Tue Jun 08 17:08:30 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
0.926578	102.898363	0.000000
0.596283	88.913048	0.005005
-0.160457	47.072579	0.010010
-2.069178	7.577363	0.015014
-6.269006	-8.170297	0.020019
-12.289024	-7.139310	0.025024
-17.064749	-12.351658	0.030029
-21.571891	-10.168967	0.035034
-25.624808	-15.096318	0.040038
-29.053416	-11.047631	0.045043
-32.661193	-14.387201	0.050048
-36.589012	-9.576773	0.055053
-39.912139	-14.975406	0.060058
-43.787294	-14.929080	0.065062
-47.446572	-12.463878	0.070067
-51.378788	-5.763993	0.075072
-55.295297	-15.362029	0.080077
-59.043499	-12.448178	0.085082
-62.844580	-8.863327	0.090086
-66.459121	-13.207826	0.095091
-69.989347	-7.660732	0.100096
-73.708614	-12.559993	0.105101
-77.717585	-9.847712	0.110106
-81.691652	-2.086748	0.115110
-85.015274	-14.379275	0.120115
-89.122435	-6.890729	0.125120
-92.757053	-15.676991	0.130125
-96.597875	-9.819268	0.135130
-100.436394	-6.679910	0.140134
-103.745516	-20.061934	0.145139
-107.766788	-9.815658	0.150144
-111.962746	-18.223426	0.155149
-115.510183	-13.993655	0.160154
-119.464198	-13.523243	0.165158
-122.625369	-14.916828	0.170163
-126.919515	0.037789	0.175168
-130.508676	-10.468097	0.180173
-134.355083	-15.195117	0.185178
-137.997608	-9.426231	0.190182
-141.405072	-13.535407	0.195187
-145.413138	-7.081371	0.200192
-149.164688	-12.117915	0.205197
-152.614685	-12.095857	0.210202
-157.086969	-17.658486	0.215206
-160.513004	-21.217787	0.220211
-164.151791	-12.749313	0.225216
-168.146700	-16.782196	0.230221
-172.136394	-9.055193	0.235226
-175.929489	-9.299519	0.240230
-179.329546	-19.487677	0.245235
-183.625562	-5.790640	0.250240
-186.970990	-11.481760	0.255245
-190.991675	-11.810981	0.260250
-194.555940	-7.284205	0.265254
-198.064212	-20.929998	0.270259
-202.106863	-6.778275	0.275264
-205.302888	-9.203912	0.280269
-209.258374	-10.403188	0.285274
-213.195735	-7.572028	0.290278
-216.984760	-3.643749	0.295283
-220.809349	-6.809411	0.300288
-224.516641	-5.696795	0.305293
-228.338805	-3.802685	0.310298
-232.149535	-1.989474	0.315302
-235.497266	-12.987429	0.320307
-239.956522	-10.210017	0.325312
-243.641921	-16.526418	0.330317
-246.898588	-19.774853	0.335322
-250.924903	-9.756138	0.340326
-254.194760	-16.319447	0.345331
-258.155733	-6.367585	0.350336
-262.226799	-15.301455	0.355341
-265.853860	-13.966530	0.360346
-269.866408	-8.139607	0.365350
-273.369883	-14.868475	0.370355
-277.291936	-8.525788	0.375360
-280.984809	-17.645285	0.380365
-284.581373	-20.658958	0.385370
-288.910184	-13.550624	0.390374
-292.265766	-14.798645	0.395379
-295.699648	-13.229218	0.400384
-299.458471	-10.557284	0.405389
-303.396013	-6.376900	0.410394
-307.404871	-7.198274	0.415398
-310.892358	-14.599280	0.420403
-314.930572	-2.968845	0.425408
-318.674532	-18.975119	0.430413
-322.450839	-13.981251	0.435418
-326.146497	-7.642623	0.440422
-329.452002	-18.748386	0.445427
-333.582894	-18.693469	0.450432
-337.482406	-10.353425	0.455437
-341.308092	-16.549762	0.460442
-345.111245	-3.366973	0.465446
-348.549639	-11.408693	0.470451
-352.348183	-11.677197	0.475456
-356.413693	-11.703337	0.480461
-359.984718	-15.034334	0.485466
-363.811095	-9.183613	0.490470
-367.685384	-8.924410	0.495475
-371.128294	-8.789329	0.500480
-374.969715	-14.605989	0.505485
-378.384660	-22.100687	0.510490
-382.612595	-3.609585	0.515494
-386.059968	-14.473482	0.520499
-389.966303	-15.066464	0.525504
-394.057394	-10.443247	0.530509
-397.871051	-14.394122	0.535514
-401.401502	-11.083171	0.540518
-404.847977	-13.139272	0.545523
-409.216492	-4.031920	0.550528
-412.592262	-16.787679	0.555533
-416.212797	-15.847278	0.560538
-420.254530	-8.997269	0.565542
-423.907892	-19.103868	0.570547
-427.715436	-12.125883	0.575552
-431.424918	-7.254700	0.580557
-435.184805	-6.086708	0.585562
-439.101105	-4.562298	0.590566
-442.466744	-19.622498	0.595571
-446.684579	-8.907266	0.600576
-450.129422	-11.080445	0.605581
-453.796813	-13.328327	0.610586
-457.792976	-10.270177	0.615590
-461.257187	-11.188008	0.620595
-465.483480	-6.755465	0.625600
-469.334880	-13.054238	0.630605
-473.023677	-9.389643	0.635610
-476.732961	-8.104386	0.640614
-479.948021	-14.114060	0.645619
-483.833048	-6.014789	0.650624
-487.833825	-9.583769	0.655629
-491.700958	-14.269016	0.660634
-495.943933	-8.639590	0.665638
-498.930123	-13.040607	0.670643
-503.202390	-12.899703	0.675648
-506.824598	-3.291536	0.680653
-510.222580	-8.496570	0.685658
-514.163302	-8.532135	0.690662
-517.804741	-14.781234	0.695667
-521.782753	-9.465252	0.700672
-525.403956	-5.565914	0.705677
-529.425254	-15.506269	0.710682
-533.076235	-2.646276	0.715686
-536.565082	-14.029068	0.720691
-540.420641	-11.245610	0.725696
-544.239930	-8.041297	0.730701
-547.921130	-14.047511	0.735706
-552.376892	-8.597825	0.740710
-555.790624	-12.173130	0.745715
-559.532736	-9.476221	0.750720
-562.996005	-8.974367	0.755725
-566.458472	-8.302134	0.760730
-570.520142	-10.498843	0.765734
-574.313419	-15.981760	0.770739
-578.169829	-7.407360	0.775744
-581.873982	-10.072348	0.780749
-585.533225	-9.789463	0.785754
-589.439299	-7.617776	0.790758
-593.015166	-9.555216	0.795763
-597.000996	-5.024876	0.800768
-600.844674	-7.613411	0.805773
-604.895655	-15.807537	0.810778
-608.469313	-0.803679	0.815782
-612.178726	-5.657186	0.820787
-615.638161	-8.044423	0.825792
-619.231489	-9.809120	0.830797
-623.227022	-12.616294	0.835802
-626.906493	-3.936831	0.840806
-630.412529	-8.980340	0.845811
-634.573507	-1.021870	0.850816
-638.182749	-5.825047	0.855821
-641.816114	-16.085258	0.860826
-645.910136	-7.029932	0.865830
-650.027093	-12.535783	0.870835
-653.623388	-13.475396	0.875840
-657.205520	-17.888102	0.880845
-661.018566	-18.527639	0.885850
-664.782534	-11.073033	0.890854
-668.571746	-12.146885	0.895859
-671.894023	-4.894374	0.900864
-675.739768	-11.321415	0.905869
-679.822868	-17.560096	0.910874
-683.271160	-10.784865	0.915878
-686.852778	-15.015674	0.920883
-691.170742	-11.458445	0.925888
-695.000320	-21.928859	0.930893
-698.652658	-21.031321	0.935898
-702.649769	-4.221180	0.940902
-706.110229	-18.492419	0.945907
-709.759060	-7.549375	0.950912
-713.390262	-14.900895	0.955917
-717.045881	-11.932932	0.960922
-720.972275	-8.144474	0.965926
-724.697115	-9.451150	0.970931
-728.583728	-7.295708	0.975936
-732.692341	-9.282512	0.980941
-736.134827	-11.249826	0.985946
-739.908563	-8.764825	0.990950
-743.716306	-10.119226	0.995955
-747.371359	-4.770064	1.000960
-751.181213	-9.046510	1.005965
-754.670297	-13.501942	1.010970
-758.859454	-4.734511	1.015974
-761.950438	-10.686314	1.020979
-766.229638	-3.611717	1.025984
-769.993546	-9.884173	1.030989
-773.313469	-11.120575	1.035994
-777.450319	-11.702067	1.040998
-781.455005	-10.537949	1.046003
-785.296532	-3.587001	1.051008
-789.296293	-4.497515	1.056013
-792.713417	-10.282010	1.061018
-796.408288	-9.614310	1.066022
-799.964873	-7.920814	1.071027
-803.674793	-4.931224	1.076032
-807.345597	-2.421204	1.081037
-811.291122	-7.873825	1.086042
-815.579315	-10.758472	1.091046
-819.141813	-16.382211	1.096051
-822.441666	-7.331609	1.101056
-826.373901	-3.369965	1.106061
-829.872831	-6.776486	1.111066
-833.976351	-3.771809	1.116070
-837.708803	-13.306724	1.121075
-841.315892	-12.805620	1.126080
-845.258470	-11.938662	1.131085
-848.961383	-16.442566	1.136090
-852.867352	-8.298752	1.141094
-856.424007	-16.144872	1.146099
-860.142811	-3.524834	1.151104
-864.006450	-4.621262	1.156109
-867.850394	-9.927065	1.161114
-871.506227	-6.922232	1.166118
-875.066132	-16.886564	1.171123
-879.142264	-10.348791	1.176128
-882.853552	-7.709006	1.181133
-886.520032	-15.156539	1.186138
-890.506256	-10.901385	1.191142
-893.867994	-13.326476	1.196147
-897.799483	-11.439084	1.201152
-901.409561	-15.263798	1.206157
-905.539106	-12.845465	1.211162
-909.608399	-8.845618	1.216166
-912.889596	-12.599683	1.221171
-916.566041	-10.631722	1.226176
-920.487441	-11.746207	1.231181
-924.103970	-17.154145	1.236186
-928.330486	-11.906466	1.241190
-931.990012	-21.994155	1.246195
-935.628451	-16.760192	1.251200
-939.218610	-9.058913	1.256205
-942.696061	-18.785512	1.261210
-946.531019	-0.537084	1.266214
-950.141227	-8.926519	1.271219
-954.301050	-6.571621	1.276224
-958.110984	-13.409901	1.281229
-962.189435	-13.005395	1.286234
-965.755998	-2.281929	1.291238
-969.193467	-10.907036	1.296243
-972.465863	-9.962004	1.301248
-976.467488	-15.228791	1.306253
-980.394987	-14.505209	1.311258
-984.553852	-10.537282	1.316262
-988.047811	-18.328129	1.321267
-992.013592	-7.907134	1.326272
-995.951361	-18.450641	1.331277
-999.584546	-17.135777	1.336282
-1003.403345	-13.734203	1.341286
-1007.068719	-17.852464	1.346291
-1010.676413	-13.395370	1.351296
-1014.004115	-10.514645	1.356301
-1017.984207	-20.772199	1.361306
-1021.722190	-12.451842	1.366310
-1025.489856	-14.109688	1.371315
-1029.846064	-9.335397	1.376320
-1033.403799	-11.368727	1.381325
-1036.954508	-15.654663	1.386330
-1041.253141	-9.151961	1.391334
-1044.959162	-15.987472	1.396339
-1048.366977	-8.464248	1.401344
-1051.956628	-8.012143	1.406349
-1055.599715	-13.702355	1.411354
-1059.747702	-10.930212	1.416358
-1063.432260	-18.460125	1.421363
-1067.066515	-14.227355	1.426368
-1070.667897	-16.073567	1.431373
-1074.609400	-8.240418	1.436378
-1078.788214	-2.277289	1.441382
-1082.488778	-12.918671	1.446387
-1086.010055	-10.542245	1.451392
-1089.634044	-13.788133	1.456397
-1093.353061	-13.921628	1.461402
-1097.081144	-3.056264	1.466406
-1101.144331	-7.526499	1.471411
-1104.631508	-4.974348	1.476416
-1108.399494	-6.774949	1.481421
-1111.997885	-16.552858	1.486426
-1115.784482	-8.990992	1.491430
-1119.723659	-17.045903	1.496435
-1123.490667	-11.847734	1.501440
-1127.603096	-0.220089	1.506445
-1131.163386	-7.589322	1.511450
-1134.844037	-2.383077	1.516454
-1138.196406	-16.870604	1.521459
-1142.340405	-16.031546	1.526464
-1146.461610	-12.981706	1.531469
-1149.848547	-7.502227	1.536474
-1153.955844	-8.378142	1.541478
-1157.420711	-11.844305	1.546483
-1160.875809	-10.276094	1.551488
-1164.742391	-8.658139	1.556493
-1168.276121	-16.553694	1.561498
-1172.423718	-11.974155	1.566502
-1175.874051	-16.510081	1.571507
-1180.299702	-14.999381	1.576512
-1184.372012	-12.700342	1.581517
-1187.507191	-21.696473	1.586522
-1191.608746	-12.029571	1.591526
-1194.975313	-6.104382	1.596531
-1199.073333	-11.371366	1.601536
-1202.809926	-11.012707	1.606541
-1206.185923	-17.165060	1.611546
-1210.092728	-9.910474	1.616550
-1213.740143	-11.671689	1.621555
-1217.672223	-12.915499	1.626560
-1221.179501	-16.542468	1.631565
-1224.876361	-11.701234	1.636570
-1228.895198	-15.603079	1.641574
-1232.168536	-13.989057	1.646579
-1236.097776	-12.822477	1.651584
-1240.413526	-14.783471	1.656589
-1243.980039	-16.633151	1.661594
-1247.812189	-18.106445	1.666598
-1251.254397	-16.326050	1.671603
-1255.186666	-14.008762	1.676608
-1259.112665	-17.232629	1.681613
-1262.330902	-15.524240	1.686618
-1266.755174	-3.975149	1.691622
-1270.181123	-10.011511	1.696627
-1274.394696	-10.279760	1.701632
-1277.668319	-6.217298	1.706637
-1281.459054	-16.471969	1.711642
-1285.455267	-6.446527	1.716646
-1288.635329	-6.164429	1.721651
-1292.719235	-9.544287	1.726656
-1296.558787	-10.146336	1.731661
-1300.169285	-11.197425	1.736666
-1304.379490	-5.542093	1.741670
-1307.794493	-9.482050	1.746675
-1311.646994	-1.686088	1.751680
-1315.501659	-0.007679	1.756685
-1318.932624	-8.331639	1.761690
-1323.030921	-2.104241	1.766694
-1326.981931	-5.636355	1.771699
-1330.556716	-14.965383	1.776704
-1334.292192	-12.056611	1.781709
-1337.692428	-11.678243	1.786714
-1341.540481	-4.149446	1.791718
-1345.178831	-11.695713	1.796723
-1349.032450	-2.456488	1.801728
-1353.290180	-3.907109	1.806733
-1356.825170	-11.011682	1.811738
-1360.756000	-1.613932	1.816742
-1363.970723	-10.768349	1.821747
-1367.837937	-8.215441	1.826752
-1371.779213	-6.416325	1.831757
-1375.682361	-10.773649	1.836762
-1379.525175	-6.644130	1.841766
-1383.007960	-10.014266	1.846771
-1387.005885	-13.636935	1.851776
-1390.654896	-11.428569	1.856781
-1393.909085	-17.705489	1.861786
-1398.222065	-14.031596	1.866790
-1401.681083	-10.872252	1.871795
-1405.638569	-14.081095	1.876800
-1409.839651	-9.537536	1.881805
-1413.143169	-22.121631	1.886810
-1417.171095	-7.431540	1.891814
-1420.664118	-11.216692	1.896819
-1423.968127	-11.288564	1.901824
-1427.965006	-5.755807	1.906829
-1431.897861	-12.279637	1.911834
-1436.007685	-16.033023	1.916838
-1439.767244	-24.728274	1.921843
-1443.351852	-16.993227	1.926848
-1447.108645	-13.741645	1.931853
-1450.415761	-19.086211	1.936858
-1454.345271	-6.351783	1.941862
-1458.094986	-19.472952	1.946867
-1461.901599	-11.981964	1.951872
-1466.030439	-4.820451	1.956877
-1469.703870	-8.958615	1.961882
-1473.557684	-10.506524	1.966886
-1477.289262	-17.092908	1.971891
-1481.061700	-11.168040	1.976896
-1484.715734	-4.808019	1.981901
-1488.247642	-16.043973	1.986906
-1492.165370	-13.422675	1.991910
-1495.925848	-15.571153	1.996915
-1499.994110	-11.302532	2.006912
-1500.849975	-12.045932	2.016909
-1497.818719	-11.824131	2.026906
-1495.436178	-10.556603	2.036902
-1493.299166	-9.470187	2.046899
-1491.514531	-14.213435	2.056896
-1489.476703	-13.769582	2.066893
-1487.705963	-17.106657	2.076890
-1486.023179	-9.540598	2.086886
-1483.712853	-10.813711	2.096883
-1481.693145	-16.146681	2.106880
-1479.988633	-8.979166	2.116877
-1478.101492	-11.761995	2.126874
-1476.332877	-18.367479	2.136870
-1474.325633	-6.901501	2.146867
-1472.491081	-12.566253	2.156864
-1470.383047	-15.437612	2.166861
-1468.927872	-8.014239	2.176858
-1466.801646	-5.630853	2.186854
-1464.881465	-10.232971	2.196851
-1463.084406	-10.117659	2.206848
-1460.953922	-18.521063	2.216845
-1459.246049	-11.345027	2.226842
-1457.199011	-16.289843	2.236838
-1455.562532	-7.078459	2.246835
-1453.682420	-11.499796	2.256832
-1451.496744	-13.673503	2.266829
-1449.560283	-19.137200	2.276826
-1447.997719	-20.237574	2.286822
-1446.250890	-17.503267	2.296819
-1444.128857	-16.583401	2.306816
-1442.239652	-16.136916	2.316813
-1440.414264	-17.542090	2.326810
-1438.295607	-21.567690	2.336806
-1436.581097	-19.949827	2.346803
-1435.004024	-15.495646	2.356800
-1432.919614	-16.180186	2.366797
-1430.871177	-13.200090	2.376794
-1428.983995	-11.679860	2.386790
-1426.957181	-15.296841	2.396787
-1425.220791	-10.712729	2.406784
-1423.677204	-13.870854	2.416781
-1421.557318	-9.886546	2.426778
-1419.810909	-10.852108	2.436774
-1417.591144	-17.233920	2.446771
-1416.042498	-13.317075	2.456768
-1414.003721	-16.367397	2.466765
-1412.313736	-13.776651	2.476762
-1410.369328	-11.807800	2.486758
-1408.421737	-16.533164	2.496755
-1406.346084	-14.245395	2.506752
-1404.701598	-10.978134	2.516749
-1402.697932	-16.275907	2.526746
-1400.761211	-18.070895	2.536742
-1398.837730	-11.537722	2.546739
-1397.134309	-6.480794	2.556736
-1395.347031	-20.305593	2.566733
-1393.324610	-21.083802	2.576730
-1391.334948	-21.173459	2.586726
-1389.507682	-11.832782	2.596723
-1387.878228	-17.658294	2.606720
-1385.882673	-14.486898	2.616717
-1383.881139	-12.386757	2.626714
-1381.972598	-16.950875	2.636710
-1380.352827	-17.216883	2.646707
-1378.793059	-14.660665	2.656704
-1376.580604	-16.750802	2.666701
-1374.678820	-17.628424	2.676698
-1372.619248	-17.042811	2.686694
-1371.059275	-16.276136	2.696691
-1368.783383	-9.022148	2.706688
-1367.150234	-18.540340	2.716685
-1365.110099	-22.719197	2.726682
-1363.267920	-19.935231	2.736678
-1361.435379	-20.651168	2.746675
-1359.721764	-21.535192	2.756672
-1357.553471	-17.407010	2.766669
-1355.863359	-22.705442	2.776666
-1354.127601	-13.781389	2.786662
-1352.096427	-16.226101	2.796659
-1350.096853	-11.160740	2.806656
-1348.116218	-15.860929	2.816653
-1346.356620	-18.749842	2.826650
-1344.601385	-14.681913	2.836646
-1342.873638	-10.619536	2.846643
-1340.844614	-8.637914	2.856640
-1338.742678	-12.089520	2.866637
-1337.053898	-19.529362	2.876634
-1334.938034	-21.098204	2.886630
-1333.253966	-19.749344	2.896627
-1331.652055	-16.401626	2.906624
-1329.314128	-19.248776	2.916621
-1327.651819	-5.527675	2.926618
-1325.583928	-9.959476	2.936614
-1324.076977	-14.409542	2.946611
-1322.234630	-7.993600	2.956608
-1319.941307	-9.563670	2.966605
-1318.110492	-17.743629	2.976602
-1316.446289	-14.991910	2.986598
-1314.466840	-17.275169	2.996595
-1312.588136	-14.542505	3.006592
-1310.774919	-17.574986	3.016589
-1308.838674	-13.169793	3.026586
-1306.794816	-11.380008	3.036582
-1305.358313	-14.488876	3.046579
-1303.400181	-12.595048	3.056576
-1301.134387	-16.291749	3.066573
-1299.659517	-14.439410	3.076570
-1297.572198	-11.488448	3.086566
-1295.707348	-12.294876	3.096563
-1293.801565	-18.751938	3.106560
-1291.975863	-11.740308	3.116557
-1290.142874	-14.145816	3.126554
-1288.089490	-18.794450	3.136550
-1286.432784	-18.222201	3.146547
-1284.560168	-14.687387	3.156544
-1282.286761	-10.743992	3.166541
-1280.695685	-14.410167	3.176538
-1279.014029	-18.740042	3.186534
-1277.080080	-13.785491	3.196531
-1275.138307	-17.784195	3.206528
-1273.302598	-15.748393	3.216525
-1271.177857	-15.826414	3.226522
-1269.392796	-17.519417	3.236518
-1267.684744	-19.648547	3.246515
-1265.725211	-16.963732	3.256512
-1263.605366	-13.291941	3.266509
-1261.769219	-18.089794	3.276506
-1260.072203	-18.339381	3.286502
-1257.989148	-17.390593	3.296499
-1256.175104	-17.892662	3.306496
-1254.748994	-14.447138	3.316493
-1252.807072	-16.997411	3.326490
-1250.620569	-16.013823	3.336486
-1248.762991	-18.359512	3.346483
-1246.854076	-12.816130	3.356480
-1245.101737	-13.875909	3.366477
-1243.172887	-11.090566	3.376474
-1241.438633	-16.527752	3.386470
-1239.447507	-19.842112	3.396467
-1237.368678	-10.500291	3.406464
-1235.873952	-10.157090	3.416461
-1233.595037	-17.987147	3.426458
-1231.797816	-15.195398	3.436454
-1230.018370	-15.052853	3.446451
-1228.236101	-10.878852	3.456448
-1226.512300	-12.019484	3.466445
-1224.184312	-18.540331	3.476442
-1222.486631	-22.071451	3.486438
-1220.610456	-12.626447	3.496435
-1218.809167	-10.685487	3.506432
-1216.906051	-11.108775	3.516429
-1215.188867	-14.461841	3.526426
-1212.953288	-16.059482	3.536422
-1211.180153	-16.872255	3.546419
-1209.417027	-19.365721	3.556416
-1207.709402	-18.305800	3.566413
-1205.835249	-15.411848	3.576410
-1203.924291	-14.112173	3.586406
-1201.821081	-21.916782	3.596403
-1199.924817	-23.123379	3.606400
-1198.006263	-24.312066	3.616397
-1196.068287	-18.587506	3.626394
-1194.351071	-21.020914	3.636390
-1192.675130	-23.309303	3.646387
-1190.559991	-16.803796	3.656384
-1188.961292	-17.290592	3.666381
-1186.719799	-14.886936	3.676378
-1185.035486	-19.231857	3.686374
-1182.874746	-13.829304	3.696371
-1181.224477	-20.040492	3.706368
-1179.471031	-17.252662	3.716365
-1177.712568	-13.440121	3.726362
-1175.334710	-20.258802	3.736358
-1173.998170	-21.450289	3.746355
-1171.984039	-17.608140	3.756352
-1169.914553	-12.873624	3.766349
-1168.062347	-21.617612	3.776346
-1166.104052	-12.696897	3.786342
-1164.315923	-14.434253	3.796339
-1162.491587	-10.798609	3.806336
-1160.804537	-9.994788	3.816333
-1158.749837	-13.222809	3.826330
-1156.469883	-20.365736	3.836326
-1154.707855	-18.393504	3.846323
-1153.448623	-14.965131	3.856320
-1151.143822	-9.311044	3.866317
-1149.265786	-15.140829	3.876314
-1147.479123	-13.741137	3.886310
-1145.691493	-19.193382	3.896307
-1143.666131	-21.009406	3.906304
-1141.806412	-17.115038	3.916301
-1140.017351	-13.492692	3.926298
-1137.831085	-13.049257	3.936294
-1136.027360	-14.693243	3.946291
-1134.266402	-10.448748	3.956288
-1132.605812	-11.487195	3.966285
-1130.622551	-11.074897	3.976282
-1128.714095	-17.080234	3.986278
-1126.708922	-12.202651	3.996275
-1125.081349	-13.120814	4.006272
-1123.192378	-8.940582	4.016269
-1121.073092	-14.365589	4.026266
-1119.122170	-15.086732	4.036262
-1117.404650	-11.343408	4.046259
-1115.620662	-7.914622	4.056256
-1113.710633	-11.897533	4.066253
-1111.837959	-7.041848	4.076250
-1109.773085	-10.417822	4.086246
-1107.890895	-10.354125	4.096243
-1106.514639	-6.842283	4.106240
-1104.247615	-4.450076	4.116237
-1102.501921	-17.027881	4.126234
-1100.475648	-14.318478	4.136230
-1098.708771	-12.408311	4.146227
-1096.598657	-10.787091	4.156224
-1094.838786	-9.670093	4.166221
-1092.757395	-12.574642	4.176218
-1090.846001	-14.716883	4.186214
-1089.571188	-9.295345	4.196211
-1087.648303	-9.353633	4.206208
-1085.570732	-10.793660	4.216205
-1083.574635	-10.485904	4.226202
-1081.900517	-17.860310	4.236198
-1079.650306	-19.435102	4.246195
-1077.574096	-17.702925	4.256192
-1076.298784	-12.243925	4.266189
-1074.675507	-11.314113	4.276186
-1072.755446	-11.928762	4.286182
-1070.714658	-11.214097	4.296179
-1068.537212	-16.727713	4.306176
-1066.543225	-16.096699	4.316173
-1064.983330	-15.242158	4.326170
-1062.954488	-19.867509	4.336166
-1061.251003	-3.529522	4.346163
-1059.143639	-7.213526	4.356160
-1057.411554	-18.212087	4.366157
-1055.577993	-12.726411	4.376154
-1053.608822	-18.882443	4.386150
-1051.706883	-14.937185	4.396147
-1050.126816	-12.238882	4.406144
-1048.168457	-11.159106	4.416141
-1045.950027	-11.696922	4.426138
-1043.931616	-14.506455	4.436134
-1042.313731	-11.617432	4.446131
-1040.383111	-19.689148	4.456128
-1038.750802	-22.662400	4.466125
-1036.714422	-16.542842	4.476122
-1035.027258	-18.098403	4.486118
-1032.755839	-15.133066	4.496115
-1031.050551	-17.309058	4.506112
-1029.444023	-19.655027	4.516109
-1027.220290	-18.601042	4.526106
-1025.561836	-22.096506	4.536102
-1023.751030	-21.766000	4.546099
-1021.666524	-18.782794	4.556096
-1019.937485	-20.426952	4.566093
-1018.002391	-20.535916	4.576090
-1016.127815	-14.996006	4.586086
-1014.115542	-20.706905	4.596083
-1012.410309	-17.406829	4.606080
-1010.719993	-14.433798	4.616077
-1008.392871	-9.272728	4.626074
-1006.647141	-14.316196	4.636070
-1004.632750	-16.045698	4.646067
-1002.902229	-12.331034	4.656064
-1001.108267	-10.652721	4.666061
-999.371049	-12.884770	4.676058
-997.637858	-10.263718	4.686054
-995.541406	-11.168665	4.696051
-993.256551	-14.980331	4.706048
-991.953326	-14.153230	4.716045
-989.758007	-16.154076	4.726042
-988.048703	-10.032085	4.736038
-985.990120	-11.091772	4.746035
-984.234292	-12.262310	4.756032
-982.588497	-10.911081	4.766029
-980.175911	-11.549381	4.776026
-978.656732	-18.240709	4.786022
-976.372141	-20.661966	4.796019
-974.837358	-14.906011	4.806016
-973.314722	-14.961140	4.816013
-971.307019	-13.914697	4.826010
-968.869177	-13.343632	4.836006
-967.311752	-17.552083	4.846003
-965.363526	-11.428021	4.856000
-963.599192	-10.483255	4.865997
-961.726259	-11.084627	4.875994
-959.577702	-18.169339	4.885990
-957.976080	-12.028059	4.895987
-955.908449	-12.834769	4.905984
-954.144925	-11.149234	4.915981
-952.334436	-18.399597	4.925978
-950.502791	-17.486538	4.935974
-948.451481	-12.879202	4.945971
-946.818183	-14.061888	4.955968
-944.725144	-20.301189	4.965965
-942.924708	-13.122218	4.975962
-941.095347	-19.754938	4.985958
-939.091913	-18.025611	4.995955
-937.403339	-21.163805	5.005952
-935.723881	-15.885979	5.015949
-933.331700	-13.917094	5.025946
-931.331792	-23.291031	5.035942
-929.603659	-17.346536	5.045939
-928.045863	-16.133126	5.055936
-926.169671	-16.277386	5.065933
-923.762720	-13.830059	5.075930
-922.274658	-18.207991	5.085926
-920.489216	-16.968052	5.095923
-918.710664	-18.018763	5.105920
-916.748512	-22.874868	5.115917
-914.864526	-20.917144	5.125914
-912.901425	-21.400786	5.135910
-911.191262	-22.708498	5.145907
-909.056831	-16.969692	5.155904
-907.048132	-14.655154	5.165901
-905.276897	-17.481872	5.175898
-903.566730	-11.657980	5.185894
-901.751747	-21.053122	5.195891
-899.681136	-23.715837	5.205888
-897.919869	-16.425786	5.215885
-895.595264	-26.737557	5.225882
-894.311494	-23.980429	5.235878
-892.418099	-18.025160	5.245875
-890.378434	-19.249125	5.255872
-888.402093	-18.296062	5.265869
-886.538354	-16.760097	5.275866
-884.750546	-18.520999	5.285862
-882.739664	-19.385910	5.295859
-880.800669	-17.547876	5.305856
-879.321952	-13.563478	5.315853
-877.364619	-21.900560	5.325850
-875.195015	-22.843300	5.335846
-873.327275	-22.996757	5.345843
-871.668836	-23.176730	5.355840
-869.782159	-17.499711	5.365837
-868.000541	-15.989557	5.375834
-866.187130	-17.309442	5.385830
-864.146767	-23.252348	5.395827
-862.260566	-18.318637	5.405824
-860.249535	-16.444743	5.415821
-858.346401	-18.591396	5.425818
-856.661498	-16.836599	5.435814
-854.611110	-23.748701	5.445811
-852.934606	-17.827716	5.455808
-851.387479	-14.676696	5.465805
-849.095026	-15.182064	5.475802
-846.668180	-15.650030	5.485798
-845.242386	-16.550449	5.495795
-843.628551	-21.490200	5.505792
-841.635621	-17.699968	5.515789
-839.748638	-19.945806	5.525786
-837.756900	-18.747169	5.535782
-836.056348	-20.917927	5.545779
-833.976920	-17.824674	5.555776
-832.079545	-12.705929	5.565773
-830.493099	-18.085590	5.575770
-828.573435	-14.438884	5.585766
-826.354466	-19.629911	5.595763
-824.703545	-12.178210	5.605760
-822.997747	-15.710185	5.615757
-820.936652	-13.321603	5.625754
-819.129906	-13.658617	5.635750
-816.962787	-18.622979	5.645747
-815.269933	-14.552795	5.655744
-813.729731	-14.103429	5.665741
-811.420187	-13.222538	5.675738
-809.447943	-17.085189	5.685734
-807.834707	-13.251111	5.695731
-806.068806	-13.097764	5.705728
-804.015386	-13.445888	5.715725
-802.050416	-21.797296	5.725722
-800.340012	-13.442063	5.735718
-798.407761	-22.273569	5.745715
-796.394517	-13.322559	5.755712
-794.865727	-15.430625	5.765709
-792.871825	-13.501589	5.775706
-791.144412	-12.897411	5.785702
-789.012513	-16.941194	5.795699
-787.304952	-9.501962	5.805696
-785.197751	-6.381436	5.815693
-783.241235	-8.931643	5.825690
-781.302545	-14.129086	5.835686
-779.646821	-13.913740	5.845683
-778.047866	-10.990929	5.855680
-776.146083	-5.516034	5.865677
-773.879367	-9.516159	5.875674
-772.343479	-12.486999	5.885670
-770.131411	-13.750775	5.895667
-768.549150	-3.275738	5.905664
-766.131370	-6.108244	5.915661
-764.515771	-7.771962	5.925658
-762.536782	-5.048344	5.935654
-760.885114	-5.748399	5.945651
-759.019971	-1.618043	5.955648
-757.396260	-9.401442	5.965645
-755.605831	-4.408950	5.975642
-753.264946	-8.281099	5.985638
-751.316184	-10.330413	5.995635
-749.875879	-8.030091	6.005632
-747.818044	-4.758006	6.015629
-745.943404	-3.298147	6.025626
-743.730650	-9.542502	6.035622
-742.273947	-13.465643	6.045619
-740.379795	-8.901967	6.055616
-738.468856	-7.706409	6.065613
-736.346915	-7.141068	6.075610
-734.729678	-8.612983	6.085606
-732.939973	-4.709563	6.095603
-730.897143	-9.045511	6.105600
-728.842620	-7.105111	6.115597
-726.921867	-5.568977	6.125594
-725.179099	-10.585361	6.135590
-723.715980	-8.973850	6.145587
-721.168796	-1.525729	6.155584
-719.601154	-6.520753	6.165581
-717.832386	-2.587648	6.175578
-715.866842	-9.316384	6.185574
-714.092505	-8.011611	6.195571
-712.035493	-12.724646	6.205568
-709.729371	-7.079610	6.215565
-708.527430	-11.676332	6.225562
-706.581160	-6.922792	6.235558
-704.548796	-7.689344	6.245555
-702.515564	-8.135526	6.255552
-701.176911	-12.169212	6.265549
-699.170997	-8.855390	6.275546
-696.941315	-7.227611	6.285542
-695.061613	-9.058748	6.295539
-693.467597	-6.048107	6.305536
-691.546661	-7.046887	6.315533
-689.656866	1.794958	6.325530
-687.842419	-11.250617	6.335526
-685.612896	-9.154082	6.345523
-683.688949	-8.827039	6.355520
-682.053360	-10.500086	6.365517
-680.379865	-5.049991	6.375514
-678.455514	-9.397993	6.385510
-676.255821	-12.390236	6.395507
-674.651930	-12.569073	6.405504
-672.687730	-8.826782	6.415501
-670.875757	-3.790522	6.425498
-668.878578	-7.137691	6.435494
-666.781716	-6.212319	6.445491
-665.070530	-13.227784	6.455488
-663.282168	-8.714684	6.465485
-661.530363	-9.167488	6.475482
-659.864665	-14.276935	6.485478
-657.587337	-5.129684	6.495475
-655.585899	-6.062429	6.505472
-654.631099	-11.682225	6.515469
-652.421922	-9.080261	6.525466
-649.804058	-8.343089	6.535462
-648.288207	-9.902307	6.545459
-646.603321	-15.127678	6.555456
-644.562239	-12.981791	6.565453
-642.246895	-10.950943	6.575450
-640.930556	-12.399646	6.585446
-639.370163	-10.067724	6.595443
-637.100073	-9.341215	6.605440
-634.911941	-8.375370	6.615437
-633.180712	-10.756830	6.625434
-631.406811	-9.380019	6.635430
-629.533764	-12.796373	6.645427
-628.040203	-12.261476	6.655424
-625.813792	-4.882742	6.665421
-623.764500	-8.720995	6.675418
-621.758181	-14.840157	6.685414
-620.264341	-16.541027	6.695411
-618.272445	-12.568311	6.705408
-616.366190	-6.955384	6.715405
-614.414011	-9.210342	6.725402
-612.833174	-1.046984	6.735398
-610.929828	-8.190258	6.745395
-608.759774	-12.874431	6.755392
-607.187249	-3.540604	6.765389
-605.016367	-5.890787	6.775386
-603.365296	-7.803987	6.785382
-601.083843	-5.977553	6.795379
-599.655146	-9.697056	6.805376
-598.060889	-1.520581	6.815373
-595.689429	-6.511216	6.825370
-593.744186	-7.801445	6.835366
-591.978882	-11.945066	6.845363
-589.945637	-10.022288	6.855360
-588.508570	-3.906356	6.865357
-586.453660	-10.133043	6.875354
-584.480124	-14.493002	6.885350
-582.331606	-16.715635	6.895347
-580.556121	-12.769396	6.905344
-578.935744	-8.730541	6.915341
-577.151307	-7.743614	6.925338
-575.085391	-13.814098	6.935334
-573.389318	-15.378525	6.945331
-571.429760	-8.878378	6.955328
-569.692261	-2.505325	6.965325
-567.602284	-9.409489	6.975322
-565.811765	-11.062048	6.985318
-563.754579	-8.810596	6.995315
-561.839705	-9.242729	7.005312
-560.136642	-10.326190	7.015309
-558.540460	-3.536042	7.025306
-556.289308	-11.144067	7.035302
-554.323900	-9.047200	7.045299
-552.592781	-4.569281	7.055296
-550.679195	-11.490203	7.065293
-548.781619	-10.426245	7.075290
-547.004332	-7.393638	7.085286
-545.548847	-10.401989	7.095283
-543.138359	-3.385188	7.105280
-541.391838	-9.919775	7.115277
-539.457272	-5.590974	7.125274
-537.532896	-10.090687	7.135270
-535.459358	-13.544566	7.145267
-533.626554	-13.840089	7.155264
-532.058286	-15.853668	7.165261
-530.515412	-10.384259	7.175258
-528.137212	-9.437533	7.185254
-526.234398	-10.488857	7.195251
-524.526423	-7.917024	7.205248
-522.518624	-7.134387	7.215245
-520.980404	-11.107811	7.225242
-518.903438	-11.772852	7.235238
-517.137402	-11.681064	7.245235
-515.191646	-9.815564	7.255232
-513.010249	-4.873834	7.265229
-511.086477	-11.196950	7.275226
-509.562513	-11.002765	7.285222
-507.517836	-11.460306	7.295219
-505.950328	-6.517980	7.305216
-503.985393	-6.331472	7.315213
-501.895859	-9.412629	7.325210
-499.908004	-7.104591	7.335206
-498.113114	-6.614628	7.345203
-496.117315	-8.601161	7.355200
-494.415094	-5.164390	7.365197
-492.851600	-6.427811	7.375194
-490.879182	-8.713460	7.385190
-488.696657	-8.840531	7.395187
-486.725407	-12.481956	7.405184
-485.120869	-7.061047	7.415181
-483.106088	-7.189373	7.425178
-481.259221	-1.702932	7.435174
-479.381555	-9.907647	7.445171
-477.588406	-4.850282	7.455168
-475.602934	-7.133421	7.465165
-473.903023	-2.761958	7.475162
-471.980119	-6.457924	7.485158
-469.780356	-8.343484	7.495155
-468.056396	-5.454641	7.505152
-466.659732	-6.592210	7.515149
-464.745549	-4.627208	7.525146
-462.388434	-1.675858	7.535142
-460.400977	-8.615746	7.545139
-458.775312	-10.513470	7.555136
-457.043861	-8.567703	7.565133
-455.080592	-5.634939	7.575130
-453.240011	-9.994171	7.585126
-451.056239	-11.914129	7.595123
-449.291489	-5.597865	7.605120
-447.510754	-7.159776	7.615117
-445.807686	-12.900005	7.625114
-443.770312	-10.719395	7.635110
-441.409026	-16.524325	7.645107
-440.168973	-12.620936	7.655104
-438.401477	-11.252431	7.665101
-436.338495	-11.905944	7.675098
-434.095985	-13.230898	7.685094
-432.582755	-18.435840	7.695091
-430.771344	-17.258245	7.705088
-428.958590	-14.567605	7.715085
-427.049137	-11.186909	7.725082
-425.017621	-15.786371	7.735078
-423.075738	-12.841230	7.745075
-421.060896	-6.502251	7.755072
-419.220610	-9.213770	7.765069
-417.511986	-11.103579	7.775066
-415.617450	-5.082261	7.785062
-413.739669	-5.640365	7.795059
-411.822298	-5.997376	7.805056
-410.302618	-8.833715	7.815053
-408.169806	-3.417240	7.825050
-406.147352	-7.381613	7.835046
-404.320277	-7.111339	7.845043
-402.437220	-10.992515	7.855040
-400.644002	-9.281408	7.865037
-398.788872	-7.267120	7.875034
-396.719893	-6.995262	7.885030
-394.960827	-9.447806	7.895027
-393.001424	-9.005387	7.905024
-391.437565	-10.041588	7.915021
-389.395090	-6.277412	7.925018
-387.500964	-8.438136	7.935014
-385.430082	-14.680919	7.945011
-383.789926	-8.964134	7.955008
-381.999936	-10.062441	7.965005
-380.049205	-11.775609	7.975002
-378.193977	-14.368344	7.984998
-376.244424	-11.350196	7.994995
-374.370202	-5.853380	8.004992
-372.404969	-8.922643	8.014989
-370.671823	-9.166225	8.024986
-368.751504	-13.891239	8.034982
-366.397559	-15.631675	8.044979
-364.954138	-9.528999	8.054976
-363.055676	-11.445029	8.064973
-361.352320	-8.976673	8.074970
-359.485452	-11.612896	8.084966
-357.692762	-10.013526	8.094963
-355.324855	-6.269981	8.104960
-353.783881	-9.874696	8.114957
-352.133219	-13.048867	8.124954
-350.112979	-14.249495	8.134950
-347.622073	-14.253920	8.144947
-346.144868	-13.001572	8.154944
-344.317455	-16.263364	8.164941
-342.343491	-13.469127	8.174938
-340.798053	-18.377624	8.184934
-338.749928	-19.688553	8.194931
-336.496404	-18.141348	8.204928
-334.914637	-12.548901	8.214925
-333.172610	-15.425331	8.224922
-331.071695	-16.069890	8.234918
-329.412868	-13.514446	8.244915
-327.527197	-12.415546	8.254912
-325.561413	-5.735331	8.264909
-323.679869	-11.763814	8.274906
-321.838974	-11.718383	8.284902
-320.045666	-11.732370	8.294899
-317.811388	-12.341701	8.304896
-316.235544	-3.435537	8.314893
-314.434604	0.923409	8.324890
-312.395489	-5.463686	8.334886
-310.479290	-9.992736	8.344883
-308.909436	-4.554342	8.354880
-306.802415	-6.792258	8.364877
-304.755991	-6.346941	8.374874
-303.046905	-5.909367	8.384870
-301.310799	-10.526088	8.394867
-299.443233	-3.136200	8.404864
-297.255093	-3.710338	8.414861
-295.477308	-6.229687	8.424858
-293.688908	-6.550694	8.434854
-291.470268	-9.359073	8.444851
-289.570441	-14.661508	8.454848
-288.389043	-14.021574	8.464845
-286.229887	-11.773249	8.474842
-284.151814	-11.995336	8.484838
-282.560404	-13.710067	8.494835
-280.700490	-16.028498	8.504832
-278.707949	-7.277576	8.514829
-276.677491	-7.587926	8.524826
-274.922652	-11.039595	8.534822
-273.245719	-15.230785	8.544819
-270.971390	-17.470110	8.554816
-269.195205	-9.142501	8.564813
-267.509672	-11.549583	8.574810
-265.526149	-9.556469	8.584807
-263.442931	-10.143817	8.594803
-261.675592	-10.072702	8.604800
-260.150363	-4.871272	8.614797
-258.130339	-13.696708	8.624794
-255.803947	-5.479266	8.634791
-253.813640	-13.879095	8.644787
-252.558055	-12.691855	8.654784
-250.601861	-13.225794	8.664781
-248.925242	-10.975313	8.674778
-246.460130	-16.415392	8.684775
-244.247305	-13.804748	8.694771
-243.116732	-26.963311	8.704768
-241.269071	-18.713953	8.714765
-239.285054	-24.052938	8.724762
-237.154268	-18.074428	8.734759
-235.701690	-19.054341	8.744755
-233.868058	-19.695301	8.754752
-231.934614	-19.707203	8.764749
-229.433613	-18.613411	8.774746
-227.671356	-11.428726	8.784743
-226.062155	-17.038963	8.794739
-224.578267	-15.664017	8.804736
-222.596241	-9.845339	8.814733
-220.525468	-15.128851	8.824730
-218.840251	-17.609767	8.834727
-216.589037	-22.969275	8.844723
-215.176904	-25.670914	8.854720
-212.927983	-17.873322	8.864717
-210.782742	-19.842284	8.874714
-209.333649	-20.167115	8.884711
-207.295220	-17.686605	8.894707
-205.300856	-13.920017	8.904704
-203.708095	-18.009800	8.914701
-201.804077	-22.576634	8.924698
-199.708189	-18.276921	8.934695
-198.126869	-23.374909	8.944691
-195.948563	-16.372225	8.954688
-194.248703	-23.050456	8.964685
-192.435874	-20.011542	8.974682
-190.831737	-19.851153	8.984679
-188.575507	-21.359348	8.994675
-186.633663	-22.910058	9.004672
-184.888497	-19.756780	9.014669
-183.002347	-20.964376	9.024666
-180.983508	-13.960418	9.034663
-178.764270	-23.464977	9.044659
-177.338530	-17.633083	9.054656
-175.890825	-15.746830	9.064653
-173.561211	-15.034637	9.074650
-171.299932	-17.600101	9.084647
-169.862521	-15.418041	9.094643
-168.131014	-15.663240	9.104640
-166.056140	-16.549081	9.114637
-164.571120	-18.023021	9.124634
-162.609342	-18.601354	9.134631
-160.062345	-16.443190	9.144627
-158.718896	-20.922175	9.154624
-157.022516	-17.283099	9.164621
-154.549739	-13.583116	9.174618
-152.880116	-16.126941	9.184615
-150.914310	-20.683010	9.194611
-149.219919	-16.156727	9.204608
-147.435087	-11.474428	9.214605
-145.532564	-8.984018	9.224602
-143.579817	-9.330383	9.234599
-141.592271	-17.179557	9.244595
-139.814127	-12.980642	9.254592
-137.970316	-10.820442	9.264589
-136.044009	-10.715281	9.274586
-134.223334	-9.654553	9.284583
-132.403474	-7.811948	9.294579
-130.312288	-7.116547	9.304576
-128.515556	-4.941549	9.314573
-127.035721	-7.201464	9.324570
-124.687496	-13.488543	9.334567
-122.716074	-9.398250	9.344563
-121.027105	-8.733069	9.354560
-119.430400	-6.073221	9.364557
-116.937778	-8.220276	9.374554
-115.503503	-9.730949	9.384551
-113.644170	-4.087597	9.394547
-111.625517	-6.137169	9.404544
-109.958695	-4.285700	9.414541
-108.173631	-5.265282	9.424538
-106.253448	-11.562344	9.434535
-103.807184	-8.252208	9.444531
-102.058438	-12.128024	9.454528
-100.519130	-10.067750	9.464525
-98.761655	-7.723970	9.474522
-96.516639	-7.714941	9.484519
-94.479276	-7.995567	9.494515
-93.120572	-10.767450	9.504512
-91.349282	-0.228072	9.514509
-88.924391	-9.575794	9.524506
-87.225312	-8.336505	9.534503
-85.593824	-11.577253	9.544499
-83.638393	-7.420568	9.554496
-81.731089	-7.734611	9.564493
-79.861125	-10.591393	9.574490
-77.810590	-6.964793	9.584487
-75.916460	-12.869274	9.594483
-73.886821	-9.731925	9.604480
-72.420093	-3.761970	9.614477
-70.698112	-1.868961	9.624474
-68.518451	-4.077731	9.634471
-66.431234	-1.479443	9.644467
-64.761171	-2.430200	9.654464
-62.752676	-5.693299	9.664461
-60.918702	-4.526531	9.674458
-59.104588	-0.653080	9.684455
-56.996885	-12.408199	9.694451
-55.447059	-11.404148	9.704448
-53.704543	-6.699136	9.714445
-51.584346	-10.510973	9.724442
-50.087881	-8.906922	9.734439
-47.799744	-4.807663	9.744435
-46.102200	-3.032181	9.754432
-44.072223	-2.438485	9.764429
-42.272443	-5.278872	9.774426
-40.280787	-5.877688	9.784423
-38.456772	-1.925697	9.794419
-36.553978	-6.192295	9.804416
-34.809278	-9.635819	9.814413
-32.550313	-7.208452	9.824410
-30.952738	-0.610389	9.834407
-29.254601	-5.574229	9.844403
-27.380692	-9.375049	9.854400
-25.308004	-12.068566	9.864397
-23.597258	-0.293999	9.874394
-21.782887	-5.032732	9.884391
-19.600887	0.576288	9.894387
-17.848815	-0.949720	9.904384
-15.745094	-9.115581	9.914381
-14.140580	-13.116819	9.924378
-12.302344	-5.113918	9.934375
-10.456580	-4.319074	9.944371
-8.394391	-8.115809	9.954368
-6.570702	-10.052074	9.964365
-4.782223	0.976049	9.974362
-3.831872	19.976340	9.984359
-2.190543	53.217622	9.994355
-1.212894	101.925438	10.004352
0.000000	164.976232	10.009357
0.889196	187.493058	10.014362
1.466566	231.923973	10.019367
2.424274	249.951081	10.024371
2.398530	272.647402	10.029376
2.109776	299.664048	10.034381
2.708665	310.538084	10.039386
2.557248	333.204332	10.044391
2.907643	335.535845	10.049395
2.992470	343.501333	10.054400
3.036259	363.673868	10.059405
4.011503	372.764413	10.064410
3.891669	388.419435	10.069415
3.981035	391.271745	10.074419
4.098445	388.310928	10.079424
4.039766	390.912711	10.084429
4.092971	390.250705	10.089434
4.144970	400.866876	10.094439
4.341787	391.635720	10.099443
4.147472	375.185088	10.104448
3.903511	379.978943	10.109453
4.200055	378.376437	10.114458
4.086384	385.494568	10.119463
4.398387	403.074430	10.124467
4.644694	405.833126	10.129472
4.349805	401.617130	10.134477
4.413733	390.153717	10.139482
4.274775	397.305399	10.144487
4.541362	412.261453	10.149491
4.658550	413.481560	10.154496
4.515673	409.432122	10.159501
4.680011	412.251450	10.164506
4.661984	420.371186	10.169511
4.736962	426.763860	10.174515
4.570395	432.820202	10.179520
4.509831	424.503123	10.184525
4.948105	432.720281	10.189530
4.631590	443.330193	10.194535
4.885125	437.218643	10.199539
4.963712	433.819623	10.204544
4.746817	439.247121	10.209549
4.844552	433.903179	10.214554
4.889101	439.469791	10.219559
4.861463	443.571731	10.224563
4.679437	451.106992	10.229568
4.697921	453.720818	10.234573
5.169945	462.857829	10.239578
5.071770	479.812998	10.244583
5.392392	477.929653	10.249587
5.699060	479.571209	10.254592
5.150265	477.245635	10.259597
5.330161	480.359535	10.264602
5.402604	489.311660	10.269607
5.550640	481.915200	10.274611
5.363088	486.609813	10.279616
5.293337	493.653361	10.284621
5.642188	490.966254	10.289626
5.502519	487.178736	10.294631
5.798882	495.464467	10.299635
5.880245	504.998079	10.304640
5.844664	510.883577	10.309645
6.218432	513.690304	10.314650
5.781419	515.944094	10.319655
5.973157	519.054787	10.324659
5.842386	521.808685	10.329664
5.745939	526.213751	10.334669
6.405213	530.025839	10.339674
5.964228	538.777479	10.344679
5.902641	528.324271	10.349683
5.801952	529.546218	10.354688
6.086648	534.047380	10.359693
5.927688	534.021726	10.364698
6.121867	544.647168	10.369703
6.416867	554.519564	10.374707
6.665629	567.656772	10.379712
6.603415	573.531860	10.384717
6.737792	570.493892	10.389722
6.527300	575.186544	10.394727
6.592203	577.944401	10.399731
6.850844	581.240999	10.404736
6.638293	573.035950	10.409741
6.912702	575.505657	10.414746
6.664020	582.801758	10.419751
6.822044	578.852654	10.424755
6.937863	583.591990	10.429760
6.502221	582.643933	10.434765
6.912310	577.993209	10.439770
6.655378	583.854319	10.444775
7.049377	580.518422	10.449779
7.070614	586.489730	10.454784
6.952561	582.944792	10.459789
7.088711	583.789040	10.464794
7.079467	597.821540	10.469799
7.598733	612.114742	10.474803
7.642817	611.179167	10.479808
7.169507	605.153885	10.484813
7.412915	610.868432	10.489818
7.643485	621.299403	10.494823
7.522873	632.523995	10.499827
7.529205	623.757588	10.504832
7.619859	625.300806	10.509837
7.693022	626.116779	10.514842
7.173371	627.675429	10.519847
7.321928	628.301242	10.524851
7.545801	640.390832	10.529856
7.672742	637.248339	10.534861
7.631793	640.374085	10.539866
7.339413	642.920850	10.544871
7.583057	653.563937	10.549875
7.827977	670.122600	10.554880
7.864201	667.962344	10.559885
8.271231	666.190080	10.564890
8.108767	672.751457	10.569895
8.312079	668.903116	10.574899
8.522420	666.417355	10.579904
7.964277	675.358102	10.584909
8.468134	666.391897	10.589914
8.132076	675.368774	10.594919
8.123365	673.537925	10.599923
8.533216	671.655837	10.604928
8.316848	675.957956	10.609933
8.485931	677.200370	10.614938
8.307108	688.206041	10.619943
8.538455	683.847242	10.624947
8.797400	696.938210	10.629952
8.568086	707.079016	10.634957
8.862195	701.329085	10.639962
8.663862	707.295849	10.644967
8.862560	705.154309	10.649971
9.310620	704.007362	10.654976
8.950767	701.302391	10.659981
8.644256	702.831609	10.664986
8.754235	707.131071	10.669991
8.867269	710.484635	10.674995
9.039561	703.342064	10.680000
8.762421	711.305855	10.685005
8.846232	702.715984	10.690010
8.655435	713.122159	10.695015
9.167951	723.234467	10.700019
9.337367	738.229600	10.705024
9.155828	741.336050	10.710029
9.347004	743.543348	10.715034
9.214930	744.582802	10.720039
9.350191	741.650042	10.725043
9.727058	743.779320	10.730048
9.366634	744.820426	10.735053
9.871406	742.323250	10.740058
9.885671	750.048416	10.745063
9.856311	747.948340	10.750067
9.553220	747.815952	10.755072
9.566336	755.360532	10.760077
9.703792	751.344649	10.765082
9.360200	752.833257	10.770087
9.721882	750.098118	10.775091
9.907858	768.194992	10.780096
10.090957	777.996322	10.785101
10.221306	774.338094	10.790106
9.969164	780.942524	10.795111
10.312261	779.299234	10.800115
10.171759	781.414592	10.805120
10.329669	786.133351	10.810125
10.721079	774.399959	10.815130
10.789519	776.926328	10.820135
10.675176	765.995303	10.825139
10.577887	756.135027	10.830144
10.544110	759.125753	10.835149
10.598899	751.261609	10.840154
10.513374	759.296779	10.845159
10.808453	748.398199	10.850163
10.929311	750.952681	10.855168
10.462716	761.007496	10.860173
10.757414	752.127235	10.865178
10.492567	754.274566	10.870183
10.558541	750.447779	10.875187
11.084818	769.992204	10.880192
10.912195	781.210031	10.885197
10.977246	774.777384	10.890202
10.879083	787.544793	10.895207
10.942383	783.123202	10.900211
10.820881	787.844080	10.905216
10.887903	789.636889	10.910221
11.106378	790.850712	10.915226
10.720801	794.118865	10.920231
10.799204	791.321369	10.925235
11.198996	789.635200	10.930240
11.096141	787.726927	10.935245
11.198374	807.929095	10.940250
10.992073	824.843967	10.945255
11.535925	822.407183	10.950259
11.926862	825.329839	10.955264
11.575302	831.355291	10.960269
11.891123	825.392383	10.965274
11.465349	829.975971	10.970279
11.930044	827.983016	10.975283
11.827127	831.614024	10.980288
11.463936	826.270819	10.985293
11.531596	838.469056	10.990298
11.937389	840.186419	10.995303
11.956054	837.080608	11.000307
12.226612	829.060222	11.005312
11.957044	830.508513	11.010317
11.969584	832.517903	11.015322
11.945977	839.960663	11.020327
12.134742	828.367764	11.025331
12.268236	824.752010	11.030336
12.330638	824.896426	11.035341
12.798522	824.481852	11.040346
12.742192	830.568788	11.045351
12.638988	824.221810	11.050355
12.505116	820.453348	11.055360
12.520486	833.072646	11.060365
12.958937	826.957662	11.065370
12.480652	828.286215	11.070375
12.482657	829.599919	11.075379
12.657511	821.945677	11.080384
12.648425	830.292247	11.085389
12.904961	835.830550	11.090394
12.911466	840.898176	11.095399
13.057219	832.964711	11.100403
12.986660	817.842377	11.105408
12.678686	807.320306	11.110413
12.988475	813.543013	11.115418
13.222687	824.395070	11.120423
12.648116	819.119293	11.125427
12.836716	823.794513	11.130432
12.687796	839.300633	11.135437
12.916371	834.344644	11.140442
13.061474	835.567499	11.145447
13.197649	841.186833	11.150451
13.000873	835.817461	11.155456
12.861339	843.510228	11.160461
12.921731	828.279381	11.165466
12.643628	853.549257	11.170471
13.164442	858.315159	11.175475
13.468519	862.622042	11.180480
13.568814	867.984646	11.185485
13.643834	865.510214	11.190490
13.615503	867.456353	11.195495
13.707345	868.326372	11.200499
13.823177	862.961024	11.205504
13.372134	876.030190	11.210509
13.620222	858.009921	11.215514
13.935591	866.994033	11.220519
13.859630	864.379699	11.225523
13.731468	866.054010	11.230528
13.886895	878.865251	11.235533
14.379306	884.543917	11.240538
14.365793	885.022662	11.245543
14.424698	870.122420	11.250547
14.418721	857.741448	11.255552
14.338631	864.105626	11.260557
14.542979	856.296707	11.265562
14.792889	862.908250	11.270567
14.336562	851.943036	11.275571
14.571670	854.392289	11.280576
14.792515	856.827015	11.285581
14.799033	855.146295	11.290586
14.338563	861.191614	11.295591
14.505025	856.802840	11.300595
14.723969	862.439176	11.305600
14.273804	865.043423	11.310605
14.229401	859.145028	11.315610
14.427640	864.434786	11.320615
14.529341	863.823655	11.325619
14.309770	868.320979	11.330624
14.667250	883.022299	11.335629
14.980935	882.066536	11.340634
14.930283	897.649417	11.345639
14.498634	896.545525	11.350643
14.852616	890.276842	11.355648
14.658337	889.771720	11.360653
14.853906	892.380126	11.365658
15.082026	898.530423	11.370663
15.250310	896.028154	11.375667
14.966923	900.626427	11.380672
15.102766	915.719855	11.385677
15.614579	919.879428	11.390682
15.784789	927.916233	11.395687
15.617169	912.805317	11.400691
15.712679	898.827976	11.405696
15.875246	896.659842	11.410701
15.738785	898.891759	11.415706
15.532249	898.694657	11.420711
15.477288	892.614903	11.425715
15.625856	899.482255	11.430720
15.190775	904.217064	11.435725
15.573628	907.707960	11.440730
15.822611	924.215672	11.445735
16.023732	920.817642	11.450739
16.015971	918.987391	11.455744
16.415758	928.219563	11.460749
16.211969	913.928000	11.465754
16.354544	908.252132	11.470759
16.095741	902.349428	11.475763
16.021840	892.447556	11.480768
15.753689	900.869766	11.485773
16.120147	912.063549	11.490778
16.324994	929.930403	11.495783
16.307149	929.123058	11.500787
16.692046	922.313013	11.505792
16.156794	928.886308	11.510797
16.552728	933.864301	11.515802
16.270054	938.339701	11.520807
15.923567	931.058606	11.525811
16.163132	938.611423	11.530816
15.967447	940.553896	11.535821
16.188096	933.837927	11.540826
16.535244	954.747896	11.545831
17.121500	945.916615	11.550835
17.648611	933.313526	11.555840
17.234574	931.145564	11.560845
17.430712	916.236749	11.565850
17.334735	910.150205	11.570855
17.045212	912.986652	11.575859
17.413749	909.341239	11.580864
17.276331	916.705655	11.585869
17.355164	907.976000	11.590874
17.367947	914.904534	11.595879
17.271431	910.753859	11.600883
17.432034	905.957526	11.605888
17.188694	906.096732	11.610893
17.381870	902.885593	11.615898
17.425886	920.317384	11.620903
17.388097	915.288618	11.625907
17.431224	912.923856	11.630912
17.309372	928.739632	11.635917
17.553173	910.014648	11.640922
17.447327	917.438388	11.645927
17.319773	923.152311	11.650931
17.464156	916.019955	11.655936
17.593403	919.487231	11.660941
17.827875	919.702803	11.665946
17.693569	922.672112	11.670951
17.573381	918.347468	11.675955
17.658560	911.214212	11.680960
17.460886	925.458523	11.685965
17.838895	930.850507	11.690970
18.162166	942.931186	11.695975
18.320641	951.131461	11.700979
18.508722	944.908570	11.705984
17.973356	927.618596	11.710989
17.961251	924.681858	11.715994
18.341723	944.123608	11.720999
18.084998	947.882065	11.726003
18.435445	945.538818	11.731008
17.995153	953.192810	11.736013
18.259912	943.400604	11.741018
18.339573	951.197158	11.746023
18.454603	952.979386	11.751027
18.056158	950.891642	11.756032
17.920301	956.530818	11.761037
18.001534	961.304619	11.766042
18.012406	978.336764	11.771047
18.394885	977.277622	11.776051
18.439066	977.481610	11.781056
18.505038	993.843932	11.786061
18.948577	981.326186	11.791066
18.605823	990.165050	11.796071
19.224848	994.487051	11.801075
19.838827	980.507586	11.806080
19.517877	985.782586	11.811085
19.555429	965.915399	11.816090
19.265559	967.991260	11.821095
19.260558	967.905656	11.826099
19.935460	967.662032	11.831104
19.463390	966.752958	11.836109
19.430456	955.969683	11.841114
19.305565	951.399521	11.846119
19.766644	963.247774	11.851123
19.769168	943.751751	11.856128
19.349263	948.383313	11.861133
19.524105	943.320055	11.866138
19.501832	944.414511	11.871143
19.199911	945.527309	11.876147
19.663866	952.696662	11.881152
19.690557	966.426491	11.886157
19.837601	965.517058	11.891162
19.630923	970.973381	11.896167
19.489935	973.172927	11.901171
19.680858	972.897415	11.906176
19.474291	981.230952	11.911181
20.031983	975.325992	11.916186
19.859372	972.897158	11.921191
19.796950	970.909693	11.926195
19.980912	972.852210	11.931200
19.593881	982.618000	11.936205
19.659519	986.833958	11.941210
20.204578	997.667972	11.946215
20.531935	1003.885771	11.951219
20.581706	1002.987881	11.956224
20.398062	1002.698431	11.961229
20.395754	1004.299468	11.966234
20.303564	1005.606442	11.971239
20.667737	1004.579253	11.976243
20.881734	1006.989519	11.981248
20.553437	1012.660130	11.986253
20.781767	1012.576361	11.991258
20.722722	999.384903	11.996263
20.614512	998.853967	12.001267
21.037482	993.801441	12.006272
20.834671	992.756594	12.011277
21.065446	975.512051	12.016282
20.707073	971.168625	12.021287
21.004192	974.024501	12.026291
20.789314	969.636736	12.031296
20.839766	972.835298	12.036301
20.984341	968.459719	12.041306
21.380885	968.366452	12.046311
20.891529	969.613229	12.051315
20.763538	970.059894	12.056320
20.499471	973.884353	12.061325
20.534420	973.499399	12.066330
20.445997	977.107824	12.071335
20.282207	980.054173	12.076339
20.576554	972.693185	12.081344
20.541461	977.514173	12.086349
20.768464	991.295733	12.091354
20.941883	1009.374515	12.096359
20.774777	999.402897	12.101363
21.094093	994.257615	12.106368
20.538074	985.822289	12.111373
20.696340	980.726335	12.116378
20.880117	991.280446	12.121383
21.054049	982.792601	12.126387
20.622634	984.996154	12.131392
20.317826	992.242069	12.136397
20.499090	992.347159	12.141402
20.929866	1008.303924	12.146407
20.931685	1008.618597	12.151411
21.265645	1003.230802	12.156416
20.638769	991.784730	12.161421
20.842421	978.793380	12.166426
20.898367	983.117183	12.171431
20.550509	983.826544	12.176435
20.806620	977.852107	12.181440
20.589240	982.381850	12.186445
20.680519	986.354203	12.191450
21.169539	1009.055312	12.196455
21.130739	992.100128	12.201459
21.149783	982.655946	12.206464
20.682541	984.356826	12.211469
20.785141	980.947254	12.216474
20.944925	981.239975	12.221479
20.911228	976.097593	12.226483
21.086299	977.416373	12.231488
21.102646	983.430909	12.236493
21.234590	973.845007	12.241498
20.966145	981.420208	12.246503
21.100096	975.680663	12.251507
21.064925	967.966043	12.256512
20.487109	960.678807	12.261517
20.707768	958.120969	12.266522
20.563117	954.815768	12.271527
20.781444	971.009050	12.276531
20.844014	961.451630	12.281536
21.088902	971.362094	12.286541
20.773471	962.825137	12.291546
20.606185	958.734345	12.296551
20.721565	958.706653	12.301555
20.920814	950.784877	12.306560
20.474211	964.947956	12.311565
20.797543	971.658273	12.316570
20.827899	978.552244	12.321575
20.739680	982.972606	12.326579
20.922396	975.111284	12.331584
20.533387	974.255073	12.336589
20.721730	981.576694	12.341594
21.064291	980.136765	12.346599
20.722632	974.655212	12.351603
20.807168	963.214688	12.356608
20.611951	973.730345	12.361613
20.844172	973.678278	12.366618
20.645253	976.828807	12.371623
20.884706	977.993655	12.376627
20.871615	972.864714	12.381632
20.752271	979.432643	12.386637
20.690770	971.563458	12.391642
20.657835	967.828575	12.396647
20.884231	989.417318	12.401651
21.291483	982.550915	12.406656
20.564940	968.976164	12.411661
20.615296	958.542157	12.416666
20.723069	963.312199	12.421671
20.855744	970.880595	12.426675
20.672115	969.124701	12.431680
20.690799	975.923962	12.436685
20.731550	988.692982	12.441690
20.848483	993.682120	12.446695
20.770847	999.688696	12.451699
21.087916	989.297756	12.456704
20.871009	985.421912	12.461709
20.984919	973.685423	12.466714
20.830195	971.385364	12.471719
20.383368	964.422245	12.476723
20.717089	962.599756	12.481728
20.418322	974.948951	12.486733
20.744990	979.647520	12.491738
20.791721	991.847098	12.496743
21.259740	1000.074064	12.501747
21.262289	984.225351	12.506752
21.024538	977.329011	12.511757
21.142461	975.532072	12.516762
20.543984	972.637044	12.521767
20.366142	971.245288	12.526771
20.854195	974.265401	12.531776
21.001873	969.033898	12.536781
20.902545	968.659730	12.541786
20.947418	968.776363	12.546791
20.836796	970.138600	12.551795
21.063285	970.761329	12.556800
21.091447	977.136599	12.561805
21.251915	974.631315	12.566810
21.129216	969.782088	12.571815
20.629235	960.857959	12.576819
20.691855	946.901214	12.581824
20.656856	961.511217	12.586829
21.135502	967.092406	12.591834
20.523619	957.277599	12.596839
20.736881	966.567828	12.601843
20.837082	968.715757	12.606848
20.662382	970.732004	12.611853
20.821928	965.778730	12.616858
20.958441	966.409781	12.621863
20.557597	961.380088	12.626867
20.678190	962.744129	12.631872
20.508548	975.039212	12.636877
20.790093	976.021186	12.641882
21.125920	980.620685	12.646887
20.784277	981.362928	12.651891
20.923629	976.411139	12.656896
20.729679	970.110054	12.661901
20.594767	970.310011	12.666906
20.862150	969.683496	12.671911
20.950605	980.337627	12.676915
20.584535	958.020843	12.681920
20.525431	965.261724	12.686925
20.785235	973.875689	12.691930
20.879522	973.930956	12.696935
20.784692	979.237053	12.701939
21.150258	971.134384	12.706944
21.049606	962.675470	12.711949
21.111997	954.832815	12.716954
21.147413	952.618974	12.721959
20.872400	948.679286	12.726963
20.704469	947.166227	12.731968
20.670978	947.958267	12.736973
20.521875	945.151197	12.741978
20.832841	951.696652	12.746983
20.403213	953.275423	12.751987
20.613497	942.889796	12.756992
20.660971	950.920025	12.761997
20.603318	946.831755	12.767002
20.589526	950.935797	12.772007
20.888516	972.421676	12.777011
20.920359	972.098045	12.782016
20.782038	964.006377	12.787021
20.750855	955.856082	12.792026
20.860568	945.352697	12.797031
20.519128	953.476844	12.802035
20.957811	967.385510	12.807040
20.713530	962.056607	12.812045
20.598974	950.315886	12.817050
20.846344	966.395632	12.822055
20.779417	987.894138	12.827059
21.000833	974.738693	12.832064
20.810520	974.620913	12.837069
20.703210	964.236041	12.842074
20.669128	961.758984	12.847079
20.688517	971.333506	12.852083
20.719344	962.295473	12.857088
20.776153	977.486591	12.862093
20.939045	984.123762	12.867098
20.973294	977.431444	12.872103
20.974411	962.950757	12.877107
20.573976	951.853126	12.882112
20.274270	967.548252	12.887117
20.658491	980.997322	12.892122
20.798548	985.869598	12.897127
20.862194	990.861950	12.902131
20.825358	985.509709	12.907136
20.544472	994.954545	12.912141
20.718667	991.512564	12.917146
21.004595	992.262867	12.922151
20.964589	993.796156	12.927155
21.202392	987.689064	12.932160
20.540904	973.101316	12.937165
20.658926	952.730481	12.942170
21.154667	958.361236	12.947175
20.698092	961.361333	12.952179
20.842549	954.281841	12.957184
20.712713	957.682231	12.962189
20.539633	958.847150	12.967194
20.991503	952.134556	12.972199
20.532719	965.050387	12.977203
20.799641	951.666502	12.982208
20.842669	961.948279	12.987213
20.782334	960.322430	12.992218
20.813703	953.667721	12.997223
20.425688	965.082083	13.002227
20.939061	968.343380	13.007232
20.650053	989.454045	13.012237
20.984405	985.234608	13.017242
20.921820	974.682587	13.022247
20.737510	968.352218	13.027251
20.968763	953.908661	13.032256
20.514616	956.915840	13.037261
20.637017	952.498278	13.042266
20.913048	964.238128	13.047271
20.845519	969.507962	13.052275
21.039511	953.853034	13.057280
20.692882	966.155166	13.062285
20.598901	951.754346	13.067290
20.687827	966.659290	13.072295
20.607421	980.866572	13.077299
20.972270	974.811124	13.082304
20.867251	973.610170	13.087309
21.107010	968.705116	13.092314
21.119228	955.505818	13.097319
21.295769	958.282497	13.102323
21.040073	949.102544	13.107328
20.974172	968.084017	13.112333
20.888191	962.385342	13.117338
20.966077	963.582627	13.122343
20.770963	967.375525	13.127347
20.785203	962.485059	13.132352
20.695468	960.552411	13.137357
20.927850	963.780567	13.142362
20.894737	958.714275	13.147367
20.657578	966.782260	13.152371
20.776967	967.248485	13.157376
21.117188	971.756044	13.162381
21.158818	960.127089	13.167386
21.027630	945.393182	13.172391
20.826041	941.055646	13.177395
20.427467	937.872142	13.182400
20.619518	938.133672	13.187405
20.683392	933.488125	13.192410
20.713923	939.156397	13.197415
20.573101	951.354942	13.202419
21.033760	958.558021	13.207424
20.782748	949.009373	13.212429
20.845131	942.779217	13.217434
20.775936	936.797017	13.222439
20.623262	942.924595	13.227443
20.636027	941.231347	13.232448
20.603144	957.922027	13.237453
20.775805	969.779471	13.242458
20.975792	965.545182	13.247463
20.851032	969.746806	13.252467
20.680178	967.856880	13.257472
20.824357	970.168980	13.262477
20.968557	966.842278	13.267482
20.962992	945.345541	13.272487
20.630374	948.753065	13.277491
20.706085	927.775310	13.282496
20.536161	943.860658	13.287501
20.592874	965.123989	13.292506
20.898839	963.708494	13.297511
20.993387	976.662490	13.302515
21.066044	962.074407	13.307520
20.913562	957.177791	13.312525
20.589787	943.502428	13.317530
21.191105	944.549573	13.322535
20.707144	945.472925	13.327539
20.680062	935.753655	13.332544
20.673191	943.787671	13.337549
20.290059	937.231273	13.342554
20.621184	946.390361	13.347559
20.840132	965.647465	13.352563
20.937231	963.204363	13.357568
20.849580	963.239903	13.362573
21.101812	966.027290	13.367578
20.776108	944.702284	13.372583
20.772001	944.544290	13.377587
20.600388	937.717548	13.382592
20.550637	935.754363	13.387597
20.438540	956.971626	13.392602
20.559347	971.948476	13.397607
20.679692	983.459639	13.402611
20.767363	976.559610	13.407616
21.005011	977.414899	13.412621
20.661097	974.550436	13.417626
20.949894	973.196700	13.422631
20.612881	978.296820	13.427635
21.201543	978.174957	13.432640
21.199265	980.211774	13.437645
20.526581	968.330285	13.442650
20.685298	960.467954	13.447655
20.593983	973.904602	13.452659
20.859767	973.459151	13.457664
20.591044	974.885994	13.462669
20.696393	979.645009	13.467674
20.899801	979.358673	13.472679
20.792993	988.556949	13.477683
20.789570	982.716218	13.482688
21.185664	983.784736	13.487693
20.884811	972.382649	13.492698
20.782929	965.626834	13.497703
20.647489	955.253501	13.502707
20.821113	947.711514	13.507712
20.709742	955.813979	13.512717
20.662159	954.570812	13.517722
20.857371	961.094275	13.522727
20.617317	975.150898	13.527731
20.875643	975.272776	13.532736
21.077145	972.587168	13.537741
20.707678	964.386710	13.542746
20.760938	948.593285	13.547751
20.845907	954.434992	13.552755
21.035731	944.774842	13.557760
20.586630	949.907593	13.562765
20.803640	948.874059	13.567770
21.001950	953.588707	13.572775
