.834241
955.106061	40.875249	69.839246
954.178364	39.533438	69.844250
953.461143	40.909516	69.849255
953.108356	38.346673	69.854260
952.439627	47.403519	69.859265
951.507802	43.563072	69.864270
950.149433	43.194183	69.869274
950.044362	38.765327	69.874279
949.697156	43.535750	69.879284
948.961452	46.216768	69.884289
949.042851	38.278923	69.889294
948.165903	38.903187	69.894298
947.211457	40.952623	69.899303
946.839178	44.677395	69.904308
945.936132	39.941147	69.909313
944.795882	35.581428	69.914318
943.785535	38.557364	69.919322
943.344543	33.059917	69.924327
943.204824	37.744279	69.929332
942.831974	42.911836	69.934337
942.396533	29.087693	69.939342
941.103595	44.154418	69.944346
940.436525	36.919860	69.949351
939.594596	46.210436	69.954356
939.664460	48.417983	69.959361
938.849644	34.905902	69.964366
937.856987	36.968199	69.969370
937.433072	38.542322	69.974375
936.265205	40.690282	69.979380
935.053782	45.332414	69.984385
934.423430	43.111173	69.989390
934.382010	41.344829	69.994394
933.761397	34.272441	69.999399
933.292137	38.802069	70.004404
932.447610	46.443968	70.009409
932.442008	33.071180	70.014414
931.417000	29.146443	70.019418
930.605329	39.985435	70.024423
930.114986	33.245587	70.029428
929.377744	32.019577	70.034433
928.777199	27.569010	70.039438
927.399713	42.180503	70.044442
926.809534	37.246605	70.049447
926.717366	32.527006	70.054452
926.157006	40.933743	70.059457
925.729616	34.453888	70.064462
924.619112	32.789333	70.069466
923.997874	31.383991	70.074471
923.398781	31.522537	70.079476
922.422140	40.516858	70.084481
921.739292	37.572807	70.089486
920.736095	41.984684	70.094490
920.215809	28.900171	70.099495
920.357726	33.966142	70.104500
919.623472	44.450845	70.109505
919.635426	32.249334	70.114510
917.852930	36.673106	70.119514
917.465449	40.584814	70.124519
916.903914	34.154381	70.129524
916.189481	46.501907	70.134529
915.060499	40.246023	70.139534
914.364641	36.292545	70.144538
913.680677	42.652536	70.149543
913.654570	39.987960	70.154548
912.961313	38.298127	70.159553
912.280007	30.981548	70.164558
911.150599	34.744813	70.169562
910.733751	33.755232	70.174567
910.674810	43.334052	70.179572
909.323241	44.480115	70.184577
908.459475	29.851885	70.189582
907.667707	33.628372	70.194586
907.136393	35.540611	70.199591
907.075298	34.541414	70.204596
906.608607	42.928557	70.209601
905.517258	32.542636	70.214606
904.550576	39.551016	70.219610
903.776161	34.205017	70.224615
903.615710	35.177075	70.229620
903.113976	33.174194	70.234625
902.579229	29.362459	70.239630
901.739624	37.169293	70.244634
900.979371	29.940444	70.249639
900.085503	29.837390	70.254644
898.789415	39.915054	70.259649
898.127183	34.362748	70.264654
897.792809	41.651628	70.269658
897.330151	35.755287	70.274663
897.211778	42.194453	70.279668
896.428236	50.079318	70.284673
896.419642	36.013924	70.289678
895.587685	39.278246	70.294682
894.446679	34.699209	70.299687
893.405451	36.928903	70.304692
892.348684	34.625186	70.309697
891.892800	32.409990	70.314702
891.147930	36.219892	70.319706
890.699708	38.494066	70.324711
890.550441	37.025654	70.329716
890.005612	39.774639	70.334721
889.466497	31.536127	70.339726
888.051253	37.016421	70.344730
887.845629	35.636606	70.349735
887.613268	41.209946	70.354740
886.221213	42.076780	70.359745
885.570586	37.680978	70.364750
884.779917	38.175613	70.369754
884.515976	45.411776	70.374759
883.960452	34.698836	70.379764
882.588470	46.476915	70.384769
882.303398	39.866116	70.389774
881.597936	43.172718	70.394778
881.111054	46.604507	70.399783
880.613666	33.363324	70.404788
879.479963	39.994546	70.409793
878.552936	38.231475	70.414798
877.956700	38.294147	70.419802
877.693500	38.548448	70.424807
877.685857	31.896057	70.429812
876.708654	43.162858	70.434817
875.938088	38.926540	70.439822
875.259977	43.559834	70.444826
874.722088	42.142591	70.449831
873.830472	38.262910	70.454836
872.729347	41.544128	70.459841
872.220547	39.514830	70.464846
871.742150	45.980531	70.469850
871.518446	42.651941	70.474855
870.749561	44.110691	70.479860
870.117798	45.257023	70.484865
869.241174	43.480189	70.489870
868.082378	42.855705	70.494874
867.680857	43.982338	70.499879
866.851240	38.349763	70.504884
866.166299	38.981416	70.509889
865.646652	41.506628	70.514894
865.167380	53.669811	70.519898
864.806685	45.249560	70.524903
864.335059	41.968172	70.529908
862.844810	45.284070	70.534913
862.970410	41.851050	70.539918
862.186779	38.752571	70.544922
860.759564	44.592931	70.549927
860.430307	43.829918	70.554932
859.513866	44.120323	70.559937
859.373530	34.388588	70.564942
859.000569	43.202943	70.569946
858.174935	46.724332	70.574951
857.165403	44.939477	70.579956
856.320230	50.883032	70.584961
855.943131	38.942757	70.589966
855.583767	40.683846	70.594970
854.908555	53.350695	70.599975
853.920726	38.100734	70.604980
853.106710	40.710312	70.609985
852.698213	35.157973	70.614990
852.313982	45.862974	70.619994
851.152379	42.094274	70.624999
850.341410	38.497611	70.630004
849.856281	40.848369	70.635009
849.742785	46.459374	70.640014
848.558603	35.894776	70.645018
847.480596	44.291107	70.650023
846.937841	33.155223	70.655028
846.263003	46.994308	70.660033
846.374759	36.118927	70.665038
846.148841	46.170793	70.670042
844.898693	49.421888	70.675047
844.365318	39.211581	70.680052
843.434192	47.555916	70.685057
842.774011	39.288016	70.690062
841.699624	38.953013	70.695066
840.930559	39.108051	70.700071
840.581218	32.869039	70.705076
839.915545	39.776135	70.710081
839.649859	38.249907	70.715086
839.464464	40.979566	70.720090
838.222849	42.556790	70.725095
837.481489	39.052411	70.730100
