Tue Jun 08 17:11:35 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
0.090760	94.455643	0.000000
-0.364570	81.214547	0.005005
-0.985197	57.678110	0.010010
-2.979836	19.769829	0.015014
-7.135662	17.039745	0.020019
-12.125739	14.381661	0.025024
-17.610101	15.046543	0.030029
-21.920703	12.428270	0.035034
-24.931670	7.524795	0.040038
-29.156865	16.702022	0.045043
-32.698229	12.704574	0.050048
-36.486574	15.691651	0.055053
-40.545862	21.158186	0.060058
-44.349596	9.774913	0.065062
-48.252402	14.765440	0.070067
-51.687850	5.719657	0.075072
-55.220554	19.886113	0.080077
-58.952026	7.260941	0.085082
-62.679261	14.594768	0.090086
-66.952607	13.276247	0.095091
-70.223135	6.434288	0.100096
-74.296828	20.684050	0.105101
-77.671452	23.049200	0.110106
-81.599152	15.034364	0.115110
-85.395257	7.716921	0.120115
-89.149673	8.758614	0.125120
-92.962397	7.825310	0.130125
-97.011790	9.602810	0.135130
-100.416993	6.472142	0.140134
-104.385238	14.259801	0.145139
-107.418636	13.359041	0.150144
-111.738793	13.423366	0.155149
-115.679190	13.346394	0.160154
-119.336543	9.651916	0.165158
-123.340684	18.553699	0.170163
-126.364467	7.272397	0.175168
-130.564288	8.983755	0.180173
-134.370133	2.702565	0.185178
-138.039818	4.855875	0.190182
-142.176997	10.349269	0.195187
-145.704261	3.722704	0.200192
-149.595746	16.813190	0.205197
-153.560567	9.772620	0.210202
-157.285066	9.189743	0.215206
-160.745799	11.842464	0.220211
-164.697951	16.719977	0.225216
-168.519380	6.719768	0.230221
-171.935105	8.085523	0.235226
-175.335921	6.964419	0.240230
-179.324179	15.378422	0.245235
-183.339701	10.205661	0.250240
-187.357800	9.879989	0.255245
-191.206635	7.455039	0.260250
-195.008911	10.450552	0.265254
-198.806182	13.669405	0.270259
-202.020855	1.362293	0.275264
-205.696847	4.870197	0.280269
-209.200268	14.177188	0.285274
-212.981184	5.729573	0.290278
-217.235258	9.681608	0.295283
-220.922410	9.158690	0.300288
-225.229025	10.480321	0.305293
-228.708241	17.308345	0.310298
-232.043344	7.264256	0.315302
-235.934023	16.983846	0.320307
-239.518838	10.603265	0.325312
-243.295656	16.797915	0.330317
-247.375637	11.771656	0.335322
-251.065035	6.042533	0.340326
-255.039388	13.816360	0.345331
-258.609533	4.209688	0.350336
-262.380224	7.837293	0.355341
-266.225431	5.518358	0.360346
-269.631646	4.868353	0.365350
-273.389597	4.114875	0.370355
-277.511973	4.769867	0.375360
-281.161009	8.754752	0.380365
-284.876012	10.791618	0.385370
-288.676712	7.363040	0.390374
-292.401334	13.989270	0.395379
-295.962164	4.247228	0.400384
-299.891522	11.624188	0.405389
-303.910009	8.689659	0.410394
-307.222979	3.958577	0.415398
-311.431268	20.597490	0.420403
-314.994504	9.669376	0.425408
-318.595377	10.159563	0.430413
-322.776190	12.289386	0.435418
-326.192116	3.450083	0.440422
-330.030629	17.630483	0.445427
-333.674617	10.874502	0.450432
-337.788427	18.188011	0.455437
-341.443158	16.133289	0.460442
-345.018785	4.955113	0.465446
-348.730022	11.709738	0.470451
-352.279568	10.478108	0.475456
-356.294919	10.263031	0.480461
-360.013869	9.259006	0.485466
-363.851140	0.657003	0.490470
-367.978864	8.422888	0.495475
-371.576721	5.565861	0.500480
-375.199443	11.090802	0.505485
-378.665883	18.381707	0.510490
-382.792343	12.632155	0.515494
-386.574463	8.821556	0.520499
-390.026964	15.797862	0.525504
-393.969499	9.839546	0.530509
-398.076498	9.363537	0.535514
-401.378084	7.905081	0.540518
-405.629446	18.073096	0.545523
-408.919870	3.761402	0.550528
-412.790703	2.312986	0.555533
-416.467033	6.676052	0.560538
-420.153886	14.319775	0.565542
-424.358954	9.061349	0.570547
-427.968962	7.256380	0.575552
-431.707914	4.112974	0.580557
-435.554182	10.648083	0.585562
-438.753281	10.933659	0.590566
-443.159047	21.315289	0.595571
-446.288760	4.869494	0.600576
-450.147026	4.845036	0.605581
-454.350235	5.568133	0.610586
-457.774381	9.371689	0.615590
-461.777034	8.402213	0.620595
-465.256786	5.000435	0.625600
-469.350732	12.924416	0.630605
-473.172695	15.874986	0.635610
-476.636952	4.364821	0.640614
-480.532496	18.749705	0.645619
-483.994114	12.414116	0.650624
-488.291709	15.601817	0.655629
-491.785246	15.707832	0.660634
-495.444685	7.618560	0.665638
-499.625963	10.355292	0.670643
-503.077116	12.073928	0.675648
-507.018966	7.795482	0.680653
-511.205050	10.584362	0.685658
-514.200116	10.810118	0.690662
-518.028993	16.512635	0.695667
-521.668045	12.887988	0.700672
-525.371448	19.701402	0.705677
-529.402708	11.175860	0.710682
-533.110131	9.330065	0.715686
-537.222603	13.010615	0.720691
-540.661344	6.348281	0.725696
-544.424366	20.468123	0.730701
-548.038286	17.945159	0.735706
-551.510686	11.210455	0.740710
-556.311159	15.526930	0.745715
-559.968515	15.665844	0.750720
-563.408897	27.201448	0.755725
-567.459088	13.621395	0.760730
-570.412683	12.868696	0.765734
-574.460361	15.850975	0.770739
-578.466525	16.097910	0.775744
-581.995370	11.878921	0.780749
-586.134167	9.052137	0.785754
-589.591669	13.498967	0.790758
-593.290866	22.586021	0.795763
-597.064955	8.648386	0.800768
-600.734426	14.762137	0.805773
-604.941663	17.699196	0.810778
-607.915529	3.653076	0.815782
-612.349397	6.487724	0.820787
-616.125184	10.775259	0.825792
-619.713929	16.488358	0.830797
-623.537885	21.560558	0.835802
-627.267880	5.358448	0.840806
-631.090834	11.406986	0.845811
-635.086897	10.205241	0.850816
-638.449214	18.119862	0.855821
-642.436515	11.884881	0.860826
-645.776795	8.013692	0.865830
-649.849232	15.201163	0.870835
-653.518968	11.335994	0.875840
-657.002693	14.539308	0.880845
-661.216981	12.428921	0.885850
-664.862642	10.754206	0.890854
-669.070677	12.232227	0.895859
-672.425310	4.749579	0.900864
-676.031762	6.892469	0.905869
-679.865760	9.024679	0.910874
-683.158968	9.301715	0.915878
-687.519877	11.482517	0.920883
-691.284906	-0.517764	0.925888
-694.975004	9.343398	0.930893
-698.955999	11.226134	0.935898
-702.381766	4.607105	0.940902
-706.246194	16.437395	0.945907
-709.719271	9.316132	0.950912
-713.677835	4.858792	0.955917
-717.441444	7.548911	0.960922
-721.098923	10.326600	0.965926
-725.362716	16.456795	0.970931
-728.878731	5.461759	0.975936
-732.286617	3.619595	0.980941
-736.258091	13.155292	0.985946
-740.289301	10.326376	0.990950
-744.301439	12.235813	0.995955
-747.754716	8.844724	1.000960
-751.261046	12.274999	1.005965
-755.085635	13.289426	1.010970
-758.413227	14.971658	1.015974
-762.637806	18.934528	1.020979
-766.155990	14.012076	1.025984
-770.204462	5.588413	1.030989
-774.351813	7.785537	1.035994
-777.760118	1.927335	1.040998
-781.537188	9.027118	1.046003
-785.119195	10.539895	1.051008
-788.843377	16.830933	1.056013
-792.848380	13.525499	1.061018
-796.466249	6.616257	1.066022
-800.444082	10.882178	1.071027
-804.150083	8.955065	1.076032
-807.608532	18.148970	1.081037
-811.493051	14.691831	1.086042
-815.163713	6.455978	1.091046
-819.299842	17.571995	1.096051
-822.841003	7.519976	1.101056
-826.409778	6.588068	1.106061
-830.536494	20.121640	1.111066
-834.027375	8.839775	1.116070
-837.902508	14.089473	1.121075
-841.576266	3.780782	1.126080
-844.980797	11.502671	1.131085
-849.195210	16.137641	1.136090
-852.868440	3.176438	1.141094
-856.623761	12.729599	1.146099
-860.523863	11.990766	1.151104
-864.221384	-0.755084	1.156109
-868.131081	13.951826	1.161114
-871.406374	7.377765	1.166118
-875.634600	6.231095	1.171123
-879.174473	7.203467	1.176128
-882.640738	11.799245	1.181133
-887.081975	16.132950	1.186138
-890.426039	4.710290	1.191142
-894.514739	9.251489	1.196147
-897.957245	3.825938	1.201152
-902.003254	10.557937	1.206157
-905.701447	14.254145	1.211162
-909.352915	9.726513	1.216166
-913.840012	18.040051	1.221171
-917.159804	15.583352	1.226176
-920.321482	15.787071	1.231181
-924.240849	13.375284	1.236186
-927.724066	3.985603	1.241190
-931.717347	24.950388	1.246195
-935.436073	10.109584	1.251200
-939.471882	7.551235	1.256205
-943.495644	10.141743	1.261210
-947.205779	6.895962	1.266214
-950.922620	17.122671	1.271219
-954.436910	19.035246	1.276224
-958.355483	18.874366	1.281229
-961.878130	15.534045	1.286234
-965.435964	10.519898	1.291238
-969.716296	7.559119	1.296243
-973.358832	11.704870	1.301248
-977.228678	10.688997	1.306253
-981.035295	18.468569	1.311258
-984.350763	13.096274	1.316262
-988.284718	12.157333	1.321267
-991.669528	5.068927	1.326272
-995.228872	6.500227	1.331277
-999.535014	15.156170	1.336282
-1003.533325	15.789751	1.341286
-1007.368398	14.744648	1.346291
-1011.256259	16.759691	1.351296
-1014.877396	12.794929	1.356301
-1018.500046	12.199643	1.361306
-1022.172562	5.132241	1.366310
-1026.379119	12.333195	1.371315
-1029.328779	12.525065	1.376320
-1033.387859	7.314430	1.381325
-1037.245532	12.273558	1.386330
-1041.098235	5.701680	1.391334
-1044.795717	12.076750	1.396339
-1048.398033	11.910597	1.401344
-1052.610036	6.091945	1.406349
-1055.992862	15.189757	1.411354
-1059.537713	-1.323530	1.416358
-1063.565325	8.349956	1.421363
-1067.249952	12.245267	1.426368
-1070.915808	13.288371	1.431373
-1074.998873	7.140522	1.436378
-1078.492665	5.552581	1.441382
-1082.542109	13.679036	1.446387
-1086.042261	7.010353	1.451392
-1089.444309	10.627838	1.456397
-1094.045211	24.057536	1.461402
-1097.476407	12.257682	1.466406
-1101.475096	11.337857	1.471411
-1104.576371	8.431715	1.476416
-1108.498013	5.915108	1.481421
-1112.480233	7.179530	1.486426
-1116.129415	12.489341	1.491430
-1119.894117	13.166200	1.496435
-1123.659297	14.699261	1.501440
-1127.777480	9.974096	1.506445
-1131.561117	12.380660	1.511450
-1135.115845	8.217907	1.516454
-1138.958726	16.968100	1.521459
-1142.335391	15.599684	1.526464
-1146.045017	1.187774	1.531469
-1150.136168	7.261872	1.536474
-1153.558821	2.431903	1.541478
-1157.641450	10.510439	1.546483
-1161.384769	9.499059	1.551488
-1165.274864	15.322349	1.556493
-1169.329358	16.206898	1.561498
-1172.662195	6.958184	1.566502
-1176.293366	10.225507	1.571507
-1179.558063	12.462082	1.576512
-1184.034314	8.793123	1.581517
-1188.087457	15.013088	1.586522
-1191.564183	12.208591	1.591526
-1195.604332	9.835960	1.596531
-1199.212425	12.938299	1.601536
-1202.485793	8.332976	1.606541
-1206.274087	14.048036	1.611546
-1209.689904	7.953882	1.616550
-1213.909147	13.338385	1.621555
-1218.063201	9.160614	1.626560
-1221.572273	11.809422	1.631565
-1225.240823	7.529334	1.636570
-1228.891898	3.607800	1.641574
-1232.608353	6.019885	1.646579
-1236.511290	13.194149	1.651584
-1240.268844	10.730400	1.656589
-1244.611391	10.811928	1.661594
-1247.830143	2.096279	1.666598
-1251.681192	8.465127	1.671603
-1255.521291	6.965231	1.676608
-1259.103154	-3.508818	1.681613
-1262.889173	11.238721	1.686618
-1266.716902	2.840028	1.691622
-1270.499540	9.235035	1.696627
-1273.901857	7.613787	1.701632
-1278.125598	6.429255	1.706637
-1281.835533	12.739555	1.711642
-1285.319389	8.502400	1.716646
-1289.227526	13.702893	1.721651
-1292.746039	2.774738	1.726656
-1296.709444	2.665290	1.731661
-1300.691076	7.751319	1.736666
-1304.305565	6.261662	1.741670
-1308.226057	8.303495	1.746675
-1311.940431	5.531237	1.751680
-1315.419646	1.914579	1.756685
-1319.233899	11.201139	1.761690
-1322.969431	8.768024	1.766694
-1326.905644	5.120536	1.771699
-1330.794605	5.340148	1.776704
-1334.646824	9.138556	1.781709
-1338.508184	7.859477	1.786714
-1341.973475	4.026520	1.791718
-1345.422645	9.561876	1.796723
-1348.965427	4.837177	1.801728
-1352.820660	10.041662	1.806733
-1357.163654	17.571070	1.811738
-1360.771523	11.446094	1.816742
-1364.790610	15.605140	1.821747
-1368.253729	9.647135	1.826752
-1371.816761	11.578287	1.831757
-1375.724349	6.701161	1.836762
-1378.923424	1.015156	1.841766
-1383.412925	9.195358	1.846771
-1387.288636	6.635999	1.851776
-1391.001135	6.303161	1.856781
-1394.666151	14.206364	1.861786
-1398.401781	7.561838	1.866790
-1402.016098	6.880197	1.871795
-1405.537010	8.057361	1.876800
-1409.010276	8.311023	1.881805
-1413.606472	9.795661	1.886810
-1416.930709	6.530200	1.891814
-1420.980217	14.102006	1.896819
-1424.845452	14.817721	1.901824
-1428.382188	6.419328	1.906829
-1432.095382	10.153680	1.911834
-1435.471262	9.804893	1.916838
-1439.615214	8.100810	1.921843
-1443.498975	12.154581	1.926848
-1447.382602	8.840781	1.931853
-1451.371915	12.419312	1.936858
-1454.710886	8.837097	1.941862
-1458.684594	8.096862	1.946867
-1461.975255	14.739854	1.951872
-1465.709323	6.178440	1.956877
-1469.598936	17.505667	1.961882
-1473.197244	5.771197	1.966886
-1477.311015	4.888478	1.971891
-1481.088896	9.590748	1.976896
-1484.862291	6.992986	1.981901
-1489.008532	8.452505	1.986906
-1492.717949	0.949824	1.991910
-1496.159299	12.825269	1.996915
-1500.039157	5.359600	2.006912
-1500.917301	2.084432	2.016909
-1498.606408	1.409218	2.026906
-1495.570217	10.284519	2.036902
-1493.498822	6.719185	2.046899
-1491.581799	7.893642	2.056896
-1489.755575	8.396431	2.066893
-1487.764092	10.626744	2.076890
-1486.125193	7.005298	2.086886
-1483.874955	6.678417	2.096883
-1481.992248	6.930031	2.106880
-1480.402476	6.939518	2.116877
-1478.226036	2.828541	2.126874
-1476.331267	6.203798	2.136870
-1474.400295	5.946394	2.146867
-1472.752190	8.609970	2.156864
-1470.989341	8.807881	2.166861
-1468.558827	9.393798	2.176858
-1466.905096	9.028314	2.186854
-1465.357817	6.243466	2.196851
-1463.092250	9.516693	2.206848
-1461.066791	7.822680	2.216845
-1459.407883	11.175627	2.226842
-1457.675601	7.035046	2.236838
-1455.851185	1.318748	2.246835
-1453.714446	6.668411	2.256832
-1451.830563	2.809262	2.266829
-1449.972912	6.296034	2.276826
-1447.988635	3.015617	2.286822
-1446.160696	3.254920	2.296819
-1444.237743	6.789363	2.306816
-1442.325227	10.272643	2.316813
-1440.510802	9.462222	2.326810
-1438.812564	7.601534	2.336806
-1436.748753	3.907506	2.346803
-1434.912777	5.199853	2.356800
-1433.376863	1.016345	2.366797
-1431.148822	4.267582	2.376794
-1429.077475	1.386395	2.386790
-1427.486581	4.935207	2.396787
-1425.417152	5.667358	2.406784
-1423.595962	5.705483	2.416781
-1421.645833	5.678777	2.426778
-1419.873523	10.830226	2.436774
-1418.148686	7.161239	2.446771
-1416.140580	10.028577	2.456768
-1414.293158	3.873610	2.466765
-1412.235980	3.387465	2.476762
-1410.481781	16.734732	2.486758
-1408.827801	8.304178	2.496755
-1406.550322	8.405018	2.506752
-1404.534807	2.174150	2.516749
-1402.983254	3.356496	2.526746
-1401.283076	2.015585	2.536742
-1399.283819	3.976655	2.546739
-1397.217263	5.154715	2.556736
-1395.378407	4.352369	2.566733
-1393.640205	4.363661	2.576730
-1391.674963	3.932049	2.586726
-1389.761271	-1.059332	2.596723
-1387.987213	2.927146	2.606720
-1386.198486	6.664496	2.616717
-1384.335553	11.241964	2.626714
-1382.157828	7.138320	2.636710
-1380.428176	3.777179	2.646707
-1377.957484	9.167138	2.656704
-1376.597899	8.932049	2.666701
-1374.898112	12.419102	2.676698
-1372.953227	10.091220	2.686694
-1370.804448	5.220314	2.696691
-1369.258075	4.242159	2.706688
-1367.413526	7.063713	2.716685
-1365.322529	10.000229	2.726682
-1363.627546	11.082863	2.736678
-1361.987005	5.284362	2.746675
-1359.627072	6.163461	2.756672
-1357.783127	7.522450	2.766669
-1355.803456	4.975188	2.776666
-1354.178151	15.380156	2.786662
-1352.292722	10.291677	2.796659
-1350.270874	3.436892	2.806656
-1348.491207	11.033462	2.816653
-1346.258663	4.140511	2.826650
-1344.908592	15.540078	2.836646
-1342.952636	6.208369	2.846643
-1340.698542	4.959668	2.856640
-1339.456810	6.850908	2.866637
-1337.254968	4.344140	2.876634
-1335.272525	-1.388190	2.886630
-1333.301089	6.092847	2.896627
-1331.809975	4.420723	2.906624
-1329.546220	2.450691	2.916621
-1327.814931	3.503786	2.926618
-1326.002318	2.286264	2.936614
-1324.014273	0.683316	2.946611
-1322.122614	3.867506	2.956608
-1320.483109	6.317234	2.966605
-1318.387167	0.449223	2.976602
-1316.444069	0.579091	2.986598
-1314.825844	2.579169	2.996595
-1312.841055	-1.203588	3.006592
-1311.036463	5.211386	3.016589
-1308.956010	-5.010755	3.026586
-1307.112428	-3.186519	3.036582
-1305.050607	-5.788573	3.046579
-1303.548716	1.425341	3.056576
-1301.503716	-0.764385	3.066573
-1299.740088	2.664309	3.076570
-1297.682336	0.002884	3.086566
-1295.934157	-1.743416	3.096563
-1294.163113	3.588920	3.106560
-1291.945021	3.168070	3.116557
-1290.451954	5.476973	3.126554
-1288.382163	4.803368	3.136550
-1286.444988	-0.827503	3.146547
-1284.588549	8.957629	3.156544
-1282.757111	3.180907	3.166541
-1280.807926	7.145262	3.176538
-1279.022592	4.126729	3.186534
-1277.327049	5.086392	3.196531
-1275.122347	0.790442	3.206528
-1273.355519	3.305267	3.216525
-1271.354071	6.877693	3.226522
-1269.630939	5.309993	3.236518
-1267.929379	-0.788250	3.246515
-1265.764582	-1.409789	3.256512
-1263.903766	-4.902489	3.266509
-1262.206225	-1.002009	3.276506
-1260.082497	5.645103	3.286502
-1258.282841	-2.495832	3.296499
-1256.443512	-3.545996	3.306496
-1254.520449	0.680930	3.316493
-1252.888299	4.161866	3.326490
-1251.012978	4.701382	3.336486
-1248.950461	-2.655938	3.346483
-1247.022257	5.693735	3.356480
-1245.083231	4.049050	3.366477
-1243.329391	8.269873	3.376474
-1241.611922	9.045570	3.386470
-1240.027981	6.808587	3.396467
-1237.886807	9.109749	3.406464
-1235.650065	3.241700	3.416461
-1234.066479	4.496465	3.426458
-1232.181194	3.002106	3.436454
-1230.016379	9.756001	3.446451
-1228.412705	1.034575	3.456448
-1226.369962	6.557014	3.466445
-1224.760474	5.638024	3.476442
-1222.249731	9.014327	3.486438
-1220.784883	9.191990	3.496435
-1218.776657	1.562614	3.506432
-1216.936416	7.447070	3.516429
-1215.450804	2.347873	3.526426
-1213.736260	1.630188	3.536422
-1211.515497	5.506046	3.546419
-1209.460563	8.479664	3.556416
-1207.673378	8.931976	3.566413
-1205.870052	9.795698	3.576410
-1203.690728	7.833906	3.586406
-1201.934221	6.458502	3.596403
-1200.065371	5.905209	3.606400
-1198.318779	8.147291	3.616397
-1196.698064	14.201460	3.626394
-1194.633364	6.163625	3.636390
-1192.524448	7.287090	3.646387
-1190.569189	8.777220	3.656384
-1189.080732	7.373948	3.666381
-1187.227384	4.096764	3.676378
-1185.184288	5.086888	3.686374
-1183.327993	5.374791	3.696371
-1181.214461	9.597107	3.706368
-1179.523485	11.689480	3.716365
-1177.729736	7.787034	3.726362
-1175.877550	10.606576	3.736358
-1174.132482	8.540738	3.746355
-1171.767946	3.062978	3.756352
-1170.084551	10.101139	3.766349
-1168.426308	7.815852	3.776346
-1166.381258	9.067280	3.786342
-1164.206539	10.420143	3.796339
-1163.135741	4.500994	3.806336
-1160.856324	5.277446	3.816333
-1158.729101	4.486544	3.826330
-1156.925854	3.737840	3.836326
-1154.933565	3.919803	3.846323
-1153.478699	4.207491	3.856320
-1151.230509	8.542257	3.866317
-1149.601795	8.917866	3.876314
-1147.670513	5.464092	3.886310
-1145.858147	8.286929	3.896307
-1143.643168	3.207945	3.906304
-1141.919910	0.620629	3.916301
-1140.045812	1.754802	3.926298
-1138.361751	3.499012	3.936294
-1136.730974	7.634704	3.946291
-1134.816353	4.804673	3.956288
-1132.424326	7.593979	3.966285
-1130.635842	4.165128	3.976282
-1128.858350	3.083348	3.986278
-1127.101252	1.707873	3.996275
-1124.921494	3.223903	4.006272
-1123.293534	4.820458	4.016269
-1121.340884	10.878129	4.026266
-1119.509312	13.398506	4.036262
-1117.644187	4.938109	4.046259
-1115.719188	4.244791	4.056256
-1113.618826	7.440276	4.066253
-1112.061889	9.120960	4.076250
-1110.310950	6.516651	4.086246
-1108.305971	1.391934	4.096243
-1106.227423	5.600537	4.106240
-1104.411489	4.346968	4.116237
-1102.574664	7.797567	4.126234
-1101.064810	4.180630	4.136230
-1098.882309	8.437784	4.146227
-1096.727343	7.935000	4.156224
-1094.998047	6.184908	4.166221
-1093.221772	-0.116202	4.176218
-1091.271498	7.853528	4.186214
-1089.493623	8.430795	4.196211
-1087.623696	2.131785	4.206208
-1085.657134	4.644411	4.216205
-1084.094545	8.361450	4.226202
-1081.914227	7.981578	4.236198
-1080.017863	5.417521	4.246195
-1078.002427	3.173691	4.256192
-1076.313223	7.651906	4.266189
-1074.585136	4.553173	4.276186
-1072.483764	10.521705	4.286182
-1070.583328	4.820554	4.296179
-1068.994788	9.592310	4.306176
-1066.787664	8.102438	4.316173
-1065.184817	4.958422	4.326170
-1063.159434	5.447753	4.336166
-1061.174424	5.312469	4.346163
-1059.847557	-1.595180	4.356160
-1057.019109	3.295664	4.366157
-1055.610038	-1.256807	4.376154
-1054.159396	0.389981	4.386150
-1051.888087	-2.744311	4.396147
-1050.287185	3.652017	4.406144
-1047.661957	3.685440	4.416141
-1046.553018	2.643787	4.426138
-1044.294641	10.338140	4.436134
-1042.577324	3.665395	4.446131
-1040.668373	4.072763	4.456128
-1038.720383	6.568445	4.466125
-1036.874700	8.548554	4.476122
-1035.260789	10.437248	4.486118
-1033.427897	6.035703	4.496115
-1031.437469	12.898700	4.506112
-1029.249205	13.012296	4.516109
-1027.450719	12.066462	4.526106
-1025.632666	7.325610	4.536102
-1023.755888	1.307629	4.546099
-1021.979841	6.077641	4.556096
-1020.044644	5.337561	4.566093
-1017.940186	4.497679	4.576090
-1016.310598	7.781947	4.586086
-1014.488228	7.844550	4.596083
-1012.540435	1.862201	4.606080
-1010.602531	0.376292	4.616077
-1008.849925	2.299279	4.626074
-1007.337814	0.707048	4.636070
-1004.887839	3.316934	4.646067
-1003.025605	-3.583419	4.656064
-1001.276219	-0.166372	4.666061
-999.355177	-5.556441	4.676058
-997.599426	4.537007	4.686054
-995.587036	6.520130	4.696051
-993.775571	-5.244461	4.706048
-991.959846	6.538894	4.716045
-989.982525	0.859355	4.726042
-987.883843	3.293621	4.736038
-986.462166	4.769538	4.746035
-984.405033	8.042860	4.756032
-982.564706	10.769283	4.766029
-980.741582	9.615705	4.776026
-978.687653	19.447729	4.786022
-976.741639	18.393593	4.796019
-975.005526	7.903056	4.806016
-973.178340	6.460673	4.816013
-971.241933	8.262014	4.826010
-969.264871	10.684763	4.836006
-967.530977	15.793624	4.846003
-965.657538	8.178393	4.856000
-963.597923	4.577382	4.865997
-961.992148	8.399297	4.875994
-959.998469	9.093702	4.885990
-958.242829	11.699908	4.895987
-956.228063	4.112984	4.905984
-954.469802	5.359607	4.915981
-952.467541	6.265562	4.925978
-950.530343	8.191664	4.935974
-948.362292	1.007628	4.945971
-946.968976	1.636747	4.955968
-944.989118	7.279213	4.965965
-942.989037	4.325908	4.975962
-941.240461	7.701229	4.985958
-939.357537	9.450114	4.995955
-937.228844	2.473212	5.005952
-935.571207	2.744345	5.015949
-933.924335	1.168921	5.025946
-931.962223	4.272437	5.035942
-930.092473	10.511219	5.045939
-928.033083	7.920819	5.055936
-926.119608	6.988879	5.065933
-924.460990	6.261148	5.075930
-922.504133	5.693657	5.085926
-920.228660	4.096089	5.095923
-918.869865	-3.540246	5.105920
-916.795446	3.527733	5.115917
-914.935616	11.659710	5.125914
-912.987209	10.029368	5.135910
-911.257950	6.786242	5.145907
-909.219317	3.460763	5.155904
-907.436230	2.621167	5.165901
-905.214948	3.369402	5.175898
-903.862988	5.635883	5.185894
-902.134810	5.451888	5.195891
-899.694113	2.468413	5.205888
-897.674479	2.940236	5.215885
-896.448352	3.571592	5.225882
-894.337772	-0.330594	5.235878
-892.357473	4.961270	5.245875
-890.600413	5.545751	5.255872
-888.590045	10.014368	5.265869
-886.588313	7.184900	5.275866
-884.989020	8.561202	5.285862
-883.040165	3.275479	5.295859
-881.327044	1.024746	5.305856
-879.481926	6.206241	5.315853
-877.324555	5.441919	5.325850
-875.562364	11.894427	5.335846
-873.932845	5.287394	5.345843
-871.866165	4.194413	5.355840
-870.002283	5.675482	5.365837
-867.892359	4.869907	5.375834
-866.337012	6.730780	5.385830
-864.341074	5.429021	5.395827
-862.082341	10.619360	5.405824
-860.221187	9.698011	5.415821
-858.807555	9.388995	5.425818
-856.825631	7.117422	5.435814
-854.794602	13.134115	5.445811
-853.006197	10.229829	5.455808
-851.114018	8.092624	5.465805
-849.534491	1.637643	5.475802
-847.546796	4.832451	5.485798
-845.532709	3.820043	5.495795
-843.513180	1.619089	5.505792
-841.789191	0.117013	5.515789
-839.834199	3.533224	5.525786
-837.926143	2.778913	5.535782
-836.270794	-0.597727	5.545779
-834.046564	-0.639595	5.555776
-832.364626	0.758900	5.565773
-830.533083	-3.944672	5.575770
-828.656142	2.071605	5.585766
-826.815409	4.571176	5.595763
-824.785337	1.422678	5.605760
-823.149284	-0.926255	5.615757
-820.926984	-1.607238	5.625754
-819.175572	4.211248	5.635750
-817.451337	2.079170	5.645747
-815.428723	0.188731	5.655744
-813.355390	7.994423	5.665741
-811.741798	6.329509	5.675738
-810.082204	1.384342	5.685734
-808.224199	6.436006	5.695731
-806.098865	3.261284	5.705728
-804.208284	4.353258	5.715725
-802.444647	0.215439	5.725722
-800.477615	1.094710	5.735718
-798.653194	6.117364	5.745715
-796.862140	2.028590	5.755712
-794.894586	3.812020	5.765709
-792.914318	5.523316	5.775706
-791.226194	8.394514	5.785702
-789.134677	4.111104	5.795699
-787.289593	2.277628	5.805696
-785.402160	7.822615	5.815693
-783.627545	4.273761	5.825690
-781.845412	9.157848	5.835686
-779.548497	8.640739	5.845683
-778.042020	7.259410	5.855680
-776.165520	8.137237	5.865677
-774.148689	2.679039	5.875674
-772.443537	9.732623	5.885670
-770.793307	9.988098	5.895667
-768.575117	5.418558	5.905664
-766.392381	10.228759	5.915661
-764.678742	8.373983	5.925658
-763.182016	9.836306	5.935654
-761.127013	6.489111	5.945651
-758.994893	7.353505	5.955648
-757.130513	12.231393	5.965645
-755.475438	12.401862	5.975642
-753.663613	11.710738	5.985638
-751.458114	12.664112	5.995635
-749.958430	17.168283	6.005632
-748.062018	13.264581	6.015629
-745.948158	16.501022	6.025626
-744.272672	11.779998	6.035622
-742.235934	11.869555	6.045619
-740.975984	8.978152	6.055616
-738.725739	10.408383	6.065613
-736.533458	7.417042	6.075610
-734.458301	12.990306	6.085606
-733.202962	15.896285	6.095603
-731.026841	11.311454	6.105600
-728.954338	7.596092	6.115597
-727.273055	9.999374	6.125594
-725.332668	12.033323	6.135590
-723.699337	12.092133	6.145587
-721.583660	7.295571	6.155584
-719.687620	8.913466	6.165581
-718.338013	10.963047	6.175578
-716.370205	16.321965	6.185574
-713.860172	14.296936	6.195571
-712.110983	13.375104	6.205568
-710.387935	13.120532	6.215565
-708.223115	11.734529	6.225562
-706.689104	11.451933	6.235558
-704.875388	10.614671	6.245555
-703.010207	11.044326	6.255552
-701.148029	6.791617	6.265549
-699.124067	12.341674	6.275546
-697.306391	7.225555	6.285542
-695.461174	7.366971	6.295539
-693.279544	7.956133	6.305536
-691.773423	4.139195	6.315533
-690.097264	8.163744	6.325530
-687.799182	8.430585	6.335526
-685.995523	10.682067	6.345523
-683.989575	5.151077	6.355520
-682.321545	4.040045	6.365517
-680.348280	2.413443	6.375514
-678.342248	10.914875	6.385510
-676.692877	9.728400	6.395507
-674.768442	12.862222	6.405504
-672.704202	6.748569	6.415501
-671.016013	10.087738	6.425498
-669.348852	6.975106	6.435494
-667.570016	7.523930	6.445491
-665.403230	13.262909	6.455488
-663.465772	10.599886	6.465485
-661.553928	9.718928	6.475482
-659.560401	8.114546	6.485478
-657.941396	7.209147	6.495475
-656.283112	7.839526	6.505472
-654.141271	3.988992	6.515469
-652.065987	-0.260349	6.525466
-650.216224	6.209248	6.535462
-648.675301	5.844467	6.545459
-646.676588	12.590056	6.555456
-644.331570	8.786864	6.565453
-642.888966	8.571353	6.575450
-640.909208	10.591472	6.585446
-639.400954	12.243541	6.595443
-637.534524	7.412720	6.605440
-635.411039	8.411054	6.615437
-633.277029	8.840847	6.625434
-631.439921	8.596373	6.635430
-629.650278	9.996624	6.645427
-627.987872	8.959296	6.655424
-625.757473	4.414602	6.665421
-624.192076	10.131124	6.675418
-622.349089	12.953292	6.685414
-620.190308	12.534665	6.695411
-618.319131	13.298073	6.705408
-616.517194	11.623040	6.715405
-614.828118	6.806853	6.725402
-612.793879	11.791221	6.735398
-610.998440	13.980122	6.745395
-609.174528	12.685469	6.755392
-607.027235	13.310207	6.765389
-605.702236	12.154520	6.775386
-603.529355	13.068908	6.785382
-601.609445	12.827233	6.795379
-599.783154	13.196024	6.805376
-597.666637	11.732206	6.815373
-595.973038	10.577693	6.825370
-593.731119	14.792129	6.835366
-592.138581	12.440071	6.845363
-590.331381	7.052696	6.855360
-588.416299	4.444921	6.865357
-586.882035	8.636534	6.875354
-584.833231	10.606891	6.885350
-582.905007	14.712333	6.895347
-581.113315	11.874772	6.905344
-578.965166	11.425582	6.915341
-577.063936	9.865133	6.925338
-575.546984	12.314459	6.935334
-573.438376	4.755051	6.945331
-571.188979	12.161146	6.955328
-569.553810	2.761052	6.965325
-567.853693	10.699689	6.975322
-565.990948	6.580122	6.985318
-564.179307	9.593444	6.995315
-562.358152	2.057676	7.005312
-560.271902	9.763281	7.015309
-558.327762	4.247689	7.025306
-556.835239	3.364820	7.035302
-554.907087	13.501642	7.045299
-552.454291	15.220503	7.055296
-550.984177	11.924748	7.065293
-549.066264	10.501749	7.075290
-546.987701	8.683638	7.085286
-545.075251	14.328395	7.095283
-543.667483	8.079237	7.105280
-541.786550	11.656902	7.115277
-539.579359	6.600079	7.125274
-537.602082	5.912273	7.135270
-536.086494	4.252415	7.145267
-533.875940	8.282167	7.155264
-532.083777	9.356765	7.165261
-530.590681	-1.312868	7.175258
-528.633829	2.886883	7.185254
-526.490192	-0.262793	7.195251
-524.655952	1.448787	7.205248
-522.532045	5.248773	7.215245
-520.692394	1.705061	7.225242
-519.283049	6.165537	7.235238
-517.182804	16.498916	7.245235
-515.158336	9.301753	7.255232
-513.363447	10.065649	7.265229
-511.725595	13.118299	7.275226
-509.381160	0.894058	7.285222
-507.612689	1.805555	7.295219
-505.948028	3.336775	7.305216
-503.914563	2.857896	7.315213
-502.259304	-0.818581	7.325210
-500.186084	2.816219	7.335206
-498.420989	8.028621	7.345203
-496.232594	0.328693	7.355200
-494.322297	3.393490	7.365197
-492.923164	7.988916	7.375194
-490.958895	12.167655	7.385190
-489.005239	-1.119052	7.395187
-486.876534	2.807388	7.405184
-485.178146	1.200760	7.415181
-483.340776	5.248720	7.425178
-481.653967	10.365878	7.435174
-479.656371	11.583495	7.445171
-477.725167	3.725743	7.455168
-475.979496	8.020640	7.465165
-474.031614	6.621382	7.475162
-471.916307	9.064916	7.485158
-470.065388	9.755588	7.495155
-468.500450	5.890686	7.505152
-466.398518	6.954059	7.515149
-464.539056	4.387099	7.525146
-462.759815	3.447561	7.535142
-461.148625	3.496830	7.545139
-459.321315	10.068389	7.555136
-456.976668	7.899563	7.565133
-455.111167	6.896618	7.575130
-453.358805	12.924973	7.585126
-451.525621	8.804591	7.595123
-449.468726	7.407982	7.605120
-447.796765	9.943398	7.615117
-445.932255	10.276056	7.625114
-443.913547	8.938564	7.635110
-442.157353	13.174761	7.645107
-440.171034	7.234235	7.655104
-438.089675	9.288792	7.665101
-436.515031	9.722955	7.675098
-434.442243	11.075107	7.685094
-432.586916	14.347369	7.695091
-431.145016	10.268828	7.705088
-428.868479	8.868931	7.715085
-426.831316	10.271858	7.725082
-424.978852	12.568830	7.735078
-423.555217	9.707523	7.745075
-421.729743	2.401075	7.755072
-419.743171	6.356677	7.765069
-417.494555	11.339543	7.775066
-415.661693	12.455424	7.785062
-414.264951	10.783191	7.795059
-412.027634	6.757904	7.805056
-409.996120	10.627550	7.815053
-408.348579	12.998020	7.825050
-406.559715	15.331995	7.835046
-404.272659	17.053290	7.845043
-402.676476	13.807090	7.855040
-400.750718	9.770045	7.865037
-399.018326	9.151184	7.875034
-396.955651	14.682110	7.885030
-395.272951	14.853905	7.895027
-393.342194	8.169254	7.905024
-391.559040	10.433866	7.915021
-389.568928	7.483296	7.925018
-387.580762	6.398078	7.935014
-385.928151	9.416233	7.945011
-383.873450	9.351507	7.955008
-381.835348	14.630953	7.965005
-379.867371	10.989792	7.975002
-378.415714	7.847437	7.984998
-376.572241	12.729094	7.994995
-374.522218	12.241901	8.004992
-372.641005	7.691220	8.014989
-370.578073	11.080844	8.024986
-368.993955	14.432461	8.034982
-367.092704	7.137927	8.044979
-365.230830	2.567646	8.054976
-363.179762	12.868447	8.064973
-361.295254	7.996292	8.074970
-359.690854	7.634949	8.084966
-357.604660	9.624691	8.094963
-355.690512	9.548915	8.104960
-353.769447	4.306104	8.114957
-352.059350	9.706249	8.124954
-350.099457	9.072885	8.134950
-348.450328	8.478996	8.144947
-346.373514	10.806681	8.154944
-344.579619	4.907499	8.164941
-342.458431	8.093883	8.174938
-340.668305	7.488854	8.184934
-339.189068	11.243016	8.194931
-337.083321	10.078368	8.204928
-335.042252	18.277177	8.214925
-333.200009	10.371103	8.224922
-331.512368	13.457968	8.234918
-329.626780	14.843073	8.244915
-327.212293	12.334698	8.254912
-325.368377	3.462043	8.264909
-324.163692	8.033578	8.274906
-322.196231	14.508050	8.284902
-320.052241	11.581701	8.294899
-318.053753	3.612869	8.304896
-316.123425	5.147995	8.314893
-314.394698	8.829730	8.324890
-312.534357	6.335793	8.334886
-311.006277	9.292740	8.344883
-309.374147	6.534819	8.354880
-306.973931	6.714783	8.364877
-304.907753	5.914211	8.374874
-303.161086	3.397488	8.384870
-301.344129	6.789815	8.394867
-299.526799	3.243296	8.404864
-297.708272	3.034554	8.414861
-295.763528	8.692863	8.424858
-294.054933	12.292695	8.434854
-291.962130	3.408977	8.444851
-289.774739	3.503728	8.454848
-288.226942	7.954769	8.464845
-286.325502	2.379813	8.474842
-284.682939	3.545779	8.484838
-282.584703	7.738790	8.494835
-280.529767	6.647699	8.504832
-278.789239	-1.398596	8.514829
-277.244670	2.651463	8.524826
-275.097687	3.894138	8.534822
-273.134861	4.642764	8.544819
-271.118693	8.506021	8.554816
-269.479052	-0.090496	8.564813
-267.648183	5.666401	8.574810
-265.607243	2.996857	8.584807
-263.953105	0.858036	8.594803
-261.961511	-0.794058	8.604800
-259.966619	3.639985	8.614797
-258.091028	5.840977	8.624794
-256.199076	-0.701801	8.634791
-254.613168	8.279782	8.644787
-252.895044	7.036217	8.654784
-250.397234	5.954150	8.664781
-248.890806	4.129571	8.674778
-246.964852	12.040296	8.684775
-244.852384	9.946968	8.694771
-243.363462	10.538970	8.704768
-241.421425	8.427844	8.714765
-239.303357	3.398297	8.724762
-237.584600	9.275218	8.734759
-235.654880	7.990230	8.744755
-233.899157	5.639155	8.754752
-231.900938	2.487282	8.764749
-229.527377	-0.296996	8.774746
-228.021694	0.087021	8.784743
-226.656265	0.146908	8.794739
-224.248135	-4.133650	8.804736
-222.122784	-5.941855	8.814733
-220.929486	-5.433121	8.824730
-218.941813	-5.829718	8.834727
-216.968312	1.187187	8.844723
-215.013738	-1.205495	8.854720
-213.153318	-0.415960	8.864717
-211.321791	1.097031	8.874714
-209.488025	-0.112997	8.884711
-207.260318	-1.356994	8.894707
-205.961310	3.965513	8.904704
-203.511682	-0.919718	8.914701
-201.962544	0.766992	8.924698
-200.490061	-5.043026	8.934695
-198.206980	1.135106	8.944691
-196.144804	2.147726	8.954688
-194.307320	-9.573673	8.964685
-192.542223	-2.738780	8.974682
-190.526061	0.975124	8.984679
-188.971362	0.501825	8.994675
-186.820780	4.061072	9.004672
-184.985660	1.358490	9.014669
-183.087782	-5.249699	9.024666
-181.150305	-6.142754	9.034663
-179.624260	-1.680434	9.044659
-177.590366	-3.616002	9.054656
-175.500955	-0.395630	9.064653
-173.740082	-5.768984	9.074650
-172.093018	-3.533110	9.084647
-170.103017	-0.349041	9.094643
-168.021722	-3.598524	9.104640
-166.002966	-3.696903	9.114637
-164.466751	-0.500613	9.124634
-162.425134	0.234945	9.134631
-160.586695	-2.134635	9.144627
-158.755212	1.900254	9.154624
-156.605619	1.765214	9.164621
-155.006504	0.154784	9.174618
-153.251694	-4.526688	9.184615
-151.343514	-0.896608	9.194611
-149.314624	1.254034	9.204608
-147.890019	3.616202	9.214605
-145.718681	-5.543349	9.224602
-143.991351	1.111504	9.234599
-141.730059	2.670574	9.244595
-139.938208	7.609803	9.254592
-138.280570	4.893805	9.264589
-136.057603	1.499498	9.274586
-134.192646	5.210510	9.284583
-132.382494	4.494234	9.294579
-130.645920	2.795029	9.304576
-128.771615	7.013478	9.314573
-126.841369	-0.580377	9.324570
-125.088822	12.865894	9.334567
-123.257830	12.449968	9.344563
-120.982431	6.830701	9.354560
-119.368705	4.578714	9.364557
-117.674389	7.970417	9.374554
-115.723360	14.909819	9.384551
-113.611345	10.348109	9.394547
-111.731740	9.062282	9.404544
-110.131843	8.661882	9.414541
-108.218632	7.641806	9.424538
-106.006556	17.652724	9.434535
-104.196424	13.891720	9.444531
-102.764870	13.026171	9.454528
-100.734841	14.322977	9.464525
-98.708666	10.435213	9.474522
-96.691744	5.536496	9.484519
-94.891108	13.267230	9.494515
-93.137285	12.454315	9.504512
-91.230124	6.302617	9.514509
-89.499402	5.926427	9.524506
-87.492544	10.028500	9.534503
-85.622157	14.646811	9.544499
-83.447576	10.420199	9.554496
-81.915296	8.839434	9.564493
-80.256656	8.659382	9.574490
-78.138321	7.203791	9.584487
-75.925589	9.916558	9.594483
-74.332891	9.707504	9.604480
-72.347617	9.431133	9.614477
-70.539131	9.502832	9.624474
-68.711671	9.870851	9.634471
-66.896107	11.939549	9.644467
-65.019780	10.302955	9.654464
-63.187378	9.683275	9.664461
-61.269124	1.653598	9.674458
-59.215265	2.054333	9.684455
-57.409712	10.466778	9.694451
-55.552218	11.870257	9.704448
-53.733982	9.300643	9.714445
-51.523693	11.220643	9.724442
-49.837865	13.418698	9.734439
-48.507116	6.610596	9.744435
-46.164308	7.453439	9.754432
-44.155487	8.385961	9.764429
-42.460181	9.640198	9.774426
-40.541627	13.850312	9.784423
-38.680607	5.700033	9.794419
-36.786309	3.754867	9.804416
-35.307976	8.381933	9.814413
-32.964187	7.367891	9.824410
-30.919374	13.810277	9.834407
-29.289122	6.077396	9.844403
-27.428564	8.429274	9.854400
-25.510566	5.238280	9.864397
-23.894279	4.150982	9.874394
-21.834263	7.123139	9.884391
-19.775438	6.163894	9.894387
-17.778883	13.001081	9.904384
-16.231260	8.782010	9.914381
-14.355695	5.928697	9.924378
-12.518111	7.575503	9.934375
-10.457609	18.195016	9.944371
-8.603565	11.803467	9.954368
-6.760909	6.180197	9.964365
-4.828513	7.179194	9.974362
-3.498056	26.036493	9.984359
-2.604767	55.870047	9.994355
-1.110786	121.747741	10.004352
0.000000	158.815548	10.009357
0.397601	201.683307	10.014362
0.874867	230.517986	10.019367
1.612912	259.526283	10.024371
1.818042	293.711554	10.029376
2.547566	307.928172	10.034381
2.475676	328.267729	10.039386
3.143348	341.385035	10.044391
3.117809	356.043779	10.049395
3.162548	361.922577	10.054400
3.132592	363.413455	10.059405
3.224243	361.480209	10.064410
3.470849	369.502856	10.069415
3.400825	381.090042	10.074419
3.671744	395.681020	10.079424
4.052005	394.842579	10.084429
4.010162	404.572528	10.089434
3.852515	395.800464	10.094439
4.043737	411.179167	10.099443
4.023209	395.181123	10.104448
3.821434	381.673278	10.109453
3.740453	388.077699	10.114458
4.575317	399.506194	10.119463
4.221622	388.259300	10.124467
3.667220	389.286704	10.129472
4.286587	398.558686	10.134477
4.398571	410.827158	10.139482
4.567662	406.723085	10.144487
4.455044	392.990741	10.149491
4.243514	393.621475	10.154496
4.312826	400.388933	10.159501
4.379442	401.472483	10.164506
3.982819	403.853173	10.169511
4.183864	411.718266	10.174515
4.548690	427.539700	10.179520
5.014025	435.390278	10.184525
4.614436	437.297816	10.189530
4.819656	436.114401	10.194535
4.990107	439.079549	10.199539
4.667930	444.144219	10.204544
5.192000	447.091763	10.209549
4.987717	447.791912	10.214554
4.915739	446.320511	10.219559
4.680986	448.181236	10.224563
4.719735	450.804245	10.229568
5.102698	452.762338	10.234573
4.728147	460.460105	10.239578
4.944431	446.037002	10.244583
5.079231	448.401183	10.249587
4.691716	457.322441	10.254592
4.971733	457.010377	10.259597
5.176782	461.053504	10.264602
5.052169	467.896477	10.269607
5.394899	472.351774	10.274611
5.153496	476.919069	10.279616
5.514942	476.083457	10.284621
4.930317	483.494371	10.289626
5.594337	482.779767	10.294631
5.190660	491.839599	10.299635
5.441901	492.204287	10.304640
5.392541	483.852538	10.309645
5.438950	488.805078	10.314650
5.927645	505.311908	10.319655
5.932417	514.246459	10.324659
5.795391	520.675544	10.329664
6.269105	515.675688	10.334669
5.859758	512.662706	10.339674
5.985353	503.509264	10.344679
5.834949	510.987445	10.349683
5.936930	530.885363	10.354688
6.091501	526.519678	10.359693
6.175046	527.260082	10.364698
5.925285	525.109048	10.369703
6.358516	531.473518	10.374707
6.103872	529.992773	10.379712
6.597129	529.500466	10.384717
6.387588	534.961102	10.389722
6.418276	534.582843	10.394727
6.371381	541.555412	10.399731
6.083456	533.319143	10.404736
6.628961	532.628016	10.409741
6.380368	535.913314	10.414746
6.490183	537.694443	10.419751
6.433437	534.126017	10.424755
6.391784	552.857708	10.429760
6.626994	562.779455	10.434765
6.778879	563.285123	10.439770
6.819052	569.677531	10.444775
6.971123	575.989967	10.449779
7.212923	575.605903	10.454784
7.400879	558.620262	10.459789
7.244665	570.895767	10.464794
6.945094	574.376914	10.469799
7.145881	578.153179	10.474803
6.931554	585.419336	10.479808
7.037713	578.485961	10.484813
7.143092	575.938116	10.489818
7.076133	579.193070	10.494823
7.322759	580.628651	10.499827
7.370826	587.393517	10.504832
7.392466	582.303788	10.509837