20.574706	949.311963	13.577779
20.727647	946.197319	13.582784
20.809309	952.245644	13.587789
20.995807	950.347345	13.592794
21.076264	946.688158	13.597799
20.654924	961.339137	13.602803
21.223948	948.522009	13.607808
20.698135	947.981754	13.612813
20.700382	948.608587	13.617818
20.732929	950.420747	13.622823
20.581194	953.043709	13.627827
20.858426	946.305008	13.632832
20.618719	953.587901	13.637837
20.841954	945.845962	13.642842
20.850132	952.222674	13.647847
20.615321	954.971196	13.652851
21.123008	949.548107	13.657856
20.990152	950.958364	13.662861
20.997996	959.603284	13.667866
21.333958	950.382284	13.672871
21.028407	952.825172	13.677875
20.958374	946.831665	13.682880
20.991415	952.059777	13.687885
20.956526	940.713560	13.692890
21.170262	930.546033	13.697895
20.676839	924.180260	13.702899
20.636425	913.675794	13.707904
20.505737	920.611167	13.712909
20.656948	919.316945	13.717914
20.908088	915.428765	13.722919
20.555082	917.368998	13.727923
20.762334	919.907906	13.732928
20.943034	938.648116	13.737933
20.737234	933.322099	13.742938
20.652877	922.599768	13.747943
20.515181	937.269988	13.752947
21.009289	943.611145	13.757952
20.809243	945.906076	13.762957
20.623824	946.863110	13.767962
20.863053	941.639998	13.772967
20.727964	943.548793	13.777971
21.154449	951.591803	13.782976
20.688893	934.561034	13.787981
20.578506	928.037219	13.792986
20.725862	925.535770	13.797991
20.536802	947.067002	13.802995
20.746372	950.417093	13.808000
20.779281	949.439203	13.813005
20.672779	958.975698	13.818010
20.971763	961.728226	13.823015
20.576202	958.144729	13.828019
20.986134	962.434282	13.833024
20.863871	961.889573	13.838029
20.969682	956.498279	13.843034
20.813241	944.945532	13.848039
20.784139	934.281614	13.853043
20.734811	925.909841	13.858048
20.582773	934.759396	13.863053
20.642353	954.400650	13.868058
20.888175	956.327427	13.873063
20.848601	963.933642	13.878067
20.863128	962.613114	13.883072
20.818402	952.236072	13.888077
20.740563	937.243948	13.893082
20.834153	931.147394	13.898087
20.868719	933.905384	13.903091
20.676630	934.075671	13.908096
20.874815	930.648143	13.913101
20.806265	929.937122	13.918106
20.776585	933.444281	13.923111
20.764557	928.627408	13.928115
20.655611	923.124526	13.933120
20.728962	930.392023	13.938125
20.852506	943.143653	13.943130
20.638265	932.346085	13.948135
20.664176	946.936552	13.953139
20.787202	953.265548	13.958144
20.989008	962.294054	13.963149
20.790238	956.888666	13.968154
20.668401	941.441847	13.973159
20.507267	952.858748	13.978163
20.872512	954.212420	13.983168
20.805073	962.068542	13.988173
21.307822	952.435262	13.993178
21.246642	941.998285	13.998183
20.961258	944.962317	14.003187
21.247534	937.496151	14.008192
20.932488	931.868011	14.013210
20.740203	936.912330	14.018227
21.086941	931.017821	14.023245
20.991044	937.335072	14.028263
21.127720	937.988048	14.033280
21.293127	936.332790	14.038298
20.980671	928.043651	14.043315
20.374665	912.514198	14.048333
20.273067	924.592257	14.053351
20.479398	926.280212	14.058368
20.687787	938.909899	14.063386
20.684581	933.886861	14.068403
20.643272	945.373458	14.073421
20.406820	944.476910	14.078439
20.863343	951.193975	14.083456
21.185146	971.576834	14.088474
20.723151	974.479457	14.093491
21.253963	971.854789	14.098509
21.071695	976.740699	14.103527
21.014984	971.617366	14.108544
21.020482	971.781774	14.113562
20.703227	972.200746	14.118579
20.684380	967.548909	14.123597
20.803185	971.631963	14.128615
20.986372	969.242106	14.133632
20.984241	978.888022	14.138650
20.884763	1001.174381	14.143667
21.376881	1005.730487	14.148685
21.180643	1008.453684	14.153703
21.393162	1008.116028	14.158720
21.502988	1009.666983	14.163738
21.001440	1013.379603	14.168755
21.122131	1005.018521	14.173773
21.359740	1010.765199	14.178791
21.157228	1008.134749	14.183808
21.051622	1005.994809	14.188826
20.860545	1009.047066	14.193843
21.239716	1007.699270	14.198861
21.000648	1005.492835	14.203879
21.547368	1027.500711	14.208896
21.728164	1034.165079	14.213914
21.733683	1037.174186	14.218931
21.498172	1015.036525	14.223949
21.494430	1009.068997	14.228967
21.293208	1006.880485	14.233984
21.650759	1026.307610	14.239002
21.833858	1036.513579	14.244019
21.972497	1025.247224	14.249037
21.722362	1020.794093	14.254055
21.407931	1010.861819	14.259072
21.726870	1010.020843	14.264090
21.784345	1005.089748	14.269107
21.726696	999.470468	14.274125
21.525012	1005.811790	14.279143
21.663880	1015.606795	14.284160
22.055356	1032.687388	14.289178
21.859312	1029.682570	14.294195
22.297737	1006.145026	14.299213
22.169726	1015.581034	14.304231
21.860926	1011.656112	14.309248
22.254018	1010.149225	14.314266
21.873834	1011.962946	14.319283
21.646309	1006.646037	14.324301
21.668240	1008.274664	14.329319
22.006346	1008.433232	14.334336
22.028613	1009.552316	14.339354
21.682044	1007.409197	14.344371
21.992712	1002.483515	14.349389
21.814045	1000.633287	14.354407
21.454023	1004.974050	14.359424
21.762354	1021.324737	14.364442
22.059157	1032.134484	14.369459
22.511524	1030.774924	14.374477
22.194589	1045.884709	14.379495
22.114321	1038.586094	14.384512
22.314145	1031.600117	14.389530
22.186756	1030.827396	14.394547
22.189630	1020.586758	14.399565
22.035459	1021.086045	14.404583
21.930025	1035.299651	14.409600
22.478662	1035.713877	14.414618
22.120510	1034.981507	14.419635
22.358037	1033.025664	14.424653
22.282483	1044.788304	14.429671
22.351531	1040.537942	14.434688
22.332540	1032.429158	14.439706
22.171294	1040.132560	14.444723
22.439577	1029.764122	14.449741
22.569105	1041.249453	14.454759
22.159334	1050.182568	14.459776
22.484767	1031.994290	14.464794
22.471355	1042.114656	14.469811
22.448570	1036.877996	14.474829
22.304394	1035.495508	14.479847
22.294266	1040.800777	14.484864
22.888452	1040.587856	14.489882
22.380442	1045.775324	14.494899
22.751885	1040.802593	14.499917
22.449150	1041.108045	14.504935
22.590797	1040.782934	14.509952
22.661329	1038.278513	14.514970
22.368605	1043.388515	14.519987
22.574315	1041.066838	14.525005
22.633468	1042.861147	14.530023
22.291263	1039.856187	14.535040
22.763061	1038.296430	14.540058
22.384353	1039.628763	14.545075
22.625816	1036.662326	14.550093
22.775562	1037.168960	14.555111
22.684883	1044.365347	14.560128
23.260589	1054.738285	14.565146
23.056907	1051.481603	14.570163
23.148368	1043.790523	14.575181
23.212947	1045.992595	14.580199
22.879102	1039.426879	14.585216
23.000119	1037.443763	14.590234
22.635423	1048.223224	14.595251
22.683807	1035.975803	14.600269
22.862055	1046.823999	14.605287
22.726344	1045.875524	14.610304
22.821960	1036.043417	14.615322
22.834706	1051.749093	14.620339
22.929700	1060.595278	14.625357
22.905380	1070.626186	14.630375
22.955348	1076.591294	14.635392
23.394306	1065.353347	14.640410
23.314902	1078.794360	14.645427
23.726051	1066.072482	14.650445
23.509968	1053.801487	14.655463
23.273363	1045.461876	14.660480
23.394368	1039.024096	14.665498
22.983739	1044.939806	14.670515
23.130285	1043.584250	14.675533
23.148857	1041.194650	14.680551
23.157156	1035.517589	14.685568
23.538520	1040.759673	14.690586
23.274770	1038.238150	14.695603
23.186854	1039.650558	14.700621
23.415173	1054.045165	14.705639
23.379649	1064.114214	14.710656
23.913322	1059.884587	14.715674
23.482184	1055.808175	14.720691
23.107191	1039.366086	14.725709
23.341941	1047.053177	14.730727
23.363085	1066.651818	14.735744
23.707624	1070.170172	14.740762
23.247484	1066.096760	14.745779
23.372474	1067.202961	14.750797
23.497667	1061.930685	14.755815
23.380947	1068.637022	14.760832
23.493298	1062.690123	14.765850
23.518867	1072.547506	14.770867
23.711025	1063.599292	14.775885
23.581679	1075.695219	14.780903
23.509159	1071.675436	14.785920
23.959235	1068.201536	14.790938
23.756057	1080.636134	14.795955
23.415456	1068.806194	14.800973
23.717320	1061.726325	14.805991
23.409394	1075.485278	14.811008
23.615448	1071.527584	14.816026
23.593837	1084.963025	14.821043
23.894995	1088.859716	14.826061
24.204569	1092.628970	14.831079
23.857082	1101.936112	14.836096
23.889336	1091.759293	14.841114
23.756612	1092.836053	14.846131
24.050396	1099.757083	14.851149
23.987770	1099.281153	14.856167
23.778590	1100.836019	14.861184
24.303486	1098.881690	14.866202
23.891483	1106.237535	14.871219
23.849729	1102.099075	14.876237
24.180167	1098.701984	14.881255
23.933768	1105.998725	14.886272
24.186593	1092.692899	14.891290
24.060287	1097.306239	14.896307
23.976534	1103.914018	14.901325
24.276526	1101.110776	14.906343
24.054401	1098.472255	14.911360
24.626433	1099.879007	14.916378
24.101743	1098.375912	14.921395
24.068342	1097.878040	14.926413
24.396042	1091.920983	14.931431
24.088578	1106.575623	14.936448
24.351928	1100.810318	14.941466
24.182322	1098.489196	14.946483
24.244195	1099.358957	14.951501
24.367949	1098.184877	14.956519
24.189477	1104.502573	14.961536
24.476416	1100.863707	14.966554
24.644110	1103.099293	14.971571
24.356776	1104.031683	14.976589
24.489174	1097.748630	14.981607
24.042647	1103.885888	14.986624
24.547958	1115.468669	14.991642
24.853419	1120.677334	14.996659
24.726751	1116.251829	15.001677
24.929009	1099.033488	15.006695
24.584068	1092.337357	15.011712
24.432749	1099.377617	15.016730
24.623688	1098.508973	15.021747
24.577833	1106.495404	15.026765
25.197616	1111.771444	15.031783
24.846450	1110.192530	15.036800
24.812782	1104.826994	15.041818
24.826084	1090.769653	15.046835
24.480606	1102.303790	15.051853
24.996914	1099.624891	15.056871
24.800470	1108.086389	15.061888
24.772555	1114.136524	15.066906
24.734144	1119.152551	15.071923
25.249080	1119.352461	15.076941
25.207924	1120.378875	15.081959
24.767429	1112.419882	15.086976
24.855781	1104.327699	15.091994
24.846054	1116.214550	15.097011
24.802269	1123.941953	15.102029
25.337778	1118.054776	15.107047
24.795989	1115.613197	15.112064
24.905100	1115.533446	15.117082
24.769960	1118.511562	15.122099
24.798133	1118.513803	15.127117
25.187202	1113.525428	15.132135
25.130997	1119.777675	15.137152
25.095805	1122.154750	15.142170
25.454753	1115.670237	15.147187
25.150640	1122.369746	15.152205
25.187658	1123.510327	15.157223
25.175487	1115.612552	15.162240
25.447636	1121.123408	15.167258
25.358143	1119.331505	15.172275
25.152949	1127.627966	15.177293
25.551752	1122.434753	15.182311
25.356065	1125.913448	15.187328
25.540380	1122.140586	15.192346
25.268691	1120.136593	15.197363
25.294444	1124.923493	15.202381
25.335859	1122.757542	15.207399
25.173807	1137.750302	15.212416
25.545559	1145.739962	15.217434
26.079103	1152.421074	15.222451
25.412192	1140.623008	15.227469
25.503216	1141.745275	15.232487
25.277358	1160.419768	15.237504
25.750506	1162.259263	15.242522
25.849009	1149.014889	15.247539
25.817075	1159.875181	15.252557
25.892332	1149.735050	15.257575
25.227145	1157.377261	15.262592
25.599557	1154.619472	15.267610
25.885191	1157.596719	15.272627
25.484155	1153.601347	15.277645
25.888528	1150.514824	15.282663
25.751878	1158.656230	15.287680
25.763758	1151.386649	15.292698
25.738935	1147.958325	15.297715
25.793989	1152.930382	15.302733
26.048627	1145.668006	15.307751
25.855459	1146.447234	15.312768
26.017047	1154.420566	15.317786
26.036717	1150.847593	15.322803
25.844550	1154.905266	15.327821
26.137009	1155.690610	15.332839
25.974126	1157.720262	15.337856
25.634987	1155.491196	15.342874
26.275484	1160.386899	15.347891
26.070912	1171.574460	15.352909
26.324775	1170.440672	15.357927
26.136796	1162.558447	15.362944
26.558234	1159.183540	15.367962
26.515854	1151.040118	15.372979
26.436527	1152.379404	15.377997
26.435439	1145.264424	15.383015
26.323087	1150.623874	15.388032
26.059319	1144.287850	15.393050
26.206485	1142.314806	15.398067
25.981310	1150.046547	15.403085
26.186737	1156.149218	15.408103
26.623723	1169.802980	15.413120
26.694377	1161.683878	15.418138
26.449456	1160.664743	15.423155
26.346288	1168.405499	15.428173
26.760682	1168.514766	15.433191
26.850268	1173.094657	15.438208
26.590680	1154.191905	15.443226
26.814450	1144.486982	15.448243
26.464257	1152.294888	15.453261
26.478988	1145.020884	15.458279
26.362189	1155.199209	15.463296
26.816664	1153.699897	15.468314
27.257339	1158.410156	15.473331
27.104990	1160.456113	15.478349
27.125529	1146.299048	15.483367
26.849718	1150.218686	15.488384
26.798150	1140.016440	15.493402
26.916816	1144.796078	15.498419
26.585926	1143.488509	15.503437
27.066008	1142.817553	15.508455
26.826312	1146.184103	15.513472
26.894441	1145.247134	15.518490
26.890857	1139.357882	15.523507
26.773079	1147.505497	15.528525
27.149494	1150.512851	15.533543
26.827457	1144.258870	15.538560
26.288553	1149.102034	15.543578
26.901814	1150.209179	15.548595
26.677227	1172.067588	15.553613
26.800159	1175.336536	15.558631
26.847917	1184.651164	15.563648
26.948952	1180.033832	15.568666
26.945107	1175.659699	15.573683
26.600000	1186.305571	15.578701
27.508627	1185.850533	15.583719
27.231291	1190.960307	15.588736
27.099243	1195.481345	15.593754
27.299310	1197.565713	15.598771
27.521234	1206.797733	15.603789
27.552594	1206.285604	15.608807
27.333113	1193.243363	15.613824
27.349896	1207.627132	15.618842
27.578311	1192.962690	15.623859
27.203894	1198.324170	15.628877
27.404591	1203.287810	15.633895
27.707617	1208.678434	15.638912
27.565950	1210.677287	15.643930
27.890686	1207.302412	15.648947
27.563029	1193.903094	15.653965
27.558252	1176.719769	15.658983
27.373132	1190.069939	15.664000
27.631699	1200.187087	15.669018
27.923545	1194.554669	15.674035
27.671216	1202.520639	15.679053
27.810424	1197.907388	15.684071
27.890842	1190.334675	15.689088
27.618873	1188.910692	15.694106
27.789429	1189.530309	15.699123
27.726746	1193.451609	15.704141
27.829248	1196.359859	15.709159
27.976346	1199.446306	15.714176
27.748377	1200.861478	15.719194
28.317631	1193.393945	15.724211
28.355719	1185.405227	15.729229
28.250880	1173.466276	15.734247
28.134465	1170.758039	15.739264
27.775915	1165.817506	15.744282
28.142156	1158.518665	15.749299
27.967949	1168.274522	15.754317
28.141779	1156.583893	15.759335
27.995128	1169.969186	15.764352
27.765759	1168.711538	15.769370
28.049396	1165.451602	15.774387
28.296298	1188.610809	15.779405
28.208958	1197.296190	15.784423
28.303964	1199.737182	15.789440
28.240151	1203.613399	15.794458
28.567817	1203.311515	15.799475
28.150511	1187.367117	15.804493
28.062084	1192.106679	15.809511
28.330194	1199.910577	15.814528
28.075894	1204.788828	15.819546
28.372736	1197.182155	15.824563
28.425983	1204.891387	15.829581
28.625290	1200.779292	15.834599
28.343399	1193.294682	15.839616
28.401836	1203.206754	15.844634
28.612853	1204.361213	15.849651
27.944403	1205.105779	15.854669
28.095709	1206.451200	15.859687
28.488668	1202.451585	15.864704
28.542506	1205.592215	15.869722
28.838787	1202.350972	15.874739
28.449395	1210.103811	15.879757
28.679869	1228.433588	15.884775
28.687679	1235.001706	15.889792
28.724128	1242.598866	15.894810
28.844904	1240.028707	15.899827
28.769482	1240.881854	15.904845
29.098055	1233.773705	15.909863
29.071461	1230.153523	15.914880
28.737576	1238.968606	15.919898
28.960411	1230.525712	15.924915
28.833735	1245.121924	15.929933
28.746806	1241.041177	15.934951
29.443043	1233.083308	15.939968
29.027821	1242.900221	15.944986
29.204844	1235.801517	15.950003
29.462800	1230.390270	15.955021
29.177957	1218.108491	15.960039
29.384199	1206.045701	15.965056
29.191860	1202.048003	15.970074
29.439526	1199.445857	15.975091
29.193981	1193.613425	15.980109
29.049636	1193.755884	15.985127
29.272797	1195.685098	15.990144
29.022156	1193.579841	15.995162
28.989587	1200.928950	16.000179
29.137066	1206.634848	16.005197
29.378793	1217.824672	16.010215
29.609868	1223.582392	16.015232
28.947233	1227.654598	16.020250
29.685261	1228.442695	16.025267
29.463773	1232.977897	16.030285
29.367993	1228.883708	16.035303
29.652420	1226.509528	16.040320
29.452751	1228.024978	16.045338
29.400529	1222.488158	16.050355
29.606441	1233.135660	16.055373
29.318310	1227.593612	16.060391
29.391974	1219.068810	16.065408
28.811896	1231.797695	16.070426
29.149007	1234.283018	16.075443
29.139225	1250.888505	16.080461
29.232220	1254.460266	16.085479
29.717117	1256.252085	16.090496
29.620830	1262.192335	16.095514
29.911833	1258.322795	16.100531
29.584508	1254.161596	16.105549
29.534322	1262.797332	16.110567
29.983196	1261.487570	16.115584
30.079761	1269.237836	16.120602
30.030881	1265.028500	16.125619
29.892882	1257.311296	16.130637
29.914273	1276.858580	16.135655
30.729154	1266.189953	16.140672
30.491144	1265.875201	16.145690
30.601249	1262.698151	16.150707
30.470520	1252.595238	16.155725
30.351829	1259.405547	16.160743
30.306972	1252.296447	16.165760
29.938675	1256.364264	16.170778
30.460751	1251.041990	16.175795
30.375318	1250.764471	16.180813
30.321650	1249.494016	16.185831
30.528306	1252.465923	16.190848
30.447692	1257.668379	16.195866
30.441951	1253.449682	16.200883
30.213746	1252.022914	16.205901
30.308688	1254.402109	16.210919
30.605794	1250.874469	16.215936
30.618687	1259.808865	16.220954
30.694382	1250.444646	16.225971
30.419958	1252.094579	16.230989
29.941223	1254.916651	16.236007
30.121120	1255.927617	16.241024
30.252550	1254.153731	16.246042
30.124285	1248.148007	16.251059
30.392843	1252.081828	16.256077
30.633973	1261.781496	16.261095
30.645496	1265.440463	16.266112
30.269022	1277.422208	16.271130
30.604016	1265.223508	16.276147
30.437002	1275.742835	16.281165
30.354870	1278.292957	16.286183
30.784083	1264.112179	16.291200
30.862205	1273.122808	16.296218
30.819811	1297.115705	16.301235
30.928960	1297.784047	16.306253
30.958153	1288.730956	16.311271
31.330124	1282.667015	16.316288
31.178485	1293.058508	16.321306
31.044353	1281.079611	16.326323
31.090287	1285.970590	16.331341
30.847892	1289.582144	16.336359
31.288833	1287.514222	16.341376
31.166329	1292.272256	16.346394
31.115902	1284.813277	16.351411
31.445211	1281.869926	16.356429
31.681024	1279.335160	16.361447
32.184153	1257.028385	16.366464
31.911552	1249.679568	16.371482
31.724643	1242.724761	16.376499
31.832606	1233.685757	16.381517
31.971162	1235.818475	16.386535
32.212425	1229.500562	16.391552
31.689865	1219.302630	16.396570
31.651656	1213.624423	16.401587
31.613971	1211.307440	16.406605
31.403452	1218.072839	16.411623
31.753654	1198.335106	16.416640
31.461037	1215.243795	16.421658
31.614851	1208.957813	16.426675
31.629942	1211.206192	16.431693
31.713582	1215.211475	16.436711
31.805663	1212.340308	16.441728
31.551438	1214.062371	16.446746
31.661092	1216.043335	16.451763
31.783775	1214.422935	16.456781
31.830030	1220.904527	16.461799
31.930179	1215.556171	16.466816
31.823477	1218.900722	16.471834
31.939584	1225.166386	16.476851
31.655237	1227.466893	16.481869
31.461509	1232.600144	16.486887
32.273027	1239.183631	16.491904
31.989138	1237.273455	16.496922
31.778461	1244.918105	16.501939
31.946364	1239.176988	16.506957
32.028137	1242.495924	16.511975
32.489133	1237.849934	16.516992
32.436266	1245.273415	16.522010
32.558579	1241.816693	16.527027
32.691625	1241.593456	16.532045
32.444797	1232.264858	16.537063
32.382316	1217.182509	16.542080
32.393574	1223.800036	16.547098
32.118729	1225.924095	16.552115
32.018310	1220.546734	16.557133
31.955231	1230.340669	16.562151
32.431006	1230.305936	16.567168
32.570404	1244.265927	16.572186
32.099214	1249.229806	16.577203
32.362131	1247.653082	16.582221
32.300172	1250.796251	16.587239
32.249733	1239.360172	16.592256
31.992840	1251.674182	16.597274
32.366525	1254.202455	16.602291
32.441439	1270.790293	16.607309
32.409912	1281.513186	16.612327
32.471354	1278.725614	16.617344
32.522635	1277.113118	16.622362
32.467820	1284.771226	16.627379
32.255902	1277.037549	16.632397
32.753714	1283.083054	16.637415
32.530426	1285.545951	16.642432
32.931878	1292.822658	16.647450
32.946582	1304.924382	16.652467
32.822012	1298.907768	16.657485
33.012974	1311.121810	16.662503
33.138124	1311.197591	16.667520
33.190741	1304.685198	16.672538
33.245724	1306.891709	16.677555
33.634600	1310.854527	16.682573
32.865402	1302.510018	16.687591
33.038626	1303.568593	16.692608
33.228243	1304.238495	16.697626
33.006905	1305.663957	16.702643
33.467797	1305.332931	16.707661
33.118566	1311.022445	16.712679
33.449512	1310.399495	16.717696
33.575187	1306.164945	16.722714
33.248151	1315.936073	16.727731
33.173882	1303.213755	16.732749
32.937412	1316.061766	16.737767
33.059612	1310.220575	16.742784
33.306090	1311.663478	16.747802
32.975890	1313.446220	16.752819
33.699790	1322.884399	16.757837
34.135960	1316.230644	16.762855
34.028612	1307.290330	16.767872
33.985482	1295.644670	16.772890
34.014445	1299.085280	16.777907
33.965578	1284.148578	16.782925
33.763966	1287.801962	16.787943
33.901185	1290.843661	16.792960
33.850778	1289.425386	16.797978
33.635065	1294.789613	16.802995
34.058981	1290.404319	16.808013
33.662308	1293.192247	16.813031
34.011215	1293.000904	16.818048
34.267054	1285.854803	16.823066
33.777102	1290.795531	16.828083
34.401780	1285.988775	16.833101
34.039593	1286.379233	16.838119
33.955788	1288.265804	16.843136
34.100721	1284.095287	16.848154
33.955792	1287.511767	16.853171
34.166746	1285.097021	16.858189
33.956655	1285.298001	16.863207
33.754020	1286.027279	16.868224
34.152787	1290.504585	16.873242
33.967624	1299.595413	16.878259
34.291507	1311.113770	16.883277
34.505765	1321.428375	16.888295
34.638661	1320.476749	16.893312
34.442734	1315.354727	16.898330
34.434223	1330.513097	16.903347
34.312464	1323.272648	16.908365
34.460733	1327.948833	16.913383
34.437272	1330.605451	16.918400
34.502523	1314.697884	16.923418
34.273165	1322.199304	16.928435
34.532049	1320.027539	16.933453
34.461496	1317.653965	16.938471
34.273447	1322.807534	16.943488
34.654746	1317.641277	16.948506
34.233800	1329.879923	16.953523
34.720283	1334.404020	16.958541
34.861694	1344.997297	16.963559
35.041863	1357.109673	16.968576
35.216672	1347.141733	16.973594
34.809729	1357.016752	16.978611
34.971980	1346.581236	16.983629
34.889883	1349.714490	16.988647
34.937548	1349.426354	16.993664
35.163256	1353.580954	16.998682
35.188634	1358.459731	17.003699
35.133473	1349.701802	17.008717
35.101100	1352.598557	17.013735
34.973713	1354.043746	17.018752
34.905046	1342.580793	17.023770
34.816676	1345.950577	17.028787
35.000640	1347.358134	17.033805
34.919142	1352.778905	17.038823
35.362185	1365.599439	17.043840
35.273749	1371.145433	17.048858
35.060207	1381.846841	17.053875
35.483611	1379.839793	17.058893
35.246234	1385.428653	17.063911
35.415872	1384.893599	17.068928
35.791832	1372.001505	17.073946
35.730555	1383.376482	17.078963
35.868576	1378.015278	17.083981
35.768981	1381.613788	17.088999
35.753284	1380.815205	17.094016
35.928840	1373.871823	17.099034
35.770492	1388.830327	17.104051
35.705798	1372.625264	17.109069
36.358829	1379.999050	17.114087
35.636563	1359.490959	17.119104
35.809725	1359.530553	17.124122
35.886353	1365.535300	17.129139
35.592571	1375.889008	17.134157
35.846865	1379.875312	17.139175
35.673070	1376.692578	17.144192
36.153992	1380.700270	17.149210
35.800743	1393.907375	17.154227
36.114479	1379.419487	17.159245
36.201101	1372.518522	17.164263
36.015394	1365.811902	17.169280
35.910948	1370.368026	17.174298
35.848777	1372.710785	17.179315
36.327521	1381.457890	17.184333
36.124628	1382.253758	17.189351
36.113097	1382.332105	17.194368
36.188655	1387.402701	17.199386
35.944268	1413.356580	17.204403
36.369063	1405.891272	17.209421
36.394909	1408.462670	17.214439
36.153337	1412.734018	17.219456
36.631001	1405.221453	17.224474
36.645638	1411.992038	17.229491
36.933176	1406.360283	17.234509
36.612905	1409.386338	17.239527
36.436977	1423.017048	17.244544
36.779345	1415.963544	17.249562
36.290435	1417.875486	17.254579
36.757563	1408.429494	17.259597
36.905807	1411.230326	17.264615
36.575707	1409.814319	17.269632
36.730640	1407.274501	17.274650
36.837293	1407.255806	17.279667
36.949623	1409.502898	17.284685
37.045952	1416.177975	17.289703
37.232635	1416.667265	17.294720
37.086982	1404.878455	17.299738
36.769309	1410.999645	17.304755
36.839370	1419.604221	17.309773
37.314798	1434.178489	17.314791
37.090250	1442.694992	17.319808
37.190569	1430.862415	17.324826
37.190388	1439.471958	17.329843
37.181572	1439.431324	17.334861
37.262559	1432.121021	17.339879
37.281624	1435.859057	17.344896
37.430233	1425.482920	17.349914
37.198094	1436.393086	17.354931
37.182540	1448.481603	17.359949
37.369974	1431.212676	17.364967
37.077788	1439.783297	17.369984
37.586314	1436.009504	17.375002
37.604556	1439.715002	17.380019
37.748962	1429.156100	17.385037
37.748764	1427.085833	17.390055
37.615173	1425.304211	17.395072
37.761238	1430.607639	17.400090
37.549896	1437.970972	17.405107
37.373197	1435.670702	17.410125
37.458996	1429.697505	17.415143
37.491673	1455.316915	17.420160
37.724712	1459.074970	17.425178
37.755693	1459.138548	17.430195
37.754083	1457.768984	17.435213
37.948221	1462.143221	17.440231
37.773031	1468.580591	17.445248
38.390786	1453.992868	17.450266
37.937517	1455.109648	17.455283
38.292574	1454.400661	17.460301
38.480795	1450.482942	17.465319
37.962198	1457.100849	17.470336
38.097986	1449.053116	17.475354
37.969361	1452.691268	17.480371
38.333658	1457.797431	17.485389
38.322224	1455.012872	17.490407
38.180258	1464.802761	17.495424
38.545975	1471.752574	17.500442
38.713471	1487.252612	17.505459
38.518143	1472.586928	17.510477
38.390481	1456.548889	17.515495
38.389373	1475.511243	17.520512
38.686127	1478.770927	17.525530
38.770003	1492.012237	17.530547
38.687339	1492.326426	17.535565
39.021342	1485.328661	17.540583
38.966723	1486.615308	17.545600
39.149395	1467.297339	17.550618
38.937277	1463.048607	17.555635
38.684279	1460.977185	17.560653
38.896409	1449.598307	17.565671
38.884424	1458.355174	17.570688
39.099922	1447.465929	17.575706
38.909833	1452.347027	17.580723
39.222277	1448.133573	17.585741
39.064371	1447.716885	17.590759
38.999932	1453.973827	17.595776
38.846558	1450.686779	17.600794
38.631806	1476.796329	17.605811
38.657226	1487.045379	17.610829
39.021650	1473.264536	17.615847
38.722878	1486.697049	17.620864
39.146453	1482.687391	17.625882
38.956923	1488.319270	17.630899
39.183395	1507.623392	17.635917
39.371133	1515.304994	17.640935
39.460134	1509.117416	17.645952
39.750219	1506.504405	17.650970
39.752836	1500.966746	17.655987
39.766680	1508.940391	17.661005
40.288413	1492.198002	17.666023
39.620000	1478.116625	17.671040
39.912196	1479.975372	17.676058
40.048586	1479.967723	17.681075
39.940295	1474.366009	17.686093
39.991489	1463.939612	17.691111
39.808631	1476.239924	17.696128
39.773779	1461.637692	17.701146
39.893342	1467.628817	17.706163
39.680312	1467.798410	17.711181
39.886601	1466.868841	17.716199
39.718116	1473.211746	17.721216
39.781593	1465.587074	17.726234
40.065832	1481.420670	17.731251
40.274621	1492.204486	17.736269
40.212556	1490.229472	17.741287
40.003702	1492.539910	17.746304
40.288247	1489.373463	17.751322
40.517993	1505.476690	17.756339
40.082278	1495.647191	17.761357
40.424498	1491.865280	17.766375
40.563776	1498.028252	17.771392
40.315964	1495.285787	17.776410
40.667185	1497.521071	17.781427
40.604047	1499.410424	17.786445
40.415906	1498.300813	17.791463
40.606481	1510.156379	17.796480
40.540439	1502.701155	17.801498
40.474090	1500.506772	17.806515
40.419024	1501.989974	17.811533
40.489760	1503.022429	17.816551
40.612286	1510.598268	17.821568
40.559563	1499.262007	17.826586
40.650024	1501.569954	17.831603
40.426490	1499.275342	17.836621
40.526113	1496.329594	17.841639
40.571118	1519.570370	17.846656
40.971292	1534.245834	17.851674
41.165519	1534.175901	17.856691
40.673076	1542.541516	17.861709
40.936626	1539.387714	17.866727
41.007433	1535.199128	17.871744
40.947212	1540.818306	17.876762
40.969623	1536.130482	17.881779
40.900534	1537.286923	17.886797
40.978678	1535.245734	17.891815
41.164018	1543.848333	17.896832
41.386886	1562.225482	17.901850
41.176819	1562.216990	17.906867
41.361473	1565.147055	17.911885
41.656371	1566.112339	17.916903
42.200001	1562.543151	17.921920
41.833777	1549.369847	17.926938
41.811245	1531.919461	17.931955
41.460983	1529.398513	17.936973
41.866549	1523.762231	17.941991
41.606105	1526.574485	17.947008
41.717964	1523.307309	17.952026
41.853249	1515.547060	17.957043
41.760876	1533.764422	17.962061
41.776783	1522.953049	17.967079
41.812156	1530.586364	17.972096
41.625078	1548.798324	17.977114
41.735163	1560.522831	17.982131
41.795110	1561.603601	17.987149
42.030239	1555.492537	17.992167
42.199798	1560.521479	17.997184
42.027841	1559.657148	18.002202
42.377756	1553.809506	18.007219
42.064170	1557.398677	18.012237
42.413026	1553.634513	18.017255
42.331256	1563.297595	18.022272
42.520841	1558.599215	18.027290
42.658381	1551.259080	18.032307
42.050468	1565.504192	18.037325
42.404688	1551.855360	18.042343
42.143813	1561.871229	18.047360
42.057184	1562.438095	18.052378
42.011158	1563.646101	18.057395
42.338625	1575.670788	18.062413
42.689192	1580.979761	18.067431
42.768189	1579.725121	18.072448
42.646469	1584.081884	18.077466
42.646496	1592.694625	18.082483
42.664710	1591.170847	18.087501
42.560101	1576.313509	18.092519
42.636860	1588.196522	18.097536
42.744963	1586.946735	18.102554
43.027639	1581.025563	18.107571
42.619615	1582.602754	18.112589
42.875321	1587.823258	18.117607
42.835539	1588.998303	18.122624
42.799473	1598.765787	18.127642
43.420318	1600.777281	18.132659
43.111339	1619.435467	18.137677
43.296393	1614.891801	18.142695
43.753129	1607.796948	18.147712
43.564848	1617.121985	18.152730
43.616179	1590.669281	18.157747
43.622917	1589.275438	18.162765
43.738109	1580.001505	18.167783
43.440424	1573.237214	18.172800
43.495717	1573.860465	18.177818
43.396076	1583.113585	18.182835
43.345320	1584.458246	18.187853
43.932896	1582.547451	18.192871
43.877623	1578.749407	18.197888
43.945969	1588.679319	18.202906
43.565270	1575.377357	18.207923
43.355408	1587.518982	18.212941
43.482267	1587.574392	18.217959
43.708011	1602.876742	18.222976
43.675044	1603.793504	18.227994
43.698734	1600.045310	18.233011
43.466244	1610.357165	18.238029
43.444165	1611.715811	18.243047
43.737006	1609.730333	18.248064
43.584778	1632.504643	18.253082
44.302325	1629.106039	18.258099
44.181634	1642.768813	18.263117
44.548155	1631.740936	18.268135
44.582004	1645.999729	18.273152
44.569229	1637.575355	18.278170
44.704037	1629.264282	18.283187
44.634266	1617.709179	18.288205
44.602306	1607.832042	18.293223
44.338933	1595.099383	18.298240
44.385615	1612.764985	18.303258
44.840056	1613.946253	18.308275
44.901034	1617.142442	18.313293
45.168826	1606.453199	18.318311
44.762275	1593.007212	18.323328
44.664198	1597.493011	18.328346
44.927872	1590.804141	18.333363
44.968255	1595.482760	18.338381
44.979201	1585.475432	18.343399
44.895384	1582.418190	18.348416
44.755502	1594.315514	18.353434
44.903256	1595.311539	18.358451
44.598896	1594.663235	18.363469
45.145493	1612.820751	18.368487
45.203460	1621.058966	18.373504
45.401859	1632.891628	18.378522
45.437886	1630.906866	18.383539
45.377481	1633.764773	18.388557
45.108498	1624.897664	18.393575
45.195797	1620.173096	18.398592
44.771606	1628.980649	18.403610
44.971085	1628.469609	18.408627
45.063142	1627.244225	18.413645
44.843277	1632.167103	18.418663
45.055281	1641.123492	18.423680
45.275936	1652.634994	18.428698
45.125952	1648.675592	18.433715
45.227256	1653.894241	18.438733
45.180828	1658.108179	18.443751
45.582302	1655.649689	18.448768
45.666551	1681.115335	18.453786
46.035581	1677.159079	18.458803
45.974477	1686.829324	18.463821
45.916915	1682.503634	18.468839
45.835978	1680.834622	18.473856
45.842867	1688.639847	18.478874
46.083367	1683.507848	18.483891
46.139711	1690.689169	18.488909
45.858562	1688.427243	18.493927
46.094884	1690.744073	18.498944
45.878885	1689.167516	18.503962
46.389676	1684.878651	18.508979
46.220031	1689.772461	18.513997
46.311902	1697.459565	18.519015
46.336366	1682.310673	18.524032
46.138924	1684.098650	18.529050
46.464760	1683.265516	18.534067
46.411446	1680.813331	18.539085
46.209794	1688.978363	18.544103
46.834780	1693.204773	18.549120
46.768761	1702.810116	18.554138
47.333882	1698.184728	18.559155
47.403943	1691.775889	18.564173
46.995658	1674.235950	18.569191
47.002235	1672.127870	18.574208
46.612611	1673.297145	18.579226
46.880192	1684.025733	18.584243
46.826382	1681.366129	18.589261
46.759945	1679.139448	18.594279
47.045281	1669.678400	18.599296
46.766872	1677.805005	18.604314
47.062654	1689.590302	18.609331
47.138681	1702.427183	18.614349
46.937504	1703.639751	18.619367
47.445695	1700.895996	18.624384
47.323036	1705.071830	18.629402
47.303933	1701.921176	18.634419
47.416045	1707.065145	18.639437
47.053007	1703.588766	18.644455
47.489852	1700.120543	18.649472
47.332424	1700.086488	18.654490
47.204113	1703.397440	18.659507
47.386184	1698.584939	18.664525
47.481170	1705.227690	18.669543
47.627159	1710.181579	18.674560
47.654739	1735.857053	18.679578
47.789823	1731.604239	18.684595
47.926944	1736.090309	18.689613
47.732177	1740.054866	18.694631
48.205392	1731.341191	18.699648
47.763940	1736.245785	18.704666
47.996260	1729.450014	18.709683
47.902869	1733.065259	18.714701
48.058636	1733.910689	18.719719
48.331886	1732.058886	18.724736
47.946712	1733.992454	18.729754
48.132087	1734.563091	18.734771
48.029783	1731.547182	18.739789
48.150376	1738.863984	18.744807
48.271673	1730.732754	18.749824
48.008700	1733.685258	18.754842
48.251690	1745.879697	18.759859
48.368412	1756.344794	18.764877
48.263201	1759.172606	18.769895
48.472382	1760.748734	18.774912
48.605846	1757.195094	18.779930
48.619850	1753.739898	18.784947
48.674238	1758.293709	18.789965
48.574957	1766.199074	18.794983
48.844012	1755.522901	18.800000
48.381508	1760.840610	18.805018
48.933083	1766.520353	18.810035
49.047097	1781.568379	18.815053
49.341950	1779.746729	18.820071
49.468561	1766.440708	18.825088
49.194149	1752.204512	18.830106
49.347711	1746.805475	18.835123
49.633461	1746.630075	18.840141
48.947119	1744.315548	18.845159
49.261639	1745.134550	18.850176
49.393954	1746.517924	18.855194
49.134675	1744.990125	18.860211
49.473287	1750.538244	18.865229
49.382366	1771.664646	18.870247
49.796559	1770.404891	18.875264
49.508341	1777.885906	18.880282
49.805711	1778.483807	18.885299
49.837699	1779.742635	18.890317
49.296346	1785.628663	18.895335
49.462715	1771.530292	18.900352
49.483997	1773.349685	18.905370
49.733000	1778.993895	18.910387
49.854415	1773.401517	18.915405
49.815753	1775.115031	18.920423
49.776069	1772.464015	18.925440
50.039337	1773.433948	18.930458
50.010564	1768.314619	18.935475
50.141027	1768.348936	18.940493
49.946718	1776.409198	18.945511
50.327964	1784.481432	18.950528
50.329601	1794.331168	18.955546
50.224006	1798.218632	18.960563
50.542421	1793.140571	18.965581
50.512752	1801.842781	18.970599
50.848479	1794.027554	18.975616
50.749499	1794.602058	18.980634
50.855497	1776.094590	18.985651
50.999352	1760.633386	18.990669
50.538779	1767.172568	18.995687
50.920176	1769.103076	19.000704
50.916870	1762.951304	19.005722
50.873376	1765.274776	19.010739
51.090471	1758.699739	19.015757
50.943858	1759.213896	19.020775
51.023153	1753.996900	19.025792
51.033805	1756.900528	19.030810
50.847698	1757.486424	19.035827
51.169219	1757.611229	19.040845
50.779505	1762.738878	19.045863
51.153561	1764.287921	19.050880
51.305761	1757.119213	19.055898
50.931681	1766.523836	19.060915
51.417142	1763.560713	19.065933
51.402377	1783.719235	19.070951
51.447125	1794.890089	19.075968
51.383808	1797.203576	19.080986
51.213183	1797.823045	19.086003
51.765118	1792.264342	19.091021
51.343036	1794.494438	19.096039
51.724831	1803.656879	19.101056
51.702031	1799.235815	19.106074
51.170761	1795.748489	19.111091
51.126505	1792.833259	19.116109
50.960760	1806.034944	19.121127
51.498884	1813.889722	19.126144
51.048512	1813.440084	19.131162
51.145519	1830.927204	19.136179
51.949049	1839.848837	19.141197
51.471063	1854.547191	19.146215
51.903100	1849.272444	19.151232
51.965954	1855.223041	19.156250
52.109522	1853.463151	19.161267
52.296352	1857.747797	19.166285
52.153860	1882.859682	19.171303
52.772284	1886.354500	19.176320
52.708351	1878.732177	19.181338
52.613505	1867.291045	19.186355
52.824717	1852.372998	19.191373
52.431283	1849.388079	19.196391
52.838672	1859.886099	19.201408
52.839424	1850.622571	19.206426
52.657211	1847.703421	19.211443
53.121507	1848.369174	19.216461
52.894857	1853.328328	19.221479
53.083439	1835.942208	19.226496
53.162039	1834.497828	19.231514
53.004521	1845.938072	19.236531
53.478522	1835.735827	19.241549
53.327831	1840.987898	19.246567
53.456618	1832.538755	19.251584
53.595712	1832.126655	19.256602
53.571674	1832.774937	19.261619
53.481985	1825.344087	19.266637
53.446644	1838.166704	19.271655
53.306265	1832.107312	19.276672
53.023877	1831.705655	19.281690
53.151218	1830.721088	19.286707
53.411861	1824.330314	19.291725
53.352387	1824.974433	19.296743
53.304846	1838.702012	19.301760
53.394336	1847.284593	19.306778
53.568830	1860.195679	19.311795
54.033287	1859.502964	19.316813
53.562291	1861.685148	19.321831
54.050155	1859.726843	19.326848
53.937876	1858.716025	19.331866
53.910026	1869.615485	19.336883
54.211484	1858.277697	19.341901
54.088635	1853.783995	19.346919
53.684016	1860.549873	19.351936
53.642837	1863.679364	19.356954
53.551329	1865.875631	19.361971
54.239152	1866.985802	19.366989
54.469531	1884.558005	19.372007
54.298437	1883.326136	19.377024
54.344325	1878.707817	19.382042
54.304623	1894.620603	19.387059
55.109896	1876.313250	19.392077
54.747991	1878.605490	19.397095
54.874117	1878.984690	19.402112
54.796458	1884.967263	19.407130
54.854269	1891.369584	19.412147
54.821391	1880.162338	19.417165
54.935877	1879.960782	19.422183
54.965722	1891.978465	19.427200
55.347777	1873.910624	19.432218
54.817582	1879.166346	19.437235
54.921177	1877.405432	19.442253
54.881433	1872.606100	19.447271
55.039831	1875.069013	19.452288
55.064038	1871.178521	19.457306
54.802906	1874.363443	19.462323
55.015832	1881.784183	19.467341
55.088547	1905.077482	19.472359
54.831553	1905.987782	19.477376
55.140136	1899.997867	19.482394
55.141680	1916.542270	19.487411
55.628985	1914.638391	19.492429
55.451699	1922.626116	19.497447
55.572854	1934.213948	19.502464
55.547409	1939.872195	19.507482
55.884098	1937.644483	19.512499
56.548322	1923.863823	19.517517
57.304293	1908.036078	19.522535
57.569652	1893.071302	19.527552
57.658173	1866.529067	19.532570
57.114409	1856.853312	19.537587
57.356261	1832.116578	19.542605
56.792913	1814.241208	19.547623
56.587402	1809.696721	19.552640
56.794341	1801.101503	19.557658
56.576093	1805.308320	19.562675
56.472380	1796.431283	19.567693
56.601793	1796.305525	19.572711
56.647070	1806.517518	19.577728
56.726921	1797.425915	19.582746
56.286480	1801.885025	19.587763
56.575645	1808.700066	19.592781
56.571166	1802.087399	19.597799
56.150261	1795.964684	19.602816
56.383730	1793.037278	19.607834
56.420820	1793.119891	19.612851
56.705567	1813.660620	19.617869
56.663888	1830.970706	19.622887
56.663266	1836.254141	19.627904
56.975753	1830.265945	19.632922
56.624876	1837.258850	19.637939
56.793833	1837.149543	19.642957
57.112538	1841.078462	19.647975
57.060829	1858.403291	19.652992
57.096010	1870.328693	19.658010
56.848988	1869.868995	19.663027
57.254332	1865.104002	19.668045
56.900280	1872.431367	19.673063
56.759607	1873.845806	19.678080
57.007012	1893.913847	19.683098
56.995317	1898.873568	19.688115
57.389548	1907.111378	19.693133
57.402506	1912.914626	19.698151
57.829980	1924.963388	19.703168
57.827665	1931.053157	19.708186
57.849526	1938.548812	19.713203
58.062343	1941.985607	19.718221
58.401130	1934.668277	19.723239
58.149738	1936.672646	19.728256
58.226246	1935.523536	19.733274
57.896785	1943.144789	19.738291
57.987774	1947.542360	19.743309
58.215771	1941.244549	19.748327
58.360980	1939.242605	19.753344
58.329230	1933.676428	19.758362
57.898365	1953.025287	19.763379
58.284774	1965.127584	19.768397
58.589962	1970.364147	19.773415
58.455032	1976.500294	19.778432
58.991984	1966.989235	19.783450
58.428328	1970.825729	19.788467
58.603142	1969.676301	19.793485
58.833286	1966.677769	19.798503
58.739132	1971.760720	19.803520
59.061879	1987.950090	19.808538
58.925173	2000.292514	19.813555
59.227982	2002.103043	19.818573
59.427364	1998.249819	19.823591
58.794953	1994.068272	19.828608
59.382554	1990.922220	19.833626
59.154332	1997.132251	19.838643
59.023532	1996.689637	19.843661
58.885184	1999.692881	19.848679
58.982655	2001.142891	19.853696
59.214854	2014.049724	19.858714
59.088828	2019.638223	19.863731
59.584027	2022.412365	19.868749
59.797038	2019.964868	19.873767
59.742143	2021.818219	19.878784
59.873613	2012.028571	19.883802
59.961758	2016.581789	19.888819
59.796078	2012.252887	19.893837
59.944999	2007.186884	19.898855
59.648977	2016.078205	19.903872
59.890846	2016.731700	19.908890
59.829714	2038.743242	19.913907
60.216325	2040.318511	19.918925
59.816810	2043.643743	19.923943
60.204095	2055.544358	19.928960
60.300252	2043.963248	19.933978
60.194320	2056.182313	19.938995
60.465523	2051.866700	19.944013
60.315024	2055.379983	19.949031
60.288627	2071.269011	19.954048
60.323593	2074.572130	19.959066
60.475284	2084.487280	19.964083
60.715517	2074.196202	19.969101
60.909964	2072.869754	19.974119
61.211033	2076.363112	19.979136
60.925796	2069.549612	19.984154
61.189756	2071.096299	19.989171
60.573148	2072.365941	19.994189
60.833007	2081.563234	19.999207
60.835041	2100.242695	20.004224
61.245068	2092.393321	20.009242
61.066032	2105.580211	20.014259
61.210956	2103.215644	20.019277
61.334443	2103.285810	20.024295
61.478517	2100.931627	20.029312
61.569221	2106.082943	20.034330
62.072109	2112.399992	20.039347
61.836178	2110.787432	20.044365
62.121789	2103.664208	20.049383
61.773234	2099.929707	20.054400
61.955793	2101.274180	20.059418
61.982230	2096.244505	20.064435
62.031940	2100.700385	20.069453
62.114385	2096.153304	20.074471
61.856246	2110.127886	20.079488
62.233012	2119.275626	20.084506
62.196636	2122.794953	20.089523
62.152625	2120.302910	20.094541
62.359029	2119.880051	20.099559
62.457192	2124.759189	20.104576
62.420921	2113.415724	20.109594
62.528971	2118.977515	20.114611
62.613142	2119.167036	20.119629
62.846535	2106.459044	20.124647
62.857781	2108.463688	20.129664
62.942541	2104.724198	20.134682
62.828358	2107.547310	20.139699
63.174164	2101.917132	20.144717
63.139230	2099.574738	20.149735
63.007764	2109.566407	20.154752
62.982600	2101.851489	20.159770
63.209846	2108.368572	20.164787
63.073990	2106.312022	20.169805
63.551870	2103.220198	20.174823
63.323459	2107.150451	20.179840
63.160120	2107.899015	20.184858
62.939287	2103.545680	20.189875
63.099878	2112.605263	20.194893
63.032841	2111.438619	20.199911
62.964664	2129.100870	20.204928
63.333623	2134.258042	20.209946
63.260642	2141.618064	20.214963
63.354265	2140.431748	20.219981
63.601012	2153.519693	20.224999
63.545538	2170.314332	20.230016
63.738919	2173.002825	20.235034
63.626862	2180.595582	20.240051
63.758894	2179.389291	20.245069
64.718185	2148.180090	20.250087
64.951333	2152.308429	20.255104
65.361274	2140.289144	20.260122
65.496406	2133.427172	20.265139
64.954204	2122.625623	20.270157
65.206155	2109.772693	20.275175
64.788286	2109.245020	20.280192
64.999224	2103.396196	20.285210
64.727411	2106.759005	20.290227
64.862108	2107.427335	20.295245
65.165325	2110.714397	20.300263
65.491996	2109.630670	20.305280
65.454273	2082.745881	20.310298
65.286972	2077.669100	20.315315
65.281252	2078.849367	20.320333
65.298440	2071.371726	20.325351
65.170972	2069.550784	20.330368
65.146849	2066.011492	20.335386
65.252263	2072.532122	20.340403
64.686655	2066.030114	20.345421
65.623001	2084.616315	20.350439
65.122782	2090.912391	20.355456
65.466579	2094.405122	20.360474
65.213816	2100.548525	20.365491
65.057441	2113.117276	20.370509
65.151845	2112.667155	20.375527
65.043150	2118.680339	20.380544
65.224487	2126.996110	20.385562
65.719668	2136.375565	20.390579
65.013272	2136.378528	20.395597
65.516961	2136.704031	20.400615
65.437379	2163.173495	20.405632
65.430623	2165.125319	20.410650
65.612826	2178.042434	20.415667
65.474909	2181.822525	20.420685
66.035726	2193.881712	20.425703
66.310834	2199.325902	20.430720
66.529854	2197.855053	20.435738
66.803223	2201.779630	20.440755
66.621787	2201.495713	20.445773
67.171079	2203.692420	20.450791
67.006965	2202.253392	20.455808
66.976290	2204.006929	20.460826
67.193306	2202.376556	20.465843
66.744109	2204.398725	20.470861
66.873478	2205.471970	20.475879
66.836898	2200.668846	20.480896
66.509690	2206.769139	20.485914
66.744701	2202.326600	20.490931
66.578782	2210.496407	20.495949
67.097213	2218.057479	20.500967
66.913382	2232.429729	20.505984
67.257846	2231.720166	20.511002
67.420260	2223.321750	20.516019
67.293283	2232.259812	20.521037
67.679870	2231.819447	20.526055
67.837843	2240.217249	20.531072
67.474142	2237.039725	20.536090
67.973124	2246.744628	20.541107
67.924020	2270.347195	20.546125
68.119192	2268.251985	20.551143
68.036037	2268.330016	20.556160
67.905099	2267.766532	20.561178
68.246592	2263.252168	20.566195
68.139295	2264.747940	20.571213
67.959573	2269.855108	20.576231
67.867035	2270.563977	20.581248
67.908679	2261.992515	20.586266
68.093519	2269.799810	20.591283
67.788205	2294.187396	20.596301
68.155782	2301.454638	20.601319
68.564014	2298.267613	20.606336
68.773999	2298.183559	20.611354
69.175784	2287.027113	20.616371
69.087669	2293.341607	20.621389
68.713148	2283.218394	20.626407
68.742088	2287.182536	20.631424
68.575164	2290.639229	20.636442
69.057383	2299.216943	20.641459
69.055824	2311.193080	20.646477
68.956439	2309.810672	20.651495
69.115790	2310.368468	20.656512
69.227399	2313.900268	20.661530
69.529646	2306.362225	20.666547
69.207922	2317.412001	20.671565
69.604154	2313.391467	20.676583
69.657975	2307.467126	20.681600
69.659959	2312.798313	20.686618
69.827122	2300.084194	20.691635
69.572671	2304.139451	20.696653
69.604913	2310.772741	20.701671
70.007687	2329.127039	20.706688
69.680548	2336.871724	20.711706
70.078700	2333.301321	20.716723
70.488282	2337.346698	20.721741
70.701030	2329.403448	20.726759
70.965502	2331.955352	20.731776
70.876045	2329.272610	20.736794
71.200780	2304.766630	20.741811
71.104294	2287.481253	20.746829
70.969350	2270.129249	20.751847
71.007301	2269.232827	20.756864
71.299205	2280.885359	20.761882
71.039723	2274.661146	20.766899
70.975207	2279.578460	20.771917
70.810593	2271.699935	20.776935
70.991843	2273.124189	20.781952
71.241250	2279.643057	20.786970
71.454751	2278.232999	20.791987
71.123038	2281.236765	20.797005
71.227335	2276.989081	20.802023
71.322182	2278.269856	20.807040
71.037019	2279.629168	20.812058
71.519382	2271.217613	20.817075
71.506864	2281.898557	20.822093
71.259600	2281.135297	20.827111
71.339280	2279.024446	20.832128
71.134116	2281.919102	20.837146
71.517557	2304.478123	20.842163
71.418442	2312.432562	20.847181
71.758931	2311.528371	20.852199
72.174106	2312.379370	20.857216
71.918082	2312.739045	20.862234
71.886227	2302.054632	20.867251
71.760734	2332.714009	20.872269
71.740111	2347.045782	20.877287
72.293995	2340.552156	20.882304
72.022087	2350.753911	20.887322
72.102787	2357.966408	20.892339
72.255565	2369.768076	20.897357
72.547690	2379.172252	20.902375
72.430849	2384.256075	20.907392
72.125515	2388.842996	20.912410
72.685212	2382.016020	20.917427
72.406356	2388.360102	20.922445
72.519498	2389.091992	20.927463
72.429583	2397.331557	20.932480
72.720294	2407.759780	20.937498
72.797108	2407.435522	20.942515
72.514044	2412.803012	20.947533
72.970041	2429.322809	20.952551
73.327556	2429.476497	20.957568
73.348835	2441.054265	20.962586
73.495210	2437.944395	20.967603
73.291030	2444.459980	20.972621
73.557930	2431.511297	20.977639
73.812489	2430.709248	20.982656
73.469594	2432.907740	20.987674
74.115799	2439.179091	20.992691
74.376532	2452.038867	20.997709
74.698851	2432.482741	21.002727
74.772951	2417.413227	21.007744
74.641110	2418.209956	21.012762
74.671059	2404.823887	21.017779
74.623920	2407.226831	21.022797
74.578941	2412.269992	21.027815
74.829477	2405.738568	21.032832
74.777981	2414.901627	21.037850
74.841893	2407.595766	21.042867
73.983534	2416.744375	21.047885
74.328223	2414.918049	21.052903
74.645753	2409.330411	21.057920
74.219127	2413.564057	21.062938
74.454406	2427.110966	21.067955
74.722128	2439.293045	21.072973
74.565107	2435.406707	21.077991
74.739618	2443.531660	21.083008
74.572437	2462.870589	21.088026
74.623545	2466.174174	21.093043
75.137824	2477.507579	21.098061
74.997243	2480.519567	21.103079
75.552310	2483.598150	21.108096
75.433325	2499.277856	21.113114
75.954203	2499.179092	21.118131
75.788496	2503.017576	21.123149
75.665405	2503.182783	21.128167
75.977912	2499.614425	21.133184
76.106349	2501.951844	21.138202
75.964193	2500.473584	21.143219
75.928355	2501.575961	21.148237
75.865430	2508.556414	21.153255
76.407947	2503.483021	21.158272
76.543699	2507.363542	21.163290
76.296298	2495.448019	21.168307
76.393351	2496.107070	21.173325
76.365465	2507.058563	21.178343
76.660895	2514.502868	21.183360
76.622918	2528.754303	21.188378
77.030834	2527.037618	21.193395
76.879421	2534.629417	21.198413
77.000232	2533.977087	21.203431
77.250774	2521.207542	21.208448
77.083601	2523.430261	21.213466
77.227869	2526.394997	21.218483
77.241228	2528.077231	21.223501
77.293058	2530.287605	21.228519
77.562272	2523.273321	21.233536
77.459804	2523.835848	21.238554
77.558856	2525.144273	21.243571
77.592584	2515.143078	21.248589
77.214939	2520.274020	21.253607
77.806456	2522.160334	21.258624
77.470279	2523.117319	21.263642
77.331730	2524.326297	21.268659
77.485762	2531.197900	21.273677
77.558555	2547.038509	21.278695
77.859564	2549.229794	21.283712
77.750870	2556.827669	21.288730
77.856049	2568.032817	21.293747
78.034574	2579.032452	21.298765
78.151098	2581.200242	21.303783
78.368057	2579.198123	21.308800
78.294319	2580.983498	21.313818
78.028903	2583.252207	21.318835
78.265694	2593.078669	21.323853
78.367368	2613.751459	21.328871
78.935481	2602.354427	21.333888
78.864662	2613.141671	21.338906
79.094502	2611.604351	21.343923
78.774221	2599.821738	21.348941
78.777381	2614.719068	21.353959
79.276341	2625.787445	21.358976
79.074112	2641.324056	21.363994
79.331462	2638.383344	21.369011
79.538187	2636.705865	21.374029
79.650665	2646.123675	21.379047
79.712147	2642.183287	21.384064
79.853165	2638.727779	21.389082
79.675876	2629.899896	21.394099
80.003123	2626.387262	21.399117
80.069482	2634.077232	21.404135
79.826190	2629.993000	21.409152
79.772401	2636.236380	21.414170
80.028430	2643.289794	21.419187
80.184967	2650.365780	21.424205
80.099763	2662.969233	21.429223
80.573242	2652.873659	21.434240
80.530818	2649.566940	21.439258
80.794377	2651.607939	21.444275
80.869723	2650.955523	21.449293
80.692545	2656.823932	21.454311
81.119089	2649.113996	21.459328
80.920191	2649.209508	21.464346
80.963211	2650.066838	21.469363
80.968088	2647.498601	21.474381
80.864215	2649.067063	21.479399
81.417078	2638.731076	21.484416
80.989146	2638.365765	21.489434
81.127243	2635.021801	21.494451
81.492529	2651.080135	21.499469
81.271831	2667.583103	21.504487
81.735797	2668.228873	21.509504
81.623443	2674.654780	21.514522
81.499321	2682.290013	21.519539
81.898041	2678.380005	21.524557
81.544381	2677.203390	21.529575
81.473105	2681.810122	21.534592
81.924042	2690.050047	21.539610
81.750815	2681.458490	21.544627
82.137947	2689.991294	21.549645
82.126985	2705.507778	21.554663
82.437271	2700.208735	21.559680
82.096138	2708.661640	21.564698
82.169905	2701.772927	21.569715
82.423019	2703.179387	21.574733
82.272384	2708.147827	21.579751
82.773610	2725.068131	21.584768
82.470823	2726.089494	21.589786
82.626294	2736.702570	21.594803
82.939613	2733.841238	21.599821
82.910983	2733.771315	21.604839
83.344115	2730.631915	21.609856
83.482866	2731.415347	21.614874
83.451455	2729.644014	21.619891
83.520373	2726.585957	21.624909
83.261789	2735.114504	21.629927
83.605785	2731.169763	21.634944
83.101095	2745.918807	21.639962
83.119346	2758.569967	21.644979
83.238730	2751.774217	21.649997
83.206375	2775.089579	21.655015
83.530512	2786.688135	21.660032
83.670173	2795.842271	21.665050
83.565181	2804.380751	21.670067
83.753896	2795.793235	21.675085
84.084147	2812.676005	21.680103
84.530195	2815.226786	21.685120
84.677791	2821.311282	21.690138
84.739539	2817.449560	21.695155
84.695466	2813.922576	21.700173
84.725223	2820.490353	21.705191
85.041619	2812.654313	21.710208
84.948003	2809.869032	21.715226
84.847674	2810.380011	21.720243
85.084603	2809.781792	21.725261
85.187660	2808.226812	21.730279
85.060806	2800.017077	21.735296
84.780507	2800.684129	21.740314
85.048670	2813.341317	21.745331
85.381544	2820.179236	21.750349
85.135623	2837.969625	21.755367
85.810845	2828.795439	21.760384
85.702912	2829.319536	21.765402
85.850384	2834.952791	21.770419
85.932842	2828.963491	21.775437
86.040228	2830.918668	21.780455
85.845072	2832.050744	21.785472
85.722508	2832.364710	21.790490
85.408813	2837.596622	21.795507
85.650968	2848.582388	21.800525
86.063551	2856.928995	21.805543
86.080794	2861.998649	21.810560
86.252681	2864.367263	21.815578
86.013835	2875.910404	21.820595
86.579575	2880.774985	21.825613
86.486017	2879.497846	21.830631
86.687835	2887.666389	21.835648
86.881534	2885.279169	21.840666
87.076885	2880.229735	21.845683
87.198202	2876.264855	21.850701
87.015597	2879.156539	21.855719
87.219889	2885.974002	21.860736
87.612200	2894.352458	21.865754
87.483148	2905.294795	21.870771
87.704996	2910.130135	21.875789
87.929640	2912.966970	21.880807
87.851730	2909.397725	21.885824
87.777718	2905.199343	21.890842
87.694040	2912.926985	21.895859
88.080881	2909.454476	21.900877
87.870008	2910.899548	21.905895
88.037727	2910.634513	21.910912
88.391914	2908.526922	21.915930
88.363246	2909.470587	21.920947
88.688232	2913.565271	21.925965
88.795649	2909.881560	21.930983
88.868607	2907.259081	21.936000
88.635814	2916.019571	21.941018
88.710526	2920.009890	21.946035
88.762757	2913.467363	21.951053
88.771321	2914.582633	21.956071
88.791144	2919.100574	21.961088
89.157603	2909.429562	21.966106
88.974001	2913.829590	21.971123
88.998094	2929.939616	21.976141
88.733002	2941.442414	21.981159
88.999086	2940.475341	21.986176
88.988899	2940.751142	21.991194
88.914317	2954.038181	21.996211
89.392356	2971.435262	22.001229
89.347689	2976.480126	22.006247
89.255425	2975.798152	22.011264
89.339397	2983.021401	22.016282
89.696083	2996.952007	22.021299
89.945487	2994.246497	22.026317
89.783856	3005.476435	22.031335
89.747904	3004.828121	22.036352
90.323593	3007.106267	22.041370
90.299148	3025.147144	22.046387
90.438270	3018.344746	22.051405
90.907565	3022.782510	22.056423
91.001929	3015.381365	22.061440
91.495224	3011.589736	22.066458
91.168162	3020.115212	22.071475
91.281538	2996.696573	22.076493
91.493046	2986.835500	22.081511
91.649045	2977.159575	22.086528
91.656091	2974.502706	22.091546
91.279630	2978.271116	22.096563
91.376304	2977.600854	22.101581
91.536957	2974.939702	22.106599
91.327122	2981.679357	22.111616
91.563810	2988.014051	22.116634
91.494680	3005.346676	22.121651
91.382704	3008.953980	22.126669
91.343925	3017.064605	22.131687
91.111235	3014.474818	22.136704
91.306452	3035.370758	22.141722
91.369010	3055.219958	22.146739
91.443686	3055.430808	22.151757
91.734670	3064.378808	22.156775
91.892488	3074.006469	22.161792
92.266632	3085.950289	22.166810
92.126989	3107.498342	22.171827
92.371098	3106.268043	22.176845
92.592205	3104.243884	22.181863
92.975844	3107.717415	22.186880
93.120020	3119.634531	22.191898
93.115581	3126.706039	22.196915
93.922461	3110.714007	22.201933
93.747704	3100.585943	22.206951
93.643611	3087.450666	22.211968
93.926454	3077.887607	22.216986
94.196058	3076.396194	22.222003
94.018180	3081.226084	22.227021
94.011205	3075.993907	22.232039
93.990541	3074.879882	22.237056
94.669396	3068.886692	22.242074
94.720262	3065.373303	22.247091
94.535738	3065.245834	22.252109
95.057963	3056.960129	22.257127
95.027866	3044.402086	22.262144
95.202368	3032.433514	22.267162
94.778640	3029.640994	22.272179
94.915572	3028.718897	22.277197
95.067758	3029.460663	22.282215
94.824724	3028.309946	22.287232
94.865761	3019.547585	22.292250
94.593909	3029.451283	22.297267
94.866042	3025.408532	22.302285
94.872836	3028.567833	22.307303
94.790448	3033.857025	22.312320
94.571436	3035.312166	22.317338
94.770036	3058.121331	22.322355
95.068408	3065.794576	22.327373
95.199062	3063.514220	22.332391
95.324236	3076.890765	22.337408
95.498502	3088.936586	22.342426
95.386972	3099.696489	22.347443
95.290170	3099.970603	22.352461
95.340035	3107.245436	22.357479
95.409366	3127.706293	22.362496
95.571563	3129.584380	22.367514
95.641565	3148.868526	22.372531
95.934696	3156.812063	22.377549
95.922319	3166.000356	22.382567
95.824423	3178.641050	22.387584
95.990836	3186.760689	22.392602
96.318860	3188.831662	22.397619
96.144933	3199.181769	22.402637
96.938992	3194.804563	22.407655
96.783609	3212.702714	22.412672
97.429224	3205.937052	22.417690
97.311563	3208.081284	22.422707
97.421289	3202.826695	22.427725
97.813166	3207.262034	22.432743
97.689779	3215.205337	22.437760
97.858006	3210.188801	22.442778
98.082080	3210.872573	22.447795
98.054837	3214.291345	22.452813
98.046505	3210.317105	22.457831
97.865986	3211.789290	22.462848
97.994282	3203.813613	22.467866
98.022993	3209.891864	22.472883
98.286118	3210.713067	22.477901
98.227470	3219.194998	22.482919
98.120611	3242.215884	22.487936
98.371383	3235.538378	22.492954
98.261349	3241.471886	22.497971
98.487136	3246.275941	22.502989
98.605464	3248.449027	22.508007
98.306779	3266.709674	22.513024
98.551746	3269.627362	22.518042
98.757574	3280.054968	22.523059
99.010087	3295.678080	22.528077
99.258982	3299.997769	22.533095
99.078667	3305.954377	22.538112
99.627661	3295.016133	22.543130
99.514040	3302.226938	22.548147
99.513864	3302.998775	22.553165
99.785801	3301.661306	22.558183
100.003757	3312.898845	22.563200
100.544639	3320.490475	22.568218
100.359896	3318.287780	22.573235
100.198716	3305.160533	22.578253
100.308346	3297.974796	22.583271
100.511252	3323.862235	22.588288
100.654357	3317.750517	22.593306
100.431988	3326.997743	22.598323
100.421529	3327.524834	22.603341
100.813891	3319.247868	22.608359
100.695090	3320.718145	22.613376
100.398924	3323.487614	22.618394
100.740264	3321.221507	22.623411
100.920133	3330.861297	22.628429
101.403803	3340.579749	22.633447
101.246844	3343.914463	22.638464
101.703941	3344.659891	22.643482
101.718470	3329.866704	22.648499
101.889785	3333.765748	22.653517
102.108673	3335.760942	22.658535
101.773768	3340.313826	22.663552
101.788675	3332.938755	22.668570
101.832809	3341.387379	22.673587
102.139291	3341.107213	22.678605
102.527693	3343.790829	22.683623
102.296771	3361.518594	22.688640
102.451575	3361.821247	22.693658
102.810928	3358.165123	22.698675
102.367748	3358.122160	22.703693
102.554944	3354.104125	22.708711
102.384326	3354.316078	22.713728
102.514338	3354.615893	22.718746
102.580773	3379.469892	22.723763
102.755893	3392.151374	22.728781
102.994254	3390.860608	22.733799
102.724257	3400.012869	22.738816
102.889714	3413.108716	22.743834
103.246188	3422.929358	22.748851
102.930104	3432.052523	22.753869
103.504741	3441.266355	22.758887
103.344537	3448.556881	22.763904
104.044430	3448.310867	22.768922
104.135177	3451.195171	22.773939
104.195091	3454.279294	22.778957
104.341296	3450.987325	22.783975
104.404143	3457.300032	22.788992
104.406459	3477.795672	22.794010
104.641774	3480.485079	22.799027
104.804614	3481.243944	22.804045
104.720146	3477.367748	22.809063
104.784925	3482.672027	22.814080
104.906526	3484.529552	22.819098
104.889284	3481.585355	22.824115
104.657328	3479.452950	22.829133
105.384765	3502.544625	22.834151
105.394335	3509.971468	22.839168
105.153532	3504.138140	22.844186
105.401626	3511.124787	22.849203
105.103601	3509.345516	22.854221
105.223775	3524.714313	22.859239
105.691873	3535.824858	22.864256
106.036393	3537.707967	22.869274
105.943711	3537.645870	22.874291
106.003016	3548.367341	22.879309
106.524268	3537.451802	22.884327
106.077602	3548.110372	22.889344
106.149216	3556.326788	22.894362
106.363544	3559.645152	22.899379
106.271123	3579.968932	22.904397
106.497752	3572.002991	22.909415
106.383830	3574.866486	22.914432
106.740426	3585.951288	22.919450
106.887928	3605.636979	22.924467
106.956823	3611.420238	22.929485
107.069803	3603.001998	22.934503
107.034656	3608.962186	22.939520
107.800104	3624.353561	22.944538
108.315294	3615.918343	22.949555
107.908661	3626.019577	22.954573
107.801907	3616.902602	22.959591
108.272929	3626.951038	22.964608
108.108068	3618.590660	22.969626
108.203382	3627.667037	22.974643
108.125740	3620.321874	22.979661
108.389660	3620.601889	22.984679
108.489343	3618.263756	22.989696
108.469844	3614.422856	22.994714
108.420982	3621.818814	22.999731
108.883358	3635.697216	23.004749
108.753786	3625.503573	23.009767
109.104631	3641.792225	23.014784
109.014198	3637.679947	23.019802
109.160622	3632.784367	23.024819
109.023622	3642.476307	23.029837
109.134071	3658.837693	23.034855
109.565024	3675.248112	23.039872