836.871415	45.084770	70.735105
835.941428	35.752358	70.740110
834.973607	42.801599	70.745114
834.158538	42.470729	70.750119
833.956136	44.831479	70.755124
833.306163	45.446095	70.760129
833.262269	43.039948	70.765134
833.004060	41.141013	70.770138
831.720549	43.997188	70.775143
831.475395	36.401455	70.780148
830.054057	42.637109	70.785153
829.212659	31.790792	70.790158
828.528030	44.235049	70.795162
827.425399	39.197901	70.800167
827.525031	39.999498	70.805172
827.135562	39.413766	70.810177
826.688817	41.221532	70.815182
825.607771	42.273519	70.820186
824.808669	47.500276	70.825191
824.367196	47.764591	70.830196
823.972858	42.419027	70.835201
823.215639	44.129193	70.840206
822.015563	42.710124	70.845210
821.616565	48.053075	70.850215
821.265720	38.921449	70.855220
819.902969	45.644809	70.860225
819.094231	41.053875	70.865230
818.685029	40.389423	70.870234
818.159597	43.602436	70.875239
818.169973	37.810598	70.880244
817.235554	47.005716	70.885249
816.299935	41.695635	70.890254
815.498286	45.938013	70.895258
814.919770	40.224152	70.900263
814.972660	36.461370	70.905268
813.442215	47.972146	70.910273
812.544533	36.935350	70.915278
812.162884	38.789201	70.920282
811.637167	42.543812	70.925287
811.841155	32.744027	70.930292
810.802273	39.304942	70.935297
810.063915	39.631164	70.940302
809.268216	38.921212	70.945306
808.283383	42.120552	70.950311
807.550540	37.001124	70.955316
806.304491	39.278945	70.960321
805.992119	41.157638	70.965326
805.709963	41.416769	70.970330
804.988652	40.156078	70.975335
804.875176	39.023363	70.980340
803.754333	47.726628	70.985345
803.163660	31.615679	70.990350
802.424233	32.160757	70.995354
801.760980	31.432856	71.000359
801.373661	30.891755	71.005364
800.096484	46.455111	71.010369
799.213704	34.739620	71.015374
798.735086	39.421244	71.020378
798.096079	43.643659	71.025383
797.884283	44.613463	71.030388
797.262219	41.910455	71.035393
796.918512	44.638418	71.040398
795.895672	43.595158	71.045402
795.076298	36.866695	71.050407
795.112589	32.988738	71.055412
793.790254	41.674413	71.060417
793.217217	41.683782	71.065422
792.497460	36.938279	71.070426
791.818063	41.102879	71.075431
791.579763	35.351272	71.080436
790.384169	41.136974	71.085441
789.771942	38.608325	71.090446
789.308991	44.442600	71.095450
788.771271	41.150045	71.100455
788.049147	39.858314	71.105460
786.765339	39.552485	71.110465
786.199939	35.986004	71.115470
785.954901	32.894750	71.120474
785.305799	38.084762	71.125479
784.856305	37.379454	71.130484
783.835558	39.784468	71.135489
783.119295	36.398558	71.140494
782.225583	35.988410	71.145498
781.938385	41.048540	71.150503
781.751318	37.072271	71.155508
780.882769	43.182459	71.160513
779.893581	48.794263	71.165518
779.171665	45.070654	71.170522
779.065511	46.781400	71.175527
778.037631	33.342972	71.180532
776.776995	43.557472	71.185537
776.152668	34.422574	71.190542
775.962115	38.149378	71.195546
775.453318	44.577263	71.200551
775.409674	38.196687	71.205556
773.918829	44.021917	71.210561
773.564088	34.986095	71.215566
773.105528	40.422928	71.220570
772.337217	43.502689	71.225575
770.998311	35.330153	71.230580
770.304456	45.922014	71.235585
770.171012	44.034867	71.240590
769.764570	33.890069	71.245594
769.323915	43.576497	71.250599
768.492492	41.377095	71.255604
767.624064	46.677308	71.260609
767.044519	44.529886	71.265614
765.916511	41.127672	71.270618
764.926733	41.486706	71.275623
764.617635	34.333360	71.280628
763.510446	38.332045	71.285633
763.493623	41.579114	71.290638
763.344961	36.941830	71.295642
761.923174	39.290815	71.300647
761.313036	33.987756	71.305652
760.841248	42.386430	71.310657
760.621012	38.037313	71.315662
759.829453	35.248484	71.320666
758.842476	37.446412	71.325671
758.021992	28.718130	71.330676
757.556860	41.680543	71.335681
756.992011	43.934444	71.340686
756.066506	39.381684	71.345690
755.044862	45.887949	71.350695
754.585093	37.708497	71.355700
754.576281	39.353623	71.360705
753.859996	35.295127	71.365710
753.016317	37.059190	71.370714
751.915653	41.734881	71.375719
751.718993	38.751388	71.380724
751.301860	43.181312	71.385729
750.430685	36.929471	71.390734
749.834669	39.399094	71.395738
748.509907	44.147515	71.400743
748.600487	36.160746	71.405748
747.469326	37.711965	71.410753
746.497085	43.016543	71.415758
745.932618	38.954146	71.420762
745.817370	40.321863	71.425767
745.361603	33.031022	71.430772
744.861179	40.654249	71.435777
743.119740	37.774340	71.440782
742.759258	36.888403	71.445786
741.792907	44.241729	71.450791
741.764554	41.885027	71.455796
741.621707	31.440884	71.460801
740.773534	36.403305	71.465806
739.566533	35.866449	71.470810
738.659879	46.148599	71.475815
738.499386	30.442768	71.480820
738.436027	38.269002	71.485825
737.088816	38.483230	71.490830
736.360632	33.988248	71.495834
736.108050	44.683323	71.500839
734.784289	31.665841	71.505844
733.855284	36.934198	71.510849
733.292276	32.814321	71.515854
732.658305	33.780267	71.520858
732.044256	38.093932	71.525863
732.020880	33.987790	71.530868
731.355080	34.622497	71.535873
730.951653	31.623509	71.540878
730.110665	33.254489	71.545882
729.079485	34.895552	71.550887
728.806633	28.156376	71.555892
727.741597	31.338285	71.560897
726.707902	40.348320	71.565902
726.071834	38.738716	71.570906
725.773436	42.653328	71.575911
725.799825	35.185950	71.580916
724.681378	41.653146	71.585921
723.649424	39.128125	71.590926
723.362290	39.890191	71.595930
722.806242	46.982980	71.600935
722.141284	36.826821	71.605940
720.978060	38.410379	71.610945
720.142198	37.572330	71.615950
720.180546	33.934010	71.620954
719.289816	41.382140	71.625959
718.372045	33.450094	71.630964