7.449740	581.846366	10.514842
7.682789	587.516126	10.519847
7.761088	588.038754	10.524851
7.374323	591.487488	10.529856
7.640449	593.971670	10.534861
7.697434	599.878853	10.539866
7.593104	593.446153	10.544871
7.600762	598.009068	10.549875
7.664704	602.824432	10.554880
8.168177	599.513215	10.559885
8.013915	611.552766	10.564890
7.635872	597.622205	10.569895
7.694278	608.262697	10.574899
8.031772	624.665713	10.579904
8.518556	617.650875	10.584909
8.457345	624.370548	10.589914
8.136689	625.198023	10.594919
8.070876	631.361529	10.599923
8.184454	626.642460	10.604928
8.310445	630.186438	10.609933
8.211406	636.718791	10.614938
8.020813	639.736804	10.619943
8.179810	635.715321	10.624947
8.228971	641.464786	10.629952
8.406182	625.864432	10.634957
8.514479	629.467889	10.639962
8.167150	635.790978	10.644967
8.549474	642.093172	10.649971
8.589113	648.334523	10.654976
9.112401	651.043825	10.659981
9.154863	662.937583	10.664986
8.715902	655.289633	10.669991
9.330294	643.777488	10.674995
8.705150	644.167711	10.680000
8.647843	645.613570	10.685005
9.052784	655.288779	10.690010
8.874479	664.514143	10.695015
9.378404	661.164547	10.700019
9.510582	661.581627	10.705024
9.150070	667.693836	10.710029
9.243278	678.463011	10.715034
9.189527	671.315439	10.720039
9.011874	661.454049	10.725043
8.982268	667.056770	10.730048
9.022269	665.221551	10.735053
8.884378	676.481127	10.740058
9.114668	670.157597	10.745063
9.966462	678.240450	10.750067
9.365416	679.114820	10.755072
9.756550	685.205920	10.760077
9.844029	686.396437	10.765082
10.115220	675.926381	10.770087
10.250596	666.052368	10.775091
9.956784	672.332350	10.780096
10.231548	662.213393	10.785101
10.139803	671.148399	10.790106
9.964683	668.178513	10.795111
9.928272	660.065233	10.800115
9.699577	678.364946	10.805120
10.177063	668.466615	10.810125
9.688718	673.330907	10.815130
9.722103	673.031128	10.820135
9.778993	674.438068	10.825139
9.527147	705.229781	10.830144
10.255227	700.222568	10.835149
10.253246	701.610789	10.840154
10.380774	706.991586	10.845159
10.291043	694.134112	10.850163
10.647426	703.227954	10.855168
10.722153	694.266671	10.860173
10.283822	695.749444	10.865178
10.442321	697.773292	10.870183
10.551561	687.295866	10.875187
10.102591	701.374655	10.880192
10.872173	705.888672	10.885197
11.091095	721.116489	10.890202
10.729332	715.664569	10.895207
10.819953	702.324596	10.900211
10.946402	711.903120	10.905216
11.392887	721.912294	10.910221
10.845189	709.703318	10.915226
11.185279	707.126262	10.920231
10.989126	698.380760	10.925235
11.258958	706.309206	10.930240
11.093320	697.299531	10.935245
11.413326	707.532876	10.940250
11.345893	702.855083	10.945255
11.322656	699.128902	10.950259
11.367518	708.029455	10.955264
11.432485	693.835748	10.960269
11.122892	706.403704	10.965274
11.478182	716.835871	10.970279
11.946086	723.384735	10.975283
11.634871	723.993890	10.980288
11.630835	709.114910	10.985293
11.622659	707.715832	10.990298
11.671639	717.743818	10.995303
11.717843	725.412992	11.000307
11.710455	731.789542	11.005312
11.932336	718.670202	11.010317
11.958268	732.065632	11.015322
12.097603	727.727371	11.020327
12.263801	730.421732	11.025331
12.008446	726.801263	11.030336
12.175353	713.044394	11.035341
11.980486	717.724961	11.040346
11.820548	729.550844	11.045351
11.849841	737.213450	11.050355
12.160967	733.353354	11.055360
12.131742	727.486789	11.060365
11.935120	736.749677	11.065370
12.085387	738.274030	11.070375
12.443165	732.765442	11.075379
11.923333	738.396979	11.080384
12.236959	733.472265	11.085389
12.468138	751.115331	11.090394
12.830299	765.717459	11.095399
12.958076	765.598858	11.100403
12.485800	753.472046	11.105408
12.909599	745.001530	11.110413
12.701134	744.655982	11.115418
12.701483	742.835052	11.120423
13.188662	751.899786	11.125427
12.773171	753.044312	11.130432
12.841199	751.512956	11.135437
13.080874	766.214637	11.140442
12.954369	774.795669	11.145447
13.131890	770.104671	11.150451
13.248107	780.614582	11.155456
13.590562	767.732286	11.160461
12.951729	761.450766	11.165466
12.893256	760.494905	11.170471
13.413657	769.360535	11.175475
13.233563	782.090687	11.180480
12.789245	777.738013	11.185485
12.868327	778.678139	11.190490
12.985552	774.844963	11.195495
13.314927	777.456882	11.200499
12.843274	783.605955	11.205504
13.509000	783.236437	11.210509
13.517343	787.563637	11.215514
13.819182	795.535982	11.220519
13.958570	790.160738	11.225523
13.875120	794.052106	11.230528
14.160245	792.271553	11.235533
14.137145	795.384034	11.240538
13.973404	782.855355	11.245543
14.090278	779.394864	11.250547
13.699119	773.782571	11.255552
13.951715	778.201308	11.260557
13.869116	795.540203	11.265562
14.004513	802.296899	11.270567
14.116157	795.388539	11.275571
14.085008	807.653839	11.280576
13.973800	799.301868	11.285581
14.339398	807.259340	11.290586
14.092834	805.211137	11.295591
14.199372	798.992457	11.300595
14.040661	815.842722	11.305600
14.385326	800.416374	11.310605
14.243055	811.258778	11.315610
14.249702	819.595560	11.320615
14.905548	825.074496	11.325619
14.387485	836.983573	11.330624
14.961532	821.438139	11.335629
14.651898	832.296228	11.340634
14.573413	832.828773	11.345639
14.959635	838.852883	11.350643
14.675600	836.875048	11.355648
15.242766	831.596178	11.360653
15.328445	839.523110	11.365658
14.597670	826.772675	11.370663
15.095673	826.334811	11.375667
14.852033	836.673568	11.380672
15.097793	823.900567	11.385677
15.236722	828.030127	11.390682
15.319056	830.773226	11.395687
15.616444	821.949349	11.400691
15.429223	830.577531	11.405696
15.774955	825.551759	11.410701
15.888059	826.043955	11.415706
15.597053	808.835431	11.420711
15.889171	802.550983	11.425715
15.336993	797.107998	11.430720
15.440336	799.254604	11.435725
15.266806	797.390851	11.440730
15.307486	803.818004	11.445735
15.683777	818.004081	11.450739
15.410341	829.117667	11.455744
15.780091	830.469005	11.460749
15.644473	839.879782	11.465754
15.733900	827.230293	11.470759
15.751038	827.521446	11.475763
15.572431	832.708858	11.480768
15.800675	830.459244	11.485773
15.587299	836.428662	11.490778
15.512484	846.455851	11.495783
16.443110	851.757026	11.500787
15.980188	861.483274	11.505792
16.381095	854.554107	11.510797
16.449720	857.564821	11.515802
16.501573	860.199864	11.520807
16.947327	848.753589	11.525811
16.597628	835.256107	11.530816
16.743844	830.268489	11.535821
16.440422	832.351818	11.540826
16.257280	833.516905	11.545831
16.446511	821.982003	11.550835
16.207292	826.260082	11.555840
16.495696	840.339671	11.560845
16.590861	856.160017	11.565850
16.676277	862.403868	11.570855
16.906302	854.894533	11.575859
16.726789	852.802854	11.580864
16.808752	854.346825	11.585869
16.984492	864.854876	11.590874
16.951191	859.877502	11.595879
17.420641	858.500728	11.600883
17.044004	864.993142	11.605888
17.177667	864.290513	11.610893
17.280292	859.996404	11.615898
17.034924	868.784575	11.620903
17.280187	863.657203	11.625907
16.894568	870.623259	11.630912
17.199972	857.506851	11.635917
16.954726	861.784788	11.640922
16.875360	871.340674	11.645927
17.379554	857.686503	11.650931
17.238607	884.620391	11.655936
18.010955	871.858116	11.660941
18.130565	862.493519	11.665946
17.773264	857.466304	11.670951
18.130811	842.875722	11.675955
17.994447	849.089700	11.680960
18.274359	843.363505	11.685965
17.896286	844.020048	11.690970
18.066139	846.470254	11.695975
18.296642	836.957976	11.700979
17.904262	846.476727	11.705984
17.893958	840.133591	11.710989
18.239968	847.347611	11.715994
18.190115	851.910593	11.720999
18.452516	853.015473	11.726003
17.762263	854.293957	11.731008
17.958659	839.753902	11.736013
17.976702	848.445584	11.741018
17.853312	847.014932	11.746023
18.054263	848.319820	11.751027
18.026407	856.395305	11.756032
18.156586	855.366829	11.761037
18.152073	856.585763	11.766042
17.986939	877.716883	11.771047
18.451435	880.647491	11.776051
18.103093	886.553227	11.781056
18.520709	886.990451	11.786061
18.402799	892.634445	11.791066
18.556752	894.187787	11.796071
18.898566	889.821476	11.801075
18.480788	888.484717	11.806080
19.118913	884.315100	11.811085
18.591543	889.002203	11.816090
18.689004	900.864608	11.821095
19.206138	905.736967	11.826099
19.008826	910.746429	11.831104
19.448339	909.086628	11.836109
18.944012	899.522280	11.841114
19.081593	911.786363	11.846119
19.620023	906.499764	11.851123
18.975913	910.580053	11.856128
19.393988	908.243012	11.861133
19.221977	907.915682	11.866138
19.215715	911.945818	11.871143
19.291481	914.071116	11.876147
19.353269	917.512879	11.881152
19.589975	920.068869	11.886157
19.553890	922.351898	11.891162
19.433999	918.501317	11.896167
19.510365	904.981248	11.901171
19.096384	912.624417	11.906176
19.176427	908.109563	11.911181
19.621139	925.481744	11.916186
19.668480	931.590836	11.921191
19.608001	948.568875	11.926195
20.047131	948.452942	11.931200
20.368971	934.308921	11.936205
20.598125	938.698170	11.941210
20.199981	924.585236	11.946215
20.091978	911.371112	11.951219
19.861167	916.518951	11.956224
20.031631	912.118855	11.961229
20.166978	920.241390	11.966234
20.303027	925.058306	11.971239
20.201134	931.098644	11.976243
20.108210	938.607437	11.981248
20.382328	939.104003	11.986253
20.286644	942.305931	11.991258
20.149448	949.936003	11.996263
20.737355	939.209365	12.001267
20.503852	948.273834	12.006272
20.625632	941.711038	12.011277
20.718104	943.994527	12.016282
20.874168	943.955944	12.021287
20.791052	935.001060	12.026291
20.690811	946.388190	12.031296
21.084341	938.317890	12.036301
20.847901	919.954763	12.041306
20.574761	916.510981	12.046311
20.920625	901.369326	12.051315
20.572330	905.272973	12.056320
20.327758	911.886841	12.061325
20.699223	910.175945	12.066330
20.737632	915.881961	12.071335
20.678281	911.447848	12.076339
20.391008	915.001959	12.081344
20.355477	907.794707	12.086349
20.446606	905.224385	12.091354
20.368585	912.259298	12.096359
20.812694	916.614449	12.101363
20.583950	917.186576	12.106368
21.049845	909.038357	12.111373
21.249692	910.098310	12.116378
20.797128	908.276465	12.121383
21.100820	906.735477	12.126387
20.610292	911.336139	12.131392
20.390882	902.892137	12.136397
20.900426	914.465611	12.141402
20.981831	915.256927	12.146407
21.243444	909.713055	12.151411
20.838287	906.864669	12.156416
20.823268	887.640202	12.161421
20.621059	886.932791	12.166426
20.474156	892.772413	12.171431
20.620218	884.979436	12.176435
20.106059	886.783512	12.181440
20.457587	882.601852	12.186445
20.442544	886.479540	12.191450
20.486495	893.560637	12.196455
20.922750	893.318883	12.201459
20.462984	894.720875	12.206464
20.613671	881.524001	12.211469
20.702060	887.430645	12.216474
20.518548	889.630000	12.221479
20.649117	883.206640	12.226483
20.455390	895.277650	12.231488
20.553928	890.611606	12.236493
20.737859	896.244112	12.241498
20.770650	897.488626	12.246503
20.818982	892.805926	12.251507
20.824961	894.787268	12.256512
20.886673	894.660257	12.261517
20.214957	891.546133	12.266522
20.034175	892.493322	12.271527
20.456005	884.149383	12.276531
20.203497	891.094995	12.281536
20.616308	904.105296	12.286541
20.645685	923.657747	12.291546
20.346028	929.957386	12.296551
20.646588	929.794949	12.301555
20.534954	934.095787	12.306560
20.582679	923.284541	12.311565
20.626727	930.699583	12.316570
20.324313	925.637672	12.321575
20.672914	919.483228	12.326579
20.575539	926.688044	12.331584
20.390679	934.133651	12.336589
20.628483	926.859788	12.341594
20.641869	920.341638	12.346599
20.569128	929.628794	12.351603
20.641707	930.336362	12.356608
20.930435	925.997300	12.361613
21.030375	929.939758	12.366618
20.803921	919.833152	12.371623
20.769863	897.579987	12.376627
20.392166	903.424447	12.381632
20.489930	901.534297	12.386637
20.648641	901.007370	12.391642
20.951849	905.645621	12.396647
20.908202	906.570482	12.401651
20.493281	901.536159	12.406656
20.702296	905.845563	12.411661
20.553948	904.422344	12.416666
20.579228	909.999557	12.421671
20.559421	898.670175	12.426675
20.594606	906.539484	12.431680
20.588221	909.793988	12.436685
20.921981	904.181301	12.441690
20.689406	910.877979	12.446695
20.801842	905.018637	12.451699
20.550580	908.633282	12.456704
20.431898	903.749480	12.461709
20.641630	907.292190	12.466714
20.150640	912.115561	12.471719
20.557096	900.315990	12.476723
20.482645	907.227132	12.481728
20.385956	915.314843	12.486733
20.647502	908.589151	12.491738
20.306873	909.530590	12.496743
20.960735	909.559417	12.501747
20.465847	911.797557	12.506752
20.374490	910.524433	12.511757
20.387563	905.442778	12.516762
20.399819	907.044890	12.521767
20.605058	917.714102	12.526771
20.530822	931.188852	12.531776
20.636392	931.566291	12.536781
20.897089	931.093718	12.541786
20.605314	920.485157	12.546791
20.701674	913.993440	12.551795
20.111951	916.236789	12.556800
20.495786	928.138534	12.561805
20.698725	932.844117	12.566810
20.859215	941.475900	12.571815
21.340129	923.867663	12.576819
21.254728	918.855782	12.581824
21.079861	918.849466	12.586829
20.609392	917.886866	12.591834
20.435366	914.683063	12.596839
20.516740	919.364879	12.601843
20.501222	917.556913	12.606848
20.566413	913.759862	12.611853
20.677831	908.001745	12.616858
20.325883	920.003981	12.621863
20.660863	912.863068	12.626867
20.514841	916.245725	12.631872
20.629087	920.619540	12.636877
20.743934	918.154885	12.641882
20.782821	916.089303	12.646887
20.991045	912.947065	12.651891
20.627066	913.222645	12.656896
20.565203	914.677204	12.661901
20.559044	919.032584	12.666906
20.799007	922.903664	12.671911
21.133931	918.571684	12.676915
21.027530	899.885497	12.681920
20.622228	895.655967	12.686925
20.563441	885.401820	12.691930
20.372197	889.704848	12.696935
20.913638	880.182257	12.701939
20.439772	889.332904	12.706944
20.668596	889.416844	12.711949
20.979615	886.063962	12.716954
20.850716	888.011192	12.721959
20.735360	874.243761	12.726963
20.912991	888.300545	12.731968
20.365296	890.617604	12.736973
20.386901	900.320405	12.741978
20.200830	902.393491	12.746983
20.467687	886.339352	12.751987
20.493155	892.270996	12.756992
20.194107	887.075101	12.761997
20.401435	883.527237	12.767002
20.356051	884.682524	12.772007
20.372911	887.637383	12.777011
20.602379	909.172595	12.782016
20.456865	913.708576	12.787021
20.499886	918.673282	12.792026
20.555681	930.394434	12.797031
20.787175	926.434656	12.802035
20.935101	922.385788	12.807040
20.577686	911.435595	12.812045
20.628805	893.881346	12.817050
20.253801	899.969682	12.822055
20.409925	904.324471	12.827059
20.711836	922.458889	12.832064
20.528474	925.872819	12.837069
20.648473	930.980250	12.842074
20.886200	940.802335	12.847079
20.642226	906.782993	12.852083
20.218474	910.806947	12.857088
20.543855	924.456724	12.862093
20.729421	928.893707	12.867098
20.561654	924.055814	12.872103
20.535091	924.084069	12.877107
20.505479	932.578312	12.882112
20.592100	930.110205	12.887117
20.260189	927.453334	12.892122
20.412663	932.692170	12.897127
20.606806	934.545729	12.902131
20.692463	938.023273	12.907136
20.653200	934.549255	12.912141
20.658419	929.834463	12.917146
20.782046	934.089437	12.922151
20.830320	940.706791	12.927155
20.765766	941.753659	12.932160
20.742389	923.178735	12.937165
20.744933	907.780151	12.942170
20.417604	913.076378	12.947175
20.748267	899.981655	12.952179
20.756236	898.789001	12.957184
20.789614	900.904986	12.962189
21.006265	905.338212	12.967194
20.984187	905.139121	12.972199
20.715517	906.616506	12.977203
20.882845	907.130592	12.982208
20.875015	906.969321	12.987213
21.231381	899.943956	12.992218
20.772157	900.363760	12.997223
20.777765	884.006261	13.002227
20.784880	882.025078	13.007232
19.963451	875.884553	13.012237
20.483724	876.326280	13.017242
20.542326	891.323993	13.022247
20.519912	890.512334	13.027251
20.405085	907.500831	13.032256
20.159307	902.806582	13.037261
20.547091	904.881539	13.042266
20.541227	903.182840	13.047271
20.819423	894.297081	13.052275
20.264122	895.964925	13.057280
20.458251	903.765928	13.062285
20.622608	901.571862	13.067290
20.765516	901.122249	13.072295
20.641100	902.044379	13.077299
20.450865	909.303792	13.082304
20.320407	901.440193	13.087309
20.280164	905.857860	13.092314
20.324558	903.617259	13.097319
20.419756	897.124170	13.102323
20.837237	904.022807	13.107328
20.658182	908.117699	13.112333
20.788288	905.440826	13.117338
20.448364	911.399206	13.122343
20.641877	910.843417	13.127347
20.567396	911.873432	13.132352
20.193887	913.294584	13.137357
20.081807	907.219132	13.142362
20.256366	915.837831	13.147367
20.472372	928.775713	13.152371
20.834481	943.162888	13.157376
20.714763	939.369114	13.162381
20.736226	933.268782	13.167386
20.234095	927.900063	13.172391
20.695798	937.153220	13.177395
20.602901	957.116675	13.182400
20.476288	951.115540	13.187405
20.454843	949.476349	13.192410
20.698023	953.278990	13.197415
20.596618	946.726827	13.202419
20.976151	957.300657	13.207424
20.569165	940.243319	13.212429
20.744355	924.680908	13.217434
20.151636	920.731397	13.222439
20.212355	920.826792	13.227443
20.428190	947.159225	13.232448
20.572508	949.538036	13.237453
20.835446	945.189180	13.242458
20.324009	952.958814	13.247463
20.616974	946.684427	13.252467
20.507014	950.692089	13.257472
20.672662	945.742155	13.262477
20.604482	948.757791	13.267482
20.506862	946.243113	13.272487
20.485594	943.694818	13.277491
20.664742	954.492081	13.282496
20.695812	952.417177	13.287501
21.009208	951.709780	13.292506
20.686953	957.326860	13.297511
20.978812	951.287922	13.302515
20.566373	934.002975	13.307520
20.420745	925.576706	13.312525
20.469312	928.706530	13.317530
20.279716	943.168167	13.322535
20.886385	937.493677	13.327539
20.804689	950.895906	13.332544
20.690486	937.305458	13.337549
20.845360	924.330460	13.342554
20.848415	916.648039	13.347559
20.748156	920.532847	13.352563
20.360884	917.017450	13.357568
20.688600	913.834198	13.362573
20.824155	917.157525	13.367578
20.639337	922.616819	13.372583
20.567746	909.175403	13.377587
20.583227	911.498141	13.382592
20.517892	907.961495	13.387597
20.983141	915.367864	13.392602
20.840129	920.757227	13.397607
21.191728	914.227275	13.402611
21.139697	916.001461	13.407616
20.733465	905.810426	13.412621
21.016965	894.175229	13.417626
20.664566	891.323721	13.422631
20.736082	891.720420	13.427635
20.721195	888.475126	13.432640
20.644956	886.401656	13.437645
20.963334	884.873152	13.442650
20.730121	889.172718	13.447655
20.577738	883.292079	13.452659
20.456873	880.594688	13.457664
20.537177	882.733020	13.462669
20.842490	878.574284	13.467674
20.539324	888.748020	13.472679
20.971893	884.479043	13.477683
20.688832	893.182508	13.482688
20.537261	891.678527	13.487693
20.813151	889.811127	13.492698
20.706764	896.413927	13.497703
20.630902	888.964522	13.502707
20.767620	891.165024	13.507712
20.602466	899.028021	13.512717
20.723923	899.362473	13.517722
20.609741	894.710400	13.522727
20.260842	878.065140	13.527731
20.718619	885.419882	13.532736
20.327782	891.469878	13.537741
20.384454	878.636491	13.542746
20.424806	891.330514	13.547751
20.452889	894.741736	13.552755
20.362170	890.740108	13.557760
20.496952	888.345460	13.562765
20.347913	882.044252	13.567770
20.290253	898.434391	13.572775
20.548056	886.168481	13.577779
20.777648	891.015926	13.582784
20.363214	891.011212	13.587789
20.597143	890.089287	13.592794
20.333283	889.404288	13.597799
20.502248	895.127385	13.602803
20.692735	893.389100	13.607808
20.831200	890.380009	13.612813
20.898115	890.218160	13.617818
20.360128	898.650734	13.622823
20.559010	894.764845	13.627827
20.465994	896.166324	13.632832
20.667356	896.852993	13.637837
20.720441	893.778805	13.642842
20.429061	900.030434	13.647847
20.306011	893.917000	13.652851
20.481057	900.357076	13.657856
20.268882	895.687068	13.662861
20.642278	904.665218	13.667866
20.499401	921.224727	13.672871
20.740640	923.322050	13.677875
20.885063	923.139411	13.682880
20.814405	912.289655	13.687885
21.081843	894.235293	13.692890
20.393496	903.503643	13.697895
20.535344	901.776459	13.702899
20.415666	901.286211	13.707904
20.675246	902.184739	13.712909
20.528730	898.467411	13.717914
20.588584	904.359612	13.722919
20.753594	893.167097	13.727923
20.878374	892.792433	13.732928
20.492505	897.083833	13.737933
20.515395	888.339746	13.742938
20.670284	900.172173	13.747943
20.900658	897.587451	13.752947
20.596503	898.367505	13.757952
20.516767	899.669602	13.762957
20.643008	896.280900	13.767962
20.477268	897.823925	13.772967
20.437409	897.173940	13.777971
20.421586	894.865902	13.782976
20.568291	907.245259	13.787981
20.644740	894.399389	13.792986
20.505514	904.305029	13.797991
20.606053	896.127882	13.802995
20.516112	897.355545	13.808000
20.504352	905.550268	13.813005
20.739385	896.227439	13.818010
20.502753	904.106641	13.823015
20.714172	895.481802	13.828019
20.733752	902.005376	13.833024
20.571006	904.938139	13.838029
20.127296	903.479510	13.843034
20.617736	909.078809	13.848039
20.969669	899.638830	13.853043
20.735883	901.922201	13.858048
20.870324	906.132287	13.863053
21.384169	900.139386	13.868058
21.053285	902.330458	13.873063
20.844920	900.217272	13.878067
20.459280	888.782860	13.883072
20.418998	895.662876	13.888077
20.814562	903.409604	13.893082
20.398293	903.782964	13.898087
20.545477	904.543660	13.903091
20.946008	906.048015	13.908096
20.706832	892.311272	13.913101
20.603166	879.733135	13.918106
20.440661	877.014465	13.923111
20.934606	880.667515	13.928115
21.017746	881.232350	13.933120
20.950846	876.863489	13.938125
21.090286	873.178058	13.943130
20.822744	875.028664	13.948135
20.669697	866.148572	13.953139
20.770823	876.303902	13.958144
20.826337	872.754044	13.963149
20.982090	868.859372	13.968154
20.913465	870.787581	13.973159
20.376922	844.994633	13.978163
20.285139	845.810113	13.983168
20.299868	861.604783	13.988173
20.780769	876.370603	13.993178
20.508611	880.571056	13.998183
20.564407	870.024118	14.003187
20.681939	870.859763	14.008192
20.638760	873.121720	14.013210
20.554797	874.104698	14.018227
20.326034	878.625323	14.023245
20.169691	875.355875	14.028263
20.218272	872.197757	14.033280
20.254495	880.734623	14.038298
20.297969	870.296606	14.043315
20.384285	877.070440	14.048333
20.641164	889.685881	14.053351
20.667036	899.047026	14.058368
20.294137	912.168916	14.063386
21.027900	898.056781	14.068403
20.657479	905.027056	14.073421
20.769200	906.381629	14.078439
21.085885	906.353728	14.083456
20.787313	909.273628	14.088474
20.831262	906.104880	14.093491
20.570127	916.373568	14.098509
20.638575	912.354105	14.103527
20.947208	912.063000	14.108544
20.836424	915.816115	14.113562
21.149625	906.527181	14.118579
20.643383	916.051229	14.123597
20.800095	909.792865	14.128615
20.588532	910.302415	14.133632
20.577996	915.229759	14.138650
20.834743	922.452375	14.143667
21.121607	944.279868	14.148685
21.047924	946.622991	14.153703
21.022072	948.075570	14.158720
21.151400	956.945357	14.163738
21.115827	938.614796	14.168755
21.066890	950.917342	14.173773
21.069062	956.883142	14.178791
21.154741	951.680713	14.183808
21.089097	954.945750	14.188826
21.216438	947.973067	14.193843
20.878962	946.569036	14.198861
21.145073	953.824710	14.203879
20.890387	947.769948	14.208896
21.108160	954.449225	14.213914
21.407828	952.722551	14.218931
21.316918	948.732764	14.223949
21.330647	946.455076	14.228967
21.365630	942.170459	14.233984
21.487620	952.573101	14.239002
21.453855	951.955243	14.244019
21.588788	951.374606	14.249037
21.487953	949.480365	14.254055
21.785534	945.963770	14.259072
21.030308	957.419243	14.264090
21.292558	953.589785	14.269107
21.537078	964.320269	14.274125
21.796848	966.965302	14.279143
21.870860	957.712230	14.284160
21.558769	953.472550	14.289178
21.795924	947.403149	14.294195
21.625105	950.565344	14.299213
21.523089	947.584617	14.304231
21.669230	941.846986	14.309248
21.436479	953.525100	14.314266
21.420149	961.959990	14.319283
21.618965	968.922071	14.324301
21.663216	983.989566	14.329319
22.037685	980.774370	14.334336
21.941440	986.464514	14.339354
22.365526	977.895161	14.344371
22.525234	956.236380	14.349389
22.395964	946.455925	14.354407
22.366776	944.332850	14.359424
22.216118	958.810075	14.364442
21.804089	947.972513	14.369459
21.761393	936.279455	14.374477
22.006541	949.255641	14.379495
22.105771	941.736956	14.384512
21.892164	945.978999	14.389530
21.963771	946.760099	14.394547
22.145161	945.295061	14.399565
21.828523	953.057371	14.404583
22.208408	950.263722	14.409600
21.984981	950.850509	14.414618
22.013252	947.788384	14.419635
22.165673	942.921389	14.424653
21.859894	951.007449	14.429671
22.066634	943.247873	14.434688
22.017608	950.092980	14.439706
21.793209	945.281930	14.444723
21.551433	955.615833	14.449741
21.284320	954.011141	14.454759
21.936529	963.290134	14.459776
21.911672	979.052985	14.464794
21.915752	984.842865	14.469811
21.920524	986.549664	14.474829
21.895532	985.420422	14.479847
22.108151	991.920271	14.484864
22.067317	986.034748	14.489882
22.557627	981.141306	14.494899
22.245237	986.620461	14.499917
22.104498	993.097819	14.504935
22.552800	1000.885310	14.509952
22.703846	1011.364511	14.514970
22.750750	993.651680	14.519987
22.830654	984.738551	14.525005
22.432406	975.707001	14.530023
22.848741	971.373921	14.535040
22.533168	982.473697	14.540058
22.554216	981.727927	14.545075
22.693748	983.129317	14.550093
22.721497	978.143125	14.555111
22.962753	982.638315	14.560128
22.533725	983.173735	14.565146
22.803194	975.757743	14.570163
22.661682	976.216699	14.575181
22.346322	985.876970	14.580199
22.522571	978.619884	14.585216
22.387747	981.727879	14.590234
22.808621	979.145322	14.595251
22.819797	977.221242	14.600269
22.628889	981.900379	14.605287
22.883210	972.032878	14.610304
22.519128	985.849035	14.615322
22.633004	992.410305	14.620339
22.567991	999.989722	14.625357
22.815009	1008.058202	14.630375
23.017706	1005.786297	14.635392
23.159127	1006.243597	14.640410
22.976325	1016.695391	14.645427
23.068872	1008.758891	14.650445
22.757854	1012.158143	14.655463
23.234369	999.568871	14.660480
23.027401	1008.927875	14.665498
23.010712	1011.675438	14.670515
23.316306	1004.649725	14.675533
23.112732	1016.216970	14.680551
23.223198	1011.168551	14.685568
23.166480	1008.895451	14.690586
23.181616	1017.268279	14.695603
23.325380	1006.506260	14.700621
23.092037	1004.699303	14.705639
23.435122	997.111219	14.710656
23.467146	988.045262	14.715674
23.163459	984.009659	14.720691
23.333283	980.896484	14.725709
23.007854	986.477882	14.730727
22.968281	996.735014	14.735744
23.286648	1001.833174	14.740762
23.322327	1011.673841	14.745779
23.431790	1007.027593	14.750797
23.376701	1013.790296	14.755815
23.446203	1015.206058	14.760832
23.401375	1020.323579	14.765850
23.183178	1008.829074	14.770867
23.691208	1005.692948	14.775885
23.195580	1011.586628	14.780903
23.590229	1009.436153	14.785920
23.482917	1013.839530	14.790938
23.469986	1008.655565	14.795955
23.720903	1006.503354	14.800973
23.272952	1017.970758	14.805991
23.323080	1010.713626	14.811008
23.616876	1014.695056	14.816026
23.333987	1006.469754	14.821043
23.673348	1007.720340	14.826061
23.332685	1016.568768	14.831079
23.658275	1027.820474	14.836096
23.458384	1041.156921	14.841114
23.592539	1042.078100	14.846131
23.875013	1034.453143	14.851149
24.283869	1041.618237	14.856167
24.200612	1026.668833	14.861184
24.059233	1010.467113	14.866202
23.953096	1005.738530	14.871219
24.099273	1002.027395	14.876237
23.767585	1005.104576	14.881255
23.971435	1001.568210	14.886272
23.834203	1008.962362	14.891290
23.681258	1006.450625	14.896307
23.983175	1000.204733	14.901325
23.758017	1003.409722	14.906343
23.860374	1010.968323	14.911360
23.828787	1024.304641	14.916378
24.095210	1024.064475	14.921395
24.100011	1028.602189	14.926413
24.050149	1035.115955	14.931431
23.998115	1024.787524	14.936448
24.256737	1031.094843	14.941466
24.349323	1037.320388	14.946483
24.206698	1020.290464	14.951501
24.018191	1033.152871	14.956519
24.145794	1028.662572	14.961536
24.376848	1032.162602	14.966554
24.332659	1041.584274	14.971571
24.271160	1032.974122	14.976589
24.217604	1034.378306	14.981607
24.943378	1032.395874	14.986624
24.754660	1032.955452	14.991642
24.729118	1033.775656	14.996659
24.546121	1017.998023	15.001677
24.376819	1004.797376	15.006695
24.003846	1009.871149	15.011712
24.395999	1026.045655	15.016730
24.561828	1027.870131	15.021747
24.791533	1026.702334	15.026765
24.572405	1034.032581	15.031783
24.574085	1031.315576	15.036800
24.876983	1036.368758	15.041818
24.561642	1038.643871	15.046835
24.793200	1026.840332	15.051853
24.594197	1023.009621	15.056871
24.344534	1027.871299	15.061888
24.968857	1028.611578	15.066906
24.654369	1033.747777	15.071923
25.027626	1028.862184	15.076941
24.790077	1035.341197	15.081959
24.972851	1028.268416	15.086976
24.823645	1019.131144	15.091994
24.340995	1022.772440	15.097011
25.028592	1028.463255	15.102029
24.806477	1032.329587	15.107047
24.760527	1035.791279	15.112064
24.576012	1029.183863	15.117082
24.469238	1042.356697	15.122099
24.486855	1029.554327	15.127117
24.341824	1034.224433	15.132135
24.465339	1043.277956	15.137152
24.690044	1058.315371	15.142170
24.428165	1065.228521	15.147187
25.046732	1061.747030	15.152205
25.101254	1068.444897	15.157223
25.049078	1059.450427	15.162240
25.169894	1058.054429	15.167258
24.754986	1060.195424	15.172275
25.400698	1060.325299	15.177293
24.756207	1061.998534	15.182311
25.205192	1063.328368	15.187328
25.490040	1058.502810	15.192346
25.150526	1068.001906	15.197363
25.537217	1060.660271	15.202381
25.375900	1062.842440	15.207399
25.492556	1053.529633	15.212416
25.323575	1063.488500	15.217434
25.330483	1057.645950	15.222451
25.817663	1066.775728	15.227469
25.336209	1066.683870	15.232487
25.359728	1061.556240	15.237504
25.665234	1058.505620	15.242522
25.233943	1064.696185	15.247539
25.347503	1068.382523	15.252557
25.594079	1073.451674	15.257575
25.449839	1062.381883	15.262592
25.786086	1061.007614	15.267610
25.656293	1064.957345	15.272627
25.830909	1062.257537	15.277645
25.475977	1066.834497	15.282663
25.246581	1072.304571	15.287680
25.655980	1076.574094	15.292698
25.998646	1085.286501	15.297715
26.055178	1067.848727	15.302733
26.005905	1064.680969	15.307751
25.916596	1064.492346	15.312768
25.923665	1063.836377	15.317786
25.776640	1058.584828	15.322803
26.003501	1059.491688	15.327821
25.771270	1062.545134	15.332839
25.998769	1059.129907	15.337856
25.978072	1053.409029	15.342874
25.858876	1060.637109	15.347891
25.909738	1054.344864	15.352909
25.997225	1059.828323	15.357927
25.664457	1060.703567	15.362944
25.624726	1060.653305	15.367962
26.056713	1080.232318	15.372979
26.185213	1079.978001	15.377997
26.405050	1086.575479	15.383015
26.560344	1075.442904	15.388032
26.691388	1062.706499	15.393050
26.169651	1052.542841	15.398067
26.183243	1047.437392	15.403085
26.382499	1045.432233	15.408103
26.016720	1045.991852	15.413120
26.185186	1044.940467	15.418138
26.363580	1052.654961	15.423155
26.662516	1039.269271	15.428173
26.612113	1045.801640	15.433191
26.713713	1045.401925	15.438208
26.738252	1042.403419	15.443226
26.619910	1050.414082	15.448243
26.435351	1051.219422	15.453261
26.382893	1046.645416	15.458279
26.292625	1052.224315	15.463296
26.506744	1044.636666	15.468314
26.290223	1049.450932	15.473331
26.294663	1047.026780	15.478349
26.351787	1047.545782	15.483367
26.064770	1050.840132	15.488384
26.265367	1048.242179	15.493402
26.505876	1054.834918	15.498419
26.421205	1062.478370	15.503437
26.584950	1081.843515	15.508455
26.450152	1085.705914	15.513472
27.055537	1074.246937	15.518490
27.123524	1082.593414	15.523507
27.053223	1073.257922	15.528525
26.740986	1069.704901	15.533543
26.789079	1081.190853	15.538560
27.343837	1077.894722	15.543578
26.875374	1064.023609	15.548595
26.787158	1055.628672	15.553613
26.880938	1054.133365	15.558631
26.592166	1058.967897	15.563648
27.174815	1068.536854	15.568666
27.327466	1080.105279	15.573683
27.393229	1060.024785	15.578701
27.279285	1045.712167	15.583719
27.026266	1049.581046	15.588736
27.395467	1048.293655	15.593754
27.231245	1051.038960	15.598771
26.934519	1047.312799	15.603789
26.958038	1047.777716	15.608807
26.801410	1048.764108	15.613824
27.081021	1061.145065	15.618842
27.223454	1074.774055	15.623859
27.092673	1089.166491	15.628877
27.026614	1081.711907	15.633895
27.133779	1092.374685	15.638912
27.209615	1082.756631	15.643930
27.108385	1085.769115	15.648947
26.957342	1086.124189	15.653965
27.088237	1083.839385	15.658983
26.883639	1086.565238	15.664000
27.221263	1089.661154	15.669018
27.338737	1100.362330	15.674035
27.346957	1103.715529	15.679053
27.503362	1097.771734	15.684071
27.727347	1104.158256	15.689088
27.655243	1093.880074	15.694106
27.590894	1103.486356	15.699123
27.732537	1102.015124	15.704141
27.707512	1097.099759	15.709159
27.980313	1097.750694	15.714176
28.129608	1090.437149	15.719194
27.745035	1096.777603	15.724211
27.752826	1092.950792	15.729229
27.737730	1081.299353	15.734247
27.447651	1089.550128	15.739264
27.857339	1088.755830	15.744282
28.132156	1090.347831	15.749299
27.846521	1103.686432	15.754317
27.944490	1097.605402	15.759335
28.028516	1103.700541	15.764352
27.937322	1094.861964	15.769370
27.699536	1094.664149	15.774387
27.792190	1101.587400	15.779405
27.980377	1094.467201	15.784423
27.921217	1105.958567	15.789440
28.036629	1093.260647	15.794458
27.943875	1098.770299	15.799475
28.187310	1094.862137	15.804493
28.276965	1095.146411	15.809511
27.856368	1104.776764	15.814528
28.304530	1089.150706	15.819546
28.067296	1103.453918	15.824563
28.132178	1105.161055	15.829581
28.292506	1094.553628	15.834599
28.183649	1103.689945	15.839616
28.459871	1104.111536	15.844634
28.162406	1103.099087	15.849651
28.300083	1105.879653	15.854669
28.451957	1103.767248	15.859687
28.307196	1102.431349	15.864704
28.613831	1095.440065	15.869722
28.559141	1102.076744	15.874739
28.307845	1107.966759	15.879757
28.712577	1102.380811	15.884775
28.933802	1106.879471	15.889792
28.798119	1102.494928	15.894810
28.666962	1098.760448	15.899827
28.682942	1104.257759	15.904845
28.930414	1107.336455	15.909863
28.735132	1109.366566	15.914880
28.711047	1107.019741	15.919898
28.931700	1105.355421	15.924915
28.802649	1105.142113	15.929933
28.612175	1103.402603	15.934951
28.577544	1106.330438	15.939968
28.553012	1106.259852	15.944986
28.707817	1110.252539	15.950003
28.228893	1113.823132	15.955021
28.841503	1130.094604	15.960039
28.491522	1137.386700	15.965056
28.929608	1127.602957	15.970074
28.663925	1126.368898	15.975091
28.857227	1137.545326	15.980109
28.959769	1130.126384	15.985127
29.221773	1132.440722	15.990144
28.959707	1135.152026	15.995162
29.013757	1132.980398	16.000179
28.639831	1131.653077	16.005197
29.023303	1144.060785	16.010215
29.074268	1152.155079	16.015232
29.265313	1148.215332	16.020250
29.641698	1146.914889	16.025267
29.551316	1144.514460	16.030285
29.553576	1125.900005	16.035303
29.206350	1126.460382	16.040320
29.351118	1118.019165	16.045338
29.663641	1115.052377	16.050355
29.255503	1115.387746	16.055373
29.397674	1118.869962	16.060391
29.568579	1112.052742	16.065408
29.614563	1117.466954	16.070426
29.665837	1117.903096	16.075443
29.659468	1114.280692	16.080461
29.873623	1110.160600	16.085479
29.327482	1120.338906	16.090496
29.111764	1125.849176	16.095514
29.523696	1138.278380	16.100531
29.671749	1155.538658	16.105549
29.635066	1155.503228	16.110567
29.886237	1156.495304	16.115584
29.697318	1145.206718	16.120602
29.857266	1147.000717	16.125619
29.911808	1151.593723	16.130637
29.964043	1142.424203	16.135655
30.085539	1156.460823	16.140672
29.919239	1150.527846	16.145690
30.182493	1146.475317	16.150707
29.994040	1137.356123	16.155725
30.298692	1123.308698	16.160743
30.322811	1121.108343	16.165760
30.188166	1110.833785	16.170778
30.106296	1116.786888	16.175795
29.899014	1118.301301	16.180813
29.908673	1116.917663	16.185831
29.818465	1117.609184	16.190848
29.234762	1135.647316	16.195866
29.905175	1138.483017	16.200883
29.901318	1143.038785	16.205901
29.780832	1145.026154	16.210919
30.110395	1160.342957	16.215936
30.187771	1153.347251	16.220954
30.135199	1159.650493	16.225971
30.243568	1177.918469	16.230989
30.433911	1174.245393	16.236007
30.517952	1183.196702	16.241024
30.509387	1184.977862	16.246042
30.615385	1179.995515	16.251059
30.491080	1177.541836	16.256077
30.579502	1175.380847	16.261095
30.746850	1182.422834	16.266112
30.510539	1163.046810	16.271130
30.798560	1161.575281	16.276147
31.017842	1159.116244	16.281165
30.983682	1146.469518	16.286183
30.865942	1153.243417	16.291200
30.912882	1150.819442	16.296218
30.658379	1145.742997	16.301235
30.907562	1153.424536	16.306253
30.828524	1144.222400	16.311271
30.654042	1148.448340	16.316288
30.700666	1147.140651	16.321306
30.576554	1146.792233	16.326323
30.349299	1154.920451	16.331341
30.802303	1164.084495	16.336359
30.965813	1171.188558	16.341376
31.140256	1182.020586	16.346394
31.277650	1176.445012	16.351411
31.165564	1175.929950	16.356429
31.064126	1179.095257	16.361447
31.189790	1174.195373	16.366464
31.023092	1178.610947	16.371482
31.331111	1176.082751	16.376499
31.022279	1176.785379	16.381517
31.010236	1171.053917	16.386535
31.037357	1178.845596	16.391552
30.751741	1184.319835	16.396570
31.200133	1173.149537	16.401587
30.857703	1180.339168	16.406605
31.396969	1171.613730	16.411623
31.091992	1179.258789	16.416640
31.014519	1180.787175	16.421658
31.388644	1187.071211	16.426675
31.333063	1200.649214	16.431693
31.410864	1200.360278	16.436711
31.682947	1198.593422	16.441728
31.504852	1201.421060	16.446746
31.933130	1195.163663	16.451763
31.630428	1205.911360	16.456781
31.857676	1201.131070	16.461799
31.731077	1203.590793	16.466816
31.525133	1201.636583	16.471834
31.958698	1199.673128	16.476851
31.600323	1198.102957	16.481869
31.679230	1201.412558	16.486887
31.758838	1208.133352	16.491904
31.574941	1209.205932	16.496922
31.678366	1203.966909	16.501939
31.543434	1206.429243	16.506957
31.653341	1201.756086	16.511975
31.348353	1202.705320	16.516992
31.756057	1211.642101	16.522010
31.891773	1212.764615	16.527027
32.086583	1233.485367	16.532045
32.336286	1229.997000	16.537063
32.430018	1218.672891	16.542080
31.863770	1219.038521	16.547098
32.285199	1216.929888	16.552115
32.645072	1217.487941	16.557133
32.276724	1206.420642	16.562151
32.222441	1205.886612	16.567168
32.048476	1201.336937	16.572186
32.287359	1195.227377	16.577203
32.292681	1208.244505	16.582221
32.179599	1223.459297	16.587239
32.592420	1228.001527	16.592256
31.985921	1231.191229	16.597274
32.457578	1226.479666	16.602291
32.829582	1230.071727	16.607309
32.758282	1234.388276	16.612327
32.640399	1230.990887	16.617344
32.534035	1236.665927	16.622362
32.239234	1227.929512	16.627379
32.418230	1236.340511	16.632397
32.250201	1230.626322	16.637415
32.937037	1230.807817	16.642432
32.645782	1233.316250	16.647450
32.910498	1224.978042	16.652467
32.744403	1232.790276	16.657485
32.720292	1227.447510	16.662503
32.667133	1228.566579	16.667520
32.383846	1233.703400	16.672538
32.487352	1228.024947	16.677555
32.592204	1237.562140	16.682573
32.888797	1247.876771	16.687591
33.444926	1249.244163	16.692608
33.088110	1259.367655	16.697626
33.092275	1252.727400	16.702643
33.206263	1257.052348	16.707661
33.078410	1249.266123	16.712679
33.216391	1250.472904	16.717696
33.312400	1255.514382	16.722714
33.719972	1240.689691	16.727731
33.166469	1230.847530	16.732749
33.086919	1227.531373	16.737767
33.215191	1224.914686	16.742784
33.312940	1244.894550	16.747802
33.583905	1244.346491	16.752819
33.516359	1240.099845	16.757837
33.326097	1236.112845	16.762855
33.302000	1231.387845	16.767872
33.349282	1255.770061	16.772890
33.632441	1253.204380	16.777907
33.931852	1248.705430	16.782925
33.581624	1245.970369	16.787943
33.390655	1226.756191	16.792960
33.614527	1242.913709	16.797978
33.562159	1250.822999	16.802995
33.697843	1251.995526	16.808013
33.625591	1251.523636	16.813031
33.942615	1257.248544	16.818048
33.356558	1253.586508	16.823066
33.585116	1247.464130	16.828083
33.891911	1248.074989	16.833101
33.440928	1253.711476	16.838119
33.987998	1254.905209	16.843136
33.635821	1257.200450	16.848154
33.361564	1256.803356	16.853171
33.363271	1256.762919	16.858189
33.514469	1276.293069	16.863207
34.192244	1278.547168	16.868224
33.999610	1284.863845	16.873242
34.483578	1280.523416	16.878259
34.254575	1271.157924	16.883277
34.386084	1278.019469	16.888295
34.515728	1275.881322	16.893312
34.759443	1274.120109	16.898330