109.278877	3671.925466	23.044890
109.285301	3670.052242	23.049907
109.391780	3684.115351	23.054925
109.470279	3700.126264	23.059943
109.718940	3703.387578	23.064960
109.736622	3720.105171	23.069978
110.048569	3726.272895	23.074995
109.791860	3744.529259	23.080013
110.016721	3742.765859	23.085031
110.132296	3752.479938	23.090048
110.231708	3758.228878	23.095066
110.845474	3760.950330	23.100083
110.770820	3763.141607	23.105101
111.029350	3767.118745	23.110119
111.517722	3779.028548	23.115136
112.060099	3781.694509	23.120154
112.054700	3748.654914	23.125171
111.990440	3749.645686	23.130189
112.327717	3736.786258	23.135207
112.418198	3743.278640	23.140224
112.325508	3744.500325	23.145242
112.658087	3728.207788	23.150259
112.521789	3715.250779	23.155277
112.243454	3703.282934	23.160295
112.337380	3707.752168	23.165312
112.588023	3702.580368	23.170330
112.530791	3704.113372	23.175347
112.125822	3711.200251	23.180365
112.328506	3719.542350	23.185383
112.621494	3735.419655	23.190400
112.001920	3735.785762	23.195418
112.822706	3748.098512	23.200435
112.686037	3764.318860	23.205453
112.757800	3765.919543	23.210471
112.778228	3770.803857	23.215488
113.068631	3796.034393	23.220506
113.255932	3803.707352	23.225523
113.104646	3815.217264	23.230541
113.333044	3818.971964	23.235559
113.452788	3835.162605	23.240576
113.182891	3842.539063	23.245594
113.712425	3856.678658	23.250611
113.910169	3867.393152	23.255629
114.184164	3873.365026	23.260647
114.126533	3878.057979	23.265664
113.982115	3881.559202	23.270682
114.189023	3891.657812	23.275699
114.567018	3909.674028	23.280717
114.688534	3902.238672	23.285735
115.094778	3912.145602	23.290752
114.818268	3930.816705	23.295770
114.782388	3935.966695	23.300787
114.840793	3938.625864	23.305805
115.101527	3946.465878	23.310823
115.681153	3959.535285	23.315840
115.366156	3969.854946	23.320858
115.326148	3966.711359	23.325875
115.325960	3978.053717	23.330893
116.011557	3987.552867	23.335911
116.138115	3989.265470	23.340928
116.161595	4002.635819	23.345946
116.589491	3991.732036	23.350963
116.319517	3996.660691	23.355981
116.867678	3997.299968	23.360999
116.485433	3995.679210	23.366016
116.550262	4022.176660	23.371034
117.085530	4011.337944	23.376051
116.457762	4033.045762	23.381069
116.638532	4027.759030	23.386087
117.061169	4046.886945	23.391104
116.940720	4065.544842	23.396122
117.589317	4049.742042	23.401139
118.130836	4043.824806	23.406157
118.112579	4038.579279	23.411175
118.594907	4033.459017	23.416192
118.689151	4030.738978	23.421210
119.002821	4021.851350	23.426227
118.766741	4009.952426	23.431245
118.559403	4004.224227	23.436263
118.550880	3993.182605	23.441280
118.707196	3992.656448	23.446298
118.660453	3990.282717	23.451315
118.634754	4002.548606	23.456333
118.472097	4017.371724	23.461351
118.792136	4034.804161	23.466368
118.785946	4038.933077	23.471386
119.292434	4034.460028	23.476403
119.306632	4037.754519	23.481421
119.236577	4057.433176	23.486439
119.688591	4057.481690	23.491456
119.016476	4067.232545	23.496474
119.190196	4060.319804	23.501491
119.523905	4078.466673	23.506509
119.531857	4088.026922	23.511527
119.619293	4087.308578	23.516544
119.835799	4098.063333	23.521562
120.212287	4100.316724	23.526579
120.224834	4117.144309	23.531597
119.990633	4113.745716	23.536615
120.621076	4117.151961	23.541632
120.807687	4138.192611	23.546650
120.785035	4130.013150	23.551667
121.417635	4123.120955	23.556685
121.528122	4122.331711	23.561703
122.319818	4115.000323	23.566720
121.977067	4123.547195	23.571738
122.513733	4118.289211	23.576755
122.202130	4110.336507	23.581773
122.458278	4112.033997	23.586791
122.885532	4106.283611	23.591808
122.343346	4088.300011	23.596826
122.637338	4079.021918	23.601843
122.638312	4077.412642	23.606861
122.618095	4080.572059	23.611879
122.489494	4066.971536	23.616896
122.189568	4094.564199	23.621914
122.390767	4098.621347	23.626931
123.319280	4105.424668	23.631949
123.430767	4113.833019	23.636967
123.091570	4101.643744	23.641984
123.163265	4112.947098	23.647002
122.833930	4106.760906	23.652019
123.107821	4128.898693	23.657037
122.945213	4151.314546	23.662055
122.925449	4151.710152	23.667072
123.337235	4168.598519	23.672090
123.486553	4167.809705	23.677107
123.549137	4185.243125	23.682125
123.915285	4194.542765	23.687143
124.261566	4192.535606	23.692160
124.439295	4188.670207	23.697178
124.810172	4193.204731	23.702195
124.770631	4192.707418	23.707213
124.597514	4190.756219	23.712231
124.957476	4190.885099	23.717248
125.128810	4215.416048	23.722266
125.123793	4214.249640	23.727283
125.057507	4215.106104	23.732301
125.248582	4225.554196	23.737319
125.770462	4219.851345	23.742336
125.505156	4214.328337	23.747354
125.733401	4218.180825	23.752371
125.909278	4240.626203	23.757389
125.863893	4244.826477	23.762407
126.127277	4244.520607	23.767424
126.352276	4257.930662	23.772442
126.075460	4251.777941	23.777459
126.561112	4248.849782	23.782477
126.428419	4276.937074	23.787495
126.355508	4272.481373	23.792512
126.376220	4280.456428	23.797530
126.447991	4296.124121	23.802547
126.525387	4305.346519	23.807565
126.733164	4311.755230	23.812583
127.066653	4330.098546	23.817600
126.736213	4341.241013	23.822618
127.106109	4346.790212	23.827635
127.813546	4361.003731	23.832653
127.274382	4379.187164	23.837671
127.773851	4385.546688	23.842688
127.538935	4395.366142	23.847706
127.934077	4406.633948	23.852723
128.154241	4410.105080	23.857741
127.878538	4421.767507	23.862759
128.143834	4434.079148	23.867776
128.330563	4453.674895	23.872794
128.319533	4448.190129	23.877811
129.097119	4469.320516	23.882829
129.012747	4480.469731	23.887847
129.239444	4477.083413	23.892864
129.641933	4473.067571	23.897882
129.491949	4480.664783	23.902899
129.469473	4476.373658	23.907917
129.551567	4502.622424	23.912935
129.868620	4499.033155	23.917952
129.802505	4504.262551	23.922970
130.256187	4508.541168	23.927987
130.727159	4510.287727	23.933005
129.872646	4521.335854	23.938023
130.408219	4524.485934	23.943040
130.477691	4528.771348	23.948058
130.410624	4522.652664	23.953075
130.751223	4536.470824	23.958093
130.493032	4559.325811	23.963111
131.121880	4555.616130	23.968128
130.890480	4566.177040	23.973146
130.819509	4565.813488	23.978163
131.580461	4570.275739	23.983181
131.639190	4589.399748	23.988199
131.520733	4579.283923	23.993216
131.960245	4584.573166	23.998234
131.699403	4593.855292	24.003251
132.166452	4604.909277	24.008269
132.256822	4622.618028	24.013287
132.836961	4613.897054	24.018304
132.940709	4619.331297	24.023322
132.768586	4616.180298	24.028339
133.218523	4610.476253	24.033357
132.856787	4619.136126	24.038375
133.093894	4610.535394	24.043392
133.000177	4618.734235	24.048410
133.308660	4634.532601	24.053427
133.352978	4631.684756	24.058445
133.167406	4641.395084	24.063463
133.650371	4645.447392	24.068480
133.865305	4671.564184	24.073498
133.693586	4677.552912	24.078515
134.317125	4671.831687	24.083533
133.515018	4671.080714	24.088551
134.233100	4690.310778	24.093568
134.057515	4707.433526	24.098586
134.062430	4704.649133	24.103603
134.336335	4726.156064	24.108621
134.327249	4736.909756	24.113639
134.861320	4738.841649	24.118656
135.163403	4761.305513	24.123674
135.309748	4765.836950	24.128691
135.505888	4758.395489	24.133709
135.540556	4757.538872	24.138727
135.969586	4752.184138	24.143744
136.145470	4766.801843	24.148762
135.847799	4787.108010	24.153779
136.121636	4784.258599	24.158797
136.205784	4786.297558	24.163815
136.419484	4790.146378	24.168832
136.298095	4787.824706	24.173850
136.405620	4815.680372	24.178867
137.261390	4814.501047	24.183885
136.903454	4826.184167	24.188903
136.883983	4824.212851	24.193920
136.985419	4830.277683	24.198938
137.198458	4840.245888	24.203955
137.347963	4856.299359	24.208973
137.011517	4865.960861	24.213991
137.189191	4865.076573	24.219008
137.190180	4885.348207	24.224026
137.395022	4897.664272	24.229043
137.931673	4907.373041	24.234061
138.017230	4929.981383	24.239079
138.117240	4927.014454	24.244096
138.166960	4931.651507	24.249114
138.427384	4932.023518	24.254131
138.836978	4935.344933	24.259149
139.093607	4943.387001	24.264167
139.352792	4944.358631	24.269184
139.432564	4942.476620	24.274202
139.402207	4939.731314	24.279219
139.670797	4936.687437	24.284237
139.660806	4937.142037	24.289255
139.414344	4946.683404	24.294272
139.651129	4963.048112	24.299290
139.703732	4978.987568	24.304307
139.971946	4969.638549	24.309325
140.415758	4983.317321	24.314343
140.545710	5000.061128	24.319360
140.441043	5002.779938	24.324378
140.705584	5007.791346	24.329395
140.995544	4994.436488	24.334413
140.889310	5006.883943	24.339431
140.857244	5020.638024	24.344448
141.048408	5028.101400	24.349466
141.301727	5040.204474	24.354483
141.281344	5027.623499	24.359501
141.155511	5045.780944	24.364519
141.387485	5061.923670	24.369536
141.761586	5063.230844	24.374554
141.325793	5092.131630	24.379571
142.170153	5087.172671	24.384589
142.174769	5102.908597	24.389607
141.984920	5117.167133	24.394624
142.428652	5131.295803	24.399642
142.218987	5141.039709	24.404659
142.491501	5152.844204	24.409677
142.918297	5168.649602	24.414695
142.720848	5179.871465	24.419712
142.594845	5189.330889	24.424730
142.633908	5201.324308	24.429747
143.128269	5214.054925	24.434765
143.288962	5230.274631	24.439783
143.585598	5242.308208	24.444800
144.014171	5252.868285	24.449818
144.028052	5262.082437	24.454835
144.158374	5256.526687	24.459853
144.207414	5275.147498	24.464871
144.607738	5297.173088	24.469888
144.758450	5284.227031	24.474906
144.739810	5295.865721	24.479923
145.035781	5308.911624	24.484941
145.214845	5316.488272	24.489959
145.232880	5318.129042	24.494976
145.530503	5320.997129	24.499994
145.494224	5320.987580	24.505011
145.545704	5315.446901	24.510029
145.703702	5329.677504	24.515047
145.843539	5352.239334	24.520064
146.017448	5348.119891	24.525082
146.002604	5356.884533	24.530099
146.281382	5369.281236	24.535117
146.302942	5385.569061	24.540135
146.613410	5391.364334	24.545152
146.499138	5393.757970	24.550170
146.929074	5411.539358	24.555187
146.950279	5416.052262	24.560205
146.764938	5423.793040	24.565223
146.997682	5434.144991	24.570240
147.487466	5441.037502	24.575258
147.315229	5452.426949	24.580275
147.413998	5460.623157	24.585293
147.849598	5473.822488	24.590311
147.723107	5484.176977	24.595328
147.998936	5484.414819	24.600346
148.086339	5508.393448	24.605363
148.347755	5509.525420	24.610381
148.553658	5528.569405	24.615399
148.489458	5538.402044	24.620416
148.999403	5535.063046	24.625434
148.862801	5553.378876	24.630451
149.556500	5567.762832	24.635469
149.557689	5569.824778	24.640487
149.389730	5574.569438	24.645504
149.698429	5578.096544	24.650522
149.475337	5598.097150	24.655539
149.903669	5608.407022	24.660557
150.137513	5608.303905	24.665575
150.296511	5632.220035	24.670592
150.467722	5633.155591	24.675610
150.254364	5644.642808	24.680627
150.405860	5638.033304	24.685645
150.712782	5658.166833	24.690663
150.480656	5668.188239	24.695680
150.972447	5688.847013	24.700698
150.995925	5703.987954	24.705715
151.494859	5698.795792	24.710733
151.668570	5714.333193	24.715751
151.480303	5738.810774	24.720768
151.647623	5733.809355	24.725786
151.782323	5756.487642	24.730803
151.738316	5764.025550	24.735821
152.290593	5771.077635	24.740839
152.157174	5796.080748	24.745856
152.435900	5791.621055	24.750874
152.398684	5813.015800	24.755891
152.789478	5823.127445	24.760909
153.104763	5833.155153	24.765927
153.043250	5847.550669	24.770944
153.480023	5857.555992	24.775962
153.292803	5867.973128	24.780979
153.751546	5871.715616	24.785997
153.707085	5879.463185	24.791015
153.867556	5904.031688	24.796032
154.037009	5901.398476	24.801050
153.608075	5917.781400	24.806067
154.287358	5930.691999	24.811085
154.495049	5941.761449	24.816103
153.963295	5948.908068	24.821120
154.656854	5965.774471	24.826138
154.886592	5982.617212	24.831155
155.174815	5987.282219	24.836173
155.616290	6002.646392	24.841191
155.650117	6017.300627	24.846208
155.871951	6019.576087	24.851226
155.440574	6035.657069	24.856243
155.540992	6034.006917	24.861261
155.681942	6042.742077	24.866279
155.337649	6057.999175	24.871296
155.566694	6072.855522	24.876314
156.130913	6089.336193	24.881331
156.748939	6101.849398	24.886349
156.651919	6108.797106	24.891367
156.657364	6130.475629	24.896384
157.244444	6132.790897	24.901402
157.298853	6143.925361	24.906419
157.152560	6148.612125	24.911437
157.582029	6160.107674	24.916455
157.324550	6174.788358	24.921472
157.735047	6188.325791	24.926490
157.712704	6205.094610	24.931507
157.955272	6222.652229	24.936525
158.346347	6219.565847	24.941543
158.479460	6238.899648	24.946560
158.934612	6249.544060	24.951578
159.469824	6257.861218	24.956595
159.318125	6262.261423	24.961613
160.060862	6257.420363	24.966631
159.834963	6257.669394	24.971648
160.020049	6257.743993	24.976666
160.332792	6253.895127	24.981683
160.084039	6250.871157	24.986701
160.563002	6261.265726	24.991719
160.609422	6277.151613	24.996736
160.659467	6283.385718	25.001754
160.871012	6293.266079	25.006771
160.709940	6286.439700	25.011789
160.680244	6284.605443	25.016807
160.808962	6304.845172	25.021824
161.517446	6318.330847	25.026842
161.138129	6322.512501	25.031859
161.105760	6336.082652	25.036877
161.519316	6350.275874	25.041895
161.539201	6363.509397	25.046912
161.951852	6375.076517	25.051930
161.827685	6392.928782	25.056947
161.851942	6402.415943	25.061965
162.267049	6398.750366	25.066983
162.073906	6421.804040	25.072000
162.408071	6432.518154	25.077018
162.671584	6432.903855	25.082035
162.455686	6452.215031	25.087053
162.951561	6460.023863	25.092071
162.939952	6469.324218	25.097088
163.199766	6484.112656	25.102106
163.361947	6501.627646	25.107123
163.547917	6527.075786	25.112141
163.844381	6521.834570	25.117159
163.616834	6534.326854	25.122176
164.012484	6540.159938	25.127194
164.282739	6546.326462	25.132211
164.501500	6571.506736	25.137229
164.851774	6579.888852	25.142247
164.947069	6578.812995	25.147264
165.017966	6580.960013	25.152282
165.354151	6602.055485	25.157299
165.452349	6604.097784	25.162317
166.132700	6599.950287	25.167335
166.320010	6606.421729	25.172352
166.286619	6611.465024	25.177370
166.794418	6622.492168	25.182387
166.594104	6634.336279	25.187405
166.501775	6638.163964	25.192423
166.779734	6639.541322	25.197440
166.569338	6634.836755	25.202458
166.952331	6658.578172	25.207475
166.973094	6667.603686	25.212493
167.299252	6673.832362	25.217511
167.102305	6689.208957	25.222528
167.232018	6692.596843	25.227546
167.561205	6703.992603	25.232563
167.759482	6725.352927	25.237581
168.059296	6738.877505	25.242599
167.740199	6754.782410	25.247616
168.034126	6768.909860	25.252634
168.535477	6778.041325	25.257651
168.580898	6793.524570	25.262669
168.793868	6800.141363	25.267687
168.494758	6819.664183	25.272704
168.913161	6833.578142	25.277722
168.939792	6845.708058	25.282739
169.179353	6865.929496	25.287757
169.674586	6876.341374	25.292775
169.666642	6890.802694	25.297792
170.034370	6906.178018	25.302810
169.888788	6916.808481	25.307827
170.021369	6939.202068	25.312845
170.428990	6939.073097	25.317863
170.783492	6947.624837	25.322880
170.830891	6970.668000	25.327898
171.481178	6975.003397	25.332915
171.691748	6981.425315	25.337933
171.736607	6981.449908	25.342951
171.799579	6984.735072	25.347968
172.013058	6978.754051	25.352986
172.183591	6991.465195	25.358003
172.154471	7013.543143	25.363021
172.534291	7008.686874	25.368039
172.545966	7013.892727	25.373056
172.408976	7012.139799	25.378074
172.686135	7029.296922	25.383091
172.706153	7038.814334	25.388109
172.809494	7047.622664	25.393127
172.995624	7060.212238	25.398144
173.203250	7068.217305	25.403162
173.318152	7080.620589	25.408179
173.461554	7111.091846	25.413197
173.960367	7108.261759	25.418215
173.828196	7135.989258	25.423232
174.022155	7144.234611	25.428250
174.285587	7146.371548	25.433267
174.267446	7171.004127	25.438285
174.353795	7175.814377	25.443303
174.459948	7201.315085	25.448320
174.714109	7208.704090	25.453338
174.933105	7237.547705	25.458355
174.836548	7248.096720	25.463373
175.246958	7268.547768	25.468391
175.468439	7283.393147	25.473408
176.016324	7304.096396	25.478426
176.025078	7313.887683	25.483443
176.153049	7325.363282	25.488461
176.809364	7344.426758	25.493479
176.280933	7347.551833	25.498496
176.546732	7355.223298	25.503514
176.702822	7372.552795	25.508531
176.760714	7394.733730	25.513549
177.206443	7414.135893	25.518567
177.722420	7426.897669	25.523584
177.271945	7429.129448	25.528602
177.649080	7446.432950	25.533619
177.717074	7459.864742	25.538637
177.691029	7474.244610	25.543655
178.401350	7495.931773	25.548672
178.875563	7508.327365	25.553690
179.153381	7522.903341	25.558707
179.188812	7522.342653	25.563725
179.082291	7526.393560	25.568743
179.458378	7555.205304	25.573760
179.367556	7560.739291	25.578778
179.785141	7565.059597	25.583795
179.463459	7582.290028	25.588813
179.847412	7591.668968	25.593831
180.157829	7605.153072	25.598848
179.891999	7624.920104	25.603866
180.393956	7623.432569	25.608883
180.495363	7647.334801	25.613901
180.365100	7652.492715	25.618919
180.843848	7666.821675	25.623936
181.036943	7686.784266	25.628954
181.482587	7688.899496	25.633971
181.446450	7706.415136	25.638989
181.608123	7720.570037	25.644007
181.693441	7721.031224	25.649024
181.838303	7733.630764	25.654042
182.222464	7746.700572	25.659059
182.562337	7759.224163	25.664077
182.729020	7767.230297	25.669095
182.918283	7788.524258	25.674112
182.806450	7787.345962	25.679130
183.196042	7802.107071	25.684148
183.296632	7815.573751	25.689165
183.737751	7817.358111	25.694183
184.059766	7840.630391	25.699200
184.190912	7863.298880	25.704218
184.734393	7854.253936	25.709236
184.067975	7862.335961	25.714253
184.411863	7874.539108	25.719271
184.358104	7891.565595	25.724288
184.803850	7904.575344	25.729306
185.203416	7916.226971	25.734324
185.088136	7928.266224	25.739341
185.403299	7942.252418	25.744359
185.808494	7947.135081	25.749376
185.928211	7958.015392	25.754394
187.182018	7921.589059	25.759412
187.871339	7914.700508	25.764429
187.892406	7920.552618	25.769447
188.153318	7913.425534	25.774464
188.149887	7899.296877	25.779482
188.170825	7876.235909	25.784500
188.422396	7859.752169	25.789517
189.199070	7847.668101	25.794535
189.386558	7822.082126	25.799552
189.565303	7810.704033	25.804570
189.771942	7790.167759	25.809588
189.917647	7781.348599	25.814605
189.814014	7766.778736	25.819623
189.609847	7754.352378	25.824640
189.355027	7763.332788	25.829658
189.596001	7754.431137	25.834676
189.511707	7763.499698	25.839693
189.553892	7752.229349	25.844711
189.268316	7754.870918	25.849728
189.337591	7770.209215	25.854746
189.545089	7786.597598	25.859764
189.579915	7797.352125	25.864781
189.451896	7819.252761	25.869799
190.145041	7829.294162	25.874816
189.870494	7860.646767	25.879834
189.929770	7863.786216	25.884852
190.022646	7895.665182	25.889869
189.958042	7906.728312	25.894887
189.879127	7934.357462	25.899904
190.157289	7968.593432	25.904922
190.359862	7988.766695	25.909940
190.644420	8014.432701	25.914957
190.836127	8046.911879	25.919975
191.085043	8057.648001	25.924992
191.234953	8088.041217	25.930010
191.779803	8109.584260	25.935028
191.762150	8139.875520	25.940045
192.100848	8156.447410	25.945063
192.651788	8180.602685	25.950080
192.689375	8198.370930	25.955098
192.916605	8209.180987	25.960116
193.382704	8228.974556	25.965133
194.067867	8244.099013	25.970151
194.122677	8247.449649	25.975168
194.190187	8265.624080	25.980186
194.573080	8280.499437	25.985204
194.764452	8290.942269	25.990221
194.976754	8304.381544	25.995239
195.298598	8306.514929	26.000256
195.128637	8317.102436	26.005274
195.371904	8317.534203	26.010292
195.569095	8343.634044	26.015309
195.628039	8355.275838	26.020327
196.210280	8361.132757	26.025344
196.097224	8380.347472	26.030362
196.068675	8381.564814	26.035380
196.411557	8407.006373	26.040397
196.394597	8421.532854	26.045415
196.672790	8432.067251	26.050432
196.642104	8448.676762	26.055450
197.225074	8466.071349	26.060468
197.587142	8478.122153	26.065485
197.582937	8484.518463	26.070503
197.631778	8506.671758	26.075520
197.843596	8523.088514	26.080538
197.955357	8537.079368	26.085556
198.179337	8559.222409	26.090573
198.401974	8574.443006	26.095591
198.645572	8591.813967	26.100608
198.760517	8600.341479	26.105626
199.155017	8603.404702	26.110644
199.592411	8614.734432	26.115661
199.837887	8635.021689	26.120679
200.139076	8641.433468	26.125696
200.176065	8653.232869	26.130714
200.501150	8667.585916	26.135732
200.514507	8673.445136	26.140749
200.298585	8680.087381	26.145767
200.653133	8701.462153	26.150784
200.700441	8714.262751	26.155802
201.006139	8733.359623	26.160820
201.246835	8749.215442	26.165837
200.980142	8762.563092	26.170855
201.679828	8780.204304	26.175872
201.799676	8791.862760	26.180890
201.994453	8810.754989	26.185908
201.903410	8825.563187	26.190925
202.214678	8851.417397	26.195943
202.745005	8861.111555	26.200960
202.835437	8884.230444	26.205978
203.249228	8890.870406	26.210996
203.113580	8902.400986	26.216013
203.369189	8923.659077	26.221031
203.845680	8924.872614	26.226048
203.759597	8945.280123	26.231066
203.789225	8962.157148	26.236084
204.358751	8983.965006	26.241101
204.417717	8995.259026	26.246119
204.730157	8998.391541	26.251136
204.802124	9018.140191	26.256154
204.962646	9026.237037	26.261172
205.316935	9045.942054	26.266189
205.611701	9057.941013	26.271207
205.757662	9068.268439	26.276224
205.962824	9078.631420	26.281242
206.723502	9092.666733	26.286260
206.804780	9106.147257	26.291277
207.115215	9124.960151	26.296295
207.114937	9119.489274	26.301312
207.175363	9125.693552	26.306330
207.548087	9133.149000	26.311348
207.630426	9137.983375	26.316365
207.573864	9149.010523	26.321383
208.259966	9152.564343	26.326400
208.201172	9172.091358	26.331418
208.161215	9185.149949	26.336436
208.540097	9195.116083	26.341453
208.622907	9200.676807	26.346471
208.780615	9225.201234	26.351488
209.308337	9240.472588	26.356506
209.145280	9253.375853	26.361524
209.744002	9266.485759	26.366541
209.601928	9277.349594	26.371559
210.129999	9290.495266	26.376576
210.047236	9309.547530	26.381594
210.273876	9320.168558	26.386612
210.514940	9338.368023	26.391629
210.400519	9351.639632	26.396647
211.562814	9356.405561	26.401664
211.720229	9375.620005	26.406682
212.114170	9368.699540	26.411700
212.382692	9372.972620	26.416717
212.087533	9378.398073	26.421735
212.327204	9389.752787	26.426752
212.360177	9395.805876	26.431770
212.724898	9403.248640	26.436788
212.769835	9416.927894	26.441805
212.456522	9428.423120	26.446823
212.959117	9425.957569	26.451840
213.061222	9456.033799	26.456858
212.877925	9472.725672	26.461876
213.393212	9493.421579	26.466893
213.573190	9508.204431	26.471911
213.817312	9522.897513	26.476928
214.418394	9542.855503	26.481946
214.427542	9551.415046	26.486964
214.733779	9562.375562	26.491981
214.568887	9583.810601	26.496999
214.987435	9601.522967	26.502016
215.098236	9613.787087	26.507034
215.588873	9643.048576	26.512052
215.956229	9638.830278	26.517069
215.958342	9653.730418	26.522087
216.149561	9661.084859	26.527104
216.489062	9673.798314	26.532122
216.999698	9687.960524	26.537140
217.009788	9690.935424	26.542157
216.880393	9707.533207	26.547175
217.067666	9722.307125	26.552192
217.330421	9736.609566	26.557210
217.704128	9764.206805	26.562228
218.335852	9769.111081	26.567245
218.634322	9789.611316	26.572263
218.786536	9796.881109	26.577280
218.973283	9797.578674	26.582298
219.324738	9801.306613	26.587316
219.571657	9818.174073	26.592333
219.632624	9844.681032	26.597351
219.326085	9838.055350	26.602368
219.710130	9855.274383	26.607386
219.685852	9877.368027	26.612404
219.880310	9885.100206	26.617421
219.773461	9916.804663	26.622439
220.287549	9926.711832	26.627456
220.311845	9950.554267	26.632474
220.392601	9971.553761	26.637492
220.954870	9990.847665	26.642509
220.951396	10005.095125	26.647527
221.687524	10018.839205	26.652544
222.290695	10039.194556	26.657562
222.125420	10047.122418	26.662580
223.083899	10058.318150	26.667597
222.720983	10080.793157	26.672615
223.020131	10071.803839	26.677632
223.358252	10095.108920	26.682650
223.031447	10109.900397	26.687668
223.444338	10116.700181	26.692685
223.727873	10141.286370	26.697703
223.496010	10155.880395	26.702720
223.757238	10175.393158	26.707738
223.735770	10187.789117	26.712756
224.052264	10199.551978	26.717773
224.322004	10218.967209	26.722791
224.461286	10238.800359	26.727808
225.059012	10250.782944	26.732826
226.158654	10254.327590	26.737844
227.006941	10244.545957	26.742861
227.215495	10240.852689	26.747879
227.094093	10245.169201	26.752896
227.468849	10236.335447	26.757914
227.574749	10247.080210	26.762932
227.796088	10240.333940	26.767949
227.683337	10241.461061	26.772967
227.876075	10248.772962	26.777984
227.835688	10245.840942	26.783002
227.861880	10250.496174	26.788020
228.099626	10251.525398	26.793037
228.420013	10276.119658	26.798055
228.329986	10277.690424	26.803072
229.009400	10291.026863	26.808090
229.133062	10295.017731	26.813108
229.578027	10292.117547	26.818125
229.621400	10296.817122	26.823143
230.131268	10314.284546	26.828160
229.952492	10323.300609	26.833178
230.450475	10336.059910	26.838196
230.703104	10330.542122	26.843213
230.206690	10344.893284	26.848231
230.282158	10364.474360	26.853248
230.693414	10384.656607	26.858266
230.702151	10401.521378	26.863284
231.278623	10416.145699	26.868301
231.481525	10444.060179	26.873319
231.705279	10456.697964	26.878336
232.034595	10462.175897	26.883354
231.876114	10484.272883	26.888372
231.851552	10491.596927	26.893389
232.537924	10524.168851	26.898407
232.651352	10544.310946	26.903424
232.910677	10569.128859	26.908442
232.920683	10587.270054	26.913460
233.402762	10600.943140	26.918477
233.759872	10628.146003	26.923495
233.948197	10652.553879	26.928512
234.580700	10659.412379	26.933530
234.210288	10682.009265	26.938548
235.114646	10683.962759	26.943565
235.276716	10699.198892	26.948583
235.645007	10704.507912	26.953600
236.025889	10702.419186	26.958618
235.661411	10715.381773	26.963636
235.984602	10729.671581	26.968653
236.091700	10743.409061	26.973671
236.402885	10761.651687	26.978688
236.616241	10775.177148	26.983706
236.341381	10807.536189	26.988724
237.235529	10802.897941	26.993741
237.164160	10824.507690	26.998759
236.843383	10847.564337	27.003776
237.120752	10858.332118	27.008794
237.047254	10886.047318	27.013812
237.740756	10912.969222	27.018829
237.881703	10940.857353	27.023847
237.835074	10957.297240	27.028864
238.415889	10975.459221	27.033882
238.425546	11010.129022	27.038900
238.927158	11013.268908	27.043917
239.373669	11043.583741	27.048935
239.475524	11069.748444	27.053952
239.999076	11081.887770	27.058970
240.174038	11115.676893	27.063988
240.678507	11115.615624	27.069005
240.944490	11136.126283	27.074023
240.730566	11151.822842	27.079040
241.773522	11164.456292	27.084058
241.746395	11185.264672	27.089076
241.998132	11185.445289	27.094093
242.372710	11207.968790	27.099111
242.208955	11223.644211	27.104128
242.933875	11218.995457	27.109146
242.784737	11244.680255	27.114164
242.983673	11252.068768	27.119181
242.796614	11275.054243	27.124199
243.035936	11295.487723	27.129216
243.240364	11311.673760	27.134234
243.252034	11333.375538	27.139252
244.099847	11358.040204	27.144269
244.338376	11380.798438	27.149287
244.418696	11407.758498	27.154304
244.950271	11421.365484	27.159322
245.177800	11448.632904	27.164340
245.273508	11464.918102	27.169357
245.662908	11482.115883	27.174375
245.693912	11503.801965	27.179392
246.505061	11509.320592	27.184410
246.583861	11537.147901	27.189428
246.741224	11536.495258	27.194445
246.589782	11551.106687	27.199463
246.735923	11577.698003	27.204480
247.421026	11589.888818	27.209498
247.403270	11617.297848	27.214516
247.994200	11633.944330	27.219533
248.571928	11633.158170	27.224551
248.993303	11651.520017	27.229568
249.261327	11656.318588	27.234586
249.763588	11648.924721	27.239604
249.734977	11652.302181	27.244621
250.186942	11662.558324	27.249639
250.204849	11681.211571	27.254656
250.356921	11681.700833	27.259674
250.590642	11687.917363	27.264692
250.917117	11694.556117	27.269709
251.159663	11706.443067	27.274727
251.049721	11719.290323	27.279744
251.296164	11712.153032	27.284762
251.510675	11723.318274	27.289780
252.095241	11737.948707	27.294797
252.193021	11741.022422	27.299815
252.254555	11750.373164	27.304832
252.263334	11756.777994	27.309850
252.234214	11771.485276	27.314868
252.563741	11787.264229	27.319885
253.050551	11808.256382	27.324903
253.000518	11825.531422	27.329920
253.338414	11846.071624	27.334938
253.379965	11871.461532	27.339956
253.762276	11891.429974	27.344973
254.243068	11908.105072	27.349991
254.337220	11932.997502	27.355008
254.316207	11952.061183	27.360026
254.430669	11976.100735	27.365044
255.121898	12006.419544	27.370061
255.406917	12021.963648	27.375079
255.454903	12045.924865	27.380096
255.867548	12060.578752	27.385114
256.122793	12087.156925	27.390132
256.521607	12096.049747	27.395149
256.762439	12112.945849	27.400167
257.078685	12129.501232	27.405184
257.368587	12147.892477	27.410202
257.597583	12163.843475	27.415220
258.197949	12177.929447	27.420237
258.693768	12171.696401	27.425255
258.928486	12195.621103	27.430272
259.677574	12187.584226	27.435290
259.963332	12199.620155	27.440308
259.725463	12198.761003	27.445325
260.772926	12206.825619	27.450343
260.827815	12216.809751	27.455360
260.766775	12222.117210	27.460378
260.744973	12225.255641	27.465396
261.019908	12225.211655	27.470413
261.099381	12236.030029	27.475431
261.328398	12269.238601	27.480448
261.333051	12273.255083	27.485466
261.582029	12288.380092	27.490484
261.630333	12303.381907	27.495501
262.000627	12323.825748	27.500519
262.359626	12340.742809	27.505536
262.494452	12358.738495	27.510554
262.478818	12380.692204	27.515572
262.518520	12405.208555	27.520589
263.140798	12419.082943	27.525607
262.609752	12449.440283	27.530624
263.197411	12472.245794	27.535642
263.546337	12499.308187	27.540660
263.834071	12527.082456	27.545677
264.353215	12555.297805	27.550695
264.321297	12576.483876	27.555712
263.955588	12589.459182	27.560730
264.510500	12616.765425	27.565748
264.979392	12650.720110	27.570765
265.373157	12671.455087	27.575783
265.911101	12692.954987	27.580800
266.382548	12713.763387	27.585818
266.327770	12730.222212	27.590836
266.583475	12751.327689	27.595853
267.079763	12767.944272	27.600871
267.423352	12788.864518	27.605888
267.745080	12816.028236	27.610906
269.001986	12798.858908	27.615924
269.491891	12798.434492	27.620941
269.919867	12792.474471	27.625959
269.777669	12792.410568	27.630976
270.270902	12797.027455	27.635994
270.017263	12796.517709	27.641012
270.091487	12810.495823	27.646029
270.566676	12816.050423	27.651047
270.610915	12820.575632	27.656064
271.016581	12840.741395	27.661082
271.122073	12843.667421	27.666100
271.365772	12860.253316	27.671117
271.917561	12877.607563	27.676135
271.716052	12892.999473	27.681152
271.585316	12911.410087	27.686170
272.155284	12929.385404	27.691188
271.987816	12957.525272	27.696205
272.552225	12964.883443	27.701223
272.334445	12990.204477	27.706240
273.056074	13013.140663	27.711258
272.849973	13026.366349	27.716276
272.893409	13064.752732	27.721293
273.313034	13093.381669	27.726311
273.383540	13122.436150	27.731328
273.930738	13158.118491	27.736346
274.089004	13175.819474	27.741364
274.288450	13206.975032	27.746381
275.169993	13238.384128	27.751399
275.390803	13263.256868	27.756416
275.600751	13282.343977	27.761434
275.954490	13294.955379	27.766452
276.328357	13324.115834	27.771469
277.228317	13343.478782	27.776487
277.143482	13355.706746	27.781504
277.451774	13363.570802	27.786522
278.015047	13372.518094	27.791540
277.867178	13390.317487	27.796557
278.354178	13404.575260	27.801575
278.682814	13415.863951	27.806592
278.735837	13437.167392	27.811610
279.174697	13433.474918	27.816628
279.412563	13455.556837	27.821645
279.682297	13468.400278	27.826663
279.339450	13487.814065	27.831680
280.141782	13505.978731	27.836698
280.441321	13512.231962	27.841716
280.568780	13543.334297	27.846733
280.487229	13556.025235	27.851751
280.471050	13577.044401	27.856768
280.343347	13597.891993	27.861786
281.420121	13622.232410	27.866804
281.293721	13667.510320	27.871821
281.774581	13688.526398	27.876839
282.061950	13702.021108	27.881856
282.451500	13730.005353	27.886874
282.964821	13739.450020	27.891892
283.285024	13770.410993	27.896909
283.776742	13789.387350	27.901927
283.724957	13807.864241	27.906944
284.256342	13828.031737	27.911962
284.509120	13839.374702	27.916980
284.726956	13861.731701	27.921997
285.072943	13865.474132	27.927015
285.717836	13893.700180	27.932032
285.568805	13900.449706	27.937050
286.055532	13914.354905	27.942068
286.021427	13939.010711	27.947085
286.525445	13955.526300	27.952103
286.366232	13976.579947	27.957120
287.041170	13997.060351	27.962138
287.114154	14019.491253	27.967156
287.246340	14043.600146	27.972173
287.968191	14062.780110	27.977191
287.966100	14083.896807	27.982208
288.204127	14099.354789	27.987226
288.872081	14123.066187	27.992244
288.890368	14152.196059	27.997261
289.266806	14160.064580	28.002279
289.321772	14189.312751	28.007296
289.559293	14208.419851	28.012314
289.938367	14231.181599	28.017332
289.982600	14254.766808	28.022349
290.200416	14284.207906	28.027367
290.668473	14314.099525	28.032384
290.894971	14343.190894	28.037402
291.716148	14357.854056	28.042420
291.490635	14382.533871	28.047437
292.095403	14413.661647	28.052455
292.108325	14427.877041	28.057472
292.263360	14461.383289	28.062490
293.346882	14470.978121	28.067508
293.544431	14497.205970	28.072525
294.330246	14514.094679	28.077543
294.672353	14509.182781	28.082560
295.050357	14539.824772	28.087578
295.405472	14538.091498	28.092596
295.523704	14545.424401	28.097613
295.438656	14544.359234	28.102631
295.537228	14550.592138	28.107648
295.902105	14564.317012	28.112666
296.376195	14571.650409	28.117684
296.310012	14595.773615	28.122701
296.837419	14602.665996	28.127719
297.200643	14621.460424	28.132736
297.172239	14643.236490	28.137754
297.456293	14651.872955	28.142772
297.367863	14671.934923	28.147789
297.881641	14695.799673	28.152807
298.225159	14717.568837	28.157824
298.271146	14741.382998	28.162842
298.736277	14767.901161	28.167860
298.266994	14792.538248	28.172877
298.950763	14813.795258	28.177895
299.811563	14835.702903	28.182912
300.494664	14852.540210	28.187930
300.838189	14868.545138	28.192948
301.270118	14889.684629	28.197965
301.412357	14908.824634	28.202983
301.902160	14909.978051	28.208000
302.115108	14923.453415	28.213018
302.667483	14935.114637	28.218036
302.658758	14957.964344	28.223053
302.635919	14971.147563	28.228071
303.101171	14975.575986	28.233088
302.946022	14994.292596	28.238106
303.321719	15017.415401	28.243124
303.799414	15040.125108	28.248141
303.662229	15065.392944	28.253159
303.974162	15085.900666	28.258176
304.384115	15105.619228	28.263194
305.145271	15116.254881	28.268212
304.878186	15153.802424	28.273229
305.390881	15171.663911	28.278247
306.168585	15190.684295	28.283264
306.212865	15210.046357	28.288282
306.450809	15233.833055	28.293300
306.624617	15250.602002	28.298317
307.070298	15279.898629	28.303335
307.440617	15300.781232	28.308352
307.294812	15320.699338	28.313370
307.921812	15338.077977	28.318388
308.137948	15365.141043	28.323405
308.362062	15378.835549	28.328423
309.055510	15401.336955	28.333440
309.432383	15425.421688	28.338458
309.530645	15446.382629	28.343476
309.919424	15469.234270	28.348493
309.775096	15494.915406	28.353511
310.744182	15514.012131	28.358528
310.700457	15538.194334	28.363546
311.135431	15554.441197	28.368564
311.339577	15572.467919	28.373581
311.364195	15589.612726	28.378599
312.147108	15595.660953	28.383616
311.828606	15630.109831	28.388634
312.286114	15645.670362	28.393652
312.332978	15661.280795	28.398669
312.620237	15694.070127	28.403687
312.778064	15730.422205	28.408704
313.500339	15759.692769	28.413722
313.616897	15778.385762	28.418740
313.884404	15818.377972	28.423757
314.024933	15839.965864	28.428775
314.694143	15868.016147	28.433792
314.379363	15897.458386	28.438810
315.180321	15931.889427	28.443828
315.535603	15951.736596	28.448845
315.892256	15981.190018	28.453863
316.431991	16002.310878	28.458880
316.738983	16032.743955	28.463898
317.507818	16056.321039	28.468916
317.450599	16076.136587	28.473933
318.011818	16101.527486	28.478951
318.575724	16106.522575	28.483968
319.169452	16117.556449	28.488986
319.747800	16120.523400	28.494004
320.172070	16136.537786	28.499021
320.099856	16136.335757	28.504039
320.571237	16148.358528	28.509056
320.774460	16170.522524	28.514074
321.081078	16169.522543	28.519092
321.169098	16181.363546	28.524109
321.500351	16208.826003	28.529127
321.765348	16215.987887	28.534144
321.518822	16241.396054	28.539162
321.744815	16262.195831	28.544180
321.826463	16289.135269	28.549197
322.318047	16321.934960	28.554215
323.016902	16341.775733	28.559232
323.064595	16381.105464	28.564250
323.225446	16405.529738	28.569268
323.559862	16439.091209	28.574285
323.872689	16469.987555	28.579303
324.772205	16473.608921	28.584320
325.228679	16495.752017	28.589338
326.012725	16499.542939	28.594356
326.411860	16515.089070	28.599373
327.189010	16526.774377	28.604391
327.683243	16529.654929	28.609408
327.657773	16538.337547	28.614426
328.256519	16526.131059	28.619444
328.684449	16517.743598	28.624461
329.289314	16527.804756	28.629479
329.431057	16515.080708	28.634496
329.519165	16514.948936	28.639514
329.870391	16519.859218	28.644532
330.104314	16525.779604	28.649549
330.043317	16535.467767	28.654567
330.256169	16535.858486	28.659584
330.417292	16550.277304	28.664602
330.649881	16554.539520	28.669620
330.852764	16571.796666	28.674637
330.660738	16593.046845	28.679655
330.846940	16607.404662	28.684672
330.978002	16627.833363	28.689690
331.158042	16660.332417	28.694708
331.645599	16678.787854	28.699725
331.805856	16716.450120	28.704743
332.361439	16729.324355	28.709760
332.285863	16762.542138	28.714778
332.742441	16796.564212	28.719796
333.081439	16828.976446	28.724813
333.347225	16863.624106	28.729831
334.127274	16886.174171	28.734848
334.496558	16919.763741	28.739866
334.603776	16947.510166	28.744884
335.168572	16972.372090	28.749901
335.418400	17003.510388	28.754919
335.894840	17023.781063	28.759936
336.165732	17051.501186	28.764954
336.511621	17076.364522	28.769972
336.734115	17106.180297	28.774989
336.734600	17139.727890	28.780007
337.222131	17156.326755	28.785024
337.893900	17189.127228	28.790042
338.194167	17206.921691	28.795060
338.913504	17226.726907	28.800077
339.409552	17251.080784	28.805095
339.803650	17266.943781	28.810112
340.056199	17293.489802	28.815130
340.590288	17300.232406	28.820148
341.048110	17309.515223	28.825165
340.916095	17326.108505	28.830183
341.291126	17356.937503	28.835200
341.389198	17379.499491	28.840218
341.849518	17405.972246	28.845236
342.201002	17426.537563	28.850253
342.498077	17459.426431	28.855271
342.987062	17479.451150	28.860288
343.174744	17501.994792	28.865306
343.539952	17530.426323	28.870324
344.040927	17551.659847	28.875341
344.071623	17580.897644	28.880359
344.764197	17590.862439	28.885376
345.278008	17619.227664	28.890394
345.776445	17630.386084	28.895412
346.382439	17636.109096	28.900429
346.650818	17653.895312	28.905447
347.568841	17643.427402	28.910464
348.037240	17648.399919	28.915482
348.144281	17649.054741	28.920500
348.648846	17643.737298	28.925517
348.740210	17656.297676	28.930535
349.353059	17663.337510	28.935552
349.787689	17669.532909	28.940570
349.661617	17671.028566	28.945588
349.716122	17671.878424	28.950605
349.688083	17686.532440	28.955623
350.325706	17707.750628	28.960640
350.092939	17719.136897	28.965658
350.187261	17738.423950	28.970676
350.644089	17764.781209	28.975693
350.680776	17793.269490	28.980711
351.082452	17812.098779	28.985728
351.364216	17852.842287	28.990746
351.193398	17879.067654	28.995764
351.732741	17916.005498	29.000781
351.529764	17955.416574	29.005799
351.878696	17989.647139	29.010816
352.199348	18038.070215	29.015834
352.212807	18091.988432	29.020852
353.038577	18130.249285	29.025869
353.104422	18181.639430	29.030887
353.474184	18220.016476	29.035904
354.277827	18265.076543	29.040922
354.514424	18310.866129	29.045940
354.875024	18344.078508	29.050957
355.364652	18385.598058	29.055975
356.929979	18386.408180	29.060992
357.802440	18415.120054	29.066010
358.717286	18425.887593	29.071028
359.439660	18434.501364	29.076045
359.582828	18452.793906	29.081063
359.602951	18447.306979	29.086080
359.761777	18458.366496	29.091098
359.996501	18475.306404	29.096116
360.293166	18476.687114	29.101133
360.334957	18507.532772	29.106151
360.318551	18519.929378	29.111168
360.802473	18549.625663	29.116186
360.988212	18574.345243	29.121204
361.456336	18595.320850	29.126221
361.899050	18617.335107	29.131239
362.045307	18648.722824	29.136256
362.321084	18668.307786	29.141274
362.511054	18693.023662	29.146292
363.145520	18720.701582	29.151309
363.857088	18757.725283	29.156327
364.303335	18768.951747	29.161344
364.879176	18785.239113	29.166362
364.836283	18816.151878	29.171380
365.461897	18820.591701	29.176397
366.562033	18830.388068	29.181415
366.836347	18843.075645	29.186432
367.287582	18847.236337	29.191450
367.516657	18850.017693	29.196468
367.813962	18870.300812	29.201485
367.765962	18881.572638	29.206503
367.989114	18885.162262	29.211520
368.191137	18899.470459	29.216538
368.412640	18921.411082	29.221556
368.721695	18941.345409	29.226573
368.573863	18959.619000	29.231591
368.930258	18987.562595	29.236608
369.366559	19026.688456	29.241626
369.229672	19057.516865	29.246644
369.824064	19088.313031	29.251661
369.735406	19122.280334	29.256679
370.180838	19166.306844	29.261696
370.869765	19198.774059	29.266714
370.702042	19253.907981	29.271732
371.100777	19291.678635	29.276749
371.495908	19331.389329	29.281767
371.960285	19371.537608	29.286784
372.413717	19411.299989	29.291802
372.760968	19459.355224	29.296820
373.322298	19496.393683	29.301837
373.575674	19543.705270	29.306855
373.710774	19573.762718	29.311872
374.353736	19613.933001	29.316890
374.360468	19662.200110	29.321908
375.087802	19701.030113	29.326925
375.633869	19742.633211	29.331943
376.013911	19785.368581	29.336960
376.919343	19825.123852	29.341978
377.153053	19862.372204	29.346996
377.612878	19883.823863	29.352013
378.038943	19920.241544	29.357031
378.417189	19944.892299	29.362048
379.025001	19969.177360	29.367066
379.284770	19999.291460	29.372084
380.058150	20024.268806	29.377101
380.262354	20051.789290	29.382119
380.520324	20080.629818	29.387136
381.147127	20103.852232	29.392154
380.951282	20140.736469	29.397172
381.269820	20166.195626	29.402189
381.371953	20209.865840	29.407207
381.858616	20243.512894	29.412224
382.457324	20274.725179	29.417242
382.587917	20326.035066	29.422260
383.030549	20359.149056	29.427277
383.686436	20393.563687	29.432295
384.309505	20430.148957	29.437312
385.348631	20435.218451	29.442330
385.665924	20452.970861	29.447348
386.023006	20485.215174	29.452365
386.471035	20493.192694	29.457383
386.694463	20513.697009	29.462400
387.416717	20521.395758	29.467418
387.575844	20547.573449	29.472436
388.188069	20545.527463	29.477453
388.273318	20564.667928	29.482471
388.533447	20582.729865	29.487488
388.910087	20591.276281	29.492506
389.099738	20616.365576	29.497524
389.607629	20634.377224	29.502541
390.055637	20658.093049	29.507559
390.615229	20685.526854	29.512576
391.023965	20700.854469	29.517594
391.111412	20726.114393	29.522612
391.485170	20741.599415	29.527629
391.719678	20768.865154	29.532647
391.848490	20795.023192	29.537664
392.136685	20824.854789	29.542682
392.341325	20860.386835	29.547700
392.826118	20886.187563	29.552717
392.948611	20915.036959	29.557735
393.637278	20956.851977	29.562752
394.376436	20988.145582	29.567770
394.247085	21028.347502	29.572788
394.300392	21064.183434	29.577805
394.778101	21098.164859	29.582823
395.234362	21142.547869	29.587840
395.805698	21172.711578	29.592858
396.019097	21219.479633	29.597876
396.315364	21262.075394	29.602893
396.916007	21297.322880	29.607911
396.856815	21341.234949	29.612928
397.490739	21372.979363	29.617946
397.714456	21433.104041	29.622964
398.981911	21458.424598	29.627981
399.483917	21496.929919	29.632999
399.429976	21525.998235	29.638016
400.142845	21561.933490	29.643034
400.604613	21603.601331	29.648052
401.226466	21637.163327	29.653069
401.414179	21664.570981	29.658087
400.915487	21708.844732	29.663104
401.515284	21738.353301	29.668122
402.209997	21774.908692	29.673140
402.494207	21816.091826	29.678157
403.067688	21857.938260	29.683175
403.229536	21905.801959	29.688192
403.393880	21947.162067	29.693210
403.896174	21988.454899	29.698228
404.098454	22032.230895	29.703245
404.929533	22066.693013	29.708263
405.225355	22109.507007	29.713280
406.083911	22138.378992	29.718298
406.690614	22175.229444	29.723316
407.275102	22206.346793	29.728333
407.927463	22237.124558	29.733351
408.145313	22272.212577	29.738368
408.879180	22284.557475	29.743386
408.954494	22308.359970	29.748404
409.403587	22330.515163	29.753421
410.160007	22348.735203	29.758439
410.180872	22379.605673	29.763456
410.464547	22397.600845	29.768474
410.924111	22418.470696	29.773492
411.210318	22450.566871	29.778509
411.482301	22478.111202	29.783527
411.822077	22519.370089	29.788544
412.188248	22536.332534	29.793562
412.889361	22568.865622	29.798580
413.513278	22599.371364	29.803597
413.688473	22626.550887	29.808615
413.897984	22659.710880	29.813632
414.131875	22681.717320	29.818650
414.610648	22707.290020	29.823668
415.045545	22744.410849	29.828685
415.521205	22778.228810	29.833703
415.705456	22818.275535	29.838720
416.447383	22842.002386	29.843738
416.786644	22884.378771	29.848756
416.781143	22923.489965	29.853773
417.426593	22957.749140	29.858791
417.774726	22989.088199	29.863808
419.116576	23011.630634	29.868826
419.676814	23031.190812	29.873844
419.865378	23048.534303	29.878861
421.143074	23060.357620	29.883879
421.825239	23075.850268	29.888896
422.875660	23056.632200	29.893914
422.954780	23064.749851	29.898932
423.504660	23079.681667	29.903949
423.907662	23086.204633	29.908967
423.825608	23098.601630	29.913984
424.393038	23094.154890	29.919002
425.072017	23111.291397	29.924020
424.945006	23125.336245	29.929037
425.242231	23124.600858	29.934055
425.184839	23149.121163	29.939072
425.458172	23163.605249	29.944090
425.927417	23191.331404	29.949108
425.902974	23225.989782	29.954125
426.492238	23250.456193	29.959143
426.596842	23282.427342	29.964160
427.036141	23310.524700	29.969178
427.593079	23346.017315	29.974196
427.752770	23384.057232	29.979213
428.139831	23417.311277	29.984231
428.111078	23457.219362	29.989248
428.808161	23489.073596	29.994266
429.126661	23537.959036	29.999284
429.167481	23582.488966	30.004301
429.896934	23622.163417	30.009319
429.924449	23666.831475	30.014336
430.569313	23699.335349	30.019354
431.753116	23731.333729	30.024372
431.898030	23763.100148	30.029389
432.515381	23787.168236	30.034407
433.112074	23818.352665	30.039424
433.462475	23849.030520	30.044442
433.860189	23871.770583	30.049460
434.552018	23898.488236	30.054477
435.136493	23922.249877	30.059495
435.287712	23947.990959	30.064512
435.556046	23973.759324	30.069530
436.349981	23994.904997	30.074548
436.423232	24037.872344	30.079565
436.874623	24069.634125	30.084583
437.298443	24097.041483	30.089600
437.757907	24124.903302	30.094618
438.158872	24163.077080	30.099636
437.935116	24198.112230	30.104653
438.943423	24240.131277	30.109671
439.092878	24275.919594	30.114688
439.255907	24314.528769	30.119706
439.871967	24355.971835	30.124724
439.968845	24407.834392	30.129741
440.656087	24446.666311	30.134759
441.350696	24485.875577	30.139776
441.430882	24527.470814	30.144794
441.605834	24573.166351	30.149812
442.145903	24624.682339	30.154829
442.716374	24669.862435	30.159847
442.787503	24724.540904	30.164864
443.633333	24767.544859	30.169882
444.252027	24805.663822	30.174900
444.836580	24855.308623	30.179917
445.110495	24901.158406	30.184935
445.531022	24943.680502	30.189952
446.086421	24985.766360	30.194970
446.526966	25044.574780	30.199988
446.607434	25084.146153	30.205005
447.325181	25130.784809	30.210023
447.493852	25175.757486	30.215040
447.793913	25222.685622	30.220058
448.249615	25279.041211	30.225076
448.453138	25335.443351	30.230093
449.305691	25380.640057	30.235111
449.699338	25446.126502	30.240128
450.294109	25482.724270	30.245146
451.233067	25524.048561	30.250164
451.660567	25574.132424	30.255181
452.657309	25597.279995	30.260199
452.920181	25639.859205	30.265216
453.332868	25672.987023	30.270234
454.019026	25710.184751	30.275252
454.410904	25736.720060	30.280269
454.740908	25770.019960	30.285287
455.115259	25812.700365	30.290304
455.476784	25846.301005	30.295322
456.159627	25874.439671	30.300340
456.158119	25911.512763	30.305357
456.160176	25940.619937	30.310375
456.298786	25984.379025	30.315392
456.988117	26022.075307	30.320410
458.418746	26053.480502	30.325428
458.311482	26098.285181	30.330445
458.837395	26140.259018	30.335463
459.310287	26176.705630	30.340480
459.811609	26208.046367	30.345498
460.297097	26245.276474	30.350516
460.655492	26287.803047	30.355533
461.029732	26321.541231	30.360551
461.545041	26356.848424	30.365568
462.027537	26395.416950	30.370586
462.710341	26438.553942	30.375604
463.029906	26484.172943	30.380621
463.565033	26503.719288	30.385639
464.185718	26544.065804	30.390656
464.755951	26583.960469	30.395674
465.471061	26612.769916	30.400692
466.125289	26651.325357	30.405709
466.879015	26676.746416	30.410727
467.260177	26704.184140	30.415744
468.144306	26737.255287	30.420762
468.740045	26747.175839	30.425780
468.797050	26784.669808	30.430797
469.397002	26800.227227	30.435815
469.425825	26823.387715	30.440832
469.513146	26853.078052	30.445850
470.141487	26883.940801	30.450868
470.309764	26929.230400	30.455885
470.478681	26956.887869	30.460903
470.680054	27002.017401	30.465920
471.239148	27051.294267	30.470938
471.783895	27087.386599	30.475956
472.547891	27122.599100	30.480973
473.316193	27150.330839	30.485991
474.301369	27183.991247	30.491008
474.666129	27223.812167	30.496026
475.289028	27247.568640	30.501044
475.545591	27283.745463	30.506061
476.122411	27300.102317	30.511079
476.716837	27340.253266	30.516096
477.292871	27361.333139	30.521114
478.213225	27374.684555	30.526132
478.434178	27405.223675	30.531149
478.701033	27430.461100	30.536167
479.114655	27447.451793	30.541184
479.264938	27478.684605	30.546202
479.624429	27506.799296	30.551220
479.996493	27538.615726	30.556237
480.285323	27574.781313	30.561255
480.790317	27610.749033	30.566272
480.980667	27660.103422	30.571290
481.170564	27691.560135	30.576308
481.401934	27736.282591	30.581325
481.764823	27782.648433	30.586343
482.420932	27829.349059	30.591360
482.821012	27873.200584	30.596378
483.431301	27919.477072	30.601396
483.417223	27973.517789	30.606413
483.812700	28021.304727	30.611431
484.238521	28064.133259	30.616448
484.549980	28127.709843	30.621466
485.082981	28177.981870	30.626484
485.365687	28241.705769	30.631501
486.253132	28296.337587	30.636519
487.098731	28344.041965	30.641536
488.211432	28381.525673	30.646554
489.276228	28413.732956	30.651572
490.003484	28452.182052	30.656589
490.565708	28491.852126	30.661607
491.041127	28506.987545	30.666624
491.354146	28535.055058	30.671642
491.973552	28566.124234	30.676660
492.464033	28596.417320	30.681677
492.805622	28637.441200	30.686695
493.417782	28666.678687	30.691712
493.040964	28709.848251	30.696730
493.742019	28741.553699	30.701748
494.050777	28792.108851	30.706765
494.391634	28835.528055	30.711783
494.857340	28882.702672	30.716800
494.933334	28940.794741	30.721818
495.441240	28989.085645	30.726836
495.092036	29048.891608	30.731853
495.941750	29105.334008	30.736871
496.333706	29166.515237	30.741888
496.433326	29243.292442	30.746906
496.934116	29298.365941	30.751924
497.872939	29367.064533	30.756941
498.398075	29434.610045	30.761959
498.883012	29499.613263	30.766976
499.226326	29569.130921	30.771994
499.719867	29623.985809	30.777012
499.998874	29699.607824	30.782029
500.985532	29758.508902	30.787047
501.589774	29829.115623	30.792064
501.800547	29888.109058	30.797082
502.788674	29938.872926	30.802100
503.473955	29996.627414	30.807117
504.551764	30044.044183	30.812135
505.756331	30082.086897	30.817152
506.505153	30120.182541	30.822170
506.509395	30155.764807	30.827188
507.144272	30196.331857	30.832205
507.371325	30237.562089	30.837223
508.219258	30274.527235	30.842240
508.869871	30316.742131	30.847258
509.518676	30341.508082	30.852276
510.041596	30377.377413	30.857293
509.877412	30405.188881	30.862311
510.634748	30428.330255	30.867328
511.104083	30462.867889	30.872346
511.874628	30494.208022	30.877364
512.089276	30529.726587	30.882381
512.548951	30562.401211	30.887399
512.967996	30596.225127	30.892416
513.017733	30634.668855	30.897434
513.523499	30675.233881	30.902452
514.226607	30717.585889	30.907469
514.190568	30775.422334	30.912487
514.631883	30813.329188	30.917504
515.108978	30877.792908	30.922522
515.319978	30930.223190	30.927540
515.670894	30993.569813	30.932557
516.270330	31050.872274	30.937575
516.304401	31109.208983	30.942592
516.620500	31179.318231	30.947610
517.409116	31245.497011	30.952628
518.328572	31303.979276	30.957645
518.396647	31367.044355	30.962663
519.213635	31427.908113	30.967680
519.637133	31513.024040	30.972698
520.501929	31578.544105	30.977716
520.839496	31645.789364	30.982733
521.781412	31694.309903	30.987751
523.389397	31732.050371	30.992768
524.029866	31778.028850	30.997786
524.957241	31819.442541	31.002804
525.132692	31854.762191	31.007821
525.442093	31893.542821	31.012839
526.140404	31923.370510	31.017856
526.762133	31969.393718	31.022874
527.267173	32012.407572	31.027892
527.749134	32040.871400	31.032909
528.704198	32075.300539	31.037927
529.620713	32100.032544	31.042944
529.711836	32143.092389	31.047962
529.969937	32175.315377	31.052980
530.283867	32213.818223	31.057997
530.277549	32264.926387	31.063015
531.097065	32309.550149	31.068032
531.375707	32366.586761	31.073050
531.624310	32411.441139	31.078068
532.340091	32466.765329	31.083085
532.255048	32517.275481	31.088103
532.977873	32576.515129	31.093120
532.961167	32641.760946	31.098138
533.283520	32710.944167	31.103156
534.052100	32780.521418	31.108173
534.250530	32852.680274	31.113191
535.220191	32915.858266	31.118208
535.590298	32988.502657	31.123226
535.962333	33044.764858	31.128244
536.509969	33109.350777	31.133261
536.725654	33177.970234	31.138279
537.347801	33232.558570	31.143296
537.599897	33311.242801	31.148314
538.085903	33372.251941	31.153332
539.161504	33440.832366	31.158349
539.369174	33510.063559	31.163367
539.924320	33583.322462	31.168384
540.903760	33651.771837	31.173402
542.092589	33710.383086	31.178420
542.913093	33773.476037	31.183437
543.244149	33827.263933	31.188455
543.726643	33872.463759	31.193472
543.976514	33938.189341	31.198490
544.279886	33995.618230	31.203508
545.095872	34053.234048	31.208525
545.393988	34119.914621	31.213543
545.848997	34174.872150	31.218560
546.426436	34250.613774	31.223578
546.944056	34326.274437	31.228596
547.496790	34386.401338	31.233613
548.067344	34453.270014	31.238631
548.915348	34513.053226	31.243648
549.649680	34574.771890	31.248666
551.409213	34596.011087	31.253684
552.363318	34639.478211	31.258701
552.712910	34694.704721	31.263719
553.807237	34730.254477	31.268736
554.055259	34762.341798	31.273754
554.720763	34799.268663	31.278772
555.313324	34834.595290	31.283789
555.482079	34874.025058	31.288807
556.272100	34917.931272	31.293824
556.730140	34949.111829	31.298842
557.146351	34989.010756	31.303860
557.983892	35028.171619	31.308877
558.220429	35067.653320	31.313895
558.505924	35104.525981	31.318912
558.774314	35154.894581	31.323930
559.511358	35199.347117	31.328948
560.386378	35234.076942	31.333965
560.374796	35295.171521	31.338983
560.685097	35335.982581	31.344000
561.017339	35397.009124	31.349018
560.974692	35461.811907	31.354036
561.834371	35518.995656	31.359053
562.071931	35581.301563	31.364071
562.836406	35659.715686	31.369088
563.237137	35726.861197	31.374106
563.916989	35788.593332	31.379124
564.539767	35853.529696	31.384141
564.822819	35925.941981	31.389159
565.508264	35979.770242	31.394176
566.304144	36033.630243	31.399194
566.697467	36095.182093	31.404212
567.879076	36155.724766	31.409229
567.817950	36212.538183	31.414247
568.800203	36262.957991	31.419264
569.064134	36325.640698	31.424282
569.747900	36379.236851	31.429300
570.750493	36423.943594	31.434317
571.091638	36490.590782	31.439335
571.775752	36529.724358	31.444352
572.271274	36601.326428	31.449370
572.723311	36648.403882	31.454388
573.640728	36695.310186	31.459405
574.290501	36743.771281	31.464423
575.507236	36781.794590	31.469440
576.518384	36819.442852	31.474458
577.109248	36867.724979	31.479476
577.803200	36904.013632	31.484493
577.866974	36952.414697	31.489511
577.912355	36987.643554	31.494528
578.742635	37035.323237	31.499546
579.113907	37089.937771	31.504564
579.869261	37129.234041	31.509581
580.538769	37181.256701	31.514599
580.863961	37222.732320	31.519616
581.108636	37276.068580	31.524634
582.043792	37335.767236	31.529652
582.881274	37378.099266	31.534669
582.991610	37437.074651	31.539687
583.205565	37495.199118	31.544704
584.058368	37542.222839	31.549722
584.634079	37617.192769	31.554740
584.965323	37652.718004	31.559757
585.060581	37725.965075	31.564775
585.874109	37797.801444	31.569792
586.221439	37857.135319	31.574810
586.876294	37928.273341	31.579828
587.490923	37997.439258	31.584845
588.135659	38069.409781	31.589863
588.519457	38140.509832	31.594880
589.414512	38208.608867	31.599898
590.113053	38278.667458	31.604916
590.999113	38329.387249	31.609933
591.593531	38388.718387	31.614951
592.273395	38451.659097	31.619968
593.142690	38504.228977	31.624986
593.360239	38567.192465	31.630004
593.989276	38623.866692	31.635021
594.570457	38694.212147	31.640039
595.031351	38748.570023	31.645056
595.894372	38809.627499	31.650074
596.054151	38876.437540	31.655092
596.570520	38944.869356	31.660109
597.034112	39013.427273	31.665127
597.638686	39073.197684	31.670144
598.430626	39140.806412	31.675162
598.247196	39211.448994	31.680180
599.133772	39272.598675	31.685197
599.400538	39342.934171	31.690215
599.891333	39421.354454	31.695232
600.647765	39477.043439	31.700250
602.428334	39517.738200	31.705268
604.173544	39556.156598	31.710285
604.385266	39599.115544	31.715303
604.896110	39644.536327	31.720320
605.669324	39691.828585	31.725338
606.135252	39747.909116	31.730356
606.943655	39777.970803	31.735373
607.207378	39834.660820	31.740391
607.149116	39890.414858	31.745408
607.969289	39940.411618	31.750426
608.466300	40006.969068	31.755444
608.626394	40060.656207	31.760461
609.380247	40123.523638	31.765479
609.892712	40187.837551	31.770496
610.442997	40252.334634	31.775514
610.622097	40318.117342	31.780532
611.244820	40385.263936	31.785549
611.678346	40469.378159	31.790567
612.154892	40540.585203	31.795584
612.840840	40613.925625	31.800602
613.587288	40695.979296	31.805620
614.134919	40771.973981	31.810637
614.675576	40853.327972	31.815655
615.191087	40939.109912	31.820672
615.763521	41012.329276	31.825690
616.248832	41087.593971	31.830708
617.428210	41168.022179	31.835725
617.821290	41248.023446	31.840743
618.076856	41336.746980	31.845760
618.931863	41415.429007	31.850778
619.607880	41504.583318	31.855796
620.106532	41584.747908	31.860813
620.619145	41670.461084	31.865831
621.044995	41750.133677	31.870848
621.943366	41835.216350	31.875866
622.416289	41925.834601	31.880884
623.044124	42011.687469	31.885901
623.624536	42091.224523	31.890919
624.153151	42188.790321	31.895936
624.945691	42265.235365	31.900954
625.911683	42348.761632	31.905972
626.916206	42426.272974	31.910989
627.747497	42504.240577	31.916007
628.442737	42580.845665	31.921024
629.305297	42654.905853	31.926042
629.250770	42721.993732	31.931060
630.228254	42801.699430	31.936077
630.689978	42872.201122	31.941095
631.044485	42951.527917	31.946112
632.522783	43000.652842	31.951130
633.257000	43069.791881	31.956148
633.806397	43122.451728	31.961165
634.204614	43193.855949	31.966183
634.362915	43262.014454	31.971200
635.097331	43321.965697	31.976218
635.182512	43409.263068	31.981236
635.969955	43474.592664	31.986253
636.522272	43551.308285	31.991271
636.733470	43641.158642	31.996288
637.346791	43723.273632	32.001306
637.990106	43811.023523	32.006324
638.452147	43896.638672	32.011341
638.928454	43991.270288	32.016359
639.765119	44082.521834	32.021376
640.768200	44171.174879	32.026394
641.046321	44248.723432	32.031412
642.345811	44330.834032	32.036429
643.373789	44398.386602	32.041447
643.793268	44496.472497	32.046464
644.465766	44572.284318	32.051482