717.367117	42.693611	71.635969
717.054513	40.174432	71.640974
716.570465	39.104019	71.645978
716.091038	42.049829	71.650983
715.774076	38.178314	71.655988
714.761997	39.384684	71.660993
713.754284	40.979891	71.665998
713.395483	39.728557	71.671002
712.513305	39.657875	71.676007
711.534447	34.131427	71.681012
710.777189	33.407802	71.686017
710.344438	37.929607	71.691022
710.140478	35.304190	71.696026
709.525278	40.836935	71.701031
709.139570	37.354939	71.706036
707.828077	34.999383	71.711041
707.280465	32.758478	71.716046
706.505281	40.814017	71.721050
705.986025	43.530218	71.726055
705.804756	39.494544	71.731060
704.583797	49.772915	71.736065
703.545279	44.588641	71.741070
703.373776	39.343860	71.746074
702.674588	42.253903	71.751079
702.531884	38.315038	71.756084
701.284199	41.531007	71.761089
700.602314	45.649072	71.766094
700.262482	39.331083	71.771098
699.335361	38.561564	71.776103
698.369967	32.199965	71.781108
697.622247	41.869131	71.786113
697.074279	34.910655	71.791118
697.143220	32.342298	71.796122
696.179839	40.472708	71.801127
696.005849	29.683402	71.806132
695.085373	28.124105	71.811137
694.424985	25.992913	71.816142
693.673037	30.599003	71.821146
692.066292	32.035140	71.826151
691.461287	26.877261	71.831156
691.295269	40.189852	71.836161
690.509711	30.465658	71.841166
690.550355	28.082140	71.846170
689.588651	33.967518	71.851175
689.256061	28.928355	71.856180
687.877442	23.358303	71.861185
687.293783	31.859817	71.866190
687.125683	26.468020	71.871194
686.477507	38.675909	71.876199
686.400246	29.489154	71.881204
685.289079	33.097371	71.886209
684.281041	31.258620	71.891214
682.900555	29.219217	71.896218
681.815901	37.300538	71.901223
682.130090	34.175853	71.906228
681.449846	39.134774	71.911233
680.866122	36.431927	71.916238
680.773252	26.543283	71.921242
679.931320	39.608925	71.926247
679.173933	36.713605	71.931252
678.343570	37.405721	71.936257
677.629169	26.539669	71.941262
677.107425	34.198913	71.946266
675.635888	41.915884	71.951271
675.300199	28.430356	71.956276
674.602015	32.637260	71.961281
673.994004	35.178414	71.966286
674.100477	29.501565	71.971290
673.425669	34.469027	71.976295
672.632750	31.920436	71.981300
671.435400	30.401868	71.986305
670.904936	39.405428	71.991310
670.791515	27.226617	71.996314
669.660769	42.161375	72.001319
668.990412	33.737771	72.006324
668.217182	36.351439	72.011329
667.495895	34.373965	72.016334
667.416370	39.803098	72.021338
666.339569	44.407221	72.026343
665.822846	35.909140	72.031348
665.277039	30.488111	72.036353
664.510325	40.050406	72.041358
663.698222	25.879571	72.046362
662.828420	37.250741	72.051367
662.234207	29.393931	72.056372
661.835811	36.694170	72.061377
660.905499	34.473444	72.066382
660.442527	25.492503	72.071386
659.481028	37.984584	72.076391
658.989886	30.379312	72.081396
658.653647	31.761601	72.086401
658.067352	41.103525	72.091406
657.409264	35.618051	72.096410
656.327556	48.232176	72.101415
656.021185	30.647249	72.106420
655.712759	37.635248	72.111425
654.545365	40.571039	72.116430
653.518345	30.385357	72.121434
652.837450	37.941614	72.126439
652.416760	40.876971	72.131444
652.192703	37.460835	72.136449
650.957027	42.545311	72.141454
649.995015	37.568198	72.146458
649.590225	43.588291	72.151463
649.456394	37.362117	72.156468
648.676321	34.077554	72.161473
647.856461	35.627169	72.166478
647.510378	30.659398	72.171482
646.553303	34.303983	72.176487
645.838871	34.610342	72.181492
645.774438	28.036774	72.186497
644.443830	31.726013	72.191502
643.845665	29.469701	72.196506
643.180224	36.089811	72.201511
642.783665	28.614777	72.206516
641.981455	29.984931	72.211521
640.933853	32.532721	72.216526
641.000293	25.602410	72.221530
639.926437	32.256571	72.226535
639.663778	30.697078	72.231540
638.632781	33.338729	72.236545
637.583378	34.787153	72.241550
637.286394	27.861872	72.246554
636.431826	42.623007	72.251559
636.151873	35.210095	72.256564
635.303069	36.023002	72.261569
634.155369	37.851011	72.266574
633.758973	26.706290	72.271578
633.065798	27.669366	72.276583
632.732590	35.702866	72.281588
632.715964	34.328972	72.286593
631.554078	40.880595	72.291598
631.101098	22.503347	72.296602
630.046914	28.209191	72.301607
629.657758	26.599140	72.306612
628.748898	34.238661	72.311617
627.554712	32.474839	72.316622
627.424331	26.512538	72.321626
627.446047	28.116117	72.326631
626.170535	27.846803	72.331636
625.421904	30.837161	72.336641
624.458383	32.536122	72.341646
624.132641	22.130049	72.346650
623.427443	32.206377	72.351655
622.511313	33.954848	72.356660
621.565188	29.970888	72.361665
621.040910	33.681055	72.366670
620.759434	28.452759	72.371674
620.349976	27.502202	72.376679
620.016862	26.268580	72.381684
619.309371	28.675213	72.386689
618.416322	28.670355	72.391694
618.111572	26.007350	72.396698
616.531979	35.634709	72.401703
616.068900	29.243122	72.406708
615.345875	30.301309	72.411713
614.704182	31.230699	72.416718
614.455846	28.838276	72.421722
613.436236	31.001560	72.426727
612.705097	23.800161	72.431732
612.137785	25.742276	72.436737
611.027994	32.468910	72.441742
611.045919	20.851787	72.446746
610.450944	36.030256	72.451751
609.284440	27.382219	72.456756
608.647450	18.809243	72.461761
608.073189	28.807877	72.466766
608.025757	31.529687	72.471770
607.187621	26.024552	72.476775
606.160852	20.860799	72.481780
605.665123	32.163535	72.486785
604.893435	30.607184	72.491790
604.812454	27.839529	72.496794
603.509388	27.705198	72.501799
602.599403	25.279304	72.506804
602.145592	32.219977	72.511809
601.443128	37.723076	72.516814
601.389478	30.827155	72.521818
600.340569	29.128839	72.526823