34.772537	1251.873008	16.903347
34.621277	1246.792609	16.908365
34.434723	1239.262931	16.913383
34.589247	1236.818922	16.918400
34.507104	1238.230388	16.923418
34.631165	1242.792996	16.928435
34.532377	1241.780333	16.933453
34.402820	1239.770891	16.938471
34.663230	1235.883408	16.943488
34.574267	1239.957296	16.948506
34.903765	1233.975504	16.953523
34.578316	1227.089385	16.958541
34.630551	1230.705167	16.963559
34.686879	1231.954690	16.968576
34.354803	1234.311840	16.973594
34.507253	1232.772990	16.978611
34.839982	1232.600989	16.983629
34.672562	1243.217634	16.988647
35.051744	1233.703002	16.993664
34.729901	1234.775217	16.998682
34.682984	1235.065192	17.003699
34.873111	1247.226188	17.008717
34.490379	1271.367168	17.013735
35.016159	1267.114071	17.018752
34.817092	1268.316038	17.023770
34.970848	1275.025329	17.028787
35.332548	1268.829323	17.033805
35.085940	1272.874732	17.038823
35.240169	1274.233468	17.043840
35.139986	1277.571823	17.048858
34.884911	1267.759975	17.053875
35.487395	1270.328584	17.058893
35.495480	1273.247946	17.063911
35.383612	1264.089166	17.068928
34.902611	1278.289045	17.073946
35.050388	1280.795446	17.078963
35.099485	1267.435860	17.083981
34.794839	1272.650771	17.088999
35.371613	1282.375213	17.094016
35.419861	1296.985593	17.099034
35.207387	1294.852946	17.104051
35.594532	1298.841676	17.109069
35.241352	1306.965969	17.114087
35.460878	1307.020876	17.119104
35.495467	1306.214889	17.124122
35.333648	1303.870782	17.129139
35.972323	1299.543197	17.134157
35.242210	1307.688413	17.139175
35.629231	1319.535760	17.144192
35.797952	1333.611691	17.149210
36.016330	1331.733939	17.154227
36.267209	1328.388274	17.159245
36.413939	1324.813201	17.164263
36.507625	1300.618965	17.169280
36.518453	1301.938504	17.174298
36.227091	1304.441061	17.179315
36.192903	1291.035492	17.184333
35.954800	1305.681195	17.189351
36.246506	1291.291714	17.194368
36.182038	1282.218899	17.199386
36.070177	1301.172868	17.204403
36.083465	1290.136541	17.209421
36.071786	1292.960861	17.214439
36.308310	1297.143934	17.219456
36.150470	1302.031689	17.224474
36.370344	1295.650915	17.229491
36.477882	1294.731232	17.234509
36.158438	1304.947567	17.239527
35.927101	1316.691463	17.244544
36.146798	1333.748299	17.249562
36.209346	1327.651596	17.254579
36.036716	1322.830371	17.259597
36.224710	1334.071636	17.264615
36.293854	1338.914186	17.269632
36.435056	1350.904893	17.274650
36.715641	1358.638636	17.279667
37.099075	1350.677289	17.284685
36.785327	1356.416278	17.289703
36.552077	1359.393964	17.294720
37.021475	1358.443734	17.299738
37.069214	1348.260989	17.304755
37.378223	1345.686530	17.309773
37.366975	1348.497006	17.314791
37.352431	1337.126016	17.319808
37.241864	1323.916209	17.324826
37.130534	1323.847904	17.329843
37.287554	1312.671946	17.334861
36.979209	1311.182957	17.339879
37.456043	1313.030529	17.344896
37.198181	1321.179830	17.349914
36.952459	1321.639731	17.354931
37.355246	1318.073124	17.359949
37.086333	1320.116280	17.364967
37.106140	1303.676757	17.369984
37.121399	1318.896411	17.375002
37.181440	1336.892125	17.380019
37.452841	1337.290532	17.385037
37.617092	1342.164025	17.390055
37.699022	1338.340191	17.395072
38.042552	1339.231004	17.400090
37.968620	1316.372689	17.405107
38.015355	1302.757943	17.410125
38.071460	1304.345729	17.415143
37.914314	1306.103949	17.420160
37.965293	1299.638734	17.425178
38.010429	1305.384290	17.430195
38.228893	1295.390438	17.435213
37.679960	1308.001846	17.440231
37.675197	1305.619786	17.445248
37.780304	1302.154225	17.450266
37.807796	1303.631552	17.455283
37.854765	1299.888926	17.460301
37.822076	1306.901482	17.465319
37.822953	1299.490834	17.470336
37.889367	1299.680270	17.475354
37.382882	1303.267442	17.480371
37.805608	1306.403934	17.485389
37.527057	1326.403928	17.490407
37.995165	1330.768191	17.495424
37.837854	1335.331820	17.500442
37.772558	1339.337891	17.505459
37.829304	1336.599972	17.510477
38.022376	1351.017052	17.515495
38.315916	1361.177544	17.520512
38.500065	1363.227286	17.525530
38.554747	1378.317393	17.530547
38.602690	1370.542703	17.535565
38.210992	1382.208620	17.540583
38.335905	1377.176900	17.545600
38.365989	1378.723088	17.550618
38.315792	1383.021885	17.555635
38.569288	1370.763101	17.560653
38.430807	1381.150841	17.565671
38.533662	1374.545586	17.570688
39.083417	1374.093832	17.575706
38.870187	1365.108292	17.580723
38.552505	1364.020148	17.585741
38.448256	1371.437953	17.590759
38.649118	1385.717102	17.595776
39.011676	1385.583691	17.600794
39.032261	1378.032212	17.605811
39.492549	1383.707011	17.610829
39.216659	1387.367275	17.615847
39.078577	1384.365873	17.620864
39.528451	1382.808695	17.625882
39.261368	1376.799988	17.630899
39.064294	1367.144684	17.635917
39.073473	1371.123032	17.640935
39.213431	1379.408900	17.645952
38.998428	1384.296243	17.650970
39.099402	1387.732429	17.655987
39.228192	1391.527267	17.661005
39.096083	1393.058347	17.666023
39.440582	1392.165360	17.671040
39.165890	1377.392549	17.676058
39.407943	1390.463345	17.681075
39.960505	1383.684911	17.686093
39.705477	1378.586036	17.691111
39.525619	1380.076872	17.696128
39.554305	1380.066458	17.701146
39.462435	1387.423481	17.706163
39.618199	1383.746047	17.711181
39.477130	1393.899571	17.716199
39.685218	1403.782980	17.721216
40.302431	1404.515051	17.726234
39.956912	1406.609152	17.731251
40.333971	1408.799071	17.736269
40.137462	1384.863141	17.741287
40.171482	1384.281679	17.746304
40.019100	1370.987260	17.751322
39.791013	1375.243320	17.756339
40.321617	1373.772310	17.761357
40.261408	1376.940431	17.766375
40.105671	1379.755211	17.771392
40.314427	1375.524548	17.776410
40.094273	1381.183320	17.781427
40.300623	1390.346477	17.786445
40.329714	1403.624286	17.791463
40.661087	1393.380676	17.796480
40.712547	1402.648358	17.801498
40.299197	1383.196891	17.806515
40.899585	1386.572256	17.811533
40.570088	1381.168400	17.816551
40.189341	1377.514444	17.821568
40.426182	1384.263086	17.826586
40.147096	1399.474618	17.831603
40.275106	1392.788264	17.836621
40.515886	1407.629542	17.841639
40.613838	1411.810812	17.846656
40.843127	1401.079925	17.851674
40.607824	1408.757248	17.856691
41.218424	1399.538699	17.861709
40.779114	1405.035822	17.866727
40.621964	1406.155802	17.871744
41.002741	1409.904291	17.876762
41.215639	1412.184961	17.881779
41.205579	1409.359262	17.886797
41.136532	1406.902373	17.891815
40.633287	1407.162705	17.896832
40.908930	1407.055614	17.901850
41.084536	1430.842425	17.906867
40.912435	1438.315205	17.911885
41.468146	1436.201634	17.916903
40.933194	1438.001019	17.921920
41.199588	1432.252041	17.926938
41.174023	1443.491808	17.931955
41.009787	1438.729350	17.936973
41.091920	1441.151354	17.941991
40.936044	1453.603746	17.947008
41.672109	1455.311999	17.952026
41.595111	1468.896664	17.957043
42.024521	1466.395253	17.962061
42.116711	1455.338982	17.967079
41.566187	1447.811758	17.972096
42.000978	1444.667237	17.977114
41.816901	1439.125032	17.982131
41.780164	1438.209208	17.987149
42.147230	1431.415703	17.992167
41.843141	1426.660295	17.997184
42.042013	1421.109531	18.002202
41.642062	1433.605330	18.007219
42.055396	1446.193612	18.012237
42.403310	1457.233121	18.017255
42.189247	1465.323407	18.022272
42.211725	1452.348580	18.027290
42.056161	1446.429005	18.032307
42.235898	1461.882042	18.037325
42.403635	1459.723558	18.042343
42.248319	1465.252333	18.047360
42.328856	1455.074133	18.052378
42.488097	1464.030035	18.057395
42.152951	1461.906585	18.062413
42.307311	1459.561005	18.067431
42.051893	1463.835949	18.072448
42.197370	1458.170691	18.077466
42.297494	1466.253571	18.082483
41.988124	1461.189578	18.087501
42.137454	1469.822347	18.092519
42.339500	1477.679469	18.097536
42.661085	1477.637343	18.102554
42.771401	1484.819574	18.107571
42.608644	1482.288573	18.112589
42.862938	1477.938647	18.117607
42.597419	1487.928904	18.122624
42.826640	1482.577659	18.127642
42.932525	1485.926402	18.132659
42.566749	1481.472528	18.137677
42.998111	1488.802888	18.142695
43.111385	1509.080066	18.147712
43.406972	1505.765679	18.152730
43.365563	1499.942272	18.157747
43.251144	1483.614951	18.162765
43.394899	1484.716027	18.167783
43.088951	1492.522050	18.172800
43.302461	1493.239475	18.177818
43.273375	1499.744754	18.182835
43.578973	1507.790064	18.187853
43.334755	1497.807687	18.192871
43.225182	1506.097030	18.197888
43.542245	1508.754779	18.202906
43.319810	1509.713500	18.207923
43.347638	1506.689141	18.212941
43.728543	1504.979193	18.217959
43.379418	1507.254652	18.222976
43.445223	1501.819596	18.227994
43.797526	1504.776058	18.233011
43.651048	1514.170272	18.238029
43.490532	1510.638778	18.243047
43.471139	1517.959023	18.248064
43.885864	1520.137776	18.253082
44.232429	1530.191245	18.258099
44.068047	1533.635159	18.263117
43.956138	1536.034535	18.268135
44.249831	1534.793128	18.273152
44.237111	1534.719333	18.278170
44.322782	1541.850692	18.283187
44.223908	1537.604612	18.288205
44.427201	1529.674454	18.293223
44.142108	1535.921641	18.298240
44.212308	1526.224745	18.303258
44.514013	1522.751415	18.308275
44.215125	1532.801759	18.313293
44.451287	1532.118304	18.318311
44.234912	1530.445002	18.323328
44.537787	1531.112064	18.328346
44.553365	1528.750501	18.333363
44.227965	1529.751289	18.338381
44.425101	1523.799563	18.343399
44.662367	1540.300012	18.348416
44.470798	1549.460613	18.353434
44.825522	1556.582862	18.358451
44.378420	1563.165743	18.363469
45.014688	1555.185356	18.368487
44.657370	1553.092075	18.373504
45.192712	1561.243314	18.378522
45.210588	1550.288309	18.383539
45.185000	1561.401773	18.388557
45.222803	1559.723870	18.393575
45.376286	1570.057346	18.398592
45.415975	1555.933689	18.403610
45.588710	1557.232579	18.408627
45.286859	1575.923360	18.413645
45.451263	1560.122627	18.418663
45.189466	1555.357959	18.423680
45.232987	1557.481057	18.428698
45.418856	1551.024899	18.433715
45.370348	1553.879599	18.438733
45.537028	1550.609354	18.443751
45.676392	1558.367410	18.448768
46.181427	1547.565128	18.453786
46.141370	1550.239620	18.458803
45.736650	1546.135354	18.463821
46.021820	1541.511584	18.468839
45.631361	1536.733938	18.473856
45.759311	1543.408396	18.478874
45.496690	1545.805264	18.483891
45.303530	1553.220286	18.488909
45.636750	1547.862608	18.493927
45.355952	1555.588357	18.498944
45.443460	1553.224695	18.503962
46.077416	1560.580597	18.508979
45.969912	1573.722504	18.513997
45.964736	1576.919029	18.519015
46.323792	1584.992619	18.524032
45.918350	1578.465765	18.529050
46.131938	1576.832532	18.534067
45.964181	1586.026478	18.539085
46.220536	1582.237648	18.544103
45.903343	1587.417408	18.549120
46.328682	1602.607192	18.554138
46.902613	1605.992261	18.559155
46.778303	1615.992645	18.564173
47.108536	1591.354602	18.569191
46.738676	1578.054769	18.574208
46.697952	1574.867722	18.579226
46.936813	1573.935745	18.584243
46.559942	1575.892313	18.589261
46.775621	1573.969715	18.594279
46.884847	1582.168430	18.599296
46.859686	1576.974559	18.604314
47.181601	1579.481472	18.609331
47.073723	1589.673137	18.614349
46.865264	1578.398217	18.619367
46.608090	1590.755869	18.624384
46.861890	1606.499140	18.629402
47.409362	1606.990790	18.634419
47.508335	1601.639787	18.639437
47.627774	1602.354840	18.644455
47.508987	1601.589310	18.649472
47.332968	1601.087951	18.654490
47.498868	1598.842352	18.659507
47.465758	1605.852358	18.664525
47.620316	1600.178405	18.669543
47.811377	1600.081090	18.674560
47.492210	1599.938563	18.679578
47.352043	1597.529274	18.684595
47.296552	1603.454021	18.689613
47.398159	1601.782892	18.694631
47.387415	1603.188842	18.699648
47.311235	1616.330139	18.704666
47.782347	1593.653592	18.709683
47.665693	1608.033452	18.714701
47.828000	1627.212099	18.719719
48.154731	1623.224558	18.724736
47.788856	1626.734932	18.729754
48.060038	1625.413510	18.734771
47.813975	1630.522027	18.739789
48.258490	1619.699754	18.744807
48.273792	1620.954767	18.749824
48.001732	1625.661395	18.754842
48.322766	1627.110475	18.759859
48.413077	1615.708311	18.764877
48.615246	1619.396913	18.769895
48.508327	1614.071756	18.774912
48.400208	1620.313834	18.779930
48.398226	1618.990422	18.784947
48.562464	1614.631879	18.789965
48.523414	1615.140615	18.794983
48.371099	1611.959306	18.800000
48.173099	1615.356634	18.805018
48.542416	1620.354915	18.810035
48.641475	1643.160182	18.815053
48.757030	1647.684599	18.820071
48.663936	1650.176053	18.825088
48.946432	1647.374963	18.830106
49.421409	1652.726441	18.835123
49.133318	1661.105929	18.840141
49.463499	1661.163522	18.845159
49.490308	1653.611631	18.850176
49.212891	1642.781607	18.855194
49.303490	1625.033006	18.860211
49.085304	1636.960340	18.865229
48.877436	1645.400089	18.870247
49.529094	1647.846541	18.875264
49.302015	1653.111671	18.880282
49.833922	1649.871712	18.885299
49.664456	1653.020427	18.890317
49.790168	1646.950177	18.895335
49.532963	1643.847481	18.900352
49.109084	1649.423941	18.905370
49.400380	1641.440445	18.910387
49.328801	1644.572376	18.915405
49.649583	1645.127700	18.920423
49.383787	1637.783875	18.925440
49.380286	1647.552913	18.930458
49.524860	1660.683567	18.935475
49.743061	1668.048196	18.940493
49.371120	1670.835915	18.945511
49.674272	1671.096985	18.950528
49.649851	1676.288396	18.955546
49.840993	1690.933313	18.960563
50.282831	1698.717148	18.965581
50.280635	1703.632679	18.970599
50.562689	1702.942924	18.975616
50.272266	1700.949977	18.980634
50.660440	1701.992625	18.985651
50.885262	1701.565075	18.990669
50.268006	1699.062744	18.995687
50.725260	1699.311568	19.000704
50.596224	1702.085996	19.005722
50.566457	1702.911290	19.010739
50.702139	1699.154540	19.015757
50.647745	1698.779586	19.020775
50.970547	1698.995944	19.025792
50.861535	1700.994408	19.030810
50.996729	1692.223776	19.035827
50.625101	1689.419461	19.040845
50.724711	1695.411361	19.045863
51.231743	1692.313470	19.050880
50.904519	1688.868004	19.055898
51.018707	1689.392207	19.060915
51.262007	1695.486258	19.065933
50.854554	1689.912567	19.070951
50.923759	1686.840130	19.075968
50.896074	1694.258741	19.080986
51.006009	1687.644660	19.086003
50.964319	1702.699235	19.091021
51.374069	1719.475062	19.096039
51.752051	1720.942737	19.101056
51.493652	1724.918227	19.106074
51.495672	1723.445283	19.111091
51.268844	1719.218334	19.116109
51.476486	1725.166131	19.121127
51.587352	1720.018191	19.126144
51.279345	1725.329114	19.131162
51.243321	1727.324124	19.136179
51.597146	1746.375976	19.141197
51.784257	1753.548315	19.146215
51.788880	1750.209739	19.151232
51.838535	1756.784312	19.156250
52.159697	1749.898529	19.161267
52.181696	1753.791302	19.166285
51.886035	1754.137321	19.171303
52.537555	1749.299086	19.176320
52.053122	1753.924433	19.181338
52.258909	1756.613510	19.186355
52.186987	1746.360066	19.191373
52.214462	1752.662029	19.196391
52.838541	1763.514234	19.201408
52.811293	1767.872596	19.206426
52.280993	1756.178260	19.211443
52.332808	1758.521643	19.216461
52.020163	1773.732991	19.221479
52.218127	1781.721691	19.226496
52.313755	1783.362601	19.231514
52.561992	1780.220469	19.236531
52.931903	1787.369357	19.241549
52.531738	1793.917905	19.246567
53.278907	1797.414673	19.251584
53.713869	1793.577845	19.256602
53.699807	1771.246855	19.261619
54.019359	1765.688273	19.266637
53.918801	1764.942446	19.271655
54.191887	1753.080448	19.276672
53.580484	1739.932137	19.281690
53.811033	1730.993148	19.286707
53.750765	1728.012200	19.291725
53.379146	1723.107630	19.296743
53.769450	1718.057861	19.301760
53.411706	1725.849255	19.306778
53.620917	1727.026537	19.311795
53.573016	1724.803402	19.316813
53.498969	1729.754885	19.321831
53.614392	1726.653253	19.326848
53.114334	1732.416446	19.331866
53.749952	1728.346783	19.336883
53.739369	1728.071810	19.341901
53.701214	1736.649853	19.346919
54.034085	1748.465469	19.351936
54.148477	1760.830031	19.356954
53.929742	1755.523210	19.361971
54.163451	1761.133046	19.366989
54.405990	1765.191579	19.372007
54.547317	1762.154405	19.377024
54.299959	1757.704954	19.382042
54.003518	1753.474969	19.387059
54.065000	1752.358407	19.392077
54.179050	1766.039724	19.397095
54.500024	1752.094857	19.402112
54.255560	1760.201138	19.407130
54.273140	1760.241453	19.412147
54.332791	1752.151536	19.417165
54.013190	1766.071789	19.422183
54.239539	1768.291538	19.427200
54.448815	1796.539814	19.432218
54.425294	1794.611344	19.437235
54.556700	1796.858400	19.442253
54.170321	1803.926700	19.447271
54.905435	1809.400583	19.452288
55.129503	1815.396785	19.457306
55.221488	1822.879596	19.462323
55.487733	1812.914236	19.467341
55.199176	1819.427515	19.472359
55.774403	1818.497705	19.477376
55.480687	1822.600156	19.482394
55.488348	1811.460082	19.487411
55.568889	1816.625669	19.492429
55.446427	1817.744849	19.497447
55.632718	1812.262254	19.502464
55.888689	1812.752309	19.507482
55.459545	1816.853170	19.512499
55.763733	1813.004109	19.517517
55.699638	1811.984673	19.522535
55.814347	1813.641608	19.527552
55.608709	1815.174704	19.532570
55.749490	1823.355536	19.537587
55.825303	1819.543265	19.542605
55.558836	1813.840620	19.547623
55.972409	1818.608910	19.552640
55.645386	1816.922260	19.557658
55.388129	1828.427251	19.562675
55.338821	1840.320668	19.567693
55.368268	1850.188133	19.572711
55.986952	1860.922025	19.577728
56.036831	1861.566329	19.582746
55.936486	1864.971380	19.587763
56.739901	1857.581555	19.592781
56.485283	1865.086011	19.597799
56.577998	1855.162581	19.602816
56.521283	1857.343068	19.607834
56.714751	1860.964707	19.612851
57.037049	1859.245083	19.617869
56.771381	1860.319124	19.622887
57.132789	1852.717645	19.627904
57.070557	1858.143975	19.632922
56.841644	1860.580391	19.637939
57.350572	1848.725136	19.642957
56.819571	1859.964446	19.647975
56.876119	1850.823303	19.652992
57.252508	1854.243478	19.658010
57.131202	1854.408800	19.663027
57.327003	1850.981513	19.668045
57.312715	1852.961787	19.673063
57.230948	1864.334342	19.678080
57.756308	1865.777552	19.683098
57.778306	1872.388810	19.688115
57.884459	1853.451699	19.693133
57.807659	1855.860066	19.698151
57.934630	1844.055338	19.703168
57.939423	1850.844755	19.708186
57.974614	1848.014762	19.713203
58.472828	1839.931115	19.718221
58.187562	1846.724979	19.723239
57.899555	1849.680645	19.728256
58.264744	1851.537189	19.733274
58.034327	1843.305594	19.738291
58.241783	1843.155855	19.743309
57.945021	1845.952765	19.748327
57.459565	1837.403830	19.753344
57.582087	1843.525735	19.758362
57.824505	1867.111182	19.763379
57.995475	1867.907581	19.768397
57.894169	1880.119037	19.773415
57.817740	1884.520513	19.778432
58.357342	1893.153544	19.783450
58.176902	1902.369931	19.788467
58.449840	1907.202523	19.793485
58.387310	1910.521169	19.798503
58.512006	1911.273529	19.803520
58.700957	1913.113834	19.808538
58.647256	1936.934824	19.813555
58.774733	1943.701279	19.818573
58.982566	1950.494123	19.823591
58.896288	1946.005582	19.828608
59.054036	1937.432548	19.833626
59.053072	1949.909175	19.838643
59.443537	1939.201082	19.843661
58.964341	1946.729512	19.848679
59.161290	1949.877284	19.853696
58.803890	1934.277068	19.858714
58.893783	1947.168881	19.863731
59.464828	1957.548362	19.868749
59.551166	1972.470995	19.873767
59.439790	1971.810883	19.878784
59.871129	1967.255248	19.883802
59.397527	1977.972134	19.888819
59.903978	1964.767430	19.893837
59.677539	1965.845778	19.898855
59.628621	1973.950930	19.903872
59.671775	1967.526945	19.908890
59.385845	1970.527952	19.913907
60.135846	1980.967724	19.918925
60.059040	2002.559799	19.923943
60.227079	2000.288577	19.928960
60.371842	1997.168080	19.933978
60.548036	1994.527301	19.938995
60.793288	1978.348063	19.944013
60.721939	1993.589129	19.949031
60.810996	1973.868871	19.954048
61.064659	1952.936402	19.959066
60.523906	1953.365395	19.964083
60.654814	1948.542728	19.969101
60.669267	1953.961849	19.974119
60.386378	1947.079136	19.979136
60.666547	1962.855654	19.984154
60.561703	1981.542278	19.989171
60.940859	1982.541212	19.994189
60.681946	1985.837630	19.999207
60.749944	1985.878358	20.004224
60.913532	1979.645559	20.009242
60.955917	1985.733221	20.014259
61.210930	1989.443958	20.019277
61.108666	2001.185924	20.024295
60.943574	2008.237244	20.029312
61.592363	2002.474868	20.034330
61.148679	2016.599318	20.039347
61.121235	2012.623184	20.044365
61.435358	2017.709021	20.049383
61.280928	2025.066043	20.054400
61.578001	2020.506637	20.059418
61.570350	2040.397701	20.064435
61.988601	2047.049772	20.069453
62.130677	2047.682608	20.074471
61.762233	2049.605106	20.079488
61.986578	2048.644879	20.084506
61.840324	2056.079658	20.089523
62.389450	2049.342482	20.094541
62.080402	2055.401829	20.099559
62.007903	2054.327117	20.104576
62.082136	2055.790202	20.109594
61.602985	2054.450123	20.114611
62.100775	2048.623055	20.119629
61.980429	2060.751684	20.124647
62.328086	2068.568783	20.129664
62.528892	2077.224170	20.134682
62.534849	2081.133163	20.139699
62.495749	2078.836411	20.144717
62.497902	2070.288799	20.149735
62.507803	2079.728992	20.154752
62.780827	2074.533053	20.159770
62.516987	2078.896232	20.164787
62.936684	2093.588968	20.169805
63.077777	2105.460573	20.174823
63.445322	2108.079059	20.179840
63.410835	2101.508859	20.184858
63.170417	2104.903719	20.189875
63.447623	2092.414686	20.194893
63.462816	2099.429625	20.199911
63.706431	2092.288447	20.204928
63.399989	2096.473869	20.209946
63.508430	2103.161362	20.214963
63.693278	2094.604858	20.219981
63.713048	2097.881871	20.224999
63.624425	2094.546214	20.230016
63.687625	2087.476133	20.235034
63.480197	2097.619832	20.240051
63.989772	2089.926685	20.245069
64.266018	2087.204554	20.250087
64.044265	2087.248496	20.255104
64.026138	2080.502641	20.260122
64.405275	2081.701613	20.265139
64.596682	2084.943683	20.270157
64.671722	2083.588126	20.275175
64.797025	2076.394788	20.280192
64.761168	2080.051070	20.285210
64.696643	2087.668731	20.290227
64.401646	2086.815260	20.295245
64.350231	2076.807331	20.300263
64.432929	2085.262074	20.305280
64.547798	2074.861019	20.310298
64.963804	2079.651418	20.315315
64.815206	2081.364944	20.320333
64.733535	2077.723726	20.325351
64.646926	2084.280849	20.330368
65.152750	2085.952265	20.335386
64.977264	2108.107544	20.340403
64.915278	2107.243261	20.345421
65.405384	2109.397364	20.350439
64.923582	2113.018283	20.355456
65.376941	2111.238756	20.360474
65.293116	2115.815211	20.365491
65.107353	2119.339701	20.370509
65.360415	2102.683731	20.375527
64.915299	2111.770003	20.380544
65.267071	2116.238701	20.385562
65.617805	2135.545140	20.390579
65.674052	2146.682002	20.395597
65.908263	2144.204504	20.400615
65.751795	2146.972688	20.405632
66.071551	2139.062419	20.410650
65.846121	2140.039016	20.415667
65.951484	2134.131932	20.420685
66.248417	2129.318152	20.425703
66.248894	2137.374363	20.430720
66.175373	2131.292408	20.435738
66.600253	2137.347233	20.440755
66.257562	2134.437072	20.445773
66.298654	2129.700230	20.450791
66.032957	2140.864722	20.455808
66.504021	2146.305246	20.460826
67.054305	2159.730989	20.465843
67.062907	2137.418429	20.470861
67.214556	2133.621038	20.475879
66.831100	2127.427630	20.480896
67.272262	2111.371776	20.485914
66.855322	2113.241170	20.490931
67.121776	2115.772249	20.495949
67.631320	2107.182909	20.500967
67.504510	2103.369477	20.505984
67.482523	2095.598540	20.511002
67.567925	2099.160799	20.516019
67.622252	2085.719685	20.521037
67.813254	2100.769006	20.526055
67.372927	2104.188297	20.531072
67.837518	2093.869810	20.536090
67.794441	2102.391015	20.541107
67.447989	2108.212272	20.546125
67.723622	2099.555543	20.551143
67.658441	2107.205220	20.556160
67.931828	2103.549979	20.561178
67.561664	2108.859874	20.566195
67.458728	2115.860423	20.571213
68.073585	2121.112483	20.576231
68.261476	2136.401382	20.581248
68.409579	2133.982749	20.586266
68.208224	2127.725046	20.591283
68.067075	2146.436205	20.596301
68.421907	2132.692312	20.601319
68.234904	2135.214512	20.606336
68.120759	2138.900768	20.611354
68.317238	2141.177669	20.616371
68.326751	2150.406522	20.621389
69.020115	2164.251110	20.626407
68.580662	2172.255974	20.631424
69.054787	2164.277488	20.636442
68.969394	2166.272749	20.641459
68.613079	2165.299058	20.646477
69.395484	2163.622190	20.651495
68.941272	2164.260004	20.656512
68.913782	2162.748765	20.661530
68.687684	2159.778446	20.666547
69.042411	2160.099592	20.671565
69.383048	2161.952509	20.676583
69.256461	2170.425855	20.681600
69.234452	2179.149820	20.686618
69.270081	2190.521779	20.691635
69.264959	2200.988787	20.696653
69.332342	2182.628876	20.701671
69.374772	2194.724976	20.706688
69.678492	2207.125946	20.711706
69.760245	2212.382021	20.716723
69.934564	2215.314010	20.721741
70.082135	2209.068903	20.726759
69.693008	2224.244185	20.731776
70.091358	2214.252379	20.736794
70.335432	2214.580684	20.741811
70.091145	2216.470890	20.746829
70.054962	2206.555162	20.751847
70.502789	2220.849044	20.756864
70.415174	2231.323915	20.761882
70.384391	2231.925362	20.766899
70.225789	2231.687176	20.771917
70.617185	2232.552513	20.776935
70.472927	2236.314044	20.781952
70.606983	2235.042859	20.786970
70.627889	2240.914978	20.791987
70.178925	2259.807411	20.797005
70.547317	2259.087476	20.802023
70.806224	2273.542949	20.807040
70.930240	2268.146081	20.812058
70.966503	2278.079981	20.817075
70.993409	2283.970776	20.822093
71.172352	2287.090203	20.827111
71.243463	2302.559941	20.832128
71.226529	2296.880881	20.837146
71.504667	2298.821708	20.842163
71.568506	2318.276788	20.847181
71.909310	2314.290993	20.852199
71.906195	2324.114332	20.857216
71.713218	2319.060815	20.862234
72.045616	2322.058650	20.867251
72.149961	2322.335312	20.872269
72.168128	2321.648643	20.877287
72.075995	2319.790148	20.882304
72.154598	2312.559819	20.887322
72.834891	2313.789869	20.892339
72.352202	2310.411473	20.897357
72.686871	2314.765821	20.902375
72.607123	2316.515213	20.907392
72.699633	2317.463299	20.912410
72.865275	2305.896907	20.917427
72.603195	2315.242511	20.922445
72.695706	2306.278823	20.927463
72.661047	2312.273899	20.932480
72.789446	2305.672143	20.937498
72.899262	2308.208846	20.942515
72.614529	2319.112908	20.947533
72.847421	2321.206399	20.952551
73.170712	2335.608365	20.957568
73.331760	2343.469410	20.962586
73.273004	2342.980209	20.967603
73.182443	2335.702483	20.972621
73.341541	2331.014651	20.977639
73.158900	2347.217809	20.982656
73.234885	2338.042729	20.987674
73.663073	2348.701730	20.992691
73.401616	2369.727843	20.997709
73.746100	2363.048065	21.002727
73.851908	2373.416629	21.007744
73.698904	2365.970038	21.012762
74.066869	2371.184184	21.017779
73.751866	2380.319967	21.022797
73.967139	2364.840464	21.027815
74.029862	2378.955595	21.032832
74.036235	2394.860999	21.037850
74.258135	2396.510645	21.042867
74.225682	2402.038373	21.047885
74.814951	2395.752904	21.052903
74.764710	2386.677403	21.057920
74.998825	2381.327772	21.062938
75.548951	2374.737162	21.067955
75.495144	2376.499439	21.072973
75.748454	2369.558867	21.077991
75.535778	2358.863725	21.083008
75.274835	2354.013217	21.088026
75.849238	2343.406802	21.093043
75.417917	2341.938792	21.098061
75.534540	2334.804313	21.103079
75.572504	2334.170164	21.108096
75.753578	2335.827590	21.113114
75.662307	2335.694412	21.118131
75.633415	2342.539826	21.123149
75.435353	2346.463387	21.128167
75.595257	2341.836053	21.133184
75.078680	2344.401402	21.138202
75.295317	2342.679761	21.143219
75.123198	2370.747574	21.148237
75.553318	2372.572576	21.153255
75.519851	2384.432189	21.158272
75.520136	2401.570337	21.163290
75.753105	2401.635154	21.168307
75.718149	2412.552371	21.173325
75.812350	2421.488867	21.178343
75.940943	2432.179601	21.183360
75.925291	2443.736155	21.188378
76.539330	2430.456309	21.193395
76.587453	2435.209480	21.198413
76.529349	2431.493655	21.203431
77.043328	2449.951102	21.208448
77.057782	2460.644886	21.213466
77.138009	2450.958693	21.218483
77.198047	2443.092012	21.223501
77.180983	2439.208493	21.228519
77.269613	2433.411270	21.233536
77.023579	2441.290179	21.238554
77.282340	2455.981318	21.243571
77.219031	2459.032846	21.248589
77.262358	2457.626779	21.253607
77.206511	2463.277457	21.258624
77.111926	2466.087064	21.263642
77.323605	2465.487704	21.268659
77.412784	2482.354752	21.273677
77.604902	2483.903984	21.278695
77.676033	2492.794074	21.283712
77.706955	2501.072850	21.288730
77.961267	2494.057236	21.293747
78.024278	2499.588320	21.298765
78.111493	2504.567133	21.303783
78.237991	2512.839766	21.308800
78.290807	2522.628439	21.313818
78.371341	2512.157772	21.318835
78.572918	2518.077774	21.323853
78.705329	2517.550280	21.328871
78.924334	2516.882723	21.333888
78.598654	2521.566126	21.338906
78.627095	2513.625286	21.343923
78.776981	2518.747716	21.348941
78.762047	2515.951397	21.353959
78.988179	2518.709178	21.358976
78.758282	2541.293365	21.363994
79.365637	2545.348228	21.369011
78.748049	2542.232320	21.374029
78.772244	2550.313815	21.379047
79.139454	2542.783465	21.384064
79.198145	2569.404736	21.389082
79.544508	2572.203342	21.394099
79.513565	2575.442290	21.399117
79.439241	2576.641080	21.404135
79.531747	2578.079818	21.409152
79.544581	2574.126561	21.414170
80.088369	2584.515469	21.419187
80.268906	2602.815265	21.424205
80.244046	2607.866090	21.429223
80.643471	2599.159120	21.434240
80.457901	2593.096195	21.439258
80.740144	2592.995846	21.444275
80.793041	2597.230048	21.449293
80.829414	2577.750388	21.454311
80.696307	2573.553602	21.459328
80.505713	2566.152736	21.464346
81.214107	2569.927247	21.469363
81.086040	2561.289469	21.474381
81.242370	2565.442927	21.479399
81.512728	2571.044018	21.484416
81.202251	2553.963624	21.489434
81.287544	2554.185279	21.494451
80.978229	2557.241988	21.499469
81.135043	2555.386462	21.504487
81.126206	2553.740468	21.509504
81.341297	2571.794106	21.514522
81.382778	2574.145684	21.519539
81.398749	2584.139959	21.524557
81.295646	2588.984470	21.529575
81.752080	2590.603378	21.534592
81.649386	2588.593879	21.539610
81.856425	2588.000824	21.544627
81.651540	2596.976096	21.549645
81.732473	2608.758774	21.554663
82.456675	2612.885766	21.559680
82.389905	2619.099887	21.564698
82.573777	2608.537410	21.569715
82.708456	2607.776414	21.574733
82.412167	2607.713822	21.579751
82.827492	2607.049617	21.584768
82.773447	2612.685076	21.589786
82.704419	2603.460675	21.594803
83.031334	2605.846801	21.599821
82.879093	2603.306331	21.604839
82.979672	2602.746490	21.609856
83.062527	2603.786816	21.614874
82.844502	2595.107739	21.619891
83.235724	2600.595978	21.624909
82.943700	2606.378552	21.629927
83.739342	2599.130690	21.634944
83.836977	2607.505977	21.639962
83.497077	2595.039259	21.644979
83.104120	2599.349901	21.649997
83.396864	2608.119371	21.655015
83.657635	2612.588065	21.660032
83.797985	2614.584057	21.665050
84.170365	2603.711264	21.670067
84.621048	2604.623950	21.675085
84.081409	2605.328402	21.680103
84.297720	2602.519198	21.685120
84.160537	2602.735681	21.690138
84.066643	2605.292394	21.695155
84.175904	2604.683813	21.700173
84.415089	2627.635025	21.705191
84.745083	2626.322341	21.710208
84.701877	2634.394172	21.715226
84.690899	2638.069945	21.720243
84.949621	2635.896098	21.725261
84.865671	2644.482882	21.730279
84.811466	2639.330653	21.735296
84.557358	2639.927088	21.740314
85.052198	2639.310679	21.745331
85.023659	2642.261777	21.750349
85.128098	2669.739307	21.755367
85.445901	2670.755896	21.760384
85.225015	2670.563033	21.765402
85.153290	2665.103507	21.770419
85.712603	2670.377093	21.775437
85.507771	2669.675087	21.780455
85.853191	2662.892642	21.785472
85.583503	2663.757151	21.790490
85.528333	2670.615088	21.795507
86.048714	2681.172669	21.800525
86.112835	2688.382670	21.805543
86.228199	2683.965271	21.810560
86.215544	2691.780668	21.815578
86.458029	2680.965531	21.820595
86.411357	2674.467664	21.825613
86.380923	2684.125803	21.830631
86.379958	2673.909988	21.835648
86.774156	2696.160589	21.840666
86.927232	2705.410834	21.845683
87.152958	2700.011344	21.850701
87.044483	2706.595708	21.855719
87.351151	2702.110854	21.860736
87.329520	2705.783744	21.865754
87.404729	2705.784255	21.870771
87.207353	2695.381588	21.875789
86.901642	2703.830014	21.880807
87.283677	2697.517741	21.885824
87.470525	2702.273987	21.890842
87.346287	2697.896087	21.895859
87.519821	2716.271247	21.900877
87.666248	2729.524158	21.905895
87.961696	2733.569543	21.910912
87.751073	2733.485963	21.915930
87.654471	2736.306201	21.920947
88.045036	2732.259007	21.925965
87.968920	2747.035395	21.930983
88.143267	2756.827793	21.936000
88.168717	2773.400513	21.941018
87.957958	2773.522505	21.946035
88.401624	2763.664342	21.951053
88.194957	2783.799563	21.956071
88.875884	2789.440600	21.961088
88.607272	2801.773992	21.966106
88.683713	2800.707952	21.971123
89.131250	2802.569399	21.976141
89.009500	2809.445899	21.981159
88.963252	2809.338075	21.986176
89.170751	2809.660852	21.991194
89.255050	2831.533985	21.996211
89.413872	2830.004916	22.001229
89.575062	2831.281481	22.006247
89.869659	2829.748823	22.011264
89.955951	2827.664365	22.016282
89.835964	2826.754069	22.021299
90.344540	2821.332035	22.026317
89.926712	2825.420187	22.031335
90.267963	2820.812026	22.036352
90.360778	2822.751616	22.041370
90.138317	2824.935057	22.046387
90.049649	2822.605740	22.051405
90.158031	2831.647934	22.056423
90.404195	2817.823632	22.061440
90.175584	2823.252830	22.066458
90.263897	2850.553093	22.071475
90.624540	2847.255235	22.076493
90.380980	2858.069916	22.081511
90.792659	2858.004867	22.086528
90.554538	2858.340252	22.091546
90.581948	2877.699101	22.096563
90.730273	2880.567943	22.101581
91.005505	2884.881451	22.106599
91.123196	2886.533265	22.111616
91.164679	2905.508561	22.116634
91.189991	2913.341185	22.121651
91.527114	2917.869332	22.126669
91.353501	2924.841404	22.131687
91.673910	2922.724672	22.136704
91.593148	2923.441034	22.141722
91.659633	2940.339242	22.146739
92.313547	2943.932599	22.151757
91.981206	2946.360922	22.156775
91.959942	2942.124386	22.161792
92.150041	2946.276882	22.166810
92.292659	2949.642087	22.171827
92.619656	2958.487788	22.176845
92.415372	2968.611425	22.181863
92.776528	2966.780673	22.186880
92.950415	2968.005456	22.191898
92.963511	2969.891001	22.196915
93.154806	2975.111227	22.201933
93.097901	2980.918995	22.206951
93.350369	2971.935381	22.211968
93.461402	2972.648790	22.216986
92.987946	2972.136159	22.222003
93.294313	2959.012576	22.227021
93.160972	2976.253804	22.232039
93.173500	2994.504105	22.237056
93.827195	2994.442456	22.242074
93.564913	2983.266317	22.247091
93.437825	2995.827615	22.252109
93.369112	3007.217267	22.257127
93.674463	3026.804295	22.262144
93.808674	3026.605677	22.267162
93.815712	3032.235539	22.272179
94.177941	3035.815920	22.277197
94.368681	3050.190865	22.282215
94.449283	3059.768769	22.287232
94.529429	3051.974730	22.292250
94.437096	3059.990622	22.297267
94.842750	3051.806064	22.302285
94.992386	3047.737878	22.307303
94.985519	3046.623887	22.312320
95.283455	3050.275148	22.317338
94.808289	3061.297425	22.322355
95.496634	3065.169218	22.327373
95.472808	3081.916885	22.332391
95.395789	3082.234893	22.337408
95.606878	3073.611931	22.342426
95.600754	3078.884151	22.347443
95.802481	3070.540805	22.352461
95.746330	3078.880491	22.357479
95.806063	3080.116978	22.362496
95.926674	3074.312461	22.367514
95.726831	3079.140630	22.372531
96.085981	3073.485020	22.377549
96.084247	3086.013087	22.382567
96.311232	3094.867348	22.387584
96.481855	3097.845817	22.392602
96.975731	3088.672688	22.397619
96.903852	3093.188311	22.402637
97.029994	3093.710908	22.407655
97.232374	3092.212937	22.412672
97.228817	3084.323761	22.417690
96.908570	3100.863160	22.422707
97.081955	3087.029836	22.427725
97.340356	3094.163400	22.432743
97.272583	3093.736363	22.437760
97.446081	3094.279981	22.442778
97.352308	3096.002723	22.447795
97.122000	3092.319414	22.452813
97.259657	3119.513239	22.457831
97.289062	3132.174615	22.462848
97.427444	3133.013291	22.467866
97.592760	3147.872313	22.472883
97.860664	3152.436022	22.477901
98.087648	3155.860840	22.482919
97.923413	3157.245202	22.487936
98.074363	3156.146675	22.492954
98.467820	3177.964138	22.497971
98.512597	3185.079237	22.502989
98.824266	3181.200607	22.508007
98.990063	3180.625628	22.513024
99.214489	3175.301019	22.518042
98.913940	3176.055071	22.523059
99.139138	3171.958148	22.528077
99.090402	3173.217176	22.533095
99.028098	3178.730605	22.538112
99.338620	3174.193767	22.543130
99.241294	3185.454567	22.548147
99.513778	3193.634014	22.553165
99.242043	3206.996821	22.558183
99.588476	3215.985823	22.563200
99.897292	3208.600631	22.568218
99.613401	3219.600464	22.573235
99.406072	3214.183684	22.578253
99.853327	3231.382358	22.583271
99.532799	3244.662991	22.588288
99.725116	3243.391189	22.593306
99.791657	3251.097990	22.598323
100.032357	3259.321512	22.603341
100.155549	3277.105040	22.608359
100.321185	3281.092491	22.613376
100.608105	3275.234187	22.618394
100.560291	3295.397956	22.623411
100.782433	3312.398252	22.628429
101.270266	3311.440428	22.633447
101.606511	3309.816316	22.638464
101.662656	3301.307214	22.643482
101.564188	3304.385410	22.648499
101.891809	3291.531984	22.653517
102.087544	3295.794654	22.658535
101.834332	3302.986096	22.663552
101.794968	3297.717696	22.668570
101.586285	3291.152840	22.673587
101.847786	3295.997278	22.678605
101.858598	3280.723620	22.683623
101.945477	3278.078251	22.688640
102.479721	3278.099301	22.693658
102.647727	3291.447433	22.698675
102.388219	3293.470323	22.703693
102.300408	3293.349144	22.708711
102.655247	3309.754123	22.713728
102.865611	3302.563757	22.718746
102.712484	3314.924217	22.723763
102.422981	3306.766560	22.728781
102.882412	3320.234871	22.733799
102.814767	3333.837660	22.738816
103.253753	3337.204120	22.743834
103.122122	3344.010877	22.748851
103.226691	3351.330021	22.753869
103.339959	3341.313135	22.758887
103.241444	3366.040236	22.763904
103.893156	3362.008756	22.768922
103.915232	3360.679497	22.773939
104.044532	3356.584791	22.778957
104.210915	3352.092303	22.783975
103.960090	3352.785071	22.788992
104.719304	3341.253985	22.794010
104.533127	3350.297359	22.799027
104.678635	3347.222150	22.804045
104.942398	3344.331437	22.809063
104.812803	3353.005978	22.814080
104.947149	3343.184734	22.819098
104.976141	3354.397221	22.824115
105.119686	3365.966539	22.829133
105.313308	3370.878555	22.834151
105.171735	3380.278160	22.839168
105.248852	3377.400538	22.844186
105.619722	3383.911669	22.849203
105.147702	3378.933999	22.854221
105.589427	3370.964403	22.859239
105.411254	3386.102270	22.864256
105.829920	3382.380878	22.869274
105.492392	3379.998846	22.874291
105.705017	3394.644432	22.879309
105.859880	3404.572888	22.884327
105.959883	3409.222164	22.889344
106.259897	3403.200902	22.894362
106.629071	3405.730336	22.899379
106.315738	3406.652770	22.904397
106.628723	3407.994718	22.909415
106.667400	3432.188052	22.914432
106.910777	3439.247954	22.919450
106.937444	3435.600053	22.924467
106.765177	3440.667753	22.929485
107.045850	3441.414321	22.934503
106.919952	3447.523131	22.939520
106.994446	3439.509347	22.944538
107.108839	3461.840507	22.949555
106.960844	3468.018482	22.954573
107.303059	3462.802747	22.959591
106.994373	3479.220846	22.964608
107.256187	3486.640684	22.969626
107.129778	3497.519989	22.974643
107.369801	3518.294692	22.979661
108.004950	3517.640812	22.984679
108.392773	3514.780781	22.989696
108.595942	3509.709368	22.994714
108.590990	3519.599926	22.999731
108.585441	3519.204739	23.004749
109.102883	3528.249663	23.009767
108.812195	3552.401986	23.014784
109.002072	3551.485780	23.019802
108.914852	3552.222178	23.024819
108.824838	3551.757199	23.029837
109.020068	3550.883392	23.034855
109.057269	3560.689566	23.039872
109.297260	3572.724504	23.044890
109.540578	3579.239469	23.049907
109.364806	3582.901972	23.054925
109.853719	3575.388861	23.059943
109.485813	3583.533383	23.064960
109.894420	3597.145323	23.069978
110.228151	3606.710880	23.074995
110.117504	3605.853280	23.080013
110.747539	3609.607620	23.085031
110.563378	3600.878862	23.090048
110.646370	3592.140539	23.095066
110.792351	3589.636203	23.100083
110.761935	3595.104931	23.105101
110.972620	3587.762376	23.110119
110.917318	3589.853468	23.115136
110.853710	3604.050426	23.120154
111.152320	3619.513175	23.125171
110.929480	3612.957699	23.130189
111.496804	3622.849448	23.135207