645.047135	44655.627755	32.056500
645.338316	44734.811828	32.061517
645.947967	44822.780591	32.066535
646.350441	44919.058955	32.071552
646.912646	44999.375597	32.076570
647.561776	45102.433729	32.081588
648.220929	45196.405286	32.086605
648.759547	45287.931587	32.091623
649.096211	45393.400664	32.096640
649.959294	45486.489220	32.101658
650.773475	45581.828796	32.106676
651.713322	45658.300225	32.111693
653.092384	45736.098887	32.116711
654.622332	45805.108433	32.121728
655.513874	45870.681096	32.126746
656.509624	45948.221012	32.131764
657.332950	46009.466650	32.136781
658.048803	46066.751699	32.141799
657.864697	46132.490585	32.146816
658.512711	46192.402542	32.151834
659.100666	46259.834992	32.156852
659.528973	46324.566400	32.161869
660.062656	46394.039300	32.166887
660.707107	46468.827604	32.171904
661.538470	46541.427150	32.176922
661.932492	46628.844290	32.181940
662.323442	46707.684690	32.186957
662.771474	46783.284786	32.191975
663.824414	46863.983145	32.196992
664.422929	46948.006359	32.202010
665.353505	47014.027886	32.207028
666.053809	47082.015626	32.212045
667.495720	47146.257186	32.217063
667.701270	47213.865884	32.222080
668.560424	47276.492766	32.227098
669.072363	47340.783751	32.232116
670.078644	47407.709572	32.237133
670.878414	47458.557246	32.242151
671.440582	47519.337647	32.247168
672.395773	47566.008936	32.252186
672.928084	47614.692007	32.257204
673.691627	47669.841798	32.262221
674.491489	47710.712884	32.267239
675.053936	47775.179855	32.272256
675.570091	47819.962465	32.277274
676.166140	47881.243546	32.282292
676.801946	47935.787463	32.287309
677.505322	47986.204555	32.292327
678.059467	48051.236068	32.297344
678.770583	48112.311826	32.302362
679.185603	48179.212124	32.307380
679.514918	48243.474240	32.312397
680.332689	48309.064724	32.317415
680.457556	48392.275222	32.322432
681.404176	48465.168665	32.327450
681.615422	48543.987358	32.332468
682.273169	48630.929379	32.337485
682.719313	48705.147598	32.342503
682.945112	48799.858538	32.347520
683.694957	48887.146006	32.352538
684.879597	48973.279154	32.357556
686.059500	49050.961134	32.362573
687.165337	49117.999024	32.367591
687.791745	49199.440383	32.372608
688.286410	49270.190624	32.377626
689.275549	49345.625945	32.382644
689.806768	49422.277114	32.387661
690.872218	49495.362551	32.392679
691.197101	49572.232860	32.397696
692.328278	49638.870220	32.402714
693.159000	49703.708288	32.407732
693.793357	49772.983434	32.412749
694.553101	49830.032101	32.417767
695.153906	49899.938872	32.422784
695.927136	49971.136706	32.427802
696.499797	50041.661600	32.432820
696.968945	50122.641003	32.437837
697.358481	50195.983846	32.442855
698.116925	50265.296346	32.447872
698.480870	50353.193498	32.452890
699.035852	50433.837292	32.457908
699.443440	50528.367565	32.462925
700.293189	50610.477827	32.467943
700.661357	50715.168247	32.472960
701.196886	50802.677919	32.477978
701.819161	50891.512486	32.482996
702.384925	50993.460228	32.488013
703.303578	51090.236932	32.493031
704.070593	51188.158351	32.498048
704.241833	51282.486354	32.503066
705.130231	51374.423829	32.508084
705.520975	51471.640333	32.513101
706.403469	51558.095706	32.518119
706.901778	51671.146567	32.523136
707.598235	51763.775819	32.528154
708.284895	51852.805887	32.533172
708.628550	51960.817817	32.538189
709.338095	52060.503543	32.543207
709.492028	52184.755216	32.548224
710.249337	52293.582655	32.553242
711.009601	52416.468281	32.558260
711.511718	52523.773779	32.563277
712.625156	52645.267175	32.568295
713.357332	52752.408140	32.573312
714.255301	52861.934910	32.578330
715.302169	52974.817138	32.583348
715.702684	53093.453117	32.588365
716.783470	53192.505986	32.593383
718.469410	53281.516652	32.598400
719.597448	53371.577388	32.603418
720.641629	53452.244535	32.608436
722.156429	53530.417690	32.613453
722.924016	53594.565430	32.618471
724.013081	53665.261293	32.623488
724.747822	53725.276372	32.628506
725.993235	53782.373387	32.633524
726.546341	53857.989220	32.638541
727.277506	53916.299439	32.643559
727.716115	53985.212248	32.648576
728.212367	54045.010078	32.653594
729.096660	54112.406305	32.658612
729.288605	54190.018816	32.663629
730.243194	54249.757707	32.668647
730.682035	54323.385496	32.673664
731.513364	54395.796289	32.678682
732.373088	54464.423781	32.683700
733.114520	54547.333581	32.688717
733.743466	54623.211046	32.693735
733.968798	54695.657226	32.698752
734.296173	54773.394145	32.703770
735.204750	54858.848441	32.708788
735.542107	54945.374083	32.713805
736.120810	55036.496962	32.718823
736.957640	55136.561815	32.723840
737.301032	55242.272538	32.728858
737.965904	55326.645772	32.733876
737.999431	55442.919415	32.738893
738.460962	55553.932319	32.743911
739.360222	55665.736597	32.748928
739.690099	55787.440288	32.753946
740.636647	55906.637729	32.758964
741.621554	56013.057823	32.763981
743.148757	56110.772222	32.768999
744.531690	56206.129379	32.774016
745.525174	56291.164480	32.779034
746.375263	56369.292012	32.784052
746.638873	56465.214980	32.789069
747.629749	56550.049398	32.794087
748.023217	56635.454155	32.799104
748.444047	56723.692090	32.804122
749.040475	56815.237102	32.809140
749.619841	56916.106963	32.814157
750.441145	57006.830686	32.819175
750.820249	57116.577112	32.824192
752.079966	57219.310026	32.829210
753.143873	57312.622591	32.834228
754.062228	57405.575009	32.839245
754.264440	57496.653450	32.844263
755.035459	57590.181780	32.849280
755.729173	57687.142856	32.854298
757.135864	57785.347378	32.859316
757.398020	57885.992013	32.864333
758.081364	57988.170284	32.869351
758.905165	58087.455714	32.874368
759.165262	58201.576586	32.879386
760.363385	58300.640939	32.884404
761.106286	58399.265500	32.889421
761.995199	58497.018628	32.894439
763.170809	58608.317857	32.899456
763.756644	58702.199043	32.904474
764.594492	58802.635842	32.909492
765.073048	58904.354494	32.914509
765.845398	59003.413038	32.919527
766.523580	59108.334518	32.924544
766.729016	59224.973343	32.929562
767.737282	59340.148030	32.934580
768.195136	59462.256383	32.939597
768.688745	59579.062762	32.944615
769.237197	59704.740765	32.949632
769.712217	59829.977035	32.954650
770.701364	59949.355288	32.959668
771.623772	60077.575616	32.964685
772.877417	60187.277280	32.969703
773.906326	60300.450177	32.974720
774.589439	60420.186985	32.979738
775.945723	60522.073048	32.984756
776.242964	60656.288726	32.989773
777.115066	60757.336048	32.994791
778.231279	60869.005400	32.999808
778.769390	60989.781702	33.004826
779.272836	61106.026195	33.009844
780.337360	61218.268859	33.014861
781.447466	61326.224987	33.019879
782.346606	61431.133134	33.024896
783.269913	61540.121105	33.029914
784.348419	61634.430688	33.034932
785.409658	61730.355555	33.039949
786.643422	61822.193115	33.044967
787.906962	61899.588337	33.049984
788.868057	61979.943421	33.055002
789.761518	62046.087575	33.060020
790.543804	62125.626803	33.065037
791.451881	62182.723145	33.070055
792.010993	62253.053035	33.075072
792.436510	62330.612373	33.080090
793.223008	62396.567364	33.085108
793.883477	62479.074568	33.090125
794.530745	62556.546198	33.095143
795.062225	62613.139302	33.100160
796.149282	62691.964752	33.105178
796.820465	62769.173899	33.110196
797.135554	62860.528625	33.115213
797.847292	62951.822135	33.120231
798.301985	63041.465895	33.125248
798.808875	63140.634050	33.130266
799.535665	63249.026182	33.135284
799.820096	63359.391140	33.140301
800.842016	63462.796623	33.145319
801.549108	63565.491615	33.150336
802.223057	63684.136237	33.155354
802.865226	63798.924364	33.160372
803.315261	63919.005784	33.165389
803.969297	64045.520213	33.170407
804.790911	64169.686566	33.175424
805.304875	64295.815574	33.180442
806.506693	64424.975867	33.185460
807.020281	64562.682079	33.190477
808.028485	64688.627641	33.195495
809.002907	64815.281496	33.200512
809.764042	64950.374757	33.205530
810.515149	65067.515641	33.210548
811.151337	65210.446170	33.215565
812.288199	65332.460103	33.220583
813.590944	65452.707702	33.225600
814.329755	65573.899767	33.230618
815.306520	65695.058094	33.235636
815.936386	65828.655777	33.240653
816.956520	65942.316057	33.245671
818.030287	66058.528360	33.250688
818.679606	66175.914113	33.255706
820.022785	66292.214328	33.260724
821.058756	66390.991069	33.265741
821.927100	66501.089133	33.270759
823.034907	66606.556527	33.275776
823.411203	66730.011252	33.280794
824.184174	66834.278916	33.285812
825.393465	66925.687815	33.290829
826.617497	67031.542069	33.295847
827.735379	67128.860305	33.300864
828.082125	67230.718062	33.305882
828.891432	67328.614856	33.310900
830.142464	67416.079586	33.315917
831.111082	67514.089050	33.320935
832.525431	67609.417579	33.325952
833.164729	67699.934732	33.330970
833.657610	67771.381962	33.335988
834.570666	67856.712316	33.341005
834.807788	67948.797955	33.346023
835.567282	68036.241926	33.351040
836.033316	68138.905580	33.356058
836.389741	68234.639401	33.361076
837.401545	68338.645883	33.366093
837.913604	68443.756493	33.371111
838.455317	68549.058558	33.376128
839.203065	68671.828566	33.381146
839.912891	68787.675463	33.386164
840.823405	68902.925839	33.391181
841.263705	69029.190424	33.396199
842.104519	69149.544350	33.401216
842.581838	69283.151848	33.406234
843.849273	69410.396248	33.411252
844.515735	69532.729800	33.416269
845.161481	69666.867296	33.421287
846.031821	69804.337621	33.426304
846.601002	69944.339255	33.431322
847.226625	70080.879414	33.436340
848.431024	70217.947353	33.441357
849.093453	70369.786366	33.446375
849.914095	70504.152047	33.451392
850.947004	70659.818759	33.456410
851.748996	70789.939798	33.461428
853.079775	70937.102488	33.466445
853.675837	71076.322660	33.471463
854.443173	71209.999879	33.476480
855.426886	71358.597165	33.481498
856.194903	71487.722676	33.486516
857.461133	71629.892452	33.491533
857.953852	71777.583801	33.496551
858.664347	71911.584937	33.501568
859.547410	72064.827248	33.506586
860.654506	72215.382393	33.511604
861.311703	72349.382690	33.516621
861.630440	72513.318006	33.521639
862.676811	72665.012375	33.526656
863.589326	72803.778263	33.531674
864.672692	72954.924398	33.536692
865.960676	73105.113147	33.541709
866.590276	73254.707329	33.546727
867.679315	73405.963109	33.551744
868.703806	73553.695500	33.556762
869.500039	73693.732871	33.561780
870.977697	73826.722518	33.566797
871.520362	73972.124182	33.571815
872.486210	74110.142840	33.576832
873.477000	74252.376764	33.581850
874.402682	74389.600788	33.586868
875.026238	74524.720602	33.591885
876.175997	74656.500086	33.596903
877.279646	74793.354580	33.601920
878.125603	74920.677933	33.606938
878.689315	75054.710663	33.611956
879.658673	75183.867638	33.616973
880.487018	75306.578879	33.621991
881.556020	75421.615081	33.627008
882.502755	75546.932323	33.632026
883.555301	75662.750590	33.637044
884.690105	75778.498444	33.642061
885.893335	75896.265607	33.647079
887.373401	75995.003602	33.652096
887.897287	76111.053892	33.657114
888.568330	76213.663382	33.662132
889.446451	76325.194702	33.667149
890.246694	76450.814098	33.672167
891.233436	76556.552808	33.677184
892.074463	76676.207855	33.682202
892.699030	76795.375588	33.687220
893.550206	76910.747734	33.692237
894.235102	77038.502925	33.697255
895.216525	77146.155667	33.702272
896.472628	77282.075748	33.707290
896.914532	77403.049181	33.712308
898.192250	77526.638163	33.717325
898.619238	77658.736246	33.722343
899.823855	77774.324297	33.727360
901.119531	77888.410763	33.732378
902.237150	78007.019699	33.737396
903.455529	78126.212967	33.742413
904.147140	78242.738948	33.747431
905.288815	78353.204046	33.752448
905.643244	78476.646372	33.757466
906.713258	78596.917650	33.762484
907.938840	78709.989115	33.767501
908.393743	78840.798785	33.772519
909.169105	78952.626396	33.777536
910.466170	79061.752489	33.782554
911.112533	79182.871221	33.787572
912.076086	79303.948929	33.792589
912.673023	79437.799622	33.797607
913.807922	79558.064874	33.802624
914.584470	79682.915490	33.807642
915.170937	79809.032992	33.812660
916.002358	79937.500639	33.817677
916.621275	80075.343294	33.822695
917.555249	80216.390985	33.827712
918.626605	80345.034931	33.832730
919.424448	80482.881028	33.837748
921.198704	80610.336895	33.842765
921.616743	80746.864088	33.847783
923.144080	80865.253249	33.852800
924.294949	80986.820248	33.857818
925.039048	81114.411045	33.862836
926.289964	81234.298278	33.867853
926.808930	81360.910378	33.872871
927.848304	81463.727258	33.877888
929.028260	81574.289954	33.882906
929.823047	81688.816531	33.887924
930.902174	81795.614051	33.892941
932.010584	81906.412035	33.897959
932.606802	82008.864345	33.902976
933.314478	82132.341790	33.907994
934.014866	82243.571905	33.913012
935.110070	82351.198085	33.918029
935.308647	82482.844305	33.923047
935.923976	82609.459389	33.928064
936.697506	82741.065555	33.933082
937.423306	82884.348100	33.938100
938.025149	83020.806620	33.943117
938.380479	83172.658266	33.948135
939.088327	83330.942422	33.953152
939.892575	83484.395975	33.958170
940.678722	83666.004530	33.963188
941.314897	83827.025132	33.968205
941.969557	84001.654254	33.973223
943.099707	84177.804133	33.978240
943.938053	84364.300405	33.983258
944.478586	84558.189299	33.988276
945.820092	84731.295148	33.993293
946.589146	84921.420854	33.998311
947.520136	85096.839736	34.003328
948.949739	85278.622670	34.008346
949.462569	85470.252095	34.013364
951.285802	85637.055397	34.018381
952.059478	85824.321000	34.023399
953.096878	86004.063109	34.028416
954.083608	86179.366573	34.033434
955.207035	86357.571548	34.038452
956.197180	86532.541640	34.043469
957.008020	86724.598458	34.048487
958.191643	86902.657987	34.053504
959.637361	87069.498042	34.058522
960.498344	87246.830674	34.063540
961.801648	87405.647710	34.068557
963.510455	87569.370573	34.073575
964.487973	87730.776965	34.078592
965.325347	87892.986861	34.083610
966.185809	88058.706296	34.088628
967.343234	88211.851558	34.093645
967.936424	88382.624985	34.098663
969.278178	88538.962090	34.103680
970.266696	88700.512351	34.108698
970.733888	88871.709538	34.113716
971.478576	89033.879713	34.118733
972.169715	89205.319388	34.123751
973.507464	89373.687586	34.128768
974.025301	89549.279547	34.133786
974.859270	89733.084422	34.138804
975.874268	89903.505233	34.143821
976.666846	90083.712252	34.148839
977.860862	90250.883298	34.153856
979.285113	90421.326271	34.158874
980.488413	90592.339936	34.163892
981.828077	90736.906436	34.168909
982.879194	90885.137280	34.173927
983.865284	91030.057215	34.178944
985.262012	91174.065876	34.183962
986.016426	91337.724524	34.188980
987.135523	91469.864029	34.193997
987.639852	91624.579485	34.199015
988.866071	91776.235363	34.204032
990.113676	91907.317164	34.209050
991.055381	92073.955236	34.214068
992.176060	92219.302237	34.219085
992.893317	92371.371758	34.224103
993.939743	92524.215056	34.229120
994.657088	92677.894222	34.234138
995.491399	92841.112439	34.239156
996.657854	92988.551329	34.244173
997.522992	93151.044702	34.249191
998.356686	93312.531726	34.254208
999.942437	93458.477367	34.259226
1000.841219	93617.157352	34.264244
1001.934968	93769.664748	34.269261
1003.266366	93924.588489	34.274279
1004.208562	94085.346652	34.279296
1005.091294	94242.988897	34.284314
1005.791000	94401.296508	34.289332
1006.792757	94555.255113	34.294349
1007.878375	94718.259053	34.299367
1008.217938	94879.309104	34.304384
1009.593792	95046.481533	34.309402
1010.123218	95230.442869	34.314420
1010.786372	95404.108196	34.319437
1012.030622	95584.505915	34.324455
1013.583439	95751.070325	34.329472
1014.596542	95917.734587	34.334490
1015.752012	96095.504956	34.339508
1016.848979	96248.767603	34.344525
1018.117713	96412.396921	34.349543
1018.946235	96587.282922	34.354560
1020.032663	96748.432292	34.359578
1020.900618	96926.359033	34.364596
1021.783613	97098.061115	34.369613
1022.583347	97279.667640	34.374631
1023.428825	97451.125292	34.379648
1024.049562	97631.688703	34.384666
1025.113502	97820.699215	34.389684
1026.008062	98012.373903	34.394701
1027.073615	98203.343309	34.399719
1027.922581	98403.677206	34.404736
1029.067190	98587.411951	34.409754
1029.798615	98784.286721	34.414772
1030.918096	98979.190795	34.419789
1031.862364	99174.417597	34.424807
1032.545704	99376.009417	34.429824
1033.808592	99558.426562	34.434842
1034.650049	99754.124903	34.439860
1036.076309	99935.560668	34.444877
1037.216761	100113.754159	34.449895
1038.345783	100303.170692	34.454912
1039.836784	100469.478905	34.459930
1040.769662	100648.091524	34.464948
1042.067499	100815.600089	34.469965
1043.159719	100989.533845	34.474983
1044.239376	101163.141653	34.480000
1045.622462	101330.347667	34.485018
1046.562312	101506.128247	34.490036
1047.495111	101678.694518	34.495053
1048.434273	101855.414714	34.500071
1049.307146	102037.567790	34.505088
1050.434094	102214.992790	34.510106
1051.385609	102396.539667	34.515124
1052.515210	102562.935777	34.520141
1053.269015	102754.587333	34.525159
1054.136802	102943.485176	34.530176
1055.954107	103134.982734	34.535194
1056.731967	103325.545144	34.540212
1057.575142	103499.633182	34.545229
1058.715583	103680.345990	34.550247
1059.673936	103882.444771	34.555264
1061.169889	104059.173071	34.560282
1061.686812	104247.962989	34.565300
1062.946934	104434.663842	34.570317
1064.367566	104620.971222	34.575335
1065.476585	104822.722047	34.580352
1066.447253	104998.875249	34.585370
1067.298567	105198.101887	34.590388
1068.091864	105383.901376	34.595405
1069.059405	105585.682182	34.600423
1070.223693	105790.052707	34.605440
1071.533638	105985.229501	34.610458
1072.287864	106187.292007	34.615476
1073.163266	106390.918582	34.620493
1074.555375	106589.999612	34.625511
1075.408528	106797.369682	34.630528
1076.386943	106996.980541	34.635546
1077.218514	107216.162876	34.640564
1078.063497	107429.745916	34.645581
1079.310668	107637.890966	34.650599
1080.256206	107851.054754	34.655616
1081.783628	108058.445679	34.660634
1082.743009	108275.385238	34.665652
1083.980778	108477.977373	34.670669
1085.622611	108676.904263	34.675687
1086.759005	108876.501847	34.680704
1088.366644	109066.456116	34.685722
1089.467905	109262.832274	34.690740
1090.714394	109464.277439	34.695757
1091.867765	109643.419134	34.700775
1092.971219	109845.638985	34.705792
1094.108667	110026.078029	34.710810
1095.093337	110201.971196	34.715828
1095.937457	110383.412906	34.720845
1097.358623	110547.718089	34.725863
1098.419019	110735.674604	34.730880
1099.626940	110903.679580	34.735898
1100.239138	111083.835383	34.740916
1101.505214	111272.507757	34.745933
1102.568552	111444.151318	34.750951
1103.393267	111637.652507	34.755968
1105.277250	111804.482980	34.760986
1106.484128	111983.681286	34.766004
1107.670943	112156.663662	34.771021
1108.955900	112326.310986	34.776039
1109.896078	112499.363040	34.781056
1111.688415	112659.372917	34.786074
1112.653380	112826.176778	34.791092
1113.844797	112996.642331	34.796109
1115.023129	113159.484106	34.801127
1115.917066	113334.703023	34.806144
1117.007357	113493.368159	34.811162
1118.223338	113669.610934	34.816180
1118.606510	113848.480675	34.821197
1119.550638	114016.967541	34.826215
1120.615332	114210.394623	34.831232
1121.713963	114388.765168	34.836250
1122.971505	114572.747837	34.841268
1123.980557	114764.427055	34.846285
1125.679163	114946.347392	34.851303
1126.202596	115140.494291	34.856320
1126.906121	115327.338813	34.861338
1128.203693	115524.003899	34.866356
1129.034390	115710.436353	34.871373
1130.122128	115911.397351	34.876391
1130.955892	116122.958031	34.881408
1132.171253	116335.823388	34.886426
1133.079980	116541.634372	34.891444
1133.989932	116762.208448	34.896461
1135.293914	116959.832552	34.901479
1136.104394	117178.488128	34.906496
1137.781147	117394.690844	34.911514
1139.028639	117608.142919	34.916532
1140.292863	117828.753128	34.921549
1141.364558	118045.545779	34.926567
1142.514071	118251.378313	34.931584
1144.669757	118426.678309	34.936602
1146.959413	118599.840211	34.941620
1148.552948	118771.867788	34.946637
1150.552589	118926.808283	34.951655
1151.987183	119096.672710	34.956672
1153.275385	119250.228726	34.961690
1154.947042	119386.194176	34.966708
1156.070930	119543.530834	34.971725
1157.044819	119678.387874	34.976743
1157.634707	119845.473906	34.981760
1158.324470	119990.303530	34.986778
1159.289031	120142.817080	34.991796
1160.059519	120297.873820	34.996813
1160.855143	120450.506579	35.001831
1161.481766	120600.127589	35.006848
1162.358194	120779.361009	35.011866
1163.220670	120952.109362	35.016884
1164.062755	121134.886536	35.021901
1164.936266	121314.440486	35.026919
1165.300305	121507.592303	35.031936
1166.272031	121705.812002	35.036954
1167.152198	121915.986945	35.041972
1167.871035	122126.038893	35.046989
1169.172371	122351.226122	35.052007
1169.795677	122583.501586	35.057024
1170.733788	122801.467033	35.062042
1171.792376	123037.955165	35.067060
1172.648529	123287.787377	35.072077
1173.566577	123531.958442	35.077095
1174.862040	123780.705567	35.082112
1176.003641	124027.846086	35.087130
1177.898603	124272.020586	35.092148
1178.421993	124533.162052	35.097165
1179.773728	124781.692206	35.102183
1180.895393	125042.545454	35.107200
1182.204981	125295.637157	35.112218
1183.690829	125549.549971	35.117236
1184.573164	125799.993856	35.122253
1185.814469	126054.358267	35.127271
1187.208940	126316.886676	35.132288
1188.669651	126572.599353	35.137306
1189.707595	126829.932893	35.142324
1190.922101	127098.620878	35.147341
1192.156939	127348.547860	35.152359
1193.187485	127626.182771	35.157376
1194.522438	127879.189695	35.162394
1195.562323	128136.406849	35.167412
1197.072710	128400.960995	35.172429
1198.479982	128652.808220	35.177447
1200.043295	128898.850396	35.182464
1202.075635	129140.719749	35.187482
1204.028778	129377.064927	35.192500
1205.796200	129615.471885	35.197517
1207.222423	129828.028165	35.202535
1208.624033	130046.395967	35.207552
1210.208667	130255.403862	35.212570
1211.560120	130456.808930	35.217588
1212.184128	130676.378983	35.222605
1213.556914	130883.310186	35.227623
1214.692094	131105.686001	35.232640
1215.288772	131324.783412	35.237658
1216.755158	131540.678210	35.242676
1217.713166	131772.546136	35.247693
1218.679611	131982.748604	35.252711
1219.545114	132221.899710	35.257728
1220.288996	132456.167166	35.262746
1221.583560	132667.623664	35.267764
1222.559282	132900.929146	35.272781
1223.818302	133124.907615	35.277799
1224.954203	133352.331725	35.282816
1226.008367	133579.746040	35.287834
1227.089322	133805.547219	35.292852
1228.058933	134052.414784	35.297869
1228.835659	134294.068399	35.302887
1230.082587	134547.839876	35.307904
1230.940847	134798.941273	35.312922
1232.161840	135053.570500	35.317940
1233.169529	135319.332016	35.322957
1234.230483	135576.388888	35.327975
1235.819528	135851.500787	35.332992
1236.885924	136105.593921	35.338010
1238.060697	136372.286086	35.343028
1238.993465	136655.276478	35.348045
1240.581346	136918.707083	35.353063
1242.261413	137185.889727	35.358080
1243.151034	137457.317929	35.363098
1244.924806	137732.045785	35.368116
1246.333301	137991.356501	35.373133
1248.080851	138254.060037	35.378151
1249.348962	138511.205118	35.383168
1250.887388	138772.414155	35.388186
1252.290535	139027.359024	35.393204
1253.323174	139293.794009	35.398221
1254.576356	139540.488196	35.403239
1256.431522	139795.183820	35.408256
1258.184715	140036.216593	35.413274
1259.958521	140270.615602	35.418292
1261.418937	140504.017343	35.423309
1263.056795	140733.548025	35.428327
1264.430496	140966.333659	35.433344
1265.259208	141197.413446	35.438362
1266.623475	141434.946432	35.443380
1267.666839	141670.519669	35.448397
1268.705853	141897.662294	35.453415
1270.245483	142135.055838	35.458432
1271.036136	142367.608125	35.463450
1272.527466	142609.819307	35.468468
1273.453951	142860.688791	35.473485
1274.396883	143098.622070	35.478503
1275.822267	143352.858980	35.483520
1276.748078	143597.177349	35.488538
1278.153319	143839.677907	35.493556
1279.469258	144093.444200	35.498573
1280.601368	144348.283664	35.503591
1281.878963	144595.034237	35.508608
1282.798717	144863.052270	35.513626
1284.167483	145120.393075	35.518644
1285.605788	145383.265967	35.523661
1287.149680	145630.662824	35.528679
1288.486769	145890.335356	35.533696
1289.161988	146151.480056	35.538714
1290.736964	146390.480846	35.543732
1292.174204	146626.031690	35.548749
1293.345186	146880.374836	35.553767
1294.988867	147109.577374	35.558784
1295.410028	147348.743809	35.563802
1297.028657	147598.487424	35.568820
1298.345634	147848.880456	35.573837
1299.642862	148085.758206	35.578855
1300.764066	148337.037793	35.583872
1301.617014	148605.779310	35.588890
1303.093621	148859.398722	35.593908
1304.284524	149125.511347	35.598925
1305.253038	149388.848133	35.603943
1306.509943	149650.272870	35.608960
1307.443863	149932.873317	35.613978
1308.744287	150211.481099	35.618996
1309.809711	150493.200676	35.624013
1311.234628	150781.380442	35.629031
1312.274314	151077.695485	35.634048
1312.941765	151376.892444	35.639066
1314.456382	151673.067345	35.644084
1315.353373	151982.186978	35.649101
1316.721635	152291.241088	35.654119
1318.083018	152598.142421	35.659136
1319.628133	152910.786317	35.664154
1321.123378	153210.971947	35.669172
1322.765560	153522.690787	35.674189
1324.640078	153822.549777	35.679207
1325.967714	154134.327284	35.684224
1327.397031	154440.546347	35.689242
1328.990859	154737.352393	35.694260
1330.216283	155036.405613	35.699277
1331.276687	155337.671237	35.704295
1333.160669	155628.294390	35.709312
1334.474527	155931.411252	35.714330
1335.455076	156233.788227	35.719348
1336.613052	156541.109998	35.724365
1338.251316	156840.080557	35.729383
1339.704727	157139.478222	35.734400
1341.104526	157443.619235	35.739418
1343.074931	157719.818274	35.744436
1344.394699	158019.295985	35.749453
1346.114988	158306.084209	35.754471
1348.145767	158582.253322	35.759488
1350.052013	158848.055179	35.764506
1351.916813	159111.214292	35.769524
1352.920912	159378.417249	35.774541
1354.562465	159629.375017	35.779559
1355.931423	159882.981782	35.784576
1357.023788	160152.521664	35.789594
1358.508261	160413.039008	35.794612
1360.112278	160666.508760	35.799629
1361.261437	160933.113142	35.804647
1362.586756	161179.351130	35.809664
1363.716535	161439.427988	35.814682
1364.961490	161685.784153	35.819700
1365.996653	161945.207838	35.824717
1366.916004	162198.410559	35.829735
1367.941689	162445.747501	35.834752
1369.118517	162719.349229	35.839770
1370.416249	162996.560743	35.844788
1371.685202	163258.477199	35.849805
1372.284947	163547.256277	35.854823
1373.530027	163826.068091	35.859840
1374.483272	164118.368499	35.864858
1376.067453	164406.007745	35.869876
1377.376943	164705.686451	35.874893
1378.674487	165008.008444	35.879911
1380.275096	165311.815945	35.884928
1380.801254	165624.628057	35.889946
1382.397554	165917.591585	35.894964
1384.251875	166227.427125	35.899981
1385.440079	166542.593965	35.904999
1386.872905	166847.874440	35.910016
1388.122580	167157.540688	35.915034
1389.702448	167466.492693	35.920052
1391.354682	167781.322241	35.925069
1392.837261	168082.643414	35.930087
1394.885341	168388.869429	35.935104
1396.494585	168697.367879	35.940122
1398.015330	168980.415435	35.945140
1399.650012	169278.317559	35.950157
1401.491544	169580.348439	35.955175
1402.776977	169876.816762	35.960192
1404.130256	170166.575051	35.965210
1405.729112	170457.333677	35.970228
1407.242776	170744.327022	35.975245
1408.480213	171041.470769	35.980263
1409.845542	171338.492963	35.985280
1411.246971	171635.904228	35.990298
1412.533868	171932.867397	35.995316
1413.434455	172222.677620	36.000333
1414.412558	172535.560482	36.005351
1416.085410	172846.549771	36.010368
1417.226349	173174.003148	36.015386
1418.493890	173480.014933	36.020404
1420.213490	173800.291992	36.025421
1421.740231	174113.852538	36.030439
1423.560264	174414.597666	36.035456
1425.320627	174725.837722	36.040474
1426.942179	175026.455545	36.045492
1428.838571	175317.738113	36.050509
1429.886385	175622.823523	36.055527
1431.950559	175909.753058	36.060544
1433.221193	176211.821414	36.065562
1434.671493	176494.798045	36.070580
1436.031816	176784.518235	36.075597
1437.300954	177077.466688	36.080615
1438.981685	177358.263774	36.085632
1440.530116	177659.848956	36.090650
1441.843183	177932.411607	36.095668
1443.116190	178209.424757	36.100685
1444.189725	178478.363280	36.105703
1445.940349	178763.598268	36.110720
1446.765630	179038.775936	36.115738
1448.114689	179319.526169	36.120756
1450.119590	179610.459162	36.125773
1450.987681	179893.439770	36.130791
1452.306594	180191.943811	36.135808
1453.428702	180494.011739	36.140826
1454.873033	180793.614628	36.145844
1456.309334	181097.066455	36.150861
1457.456869	181405.989227	36.155879
1458.988756	181697.344541	36.160896
1460.335728	182012.722687	36.165914
1462.248592	182317.051756	36.170932
1464.459932	182611.570471	36.175949
1465.723986	182925.102181	36.180967
1467.432161	183220.801872	36.185984
1468.749087	183517.610944	36.191002
1470.276241	183820.427651	36.196020
1472.056079	184114.456998	36.201037
1473.446200	184434.258869	36.206055
1474.965453	184730.100423	36.211072
1476.066497	185041.107797	36.216090
1477.349756	185359.993855	36.221108
1478.676212	185666.624827	36.226125
1479.535785	185994.345613	36.231143
1481.203286	186318.794608	36.236160
1482.605936	186661.201937	36.241178
1483.445225	187005.370609	36.246196
1485.035506	187406.003207	36.251213
1486.248228	187732.086570	36.256231
1488.092117	188074.858247	36.261248
1489.889339	188423.606235	36.266266
1491.410941	188756.218036	36.271284
1492.998036	189097.351174	36.276301
1493.953663	189432.754803	36.281319
1495.508752	189775.674485	36.286336
1497.075437	190123.862417	36.291354
1498.710948	190471.900909	36.296372
1500.406644	190817.772946	36.301389
1501.680101	191172.973771	36.306407
1503.332706	191505.793943	36.311424
1505.092360	191858.833496	36.316442
1506.229113	192219.535230	36.321460
1508.204064	192554.083111	36.326477
1509.160843	192916.406507	36.331495
1510.740023	193268.062923	36.336512
1512.252825	193629.343050	36.341530
1513.676399	193987.022252	36.346548
1515.102978	194337.669570	36.351565
1516.437190	194717.521815	36.356583
1517.750690	195074.438672	36.361600
1519.581489	195431.370499	36.366618
1520.846760	195777.038247	36.371636
1522.690788	196118.139789	36.376653
1523.800352	196463.025178	36.381671
1525.614180	196808.096515	36.386688
1527.086067	197167.803224	36.391706
1528.262725	197508.238794	36.396724
1529.922491	197860.591302	36.401741
1531.037737	198216.631828	36.406759
1532.419919	198569.594067	36.411776
1533.704259	198937.950178	36.416794
1535.105438	199310.427270	36.421812
1536.670997	199677.240920	36.426829
1537.988428	200068.209777	36.431847
1539.173851	200454.975349	36.436864
1540.779833	200839.791901	36.441882
1542.244700	201234.169938	36.446900
1543.733299	201615.633298	36.451917
1545.110844	202016.620142	36.456935
1547.102147	202399.614020	36.461952
1549.020263	202795.890826	36.466970
1550.488783	203186.761473	36.471988
1552.465469	203565.446728	36.477005
1554.088192	203960.611996	36.482023
1556.072759	204341.420163	36.487040
1558.244859	204721.131523	36.492058
1559.982110	205099.471620	36.497076
1561.876534	205463.603504	36.502093
1563.745136	205851.130413	36.507111
1565.507644	206207.111019	36.512128
1567.236327	206567.720942	36.517146
1568.880765	206933.870401	36.522164
1570.511979	207286.094266	36.527181
1571.689744	207645.304860	36.532199
1573.129989	208013.855851	36.537216
1574.626666	208386.766910	36.542234
1575.928901	208760.271601	36.547252
1577.520334	209135.836329	36.552269
1579.071099	209518.165071	36.557287
1580.759587	209886.376942	36.562304
1582.358955	210267.100696	36.567322
1583.548794	210650.639006	36.572340
1585.306708	211024.761181	36.577357
1586.757494	211398.810492	36.582375
1588.431475	211778.537475	36.587392
1590.252685	212158.875780	36.592410
1591.897375	212545.823729	36.597428
1592.889246	212922.827690	36.602445
1594.290165	213316.982588	36.607463
1596.155382	213701.738830	36.612480
1597.591219	214093.249658	36.617498
1599.355682	214491.994988	36.622516
1601.548449	214886.427252	36.627533
1602.891307	215275.926961	36.632551
1604.208313	215675.337841	36.637568
1605.605516	216053.199042	36.642586
1606.583985	216433.368350	36.647604
1607.822558	216814.383519	36.652621
1609.278099	217203.211074	36.657639
1610.740036	217588.178435	36.662656
1612.546909	217974.789900	36.667674
1613.728593	218384.165338	36.672692
1615.875167	218785.884630	36.677709
1617.003817	219194.789666	36.682727
1618.392742	219609.798246	36.687744
1619.798538	220010.480458	36.692762
1621.565362	220429.110312	36.697780
1623.300257	220846.782018	36.702797
1625.337332	221256.224982	36.707815
1626.712346	221662.633157	36.712832
1628.587542	222076.246820	36.717850
1630.349233	222509.921614	36.722868
1632.225794	222915.206914	36.727885
1633.734444	223340.215922	36.732903
1635.302597	223764.124035	36.737920
1636.960888	224180.855400	36.742938
1638.702970	224594.221014	36.747956
1640.626365	225014.719775	36.752973
1642.612928	225432.211883	36.757991
1644.671270	225838.212138	36.763008
1646.543986	226243.356389	36.768026
1648.387939	226652.342247	36.773044
1650.648392	227046.576607	36.778061
1652.964198	227439.659603	36.783079
1654.819830	227828.047126	36.788096
1656.668781	228206.784603	36.793114
1657.901610	228596.195205	36.798132
1659.427257	228979.943174	36.803149
1661.131419	229368.716376	36.808167
1662.493470	229759.809808	36.813184
1664.347591	230135.223843	36.818202
1665.598682	230543.712561	36.823220
1667.201513	230933.904151	36.828237
1668.738550	231330.407458	36.833255
1669.939309	231738.399846	36.838272
1672.150121	232137.304578	36.843290
1673.588965	232547.137935	36.848308
1675.012078	232963.198333	36.853325
1676.019781	233379.407014	36.858343
1677.743698	233809.896843	36.863360
1679.256437	234227.418206	36.868378
1680.166711	234667.625707	36.873396
1681.619246	235107.690679	36.878413
1683.058896	235564.803497	36.883431
1684.209304	236015.997443	36.888448
1685.804645	236472.831734	36.893466
1687.251450	236958.396723	36.898484
1688.749753	237427.214091	36.903501
1690.136446	237913.680654	36.908519
1691.710712	238398.439674	36.913536
1693.209211	238861.874850	36.918554
1694.978417	239329.608440	36.923572
1696.953882	239795.351697	36.928589
1698.461407	240263.360513	36.933607
1700.203727	240730.288545	36.938624
1702.128059	241199.929758	36.943642
1704.007972	241677.911431	36.948660
1705.784297	242140.238297	36.953677
1706.924460	242619.542079	36.958695
1709.185684	243094.412626	36.963712
1711.325959	243577.357265	36.968730
1712.560680	244046.892530	36.973748
1713.999312	244527.697816	36.978765
1715.924129	245010.783076	36.983783
1717.376596	245496.998153	36.988800
1719.278899	245975.439860	36.993818
1721.241726	246470.790134	36.998836
1722.986320	246963.536457	37.003853
1724.928391	247445.453329	37.008871
1726.796120	247938.255917	37.013888
1729.096302	248419.731520	37.018906
1730.796591	248903.875928	37.023924
1732.454679	249380.229271	37.028941
1734.826163	249844.064287	37.033959
1736.877993	250323.729663	37.038976
1739.080398	250776.315343	37.043994
1741.078247	251249.462032	37.049012
1743.313852	251709.079287	37.054029
1745.439825	252169.274427	37.059047
1746.762181	252627.143174	37.064064
1749.027597	253068.694389	37.069082
1750.262590	253526.578472	37.074100
1752.285457	253974.979568	37.079117
1753.655319	254435.254187	37.084135
1755.332531	254894.841267	37.089152
1756.981847	255349.250961	37.094170
1758.672361	255826.694384	37.099188
1760.160134	256285.806022	37.104205
1761.769846	256760.748425	37.109223
1763.532896	257236.172660	37.114240
1765.102944	257693.034738	37.119258
1766.539474	258182.257882	37.124276
1768.348873	258664.583697	37.129293
1769.665057	259154.284489	37.134311
1771.426892	259653.104855	37.139328
1773.340635	260140.543841	37.144346
1774.738279	260638.841854	37.149364
1776.428526	261149.816553	37.154381
1778.255163	261646.440272	37.159399
1779.474581	262157.748956	37.164416
1781.552388	262668.834245	37.169434
1783.106362	263181.304321	37.174452
1784.785542	263697.664635	37.179469
1786.936471	264202.334610	37.184487
1788.747717	264723.142331	37.189504
1791.284085	265219.540231	37.194522
1793.163727	265703.348482	37.199540
1794.774324	266174.246748	37.204557
1797.369309	266655.162677	37.209575
1798.949634	267122.254629	37.214592
1801.297698	267578.037449	37.219610
1803.267301	268051.412394	37.224628
1805.001457	268515.707399	37.229645
1807.079327	268977.199491	37.234663
1808.167331	269450.189874	37.239680
1809.583431	269919.236831	37.244698
1811.574678	270395.373638	37.249716
1813.131969	270871.126672	37.254733
1814.661690	271356.536605	37.259751
1815.812867	271860.478062	37.264768
1817.790341	272349.061170	37.269786
1819.585691	272857.183561	37.274804
1821.614526	273359.219237	37.279821
1823.729764	273859.867384	37.284839
1825.327954	274362.076253	37.289856
1827.033203	274880.777141	37.294874
1828.904980	275396.552506	37.299892
1830.099185	275916.278269	37.304909
1831.870575	276437.529762	37.309927
1833.606985	276960.360849	37.314944
1835.191342	277487.509507	37.319962
1837.460695	278026.148207	37.324980
1838.762318	278577.524778	37.329997
1840.832270	279126.431350	37.335015
1841.867997	279675.690985	37.340032
1843.487482	280221.750093	37.345050
1845.297332	280799.475884	37.350068
1846.340966	281370.828030	37.355085
1848.492033	281957.458134	37.360103
1849.924455	282542.532560	37.365120
1851.666033	283131.743116	37.370138
1853.731150	283725.773069	37.375156
1855.466910	284322.422511	37.380173
1857.687039	284914.109758	37.385191
1859.449799	285529.393806	37.390208
1861.032412	286121.642327	37.395226
1863.076762	286744.289839	37.400244
1865.054618	287353.813925	37.405261
1867.168279	287947.487689	37.410279
1869.763238	288550.779260	37.415296
1872.167759	289145.591589	37.420314
1873.825708	289739.233415	37.425332
1875.638373	290342.345417	37.430349
1877.737932	290930.165614	37.435367
1879.648458	291526.651061	37.440384
1881.749209	292113.246008	37.445402
1883.427358	292708.469782	37.450420
1885.102634	293302.344778	37.455437
1887.796867	293888.016277	37.460455
1889.487988	294480.028130	37.465472
1891.641210	295060.731509	37.470490
1893.948737	295622.077069	37.475508
1895.678794	296177.600578	37.480525
1897.961516	296722.892685	37.485543
1900.067736	297257.671857	37.490560
1902.368883	297804.732864	37.495578
1904.195698	298349.992550	37.500596
1906.142459	298883.266382	37.505613
1908.118432	299415.719562	37.510631
1909.688883	299960.150517	37.515648
1911.541247	300502.574531	37.520666
1913.663881	301048.199995	37.525684
1915.427575	301594.772512	37.530701
1917.382725	302129.321713	37.535719
1918.919630	302688.218464	37.540736
1920.815296	303236.028266	37.545754
1922.432503	303792.212271	37.550772
1924.782236	304351.010212	37.555789
1926.721539	304913.252374	37.560807
1928.191833	305473.666334	37.565824
1929.731494	306044.832438	37.570842
1931.331477	306633.507160	37.575860
1933.280782	307222.854366	37.580877
1935.031780	307803.292119	37.585895
1937.051763	308397.748436	37.590912
1939.272433	308981.601754	37.595930
1940.841859	309572.621770	37.600948
1942.842520	310169.328026	37.605965
1944.978676	310767.885615	37.610983
1946.682642	311370.270678	37.616000
1948.665327	311971.308138	37.621018
1951.403230	312560.911434	37.626036
1953.084929	313163.209514	37.631053
1955.496067	313753.214534	37.636071
1957.718638	314357.847851	37.641088
1960.362649	314946.076444	37.646106
1962.602637	315515.705739	37.651124
1964.990419	316104.400058	37.656141
1967.065181	316666.989073	37.661159
1968.990587	317240.949129	37.666176
1970.801804	317814.949223	37.671194
1973.178090	318387.400439	37.676212
1974.872991	318956.941684	37.681229
1976.941054	319521.259804	37.686247
1978.838910	320101.522120	37.691264
1980.629112	320680.401141	37.696282
1982.621321	321249.820576	37.701300
1984.172025	321840.257168	37.706317
1986.378975	322419.785309	37.711335
1988.223031	323016.355716	37.716352
1989.680327	323602.475312	37.721370
1991.755182	324202.777708	37.726388
1993.490169	324797.826008	37.731405
1995.214724	325388.097138	37.736423
1997.051041	325998.526990	37.741440
1998.538489	326606.801420	37.746458
2000.780720	327193.640100	37.751476
2002.315001	327788.438643	37.756493
2004.126073	328378.969407	37.761511
2006.004309	328978.723424	37.766528
2007.253837	329585.686867	37.771546
2009.348294	330194.961724	37.776564
2011.721488	330813.397401	37.781581
2013.369481	331442.409123	37.786599
2014.797684	332067.643353	37.791616
2016.642259	332703.511744	37.796634
2018.984326	333330.326637	37.801652
2020.833677	333980.724607	37.806669
2022.691662	334628.676194	37.811687
2025.104509	335280.560938	37.816704
2027.213450	335929.544958	37.821722
2029.830969	336575.870107	37.826740
2031.876411	337217.893637	37.831757
2034.532738	337849.549936	37.836775
2036.949602	338487.737150	37.841792
2038.899751	339125.564513	37.846810
2040.722210	339756.070161	37.851828
2042.752317	340409.451650	37.856845
2044.836885	341054.616972	37.861863
2047.087675	341699.542216	37.866880
2048.974695	342350.663060	37.871898
2051.081747	342986.179393	37.876916
2053.214824	343645.488916	37.881933
2055.636386	344291.060362	37.886951
2057.465948	344948.373058	37.891968
2059.256482	345603.703545	37.896986
2061.571789	346257.056943	37.902004
2063.153977	346928.189359	37.907021
2065.254977	347587.295652	37.912039
2067.135073	348254.652240	37.917056
2068.899450	348930.570591	37.922074
2071.336016	349605.780010	37.927092
2073.693871	350282.844947	37.932109
2075.908336	350960.735900	37.937127
2078.354174	351620.306519	37.942144
2079.833186	352295.993089	37.947162
2082.157088	352973.275319	37.952180
2083.952742	353661.344868	37.957197
2085.990476	354330.407700	37.962215
2088.186204	355020.822379	37.967232
2090.200551	355695.322491	37.972250
2092.810766	356364.178495	37.977268
2095.294324	357038.753898	37.982285
2097.644321	357716.715343	37.987303
2100.061169	358396.049373	37.992320
2101.874856	359067.051970	37.997338
2104.299649	359737.862654	38.002356
2106.270278	360413.433026	38.007373
2108.319688	361069.215593	38.012391
2110.400362	361735.129367	38.017408
2111.902427	362409.654455	38.022426
2114.095837	363064.262461	38.027444
2116.043643	363719.129584	38.032461
2117.678899	364373.227135	38.037479
2119.723873	365026.456956	38.042496
2121.961300	365681.900122	38.047514
2124.598182	366329.729836	38.052532
2126.498358	366990.965688	38.057549
2128.696626	367648.613007	38.062567
2130.877470	368301.153260	38.067584
2132.898327	368975.370081	38.072602
2135.070599	369630.804815	38.077620
2136.880386	370307.340980	38.082637
2139.194683	370976.245422	38.087655
2140.761405	371664.388171	38.092672
2142.271405	372355.139501	38.097690
2144.104890	373048.053750	38.102708
2145.771326	373770.401150	38.107725
2147.679198	374487.797774	38.112743
2149.625921	375217.117212	38.117760
2151.463299	375960.311231	38.122778
2153.677185	376697.896557	38.127796
2155.635917	377455.947921	38.132813
2157.712345	378202.627403	38.137831
2159.503155	378955.855759	38.142848
2161.956376	379724.750702	38.147866
2164.095763	380487.418608	38.152884
2166.009571	381277.845719	38.157901
2167.596888	382059.334094	38.162919
2170.014016	382846.239601	38.167936
2171.526738	383660.205529	38.172954
2173.929937	384461.854720	38.177972
2176.158351	385277.761327	38.182989
2178.469794	386082.883814	38.188007
2181.450503	386878.542274	38.193024
2184.119523	387689.139473	38.198042
2186.942882	388471.931754	38.203060
2189.354793	389275.382899	38.208077
2191.668448	390060.021669	38.213095
2194.106121	390845.785019	38.218112
2196.303056	391638.995707	38.223130
2198.614857	392424.688836	38.228148
2200.957749	393215.805270	38.233165
2203.018181	394006.796915	38.238183
2205.358442	394801.698578	38.243200
2207.208249	395587.564420	38.248218
2209.965595	396374.926611	38.253236
2212.275960	397163.332247	38.258253
2214.455121	397941.196916	38.263271
2217.077834	398720.459814	38.268288
2219.597125	399499.567130	38.273306
2221.980216	400275.052912	38.278324
2224.029080	401058.505499	38.283341
2226.095597	401822.549939	38.288359
2228.485378	402605.090273	38.293376
2230.249601	403375.224781	38.298394
2232.374108	404135.623430	38.303412
2234.398303	404889.659188	38.308429
2236.410840	405639.217381	38.313447
2238.509045	406400.267064	38.318464
2240.486105	407163.672056	38.323482
2242.755988	407924.193541	38.328500
2245.073491	408689.726279	38.333517
2247.310835	409462.900624	38.338535
2249.566340	410229.514270	38.343552
2251.455536	411007.414445	38.348570
2253.886283	411788.213115	38.353588
2256.347445	412567.058395	38.358605
2258.224644	413354.059476	38.363623
2260.768272	414134.439252	38.368640
2262.975721	414919.791307	38.373658
2265.395017	415719.239506	38.378676
2267.929696	416518.896171	38.383693
2269.494219	417326.948770	38.388711
2271.583895	418114.552099	38.393728
2273.341095	418939.536509	38.398746
2275.964973	419752.850060	38.403764
2277.829094	420579.888859	38.408781
2279.883178	421419.526933	38.413799
2282.246452	422254.931389	38.418816
2284.221382	423109.462775	38.423834
2286.181098	423962.144042	38.428852
2288.292313	424814.921315	38.433869
2290.469753	425682.288796	38.438887
2292.847447	426551.565135	38.443904
2295.456961	427425.326430	38.448922
2297.925600	428283.335873	38.453940
2300.458033	429140.037714	38.458957
2303.510743	429999.757789	38.463975
2306.241569	430854.996314	38.468992
2308.972844	431703.319589	38.474010
2311.995843	432559.407053	38.479028
2314.169099	433402.297014	38.484045
2316.213147	434249.631766	38.489063
2319.376187	435086.470296	38.494080
2321.557654	435954.872301	38.499098
2324.182337	436772.813786	38.504116
2326.605687	437605.788907	38.509133
2328.826579	438440.741066	38.514151
2331.611002	439266.457820	38.519168
2333.865819	440097.142256	38.524186
2336.266961	440921.901399	38.529204
2338.920923	441739.199771	38.534221
2341.203847	442569.634154	38.539239
2343.567047	443385.149892	38.544256
2345.601229	444214.450962	38.549274
2347.651241	445043.161020	38.554292
2349.652709	445879.991349	38.559309
2351.774647	446720.258466	38.564327
2354.317682	447553.743950	38.569344
2356.264014	448396.149712	38.574362
2358.508354	449215.661369	38.579380
2360.684659	450036.518172	38.584397
2362.318033	450853.339275	38.589415
2364.631802	451683.564683	38.594432
2367.074207	452527.742053	38.599450
2368.833785	453366.489993	38.604468
2371.131034	454206.527583	38.609485
2373.498234	455060.928687	38.614503
2376.110931	455914.190260	38.619520
2377.770582	456782.796485	38.624538
2380.165246	457654.626895	38.629556
2382.218804	458531.533060	38.634573
2384.527048	459411.541952	38.639591
2387.073359	460289.044985	38.644608
2389.492219	461194.684999	38.649626
2391.371350	462096.483898	38.654644
2393.883730	463004.855171	38.659661
2396.204971	463924.032251	38.664679
2398.590462	464837.697062	38.669696
2400.907146	465763.913553	38.674714
2403.102907	466685.002602	38.679732
2406.156821	467603.576500	38.684749
2408.002486	468543.837165	38.689767
2410.264272	469490.750536	38.694784
2412.662779	470433.753615	38.699802
2414.984025	471397.081960	38.704820
2417.704840	472342.409808	38.709837
2419.867006	473301.727192	38.714855
2422.228645	474272.982736	38.719872
2424.582921	475260.654431	38.724890
2426.741790	476236.185253	38.729908
2429.822734	477208.880495	38.734925
2431.663580	478203.400620	38.739943
2434.525686	479191.278648	38.744960
2436.836015	480176.975327	38.749978
2439.043257	481167.129547	38.754996
2441.989154	482162.757710	38.760013
2444.560704	483146.832957	38.765031
2447.070018	484134.297293	38.770048
2450.359979	485132.779903	38.775066
2452.473249	486108.035722	38.780084
2455.450238	487083.947816	38.785101
2457.742467	488078.042037	38.790119
2461.156228	489058.210533	38.795136
2463.761402	490037.351480	38.800154
2466.236596	491004.751444	38.805172
2469.094900	491963.553984	38.810189
2471.355080	492926.946225	38.815207
2474.226596	493895.426837	38.820224
2476.805383	494851.692669	38.825242
2478.834999	495815.212500	38.830260
2481.556890	496782.241425	38.835277
2483.502614	497753.433104	38.840295
2486.002399	498717.916237	38.845312
2487.995307	499678.243645	38.850330
2490.598190	500625.045788	38.855348
2492.761488	501564.354256	38.860365
2495.098062	502509.529993	38.865383
2497.610944	503462.638718	38.870400
2500.238529	504402.007310	38.875418
2502.819247	505350.001797	38.880436
2505.384923	506289.876414	38.885453
2507.830797	507247.311248	38.890471
2510.703962	508190.853519	38.895488
2513.680746	509125.147947	38.900506
2515.951380	510066.816951	38.905524
2518.871362	511005.899676	38.910541
2521.199169	511966.397092	38.915559
2523.579123	512915.941276	38.920576
2526.063156	513874.027346	38.925594
2528.561818	514827.063424	38.930612
2530.843634	515791.314426	38.935629
2533.025068	516774.819556	38.940647
2535.643114	517748.413470	38.945664
2537.911181	518718.932432	38.950682
2540.327489	519703.469293	38.955700
2543.090560	520689.797376	38.960717
2545.762370	521679.300487	38.965735
2548.028074	522690.364192	38.970752
2550.594638	523693.099763	38.975770
2552.902277	524693.999675	38.980788
2555.424078	525705.471041	38.985805
2557.621018	526728.811965	38.990823
2560.454505	527748.449164	38.995840
2563.178156	528783.490256	39.000858
2565.957831	529799.470663	39.005876
2568.876384	530823.763113	39.010893
2571.398606	531846.289727	39.015911
2574.175210	532866.385781	39.020928
2576.978109	533902.409171	39.025946
2579.626768	534930.030972	39.030964
2582.034508	535944.537536	39.035981
2584.447567	536988.556679	39.040999
2587.243277	538010.498140	39.046016
2589.422595	539040.319447	39.051034
2592.237630	540081.527164	39.056052
2595.313509	541114.313797	39.061069
2598.224905	542144.789204	39.066087
2600.718488	543181.094095	39.071104
2603.297390	544216.301559	39.076122
2605.900192	545252.232317	39.081140
2608.754441	546286.534059	39.086157
2611.307671	547319.653199	39.091175
2613.694585	548360.163605	39.096192
2616.600921	549392.613630	39.101210
2619.278550	550436.233960	39.106228
2621.908321	551461.687628	39.111245
2624.365623	552504.331846	39.116263
2627.200107	553531.704162	39.121280
2630.200660	554551.934301	39.126298
2632.765021	555551.157710	39.131316
2635.734584	556547.574059	39.136333
2638.272052	557537.860212	39.141351
2640.834987	558529.424309	39.146368
2643.535057	559513.355571	39.151386
2646.058841	560502.366641	39.156404
2649.116626	561483.477168	39.161421
2651.684576	562470.373093	39.166439
2654.182532	563463.684162	39.171456
2656.917157	564448.794342	39.176474
2659.245793	565446.099742	39.181492
2662.168173	566429.821543	39.186509
2665.074580	567429.234070	39.191527
2667.546419	568435.720675	39.196544
2671.088129	569421.114527	39.201562
2673.504267	570420.727678	39.206580
2676.155294	571405.617640	39.211597
2678.952354	572403.553536	39.216615
2681.461579	573402.212119	39.221632
2684.037911	574404.041019	39.226650
2686.473793	575418.305960	39.231668
2689.370000	576433.513306	39.236685
2692.054473	577449.125246	39.241703
2694.277657	578471.403604	39.246720
2697.087748	579500.719043	39.251738
2699.177672	580537.092207	39.256756
2702.053179	581565.420821	39.261773
2704.735995	582608.487252	39.266791
2707.027133	583651.631430	39.271808
2709.932191	584697.839548	39.276826
2712.234631	585773.234374	39.281844
2715.394301	586831.244537	39.286861
2718.029017	587907.494330	39.291879
2720.406605	588990.306262	39.296896
2722.959268	590055.702039	39.301914
2725.395415	591152.137456	39.306932
2727.949418	592240.034272	39.311949
2730.595392	593331.972972	39.316967
2733.586506	594438.077316	39.321984
2736.937505	595533.597715	39.327002
2739.849133	596642.712544	39.332020
2742.449558	597733.847221	39.337037
2745.282894	598845.268839	39.342055
2747.830032	599953.778561	39.347072
2750.849951	601054.391122	39.352090
2753.410242	602163.786753	39.357108
2756.802240	603257.766603	39.362125
2759.807218	604366.872062	39.367143
2762.747220	605467.923406	39.372160
2765.999217	606565.061423	39.377178
2768.910793	607664.702548	39.382196
2771.644740	608751.108914	39.387213
2774.526432	609849.740525	39.392231
2776.717817	610937.777978	39.397248
2779.860133	612015.693859	39.402266
2782.465238	613091.746411	39.407284
2784.716248	614143.302642	39.412301
2787.623256	615198.996431	39.417319
2790.040753	616264.371357	39.422336
2792.711132	617326.700028	39.427354
2794.856541	618403.310679	39.432372
2797.350624	619477.056336	39.437389
2799.939145	620566.121821	39.442407
2802.038762	621668.103314	39.447424
2805.328589	622777.063641	39.452442
2806.967376	623898.231743	39.457460
2809.486101	625035.816826	39.462477
2812.089734	626175.863461	39.467495
2814.731741	627332.961846	39.472512
2817.382522	628517.498079	39.477530
2819.993055	629692.221508	39.482548
2822.829764	630875.512355	39.487565
2825.755821	632062.698053	39.492583
2828.401555	633272.158814	39.497600
2831.636510	634457.821285	39.502618
2834.016446	635666.649704	39.507636
2837.113901	636877.459729	39.512653
2840.207453	638082.590220	39.517671
2842.629466	639313.784455	39.522688
2845.485604	640544.207827	39.527706
2848.501046	641793.208187	39.532724
2851.443662	643021.272712	39.537741
2854.413003	644264.242059	39.542759
2856.872104	645516.119545	39.547776
2860.492980	646748.151751	39.552794
2863.794298	648002.666089	39.557812
2866.549269	649237.181480	39.562829
2869.510438	650481.375088	39.567847
2872.321447	651743.723905	39.572864
2875.524806	652989.703518	39.577882
2878.121705	654250.423266	39.582900
2881.032111	655494.541677	39.587917
2883.950363	656756.478031	39.592935
2886.449124	658029.227317	39.597952
2889.727219	659295.901665	39.602970
2892.510376	660564.734969	39.607988
2895.669040	661833.685758	39.613005
2898.937819	663102.151735	39.618023
2901.958236	664377.160076	39.623040
2905.309862	665641.045763	39.628058
2907.417933	666905.871511	39.633076
2910.725755	668180.719373	39.638093
2913.736651	669442.614941	39.643111
2916.135051	670716.778316	39.648128
2919.211334	671990.106159	39.653146
2921.990440	673274.248370	39.658164
2925.172120	674546.563574	39.663181
2928.474746	675818.286406	39.668199
2931.362425	677103.869113	39.673216
2934.399322	678350.244289	39.678234
2937.221501	679596.338335	39.683252
2940.158341	680819.791753	39.688269
2942.637321	682052.745153	39.693287
2945.336163	683296.617818	39.698304
2947.935541	684533.783156	39.703322
2950.519345	685797.888395	39.708340
2953.545453	687033.348096	39.713357
2956.207975	688298.131641	39.718375
2959.150007	689563.234986	39.723392
2962.577798	690815.920133	39.728410
2965.441608	692080.977676	39.733428
2968.310022	693370.407788	39.738445
2971.728551	694633.270378	39.743463
2974.494906	695913.518869	39.748480
2977.505958	697199.042796	39.753498
2980.373996	698482.965026	39.758516
2983.231520	699771.855395	39.763533
2986.406104	701063.821404	39.768551
2989.308145	702365.552135	39.773568
2992.793545	703661.091636	39.778586
2995.542871	704975.039613	39.783604
2998.219641	706285.084494	39.788621
3001.351760	707592.820966	39.793639
3004.330249	708921.526070	39.798656
3007.165833	710240.939032	39.803674
3010.409138	711576.213835	39.808692
3013.025090	712901.437305	39.813709
3016.164329	714234.775247	39.818727
3019.039280	715590.359027	39.823744
3022.521633	716931.818327	39.828762
3025.429865	718280.183297	39.833780
3028.120887	719633.806484	39.838797
3031.400384	720984.438305	39.843815
3034.548688	722352.618960	39.848832
3037.222330	723712.053204	39.853850
3040.325548	725091.796527	39.858868
3043.486081	726470.457464	39.863885
3046.444390	727844.671351	39.868903
3049.461659	729224.421895	39.873920
3053.089350	730604.870317	39.878938
3056.141863	731987.156023	39.883956
3059.150376	733367.187771	39.888973
3062.456720	734731.481737	39.893991
3065.496011	736124.064074	39.899008
3068.638047	737501.780204	39.904026
3071.606223	738894.876560	39.909044
3074.743752	740271.520257	39.914061
3078.153969	741657.543278	39.919079
3081.204334	743042.742517	39.924096
3084.433768	744405.580442	39.929114
3087.662491	745791.445956	39.934132
3090.853608	747183.280824	39.939149
3093.966452	748556.057344	39.944167
3097.146717	749940.155935	39.949184
3100.192026	751300.189686	39.954202
3103.692914	752646.313030	39.959220
3106.362838	753969.790818	39.964237
3109.592970	755284.033198	39.969255
3113.050402	756607.460545	39.974272
3116.194608	757927.708828	39.979290
3119.467327	759252.084162	39.984308
3122.246942	760585.166552	39.989325
3124.637797	761920.636964	39.994343
3127.649489	763260.976582	39.999360
3130.217806	764598.152482	40.004378
3132.902469	765960.484575	40.009396
3135.439594	767345.103397	40.014413
3138.097355	768731.113823	40.019431
3140.934949	770149.064366	40.024448
3143.662490	771561.504614	40.029466
3146.356740	772989.296857	40.034484
3148.896739	774447.575697	40.039501
3151.960219	775902.969882	40.044519
3154.857602	777372.924379	40.049536
3157.309899	778851.637206	40.054554
3160.228893	780352.929360	40.059572
3163.054388	781875.753025	40.064589
3166.597547	783388.665711	40.069607
3169.706910	784927.760669	40.074624
3172.818185	786456.914673	40.079642
3176.432160	788002.121252	40.084660
3179.677986	789550.924322	40.089677
3183.450586	791096.945863	40.094695
3186.901456	792655.416694	40.099712
3189.680872	794203.421230	40.104730
3192.831763	795764.286407	40.109748
3196.164369	797341.999267	40.114765
3199.389153	798915.358926	40.119783
3202.317356	800500.788573	40.124800
3205.313414	802095.330554	40.129818
3208.384846	803683.034324	40.134836
3211.546039	805288.394258	40.139853
3214.199199	806896.933102	40.144871
3217.516217	808521.689778	40.149888
3220.663585	810145.450267	40.154906
3223.799228	811785.477011	40.159924
3226.903912	813434.728379	40.164941
3229.892579	815078.955693	40.169959
3232.770680	816728.799939	40.174976
3236.437864	818387.517372	40.179994
3240.039290	820052.465090	40.185012
3243.167388	821716.147171	40.190029
3246.213254	823380.982868	40.195047
3249.276845	825046.806415	40.200064
3252.415548	826721.548969	40.205082
3255.761353	828400.551146	40.210100
3259.034912	830083.514720	40.215117
3262.394106	831771.868813	40.220135
3265.811494	833459.916491	40.225152
3268.953164	835137.054936	40.230170
3272.147360	836777.788038	40.235188
3275.220671	838421.475864	40.240205
3278.896257	840049.900439	40.245223
3282.211698	841687.691280	40.250240
3285.415142	843319.535064	40.255258
3288.757231	844961.913725	40.260276
3291.841242	846600.505400	40.265293
3295.220600	848233.662881	40.270311
3298.455100	849878.361053	40.275328
3301.959858	851528.596219	40.280346
3305.765774	853180.960022	40.285364
3308.406936	854839.192499	40.290381
3311.425206	856504.479254	40.295399
3314.824347	858171.478363	40.300416
3317.695428	859843.444345	40.305434
3321.596326	861520.008586	40.310452
3324.659274	863208.170275	40.315469
3328.286411	864888.498249	40.320487
3331.660790	866585.928757	40.325504
3334.780809	868281.663505	40.330522
3338.412191	869972.667789	40.335540
3341.374432	871688.173661	40.340557
3345.082807	873394.640474	40.345575
3348.423991	875115.376663	40.350592
3351.265167	876832.988843	40.355610
3354.744373	878555.981997	40.360628
3357.919877	880291.949871	40.365645
3361.427155	882020.679663	40.370663
3364.956445	883757.002713	40.375680
3368.149642	885494.986346	40.380698
3371.575183	887234.144092	40.385716
3374.574259	889006.132422	40.390733
3377.969234	890760.241895	40.395751
3380.991805	892533.448435	40.400768
3383.879997	894313.932689	40.405786
3387.196883	896102.264049	40.410804
3389.970098	897900.236333	40.415821
3393.598453	899712.991758	40.420839
3396.810979	901537.168945	40.425856
3400.021140	903361.810013	40.430874
3403.362513	905191.122066	40.435892
3406.850379	907029.711463	40.440909
3410.475774	908860.167897	40.445927
3414.322169	910704.874513	40.450944
3417.599380	912545.215923	40.455962
3420.681815	914379.209538	40.460980
3424.196147	916236.609815	40.465997
3427.838807	918093.641184	40.471015
3430.975964	919952.232522	40.476032
3434.044751	921816.620901	40.481050
3437.767580	923691.084542	40.486068
3440.803298	925568.651266	40.491085
3443.951329	927443.334779	40.496103
3447.354829	929334.935517	40.501120
3450.872051	931205.615190	40.506125
3454.595528	933024.852464	40.511130
3457.540223	934794.772617	40.516135
3460.915196	936489.328210	40.521140
3464.480336	938129.623546	40.526144
3467.119439	939695.487677	40.531149
3470.584764	941178.927616	40.536154
3473.493814	942604.766262	40.541159
3476.497864	943933.587025	40.546164
3479.186796	945191.283653	40.551168
3481.684072	946367.550644	40.556173
3484.730732	947477.912858	40.561178
3487.052338	948510.289709	40.566183
3489.489965	949467.453803	40.571188
3491.664568	950357.640097	40.576192
3493.671109	951213.093471	40.581197
3496.078397	951972.165032	40.586202
3497.761043	952694.088163	40.591207