599.425886	32.802088	72.531828
598.830658	29.220223	72.536833
598.222576	31.940597	72.541838
598.309111	30.215101	72.546842
596.803130	31.092061	72.551847
596.202664	35.138555	72.556852
595.534992	29.660264	72.561857
594.800359	28.750424	72.566862
594.681315	25.492346	72.571866
594.155040	31.866389	72.576871
593.079982	32.896479	72.581876
592.743496	24.076239	72.586881
591.835524	30.173462	72.591886
591.172350	32.044772	72.596890
589.871908	40.379383	72.601895
589.489708	37.684256	72.606900
588.963005	32.840986	72.611905
588.459893	38.530970	72.616910
588.159838	27.709206	72.621914
587.018342	28.874225	72.626919
586.204205	31.987516	72.631924
585.724151	30.067403	72.636929
585.274816	36.717986	72.641934
584.965791	25.516861	72.646938
583.407071	34.010584	72.651943
582.521761	31.551258	72.656948
582.153658	36.442496	72.661953
581.212052	37.829044	72.666958
581.326889	34.822980	72.671962
580.884172	35.158973	72.676967
579.988929	29.934796	72.681972
579.392688	29.271626	72.686977
578.551289	37.594688	72.691982
578.225582	27.907388	72.696986
577.462186	41.605331	72.701991
576.241525	30.594348	72.706996
575.829744	26.491610	72.712001
575.337121	37.874734	72.717006
574.977099	32.150719	72.722010
573.858950	39.200881	72.727015
573.045614	26.251138	72.732020
572.749279	23.971542	72.737025
571.890029	30.951290	72.742030
571.329559	33.487861	72.747034
570.155710	42.065244	72.752039
569.679830	32.763653	72.757044
569.298202	36.176635	72.762049
568.907827	38.706167	72.767054
568.549754	35.351288	72.772058
567.170526	35.747093	72.777063
566.562221	26.598451	72.782068
566.461451	36.169008	72.787073
565.460240	40.274302	72.792078
564.434278	31.604170	72.797082
563.836265	32.259651	72.802087
563.376723	32.770623	72.807092
563.093944	33.754175	72.812097
562.065957	41.346622	72.817102
561.198336	42.131189	72.822106
560.585030	40.109969	72.827111
560.027997	35.404523	72.832116
559.791646	35.613191	72.837121
558.186208	40.041476	72.842126
557.624022	31.429638	72.847130
556.930156	34.373518	72.852135
556.539241	33.747008	72.857140
556.235804	28.134084	72.862145
555.818769	42.986823	72.867150
555.358113	34.935053	72.872154
554.359959	38.038040	72.877159
553.629233	29.700199	72.882164
552.996022	29.122310	72.887169
551.866291	33.369224	72.892174
551.520618	24.130984	72.897178
550.572433	30.271811	72.902183
550.328742	36.480603	72.907188
548.926428	41.388005	72.912193
547.950832	40.406571	72.917198
547.721992	30.223100	72.922202
547.269771	35.768583	72.927207
546.690757	35.518099	72.932212
546.900041	25.278507	72.937217
546.104705	38.738382	72.942222
545.320113	23.555958	72.947226
544.093829	36.662986	72.952231
543.607710	35.592948	72.957236
542.796209	31.319902	72.962241
541.841707	31.843058	72.967246
541.572770	28.933542	72.972250
540.934077	29.658756	72.977255
540.433272	29.328165	72.982260
539.818497	30.606617	72.987265
538.515402	38.551713	72.992270
538.193282	26.919444	72.997274
537.862579	28.933122	73.002279
536.954251	32.301756	73.007284
536.136548	33.135797	73.012289
535.031318	40.419001	73.017294
534.689499	29.247974	73.022298
534.117980	32.481533	73.027303
533.961983	34.195688	73.032308
533.470255	35.723436	73.037313
532.288528	38.465930	73.042318
531.808296	28.043317	73.047322
531.040273	32.348250	73.052327
530.209697	26.867888	73.057332
529.522589	33.871431	73.062337
528.357269	30.105042	73.067342
528.085959	36.766172	73.072346
527.544968	29.515631	73.077351
527.496218	39.647240	73.082356
526.867084	30.784789	73.087361
525.294996	36.536371	73.092366
525.290469	30.579354	73.097370
524.650865	36.148263	73.102375
523.567440	35.077159	73.107380
522.953441	28.684212	73.112385
521.912488	34.751735	73.117390
521.614478	28.878163	73.122394
521.392742	31.915612	73.127399
520.802547	33.636275	73.132404
519.710566	24.364878	73.137409
518.610031	33.845439	73.142414
518.489103	34.805601	73.147418
517.831904	32.538504	73.152423
517.533925	30.643250	73.157428
516.459497	28.856964	73.162433
515.710134	35.665530	73.167438
515.497958	30.815349	73.172442
514.433197	34.636293	73.177447
513.460512	42.705165	73.182452
512.978577	34.299833	73.187457
512.106198	37.839933	73.192462
512.134496	32.742111	73.197466
511.587093	32.310962	73.202471
510.788913	40.200333	73.207476
509.743490	27.933762	73.212481
509.132623	38.550087	73.217486
508.881622	36.968870	73.222490
507.410023	34.927766	73.227495
506.800974	30.756608	73.232500
506.430907	35.649369	73.237505
505.721923	30.808533	73.242510
505.752109	33.607430	73.247514
504.836783	32.732514	73.252519
503.790868	28.173217	73.257524
503.290605	25.735161	73.262529
502.590670	35.950718	73.267534
502.025685	37.953627	73.272538
500.978327	36.888979	73.277543
500.166245	40.862408	73.282548
499.751275	24.678821	73.287553
499.292338	29.342479	73.292558
498.966576	25.427107	73.297562
498.351570	31.930430	73.302567
496.863112	36.618145	73.307572
496.355235	32.899362	73.312577
495.735607	38.069741	73.317582
495.629822	28.316746	73.322586
494.837284	30.977953	73.327591
493.846534	33.339198	73.332596
493.550485	31.631499	73.337601
492.566314	34.954718	73.342606
492.257230	28.430980	73.347610
491.065047	34.588366	73.352615
490.235243	37.699619	73.357620
489.867361	31.303580	73.362625
489.281116	35.710389	73.367630
489.122001	34.340783	73.372634
488.392338	30.908282	73.377639
487.502026	27.759084	73.382644
486.589750	33.006055	73.387649
486.124641	36.153889	73.392654
485.393256	31.655955	73.397658
484.581762	33.561772	73.402663
483.654726	31.325130	73.407668
483.273660	25.817487	73.412673
482.668145	33.440962	73.417678
482.524875	25.736643	73.422682
481.661196	32.060356	73.427687