111.476133	3633.696543	23.140224
111.487743	3629.522706	23.145242
111.516299	3628.768830	23.150259
111.476139	3632.215924	23.155277
111.803911	3636.586004	23.160295
111.907537	3652.856413	23.165312
111.871558	3660.840108	23.170330
112.410070	3646.768066	23.175347
112.006786	3662.788300	23.180365
112.324922	3661.138117	23.185383
112.273531	3683.679946	23.190400
112.373182	3687.588240	23.195418
112.638238	3681.476780	23.200435
112.446770	3692.928926	23.205453
113.141242	3695.940567	23.210471
113.461549	3709.868604	23.215488
113.364298	3705.976466	23.220506
113.710548	3709.373871	23.225523
113.322628	3715.537943	23.230541
113.364734	3701.607661	23.235559
113.739983	3705.827067	23.240576
113.379622	3708.762004	23.245594
113.992099	3713.878767	23.250611
113.950821	3733.726151	23.255629
114.287757	3735.890210	23.260647
114.162895	3743.457582	23.265664
114.331247	3741.273089	23.270682
114.544610	3739.471527	23.275699
114.581577	3748.194914	23.280717
113.954878	3750.694297	23.285735
114.132881	3768.257909	23.290752
114.843741	3772.507220	23.295770
114.835760	3771.480004	23.300787
115.150194	3786.957532	23.305805
115.164969	3787.259816	23.310823
115.497234	3793.466635	23.315840
115.327034	3794.591379	23.320858
115.561483	3789.620053	23.325875
115.493777	3800.590315	23.330893
115.686653	3804.573230	23.335911
115.931239	3821.172492	23.340928
115.751807	3825.893424	23.345946
116.159932	3822.673076	23.350963
115.753353	3833.600643	23.355981
116.009718	3839.865386	23.360999
116.263199	3862.809650	23.366016
116.476019	3862.474681	23.371034
116.656625	3852.437264	23.376051
116.752646	3867.126908	23.381069
116.829279	3878.898674	23.386087
116.733151	3891.207281	23.391104
116.784563	3893.392746	23.396122
117.174588	3893.620462	23.401139
117.094095	3905.260876	23.406157
117.556944	3910.096190	23.411175
117.682724	3920.782119	23.416192
117.526816	3921.831175	23.421210
118.019997	3909.485224	23.426227
117.890684	3921.715271	23.431245
117.964394	3914.256643	23.436263
118.178825	3917.718435	23.441280
118.177185	3923.229600	23.446298
118.422706	3930.743016	23.451315
118.544519	3942.485030	23.456333
118.719243	3943.122195	23.461351
118.724711	3940.581248	23.466368
118.550455	3941.771281	23.471386
118.686656	3938.907056	23.476403
119.013187	3967.880670	23.481421
118.643351	3962.134705	23.486439
119.002428	3966.575121	23.491456
119.109198	3986.562839	23.496474
119.428129	3994.599273	23.501491
119.568222	4012.696566	23.506509
119.509864	3996.392855	23.511527
119.889138	3995.334677	23.516544
119.911506	4018.666124	23.521562
120.478857	4014.334692	23.526579
120.772888	4025.411643	23.531597
121.039393	4018.562603	23.536615
121.031339	4018.124515	23.541632
120.989018	4019.408502	23.546650
121.343508	4010.022457	23.551667
121.031901	4015.802598	23.556685
121.122400	4009.446062	23.561703
121.154509	4009.225557	23.566720
121.057566	4010.455898	23.571738
121.294019	4010.613069	23.576755
121.540020	4009.411552	23.581773
121.452500	4012.512424	23.586791
121.691449	4035.425564	23.591808
121.765165	4041.550001	23.596826
122.169401	4040.086648	23.601843
121.883239	4042.962456	23.606861
121.882479	4047.940301	23.611879
122.122114	4053.508599	23.616896
122.222907	4063.689325	23.621914
122.504248	4073.534299	23.626931
122.854994	4074.624100	23.631949
122.863206	4078.796264	23.636967
122.922653	4078.563196	23.641984
123.030594	4100.296205	23.647002
123.237329	4107.275265	23.652019
123.185993	4115.021600	23.657037
122.968123	4113.382925	23.662055
123.027055	4117.766149	23.667072
123.152458	4137.023895	23.672090
123.605739	4130.160903	23.677107
123.755976	4142.488117	23.682125
124.024743	4139.412890	23.687143
124.355968	4133.473427	23.692160
123.965996	4143.189370	23.697178
124.567337	4152.925978	23.702195
124.138084	4163.804888	23.707213
124.402578	4164.647205	23.712231
124.812152	4160.223852	23.717248
124.772342	4169.050422	23.722266
124.726279	4160.014924	23.727283
124.757746	4179.953575	23.732301
125.032232	4192.676964	23.737319
124.941694	4188.036107	23.742336
124.981848	4208.401768	23.747354
125.097502	4216.852797	23.752371
124.826815	4232.564968	23.757389
125.000063	4234.968242	23.762407
125.721074	4243.411596	23.767424
126.136864	4251.797014	23.772442
126.294855	4240.388043	23.777459
126.347420	4245.307189	23.782477
126.339042	4261.187076	23.787495
126.699446	4264.762543	23.792512
126.773768	4265.972994	23.797530
127.228683	4251.693428	23.802547
127.390648	4265.280496	23.807565
127.268240	4271.355157	23.812583
127.540183	4257.401524	23.817600
127.272752	4262.739414	23.822618
127.393421	4264.553114	23.827635
127.089252	4267.039813	23.832653
127.323176	4280.633461	23.837671
127.640661	4286.088468	23.842688
127.726547	4291.202759	23.847706
127.808733	4292.171640	23.852723
128.155139	4314.082234	23.857741
128.269243	4331.599930	23.862759
128.370785	4333.616974	23.867776
128.012801	4339.298853	23.872794
128.548639	4341.027211	23.877811
128.522202	4353.094243	23.882829
128.574313	4357.103006	23.887847
128.981535	4374.803638	23.892864
128.941138	4394.272062	23.897882
129.668982	4384.074335	23.902899
129.776223	4386.732325	23.907917
129.716215	4394.985939	23.912935
129.959399	4386.240194	23.917952
129.933420	4386.900758	23.922970
130.138576	4383.174783	23.927987
130.191774	4379.782821	23.933005
130.094010	4395.199290	23.938023
130.351492	4403.642645	23.943040
129.930811	4411.104311	23.948058
130.016053	4398.171035	23.953075
130.146653	4422.833730	23.958093
130.368297	4443.848305	23.963111
130.614908	4438.385574	23.968128
130.526124	4454.266050	23.973146
130.968589	4465.259580	23.978163
131.376439	4471.305637	23.983181
131.085307	4468.417697	23.988199
131.620725	4471.756062	23.993216
131.690960	4493.872564	23.998234
131.826955	4483.662028	24.003251
131.555362	4494.495232	24.008269
131.410732	4504.977447	24.013287
132.451917	4511.830175	24.018304
132.377042	4523.102254	24.023322
132.419343	4524.871134	24.028339
132.655009	4519.528397	24.033357
132.602074	4524.897339	24.038375
132.948586	4516.764704	24.043392
132.917507	4547.535845	24.048410
133.349333	4550.197291	24.053427
133.588206	4549.271055	24.058445
133.466579	4550.318999	24.063463
133.870469	4548.464207	24.068480
133.358634	4551.091305	24.073498
133.558412	4551.842347	24.078515
134.000783	4565.389478	24.083533
134.178093	4577.161045	24.088551
134.335801	4574.665572	24.093568
134.529576	4580.835798	24.098586
134.313422	4583.609910	24.103603
134.755525	4585.733219	24.108621
134.407499	4610.363263	24.113639
134.961499	4609.386152	24.118656
134.728280	4606.356723	24.123674
134.969175	4616.599639	24.128691
134.742672	4628.656284	24.133709
134.995535	4641.551510	24.138727
134.908394	4634.153199	24.143744
135.137458	4668.559043	24.148762
135.618482	4672.630619	24.153779
135.985734	4670.496968	24.158797
136.286386	4688.690381	24.163815
136.925896	4679.674896	24.168832
137.127910	4659.616860	24.173850
137.232534	4663.049597	24.178867
137.478642	4652.928770	24.183885
137.350800	4643.882599	24.188903
137.597522	4638.427658	24.193920
137.770144	4635.563366	24.198938
137.443182	4639.459966	24.203955
137.788517	4641.120200	24.208973
137.507543	4640.091681	24.213991
137.737631	4644.650496	24.219008
137.797640	4643.893543	24.224026
137.701586	4636.247864	24.229043
137.770295	4637.816896	24.234061
137.542492	4658.233797	24.239079
137.932730	4662.368980	24.244096
138.063029	4669.429918	24.249114
138.121154	4673.605498	24.254131
138.232286	4686.844053	24.259149
138.222880	4705.880646	24.264167
138.558250	4707.932479	24.269184
138.689993	4727.035479	24.274202
138.684699	4736.325095	24.279219
138.922829	4740.534421	24.284237
139.158274	4757.444205	24.289255
139.483332	4763.771580	24.294272
139.405336	4772.732630	24.299290
139.431329	4778.266135	24.304307
140.010220	4789.165617	24.309325
139.861951	4795.238610	24.314343
139.904615	4791.662481	24.319360
140.168540	4800.119123	24.324378
140.475308	4823.288792	24.329395
140.891633	4817.967758	24.334413
140.433486	4828.273938	24.339431
140.722223	4821.523138	24.344448
140.876428	4839.533104	24.349466
140.832433	4854.377631	24.354483
141.172478	4858.467910	24.359501
141.305133	4856.046789	24.364519
141.551303	4867.106546	24.369536
141.854975	4878.821231	24.374554
141.995398	4882.538522	24.379571
142.047949	4882.211319	24.384589
142.262763	4880.821324	24.389607
142.494182	4891.048715	24.394624
143.605143	4874.947708	24.399642
143.983902	4864.199879	24.404659
144.139054	4844.004715	24.409677
144.103946	4841.545406	24.414695
143.864206	4823.114564	24.419712
143.727556	4802.303126	24.424730
143.961444	4799.518882	24.429747
144.226341	4797.718608	24.434765
144.417132	4792.120399	24.439783
144.215407	4792.038425	24.444800
144.389507	4788.545310	24.449818
144.095298	4799.398351	24.454835
144.410737	4792.972222	24.459853
144.269739	4801.451809	24.464871
144.153056	4820.420289	24.469888
144.831398	4832.079375	24.474906
144.545897	4833.734353	24.479923
144.686737	4824.352950	24.484941
144.665114	4848.469784	24.489959
144.804067	4856.017665	24.494976
145.081387	4863.378786	24.499994
144.944574	4870.314685	24.505011
145.325904	4884.455418	24.510029
145.024413	4895.307410	24.515047
145.234198	4904.741414	24.520064
145.656226	4920.856152	24.525082
145.470268	4937.657209	24.530099
145.710271	4941.600040	24.535117
145.534003	4957.788237	24.540135
146.065526	4966.618127	24.545152
146.282067	4982.606684	24.550170
146.144667	4994.427787	24.555187
146.601353	5010.001066	24.560205
147.041110	5021.645269	24.565223
147.055573	5019.386952	24.570240
147.398364	5023.972242	24.575258
147.513965	5045.959651	24.580275
148.116014	5043.718750	24.585293
147.951799	5051.235991	24.590311
147.952323	5045.633290	24.595328
148.023450	5046.104738	24.600346
148.503672	5055.604319	24.605363
148.991910	5069.590626	24.610381
149.452862	5069.438371	24.615399
149.028226	5065.872187	24.620416
149.300809	5066.029480	24.625434
149.053276	5076.984980	24.630451
149.303964	5068.744041	24.635469
149.220037	5065.098971	24.640487
149.549187	5070.371879	24.645504
149.685861	5068.746362	24.650522
149.569396	5088.977746	24.655539
149.554150	5098.475649	24.660557
149.743143	5105.043882	24.665575
149.708168	5117.412272	24.670592
150.231979	5123.075589	24.675610
149.959202	5135.020037	24.680627
150.117306	5156.250456	24.685645
150.276315	5169.714357	24.690663
150.165302	5174.650018	24.695680
150.779693	5192.739031	24.700698
150.904398	5201.894785	24.705715
150.732836	5212.545130	24.710733
150.746236	5226.609826	24.715751
151.394231	5239.677256	24.720768
152.017778	5237.824903	24.725786
151.934154	5243.792464	24.730803
152.955121	5233.180047	24.735821
153.234065	5221.792173	24.740839
153.638932	5215.169380	24.745856
154.135149	5211.813145	24.750874
153.779854	5218.614937	24.755891
153.862198	5195.857707	24.760909
154.031623	5185.870201	24.765927
153.432917	5181.553253	24.770944
153.589756	5173.845057	24.775962
153.576386	5185.617472	24.780979
153.897102	5184.653541	24.785997
154.085510	5174.525734	24.791015
153.989678	5195.791862	24.796032
154.286253	5197.506201	24.801050
154.015552	5211.733011	24.806067
154.284825	5202.686183	24.811085
154.590566	5209.862218	24.816103
154.222868	5213.230325	24.821120
154.757813	5228.430441	24.826138
154.679795	5248.607389	24.831155
155.038000	5248.570418	24.836173
155.057690	5262.218965	24.841191
155.086778	5273.621837	24.846208
155.407918	5264.343960	24.851226
155.133778	5286.177179	24.856243
155.374869	5301.923973	24.861261
155.502615	5310.795707	24.866279
155.591471	5335.737940	24.871296
156.037442	5344.079385	24.876314
155.807542	5363.480663	24.881331
156.156064	5370.762074	24.886349
156.493602	5379.975968	24.891367
156.728108	5402.986373	24.896384
156.959088	5405.913188	24.901402
156.832175	5409.987565	24.906419
156.942112	5426.655707	24.911437
157.581128	5428.259382	24.916455
157.564713	5450.401525	24.921472
157.932996	5461.008328	24.926490
157.807795	5471.442950	24.931507
158.053774	5466.198954	24.936525
158.188724	5493.100370	24.941543
158.088819	5496.069747	24.946560
158.485326	5493.337063	24.951578
158.808080	5516.642851	24.956595
159.590258	5521.536566	24.961613
159.459818	5529.512188	24.966631
158.931270	5527.922682	24.971648
159.385347	5527.352556	24.976666
159.834213	5545.075718	24.981683
160.197636	5534.109517	24.986701
160.304617	5542.787232	24.991719
160.458067	5548.219600	24.996736
161.023505	5543.153182	25.001754
161.064644	5536.777716	25.006771
160.975825	5540.536036	25.011789
161.324112	5534.278846	25.016807
161.345262	5533.244158	25.021824
161.503097	5531.553529	25.026842
161.663945	5538.090534	25.031859
162.062165	5524.619051	25.036877
162.177084	5533.265468	25.041895
161.866351	5536.008695	25.046912
162.220471	5538.665518	25.051930
161.934411	5548.319602	25.056947
161.847261	5562.021380	25.061965
162.263926	5562.020861	25.066983
162.380735	5565.723457	25.072000
162.628632	5575.493973	25.077018
162.327685	5594.590273	25.082035
162.464673	5602.100250	25.087053
162.548890	5608.171506	25.092071
162.170835	5636.640387	25.097088
162.416278	5644.530363	25.102106
162.698403	5665.603145	25.107123
162.795956	5679.774333	25.112141
163.116337	5696.933648	25.117159
163.200158	5722.635898	25.122176
163.238999	5729.018241	25.127194
164.788766	5723.090646	25.132211
166.098719	5714.976566	25.137229
166.349205	5708.359556	25.142247
166.188711	5694.700138	25.147264
166.328725	5681.159359	25.152282
166.276318	5676.598961	25.157299
166.744187	5669.714697	25.162317
167.281193	5641.393409	25.167335
167.073355	5640.458621	25.172352
167.127332	5625.828296	25.177370
166.778943	5606.295073	25.182387
166.738826	5603.102379	25.187405
167.040648	5587.146459	25.192423
166.977710	5594.704884	25.197440
166.916572	5595.855953	25.202458
166.907076	5607.994291	25.207475
166.719541	5618.835902	25.212493
167.011237	5621.100145	25.217511
166.881628	5637.084111	25.222528
167.287078	5649.457760	25.227546
167.543368	5663.470966	25.232563
167.327087	5676.289134	25.237581
167.669215	5696.172498	25.242599
167.677913	5707.290094	25.247616
167.612630	5716.960783	25.252634
167.550987	5736.467579	25.257651
167.836802	5759.639060	25.262669
168.150179	5783.268227	25.267687
167.760212	5814.575963	25.272704
168.094464	5820.969143	25.277722
168.642231	5847.033174	25.282739
168.907148	5870.046919	25.287757
169.370969	5879.062224	25.292775
169.519376	5893.267421	25.297792
170.018256	5888.984254	25.302810
170.371994	5895.124422	25.307827
170.874581	5908.895547	25.312845
170.958607	5918.302089	25.317863
171.115329	5925.506358	25.322880
171.184788	5916.205869	25.327898
171.389760	5927.225380	25.332915
171.290824	5922.637441	25.337933
171.641925	5912.627003	25.342951
171.164704	5922.604743	25.347968
171.655659	5940.251816	25.352986
171.826486	5958.069579	25.358003
171.825982	5958.343804	25.363021
171.975671	5954.936542	25.368039
171.936054	5970.654925	25.373056
172.142861	5987.691450	25.378074
172.249954	6001.647821	25.383091
172.185790	6017.297201	25.388109
172.746768	6025.763444	25.393127
172.524734	6048.886130	25.398144
173.062502	6060.537931	25.403162
172.416673	6067.386734	25.408179
172.675931	6092.909054	25.413197
173.327151	6094.343716	25.418215
173.751238	6099.292700	25.423232
174.433578	6108.433733	25.428250
174.686451	6126.843371	25.433267
174.796946	6136.288829	25.438285
175.365185	6121.612430	25.443303
175.578009	6119.304987	25.448320
175.588041	6127.922445	25.453338
175.640321	6120.983196	25.458355
175.443559	6120.362353	25.463373
175.605476	6121.782430	25.468391
175.628891	6130.432255	25.473408
175.812700	6139.463413	25.478426
176.227263	6144.938662	25.483443
176.506577	6168.868060	25.488461
176.952821	6166.804173	25.493479
176.997639	6182.527984	25.498496
176.698167	6184.480097	25.503514
176.917907	6181.290792	25.508531
176.736386	6203.632432	25.513549
177.219984	6211.021838	25.518567
177.131375	6225.804397	25.523584
177.219486	6242.299899	25.528602
177.478643	6254.872397	25.533619
177.566202	6273.165602	25.538637
177.640951	6282.399863	25.543655
177.982327	6297.539663	25.548672
178.407499	6310.457914	25.553690
178.776566	6315.468387	25.558707
178.781373	6338.558907	25.563725
178.994541	6340.374322	25.568743
179.380030	6349.452163	25.573760
179.263611	6366.068715	25.578778
179.606404	6370.109294	25.583795
179.698704	6380.580483	25.588813
180.009302	6383.987738	25.593831
179.907293	6412.672992	25.598848
180.189616	6409.343727	25.603866
180.487109	6412.138019	25.608883
180.342276	6435.500102	25.613901
181.118344	6442.288072	25.618919
180.970987	6446.924716	25.623936
181.210399	6455.838603	25.628954
181.371340	6460.664236	25.633971
180.929029	6470.482723	25.638989
181.227800	6474.539540	25.644007
181.278545	6494.399016	25.649024
181.586430	6514.553951	25.654042
181.915860	6526.375723	25.659059
181.792181	6543.115015	25.664077
182.225938	6552.636069	25.669095
182.830256	6562.337429	25.674112
182.623190	6571.399601	25.679130
183.164422	6578.012046	25.684148
183.033801	6582.077115	25.689165
183.785183	6579.425998	25.694183
184.170482	6590.568666	25.699200
184.626077	6596.917728	25.704218
185.342463	6594.523896	25.709236
184.908319	6586.194761	25.714253
185.145394	6584.265147	25.719271
185.636480	6589.780999	25.724288
185.677559	6591.181660	25.729306
185.705516	6570.563407	25.734324
185.614437	6570.210377	25.739341
185.723508	6580.704818	25.744359
185.837908	6579.446116	25.749376
185.786608	6587.592241	25.754394
185.621440	6584.186041	25.759412
185.578515	6609.389967	25.764429
185.974138	6613.371137	25.769447
185.942345	6632.423323	25.774464
186.142532	6657.119308	25.779482
186.255838	6664.876471	25.784500
186.800451	6688.134917	25.789517
186.733016	6693.538584	25.794535
186.950154	6720.859668	25.799552
186.979140	6734.347182	25.804570
187.670796	6749.447061	25.809588
187.470434	6769.292419	25.814605
187.887174	6783.509129	25.819623
188.238174	6791.775455	25.824640
188.501167	6803.841208	25.829658
188.659012	6808.570584	25.834676
188.857197	6823.989873	25.839693
188.992452	6826.161370	25.844711
189.153001	6842.469407	25.849728
189.184543	6855.602099	25.854746
189.505625	6862.981858	25.859764
189.881239	6885.299841	25.864781
190.283872	6886.033557	25.869799
190.055725	6889.277255	25.874816
190.297178	6903.275190	25.879834
190.756830	6904.142504	25.884852
190.481298	6910.568969	25.889869
191.152911	6909.837048	25.894887
191.319995	6926.322082	25.899904
191.213594	6939.264220	25.904922
191.467091	6935.335582	25.909940
191.534603	6951.547029	25.914957
191.863369	6955.448367	25.919975
191.965967	6975.917153	25.924992
191.640339	6983.073818	25.930010
192.021519	6993.287135	25.935028
192.458854	7016.618805	25.940045
192.463908	7020.786768	25.945063
192.457674	7041.256175	25.950080
192.840223	7058.834056	25.955098
193.312238	7067.850211	25.960116
193.463612	7078.552786	25.965133
193.914989	7078.057128	25.970151
194.687744	7094.596064	25.975168
194.781710	7099.998197	25.980186
195.264172	7091.433684	25.985204
195.070795	7093.967204	25.990221
195.053831	7093.908683	25.995239
195.506118	7089.160534	26.000256
195.019345	7100.075711	26.005274
195.078772	7096.710464	26.010292
195.642061	7122.105903	26.015309
195.576713	7112.027460	26.020327
195.822515	7122.167172	26.025344
196.005886	7156.526359	26.030362
196.026457	7157.335035	26.035380
196.121637	7168.415977	26.040397
196.071667	7190.216516	26.045415
196.551767	7202.830665	26.050432
196.538835	7220.333932	26.055450
197.031479	7236.657130	26.060468
197.067205	7262.486693	26.065485
197.317839	7270.107170	26.070503
197.660953	7282.676328	26.075520
197.581439	7295.018589	26.080538
197.875179	7302.745920	26.085556
197.926394	7327.500775	26.090573
197.916270	7344.587752	26.095591
198.468374	7356.395604	26.100608
198.605433	7376.799123	26.105626
199.012645	7387.420237	26.110644
198.866414	7411.120360	26.115661
199.084389	7427.123733	26.120679
199.928060	7429.179393	26.125696
199.636690	7446.783416	26.130714
199.961334	7451.996447	26.135732
200.403226	7479.173949	26.140749
200.842055	7481.723627	26.145767
201.117937	7478.289685	26.150784
201.342195	7483.978423	26.155802
201.998586	7502.056572	26.160820
201.997145	7513.185826	26.165837
202.221143	7503.755514	26.170855
202.727386	7503.497016	26.175872
202.198510	7509.555136	26.180890
202.361130	7508.509463	26.185908
202.497753	7504.627506	26.190925
202.680258	7499.844342	26.195943
203.379087	7492.338333	26.200960
202.980327	7494.785802	26.205978
203.420740	7515.898496	26.210996
204.330257	7513.708553	26.216013
204.449475	7508.209112	26.221031
204.898785	7501.291803	26.226048
204.561774	7508.862662	26.231066
205.298138	7504.639202	26.236084
204.961004	7497.519533	26.241101
204.713718	7502.701424	26.246119
204.988278	7509.916147	26.251136
204.798081	7496.578541	26.256154
205.088946	7518.917453	26.261172
205.126217	7521.935376	26.266189
204.884702	7539.805892	26.271207
205.631115	7552.989140	26.276224
205.315305	7574.660095	26.281242
205.443912	7598.121951	26.286260
205.861017	7612.173116	26.291277
205.793312	7633.491232	26.296295
206.057791	7655.663907	26.301312
206.210828	7678.579695	26.306330
206.732758	7700.317556	26.311348
207.005235	7708.774285	26.316365
207.217420	7737.726318	26.321383
207.714653	7750.182769	26.326400
207.382811	7771.185536	26.331418
207.763052	7784.475859	26.336436
207.772667	7803.167831	26.341453
208.217748	7825.384622	26.346471
208.629293	7835.234039	26.351488
208.775049	7853.831043	26.356506
209.348053	7865.058234	26.361524
209.996836	7872.638324	26.366541
210.371871	7882.468819	26.371559
211.142776	7865.296587	26.376576
210.676267	7872.313931	26.381594
211.033198	7879.505248	26.386612
211.354310	7868.349338	26.391629
211.066113	7878.878066	26.396647
211.266382	7869.747820	26.401664
211.396396	7875.089677	26.406682
211.823335	7889.299324	26.411700
211.680333	7888.098036	26.416717
212.186564	7895.098330	26.421735
212.898124	7876.201522	26.426752
213.700148	7870.760594	26.431770
213.788740	7867.845536	26.436788
214.114102	7856.974876	26.441805
214.034861	7848.579514	26.446823
214.190112	7836.321566	26.451840
213.808167	7832.927046	26.456858
213.630742	7834.292793	26.461876
214.029499	7829.786794	26.466893
213.815059	7851.404506	26.471911
214.317437	7856.575389	26.476928
214.263422	7858.906307	26.481946
214.404635	7866.638000	26.486964
214.431179	7885.433519	26.491981
213.987910	7904.891777	26.496999
214.304598	7924.440375	26.502016
214.258349	7948.436123	26.507034
214.664430	7967.067415	26.512052
214.995841	7992.142383	26.517069
214.788870	8022.116873	26.522087
215.564557	8037.559662	26.527104
215.749594	8068.792136	26.532122
215.772260	8090.264746	26.537140
216.411400	8100.655930	26.542157
216.551981	8124.864924	26.547175
216.794578	8138.149987	26.552192
216.955282	8155.703290	26.557210
217.283100	8173.114522	26.562228
217.585431	8196.349732	26.567245
217.631210	8212.556726	26.572263
218.050557	8233.814997	26.577280
218.205264	8245.261481	26.582298
218.646010	8261.612744	26.587316
218.731485	8270.301931	26.592333
219.138883	8289.514783	26.597351
219.777830	8288.381110	26.602368
220.035559	8302.420022	26.607386
220.088271	8313.561819	26.612404
220.806524	8306.007992	26.617421
220.842120	8311.410297	26.622439
221.224617	8312.530420	26.627456
221.513053	8308.201552	26.632474
221.527651	8322.704430	26.637492
221.261416	8332.565555	26.642509
221.457085	8348.817896	26.647527
222.031610	8343.568648	26.652544
222.023544	8356.419438	26.657562
221.988331	8374.088496	26.662580
222.175253	8372.082186	26.667597
222.344302	8401.156256	26.672615
222.741207	8409.885099	26.677632
223.299801	8417.421824	26.682650
223.171114	8431.309646	26.687668
223.424640	8432.369163	26.692685
223.821985	8448.274269	26.697703
224.229057	8457.920790	26.702720
224.360385	8461.926461	26.707738
224.465214	8451.694318	26.712756
224.771819	8459.356979	26.717773
224.506459	8475.243352	26.722791
225.025895	8481.011841	26.727808
225.140040	8488.018155	26.732826
224.931021	8504.921441	26.737844
225.255685	8511.457585	26.742861
225.301057	8528.924709	26.747879
225.450398	8548.031629	26.752896
225.821942	8568.164059	26.757914
225.889852	8592.914850	26.762932
226.270139	8600.119821	26.767949
226.352797	8621.242511	26.772967
227.033434	8641.767966	26.777984
227.001023	8650.231760	26.783002
226.754163	8671.516569	26.788020
227.384494	8692.599836	26.793037
227.745513	8718.286164	26.798055
227.673111	8730.393529	26.803072
227.929694	8750.666432	26.808090
228.068227	8773.836801	26.813108
228.859667	8784.061302	26.818125
229.196743	8809.238206	26.823143
229.339455	8815.358955	26.828160
229.636862	8817.294940	26.833178
229.561761	8845.487518	26.838196
230.354304	8853.093072	26.843213
230.473074	8861.256892	26.848231
230.659879	8881.357564	26.853248
230.568376	8893.288695	26.858266
230.726665	8919.322083	26.863284
231.209151	8924.154009	26.868301
231.006416	8940.963707	26.873319
231.367743	8951.318767	26.878336
231.972851	8977.530924	26.883354
231.580760	8991.046814	26.888372
232.363958	9004.187930	26.893389
232.392389	9013.891023	26.898407
233.233372	9032.910690	26.903424
233.175828	9040.419387	26.908442
233.094182	9047.651743	26.913460
233.373929	9062.757455	26.918477
233.635983	9080.514994	26.923495
233.954688	9096.266407	26.928512
234.319230	9107.678325	26.933530
234.323957	9116.983734	26.938548
234.693861	9133.232214	26.943565
234.750148	9151.923264	26.948583
235.230772	9166.312353	26.953600
235.289589	9178.451135	26.958618
235.423903	9205.784341	26.963636
236.432614	9206.342594	26.968653
236.130322	9212.248262	26.973671
236.259846	9227.802174	26.978688
236.600508	9233.488916	26.983706
236.797993	9245.739493	26.988724
237.246876	9255.436843	26.993741
237.390622	9263.681675	26.998759
237.435963	9260.243545	27.003776
238.175971	9277.593199	27.008794
238.160213	9297.297359	27.013812
238.401594	9293.436413	27.018829
238.357053	9306.037365	27.023847
238.393707	9325.042402	27.028864
238.933844	9334.226223	27.033882
238.351277	9350.431762	27.038900
239.092841	9359.830039	27.043917
239.081595	9391.576958	27.048935
239.067935	9404.103361	27.053952
239.538557	9424.387696	27.058970
239.864135	9456.140037	27.063988
240.049255	9477.053253	27.069005
240.425447	9492.272048	27.074023
240.283210	9516.752214	27.079040
240.603575	9529.207277	27.084058
241.056161	9545.788668	27.089076
241.392078	9563.321350	27.094093
241.685171	9587.344093	27.099111
241.996376	9598.004406	27.104128
242.266098	9612.324468	27.109146
242.313474	9640.842531	27.114164
242.796654	9644.193334	27.119181
242.922547	9663.816931	27.124199
242.867387	9694.746266	27.129216
243.280808	9715.322835	27.134234
243.485948	9737.584974	27.139252
243.688210	9761.328874	27.144269
243.961739	9782.843462	27.149287
244.382262	9796.184489	27.154304
245.488591	9790.668715	27.159322
245.767564	9803.138963	27.164340
246.749505	9804.035901	27.169357
247.001447	9807.549286	27.174375
246.977595	9790.400950	27.179392
247.583302	9783.314838	27.184410
247.400608	9778.049955	27.189428
247.642520	9764.285002	27.194445
247.876934	9773.078684	27.199463
247.689615	9782.340181	27.204480
248.185156	9789.385689	27.209498
247.890549	9803.613556	27.214516
248.096142	9807.119128	27.219533
248.347510	9804.786439	27.224551
248.214354	9827.497485	27.229568
248.608052	9826.780794	27.234586
248.897573	9842.315752	27.239604
249.291448	9851.093174	27.244621
249.498728	9862.605070	27.249639
250.066616	9887.074381	27.254656
250.354221	9888.558350	27.259674
250.114041	9898.712995	27.264692
250.555440	9899.805019	27.269709
250.593479	9920.874811	27.274727
250.813950	9928.883069	27.279744
250.968329	9938.954351	27.284762
250.917297	9948.906419	27.289780
250.983298	9965.529293	27.294797
251.328220	9993.287865	27.299815
251.692090	10012.176164	27.304832
252.036640	10016.181132	27.309850
251.656385	10036.974519	27.314868
251.849964	10056.130005	27.319885
252.349212	10088.295047	27.324903
252.105159	10114.073128	27.329920
253.007895	10131.356417	27.334938
252.844982	10173.548607	27.339956
253.740192	10182.722481	27.344973
253.918619	10198.599868	27.349991
254.175114	10222.431273	27.355008
254.715625	10221.366358	27.360026
255.027975	10242.969454	27.365044
255.260391	10254.967404	27.370061
255.574256	10268.196310	27.375079
255.612582	10291.874537	27.380096
256.033564	10301.362988	27.385114
256.444065	10313.454947	27.390132
256.837495	10325.012481	27.395149
257.411211	10335.730716	27.400167
257.355381	10339.991917	27.405184
257.865074	10347.236953	27.410202
257.907086	10362.130920	27.415220
258.446513	10378.247592	27.420237
258.169936	10372.012130	27.425255
258.377849	10390.741653	27.430272
258.920042	10398.669786	27.435290
258.749580	10417.092296	27.440308
258.984623	10441.599012	27.445325
259.328522	10447.252538	27.450343
260.169483	10456.431141	27.455360
260.594086	10449.731928	27.460378
261.025085	10454.462838	27.465396
261.263446	10454.905785	27.470413
261.745388	10457.335101	27.475431
261.428654	10483.134103	27.480448
261.758317	10481.884694	27.485466
261.896085	10490.417982	27.490484
261.820271	10485.114063	27.495501
262.460792	10497.040666	27.500519
262.036787	10505.526850	27.505536
262.563756	10518.618579	27.510554
262.736413	10530.932693	27.515572
262.903043	10551.579419	27.520589
263.463601	10563.385829	27.525607
263.315072	10581.691304	27.530624
263.785700	10603.192111	27.535642
264.146239	10608.609614	27.540660
264.406553	10629.078066	27.545677
264.794216	10627.483045	27.550695
264.783203	10637.758032	27.555712
265.013400	10652.657831	27.560730
265.647274	10663.794611	27.565748
265.767915	10676.362011	27.570765
266.391266	10684.085694	27.575783
266.151553	10696.699117	27.580800
266.134998	10701.290918	27.585818
266.473146	10720.319978	27.590836
266.439479	10743.798461	27.595853
266.948808	10750.197495	27.600871
266.922984	10763.872696	27.605888
267.876357	10789.517519	27.610906
268.159990	10797.546899	27.615924
268.405787	10805.138369	27.620941
268.929156	10806.914527	27.625959
269.271583	10830.829803	27.630976
269.285766	10838.451532	27.635994
269.444651	10847.323357	27.641012
269.928265	10861.335236	27.646029
270.048153	10866.248816	27.651047
270.088600	10884.479691	27.656064
270.442065	10899.355436	27.661082
270.856452	10900.652302	27.666100
270.874892	10930.786580	27.671117
271.353213	10939.063170	27.676135
271.543027	10963.160813	27.681152
271.930836	10978.809240	27.686170
272.031664	10987.642240	27.691188
271.636073	11006.323053	27.696205
272.589887	11015.501547	27.701223
272.246691	11043.762806	27.706240
272.521918	11068.058712	27.711258
273.387437	11085.253277	27.716276
273.082642	11112.612956	27.721293
273.600476	11129.678051	27.726311
273.498295	11159.995746	27.731328
273.881193	11180.051478	27.736346
274.145059	11205.884484	27.741364
274.546718	11227.120577	27.746381
274.842619	11244.420823	27.751399
274.922958	11280.940251	27.756416
275.514854	11293.329646	27.761434
275.814433	11314.980485	27.766452
276.042068	11341.467625	27.771469
276.216823	11359.267843	27.776487
276.436208	11386.894297	27.781504
276.808062	11413.613713	27.786522
277.451783	11434.060014	27.791540
277.511450	11458.538436	27.796557
277.914597	11473.532268	27.801575
278.015852	11495.965917	27.806592
278.407970	11509.109929	27.811610
279.456811	11499.022164	27.816628
279.490836	11506.825191	27.821645
280.019761	11497.674403	27.826663
280.427280	11512.774687	27.831680
280.784124	11521.124404	27.836698
281.102253	11526.525847	27.841716
280.615409	11536.859318	27.846733
281.117022	11525.409149	27.851751
281.037774	11542.737767	27.856768
281.088530	11551.915333	27.861786
281.449681	11577.105023	27.866804
281.343997	11593.840937	27.871821
281.961199	11619.450137	27.876839
282.415197	11636.465245	27.881856
282.560775	11653.835819	27.886874
282.755514	11663.289779	27.891892
283.141519	11692.593391	27.896909
283.534060	11709.436296	27.901927
283.742317	11724.813630	27.906944
283.988592	11733.478691	27.911962
284.438266	11750.811431	27.916980
284.352629	11769.975820	27.921997
284.803440	11791.029291	27.927015
285.196767	11806.045601	27.932032
285.584191	11826.648221	27.937050
286.012843	11843.034344	27.942068
285.785907	11865.051955	27.947085
286.279852	11880.607412	27.952103
286.657780	11911.120008	27.957120
286.896285	11928.041549	27.962138
287.434980	11939.170308	27.967156
287.405741	11973.858273	27.972173
287.563369	11974.259944	27.977191
287.790156	11997.895740	27.982208
287.951287	12016.833730	27.987226
288.953634	12021.591681	27.992244
288.964759	12045.371678	27.997261
289.475473	12053.296567	28.002279
289.909085	12068.424415	28.007296
289.742447	12091.090766	28.012314
290.130397	12097.470165	28.017332
289.988133	12121.293899	28.022349
290.447579	12141.290415	28.027367
290.999181	12153.523471	28.032384
291.260249	12174.676152	28.037402
291.388574	12193.076244	28.042420
291.592504	12210.705332	28.047437
292.389198	12215.186538	28.052455
293.706651	12212.568348	28.057472
293.986135	12220.068026	28.062490
294.455880	12208.473124	28.067508
294.789171	12222.628570	28.072525
295.007008	12219.032595	28.077543
295.223096	12219.047584	28.082560
295.017102	12219.079755	28.087578
295.235712	12217.674317	28.092596
295.119536	12215.407440	28.097613
295.660734	12232.706095	28.102631
295.514604	12246.857052	28.107648
295.670301	12262.518130	28.112666
295.896613	12277.450028	28.117684
295.904320	12294.408355	28.122701
295.941156	12312.841599	28.127719
296.310666	12338.860024	28.132736
296.318921	12355.627621	28.137754
296.565002	12382.537242	28.142772
296.396706	12422.112064	28.147789
296.933951	12452.767002	28.152807
297.057368	12485.171416	28.157824
296.970952	12525.991715	28.162842
297.895179	12555.732604	28.167860
298.089268	12587.163713	28.172877
298.756182	12615.327051	28.177895
299.318044	12643.744852	28.182912
299.561584	12673.711370	28.187930
300.057257	12684.789701	28.192948
300.438043	12714.542067	28.197965
300.400459	12734.988571	28.202983
300.589932	12764.137085	28.208000
300.755425	12787.847570	28.213018
301.623016	12807.087779	28.218036
301.811625	12836.107331	28.223053
301.871927	12852.597004	28.228071
302.172588	12879.405097	28.233088
302.427349	12919.745508	28.238106
302.932344	12937.358452	28.243124
303.334575	12969.038314	28.248141
303.640619	12980.812882	28.253159
304.068542	12998.535244	28.258176
304.260067	13023.302320	28.263194
305.053703	13046.431113	28.268212
305.251975	13065.138568	28.273229
305.945991	13093.252377	28.278247
306.324480	13103.301391	28.283264
306.305845	13116.800802	28.288282
306.986723	13118.414686	28.293300
306.957034	13147.543127	28.298317
306.950248	13159.573184	28.303335
307.306367	13182.553350	28.308352
307.591227	13204.188726	28.313370
307.970922	13217.216462	28.318388
307.921509	13239.257499	28.323405
308.088088	13268.858450	28.328423
308.427146	13286.161344	28.333440
308.391612	13317.103629	28.338458
308.902621	13340.676887	28.343476
309.202657	13378.856098	28.348493
309.644174	13401.290777	28.353511
310.160989	13423.595947	28.358528
310.036554	13446.151330	28.363546
310.867796	13466.441951	28.368564
311.114066	13491.499817	28.373581
311.349277	13503.865346	28.378599
311.802241	13517.768133	28.383616
311.938670	13541.040214	28.388634
312.340578	13559.319292	28.393652
312.349732	13588.813827	28.398669
312.923776	13613.729013	28.403687
313.456409	13626.168175	28.408704
313.086834	13661.625727	28.413722
313.655855	13668.389241	28.418740
313.644298	13694.371102	28.423757
314.019623	13709.559322	28.428775
314.708320	13740.028364	28.433792
314.850366	13768.559473	28.438810
315.600936	13787.554523	28.443828
315.977675	13813.411703	28.448845
315.712311	13827.653804	28.453863
316.289868	13857.828455	28.458880
315.943179	13891.734772	28.463898
316.437553	13908.537271	28.468916
317.194048	13933.612389	28.473933
317.536856	13952.945470	28.478951
318.186666	13974.331744	28.483968
318.661508	13997.530706	28.488986
319.237687	14014.603008	28.494004
319.333998	14029.364910	28.499021
319.855594	14048.153621	28.504039
320.376928	14048.294410	28.509056
320.413050	14073.583052	28.514074
321.175742	14081.133168	28.519092
321.012184	14088.526798	28.524109
320.774864	14117.727215	28.529127
321.208610	14131.337490	28.534144
321.254774	14160.298675	28.539162
321.550961	14182.576489	28.544180
321.847472	14212.208881	28.549197
322.307970	14230.585847	28.554215
323.032970	14247.238831	28.559232
323.129396	14275.595795	28.564250
323.570732	14287.158968	28.569268
324.087238	14317.040715	28.574285
324.590364	14330.063943	28.579303
324.354508	14346.155070	28.584320
325.148572	14364.621605	28.589338
326.256137	14356.274828	28.594356
327.111620	14357.406543	28.599373
327.231570	14359.249100	28.604391
327.544968	14356.906724	28.609408
327.980708	14385.929211	28.614426
328.337677	14392.644254	28.619444
328.443563	14386.664827	28.624461
328.372293	14387.394242	28.629479
328.682473	14380.646856	28.634496
328.720495	14388.494702	28.639514
329.212292	14389.731310	28.644532
328.947569	14402.170589	28.649549
328.976166	14417.095762	28.654567
329.238370	14436.942892	28.659584
329.289062	14460.327115	28.664602
329.560395	14482.029540	28.669620
329.656798	14508.027280	28.674637
329.698319	14536.983616	28.679655
330.397416	14559.798164	28.684672
330.163261	14598.752694	28.689690
330.702582	14636.356306	28.694708
330.839370	14674.637429	28.699725
331.120273	14709.534932	28.704743
331.646079	14735.927583	28.709760
332.026709	14776.115409	28.714778
332.848361	14806.621963	28.719796
333.530435	14837.001174	28.724813
333.570260	14865.007883	28.729831
334.099331	14886.466479	28.734848
334.531436	14906.776852	28.739866
335.112495	14913.658619	28.744884
335.718245	14943.160510	28.749901
335.790284	14955.975963	28.754919
336.547468	14969.734840	28.759936
336.758452	14971.642255	28.764954
337.293908	14995.286206	28.769972
337.343952	15006.212348	28.774989
337.056502	15033.378524	28.780007
337.645118	15060.038357	28.785024
337.816126	15081.858071	28.790042
338.008982	15108.191735	28.795060
338.566432	15126.851006	28.800077
338.610625	15168.252872	28.805095
339.173728	15182.032579	28.810112
339.474617	15215.966179	28.815130
339.489605	15236.466670	28.820148
339.873877	15266.202557	28.825165
340.429012	15301.667494	28.830183
340.716102	15325.936144	28.835200
340.521947	15357.249916	28.840218
340.952631	15393.187205	28.845236
341.259035	15422.931990	28.850253
341.368571	15472.263375	28.855271
341.742327	15496.649833	28.860288
342.321983	15532.749477	28.865306
342.774569	15562.240889	28.870324
343.177849	15599.368730	28.875341
343.540410	15647.605849	28.880359
343.951245	15660.001221	28.885376
344.626915	15688.147831	28.890394
345.246144	15712.650171	28.895412
345.695153	15721.960428	28.900429
345.968285	15755.067572	28.905447
346.461130	15773.363472	28.910464
346.954242	15796.058973	28.915482
347.145144	15801.359107	28.920500
347.955337	15807.238823	28.925517
347.916008	15818.311655	28.930535
348.676591	15820.441827	28.935552
348.857328	15832.501589	28.940570
348.858940	15832.930101	28.945588
349.334742	15851.287335	28.950605
349.301706	15867.231673	28.955623
349.674723	15887.802445	28.960640
349.851728	15909.199751	28.965658
349.828904	15942.969625	28.970676
350.129911	15963.149279	28.975693
350.327313	15991.263296	28.980711
350.676362	16021.098004	28.985728
350.947466	16060.331931	28.990746
350.878527	16097.696303	28.995764
351.254038	16128.100473	29.000781
351.688555	16167.079645	29.005799
352.305481	16194.469477	29.010816
353.317635	16226.896012	29.015834
353.749982	16257.963804	29.020852
354.092470	16275.017020	29.025869
354.410833	16303.170737	29.030887
354.903253	16324.389983	29.035904
355.264661	16351.522772	29.040922
355.286978	16379.494045	29.045940
356.063279	16389.719660	29.050957
355.742084	16422.661999	29.055975
356.630580	16439.801520	29.060992
357.009382	16469.884162	29.066010
357.374567	16498.506265	29.071028
357.381867	16513.689199	29.076045
357.926727	16540.798738	29.081063
358.360121	16566.617407	29.086080
358.684656	16597.439468	29.091098
358.779256	16625.717207	29.096116
359.192076	16640.126088	29.101133
359.825203	16667.026803	29.106151
360.343486	16694.552599	29.111168
360.534920	16719.402470	29.116186
360.788250	16750.050996	29.121204
361.244277	16771.366908	29.126221
360.826776	16811.570328	29.131239
361.720927	16835.872718	29.136256
362.387020	16863.591014	29.141274
362.502340	16898.423751	29.146292
362.959229	16923.884242	29.151309