3499.600636	953338.027677	40.596212
3501.835627	953918.579808	40.601216
3503.176338	954462.261310	40.606221
3504.746110	954940.164611	40.611226
3506.339881	955359.791705	40.616231
3507.961113	955728.997014	40.621236
3509.352110	956052.833392	40.626240
3510.503878	956321.998262	40.631245
3512.151809	956550.291871	40.636250
3513.631602	956733.421937	40.641255
3514.742336	956862.116178	40.646260
3516.461774	956962.477482	40.651264
3517.174607	957018.219925	40.656269
3518.168449	957031.967216	40.661274
3518.936200	957025.465725	40.666279
3520.179395	956982.326438	40.671284
3521.217682	956906.487006	40.676288
3521.478200	956806.668842	40.681293
3522.266142	956666.769868	40.686298
3523.239199	956512.623701	40.691303
3523.486152	956327.917654	40.696308
3524.060127	956117.958261	40.701312
3524.881137	955902.753705	40.706317
3525.357392	955654.858074	40.711322
3525.668625	955406.489793	40.716327
3526.626932	955127.020170	40.721332
3527.107499	954818.891715	40.726336
3527.184245	954512.874779	40.731341
3528.058213	954175.524120	40.736346
3528.878884	953829.533504	40.741351
3529.129367	953471.164997	40.746356
3529.775212	953097.309274	40.751360
3529.761381	952708.143427	40.756365
3530.319748	952301.786603	40.761370
3530.231591	951885.407897	40.766375
3530.200748	951460.454609	40.771380
3530.423820	951037.192682	40.776384
3530.624449	950616.825762	40.781389
3531.169871	950178.668882	40.786394
3531.172355	949739.897519	40.791399
3531.286720	949293.704471	40.796404
3531.749532	948835.647300	40.801408
3531.826293	948381.919821	40.806413
3532.273361	947916.608128	40.811418
3532.033192	947446.970066	40.816423
3532.030089	946976.387227	40.821428
3532.368748	946499.482381	40.826432
3532.346860	946016.756534	40.831437
3532.281484	945528.536821	40.836442
3532.472180	945038.408196	40.841447
3532.630831	944539.526382	40.846452
3532.802081	944038.583421	40.851456
3532.823063	943540.681542	40.856461
3533.150981	943022.089995	40.861466
3533.286427	942522.346561	40.866471
3532.975356	942001.654612	40.871476
3533.518774	941479.423281	40.876480
3533.433278	940954.564175	40.881485
3533.468233	940428.289979	40.886490
3533.845495	939904.682790	40.891495
3533.529149	939361.208266	40.896500
3534.018768	938826.835966	40.901504
3534.043070	938295.747170	40.906509
3534.121399	937749.928245	40.911514
3534.206105	937219.006996	40.916519
3534.584776	936660.847233	40.921524
3534.771629	936099.592068	40.926528
3534.436228	935543.736327	40.931533
3534.443462	934979.898293	40.936538
3534.682859	934424.497065	40.941543
3534.632399	933860.644476	40.946548
3534.791843	933291.802445	40.951552
3534.404047	932730.860458	40.956557
3534.848183	932151.771500	40.961562
3534.433992	931582.362850	40.966567
3534.325457	931024.646626	40.971572
3534.705534	930444.709361	40.976576
3534.806841	929882.421021	40.981581
3534.854028	929301.935300	40.986586
3534.614368	928731.037541	40.991591
3534.344276	928147.310709	40.996596
3534.545764	927575.349015	41.001600
3534.484621	927003.466683	41.006605
3534.670045	926424.083626	41.011610
3534.391347	925853.075570	41.016615
3534.493312	925274.734797	41.021620
3534.381329	924695.406928	41.026624
3534.371320	924119.074359	41.031629
3534.630935	923539.269531	41.036634
3534.594404	922956.953148	41.041639
3534.474972	922375.164542	41.046644
3534.666478	921796.721250	41.051648
3534.181175	921215.254105	41.056653
3534.631960	920621.831428	41.061658
3534.605455	920036.119449	41.066663
3534.731484	919454.069343	41.071668
3534.883713	918861.465935	41.076672
3534.981382	918272.944071	41.081677
3534.910734	917677.170165	41.086682
3534.771897	917084.518138	41.091687
3534.727930	916476.482202	41.096692
3534.654267	915893.794801	41.101696
3534.808674	915297.239996	41.106701
3534.815201	914697.179113	41.111706
3534.685153	914103.334156	41.116711
3534.585395	913505.182302	41.121716
3534.857844	912901.026616	41.126720
3534.615197	912308.835679	41.131725
3534.514249	911710.198776	41.136730
3534.346763	911118.733345	41.141735
3534.318322	910509.451995	41.146740
3534.574878	909914.315867	41.151744
3534.412823	909326.414666	41.156749
3534.543875	908719.413510	41.161754
3534.910036	908121.269896	41.166759
3534.760113	907511.388454	41.171764
3535.112488	906899.425709	41.176768
3534.793780	906295.127361	41.181773
3534.768873	905687.048433	41.186778
3534.752383	905084.881010	41.191783
3534.727082	904465.287787	41.196788
3534.946734	903856.002092	41.201792
3534.721196	903252.321376	41.206797
3534.931231	902637.308389	41.211802
3534.681248	902023.850126	41.216807
3534.591184	901414.640091	41.221812
3534.660719	900800.993108	41.226816
3534.657461	900183.044012	41.231821
3534.679003	899571.394251	41.236826
3534.675473	898972.523382	41.241831
3534.321682	898351.342890	41.246836
3534.569040	897738.392961	41.251840
3534.525185	897127.937212	41.256845
3534.699143	896512.258814	41.261850
3534.497018	895893.099789	41.266855
3534.446644	895284.667816	41.271860
3534.694942	894662.108968	41.276864
3534.561804	894044.185347	41.281869
3534.545120	893426.947736	41.286874
3534.382938	892812.760909	41.291879
3534.189957	892189.909734	41.296884
3534.285966	891572.838417	41.301888
3534.221608	890971.197667	41.306893
3533.931787	890345.454358	41.311898
3534.101833	889744.224600	41.316903
3533.920210	889127.420124	41.321908
3534.143122	888518.121767	41.326912
3533.800668	887911.563914	41.331917
3534.313635	887286.123431	41.336922
3533.848554	886676.456970	41.341927
3533.768998	886073.627565	41.346932
3534.036061	885459.643077	41.351936
3533.861415	884841.119564	41.356941
3534.178921	884211.604180	41.361946
3534.364805	883594.241017	41.366951
3533.965136	882978.461187	41.371956
3534.337177	882360.934956	41.376960
3533.627651	881737.620355	41.381965
3533.845249	881113.790120	41.386970
3534.049267	880505.296553	41.391975
3533.774449	879877.156050	41.396980
3534.176438	879263.364919	41.401984
3533.957660	878637.406744	41.406989
3533.938042	878013.188794	41.411994
3533.761448	877401.239233	41.416999
3533.763019	876780.278409	41.422004
3533.739838	876158.189895	41.427008
3533.457365	875544.610976	41.432013
3533.773200	874918.940557	41.437018
3533.783233	874306.443206	41.442023
3533.716911	873682.937164	41.447028
3534.043083	873068.124021	41.452032
3533.560134	872448.923354	41.457037
3533.581329	871813.954009	41.462042
3533.783164	871202.557771	41.467047
3533.508189	870579.925016	41.472052
3533.720628	869957.046844	41.477056
3533.560429	869353.673402	41.482061
3533.768068	868716.788861	41.487066
3533.871963	868091.405017	41.492071
3533.404724	867467.412319	41.497076
3533.742502	866838.945332	41.502080
3533.605713	866219.426372	41.507085
3533.857272	865594.242076	41.512090
3533.627691	864971.599911	41.517095
3533.752083	864335.137962	41.522100
3533.752919	863717.280222	41.527104
3533.754917	863092.752990	41.532109
3533.742154	862458.836597	41.537114
3533.812663	861832.321432	41.542119
3533.651373	861191.010018	41.547124
3533.829595	860562.693170	41.552128
3533.610702	859943.515672	41.557133
3533.804482	859302.430114	41.562138
3533.680498	858673.677970	41.567143
3533.532647	858043.114920	41.572148
3533.438889	857406.545945	41.577152
3533.127523	856785.410245	41.582157
3533.408879	856158.955622	41.587162
3533.356788	855519.168141	41.592167
3533.118264	854897.342197	41.597172
3533.531416	854271.547817	41.602176
3533.348587	853644.234733	41.607181
3533.358030	853009.429518	41.612186
3533.646229	852378.501387	41.617191
3533.563269	851749.810674	41.622196
3533.518786	851119.784057	41.627200
3532.938340	850481.120858	41.632205
3532.991472	849841.018020	41.637210
3533.002268	849214.974686	41.642215
3533.049047	848589.738528	41.647220
3533.218558	847960.230941	41.652224
3533.021897	847331.306634	41.657229
3533.196845	846696.508472	41.662234
3532.978439	846070.090778	41.667239
3532.928221	845445.822429	41.672244
3532.998894	844812.214776	41.677248
3532.939162	844199.418777	41.682253
3533.031200	843552.427635	41.687258
3532.935994	842924.310204	41.692263
3532.798354	842292.725705	41.697268
3532.753667	841664.668991	41.702272
3532.996135	841038.548146	41.707277
3533.054371	840407.424003	41.712282
3532.828185	839783.647773	41.717287
3532.589451	839147.134192	41.722292
3532.804819	838516.575070	41.727296
3532.955330	837893.280168	41.732301
3532.892578	837256.595887	41.737306
3533.093676	836625.071295	41.742311
3533.051072	835998.453164	41.747316
3532.749863	835355.131223	41.752320
3532.788853	834722.079980	41.757325
3532.714413	834083.471050	41.762330
3532.570702	833466.675145	41.767335
3532.625111	832829.578797	41.772340
3532.771681	832199.823451	41.777344
3532.537769	831567.484006	41.782349
3532.467766	830934.273348	41.787354
3532.722337	830302.263550	41.792359
3532.574615	829676.169545	41.797364
3532.575625	829035.533296	41.802368
3532.367969	828398.776824	41.807373
3532.669952	827764.655221	41.812378
3532.517668	827133.040796	41.817383
3532.519283	826502.951089	41.822388
3532.573709	825857.986046	41.827392
3532.456581	825238.250987	41.832397
3532.494788	824596.584805	41.837402
3532.499648	823966.494069	41.842407
3532.372889	823336.805119	41.847412
3532.324307	822701.273788	41.852416
3532.309309	822069.195372	41.857421
3532.346486	821428.441654	41.862426
3532.507894	820797.824578	41.867431
3532.550067	820164.233246	41.872436
3532.792562	819526.634137	41.877440
3532.542890	818891.698950	41.882445
3532.720919	818245.720863	41.887450
3532.335137	817605.891589	41.892455
3532.391582	816962.793711	41.897460
3532.399154	816335.153859	41.902464
3532.295826	815700.426693	41.907469
3532.577760	815058.721342	41.912474
3532.327821	814429.771421	41.917479
3532.334475	813786.179770	41.922484
3532.726235	813144.027112	41.927488
3532.481405	812507.013598	41.932493
3532.560048	811858.769101	41.937498
3532.252856	811218.706071	41.942503
3532.016374	810574.945907	41.947508
3531.839320	809933.122285	41.952512
3531.762487	809308.022266	41.957517
3531.760547	808676.483045	41.962522
3531.750677	808047.139954	41.967527
3531.482676	807412.196668	41.972532
3531.780733	806784.692784	41.977536
3531.739637	806159.786248	41.982541
3531.979596	805520.805937	41.987546
3531.617225	804888.436749	41.992551
3531.728469	804254.310394	41.997556
3531.813159	803623.757616	42.002560
3531.390111	803001.176274	42.007565
3531.508487	802358.537873	42.012570
3531.520101	801733.315453	42.017575
3531.127302	801112.371957	42.022580
3531.555923	800484.414505	42.027584
3531.482923	799867.276991	42.032589
3531.186556	799229.518498	42.037594
3531.399288	798605.940142	42.042599
3531.114369	797977.680206	42.047604
3531.170022	797350.875383	42.052608
3531.228935	796729.607872	42.057613
3531.144976	796085.880013	42.062618
3531.100448	795475.364539	42.067623
3530.896039	794856.379726	42.072628
3531.258093	794220.944628	42.077632
3531.081132	793606.851713	42.082637
3530.818884	792975.681367	42.087642
3530.531397	792352.315306	42.092647
3530.793786	791735.331555	42.097652
3530.657852	791114.727150	42.102656
3530.711348	790495.460060	42.107661
3530.861837	789881.427201	42.112666
3530.785210	789259.666696	42.117671
3530.700619	788629.353058	42.122676
3530.925387	788009.150651	42.127680
3530.860706	787393.513349	42.132685
3530.646851	786766.938011	42.137690
3531.015086	786152.249410	42.142695
3530.615521	785528.201384	42.147700
3530.663333	784904.464682	42.152704
3530.558235	784295.742911	42.157709
3530.788121	783658.297608	42.162714
3530.839592	783038.182972	42.167719
3530.457160	782417.646115	42.172724
3530.385762	781794.199249	42.177728
3530.492979	781176.028669	42.182733
3530.381973	780557.940551	42.187738
3530.321213	779944.562325	42.192743
3530.381918	779325.847250	42.197748
3530.681008	778691.884929	42.202752
3530.618668	778079.922899	42.207757
3530.549580	777461.168763	42.212762
3530.497941	776841.177725	42.217767
3529.966126	776226.088126	42.222772
3530.320375	775598.883784	42.227776
3530.152811	774999.083523	42.232781
3530.195608	774369.217543	42.237786
3530.147644	773751.522548	42.242791
3530.309016	773132.804096	42.247796
3530.441347	772513.250433	42.252800
3530.072028	771905.942959	42.257805
3530.059756	771286.211830	42.262810
3530.149616	770669.809524	42.267815
3529.739633	770050.485435	42.272820
3529.969813	769427.009766	42.277824
3530.255726	768823.818905	42.282829
3529.599911	768197.336164	42.287834
3529.500826	767590.020946	42.292839
3529.592387	766981.194333	42.297844
3529.888581	766367.009606	42.302848
3530.019344	765753.443092	42.307853
3530.061525	765136.637219	42.312858
3530.164934	764518.044523	42.317863
3529.398914	763913.254055	42.322868
3529.812992	763292.929283	42.327872
3529.574776	762682.723073	42.332877
3529.628987	762073.551401	42.337882
3529.853180	761455.227312	42.342887
3529.550936	760843.205737	42.347892
3529.787183	760228.872242	42.352896
3529.300706	759628.620916	42.357901
3529.484372	759008.869710	42.362906
3529.751746	758402.028498	42.367911
3529.124252	757793.564533	42.372916
3529.429391	757178.921999	42.377920
3529.171209	756578.044286	42.382925
3529.798460	755966.900353	42.387930
3529.661386	755354.011711	42.392935
3529.329210	754746.783335	42.397940
3529.283786	754124.303348	42.402944
3529.162423	753519.360159	42.407949
3529.152656	752916.818627	42.412954
3529.253663	752304.829679	42.417959
3529.234303	751710.934322	42.422964
3529.315369	751088.581191	42.427968
3529.183300	750481.869546	42.432973
3529.061600	749883.010769	42.437978
3529.426589	749282.738203	42.442983
3528.941541	748666.954469	42.447988
3528.989820	748054.686411	42.452992
3529.003088	747454.233292	42.457997
3528.947828	746848.310400	42.463002
3528.866976	746240.911663	42.468007
3528.554694	745633.356786	42.473012
3528.876310	745040.225484	42.478016
3529.171082	744433.115973	42.483021
3528.953391	743829.506796	42.488026
3528.714695	743225.656930	42.493031
3528.902780	742624.752725	42.498036
3529.376532	742021.677293	42.503040
3529.050846	741417.752655	42.508045
3528.939234	740798.070291	42.513050
3529.114510	740193.669617	42.518055
3528.549124	739600.822694	42.523060
3528.791179	738986.872401	42.528064
3528.696596	738395.388006	42.533069
3528.324381	737785.406492	42.538074
3528.504345	737179.142520	42.543079
3528.325364	736581.699957	42.548084
3528.349446	735981.901936	42.553088
3528.077877	735385.671929	42.558093
3528.013691	734787.085692	42.563098
3528.338035	734199.968665	42.568103
3528.217196	733599.521695	42.573108
3528.333430	733009.977403	42.578112
3528.244504	732422.701844	42.583117
3528.462718	731817.064281	42.588122
3528.302562	731233.327841	42.593127
3527.639155	730629.682329	42.598132
3528.091795	730029.465222	42.603136
3527.953741	729446.932787	42.608141
3527.947130	728851.113803	42.613146
3528.334230	728255.629573	42.618151
3527.982196	727670.084088	42.623156
3527.993441	727071.754178	42.628160
3527.617458	726482.907786	42.633165
3527.761812	725891.998019	42.638170
3527.802349	725300.666896	42.643175
3527.538616	724719.105656	42.648180
3527.710685	724131.036773	42.653184
3527.484071	723551.814352	42.658189
3527.774986	722967.903492	42.663194
3527.600272	722389.234556	42.668199
3527.342316	721799.585520	42.673204
3527.370838	721201.270223	42.678208
3527.275807	720636.690698	42.683213
3527.390323	720042.242554	42.688218
3527.533280	719459.348214	42.693223
3527.387710	718888.560102	42.698228
3527.770144	718283.131436	42.703232
3527.168703	717718.191866	42.708237
3527.235482	717130.634753	42.713242
3527.000664	716552.411719	42.718247
3527.038317	715975.937321	42.723252
3527.211113	715396.920034	42.728256
3526.782900	714821.487359	42.733261
3526.952909	714242.440462	42.738266
3527.152771	713675.751711	42.743271
3526.982042	713098.271824	42.748276
3526.979625	712519.036583	42.753280
3526.778958	711946.345631	42.758285
3526.693882	711364.415327	42.763290
3526.948296	710795.241087	42.768295
3527.018511	710232.264171	42.773300
3527.543978	709649.963060	42.778304
3527.187531	709076.409899	42.783309
3527.365828	708496.918595	42.788314
3527.339611	707909.578720	42.793319
3527.052812	707328.995277	42.798324
3527.482165	706741.149771	42.803329
3527.122822	706162.833277	42.808333
3527.255983	705574.511410	42.813338
3527.222859	704999.934317	42.818343
3526.964057	704419.149061	42.823348
3527.105327	703827.378649	42.828353
3526.987168	703261.889042	42.833357
3526.870122	702666.904095	42.838362
3527.251410	702098.222837	42.843367
3526.716782	701523.748335	42.848372
3526.549439	700935.608692	42.853377
3526.600877	700370.994510	42.858381
3526.497026	699791.362936	42.863386
3526.667472	699221.485834	42.868391
3526.672474	698655.575720	42.873396
3526.387483	698077.849225	42.878401
3526.342925	697505.560904	42.883405
3526.619254	696934.274036	42.888410
3526.661410	696362.791117	42.893415
3526.251998	695806.063960	42.898420
3526.272534	695227.749663	42.903425
3526.293027	694661.281012	42.908429
3525.809155	694088.795634	42.913434
3525.960156	693525.812113	42.918439
3525.564948	692969.500342	42.923444
3525.967156	692415.255584	42.928449
3525.937041	691868.212277	42.933453
3525.788752	691302.602153	42.938458
3525.683255	690739.883688	42.943463
3525.647501	690182.739231	42.948468
3525.776682	689620.755830	42.953473
3525.569051	689070.138379	42.958477
3525.281957	688515.918173	42.963482
3525.613306	687967.280469	42.968487
3525.594331	687420.709323	42.973492
3525.457049	686859.046197	42.978497
3525.542932	686308.358583	42.983501
3525.827027	685759.992548	42.988506
3525.876590	685193.664593	42.993511
3525.552615	684648.221855	42.998516
3525.614620	684086.601173	43.003521
3525.568852	683534.174141	43.008525
3525.707918	682983.723222	43.013530
3525.695466	682430.874950	43.018535
3525.262173	681877.019322	43.023540
3525.762867	681320.779591	43.028545
3525.260438	680770.254744	43.033549
3525.311767	680219.253612	43.038554
3525.583071	679661.806757	43.043559
3525.141432	679118.643029	43.048564
3525.111516	678570.345998	43.053569
3524.878141	678024.740982	43.058573
3525.014058	677478.741713	43.063578
3525.108394	676936.852282	43.068583
3524.987746	676390.583388	43.073588
3525.253775	675845.711006	43.078593
3524.843499	675305.755422	43.083597
3524.692592	674763.132906	43.088602
3525.455215	674222.914140	43.093607
3524.671958	673681.432831	43.098612
3524.726654	673130.905457	43.103617
3524.889401	672598.569724	43.108621
3524.779039	672040.978440	43.113626
3524.700443	671503.637012	43.118631
3524.525189	670974.357256	43.123636
3524.692979	670422.604428	43.128641
3524.453536	669894.072448	43.133645
3524.140814	669353.556862	43.138650
3524.300109	668825.146150	43.143655
3524.215230	668306.820443	43.148660
3524.475969	667768.659383	43.153665
3524.362465	667240.705397	43.158669
3524.502349	666703.102920	43.163674
3524.508394	666175.917150	43.168679
3524.439447	665643.926505	43.173684
3524.621289	665095.751260	43.178689
3524.365065	664582.189868	43.183693
3524.405883	664044.853331	43.188698
3524.695061	663496.318533	43.193703
3524.492955	662969.140833	43.198708
3523.970620	662427.269368	43.203713
3523.731593	661914.160728	43.208717
3523.518141	661390.441156	43.213722
3523.889656	660858.159363	43.218727
3523.800301	660350.231761	43.223732
3523.935701	659816.485545	43.228737
3523.726767	659296.394849	43.233741
3523.695998	658777.893022	43.238746
3523.746618	658258.101640	43.243751
3523.901846	657739.462691	43.248756
3523.824037	657216.991783	43.253761
3523.791524	656699.827214	43.258765
3523.512523	656173.041074	43.263770
3523.700399	655657.281526	43.268775
3523.207463	655147.453302	43.273780
3523.503754	654617.589037	43.278785
3523.877585	654106.659868	43.283789
3523.345129	653591.613805	43.288794
3523.688444	653069.998369	43.293799
3523.216454	652554.288391	43.298804
3523.515511	652033.974296	43.303809
3523.440584	651537.573876	43.308813
3522.769054	651020.619067	43.313818
3523.240361	650509.536989	43.318823
3523.013922	650017.632432	43.323828
3523.236220	649495.849285	43.328833
3523.035616	648997.844411	43.333837
3522.825761	648489.323042	43.338842
3523.176296	647981.629525	43.343847
3522.921359	647486.456779	43.348852
3523.332934	646967.407557	43.353857
3523.245758	646464.059645	43.358861
3523.195144	645957.331575	43.363866
3523.137547	645445.480912	43.368871
3523.051114	644943.956098	43.373876
3522.661530	644435.259850	43.378881
3522.867430	643924.586658	43.383885
3522.603423	643427.465951	43.388890
3522.825642	642929.687873	43.393895
3522.811351	642435.975546	43.398900
3522.717179	641922.302795	43.403905
3522.930004	641430.252828	43.408909
3523.153233	640931.926680	43.413914
3523.087970	640415.672729	43.418919
3522.737630	639926.696808	43.423924
3522.869460	639405.907300	43.428929
3522.928335	638899.808175	43.433933
3523.017041	638397.580340	43.438938
3523.392183	637890.877294	43.443943
3522.708383	637388.982150	43.448948
3522.531620	636879.422231	43.453953
3522.178926	636386.176046	43.458957
3522.009956	635889.673040	43.463962
3522.522845	635388.526907	43.468967
3522.337812	634904.587449	43.473972
3522.317584	634409.088828	43.478977
3522.297949	633916.618855	43.483981
3522.319886	633432.475391	43.488986
3522.514413	632926.610985	43.493991
3522.159401	632439.833445	43.498996
3522.320646	631948.741000	43.504001
3522.137124	631456.633292	43.509005
3522.072832	630966.734505	43.514010
3522.219758	630462.010371	43.519015
3521.929324	629985.018727	43.524020
3522.166058	629495.350336	43.529025
3521.985339	629007.833086	43.534029
3522.113785	628519.990199	43.539034
3521.805632	628030.597174	43.544039
3521.549667	627551.436843	43.549044
3521.826393	627072.814827	43.554049
3521.647146	626599.757206	43.559053
3521.511732	626117.206632	43.564058
3521.579611	625634.449227	43.569063
3521.726488	625158.918171	43.574068
3521.826675	624689.033267	43.579073
3521.755702	624202.728982	43.584077
3521.711322	623722.909423	43.589082
3521.571862	623234.719625	43.594087
3521.193015	622773.297585	43.599092
3521.087136	622290.819697	43.604097
3521.239598	621822.202854	43.609101
3521.101774	621349.857801	43.614106
3521.233400	620880.101404	43.619111
3521.099004	620411.722778	43.624116
3521.326406	619941.758955	43.629121
3521.227410	619471.429617	43.634125
3520.988763	619012.177899	43.639130
3520.996808	618549.106288	43.644135
3520.929497	618086.378628	43.649140
3521.129546	617616.318886	43.654145
3520.825388	617158.854446	43.659149
3520.751682	616692.410145	43.664154
3520.865226	616229.773391	43.669159
3520.460073	615775.526275	43.674164
3520.633758	615309.431969	43.679169
3520.369928	614864.145741	43.684173
3520.801454	614405.789124	43.689178
3521.061662	613947.944013	43.694183
3520.737655	613492.435699	43.699188
3520.713898	613019.660449	43.704193
3520.690192	612575.594520	43.709197
3520.804620	612106.717644	43.714202
3521.161830	611647.457092	43.719207
3521.190867	611192.495908	43.724212
3520.800336	610727.558331	43.729217
3520.662854	610266.168880	43.734221
3520.490228	609820.413516	43.739226
3520.844024	609358.802379	43.744231
3520.558729	608894.372297	43.749236
3520.367761	608435.524476	43.754241
3520.680457	607981.888790	43.759245
3520.144290	607533.847302	43.764250
3520.693760	607089.114050	43.769255
3520.549682	606632.492122	43.774260
3520.345369	606178.169690	43.779265
3520.341929	605725.650954	43.784269
3520.342393	605284.552529	43.789274
3520.391672	604830.985591	43.794279
3520.223475	604381.150623	43.799284
3519.937209	603931.619055	43.804289
3520.015507	603478.896351	43.809293
3519.844909	603039.245293	43.814298
3520.188954	602595.023108	43.819303
3520.158817	602148.288083	43.824308
3520.105476	601711.526812	43.829313
3519.879707	601263.887288	43.834317
3520.006418	600818.278132	43.839322
3519.964085	600368.765490	43.844327
3519.601144	599932.390891	43.849332
3519.874874	599491.674518	43.854337
3519.765725	599058.687077	43.859341
3519.653133	598625.683984	43.864346
3519.701508	598190.177268	43.869351
3519.614659	597753.823781	43.874356
3519.696260	597311.149322	43.879361
3519.542103	596882.907983	43.884365
3519.571947	596452.912310	43.889370
3519.686436	596013.396256	43.894375
3519.528852	595581.191078	43.899380
3519.668286	595150.325222	43.904385
3519.839199	594717.881367	43.909389
3519.508251	594285.055244	43.914394
3519.355444	593851.831169	43.919399
3519.270916	593414.913159	43.924404
3519.539141	592982.539372	43.929409
3519.501209	592565.621571	43.934413
3519.163295	592133.872602	43.939418
3519.418762	591699.896849	43.944423
3519.417184	591271.072729	43.949428
3519.474959	590847.497503	43.954433
3519.039399	590422.082401	43.959437
3518.817779	589994.354822	43.964442
3519.442215	589570.436308	43.969447
3519.032608	589158.033734	43.974452
3518.918630	588728.132120	43.979457
3518.885637	588313.224354	43.984461
3518.946023	587887.332507	43.989466
3519.083667	587470.959471	43.994471
3518.511410	587050.220913	43.999476
3518.469339	586634.351993	44.004481
3518.597637	586226.580643	44.009485
3518.446498	585812.762301	44.014490
3518.667275	585397.006734	44.019495
3518.394417	584989.362488	44.024500
3518.626503	584571.515945	44.029505
3519.187502	584163.902526	44.034509
3518.736284	583756.347676	44.039514
3518.806872	583322.200133	44.044519
3518.558495	582919.659349	44.049524
3518.252717	582513.495674	44.054529
3518.226333	582100.031781	44.059533
3518.124444	581705.469109	44.064538
3518.388101	581304.547040	44.069543
3517.848994	580900.983722	44.074548
3518.385756	580491.491807	44.079553
3518.197563	580091.311009	44.084557
3518.150096	579679.377776	44.089562
3518.338472	579281.972290	44.094567
3518.036275	578890.671772	44.099572
3518.047327	578486.231144	44.104577
3517.980757	578091.797620	44.109581
3517.789697	577689.427149	44.114586
3518.221412	577289.300898	44.119591
3517.840747	576896.542446	44.124596
3518.240329	576495.390208	44.129601
3518.231824	576097.362685	44.134605
3518.022460	575698.853741	44.139610
3517.933432	575297.243293	44.144615
3517.796176	574910.818710	44.149620
3517.893636	574514.130890	44.154625
3517.620973	574114.727000	44.159629
3517.580358	573731.016098	44.164634
3517.980304	573328.655236	44.169639
3517.384651	572945.719346	44.174644
3517.718324	572558.739294	44.179649
3517.566946	572172.132017	44.184653
3517.347709	571779.436652	44.189658
3517.908922	571384.885133	44.194663
3517.509428	571009.554904	44.199668
3517.255493	570620.703715	44.204673
3517.722441	570238.158281	44.209677
3517.733800	569857.792534	44.214682
3517.869096	569462.649993	44.219687
3517.182897	569081.524621	44.224692
3517.293252	568681.983966	44.229697
3517.073990	568305.033228	44.234701
3516.851232	567933.054389	44.239706
3517.290099	567555.767854	44.244711
3517.208141	567169.298272	44.249716
3517.385270	566789.265647	44.254721
3517.826850	566413.102638	44.259725
3517.412804	566026.151968	44.264730
3517.285774	565649.107307	44.269735
3517.349934	565263.964858	44.274740
3517.202981	564874.920453	44.279745
3516.866362	564505.076682	44.284749
3516.964498	564134.846044	44.289754
3516.986366	563741.509922	44.294759
3516.736395	563387.226065	44.299764
3517.115585	563009.111732	44.304769
3517.195270	562633.806695	44.309773
3517.055140	562261.247250	44.314778
3516.746760	561882.311262	44.319783
3516.409799	561524.769041	44.324788
3516.436462	561147.063666	44.329793
3516.544057	560784.742360	44.334797
3516.554046	560434.916200	44.339802
3516.669913	560063.005715	44.344807
3516.638744	559698.361593	44.349812
3516.591213	559327.112842	44.354817
3516.619701	558966.265677	44.359821
3516.500710	558603.872528	44.364826
3516.410376	558233.708278	44.369831
3516.357231	557883.069568	44.374836
3516.275048	557511.674904	44.379841
3516.113902	557158.214815	44.384845
3515.854367	556799.473173	44.389850
3516.140675	556443.046502	44.394855
3516.256201	556093.893208	44.399860
3515.993683	555731.496360	44.404865
3516.129938	555390.179540	44.409869
3516.201381	555041.106938	44.414874
3516.212477	554684.377950	44.419879
3515.887508	554334.850795	44.424884
3516.269179	553986.654926	44.429889
3516.353594	553624.141701	44.434893
3515.861828	553280.762229	44.439898
3516.310040	552927.892212	44.444903
3515.439823	552578.110084	44.449908
3515.798181	552225.337773	44.454913
3515.981812	551891.381260	44.459917
3515.792488	551543.673175	44.464922
3515.748890	551183.484490	44.469927
3515.499954	550850.231214	44.474932
3515.871951	550503.610018	44.479937
3515.759619	550152.728637	44.484941
3515.793715	549828.523566	44.489946
3516.058024	549474.032588	44.494951
3515.990466	549131.180928	44.499956
3516.100116	548776.547022	44.504961
3516.041695	548440.127740	44.509965
3515.728555	548086.757766	44.514970
3516.026382	547734.131236	44.519975
3515.662648	547405.097718	44.524980
3515.454412	547057.278336	44.529985
3515.818471	546706.983246	44.534989
3515.307170	546370.338476	44.539994
3515.659698	546034.899084	44.544999
3515.529697	545695.753017	44.550004
3515.548355	545348.507108	44.555009
3515.860194	545018.797108	44.560013
3515.616056	544680.250595	44.565018
3515.874533	544330.669504	44.570023
3515.229339	544010.173978	44.575028
3515.125222	543663.209320	44.580033
3515.292568	543319.265325	44.585037
3515.187774	542999.813928	44.590042
3514.945698	542672.865621	44.595047
3514.697653	542343.843282	44.600052
3514.656089	542012.962630	44.605057
3514.890204	541694.734590	44.610061
3514.590790	541374.220314	44.615066
3514.882534	541042.906857	44.620071
3514.746363	540723.257568	44.625076
3514.627421	540400.723491	44.630081
3514.821825	540083.474358	44.635085
3514.527405	539761.611230	44.640090
3514.537942	539436.813918	44.645095
3514.401805	539132.813726	44.650100
3514.532619	538815.446094	44.655105
3514.296054	538502.068240	44.660109
3514.206632	538192.037755	44.665114
3514.403161	537884.322367	44.670119
3514.259465	537577.061936	44.675124
3514.310626	537257.100561	44.680129
3514.170003	536954.668643	44.685133
3514.368382	536652.979545	44.690138
3514.125730	536336.730137	44.695143
3514.090333	536028.560274	44.700148
3514.244975	535717.274011	44.705153
3513.972094	535424.266036	44.710157
3513.795744	535117.109611	44.715162
3514.150017	534809.755117	44.720167
3513.818315	534530.007552	44.725172
3513.778628	534230.628912	44.730177
3513.776386	533922.912727	44.735181
3513.835036	533622.344221	44.740186
3513.595336	533324.847772	44.745191
3513.431393	533032.579821	44.750196
3513.917987	532735.653653	44.755201
3513.610099	532451.875548	44.760205
3513.391920	532153.493550	44.765210
3514.148704	531852.668198	44.770215
3514.172149	531569.472276	44.775220
3514.121507	531264.786102	44.780225
3513.961352	530968.741672	44.785229
3513.753270	530671.740572	44.790234
3513.690797	530370.267520	44.795239
3513.642217	530080.443873	44.800244
3513.993034	529790.748171	44.805249
3513.795388	529497.557051	44.810253
3513.279510	529205.524754	44.815258
3513.490516	528903.015879	44.820263
3513.543238	528627.782974	44.825268
3513.379091	528337.793227	44.830273
3513.494542	528049.920437	44.835277
3513.228615	527765.034720	44.840282
3513.397299	527478.908344	44.845287
3513.014007	527196.252658	44.850292
3513.396099	526910.179800	44.855297
3513.085286	526628.560946	44.860301
3512.849089	526362.724320	44.865306
3513.224937	526074.011431	44.870311
3513.354184	525806.436577	44.875316
3513.297017	525516.878127	44.880321
3512.735824	525239.566760	44.885325
3512.258402	524960.569925	44.890330
3512.673037	524692.219549	44.895335
3512.674836	524433.325383	44.900340
3512.665709	524155.344265	44.905345
3512.799113	523888.340169	44.910349
3512.820001	523621.451507	44.915354
3513.026245	523341.853358	44.920359
3512.635823	523073.611450	44.925364
3512.905734	522805.453982	44.930369
3513.112302	522533.212609	44.935373
3512.934725	522257.042876	44.940378
3512.968814	521977.347791	44.945383
3512.657217	521705.432425	44.950388
3512.736613	521436.222735	44.955393
3512.545566	521168.367371	44.960397
3512.555469	520912.239131	44.965402
3512.760963	520633.449416	44.970407
3512.817876	520383.263160	44.975412
3512.548753	520111.412940	44.980417
3512.780085	519847.754763	44.985421
3512.744452	519576.259137	44.990426
3512.871929	519304.175284	44.995431
3512.641697	519054.167731	45.000436
3512.620152	518776.695917	45.005441
3512.824160	518504.736279	45.010445
3512.609838	518249.914738	45.015450
3512.428948	517980.082304	45.020455
3512.404962	517720.370671	45.025460
3512.366445	517457.171938	45.030465
3512.470370	517197.884225	45.035469
3512.316048	516937.828049	45.040474
3512.611065	516675.771288	45.045479
3512.307234	516425.127319	45.050484
3512.242848	516162.213959	45.055489
3512.423638	515910.064491	45.060493
3512.213379	515662.827204	45.065498
3512.129475	515406.926041	45.070503
3512.277695	515150.172742	45.075508
3512.463034	514889.822053	45.080513
3512.146668	514629.401102	45.085517
3511.962309	514393.607026	45.090522
3512.270133	514126.857130	45.095527
3512.018215	513882.579344	45.100532
3511.811838	513621.617540	45.105537
3512.010650	513375.840234	45.110541
3511.902795	513127.130502	45.115546
3511.970568	512876.517408	45.120551
3511.893531	512639.971169	45.125556
3511.859678	512380.828658	45.130561
3512.319095	512139.433786	45.135565
3511.938577	511896.763829	45.140570
3512.040853	511643.901924	45.145575
3511.862728	511399.320166	45.150580
3511.632268	511146.406022	45.155585
3511.708564	510900.863541	45.160589
3511.757291	510664.720905	45.165594
3511.887725	510415.624397	45.170599
3511.553837	510182.420253	45.175604
3511.842379	509932.783815	45.180609
3511.782966	509687.195131	45.185613
3511.666237	509455.206584	45.190618
3511.964328	509207.123712	45.195623
3511.770158	508968.874739	45.200628
3511.503178	508729.118485	45.205633
3511.674375	508485.291231	45.210637
3511.251644	508244.796196	45.215642
3511.329370	508002.645333	45.220647
3511.563422	507782.601157	45.225652
3511.273180	507542.780505	45.230657
3511.485591	507299.938961	45.235661
3511.444558	507078.820139	45.240666
3511.653357	506830.007972	45.245671
3511.352529	506612.768440	45.250676
3511.131978	506378.528952	45.255681
3511.537133	506140.539883	45.260685
3511.469258	505921.835945	45.265690
3511.354677	505674.173145	45.270695
3511.284730	505450.762223	45.275700
3511.239425	505216.172623	45.280705
3511.434852	504980.426416	45.285709
3511.085805	504756.143643	45.290714
3511.598050	504520.033334	45.295719
3511.477821	504288.122298	45.300724
3511.556502	504055.971774	45.305729
3511.569554	503819.936510	45.310733
3511.376637	503597.127661	45.315738
3511.402761	503355.674117	45.320743
3511.198554	503124.468585	45.325748
3511.250813	502883.306914	45.330753
3511.151570	502661.126504	45.335757
3510.813140	502442.017381	45.340762
3511.159148	502212.878983	45.345767
3510.903084	501993.547555	45.350772
3510.560349	501773.115668	45.355777
3511.081520	501555.516390	45.360781
3510.717070	501326.790270	45.365786
3510.806454	501114.062189	45.370791
3510.751096	500899.940315	45.375796
3510.590950	500681.434541	45.380801
3510.708112	500464.547131	45.385805
3510.758132	500254.899071	45.390810
3510.843603	500028.808583	45.395815
3510.791839	499824.936884	45.400820
3510.515318	499599.660818	45.405825
3510.874273	499382.616785	45.410829
3510.417445	499163.079663	45.415834
3510.464260	498956.652041	45.420839
3510.354795	498753.889516	45.425844
3510.193915	498542.384716	45.430849
3510.462086	498330.146551	45.435853
3510.533670	498121.175797	45.440858
3510.639417	497908.504849	45.445863
3510.185841	497707.912341	45.450868
3510.362499	497494.718285	45.455873
3510.068118	497284.737498	45.460877
3510.267232	497087.869696	45.465882
3509.989474	496882.129248	45.470887
3510.021729	496685.993255	45.475892
3510.193174	496479.715988	45.480897
3510.059213	496276.472354	45.485901
3510.031592	496080.491232	45.490906
3510.415934	495874.675953	45.495911
3510.229793	495668.753246	45.500916
3510.195154	495459.211032	45.505921
3510.315045	495266.634623	45.510925
3510.292210	495076.154177	45.515930
3510.092186	494864.457854	45.520935
3509.976758	494672.370069	45.525940
3510.120132	494465.465938	45.530945
3510.250607	494267.969867	45.535949
3509.838175	494075.673102	45.540954
3509.995484	493868.253461	45.545959
3509.975937	493662.328432	45.550964
3510.023627	493474.195383	45.555969
3510.179221	493273.951855	45.560973
3509.616188	493078.684948	45.565978
3510.016084	492869.896458	45.570983
3509.794907	492695.813267	45.575988
3509.760451	492506.267097	45.580993
3509.677484	492309.138822	45.585997
3509.466800	492122.754971	45.591002
3509.857122	491927.817996	45.596007
3509.595567	491730.561771	45.601012
3509.533747	491544.550922	45.606017
3509.513084	491353.724847	45.611021
3509.542430	491165.923626	45.616026
3509.604544	490974.573281	45.621031
3509.551872	490794.320278	45.626036
3509.339174	490608.375635	45.631041
3509.568505	490423.264203	45.636045
3509.600659	490253.767595	45.641050
3509.581571	490066.114416	45.646055
3509.489926	489877.560860	45.651060
3509.233210	489700.114007	45.656065
3509.342618	489507.727366	45.661069
3509.083573	489324.003043	45.666074
3509.506205	489149.419787	45.671079
3509.041883	488976.908948	45.676084
3509.009035	488799.971218	45.681089
3509.241079	488620.557684	45.686093
3508.794844	488455.628474	45.691098
3509.034864	488270.340375	45.696103
3509.201698	488100.799684	45.701108
3509.007050	487923.475843	45.706113
3508.978610	487754.572337	45.711117
3508.924600	487582.888428	45.716122
3509.106201	487407.974616	45.721127
3509.060154	487250.707902	45.726132
3508.969970	487067.791149	45.731137
3509.125296	486896.722600	45.736141
3508.878668	486726.884919	45.741146
3509.076162	486543.255699	45.746151
3509.016007	486378.595158	45.751156
3509.075426	486214.216293	45.756161
3509.249531	486039.543115	45.761165
3509.335911	485867.008687	45.766170
3509.229266	485680.588355	45.771175
3509.038284	485512.753733	45.776180
3508.824585	485338.797714	45.781185
3508.833821	485167.737257	45.786189
3509.034476	485013.647364	45.791194
3509.187790	484834.512111	45.796199
3508.911078	484661.218100	45.801204
3508.780022	484495.438604	45.806209
3508.819624	484320.872575	45.811213
3509.116800	484158.509019	45.816218
3509.017356	483992.567576	45.821223
3508.642691	483827.430769	45.826228
3508.738392	483660.390020	45.831233
3509.000629	483497.672082	45.836237
3508.536385	483334.216245	45.841242
3508.604838	483157.457408	45.846247
3508.496776	483005.882902	45.851252
3509.003855	482847.520764	45.856257
3508.976315	482685.755964	45.861261
3508.549357	482527.601078	45.866266
3508.762115	482360.730609	45.871271
3508.681622	482199.425996	45.876276
3508.585761	482037.211421	45.881281
3508.799828	481875.549882	45.886285
3508.437207	481716.364450	45.891290
3508.534176	481554.922485	45.896295
3508.433743	481407.483919	45.901300
3508.663823	481240.195081	45.906305
3508.579702	481078.830370	45.911309
3508.275683	480928.284123	45.916314
3508.240226	480765.440265	45.921319
3507.967612	480619.948261	45.926324
3508.143853	480462.633969	45.931329
3508.358065	480323.637404	45.936333
3508.170913	480173.874859	45.941338
3508.488049	480026.708038	45.946343
3508.147619	479871.501763	45.951348
3508.298933	479717.627687	45.956353
3508.214050	479565.918891	45.961357
3508.326655	479419.693302	45.966362
3508.210681	479260.494652	45.971367
3508.245004	479113.216805	45.976372
3508.036280	478963.447911	45.981377
3507.908803	478816.448412	45.986381
3507.704719	478684.497243	45.991386
3507.963085	478528.620308	45.996391
3507.829084	478397.718280	46.001396
3508.043544	478253.440410	46.006401
3508.340559	478097.198775	46.011405
3507.912503	477959.356947	46.016410
3507.853127	477811.831398	46.021415
3507.956821	477670.605633	46.026420
3507.782994	477533.679156	46.031425
3508.032848	477393.641434	46.036429
3507.973825	477257.351491	46.041434
3507.999126	477107.071677	46.046439
3508.018862	476965.551003	46.051444
3507.988869	476819.278233	46.056449
3507.845022	476671.909801	46.061453
3507.823537	476546.747480	46.066458
3507.750177	476402.757304	46.071463
3507.867736	476266.024760	46.076468
3507.577256	476120.803582	46.081473
3507.651537	475980.987579	46.086477
3507.337381	475844.831964	46.091482
3507.591772	475712.629142	46.096487
3507.486884	475586.006074	46.101492
3507.766744	475456.733973	46.106497
3507.895874	475313.257694	46.111501
3507.371248	475196.527202	46.116506
3507.406202	475062.027863	46.121511
3507.782336	474923.215688	46.126516
3507.596590	474793.562697	46.131521
3507.438728	474657.624820	46.136525
3507.155691	474535.785015	46.141530
3507.485210	474405.484295	46.146535
3507.467451	474281.217462	46.151540
3507.310455	474148.871132	46.156545
3507.907270	474014.065682	46.161549
3507.116796	473896.055715	46.166554
3507.186782	473761.439664	46.171559
3507.093463	473637.232059	46.176564
3507.215543	473505.745043	46.181569
3507.509895	473381.975963	46.186573
3507.131111	473254.168293	46.191578
3507.394418	473127.414902	46.196583
3507.795963	473009.600922	46.201588
3507.592290	472885.862936	46.206593
3507.759197	472742.360323	46.211597
3507.619672	472617.546080	46.216602
3507.239467	472492.873386	46.221607
3506.896506	472369.966079	46.226612
3506.626764	472240.410911	46.231617
3506.951578	472124.427686	46.236621
3506.911366	472011.950000	46.241626
3507.081281	471883.178275	46.246631
3507.090937	471770.336099	46.251636
3507.116623	471651.514160	46.256641
3507.237348	471524.369075	46.261645
3507.020690	471403.307812	46.266650
3506.931757	471291.745784	46.271655
3506.705384	471182.789624	46.276660
3506.689905	471057.032137	46.281665
3507.052368	470945.137738	46.286669
3507.079949	470851.888111	46.291674
3506.880455	470713.649398	46.296679
3506.939718	470614.568488	46.301684
3506.775713	470494.809284	46.306689
3506.753511	470369.757460	46.311693
3506.717832	470251.393013	46.316698
3507.005764	470150.751101	46.321703
3506.753893	470035.967792	46.326708
3506.796321	469931.010611	46.331713
3506.918798	469814.287929	46.336717
3506.747314	469708.150388	46.341722
3506.819487	469585.913792	46.346727
3506.799847	469474.633106	46.351732
3506.534798	469370.991642	46.356737
3506.778996	469258.803538	46.361741
3506.888530	469152.209676	46.366746
3506.739598	469037.402740	46.371751
3506.899416	468933.737001	46.376756
3506.522656	468826.413872	46.381761
3506.847769	468705.394785	46.386765
3506.594452	468621.249361	46.391770
3506.980727	468498.445585	46.396775
3506.677230	468382.445356	46.401780
3506.601185	468279.474851	46.406785
3506.815929	468165.816308	46.411789
3506.344743	468064.583770	46.416794
3506.406087	467959.409844	46.421799
3506.709875	467852.066342	46.426804
3506.667086	467740.880787	46.431809
3506.678537	467634.801760	46.436813
3506.449837	467537.223039	46.441818
3506.590850	467427.068096	46.446823
3506.501429	467324.094726	46.451828
3506.482891	467227.491715	46.456833
3506.680538	467128.622304	46.461837
3506.322999	467027.162232	46.466842
3506.204150	466927.585934	46.471847
3506.558972	466833.146212	46.476852
3506.577473	466721.944280	46.481857
3506.612469	466618.439278	46.486861
3506.632223	466522.991373	46.491866
3506.709174	466407.572805	46.496871
3506.708031	466308.479813	46.501876
3506.718056	466199.657388	46.506881
3506.620150	466087.965053	46.511885
3506.292667	465995.562870	46.516890
3506.414727	465896.142749	46.521895
3506.454520	465789.947370	46.526900
3506.463629	465685.783163	46.531905
3506.644692	465584.578162	46.536909
3506.343723	465491.561080	46.541914
3506.376856	465383.034086	46.546919
3506.536857	465288.569401	46.551924
3506.170579	465190.546291	46.556929
3506.449640	465086.991401	46.561933
3506.511324	464989.147523	46.566938
3506.539727	464880.922510	46.571943
3506.526716	464793.274060	46.576948
3506.520742	464685.155155	46.581953
3506.746325	464584.494648	46.586957
3506.216660	464500.935689	46.591962
3506.207663	464393.474334	46.596967
3506.301781	464296.178753	46.601972
3506.227431	464203.066127	46.606977
3506.408205	464097.394737	46.611981
3506.192782	464010.435988	46.616986
3506.281926	463912.176659	46.621991
3505.993467	463815.248003	46.626996
3506.256558	463723.139489	46.632001
3506.405986	463629.327227	46.637005
3505.920378	463546.364663	46.642010
3506.050501	463442.573106	46.647015
3506.133562	463356.472513	46.652020
3505.776335	463273.182853	46.657025
3505.912794	463177.445206	46.662029
3505.754515	463096.096930	46.667034
3505.902404	463001.673881	46.672039
3506.009560	462914.047129	46.677044
3505.950481	462832.123447	46.682049
3506.106373	462737.343065	46.687053
3505.459247	462657.191185	46.692058
3505.973216	462569.088064	46.697063
3505.826176	462484.441712	46.702068
3505.899694	462398.743907	46.707073
3505.699758	462309.900103	46.712077
3505.710213	462228.215383	46.717082
3506.135825	462150.411863	46.722087
3506.051492	462060.331061	46.727092
3505.563365	461971.382915	46.732097
3505.884330	461881.485455	46.737101
3505.453804	461812.491822	46.742106
3505.876587	461722.626925	46.747111
3505.971726	461652.225474	46.752116
3505.751128	461566.574262	46.757121
3505.976388	461475.880515	46.762125
3505.809860	461395.590752	46.767130
3505.795266	461301.187277	46.772135
3505.687933	461233.859359	46.777140
3505.779515	461144.656474	46.782145
3505.998390	461056.444950	46.787149
3505.901411	460983.236121	46.792154
3505.906056	460892.374663	46.797159
3505.856658	460807.552405	46.802164
3505.596167	460713.694864	46.807169
3505.905127	460638.388415	46.812173
3505.729102	460555.816443	46.817178
3505.682555	460475.502456	46.822183
3505.970484	460400.350723	46.827188
3505.371247	460322.512284	46.832193
3506.012735	460237.012175	46.837197
3505.389125	460163.738203	46.842202
3505.648287	460082.154173	46.847207
3505.970764	460016.117016	46.852212
3505.637591	459925.156772	46.857217
3505.786619	459850.584131	46.862221
3505.658449	459761.868646	46.867226
3505.663898	459683.519028	46.872231
3505.888232	459603.053904	46.877236
3505.907537	459525.613514	46.882241
3505.910823	459442.043396	46.887245
3505.899646	459369.270072	46.892250
3505.816904	459274.817908	46.897255
3505.999026	459198.159316	46.902260
3505.503705	459126.329324	46.907265
3505.989076	459048.858184	46.912269
3505.882979	458967.889436	46.917274
3505.928061	458877.873428	46.922279
3505.446393	458801.377331	46.927284
3505.559938	458732.837566	46.932289
3505.791772	458643.295422	46.937293
3505.606656	458570.903655	46.942298
3505.826158	458501.027292	46.947303
3505.966333	458411.753170	46.952308
3505.605317	458336.501734	46.957313
3505.859663	458243.254185	46.962317
3505.432851	458171.257014	46.967322
3505.860310	458093.589338	46.972327
3505.756160	458015.555986	46.977332
3505.584907	457939.814516	46.982337
3505.462662	457855.853740	46.987341
3505.524818	457793.908334	46.992346
3505.928662	457725.214191	46.997351
3505.855056	457650.265890	47.002356
3505.572062	457564.354683	47.007361
3505.632493	457489.332213	47.012365
3505.471957	457421.544341	47.017370
3505.331822	457343.767945	47.022375
3505.632349	457266.524222	47.027380
3505.502087	457199.287963	47.032385
3505.453015	457117.896532	47.037389
3505.476880	457052.508807	47.042394
3505.451970	456972.430476	47.047399
3505.551399	456902.721115	47.052404
3505.578894	456828.563461	47.057409
3505.622875	456747.408075	47.062413
3505.417758	456682.767852	47.067418
3505.665948	456599.498879	47.072423
3505.690856	456528.280364	47.077428
3505.353559	456474.306181	47.082433
3505.604308	456396.966259	47.087437
3504.946730	456322.214105	47.092442
3505.322337	456254.128019	47.097447
3505.391936	456191.365427	47.102452
3505.369047	456122.282508	47.107457
3505.419752	456047.611154	47.112461
3505.169395	455978.617271	47.117466
3505.057114	455904.733535	47.122471
3505.196225	455839.626340	47.127476
3505.304677	455784.357693	47.132481
3505.203567	455713.816778	47.137485
3505.500249	455648.935510	47.142490
3505.321134	455573.338567	47.147495
3505.303556	455504.708837	47.152500
3505.064967	455448.940954	47.157505
3505.105843	455378.374632	47.162509
3505.005254	455319.794923	47.167514
3505.193131	455251.737532	47.172519
3505.129202	455184.686013	47.177524
3505.155902	455127.097809	47.182529
3505.075646	455062.228340	47.187533
3505.147731	455010.410722	47.192538
3505.097780	454936.563515	47.197543
3505.393696	454878.725882	47.202548
3505.119293	454809.225230	47.207553
3505.414350	454744.189284	47.212557
3505.031810	454680.637485	47.217562
3505.060098	454618.029163	47.222567
3505.087390	454549.084406	47.227572
3504.571086	454494.679302	47.232577
3504.674787	454434.186582	47.237581
3504.855290	454386.454888	47.242586
3504.717487	454325.090630	47.247591
3504.816719	454262.215646	47.252596
3504.911917	454212.318354	47.257601
3505.253603	454149.857856	47.262605
3504.805819	454098.532228	47.267610
3504.838955	454032.829049	47.272615
3504.862503	453975.440907	47.277620
3504.798888	453921.970838	47.282625
3504.988552	453858.724325	47.287629
3504.948795	453810.623353	47.292634
3504.913918	453743.359370	47.297639
3505.063786	453691.373049	47.302644
3505.275096	453628.020742	47.307649
3505.706129	453559.966897	47.312653
3504.891687	453501.909411	47.317658
3504.887594	453445.538385	47.322663
3505.190953	453383.284875	47.327668
3504.810047	453316.281352	47.332673
3504.316912	453263.389849	47.337677
3504.467210	453215.001559	47.342682
3504.856193	453154.101490	47.347687
3504.910220	453105.780076	47.352692
3504.751589	453060.283083	47.357697
3504.816575	453001.567075	47.362701
3504.722095	452947.136531	47.367706
3504.546606	452897.434348	47.372711
3505.034722	452844.881179	47.377716
3504.627984	452798.057191	47.382721
3504.582610	452729.372204	47.387725
3504.616404	452684.247092	47.392730
3504.589335	452625.748514	47.397735
3504.706127	452582.687547	47.402740
3504.415244	452530.317284	47.407745
3504.709371	452481.395751	47.412749
3504.563095	452431.890243	47.417754
3504.613262	452385.494268	47.422759
3504.841373	452318.586298	47.427764
3504.227086	452278.944819	47.432769
3504.434851	452223.903094	47.437773
3504.374012	452192.379872	47.442778
3504.759546	452127.877868	47.447783
3504.688743	452091.185069	47.452788
3504.407840	452041.346731	47.457793
3504.643517	451990.760999	47.462797
3504.413804	451947.048105	47.467802
3504.367137	451894.381043	47.472807
3504.395197	451835.059648	47.477812
3504.223914	451803.503993	47.482817
3504.504729	451761.021687	47.487821
3504.433201	451713.985909	47.492826
3504.503634	451670.880261	47.497831
3504.616163	451614.991306	47.502836
3504.208944	451584.590971	47.507841
3504.336339	451526.772692	47.512845
3504.654328	451485.500245	47.517850
3504.672004	451443.873401	47.522855
3504.471862	451398.836128	47.527860
3504.355192	451350.894651	47.532865
3504.558763	451291.744532	47.537869
3504.605969	451262.584316	47.542874
3504.353287	451203.004853	47.547879
3504.765180	451169.827673	47.552884
3504.295611	451109.676579	47.557889
3504.737424	451068.432863	47.562893
3504.330060	451021.909157	47.567898
3504.541805	450973.910735	47.572903
3504.750914	450928.599765	47.577908
3504.370290	450885.366703	47.582913
3504.914482	450822.050363	47.587917
3504.647248	450796.289414	47.592922
3504.612663	450734.795451	47.597927
3504.934644	450701.531477	47.602932
3504.813950	450645.629037	47.607937
3504.877442	450587.869761	47.612941
3504.743678	450539.675828	47.617946
3504.825199	450493.827985	47.622951
3504.551199	450448.243550	47.627956
3504.556920	450395.310237	47.632961
3504.562323	450349.069460	47.637965
3504.476122	450305.632818	47.642970
3504.631297	450267.833478	47.647975
3504.670513	450205.666230	47.652980
3504.474331	450171.627952	47.657985
3504.651029	450112.986098	47.662989
3504.323839	450084.902205	47.667994
3504.631808	450027.099635	47.672999
3504.568278	449993.444037	47.678004
3504.464184	449940.832537	47.683009
3504.489989	449891.139485	47.688013
3504.004278	449839.759054	47.693018
3504.336601	449796.706219	47.698023
3504.545458	449764.524833	47.703028
3504.255806	449722.389294	47.708033
3504.143988	449692.594895	47.713037
3504.380314	449639.062558	47.718042
3504.348647	449600.279847	47.723047
3504.463934	449566.035292	47.728052
3504.313672	449524.534700	47.733057
3504.841232	449476.935250	47.738061
3504.405759	449432.795876	47.743066
3504.152496	449389.791488	47.748071
3504.406756	449347.004580	47.753076
3504.321421	449306.506551	47.758081
3504.126128	449264.911726	47.763085
3504.220709	449219.870131	47.768090
3504.331217	449191.558191	47.773095
3504.410489	449147.482439	47.778100
3504.101617	449108.644742	47.783105
3504.380567	449070.619291	47.788109
3504.000061	449034.075400	47.793114
3504.106276	448989.386258	47.798119
3504.535576	448959.904066	47.803124
3504.176623	448927.970464	47.808129
3504.153978	448881.731239	47.813133
3504.218482	448855.454909	47.818138
3504.441961	448814.193329	47.823143
3504.386738	448770.241162	47.828148
3504.132233	448739.252843	47.833153
3504.521355	448696.441585	47.838157
3504.278285	448659.569342	47.843162
3504.225854	448611.712027	47.848167
3504.767600	448565.172916	47.853172
3504.382520	448533.598118	47.858177
3504.147180	448488.611291	47.863181
3504.293972	448460.241466	47.868186
3503.992510	448411.158561	47.873191
3504.191937	448379.534436	47.878196
3504.024637	448352.080104	47.883201
3504.314517	448297.166135	47.888205
3504.339135	448264.963207	47.893210
3504.436598	448227.322170	47.898215
3504.254849	448183.187555	47.903220
3504.039839	448150.873248	47.908225
3504.510438	448120.926471	47.913229
3504.631455	448083.230449	47.918234
3504.525546	448032.389231	47.923239
3504.445985	448001.775614	47.928244
3504.444748	447959.384466	47.933249
3504.772487	447907.911124	47.938253
3504.627526	447868.840323	47.943258
3504.458634	447822.877286	47.948263
3504.702101	447787.289554	47.953268
3504.455873	447748.337236	47.958273
3504.910924	447696.182440	47.963277
3504.590220	447654.352308	47.968282
3504.675668	447601.246223	47.973287
3504.699983	447563.616495	47.978292
3504.474746	447522.936095	47.983297
3504.770325	447479.327011	47.988301
3504.722592	447431.871890	47.993306
3504.421135	447400.433243	47.998311
3504.402148	447347.344354	48.003316
3504.532322	447316.693935	48.008321
3504.532915	447280.031224	48.013325
3504.144064	447237.501978	48.018330
3503.764265	447194.007626	48.023335
3503.904689	447149.460881	48.028340
3503.806938	447118.950512	48.033345
3503.802668	447085.077312	48.038349
3504.034212	447068.861428	48.043354
3503.901860	447046.318258	48.048359
3504.100610	446998.718663	48.053364
3504.224681	446976.334474	48.058369
3504.029980	446948.883000	48.063373
3504.045574	446915.969625	48.068378
3504.146877	446871.530398	48.073383
3504.393995	446845.118971	48.078388
3503.820417	446807.235019	48.083393
3503.933841	446767.965941	48.088397
3503.931606	446747.682198	48.093402
3503.804446	446716.618460	48.098407
3504.061728	446667.943214	48.103412
3503.778375	446646.997428	48.108417
3503.985910	446623.026590	48.113421
3503.842990	446602.766730	48.118426
3503.614946	446559.802984	48.123431
3503.977936	446518.006007	48.128436
3503.576523	446508.895866	48.133441
3503.801331	446485.885431	48.138445
3504.257467	446469.022212	48.143450
3503.729849	446428.188501	48.148455
3503.927364	446394.229036	48.153460
3503.504141	446373.053306	48.158465
3503.864139	446347.230524	48.163469
3503.773106	446329.750664	48.168474
3503.985334	446294.419323	48.173479
3503.836272	446253.064237	48.178484
3503.802699	446236.132315	48.183489
3503.770548	446207.891457	48.188493
3503.927172	446184.892341	48.193498
3503.781279	446137.755362	48.198503
3504.117580	446120.050230	48.203508
3503.889832	446102.137120	48.208513
3504.075110	446065.795766	48.213517
3503.625895	446026.469255	48.218522
3503.862417	445995.190233	48.223527
3504.288310	445978.382503	48.228532
3504.052685	445956.058660	48.233537
3504.050096	445909.505256	48.238541
3504.226148	445891.066612	48.243546
3504.107175	445865.578592	48.248551
3504.245340	445824.782182	48.253556
3504.068997	445803.513020	48.258561
3503.966883	445769.806574	48.263565
3503.864753	445729.913126	48.268570
3503.694805	445698.956637	48.273575
3503.724288	445669.842427	48.278580
3503.783543	445653.807026	48.283585
3503.806460	445626.468829	48.288589
3503.655906	445600.123764	48.293594
3503.753153	445569.020039	48.298599
3503.598286	445557.382451	48.303604
3503.708552	445537.281202	48.308609
3503.759450	445510.698778	48.313613
3503.572106	445507.079397	48.318618
3503.934944	445465.838236	48.323623
3503.982551	445427.896480	48.328628
3503.798852	445416.466592	48.333633
3503.878433	445392.516223	48.338637
3503.507747	445380.002545	48.343642
3503.788094	445347.700824	48.348647
3503.576005	445301.486150	48.353652
3503.974365	445295.991747	48.358657
3503.718513	445263.781453	48.363661
3503.571686	445256.960141	48.368666
3503.483349	445226.242603	48.373671
3503.564678	445195.394623	48.378676
3503.265706	445166.082241	48.383681
3503.519865	445135.863948	48.388685
3503.333335	445120.225113	48.393690
3503.367200	445106.374346	48.398695
3503.647433	445091.568648	48.403700
3503.180432	445081.809809	48.408705
3503.255907	445065.061198	48.413709
3503.748077	445041.648562	48.418714
3503.523534	445032.609017	48.423719
3503.449627	445013.045867	48.428724
3503.313203	445013.018431	48.433729
3503.671962	444989.070659	48.438733
3503.566276	444974.178630	48.443738
3503.821954	444945.582675	48.448743
3503.934075	444911.229724	48.453748
3503.656466	444893.679118	48.458753
3503.993019	444866.438546	48.463757
3503.566716	444853.528338	48.468762
3503.520461	444836.851049	48.473767
3503.884620	444796.876249	48.478772
3503.581378	444774.359859	48.483777
3503.383296	444749.746174	48.488781
3503.327451	444732.563291	48.493786
3503.490411	444722.189574	48.498791
3503.445061	444707.084198	48.503796
3503.498651	444700.938501	48.508801
3503.493686	444673.350275	48.513805
3503.776620	444659.355262	48.518810
3503.517528	444649.053574	48.523815
3503.875416	444620.541166	48.528820
3503.354964	444590.758661	48.533825
3503.401100	444560.930088	48.538829
3503.674236	444559.818411	48.543834
3503.491460	444534.897574	48.548839
3503.895279	444517.534603	48.553844
3503.496254	444506.445289	48.558849
3504.066111	444490.524699	48.563853
3503.658062	444457.477016	48.568858
3503.461620	444427.436098	48.573863
3503.921276	444409.809928	48.578868
3503.331630	444397.586641	48.583873
3503.449059	444381.996801	48.588877
3503.668061	444370.396164	48.593882
3503.492090	444354.450672	48.598887
3503.597781	444342.260776	48.603892
3503.486325	444314.538126	48.608897
3503.734706	444275.748599	48.613901
3503.522575	444261.634994	48.618906
3503.460216	444251.705252	48.623911
3503.778782	444229.487851	48.628916
3503.466901	444226.599545	48.633921
3503.520310	444199.152894	48.638925
3503.577543	444197.621616	48.643930
3503.764661	444167.971294	48.648935
3503.547173	444126.015192	48.653940
3503.629267	444110.025456	48.658945
3504.027141	444093.170325	48.663949
3503.919134	444074.930776	48.668954
3503.443228	444061.014228	48.673959
3503.814279	444047.206640	48.678964
3503.771803	444013.690123	48.683969
3504.152027	443985.984532	48.688973
3503.616176	443973.650384	48.693978
3503.527345	443960.682017	48.698983
3503.378402	443946.608133	48.703988
3503.340581	443929.573683	48.708993
3503.677297	443899.796016	48.713997
3503.612086	443865.420960	48.719002
3503.410349	443850.595271	48.724007
3503.819004	443832.115148	48.729012
3503.564887	443822.775840	48.734017
3503.526865	443797.220827	48.739021
3503.289099	443796.449933	48.744026
3503.313474	443778.999007	48.749031
3503.337689	443769.307848	48.754036
3503.378846	443760.425269	48.759041
3503.285825	443742.690054	48.764045
3503.282350	443727.881146	48.769050
3503.040078	443704.846053	48.774055
3503.305739	443704.597807	48.779060
3503.181607	443700.003695	48.784065
3503.279984	443683.858712	48.789069
3503.390080	443670.551899	48.794074
3503.422655	443661.924334	48.799079
3503.671221	443643.775690	48.804084
3503.255878	443642.375781	48.809089
3503.325270	443624.054844	48.814093
3503.445991	443610.340438	48.819098
3503.490061	443597.044854	48.824103
3503.480215	443557.892389	48.829108
3503.609351	443547.118141	48.834113
3503.800063	443515.944775	48.839117
3503.524314	443516.499022	48.844122
3503.462409	443499.671218	48.849127
3503.543402	443484.695567	48.854132
3503.295926	443478.043030	48.859137
3503.659387	443459.063125	48.864141
3503.638945	443451.002427	48.869146
3503.651845	443419.554975	48.874151
3503.566287	443394.109038	48.879156
3503.371325	443375.883746	48.884161
3503.578108	443352.720885	48.889165
3503.564939	443347.042667	48.894170
3503.390908	443334.697092	48.899175
3503.590255	443311.687612	48.904180
3503.292140	443310.825567	48.909185
3503.733525	443292.440833	48.914189
3503.682990	443284.537366	48.919194
3503.700426	443270.079604	48.924199
3503.425493	443228.537317	48.929204
3503.219203	443211.784661	48.934209
3503.571526	443198.892667	48.939213
3503.596619	443183.622042	48.944218
3503.355862	443177.576889	48.949223
3503.686887	443162.304731	48.954228
3503.405427	443154.187052	48.959233
3503.630675	443141.621035	48.964237
3503.409218	443130.196379	48.969242
3503.685299	443115.795790	48.974247
3503.653469	443102.107111	48.979252