480.893720	31.208264	73.432692
480.407146	38.318757	73.437697
479.561517	33.046631	73.442702
478.287912	31.667489	73.447706
477.658143	33.832282	73.452711
477.141006	34.273005	73.457716
476.921140	30.388037	73.462721
475.846907	40.563928	73.467726
475.653752	30.572894	73.472730
475.301716	34.738659	73.477735
474.149437	27.977331	73.482740
473.478759	27.917817	73.487745
472.910792	36.988590	73.492750
472.412937	33.766222	73.497754
472.033210	30.603345	73.502759
470.852329	34.613922	73.507764
470.688209	25.759824	73.512769
469.026848	36.505638	73.517774
468.310168	32.797773	73.522778
467.592955	30.061390	73.527783
467.240056	36.521381	73.532788
467.159964	33.146904	73.537793
466.520778	36.474560	73.542798
465.882094	39.847128	73.547802
465.027351	31.147688	73.552807
464.178414	43.043424	73.557812
463.432264	37.933453	73.562817
463.155328	39.137443	73.567822
462.638950	40.580612	73.572826
461.816586	37.920666	73.577831
461.126494	39.731872	73.582836
460.774052	35.244001	73.587841
459.380876	38.623500	73.592846
458.456335	37.785301	73.597850
458.033417	39.417706	73.602855
457.343194	34.706287	73.607860
457.249275	32.860144	73.612865
456.437029	38.028404	73.617870
455.425375	37.066195	73.622874
454.800794	35.989501	73.627879
454.289162	35.416842	73.632884
454.053611	28.366592	73.637889
453.291921	37.394778	73.642894
452.094842	38.846048	73.647898
451.497099	34.371795	73.652903
450.966954	37.459728	73.657908
450.927576	31.330672	73.662913
449.846238	38.383228	73.667918
448.766808	43.677404	73.672922
448.459620	42.748019	73.677927
447.790945	35.468848	73.682932
447.454728	39.191010	73.687937
445.969384	44.788812	73.692942
445.509529	43.509426	73.697946
444.908870	42.845846	73.702951
444.443556	46.149631	73.707956
444.448347	33.949015	73.712961
442.968553	36.795104	73.717966
442.318566	35.909465	73.722970
441.992070	39.527335	73.727975
441.150644	34.911301	73.732980
440.984764	42.734164	73.737985
439.931253	38.059347	73.742990
439.083715	34.370360	73.747994
438.748950	31.742512	73.752999
437.646524	35.539927	73.758004
436.832401	38.390752	73.763009
435.867367	34.711243	73.768014
435.323375	35.893503	73.773018
435.006264	37.030173	73.778023
434.639950	41.279305	73.783028
434.661811	33.236445	73.788033
433.729215	40.466003	73.793038
432.955023	41.438648	73.798042
432.167530	39.453614	73.803047
430.701516	45.657546	73.808052
430.405202	36.648084	73.813057
429.343787	44.045369	73.818062
428.922595	35.623329	73.823066
428.780558	38.319904	73.828071
428.130953	48.171999	73.833076
427.995165	38.673212	73.838081
427.013824	42.116347	73.843086
426.200455	36.353995	73.848090
425.042742	37.514332	73.853095
423.747232	40.065572	73.858100
423.443394	30.434941	73.863105
422.849301	34.707318	73.868110
422.485203	39.007777	73.873114
422.076188	33.028510	73.878119
421.449765	39.417357	73.883124
421.286454	34.867870	73.888129
420.399739	31.922532	73.893134
419.622716	30.852626	73.898138
419.053305	28.888640	73.903143
417.608684	32.059478	73.908148
416.956595	26.314490	73.913153
416.421613	28.862890	73.918158
415.981863	20.675343	73.923162
415.723673	28.903599	73.928167
415.398406	37.637931	73.933172
414.461733	24.553465	73.938177
413.632037	28.850822	73.943182
412.542618	33.725159	73.948186
411.696694	26.668207	73.953191
411.287581	36.767222	73.958196
410.401030	28.674398	73.963201
410.178818	32.645427	73.968206
409.808584	24.933831	73.973210
409.095767	31.470105	73.978215
407.876213	42.711373	73.983220
407.329782	22.197439	73.988225
406.530736	31.631477	73.993230
406.633358	29.467460	73.998234
405.676759	30.915422	74.003239
404.636612	34.082469	74.008244
404.242645	37.629408	74.013249
403.690378	36.409283	74.018254
402.483053	34.154382	74.023258
401.680532	25.452328	74.028263
401.140786	34.485898	74.033268
400.966254	28.348038	74.038273
400.459205	24.599920	74.043278
399.967384	26.190849	74.048282
398.937919	20.124906	74.053287
397.861974	24.625508	74.058292
397.396079	25.467565	74.063297
397.050617	31.946410	74.068302
396.370152	30.630632	74.073306
395.175633	22.210090	74.078311
394.251904	30.608059	74.083316
393.871412	29.662822	74.088321
393.485078	35.806062	74.093326
392.903725	32.321716	74.098330
393.149542	34.994845	74.103335
391.756078	32.883156	74.108340
391.263601	31.331885	74.113345
390.815776	33.710228	74.118350
389.502300	35.136858	74.123354
388.679840	29.452650	74.128359
387.642418	31.853095	74.133364
387.384663	24.718244	74.138369
387.056328	27.104133	74.143374
386.466379	26.728051	74.148378
386.394594	29.120497	74.153383
385.036917	30.322612	74.158388
384.848892	22.987139	74.163393
383.880789	27.761351	74.168398
382.893460	29.736789	74.173402
382.204239	28.290680	74.178407
381.324820	37.380887	74.183412
380.955605	25.491078	74.188417
381.011131	28.220105	74.193422
379.757327	27.936086	74.198426
379.130646	18.252647	74.203431
378.192905	33.564054	74.208436
377.666354	30.738568	74.213441
376.882974	34.291459	74.218446
375.703244	34.800356	74.223450
375.347135	20.242807	74.228455
374.678697	29.719195	74.233460
374.590271	28.284984	74.238465
374.218632	26.027784	74.243470
373.715297	28.164998	74.248474
372.667871	20.019238	74.253479
371.575057	29.140487	74.258484
371.199894	25.330694	74.263489
370.541887	22.076978	74.268494
369.596134	30.980404	74.273498
368.904131	26.447327	74.278503
368.223587	30.231658	74.283508
368.023856	23.650122	74.288513
367.424574	29.806962	74.293518
366.389088	29.466190	74.298522
365.766586	18.981164	74.303527
365.140813	23.724733	74.308532
364.731932	28.820714	74.313537
364.352180	31.666969	74.318542
363.145422	30.889394	74.323546