362.960467	16949.534791	29.156327
363.293998	16984.030780	29.161344
363.614144	17016.074559	29.166362
363.904956	17044.215331	29.171380
364.356337	17075.465833	29.176397
364.218358	17122.651633	29.181415
364.817185	17152.880670	29.186432
365.148534	17185.567638	29.191450
365.601999	17232.396993	29.196468
366.196897	17250.817340	29.201485
366.450559	17277.293782	29.206503
367.248921	17303.806188	29.211520
367.489014	17331.152118	29.216538
367.584989	17365.840952	29.221556
368.170138	17386.074530	29.226573
368.602310	17425.954082	29.231591
368.711502	17444.941874	29.236608
369.213576	17472.414978	29.241626
369.422708	17504.248545	29.246644
370.528503	17532.165335	29.251661
370.632181	17557.909617	29.256679
371.087711	17587.705230	29.261696
371.523081	17592.811116	29.266714
371.705065	17624.315340	29.271732
372.199793	17650.922902	29.276749
372.480787	17669.946145	29.281767
372.383352	17695.241106	29.286784
373.171737	17725.385092	29.291802
373.541280	17765.071234	29.296820
373.978035	17783.779403	29.301837
374.026075	17811.370290	29.306855
374.910883	17833.927344	29.311872
375.188783	17857.805543	29.316890
375.203984	17887.279861	29.321908
375.707201	17907.605364	29.326925
376.211955	17952.025264	29.331943
376.500368	17974.547556	29.336960
376.756739	17997.586179	29.341978
377.080377	18034.468226	29.346996
377.662542	18055.111460	29.352013
377.804463	18087.124770	29.357031
378.500622	18115.662967	29.362048
378.888594	18143.137808	29.367066
379.435397	18167.572618	29.372084
380.337791	18176.336733	29.377101
380.646212	18197.698682	29.382119
381.186843	18204.593489	29.387136
381.820660	18224.174919	29.392154
382.177654	18236.791129	29.397172
382.916689	18244.106009	29.402189
383.014920	18266.748001	29.407207
383.231129	18274.757908	29.412224
383.767045	18283.365739	29.417242
383.750517	18300.870397	29.422260
384.217617	18309.669768	29.427277
384.127787	18340.566054	29.432295
384.419886	18355.764914	29.437312
384.396079	18379.976197	29.442330
384.658782	18414.255510	29.447348
385.136311	18435.598241	29.452365
385.917491	18460.098946	29.457383
386.072333	18490.639830	29.462400
386.438487	18509.088156	29.467418
386.302898	18544.465524	29.472436
386.844179	18572.179667	29.477453
387.085627	18610.168088	29.482471
387.428055	18639.909278	29.487488
387.407659	18666.477451	29.492506
387.676858	18710.298036	29.497524
388.295556	18751.383280	29.502541
388.874180	18782.734987	29.507559
388.805736	18825.420217	29.512576
389.130549	18859.759165	29.517594
389.642494	18912.241788	29.522612
390.445743	18946.090567	29.527629
390.909971	18987.772035	29.532647
391.455097	19021.055032	29.537664
392.030875	19043.605192	29.542682
392.594754	19075.702583	29.547700
393.250549	19106.084629	29.552717
393.436859	19127.230609	29.557735
393.713105	19157.026626	29.562752
394.673247	19180.414536	29.567770
395.006162	19201.855552	29.572788
395.688027	19214.210278	29.577805
396.340625	19228.477818	29.582823
396.460630	19245.685715	29.587840
396.586702	19262.988768	29.592858
396.616837	19299.305826	29.597876
396.790363	19323.494105	29.602893
396.997753	19359.785646	29.607911
397.019044	19391.888331	29.612928
397.203295	19427.849723	29.617946
397.864503	19469.596381	29.622964
398.537163	19513.690480	29.627981
398.582191	19557.870180	29.632999
398.396677	19601.622795	29.638016
399.615529	19651.498510	29.643034
399.911194	19687.278957	29.648052
400.657942	19718.898445	29.653069
400.677341	19760.114081	29.658087
400.773231	19812.264006	29.663104
401.340878	19842.219422	29.668122
401.897110	19882.269596	29.673140
402.309856	19918.572869	29.678157
402.762851	19957.311712	29.683175
402.694759	20008.905369	29.688192
403.510373	20047.017796	29.693210
404.081618	20097.319587	29.698228
404.358890	20144.967744	29.703245
404.550988	20174.817818	29.708263
404.693346	20222.544501	29.713280
405.390542	20262.336476	29.718298
406.143026	20298.114038	29.723316
406.826337	20334.933172	29.728333
407.310343	20367.540243	29.733351
407.211801	20407.617145	29.738368
408.275434	20421.171927	29.743386
408.345589	20460.917301	29.748404
409.070206	20489.773164	29.753421
409.531163	20504.946602	29.758439
410.052856	20532.992148	29.763456
410.946845	20536.006765	29.768474
411.268150	20553.470050	29.773492
411.929898	20564.698649	29.778509
412.561817	20585.093637	29.783527
412.824269	20593.080955	29.788544
413.374081	20606.563107	29.793562
413.689159	20615.853327	29.798580
414.111144	20638.044080	29.803597
414.473600	20641.372138	29.808615
414.495125	20650.547117	29.813632
415.113443	20673.626710	29.818650
415.294799	20697.192767	29.823668
415.401263	20725.010193	29.828685
415.772611	20738.892011	29.833703
415.707014	20783.499106	29.838720
416.010515	20803.288370	29.843738
416.508311	20842.909319	29.848756
416.971034	20880.101731	29.853773
417.261058	20912.147049	29.858791
417.644484	20957.382498	29.863808
418.366337	20979.117061	29.868826
418.355922	21013.784318	29.873844
418.724919	21048.534850	29.878861
419.301867	21077.467483	29.883879
419.389986	21124.436489	29.888896
419.571041	21151.989533	29.893914
420.255734	21204.416549	29.898932
420.508141	21255.030288	29.903949
421.291413	21288.147635	29.908967
420.811833	21340.356716	29.913984
421.843026	21378.370546	29.919002
422.567349	21427.782762	29.924020
423.154854	21463.802362	29.929037
423.983195	21493.998290	29.934055
424.443722	21536.632805	29.939072
425.259263	21544.749711	29.944090
425.620477	21571.618147	29.949108
425.733785	21597.084664	29.954125
426.347441	21636.581955	29.959143
426.716314	21664.661868	29.964160
427.069860	21690.820620	29.969178
427.885600	21722.840450	29.974196
428.244628	21745.502323	29.979213
428.439028	21775.274390	29.984231
428.493499	21809.810722	29.989248
428.878344	21838.203570	29.994266
429.615277	21871.279533	29.999284
429.961106	21899.210820	30.004301
431.464668	21905.986299	30.009319
432.327812	21919.229725	30.014336
432.907204	21923.549026	30.019354
433.297786	21927.408679	30.024372
433.166447	21930.351687	30.029389
433.906679	21942.922344	30.034407
433.907124	21965.781577	30.039424
433.894990	21970.060332	30.044442
434.298154	21986.892904	30.049460
434.712203	22001.008133	30.054477
435.612464	22021.625372	30.059495
435.500233	22040.943274	30.064512
436.035156	22058.037188	30.069530
436.397878	22078.973692	30.074548
436.292235	22101.280430	30.079565
436.693027	22121.075057	30.084583
436.961015	22165.101896	30.089600
437.494882	22196.136439	30.094618
437.901786	22219.008359	30.099636
437.879904	22265.125718	30.104653
438.347579	22303.558312	30.109671
438.759009	22342.319179	30.114688
439.467526	22385.041054	30.119706
439.921771	22419.962705	30.124724
440.256830	22466.647078	30.129741
440.808552	22496.754994	30.134759
440.844483	22546.096028	30.139776
441.402396	22572.913412	30.144794
441.764549	22620.517681	30.149812
442.157428	22671.062659	30.154829
443.136001	22696.423542	30.159847
443.662689	22729.718557	30.164864
444.532413	22758.075578	30.169882
445.176127	22784.654655	30.174900
445.725086	22814.650060	30.179917
446.316315	22834.422343	30.184935
446.652648	22862.378912	30.189952
446.947975	22888.715064	30.194970
447.291537	22913.248335	30.199988
447.169513	22945.790726	30.205005
447.952673	22979.591084	30.210023
448.234814	23011.654313	30.215040
448.400429	23050.960405	30.220058
449.096039	23080.625201	30.225076
449.411199	23120.807895	30.230093
450.144428	23156.433915	30.235111
450.319341	23198.473354	30.240128
450.250739	23246.821848	30.245146
450.924219	23274.147264	30.250164
451.018077	23329.915027	30.255181
451.629600	23375.513637	30.260199
451.676813	23420.101965	30.265216
452.756682	23458.022203	30.270234
453.323508	23501.190647	30.275252
453.537618	23550.005674	30.280269
454.166312	23586.101547	30.285287
454.532238	23627.393304	30.290304
454.869375	23663.129256	30.295322
456.252989	23688.589378	30.300340
456.435049	23726.380183	30.305357
457.189530	23748.115849	30.310375
457.387988	23770.514581	30.315392
457.830451	23795.811256	30.320410
458.207937	23822.645745	30.325428
458.570494	23861.046222	30.330445
458.906158	23882.207210	30.335463
459.237259	23913.645503	30.340480
459.628131	23954.804448	30.345498
459.999555	23989.547925	30.350516
460.160001	24024.371785	30.355533
461.017534	24065.085133	30.360551
461.587056	24106.456705	30.365568
462.057320	24130.818600	30.370586
462.223879	24167.436484	30.375604
462.407754	24229.241645	30.380621
463.281477	24262.423390	30.385639
463.504975	24309.210744	30.390656
463.893200	24353.433928	30.395674
464.636188	24382.222265	30.400692
464.980898	24429.585341	30.405709
465.660257	24468.601603	30.410727
466.350348	24513.950039	30.415744
467.088988	24552.546268	30.420762
467.502674	24581.274655	30.425780
467.886598	24622.739204	30.430797
468.215126	24651.056461	30.435815
468.759218	24693.029975	30.440832
469.075878	24727.957815	30.445850
469.290894	24766.943917	30.450868
469.505478	24806.264548	30.455885
470.194948	24847.131566	30.460903
470.534557	24894.070945	30.465920
471.014922	24931.844816	30.470938
471.964933	24986.323013	30.475956
472.124114	25025.325574	30.480973
472.944114	25057.319370	30.485991
473.306707	25089.309591	30.491008
473.516327	25144.170667	30.496026
474.099290	25177.580649	30.501044
474.562032	25216.279265	30.506061
475.249043	25261.866778	30.511079
475.560800	25306.966677	30.516096
476.163001	25355.136723	30.521114
476.865778	25385.337378	30.526132
477.059661	25430.886811	30.531149
477.487775	25466.472108	30.536167
478.262566	25515.896915	30.541184
478.193490	25559.346666	30.546202
479.020691	25591.690372	30.551220
478.960032	25644.495265	30.556237
479.740475	25681.683078	30.561255
480.342592	25737.535550	30.566272
480.598958	25777.819677	30.571290
480.932968	25809.406029	30.576308
481.383529	25863.385818	30.581325
481.720085	25897.527113	30.586343
482.422542	25935.618432	30.591360
482.485573	25984.299022	30.596378
483.299241	26029.330565	30.601396
483.566326	26075.730355	30.606413
484.100837	26120.765806	30.611431
484.753533	26163.613881	30.616448
485.113278	26211.976119	30.621466
486.029048	26254.855052	30.626484
486.269471	26304.730149	30.631501
486.761935	26334.659340	30.636519
487.375551	26375.050831	30.641536
487.677228	26421.041815	30.646554
488.293548	26461.186977	30.651572
488.908989	26518.049177	30.656589
489.608346	26547.107284	30.661607
490.364171	26589.629576	30.666624
490.210538	26632.531796	30.671642
490.928533	26671.170987	30.676660
491.091346	26716.079232	30.681677
491.633729	26767.970270	30.686695
492.466156	26817.174381	30.691712
492.501902	26872.436652	30.696730
492.918643	26916.503743	30.701748
493.207819	26963.507828	30.706765
493.676693	27010.945004	30.711783
494.055322	27053.801219	30.716800
494.665363	27114.553010	30.721818
495.405046	27159.937723	30.726836
495.663595	27219.544965	30.731853
496.339143	27272.865910	30.736871
497.049491	27326.017002	30.741888
497.556468	27378.389149	30.746906
498.028052	27425.426318	30.751924
498.488338	27475.964312	30.756941
499.171480	27529.492961	30.761959
499.754296	27569.835709	30.766976
500.084645	27626.580005	30.771994
500.852885	27662.704632	30.777012
501.444253	27708.046775	30.782029
502.219698	27751.208986	30.787047
502.950345	27780.535113	30.792064
503.513684	27824.771825	30.797082
503.791919	27861.785337	30.802100
504.545590	27904.626697	30.807117
504.692465	27939.416551	30.812135
505.654554	27961.475302	30.817152
506.105043	28005.097657	30.822170
506.748520	28028.239608	30.827188
507.357608	28068.878729	30.832205
507.446913	28098.763293	30.837223
508.058285	28135.464746	30.842240
508.287997	28175.664320	30.847258
508.644355	28206.809481	30.852276
509.053325	28240.122646	30.857293
509.511152	28284.820300	30.862311
509.802843	28322.933584	30.867328
509.885569	28375.286755	30.872346
510.455109	28418.820328	30.877364
511.489025	28464.621803	30.882381
511.950137	28513.966880	30.887399
512.996302	28533.371157	30.892416
513.833495	28558.856387	30.897434
514.607882	28577.111508	30.902452
515.084127	28608.990904	30.907469
515.517064	28642.070404	30.912487
516.280586	28662.217375	30.917504
516.551701	28687.137219	30.922522
517.039899	28705.561406	30.927540
517.335932	28750.256418	30.932557
517.139468	28787.356374	30.937575
518.088633	28822.054677	30.942592
518.395674	28868.183683	30.947610
518.936277	28908.331663	30.952628
518.967408	28941.597314	30.957645
519.522448	28994.167979	30.962663
520.056933	29036.058943	30.967680
520.548332	29088.751226	30.972698
520.974809	29127.635106	30.977716
521.558233	29181.119622	30.982733
521.552166	29241.100894	30.987751
522.277733	29280.978234	30.992768
522.925350	29344.416387	30.997786
522.972262	29396.561017	31.002804
523.657776	29457.232260	31.007821
524.165584	29521.455417	31.012839
524.827819	29577.341395	31.017856
525.137376	29640.030788	31.022874
525.508545	29691.581177	31.027892
526.158267	29747.043873	31.032909
526.779151	29797.807135	31.037927
527.721668	29843.306024	31.042944
528.117820	29904.608959	31.047962
528.935464	29958.547927	31.052980
529.317239	30012.312471	31.057997
530.381124	30060.646703	31.063015
530.816745	30110.076342	31.068032
531.201234	30154.286447	31.073050
531.653994	30207.080190	31.078068
532.200209	30252.897312	31.083085
532.482410	30311.864114	31.088103
533.218432	30357.772045	31.093120
533.845804	30407.560928	31.098138
534.405510	30457.307903	31.103156
535.161509	30499.404193	31.108173
535.736537	30551.906647	31.113191
536.005960	30591.461209	31.118208
536.875991	30643.496870	31.123226
537.029868	30683.112454	31.128244
537.372091	30729.842978	31.133261
537.667239	30785.394923	31.138279
538.391377	30828.349432	31.143296
538.727301	30881.263020	31.148314
538.762181	30927.289405	31.153332
539.548027	30977.402994	31.158349
539.925397	31035.797367	31.163367
540.882031	31093.840238	31.168384
541.076503	31156.898661	31.173402
541.517517	31212.307036	31.178420
542.103630	31257.185871	31.183437
542.143044	31330.160991	31.188455
543.275710	31390.607613	31.193472
543.916888	31453.357033	31.198490
544.145196	31514.678504	31.203508
544.846039	31573.580913	31.208525
544.911067	31642.368579	31.213543
546.080429	31693.403028	31.218560
546.291824	31761.124714	31.223578
546.836570	31823.188249	31.228596
547.667165	31883.937599	31.233613
547.977440	31956.831001	31.238631
548.553596	32011.063723	31.243648
549.048953	32086.103366	31.248666
549.531374	32152.218022	31.253684
550.244335	32214.913640	31.258701
550.840328	32280.453903	31.263719
551.604225	32344.520305	31.268736
551.775106	32398.788929	31.273754
552.470632	32467.080421	31.278772
553.085359	32527.490254	31.283789
553.784789	32605.261571	31.288807
554.078021	32672.423573	31.293824
555.133757	32720.690698	31.298842
556.014097	32772.011284	31.303860
557.574024	32828.870831	31.308877
557.653144	32881.209488	31.313895
558.475228	32918.313943	31.318912
558.647860	32966.575249	31.323930
558.671436	33019.160513	31.328948
559.764958	33059.349373	31.333965
560.321111	33114.380989	31.338983
560.872248	33164.512531	31.344000
561.435703	33215.298530	31.349018
561.634837	33256.591002	31.354036
562.295876	33314.126830	31.359053
562.588604	33379.994482	31.364071
563.081989	33430.041982	31.369088
564.585520	33466.418564	31.374106
565.229504	33513.186714	31.379124
566.478286	33537.642873	31.384141
567.229597	33580.899166	31.389159
567.689404	33618.366960	31.394176
568.702225	33639.698250	31.399194
568.923075	33665.735116	31.404212
569.496428	33682.249985	31.409229
569.548034	33701.429547	31.414247
569.894940	33728.511630	31.419264
570.405565	33757.440365	31.424282
570.628529	33797.268769	31.429300
571.002180	33838.412747	31.434317
571.064401	33887.516004	31.439335
571.166089	33938.133837	31.444352
572.123425	33998.922296	31.449370
572.298109	34055.000522	31.454388
572.946806	34104.773961	31.459405
573.132042	34180.131129	31.464423
573.815013	34246.187571	31.469440
574.204657	34314.409094	31.474458
574.473181	34378.993701	31.479476
575.236731	34450.651796	31.484493
575.644741	34520.707811	31.489511
576.381565	34592.472043	31.494528
577.017715	34667.214282	31.499546
577.417457	34735.296792	31.504564
578.383243	34800.252643	31.509581
578.617261	34876.412333	31.514599
579.141789	34944.354313	31.519616
580.026343	35010.571537	31.524634
580.873824	35081.586508	31.529652
581.254906	35149.102492	31.534669
581.937143	35222.898569	31.539687
582.168897	35288.632125	31.544704
583.048725	35361.874130	31.549722
583.617974	35428.288935	31.554740
584.581185	35494.718549	31.559757
584.943433	35569.303120	31.564775
585.434865	35631.073284	31.569792
586.500498	35700.004847	31.574810
586.527103	35774.227973	31.579828
587.620106	35831.278014	31.584845
587.872796	35905.062079	31.589863
588.529569	35973.799596	31.594880
589.172279	36047.094459	31.599898
589.528556	36119.681154	31.604916
590.492975	36175.277108	31.609933
591.314984	36246.897562	31.614951
592.066997	36304.578826	31.619968
592.461124	36357.422780	31.624986
593.316488	36420.765155	31.630004
594.069745	36470.243095	31.635021
595.188999	36525.993512	31.640039
595.984042	36558.425876	31.645056
596.979179	36614.191515	31.650074
597.392834	36651.335746	31.655092
598.069296	36688.536033	31.660109
598.683628	36730.014646	31.665127
599.008534	36780.185494	31.670144
599.765159	36817.145041	31.675162
600.010805	36870.050642	31.680180
600.376599	36903.728239	31.685197
600.661274	36946.400179	31.690215
600.983798	37000.186288	31.695232
601.529988	37043.520719	31.700250
601.792483	37105.451896	31.705268
602.319029	37158.673212	31.710285
603.027783	37228.988003	31.715303
603.226620	37287.168036	31.720320
603.725425	37351.884724	31.725338
603.885410	37425.725536	31.730356
604.802175	37499.383324	31.735373
604.927314	37572.952914	31.740391
605.576790	37645.798473	31.745408
606.413487	37734.244145	31.750426
606.679749	37814.132303	31.755444
607.689303	37876.534707	31.760461
608.320458	37953.750358	31.765479
608.930894	38032.538781	31.770496
609.873391	38106.936433	31.775514
610.113562	38197.263785	31.780532
610.818174	38258.517005	31.785549
611.702481	38330.987274	31.790567
612.542658	38398.016753	31.795584
613.550198	38459.518640	31.800602
614.222821	38520.358357	31.805620
615.645020	38581.906415	31.810637
616.021801	38639.798224	31.815655
616.559534	38692.576954	31.820672
617.423790	38736.309163	31.825690
618.001264	38797.750118	31.830708
618.581945	38847.279831	31.835725
619.410272	38899.526366	31.840743
619.426145	38955.397454	31.845760
620.335167	39007.409488	31.850778
621.036492	39063.930598	31.855796
621.975921	39111.896869	31.860813
623.139865	39155.790245	31.865831
623.479737	39195.872426	31.870848
624.550272	39231.220378	31.875866
624.671645	39283.267112	31.880884
624.900118	39331.469409	31.885901
626.127323	39382.730303	31.890919
626.434184	39435.796957	31.895936
626.905082	39483.339349	31.900954
627.373723	39545.047682	31.905972
627.986085	39595.776792	31.910989
628.688541	39647.586088	31.916007
628.795955	39709.003268	31.921024
629.408184	39762.747815	31.926042
629.761757	39838.617192	31.931060
630.233291	39896.837666	31.936077
631.095144	39961.558148	31.941095
631.566550	40026.153167	31.946112
632.101209	40095.776288	31.951130
632.268692	40165.847741	31.956148
632.796538	40222.705193	31.961165
633.143393	40290.245953	31.966183
633.238490	40369.609358	31.971200
634.130223	40444.568155	31.976218
634.823886	40523.854927	31.981236
634.886832	40614.650654	31.986253
635.929192	40695.930585	31.991271
636.465748	40778.740369	31.996288
636.827575	40870.995283	32.001306
637.242910	40953.782410	32.006324
638.037231	41036.372373	32.011341
638.946023	41124.575646	32.016359
639.286610	41227.854814	32.021376
640.528618	41312.102647	32.026394
641.333722	41406.443855	32.031412
641.997745	41484.584216	32.036429
642.916037	41555.943587	32.041447
643.652863	41629.869669	32.046464
644.382202	41712.982092	32.051482
644.765068	41792.554833	32.056500
645.374138	41863.930467	32.061517
646.714168	41947.674980	32.066535
646.589424	42022.725856	32.071552
647.296015	42094.297208	32.076570
647.728193	42178.551918	32.081588
648.596381	42261.968206	32.086605
649.125758	42345.379760	32.091623
649.699427	42438.745957	32.096640
650.572294	42506.188823	32.101658
651.182190	42605.697289	32.106676
652.147635	42687.968420	32.111693
653.190473	42762.042311	32.116711
653.602140	42838.990639	32.121728
654.055628	42907.343545	32.126746
654.655173	42998.099940	32.131764
655.310851	43077.985039	32.136781
656.166299	43165.291359	32.141799
655.947485	43252.794753	32.146816
657.329651	43331.454458	32.151834
658.046087	43418.176341	32.156852
658.557164	43508.435653	32.161869
659.487174	43587.688589	32.166887
660.175554	43675.556383	32.171904
660.837101	43747.305943	32.176922
661.859480	43830.333319	32.181940
662.521518	43897.021544	32.186957
663.853977	43963.345689	32.191975
664.215895	44030.227898	32.196992
664.995611	44098.668173	32.202010
665.470868	44172.184872	32.207028
666.470064	44233.202002	32.212045
667.238926	44290.838897	32.217063
667.677782	44364.984666	32.222080
668.125625	44427.198951	32.227098
668.797791	44499.511637	32.232116
668.862657	44564.981390	32.237133
669.384664	44629.113072	32.242151
670.058594	44707.985107	32.247168
670.641767	44768.787868	32.252186
671.794517	44834.504810	32.257204
672.674960	44895.866524	32.262221
673.529670	44959.493906	32.267239
673.706081	45030.955649	32.272256
674.742837	45089.758563	32.277274
675.620604	45173.002919	32.282292
676.101560	45236.651047	32.287309
676.643466	45298.580489	32.292327
676.893922	45372.866681	32.297344
677.687832	45442.111498	32.302362
678.089830	45518.655520	32.307380
678.646926	45601.129288	32.312397
679.507127	45673.568973	32.317415
680.142355	45759.816513	32.322432
680.724671	45838.336281	32.327450
681.643102	45917.045122	32.332468
681.467277	46010.838398	32.337485
682.402493	46092.835807	32.342503
683.484830	46183.960558	32.347520
684.021470	46266.339644	32.352538
684.505539	46352.419951	32.357556
685.189377	46442.767822	32.362573
686.009474	46529.587215	32.367591
686.321314	46627.190825	32.372608
687.315461	46714.265474	32.377626
687.948214	46808.565250	32.382644
688.068985	46903.161640	32.387661
689.154042	46993.433900	32.392679
689.687811	47092.947337	32.397696
690.394973	47182.400911	32.402714
691.312919	47274.203299	32.407732
691.677787	47377.464447	32.412749
692.397473	47466.563468	32.417767
693.152351	47567.317442	32.422784
694.196606	47650.405094	32.427802
695.793145	47730.571761	32.432820
696.617761	47806.859864	32.437837
697.326984	47891.954671	32.442855
697.703285	47983.531076	32.447872
698.461673	48057.750130	32.452890
699.628847	48137.451958	32.457908
700.139842	48223.883460	32.462925
701.125065	48290.601154	32.467943
701.502897	48367.921867	32.472960
701.903238	48449.158705	32.477978
702.829432	48521.910532	32.482996
703.600479	48604.739569	32.488013
704.437381	48684.613941	32.493031
704.980242	48767.065839	32.498048
705.708318	48836.890088	32.503066
705.847630	48919.146446	32.508084
706.489713	49003.357460	32.513101
707.051503	49067.569822	32.518119
707.963830	49141.482395	32.523136
708.378600	49226.314499	32.528154
709.479951	49306.310381	32.533172
709.969170	49382.709539	32.538189
711.061430	49459.169943	32.543207
711.856070	49543.856236	32.548224
712.337904	49619.423704	32.553242
713.304911	49684.497341	32.558260
713.604548	49767.715335	32.563277
714.626350	49846.280389	32.568295
715.044484	49931.980481	32.573312
715.573459	50011.944655	32.578330
716.075055	50094.409256	32.583348
716.771408	50196.412530	32.588365
717.475249	50279.696136	32.593383
718.444319	50372.657421	32.598400
719.020995	50454.731630	32.603418
719.561169	50550.319547	32.608436
720.187141	50652.210906	32.613453
720.882688	50738.858894	32.618471
721.996831	50842.765099	32.623488
722.285955	50941.057697	32.628506
723.039842	51033.509343	32.633524
723.763073	51133.908185	32.638541
724.764205	51228.169521	32.643559
725.416490	51331.140260	32.648576
726.068778	51414.696564	32.653594
727.221375	51503.556730	32.658612
727.717138	51601.337075	32.663629
728.678985	51699.000159	32.668647
729.443414	51786.196964	32.673664
730.245829	51885.000258	32.678682
730.846314	51957.864939	32.683700
731.612626	52064.768800	32.688717
732.824726	52157.242020	32.693735
733.133877	52241.833617	32.698752
734.301811	52334.732237	32.703770
734.968181	52423.483989	32.708788
735.615283	52507.658696	32.713805
736.191796	52588.876255	32.718823
737.627395	52672.114172	32.723840
738.179211	52745.912580	32.728858
739.284574	52825.922177	32.733876
739.981615	52901.692897	32.738893
741.068767	52973.448070	32.743911
741.381099	53057.019031	32.748928
742.018692	53138.872870	32.753946
742.999206	53212.479536	32.758964
743.141196	53290.823676	32.763981
744.174301	53373.495328	32.768999
744.933872	53462.071499	32.774016
745.376938	53545.590534	32.779034
746.226850	53624.225435	32.784052
746.846308	53700.290521	32.789069
748.059113	53761.702360	32.794087
748.912251	53826.967213	32.799104
749.945066	53897.938894	32.804122
750.945056	53945.158020	32.809140
751.284126	54019.781142	32.814157
752.149287	54087.957739	32.819175
752.800110	54144.216130	32.824192
753.290145	54226.813760	32.829210
754.328715	54298.095508	32.834228
754.877499	54367.350911	32.839245
755.662437	54436.427087	32.844263
756.175368	54514.838889	32.849280
756.582760	54593.964161	32.854298
757.803686	54667.174866	32.859316
758.291937	54752.498452	32.864333
758.978718	54830.944908	32.869351
759.852535	54909.258530	32.874368
759.688882	54996.002864	32.879386
760.359778	55089.138558	32.884404
760.667496	55193.806101	32.889421
762.091481	55287.748952	32.894439
762.431484	55397.669567	32.899456
762.512872	55496.051952	32.904474
763.559356	55597.884117	32.909492
763.985698	55719.425450	32.914509
764.673666	55834.148387	32.919527
765.748449	55948.654056	32.924544
765.970358	56069.809130	32.929562
766.891500	56193.556198	32.934580
767.556032	56301.599854	32.939597
768.460446	56425.028920	32.944615
769.479374	56544.761150	32.949632
770.676851	56663.281746	32.954650
771.705963	56762.468566	32.959668
772.436069	56864.759482	32.964685
772.924377	56972.862203	32.969703
774.340050	57078.285087	32.974720
775.090359	57182.002406	32.979738
776.538909	57269.017561	32.984756
777.671753	57365.655351	32.989773
778.606257	57445.510503	32.994791
779.869857	57531.762174	32.999808
780.221332	57616.824315	33.004826
780.901773	57694.512010	33.009844
781.827144	57788.634118	33.014861
782.431845	57873.875161	33.019879
783.767757	57956.621319	33.024896
784.301198	58040.137270	33.029914
784.812184	58121.243156	33.034932
785.517657	58212.396559	33.039949
786.288208	58299.892529	33.044967
786.469486	58389.651293	33.049984
787.072162	58496.687096	33.055002
788.081970	58573.361077	33.060020
788.395380	58672.148954	33.065037
788.798477	58771.882625	33.070055
789.983995	58869.422356	33.075072
790.041663	58966.865007	33.080090
790.867192	59063.310713	33.085108
791.190023	59180.257760	33.090125
791.625396	59298.917989	33.095143
792.659544	59405.132527	33.100160
793.294757	59525.188259	33.105178
794.247747	59634.401154	33.110196
794.977092	59755.263779	33.115213
795.741707	59880.400111	33.120231
796.876393	59993.881800	33.125248
797.582178	60118.037323	33.130266
798.211450	60232.921602	33.135284
799.278420	60350.550598	33.140301
800.262296	60458.289863	33.145319
801.268200	60566.853946	33.150336
802.083629	60688.326760	33.155354
803.075681	60795.503839	33.160372
804.048397	60912.001796	33.165389
804.471081	61034.378282	33.170407
805.636303	61133.954978	33.175424
806.553334	61254.585683	33.180442
807.350965	61365.022740	33.185460
808.127286	61470.912865	33.190477
808.848469	61588.355319	33.195495
810.005330	61688.770513	33.200512
810.401796	61808.437985	33.205530
811.495503	61906.715855	33.210548
812.036566	62027.554534	33.215565
813.161181	62144.115600	33.220583
813.980513	62254.635867	33.225600
814.890451	62370.116102	33.230618
815.728254	62461.253066	33.235636
816.926942	62574.225966	33.240653
817.538543	62674.189368	33.245671
818.857363	62762.173045	33.250688
819.602209	62888.228647	33.255706
820.520995	62983.690584	33.260724
821.637147	63069.017301	33.265741
822.243724	63163.939314	33.270759
823.445836	63262.167108	33.275776
823.821179	63358.589907	33.280794
825.092581	63452.191927	33.285812
825.757688	63543.862626	33.290829
826.347695	63647.538916	33.295847
827.467464	63741.414754	33.300864
827.837354	63851.173361	33.305882
828.722960	63946.809757	33.310900
829.591854	64040.963817	33.315917
830.157244	64138.773758	33.320935
831.067635	64244.319982	33.325952
831.510983	64353.012876	33.330970
832.446462	64444.160742	33.335988
833.142724	64537.644863	33.341005
833.671215	64636.392778	33.346023
834.652927	64739.153905	33.351040
835.919304	64830.145620	33.356058
836.751095	64915.711922	33.361076
837.944869	65011.970539	33.366093
838.776146	65097.929645	33.371111
839.488598	65184.427873	33.376128
840.289527	65290.130868	33.381146
840.862929	65382.767323	33.386164
842.063309	65482.870895	33.391181
842.521419	65586.187366	33.396199
842.979027	65684.003987	33.401216
843.456163	65795.587853	33.406234
844.278726	65912.297523	33.411252
845.145108	66026.446064	33.416269
845.617322	66145.739685	33.421287
846.352080	66259.665449	33.426304
846.879410	66401.029310	33.431322
847.635858	66519.112999	33.436340
848.680762	66654.396081	33.441357
849.240346	66791.862276	33.446375
850.397032	66917.403614	33.451392
851.337726	67047.952371	33.456410
852.206541	67175.978800	33.461428
853.131351	67305.640344	33.466445
853.569820	67439.413641	33.471463
854.673327	67577.253315	33.476480
855.164754	67714.775075	33.481498
856.173125	67852.259765	33.486516
857.292112	67982.733123	33.491533
858.459460	68129.948807	33.496551
859.211107	68254.833914	33.501568
859.969156	68387.287459	33.506586
860.858963	68517.948764	33.511604
861.384164	68652.264904	33.516621
862.087998	68792.368693	33.521639
863.293331	68922.795046	33.526656
864.317935	69056.724662	33.531674
865.601703	69189.820301	33.536692
865.940627	69319.834672	33.541709
866.737043	69465.750861	33.546727
868.056051	69594.543010	33.551744
868.968885	69731.739922	33.556762
869.906816	69861.591729	33.561780
870.918456	69990.660211	33.566797
871.539536	70124.374682	33.571815
872.966651	70248.498006	33.576832
873.751214	70383.925096	33.581850
874.825704	70505.890660	33.586868
876.261401	70603.163844	33.591885
877.255493	70724.436142	33.596903
879.078619	70829.744821	33.601920
879.590456	70935.107848	33.606938
880.079613	71034.606669	33.611956
881.003380	71120.738569	33.616973
882.250032	71219.299037	33.621991
882.987686	71311.604150	33.627008
883.564538	71415.162350	33.632026
883.974375	71512.001871	33.637044
884.802133	71610.496724	33.642061
885.386641	71726.235289	33.647079
886.541323	71832.017458	33.652096
887.120342	71946.607136	33.657114
887.433617	72074.372011	33.662132
888.562679	72185.991217	33.667149
888.958221	72308.525858	33.672167
890.028576	72440.210752	33.677184
890.865044	72569.084205	33.682202
891.412359	72704.996404	33.687220
892.487690	72818.487411	33.692237
893.071125	72966.816242	33.697255
894.116022	73096.643714	33.702272
894.948974	73232.244623	33.707290
895.958102	73379.826605	33.712308
896.804647	73511.151475	33.717325
897.670869	73655.553187	33.722343
898.533036	73794.220019	33.727360
899.396447	73939.844742	33.732378
900.403268	74084.946205	33.737396
901.365512	74230.378821	33.742413
901.858391	74379.763606	33.747431
903.049730	74513.154215	33.752448
904.531387	74649.924036	33.757466
905.476830	74781.498835	33.762484
906.813931	74903.696885	33.767501
907.897031	75044.692946	33.772519
909.043244	75164.926401	33.777536
910.256814	75292.024403	33.782554
910.830441	75421.674248	33.787572
911.529952	75534.636344	33.792589
912.208892	75674.276111	33.797607
913.853054	75792.492150	33.802624
914.714673	75909.482890	33.807642
915.227274	76037.331395	33.812660
916.317406	76153.949036	33.817677
917.042047	76281.402075	33.822695
917.653953	76419.919402	33.827712
918.613099	76552.704141	33.832730
919.208026	76694.629192	33.837748
920.624085	76809.979927	33.842765
921.094430	76958.512904	33.847783
922.382421	77088.657320	33.852800
923.588694	77218.455921	33.857818
924.022724	77355.681084	33.862836
924.531210	77491.262284	33.867853
925.495321	77640.284513	33.872871
926.513878	77774.616113	33.877888
927.134939	77910.408281	33.882906
928.029738	78046.881865	33.887924
929.049478	78181.133442	33.892941
929.927301	78321.577966	33.897959
930.638938	78455.744764	33.902976
931.504859	78586.444551	33.907994
932.488212	78746.142851	33.913012
933.431828	78870.954010	33.918029
933.863579	79009.752146	33.923047
935.446879	79152.813910	33.928064
935.907942	79294.442911	33.933082
936.944700	79444.761444	33.938100
938.066071	79582.078483	33.943117
939.082386	79734.395224	33.948135
940.093682	79871.593676	33.953152
941.263538	80013.162691	33.958170
941.806485	80159.603801	33.963188
942.773944	80297.780272	33.968205
943.334987	80446.776043	33.973223
944.166065	80600.256401	33.978240
945.340035	80752.350463	33.983258
946.040213	80924.879711	33.988276
947.160314	81074.346888	33.993293
948.394709	81231.242107	33.998311
949.223224	81377.161236	34.003328
951.119116	81517.438400	34.008346
952.168756	81663.580875	34.013364
953.410270	81804.769043	34.018381
954.128126	81936.114368	34.023399
955.614674	82075.130028	34.028416
956.284781	82206.213001	34.033434
957.366134	82349.829882	34.038452
958.751127	82479.115291	34.043469
959.457755	82618.995399	34.048487
960.221655	82760.878597	34.053504
961.489222	82889.926988	34.058522
962.091044	83032.845634	34.063540
963.118623	83164.967422	34.068557
963.659499	83309.372469	34.073575
964.452370	83450.577879	34.078592
965.368085	83598.520818	34.083610
966.261896	83746.601323	34.088628
967.262495	83895.221300	34.093645
967.892333	84041.121584	34.098663
969.411990	84194.368610	34.103680
970.964117	84317.080196	34.108698
971.465159	84463.675896	34.113716
972.569436	84614.946636	34.118733
973.457796	84756.447298	34.123751
974.269898	84908.124314	34.128768
975.164342	85056.250943	34.133786
975.727781	85213.262579	34.138804
976.532775	85365.525920	34.143821
977.357866	85528.443092	34.148839
977.911303	85695.641345	34.153856
978.919212	85857.168953	34.158874
980.058570	86012.979866	34.163892
981.163053	86165.481834	34.168909
982.176729	86325.214454	34.173927
983.027579	86475.426750	34.178944
984.250950	86629.341517	34.183962
984.745842	86790.994973	34.188980
985.678526	86932.102371	34.193997
986.892777	87100.228870	34.199015
987.441012	87263.274966	34.204032
988.701729	87420.441260	34.209050
989.434967	87587.039798	34.214068
990.684397	87744.096239	34.219085
991.905804	87911.126051	34.224103
992.842191	88069.269793	34.229120
994.689810	88216.632683	34.234138
995.329871	88370.652227	34.239156
996.727884	88518.334453	34.244173
998.682461	88660.606091	34.249191
999.784890	88804.252289	34.254208
1001.213109	88933.711191	34.259226
1001.896293	89069.646257	34.264244
1003.148926	89194.560831	34.269261
1004.264682	89319.467847	34.274279
1005.484894	89458.737115	34.279296
1006.294800	89592.273717	34.284314
1007.244400	89726.755482	34.289332
1007.990530	89861.184228	34.294349
1009.282766	89985.475855	34.299367
1009.935556	90118.820742	34.304384
1010.787901	90250.695458	34.309402
1011.324651	90398.979706	34.314420
1012.273652	90543.941010	34.319437
1012.999762	90705.688744	34.324455
1013.619433	90862.316328	34.329472
1014.941122	91015.508093	34.334490
1015.551996	91185.760150	34.339508
1016.695530	91353.263791	34.344525
1017.362302	91515.140974	34.349543
1017.924078	91692.411759	34.354560
1018.945194	91862.870443	34.359578
1019.339879	92052.015172	34.364596
1020.146966	92240.812229	34.369613
1021.594257	92417.449221	34.374631
1022.831457	92601.193860	34.379648
1024.287330	92764.583567	34.384666
1025.333975	92952.325944	34.389684
1026.431472	93123.672790	34.394701
1027.716752	93297.520665	34.399719
1028.510731	93472.131203	34.404736
1030.195209	93632.949157	34.409754
1031.457266	93803.411634	34.414772
1032.309243	93966.855714	34.419789
1033.365876	94137.260703	34.424807
1033.938040	94303.514877	34.429824
1035.265721	94461.481042	34.434842
1036.231142	94626.245712	34.439860
1036.961136	94784.303603	34.444877
1038.030278	94938.176990	34.449895
1038.581009	95112.581128	34.454912
1039.147200	95285.185968	34.459930
1040.284723	95462.353446	34.464948
1041.217607	95636.398250	34.469965
1042.196004	95807.163530	34.474983
1042.943692	95998.582155	34.480000
1044.326652	96174.193258	34.485018
1044.924625	96361.297396	34.490036
1045.833760	96550.673049	34.495053
1047.555865	96737.201305	34.500071
1048.322975	96931.149685	34.505088
1049.550048	97107.104176	34.510106
1050.993840	97293.608214	34.515124
1051.407748	97484.690047	34.520141
1052.377210	97683.604723	34.525159
1053.477064	97886.854456	34.530176
1054.726363	98076.867007	34.535194
1055.674318	98264.311436	34.540212
1056.734266	98452.016640	34.545229
1058.476366	98633.597979	34.550247
1059.526884	98831.963222	34.555264
1060.352699	99022.517499	34.560282
1061.381558	99215.254438	34.565300
1063.108671	99419.061070	34.570317
1063.836541	99607.116499	34.575335
1065.029974	99784.513446	34.580352
1066.123708	99971.293212	34.585370
1067.196660	100159.508853	34.590388
1068.487569	100344.813926	34.595405
1069.962026	100522.636369	34.600423
1071.101632	100711.921017	34.605440
1072.335983	100894.858932	34.610458
1073.622898	101067.911320	34.615476
1074.670107	101234.996861	34.620493
1075.723126	101403.741465	34.625511
1077.080748	101576.272232	34.630528
1078.068174	101749.196794	34.635546
1079.050968	101927.138346	34.640564
1080.065189	102104.024585	34.645581
1081.553816	102283.097725	34.650599
1082.143301	102457.019601	34.655616
1082.911983	102636.129769	34.660634
1083.978174	102819.458222	34.665652
1084.696259	103003.126180	34.670669
1086.370255	103179.273447	34.675687
1086.881771	103380.710243	34.680704
1087.841552	103553.208130	34.685722
1088.614282	103753.007236	34.690740
1089.526365	103954.899084	34.695757
1090.558915	104148.628024	34.700775
1091.226874	104357.442014	34.705792
1092.041815	104553.174304	34.710810
1093.178748	104754.007811	34.715828
1094.044990	104951.266780	34.720845
1095.148256	105150.348499	34.725863
1096.119272	105354.634702	34.730880
1097.232372	105562.761269	34.735898
1098.585524	105760.474806	34.740916
1099.724149	105973.615969	34.745933
1100.755694	106169.221658	34.750951
1101.833035	106387.759772	34.755968
1102.971182	106577.903622	34.760986
1104.287087	106796.328199	34.766004
1105.259407	106999.537337	34.771021
1106.551964	107205.847200	34.776039
1107.558277	107421.783806	34.781056
1108.709659	107627.525702	34.786074
1109.972944	107832.958653	34.791092
1110.916830	108042.640674	34.796109
1112.234388	108253.843737	34.801127
1113.413319	108459.435190	34.806144
1114.546002	108673.916000	34.811162
1116.261734	108877.556570	34.816180
1117.025009	109077.244739	34.821197
1118.460914	109278.656019	34.826215
1119.677878	109490.949932	34.831232
1121.158327	109671.872569	34.836250
1122.913602	109864.847293	34.841268
1123.878209	110068.675958	34.846285
1125.340228	110254.140752	34.851303
1126.513146	110456.213732	34.856320
1127.538066	110633.192142	34.861338
1128.705281	110828.731935	34.866356
1129.843385	111017.044351	34.871373
1130.839753	111198.313215	34.876391
1131.772315	111404.893599	34.881408
1132.903746	111583.608099	34.886426
1134.368862	111772.275029	34.891444
1134.813713	111977.853625	34.896461
1136.516462	112177.061195	34.901479
1137.102631	112370.202788	34.906496
1138.109784	112568.784751	34.911514
1138.949546	112775.175745	34.916532
1139.797065	112991.778483	34.921549
1140.936370	113194.206403	34.926567
1142.406505	113407.398985	34.931584
1143.836912	113608.943841	34.936602
1145.409877	113806.728134	34.941620
1146.560533	114010.642314	34.946637
1147.744535	114205.708604	34.951655
1148.658414	114408.310486	34.956672
1149.660076	114611.152181	34.961690
1150.841637	114811.645863	34.966708
1152.221057	115007.558427	34.971725
1154.364788	115181.700414	34.976743
1156.088316	115368.294469	34.981760
1156.909583	115548.696256	34.986778
1158.098269	115719.457261	34.991796
1159.040433	115902.184636	34.996813
1159.656367	116067.508658	35.001831