3503.547505	443074.889122	48.984257
3503.336453	443046.066034	48.989261
3503.423005	443040.319990	48.994266
3503.559722	443024.269407	48.999271
3503.675596	443007.765899	49.004276
3503.313609	443004.632387	49.009281
3503.516390	442993.743852	49.014285
3503.511666	442985.731016	49.019290
3503.561183	442974.970079	49.024295
3503.864202	442960.615507	49.029300
3503.626472	442944.425923	49.034305
3503.453147	442909.763496	49.039309
3503.601052	442905.528520	49.044314
3503.228242	442887.738939	49.049319
3503.525971	442872.573702	49.054324
3503.594416	442878.242576	49.059329
3504.004000	442856.718300	49.064333
3504.083807	442840.271543	49.069338
3503.620233	442805.709228	49.074343
3503.883624	442781.115944	49.079348
3503.701762	442777.038689	49.084353
3504.079204	442757.142832	49.089357
3504.030460	442722.661713	49.094362
3503.273781	442698.090348	49.099367
3503.652238	442686.461586	49.104372
3503.299838	442675.667686	49.109377
3503.598529	442654.466465	49.114381
3503.402728	442644.051571	49.119386
3503.196142	442632.979153	49.124391
3503.405604	442617.524490	49.129396
3502.995301	442614.703490	49.134401
3503.140932	442598.549632	49.139405
3503.492719	442601.177714	49.144410
3503.019800	442590.911551	49.149415
3503.537924	442570.991504	49.154420
3503.168516	442562.432138	49.159425
3503.351253	442556.415942	49.164429
3503.182006	442546.300788	49.169434
3503.240983	442529.705193	49.174439
3503.566765	442513.875553	49.179444
3503.361471	442518.171093	49.184449
3503.406839	442504.215255	49.189453
3503.089182	442486.872411	49.194458
3503.020769	442482.522128	49.199463
3503.167453	442470.983546	49.204468
3503.199786	442469.912882	49.209473
3503.285738	442458.536824	49.214477
3502.985827	442443.726935	49.219482
3503.282220	442432.872857	49.224487
3503.289277	442419.430710	49.229492
3502.989021	442418.873317	49.234497
3503.382708	442408.357657	49.239501
3503.381615	442395.170490	49.244506
3502.938153	442379.827142	49.249511
3503.336576	442374.230554	49.254516
3503.554788	442361.208803	49.259521
3503.306607	442350.396947	49.264525
3503.164849	442339.820518	49.269530
3503.234998	442337.678256	49.274535
3503.635612	442326.146961	49.279540
3502.804354	442326.643925	49.284545
3503.355092	442315.492756	49.289549
3503.428857	442304.930231	49.294554
3502.872859	442295.996853	49.299559
3503.383914	442284.497400	49.304564
3503.062616	442268.423022	49.309569
3503.042439	442260.615441	49.314573
3503.313304	442276.343359	49.319578
3503.089279	442276.330875	49.324583
3503.077200	442265.732267	49.329588
3503.107673	442267.806604	49.334593
3503.616095	442267.161849	49.339597
3503.189720	442265.155080	49.344602
3503.287175	442253.675510	49.349607
3503.219680	442239.434448	49.354612
3503.350811	442234.137068	49.359617
3503.019680	442222.172730	49.364621
3502.890167	442218.542920	49.369626
3503.022981	442199.905627	49.374631
3503.176347	442189.684502	49.379636
3503.387361	442184.627075	49.384641
3502.924979	442172.127188	49.389645
3503.116588	442170.319219	49.394650
3503.135871	442164.178661	49.399655
3503.243448	442147.168708	49.404660
3503.158253	442146.016653	49.409665
3503.448232	442133.439003	49.414669
3503.173284	442130.493386	49.419674
3502.990404	442118.808005	49.424679
3503.266800	442104.254531	49.429684
3503.273378	442105.267817	49.434689
3503.125601	442090.736038	49.439693
3503.546420	442084.222570	49.444698
3503.348759	442079.894275	49.449703
3503.416408	442073.694712	49.454708
3503.416003	442070.905094	49.459713
3503.193570	442050.502364	49.464717
3503.303365	442043.534776	49.469722
3503.104647	442032.308545	49.474727
3503.000178	442026.036914	49.479732
3502.972954	442022.693934	49.484737
3503.214508	442038.376308	49.489741
3503.373507	442044.790759	49.494746
3503.075349	442031.248323	49.499751
3503.300745	442027.608603	49.504756
3503.407352	442032.662525	49.509761
3503.203747	442017.075081	49.514765
3503.375684	442010.096872	49.519770
3503.290377	442005.191442	49.524775
3503.464929	441987.713435	49.529780
3503.068155	441960.797315	49.534785
3503.273355	441953.762687	49.539789
3503.141233	441956.372031	49.544794
3503.153202	441955.101933	49.549799
3503.116109	441953.637326	49.554804
3503.436928	441946.633676	49.559809
3503.495567	441937.087987	49.564813
3503.500809	441927.703577	49.569818
3503.069207	441896.025489	49.574823
3503.711411	441888.814780	49.579828
3503.612785	441879.245197	49.584833
3503.297168	441850.641266	49.589837
3503.283240	441844.151236	49.594842
3503.289710	441837.809887	49.599847
3503.618974	441822.587815	49.604852
3503.798014	441818.905254	49.609857
3503.954839	441807.364590	49.614861
3503.667324	441796.001233	49.619866
3503.427105	441792.085923	49.624871
3503.481383	441761.034785	49.629876
3503.335012	441738.488450	49.634881
3503.158259	441723.403432	49.639885
3503.228973	441709.290592	49.644890
3503.014904	441709.885072	49.649895
3502.976847	441714.456547	49.654900
3502.861746	441736.388134	49.659905
3503.425226	441723.256329	49.664909
3502.844014	441720.819448	49.669914
3502.964832	441722.320467	49.674919
3503.156367	441710.165160	49.679924
3503.010607	441703.038210	49.684929
3503.311496	441689.291833	49.689933
3503.499293	441680.839867	49.694938
3503.490138	441672.675138	49.699943
3503.424682	441658.940572	49.704948
3503.102876	441665.538674	49.709953
3503.159174	441641.233079	49.714957
3503.342710	441643.484229	49.719962
3503.130601	441634.897639	49.724967
3503.284677	441628.175969	49.729972
3502.874844	441624.644646	49.734977
3502.756164	441616.042096	49.739981
3502.946854	441618.241305	49.744986
3502.950441	441628.689479	49.749991
3502.976473	441635.532533	49.754996
3502.711430	441639.483390	49.760001
3502.790276	441625.470552	49.765005
3502.713332	441623.911283	49.770010
3503.011056	441621.172148	49.775015
3503.393109	441625.012520	49.780020
3503.352925	441627.251149	49.785025
3503.351895	441608.737650	49.790029
3503.561625	441592.876438	49.795034
3503.735742	441581.941372	49.800039
3503.735449	441568.195622	49.805044
3503.341184	441567.552812	49.810049
3503.528214	441559.608155	49.815053
3503.441464	441554.601426	49.820058
3503.070923	441552.990836	49.825063
3503.365079	441538.332509	49.830068
3503.175555	441533.444768	49.835073
3503.477018	441518.176509	49.840077
3503.298743	441513.895514	49.845082
3502.854160	441509.406375	49.850087
3502.739840	441501.716042	49.855092
3502.590134	441502.857487	49.860097
3502.642113	441493.921413	49.865101
3502.940365	441500.515138	49.870106
3503.046502	441497.453643	49.875111
3502.937033	441497.776655	49.880116
3502.657921	441494.933107	49.885121
3502.710454	441481.888400	49.890125
3503.023218	441490.356388	49.895130
3502.862645	441505.346967	49.900135
3503.255178	441502.135126	49.905140
3502.955552	441507.816481	49.910145
3503.249473	441493.513223	49.915149
3503.499505	441495.042918	49.920154
3502.971838	441492.546145	49.925159
3503.039773	441479.701697	49.930164
3502.964128	441474.540885	49.935169
3503.321988	441471.233515	49.940173
3503.194703	441469.784275	49.945178
3503.014770	441462.460190	49.950183
3503.563361	441449.330764	49.955188
3502.868256	441449.804495	49.960193
3503.175340	441435.498951	49.965197
3503.187312	441427.685583	49.970202
3503.094171	441425.824728	49.975207
3503.404462	441416.793795	49.980212
3503.240588	441419.459347	49.985217
3503.110502	441399.699637	49.990221
3503.287680	441407.987917	49.995226
3503.297808	441421.275553	50.000231
3503.320245	441400.221731	50.005236
3503.022435	441410.670749	50.010241
3503.175588	441411.557594	50.015245
3503.057388	441409.092343	50.020250
3502.681294	441409.359435	50.025255
3502.920465	441402.826059	50.030260
3502.802711	441403.606992	50.035265
3503.255220	441384.052130	50.040269
3502.807996	441382.911127	50.045274
3502.799426	441380.072093	50.050279
3503.065729	441401.076603	50.055284
3502.957491	441409.667230	50.060289
3502.830582	441409.283102	50.065293
3503.074359	441398.386773	50.070298
3502.653712	441396.531113	50.075303
3503.374569	441386.517053	50.080308
3502.770650	441384.489793	50.085313
3502.926560	441376.296770	50.090317
3502.795328	441391.941814	50.095322
3502.476697	441397.981502	50.100327
3502.807894	441398.787225	50.105332
3502.918741	441402.318884	50.110337
3502.542971	441386.405325	50.115341
3502.890083	441405.265672	50.120346
3503.194790	441418.097229	50.125351
3503.091321	441413.904886	50.130356
3502.847390	441409.077130	50.135361
3502.878801	441406.789224	50.140365
3502.926171	441396.991609	50.145370
3502.738809	441394.385996	50.150375
3502.605765	441401.662067	50.155380
3502.717368	441421.374178	50.160385
3502.509285	441420.090899	50.165389
3503.088138	441414.716875	50.170394
3503.036525	441418.580607	50.175399
3503.169843	441431.542865	50.180404
3502.948977	441442.435235	50.185409
3502.971363	441448.264515	50.190413
3502.803673	441430.235827	50.195418
3502.935175	441429.604685	50.200423
3503.088317	441414.818184	50.205428
3502.884631	441419.620893	50.210433
3502.741981	441417.261262	50.215437
3503.012778	441424.265480	50.220442
3503.286540	441438.218211	50.225447
3502.808044	441431.503044	50.230452
3503.125336	441428.861991	50.235457
3503.115988	441422.624668	50.240461
3502.891986	441424.539644	50.245466
3502.827616	441424.195560	50.250471
3502.849782	441415.974665	50.255476
3503.067425	441424.408198	50.260481
3503.047438	441444.751429	50.265485
3503.462947	441443.666013	50.270490
3503.065628	441437.190602	50.275495
3503.348806	441432.627908	50.280500
3502.932403	441431.532368	50.285505
3503.174119	441427.027475	50.290509
3503.102213	441421.105170	50.295514
3503.069149	441414.516834	50.300519
3503.495230	441401.661912	50.305524
3503.327949	441411.124908	50.310529
3503.099888	441402.845287	50.315533
3503.010318	441397.534666	50.320538
3502.875983	441392.383855	50.325543
3503.227411	441384.766126	50.330548
3502.968425	441386.078404	50.335553
3502.755274	441370.897911	50.340557
3502.941813	441385.271351	50.345562
3502.838720	441399.795681	50.350567
3503.034340	441402.044793	50.355572
3502.823771	441399.950372	50.360577
3503.095122	441399.904025	50.365581
3503.117682	441392.393174	50.370586
3503.017867	441390.837792	50.375591
3503.533225	441375.431467	50.380596
3503.306786	441373.846982	50.385601
3503.517640	441370.666143	50.390605
3503.293068	441364.617721	50.395610
3503.024267	441363.801313	50.400615
3503.264603	441350.927353	50.405620
3502.934561	441358.237075	50.410625
3503.073083	441348.931105	50.415629
3502.956415	441357.218854	50.420634
3502.892668	441379.142031	50.425639
3503.612941	441369.686015	50.430644
3503.397071	441386.410696	50.435649
3503.411465	441370.024724	50.440653
3503.626002	441349.496005	50.445658
3503.499866	441332.576047	50.450663
3503.673254	441306.728397	50.455668
3503.891002	441305.524572	50.460673
3503.530114	441302.035561	50.465677
3503.565866	441292.189161	50.470682
3503.136829	441291.603001	50.475687
3503.276995	441276.209946	50.480692
3502.959397	441281.336473	50.485697
3503.415768	441271.621138	50.490701
3503.113403	441268.375745	50.495706
3502.635775	441269.826808	50.500711
3502.973925	441253.233299	50.505716
3503.020328	441258.957081	50.510721
3502.943901	441248.115351	50.515725
3503.269868	441246.385813	50.520730
3502.667167	441234.670195	50.525735
3503.103310	441215.067253	50.530740
3502.950746	441184.253508	50.535745
3502.970948	441144.685789	50.540749
3503.268217	441084.121858	50.545754
3503.091290	441023.537280	50.550759
3503.035049	440941.577168	50.555764
3503.132083	440848.684894	50.560769
3503.075010	440752.622906	50.565773
3502.902515	440639.232395	50.570778
3503.175623	440519.170979	50.575783
3503.266971	440375.400551	50.580788
3502.734195	440229.300926	50.585793
3502.967577	440066.786494	50.590797
3503.189190	439895.953760	50.595802
3502.853189	439710.605616	50.600807
3503.323497	439508.479724	50.605812
3503.219250	439308.682109	50.610817
3502.956253	439084.966109	50.615821
3503.082326	438848.702158	50.620826
3503.098824	438612.403675	50.625831
3503.214598	438346.307320	50.630836
3503.096950	438076.595049	50.635841
3503.231658	437800.444311	50.640845
3502.981809	437494.373347	50.645850
3502.845554	437191.728612	50.650855
3503.042345	436872.179508	50.655860
3503.330436	436539.165775	50.660865
3503.182355	436196.581995	50.665869
3502.737250	435828.422283	50.670874
3502.312837	435464.870051	50.675879
3502.585458	435077.498685	50.680884
3502.782815	434701.194466	50.685889
3502.675249	434285.461173	50.690893
3502.916772	433865.449281	50.695898
3502.703486	433428.153944	50.700903
3502.779660	432982.783618	50.705908
3502.285499	432519.640542	50.710913
3502.155904	432033.997072	50.715917
3502.203556	431542.934150	50.720922
3501.791856	431046.712401	50.725927
3502.544399	430522.522508	50.730932
3502.116058	429997.253751	50.735937
3501.933518	429448.992401	50.740941
3502.285959	428881.189319	50.745946
3502.011623	428297.137386	50.750951
3501.886376	427698.682343	50.755956
3501.884399	427098.465477	50.760961
3502.039750	426460.900945	50.765965
3501.980046	425813.153870	50.770970
3501.790835	425154.396741	50.775975
3501.792717	424465.640417	50.780980
3501.855279	423754.569703	50.785985
3501.566617	423046.786967	50.790989
3501.662422	422313.789491	50.795994
3501.612441	421559.473121	50.800999
3501.621367	420788.141701	50.806004
3501.253489	420003.625090	50.811009
3501.140901	419197.741612	50.816013
3501.320106	418366.497428	50.821018
3501.155589	417529.800741	50.826023
3501.347983	416658.639840	50.831028
3501.140321	415785.993977	50.836033
3500.755746	414880.366987	50.841037
3501.345972	413966.340335	50.846042
3501.098562	413016.977485	50.851047
3501.266947	412046.229847	50.856052
3500.906506	411060.909693	50.861057
3500.820890	410057.627879	50.866061
3500.915784	409028.602272	50.871066
3500.326691	407990.333168	50.876071
3500.263697	406926.968230	50.881076
3500.094193	405855.680669	50.886081
3500.074838	404757.909722	50.891085
3499.977422	403644.410565	50.896090
3499.577793	402512.933757	50.901095
3499.588386	401357.055933	50.906100
3499.481858	400202.471506	50.911105
3499.538079	399004.268334	50.916109
3499.584902	397792.856206	50.921114
3499.226886	396563.067574	50.926119
3498.909346	395300.723028	50.931124
3498.989819	394039.323331	50.936129
3498.751519	392753.022219	50.941133
3498.432901	391451.483412	50.946138
3498.411518	390124.145654	50.951143
3498.459398	388784.361800	50.956148
3498.096607	387421.335266	50.961153
3498.101987	386040.395021	50.966157
3498.091832	384629.074304	50.971162
3497.530805	383218.700013	50.976167
3497.545616	381773.163211	50.981172
3497.302405	380322.801733	50.986177
3497.000296	378862.014384	50.991181
3497.008552	377365.645384	50.996186
3496.623973	375864.141423	51.001191
3496.800936	374334.075928	51.006196
3496.343900	372805.118872	51.011201
3495.969637	371238.347107	51.016205
3496.074323	369667.813620	51.021210
3495.646618	368083.672413	51.026215
3495.867619	366467.639939	51.031220
3495.314616	364847.879867	51.036225
3495.246369	363201.822491	51.041229
3495.125570	361537.034780	51.046234
3494.534198	359866.965564	51.051239
3494.901733	358173.718676	51.056244
3494.298260	356478.225904	51.061249
3493.844828	354759.005061	51.066253
3493.914611	353014.006458	51.071258
3493.540542	351258.224957	51.076263
3493.327020	349475.860114	51.081268
3493.114496	347691.997928	51.086273
3493.083170	345888.162482	51.091277
3492.886982	344073.368311	51.096282
3491.870480	342248.338201	51.101287
3492.036246	340396.877487	51.106292
3491.893206	338540.487727	51.111297
3491.460349	336670.667013	51.116301
3491.541957	334782.391890	51.121306
3491.199096	332888.979972	51.126311
3490.537449	330969.188285	51.131316
3490.342378	329035.200309	51.136321
3490.083445	327104.211097	51.141325
3490.177316	325152.658014	51.146330
3489.633790	323182.720815	51.151335
3489.135520	321189.981081	51.156340
3489.056494	319200.492479	51.161345
3488.929483	317191.909693	51.166349
3488.324042	315165.248402	51.171354
3487.932792	313137.218617	51.176359
3487.219163	311085.357325	51.181364
3487.175655	309031.033964	51.186369
3487.056722	306957.701324	51.191373
3486.611260	304884.804168	51.196378
3485.874892	302794.642889	51.201383
3485.982357	300684.147477	51.206388
3485.440752	298575.013309	51.211393
3485.174701	296455.804680	51.216397
3484.843857	294310.641112	51.221402
3484.188225	292173.104194	51.226407
3484.156680	290012.935480	51.231412
3483.652019	287846.646700	51.236417
3483.289562	285664.534444	51.241421
3482.845087	283478.327629	51.246426
3482.448642	281284.059146	51.251431
3482.273161	279064.715498	51.256436
3481.787271	276844.964677	51.261441
3481.639128	274623.119696	51.266445
3481.676917	272361.644694	51.271450
3481.157650	270111.195980	51.276455
3480.865460	267825.749770	51.281460
3480.279208	265535.729540	51.286465
3479.933068	263253.679072	51.291469
3479.600301	260945.512819	51.296474
3479.020255	258635.727488	51.301479
3478.672643	256307.969993	51.306484
3478.164142	253971.835643	51.311489
3477.768799	251636.423826	51.316493
3477.201303	249285.537774	51.321498
3476.496757	246939.167129	51.326503
3476.126700	244569.780230	51.331508
3475.656032	242202.285918	51.336513
3475.001542	239814.799705	51.341517
3474.646339	237433.448560	51.346522
3473.783911	235051.777429	51.351527
3473.130347	232646.340098	51.356532
3473.061979	230244.961969	51.361537
3472.311911	227848.957618	51.366541
3471.754789	225429.125005	51.371546
3471.144441	223009.625967	51.376551
3470.797700	220578.110645	51.381556
3470.076474	218149.333844	51.386561
3469.635723	215724.129176	51.391565
3469.299820	213280.530367	51.396570
3468.594797	210827.967759	51.401575
3468.224061	208367.318538	51.406580
3467.051734	205914.184456	51.411585
3466.471429	203450.763463	51.416589
3466.412451	200987.472089	51.421594
3465.541972	198526.820060	51.426599
3464.951728	196041.334606	51.431604
3464.335677	193565.923520	51.436609
3463.928642	191080.172655	51.441613
3463.211717	188580.026626	51.446618
3462.554453	186106.432349	51.451623
3462.172524	183601.030846	51.456628
3461.264520	181109.688869	51.461633
3460.635755	178615.563306	51.466637
3459.891460	176110.722350	51.471642
3458.955330	173608.582210	51.476647
3458.542868	171099.011340	51.481652
3457.555159	168596.743778	51.486657
3456.960778	166097.418766	51.491661
3456.350773	163586.213595	51.496666
3455.370502	161093.061149	51.501671
3455.188660	158579.045352	51.506676
3454.183666	156081.321418	51.511681
3453.299363	153570.567564	51.516685
3452.641091	151074.253157	51.521690
3452.010387	148500.947235	51.526695
3451.495011	145973.978013	51.531700
3450.436092	143471.024719	51.536705
3449.574669	140960.112871	51.541709
3448.855026	138460.682141	51.546714
3448.048066	135963.328426	51.551719
3447.514989	133458.155496	51.556724
3446.600534	130955.626493	51.561729
3445.381990	128466.305061	51.566733
3444.439606	125973.878009	51.571738
3443.296266	123492.497557	51.576743
3442.809040	121006.860798	51.581748
3441.749334	118540.215588	51.586753
3440.587339	116081.708195	51.591757
3439.959485	113619.278712	51.596762
3438.869153	111166.222405	51.601767
3437.822076	108717.539237	51.606772
3436.946642	106281.083140	51.611777
3435.712635	103854.265777	51.616781
3434.901807	101428.066970	51.621786
3433.826495	99010.294654	51.626791
3432.762188	96595.812590	51.631796
3431.637876	94204.081266	51.636801
3430.535973	91815.988704	51.641805
3429.545965	89423.894947	51.646810
3427.896344	87074.284225	51.651815
3427.152450	84719.344050	51.656820
3425.821978	82387.955635	51.661825
3424.630253	80051.372660	51.666829
3423.667693	77739.367142	51.671834
3422.461889	75451.311514	51.676839
3421.165490	73155.997513	51.681844
3419.887232	70896.569520	51.686849
3418.209610	68633.969427	51.691853
3417.191037	66405.787375	51.696858
3415.636825	64179.558667	51.701863
3414.238942	61982.830680	51.706868
3412.659026	59803.513162	51.711873
3411.613854	57643.584456	51.716877
3409.822546	55492.945495	51.721882
3408.260225	53387.347997	51.726887
3406.673954	51280.577348	51.731892
3404.985407	49218.542362	51.736897
3403.233313	47172.916671	51.741901
3401.507188	45147.728262	51.746906
3399.663613	43172.005195	51.751911
3398.163988	41212.297838	51.756916
3396.032232	39295.837854	51.761921
3393.783260	37392.292592	51.766925
3391.430919	35540.396855	51.771930
3388.841926	33741.773131	51.776935
3384.761615	32028.285264	51.781940
3379.276023	30400.243673	51.786945
3373.617310	28864.207358	51.791949
3368.233928	27391.223641	51.796954
3362.812788	26031.211218	51.801959
3357.671679	24759.687909	51.806964
3353.185622	23595.880060	51.811969
3348.578213	22525.466960	51.816973
3344.692036	21541.976347	51.821978
3340.641146	20648.379401	51.826983
3336.922277	19845.838872	51.831988
3333.300104	19129.483452	51.836993
3330.343766	18491.171997	51.841997
3327.397989	17912.286513	51.847002
3324.264678	17416.394600	51.852007
3321.838962	16985.739707	51.857012
3319.626311	16609.658499	51.862017
3317.081631	16285.326008	51.867021
3315.469292	15996.762867	51.872026
3313.349280	15768.093670	51.877031
3312.361226	15574.367030	51.882036
3311.416705	15412.527814	51.887041
3310.211098	15282.981140	51.892045
3309.424112	15168.480343	51.897050
3308.433464	15078.186967	51.902055
3307.700496	14995.993704	51.907060
3307.337291	14940.243520	51.912065
3306.610889	14891.156722	51.917069
3306.136874	14855.573759	51.922074
3305.687579	14836.346463	51.927079
3305.407301	14809.533076	51.932084
3305.017712	14800.288185	51.937089
3304.532603	14791.304571	51.942093
3304.693509	14778.588449	51.947098
3304.617342	14777.762280	51.952103
3304.396515	14766.209719	51.957108
3303.963560	14767.235032	51.962113
3303.912143	14752.390124	51.967117
3303.888086	14733.267306	51.972122
3303.104480	14723.587216	51.977127
3303.413227	14689.056154	51.982132
3303.042977	14667.473488	51.987137
3302.841698	14645.220370	51.992141
3302.587099	14598.746736	51.997146
3302.305159	14585.221425	52.002151
3302.298185	14550.325796	52.007156
3302.016750	14504.076677	52.012161
3301.668137	14459.172950	52.017165
3301.525327	14407.683791	52.022170
3300.777553	14355.794016	52.027175
3300.839239	14300.025551	52.032180
3300.698862	14240.611278	52.037185
3299.876074	14175.857046	52.042189
3299.232910	14113.202606	52.047194
3299.121345	14049.594762	52.052199
3298.416973	13982.180413	52.057204
3298.242690	13923.270856	52.062209
3297.428899	13857.945855	52.067213
3297.063782	13775.125334	52.072218
3296.356054	13701.720385	52.077223
3295.977527	13624.873076	52.082228
3295.600069	13546.082258	52.087233
3294.846215	13468.550761	52.092237
3294.784715	13391.702527	52.097242
3294.060709	13315.258580	52.102247
3293.467211	13239.996808	52.107252
3292.807831	13166.078737	52.112257
3292.124314	13092.214107	52.117261
3291.813050	13005.425134	52.122266
3290.999990	12923.385423	52.127271
3290.579882	12836.514802	52.132276
3290.224042	12750.749250	52.137281
3289.387551	12672.592490	52.142285
3289.138509	12582.840239	52.147290
3288.094333	12497.522260	52.152295
3287.761921	12407.897393	52.157300
3286.989619	12315.326983	52.162305
3286.399017	12235.061932	52.167309
3286.093305	12135.314999	52.172314
3284.974567	12058.650422	52.177319
3284.302456	11963.312368	52.182324
3284.093713	11880.338766	52.187329
3283.613589	11793.779378	52.192333
3283.312260	11700.116002	52.197338
3282.693189	11608.226527	52.202343
3281.995228	11500.549112	52.207348
3281.390644	11409.867001	52.212353
3280.115712	11312.638556	52.217357
3279.722755	11221.845495	52.222362
3279.080109	11137.001629	52.227367
3278.456363	11039.500828	52.232372
3277.931507	10947.704826	52.237377
3276.926948	10858.871577	52.242381
3276.249897	10755.090129	52.247386
3275.650169	10679.254997	52.252391
3275.020809	10583.759679	52.257396
3274.649688	10493.158108	52.262401
3273.989995	10405.805692	52.267405
3273.453012	10305.668610	52.272410
3272.339071	10219.251109	52.277415
3271.970065	10129.366897	52.282420
3271.596431	10043.888715	52.287425
3270.832233	9957.738315	52.292429
3270.236087	9858.571499	52.297434
3269.484806	9770.463998	52.302439
3268.417307	9683.167747	52.307444
3267.909710	9583.527742	52.312449
3267.435814	9499.668354	52.317453
3266.644723	9405.711583	52.322458
3265.872996	9331.327643	52.327463
3265.168909	9235.973065	52.332468
3264.939663	9144.654906	52.337473
3264.063003	9068.207914	52.342477
3263.683833	8968.974708	52.347482
3262.867403	8884.745731	52.352487
3262.413379	8793.295752	52.357492
3261.811362	8702.418169	52.362497
3260.883214	8618.260217	52.367501
3260.228833	8519.353235	52.372506
3259.548046	8440.572479	52.377511
3259.211580	8356.531235	52.382516
3258.308896	8258.263826	52.387521
3257.794438	8168.090691	52.392525
3257.053612	8074.332104	52.397530
3256.173751	7981.929493	52.402535
3255.333413	7894.203635	52.407540
3254.886231	7810.350013	52.412545
3253.929291	7727.163647	52.417549
3253.580307	7631.787089	52.422554
3252.625215	7554.612693	52.427559
3252.078053	7474.243654	52.432564
3251.751539	7387.536157	52.437569
3250.942909	7300.050592	52.442573
3250.449527	7221.338554	52.447578
3249.682310	7142.187161	52.452583
3248.739222	7053.703898	52.457588
3248.204855	6964.724809	52.462593
3247.496416	6890.096472	52.467597
3246.956238	6804.386638	52.472602
3246.308737	6733.281344	52.477607
3245.719402	6642.837320	52.482612
3244.777172	6562.215732	52.487617
3244.011030	6485.709987	52.492621
3243.527209	6398.736952	52.497626
3242.503641	6329.552862	52.502631
3242.168108	6243.501476	52.507636
3241.807825	6159.741917	52.512641
3241.187237	6093.855158	52.517645
3240.445511	6001.244482	52.522650
3239.831447	5924.828371	52.527655
3239.006353	5846.399296	52.532660
3237.959177	5766.407747	52.537665
3237.560561	5686.954173	52.542669
3236.960941	5604.642552	52.547674
3236.096769	5539.805017	52.552679
3235.606900	5462.030525	52.557684
3234.719566	5382.419512	52.562689
3233.887313	5305.745912	52.567693
3233.825552	5228.699402	52.572698
3232.701966	5164.775602	52.577703
3232.629646	5083.842283	52.582708
3231.411441	4997.366384	52.587713
3231.264946	4936.894191	52.592717
3230.588557	4858.468260	52.597722
3229.629569	4779.565061	52.602727
3228.697183	4706.650630	52.607732
3228.489067	4631.974211	52.612737
3227.578381	4548.357406	52.617741
3227.236679	4467.789106	52.622746
3226.407616	4402.635914	52.627751
3226.309912	4321.704484	52.632756
3225.286629	4237.244656	52.637761
3224.543592	4162.372811	52.642765
3223.950963	4071.819147	52.647770
3223.098449	4006.690539	52.652775
3222.358313	3928.415118	52.657780
3221.754317	3858.682084	52.662785
3221.029846	3779.171301	52.667789
3220.601683	3701.521213	52.672794
3219.740623	3630.133016	52.677799
3219.320910	3561.198132	52.682804
3218.280334	3488.660746	52.687809
3217.364192	3410.783548	52.692813
3217.421756	3341.032157	52.697818
3216.663617	3280.943965	52.702823
3215.484926	3202.889184	52.707828
3215.178996	3123.572341	52.712833
3214.187451	3050.120545	52.717837
3214.054339	2980.804434	52.722842
3213.082621	2915.132173	52.727847
3212.219852	2836.936795	52.732852
3211.727377	2772.343166	52.737857
3210.865496	2700.308689	52.742861
3210.651128	2614.935269	52.747866
3210.068817	2553.151424	52.752871
3209.390004	2481.459351	52.757876
3208.735543	2404.815993	52.762881
3207.769869	2327.421607	52.767885
3207.528808	2255.118873	52.772890
3206.803826	2195.376559	52.777895
3206.253981	2117.668189	52.782900
3205.557145	2041.038578	52.787905
3204.519831	1974.108690	52.792909
3204.048394	1893.970430	52.797914
3203.057489	1831.376510	52.802919
3202.593956	1765.342730	52.807924
3202.252570	1680.463477	52.812929
3201.283375	1613.348213	52.817933
3200.599694	1532.135212	52.822938
3199.419952	1480.603861	52.827943
3198.802950	1413.750618	52.832948
3198.365700	1340.178552	52.837953
3197.253092	1291.572964	52.842957
3196.700221	1225.664880	52.847962
3196.182015	1166.881201	52.852967
3195.587779	1101.727974	52.857972
3194.827723	1046.641871	52.862977
3194.174184	984.980968	52.867981
3193.534239	921.303981	52.872986
3192.579368	870.360715	52.877991
3192.301998	820.190046	52.882996
3192.000187	751.320737	52.888001
3191.056868	692.665941	52.893005
3190.611994	626.763636	52.898010
3189.319425	570.615964	52.903015
3188.856217	516.205361	52.908020
3188.278497	467.781351	52.913025
3187.196456	409.131584	52.918029
3186.219491	350.976845	52.923034
3185.295302	305.096987	52.928039
3184.552163	269.093306	52.933044
3183.675059	234.989937	52.938049
3182.893060	200.840394	52.943053
3181.924793	155.288635	52.948058
3180.504209	137.905898	52.953063
3179.637910	130.802727	52.958068
3178.073555	132.324422	52.963073
3176.784298	144.450470	52.968077
3176.533934	132.428354	52.973082
3175.738494	141.011819	52.978087
3175.670017	143.931863	52.983092
3175.064605	127.751947	52.988097
3174.187941	134.923922	52.993101
3174.016502	130.417769	52.998106
3173.319911	134.752067	53.003111
3172.280944	137.899098	53.008116
3171.813314	136.852816	53.013121
3170.623022	140.362009	53.018125
3170.711613	135.374071	53.023130
3170.367134	142.127897	53.028135
3168.882176	146.641494	53.033140
3168.554391	141.955606	53.038145
3168.166598	136.948795	53.043149
3168.123848	137.552519	53.048154
3166.690796	145.404149	53.053159
3165.838485	131.862938	53.058164
3165.594766	132.441393	53.063169
3164.944431	141.685710	53.068173
3164.423263	141.784209	53.073178
3163.530484	141.834489	53.078183
3163.400256	133.882816	53.083188
3162.477242	146.674963	53.088193
3161.531103	152.964757	53.093197
3161.475785	141.982581	53.098202
3159.871652	141.261520	53.103207
3159.405375	139.515155	53.108212
3159.398421	139.652509	53.113217
3158.595700	140.309496	53.118221
3157.632925	136.313534	53.123226
3157.513335	144.347331	53.128231
3156.446880	144.460837	53.133236
3156.015165	143.148294	53.138241
3155.190484	145.816622	53.143245
3154.710913	135.226270	53.148250
3153.894042	136.659342	53.153255
3153.417227	142.102781	53.158260
3153.098435	136.701297	53.163265
3152.238916	144.762040	53.168269
3151.175916	132.352200	53.173274
3150.892033	142.981378	53.178279
3149.935862	138.811003	53.183284
3149.230561	137.897301	53.188289
3148.626665	137.955069	53.193293
3148.273380	141.654413	53.198298
3147.039690	141.238347	53.203303
3146.566664	139.497872	53.208308
3146.189007	140.051844	53.213313
3145.350004	145.582821	53.218317
3145.340875	142.663770	53.223322
3144.329264	138.144060	53.228327
3143.308384	139.040817	53.233332
3142.949569	141.683630	53.238337
3142.385514	140.705929	53.243341
3141.691986	137.959861	53.248346
3140.823790	140.343920	53.253351
3140.053695	142.834374	53.258356
3140.133571	140.116429	53.263361
3139.227984	144.911957	53.268365
3138.127658	135.566063	53.273370
3137.513520	146.632185	53.278375
3137.114805	142.625511	53.283380
3136.917188	127.817086	53.288385
3135.637179	145.884189	53.293389
3134.879352	131.121739	53.298394
3133.999867	136.155168	53.303399
3133.688960	134.331340	53.308404
3133.302813	136.381598	53.313409
3132.467596	137.561629	53.318413
3132.587887	140.070480	53.323418
3131.860223	138.270489	53.328423
3131.232409	139.785734	53.333428
3129.522120	124.991028	53.338433
3129.076937	140.425153	53.343437
3128.216017	134.312631	53.348442
3127.494629	134.594154	53.353447
3127.402874	140.064170	53.358452
3126.894276	136.417712	53.363457
3125.301905	138.173544	53.368461
3125.149174	136.664132	53.373466
3125.514361	139.037195	53.378471
3124.543284	134.017550	53.383476
3123.722297	133.892547	53.388481
3122.770043	150.052383	53.393485
3122.126975	146.051537	53.398490
3120.875087	141.038817	53.403495
3119.783290	135.378234	53.408500
3119.569080	142.480452	53.413505
3119.365803	144.421705	53.418509
3118.532893	134.376458	53.423514
3118.196102	139.227959	53.428519
3117.871843	135.681057	53.433524
3117.718904	133.680638	53.438529
3116.528244	127.813139	53.443533
3115.909198	134.197435	53.448538
3114.265156	132.116263	53.453543
3113.912287	131.692996	53.458548
3113.394969	130.233640	53.463553
3112.238965	139.006603	53.468557
3112.343145	127.138659	53.473562
3111.900035	134.928521	53.478567
3111.006451	134.438564	53.483572
3110.465747	137.800465	53.488577
3109.284506	133.853682	53.493581
3108.924395	132.689169	53.498586
3108.061024	140.032560	53.503591
3107.848061	133.210926	53.508596
3107.365285	135.636503	53.513601
3106.597136	137.330066	53.518605
3106.163807	135.531499	53.523610
3104.872050	135.536275	53.528615
3104.205955	135.891246	53.533620
3104.137219	138.915540	53.538625
3102.680598	132.842437	53.543629
3101.945036	125.585110	53.548634
3100.983794	127.991780	53.553639
3101.071129	139.195012	53.558644
3100.957099	132.338318	53.563649
3100.188221	132.893215	53.568653
3099.135650	133.124356	53.573658
3098.215658	137.878138	53.578663
3097.600440	134.640682	53.583668
3096.778528	129.732924	53.588673
3096.321837	136.652363	53.593677
3096.304843	130.831830	53.598682
3095.733754	138.434354	53.603687
3094.616467	136.586863	53.608692
3093.988559	134.350238	53.613697
3093.331177	135.078319	53.618701
3093.103089	128.721105	53.623706
3090.991047	130.122852	53.628711
3090.852809	127.541647	53.633716
3090.719227	128.494040	53.638721
3089.741935	137.058842	53.643725
3089.109555	130.873334	53.648730
3088.431510	130.522207	53.653735
3088.414878	134.414288	53.658740
3087.626813	128.283802	53.663745
3086.507046	136.289539	53.668749
3086.060175	130.157203	53.673754
3085.950234	126.728420	53.678759
3084.570206	129.240594	53.683764
3084.185044	123.592310	53.688769
3083.103933	137.552226	53.693773
3082.563173	123.362171	53.698778
3082.182314	131.069554	53.703783
3081.402104	125.452848	53.708788
3081.142013	128.355891	53.713793
3080.434595	130.694327	53.718797
3079.727888	128.703663	53.723802
3078.711337	132.990797	53.728807
3078.302134	131.701257	53.733812
3077.351745	123.864077	53.738817
3076.511805	132.231334	53.743821
3075.622179	120.937404	53.748826
3074.983751	124.473104	53.753831
3074.594318	135.420694	53.758836
3074.109943	126.872718	53.763841
3073.713059	124.846485	53.768845
3073.269503	125.136200	53.773850
3072.262015	120.954089	53.778855
3070.966415	125.649682	53.783860
3070.563042	114.737665	53.788865
3070.149815	129.178706	53.793869
3069.698813	122.196442	53.798874
3068.795426	124.307843	53.803879
3068.251158	124.286748	53.808884
3067.590380	123.938989	53.813889
3067.002674	132.414724	53.818893
3066.451874	123.570214	53.823898
3065.470492	124.996274	53.828903
3064.664071	124.179991	53.833908
3064.520525	119.899605	53.838913
3063.141094	122.385234	53.843917
3062.806016	121.201054	53.848922
3062.366183	120.446079	53.853927
3061.914050	122.858131	53.858932
3061.089090	124.912318	53.863937
3059.897149	121.829069	53.868941
3060.285609	114.487854	53.873946
3059.401391	118.073839	53.878951
3058.444441	127.643690	53.883956
3057.828392	113.638221	53.888961
3056.358685	121.398623	53.893965
3056.400747	116.972052	53.898970
3056.472266	123.282956	53.903975
3054.860555	123.769508	53.908980
3054.243341	112.851008	53.913985
3053.744153	122.589740	53.918989
3053.302702	117.965924	53.923994
3052.449716	119.547675	53.928999
3051.632053	124.447785	53.934004
3051.366909	115.850518	53.939009
3050.482978	126.063535	53.944013
3049.578290	128.325157	53.949018
3049.978200	123.634551	53.954023
3048.528923	119.579642	53.959028
3047.687294	119.779880	53.964033
3046.461422	125.403409	53.969037
3046.742505	123.088841	53.974042
3046.528190	116.790071	53.979047
3045.296363	117.769465	53.984052
3044.298443	109.240175	53.989057
3043.394971	112.470644	53.994061
3043.639482	111.174012	53.999066
3042.801171	113.544289	54.004071
3041.764392	117.503704	54.009076
3041.401593	121.412692	54.014081
3040.212422	123.268199	54.019085
3039.869876	120.755460	54.024090
3039.665338	114.309762	54.029095
3038.951804	119.300234	54.034100
3037.995247	111.978058	54.039105
3036.962190	124.665443	54.044109
3036.395146	117.114082	54.049114
3035.849754	115.349277	54.054119
3035.321197	125.692224	54.059124
3034.704482	113.622618	54.064129
3033.895790	117.251752	54.069133
3033.627086	119.133132	54.074138
3033.174519	110.904598	54.079143
3031.782202	117.941270	54.084148
3031.845847	109.138622	54.089153
3030.694039	116.669052	54.094157
3029.668400	113.614631	54.099162
3029.107953	127.849908	54.104167
3028.315337	118.880547	54.109172
3028.481962	110.517396	54.114177
3027.394688	118.805335	54.119181
3026.877882	112.192344	54.124186
3026.813838	115.147936	54.129191
3025.987977	122.207422	54.134196
3025.518565	114.128999	54.139201
3024.141441	121.673460	54.144205
3023.102674	119.023115	54.149210
3022.774847	126.494070	54.154215
3022.461011	125.302315	54.159220
3021.814409	125.362262	54.164225
3020.701700	126.166574	54.169229
3019.439710	125.386696	54.174234
3019.307980	125.884442	54.179239
3018.784801	126.028691	54.184244
3018.771448	121.054630	54.189249
3017.709458	126.280696	54.194253
3017.051776	125.080987	54.199258
3016.276641	123.562672	54.204263
3015.476950	122.623277	54.209268
3015.239258	119.560136	54.214273
3014.335165	127.351002	54.219277
3013.955065	121.080167	54.224282
3013.088634	121.637535	54.229287
3012.381582	123.626581	54.234292
3011.600146	116.054228	54.239297
3011.138122	122.720763	54.244301
3010.614886	117.774226	54.249306
3009.336662	121.663985	54.254311
3008.634730	123.405452	54.259316
3008.374133	114.844913	54.264321
3007.703322	118.117734	54.269325
3006.796275	108.458218	54.274330
3006.841727	114.999352	54.279335
3005.410940	121.831819	54.284340
3005.081646	116.753461	54.289345
3003.820570	126.135683	54.294349
3003.479305	114.452822	54.299354
3003.591116	111.781135	54.304359
3002.394606	115.984554	54.309364
3001.802010	105.621983	54.314369
3000.818939	114.327105	54.319373
3000.424862	111.365293	54.324378
2999.822745	123.252743	54.329383
2999.372584	118.823839	54.334388
2998.279130	110.344832	54.339393
2997.872956	123.602844	54.344397
2997.428609	105.649995	54.349402
2997.347112	113.737256	54.354407
2995.872077	114.783875	54.359412
2994.547955	109.566837	54.364417
2994.025701	118.502685	54.369421
2994.255662	122.229072	54.374426
2993.037478	110.845662	54.379431
2992.320339	121.388984	54.384436
2991.739833	107.733902	54.389441
2991.186458	121.995593	54.394445
2990.549597	117.544516	54.399450
2989.832474	117.497309	54.404455
2989.000831	122.807960	54.409460
2988.761249	110.773395	54.414465
2987.880631	114.923626	54.419469
2987.420719	123.193577	54.424474
2986.982004	106.348556	54.429479
2986.086930	123.460935	54.434484
2985.933715	115.847947	54.439489
2984.569558	116.045117	54.444493
2983.415580	112.141475	54.449498
2983.067162	109.560669	54.454503
2982.789587	114.081131	54.459508
2982.220553	111.086061	54.464513
2981.145773	112.060342	54.469517
2980.394559	109.999144	54.474522
2979.702021	117.196897	54.479527
2978.694945	114.907058	54.484532
2978.947090	112.015213	54.489537
2977.993168	108.956838	54.494541
2977.471473	106.368538	54.499546
2977.226349	111.704881	54.504551
2975.902651	112.060135	54.509556
2975.704090	111.309333	54.514561
2975.194404	114.788302	54.519565
2974.202787	109.946677	54.524570
2973.080288	107.597224	54.529575
2972.086586	113.091878	54.534580
2972.097191	109.424618	54.539585
2971.941692	102.033470	54.544589
2970.916967	108.314589	54.549594
2970.126390	109.308594	54.554599
2969.699271	119.228817	54.559604
2969.142719	113.980488	54.564609
2968.245777	120.859891	54.569613
2967.617253	107.958265	54.574618
2966.765755	100.847101	54.579623
2966.224573	112.853995	54.584628
2965.017620	104.576759	54.589633
2964.595095	112.922813	54.594637
2964.041848	114.734795	54.599642
2963.557326	113.336561	54.604647
2962.490660	117.145571	54.609652
2962.204032	113.615152	54.614657
2961.739200	115.595574	54.619661
2960.921072	108.257263	54.624666
2960.128866	111.127684	54.629671
2959.706682	107.743191	54.634676
2959.357752	108.607650	54.639681
2958.741868	108.338678	54.644685
2957.513605	109.142222	54.649690
2956.436818	116.453794	54.654695
2955.579492	104.574142	54.659700
2955.925661	102.571734	54.664705
2954.797942	105.522777	54.669709
2954.354387	110.447775	54.674714
2953.631077	110.370841	54.679719
2952.826901	113.031735	54.684724
2952.420151	100.446291	54.689729
2952.062439	111.869215	54.694733
2951.243067	104.685854	54.699738
2950.487571	113.680503	54.704743
2949.744671	122.637479	54.709748
2948.937642	106.858803	54.714753
2947.748030	117.388916	54.719757
2947.353858	112.778747	54.724762
2947.049588	104.275026	54.729767
2946.210246	108.990956	54.734772
2945.792213	99.687621	54.739777
2944.615487	114.808568	54.744781
2944.451952	114.256645	54.749786
2944.039421	99.715531	54.754791
2943.182617	117.237798	54.759796
2943.099308	108.896838	54.764801
2942.144330	107.214669	54.769805
2940.900315	112.673945	54.774810
2940.152029	115.687650	54.779815
2939.249012	118.298333	54.784820
2938.974031	106.774289	54.789825
2938.311743	116.044320	54.794829
2937.695634	111.170507	54.799834
2937.362720	105.728841	54.804839
2936.483078	122.418196	54.809844
2936.430270	116.855240	54.814849
2935.664721	110.082277	54.819853
2934.440186	102.852503	54.824858
2933.575226	106.104033	54.829863
2932.555231	111.215168	54.834868
2932.898305	110.584567	54.839873
2931.921755	115.623544	54.844877
2931.283216	110.915008	54.849882
2930.435989	112.219086	54.854887
2929.998602	113.088400	54.859892
2929.681436	115.051878	54.864897
2929.067660	114.821233	54.869901
2927.745048	111.417725	54.874906
2927.148660	106.983428	54.879911
2926.071186	112.169121	54.884916
2925.853655	101.344590	54.889921
2925.303031	112.691534	54.894925
2924.641915	110.651658	54.899930
2923.588356	110.543139	54.904935
2923.247491	111.164649	54.909940
2923.414438	105.926899	54.914945
2922.238606	107.851591	54.919949
2921.077340	111.639668	54.924954
2920.175154	105.802273	54.929959
2919.759906	105.382180	54.934964
2919.944959	107.695217	54.939969
2919.088097	116.836266	54.944973
2918.124656	110.414879	54.949978
2917.388129	110.062716	54.954983
2916.861721	115.998560	54.959988
2916.011759	101.361287	54.964993
2914.737003	112.804743	54.969997
2914.438242	105.795309	54.975002
2914.315107	110.787917	54.980007
2913.121534	112.825773	54.985012
2912.456560	113.276492	54.990017
2911.929721	112.888496	54.995021
2911.152302	107.648712	55.000026
2910.803593	112.864206	55.005031
2910.359748	115.284717	55.010036
2910.157158	104.304873	55.015041
2909.236741	109.568726	55.020045
2908.020595	110.543494	55.025050
2907.329450	112.761141	55.030055
2906.541470	111.508321	55.035060
2906.592782	98.392648	55.040065
2905.513374	109.119841	55.045069
2904.925636	112.673334	55.050074
2904.511051	112.274444	55.055079
2903.518349	114.825065	55.060084
2902.603966	116.851526	55.065089
2901.613662	115.782884	55.070093
2901.031793	109.647995	55.075098
2900.792330	109.153654	55.080103
2899.904672	115.616221	55.085108
2899.717834	109.098438	55.090113
2898.939041	108.129043	55.095117
2898.743699	103.921865	55.100122
2898.419953	107.307482	55.105127
2897.179499	113.160094	55.110132
2896.512801	106.054467	55.115137
2895.698404	112.677404	55.120141
2894.803043	113.273284	55.125146
2894.447872	107.332150	55.130151
2892.970269	106.929798	55.135156
2893.094291	107.139898	55.140161
2892.041253	111.380787	55.145165
2891.607996	103.843304	55.150170
2891.100846	102.833014	55.155175
2890.548625	109.097733	55.160180
2890.215044	103.649082	55.165185
2889.187033	116.039164	55.170189
2887.762372	111.464979	55.175194
2887.476374	116.420685	55.180199
2886.777245	114.736248	55.185204
2886.007149	105.060466	55.190209
2885.359517	115.657431	55.195213
2884.643214	100.794042	55.200218
2884.346819	106.703602	55.205223
2883.701726	110.207688	55.210228
2883.567821	101.772756	55.215233
2882.833990	110.873437	55.220237
2882.271321	102.253233	55.225242
2880.881571	103.269516	55.230247
2879.743806	110.867823	55.235252
2879.616231	101.632094	55.240257
2878.853252	107.572051	55.245261
2878.221151	105.248546	55.250266
2877.824382	104.136106	55.255271
2877.535942	106.306644	55.260276
2877.361512	99.732274	55.265281
2876.098760	111.586564	55.270285
2874.780210	107.451344	55.275290
2874.453535	106.549156	55.280295
2873.492056	107.413700	55.285300
2873.359412	105.864159	55.290305
2872.346565	102.570357	55.295309
2871.838217	105.563587	55.300314
2871.507508	101.995318	55.305319
2870.220939	106.881234	55.310324
2869.666052	106.861183	55.315329
2869.032553	111.256160	55.320333
2868.299783	107.930282	55.325338
2868.102527	109.436307	55.330343
2867.343228	110.844969	55.335348
2866.856005	104.139717	55.340353
2866.248479	107.264368	55.345357
2865.040976	107.261114	55.350362
2864.307012	107.557055	55.355367
2863.170603	107.876774	55.360372
2862.786203	104.176370	55.365377
2862.432825	99.674503	55.370381
2861.554133	103.062989	55.375386
2861.695217	105.210646	55.380391
2861.186192	105.043420	55.385396
2860.828074	110.819059	55.390401
2859.398400	107.320581	55.395405
2858.599344	111.591883	55.400410
2857.855691	102.854197	55.405415
2857.202144	107.098656	55.410420
2857.277342	95.191114	55.415425
2856.438422	106.029179	55.420429
2855.187292	99.664083	55.425434
2854.385251	100.513224	55.430439
2853.704511	104.982193	55.435444
2853.516379	107.163219	55.440449
2852.465754	108.556540	55.445453
2852.001062	102.257562	55.450458
2851.909236	100.539603	55.455463
2850.802572	103.238387	55.460468
2849.878922	103.736480	55.465473
2848.807063	104.796334	55.470477
2848.283712	105.239041	55.475482
2848.049120	105.595688	55.480487
2847.189675	104.482194	55.485492
2846.961118	104.643210	55.490497
2846.664046	104.832514	55.495501
2846.420636	96.592352	55.500506
2844.982767	105.507440	55.505511
2843.846382	109.701397	55.510516
2843.636536	96.159063	55.515521
2842.657957	103.479515	55.520525
2842.308695	99.304174	55.525530
2841.289025	103.338055	55.530535
2839.994189	109.662588	55.535540
2840.366900	97.230134	55.540545
2839.834970	106.311702	55.545549
2838.745307	89.699169	55.550554
2838.003850	99.708228	55.555559
2837.195037	95.633927	55.560564
2837.191382	92.904613	55.565569
2836.651705	99.910849	55.570573
2835.409959	99.365970	55.575578
2834.547954	89.852755	55.580583
2833.728311	101.396056	55.585588
2833.439328	90.335476	55.590593
2832.820183	98.696571	55.595597
2832.305300	94.017053	55.600602
2831.743276	98.791776	55.605607
2831.123333	100.562667	55.610612
2830.887068	92.587728	55.615617
2829.713575	93.760873	55.620621
2828.530105	98.836799	55.625626
2828.116362	91.063899	55.630631
2827.536801	99.820850	55.635636
2827.534555	95.770542	55.640641
2826.321132	99.080059	55.645645
2824.778629	93.853820	55.650650
2824.853714	94.463850	55.655655
2824.065117	104.570571	55.660660
2823.776905	95.779532	55.665665
2822.895240	99.380893	55.670669
2822.175414	104.193245	55.675674
2821.946996	100.773284	55.680679
2821.400947	98.467449	55.685684
2820.912910	97.236801	55.690689
2819.644034	104.441873	55.695693
2818.852798	105.080361	55.700698
2819.056500	92.001816	55.705703
2817.660792	99.796574	55.710708
2817.356543	96.613779	55.715713
2815.717151	103.463371	55.720717
2815.007080	99.553377	55.725722
2814.862668	96.377607	55.730727
2813.995081	100.665754	55.735732
2813.791622	92.297589	55.740737
2813.131660	109.412000	55.745741
2812.747660	100.375233	55.750746
2812.392387	105.063704	55.755751
2811.450155	108.292535	55.760756
2811.056793	93.602922	55.765761
2809.957299	96.035230	55.770765
2809.271290	101.238502	55.775770
2808.453060	99.577196	55.780775
2807.083569	105.333060	55.785780
2806.702243	96.004532	55.790785
2806.240145	108.060266	55.795789
2806.022311	104.406793	55.800794
2805.457855	97.855671	55.805799
2804.662680	106.012389	55.810804
2804.121492	93.976128	55.815809
2803.309118	95.183872	55.820813
2802.365246	99.175593	55.825818
2801.836051	99.389572	55.830823
2800.821597	98.440338	55.835828
2800.611288	88.925090	55.840833
2799.810810	101.243909	55.845837
2799.277245	108.576728	55.850842
2798.766648	89.895163	55.855847
2797.860953	100.314782	55.860852
2797.043343	99.575057	55.865857
2796.512367	98.931996	55.870861
2796.161121	105.369598	55.875866
2796.021362	98.906545	55.880871
2795.188358	100.361363	55.885876
2793.857484	90.193710	55.890881
2792.898419	96.130077	55.895885
2792.345286	99.152280	55.900890
2791.921664	100.123063	55.905895
2791.349837	101.061940	55.910900
2790.990552	96.601353	55.915905
2789.658612	103.703527	55.920909
2788.780239	103.199971	55.925914
2788.794534	99.295254	55.930919
2788.049530	108.620471	55.935924
2787.100610	95.652874	55.940929
2786.904714	106.116574	55.945933
2786.274198	107.697439	55.950938
2785.694026	95.936257	55.955943
2784.791638	108.265000	55.960948
2783.923265	99.635883	55.965953
2783.394518	99.571505	55.970957
2783.073189	104.297989	55.975962
2782.468703	100.770996	55.980967
2781.131418	98.008310	55.985972
2780.370505	100.098159	55.990977
2779.675991	107.448617	55.995981
2779.227402	96.692813	56.000986
2779.090227	93.487783	56.005991
2778.082136	105.193555	56.010996
2777.755212	101.660174	56.016001
2776.877138	99.808186	56.021005
2776.420401	100.106491	56.026010
2775.650435	96.425814	56.031015
2774.553463	108.346116	56.036020
2774.515026	98.642416	56.041025
2773.860117	100.166663	56.046029
2772.603895	101.508298	56.051034
2772.089357	92.644243	56.056039
2771.155927	103.970554	56.061044
2770.580284	96.636241	56.066049
2770.400448	97.751274	56.071053
2769.647633	107.471367	56.076058
2769.207234	98.650294	56.081063
2767.370020	105.833306	56.086068
2767.561822	92.494702	56.091073
2766.550502	102.840801	56.096077
2765.986926	95.619686	56.101082
2765.914110	94.428993	56.106087
2764.944374	99.831152	56.111092
2764.530344	91.561351	56.116097
2763.901675	95.168817	56.121101
2763.160941	90.687380	56.126106
2762.373569	97.360963	56.131111
2761.260683	103.750720	56.136116
2761.125487	102.932257	56.141121
2760.155345	96.628504	56.146125
2759.662736	96.377562	56.151130
2758.823413	98.049380	56.156135
2757.520971	107.941965	56.161140
2757.534654	98.133441	56.166145
2756.927448	100.147680	56.171149
2756.645182	103.637523	56.176154
2756.077152	102.231084	56.181159
2755.505402	108.254020	56.186164
2754.409132	96.517504	56.191169
2753.687505	97.286600	56.196173
2753.105744	102.389560	56.201178
2752.833241	88.331001	56.206183
2751.327804	99.853757	56.211188
2750.481071	96.709612	56.216193
2749.793986	100.770341	56.221197
2749.742356	97.731475	56.226202
2749.184191	92.952791	56.231207
2748.333395	104.596154	56.236212
2748.159184	102.259929	56.241217
2747.567435	99.270354	56.246221
2746.509964	97.267066	56.251226
2745.904735	93.086146	56.256231
2744.728985	93.086570	56.261236
2744.392414	88.485139	56.266241
2744.139228	86.148205	56.271245
2743.420672	96.303345	56.276250
2742.438439	87.968040	56.281255
2741.729612	98.511902	56.286260
2741.125582	92.537146	56.291265
2740.432852	95.607289	56.296269
2740.220608	101.319704	56.301274
2738.933308	93.822832	56.306279
2737.768914	104.645085	56.311284
2737.550856	97.546492	56.316289
2736.782447	96.780998	56.321293
2736.388568	96.927645	56.326298
2736.064464	96.381860	56.331303
2735.512049	99.534597	56.336308
2735.237727	92.985608	56.341313
2734.142604	97.406993	56.346317
2733.312579	101.739648	56.351322
2732.788479	92.240938	56.356327
2731.993607	101.684805	56.361332
2731.655861	93.531439	56.366337
2730.398381	101.255218	56.371341
2729.513190	101.081643	56.376346
2729.188295	91.996898	56.381351
2728.708106	94.506519	56.386356
2728.355658	94.332279	56.391361
2727.248461	103.938475	56.396365
2725.990627	98.746898	56.401370
2725.482379	92.735247	56.406375
2724.660605	96.001917	56.411380
2724.719500	85.642929	56.416385
2723.445539	93.369127	56.421389
2723.022743	99.003059	56.426394
2723.126993	99.582839	56.431399
2722.290243	97.918792	56.436404
2721.886255	91.479597	56.441409
2720.721743	95.481409	56.446413
2719.944235	98.360393	56.451418
2719.540361	93.543894	56.456423
2718.856787	102.365993	56.461428
2718.389899	90.613493	56.466433
2717.038133	95.828725	56.471437
2716.135274	93.418895	56.476442
2715.743634	93.812259	56.481447
2715.229632	98.998373	56.486452
2715.243774	97.920708	56.491457
2714.313215	104.329438	56.496461
2713.657028	99.642509	56.501466
2712.865952	95.161791	56.506471
2711.784862	96.067331	56.511476
2711.567947	81.919155	56.516481
2710.803204	95.911022	56.521485
2710.337234	88.974807	56.526490
2709.649089	86.888269	56.531495
2708.264982	93.081237	56.536500
2707.739081	90.315671	56.541505
2707.276363	99.434350	56.546509
2706.740990	85.991506	56.551514
2706.857644	86.294437	56.556519
2705.818057	87.925888	56.561524
2704.906642	90.430273	56.566529
2703.940738	97.311607	56.571533
2703.400136	98.958424	56.576538
2702.845115	98.559476	56.581543
2702.390639	101.058388	56.586548
2701.641928	94.063136	56.591553
2700.398092	100.587384	56.596557
2700.028180	99.967723	56.601562
2699.242305	92.242266	56.606567
2698.625486	102.594357	56.611572
2698.222050	86.293256	56.616577
2698.184692	95.623824	56.621581
2697.097695	92.598518	56.626586
2696.238060	92.619127	56.631591
2695.466613	97.840956	56.636596
2695.082874	91.040288	56.641601
2694.326369	96.874150	56.646605
2694.181442	91.853135	56.651610
2693.169490	92.676599	56.656615
2691.850136	98.298389	56.661620
2691.451788	88.286367	56.666625
2691.110461	91.194215	56.671629
2690.506857	89.203357	56.676634
2690.075122	92.722694	56.681639
2688.589743	87.914620	56.686644
2687.826023	81.800599	56.691649
2687.306800	86.555773	56.696653
2686.735185	88.938132	56.701658
2686.534052	83.916860	56.706663
2685.897836	91.211562	56.711668
2685.419079	88.299391	56.716673
2684.555596	89.189055	56.721677
2683.869376	84.975414	56.726682
2683.513498	84.920180	56.731687
2682.050774	86.171607	56.736692
2680.964158	85.633008	56.741697
2680.936210	90.136056	56.746701
2680.503274	91.770392	56.751706
2679.988655	79.340035	56.756711
2679.388146	87.826228	56.761716
2679.089838	82.308424	56.766721
2678.088186	89.750851	56.771725
2676.915231	82.073411	56.776730
2676.648215	80.672372	56.781735
2675.932210	89.774736	56.786740
2674.717778	75.399198	56.791745
2674.355634	79.499514	56.796749
2673.480952	88.005335	56.801754
2673.039147	83.435716	56.806759
2672.548704	84.789364	56.811764
2672.277841	84.837622	56.816769
2671.082161	78.652973	56.821773
2669.932209	86.407713	56.826778
2669.737322	81.212880	56.831783
2669.076908	89.010650	56.836788
2668.727618	81.614777	56.841793
2668.291031	84.758770	56.846797
2667.493031	88.124404	56.851802
2666.100152	91.645012	56.856807
2665.569331	95.534566	56.861812
2665.205819	88.243355	56.866817
2664.598385	85.512652	56.871821
2664.320025	92.224754	56.876826
2663.476652	81.477257	56.881831
2662.391782	95.350954	56.886836
2661.990168	88.106913	56.891841
2661.295149	85.157110	56.896845
2660.805934	88.757718	56.901850
2660.226592	87.363488	56.906855
2659.227351	91.461002	56.911860
2658.296677	87.560721	56.916865
2657.545636	89.231275	56.921869
2656.774305	82.483054	56.926874
2656.803891	78.313242	56.931879
2656.169514	89.793291	56.936884
2655.996698	86.931061	56.941889
2654.160923	82.335259	56.946893
2653.814748	80.336323	56.951898
2653.550021	84.941420	56.956903
2652.266439	88.935174	56.961908
2652.407182	81.940656	56.966913
2652.010048	81.915765	56.971917
2650.437236	86.030799	56.976922
2650.016822	74.156702	56.981927
2649.320053	86.274630	56.986932
2648.917413	79.163399	56.991937
2648.645325	86.156654	56.996941
2647.042613	87.837795	57.001946
2646.458132	84.218593	57.006951
2645.947187	97.723407	57.011956
2645.298368	90.837404	57.016961
2644.794950	83.679452	57.021965
2644.230510	83.505140	57.026970
2643.218466	80.151257	57.031975
2642.527784	85.844792	57.036980
2641.738618	79.235015	57.041985
2641.219711	91.173338	57.046989
2640.803888	84.560922	57.051994
2640.603787	78.860947	57.056999
2639.198703	90.605367	57.062004
2638.409445	83.992842	57.067009
2637.650833	87.177278	57.072013
2637.052318	84.551235	57.077018
2637.241998	91.305694	57.082023
2636.686778	89.056711	57.087028
2636.442802	83.704093	57.092033
2635.290501	82.002426	57.097037
2634.321673	86.524203	57.102042
2633.777821	80.388794	57.107047
2632.388464	82.189779	57.112052
2631.901359	85.302541	57.117057
2631.318406	81.550453	57.122061
2630.684591	85.315906	57.127066
2630.568077	88.340058	57.132071
2629.797968	90.465835	57.137076
2629.366895	81.162033	57.142081
2628.310898	80.662026	57.147085
2627.510844	93.237338	57.152090
2627.196837	80.756121	57.157095
2626.125319	81.530175	57.162100
2625.473710	75.885674	57.167105
2624.492787	78.172615	57.172109
2623.737712	85.015544	57.177114
2623.199717	82.563099	57.182119
2622.287373	84.136498	57.187124
2622.520993	81.485444	57.192129
2621.676828	84.240441	57.197133
2621.161744	89.328058	57.202138
2621.141208	77.413238	57.207143
2619.622863	87.608779	57.212148
2619.274699	85.954780	57.217153
2618.607683	83.866618	57.222157
2618.159221	83.075265	57.227162
2617.468387	79.711082	57.232167
2616.476173	89.579458	57.237172
2615.660646	81.315558	57.242177
2614.500177	81.940614	57.247181
2613.379551	86.548736	57.252186
2614.090305	79.915451	57.257191
2612.810090	92.199828	57.262196
2611.802155	80.592740	57.267201
2611.484101	82.732819	57.272205
2610.975972	84.635004	57.277210
2610.741721	81.494737	57.282215
2610.198325	96.377946	57.287220
2609.436987	83.874517	57.292225
2608.605414	83.719822	57.297229
2607.810196	89.252420	57.302234
2607.206485	84.404180	57.307239
2606.100313	85.535861	57.312244
2605.142996	79.823625	57.317249
2604.956049	85.282240	57.322253
2604.707922	87.905351	57.327258
2603.977900	81.113765	57.332263
2602.933903	81.000910	57.337268
2602.882834	84.157947	57.342273
2602.224773	83.859516	57.347277
2601.071292	93.677702	57.352282
2600.431699	81.328724	57.357287
2599.650589	86.493395	57.362292
2599.542212	83.552657	57.367297
2598.227746	87.929452	57.372301
2597.280467	84.613847	57.377306
2596.917380	81.911644	57.382311
2596.096119	93.995598	57.387316
2595.872171	86.320946	57.392321
2595.373323	89.167701	57.397325
2594.653978	86.072860	57.402330
2594.559148	80.157926	57.407335
2593.126896	84.667353	57.412340
2592.759169	92.582456	57.417345
2591.805728	90.195113	57.422349
2591.490312	78.801217	57.427354
2591.019633	76.351480	57.432359
2589.706759	84.413545	57.437364
2588.864663	80.187885	57.442369
2588.960069	76.674302	57.447373
2588.186491	80.894294	57.452378
2587.832175	76.301048	57.457383
2586.736443	90.698822	57.462388
2586.432605	88.580156	57.467393
2585.525624	84.239670	57.472397
2584.436152	86.735432	57.477402
2583.635673	75.696820	57.482407
2582.589340	83.188338	57.487412
2582.067542	91.456610	57.492417
2581.405892	86.306841	57.497421
2581.264901	80.000338	57.502426
2580.758763	79.818039	57.507431
2580.416078	82.965324	57.512436
2580.321327	82.463628	57.517441
2579.495891	80.511103	57.522445
2577.896990	77.933719	57.527450
2577.490126	76.476070	57.532455
2575.907884	81.985714	57.537460
2575.924591	81.716799	57.542465
2574.790948	79.745122	57.547469
2574.538644	85.181752	57.552474
2574.362171	79.688132	57.557479
2573.347989	82.562591	57.562484
2573.224532	74.716036	57.567489
2572.722358	81.392579	57.572493
2571.108968	86.396778	57.577498
2570.681696	75.108455	57.582503
2569.728055	92.843806	57.587508
2569.771853	88.077899	57.592513
2569.103197	80.123235	57.597517
2567.873500	77.228932	57.602522
2567.160623	72.774353	57.607527
2566.459946	85.573452	57.612532
2565.986076	84.803420	57.617537
2565.682759	78.046658	57.622541
2565.073140	86.410465	57.627546
2564.739099	78.288472	57.632551
2563.546532	81.066720	57.637556
2562.660557	79.984651	57.642561
2562.456442	80.004530	57.647565
2561.791706	85.480089	57.652570
2560.715717	74.408059	57.657575
2559.705568	77.777998	57.662580
2558.811128	80.616199	57.667585
2558.364091	86.320980	57.672589
2557.605551	81.098967	57.677594
2558.061873	76.648582	57.682599
2557.365682	80.102213	57.687604
2556.992066	81.771413	57.692609
2555.943681	81.707078	57.697613
2554.942101	89.673303	57.702618
2554.954078	80.326536	57.707623
2553.896755	85.698688	57.712628
2552.770848	79.997523	57.717633
2552.119971	85.314796	57.722637
2551.498998	94.541443	57.727642
2551.195889	80.033047	57.732647
2550.404378	87.289170	57.737652
2549.615442	81.228434	57.742657
2549.264035	85.167055	57.747661
2548.237167	88.296310	57.752666
2547.960621	79.028473	57.757671
2546.715893	88.715818	57.762676
2545.890074	80.576849	57.767681
2545.006592	84.774978	57.772685
2544.494497	87.264405	57.777690
2544.194548	85.688614	57.782695
2543.679428	87.082016	57.787700
2543.455291	88.069630	57.792705
2543.090232	86.722858	57.797709
2542.580327	96.135774	57.802714
2541.650820	83.359545	57.807719
2540.733619	84.103680	57.812724
2539.561900	86.537723	57.817729
2538.844033	82.492932	57.822733
2537.783238	87.574769	57.827738
2537.670147	74.777788	57.832743
2536.863992	80.592118	57.837748
2536.517129	76.544297	57.842753
2536.006243	81.946187	57.847757
2535.113143	86.491740	57.852762
2534.310901	86.231781	57.857767
2533.662048	86.465846	57.862772
2533.277425	79.384709	57.867777
2532.914248	81.225014	57.872781
2531.744058	85.150854	57.877786
2530.606954	75.659494	57.882791
2529.986927	77.385820	57.887796
2529.670524	76.414404	57.892801
2529.181573	84.986916	57.897805