362.159915	28.355319	74.328551
361.619074	26.233296	74.333556
361.604523	22.639581	74.338561
360.825844	25.437764	74.343566
359.791913	32.426157	74.348570
359.526541	31.280415	74.353575
358.920289	27.823630	74.358580
358.118163	24.925780	74.363585
356.943371	28.894286	74.368590
356.790045	32.255913	74.373594
356.175997	28.269181	74.378599
355.282939	28.536331	74.383604
354.066974	22.226853	74.388609
353.539192	32.608687	74.393614
353.167620	38.019573	74.398618
353.026538	25.561756	74.403623
352.066556	31.296498	74.408628
351.368683	27.257427	74.413633
350.218266	34.638395	74.418638
349.641827	33.075468	74.423642
349.194714	30.043357	74.428647
349.107299	34.317317	74.433652
348.576764	26.427953	74.438657
347.348583	27.788269	74.443662
346.737422	29.107173	74.448666
346.105049	31.758713	74.453671
345.289757	29.161919	74.458676
344.115116	23.726361	74.463681
343.831567	29.137552	74.468686
343.074675	30.976010	74.473690
342.847464	31.256143	74.478695
342.300410	37.996106	74.483700
341.870250	28.721068	74.488705
340.863569	34.704197	74.493710
340.180689	32.084709	74.498714
339.838625	23.155344	74.503719
338.609571	28.978832	74.508724
337.626791	20.277694	74.513729
337.019304	30.358994	74.518734
336.668976	32.356706	74.523738
336.387106	31.229976	74.528743
336.052414	40.505496	74.533748
334.880453	32.546076	74.538753
334.025432	33.426806	74.543758
333.506862	35.076796	74.548762
333.310710	26.021376	74.553767
331.934290	35.548062	74.558772
331.065165	32.630910	74.563777
330.799762	31.598458	74.568782
330.405404	29.249635	74.573786
329.941787	27.392259	74.578791
328.414526	34.793612	74.583796
328.157979	18.743573	74.588801
327.654094	24.320413	74.593806
326.992576	28.239636	74.598810
326.383546	20.178613	74.603815
325.120215	26.260199	74.608820
324.568771	25.455577	74.613825
324.066753	29.664024	74.618830
323.823608	21.074135	74.623834
323.573087	18.847101	74.628839
322.052828	38.184166	74.633844
321.481959	24.792708	74.638849
321.026371	21.876127	74.643854
320.336428	28.472035	74.648858
319.423475	20.976230	74.653863
318.495765	30.071162	74.658868
318.208459	23.268603	74.663873
317.901863	26.443353	74.668878
316.932200	25.798433	74.673882
316.945752	14.445375	74.678887
315.718625	27.538752	74.683892
315.179540	24.579249	74.688897
314.633903	25.612206	74.693902
313.324970	26.155105	74.698906
312.658572	17.978399	74.703911
312.017478	31.464728	74.708916
311.689824	25.010511	74.713921
311.263055	26.274923	74.718926
310.350437	31.498688	74.723930
309.617476	24.888953	74.728935
308.796934	30.184958	74.733940
308.457684	27.514475	74.738945
308.326129	33.083947	74.743950
307.192540	35.449578	74.748954
306.704075	31.068720	74.753959
305.470426	32.175393	74.758964
305.104591	31.133711	74.763969
304.469491	26.434981	74.768974
303.231053	26.641741	74.773978
302.510134	29.103210	74.778983
301.795227	30.160051	74.783988
301.702397	25.508897	74.788993
301.033479	33.408889	74.793998
300.810800	28.028457	74.799002
300.547088	19.369864	74.804007
298.990770	27.873108	74.809012
298.553441	27.859671	74.814017
297.880330	32.024028	74.819022
297.187626	31.552682	74.824026
296.296047	29.392105	74.829031
295.483957	34.167617	74.834036
294.841269	31.074303	74.839041
294.719991	35.044216	74.844046
294.190773	27.657896	74.849050
293.442297	29.260853	74.854055
292.440780	34.739450	74.859060
291.601297	24.582533	74.864065
291.347362	25.192887	74.869070
290.560592	28.052069	74.874074
289.646545	28.867138	74.879079
289.019302	34.325794	74.884084
288.868562	34.498880	74.889089
288.521356	26.617972	74.894094
287.451259	38.362948	74.899098
287.057774	27.300689	74.904103
285.916121	31.025913	74.909108
285.381622	27.191338	74.914113
284.475580	23.136649	74.919118
283.681421	25.849870	74.924122
283.908135	25.313695	74.929127
282.601683	27.900789	74.934132
281.327349	26.109354	74.939137
280.580386	21.652817	74.944142
280.170133	33.294954	74.949146
280.228163	20.311608	74.954151
279.533796	25.833474	74.959156
279.022429	21.946387	74.964161
278.443756	21.878631	74.969166
276.986525	31.959142	74.974170
276.558856	23.808625	74.979175
275.853954	32.002136	74.984180
275.287267	29.667857	74.989185
274.879476	28.135241	74.994190
273.864135	26.812149	74.999194
273.156625	23.896520	75.004199
272.576962	26.801911	75.009204
272.426014	22.981330	75.014209
272.023123	31.998154	75.019214
270.461418	35.094764	75.024218
270.187611	25.603085	75.029223
269.343169	36.115377	75.034228
268.644765	33.705787	75.039233
267.501045	25.506698	75.044238
266.842034	37.519877	75.049242
266.253927	24.541101	75.054247
265.881582	19.534860	75.059252
265.480827	23.894100	75.064257
265.278963	27.301543	75.069262
264.732319	28.974903	75.074266
263.829377	22.792974	75.079271
263.213047	24.525644	75.084276
262.137588	28.911327	75.089281
261.339940	29.044912	75.094286
260.247454	37.915482	75.099290
260.020978	29.226825	75.104295
259.388252	25.993661	75.109300
259.341680	26.347434	75.114305
259.071854	27.691522	75.119310
257.837825	31.969395	75.124314
257.230104	29.671361	75.129319
255.596835	28.977184	75.134324
254.906620	22.581964	75.139329
254.163377	27.416726	75.144334
253.714869	26.228966	75.149338
253.727700	30.236675	75.154343
253.241166	24.281382	75.159348
252.895496	23.324269	75.164353
252.100475	27.399007	75.169358
251.187250	41.388276	75.174362
250.697461	22.734443	75.179367
249.495725	28.850089	75.184372
248.582992	33.293142	75.189377
248.301820	21.864692	75.194382
247.422182	34.546041	75.199386
247.362103	27.786247	75.204391
246.070746	34.377494	75.209396
245.412923	36.211615	75.214401
245.035530	33.630170	75.219406
243.969915	34.816208	75.224410