1160.374284	116252.303971	35.006848
1161.207026	116438.563309	35.011866
1162.303948	116630.772021	35.016884
1163.102509	116816.190680	35.021901
1164.306987	117016.290317	35.026919
1165.591707	117215.325878	35.031936
1166.282095	117434.155892	35.036954
1167.399345	117628.623234	35.041972
1167.649323	117849.685915	35.046989
1168.896054	118066.005146	35.052007
1170.090041	118301.279296	35.057024
1170.910506	118525.011850	35.062042
1172.261577	118764.039032	35.067060
1172.950407	118993.690154	35.072077
1174.049825	119243.028683	35.077095
1174.817611	119483.162658	35.082112
1175.932459	119751.460567	35.087130
1177.131985	119994.604165	35.092148
1178.149451	120260.566265	35.097165
1179.399853	120513.235198	35.102183
1180.565694	120766.351627	35.107200
1181.783829	121027.014316	35.112218
1183.079710	121278.984931	35.117236
1184.131185	121544.952645	35.122253
1185.671019	121802.892971	35.127271
1187.817981	122038.439119	35.132288
1189.536220	122276.874016	35.137306
1191.902171	122486.823821	35.142324
1193.247973	122720.332603	35.147341
1194.645186	122936.547402	35.152359
1195.987662	123155.079749	35.157376
1197.193069	123382.344118	35.162394
1198.414477	123590.507706	35.167412
1199.180858	123811.196578	35.172429
1200.775709	124028.956891	35.177447
1201.778559	124246.642662	35.182464
1202.820215	124467.897509	35.187482
1204.000352	124681.056611	35.192500
1205.582545	124898.521079	35.197517
1207.033099	125106.465619	35.202535
1208.402919	125324.996101	35.207552
1209.283042	125543.409165	35.212570
1210.361727	125757.201462	35.217588
1210.905610	125981.429579	35.222605
1212.351007	126192.842575	35.227623
1213.459669	126425.038556	35.232640
1214.199667	126658.452828	35.237658
1215.535657	126882.437749	35.242676
1216.608187	127117.636450	35.247693
1218.111458	127346.032461	35.252711
1219.444551	127575.587399	35.257728
1220.066044	127802.844768	35.262746
1221.340052	128018.609185	35.267764
1222.597379	128250.108733	35.272781
1224.077354	128456.739583	35.277799
1225.917987	128670.979068	35.282816
1226.526626	128881.425239	35.287834
1228.054993	129088.204035	35.292852
1229.529351	129312.702254	35.297869
1230.197208	129529.937089	35.302887
1231.351066	129754.721460	35.307904
1232.383970	129966.750109	35.312922
1233.612321	130196.164459	35.317940
1234.295481	130440.378840	35.322957
1235.038023	130674.075780	35.327975
1236.174708	130920.916338	35.332992
1237.107099	131179.304532	35.338010
1238.294339	131436.548247	35.343028
1239.183841	131698.941234	35.348045
1240.265071	131964.548925	35.353063
1241.316493	132235.678588	35.358080
1242.332072	132511.532700	35.363098
1243.222129	132792.240827	35.368116
1244.588503	133076.749224	35.373133
1246.303922	133359.869152	35.378151
1248.197727	133625.262462	35.383168
1249.995822	133886.135525	35.388186
1252.396519	134139.401988	35.393204
1253.722490	134401.653113	35.398221
1254.972367	134654.245708	35.403239
1256.590302	134885.604114	35.408256
1257.896911	135133.524944	35.413274
1259.141624	135368.944347	35.418292
1260.228417	135622.472370	35.423309
1261.504359	135871.494287	35.428327
1262.629683	136118.806813	35.433344
1263.794769	136372.834248	35.438362
1264.880073	136616.239442	35.443380
1265.953901	136876.359595	35.448397
1267.091566	137134.125136	35.453415
1268.152605	137406.043327	35.458432
1269.128302	137668.189688	35.463450
1270.315334	137934.587603	35.468468
1271.710639	138206.340829	35.473485
1272.780710	138474.931202	35.478503
1274.339835	138753.596590	35.483520
1275.017655	139032.668694	35.488538
1275.905954	139321.420016	35.493556
1277.326610	139595.538364	35.498573
1278.494611	139886.833285	35.503591
1279.782126	140172.644907	35.508608
1281.131952	140459.272440	35.513626
1283.058251	140733.972582	35.518644
1284.194492	141027.577654	35.523661
1285.800548	141300.016465	35.528679
1287.824664	141559.375152	35.533696
1288.706376	141837.014489	35.538714
1290.187931	142092.310574	35.543732
1291.299246	142347.976224	35.548749
1292.283050	142605.707233	35.553767
1293.499408	142872.568972	35.558784
1294.368253	143140.024814	35.563802
1295.284495	143410.746398	35.568820
1296.429009	143685.780778	35.573837
1298.048043	143967.913942	35.578855
1299.542496	144245.758787	35.583872
1300.980706	144521.078994	35.588890
1302.264361	144792.762619	35.593908
1303.919343	145066.477277	35.598925
1305.161108	145341.964153	35.603943
1306.637120	145598.566980	35.608960
1307.994436	145876.536536	35.613978
1309.800775	146138.121546	35.618996
1311.313483	146408.154602	35.624013
1312.472652	146671.452196	35.629031
1313.720545	146934.952086	35.634048
1314.867663	147204.406714	35.639066
1315.951875	147479.441915	35.644084
1317.549677	147753.706347	35.649101
1318.581602	148025.089100	35.654119
1320.265025	148293.090010	35.659136
1321.587813	148583.198318	35.664154
1322.646095	148845.602644	35.669172
1324.273460	149126.924080	35.674189
1325.290073	149393.537614	35.679207
1327.044005	149666.520906	35.684224
1328.523382	149952.478010	35.689242
1329.858802	150221.972759	35.694260
1331.184388	150495.022624	35.699277
1332.420804	150763.777094	35.704295
1334.111532	151032.722051	35.709312
1335.300871	151316.062613	35.714330
1336.074275	151588.758126	35.719348
1337.631541	151865.925859	35.724365
1338.828790	152156.412589	35.729383
1340.237299	152438.988139	35.734400
1340.948619	152737.794735	35.739418
1342.093786	153021.852954	35.744436
1343.698450	153310.109412	35.749453
1344.985586	153613.644400	35.754471
1346.523694	153899.696679	35.759488
1347.920911	154208.900346	35.764506
1349.526359	154493.524637	35.769524
1350.801527	154780.554300	35.774541
1352.144247	155079.105607	35.779559
1353.639669	155365.201097	35.784576
1354.758812	155666.141883	35.789594
1355.818476	155961.411856	35.794612
1357.656496	156256.944025	35.799629
1358.939080	156549.782503	35.804647
1360.547273	156834.308722	35.809664
1361.847997	157129.431761	35.814682
1363.500584	157396.637687	35.819700
1365.091241	157662.384340	35.824717
1365.542686	157929.367987	35.829735
1367.066763	158217.673392	35.834752
1368.502375	158489.528756	35.839770
1369.578452	158770.772146	35.844788
1370.953838	159053.374440	35.849805
1372.036223	159351.126150	35.854823
1373.859129	159621.450946	35.859840
1374.992247	159914.173952	35.864858
1376.921107	160185.943258	35.869876
1378.083500	160467.411641	35.874893
1379.210081	160756.500390	35.879911
1380.490731	161046.617791	35.884928
1382.066364	161344.451399	35.889946
1383.159830	161642.521862	35.894964
1385.259455	161927.341250	35.899981
1386.549413	162221.461633	35.904999
1388.100529	162499.159384	35.910016
1389.060193	162799.671447	35.915034
1390.372595	163096.953228	35.920052
1391.836941	163388.031955	35.925069
1393.045370	163695.917454	35.930087
1394.749272	163996.399210	35.935104
1396.118594	164293.108417	35.940122
1397.275307	164590.414300	35.945140
1399.115705	164886.374387	35.950157
1401.301014	165163.764804	35.955175
1403.536750	165437.722391	35.960192
1405.040945	165714.585696	35.965210
1406.846805	165987.211783	35.970228
1408.420820	166259.219386	35.975245
1409.564704	166530.033356	35.980263
1411.080363	166797.130882	35.985280
1412.970022	167060.904877	35.990298
1413.897404	167327.421000	35.995316
1415.596406	167589.847576	36.000333
1416.607076	167855.616553	36.005351
1418.041626	168114.132331	36.010368
1419.075182	168399.353376	36.015386
1419.932934	168682.829737	36.020404
1421.114404	168966.468154	36.025421
1422.118879	169262.130364	36.030439
1423.223817	169569.946761	36.035456
1424.375269	169876.209060	36.040474
1424.997349	170193.553458	36.045492
1426.368637	170513.385918	36.050509
1427.478308	170839.305818	36.055527
1429.022187	171161.587694	36.060544
1430.441739	171499.984333	36.065562
1432.010942	171822.520147	36.070580
1433.905695	172135.306892	36.075597
1435.249404	172469.865450	36.080615
1436.356350	172790.456371	36.085632
1437.983152	173111.290397	36.090650
1439.291798	173429.718969	36.095668
1440.869668	173738.242716	36.100685
1442.220997	174049.573805	36.105703
1443.669392	174362.463939	36.110720
1445.242549	174685.614518	36.115738
1446.184155	174996.247526	36.120756
1447.709409	175318.674325	36.125773
1448.732013	175652.179958	36.130791
1449.935627	175977.965799	36.135808
1451.449472	176307.546187	36.140826
1452.745535	176644.146386	36.145844
1454.612315	176976.602483	36.150861
1456.208219	177318.397495	36.155879
1458.070323	177645.312423	36.160896
1459.462230	177982.488844	36.165914
1460.961628	178320.029828	36.170932
1462.894291	178640.884870	36.175949
1464.496528	178969.477214	36.180967
1466.123795	179291.645043	36.185984
1467.610660	179609.155394	36.191002
1469.037045	179939.548129	36.196020
1470.696236	180279.206690	36.201037
1471.888582	180611.293677	36.206055
1473.261584	180941.841378	36.211072
1474.617025	181279.997073	36.216090
1475.705173	181624.661278	36.221108
1477.585552	181953.985988	36.226125
1479.297731	182303.497936	36.231143
1481.219159	182633.441676	36.236160
1482.586036	182963.977331	36.241178
1484.389456	183308.707434	36.246196
1485.748313	183634.818532	36.251213
1487.058657	183971.767283	36.256231
1488.513032	184309.137684	36.261248
1489.983187	184648.132177	36.266266
1490.960602	184984.686999	36.271284
1492.822467	185334.725464	36.276301
1493.657235	185687.264800	36.281319
1495.101938	186030.206937	36.286336
1496.469191	186402.055702	36.291354
1497.563490	186837.905931	36.296372
1499.399525	187205.147849	36.301389
1500.363311	187573.988470	36.306407
1502.039261	187935.930799	36.311424
1503.594424	188309.054318	36.316442
1504.917461	188692.489669	36.321460
1506.145275	189052.915977	36.326477
1507.716375	189434.168243	36.331495
1509.027010	189816.102213	36.336512
1510.862545	190204.765817	36.341530
1512.444734	190588.727385	36.346548
1513.547880	190974.906061	36.351565
1514.979939	191371.707316	36.356583
1516.258088	191743.959838	36.361600
1517.916619	192125.048750	36.366618
1519.331432	192525.237149	36.371636
1520.763489	192891.097113	36.376653
1522.579072	193266.008794	36.381671
1523.913898	193639.164099	36.386688
1525.593890	194012.262491	36.391706
1527.000419	194388.482146	36.396724
1529.265696	194752.851642	36.401741
1531.441049	195119.930034	36.406759
1533.119997	195481.521967	36.411776
1534.802084	195854.109924	36.416794
1536.064264	196204.160396	36.421812
1538.552843	196556.376971	36.426829
1539.686025	196911.328435	36.431847
1541.019360	197269.015247	36.436864
1542.446901	197622.625028	36.441882
1544.113598	198002.654657	36.446900
1545.714431	198355.717985	36.451917
1547.340887	198721.144977	36.456935
1549.143472	199083.687032	36.461952
1550.625484	199436.572979	36.466970
1552.210541	199782.040948	36.471988
1554.112609	200137.956445	36.477005
1555.653380	200498.252397	36.482023
1556.813562	200860.532474	36.487040
1558.495755	201223.791556	36.492058
1559.358009	201598.810380	36.497076
1560.517945	201982.883872	36.502093
1561.891612	202356.981015	36.507111
1563.296526	202746.857135	36.512128
1564.838197	203141.105074	36.517146
1565.934360	203538.859533	36.522164
1567.384594	203939.323472	36.527181
1569.148285	204348.928720	36.532199
1570.425846	204741.401631	36.537216
1572.514815	205152.606094	36.542234
1573.911016	205557.061874	36.547252
1575.977077	205953.938899	36.552269
1577.526924	206358.194671	36.557287
1578.956881	206768.923418	36.562304
1581.052949	207164.925102	36.567322
1582.524369	207567.486083	36.572340
1584.989908	207959.034900	36.577357
1586.767615	208349.877881	36.582375
1588.401635	208730.055527	36.587392
1590.158137	209123.572294	36.592410
1591.404106	209509.127607	36.597428
1593.057766	209895.402169	36.602445
1595.153143	210275.177549	36.607463
1597.032468	210649.683651	36.612480
1598.955530	211022.202912	36.617498
1600.112654	211398.359547	36.622516
1601.903542	211761.533074	36.627533
1603.750324	212132.850935	36.632551
1605.372431	212517.948592	36.637568
1606.988557	212889.994704	36.642586
1608.183014	213241.796592	36.647604
1610.117791	213598.324034	36.652621
1611.077642	213953.013231	36.657639
1612.032716	214328.098847	36.662656
1613.617650	214676.943909	36.667674
1614.955590	215054.963764	36.672692
1616.491964	215421.090308	36.677709
1618.333887	215806.189026	36.682727
1619.405992	216179.610838	36.687744
1621.125400	216567.120866	36.692762
1622.230954	216967.055574	36.697780
1623.573352	217357.731702	36.702797
1625.113320	217754.013960	36.707815
1625.963952	218172.995003	36.712832
1627.689699	218593.580479	36.717850
1629.335444	219022.512098	36.722868
1630.981624	219459.649182	36.727885
1632.167821	219883.710042	36.732903
1633.461379	220322.765012	36.737920
1634.750102	220762.228916	36.742938
1636.874597	221199.138591	36.747956
1638.528329	221637.197250	36.752973
1641.459236	222073.743664	36.757991
1643.132469	222524.248050	36.763008
1644.728846	222944.033700	36.768026
1646.057524	223387.589975	36.773044
1647.781383	223828.159261	36.778061
1649.487590	224276.708710	36.783079
1651.934396	224691.147825	36.788096
1654.536040	225100.227778	36.793114
1656.497665	225519.705606	36.798132
1658.546306	225928.450984	36.803149
1660.293832	226345.859857	36.808167
1662.217741	226747.237591	36.813184
1664.160797	227136.751208	36.818202
1665.893020	227544.488796	36.823220
1667.582466	227949.212218	36.828237
1669.019081	228341.330504	36.833255
1670.547123	228745.880594	36.838272
1672.040359	229153.689069	36.843290
1673.215699	229563.737536	36.848308
1674.559577	229975.536356	36.853325
1676.142359	230392.705836	36.858343
1677.651665	230826.374337	36.863360
1679.218629	231247.028758	36.868378
1680.737040	231681.358467	36.873396
1682.221524	232113.332815	36.878413
1683.775781	232541.740158	36.883431
1685.324295	232992.960075	36.888448
1687.262330	233433.217283	36.893466
1688.919501	233868.519539	36.898484
1690.560855	234295.697038	36.903501
1693.023787	234719.559768	36.908519
1694.373384	235155.400361	36.913536
1696.553183	235576.976512	36.918554
1698.594071	235993.827203	36.923572
1700.043796	236393.455808	36.928589
1701.784342	236799.030318	36.933607
1703.253999	237207.573210	36.938624
1704.634609	237611.915392	36.943642
1706.530180	238028.617276	36.948660
1708.099156	238440.269997	36.953677
1709.400716	238851.867620	36.958695
1710.308052	239285.633394	36.963712
1712.297735	239709.180891	36.968730
1714.104858	240143.581771	36.973748
1715.504868	240576.655938	36.978765
1717.514496	241020.219369	36.983783
1718.452248	241471.435266	36.988800
1720.076818	241922.483618	36.993818
1722.014971	242393.724905	36.998836
1723.163487	242856.363568	37.003853
1724.897026	243318.445626	37.008871
1726.200447	243798.028213	37.013888
1727.805614	244267.881469	37.018906
1729.684435	244757.426527	37.023924
1731.118824	245242.475820	37.028941
1732.976133	245724.887737	37.033959
1734.613448	246220.344185	37.038976
1736.369677	246709.785839	37.043994
1738.211253	247212.270584	37.049012
1739.995760	247709.634287	37.054029
1741.571355	248213.003978	37.059047
1743.264363	248734.999919	37.064064
1744.825686	249238.500113	37.069082
1746.358816	249748.254747	37.074100
1747.813286	250283.731198	37.079117
1750.011618	250808.386143	37.084135
1751.110418	251338.996098	37.089152
1752.939816	251872.758444	37.094170
1754.288789	252421.337145	37.099188
1755.655630	252968.541337	37.104205
1757.837950	253516.444606	37.109223
1759.545828	254081.068362	37.114240
1761.448938	254627.825888	37.119258
1763.541060	255175.033896	37.124276
1765.551244	255725.406034	37.129293
1767.448760	256267.770110	37.134311
1769.355108	256825.374635	37.139328
1771.390274	257376.301479	37.144346
1773.614306	257896.026237	37.149364
1776.012505	258423.062651	37.154381
1778.059554	258952.419907	37.159399
1780.063892	259476.525860	37.164416
1782.579838	259986.419947	37.169434
1784.562475	260493.763131	37.174452
1786.704388	261009.588889	37.179469
1788.270643	261508.340325	37.184487
1789.990287	262009.707157	37.189504
1791.784318	262509.841592	37.194522
1793.764851	262980.196758	37.199540
1795.233812	263472.409527	37.204557
1797.165965	263937.971077	37.209575
1798.948587	264410.391239	37.214592
1800.512636	264887.268495	37.219610
1802.097258	265357.714826	37.224628
1803.370511	265832.761083	37.229645
1805.500059	266315.433654	37.234663
1807.282335	266805.506521	37.239680
1809.593125	267288.578810	37.244698
1811.830414	267758.936254	37.249716
1813.788428	268235.335936	37.254733
1816.308762	268692.078662	37.259751
1818.217471	269165.335566	37.264768
1820.011132	269636.223617	37.269786
1821.507575	270108.965399	37.274804
1822.808362	270583.289479	37.279821
1824.803239	271054.471161	37.284839
1826.451160	271547.532188	37.289856
1828.338724	272029.374250	37.294874
1829.732601	272513.078063	37.299892
1831.159935	273002.897225	37.304909
1833.148229	273493.203732	37.309927
1834.904635	274000.162013	37.314944
1836.529511	274508.538831	37.319962
1838.348440	275009.286083	37.324980
1839.761966	275537.942275	37.329997
1841.482854	276041.091754	37.335015
1842.704941	276559.922180	37.340032
1844.502013	277099.812749	37.345050
1846.306794	277637.592194	37.350068
1847.845267	278183.391873	37.355085
1849.359635	278725.028233	37.360103
1851.498879	279284.642089	37.365120
1852.811500	279837.638802	37.370138
1854.868184	280395.917027	37.375156
1856.265664	280974.779722	37.380173
1858.579971	281538.827060	37.385191
1860.391050	282114.135076	37.390208
1862.295218	282682.389005	37.395226
1864.657627	283264.761676	37.400244
1865.987776	283835.929098	37.405261
1868.688150	284390.527248	37.410279
1870.719834	284966.853720	37.415296
1872.060815	285530.595726	37.420314
1874.184108	286093.998477	37.425332
1875.986526	286665.708971	37.430349
1878.335215	287239.736665	37.435367
1880.795309	287816.486067	37.440384
1882.108205	288376.080895	37.445402
1884.183786	288941.232444	37.450420
1885.687706	289512.118027	37.455437
1888.207747	290086.154563	37.460455
1889.812256	290663.646958	37.465472
1891.275342	291219.012399	37.470490
1893.288727	291767.347079	37.475508
1895.030972	292321.618190	37.480525
1897.259119	292862.621356	37.485543
1899.318298	293407.079704	37.490560
1900.815515	293953.968209	37.495578
1902.858825	294499.846231	37.500596
1904.845714	295052.868170	37.505613
1906.661349	295594.766583	37.510631
1908.591172	296148.351329	37.515648
1910.080411	296709.754939	37.520666
1912.277349	297259.300499	37.525684
1914.110736	297830.544311	37.530701
1915.770990	298392.925217	37.535719
1917.658303	298956.889514	37.540736
1919.750767	299539.482613	37.545754
1921.521826	300107.447452	37.550772
1923.058832	300684.642688	37.555789
1925.478345	301257.823049	37.560807
1927.687871	301840.077037	37.565824
1929.606181	302413.183476	37.570842
1931.721356	302991.230297	37.575860
1934.059847	303572.866825	37.580877
1936.064881	304148.562996	37.585895
1938.015771	304731.654833	37.590912
1940.366167	305299.538403	37.595930
1942.609016	305864.160485	37.600948
1944.253252	306439.801194	37.605965
1945.697433	307001.479245	37.610983
1947.648879	307594.937605	37.616000
1949.479691	308175.435373	37.621018
1951.242543	308752.563013	37.626036
1953.305971	309343.322699	37.631053
1955.355215	309932.988356	37.636071
1956.959475	310535.575062	37.641088
1958.868353	311134.448150	37.646106
1961.208100	311712.140511	37.651124
1962.712858	312325.826966	37.656141
1964.690390	312920.483965	37.661159
1966.905227	313530.991649	37.666176
1968.931292	314141.704184	37.671194
1971.221418	314734.692959	37.676212
1973.024497	315341.218082	37.681229
1975.124058	315936.438423	37.686247
1976.935168	316548.664880	37.691264
1978.520801	317156.201521	37.696282
1980.231953	317765.285516	37.701300
1982.372994	318393.156255	37.706317
1984.015759	319012.067006	37.711335
1986.007181	319634.111542	37.716352
1987.793247	320271.419639	37.721370
1989.722451	320889.501781	37.726388
1991.654043	321526.569357	37.731405
1993.850354	322162.188775	37.736423
1996.008096	322800.347279	37.741440
1998.551563	323434.700986	37.746458
2000.441464	324021.199821	37.751476
2002.283875	324628.266109	37.756493
2004.601020	325219.021744	37.761511
2006.973564	325816.464580	37.766528
2008.822510	326409.319504	37.771546
2011.000043	327000.309697	37.776564
2012.732915	327609.648993	37.781581
2014.683014	328209.322895	37.786599
2016.775513	328804.675732	37.791616
2018.007093	329415.833193	37.796634
2020.498851	330020.142615	37.801652
2022.268174	330641.653961	37.806669
2023.850718	331258.696941	37.811687
2026.053504	331874.230688	37.816704
2028.404652	332504.176362	37.821722
2030.729845	333116.248013	37.826740
2032.638470	333742.447058	37.831757
2034.885464	334369.748524	37.836775
2037.323109	334987.033916	37.841792
2038.891271	335617.660304	37.846810
2041.036533	336240.489095	37.851828
2042.867295	336870.522186	37.856845
2044.714190	337510.850192	37.861863
2046.850067	338142.947462	37.866880
2048.479245	338794.870825	37.871898
2050.413658	339445.565873	37.876916
2052.387489	340108.733347	37.881933
2054.106137	340755.843749	37.886951
2056.384048	341420.007393	37.891968
2057.944703	342099.665155	37.896986
2060.006558	342764.405505	37.902004
2061.701009	343459.096814	37.907021
2063.567810	344153.164662	37.912039
2065.274057	344836.691944	37.917056
2067.395115	345546.684320	37.922074
2069.282593	346249.193684	37.927092
2071.094392	346961.729430	37.932109
2073.646070	347675.827715	37.937127
2075.370374	348386.249544	37.942144
2077.114854	349120.180767	37.947162
2079.728135	349840.628685	37.952180
2081.853658	350579.494886	37.957197
2083.318711	351307.017155	37.962215
2085.943864	352040.571017	37.967232
2087.809261	352775.181072	37.972250
2089.896373	353513.876479	37.977268
2092.251893	354247.412931	37.982285
2094.187422	354992.578506	37.987303
2096.614446	355727.446811	37.992320
2098.517654	356479.289511	37.997338
2100.973033	357218.896232	38.002356
2103.346502	357953.860512	38.007373
2105.158078	358696.620207	38.012391
2107.538812	359421.179667	38.017408
2109.936501	360157.012629	38.022426
2112.067087	360873.114691	38.027444
2114.752355	361563.866610	38.032461
2116.652796	362266.587580	38.037479
2118.992355	362962.244440	38.042496
2120.985748	363657.262945	38.047514
2123.186090	364352.918300	38.052532
2125.570447	365036.226539	38.057549
2127.438081	365725.292762	38.062567
2130.009894	366414.251240	38.067584
2132.226784	367109.827243	38.072602
2134.636746	367799.903677	38.077620
2136.893008	368485.148808	38.082637
2139.019840	369168.272617	38.087655
2141.170782	369862.184235	38.092672
2143.053405	370563.686505	38.097690
2145.086132	371246.939133	38.102708
2147.497204	371946.370942	38.107725
2149.549093	372641.488156	38.112743
2152.349161	373332.634187	38.117760
2154.323000	374034.102696	38.122778
2156.788953	374714.576315	38.127796
2159.605929	375402.990069	38.132813
2161.578198	376082.557381	38.137831
2164.431122	376768.781985	38.142848
2166.255180	377449.285586	38.147866
2168.422017	378121.729270	38.152884
2171.082380	378805.434960	38.157901
2172.996976	379481.013324	38.162919
2175.372811	380158.172544	38.167936
2177.367382	380831.833300	38.172954
2179.655411	381505.987846	38.177972
2181.682721	382196.526526	38.182989
2183.804499	382893.423485	38.188007
2186.421776	383572.270626	38.193024
2188.010120	384271.181129	38.198042
2190.079770	384959.295459	38.203060
2191.905588	385651.289983	38.208077
2193.912901	386358.981240	38.213095
2195.888288	387048.866032	38.218112
2197.787301	387773.553920	38.223130
2199.495415	388502.212002	38.228148
2201.660891	389229.532607	38.233165
2203.690298	389965.680343	38.238183
2205.799930	390691.733698	38.243200
2207.653465	391449.446233	38.248218
2209.568230	392192.808724	38.253236
2211.742875	392946.981589	38.258253
2214.060553	393708.460948	38.263271
2216.661396	394454.893937	38.268288
2218.944002	395230.127379	38.273306
2221.492329	395964.771651	38.278324
2224.231316	396709.248313	38.283341
2226.737962	397468.164972	38.288359
2229.121706	398200.069265	38.293376
2230.529730	398944.513127	38.298394
2232.837914	399683.791795	38.303412
2235.138423	400397.510859	38.308429
2237.364740	401116.317601	38.313447
2239.861927	401832.931305	38.318464
2241.654437	402557.374937	38.323482
2243.790242	403278.244622	38.328500
2246.235515	404000.486786	38.333517
2248.027217	404737.794787	38.338535
2250.606693	405460.913062	38.343552
2252.956456	406199.606344	38.348570
2255.117944	406939.831709	38.353588
2257.424896	407684.065106	38.358605
2259.214182	408432.242146	38.363623
2261.599943	409186.122403	38.368640
2263.626307	409943.715633	38.373658
2265.602634	410704.436607	38.378676
2267.703436	411468.736357	38.383693
2269.496062	412248.693866	38.388711
2272.085538	413014.156657	38.393728
2274.536540	413795.424252	38.398746
2276.598632	414588.789721	38.403764
2279.123954	415364.020206	38.408781
2281.317175	416164.734689	38.413799
2283.645469	416958.183752	38.418816
2285.941499	417751.816048	38.423834
2288.468946	418543.864481	38.428852
2290.268045	419335.050209	38.433869
2292.343868	420153.534552	38.438887
2294.604390	420962.642853	38.443904
2296.478790	421792.830244	38.448922
2298.968810	422617.922110	38.453940
2301.754192	423436.454562	38.458957
2303.969155	424268.828789	38.463975
2306.456218	425095.862362	38.468992
2309.095135	425928.815692	38.474010
2311.129159	426759.413402	38.479028
2313.467334	427588.462069	38.484045
2315.286690	428423.088345	38.489063
2318.087394	429252.961463	38.494080
2320.000707	430106.899857	38.499098
2321.905387	430958.733221	38.504116
2324.483255	431818.063251	38.509133
2326.744611	432665.673113	38.514151
2329.245561	433516.095690	38.519168
2331.383953	434382.085910	38.524186
2333.492647	435250.831753	38.529204
2336.005386	436124.434650	38.534221
2337.940607	437008.172657	38.539239
2340.173399	437878.364902	38.544256
2342.771292	438755.241266	38.549274
2344.555856	439643.100663	38.554292
2346.902271	440536.950519	38.559309
2349.167704	441447.726890	38.564327
2351.389302	442334.542992	38.569344
2353.564745	443222.140356	38.574362
2355.631442	444100.968340	38.579380
2358.116501	444977.311526	38.584397
2360.691792	445850.416792	38.589415
2363.171112	446726.689460	38.594432
2365.670542	447599.634964	38.599450
2367.567718	448474.316509	38.604468
2370.175787	449352.026511	38.609485
2372.717833	450242.152081	38.614503
2374.886505	451120.318249	38.619520
2377.329951	452017.161392	38.624538
2379.818169	452916.435792	38.629556
2382.503430	453799.153282	38.634573
2384.307524	454703.573451	38.639591
2387.056326	455603.646168	38.644608
2389.292002	456504.373417	38.649626
2391.461480	457420.996824	38.654644
2394.379888	458320.161330	38.659661
2396.864969	459242.208524	38.664679
2399.058827	460161.331068	38.669696
2401.721296	461076.438919	38.674714
2403.700758	461984.747189	38.679732
2406.357627	462903.460905	38.684749
2408.743382	463830.921118	38.689767
2411.392670	464747.174105	38.694784
2414.132054	465671.150706	38.699802
2416.388866	466596.378360	38.704820
2419.537125	467509.736846	38.709837
2422.013119	468440.952150	38.714855
2424.196620	469355.044151	38.719872
2427.119799	470274.523121	38.724890
2429.578150	471195.400814	38.729908
2432.159786	472113.939078	38.734925
2434.145993	473055.922324	38.739943
2436.308172	473980.754834	38.744960
2439.090520	474914.880551	38.749978
2440.809574	475863.838306	38.754996
2443.539050	476801.513976	38.760013
2446.199627	477753.495911	38.765031
2448.007977	478695.120499	38.770048
2450.706678	479632.302380	38.775066
2452.917697	480592.089774	38.780084
2455.641006	481529.774785	38.785101
2458.497153	482493.187643	38.790119
2460.849083	483443.407391	38.795136
2463.662565	484390.216032	38.800154
2466.052551	485346.183315	38.805172
2468.429384	486303.009558	38.810189
2470.567710	487260.531013	38.815207
2473.006474	488219.361839	38.820224
2475.728243	489174.306229	38.825242
2478.190870	490144.987773	38.830260
2480.880128	491095.340019	38.835277
2483.499276	492059.376983	38.840295
2486.000172	493021.462390	38.845312
2488.814100	493953.671384	38.850330
2491.290787	494885.432682	38.855348
2494.358254	495794.793293	38.860365
2496.859040	496701.073866	38.865383
2499.253817	497611.813068	38.870400
2502.227648	498507.573803	38.875418
2504.228441	499413.489880	38.880436
2506.900261	500310.617164	38.885453
2508.950571	501228.429076	38.890471
2510.865249	502148.986586	38.895488
2512.980319	503085.443613	38.900506
2515.339772	504024.376750	38.905524
2517.684067	504970.771025	38.910541
2519.953088	505918.837036	38.915559
2522.094728	506880.834186	38.920576
2524.613192	507839.382045	38.925594
2526.909612	508817.368479	38.930612
2529.748256	509783.104619	38.935629
2532.178585	510762.158224	38.940647
2534.542442	511752.099357	38.945664
2537.361084	512738.826256	38.950682
2539.192320	513741.886579	38.955700
2541.905316	514742.464173	38.960717
2544.514535	515756.095789	38.965735
2547.091194	516761.857071	38.970752
2549.909073	517769.476364	38.975770
2551.990554	518794.384443	38.980788
2555.047718	519801.375830	38.985805
2557.909689	520826.366689	38.990823
2560.291349	521847.542462	38.995840
2563.117545	522874.818368	39.000858
2565.864540	523904.354256	39.005876
2569.346709	524907.558538	39.010893
2572.711702	525918.167745	39.015911
2575.270170	526918.927107	39.020928
2578.429353	527922.637704	39.025946
2580.615608	528918.592726	39.030964
2582.907044	529914.160266	39.035981
2585.447713	530936.849567	39.040999
2587.734670	531946.323309	39.046016
2590.237862	532964.749276	39.051034
2592.572307	533979.357994	39.056052
2594.708256	535010.535608	39.061069
2596.942161	536036.540288	39.066087
2599.284683	537084.893345	39.071104
2601.675556	538119.476372	39.076122
2604.364882	539172.898988	39.081140
2607.217692	540238.791156	39.086157
2609.364440	541298.335235	39.091175
2611.816781	542361.368432	39.096192
2614.265517	543427.992749	39.101210
2616.784694	544515.091297	39.106228
2619.375196	545589.672188	39.111245
2621.929410	546681.975008	39.116263
2624.318531	547771.856341	39.121280
2626.643601	548843.413028	39.126298
2629.065699	549926.179485	39.131316
2631.789949	551001.972131	39.136333
2634.348328	552070.017823	39.141351
2636.525924	553140.908697	39.146368
2639.128214	554215.812690	39.151386
2642.141639	555294.680554	39.156404
2644.753792	556383.076200	39.161421
2647.710902	557459.617782	39.166439
2650.528930	558551.467904	39.171456
2653.648791	559627.654361	39.176474
2656.233266	560709.469705	39.181492
2659.127472	561783.307824	39.186509
2662.023504	562868.607760	39.191527
2664.389056	563962.444333	39.196544
2667.129253	565043.672104	39.201562
2670.055464	566141.998463	39.206580
2672.477131	567229.824797	39.211597
2675.284189	568320.303975	39.216615
2677.827993	569425.291202	39.221632
2680.926608	570520.551511	39.226650
2683.339198	571626.523773	39.231668
2686.227252	572721.027120	39.236685
2688.973696	573829.257907	39.241703
2691.388368	574956.362174	39.246720
2693.977631	576057.799506	39.251738
2696.753871	577184.991447	39.256756
2699.508651	578310.027953	39.261773
2701.948108	579444.093598	39.266791
2704.654838	580577.457309	39.271808
2707.617539	581705.657931	39.276826
2709.980819	582857.271979	39.281844
2712.844082	583985.729602	39.286861
2715.355845	585132.991190	39.291879
2717.847458	586289.420385	39.296896
2720.665089	587449.441691	39.301914
2723.527328	588611.999152	39.306932
2726.419770	589764.315740	39.311949
2729.161407	590937.741290	39.316967
2731.503379	592108.814207	39.321984
2734.332180	593280.338975	39.327002
2737.020757	594455.627961	39.332020
2739.645740	595643.681994	39.337037
2742.750944	596814.956200	39.342055
2745.600596	598004.033151	39.347072
2748.893742	599177.740795	39.352090
2751.588831	600357.789559	39.357108
2754.409999	601526.632275	39.362125
2757.284309	602705.407787	39.367143
2760.073208	603884.176241	39.372160
2762.969108	605049.942637	39.377178
2765.508779	606234.364878	39.382196
2768.312322	607406.509401	39.387213
2771.303493	608588.305499	39.392231
2773.739411	609781.977587	39.397248
2776.500617	610955.008855	39.402266
2778.970871	612109.661216	39.407284
2781.897692	613259.164525	39.412301
2784.358198	614403.727611	39.417319
2787.011259	615553.088658	39.422336
2789.958414	616696.779891	39.427354
2792.745278	617851.976015	39.432372
2795.603992	619009.586523	39.437389
2798.496063	620160.321082	39.442407
2801.117122	621321.573578	39.447424
2804.183609	622476.778942	39.452442
2807.009110	623638.296318	39.457460
2809.967212	624810.005871	39.462477
2813.115669	625969.766163	39.467495
2815.662097	627132.399671	39.472512
2818.329006	628300.178670	39.477530
2820.987655	629481.861321	39.482548
2823.262169	630685.744753	39.487565
2826.026100	631883.016520	39.492583
2828.411505	633090.398805	39.497600
2830.598809	634306.010119	39.502618
2833.431170	635549.115822	39.507636
2835.950182	636799.161418	39.512653
2837.926925	638041.364975	39.517671
2840.516466	639309.903045	39.522688
2843.343641	640594.404457	39.527706
2846.250058	641882.521013	39.532724
2848.478388	643184.802329	39.537741
2851.713089	644492.478293	39.542759
2854.680033	645801.725581	39.547776
2857.595287	647107.770510	39.552794
2859.711191	648435.362931	39.557812
2862.175563	649767.453546	39.562829
2865.390845	651105.764893	39.567847
2868.211475	652469.720260	39.572864
2871.435937	653822.010771	39.577882
2873.887505	655181.369750	39.582900
2876.691032	656550.738838	39.587917
2879.627118	657911.926261	39.592935
2882.637994	659307.909980	39.597952
2885.215614	660686.791946	39.602970
2887.792739	662076.924503	39.607988
2890.526671	663488.825182	39.613005
2893.454717	664891.030738	39.618023
2896.291666	666301.901251	39.623040
2898.728157	667714.222523	39.628058
2901.402968	669153.646628	39.633076
2904.265170	670595.206002	39.638093
2907.296744	672033.034945	39.643111
2910.113797	673485.642951	39.648128
2913.062164	674933.628307	39.653146
2915.879577	676392.741086	39.658164
2918.869125	677855.668857	39.663181
2921.975406	679311.687344	39.668199
2925.096485	680775.668426	39.673216
2928.062107	682226.727629	39.678234
2931.275639	683648.166257	39.683252
2934.488320	685061.587577	39.688269
2937.587878	686457.482509	39.693287
2941.223280	687864.237338	39.698304
2944.059611	689243.018446	39.703322
2947.516269	690630.610973	39.708340
2950.537192	692023.469552	39.713357
2953.806693	693408.527699	39.718375
2957.063460	694789.254948	39.723392
2959.906065	696166.266565	39.728410
2962.443374	697543.164257	39.733428
2965.170773	698932.206072	39.738445
2968.721748	700319.052378	39.743463
2971.091102	701723.223991	39.748480
2973.840886	703124.229463	39.753498
2977.008706	704534.447987	39.758516
2979.829221	705941.770578	39.763533
2982.891674	707354.664756	39.768551
2985.730493	708790.784295	39.773568
2988.737483	710214.058268	39.778586
2991.799260	711638.420688	39.783604
2993.955688	713086.997521	39.788621
2997.243132	714521.871192	39.793639
3000.453875	715973.482061	39.798656
3003.314537	717419.163037	39.803674
3006.332273	718880.886984	39.808692
3008.924356	720346.975619	39.813709
3012.113541	721814.482464	39.818727
3014.878099	723298.458495	39.823744
3017.702324	724784.924000	39.828762
3020.517282	726279.027161	39.833780
3023.586034	727776.469230	39.838797
3027.062522	729283.987870	39.843815
3030.367318	730776.341362	39.848832
3033.347624	732276.966876	39.853850
3036.234846	733783.943353	39.858868
3039.157265	735295.664847	39.863885
3042.609202	736807.207166	39.868903
3045.883711	738320.712852	39.873920
3048.508916	739836.358960	39.878938
3052.036236	741342.534985	39.883956
3054.917916	742862.536902	39.888973
3058.066722	744382.050806	39.893991
3061.586670	745901.452400	39.899008
3064.434567	747422.200053	39.904026
3067.751928	748940.746567	39.909044
3071.108251	750468.791175	39.914061
3074.477382	751975.943619	39.919079
3077.913717	753474.565442	39.924096
3081.225094	754993.297118	39.929114
3084.464590	756481.024017	39.934132
3087.731598	757974.754180	39.939149
3091.716749	759461.277100	39.944167
3094.996124	760941.773748	39.949184
3097.946817	762403.788044	39.954202
3101.204137	763843.041501	39.959220
3103.710036	765272.018135	39.964237
3107.187235	766680.990939	39.969255
3109.865998	768105.608544	39.974272
3112.707500	769534.592095	39.979290
3115.977475	770964.404701	39.984308
3118.730944	772391.473347	39.989325
3121.791903	773819.930396	39.994343
3124.757483	775265.308757	39.999360
3127.554078	776711.410846	40.004378
3130.520782	778162.152707	40.009396
3133.313769	779633.487454	40.014413
3136.139316	781099.904944	40.019431
3138.893407	782583.790980	40.024448
3141.468642	784088.535625	40.029466
3144.619161	785585.853969	40.034484
3147.810529	787098.633858	40.039501
3151.395097	788609.161657	40.044519
3154.576938	790136.976072	40.049536
3157.514090	791657.006131	40.054554
3161.158107	793175.655900	40.059572
3163.913348	794711.510166	40.064589
3167.806095	796237.481880	40.069607
3171.092339	797783.435445	40.074624
3173.872419	799326.341339	40.079642
3177.231648	800868.216526	40.084660
3180.074344	802421.426027	40.089677
3183.330245	803971.181510	40.094695
3186.989612	805524.134382	40.099712
3190.185059	807086.245543	40.104730
3193.637478	808649.614809	40.109748
3196.617496	810212.459236	40.114765
3199.873170	811766.835419	40.119783
3203.211735	813353.847727	40.124800
3206.059823	814930.510987	40.129818
3209.324773	816506.437875	40.134836
3212.385700	818096.616381	40.139853
3215.777952	819677.478200	40.144871
3219.055196	821266.809347	40.149888
3222.066435	822853.120534	40.154906
3225.040895	824442.467104	40.159924
3228.399369	826046.373074	40.164941
3231.653522	827647.758377	40.169959
3235.171131	829251.772968	40.174976
3238.353889	830852.720159	40.179994
3242.157630	832450.291560	40.185012
3245.726952	834042.930542	40.190029
3248.859107	835639.141690	40.195047
3252.567948	837232.958182	40.200064
3255.540845	838832.386913	40.205082
3258.916762	840420.305221	40.210100
3262.251048	842014.054906	40.215117
3265.468580	843602.561318	40.220135
3268.680881	845198.150191	40.225152
3271.789170	846785.480593	40.230170
3275.318518	848328.819677	40.235188
3278.455618	849875.047603	40.240205
3281.612920	851419.818754	40.245223
3284.575613	852964.431371	40.250240
3287.432468	854517.214292	40.255258
3290.822208	856064.372216	40.260276
3293.624925	857638.105139	40.265293
3296.785354	859199.638935	40.270311
3300.281354	860772.444249	40.275328
3303.234213	862363.347838	40.280346
3306.775038	863941.912363	40.285364
3309.937728	865520.128025	40.290381
3312.678778	867114.947386	40.295399
3316.016510	868735.475623	40.300416
3319.231149	870342.035321	40.305434
3322.566260	871958.009893	40.310452
3325.666354	873587.029807	40.315469
3328.913341	875226.213136	40.320487
3331.959618	876870.485266	40.325504
3334.990284	878527.443994	40.330522
3338.729394	880180.237726	40.335540
3342.128961	881855.996911	40.340557
3345.346022	883521.647657	40.345575
3348.778376	885191.416743	40.350592
3352.336597	886876.509288	40.355610
3355.831642	888560.250978	40.360628
3358.911538	890248.970782	40.365645
3362.290131	891930.969681	40.370663
3365.837082	893631.144303	40.375680
3368.999066	895331.646644	40.380698
3372.472578	897032.452032	40.385716
3376.044442	898741.684637	40.390733
3379.227413	900460.092010	40.395751
3382.859963	902177.221955	40.400768
3385.840488	903907.309874	40.405786
3389.043332	905635.186887	40.410804
3391.784522	907380.586474	40.415821
3394.645475	909120.223632	40.420839
3398.263927	910879.363060	40.425856
3401.025951	912658.835748	40.430874
3404.555803	914430.780134	40.435892
3407.988609	916220.022241	40.440909
3410.899695	918008.380382	40.445927
3414.791139	919800.873641	40.450944
3418.449928	921602.018484	40.455962
3422.038587	923394.038923	40.460980
3425.531452	925198.511416	40.465997
3428.921429	926997.122051	40.471015
3432.649073	928796.791230	40.476032
3436.253644	930599.317613	40.481050
3439.588895	932398.403739	40.486068
3442.862099	934193.058633	40.491085
3446.713663	936004.792005	40.496103
3450.250154	937811.553239	40.501120
3453.726606	939601.452728	40.506125
3457.009705	941328.955796	40.511130
3460.338292	943007.322172	40.516135
3463.898018	944625.652321	40.521140
3467.609730	946160.183747	40.526144
3470.703603	947627.960907	40.531149
3473.735533	949015.553685	40.536154
3476.653930	950315.671726	40.541159
3479.356757	951565.701748	40.546164
3482.197240	952763.088574	40.551168
3484.741533	953867.512842	40.556173
3487.295032	954901.427583	40.561178
3490.075351	955863.166970	40.566183