2528.532147	79.293507	57.902810
2528.569946	77.107363	57.907815
2527.506802	76.089140	57.912820
2526.738454	78.441198	57.917825
2526.111318	75.690596	57.922829
2525.011904	84.499310	57.927834
2524.420280	80.407678	57.932839
2523.685139	86.705249	57.937844
2523.061660	79.727709	57.942849
2522.641666	81.286816	57.947853
2522.172550	91.177872	57.952858
2521.570407	81.274934	57.957863
2520.495594	86.302724	57.962868
2519.838853	79.069563	57.967873
2519.156844	79.595473	57.972877
2518.372699	86.605610	57.977882
2518.274627	79.815343	57.982887
2517.222971	78.042025	57.987892
2516.522643	73.856879	57.992897
2515.743579	81.630725	57.997901
2515.397417	93.466883	58.002906
2515.215236	74.295078	58.007911
2514.356071	94.150524	58.012916
2513.212738	84.186561	58.017921
2512.919735	81.904608	58.022925
2511.927039	79.345183	58.027930
2511.242164	88.964055	58.032935
2510.401415	94.746017	58.037940
2509.499074	80.181791	58.042945
2509.160614	83.776368	58.047949
2508.177538	90.867094	58.052954
2508.376220	75.016123	58.057959
2507.545231	80.644444	58.062964
2507.283362	88.038962	58.067969
2506.313113	79.767594	58.072973
2505.187798	83.496693	58.077978
2504.848486	83.360089	58.082983
2504.381729	82.271094	58.087988
2503.638714	75.769112	58.092993
2502.708919	88.073716	58.097997
2501.819904	89.261841	58.103002
2501.491482	72.632200	58.108007
2500.399961	82.846756	58.113012
2500.523992	84.287200	58.118017
2499.769949	77.954861	58.123021
2498.608228	80.394700	58.128026
2498.086942	72.964711	58.133031
2497.341770	90.066015	58.138036
2497.445426	78.369577	58.143041
2496.011170	82.945680	58.148045
2495.132708	86.537844	58.153050
2494.569093	75.221533	58.158055
2493.777241	90.813500	58.163060
2493.583507	82.033601	58.168065
2493.341654	76.015132	58.173069
2492.511686	86.202343	58.178074
2491.829013	81.709453	58.183079
2490.610474	85.225553	58.188084
2490.502796	82.619032	58.193089
2489.819900	77.339103	58.198093
2488.706874	82.564870	58.203098
2488.016408	75.937069	58.208103
2487.427297	81.848107	58.213108
2486.446588	83.409136	58.218113
2486.485228	77.987691	58.223117
2486.306430	91.078084	58.228122
2485.067951	82.480749	58.233127
2484.143383	86.026720	58.238132
2483.401817	77.611267	58.243137
2483.380282	89.323632	58.248141
2481.952569	89.014699	58.253146
2480.981928	78.122833	58.258151
2480.473713	83.920966	58.263156
2480.434399	82.466404	58.268161
2479.714187	77.601396	58.273165
2479.333787	84.906048	58.278170
2478.805971	82.254125	58.283175
2477.753047	83.215679	58.288180
2476.870892	79.216356	58.293185
2476.342032	78.805459	58.298189
2475.515890	86.065534	58.303194
2475.603081	68.125809	58.308199
2474.376319	81.334968	58.313204
2473.455798	74.116918	58.318209
2473.162838	78.518820	58.323213
2472.372218	77.114158	58.328218
2471.931066	76.801552	58.333223
2470.513381	70.357692	58.338228
2469.938130	75.319812	58.343233
2469.394663	82.944043	58.348237
2468.765199	87.738995	58.353242
2468.670706	71.992627	58.358247
2468.098439	84.294128	58.363252
2467.737147	78.268846	58.368257
2466.480065	76.446584	58.373261
2465.585077	84.664582	58.378266
2464.918888	74.823135	58.383271
2464.502766	82.721243	58.388276
2464.105940	79.242084	58.393281
2463.116489	73.608402	58.398285
2462.418731	82.552127	58.403290
2461.890016	70.941711	58.408295
2460.914267	81.418308	58.413300
2460.802680	75.669273	58.418305
2459.973691	71.757178	58.423309
2458.742789	78.886723	58.428314
2458.706200	70.713499	58.433319
2457.854074	76.870814	58.438324
2457.483135	77.212894	58.443329
2456.656368	75.475742	58.448333
2455.376739	79.191364	58.453338
2454.935993	70.042801	58.458343
2454.439299	77.806660	58.463348
2453.944801	82.408015	58.468353
2453.999794	76.552344	58.473357
2452.541940	82.467445	58.478362
2452.005778	76.825341	58.483367
2451.107272	74.727442	58.488372
2450.584473	75.468105	58.493377
2450.252343	77.419549	58.498381
2449.163994	78.231643	58.503386
2448.461900	76.450677	58.508391
2447.884949	74.510952	58.513396
2447.263396	76.353200	58.518401
2447.086188	72.801366	58.523405
2445.803939	74.901044	58.528410
2445.302523	71.186754	58.533415
2444.588200	72.858553	58.538420
2444.226745	71.204869	58.543425
2443.941493	75.034287	58.548429
2442.585991	80.202835	58.553434
2442.258606	72.873910	58.558439
2442.027042	77.826611	58.563444
2441.044362	78.989312	58.568449
2439.812123	73.069525	58.573453
2438.761561	76.456653	58.578458
2438.694452	68.268125	58.583463
2438.248953	75.471407	58.588468
2437.361166	70.378489	58.593473
2436.723738	70.028000	58.598477
2435.641538	78.036040	58.603482
2435.275601	63.882230	58.608487
2434.969023	72.447237	58.613492
2434.352866	66.989337	58.618497
2433.287252	68.716068	58.623501
2432.396162	68.338294	58.628506
2431.792220	70.195294	58.633511
2431.011669	68.400905	58.638516
2430.449117	69.559274	58.643521
2430.140867	67.845180	58.648525
2429.530938	72.615079	58.653530
2429.507522	66.080869	58.658535
2428.417266	74.831971	58.663540
2427.491199	72.619187	58.668545
2427.246327	69.031162	58.673549
2425.432985	75.622026	58.678554
2425.653286	70.394125	58.683559
2424.757976	76.625929	58.688564
2423.875625	74.917233	58.693569
2423.729319	72.947695	58.698573
2423.187908	73.109720	58.703578
2422.388599	71.870363	58.708583
2420.969632	85.291596	58.713588
2420.473189	78.848521	58.718593
2420.098465	69.775516	58.723597
2419.870391	71.590357	58.728602
2419.604982	75.110472	58.733607
2418.139247	73.397316	58.738612
2417.435765	81.843090	58.743617
2416.926602	80.890034	58.748621
2416.085010	85.650207	58.753626
2415.870364	80.272466	58.758631
2414.771762	79.224014	58.763636
2413.596231	69.765712	58.768641
2413.415240	76.053009	58.773645
2413.195900	79.902736	58.778650
2412.962767	77.221752	58.783655
2411.477434	78.173175	58.788660
2410.686394	84.443600	58.793665
2410.105579	69.053547	58.798669
2409.664153	78.300011	58.803674
2409.168858	73.895096	58.808679
2408.884033	76.992230	58.813684
2407.768914	76.684342	58.818689
2407.108094	77.679521	58.823693
2406.149610	74.912171	58.828698
2406.275316	68.203259	58.833703
2404.955216	76.777749	58.838708
2403.835260	76.204645	58.843713
2403.240449	83.189521	58.848717
2402.213464	77.448589	58.853722
2402.317691	72.281191	58.858727
2401.682262	81.087949	58.863732
2401.411862	77.439160	58.868737
2401.288940	81.940275	58.873741
2399.756199	76.469365	58.878746
2399.283025	71.532135	58.883751
2398.510670	74.074754	58.888756
2398.067777	79.254634	58.893761
2397.056188	81.064501	58.898765
2395.992729	67.992296	58.903770
2395.533854	76.135727	58.908775
2395.162366	77.815623	58.913780
2394.582090	72.229623	58.918785
2393.975101	69.956369	58.923789
2392.833312	70.752743	58.928794
2392.370105	70.701669	58.933799
2391.818847	70.011200	58.938804
2391.077449	70.649907	58.943809
2390.866699	66.716195	58.948813
2389.707154	73.506716	58.953818
2388.903837	67.193882	58.958823
2388.419024	74.251916	58.963828
2387.697996	68.713669	58.968833
2387.722619	66.488336	58.973837
2386.861513	77.475842	58.978842
2385.956563	74.081996	58.983847
2385.496084	70.086381	58.988852
2384.638154	78.711321	58.993857
2383.541376	71.112130	58.998861
2382.778504	77.071828	59.003866
2382.236814	71.176875	59.008871
2381.619077	75.185903	59.013876
2381.732665	73.019565	59.018881
2381.229553	57.686506	59.023885
2379.686403	78.617657	59.028890
2378.877674	67.260001	59.033895
2378.421455	73.550147	59.038900
2377.966656	68.440048	59.043905
2377.717712	66.413065	59.048909
2376.662092	71.648371	59.053914
2375.949302	67.325649	59.058919
2374.969818	74.707074	59.063924
2374.591589	71.568156	59.068929
2374.327197	72.182539	59.073933
2373.436789	79.299270	59.078938
2372.649442	71.447838	59.083943
2371.688990	78.740355	59.088948
2371.107035	76.130860	59.093953
2371.081857	70.495344	59.098957
2370.549765	71.365493	59.103962
2369.707296	68.024518	59.108967
2368.716804	71.523749	59.113972
2368.231976	72.190823	59.118977
2367.468600	75.273866	59.123981
2366.099361	72.052566	59.128986
2365.442460	69.436941	59.133991
2364.837312	70.516943	59.138996
2364.597823	79.503097	59.144001
2364.375222	70.365406	59.149005
2364.195331	79.921613	59.154010
2363.381621	80.593214	59.159015
2362.597083	83.640404	59.164020
2361.669077	71.865397	59.169025
2360.534343	75.568892	59.174029
2359.286124	74.039605	59.179034
2358.972253	66.736013	59.184039
2358.674850	75.373658	59.189044
2358.054223	80.468672	59.194049
2357.760424	76.183647	59.199053
2356.966553	75.069681	59.204058
2356.645942	75.064094	59.209063
2355.085823	75.758328	59.214068
2354.404783	67.586761	59.219073
2354.098884	74.666308	59.224077
2353.648179	77.071436	59.229082
2353.387328	73.822848	59.234087
2352.254945	85.073054	59.239092
2351.244339	67.911176	59.244097
2350.791225	68.458359	59.249101
2350.265132	73.955613	59.254106
2350.005962	74.657127	59.259111
2348.687043	78.619085	59.264116
2347.979087	79.300236	59.269121
2347.618154	73.402406	59.274125
2346.907346	79.708456	59.279130
2346.525970	69.415722	59.284135
2345.725507	81.119942	59.289140
2344.750240	76.177785	59.294145
2344.384067	69.304702	59.299149
2343.124205	76.002256	59.304154
2342.836289	67.056128	59.309159
2342.860109	71.880292	59.314164
2341.543607	74.525830	59.319169
2340.510658	66.642196	59.324173
2340.018346	77.458883	59.329178
2339.967107	67.184698	59.334183
2339.182891	70.862601	59.339188
2338.365942	71.410816	59.344193
2337.756476	72.024208	59.349197
2336.802931	76.091843	59.354202
2336.187775	70.570237	59.359207
2335.658627	76.213272	59.364212
2335.146285	69.698331	59.369217
2334.180263	66.730188	59.374221
2333.331674	70.309366	59.379226
2333.177413	71.089254	59.384231
2332.814093	69.660890	59.389236
2332.223625	67.475606	59.394241
2331.128496	66.109616	59.399245
2330.596882	74.373638	59.404250
2329.855458	65.026656	59.409255
2328.724333	74.254476	59.414260
2327.870950	70.532888	59.419265
2327.409619	66.092970	59.424269
2326.675881	72.050057	59.429274
2326.394533	61.140643	59.434279
2325.995669	69.458934	59.439284
2325.520094	70.708225	59.444289
2325.037589	61.532096	59.449293
2323.648180	74.731574	59.454298
2323.297636	68.412776	59.459303
2322.487671	71.783648	59.464308
2321.836351	75.378042	59.469313
2321.382022	74.627586	59.474317
2320.491955	81.761236	59.479322
2319.993052	62.408397	59.484327
2319.388172	74.657438	59.489332
2318.441579	69.951562	59.494337
2317.812226	73.377995	59.499341
2316.999632	73.792052	59.504346
2316.717710	73.020800	59.509351
2316.211317	73.954452	59.514356
2314.890088	67.655592	59.519361
2314.643856	70.890200	59.524365
2313.646502	72.725671	59.529370
2313.589410	73.278952	59.534375
2312.702823	79.899657	59.539380
2311.578213	69.188513	59.544385
2311.044843	69.812184	59.549389
2309.940808	71.904310	59.554394
2309.822622	66.883104	59.559399
2309.396820	72.592148	59.564404
2308.771819	68.495602	59.569409
2308.583988	69.394517	59.574413
2307.553562	68.341536	59.579418
2307.029143	67.749903	59.584423
2305.509218	72.881463	59.589428
2305.043196	72.062747	59.594433
2304.168988	64.853797	59.599437
2303.969929	74.497744	59.604442
2303.339082	72.148847	59.609447
2302.931409	79.286849	59.614452
2302.272542	71.380701	59.619457
2301.268451	69.733501	59.624461
2300.258505	78.425097	59.629466
2300.038539	67.845439	59.634471
2299.209847	74.435717	59.639476
2298.937942	73.449997	59.644481
2298.416317	69.959043	59.649485
2297.310932	71.448266	59.654490
2296.773554	64.743015	59.659495
2296.153414	72.484957	59.664500
2295.656478	68.579665	59.669505
2294.389071	70.324743	59.674509
2293.589435	77.209255	59.679514
2293.142009	64.317920	59.684519
2292.690478	74.354763	59.689524
2292.092201	76.889731	59.694529
2291.748466	70.398858	59.699533
2290.837944	71.751342	59.704538
2289.708312	77.604822	59.709543
2288.951511	78.335779	59.714548
2288.476762	71.985331	59.719553
2288.543861	75.130836	59.724557
2287.774958	81.067101	59.729562
2287.282248	65.439790	59.734567
2286.171067	70.133181	59.739572
2285.403843	66.726462	59.744577
2285.160375	66.965442	59.749581
2283.642067	75.425427	59.754586
2283.130838	74.411162	59.759591
2282.325445	74.681103	59.764596
2281.830924	68.469823	59.769601
2281.994625	67.005419	59.774605
2281.284827	68.175559	59.779610
2280.949161	67.735988	59.784615
2279.640129	76.819770	59.789620
2278.978935	71.834186	59.794625
2278.615270	66.380898	59.799629
2277.297649	75.851397	59.804634
2276.733311	72.614451	59.809639
2276.339584	72.979781	59.814644
2275.854703	76.676370	59.819649
2275.532115	76.710204	59.824653
2273.947001	78.081737	59.829658
2273.349554	76.609732	59.834663
2272.664294	77.952909	59.839668
2272.186943	80.959815	59.844673
2271.977844	75.374702	59.849677
2270.618905	82.886553	59.854682
2270.093581	74.574298	59.859687
2269.568549	76.038491	59.864692
2269.042675	70.998190	59.869697
2268.848558	71.585955	59.874701
2267.291201	69.343004	59.879706
2266.864519	66.878281	59.884711
2266.265221	69.542894	59.889716
2265.248747	76.726979	59.894721
2265.351526	68.860326	59.899725
2264.823132	73.006050	59.904730
2263.845155	66.148790	59.909735
2263.205535	74.537068	59.914740
2262.706146	71.154417	59.919745
2261.807414	71.394929	59.924750
2260.580567	76.247442	59.929754
2260.063660	65.441475	59.934759
2259.279458	67.970740	59.939764
2258.822197	62.888317	59.944769
2258.793269	61.418960	59.949774
2258.403755	75.890958	59.954778
2257.600378	63.696795	59.959783
2256.711778	69.460902	59.964788
2255.738625	69.873216	59.969793
2254.755192	68.758921	59.974798
2254.011072	68.973390	59.979802
2253.220083	62.524667	59.984807
2252.799887	64.877216	59.989812
2252.226371	69.249727	59.994817
2252.089917	62.041335	59.999822
2251.456039	73.220108	60.004826
2251.251142	65.033060	60.009831
2249.926275	68.333707	60.014836
2249.235299	72.384872	60.019841
2248.496472	67.044294	60.024846
2247.210452	71.436417	60.029850
2246.568758	69.753307	60.034855
2246.482296	71.050137	60.039860
2245.939631	75.735127	60.044865
2245.777926	69.009060	60.049870
2244.628149	75.868586	60.054874
2244.095374	69.549384	60.059879
2243.106694	69.503713	60.064884
2242.180178	69.656221	60.069889
2241.816467	58.623545	60.074894
2241.301314	63.968933	60.079898
2240.993736	69.726837	60.084903
2239.951429	66.472559	60.089908
2238.819569	73.562697	60.094913
2238.518915	60.160375	60.099918
2238.122304	70.608596	60.104922
2237.467698	59.832501	60.109927
2236.255836	72.540983	60.114932
2235.556113	71.433436	60.119937
2235.231314	70.460713	60.124942
2234.603821	73.347248	60.129946
2234.138560	62.476405	60.134951
2233.891740	72.920722	60.139956
2232.899059	72.692981	60.144961
2232.230236	67.269384	60.149966
2231.341535	69.473905	60.154970
2230.946552	62.884837	60.159975
2229.733040	68.751877	60.164980
2229.025905	63.505355	60.169985
2228.714384	71.295174	60.174990
2227.718201	71.954975	60.179994
2227.686466	63.880417	60.184999
2226.838079	71.679156	60.190004
2225.857013	70.204080	60.195009
2225.366970	67.080354	60.200014
2224.366501	73.774222	60.205018
2224.366387	68.137194	60.210023
2223.609232	67.121967	60.215028
2222.258157	73.940923	60.220033
2222.086090	66.972692	60.225038
2221.419345	74.917600	60.230042
2221.059869	64.583254	60.235047
2220.722549	70.538868	60.240052
2219.274399	70.192449	60.245057
2218.997095	63.698122	60.250062
2218.096224	70.815072	60.255066
2217.394905	68.496792	60.260071
2216.194526	73.240973	60.265076
2215.548313	69.807651	60.270081
2215.303005	66.321953	60.275086
2214.875324	78.114785	60.280090
2214.590072	69.403868	60.285095
2214.317172	76.351063	60.290100
2213.002895	69.752240	60.295105
2212.201032	65.122293	60.300110
2211.813684	73.130731	60.305114
2210.867146	67.449511	60.310119
2209.750494	72.673567	60.315124
2208.916910	68.054571	60.320129
2208.710535	69.230203	60.325134
2208.244618	67.801632	60.330138
2208.006513	69.630035	60.335143
2207.174897	70.146042	60.340148
2206.108308	72.509667	60.345153
2205.690938	65.386029	60.350158
2205.025067	66.904311	60.355162
2204.453094	61.049306	60.360167
2203.461866	62.905061	60.365172
2202.537784	72.957585	60.370177
2202.295506	66.203463	60.375182
2201.552674	70.207448	60.380186
2201.376462	59.985051	60.385191
2200.408713	63.904346	60.390196
2199.440244	64.383365	60.395201
2198.765418	67.342732	60.400206
2198.330273	66.424013	60.405210
2198.103375	72.043781	60.410215
2196.977830	67.265910	60.415220
2195.815610	65.619724	60.420225
2195.490291	63.024784	60.425230
2195.003367	68.587972	60.430234
2194.977551	70.685979	60.435239
2193.656004	69.224929	60.440244
2192.828312	66.891161	60.445249
2192.735722	61.055224	60.450254
2191.169133	68.961790	60.455258
2191.193977	60.042330	60.460263
2190.516506	64.947340	60.465268
2189.165183	60.418867	60.470273
2189.006021	57.775381	60.475278
2188.354012	67.235868	60.480282
2187.541128	63.332126	60.485287
2187.736193	65.777607	60.490292
2186.415141	64.535151	60.495297
2185.934031	63.107208	60.500302
2184.927025	62.753247	60.505306
2184.751740	61.038932	60.510311
2183.298170	61.699597	60.515316
2182.458781	68.645778	60.520321
2182.257520	67.627853	60.525326
2181.466456	68.880190	60.530330
2181.282695	66.315514	60.535335
2180.905248	62.494799	60.540340
2180.449527	65.416695	60.545345
2179.561537	72.989325	60.550350
2178.270396	73.443009	60.555354
2177.908493	63.669591	60.560359
2177.423488	73.606765	60.565364
2176.024526	67.722675	60.570369
2175.900179	66.733832	60.575374
2175.111287	70.085326	60.580378
2174.794062	64.277938	60.585383
2174.354610	69.157244	60.590388
2172.936348	72.204680	60.595393
2172.374068	65.589364	60.600398
2171.615767	71.001209	60.605402
2171.528668	69.181421	60.610407
2170.826106	74.032702	60.615412
2169.419997	72.566779	60.620417
2168.921854	66.130751	60.625422
2168.481956	71.219731	60.630426
2168.286466	66.426090	60.635431
2167.744300	73.283549	60.640436
2166.007097	82.108615	60.645441
2165.469416	73.753496	60.650446
2164.823758	74.765055	60.655450
2164.395433	75.545241	60.660455
2164.315003	70.838497	60.665460
2163.704064	76.554340	60.670465
2163.134628	58.696194	60.675470
2161.985232	77.728108	60.680474
2161.583262	74.326835	60.685479
2160.737499	75.108154	60.690484
2159.924669	72.194370	60.695489
2158.992656	69.943578	60.700494
2157.868137	73.607467	60.705498
2157.393813	70.354354	60.710503
2157.652046	66.437555	60.715508
2157.063601	69.304786	60.720513
2156.667515	72.403189	60.725518
2155.424173	78.960191	60.730522
2154.955960	66.701627	60.735527
2154.173514	71.034091	60.740532
2153.624070	73.096130	60.745537
2152.569718	80.876027	60.750542
2151.618177	77.794921	60.755546
2151.294296	68.921680	60.760551
2150.670876	71.243467	60.765556
2150.768489	73.139187	60.770561
2149.840888	72.294827	60.775566
2148.372768	66.150611	60.780570
2148.115051	66.362035	60.785575
2147.652416	66.345620	60.790580
2147.003502	69.222010	60.795585
2145.846225	62.170455	60.800590
2144.803603	75.339063	60.805594
2144.493708	65.715829	60.810599
2144.220636	71.535723	60.815604
2143.993741	70.925195	60.820609
2143.384277	71.099281	60.825614
2142.432088	80.577564	60.830618
2141.716013	70.003043	60.835623
2140.936372	72.842979	60.840628
2139.649915	74.459117	60.845633
2139.333287	62.894214	60.850638
2138.304458	67.779982	60.855642
2137.894973	65.549955	60.860647
2137.164036	66.823197	60.865652
2137.077502	70.006811	60.870657
2136.809709	64.762926	60.875662
2135.418511	74.311947	60.880666
2134.701318	67.579453	60.885671
2134.468628	61.018299	60.890676
2133.966510	70.874715	60.895681
2133.371978	62.817083	60.900686
2131.868501	77.212365	60.905690
2131.208879	66.574117	60.910695
2131.216803	68.373469	60.915700
2130.973043	61.006212	60.920705
2130.067152	62.421084	60.925710
2128.685433	78.021549	60.930714
2128.247099	65.566442	60.935719
2127.995965	69.946190	60.940724
2126.292741	67.948485	60.945729
2125.768780	68.309652	60.950734
2124.822980	76.831220	60.955738
2124.797434	68.080241	60.960743
2124.351097	65.658368	60.965748
2123.889600	75.024700	60.970753
2123.736702	69.699982	60.975758
2122.769335	70.561312	60.980762
2121.721486	62.507006	60.985767
2121.294053	67.916737	60.990772
2120.214740	67.114119	60.995777
2119.438101	61.325316	61.000782
2118.764469	73.358355	61.005786
2118.163184	75.766357	61.010791
2117.811783	69.137876	61.015796
2117.288729	68.403930	61.020801
2117.096422	63.891977	61.025806
2115.986307	73.981062	61.030810
2115.651332	64.427646	61.035815
2115.061189	72.009337	61.040820
2113.581004	71.428040	61.045825
2113.004052	69.404282	61.050830
2112.625657	77.112780	61.055834
2111.769653	78.752799	61.060839
2110.753999	75.568988	61.065844
2110.098767	74.029127	61.070849
2109.738349	61.720169	61.075854
2108.698396	71.548973	61.080858
2108.210082	71.126443	61.085863
2107.795513	67.460500	61.090868
2107.298287	74.061994	61.095873
2107.078574	64.987005	61.100878
2105.804531	72.125161	61.105882
2104.940705	62.003804	61.110887
2104.552438	68.084179	61.115892
2103.856075	76.070867	61.120897
2103.324697	67.184178	61.125902
2102.197590	78.104694	61.130906
2101.716629	67.376292	61.135911
2101.353680	68.650151	61.140916
2100.941958	73.252753	61.145921
2099.644914	74.792951	61.150926
2098.738143	73.230591	61.155930
2098.239560	66.043493	61.160935
2097.645588	67.516728	61.165940
2097.537201	75.481005	61.170945
2096.999241	67.277917	61.175950
2096.257045	66.404225	61.180954
2095.368815	67.641615	61.185959
2094.865624	60.321893	61.190964
2094.208277	72.197810	61.195969
2093.314188	63.531051	61.200974
2092.313481	70.582196	61.205978
2091.829381	61.164420	61.210983
2091.575644	64.536887	61.215988
2090.916485	70.750434	61.220993
2090.110281	64.569602	61.225998
2088.666812	69.577610	61.231002
2088.520007	70.621482	61.236007
2088.415729	64.508087	61.241012
2087.451856	71.041769	61.246017
2086.463838	53.809829	61.251022
2085.756641	68.265090	61.256026
2085.172065	63.744447	61.261031
2084.780888	67.165289	61.266036
2084.375668	73.151464	61.271041
2083.732048	62.825087	61.276046
2082.608783	75.310018	61.281050
2081.977280	62.674023	61.286055
2081.810117	72.779454	61.291060
2080.219124	68.248585	61.296065
2079.759091	62.595893	61.301070
2078.841717	71.734681	61.306074
2078.489620	66.109709	61.311079
2078.329141	65.524534	61.316084
2077.794244	63.943177	61.321089
2077.494659	70.625335	61.326094
2075.906879	71.732125	61.331098
2075.569165	68.707490	61.336103
2075.209269	66.240443	61.341108
2074.139467	67.790329	61.346113
2073.144423	66.576218	61.351118
2072.430700	69.365019	61.356122
2072.251085	71.371309	61.361127
2071.794441	62.071993	61.366132
2071.297565	75.331990	61.371137
2069.956322	67.756941	61.376142
2068.745613	70.202080	61.381146
2068.401903	62.105902	61.386151
2068.239331	64.299137	61.391156
2067.712452	67.786610	61.396161
2067.483632	62.373442	61.401166
2065.902967	61.496331	61.406170
2065.323777	62.841518	61.411175
2064.528353	59.773993	61.416180
2063.854423	72.712969	61.421185
2064.095201	62.081385	61.426190
2063.395074	66.274650	61.431194
2062.553681	64.987288	61.436199
2062.079440	63.105832	61.441204
2060.891338	74.873987	61.446209
2059.897233	60.271940	61.451214
2059.175828	74.533065	61.456218
2059.048237	67.964598	61.461223
2058.395265	70.319473	61.466228
2058.032472	68.889858	61.471233
2057.474390	69.962236	61.476238
2056.404736	67.631195	61.481242
2055.622576	70.929843	61.486247
2055.202731	64.986870	61.491252
2053.805898	69.397589	61.496257
2052.931642	65.234776	61.501262
2052.530698	72.701215	61.506266
2052.608545	65.508291	61.511271
2052.296137	68.106482	61.516276
2051.268320	69.337756	61.521281
2050.601069	64.775208	61.526286
2049.351051	71.887159	61.531290
2048.711493	69.116253	61.536295
2048.379240	64.451802	61.541300
2048.003868	69.070291	61.546305
2047.241140	61.527348	61.551310
2046.252584	72.162072	61.556314
2045.588966	68.197696	61.561319
2044.859488	74.765499	61.566324
2044.755294	78.362644	61.571329
2044.352828	67.020456	61.576334
2042.768695	74.202979	61.581338
2042.155491	69.441325	61.586343
2041.910563	67.990367	61.591348
2041.222805	70.089493	61.596353
2040.648236	63.169605	61.601358
2039.382675	67.851546	61.606362
2038.912219	66.074836	61.611367
2038.665702	60.153534	61.616372
2038.090793	69.068357	61.621377
2037.618231	65.871403	61.626382
2036.448340	69.958714	61.631386
2035.858886	68.525241	61.636391
2035.246228	67.182575	61.641396
2034.369889	75.055187	61.646401
2033.735444	65.180391	61.651406
2032.921847	75.433099	61.656410
2032.524680	67.198048	61.661415
2031.973088	77.744219	61.666420
2031.525447	67.911282	61.671425
2030.535273	59.658856	61.676430
2029.579341	66.187236	61.681434
2029.224541	65.932527	61.686439
2028.996188	59.641028	61.691444
2027.999839	69.105945	61.696449
2026.936111	64.206629	61.701454
2026.226498	67.752597	61.706458
2025.597481	68.971711	61.711463
2025.499729	67.846882	61.716468
2024.926744	70.992127	61.721473
2023.999565	65.502634	61.726478
2022.899458	77.610598	61.731482
2022.581724	74.341768	61.736487
2021.942617	71.835646	61.741492
2021.523876	66.195635	61.746497
2020.950079	58.604200	61.751502
2019.737267	65.439404	61.756506
2018.959422	67.936033	61.761511
2018.793014	65.315506	61.766516
2018.052582	63.531295	61.771521
2017.694420	63.463076	61.776526
2016.582630	69.031709	61.781530
2015.873551	66.484271	61.786535
2015.317261	68.674197	61.791540
2014.753196	73.009187	61.796545
2014.555118	60.961022	61.801550
2013.471658	64.287528	61.806554
2012.569167	65.127911	61.811559
2011.982977	60.724394	61.816564
2011.113933	72.122199	61.821569
2010.689075	67.040187	61.826574
2010.161935	78.777393	61.831578
2009.108612	60.614050	61.836583
2009.184623	60.387094	61.841588
2008.297493	65.113646	61.846593
2008.052617	63.407691	61.851598
2006.544928	66.978468	61.856602
2005.768720	64.082528	61.861607
2005.657311	74.676161	61.866612
2004.443659	67.222199	61.871617
2003.472568	64.040265	61.876622
2003.124326	73.116047	61.881626
2002.327430	67.736899	61.886631
2002.270801	66.675692	61.891636
2001.741415	66.140991	61.896641
2001.690144	59.878413	61.901646
2000.421814	60.485336	61.906650
1999.686888	64.961652	61.911655
1999.475180	55.128239	61.916660
1998.134999	66.477951	61.921665
1997.459653	58.513906	61.926670
1996.646209	67.717811	61.931674
1996.565310	64.644123	61.936679
1995.648262	63.775487	61.941684
1994.383659	63.411943	61.946689
1994.173143	52.752572	61.951694
1993.453527	66.622214	61.956698
1992.910397	62.089759	61.961703
1992.459020	55.469324	61.966708
1991.237125	58.933587	61.971713
1991.418961	54.716845	61.976718
1990.319503	64.913846	61.981722
1989.808965	59.273755	61.986727
1989.018384	62.144787	61.991732
1987.785974	65.786107	61.996737
1987.425249	58.756233	62.001742
1986.806612	63.391467	62.006746
1986.461567	68.721978	62.011751
1986.172184	54.331375	62.016756
1984.969181	52.958653	62.021761
1984.225868	61.245462	62.026766
1983.315312	71.197795	62.031770
1982.958241	63.180096	62.036775
1982.803654	61.969468	62.041780
1981.305435	69.877014	62.046785
1980.831980	59.827858	62.051790
1979.639391	65.560706	62.056794
1979.592765	64.415686	62.061799
1979.113427	60.451378	62.066804
1978.359382	64.469537	62.071809
1977.922996	59.073333	62.076814
1976.814915	67.150975	62.081818
1976.076094	63.498674	62.086823
1975.582397	56.368001	62.091828
1975.375830	67.125135	62.096833
1974.973080	65.266984	62.101838
1973.903144	65.369863	62.106842
1973.177516	66.117238	62.111847
1972.807988	56.193592	62.116852
1971.692085	73.253273	62.121857
1970.504151	56.636601	62.126862
1969.771765	73.148723	62.131866
1969.578393	66.189691	62.136871
1969.367701	66.042566	62.141876
1968.763161	66.814621	62.146881
1968.276785	60.927647	62.151886
1967.197181	68.124927	62.156890
1966.595138	64.152795	62.161895
1966.154198	54.282814	62.166900
1965.166306	61.797943	62.171905
1964.190709	59.841609	62.176910
1963.383539	67.850411	62.181914
1963.169382	64.867412	62.186919
1962.426273	59.777878	62.191924
1961.895788	61.565120	62.196929
1961.630280	63.684389	62.201934
1960.540561	63.597241	62.206938
1960.087155	63.001786	62.211943
1959.761525	65.220152	62.216948
1958.361928	67.843671	62.221953
1957.580636	61.456511	62.226958
1956.877984	63.107816	62.231962
1956.490866	67.257414	62.236967
1956.281927	61.074702	62.241972
1955.594441	69.224868	62.246977
1954.025508	56.283499	62.251982
1953.323636	61.793465	62.256986
1953.014210	64.737319	62.261991
1953.044993	60.950610	62.266996
1952.263649	62.932338	62.272001
1951.397858	54.189731	62.277006
1950.572124	62.722344	62.282010
1949.678356	62.703516	62.287015
1949.638828	60.527850	62.292020
1948.609832	69.250362	62.297025
1948.196570	58.472524	62.302030
1947.365687	68.431754	62.307034
1946.384848	61.361917	62.312039
1946.080559	57.509769	62.317044
1945.630798	66.017540	62.322049
1944.737482	58.871551	62.327054
1943.833317	68.980680	62.332058
1942.942637	65.383177	62.337063
1942.733307	61.354922	62.342068
1942.048523	74.714553	62.347073
1941.837147	57.353755	62.352078
1940.414780	66.185794	62.357082
1939.835319	62.938853	62.362087
1939.807424	60.141485	62.367092
1939.030577	67.697882	62.372097
1938.005501	58.020194	62.377102
1936.696921	61.896387	62.382106
1936.364529	59.040191	62.387111
1936.397366	53.999104	62.392116
1935.536201	67.986509	62.397121
1935.277057	54.448868	62.402126
1934.276439	64.896587	62.407130
1934.045598	61.419491	62.412135
1933.373466	59.136920	62.417140
1931.860699	71.630860	62.422145
1930.913106	65.227154	62.427150
1930.147834	72.056471	62.432154
1929.817901	58.773296	62.437159
1929.601352	57.853127	62.442164
1929.002275	73.612209	62.447169
1928.694039	62.022621	62.452174
1927.169587	64.756319	62.457178
1926.905349	70.772453	62.462183
1926.743131	56.423263	62.467188
1925.277719	64.756635	62.472193
1924.382513	55.037790	62.477198
1923.544263	65.956266	62.482202
1923.191558	65.015181	62.487207
1923.184487	58.354274	62.492212
1922.448464	66.567609	62.497217
1922.226239	58.071741	62.502222
1921.187826	64.936729	62.507226
1920.197682	63.996931	62.512231
1919.924895	56.999391	62.517236
1918.821945	60.973825	62.522241
1918.592169	64.573106	62.527246
1917.432751	68.560360	62.532250
1916.636351	64.602143	62.537255
1916.569991	60.193395	62.542260
1915.961272	66.744886	62.547265
1915.102745	60.526468	62.552270
1914.059117	67.177228	62.557274
1914.036139	66.406306	62.562279
1913.070291	70.396367	62.567284
1911.742755	68.128422	62.572289
1911.422387	69.217776	62.577294
1910.863259	68.160826	62.582298
1910.483234	59.601168	62.587303
1910.258322	60.054875	62.592308
1909.050182	58.540950	62.597313
1907.951694	46.786184	62.602318
1907.370018	55.708079	62.607322
1906.999581	58.451195	62.612327
1906.877960	49.716685	62.617332
1905.666011	59.753732	62.622337
1905.228591	56.263034	62.627342
1904.814681	65.634636	62.632346
1903.992290	56.621336	62.637351
1903.028619	55.287424	62.642356
1901.860412	63.509564	62.647361
1901.366612	64.845684	62.652366
1900.992242	58.997584	62.657370
1900.681411	52.462854	62.662375
1900.222004	49.201305	62.667380
1899.079494	62.221220	62.672385
1898.043006	57.864756	62.677390
1897.620778	52.830866	62.682394
1897.737879	61.177320	62.687399
1896.997033	55.966234	62.692404
1895.557546	62.841814	62.697409
1894.608318	49.645258	62.702414
1894.608518	61.347099	62.707418
1894.120404	64.051534	62.712423
1893.342126	67.019549	62.717428
1892.242017	71.215732	62.722433
1892.090143	55.970735	62.727438
1891.532350	65.118672	62.732442
1890.440105	72.306285	62.737447
1889.656784	62.058325	62.742452
1888.501269	66.229250	62.747457
1888.301084	62.924538	62.752462
1887.465675	68.161314	62.757466
1887.191774	69.317323	62.762471
1887.042648	63.593709	62.767476
1886.507630	70.223775	62.772481
1885.398996	61.175371	62.777486
1884.620560	65.165740	62.782490
1883.897549	61.013009	62.787495
1883.000531	51.588949	62.792500
1882.259193	74.323002	62.797505
1881.589489	57.233251	62.802510
1881.181995	66.591124	62.807514
1880.777180	57.162591	62.812519
1880.483597	64.524215	62.817524
1879.265377	62.308233	62.822529
1878.622370	63.131088	62.827534
1878.086948	62.153767	62.832538
1877.754454	63.009154	62.837543
1876.725900	58.950142	62.842548
1875.646072	63.720727	62.847553
1874.911904	55.970054	62.852558
1874.378549	58.755253	62.857562
1874.068656	70.128848	62.862567
1873.882927	57.891893	62.867572
1872.357470	57.480246	62.872577
1871.986195	49.944588	62.877582
1871.344219	62.676778	62.882586
1870.707226	59.769677	62.887591
1870.365756	66.152692	62.892596
1869.816225	65.306859	62.897601
1869.049360	58.983959	62.902606
1868.264955	64.189906	62.907610
1867.403865	53.931973	62.912615
1866.576582	56.060907	62.917620
1865.343433	65.272280	62.922625
1865.207115	61.613631	62.927630
1864.593730	52.990490	62.932634
1864.079903	56.577184	62.937639
1863.910150	46.287822	62.942644
1862.350428	58.589278	62.947649
1861.960704	52.737496	62.952654
1861.515953	55.816603	62.957658
1860.913225	62.947310	62.962663
1860.502799	60.469983	62.967668
1859.442492	61.698165	62.972673
1859.071360	49.775953	62.977678
1858.350601	61.538766	62.982682
1857.436744	57.666181	62.987687
1856.808162	50.018235	62.992692
1855.681423	55.964825	62.997697
1855.114052	56.402520	63.002702
1854.584698	50.702518	63.007706
1854.319054	56.656916	63.012711
1854.121608	55.811242	63.017716
1853.327597	57.298591	63.022721
1852.524616	56.603486	63.027726
1852.333159	51.704587	63.032730
1851.008927	52.931741	63.037735
1849.913717	52.183610	63.042740
1849.300458	52.104573	63.047745
1848.956590	47.614630	63.052750
1848.602801	48.124728	63.057754
1847.659539	57.645306	63.062759
1846.689089	54.723025	63.067764
1845.993193	56.800274	63.072769
1845.583699	53.526639	63.077774
1845.084110	48.241530	63.082778
1844.601017	52.512936	63.087783
1843.204582	51.566088	63.092788
1842.349621	57.279875	63.097793
1842.386388	48.689585	63.102798
1841.917610	53.209585	63.107802
1841.098927	57.689980	63.112807
1840.517607	56.350268	63.117812
1838.963583	51.493835	63.122817
1838.823476	59.268127	63.127822
1838.498607	59.680125	63.132826
1837.842900	52.772187	63.137831
1837.518503	48.910466	63.142836
1836.276376	56.884742	63.147841
1835.824498	52.731028	63.152846
1835.466622	57.933474	63.157850
1834.087537	53.535382	63.162855
1833.360980	56.103779	63.167860
1832.538799	63.069146	63.172865
1832.109434	57.301119	63.177870
1831.679089	60.949714	63.182874
1831.259768	62.379278	63.187879
1831.315957	61.009837	63.192884
1829.844822	58.589255	63.197889
1829.501888	56.581549	63.202894
1828.776542	55.523048	63.207898
1827.787353	60.834689	63.212903
1827.131191	51.194971	63.217908
1826.263190	61.931441	63.222913
1825.876013	57.877574	63.227918
1824.970551	60.295799	63.232922
1823.847315	59.930609	63.237927
1823.176470	49.422652	63.242932
1822.614825	49.665169	63.247937
1822.708322	52.319835	63.252942
1822.186275	60.201312	63.257946
1821.374645	63.834223	63.262951
1821.048174	55.352653	63.267956
1820.043163	58.891549	63.272961
1819.347006	53.099305	63.277966
1818.949483	51.232777	63.282970
1817.445073	60.019662	63.287975
1816.935791	50.606254	63.292980
1816.229848	61.601960	63.297985
1815.787340	53.276029	63.302990
1815.355655	56.543158	63.307994
1814.797559	60.667539	63.312999
1814.263317	52.313883	63.318004
1813.268868	69.310943	63.323009
1813.100856	59.328375	63.328014
1811.998520	56.850621	63.333018
1810.567117	58.653861	63.338023
1810.252263	50.435954	63.343028
1809.865490	65.114662	63.348033
1809.624310	60.953716	63.353038
1809.196699	59.809543	63.358042
1807.986998	52.467863	63.363047
1806.889757	52.469267	63.368052
1806.381469	58.579648	63.373057
1806.437668	52.047264	63.378062
1805.643066	54.454024	63.383066
1804.728445	48.327730	63.388071
1804.373658	53.428993	63.393076
1803.568860	59.446821	63.398081
1802.733585	62.543013	63.403086
1801.293816	61.273998	63.408090
1801.048627	55.559330	63.413095
1800.899093	58.002166	63.418100
1800.633377	57.221069	63.423105
1799.912659	57.812896	63.428110
1798.078327	54.146360	63.433114
1797.316729	57.441122	63.438119
1797.012450	46.825063	63.443124
1796.357616	52.608424	63.448129
1796.269809	52.613959	63.453134
1795.971586	55.676288	63.458138
1795.182141	56.483945	63.463143
1794.207662	56.317512	63.468148
1793.366102	57.635775	63.473153
1792.900295	50.559178	63.478158
1791.323868	56.830995	63.483162
1790.788756	54.630788	63.488167
1791.299843	54.664114	63.493172
1790.012276	55.753567	63.498177
1789.880645	50.011580	63.503182
1789.289020	54.496550	63.508186
1787.806789	58.795230	63.513191
1787.953735	45.916405	63.518196
1787.121738	57.457863	63.523201
1786.437659	54.139640	63.528206
1785.140535	53.501855	63.533210
1784.428461	56.373688	63.538215
1784.003061	47.276318	63.543220
1783.619229	61.057712	63.548225
1783.205506	55.096762	63.553230
1782.256469	54.210351	63.558234
1781.062442	57.112541	63.563239
1780.823236	56.447693	63.568244
1780.031647	56.030902	63.573249
1780.003039	47.720607	63.578254
1779.235281	53.866302	63.583258
1777.766463	51.914662	63.588263
1777.621236	45.998958	63.593268
1777.283946	62.034531	63.598273
1776.641325	50.307595	63.603278
1775.162473	47.777040	63.608282
1774.242782	45.233707	63.613287
1773.960238	44.976126	63.618292
1773.459661	43.986936	63.623297
1773.328183	46.118800	63.628302
1772.948586	43.081629	63.633306
1771.486000	46.846839	63.638311
1770.928930	41.446057	63.643316
1770.218614	45.255048	63.648321
1769.637503	42.073548	63.653326
1769.124404	37.753092	63.658330
1767.722177	40.004487	63.663335
1767.580983	35.269494	63.668340
1766.681752	48.085553	63.673345
1766.588077	41.433167	63.678350
1765.923441	45.447097	63.683354
1765.472976	51.624948	63.688359
1764.864949	47.070085	63.693364
1763.844840	47.981946	63.698369
1763.390437	47.313658	63.703374
1761.992140	54.109980	63.708378
1761.355847	51.599076	63.713383
1761.001171	44.726885	63.718388
1760.246820	53.848055	63.723393
1760.126073	46.811895	63.728398
1759.055113	51.616502	63.733402
1758.227339	57.601161	63.738407
1757.807677	49.686578	63.743412
1757.152906	49.799778	63.748417
1756.696543	47.719518	63.753422
1755.722604	54.722300	63.758426
1754.854108	43.578736	63.763431
1754.416504	42.157607	63.768436
1753.407649	56.591835	63.773441
1753.309266	50.613645	63.778446
1752.921146	40.658100	63.783450
1751.708801	49.441991	63.788455
1751.178168	52.757630	63.793460
1750.815549	58.597178	63.798465
1750.281591	50.983982	63.803470
1748.793459	46.091835	63.808474
1748.168554	53.808154	63.813479
1747.665140	48.530818	63.818484
1747.299080	59.633757	63.823489
1746.996377	58.159152	63.828494
1745.843488	56.449900	63.833498
1744.648536	45.702049	63.838503
1744.562107	51.055014	63.843508
1743.924056	58.616091	63.848513
1743.765950	47.023755	63.853518
1742.700975	50.990535	63.858522
1741.711174	59.050726	63.863527
1741.461188	56.922918	63.868532
1740.930461	61.155116	63.873537
1740.019328	59.607781	63.878542
1738.925680	55.417052	63.883546
1738.215871	61.674017	63.888551
1738.147782	58.126066	63.893556
1737.487615	61.384138	63.898561
1737.222325	61.268469	63.903566
1736.089194	52.638370	63.908570
1735.141951	66.984700	63.913575
1734.645047	59.012678	63.918580
1733.799939	65.224114	63.923585
1732.981540	58.587574	63.928590
1732.121531	60.056234	63.933594
1731.593870	61.783408	63.938599
1731.196503	61.056418	63.943604
1730.515945	64.561128	63.948609
1730.595144	62.973023	63.953614
1730.184490	53.189481	63.958618
1729.208346	61.761658	63.963623
1728.648356	55.680880	63.968628
1727.238199	67.659944	63.973633
1726.209122	62.982924	63.978638
1725.735038	64.741194	63.983642
1725.131777	58.864390	63.988647
1724.756968	57.454228	63.993652
1724.087077	60.033862	63.998657
1723.869118	57.771502	64.003662
1722.874407	61.978885	64.008666
1722.019833	66.159923	64.013671
1721.879534	51.227576	64.018676
1720.565189	57.228786	64.023681
1719.735732	54.297407	64.028686
1719.361631	67.437296	64.033690
1718.296046	55.195005	64.038695
1718.059473	56.200560	64.043700
1717.577773	59.100084	64.048705
1717.007882	60.675808	64.053710
1716.207540	52.544933	64.058714
1714.993021	57.181095	64.063719
1714.799924	54.295166	64.068724
1714.214540	55.506846	64.073729
1713.878141	56.817627	64.078734
1713.054203	55.552602	64.083738
1712.086954	61.536265	64.088743
1711.528622	49.505594	64.093748
1710.896509	59.356610	64.098753
1710.458082	52.183766	64.103758
1709.378523	54.521275	64.108762
1708.621554	60.324490	64.113767
1708.649121	55.493122	64.118772
1707.958952	66.810593	64.123777
1706.874911	55.183281	64.128782
1706.073524	57.190968	64.133786
1705.371261	53.699825	64.138791
1705.204982	56.160920	64.143796
1704.363523	68.404241	64.148801
1703.052363	60.792595	64.153806
1702.688605	64.334280	64.158810
1701.799231	61.998920	64.163815
1701.768578	54.382502	64.168820
1701.277463	63.969801	64.173825
1700.772255	54.812679	64.178830
1699.690361	56.487461	64.183834
1698.789737	67.701213	64.188839
1698.197493	55.774234	64.193844
1697.953437	58.011412	64.198849
1697.411298	57.203807	64.203854
1696.531118	71.212233	64.208858
1695.626413	71.129797	64.213863
1695.604408	52.918402	64.218868
1693.747262	59.424979	64.223873
1693.239358	66.469208	64.228878
1692.720046	62.585985	64.233882
1692.243906	60.312149	64.238887
1692.133513	51.279703	64.243892
1691.331578	54.660321	64.248897
1690.681532	51.201691	64.253902
1689.588484	58.791286	64.258906
1689.033805	64.126092	64.263911
1688.853136	53.568630	64.268916
1687.454485	51.520146	64.273921
1686.584609	43.802611	64.278926
1686.041193	51.730372	64.283930
1685.298559	55.882389	64.288935
1685.402791	51.138164	64.293940
1684.994463	50.920268	64.298945
1684.452399	54.381546	64.303950
1683.388166	55.634906	64.308954
1682.481702	60.779258	64.313959
1682.119602	45.903035	64.318964
1680.275949	53.551992	64.323969
1679.808730	53.776787	64.328974
1679.369775	47.718729	64.333978
1678.729199	52.407469	64.338983
1678.555673	54.647972	64.343988
1678.193936	59.281895	64.348993
1677.981871	47.564992	64.353998
1677.029430	56.568097	64.359002
1675.918065	55.290685	64.364007
1675.607207	43.309651	64.369012
1674.163107	51.667441	64.374017
1673.516280	48.677980	64.379022
1673.104030	55.209280	64.384026
1672.550591	60.719917	64.389031
1672.550023	45.320800	64.394036
1671.253845	56.415529	64.399041
1670.398759	51.341270	64.404046
1670.266653	52.231060	64.409050
1669.213036	61.569624	64.414055
1668.884566	50.060132	64.419060
1667.574271	57.806899	64.424065
1666.952480	52.121955	64.429070
1666.861759	53.240311	64.434074
1665.839532	48.634372	64.439079
1665.900015	45.048638	64.444084
1664.428642	61.096292	64.449089
1663.771326	47.092000	64.454094
1663.195920	61.597322	64.459098
1662.378584	58.471650	64.464103
1662.232172	47.823864	64.469108
1661.318499	58.670782	64.474113
1660.423812	45.650097	64.479118
1659.983165	52.935432	64.484122
1659.342984	60.683580	64.489127
1659.091638	40.336151	64.494132
1657.994975	55.340776	64.499137
1656.943555	54.868602	64.504142
1656.665532	46.655471	64.509146
1655.830903	58.175280	64.514151
1655.773614	53.062001	64.519156
1655.316907	49.334251	64.524161
1654.266460	49.391230	64.529166
1653.351904	49.754941	64.534170
1652.807332	58.165646	64.539175
1652.361010	52.657906	64.544180
1650.777401	60.899058	64.549185
1650.435158	53.737789	64.554190
1649.889743	52.204466	64.559194
1649.026810	57.351241	64.564199
1649.132103	54.769504	64.569204
1648.336314	57.361216	64.574209
1647.535909	51.191336	64.579214
1647.101587	55.567297	64.584218
1645.948332	61.898573	64.589223
1646.028623	53.306770	64.594228
1644.773368	60.304418	64.599233
1643.920563	48.039957	64.604238
1643.499359	46.171184	64.609242
1642.935290	56.282912	64.614247
1642.880792	47.593393	64.619252
1641.614706	50.948447	64.624257
1640.947727	55.588816	64.629262
1640.649168	50.928124	64.634266
1639.322048	52.017276	64.639271
1638.751565	45.639905	64.644276
1637.750145	54.275620	64.649281
1637.434022	48.755472	64.654286
1637.075292	53.561372	64.659290
1636.549397	60.698280	64.664295
1635.808770	59.321516	64.669300
1635.103712	60.104492	64.674305
1634.426128	58.017891	64.679310
1633.807388	58.668470	64.684314
1632.501821	65.121335	64.689319
1632.264496	60.562657	64.694324
1631.436444	54.119629	64.699329
1630.950929	52.995250	64.704334
1630.563862	59.901567	64.709338
1628.864644	63.082467	64.714343
1628.571890	53.332056	64.719348
1627.760284	56.747888	64.724353
1627.546610	54.508879	64.729358
1627.238795	52.671227	64.734362
1626.422177	48.779686	64.739367
1626.547377	46.240726	64.744372
1625.335342	57.373166	64.749377
1624.748930	59.839845	64.754382
1623.585685	53.029855	64.759386
1622.420562	64.552149	64.764391
1621.835758	58.495371	64.769396
1621.597634	61.834778	64.774401
1621.122278	56.630812	64.779406
1620.402895	50.555227	64.784410
1620.000909	50.520191	64.789415
1619.268392	48.431548	64.794420
1618.267505	60.216643	64.799425
1617.701366	48.970849	64.804430
1617.275748	55.821002	64.809434
1616.647095	56.183555	64.814439
1615.922642	54.462594	64.819444
1614.908354	57.487605	64.824449
1614.554212	44.819676	64.829454
1614.110974	57.972565	64.834458
1612.619072	57.053565	64.839463
1612.130823	52.227582	64.844468
1611.882842	63.530957	64.849473
1611.480298	41.661718	64.854478
1611.021069	45.477096	64.859482
1609.693281	48.627593	64.864487
1609.369777	49.312911	64.869492
1608.664503	54.960055	64.874497
1607.789628	43.722892	64.879502
1606.769539	55.888227	64.884506
1605.800769	56.304249	64.889511
1605.572017	52.262770	64.894516
1604.838620	57.936042	64.899521
1604.404691	55.584734	64.904526
1604.281726	50.309811	64.909530
1603.866933	59.550507	64.914535
1603.020212	48.255238	64.919540
1602.206835	55.573966	64.924545
1601.449919	44.702654	64.929550
1600.286320	47.904000	64.934554
1599.308035	50.324062	64.939559
1599.223907	52.288751	64.944564
1598.972849	56.603353	64.949569
1598.144313	54.636535	64.954574
1597.386466	51.461619	64.959578
1596.387734	50.423098	64.964583
1596.060824	49.355656	64.969588
1594.840788	51.073833	64.974593
1594.575740	46.233736	64.979598
1594.526337	56.168576	64.984602
1593.305094	46.519834	64.989607
1592.807181	46.616079	64.994612
1592.299575	52.512804	64.999617
1591.222649	51.759627	65.004622
1590.327118	41.363601	65.009626
1589.457852	53.292739	65.014631
1589.547777	45.663990	65.019636
1589.092453	44.250647	65.024641
1588.228939	54.906622	65.029646
1587.152828	46.329576	65.034650
1586.307138	54.211572	65.039655
1586.163233	49.414293	65.044660
1585.271604	52.655148	65.049665
1585.399873	52.232937	65.054670
1584.155951	43.668032	65.059674
1583.384280	52.739676	65.064679
1582.913300	51.215333	65.069684
1581.627495	47.517379	65.074689
1580.874110	49.825538	65.079694
1580.529635	45.256392	65.084698
1579.594293	45.890897	65.089703
1579.341877	39.376612	65.094708
1578.686195	49.094295	65.099713
1578.467914	41.378957	65.104718
1578.324053	40.725829	65.109722
1577.082330	48.049179	65.114727
1576.374480	37.929317	65.119732
1575.534382	51.674696	65.124737
1574.476644	46.860130	65.129742
1573.496990	47.240127	65.134746
1572.957506	56.937930	65.139751
1573.056662	49.491539	65.144756
1572.186435	51.687070	65.149761
1571.728569	41.950721	65.154766
1571.266930	39.870596	65.159770
1570.063145	43.349601	65.164775
1569.728348	36.831654	65.169780
1569.110315	48.978309	65.174785
1568.119583	43.886633	65.179790
1567.445661	39.512022	65.184794
1566.723971	46.136142	65.189799
1566.475861	41.889965	65.194804
1565.497026	41.940233	65.199809
1564.975921	41.156280	65.204814
1563.855957	53.360812	65.209818
1563.457812	50.519459	65.214823
1562.853373	52.463067	65.219828
1562.332642	52.213499	65.224833
1561.759081	44.479625	65.229838
1561.200085	49.196251	65.234842
1559.986035	54.875998	65.239847
1559.626098	40.346791	65.244852
1559.334748	51.379693	65.249857
1558.560116	41.726373	65.254862
1557.320151	50.627118	65.259866
1556.479311	46.662372	65.264871
1556.323254	38.884681	65.269876
1555.766688	46.285769	65.274881
1555.195895	51.695173	65.279886
1554.598784	47.787000	65.284890
1553.381180	48.153252	65.289895
1553.008133	37.713609	65.294900
1552.600436	42.474995	65.299905
1551.834041	41.387248	65.304910
1550.997532	41.865114	65.309914
1550.189174	51.071321	65.314919
1549.898895	43.256997	65.319924
1549.015824	43.812302	65.324929
1548.474327	46.651808	65.329934
1547.427064	44.580334	65.334938
1546.880748	50.931296	65.339943
1546.837678	43.109006	65.344948
1545.760720	51.045978	65.349953
1544.586123	42.762499	65.354958
1544.417726	37.035908	65.359962
1543.610005	43.888295	65.364967
1543.568142	40.338238	65.369972
1542.759001	46.761019	65.374977
1541.924831	46.361816	65.379982
1541.439800	37.104577	65.384986
1540.806059	39.751852	65.389991
1540.085269	46.016230	65.394996
1538.778451	58.554313	65.400001
1538.120954	47.469036	65.405006
1537.859367	37.226232	65.410010
1537.339281	44.245304	65.415015
1537.064464	40.902870	65.420020
1535.629694	41.359580	65.425025
1534.714304	41.288079	65.430030
1533.997089	43.526503	65.435034
1533.904057	49.474246	65.440039
1533.394218	40.358220	65.445044
1532.705571	51.035582	65.450049
1531.780583	44.184848	65.455054
1531.142333	43.837770	65.460058
1530.522987	48.717087	65.465063
1530.139697	41.631943	65.470068
1529.368131	53.003992	65.475073
1528.271047	47.082670	65.480078
1528.113818	51.618044	65.485082
1527.226531	52.135392	65.490087
1526.774944	46.182542	65.495092
1525.564675	51.483506	65.500097
1524.700958	48.111207	65.505102
1524.380335	43.869155	65.510106
1523.863503	55.345235	65.515111
1523.647417	44.039952	65.520116
1523.116098	46.068544	65.525121
1522.281176	51.061728	65.530126
1521.392466	53.737645	65.535130
1520.589865	51.711141	65.540135
1520.122425	43.916089	65.545140
1518.930217	42.392036	65.550145
1518.032085	41.539594	65.555150
1517.906345	45.122252	65.560154
1517.258936	50.165051	65.565159
1517.216094	44.876030	65.570164
1516.521154	48.318484	65.575169
1515.204792	40.897661	65.580174
1514.952630	43.643047	65.585178
1514.360262	42.458025	65.590183
1513.332593	42.431006	65.595188
1512.077605	49.716377	65.600193
1511.396895	42.086112	65.605198
1511.297534	39.245338	65.610202
1510.400989	48.341513	65.615207
1510.147313	50.200621	65.620212
1509.987941	46.982108	65.625217
1509.483274	47.031757	65.630222
1508.800084	43.274503	65.635226
1507.493014	37.365446	65.640231
1506.372874	42.950576	65.645236
1505.555577	38.718536	65.650241
1504.986434	43.114415	65.655246
1504.453164	37.398172	65.660250
1504.048302	41.053467	65.665255
1503.950144	45.804508	65.670260
1503.593214	47.686814	65.675265
1503.172558	51.246529	65.680270
1502.075654	43.592764	65.685274
1500.583634	47.353209	65.690279
1499.767848	45.816444	65.695284
1499.203388	50.453487	65.700289
1498.752054	44.766243	65.705294
1498.527809	41.387133	65.710298
1497.326784	59.038458	65.715303
1496.789100	50.231923	65.720308
1495.813023	58.907525	65.725313
1495.231420	45.815545	65.730318
1494.368770	44.798753	65.735322
1493.932426	48.952836	65.740327
1494.241002	46.519065	65.745332
1493.377880	49.577035	65.750337
1491.975190	39.614402	65.755342
1491.495302	44.016321	65.760346
1490.726482	46.826846	65.765351
1490.673764	39.886831	65.770356
1489.846099	54.336632	65.775361
1489.081815	39.564029	65.780366
1488.191203	46.950058	65.785370
1488.023656	44.638826	65.790375
1487.238739	52.267282	65.795380
1485.975193	51.549225	65.800385
1485.520835	57.406843	65.805390
1485.201179	39.277634	65.810394
1484.316864	49.081421	65.815399
1483.584219	43.610478	65.820404
1482.612936	47.299170	65.825409
1482.175642	47.413471	65.830414
1482.133406	48.124073	65.835418
1481.346302	50.605376	65.840423
1480.540913	51.675137	65.845428
1479.848641	53.766806	65.850433
1479.213027	50.314030	65.855438
1478.043845	45.595534	65.860442
1476.712904	56.271916	65.865447
1477.127952	41.670477	65.870452
1476.640812	56.392377	65.875457
1475.630678	48.828761	65.880462
1475.629183	46.358853	65.885466
1474.378523	56.052460	65.890471
1473.739197	40.326542	65.895476
1472.828374	46.893438	65.900481
1472.443979	46.814747	65.905486
1472.057089	51.222461	65.910490
1471.284150	47.276109	65.915495
1470.275379	46.786412	65.920500
1469.765257	54.195740	65.925505
1468.748789	50.675526	65.930510
1468.895872	43.717892	65.935514
1467.881694	54.419002	65.940519
1467.059992	50.014439	65.945524
1466.450120	58.495925	65.950529
1465.882074	48.442150	65.955534
1465.682739	39.267863	65.960538
1464.344889	49.686489	65.965543
1463.447682	52.760955	65.970548
1462.742901	51.706490	65.975553
1462.885125	57.939215	65.980558
1462.411723	53.031374	65.985562
1461.079231	55.408668	65.990567
1460.633505	49.442193	65.995572
1459.718856	54.312457	66.000577
1459.153632	49.190608	66.005582
1458.783883	46.523214	66.010586
1457.498761	57.101761	66.015591
1457.146910	44.146513	66.020596
1456.475668	46.754429	66.025601
1456.150836	44.508012	66.030606
1455.641616	45.189600	66.035610
1454.397704	56.814598	66.040615
1453.817274	49.049946	66.045620
1453.143153	52.717386	66.050625
1452.746281	49.552948	66.055630
1452.434184	49.679373	66.060634
1451.358085	52.726042	66.065639
1450.755304	48.372035	66.070644
1450.165095	53.574383	66.075649
1449.389623	47.125953	66.080654
1448.558632	49.785290	66.085658
1447.591880	57.102257	66.090663
1446.840324	44.678825	66.095668
1446.363297	58.660081	66.100673
1446.220170	50.076142	66.105678
1446.225117	50.339347	66.110682
1445.076706	56.824552	66.115687
1444.373751	51.043810	66.120692
1443.182276	55.288069	66.125697
1442.244373	53.410258	66.130702
1441.220744	47.008251	66.135706
1440.824106	57.298943	66.140711
1441.135731	56.293924	66.145716
1440.411971	58.653475	66.150721
1440.064632	56.431831	66.155726
1438.971490	47.197774	66.160730
1438.032681	56.710910	66.165735
1437.726191	50.687450	66.170740
1437.260393	53.975039	66.175745
1436.053644	55.815709	66.180750
1435.084441	53.441569	66.185754
1434.475040	57.145300	66.190759
1434.293672	45.994345	66.195764
1433.908062	51.834669	66.200769
1432.463351	46.453247	66.205774
1431.510489	47.151564	66.210778
1430.866259	48.818587	66.215783
1431.023457	50.740786	66.220788
1430.781992	55.773318	66.225793
1429.501192	53.992489	66.230798
1428.899025	47.323750	66.235802
1428.076924	47.971267	66.240807
1427.473698	45.498569	66.245812
1426.983097	45.048078	66.250817
1426.575589	50.314677	66.255822
1425.547093	48.694734	66.260826
1425.053011	58.058333	66.265831
1424.557775	56.127651	66.270836
1423.076688	56.867043	66.275841
1422.057865	57.795721	66.280846
1421.989588	53.073927	66.285850
1421.155985	45.564582	66.290855
1421.144094	50.673864	66.295860
1420.895455	52.327254	66.300865
1420.010190	46.330629	66.305870
1418.922740	43.137958	66.310874
1417.932323	52.783079	66.315879
1417.873901	46.981623	66.320884
1417.442197	52.011586	66.325889
1416.150629	53.675734	66.330894
1415.417877	50.168546	66.335898
1414.760356	54.613112	66.340903
1414.009393	51.264560	66.345908
1413.747793	49.262707	66.350913
1413.029086	52.585298	66.355918
1412.185436	52.858365	66.360922
1411.404084	61.793923	66.365927
1411.381068	52.051060	66.370932
1410.708544	55.540607	66.375937
1409.430467	56.662867	66.380942
1408.931108	51.777240	66.385946
1407.921236	52.020736	66.390951
1407.950346	46.017597	66.395956
1407.498622	46.202660	66.400961
1406.962957	50.036264	66.405966
1405.505502	49.680615	66.410970
1405.097855	60.819074	66.415975
1405.129858	46.280439	66.420980
1403.556627	43.506037	66.425985
1402.863488	51.506402	66.430990
1402.118197	46.551168	66.435994
1401.515390	50.170091	66.440999
1401.054319	45.396329	66.446004
1400.654397	59.203340	66.451009
1399.263839	57.987201	66.456014
1398.857719	54.837376	66.461018
1398.033561	53.775329	66.466023
1397.978536	44.188339	66.471028
1397.485595	50.990807	66.476033
1396.764191	48.467292	66.481038
1396.027758	47.653507	66.486042
1394.838525	46.292784	66.491047
1394.873839	39.396128	66.496052
1393.931750	47.150959	66.501057
1392.864144	51.810977	66.506062
1392.521268	42.418911	66.511066
1391.565473	55.723858	66.516071
1391.459413	44.104910	66.521076
1390.974397	44.010687	66.526081
1389.697985	47.877931	66.531086
1388.788900	37.850585	66.536090
1388.488389	48.484009	66.541095
1388.314544	39.954286	66.546100
1387.424347	40.291770	66.551105
1386.497295	45.691113	66.556110
1385.724879	47.501260	66.561114
1385.287930	52.718429	66.566119
1385.139628	51.779502	66.571124
1383.634127	45.398024	66.576129
1383.292369	45.508216	66.581134
1382.456748	49.652496	66.586138
1381.827105	45.524141	66.591143
1381.969191	48.547819	66.596148
1380.707880	49.152503	66.601153
1380.356674	44.294810	66.606158
1379.801950	42.198668	66.611162
1377.843629	41.126694	66.616167
1377.184746	42.252308	66.621172
1377.117767	48.287553	66.626177
1376.650200	48.515987	66.631182
1376.377420	43.372120	66.636186
1375.814625	42.465856	66.641191
1375.057990	41.790132	66.646196
1374.252530	46.013323	66.651201
1373.332768	52.773200	66.656206
1373.020212	46.033190	66.661210
1371.651602	43.798088	66.666215
1370.974910	36.441892	66.671220
1370.325161	36.425998	66.676225
1369.829468	42.807375	66.681230
1369.911064	39.837744	66.686234
1369.028349	47.940424	66.691239
1368.563821	44.252340	66.696244
1367.579028	51.633977	66.701249
1366.743909	40.640729	66.706254
1366.136466	33.624771	66.711258
1365.064101	46.122336	66.716263
1365.029351	37.347371	66.721268
1364.231566	43.970319	66.726273
1363.706553	46.601764	66.731278
1363.093851	41.356224	66.736282
1361.885370	37.908378	66.741287
1361.268022	37.470511	66.746292
1360.667158	41.013317	66.751297
1360.323177	43.748767	66.756302
1359.121338	48.098624	66.761306
1357.881115	47.856191	66.766311
1358.229045	45.178848	66.771316
1357.514115	39.567143	66.776321
1357.009898	49.897952	66.781326
1356.485473	42.288729	66.786330
1356.073884	42.363116	66.791335
1355.215893	36.529202	66.796340
1354.512482	50.503016	66.801345
1353.350360	36.938505	66.806350
1352.477996	37.386621	66.811354
1351.062168	48.200698	66.816359
1350.981305	43.794471	66.821364
1351.305529	45.079024	66.826369
1350.340732	43.608844	66.831374
1350.287149	40.758269	66.836378
1349.074608	47.504320	66.841383
1348.253856	42.710824	66.846388
1347.294403	50.233776	66.851393
1346.875407	51.596213	66.856398
1346.433050	44.963685	66.861402
1345.719386	50.980555	66.866407
1344.928246	43.363703	66.871412
1344.191238	47.337560	66.876417
1343.328559	51.090179	66.881422
1343.109861	46.315592	66.886426
1342.607793	41.769899	66.891431
1341.611231	35.583939	66.896436
1340.932866	45.699041	66.901441
1340.352835	43.616314	66.906446
1340.076499	36.147384	66.911450
1339.035525	44.884627	66.916455
1338.281037	36.164190	66.921460
1337.797400	37.965565	66.926465
1337.023648	43.472876	66.931470
1336.553445	38.117295	66.936474
1335.385498	47.268625	66.941479
1334.796184	33.922634	66.946484
1334.282801	41.936435	66.951489
1333.976465	42.052803	66.956494
1333.597264	39.889912	66.961498
1332.251525	47.585170	66.966503
1331.190111	40.682451	66.971508
1330.579673	51.092625	66.976513
1330.507794	49.689060	66.981518
1329.932447	45.704571	66.986522
1329.462117	46.000189	66.991527
1328.531269	46.095969	66.996532
1327.749929	51.196049	67.001537
1327.129983	41.759455	67.006542
1326.799077	35.994787	67.011546
1325.442947	43.049616	67.016551
1325.050996	41.049164	67.021556
1324.473557	37.255684	67.026561
1324.086458	38.697920	67.031566
1323.601760	39.883719	67.036570
1322.492921	44.945917	67.041575
1321.693865	47.540596	67.046580
1321.277275	46.072100	67.051585
1320.820762	55.334533	67.056590
1319.706528	44.996547	67.061594
1318.499570	58.596720	67.066599
1318.007903	46.200278	67.071604
1317.589016	48.710143	67.076609
1317.318809	50.482090	67.081614
1317.307662	44.103367	67.086618
1315.864036	50.429531	67.091623
1315.394324	45.380958	67.096628
1314.643229	51.132672	67.101633
1314.086630	39.047732	67.106638
1313.494322	43.797309	67.111642
1312.097413	43.181466	67.116647
1311.889730	46.663680	67.121652
1311.206886	50.801156	67.126657
1310.708318	41.106957	67.131662
1310.538896	41.702364	67.136666
1308.976878	51.938347	67.141671
1308.549400	45.551556	67.146676
1308.234580	41.301430	67.151681
1307.394543	42.085450	67.156686
1306.597711	45.947979	67.161690
1305.742010	48.613539	67.166695
1305.329313	43.562313	67.171700
1304.363079	40.945733	67.176705
1304.027016	49.793615	67.181710
1303.917166	38.937138	67.186714
1302.612911	49.857250	67.191719
1301.736607	44.702238	67.196724
1300.833368	44.928291	67.201729
1300.817731	45.011080	67.206734
1300.430577	41.589614	67.211738
1299.334527	42.049585	67.216743
1298.649660	45.489941	67.221748
1298.323725	42.195752	67.226753
1297.721261	46.576824	67.231758
1296.681882	44.771676	67.236762
1295.477054	41.193755	67.241767
1295.282175	44.140907	67.246772
1295.212404	45.535138	67.251777
1294.263265	49.889510	67.256782
1293.348574	45.863254	67.261786
1292.499023	39.667927	67.266791
1292.167844	48.953504	67.271796
1291.364925	45.763074	67.276801
1291.069761	42.793602	67.281806
1290.439098	42.383285	67.286810
1288.987573	48.374112	67.291815
1288.998636	40.856776	67.296820
1288.178438	44.930534	67.301825
1287.457557	39.112240	67.306830
1287.068573	42.542600	67.311834
1286.016306	47.650775	67.316839
1285.205630	42.257570	67.321844
1284.752499	42.436965	67.326849
1284.175475	47.786662	67.331854
1284.136833	40.963460	67.336858