244.050001	30.252253	75.229415
243.249990	35.374627	75.234420
241.968631	37.447067	75.239425
241.494026	34.956887	75.244430
241.195976	34.846954	75.249434
240.880843	34.001048	75.254439
239.436143	32.142912	75.259444
238.741267	35.152919	75.264449
238.472253	25.213215	75.269454
237.697259	23.899062	75.274458
237.405126	21.408788	75.279463
236.202030	27.318236	75.284468
235.234300	26.519854	75.289473
235.224221	21.620852	75.294478
234.678864	25.174404	75.299482
233.997601	20.735429	75.304487
232.990749	28.720583	75.309492
232.180822	22.645080	75.314497
232.188755	18.518602	75.319502
231.367166	28.355963	75.324506
230.304234	23.839130	75.329511
229.271736	33.351089	75.334516
228.673998	35.642253	75.339521
228.782866	25.944468	75.344526
228.027410	33.415640	75.349530
227.357341	21.357582	75.354535
226.316715	29.741661	75.359540
225.518678	35.524842	75.364545
225.110252	30.321511	75.369550
224.849297	33.375949	75.374554
223.910356	21.763429	75.379559
223.203636	27.740153	75.384564
222.456708	32.590945	75.389569
222.251249	32.220026	75.394574
221.085140	40.930733	75.399578
220.461496	38.102571	75.404583
219.851374	35.311168	75.409588
219.298400	38.452766	75.414593
218.838819	27.242388	75.419598
217.561406	37.397875	75.424602
216.836232	37.702585	75.429607
216.127791	34.465433	75.434612
215.861124	32.728248	75.439617
215.455104	36.099641	75.444622
214.950542	30.526366	75.449626
214.230136	29.556522	75.454631
213.487065	35.354361	75.459636
212.656833	34.048101	75.464641
212.274718	31.674694	75.469646
210.953423	33.355328	75.474650
210.039450	28.598636	75.479655
209.780937	35.363349	75.484660
209.510855	34.005675	75.489665
209.447686	32.590033	75.494670
208.275909	37.353401	75.499674
207.590931	26.997928	75.504679
207.027352	29.109959	75.509684
205.933659	35.033028	75.514689
205.078306	27.435015	75.519694
204.217786	37.450362	75.524698
204.012496	35.413332	75.529703
203.692143	35.364854	75.534708
202.895797	38.099777	75.539713
201.964570	29.890334	75.544718
201.135665	30.826607	75.549722
200.790688	32.984057	75.554727
200.106256	33.550586	75.559732
199.487919	35.138748	75.564737
198.618043	30.514623	75.569742
198.009731	27.985004	75.574746
197.419217	38.249707	75.579751
196.804497	33.411721	75.584756
196.193969	30.560791	75.589761
195.439282	35.959595	75.594766
194.710627	35.265888	75.599770
194.246922	25.594418	75.604775
193.791866	31.997319	75.609780
192.912970	31.304895	75.614785
191.807925	25.384194	75.619790
190.986170	31.431164	75.624794
190.498362	31.041546	75.629799
190.024705	29.892443	75.634804
189.590404	32.919758	75.639809
188.790580	28.839382	75.644814
187.808827	30.931131	75.649818
187.619689	28.818707	75.654823
187.117137	28.659366	75.659828
186.331066	31.331349	75.664833
185.395010	29.933111	75.669838
184.316852	32.881730	75.674842
184.003610	28.044960	75.679847
183.544526	30.812855	75.684852
183.207148	28.884123	75.689857
182.857089	31.100072	75.694862
181.559147	37.973103	75.699866
181.407066	30.059946	75.704871
180.520333	29.473071	75.709876
179.195824	33.983564	75.714881
178.808124	37.139068	75.719886
177.972326	40.670579	75.724890
177.594327	38.107401	75.729895
177.024694	45.373450	75.734900
176.170921	38.482494	75.739905
175.768594	28.383689	75.744910
174.769216	40.459164	75.749914
174.420732	43.360857	75.754919
173.668614	41.322441	75.759924
172.936320	42.273735	75.764929
172.277004	37.812059	75.769934
171.143881	38.086847	75.774938
170.842715	31.499431	75.779943
170.389705	33.292925	75.784948
170.244312	35.617861	75.789953
169.544625	31.268891	75.794958
168.441751	41.199480	75.799962
167.872483	32.729851	75.804967
166.893582	33.564351	75.809972
165.858342	39.784495	75.814977
165.741899	32.394538	75.819982
165.067809	28.398792	75.824986
164.235293	33.149401	75.829991
164.059491	37.959135	75.834996
162.826073	29.508630	75.840001
162.126031	31.191719	75.845006
161.463301	30.842747	75.850010
161.152681	30.912991	75.855015
160.957197	37.818074	75.860020
159.842139	40.005703	75.865025
158.910726	36.115643	75.870030
157.994102	36.594884	75.875034
158.253660	26.598921	75.880039
157.800499	32.355749	75.885044
157.103981	31.455236	75.890049
156.169317	32.514245	75.895054
155.111189	33.760199	75.900058
153.835053	32.589203	75.905063
153.270526	29.030964	75.910068
152.847232	39.401600	75.915073
152.585177	33.227849	75.920078
151.928844	33.980609	75.925082
151.795855	28.114715	75.930087
150.787817	27.073803	75.935092
149.606267	33.939911	75.940097
149.120636	37.960441	75.945102
148.341767	41.681527	75.950106
148.172338	31.249528	75.955111
146.884525	25.890271	75.960116
146.147554	35.061860	75.965121
145.917554	27.295479	75.970126
145.374555	36.674591	75.975130
145.225693	26.498396	75.980135
143.782921	42.800287	75.985140
143.032205	43.487523	75.990145
142.909674	30.280550	75.995150
142.378648	35.956786	76.000154
140.973123	36.406956	76.005159
140.477526	34.408646	76.010164
140.030877	44.313580	76.015169
139.746862	27.529383	76.020174
138.601170	33.707678	76.025178
138.188914	26.766309	76.030183
137.682438	27.801256	76.035188
136.724697	29.046187	76.040193
135.941252	27.764288	76.045198
134.984783	32.546019	76.050202
134.572699	28.722848	76.055207
134.182939	29.058881	76.060212
133.404717	27.573996	76.065217
132.956094	23.827744	76.070222
131.637087	38.340894	76.075226
130.988549	32.532594	76.080231
130.295533	21.681580	76.085236
129.917436	29.842362	76.090241
129.771640	28.341815	76.095246
128.757866	23.526865	76.100250
127.912841	27.782679	76.105255
127.126086	31.095011	76.110260
126.685432	29.883814	76.115265
126.780523	28.468674	76.120270