3492.339357	956740.642357	40.571188
3494.667722	957548.492813	40.576192
3496.581556	958287.417213	40.581197
3498.524738	958972.748225	40.586202
3500.741133	959595.156805	40.591207
3502.486112	960137.550521	40.596212
3504.408657	960614.924930	40.601216
3505.884133	961063.444256	40.606221
3507.787536	961444.478796	40.611226
3509.303147	961771.988810	40.616231
3510.544790	962047.041164	40.621236
3512.042521	962277.582169	40.626240
3513.196132	962476.154761	40.631245
3514.408604	962611.753365	40.636250
3515.657345	962713.367809	40.641255
3516.320992	962791.190589	40.646260
3517.860338	962808.453524	40.651264
3518.530353	962810.493163	40.656269
3519.591468	962775.652305	40.661274
3520.600018	962700.285416	40.666279
3521.003943	962612.683855	40.671284
3521.740598	962482.333742	40.676288
3522.679106	962337.258746	40.681293
3523.083543	962163.091289	40.686298
3523.950382	961964.848552	40.691303
3524.520979	961738.348772	40.696308
3525.165175	961497.921342	40.701312
3525.535877	961253.711090	40.706317
3526.222780	960971.827713	40.711322
3526.646854	960678.515864	40.716327
3526.916521	960374.538884	40.721332
3527.391506	960051.899288	40.726336
3527.843743	959717.882011	40.731341
3528.270627	959354.165648	40.736346
3528.743497	958987.577237	40.741351
3528.536092	958609.715944	40.746356
3529.294830	958229.803205	40.751360
3529.329005	957837.935959	40.756365
3529.877200	957429.588329	40.761370
3530.134361	957017.831209	40.766375
3530.027408	956587.974194	40.771380
3530.677273	956150.016180	40.776384
3530.715971	955711.345010	40.781389
3530.612236	955263.841474	40.786394
3530.810243	954794.681879	40.791399
3531.110564	954348.312957	40.796404
3531.762374	953871.058581	40.801408
3531.505482	953403.138327	40.806413
3531.768391	952914.887629	40.811418
3531.780708	952433.013965	40.816423
3531.816818	951941.286716	40.821428
3532.236034	951444.449039	40.826432
3532.318630	950953.022180	40.831437
3532.358242	950450.752236	40.836442
3532.806503	949947.564306	40.841447
3532.553915	949455.445430	40.846452
3533.184949	948943.519204	40.851456
3533.197521	948436.047741	40.856461
3533.209185	947916.853916	40.861466
3533.423875	947389.343992	40.866471
3533.125052	946869.044330	40.871476
3533.521851	946344.936396	40.876480
3533.564758	945822.941000	40.881485
3533.487152	945284.448900	40.886490
3533.244657	944750.523672	40.891495
3533.453137	944231.114577	40.896500
3533.562846	943674.709738	40.901504
3533.611458	943150.622921	40.906509
3533.628186	942603.790388	40.911514
3533.919655	942055.895254	40.916519
3533.521216	941511.029407	40.921524
3533.941709	940958.877027	40.926528
3534.078377	940413.037917	40.931533
3534.067477	939850.110098	40.936538
3534.068437	939301.302557	40.941543
3533.795483	938741.174319	40.946548
3533.694162	938180.668926	40.951552
3534.141532	937630.362879	40.956557
3534.011851	937062.072936	40.961562
3534.136154	936502.882706	40.966567
3534.028088	935941.466734	40.971572
3534.047367	935374.406277	40.976576
3533.873085	934815.086631	40.981581
3534.095655	934237.989210	40.986586
3533.981514	933672.686015	40.991591
3534.175806	933102.088230	40.996596
3534.072363	932531.383427	41.001600
3533.973791	931959.848203	41.006605
3534.034730	931398.109515	41.011610
3533.985794	930817.516110	41.016615
3533.794713	930257.138902	41.021620
3534.256252	929678.157216	41.026624
3534.364713	929103.685428	41.031629
3534.426192	928525.414245	41.036634
3534.055935	927945.425023	41.041639
3534.070428	927371.550104	41.046644
3534.233248	926792.977014	41.051648
3534.321720	926213.104824	41.056653
3534.603906	925626.891153	41.061658
3534.658476	925028.640343	41.066663
3533.983731	924439.480785	41.071668
3534.066822	923843.206727	41.076672
3534.161646	923270.414850	41.081677
3534.039199	922678.756406	41.086682
3534.394065	922098.008013	41.091687
3533.934880	921514.931922	41.096692
3534.087582	920920.917519	41.101696
3534.089750	920343.790462	41.106701
3534.112506	919752.170016	41.111706
3534.398763	919155.533649	41.116711
3534.198180	918564.398416	41.121716
3534.185667	917964.987854	41.126720
3534.079825	917376.015937	41.131725
3533.920067	916779.674995	41.136730
3533.923725	916194.405735	41.141735
3533.903917	915608.018588	41.146740
3534.442163	915008.091251	41.151744
3534.110622	914425.480828	41.156749
3534.174174	913817.897271	41.161754
3534.170201	913219.310144	41.166759
3533.887941	912628.506382	41.171764
3534.147652	912023.964624	41.176768
3534.008984	911436.282750	41.181773
3534.182218	910834.418307	41.186778
3534.261822	910238.863366	41.191783
3534.192274	909632.572750	41.196788
3534.265005	909024.841798	41.201792
3534.210900	908424.294540	41.206797
3533.971026	907822.653256	41.211802
3534.453089	907208.964980	41.216807
3533.989434	906616.678662	41.221812
3534.287873	905998.645117	41.226816
3534.024075	905396.261970	41.231821
3534.065533	904794.340040	41.236826
3534.431583	904179.950500	41.241831
3533.740183	903576.189050	41.246836
3533.927263	902970.379026	41.251840
3534.145581	902367.006681	41.256845
3533.976981	901761.512128	41.261850
3534.274691	901155.389826	41.266855
3534.018386	900549.199943	41.271860
3534.222840	899931.474769	41.276864
3534.242843	899319.505784	41.281869
3534.285818	898703.507433	41.286874
3534.510470	898084.320487	41.291879
3534.099009	897474.541995	41.296884
3534.066044	896854.104923	41.301888
3534.154893	896242.272669	41.306893
3534.009236	895626.260059	41.311898
3534.303474	895011.651195	41.316903
3533.901326	894392.359704	41.321908
3534.089160	893772.320038	41.326912
3533.837758	893159.053190	41.331917
3533.913399	892541.701275	41.336922
3534.005526	891927.856441	41.341927
3534.151992	891323.024295	41.346932
3533.961409	890699.137292	41.351936
3534.185921	890078.205788	41.356941
3533.983887	889449.736091	41.361946
3534.172227	888830.899888	41.366951
3534.044996	888206.633680	41.371956
3533.838981	887578.636755	41.376960
3533.869829	886966.301879	41.381965
3534.000398	886337.434729	41.386970
3533.593182	885718.655475	41.391975
3533.648175	885106.409209	41.396980
3533.992859	884478.561171	41.401984
3533.467698	883848.276502	41.406989
3533.233698	883233.557985	41.411994
3533.817303	882618.247429	41.416999
3533.115993	882011.612763	41.422004
3533.321332	881394.203572	41.427008
3533.469158	880775.866993	41.432013
3533.019641	880155.726277	41.437018
3533.344282	879532.384242	41.442023
3533.331806	878925.795103	41.447028
3533.419992	878302.556101	41.452032
3533.424319	877692.444808	41.457037
3533.190561	877076.398582	41.462042
3533.413114	876464.668592	41.467047
3533.130426	875845.496823	41.472052
3533.333002	875217.548505	41.477056
3533.519091	874607.376832	41.482061
3533.148073	873988.800740	41.487066
3533.435203	873367.623006	41.492071
3532.937257	872744.283275	41.497076
3533.180614	872121.333390	41.502080
3533.020611	871512.065504	41.507085
3533.177720	870893.755025	41.512090
3533.243041	870265.886842	41.517095
3533.000051	869655.666613	41.522100
3533.229098	869029.192788	41.527104
3533.062626	868421.550660	41.532109
3533.191053	867793.993816	41.537114
3533.491230	867163.526456	41.542119
3533.216147	866549.887842	41.547124
3533.054763	865926.359746	41.552128
3533.232427	865305.719495	41.557133
3533.431978	864672.871201	41.562138
3533.241115	864036.720534	41.567143
3533.129474	863418.363414	41.572148
3532.993411	862784.305577	41.577152
3532.960379	862165.029496	41.582157
3532.905426	861547.540054	41.587162
3533.054071	860923.733256	41.592167
3532.766703	860304.504783	41.597172
3532.849201	859661.432660	41.602176
3532.899597	859044.739855	41.607181
3532.733636	858423.257642	41.612186
3533.009010	857798.622542	41.617191
3532.338762	857175.835323	41.622196
3532.719671	856551.054660	41.627200
3533.023144	855934.587983	41.632205
3532.876610	855309.868026	41.637210
3533.216393	854677.997161	41.642215
3533.072674	854057.526995	41.647220
3532.518093	853422.858355	41.652224
3533.013334	852799.330557	41.657229
3533.041517	852173.094473	41.662234
3532.923653	851551.102395	41.667239
3533.127427	850910.887403	41.672244
3533.045130	850270.363003	41.677248
3532.734321	849643.149929	41.682253
3532.799827	849014.056561	41.687258
3533.165275	848373.746904	41.692263
3532.486672	847745.333917	41.697268
3532.661559	847108.627592	41.702272
3532.351203	846488.596358	41.707277
3532.218115	845859.900354	41.712282
3532.492374	845231.071639	41.717287
3531.998071	844619.362957	41.722292
3531.855734	843994.866139	41.727296
3532.315150	843375.857119	41.732301
3532.055730	842757.884581	41.737306
3532.260059	842133.533633	41.742311
3532.063576	841510.554118	41.747316
3531.926270	840886.625548	41.752320
3531.899598	840273.147249	41.757325
3531.941311	839654.917038	41.762330
3532.302603	839029.745162	41.767335
3531.740301	838408.814629	41.772340
3532.087713	837785.034398	41.777344
3532.047725	837163.259024	41.782349
3531.862264	836538.325748	41.787354
3532.088554	835913.114599	41.792359
3531.935923	835293.761935	41.797364
3532.060565	834670.349459	41.802368
3532.030694	834049.293929	41.807373
3531.678039	833421.058900	41.812378
3531.811604	832801.806965	41.817383
3531.510793	832190.282340	41.822388
3531.694400	831555.769221	41.827392
3531.465996	830940.598562	41.832397
3531.750231	830329.725216	41.837402
3531.487228	829699.549323	41.842407
3531.398843	829085.985077	41.847412
3531.420391	828467.557325	41.852416
3531.469607	827850.091711	41.857421
3531.519585	827228.854487	41.862426
3531.666365	826617.410569	41.867431
3531.488236	825999.075211	41.872436
3531.644094	825370.606583	41.877440
3531.629208	824753.053771	41.882445
3531.518870	824138.391478	41.887450
3531.767111	823511.683462	41.892455
3531.620156	822893.586778	41.897460
3531.448795	822257.151325	41.902464
3531.188166	821646.974664	41.907469
3531.059273	821028.357243	41.912474
3531.489562	820402.739815	41.917479
3531.449270	819793.576541	41.922484
3531.012879	819164.615129	41.927488
3531.148035	818544.937390	41.932493
3530.990466	817936.063385	41.937498
3530.988292	817313.994729	41.942503
3531.019586	816703.409794	41.947508
3531.216819	816079.038589	41.952512
3530.979010	815465.400978	41.957517
3530.620881	814848.154499	41.962522
3531.087648	814228.801137	41.967527
3530.813099	813621.412665	41.972532
3530.918347	813003.525184	41.977536
3531.108990	812382.922215	41.982541
3530.994488	811775.584015	41.987546
3530.963669	811143.250218	41.992551
3531.016062	810539.004007	41.997556
3530.888440	809910.636027	42.002560
3530.342535	809292.175910	42.007565
3530.683905	808684.432347	42.012570
3531.025362	808066.737464	42.017575
3530.442060	807458.796798	42.022580
3530.686854	806831.108229	42.027584
3530.957925	806221.538857	42.032589
3530.625952	805607.900856	42.037594
3530.643099	804987.677867	42.042599
3530.582283	804379.862977	42.047604
3530.823442	803763.902395	42.052608
3530.355340	803162.765192	42.057613
3530.378670	802547.909062	42.062618
3530.894324	801928.451316	42.067623
3530.518477	801312.571897	42.072628
3530.407190	800692.864593	42.077632
3530.312292	800085.312432	42.082637
3530.270593	799466.218688	42.087642
3530.643083	798843.073935	42.092647
3530.268230	798237.810912	42.097652
3530.082608	797619.459505	42.102656
3530.338919	797015.895639	42.107661
3530.367976	796400.883126	42.112666
3530.610894	795776.699604	42.117671
3530.050398	795167.323029	42.122676
3530.322740	794549.945646	42.127680
3530.249681	793945.975409	42.132685
3529.964272	793326.965007	42.137690
3529.831012	792717.007038	42.142695
3530.030430	792121.425822	42.147700
3530.232502	791497.603602	42.152704
3530.267222	790883.184821	42.157709
3530.065914	790274.548850	42.162714
3530.316385	789663.474318	42.167719
3530.298835	789049.051861	42.172724
3530.185531	788434.395773	42.177728
3530.149729	787828.321179	42.182733
3529.750179	787210.118894	42.187738
3530.033795	786595.628597	42.192743
3529.755665	785991.797414	42.197748
3529.994236	785374.211066	42.202752
3529.608360	784765.083842	42.207757
3529.345609	784163.159604	42.212762
3529.843002	783548.124023	42.217767
3529.731926	782951.381815	42.222772
3529.570742	782345.796108	42.227776
3529.577262	781733.540609	42.232781
3529.820341	781126.799411	42.237786
3529.993274	780505.902171	42.242791
3529.613959	779913.035733	42.247796
3529.882342	779297.084746	42.252800
3529.730789	778689.024888	42.257805
3529.351104	778080.362367	42.262810
3529.647377	777468.629972	42.267815
3529.657625	776867.426224	42.272820
3529.448395	776251.199125	42.277824
3529.568752	775638.948820	42.282829
3529.267255	775033.905839	42.287834
3529.726717	774435.427056	42.292839
3529.260431	773829.376916	42.297844
3529.263420	773211.034855	42.302848
3529.397652	772621.621132	42.307853
3529.235455	772016.944656	42.312858
3529.104671	771396.748747	42.317863
3529.246745	770802.656641	42.322868
3529.027778	770190.402289	42.327872
3529.211685	769586.599748	42.332877
3529.044695	768984.285658	42.337882
3529.229228	768376.590626	42.342887
3528.971583	767784.984283	42.347892
3528.933143	767172.153294	42.352896
3528.770515	766572.401733	42.357901
3528.798776	765975.674133	42.362906
3529.024837	765377.386217	42.367911
3528.832663	764791.642121	42.372916
3528.818776	764183.835075	42.377920
3528.208127	763589.736855	42.382925
3528.188893	762993.962007	42.387930
3528.424763	762397.504507	42.392935
3528.450509	761817.357985	42.397940
3528.493174	761213.541083	42.402944
3528.649423	760622.528991	42.407949
3528.230539	760039.953851	42.412954
3528.834894	759435.306576	42.417959
3528.438367	758838.822921	42.422964
3528.495534	758248.381760	42.427968
3528.856843	757649.060118	42.432973
3528.551401	757060.857957	42.437978
3528.641521	756453.543817	42.442983
3528.204842	755865.222129	42.447988
3528.309184	755270.395755	42.452992
3528.394283	754676.908314	42.457997
3528.204406	754085.100022	42.463002
3528.150260	753495.444246	42.468007
3528.325782	752903.383414	42.473012
3528.117351	752318.748578	42.478016
3527.954669	751728.284137	42.483021
3527.482099	751139.061783	42.488026
3528.215860	750549.736529	42.493031
3528.352804	749973.260016	42.498036
3528.048736	749372.859979	42.503040
3527.863578	748786.026608	42.508045
3527.604377	748200.445795	42.513050
3528.159275	747611.816281	42.518055
3528.092380	747038.218996	42.523060
3527.945045	746434.007071	42.528064
3527.990090	745850.173553	42.533069
3527.768774	745269.702288	42.538074
3527.962424	744680.616205	42.543079
3527.739637	744087.652076	42.548084
3527.460620	743502.660373	42.553088
3527.565760	742917.114494	42.558093
3527.651384	742337.905753	42.563098
3527.923206	741749.821911	42.568103
3527.709302	741166.968801	42.573108
3527.771930	740581.701252	42.578112
3527.633480	739994.149789	42.583117
3527.829951	739414.212639	42.588122
3527.794732	738820.126975	42.593127
3527.440194	738234.064393	42.598132
3527.387675	737655.722784	42.603136
3527.269473	737074.480969	42.608141
3527.393664	736496.074298	42.613146
3527.418733	735911.111441	42.618151
3527.122953	735341.400831	42.623156
3527.290710	734752.617594	42.628160
3527.424180	734170.626349	42.633165
3527.470158	733596.526554	42.638170
3527.272480	733008.419885	42.643175
3527.423970	732426.942500	42.648180
3527.580033	731847.699450	42.653184
3527.527593	731270.232587	42.658189
3527.042126	730687.550208	42.663194
3527.227676	730103.225811	42.668199
3526.983013	729527.746759	42.673204
3526.843175	728952.803170	42.678208
3527.273845	728383.862458	42.683213
3527.011439	727811.384683	42.688218
3527.196479	727225.218603	42.693223
3526.757587	726651.500609	42.698228
3526.927081	726080.709768	42.703232
3527.009521	725500.134141	42.708237
3526.696730	724933.655676	42.713242
3526.918499	724357.285640	42.718247
3526.812218	723781.575287	42.723252
3526.956290	723199.240463	42.728256
3526.993154	722633.732878	42.733261
3526.991382	722064.921920	42.738266
3527.096895	721484.405373	42.743271
3526.469775	720913.193044	42.748276
3526.274385	720339.983769	42.753280
3526.650758	719767.579157	42.758285
3526.298219	719202.448561	42.763290
3526.559577	718631.869292	42.768295
3526.402432	718065.834709	42.773300
3526.690872	717501.669179	42.778304
3526.818666	716931.244153	42.783309
3526.514484	716361.895443	42.788314
3526.577720	715791.453235	42.793319
3526.540173	715216.326647	42.798324
3526.123781	714650.452171	42.803329
3526.264120	714086.875411	42.808333
3526.210072	713518.431944	42.813338
3526.157144	712960.071751	42.818343
3526.442747	712398.242626	42.823348
3526.208569	711833.437833	42.828353
3526.285320	711260.850079	42.833357
3526.286472	710697.120309	42.838362
3526.358571	710129.618447	42.843367
3526.243827	709565.783676	42.848372
3526.000357	708998.706893	42.853377
3526.086825	708433.323175	42.858381
3525.996626	707879.748020	42.863386
3526.073509	707314.490402	42.868391
3525.886070	706757.085734	42.873396
3525.889492	706193.852065	42.878401
3526.093946	705641.770141	42.883405
3525.556582	705089.084091	42.888410
3525.805289	704523.613164	42.893415
3525.618721	703965.878146	42.898420
3525.839191	703410.471510	42.903425
3526.245857	702851.718781	42.908429
3525.797756	702294.019779	42.913434
3526.157293	701728.148167	42.918439
3526.031611	701173.054487	42.923444
3525.879635	700602.178577	42.928449
3526.200329	700037.246886	42.933453
3525.581551	699478.700500	42.938458
3525.889040	698921.997817	42.943463
3525.833105	698364.625882	42.948468
3525.757563	697801.953103	42.953473
3525.609527	697246.712690	42.958477
3525.510161	696683.823071	42.963482
3525.467407	696125.461392	42.968487
3525.250395	695583.450916	42.973492
3525.240211	695030.383638	42.978497
3525.758024	694475.650120	42.983501
3525.193071	693926.536517	42.988506
3525.081453	693377.311420	42.993511
3524.819135	692828.376386	42.998516
3524.614369	692287.454705	43.003521
3524.714087	691749.133976	43.008525
3524.426332	691213.881050	43.013530
3524.660496	690663.583486	43.018535
3524.776647	690134.066616	43.023540
3524.646658	689589.784468	43.028545
3524.614617	689057.741602	43.033549
3524.212577	688523.889304	43.038554
3524.548022	687982.415395	43.043559
3524.356693	687453.538916	43.048564
3524.552734	686918.145465	43.053569
3524.667887	686381.639095	43.058573
3524.109954	685861.192289	43.063578
3524.421073	685313.390426	43.068583
3524.453984	684788.948374	43.073588
3524.520472	684260.089577	43.078593
3524.404577	683721.622964	43.083597
3524.299202	683196.664382	43.088602
3524.249508	682663.898940	43.093607
3524.094144	682123.402652	43.098612
3524.309056	681597.699700	43.103617
3524.150353	681076.661429	43.108621
3524.030290	680550.407638	43.113626
3524.148103	680020.347748	43.118631
3523.925189	679494.200256	43.123636
3523.829873	678967.751778	43.128641
3523.959370	678441.583454	43.133645
3523.559175	677930.170778	43.138650
3523.597999	677402.015794	43.143655
3523.743357	676890.751257	43.148660
3523.774399	676365.228614	43.153665
3523.508454	675848.346690	43.158669
3523.378617	675337.242633	43.163674
3523.691564	674801.069372	43.168679
3523.605771	674300.116144	43.173684
3523.633039	673768.865725	43.178689
3524.037058	673252.721801	43.183693
3523.663487	672742.862544	43.188698
3523.469471	672214.502122	43.193703
3523.212444	671700.478828	43.198708
3523.284080	671192.303447	43.203713
3523.477021	670669.472814	43.208717
3523.281879	670176.194139	43.213722
3523.558486	669651.896683	43.218727
3523.175513	669148.774069	43.223732
3523.352859	668622.092817	43.228737
3523.255102	668120.961035	43.233741
3523.080311	667621.062596	43.238746
3522.946182	667106.667913	43.243751
3522.930239	666605.242496	43.248756
3522.780569	666096.730843	43.253761
3522.881158	665595.731060	43.258765
3522.631328	665101.249505	43.263770
3523.146892	664591.446504	43.268775
3523.196528	664088.480616	43.273780
3523.536634	663587.384422	43.278785
3523.544493	663066.910262	43.283789
3522.936967	662562.828900	43.288794
3522.765859	662049.515125	43.293799
3523.171304	661546.255368	43.298804
3522.994035	661038.677266	43.303809
3522.642322	660536.641843	43.308813
3522.576281	660037.526083	43.313818
3522.869101	659532.833019	43.318823
3522.620283	659037.490164	43.323828
3522.194376	658537.959228	43.328833
3522.618101	658035.462053	43.333837
3522.299569	657548.591329	43.338842
3522.362839	657054.092498	43.343847
3522.432389	656571.999296	43.348852
3522.423829	656069.873963	43.353857
3522.423794	655571.516209	43.358861
3522.387865	655085.672751	43.363866
3522.438892	654584.210050	43.368871
3522.213799	654094.155069	43.373876
3522.087991	653604.807829	43.378881
3521.887300	653114.749817	43.383885
3521.912740	652627.525746	43.388890
3521.702109	652139.119139	43.393895
3522.019140	651658.590591	43.398900
3522.139605	651177.872453	43.403905
3522.301157	650689.530570	43.408909
3522.140925	650212.110670	43.413914
3522.088829	649715.114412	43.418919
3522.094030	649240.567341	43.423924
3521.992105	648747.428463	43.428929
3522.155213	648254.769615	43.433933
3522.045571	647773.326609	43.438938
3522.086567	647281.839968	43.443943
3521.702230	646807.693570	43.448948
3521.609611	646322.379722	43.453953
3521.815904	645837.241292	43.458957
3521.607534	645367.345179	43.463962
3521.460432	644881.821156	43.468967
3521.468408	644405.695020	43.473972
3521.501360	643928.692331	43.478977
3521.697507	643449.439594	43.483981
3521.374688	642978.601957	43.488986
3521.588403	642498.901296	43.493991
3521.413562	642029.244264	43.498996
3521.367548	641556.743418	43.504001
3521.671939	641063.308956	43.509005
3520.903451	640597.137495	43.514010
3521.367299	640117.581943	43.519015
3521.709607	639640.625242	43.524020
3521.166028	639170.949531	43.529025
3521.261594	638692.640432	43.534029
3520.826226	638235.657494	43.539034
3521.252335	637762.250456	43.544039
3521.154005	637289.861611	43.549044
3520.761574	636821.803484	43.554049
3520.776158	636351.053196	43.559053
3520.618061	635907.727206	43.564058
3520.900355	635443.193599	43.569063
3520.720907	634982.170345	43.574068
3521.102184	634512.574722	43.579073
3521.132330	634049.322680	43.584077
3520.968542	633593.689311	43.589082
3521.106491	633125.423693	43.594087
3520.944375	632665.295606	43.599092
3520.696968	632204.861513	43.604097
3520.813000	631735.786596	43.609101
3520.360755	631285.757342	43.614106
3520.458855	630819.647568	43.619111
3521.015452	630366.052993	43.624116
3520.566329	629913.261310	43.629121
3520.870790	629448.507189	43.634125
3520.349253	628997.490665	43.639130
3520.673711	628534.495105	43.644135
3520.687278	628090.157288	43.649140
3520.292360	627634.404710	43.654145
3520.490259	627169.518465	43.659149
3520.269451	626720.156055	43.664154
3520.673344	626261.103530	43.669159
3520.382028	625817.824234	43.674164
3520.545136	625363.781891	43.679169
3520.540215	624905.592096	43.684173
3520.072839	624456.927500	43.689178
3520.475572	624015.658537	43.694183
3520.907391	623566.302213	43.699188
3520.729044	623113.124179	43.704193
3520.756186	622652.478230	43.709197
3520.544323	622201.020673	43.714202
3520.728856	621739.707628	43.719207
3520.701498	621274.302900	43.724212
3520.411330	620821.448248	43.729217
3520.037499	620367.135906	43.734221
3520.134971	619928.156437	43.739226
3519.971916	619469.812146	43.744231
3520.001387	619025.596585	43.749236
3519.680086	618586.884893	43.754241
3520.220142	618139.038141	43.759245
3519.706555	617698.268811	43.764250
3520.372724	617256.578601	43.769255
3520.094499	616809.518621	43.774260
3519.998308	616373.185427	43.779265
3519.854638	615927.018730	43.784269
3519.947769	615483.500233	43.789274
3520.098224	615032.936163	43.794279
3519.693242	614584.303260	43.799284
3519.605872	614150.637366	43.804289
3519.856113	613713.738350	43.809293
3519.448103	613281.145824	43.814298
3519.518627	612840.482779	43.819303
3519.615894	612403.457818	43.824308
3519.657525	611969.283194	43.829313
3519.937457	611527.629651	43.834317
3519.283976	611107.830931	43.839322
3519.361466	610659.558266	43.844327
3519.418835	610230.979741	43.849332
3519.135788	609793.866987	43.854337
3519.209125	609365.954646	43.859341
3519.010639	608945.946710	43.864346
3519.184915	608522.097598	43.869351
3519.198175	608091.338016	43.874356
3519.342179	607666.910025	43.879361
3519.388287	607240.024750	43.884365
3519.275834	606820.173416	43.889370
3519.312094	606383.023748	43.894375
3519.111708	605953.473003	43.899380
3519.104643	605531.599169	43.904385
3519.236151	605104.518205	43.909389
3518.644393	604682.160653	43.914394
3518.623355	604256.930252	43.919399
3518.868185	603835.753131	43.924404
3518.679966	603428.333421	43.929409
3519.014270	603001.439853	43.934413
3518.296353	602587.406363	43.939418
3518.447549	602169.094281	43.944423
3518.638908	601768.425877	43.949428
3518.607707	601348.458767	43.954433
3518.572469	600940.823858	43.959437
3518.463218	600530.526912	43.964442
3518.647252	600116.099514	43.969447
3518.580769	599695.626244	43.974452
3518.274114	599289.736010	43.979457
3518.393073	598882.001844	43.984461
3518.252559	598475.904031	43.989466
3518.293512	598064.690461	43.994471
3518.271035	597652.117589	43.999476
3518.363453	597250.254653	44.004481
3518.242931	596837.418520	44.009485
3517.937174	596439.662412	44.014490
3517.987652	596034.952859	44.019495
3518.019500	595637.212131	44.024500
3517.751223	595240.563610	44.029505
3518.034954	594835.019393	44.034509
3517.887213	594439.227015	44.039514
3518.028107	594043.723526	44.044519
3517.792862	593643.801149	44.049524
3517.643423	593249.274679	44.054529
3518.060773	592848.309782	44.059533
3517.616385	592453.254495	44.064538
3517.547131	592054.656121	44.069543
3517.655619	591664.101069	44.074548
3517.628936	591271.647364	44.079553
3517.687134	590875.197668	44.084557
3517.808978	590495.150884	44.089562
3517.846846	590095.162085	44.094567
3517.653876	589710.672815	44.099572
3517.631261	589323.177836	44.104577
3517.774828	588927.552884	44.109581
3517.331981	588532.467118	44.114586
3517.512103	588140.326887	44.119591
3517.664326	587756.770815	44.124596
3517.336618	587374.641106	44.129601
3517.557508	586991.702038	44.134605
3517.029560	586606.516758	44.139610
3517.329029	586220.625064	44.144615
3517.308736	585835.177625	44.149620
3517.443886	585449.691309	44.154625
3517.352373	585069.458237	44.159629
3517.113402	584684.363147	44.164634
3517.089793	584305.903800	44.169639
3517.005098	583925.482785	44.174644
3516.720542	583548.300886	44.179649
3517.174435	583172.087036	44.184653
3516.969674	582800.246752	44.189658
3517.055741	582423.720665	44.194663
3516.963405	582055.859981	44.199668
3516.856145	581682.159148	44.204673
3517.059554	581299.545616	44.209677
3516.875143	580928.599962	44.214682
3516.953477	580550.710248	44.219687
3517.063723	580183.009978	44.224692
3516.748077	579797.672808	44.229697
3516.996064	579422.082522	44.234701
3516.846035	579051.375904	44.239706
3516.939805	578683.130732	44.244711
3516.543462	578314.757091	44.249716
3516.541963	577944.343818	44.254721
3516.460115	577571.066673	44.259725
3516.625190	577212.521569	44.264730
3516.657309	576849.060158	44.269735
3516.875900	576483.343338	44.274740
3516.782294	576116.763738	44.279745
3516.827134	575738.279688	44.284749
3516.526605	575380.415026	44.289754
3516.361384	575005.264234	44.294759
3516.327691	574650.602537	44.299764
3515.889226	574290.466606	44.304769
3516.168595	573933.065065	44.309773
3516.151479	573585.010429	44.314778
3516.011670	573216.492233	44.319783
3515.781620	572862.718933	44.324788
3515.487613	572514.933434	44.329793
3515.536781	572168.488433	44.334797
3515.573502	571829.130069	44.339802
3515.502509	571485.856493	44.344807
3515.464535	571131.800516	44.349812
3515.376901	570793.794059	44.354817
3515.708291	570455.354805	44.359821
3515.531084	570114.728986	44.364826
3515.707510	569764.824983	44.369831
3515.524770	569416.884893	44.374836
3514.931090	569083.951450	44.379841
3515.476603	568733.402487	44.384845
3515.366246	568402.029404	44.389850
3515.294802	568066.967179	44.394855
3515.226554	567726.409801	44.399860
3515.216827	567392.023940	44.404865
3515.492498	567058.536909	44.409869
3515.416212	566729.178226	44.414874
3515.583216	566386.028413	44.419879
3515.379500	566049.929319	44.424884
3515.283523	565717.376933	44.429889
3515.293545	565374.327596	44.434893
3515.178185	565043.019553	44.439898
3515.057731	564716.486208	44.444903
3514.899876	564381.543934	44.449908
3515.183486	564048.128586	44.454913
3514.932555	563713.587656	44.459917
3515.022143	563391.264266	44.464922
3514.994810	563055.761969	44.469927
3514.986605	562735.100433	44.474932
3515.074598	562412.904086	44.479937
3515.250021	562088.721166	44.484941
3515.012425	561759.817277	44.489946
3515.021440	561416.663404	44.494951
3514.783850	561098.216300	44.499956
3514.763255	560781.940039	44.504961
3514.786931	560443.390841	44.509965
3514.280077	560129.699699	44.514970
3514.293673	559811.984167	44.519975
3514.798028	559487.479206	44.524980
3514.847560	559179.411479	44.529985
3514.707980	558855.051230	44.534989
3514.828764	558534.516590	44.539994
3514.801230	558206.847593	44.544999
3514.686911	557876.264016	44.550004
3514.595076	557574.075854	44.555009
3514.469668	557255.063257	44.560013
3514.422303	556940.764466	44.565018
3514.924554	556625.004361	44.570023
3514.918050	556305.041938	44.575028
3514.525276	555992.492355	44.580033
3514.482359	555665.569173	44.585037
3514.279242	555365.868528	44.590042
3514.444067	555046.300003	44.595047
3514.349145	554719.362516	44.600052
3513.941532	554414.587191	44.605057
3514.255316	554109.026804	44.610061
3514.053371	553808.535336	44.615066
3514.263015	553493.003032	44.620071
3514.203781	553188.190731	44.625076
3514.110925	552886.249237	44.630081
3514.256142	552571.865188	44.635085
3514.374577	552260.451265	44.640090
3514.272738	551956.424566	44.645095
3514.086803	551653.917085	44.650100
3514.040234	551348.557126	44.655105
3513.870076	551036.861928	44.660109
3513.713067	550746.121049	44.665114
3514.174941	550431.028430	44.670119
3514.253638	550123.906077	44.675124
3513.523391	549830.219705	44.680129
3513.856108	549535.539133	44.685133
3513.616870	549241.201839	44.690138
3513.975391	548938.490492	44.695143
3513.961688	548635.987192	44.700148
3513.417561	548344.807507	44.705153
3513.703021	548041.937571	44.710157
3513.468811	547755.027127	44.715162
3513.382957	547459.818816	44.720167
3513.426900	547163.825891	44.725172
3513.107056	546881.095557	44.730177
3513.568538	546591.118357	44.735181
3513.825123	546307.471277	44.740186
3513.552733	546021.186484	44.745191
3513.543017	545725.726324	44.750196
3513.353732	545431.903721	44.755201
3513.645939	545142.681183	44.760205
3513.615936	544853.759692	44.765210
3513.430785	544558.254132	44.770215
3513.525397	544273.130900	44.775220
3513.434504	543984.252108	44.780225
3513.594364	543696.080789	44.785229
3513.688429	543417.998827	44.790234
3513.462707	543120.200694	44.795239
3513.553242	542820.980792	44.800244
3513.454740	542538.729096	44.805249
3513.380038	542243.306798	44.810253
3513.442789	541955.771632	44.815258
3513.648712	541661.247223	44.820263
3513.560560	541375.087427	44.825268
3513.053341	541097.011526	44.830273
3513.087920	540807.037034	44.835277
3513.114166	540528.707513	44.840282
3513.045906	540252.305035	44.845287
3513.159261	539974.100976	44.850292
3512.969075	539696.044124	44.855297
3513.103673	539407.889811	44.860301
3513.015107	539140.345549	44.865306
3513.229076	538852.922914	44.870311
3513.429066	538567.060407	44.875316
3513.194700	538289.891341	44.880321
3513.259092	538007.067032	44.885325
3512.790132	537728.262540	44.890330
3513.009336	537448.275806	44.895335
3512.778494	537168.713507	44.900340
3512.743067	536904.043714	44.905345
3512.816235	536626.890628	44.910349
3513.116968	536360.387794	44.915354
3512.950780	536079.330192	44.920359
3513.190955	535801.577679	44.925364
3512.723812	535536.704041	44.930369
3512.861868	535249.524381	44.935373
3512.749617	534980.594362	44.940378
3512.901593	534702.734736	44.945383
3512.602770	534430.698292	44.950388
3512.610619	534171.419504	44.955393
3512.885368	533902.756440	44.960397
3512.731953	533628.510491	44.965402
3512.052606	533354.904149	44.970407
3512.466676	533096.848563	44.975412
3512.332922	532826.822442	44.980417
3512.067001	532562.818473	44.985421
3511.945303	532311.803716	44.990426
3511.820877	532049.229575	44.995431
3511.949785	531801.089925	45.000436
3511.970691	531546.555746	45.005441
3512.083365	531283.119889	45.010445
3511.867018	531030.332952	45.015450
3512.480868	530785.777100	45.020455
3512.635213	530520.352214	45.025460
3512.388217	530263.318079	45.030465
3512.567440	529997.475718	45.035469
3512.474838	529749.793220	45.040474
3512.614700	529476.882513	45.045479
3512.603883	529217.114803	45.050484
3511.957323	528960.883102	45.055489
3512.438172	528700.719487	45.060493
3512.239894	528444.755558	45.065498
3512.194258	528192.294302	45.070503
3512.126967	527928.172710	45.075508
3512.056563	527676.615406	45.080513
3512.120199	527416.853708	45.085517
3511.926759	527165.005843	45.090522
3511.554591	526915.506215	45.095527
3511.962087	526658.246893	45.100532
3511.526956	526413.898458	45.105537
3511.640634	526166.928247	45.110541
3511.577736	525924.275032	45.115546
3511.652679	525680.079846	45.120551
3511.615696	525433.476559	45.125556
3511.483034	525194.508653	45.130561
3511.822265	524950.104928	45.135565
3511.515639	524714.440565	45.140570
3511.722272	524469.193353	45.145575
3511.474231	524217.355394	45.150580
3511.476367	523976.224511	45.155585
3511.815637	523741.898713	45.160589
3511.480859	523502.786817	45.165594
3511.287288	523257.032709	45.170599
3511.496078	523012.114732	45.175604
3511.118624	522780.117936	45.180609
3511.263434	522541.565266	45.185613
3511.235092	522319.802380	45.190618
3511.226737	522079.854726	45.195623
3511.289870	521848.323805	45.200628
3511.176171	521611.365930	45.205633
3511.200383	521383.874246	45.210637
3511.333791	521149.846279	45.215642
3511.219237	520906.009801	45.220647
3511.594672	520667.893179	45.225652
3511.306063	520444.177764	45.230657
3511.390154	520203.780602	45.235661
3510.944728	519985.842327	45.240666
3511.110237	519753.857940	45.245671
3511.134253	519513.258121	45.250676
3510.962215	519285.566514	45.255681
3511.189088	519055.429676	45.260685
3510.887492	518834.066556	45.265690
3510.813620	518604.125789	45.270695
3510.854099	518376.838916	45.275700
3510.895242	518156.720661	45.280705
3510.862690	517924.338263	45.285709
3510.635587	517714.361163	45.290714
3510.789293	517490.122881	45.295719
3510.983341	517261.328479	45.300724
3510.914356	517047.526970	45.305729
3510.847325	516824.225879	45.310733
3510.748222	516600.472414	45.315738
3511.088599	516381.136377	45.320743
3510.903624	516149.510914	45.325748
3510.521303	515923.926970	45.330753
3510.689815	515701.125088	45.335757
3510.932900	515485.985779	45.340762
3510.389986	515270.270446	45.345767
3511.188677	515048.715554	45.350772
3510.679356	514837.686637	45.355777
3510.832795	514611.891086	45.360781
3510.610380	514393.835482	45.365786
3510.582316	514179.179051	45.370791
3510.579054	513959.968495	45.375796
3510.928250	513741.654601	45.380801
3511.240424	513518.291686	45.385805
3511.013412	513291.834651	45.390810
3510.807766	513072.241999	45.395815
3511.028193	512852.522992	45.400820
3510.863611	512637.413957	45.405825
3510.746126	512412.744430	45.410829
3510.764315	512193.404401	45.415834
3510.963979	511974.080852	45.420839
3510.791084	511749.663937	45.425844
3510.532156	511537.890836	45.430849
3510.515800	511320.211992	45.435853
3510.501056	511107.936648	45.440858
3510.160075	510890.357826	45.445863
3510.554569	510677.299377	45.450868
3510.417791	510471.403346	45.455873
3510.121308	510259.316298	45.460877
3509.849559	510048.990876	45.465882
3509.776553	509843.581129	45.470887
3509.835516	509642.896510	45.475892
3509.436827	509452.596830	45.480897
3509.857780	509250.127217	45.485901
3509.879255	509062.429563	45.490906
3509.677372	508870.168891	45.495911
3509.925760	508666.609487	45.500916
3509.583985	508467.241913	45.505921
3509.883758	508268.874181	45.510925
3509.868073	508069.799740	45.515930
3509.837461	507876.992446	45.520935
3510.023513	507669.792024	45.525940
3509.507674	507483.380529	45.530945
3509.811115	507277.165826	45.535949
3509.819579	507087.930894	45.540954
3509.331321	506896.352426	45.545959
3509.567914	506694.640065	45.550964
3508.979120	506509.240591	45.555969
3509.686094	506324.931926	45.560973
3509.787668	506135.214960	45.565978
3509.681977	505939.768785	45.570983
3509.778854	505745.397700	45.575988
3509.378665	505568.497736	45.580993
3509.673367	505368.982970	45.585997
3509.284292	505185.707758	45.591002
3509.369069	505002.804511	45.596007
3509.669928	504810.308244	45.601012
3509.201355	504621.934607	45.606017
3509.588964	504437.608387	45.611021
3509.521590	504256.694211	45.616026
3509.143819	504071.988996	45.621031
3509.328341	503879.855419	45.626036
3509.331462	503693.159829	45.631041
3509.440662	503512.813868	45.636045
3509.531701	503322.711857	45.641050
3509.415521	503148.719746	45.646055
3509.874409	502959.713477	45.651060
3509.900093	502764.661597	45.656065
3509.879527	502574.620480	45.661069
3509.399118	502382.279436	45.666074
3509.163684	502198.034252	45.671079
3509.292185	502017.870714	45.676084
3508.864495	501839.165273	45.681089
3509.316827	501656.818962	45.686093
3509.230265	501471.630104	45.691098
3509.086502	501304.448808	45.696103
3509.001585	501119.710753	45.701108
3509.357094	500950.013629	45.706113
3509.228011	500768.110668	45.711117
3509.511490	500588.865692	45.716122
3509.069070	500410.248351	45.721127
3509.426999	500223.806578	45.726132
3509.375427	500052.956171	45.731137
3509.408065	499865.352325	45.736141
3509.317129	499686.464875	45.741146
3508.974414	499510.450228	45.746151
3508.938305	499329.577447	45.751156
3509.030001	499160.058677	45.756161
3509.207580	498979.752408	45.761165
3508.858298	498813.036087	45.766170
3508.813126	498628.566803	45.771175
3508.994229	498457.306223	45.776180
3508.742767	498299.316679	45.781185
3508.653912	498127.087379	45.786189
3508.780574	497958.865235	45.791194
3508.585984	497793.174281	45.796199
3508.750052	497610.124577	45.801204
3508.717776	497447.639131	45.806209
3508.736493	497277.860782	45.811213
3508.962082	497114.721185	45.816218
3508.860548	496953.203668	45.821223
3508.847960	496778.216395	45.826228
3508.519272	496614.306781	45.831233
3508.691040	496438.879880	45.836237
3508.859147	496266.385225	45.841242
3508.615457	496107.412668	45.846247
3508.743742	495934.769674	45.851252
3508.312836	495774.359174	45.856257
3508.585584	495619.542398	45.861261
3508.733292	495456.703454	45.866266
3508.547902	495295.386622	45.871271
3508.647160	495121.930973	45.876276
3508.361238	494969.732628	45.881281
3508.405003	494800.582509	45.886285
3508.509263	494644.723349	45.891290
3508.456702	494487.473229	45.896295
3508.603007	494315.316400	45.901300
3508.354088	494164.925465	45.906305
3508.454033	493996.314125	45.911309
3508.516232	493835.851592	45.916314
3508.358441	493684.378567	45.921319
3508.606683	493519.935688	45.926324
3508.214722	493369.511537	45.931329
3508.456698	493207.697151	45.936333
3508.127666	493063.279271	45.941338
3508.460749	492905.645126	45.946343
3508.354665	492738.928202	45.951348
3508.291794	492580.953961	45.956353
3508.253327	492427.527035	45.961357
3508.266685	492270.447492	45.966362
3508.009899	492110.073744	45.971367
3508.543814	491962.666204	45.976372
3508.165109	491813.086075	45.981377
3508.394719	491657.582862	45.986381
3508.343584	491506.021678	45.991386
3507.954392	491351.734346	45.996391
3508.488083	491189.952222	46.001396
3508.196053	491045.055636	46.006401
3508.245251	490890.233970	46.011405
3508.026846	490741.021859	46.016410
3507.882510	490596.956360	46.021415
3508.249374	490442.734143	46.026420
3508.045449	490288.911572	46.031425
3508.087561	490147.441395	46.036429
3508.147527	489995.594947	46.041434
3507.695401	489844.795921	46.046439
3507.938382	489690.284553	46.051444
3507.882833	489562.740242	46.056449
3508.000461	489409.512684	46.061453
3508.066697	489259.935571	46.066458
3507.808020	489122.050184	46.071463
3507.883709	488966.650154	46.076468
3508.152529	488827.913382	46.081473
3507.982412	488678.776398	46.086477
3507.626190	488529.467510	46.091482
3507.846875	488389.774060	46.096487
3507.886115	488251.021278	46.101492
3507.624411	488116.417448	46.106497
3507.746460	487972.183401	46.111501