1282.801132	52.310518	67.341863
1282.273641	49.147539	67.346868
1282.129881	47.987587	67.351873
1280.755759	56.084408	67.356878
1280.211523	49.685635	67.361882
1278.966474	49.903894	67.366887
1278.866286	44.880878	67.371892
1278.640131	44.988654	67.376897
1277.448527	48.921138	67.381902
1276.830065	48.505971	67.386906
1275.610694	46.069305	67.391911
1275.769841	46.306900	67.396916
1275.067301	36.974456	67.401921
1274.613394	43.953390	67.406926
1274.029598	38.336621	67.411930
1272.937531	49.294223	67.416935
1272.531068	40.536719	67.421940
1271.715639	52.479151	67.426945
1270.928260	44.088026	67.431950
1270.032484	44.307675	67.436954
1269.712133	43.942127	67.441959
1269.168947	48.708166	67.446964
1268.537345	46.326003	67.451969
1267.306609	54.539588	67.456974
1266.205566	55.342642	67.461978
1265.824013	60.264557	67.466983
1265.267309	47.680717	67.471988
1265.075517	52.289500	67.476993
1264.756410	50.939708	67.481998
1264.485591	57.125104	67.487002
1263.075994	68.519167	67.492007
1262.546265	48.589740	67.497012
1262.301900	49.501912	67.502017
1260.750468	49.039241	67.507022
1260.274876	50.575575	67.512026
1259.225849	56.210545	67.517031
1258.967752	49.199923	67.522036
1258.873764	56.013435	67.527041
1258.314045	56.216210	67.532046
1257.465394	51.890116	67.537050
1256.613462	57.822909	67.542055
1255.831732	50.388797	67.547060
1254.763051	50.817251	67.552065
1253.682774	50.153928	67.557070
1253.486194	44.171674	67.562074
1253.031923	55.411653	67.567079
1252.777063	43.431377	67.572084
1252.274367	41.948419	67.577089
1251.359751	43.673592	67.582094
1250.642095	39.199557	67.587098
1249.871652	46.137161	67.592103
1249.455802	44.098968	67.597108
1248.436819	40.942379	67.602113
1247.293144	53.021136	67.607118
1246.952172	43.393516	67.612122
1246.601706	54.804793	67.617127
1246.386568	37.959140	67.622132
1246.077469	38.511755	67.627137
1244.612749	50.210098	67.632142
1244.299719	44.344093	67.637146
1242.613376	53.478008	67.642151
1242.073650	48.000531	67.647156
1241.704412	45.308205	67.652161
1240.717682	51.071057	67.657166
1240.670999	39.510650	67.662170
1239.771857	55.760366	67.667175
1239.911990	46.352340	67.672180
1239.049287	45.522304	67.677185
1237.758752	45.608236	67.682190
1237.374921	45.138695	67.687194
1236.763568	53.675699	67.692199
1236.493387	39.197909	67.697204
1235.073864	45.191951	67.702209
1234.465707	50.953936	67.707214
1234.376937	42.057185	67.712218
1233.514083	51.596802	67.717223
1233.072805	40.079873	67.722228
1232.198745	45.115707	67.727233
1231.555649	47.139776	67.732238
1230.882478	46.226375	67.737242
1229.080938	45.641541	67.742247
1228.744519	39.932694	67.747252
1227.941886	43.669125	67.752257
1227.988549	40.854285	67.757262
1227.489841	39.885360	67.762266
1226.859993	44.520191	67.767271
1226.844764	40.889804	67.772276
1225.681071	37.578399	67.777281
1224.535337	47.831939	67.782286
1224.249508	37.496631	67.787290
1223.441823	44.319829	67.792295
1222.607093	39.669273	67.797300
1221.572257	33.645022	67.802305
1220.823356	41.896505	67.807310
1220.801983	34.270657	67.812314
1220.134665	39.951588	67.817319
1219.783882	44.179844	67.822324
1219.253092	44.679630	67.827329
1218.044951	45.407876	67.832334
1217.601392	43.492450	67.837338
1217.031154	49.867650	67.842343
1216.323750	39.096911	67.847348
1215.197855	45.021346	67.852353
1214.058282	46.845036	67.857358
1213.697363	42.177308	67.862362
1213.344904	49.365444	67.867367
1213.162704	35.571645	67.872372
1212.792577	39.858078	67.877377
1212.095253	48.231386	67.882382
1211.062988	38.845675	67.887386
1210.385634	48.336956	67.892391
1209.266151	44.481959	67.897396
1208.476336	39.124672	67.902401
1208.172049	44.942390	67.907406
1207.525202	41.206598	67.912410
1207.306608	48.618514	67.917415
1206.867323	44.581541	67.922420
1205.721356	47.100635	67.927425
1205.216594	47.775957	67.932430
1204.270217	40.310054	67.937434
1203.193301	50.671020	67.942439
1202.298802	45.931626	67.947444
1201.907966	38.410478	67.952449
1201.193780	49.376019	67.957454
1201.091348	40.844751	67.962458
1200.568878	47.810164	67.967463
1200.093189	45.781037	67.972468
1199.295224	42.311501	67.977473
1198.378729	45.451672	67.982478
1197.726363	45.412960	67.987482
1197.281964	49.078985	67.992487
1196.110094	43.930393	67.997492
1195.358193	45.476145	68.002497
1195.030251	48.103466	68.007502
1194.810108	41.518179	68.012506
1193.999201	50.395252	68.017511
1192.935850	36.142084	68.022516
1192.104911	37.773602	68.027521
1191.793781	41.462596	68.032526
1191.448955	35.497444	68.037530
1190.270297	43.029126	68.042535
1189.352555	39.822061	68.047540
1188.921780	38.074969	68.052545
1188.364069	39.673523	68.057550
1188.253697	37.217527	68.062554
1187.048507	40.638825	68.067559
1186.307924	39.401858	68.072564
1185.631905	35.964735	68.077569
1184.990557	46.068372	68.082574
1184.666368	35.983575	68.087578
1183.905499	35.063092	68.092583
1182.991917	36.164051	68.097588
1182.441333	29.451406	68.102593
1181.766480	34.345773	68.107598
1181.685507	25.123639	68.112602
1180.879889	43.087767	68.117607
1179.565695	34.135583	68.122612
1179.320119	43.176376	68.127617
1178.816885	44.511012	68.132622
1177.950890	36.511907	68.137626
1176.690879	38.126499	68.142631
1176.314140	34.040931	68.147636
1175.860941	38.379875	68.152641
1175.041894	34.526738	68.157646
1175.113681	38.005705	68.162650
1173.807812	39.075545	68.167655
1173.361547	32.556609	68.172660
1172.957203	45.274534	68.177665
1171.862055	36.701275	68.182670
1170.975352	33.242598	68.187674
1170.073478	42.458912	68.192679
1169.748631	36.071942	68.197684
1169.277319	37.892930	68.202689
1168.791954	39.965785	68.207694
1168.409152	42.874064	68.212698
1167.091929	38.326657	68.217703
1166.688628	40.013638	68.222708
1166.337853	33.500062	68.227713
1165.240664	38.276883	68.232718
1164.456962	43.780782	68.237722
1163.358242	41.260334	68.242727
1162.936563	40.012188	68.247732
1162.444032	42.207449	68.252737
1161.994920	43.450719	68.257742
1162.190617	40.031708	68.262746
1160.778663	35.918133	68.267751
1159.904990	39.279912	68.272756
1159.418678	43.592556	68.277761
1158.978382	45.857818	68.282766
1158.128582	39.098909	68.287770
1157.506550	42.492205	68.292775
1156.795323	33.555997	68.297780
1156.668421	36.024165	68.302785
1154.838085	41.571483	68.307790
1154.581688	39.046548	68.312794
1154.024358	43.895141	68.317799
1153.562457	42.681907	68.322804
1153.017157	45.065406	68.327809
1151.833302	53.755300	68.332814
1150.959344	51.811735	68.337818
1149.971414	49.495336	68.342823
1149.744693	41.111664	68.347828
1149.621881	39.445655	68.352833
1149.025040	42.114281	68.357838
1148.833106	38.697695	68.362842
1147.390290	48.253332	68.367847
1146.733830	45.305077	68.372852
1146.347828	35.600326	68.377857
1145.764321	44.844629	68.382862
1144.712338	36.044525	68.387866
1143.973128	42.661803	68.392871
1143.427951	36.199672	68.397876
1143.080247	37.031652	68.402881
1142.212008	47.121247	68.407886
1141.984259	33.497490	68.412890
1140.738430	36.691687	68.417895
1139.994603	32.637794	68.422900
1139.686098	38.004280	68.427905
1138.673973	36.976437	68.432910
1137.928700	35.972375	68.437914
1137.509375	45.110807	68.442919
1137.296166	41.828121	68.447924
1136.670614	43.931298	68.452929
1135.669308	42.374656	68.457934
1134.964559	42.654774	68.462938
1134.031536	40.739879	68.467943
1133.580943	36.898265	68.472948
1133.279681	35.780286	68.477953
1131.786089	40.365656	68.482958
1131.485271	32.777006	68.487962
1130.536871	36.738133	68.492967
1129.972721	30.390566	68.497972
1130.003990	32.809942	68.502977
1129.342817	41.733611	68.507982
1128.473245	32.622032	68.512986
1127.598395	35.264053	68.517991
1127.037929	38.581286	68.522996
1126.648610	38.278871	68.528001
1125.578726	36.179002	68.533006
1124.903596	35.243058	68.538010
1124.062856	40.187150	68.543015
1123.751528	34.639803	68.548020
1123.702461	36.395996	68.553025
1122.374216	45.452831	68.558030
1121.502744	32.663606	68.563034
1120.668968	36.146447	68.568039
1120.243499	40.992199	68.573044
1120.358104	36.379635	68.578049
1118.892337	41.358908	68.583054
1118.398333	34.723028	68.588058
1117.478300	38.883369	68.593063
1117.202504	34.118978	68.598068
1117.024725	36.346002	68.603073
1115.708758	33.119909	68.608078
1115.124656	38.175577	68.613082
1114.583032	46.809582	68.618087
1113.743881	40.512258	68.623092
1112.698733	33.608794	68.628097
1111.831990	49.144834	68.633102
1111.335089	34.194342	68.638106
1111.217376	45.875999	68.643111
1110.344216	36.532154	68.648116
1110.401198	49.629355	68.653121
1109.525151	42.370107	68.658126
1108.573953	34.344955	68.663130
1107.682916	42.033049	68.668135
1107.623935	42.376669	68.673140
1106.438842	37.753764	68.678145
1105.361040	46.422343	68.683150
1104.664086	35.513669	68.688154
1104.169473	38.483330	68.693159
1103.837469	31.880107	68.698164
1103.876340	40.341691	68.703169
1103.033243	42.073983	68.708174
1102.265944	36.304728	68.713178
1101.301685	34.950950	68.718183
1100.677987	34.312109	68.723188
1099.563746	39.014102	68.728193
1098.828114	40.688916	68.733198
1098.409390	36.882505	68.738202
1098.131340	44.764046	68.743207
1097.844392	42.113696	68.748212
1096.995049	44.849245	68.753217
1096.136626	45.877224	68.758222
1095.269976	37.658790	68.763226
1094.577945	50.094019	68.768231
1093.822018	35.530498	68.773236
1093.246908	38.065939	68.778241
1092.291344	37.873510	68.783246
1091.931045	27.518222	68.788250
1091.420813	35.592270	68.793255
1090.566575	40.875370	68.798260
1089.802682	48.358154	68.803265
1088.831981	41.958235	68.808270
1088.758394	39.099650	68.813274
1088.259925	38.991971	68.818279
1087.828533	39.792497	68.823284
1086.926977	51.929673	68.828289
1085.815387	48.148353	68.833294
1085.583180	37.241416	68.838298
1085.348242	45.864747	68.843303
1084.267404	38.290856	68.848308
1082.880462	37.611401	68.853313
1082.244738	36.071905	68.858318
1082.551274	32.991924	68.863322
1081.536738	44.239803	68.868327
1080.397137	37.826970	68.873332
1079.490562	35.023393	68.878337
1079.042786	42.105484	68.883342
1079.082513	33.871980	68.888346
1078.539150	43.571622	68.893351
1078.123779	36.649140	68.898356
1077.043294	36.060100	68.903361
1076.430462	41.243052	68.908366
1075.941129	33.025145	68.913370
1074.642346	39.346292	68.918375
1073.885802	42.281468	68.923380
1073.408691	40.695077	68.928385
1072.762178	41.211930	68.933390
1072.467385	34.355641	68.938394
1071.213089	46.145867	68.943399
1070.426781	41.829667	68.948404
1069.802679	47.402953	68.953409
1069.641629	44.333961	68.958414
1069.036858	38.025724	68.963418
1068.738327	47.718180	68.968423
1067.533064	44.837072	68.973428
1067.007417	39.789827	68.978433
1066.213092	52.805045	68.983438
1066.003176	41.760876	68.988442
1064.339794	44.850153	68.993447
1063.589008	52.985137	68.998452
1063.190654	37.896602	69.003457
1062.608440	48.161029	69.008462
1062.830941	45.100567	69.013466
1062.080420	44.986316	69.018471
1061.200411	42.756058	69.023476
1060.575730	43.494163	69.028481
1059.460654	48.786409	69.033486
1059.172195	42.436639	69.038490
1057.538659	44.791766	69.043495
1056.981452	39.590461	69.048500
1056.852697	28.857257	69.053505
1055.981132	45.775231	69.058510
1056.195909	39.581647	69.063514
1055.631905	45.893025	69.068519
1054.575890	42.108119	69.073524
1054.107124	45.235193	69.078529
1053.037311	43.155458	69.083534
1052.348476	44.261373	69.088538
1051.313260	44.116142	69.093543
1050.680334	42.696165	69.098548
1050.233932	35.317577	69.103553
1049.833918	41.077873	69.108558
1049.716654	44.441584	69.113562
1048.186809	40.347048	69.118567
1047.574080	36.054418	69.123572
1047.254366	33.909000	69.128577
1046.420756	42.892988	69.133582
1045.833409	42.044651	69.138586
1045.039475	42.844106	69.143591
1044.189764	42.967885	69.148596
1044.074757	44.407755	69.153601
1043.389762	42.607109	69.158606
1042.518889	37.387681	69.163610
1041.520010	40.071874	69.168615
1041.017244	38.053323	69.173620
1040.504560	35.435713	69.178625
1039.750675	36.331332	69.183630
1039.430004	37.308681	69.188634
1038.354377	40.704665	69.193639
1037.580720	37.495461	69.198644
1037.113273	40.947950	69.203649
1036.781308	41.038726	69.208654
1035.726424	33.170291	69.213658
1034.847940	43.283354	69.218663
1034.224860	38.390555	69.223668
1033.904589	34.346253	69.228673
1033.467640	49.561207	69.233678
1033.006254	38.367486	69.238682
1031.758148	44.977976	69.243687
1031.400815	46.264747	69.248692
1030.974064	36.614360	69.253697
1030.020366	43.759799	69.258702
1029.265269	37.374686	69.263706
1028.597939	45.345385	69.268711
1027.690347	45.804720	69.273716
1027.604110	35.729332	69.278721
1026.359387	42.305692	69.283726
1026.181419	33.191755	69.288730
1025.550938	40.968257	69.293735
1024.777601	38.928151	69.298740
1023.851378	45.817057	69.303745
1022.816515	44.096853	69.308750
1022.457080	34.378103	69.313754
1021.967836	38.694412	69.318759
1021.476600	41.560085	69.323764
1021.390627	39.144917	69.328769
1019.595089	44.016879	69.333774
1018.985794	32.655083	69.338778
1018.278397	41.059330	69.343783
1017.905719	40.062925	69.348788
1017.912224	35.307831	69.353793
1016.804311	36.266053	69.358798
1016.064017	35.849679	69.363802
1015.424574	39.738575	69.368807
1014.831747	36.471569	69.373812
1013.626048	42.891256	69.378817
1012.629682	46.198676	69.383822
1012.110507	35.456941	69.388826
1011.758482	46.197843	69.393831
1011.136693	41.362455	69.398836
1011.256965	41.674984	69.403841
1010.717524	39.253002	69.408846
1010.324967	37.873575	69.413850
1009.194068	43.123145	69.418855
1008.772932	40.187113	69.423860
1007.280586	34.208901	69.428865
1006.372380	51.708652	69.433870
1005.887127	39.372767	69.438874
1005.178204	43.521839	69.443879
1004.817059	42.730292	69.448884
1003.676136	35.673926	69.453889
1002.639753	33.250998	69.458894
1002.831081	30.596118	69.463898
1002.599820	33.484373	69.468903
1001.848364	33.879871	69.473908
1001.263264	41.081395	69.478913
1000.022945	43.633267	69.483918
999.766732	35.848322	69.488922
999.408934	38.057231	69.493927
998.314340	38.578198	69.498932
997.435453	46.193569	69.503937
995.857948	48.177953	69.508942
995.745127	35.519361	69.513946
995.186004	38.828086	69.518951
994.759828	41.402765	69.523956
994.806536	44.674846	69.528961
993.937959	46.037722	69.533966
993.075757	41.774006	69.538970
992.233658	39.916988	69.543975
991.991475	44.393875	69.548980
991.050670	33.442522	69.553985
989.793578	41.784993	69.558990
989.284863	36.878144	69.563994
988.982897	50.279152	69.568999
988.368479	33.672062	69.574004
987.998356	37.837717	69.579009
986.865403	45.523833	69.584014
986.483211	38.666732	69.589018
985.638343	47.492794	69.594023
984.857019	42.754991	69.599028
984.205166	41.253005	69.604033
983.190705	41.862485	69.609038
982.432785	41.462555	69.614042
982.055459	44.077025	69.619047
981.967705	34.041376	69.624052
981.690703	37.420598	69.629057
980.883340	40.431591	69.634062
979.919755	40.731190	69.639066
979.262748	40.782902	69.644071
978.362094	36.663137	69.649076
977.495045	31.562276	69.654081
976.532086	36.013788	69.659086
976.415658	37.216281	69.664090
975.881822	42.967919	69.669095
975.276896	43.776463	69.674100
974.537654	38.398725	69.679105
973.913465	49.314519	69.684110
973.948599	35.969836	69.689114
972.951234	41.686387	69.694119
971.540312	35.432546	69.699124
971.330244	38.964902	69.704129
970.249813	44.778175	69.709134
969.244276	37.138926	69.714138
968.413953	39.753215	69.719143
968.356293	42.511879	69.724148
967.966978	34.025430	69.729153
967.538310	44.902210	69.734158
967.343369	39.129697	69.739162
965.911879	38.740917	69.744167
965.152936	40.324220	69.749172
964.910914	33.339309	69.754177
963.747786	44.046226	69.759182
962.968604	35.481683	69.764186
962.276707	44.606400	69.769191
961.581046	40.516265	69.774196
961.188001	43.340655	69.779201
960.690935	47.800802	69.784206
960.031114	34.508430	69.789210
958.883377	40.947014	69.794215
958.111114	38.437813	69.799220
957.650388	45.021624	69.804225
957.156729	40.147330	69.809230
957.132148	44.567216	69.814234
956.030720	49.872537	69.819239
955.123506	46.771478	69.824244
954.616414	32.227754	69.829249
954.053446	43.727502	69.834254
953.726935	34.740456	69.839258
952.367518	46.978545	69.844263
951.835657	41.954486	69.849268
951.333784	44.156100	69.854273
950.797003	45.304669	69.859278
949.926129	45.074081	69.864282
948.970394	41.619773	69.869287
948.554977	41.102774	69.874292
947.947341	38.747345	69.879297
947.380530	47.648548	69.884302
947.058684	41.273328	69.889306
946.090098	37.507819	69.894311
945.399421	37.877128	69.899316
944.529981	41.310445	69.904321
943.673157	44.637003	69.909326
943.785175	33.634037	69.914330
942.758703	43.609038	69.919335
941.949326	40.918705	69.924340
941.444317	41.309899	69.929345
940.877767	46.706766	69.934350
939.989397	41.496278	69.939354
939.118406	44.421468	69.944359
938.508036	47.061248	69.949364
938.099565	38.311254	69.954369
937.603882	45.845214	69.959374
937.379609	42.296821	69.964378
936.116353	48.467842	69.969383
935.296245	43.241322	69.974388
935.050949	34.355627	69.979393
934.118116	36.013317	69.984398
933.280495	37.934160	69.989402
932.290527	38.097373	69.994407
932.118297	35.410419	69.999412
931.548280	36.039708	70.004417
931.033131	42.984532	70.009422
930.791908	39.126823	70.014426
929.449953	46.180487	70.019431
928.368786	46.161961	70.024436
928.120895	41.141376	70.029441
927.824715	35.703164	70.034446
927.173170	31.230108	70.039450
925.805675	35.640783	70.044455
925.234119	38.069058	70.049460
925.180563	38.333201	70.054465
924.152285	49.995929	70.059470
923.767751	37.309674	70.064474
922.847843	44.188431	70.069479
922.386297	50.057555	70.074484
921.989580	39.493407	70.079489
920.530892	42.057433	70.084494
920.030435	34.356960	70.089498
919.123326	42.159134	70.094503
918.692954	39.771376	70.099508
918.431143	39.841462	70.104513
917.898170	48.570695	70.109518
917.273436	38.951868	70.114522
916.032853	48.415284	70.119527
915.654097	41.009343	70.124532
915.202662	37.784449	70.129537
914.433621	54.507645	70.134542
913.346536	36.866847	70.139546
912.826972	45.266168	70.144551
912.546521	42.598932	70.149556
911.986937	43.856798	70.154561
911.033423	56.182481	70.159566
910.381983	45.041462	70.164570
909.455747	48.409518	70.169575
908.914478	45.438022	70.174580
908.748548	42.013448	70.179585
907.468486	47.386868	70.184590
906.771036	43.754131	70.189594
906.176354	41.224788	70.194599
905.574871	51.579750	70.199604
905.356124	45.516465	70.204609
904.588078	49.363454	70.209614
903.569181	40.471313	70.214618
903.029417	47.320493	70.219623
902.621290	47.992318	70.224628
902.161934	40.237046	70.229633
900.921501	47.779355	70.234638
899.825122	38.872856	70.239642
899.191474	48.972418	70.244647
899.193254	42.599801	70.249652
899.184207	36.935187	70.254657
898.299867	51.369433	70.259662
897.259406	37.773998	70.264666
896.745156	47.770220	70.269671
895.904530	39.374496	70.274676
894.718314	32.690640	70.279681
893.686215	42.034669	70.284686
893.241855	40.568603	70.289690
893.175513	42.834174	70.294695
892.768032	44.655303	70.299700
892.107419	33.347720	70.304705
891.415551	41.067639	70.309710
890.683437	30.969873	70.314714
889.780251	45.689169	70.319719
888.915017	36.233113	70.324724
888.597958	31.379900	70.329729
888.278642	38.959831	70.334734
887.656290	43.114219	70.339738
886.560790	38.471691	70.344743
885.621432	35.990333	70.349748
885.511991	41.664551	70.354753
884.384786	40.168999	70.359758
883.870339	38.043132	70.364762
883.050467	48.116171	70.369767
882.857042	40.831644	70.374772
882.468859	37.353959	70.379777
880.910826	47.901564	70.384782
880.209571	38.117835	70.389786
879.871950	43.192879	70.394791
879.217557	46.197423	70.399796
879.191656	42.087324	70.404801
878.055552	39.808207	70.409806
877.818602	34.010928	70.414810
876.665313	42.330113	70.419815
875.794360	45.661074	70.424820
875.389403	41.301704	70.429825
874.085330	42.852077	70.434830
873.944883	50.525714	70.439834
872.947056	42.729256	70.444839
872.811071	37.526888	70.449844
872.471998	37.741255	70.454849
871.634307	47.044098	70.459854
871.320124	41.499637	70.464858
870.610851	49.314512	70.469863
869.284620	44.409153	70.474868
868.825865	42.392559	70.479873
867.605100	45.833958	70.484878
867.242972	36.971440	70.489882
867.097874	46.308019	70.494887
866.093115	42.956465	70.499892
865.393513	41.943834	70.504897
864.549039	42.337917	70.509902
864.413398	46.282242	70.514906
863.850900	47.996510	70.519911
862.445959	49.676656	70.524916
861.857307	38.233996	70.529921
860.863354	44.709412	70.534926
860.599158	33.070665	70.539930
860.467968	42.023958	70.544935
859.935366	39.906335	70.549940
858.600457	35.958076	70.554945
857.856876	41.346586	70.559950
857.471446	39.010345	70.564954
857.329963	32.418733	70.569959
856.197405	46.302627	70.574964
855.400266	44.332939	70.579969
854.451485	44.225048	70.584974
854.211550	42.999880	70.589978
853.649777	47.205076	70.594983
853.182434	49.087380	70.599988
852.641878	48.591428	70.604993
851.371428	44.593841	70.609998
851.024340	38.906212	70.615002
850.639653	41.904035	70.620007
849.261533	45.672374	70.625012
848.905375	43.514663	70.630017
847.986364	48.164317	70.635022
847.471687	45.097095	70.640026
847.296008	45.587804	70.645031
846.368656	41.482509	70.650036
845.600747	36.733361	70.655041
844.959872	48.334871	70.660046
844.714855	40.020687	70.665050
843.652726	46.050702	70.670055
842.422457	46.449292	70.675060
842.028930	45.889871	70.680065
841.434695	42.206312	70.685070
841.215835	42.951508	70.690074
841.144511	41.448001	70.695079
840.211095	46.417474	70.700084
839.592123	41.758467	70.705089
837.931169	37.738171	70.710094
837.214291	40.213449	70.715098
836.118531	45.929111	70.720103
835.947973	41.735640	70.725108
835.706592	40.083244	70.730113
835.099395	39.172021	70.735118
835.065485	41.010874	70.740122
834.150736	48.403863	70.745127
833.119938	44.472597	70.750132
832.684635	44.640689	70.755137
831.911742	46.002991	70.760142
831.265612	41.177330	70.765146
830.095022	45.908364	70.770151
829.120647	39.963069	70.775156
828.782910	34.496462	70.780161
828.035560	43.851329	70.785166
828.142031	26.023906	70.790170
827.737322	36.983805	70.795175
826.441671	44.402959	70.800180
825.711339	38.206270	70.805185
825.087994	34.215087	70.810190
824.730695	32.249802	70.815194
823.681520	38.061294	70.820199
822.749987	34.361701	70.825204
822.606727	35.654445	70.830209
821.908402	40.446685	70.835214
821.828007	25.100088	70.840218
820.511588	33.958769	70.845223
819.643379	36.521940	70.850228
819.540256	32.682428	70.855233
818.562306	33.771186	70.860238
817.571509	37.517792	70.865242
816.568409	36.257959	70.870247
815.977942	28.360963	70.875252
815.934397	33.058021	70.880257
815.143250	39.820396	70.885262
815.259164	33.904266	70.890266
814.410517	34.141581	70.895271
813.275890	38.855798	70.900276
812.901891	34.311935	70.905281
812.100106	48.040498	70.910286
811.071006	36.902623	70.915290
810.144336	31.647417	70.920295
809.849039	39.973982	70.925300
809.390476	40.471700	70.930305
808.940473	43.931478	70.935310
808.567773	37.914312	70.940314
807.023185	31.635666	70.945319
806.618037	46.308339	70.950324
806.336664	45.373283	70.955329
804.898210	43.563583	70.960334
804.374982	35.860715	70.965338
803.468111	38.151447	70.970343
802.750612	42.903160	70.975348
802.540844	33.726415	70.980353
801.915599	45.851007	70.985358
802.048953	36.184064	70.990362
800.972832	42.396866	70.995367
800.075470	34.004968	71.000372
799.529618	39.847876	71.005377
799.053844	36.696636	71.010382
798.459203	34.809505	71.015386
797.506761	42.958122	71.020391
796.807764	30.494309	71.025396
796.442133	34.319744	71.030401
795.060912	39.635910	71.035406
794.249859	28.591349	71.040410
793.603279	38.250251	71.045415
793.268163	37.603860	71.050420
792.915408	37.779130	71.055425
792.282919	48.862127	71.060430
791.951709	38.037720	71.065434
790.799348	37.015027	71.070439
789.831629	40.216530	71.075444
789.712178	30.896825	71.080449
788.832249	38.089256	71.085454
787.789043	37.668754	71.090458
786.959478	37.911094	71.095463
786.513917	40.516736	71.100468
786.521615	37.408202	71.105473
786.154244	43.177516	71.110478
785.865573	40.316710	71.115482
784.133929	32.664138	71.120487
783.696848	33.936162	71.125492
782.818889	39.155470	71.130497
781.843444	38.441930	71.135502
781.345856	34.467500	71.140506
780.563067	36.519888	71.145511
780.089833	46.248176	71.150516
779.966936	38.540287	71.155521
779.074795	37.038837	71.160526
778.088757	28.033356	71.165530
777.276236	36.545220	71.170535
777.185276	36.999314	71.175540
776.765407	36.109299	71.180545
775.434394	35.081293	71.185550
774.700498	34.201649	71.190554
774.182408	35.017051	71.195559
773.823238	39.016634	71.200564
773.213874	31.653775	71.205569
771.820239	40.043353	71.210574
771.387902	27.175865	71.215578
771.141401	38.239708	71.220583
770.575252	35.955748	71.225588
770.067900	25.909905	71.230593
769.185628	41.383865	71.235598
768.204785	34.402779	71.240602
768.032755	33.102831	71.245607
767.060121	38.066398	71.250612
765.840219	33.449162	71.255617
765.175489	44.782402	71.260622
764.918060	35.336341	71.265626
764.989480	34.531504	71.270631
764.000103	43.894281	71.275636
763.383350	31.289290	71.280641
761.948825	44.561399	71.285646
761.643005	39.510888	71.290650
761.154880	37.372240	71.295655
760.596874	32.932136	71.300660
759.782185	34.634352	71.305665
758.811380	41.800119	71.310670
758.528876	29.420097	71.315674
758.008464	33.987665	71.320679
757.295803	41.738389	71.325684
756.643485	32.866394	71.330689
755.626852	42.014378	71.335694
755.445788	36.725800	71.340698
754.334474	41.589975	71.345703
753.249000	44.231029	71.350708
752.837771	35.160639	71.355713
752.112399	44.267415	71.360718
751.689744	34.737955	71.365722
751.377651	40.827387	71.370727
751.048311	44.337153	71.375732
750.160542	40.050636	71.380737
749.167828	43.012099	71.385742
748.553413	34.422939	71.390746
748.171303	29.425762	71.395751
747.073404	41.217654	71.400756
746.328969	30.263136	71.405761
745.725856	37.859706	71.410766
745.601622	42.670054	71.415770
745.123789	42.695052	71.420775
743.692926	47.504238	71.425780
742.946073	30.020752	71.430785
742.310424	41.654124	71.435790
742.243669	38.274545	71.440794
741.115607	33.332522	71.445799
740.058282	29.314254	71.450804
740.188829	28.740854	71.455809
738.873663	42.237636	71.460814
738.771586	31.417017	71.465818
738.885186	26.280062	71.470823
736.885772	36.113472	71.475828
736.519486	29.777476	71.480833
735.949642	32.615582	71.485838
735.612662	36.967004	71.490842
735.036105	32.128262	71.495847
733.887533	36.055057	71.500852
733.473784	31.595378	71.505857
732.572686	33.564623	71.510862
732.190659	33.802146	71.515866
731.311243	34.774968	71.520871
730.702300	40.666186	71.525876
730.233487	31.589483	71.530881
729.492007	38.541110	71.535886
728.641400	41.561123	71.540890
727.714447	37.788139	71.545895
727.144420	36.844513	71.550900
726.885242	35.923423	71.555905
725.960293	41.511952	71.560910
725.421976	35.312787	71.565914
724.431008	32.380462	71.570919
723.599204	43.857974	71.575924
723.133769	39.423332	71.580929
722.408460	34.462845	71.585934
722.318823	36.572938	71.590938
722.175295	37.026960	71.595943
721.074589	37.871912	71.600948
720.713754	35.307670	71.605953
719.554470	34.055273	71.610958
718.745555	34.287771	71.615962
718.103729	40.371718	71.620967
717.492403	43.508234	71.625972
717.495236	36.267078	71.630977
716.133688	38.351912	71.635982
715.195139	34.395402	71.640986
715.074490	29.624215	71.645991
714.402692	41.898086	71.650996
713.636275	37.361067	71.656001
712.405204	35.264437	71.661006
711.557970	23.005643	71.666010
711.158629	27.271040	71.671015
710.441407	34.977943	71.676020
710.358053	29.025301	71.681025
709.630081	37.666758	71.686030
709.664227	32.916023	71.691034
708.404794	29.128954	71.696039
707.624776	31.566907	71.701044
707.164345	24.921405	71.706049
706.033951	44.998410	71.711054
704.984876	33.620456	71.716058
704.840911	41.109560	71.721063
704.024888	38.784340	71.726068
704.181704	35.758021	71.731073
703.288784	36.496333	71.736078
702.739335	36.816220	71.741082
701.762811	37.838444	71.746087
701.154265	38.134115	71.751092
700.389159	35.958454	71.756097
699.217574	31.914378	71.761102
698.635093	34.220998	71.766106
698.222416	33.247263	71.771111
697.547680	35.596528	71.776116
697.578537	29.072510	71.781121
696.113691	34.650904	71.786126
695.821310	31.843635	71.791130
695.053542	27.946687	71.796135
694.604244	35.758868	71.801140
693.882537	35.807888	71.806145
692.743603	39.363193	71.811150
692.235443	36.509604	71.816154
691.681362	29.668183	71.821159
691.347668	36.725208	71.826164
690.114984	24.444035	71.831169
689.186847	41.743909	71.836174
688.427993	31.136857	71.841178
688.225823	30.435333	71.846183
687.592917	31.933533	71.851188
687.451926	29.953309	71.856193
687.017864	35.852462	71.861198
685.787940	36.158273	71.866202
685.160551	40.726017	71.871207
684.313412	38.572307	71.876212
684.187775	27.481407	71.881217
682.980839	39.535917	71.886222
682.311225	35.658862	71.891226
681.421095	38.686441	71.896231
681.058878	33.434431	71.901236
680.925129	33.995326	71.906241
680.183122	37.953529	71.911246
679.339997	37.310101	71.916250
678.641822	40.952129	71.921255
678.092710	38.465538	71.926260
677.160493	33.660894	71.931265
676.281502	35.044946	71.936270
675.931408	37.327152	71.941274
675.421317	36.347213	71.946279
674.664036	34.380600	71.951284
673.631199	31.482696	71.956289
672.777828	40.381284	71.961294
672.251561	33.374847	71.966298
672.050098	35.891312	71.971303
671.686054	39.626881	71.976308
671.062471	28.695888	71.981313
669.906013	37.638504	71.986318
669.276775	33.194830	71.991322
668.758374	34.545133	71.996327
667.835644	43.336796	72.001332
667.385143	40.453596	72.006337
666.441850	40.297436	72.011342
666.325026	27.128434	72.016346
665.651084	25.402138	72.021351
664.277958	29.230449	72.026356
663.955637	22.186315	72.031361
663.072610	35.010682	72.036366
662.887532	32.008990	72.041370
662.314846	29.944049	72.046375
660.815410	35.314837	72.051380
660.394695	29.852996	72.056385
659.621596	39.410427	72.061390
659.224546	29.848971	72.066394
659.220847	39.580099	72.071399
658.191900	31.728255	72.076404
657.440589	25.892420	72.081409
656.434282	24.748825	72.086414
656.258603	29.221814	72.091418
655.617010	24.440017	72.096423
654.663816	33.351362	72.101428
653.894922	27.171190	72.106433
653.104823	36.162748	72.111438
652.402189	26.620886	72.116442
651.947055	33.388073	72.121447
651.747509	27.649147	72.126452
651.439335	35.779370	72.131457
650.277629	35.906144	72.136462
649.707100	30.473918	72.141466
648.584793	30.163310	72.146471
647.380812	35.693077	72.151476
646.920141	27.076815	72.156481
646.180710	33.858368	72.161486
646.744031	39.076679	72.166490
646.150916	28.818199	72.171495
645.280752	29.840369	72.176500
644.229772	32.104107	72.181505
643.534070	39.280385	72.186510
643.114948	35.405816	72.191514
642.007499	34.108245	72.196519
641.177561	41.005959	72.201524
640.449702	26.753948	72.206529
639.954307	31.633402	72.211534
639.845249	25.132176	72.216538
639.090020	41.426298	72.221543
638.466905	31.408997	72.226548
637.742475	30.545517	72.231553
636.571666	35.035846	72.236558
636.477961	37.104796	72.241562
636.062546	35.113171	72.246567
634.685143	46.089722	72.251572
633.936808	30.110392	72.256577
633.290739	40.832574	72.261582
632.743488	33.005969	72.266586
632.757154	33.063609	72.271591
631.525951	36.036741	72.276596
631.073603	33.279382	72.281601
629.989032	43.565931	72.286606
629.630116	37.571691	72.291610
629.414014	29.226934	72.296615
628.476727	42.299406	72.301620
627.946283	35.071072	72.306625
627.364944	45.805061	72.311630
626.469544	38.265457	72.316634
625.569175	38.342332	72.321639
624.569140	42.919454	72.326644
624.314258	24.786103	72.331649
623.972382	39.768029	72.336654
622.926125	28.877492	72.341658
621.798518	35.890148	72.346663
621.264428	36.627783	72.351668
620.884269	31.021245	72.356673
620.150040	32.496156	72.361678
620.088629	37.082984	72.366682
619.946299	40.428088	72.371687
618.602747	29.798869	72.376692
618.007827	26.114678	72.381697
617.081498	38.828053	72.386702
616.625228	33.228239	72.391706
615.838108	35.705709	72.396711
615.093078	28.099695	72.401716
614.808541	24.541528	72.406721
613.306739	36.435390	72.411726
612.472966	30.059907	72.416730
612.095913	35.767725	72.421735
611.250643	33.078871	72.426740
611.094695	28.135724	72.431745
610.395051	32.319558	72.436750
610.100160	27.663490	72.441754
609.807541	29.210366	72.446759
608.817176	33.414010	72.451764
608.455102	20.538079	72.456769
606.954742	25.909036	72.461774
606.365623	23.941651	72.466778
605.874076	29.000437	72.471783
604.696974	28.397270	72.476788
604.527758	23.797431	72.481793
604.286776	32.143100	72.486798
603.014670	29.644213	72.491802
602.202105	26.165857	72.496807
601.597846	34.948350	72.501812
601.224312	18.565375	72.506817
600.838174	26.984459	72.511822
600.240621	26.738684	72.516826
599.669693	25.450644	72.521831
598.819602	28.388484	72.526836
598.068893	23.709862	72.531841
596.829005	28.474517	72.536846
596.015665	17.535802	72.541850
595.442974	20.788067	72.546855
595.028915	26.128428	72.551860
594.879124	19.110796	72.556865
593.860014	22.074831	72.561870
594.029249	15.032540	72.566874
593.025307	21.860596	72.571879
592.104830	20.842039	72.576884
591.605498	20.076571	72.581889
590.235392	28.311761	72.586894
589.522194	21.657880	72.591898
589.433854	21.983245	72.596903
589.066283	22.478419	72.601908
588.576274	19.815542	72.606913
587.473431	29.572353	72.611918
586.278587	24.055274	72.616922
586.030944	23.647320	72.621927
585.817995	35.357467	72.626932
585.122247	22.217017	72.631937
583.811078	20.538337	72.636942
583.176885	27.039771	72.641946
582.705055	26.106180	72.646951
582.052714	27.166431	72.651956
582.007592	22.440339	72.656961
580.231156	31.594971	72.661966
579.423899	20.313394	72.666970
579.579416	30.098144	72.671975
578.861202	17.610855	72.676980
578.501803	22.149659	72.681985
577.119904	23.015979	72.686990
576.567240	26.629532	72.691994
575.927447	23.736939	72.696999
575.713647	28.558676	72.702004
575.227531	23.748677	72.707009
573.736985	27.933030	72.712014
573.371194	30.119250	72.717018
572.723466	22.314220	72.722023
572.115083	30.506531	72.727028
571.897973	20.905584	72.732033
571.030500	29.892243	72.737038
569.968154	23.288319	72.742042
569.194024	23.671978	72.747047
568.768116	27.132768	72.752052
568.604484	21.758336	72.757057
567.543632	23.116332	72.762062
566.801773	26.362455	72.767066
566.445398	24.186260	72.772071
565.598501	25.417603	72.777076
565.778717	13.668835	72.782081
564.428468	31.167725	72.787086
563.643273	16.054831	72.792090
563.356009	21.815941	72.797095
561.715848	28.364218	72.802100
561.308766	23.010973	72.807105
560.299777	25.796449	72.812110
560.205092	22.259440	72.817114
559.677983	33.910918	72.822119
559.025574	29.258484	72.827124
558.533447	24.708845	72.832129
557.596863	31.092761	72.837134
556.955083	24.646505	72.842138
556.597552	27.627449	72.847143
555.975464	29.754169	72.852148
554.965963	21.630624	72.857153
554.225067	22.533167	72.862158
553.900748	28.384702	72.867162
553.361739	26.280456	72.872167
552.323702	26.549476	72.877172
551.200889	30.591491	72.882177
550.548027	26.512657	72.887182
550.342901	30.929905	72.892186
549.762092	32.404984	72.897191
549.367576	30.550307	72.902196
548.375383	27.912693	72.907201
547.442790	26.723730	72.912206
546.973713	35.660290	72.917210
546.650700	25.575412	72.922215
545.722045	36.268252	72.927220
544.840669	19.999539	72.932225
544.169138	31.548662	72.937230
543.434946	28.628435	72.942234
543.323729	31.035497	72.947239
542.616462	40.345221	72.952244
542.260314	22.154643	72.957249
541.325993	32.628991	72.962254
540.406878	28.587883	72.967258
540.094007	27.736397	72.972263
538.640989	24.991439	72.977268
538.138244	24.244719	72.982273
537.508697	30.701943	72.987278
536.990229	29.844633	72.992282
537.013587	32.235742	72.997287
536.405822	35.257985	73.002292
535.217431	19.282262	73.007297
534.176862	29.975328	73.012302
534.169814	28.631334	73.017306
533.732367	24.721635	73.022311
532.280853	27.809110	73.027316
531.548842	22.624038	73.032321
530.657400	34.246368	73.037326
530.438483	27.462413	73.042330
529.849869	22.227510	73.047335
529.538022	28.526883	73.052340
528.860781	20.218134	73.057345
528.108926	27.770330	73.062350
527.458275	26.254395	73.067354
526.932216	19.271638	73.072359
525.583395	27.340571	73.077364
524.900316	20.189336	73.082369
524.462479	28.149543	73.087374
524.006849	27.566846	73.092378
523.760576	21.601088	73.097383
522.742366	33.378947	73.102388
521.792110	19.638743	73.107393
521.377466	25.081042	73.112398
520.890723	25.224424	73.117402
520.215620	20.635885	73.122407
519.000772	29.490634	73.127412
518.719662	23.948846	73.132417
518.129120	29.565357	73.137422
517.647052	22.959120	73.142426
516.782305	16.730280	73.147431
515.605998	23.772212	73.152436
514.936653	18.040781	73.157441
514.548370	23.566584	73.162446
514.098280	24.106690	73.167450
514.001368	22.858617	73.172455
512.595912	29.660359	73.177460
512.147659	18.588851	73.182465
511.418350	29.035175	73.187470
510.833262	19.677674	73.192474
509.762058	24.314369	73.197479
508.990696	30.059358	73.202484
508.742860	18.943643	73.207489
508.197010	25.486387	73.212494
507.928827	32.349825	73.217498
507.106369	27.337351	73.222503
506.132928	31.665604	73.227508
505.442200	19.513868	73.232513
504.950039	34.517976	73.237518
504.077387	36.988409	73.242522
503.192856	28.228104	73.247527
502.496582	25.139160	73.252532
502.307786	27.385840	73.257537
501.748818	27.169385	73.262542
500.829032	28.152323	73.267546
500.174330	27.787676	73.272551
499.050377	32.292107	73.277556
498.821573	27.698934	73.282561
498.484767	32.704765	73.287566
497.876224	28.914382	73.292570
497.382826	14.180961	73.297575
496.189364	28.617246	73.302580
496.027068	23.652305	73.307585
494.628357	27.678056	73.312590
493.313782	30.410124	73.317594
493.032649	15.969917	73.322599
492.621259	31.843551	73.327604
492.129856	17.162284	73.332609
491.862045	33.457738	73.337614
491.560559	21.428375	73.342618
490.605950	21.126173	73.347623
489.683033	24.531217	73.352628
488.960600	18.112218	73.357633
488.516721	26.367126	73.362638
487.327267	23.577023	73.367642
486.726596	23.015631	73.372647
486.340603	26.610894	73.377652
485.992109	26.875056	73.382657
485.039262	22.823560	73.387662
483.783088	29.290273	73.392666
483.228379	19.176432	73.397671
482.624300	37.290722	73.402676
482.478734	16.472392	73.407681
482.058877	24.170189	73.412686
481.449668	27.898826	73.417690
480.521448	23.030002	73.422695
479.272167	27.131987	73.427700
478.676412	22.857471	73.432705
478.607890	25.200377	73.437710
477.982135	20.127760	73.442714
476.950055	18.788107	73.447719
476.098590	23.575433	73.452724
476.197564	17.545785	73.457729
475.383817	24.293112	73.462734
474.584305	26.661809	73.467738
474.134663	16.238275	73.472743
473.155094	25.951870	73.477748
472.359077	19.346547	73.482753
471.340962	23.879421	73.487758
470.453848	26.672053	73.492762
470.677020	19.559343	73.497767
469.562517	23.680864	73.502772
469.599916	21.325894	73.507777
468.720802	26.463333	73.512782
467.616757	26.321734	73.517786
467.157285	18.292245	73.522791
466.300642	23.930673	73.527796
466.294088	20.557373	73.532801
465.150583	23.054487	73.537806
463.811377	12.771155	73.542810
463.538599	10.959177	73.547815
463.218019	17.659097	73.552820
463.171815	18.476162	73.557825
462.015045	27.129135	73.562830
461.183129	22.319598	73.567834
461.010720	17.469677	73.572839
460.310263	25.146483	73.577844
459.170952	21.026690	73.582849
458.520995	19.969699	73.587854
458.106590	27.038968	73.592858
457.146822	20.535126	73.597863
456.082446	24.312948	73.602868
455.494225	22.875136	73.607873
454.663604	17.915784	73.612878
454.103621	28.459402	73.617882
454.004800	16.665700	73.622887
453.539891	15.804355	73.627892
453.317709	18.773950	73.632897
452.017632	20.641488	73.637902
451.218182	21.310936	73.642906
450.593625	14.410597	73.647911
450.159152	27.506633	73.652916
449.711766	18.418033	73.657921
448.707554	27.134860	73.662926
448.002886	27.456112	73.667930
447.818505	22.297998	73.672935
446.575613	28.149846	73.677940
445.541692	25.544274	73.682945
445.067099	22.850749	73.687950
444.632540	25.981074	73.692954
443.997494	26.659848	73.697959
443.646358	33.783012	73.702964
442.933476	30.362601	73.707969
441.783671	35.086592	73.712974
441.206725	32.855843	73.717978
441.462388	26.720005	73.722983
440.083986	28.891083	73.727988
439.621469	23.658270	73.732993
438.590859	41.627772	73.737998
438.122799	29.065281	73.743002
437.436825	26.014844	73.748007
436.273579	32.531955	73.753012
435.799289	23.315735	73.758017
435.146788	31.864540	73.763022
434.947371	31.525298	73.768026
434.507479	31.052407	73.773031
433.492473	31.686169	73.778036
432.947011	29.963549	73.783041
431.838844	37.853117	73.788046
431.450485	22.252282	73.793050
431.346221	27.397068	73.798055
429.748233	30.667953	73.803060
429.217942	23.959080	73.808065
428.561991	32.632021	73.813070
428.348226	27.070809	73.818074
428.041944	20.710764	73.823079
426.935015	34.799489	73.828084
426.064589	26.613466	73.833089
425.408388	35.683929	73.838094
424.913285	34.926044	73.843098
424.418991	30.698092	73.848103
423.659313	33.272327	73.853108
422.897521	25.728835	73.858113
421.995510	38.455815	73.863118
421.334596	38.633792	73.868122
421.535688	30.203755	73.873127
419.862256	36.172020	73.878132
419.433281	34.948882	73.883137
418.637285	35.908253	73.888142
418.062107	42.833776	73.893146
418.170470	32.484346	73.898151
417.189695	43.370068	73.903156
416.574599	29.705475	73.908161
416.058492	39.617145	73.913166
414.908778	33.392161	73.918170
413.885880	35.879277	73.923175
413.208635	34.358048	73.928180
412.657994	33.031031	73.933185
412.089492	38.380106	73.938190
411.631243	36.427423	73.943194
411.571100	27.077475	73.948199
410.757724	31.625403	73.953204
410.133630	24.082790	73.958209
409.683902	25.603312	73.963214
408.279220	35.539761	73.968218
407.509498	26.947693	73.973223
406.611837	38.018894	73.978228
406.480800	27.880221	73.983233
406.235267	27.306925	73.988238
405.051692	39.250497	73.993242
404.470018	26.545653	73.998247
403.799033	37.749710	74.003252
403.364853	29.863515	74.008257
401.821114	32.877626	74.013262
400.930185	25.604545	74.018266
400.748786	26.922382	74.023271
399.987797	26.660433	74.028276
399.984124	26.795250	74.033281
399.269000	31.214244	74.038286
398.944646	31.606110	74.043290
398.233595	34.194909	74.048295
396.832134	38.585479	74.053300
396.475649	33.728818	74.058305
396.094596	37.521386	74.063310
395.123721	33.913499	74.068314
394.140705	26.876056	74.073319
393.238728	26.770893	74.078324
393.088493	17.161278	74.083329
392.209300	24.761356	74.088334
392.163910	25.818663	74.093338
391.864415	16.657365	74.098343
390.781544	30.112003	74.103348
390.137537	22.670302	74.108353
389.427109	24.209056	74.113358
388.189772	21.787561	74.118362
387.508015	23.559414	74.123367
386.921654	24.627328	74.128372
386.832747	22.273480	74.133377
385.991933	22.335853	74.138382
385.451501	23.649697	74.143386
384.701201	26.236539	74.148391
383.387086	33.126072	74.153396
383.383964	14.768870	74.158401
382.919606	19.455921	74.163406
381.852174	18.751916	74.168410
380.943241	20.612831	74.173415
380.344676	30.092205	74.178420
379.692360	22.617590	74.183425
379.318267	20.093156	74.188430
379.311356	22.887316	74.193434
378.512886	19.843146	74.198439
377.191570	26.478137	74.203444
376.850182	19.192593	74.208449
376.048248	20.612828	74.213454
375.061529	27.053513	74.218458
374.364662	23.546693	74.223463
373.834784	24.975565	74.228468
373.809018	25.358890	74.233473
373.344371	24.262259	74.238478
372.462051	25.834816	74.243482
371.591989	20.879873	74.248487
370.409546	26.004181	74.253492
369.476475	15.731804	74.258497
368.700313	16.355829	74.263502
368.432247	20.790175	74.268506
368.116831	15.269682	74.273511
367.180450	26.725649	74.278516
366.991682	29.790962	74.283521
366.831665	27.655341	74.288526
365.614149	28.186463	74.293530
364.980786	17.116320	74.298535
363.911248	26.670092	74.303540
363.859014	19.809440	74.308545
362.457404	23.237335	74.313550
361.787139	22.514608	74.318554
361.519429	23.538177	74.323559
360.928318	32.094621	74.328564
360.425437	25.903663	74.333569
359.572979	23.737906	74.338574
358.838150	20.865585	74.343578
358.207389	20.978011	74.348583
357.699038	26.136787	74.353588
357.175362	22.738834	74.358593
356.095642	27.247551	74.363598
355.400631	27.623210	74.368602
355.091633	22.525933	74.373607
354.115652	24.430710	74.378612
353.457559	18.797246	74.383617
352.441028	24.217578	74.388622
352.019463	31.758181	74.393626
351.437866	23.700696	74.398631
351.142639	35.784508	74.403636
350.770942	34.698395	74.408641
349.742900	29.336739	74.413646
348.798816	29.179199	74.418650
348.723762	25.445429	74.423655
347.163430	30.575695	74.428660
346.566134	21.132301	74.433665
346.048287	28.211406	74.438670
345.595351	25.050000	74.443674
345.851825	24.218182	74.448679
344.136613	29.423542	74.453684
343.191716	28.296727	74.458689
342.789618	24.992406	74.463694
342.310864	20.520241	74.468698
342.215444	18.759976	74.473703
341.301665	26.992004	74.478708
340.229897	19.439690	74.483713
339.556529	23.066446	74.488718
338.710274	29.149137	74.493722
338.739408	31.091644	74.498727
337.503630	22.357247	74.503732
336.569314	30.448331	74.508737
336.051346	32.779849	74.513742
335.481879	27.767869	74.518746
334.697539	25.122707	74.523751
334.640774	33.326273	74.528756
334.495650	25.521204	74.533761
333.467821	25.919567	74.538766
332.388704	31.179324	74.543770
331.892399	20.605929	74.548775
330.528135	27.852598	74.553780
329.874257	27.681639	74.558785
329.441710	31.082399	74.563790
329.187896	28.455255	74.568794
329.014061	20.670897	74.573799
328.468635	31.261757	74.578804
327.444544	30.061286	74.583809
326.584191	27.745714	74.588814
325.899417	26.909038	74.593818
324.863357	14.019617	74.598823
323.884598	24.721053	74.603828
323.469780	27.919050	74.608833
323.394257	25.234509	74.613838
322.909702	19.683012	74.618842
322.441078	22.892598	74.623847
321.289538	33.685229	74.628852
320.649976	31.612457	74.633857
319.898926	33.186603	74.638862
318.658124	32.587322	74.643866
318.182904	22.218724	74.648871
317.681983	28.008560	74.653876
317.093446	19.568218	74.658881
316.587349	24.219008	74.663886
316.137967	26.380492	74.668890
316.073096	21.679905	74.673895
314.424538	25.339995	74.678900
313.809967	21.221092	74.683905
313.425493	23.889314	74.688910
312.045531	24.009765	74.693914
311.153382	12.059575	74.698919
310.746617	19.789467	74.703924
311.037841	17.092989	74.708929
310.354041	27.709535	74.713934
309.589498	31.664142	74.718938
308.985055	30.036116	74.723943
307.721101	36.553933	74.728948
307.315552	34.750905	74.733953
306.794216	26.111555	74.738958
305.889708	23.783031	74.743962
305.002447	28.702823	74.748967
303.891400	33.350728	74.753972
303.389311	29.098079	74.758977
303.422640	30.289517	74.763982
302.708765	37.422356	74.768986
302.640829	23.095635	74.773991
302.103769	29.798322	74.778996
301.135883	22.932776	74.784001
300.461586	32.687224	74.789006
299.163373	24.300231	74.794010
298.435073	22.188598	74.799015
297.820463	38.431373	74.804020
296.969310	27.050431	74.809025
297.133428	31.592275	74.814030
296.157499	32.303048	74.819034
295.543384	21.655910	74.824039
294.553431	32.398350	74.829044
294.302449	30.371870	74.834049
293.682787	33.273420	74.839054
292.663905	42.779057	74.844058
291.892201	24.648718	74.849063
290.901611	38.793697	74.854068
290.929488	28.028234	74.859073
290.494224	27.990327	74.864078
289.660181	33.094806	74.869082
288.458747	32.212092	74.874087
287.723595	24.185675	74.879092
287.456711	31.989487	74.884097
287.162378	28.760643	74.889102
286.623882	28.403740	74.894106
285.765382	22.622674	74.899111
284.509116	36.355715	74.904116
284.196087	28.091563	74.909121
283.914768	24.725892	74.914126
282.735029	29.695423	74.919130
282.139626	30.876603	74.924135
281.314613	27.973570	74.929140
281.116268	30.607920	74.934145
280.566586	29.420485	74.939150
279.055747	34.758196	74.944154
278.421609	17.002559	74.949159
277.685545	27.748451	74.954164
277.362704	18.809054	74.959169
277.254515	20.087900	74.964174
276.510615	26.190550	74.969178
276.234339	19.853803	74.974183
274.900051	23.888697	74.979188
274.398296	29.523951	74.984193
274.050475	25.715759	74.989198
272.783039	27.944042	74.994202
271.760350	23.991407	74.999207
271.119785	27.884901	75.004212
271.099676	14.264427	75.009217
270.840553	17.885711	75.014222
269.784944	30.783879	75.019226
269.197213	14.952808	75.024231
268.335159	14.847142	75.029236
268.205989	19.050064	75.034241
267.678429	22.905637	75.039246
266.073715	20.980145	75.044250
265.936448	14.352749	75.049255
265.143680	26.555377	75.054260
264.069149	14.276877	75.059265
263.385656	18.286668	75.064270
262.541414	13.534947	75.069274
262.388392	20.997546	75.074279
261.741237	21.292784	75.079284
261.225095	14.616256	75.084289
260.423056	9.457064	75.089294
259.249885	18.831646	75.094298
259.026415	13.534209	75.099303
258.275307	19.767560	75.104308
258.169132	22.504919	75.109313
257.468282	16.276867	75.114318
256.341253	22.336246	75.119322
256.167458	22.784415	75.124327
255.756775	23.970250	75.129332
254.564174	21.125888	75.134337
253.816295	20.730672	75.139342
252.880649	25.254972	75.144346
252.805568	15.050689	75.149351
251.734141	25.451851	75.154356
251.221745	21.325709	75.159361
250.430290	20.088936	75.164366
249.578994	14.411246	75.169370
249.419855	14.638232	75.174375
248.245723	11.785972	75.179380
247.391439	18.028324	75.184385
246.744153	24.380452	75.189390
246.384125	22.792248	75.194394
246.050445	15.127665	75.199399
245.697650	25.678003	75.204404
244.806151	19.197253	75.209409
243.974005	18.388614	75.214414
242.885485	26.700731	75.219418
242.715678	13.749303	75.224423
242.035500	17.353948	75.229428
241.516320	14.889132	75.234433
240.375925	12.325547	75.239438
239.661805	21.018723	75.244442
239.314477	16.410371	75.249447
238.766011	21.278809	75.254452
238.151925	18.114647	75.259457
237.172869	12.034544	75.264462
236.470114	16.038561	75.269466
236.177930	16.902131	75.274471
235.581521	20.168359	75.279476
234.564163	15.045684	75.284481
233.571806	9.742683	75.289486
233.209189	19.495803	75.294490
232.718271	12.419850	75.299495
232.455923	18.125769	75.304500
231.859307	21.564523	75.309505
231.122243	22.413170	75.314510
230.017132	25.833697	75.319514
229.134483	12.480675	75.324519
228.071086	19.273578	75.329524
227.207615	17.774038	75.334529
227.034654	19.728288	75.339534
226.903205	23.099546	75.344538
226.526108	19.047711	75.349543
225.460879	14.367822	75.354548
224.988065	18.706615	75.359553
224.176558	17.561304	75.364558
223.276571	27.796909	75.369562
222.776122	18.686661	75.374567
222.522516	29.452090	75.379572
221.359684	18.573785	75.384577
220.641598	17.999005	75.389582
220.078304	23.773089	75.394586
219.383504	12.940871	75.399591
218.821335	23.913125	75.404596
218.116299	17.692903	75.409601
217.231427	21.753007	75.414606
216.677371	18.998533	75.419610
216.401610	21.170129	75.424615
215.855264	17.322164	75.429620
214.791901	24.988565	75.434625
214.169795	16.944766	75.439630
213.360782	21.559859	75.444634
213.099268	19.311391	75.449639
211.874918	25.565081	75.454644
211.239084	25.508276	75.459649
210.621869	23.703649	75.464654
210.292208	22.723232	75.469658
210.189906	24.286842	75.474663
209.218532	27.170928	75.479668
208.520295	18.726521	75.484673
207.925350	17.832627	75.489678
207.227742	21.914314	75.494682
206.380186	14.579386	75.499687
205.657550	24.679201	75.504692
204.748269	19.313021	75.509697
204.194531	17.420546	75.514702
203.543253	19.640328	75.519706
202.799452	20.454215	75.524711
201.649395	24.095201	75.529716
201.226369	19.641925	75.534721
201.274156	22.951277	75.539726
200.549691	32.006607	75.544730
200.224579	14.059878	75.549735
198.788602	17.666590	75.554740
198.489415	21.378422	75.559745
198.072455	25.705670	75.564750
196.504555	24.614236	75.569754
196.177909	21.510934	75.574759
195.297733	32.414160	75.579764
195.068755	19.554189	75.584769
194.427490	23.168747	75.589774
194.419335	17.271548	75.594778
193.538276	16.857332	75.599783
192.724874	16.081803	75.604788
191.637989	20.154434	75.609793
190.677583	26.140267	75.614798
189.745195	24.476901	75.619802
189.136994	19.232393	75.624807
188.616130	21.963472	75.629812
188.493843	22.718190	75.634817
188.304249	18.024388	75.639822
187.598280	22.064881	75.644826
186.550800	15.386689	75.649831
185.526298	33.067789	75.654836
185.009590	23.585751	75.659841
184.763997	23.574548	75.664846
183.678389	19.855340	75.669850
183.399094	19.121671	75.674855
182.400602	24.679455	75.679860
182.049917	21.643824	75.684865
181.487583	17.332845	75.689870
180.458662	25.078999	75.694874
179.604910	11.297119	75.699879
178.796099	17.611416	75.704884
178.466046	20.202426	75.709889
178.152800	11.278772	75.714894
177.068601	20.078808	75.719898
176.342491	17.507772	75.724903
175.641433	26.525537	75.729908
174.807007	23.740582	75.734913
174.889438	16.072964	75.739918
174.077649	24.368046	75.744922
173.232000	21.604751	75.749927
172.178581	27.743102	75.754932
171.854545	28.612530	75.759937
171.385795	19.797234	75.764942
170.861131	23.395755	75.769946
169.825807	18.974422	75.774951
169.053131	19.827998	75.779956
168.737484	20.819533	75.784961
168.275365	28.424716	75.789966
167.064306	22.071392	75.794970
166.495247	23.373587	75.799975
165.478472	34.655868	75.804980
165.532194	23.987038	75.809985
164.874200	28.745187	75.814990
164.337205	24.121595	75.819994
163.465134	24.269098	75.824999
162.359762	25.206548	75.830004
161.997714	25.662124	75.835009
161.454425	22.894365	75.840014
160.620651	20.667425	75.845018
159.877347	22.128166	75.850023
159.077156	22.255059	75.855028
158.754427	19.897491	75.860033
158.417091	24.762899	75.865038
157.624590	21.584337	75.870042
156.525493	17.879686	75.875047
155.531964	28.816157	75.880052
155.177432	22.553625	75.885057
155.015995	18.056303	75.890062
154.552551	24.838342	75.895066
153.903934	21.703006	75.900071
152.835465	31.584235	75.905076
152.340348	25.125553	75.910081
151.084766	28.529261	75.915086
150.459767	35.475964	75.920090
150.299395	20.075317	75.925095
149.931311	24.262354	75.930100
148.889283	22.012698	75.935105
147.773356	25.939143	75.940110
146.987244	23.572990	75.945114
146.704132	26.789074	75.950119
145.954373	31.388099	75.955124
145.967909	20.042126	75.960129
145.624024	29.097739	75.965134
144.193163	27.236430	75.970138
143.379348	19.580751	75.975143
142.795321	27.009081	75.980148
142.104636	24.843267	75.985153
141.034351	23.638919	75.990158
140.360306	26.727426	75.995162
140.168343	20.254276	76.000167
139.600267	31.261887	76.005172
139.296468	23.359708	76.010177
138.723295	20.454585	76.015182
137.486577	28.285707	76.020186
136.963861	25.238916	76.025191
136.220339	26.062239	76.030196
135.268129	23.296693	76.035201
134.715363	19.146703	76.040206
133.800637	36.540190	76.045210
133.373921	25.107460	76.050215
132.949008	26.971491	76.055220
132.858538	23.338264	76.060225
132.218267	29.801299	76.065230
131.182301	27.343778	76.070234
130.408580	20.744189	76.075239
129.920654	26.088148	76.080244
128.814579	28.254465	76.085249
127.985128	27.408677	76.090254
127.309696	21.936115	76.095258
127.107923	25.540467	76.100263
126.582630	23.561026	76.105268
125.913425	25.652057	76.110273
124.990499	27.651197	76.115278
123.729903	38.949231	76.120282
123.897626	19.986113	76.125287
123.519054	30.371142	76.130292
122.055512	32.624793	76.135297
121.400165	25.125098	76.140302
120.939484	36.350340	76.145306
120.632734	23.673043	76.150311
120.188888	34.557129	76.155316
119.083839	28.050259	76.160321
118.139556	20.310380	76.165326
117.556981	31.435338	76.170330
117.511801	25.068071	76.175335
117.142040	27.252627	76.180340
115.786224	30.326970	76.185345
114.886501	29.145490	76.190350
114.225716	31.209423	76.195354
113.844261	18.427710	76.200359
112.611077	30.626510	76.205364
111.997579	23.243189	76.210369
111.429853	17.188913	76.215374
110.966663	25.203595	76.220378
110.651789	12.843472	76.225383
110.265827	21.006350	76.230388
109.645096	26.035204	76.235393
108.810573	14.744235	76.240398
107.908267	24.582770	76.245402
107.234353	20.454737	76.250407
106.039190	24.800932	76.255412
105.565435	19.996389	76.260417
105.144681	24.477833	76.265422
104.635050	26.274290	76.270426
104.591873	15.114484	76.275431
103.337066	23.154356	76.280436
102.393091	19.084069	76.285441
102.119485	20.987290	76.290446
101.402263	25.779281	76.295450
100.539807	19.208332	76.300455
99.242585	22.325919	76.305460
98.780447	22.222774	76.310465
98.505254	27.501056	76.315470
97.927394	41.358200	76.320474
97.929122	29.311267	76.325479
96.743211	34.158744	76.330484
95.933171	27.692484	76.335489
95.510143	29.725922	76.340494
94.711294	32.113507	76.345498
94.138538	26.075487	76.350503
92.854493	39.748978	76.355508
92.367267	36.980300	76.360513
91.599891	30.165299	76.365518
91.076665	34.992716	76.370522
90.975112	32.000429	76.375527
90.537715	28.099070	76.380532
89.443798	26.807212	76.385537
88.841279	35.442985	76.390542
88.257189	33.788214	76.395546
87.395899	20.743788	76.400551
86.051460	23.278195	76.405556
85.815904	32.308526	76.410561
85.439489	31.055888	76.415566
84.847021	37.946496	76.420570
84.586477	30.036117	76.425575
83.579748	40.278594	76.430580
82.784367	33.970470	76.435585
82.623920	24.231599	76.440590
81.561632	33.580891	76.445594
80.679629	29.056720	76.450599
79.832019	33.961063	76.455604
79.323038	29.597928	76.460609
79.372313	28.035088	76.465614
77.894677	26.889145	76.470618
77.638124	21.600159	76.475623
76.643111	31.298683	76.480628
76.081613	26.080528	76.485633
75.472207	20.384697	76.490638
73.992896	29.197231	76.495642
73.822027	21.962230	76.500647
73.055405	34.962048	76.505652
72.621856	29.143703	76.510657
72.409420	32.013352	76.515662
72.374797	43.158054	76.520666
71.317371	32.738142	76.525671
70.060545	31.542503	76.530676
69.268447	28.046146	76.535681
69.451895	30.369137	76.540686
68.020637	29.903623	76.545690
67.226356	18.352361	76.550695
66.460277	31.853762	76.555700
66.088778	29.465881	76.560705
65.868480	25.192984	76.565710
65.259200	36.665529	76.570714
64.026308	24.268201	76.575719
63.330962	37.811952	76.580724
62.708752	32.517763	76.585729
62.493059	29.925945	76.590734
61.782928	32.873815	76.595738
61.088460	27.315718	76.600743
59.848947	35.570469	76.605748
59.598493	32.778965	76.610753
59.154753	25.790075	76.615758
58.526509	35.269812	76.620762
57.965118	29.337606	76.625767
56.826767	36.240887	76.630772
56.294408	35.518640	76.635777
55.678680	25.088140	76.640782
54.666684	36.675120	76.645786
54.101372	24.687126	76.650791
53.558760	35.025679	76.655796
52.827687	26.180777	76.660801
52.513229	35.144115	76.665806
52.171030	31.506684	76.670810
51.723169	34.155001	76.675815
50.874056	44.114689	76.680820
49.742453	36.376544	76.685825
48.597051	32.095684	76.690830
47.684987	34.441507	76.695834
47.776279	26.400161	76.700839
46.983855	33.004939	76.705844
46.446239	30.679880	76.710849
46.187643	32.563558	76.715854
45.080573	27.915361	76.720858
44.322212	27.465928	76.725863
43.726787	32.799510	76.730868
43.214857	34.188235	76.735873
42.780519	25.675726	76.740878
41.545690	39.368020	76.745882
41.077453	30.796194	76.750887
40.078767	40.928357	76.755892
40.016634	28.719102	76.760897
39.562891	42.090784	76.765902
38.605707	40.138824	76.770906
38.038437	33.282028	76.775911
37.491105	37.870834	76.780916
36.638758	30.728200	76.785921
35.576150	27.532028	76.790926
34.803329	35.277717	76.795930
34.736533	26.292484	76.800935
34.101201	33.026241	76.805940
32.727003	25.848352	76.810945
32.128419	25.455206	76.815950
31.192515	26.727160	76.820954
31.032639	31.097966	76.825959
30.463385	35.774603	76.830964
30.425559	33.039798	76.835969
29.982377	20.835492	76.840974
29.020723	31.984788	76.845978
28.424048	28.878855	76.850983
27.522878	38.747998	76.855988
25.962792	30.878472	76.860993
25.481859	35.201305	76.865998
24.813384	40.140072	76.871002
24.737084	25.056984	76.876007
24.394381	24.189338	76.881012
23.974954	26.956721	76.886017
22.711441	29.686862	76.891022
21.744152	39.182103	76.896026
21.797911	21.832388	76.901031
20.612607	34.718477	76.906036
19.636291	26.031676	76.911041
18.881627	25.437148	76.916046
18.696149	34.175489	76.921050
18.436604	26.345866	76.926055
17.551315	34.657515	76.931060
16.618287	37.458883	76.936065
15.706091	26.964360	76.941070
15.058922	33.958685	76.946074
15.167444	22.853398	76.951079
14.270887	36.888722	76.956084
13.285524	32.354658	76.961089
12.537083	27.979303	76.966094
11.679513	30.057647	76.971098
11.297626	26.770031	76.976103
10.932702	31.420319	76.981108
10.209610	25.653997	76.986113
9.336373	20.893884	76.991118
8.295073	29.236622	76.996122
8.261862	23.200054	77.001127
7.504829	25.469173	77.006132
6.850312	27.946886	77.011137
5.925680	27.563859	77.016142
5.212972	24.837013	77.021147
4.965539	16.786649	77.026151
4.395399	26.139981	77.031156
3.327783	38.040036	77.036161