125.697853	35.120085	76.125274
124.343320	28.385253	76.130279
123.459340	27.755684	76.135284
122.926251	29.275165	76.140289
123.126214	24.723820	76.145294
122.159704	28.961386	76.150298
121.490106	24.027832	76.155303
121.025243	27.468916	76.160308
120.338946	25.567246	76.165313
119.619197	24.517969	76.170318
118.829716	31.698554	76.175322
118.081496	25.723413	76.180327
117.529135	25.379998	76.185332
117.055047	25.988237	76.190337
116.591156	16.917967	76.195342
115.107520	21.942432	76.200346
114.601565	23.891839	76.205351
114.130691	23.168953	76.210356
113.564706	28.905257	76.215361
113.317711	22.919974	76.220366
111.712259	26.356084	76.225370
111.211924	29.421169	76.230375
110.976863	21.702634	76.235380
110.300159	33.049018	76.240385
110.338493	20.511148	76.245390
108.780014	31.333742	76.250394
108.125015	25.670233	76.255399
107.563808	30.767075	76.260404
106.796597	32.169205	76.265409
106.544126	25.842250	76.270414
105.717146	32.564689	76.275418
104.850306	23.895452	76.280423
104.259523	26.552518	76.285428
103.619431	31.656569	76.290433
102.990477	29.022353	76.295438
102.035476	32.976915	76.300442
101.692138	29.902968	76.305447
101.557446	29.241650	76.310452
100.206606	32.419391	76.315457
99.400176	28.400559	76.320462
98.747296	35.442867	76.325466
98.323875	30.342382	76.330471
98.087338	24.247946	76.335476
97.140890	28.742586	76.340481
96.190190	23.504752	76.345486
95.496609	30.706789	76.350490
95.104943	19.002858	76.355495
94.496973	24.197315	76.360500
93.619470	24.881033	76.365505
93.052142	23.620509	76.370510
91.992121	37.132086	76.375514
91.948034	30.903213	76.380519
91.626177	31.044067	76.385524
90.252755	31.544402	76.390529
89.652565	29.142084	76.395534
88.941277	31.969802	76.400538
88.418408	28.419825	76.405543
88.108101	26.452122	76.410548
86.927293	37.325627	76.415553
86.033705	31.515930	76.420558
85.737954	39.061847	76.425562
85.163461	33.797406	76.430567
84.921751	28.839444	76.435572
83.727117	29.933564	76.440577
83.114387	28.942124	76.445582
82.211472	19.030607	76.450586
81.817102	29.092741	76.455591
81.608024	28.690873	76.460596
80.233275	35.168564	76.465601
79.812382	23.422277	76.470606
78.641453	28.704964	76.475610
78.451702	34.112708	76.480615
78.200736	33.740124	76.485620
77.520139	25.063041	76.490625
76.470793	26.387633	76.495630
75.822542	27.988042	76.500634
75.371982	25.162598	76.505639
74.721993	25.559040	76.510644
73.824789	33.013476	76.515649
72.849065	21.989908	76.520654
72.076644	30.236846	76.525658
71.513600	31.244395	76.530663
71.348976	29.350788	76.535668
70.892127	34.789719	76.540673
70.813678	31.612733	76.545678
69.747426	38.588556	76.550682
68.816479	30.245297	76.555687
67.594435	36.671944	76.560692
66.515021	40.712577	76.565697
66.112631	26.293680	76.570702
65.726596	35.478523	76.575706
65.245651	33.233385	76.580711
65.195462	32.096952	76.585716
64.343538	31.255859	76.590721
63.582010	30.743852	76.595726
62.617992	32.350246	76.600730
62.077239	31.027936	76.605735
61.664675	23.391941	76.610740
60.516678	30.157975	76.615745
60.014697	17.839847	76.620750
59.569221	24.833963	76.625754
58.637309	19.637521	76.630759
58.345252	20.695315	76.635764
57.394232	26.840245	76.640769
56.738260	29.836498	76.645774
56.136420	32.354158	76.650778
55.755392	23.410997	76.655783
54.884010	18.162734	76.660788
53.794778	31.271580	76.665793
53.742559	24.566111	76.670798
52.950569	21.262006	76.675802
52.054137	33.005646	76.680807
51.063381	22.199385	76.685812
50.565166	29.524630	76.690817
50.247796	27.307893	76.695822
49.730968	33.365754	76.700826
48.570907	26.334336	76.705831
47.507782	27.818391	76.710836
46.946416	26.245818	76.715841
46.987825	22.966975	76.720846
46.538163	22.418474	76.725850
46.075289	27.955141	76.730855
45.305679	32.443154	76.735860
43.914672	34.357614	76.740865
43.582540	25.053593	76.745870
42.991307	27.747450	76.750874
41.843991	27.903921	76.755879
41.240955	28.788075	76.760884
40.599105	32.424105	76.765889
40.327557	21.995033	76.770894
39.714041	28.995858	76.775898
39.232710	30.329248	76.780903
38.394886	30.102283	76.785908
37.666578	30.845689	76.790913
37.266489	28.422491	76.795918
36.170952	32.512073	76.800922
35.179135	33.382759	76.805927
34.533159	30.971327	76.810932
33.804550	28.832204	76.815937
33.597085	23.992712	76.820942
33.337582	25.282148	76.825946
32.530353	20.545489	76.830951
31.451916	24.238216	76.835956
30.657682	22.248101	76.840961
30.346067	24.341815	76.845966
29.835280	21.654986	76.850970
29.430662	25.642684	76.855975
28.366248	26.215180	76.860980
27.493488	28.388134	76.865985
27.077229	25.356697	76.870990
26.662410	27.670988	76.875994
25.707253	28.815241	76.880999
24.954909	24.418098	76.886004
24.081710	33.850272	76.891009
23.764680	28.309610	76.896014
23.187139	37.747538	76.901018
21.930700	28.869217	76.906023
21.722102	25.929273	76.911028
20.770769	33.652717	76.916033
20.699063	22.696389	76.921038
20.459474	22.510531	76.926042
19.283678	34.015906	76.931047
18.202924	27.248777	76.936052
17.353281	33.392517	76.941057
17.292964	29.206305	76.946062
16.552148	29.337687	76.951066
15.211599	30.581966	76.956071
14.956902	26.713669	76.961076
14.336409	30.647994	76.966081
14.045438	26.811969	76.971086
13.829999	24.001085	76.976090
12.475609	24.147281	76.981095
11.687932	24.366825	76.986100
10.946240	23.461451	76.991105
10.729016	16.154716	76.996110
9.619951	23.859020	77.001114
9.076202	23.326260	77.006119
8.421782	22.166333	77.011124
7.768172	26.668010	77.016129
7.592961	29.699067	77.021134
6.597612	19.674745	77.026139
5.543950	23.707417	77.031143
5.246527	17.338848	77.036148
4.844126	28.141257	77.041153
4.398564	24.751712	77.046158