3507.564163	487827.443506	46.116506
3507.436066	487695.394296	46.121511
3507.505354	487549.040464	46.126516
3507.709786	487410.758807	46.131521
3507.491615	487279.835095	46.136525
3507.528562	487143.249826	46.141530
3507.727890	487011.392552	46.146535
3507.500304	486873.484031	46.151540
3507.396893	486750.785296	46.156545
3507.619764	486610.065122	46.161549
3507.604921	486465.639584	46.166554
3507.300176	486328.903878	46.171559
3507.465715	486187.431008	46.176564
3507.441703	486061.475072	46.181569
3507.522156	485923.051012	46.186573
3507.627827	485792.516350	46.191578
3507.305641	485667.823087	46.196583
3507.565578	485533.059694	46.201588
3507.425519	485406.714014	46.206593
3507.370588	485271.698729	46.211597
3507.350785	485136.423365	46.216602
3507.291971	485017.753670	46.221607
3507.350506	484866.115860	46.226612
3507.148696	484740.484491	46.231617
3507.184419	484610.003623	46.236621
3507.437056	484495.781623	46.241626
3507.558130	484367.410069	46.246631
3507.561659	484231.111552	46.251636
3507.440280	484101.311713	46.256641
3507.744833	483969.565522	46.261645
3507.948924	483837.683665	46.266650
3507.598561	483696.835656	46.271655
3507.751305	483558.077030	46.276660
3507.689293	483435.753061	46.281665
3507.519559	483302.716312	46.286669
3507.467686	483161.762478	46.291674
3507.260907	483031.564476	46.296679
3507.436982	482899.629825	46.301684
3507.273029	482774.180523	46.306689
3506.942170	482639.749072	46.311693
3507.098272	482516.824761	46.316698
3506.900800	482397.047632	46.321703
3507.117729	482269.251964	46.326708
3506.926634	482145.372022	46.331713
3507.084616	482029.733036	46.336717
3506.982917	481912.619081	46.341722
3506.713971	481800.442962	46.346727
3506.907739	481674.064327	46.351732
3506.742529	481561.312184	46.356737
3506.879027	481443.243332	46.361741
3507.180784	481315.730092	46.366746
3506.970805	481210.981411	46.371751
3507.025391	481087.558409	46.376756
3506.812124	480967.521305	46.381761
3506.681517	480841.900894	46.386765
3506.814408	480725.700944	46.391770
3506.710541	480623.968045	46.396775
3506.829336	480504.934224	46.401780
3506.872223	480389.101828	46.406785
3506.800761	480271.617640	46.411789
3507.319664	480144.312137	46.416794
3507.039851	480032.582444	46.421799
3507.031602	479907.592736	46.426804
3506.985440	479798.201043	46.431809
3506.991273	479672.144182	46.436813
3507.130781	479550.822404	46.441818
3506.802551	479438.894803	46.446823
3507.012232	479312.598128	46.451828
3506.954492	479201.787274	46.456833
3506.665521	479090.205198	46.461837
3506.945710	478969.868039	46.466842
3506.513988	478861.093410	46.471847
3506.852003	478746.313896	46.476852
3506.688121	478636.783403	46.481857
3506.578587	478515.851614	46.486861
3506.660117	478413.720225	46.491866
3506.374002	478303.044133	46.496871
3506.596999	478184.686064	46.501876
3506.381168	478096.982351	46.506881
3506.358798	477980.639397	46.511885
3506.478552	477872.574764	46.516890
3506.135519	477773.600708	46.521895
3506.599491	477667.400037	46.526900
3506.477715	477553.248445	46.531905
3506.624919	477446.746161	46.536909
3506.599645	477338.399339	46.541914
3506.355484	477235.101799	46.546919
3506.341361	477123.916419	46.551924
3506.576382	477024.282647	46.556929
3506.409474	476910.185376	46.561933
3506.704017	476807.654197	46.566938
3506.363835	476710.901747	46.571943
3506.785288	476599.486911	46.576948
3506.322119	476503.058164	46.581953
3506.391944	476395.449031	46.586957
3506.390710	476287.294421	46.591962
3506.178490	476188.238814	46.596967
3506.545172	476079.058098	46.601972
3506.823480	475981.183495	46.606977
3507.164139	475863.701758	46.611981
3507.010558	475747.721466	46.616986
3507.091733	475645.473411	46.621991
3506.787431	475525.415920	46.626996
3507.003694	475426.738780	46.632001
3507.083672	475314.209818	46.637005
3506.986029	475195.532731	46.642010
3506.786038	475087.101181	46.647015
3506.917478	474970.155851	46.652020
3506.712052	474867.344762	46.657025
3506.630466	474748.206313	46.662029
3506.721412	474640.633963	46.667034
3506.547254	474539.486798	46.672039
3506.589668	474423.717915	46.677044
3506.375045	474321.766236	46.682049
3506.181057	474223.203360	46.687053
3506.654308	474115.360123	46.692058
3506.120129	474017.664486	46.697063
3506.616952	473905.815393	46.702068
3506.196716	473807.440861	46.707073
3505.971862	473696.473350	46.712077
3506.204848	473612.013949	46.717082
3506.005891	473508.232021	46.722087
3506.056356	473411.648779	46.727092
3505.898669	473325.431659	46.732097
3505.985172	473221.650034	46.737101
3506.107500	473127.990334	46.742106
3505.835846	473033.992288	46.747111
3506.385217	472945.829524	46.752116
3505.912312	472852.067497	46.757121
3505.638692	472752.548188	46.762125
3505.573363	472663.374878	46.767130
3505.860196	472583.307679	46.772135
3506.064104	472487.655699	46.777140
3505.838949	472411.473546	46.782145
3505.769949	472308.574361	46.787149
3505.830840	472212.540230	46.792154
3505.670058	472129.052972	46.797159
3505.847878	472028.794332	46.802164
3505.975976	471944.699821	46.807169
3505.805274	471856.300349	46.812173
3505.892755	471768.362845	46.817178
3506.059897	471676.764742	46.822183
3505.973287	471577.663075	46.827188
3505.833536	471505.463789	46.832193
3505.783274	471414.711888	46.837197
3506.021758	471309.171682	46.842202
3505.619227	471236.611047	46.847207
3505.539109	471145.001922	46.852212
3505.541501	471054.239290	46.857217
3505.636549	470978.047288	46.862221
3505.572603	470889.067898	46.867226
3505.181835	470815.034802	46.872231
3505.579830	470725.418621	46.877236
3505.412467	470659.096151	46.882241
3505.357935	470573.507196	46.887245
3505.675314	470489.981661	46.892250
3505.366477	470413.096584	46.897255
3505.701366	470330.175157	46.902260
3505.694007	470248.628725	46.907265
3505.637583	470163.291488	46.912269
3505.540354	470089.762586	46.917274
3505.473682	470002.299018	46.922279
3505.576051	469919.263537	46.927284
3505.312073	469844.698467	46.932289
3505.485273	469757.648678	46.937293
3505.437935	469689.276222	46.942298
3505.095988	469611.887015	46.947303
3505.446849	469528.300865	46.952308
3505.489976	469445.779951	46.957313
3505.322335	469368.765213	46.962317
3505.436130	469306.340941	46.967322
3505.249558	469231.203052	46.972327
3505.525150	469139.067583	46.977332
3505.581026	469066.977531	46.982337
3505.521570	468984.928015	46.987341
3505.313962	468900.472028	46.992346
3505.440432	468828.976873	46.997351
3505.251433	468758.497756	47.002356
3505.302590	468687.673442	47.007361
3505.334988	468599.831908	47.012365
3505.568802	468532.420386	47.017370
3505.205086	468457.613619	47.022375
3505.236468	468381.118110	47.027380
3505.350758	468309.116524	47.032385
3505.152154	468234.230032	47.037389
3505.203441	468157.324976	47.042394
3505.109983	468095.084089	47.047399
3505.055324	468024.072751	47.052404
3505.001253	467948.248635	47.057409
3504.902641	467880.739601	47.062413
3505.020029	467810.255320	47.067418
3504.949398	467754.290936	47.072423
3505.238641	467679.065680	47.077428
3505.490898	467611.495786	47.082433
3505.035332	467535.941220	47.087437
3505.493567	467454.100674	47.092442
3505.469569	467389.920615	47.097447
3505.401242	467320.985998	47.102452
3505.248679	467247.607537	47.107457
3504.857537	467175.130736	47.112461
3505.317665	467100.228643	47.117466
3505.403043	467041.955873	47.122471
3505.271280	466961.581770	47.127476
3504.889959	466890.571344	47.132481
3504.804683	466818.547567	47.137485
3505.012341	466754.477807	47.142490
3504.705799	466693.737892	47.147495
3505.083503	466621.127720	47.152500
3505.079724	466557.042744	47.157505
3504.974302	466491.353763	47.162509
3505.324894	466416.670354	47.167514
3504.626306	466358.884000	47.172519
3504.986494	466294.178729	47.177524
3504.457855	466241.733108	47.182529
3504.488373	466170.143084	47.187533
3504.758402	466107.681697	47.192538
3504.692092	466048.114608	47.197543
3504.701582	465993.347297	47.202548
3504.759771	465932.137404	47.207553
3504.633874	465875.569032	47.212557
3504.820770	465817.781847	47.217562
3504.918239	465755.247457	47.222567
3504.979331	465694.542943	47.227572
3504.953012	465634.207804	47.232577
3504.582820	465572.816600	47.237581
3504.966256	465506.230180	47.242586
3504.848120	465458.170714	47.247591
3505.181366	465383.942245	47.252596
3504.954656	465322.221763	47.257601
3504.960376	465250.936550	47.262605
3505.358996	465192.402048	47.267610
3504.735014	465136.980510	47.272615
3505.073538	465066.195100	47.277620
3505.279946	465003.690345	47.282625
3504.891787	464933.889832	47.287629
3505.139893	464860.839189	47.292634
3505.329010	464800.667328	47.297639
3505.058976	464736.267117	47.302644
3505.074384	464676.783182	47.307649
3505.038705	464609.707924	47.312653
3504.886655	464538.497696	47.317658
3504.726304	464488.365729	47.322663
3504.813347	464430.186126	47.327668
3504.818222	464369.335060	47.332673
3505.073478	464314.217038	47.337677
3505.098146	464238.415547	47.342682
3504.723514	464183.100705	47.347687
3504.887602	464122.931019	47.352692
3504.876608	464069.124441	47.357697
3504.823493	464007.218133	47.362701
3504.809446	463949.865032	47.367706
3504.564071	463890.929897	47.372711
3504.782186	463820.819192	47.377716
3504.549914	463770.798991	47.382721
3504.469381	463718.726029	47.387725
3504.722851	463662.390435	47.392730
3504.751895	463605.130299	47.397735
3504.830729	463552.522999	47.402740
3504.468519	463503.233657	47.407745
3504.643386	463438.499840	47.412749
3504.655194	463382.508714	47.417754
3504.125310	463335.882365	47.422759
3504.675712	463279.798982	47.427764
3504.860883	463222.663075	47.432769
3504.448076	463167.655884	47.437773
3504.734805	463112.579764	47.442778
3504.607474	463055.243378	47.447783
3504.647124	463001.526549	47.452788
3504.836027	462958.678155	47.457793
3504.590653	462893.203567	47.462797
3505.096960	462842.801528	47.467802
3504.379321	462794.280471	47.472807
3504.751212	462723.278176	47.477812
3504.626762	462681.192069	47.482817
3504.161847	462621.125159	47.487821
3504.526153	462566.844995	47.492826
3504.252613	462514.953796	47.497831
3504.775806	462459.886139	47.502836
3504.503743	462414.581697	47.507841
3504.140583	462367.063155	47.512845
3505.115998	462310.043014	47.517850
3504.941902	462261.123796	47.522855
3504.604335	462203.922160	47.527860
3504.665003	462139.608928	47.532865
3504.408279	462091.007428	47.537869
3504.639036	462042.930641	47.542874
3504.401689	461986.217983	47.547879
3504.519569	461926.100107	47.552884
3504.734652	461882.484804	47.557889
3504.424843	461844.685071	47.562893
3504.842693	461777.928042	47.567898
3504.415180	461743.898022	47.572903
3504.510178	461669.088037	47.577908
3504.564428	461634.114120	47.582913
3504.668930	461573.997454	47.587917
3504.619364	461524.041667	47.592922
3504.582153	461489.691196	47.597927
3504.755715	461421.049064	47.602932
3504.452987	461374.480610	47.607937
3504.270850	461330.881237	47.612941
3504.540857	461280.870268	47.617946
3504.387213	461228.752505	47.622951
3504.751903	461184.349996	47.627956
3504.746857	461137.223408	47.632961
3504.248076	461075.840015	47.637965
3504.527880	461021.772724	47.642970
3504.414100	460970.711650	47.647975
3504.384060	460926.477312	47.652980
3504.668825	460876.006721	47.657985
3504.300627	460837.758948	47.662989
3504.706070	460776.068203	47.667994
3504.466202	460739.521301	47.672999
3504.353982	460682.175418	47.678004
3504.507845	460639.784047	47.683009
3504.285948	460587.777600	47.688013
3504.432000	460537.279156	47.693018
3504.258923	460491.395950	47.698023
3504.294186	460446.287890	47.703028
3504.204978	460401.150303	47.708033
3504.183064	460368.467601	47.713037
3504.341970	460313.202778	47.718042
3504.796237	460270.049848	47.723047
3504.623038	460218.794272	47.728052
3504.656928	460179.361674	47.733057
3504.672713	460129.441884	47.738061
3504.624013	460079.482302	47.743066
3504.663296	460030.571800	47.748071
3505.040440	459975.471485	47.753076
3504.632345	459929.677786	47.758081
3504.073143	459869.618593	47.763085
3504.130663	459825.113457	47.768090
3504.116180	459770.383511	47.773095
3504.031416	459732.896060	47.778100
3504.051806	459691.691058	47.783105
3503.939290	459650.812734	47.788109
3504.471879	459611.902002	47.793114
3504.057794	459569.301250	47.798119
3504.109620	459521.654324	47.803124
3504.089790	459487.449451	47.808129
3503.992601	459451.788035	47.813133
3504.105186	459412.441838	47.818138
3503.958044	459381.856742	47.823143
3503.825544	459324.510401	47.828148
3503.705352	459291.994748	47.833153
3503.922638	459265.959080	47.838157
3504.143194	459213.721449	47.843162
3503.942182	459188.263900	47.848167
3503.902652	459153.504340	47.853172
3503.984852	459106.256674	47.858177
3503.774542	459074.617613	47.863181
3503.985524	459038.193317	47.868186
3503.957112	458997.704735	47.873191
3503.841548	458965.694562	47.878196
3503.672133	458934.859181	47.883201
3503.870483	458901.883060	47.888205
3504.152463	458851.053045	47.893210
3504.136002	458826.779857	47.898215
3503.597995	458787.898280	47.903220
3504.126535	458742.043283	47.908225
3503.705905	458710.997046	47.913229
3503.910573	458685.773672	47.918234
3504.132388	458647.319575	47.923239
3503.951283	458614.255727	47.928244
3504.074475	458574.855388	47.933249
3503.874766	458537.942812	47.938253
3503.901374	458511.178499	47.943258
3503.981056	458482.783279	47.948263
3503.775510	458431.832718	47.953268
3504.231214	458399.572051	47.958273
3503.848833	458360.916478	47.963277
3504.105246	458327.574724	47.968282
3504.094435	458298.991968	47.973287
3503.969327	458263.789336	47.978292
3503.995961	458222.276143	47.983297
3503.693969	458196.175702	47.988301
3503.832129	458164.171606	47.993306
3503.676925	458123.246762	47.998311
3504.304066	458092.426121	48.003316
3504.013935	458061.103180	48.008321
3503.780078	458015.782161	48.013325
3503.755017	457979.041465	48.018330
3503.775812	457953.240373	48.023335
3503.731801	457931.809043	48.028340
3503.829172	457888.053033	48.033345
3503.926150	457866.141412	48.038349
3503.894104	457832.138526	48.043354
3503.646033	457801.162780	48.048359
3503.589347	457759.054657	48.053364
3504.037926	457733.991173	48.058369
3504.003769	457716.916705	48.063373
3503.971791	457663.197648	48.068378
3503.908527	457641.515878	48.073383
3503.798343	457606.258860	48.078388
3503.891073	457564.631655	48.083393
3503.539457	457537.879941	48.088397
3503.636179	457510.798218	48.093402
3503.519955	457485.019920	48.098407
3503.840066	457456.176724	48.103412
3504.138165	457421.457878	48.108417
3503.846053	457391.502704	48.113421
3503.876534	457360.833506	48.118426
3503.585122	457323.934354	48.123431
3503.772772	457289.842354	48.128436
3503.392631	457271.660839	48.133441
3503.514618	457253.697679	48.138445
3503.915830	457214.754047	48.143450
3503.886597	457185.970114	48.148455
3503.696134	457159.241064	48.153460
3503.412787	457132.679893	48.158465
3503.438208	457124.059129	48.163469
3503.749852	457082.545604	48.168474
3503.409271	457053.459848	48.173479
3503.641251	457010.388537	48.178484
3503.951148	456992.443744	48.183489
3503.971140	456974.396380	48.188493
3503.960954	456927.868955	48.193498
3503.966373	456909.671965	48.198503
3503.550735	456867.471211	48.203508
3503.756565	456829.371167	48.208513
3503.577736	456796.455994	48.213517
3504.244523	456786.306374	48.218522
3503.615704	456758.840668	48.223527
3504.101255	456719.273450	48.228532
3503.860709	456684.087763	48.233537
3503.639449	456668.716994	48.238541
3503.798151	456625.201199	48.243546
3503.881076	456599.083647	48.248551
3503.774295	456580.246597	48.253556
3503.662963	456558.825301	48.258561
3503.719577	456523.537909	48.263565
3503.631283	456485.842244	48.268570
3503.711031	456467.480104	48.273575
3503.641323	456447.065315	48.278580
3503.955029	456421.060188	48.283585
3503.614256	456380.822414	48.288589
3503.898850	456344.988916	48.293594
3503.853878	456333.186560	48.298599
3503.544744	456292.740461	48.303604
3503.815585	456261.724431	48.308609
3503.315036	456238.341769	48.313613
3503.571269	456217.364223	48.318618
3503.670290	456201.837036	48.323623
3503.671817	456172.539534	48.328628
3503.855171	456131.552836	48.333633
3503.750617	456115.553469	48.338637
3503.923161	456091.599521	48.343642
3503.536197	456064.142260	48.348647
3503.583928	456023.026437	48.353652
3503.446737	456001.558279	48.358657
3503.491349	456002.108244	48.363661
3503.773277	455971.292628	48.368666
3503.444689	455943.977299	48.373671
3503.517466	455896.622330	48.378676
3503.895368	455875.015399	48.383681
3503.586135	455860.216605	48.388685
3503.893620	455833.502153	48.393690
3503.946120	455804.448857	48.398695
3503.660320	455771.144774	48.403700
3503.735407	455755.266514	48.408705
3503.771589	455732.957455	48.413709
3503.839391	455691.178583	48.418714
3503.932442	455677.831622	48.423719
3503.688206	455647.257422	48.428724
3503.939516	455621.971566	48.433729
3504.022466	455594.179987	48.438733
3503.923148	455564.037117	48.443738
3503.733275	455545.568113	48.448743
3503.584618	455497.996580	48.453748
3503.685889	455467.616559	48.458753
3503.953692	455459.511282	48.463757
3503.696171	455420.625992	48.468762
3503.744790	455397.452724	48.473767
3503.656412	455366.750111	48.478772
3504.390597	455347.971079	48.483777
3504.093731	455310.511600	48.488781
3503.980632	455271.499986	48.493786
3503.827594	455259.005803	48.498791
3503.632882	455216.814574	48.503796
3503.547728	455188.747006	48.508801
3503.368949	455175.699579	48.513805
3503.442048	455146.489756	48.518810
3503.383680	455135.043819	48.523815
3503.255469	455116.969417	48.528820
3503.454494	455101.272244	48.533825
3503.272783	455071.092021	48.538829
3503.876778	455028.257123	48.543834
3504.123914	455010.929580	48.548839
3503.785860	454994.360916	48.553844
3503.959379	454968.276488	48.558849
3503.733506	454933.744232	48.563853
3503.750457	454900.691171	48.568858
3504.034238	454893.546061	48.573863
3503.455377	454855.120082	48.578868
3503.881079	454824.176801	48.583873
3503.389566	454809.661816	48.588877
3503.662331	454795.016323	48.593882
3503.313531	454770.541550	48.598887
3503.600421	454752.801473	48.603892
3503.532724	454719.204972	48.608897
3503.527010	454700.551684	48.613901
3503.647409	454678.784691	48.618906
3503.373486	454669.656396	48.623911
3503.412567	454664.529940	48.628916
3503.492447	454617.525620	48.633921
3503.346454	454591.089736	48.638925
3503.597912	454565.903929	48.643930
3503.628263	454547.852639	48.648935
3503.442815	454537.391202	48.653940
3503.499340	454522.833128	48.658945
3503.386801	454510.432953	48.663949
3503.678466	454471.401387	48.668954
3503.753490	454445.485183	48.673959
3503.433389	454430.484435	48.678964
3504.239041	454402.466449	48.683969
3504.015107	454375.131143	48.688973
3504.039223	454333.509023	48.693978
3503.840251	454319.349273	48.698983
3503.641116	454282.226059	48.703988
3503.567981	454257.196680	48.708993
3503.332141	454243.651477	48.713997
3503.525244	454220.908432	48.719002
3503.513725	454204.840984	48.724007
3503.394701	454198.017872	48.729012
3503.648221	454175.264460	48.734017
3503.466940	454145.741794	48.739021
3503.495533	454105.182985	48.744026
3503.679687	454095.672062	48.749031
3503.447692	454076.955457	48.754036
3503.638783	454054.972960	48.759041
3503.665301	454043.055683	48.764045
3503.966021	454002.399513	48.769050
3503.391327	453986.428054	48.774055
3503.469705	453973.082484	48.779060
3503.691039	453953.984205	48.784065
3503.768750	453919.094240	48.789069
3503.870811	453887.190946	48.794074
3503.776234	453874.381773	48.799079
3503.639330	453849.210704	48.804084
3503.653985	453811.137656	48.809089
3503.620596	453800.092252	48.814093
3504.112459	453775.472744	48.819098
3504.116167	453761.176613	48.824103
3503.731054	453717.189836	48.829108
3503.962823	453686.531418	48.834113
3503.534531	453666.124375	48.839117
3503.591079	453644.012330	48.844122
3503.386714	453613.833822	48.849127
3503.252474	453587.242553	48.854132
3503.719535	453566.530449	48.859137
3503.484310	453562.515125	48.864141
3503.390153	453539.262741	48.869146
3503.332366	453534.456706	48.874151
3503.612145	453514.739712	48.879156
3503.236678	453464.312614	48.884161
3503.222529	453459.093557	48.889165
3503.616848	453433.527108	48.894170
3503.787288	453428.124443	48.899175
3504.032226	453405.625115	48.904180
3504.173802	453377.921902	48.909185
3503.509168	453351.775752	48.914189
3504.024735	453326.543328	48.919194
3504.033695	453298.406402	48.924199
3503.707202	453268.248238	48.929204
3503.736862	453242.743818	48.934209
3503.860576	453231.316420	48.939213
3503.914322	453189.585530	48.944218
3503.562294	453170.330950	48.949223
3503.230270	453150.515292	48.954228
3503.436590	453133.243828	48.959233
3503.124759	453140.039507	48.964237
3503.715226	453106.581456	48.969242
3503.687724	453080.731730	48.974247
3503.411439	453057.205729	48.979252
3503.522980	453034.475298	48.984257
3503.609777	453029.948628	48.989261
3503.641779	453010.374849	48.994266
3503.828186	452995.489344	48.999271
3503.494626	452958.386686	49.004276
3503.628560	452938.339177	49.009281
3503.495758	452925.586634	49.014285
3503.731061	452904.609266	49.019290
3503.415463	452876.577877	49.024295
3503.432619	452849.097978	49.029300
3503.485483	452823.741163	49.034305
3503.313926	452817.078647	49.039309
3503.565133	452805.020897	49.044314
3503.352550	452791.217284	49.049319
3503.059895	452781.381603	49.054324
3503.492604	452759.102987	49.059329
3503.013926	452750.972015	49.064333
3503.190279	452732.032370	49.069338
3503.194507	452723.159887	49.074343
3503.098534	452714.101724	49.079348
3502.976301	452699.065921	49.084353
3503.324546	452698.195340	49.089357
3502.943597	452683.862748	49.094362
3503.377833	452674.308469	49.099367
3503.016593	452658.553006	49.104372
3503.253782	452619.679313	49.109377
3502.921710	452615.629643	49.114381
3503.212426	452598.951675	49.119386
3503.671852	452578.037100	49.124391
3503.205407	452563.465541	49.129396
3502.929818	452546.732138	49.134401
3503.232318	452533.448759	49.139405
3503.115863	452518.158355	49.144410
3503.001621	452511.283168	49.149415
3503.218227	452504.250094	49.154420
3503.648003	452487.396203	49.159425
3503.184510	452476.524920	49.164429
3503.100567	452474.410017	49.169434
3503.177847	452458.478131	49.174439
3503.230837	452440.776000	49.179444
3503.272996	452430.984376	49.184449
3502.757608	452422.251182	49.189453
3503.361679	452411.653851	49.194458
3503.027369	452403.802270	49.199463
3503.056060	452392.187847	49.204468
3503.122868	452376.105595	49.209473
3503.030281	452379.568799	49.214477
3503.027406	452357.921790	49.219482
3503.129147	452352.327788	49.224487
3503.043184	452330.390757	49.229492
3503.292411	452319.042817	49.234497
3503.255500	452318.237986	49.239501
3503.120951	452297.018972	49.244506
3503.153479	452297.571101	49.249511
3503.110852	452282.217219	49.254516
3503.202574	452265.978537	49.259521
3503.225146	452265.924003	49.264525
3503.593307	452259.067756	49.269530
3503.560501	452232.102538	49.274535
3503.278094	452198.893454	49.279540
3503.505134	452177.359090	49.284545
3503.210413	452172.289010	49.289549
3503.567748	452153.723511	49.294554
3503.409466	452147.869668	49.299559
3503.361606	452136.521658	49.304564
3503.506342	452123.315651	49.309569
3503.343026	452105.802260	49.314573
3503.164050	452071.155783	49.319578
3502.795694	452064.222441	49.324583
3503.018577	452053.233736	49.329588
3503.245853	452056.186101	49.334593
3502.883448	452056.907065	49.339597
3503.042057	452044.256312	49.344602
3502.967150	452040.872383	49.349607
3503.094271	452028.531182	49.354612
3503.244257	452017.504208	49.359617
3503.038489	452017.894243	49.364621
3503.118033	451997.550922	49.369626
3503.063250	451996.039363	49.374631
3503.110080	451981.785332	49.379636
3503.318802	451971.660864	49.384641
3503.014618	451960.660711	49.389645
3503.319740	451944.385339	49.394650
3503.232076	451917.834660	49.399655
3502.764009	451906.051295	49.404660
3503.290910	451896.328742	49.409665
3502.984073	451881.830843	49.414669
3503.229317	451864.095392	49.419674
3503.445439	451857.467766	49.424679
3503.430431	451851.589375	49.429684
3503.467182	451832.013669	49.434689
3503.398149	451838.362731	49.439693
3503.185541	451823.291023	49.444698
3503.553955	451806.244265	49.449703
3502.994580	451798.126694	49.454708
3503.469477	451789.072047	49.459713
3503.256311	451775.825534	49.464717
3503.552785	451762.846881	49.469722
3503.076362	451730.379948	49.474727
3502.926419	451717.122602	49.479732
3503.132573	451696.503876	49.484737
3503.052399	451681.815039	49.489741
3503.314325	451676.396297	49.494746
3503.327909	451665.443125	49.499751
3503.501925	451667.694860	49.504756
3503.626777	451654.542649	49.509761
3503.607382	451646.484913	49.514765
3503.460828	451635.609767	49.519770
3503.666804	451623.761848	49.524775
3503.221184	451588.754503	49.529780
3503.616968	451562.272917	49.534785
3503.150665	451552.719792	49.539789
3502.832084	451549.478787	49.544794
3503.144660	451532.694832	49.549799
3503.055132	451525.967193	49.554804
3503.216587	451511.946762	49.559809
3503.470426	451510.281073	49.564813
3503.383247	451486.264701	49.569818
3503.262595	451489.428652	49.574823
3503.301867	451479.434275	49.579828
3503.129295	451467.448107	49.584833
3503.048227	451461.631584	49.589837
3502.905342	451450.755714	49.594842
3503.031707	451446.424738	49.599847
3503.111713	451439.110434	49.604852
3503.490654	451421.148981	49.609857
3503.340192	451411.947454	49.614861
3503.322419	451404.700533	49.619866
3503.639344	451394.405211	49.624871
3503.520122	451368.923899	49.629876
3503.702588	451342.681254	49.634881
3503.400515	451334.367468	49.639885
3503.420398	451324.984719	49.644890
3503.499627	451307.733433	49.649895
3503.128451	451300.496119	49.654900
3503.199377	451284.057422	49.659905
3503.631799	451259.597171	49.664909
3503.449402	451240.920218	49.669914
3503.352297	451226.386048	49.674919
3502.875168	451224.084655	49.679924
3503.490487	451211.152614	49.684929
3503.362150	451195.559064	49.689933
3503.102562	451185.311378	49.694938
3503.380708	451179.179942	49.699943
3503.045878	451178.983632	49.704948
3503.440401	451164.872472	49.709953
3503.362145	451157.737191	49.714957
3503.748608	451136.225227	49.719962
3503.602308	451102.737646	49.724967
3503.421608	451086.392457	49.729972
3503.312356	451068.361958	49.734977
3503.395410	451065.255097	49.739981
3503.200069	451049.520778	49.744986
3503.498851	451045.464479	49.749991
3502.990245	451041.495340	49.754996
3503.332176	451019.788059	49.760001
3503.204814	451014.486316	49.765005
3503.155747	450996.141277	49.770010
3503.119879	450974.143556	49.775015
3502.995684	450963.061439	49.780020
3503.234677	450975.391492	49.785025
3503.375235	450951.842619	49.790029
3503.338933	450921.023076	49.795034
3503.291974	450911.905055	49.800039
3503.229989	450910.191844	49.805044
3503.269335	450895.836946	49.810049
3503.235353	450899.746692	49.815053
3502.964738	450887.574128	49.820058
3502.905727	450879.066555	49.825063
3502.755522	450871.436457	49.830068
3503.256355	450863.289589	49.835073
3503.154498	450855.955433	49.840077
3503.333867	450847.153642	49.845082
3503.277562	450841.738321	49.850087
3503.249276	450835.709808	49.855092
3502.973087	450819.887719	49.860097
3502.845184	450819.656072	49.865101
3502.715167	450804.975126	49.870106
3503.324085	450790.624303	49.875111
3502.957755	450796.314637	49.880116
3503.167371	450783.198103	49.885121
3503.004087	450778.713643	49.890125
3502.898230	450768.287399	49.895130
3503.197260	450758.299024	49.900135
3503.080466	450750.713877	49.905140
3503.240528	450733.245511	49.910145
3503.160486	450734.374611	49.915149
3503.335186	450726.435479	49.920154
3503.422836	450714.404444	49.925159
3503.171267	450722.407440	49.930164
3503.335345	450695.913616	49.935169
3503.179902	450690.008174	49.940173
3503.284587	450689.432607	49.945178
3503.323807	450679.843461	49.950183
3503.191776	450672.463692	49.955188
3503.072180	450661.279226	49.960193
3503.223559	450656.639610	49.965197
3503.490160	450646.099008	49.970202
3503.359069	450614.737486	49.975207
3503.088860	450601.297158	49.980212
3503.320019	450582.346195	49.985217
3503.012907	450576.111710	49.990221
3503.350552	450567.434879	49.995226
3503.531554	450554.525892	50.000231
3503.312874	450545.386331	50.005236
3503.597151	450528.657102	50.010241
3503.200080	450534.504860	50.015245
3503.117250	450519.917058	50.020250
3503.304395	450512.736239	50.025255
3502.987787	450510.103148	50.030260
3503.555219	450503.364405	50.035265
3503.179767	450498.358398	50.040269
3503.014476	450475.013313	50.045274
3503.207464	450452.114041	50.050279
3503.074731	450461.161576	50.055284
3503.196359	450430.010131	50.060289
3503.360462	450426.686530	50.065293
3503.590377	450413.870508	50.070298
3503.952318	450399.764395	50.075303
3503.369807	450397.937214	50.080308
3503.742875	450382.663054	50.085313
3503.580570	450368.849240	50.090317
3503.423734	450331.711700	50.095322
3503.186656	450314.817813	50.100327
3502.969401	450312.674749	50.105332
3503.090764	450293.691570	50.110337
3502.941417	450302.742010	50.115341
3502.757153	450289.185402	50.120346
3503.007577	450267.847878	50.125351
3502.773722	450278.433815	50.130356
3502.736308	450287.870764	50.135361
3503.129795	450296.575010	50.140365
3502.962947	450291.279824	50.145370
3503.045333	450292.127704	50.150375
3502.978911	450285.040805	50.155380
3503.166173	450271.471451	50.160385
3502.890374	450275.980324	50.165389
3502.743447	450266.980494	50.170394
3503.017855	450255.069411	50.175399
3502.732434	450252.583067	50.180404
3502.635527	450238.403087	50.185409
3502.794324	450233.964918	50.190413
3502.587203	450233.138367	50.195418
3502.662781	450246.916411	50.200423
3502.749956	450255.216659	50.205428
3502.950773	450248.895348	50.210433
3502.762021	450245.733371	50.215437
3502.611130	450242.412824	50.220442
3502.700513	450229.062962	50.225447
3502.692995	450237.987810	50.230452
3502.840969	450243.083457	50.235457
3502.622910	450254.579344	50.240461
3502.576367	450251.697298	50.245466
3502.907028	450239.218880	50.250471
3502.427791	450234.230529	50.255476
3502.879408	450226.446732	50.260481
3502.892361	450231.159822	50.265485
3502.583124	450243.837428	50.270490
3503.052757	450244.061468	50.275495
3502.658193	450243.824644	50.280500
3502.756939	450242.438847	50.285505
3502.297807	450236.737237	50.290509
3502.546255	450227.872689	50.295514
3502.637269	450244.740919	50.300519
3502.364948	450257.057300	50.305524
3502.818791	450255.053151	50.310529
3502.804469	450254.345787	50.315533
3502.408871	450252.081063	50.320538
3502.399522	450258.876733	50.325543
3502.770882	450273.973205	50.330548
3502.831049	450270.565923	50.335553
3502.499880	450265.805807	50.340557
3502.777095	450262.716376	50.345562
3502.966095	450253.050759	50.350567
3502.546475	450261.031923	50.355572
3502.771154	450274.125365	50.360577
3503.021868	450273.271343	50.365581
3502.842087	450274.823113	50.370586
3503.141617	450261.133178	50.375591
3502.999356	450270.233124	50.380596
3503.110104	450256.220507	50.385601
3502.931435	450254.780676	50.390605
3502.944797	450248.085757	50.395610
3503.309069	450241.888640	50.400615
3502.891449	450238.664338	50.405620
3503.083854	450231.685332	50.410625
3502.781179	450230.824395	50.415629
3502.822247	450226.609135	50.420634
3502.883996	450212.959769	50.425639
3502.827914	450209.166710	50.430644
3502.766755	450195.741127	50.435649
3502.864527	450221.328975	50.440653
3502.665461	450222.681234	50.445658
3502.706252	450226.730445	50.450663
3502.371884	450221.261037	50.455668
3502.853676	450216.463502	50.460673
3502.738656	450203.249929	50.465677
3502.606904	450208.849667	50.470682
3502.961871	450229.171280	50.475687
3502.923483	450228.315917	50.480692
3502.768731	450226.922702	50.485697
3502.952351	450227.043472	50.490701
3502.668811	450232.821226	50.495706
3502.793537	450224.434119	50.500711
3502.178324	450220.837937	50.505716
3502.814032	450227.675581	50.510721
3502.610062	450242.667505	50.515725
3502.895439	450237.345791	50.520730
3502.934218	450217.311902	50.525735
3502.717106	450197.625899	50.530740
3502.701307	450156.661311	50.535745
3502.582363	450119.973244	50.540749
3502.940432	450060.083386	50.545754
3502.956300	449994.674507	50.550759
3502.514020	449922.904407	50.555764
3502.701122	449833.736899	50.560769
3502.983633	449731.420600	50.565773
3503.080532	449625.941178	50.570778
3503.797344	449492.569731	50.575783
3503.109066	449350.259914	50.580788
3503.369907	449185.324985	50.585793
3503.493996	449027.206568	50.590797
3503.254077	448842.021781	50.595802
3503.228495	448642.956083	50.600807
3502.647728	448442.360700	50.605812
3503.154641	448230.168659	50.610817
3502.991545	448004.752863	50.615821
3502.491015	447777.059717	50.620826
3502.727798	447523.376905	50.625831
3502.183699	447272.461266	50.630836
3502.615914	447005.098135	50.635841
3502.295874	446732.434078	50.640845
3502.353476	446427.601935	50.645850
3502.502057	446127.770370	50.650855
3502.380756	445826.611440	50.655860
3502.772168	445496.200583	50.660865
3502.794286	445156.871292	50.665869
3502.958368	444799.559306	50.670874
3502.983441	444422.739525	50.675879
3502.759205	444031.400015	50.680884
3503.024657	443626.732478	50.685889
3502.854622	443217.668493	50.690893
3502.546974	442786.658677	50.695898
3502.371723	442333.199152	50.700903
3502.159153	441891.504020	50.705908
3502.282268	441420.729183	50.710913
3502.313589	440938.344117	50.715917
3502.137401	440435.643121	50.720922
3502.480381	439933.450720	50.725927
3502.044171	439406.320580	50.730932
3502.261576	438860.347391	50.735937
3502.003063	438303.585833	50.740941
3501.817178	437731.578576	50.745946
3502.321096	437130.673494	50.750951
3502.137509	436532.304950	50.755956
3501.941455	435902.162266	50.760961
3501.910899	435255.636474	50.765965
3501.716093	434603.995725	50.770970
3501.681526	433932.824869	50.775975
3501.597666	433244.492141	50.780980
3501.786367	432520.724401	50.785985
3501.347688	431814.649406	50.790989
3501.109421	431082.435144	50.795994
3501.341187	430314.340375	50.800999
3500.958053	429551.248020	50.806004
3501.073337	428751.758651	50.811009
3501.308085	427935.676295	50.816013
3501.219828	427101.704546	50.821018
3501.562692	426247.327333	50.826023
3500.947238	425387.144495	50.831028
3500.862348	424491.206598	50.836033
3501.037673	423590.622451	50.841037
3500.793747	422664.034555	50.846042
3500.998461	421710.428920	50.851047
3500.618557	420734.928934	50.856052
3500.529599	419742.865883	50.861057
3500.449122	418736.977186	50.866061
3500.323399	417707.801213	50.871066
3500.476175	416664.572158	50.876071
3500.252188	415608.771478	50.881076
3500.347037	414511.791228	50.886081
3500.186058	413405.311480	50.891085
3499.956650	412282.240240	50.896090
3499.852582	411134.975333	50.901095
3499.730454	409971.283837	50.906100
3499.468935	408781.508872	50.911105
3499.685973	407577.859382	50.916109
3499.510571	406354.361719	50.921114
3499.342301	405110.259628	50.926119
3498.977602	403859.174774	50.931124
3499.210058	402565.180291	50.936129
3499.047005	401272.666563	50.941133
3498.869650	399954.768025	50.946138
3499.166690	398614.243629	50.951143
3498.653796	397253.063139	50.956148
3498.665703	395873.283006	50.961153
3498.429509	394473.635740	50.966157
3498.304911	393055.252027	50.971162
3498.056890	391626.479502	50.976167
3497.916106	390166.948047	50.981172
3497.322155	388691.057598	50.986177
3497.836301	387204.639566	50.991181
3497.678547	385694.043765	50.996186
3498.013743	384159.144889	51.001191
3497.322075	382618.602901	51.006196
3497.591438	381048.819304	51.011201
3496.801591	379462.287073	51.016205
3496.543658	377853.851984	51.021210
3496.622214	376240.833258	51.026215
3496.309370	374612.677211	51.031220
3496.051783	372945.584110	51.036225
3495.696197	371284.505402	51.041229
3495.312968	369613.690946	51.046234
3495.208044	367905.853312	51.051239
3495.041981	366198.505878	51.056244
3495.083682	364461.009521	51.061249
3494.701982	362721.598050	51.066253
3494.475197	360963.488932	51.071258
3494.500918	359171.810076	51.076263
3493.741916	357387.484668	51.081268
3493.735903	355576.598588	51.086273
3493.703182	353753.579476	51.091277
3493.009174	351917.568878	51.096282
3492.802769	350051.554001	51.101287
3492.445810	348183.296984	51.106292
3492.459336	346298.105867	51.111297
3492.186585	344417.312707	51.116301
3491.863090	342503.958591	51.121306
3492.031095	340568.712393	51.126311
3491.306607	338642.447973	51.131316
3491.019179	336682.671745	51.136321
3490.624171	334718.944740	51.141325
3490.348739	332747.564767	51.146330
3490.164266	330747.846087	51.151335
3489.649626	328749.790903	51.156340
3489.688501	326734.848073	51.161345
3489.539311	324692.504830	51.166349
3489.338641	322653.028007	51.171354
3489.090593	320586.356477	51.176359
3488.275254	318519.612984	51.181364
3488.019521	316425.750128	51.186369
3487.651627	314334.566091	51.191373
3487.287589	312231.353992	51.196378
3487.091419	310098.927534	51.201383
3486.869313	307971.512375	51.206388
3486.283891	305829.386019	51.211393
3486.009545	303677.272176	51.216397
3485.567145	301507.335712	51.221402
3485.829757	299326.761915	51.226407
3485.469832	297141.024672	51.231412
3484.990815	294930.586045	51.236417
3484.616880	292705.034237	51.241421
3484.047959	290478.631505	51.246426
3484.088831	288247.958078	51.251431
3483.583629	285992.688668	51.256436
3483.308764	283720.688525	51.261441
3483.002353	281443.260528	51.266445
3482.260631	279157.038290	51.271450
3482.229753	276851.259895	51.276455
3481.541027	274551.119182	51.281460
3480.700486	272228.849820	51.286465
3480.740406	269906.358378	51.291469
3480.314744	267570.328911	51.296474
3479.915377	265218.006116	51.301479
3479.435553	262866.754870	51.306484
3479.069915	260502.257504	51.311489
3478.586149	258139.073658	51.316493
3477.960603	255751.309465	51.321498
3477.874306	253354.973269	51.326503
3476.999282	250962.774607	51.331508
3476.528186	248556.023360	51.336513
3476.492433	246136.424089	51.341517
3475.875214	243718.568809	51.346522
3475.490841	241286.990465	51.351527
3474.679663	238853.444079	51.356532
3474.782899	236402.016558	51.361537
3473.889636	233944.956811	51.366541
3473.489192	231484.942965	51.371546
3473.157661	228995.337512	51.376551
3472.550659	226529.910961	51.381556
3472.089233	224044.157543	51.386561
3471.352312	221546.379073	51.391565
3470.505497	219051.524559	51.396570
3470.542398	216545.015735	51.401575
3469.130238	214036.142101	51.406580
3468.953297	211526.129789	51.411585
3468.865596	209019.074015	51.416589
3468.110995	206499.984030	51.421594
3467.615198	203960.776086	51.426599
3467.107137	201425.815512	51.431604
3466.206938	198884.160224	51.436609
3465.811309	196339.594914	51.441613
3465.256905	193783.200354	51.446618
3464.645135	191226.572142	51.451623
3463.845810	188668.425767	51.456628
3463.150212	186101.741728	51.461633
3463.253303	183544.604514	51.466637
3462.409520	180970.019436	51.471642
3462.084597	178394.322995	51.476647
3460.796558	175812.772121	51.481652
3459.949310	173233.784037	51.486657
3459.550285	170648.684454	51.491661
3458.918061	168065.940554	51.496666
3458.239094	165467.205822	51.501671
3457.290797	162892.938227	51.506676
3456.649946	160296.294307	51.511681
3456.044123	157706.696897	51.516685
3455.002986	155127.294368	51.521690
3454.680986	152531.541676	51.526695
3453.505309	149945.173213	51.531700
3453.271050	147365.761331	51.536705
3452.921513	144697.239348	51.541709
3451.777039	142109.449795	51.546714
3451.331362	139510.605021	51.551719
3450.426278	136916.392613	51.556724
3449.593200	134323.153366	51.561729
3448.499034	131727.262413	51.566733
3447.563088	129147.322406	51.571738
3446.902204	126555.153333	51.576743
3445.864439	123972.233895	51.581748
3444.989141	121411.548112	51.586753
3444.140467	118834.076555	51.591757
3443.275590	116272.063835	51.596762
3442.647852	113702.043714	51.601767
3441.716051	111148.818795	51.606772
3440.890225	108588.823633	51.611777
3440.250413	106036.247904	51.616781
3438.723220	103498.070238	51.621786
3437.649683	100952.858656	51.626791
3436.802077	98428.352675	51.631796
3435.360693	95899.086670	51.636801
3434.525256	93397.049745	51.641805
3433.614478	90894.972425	51.646810
3432.519132	88392.547385	51.651815
3431.159477	85911.058614	51.656820
3430.322252	83440.980423	51.661825
3429.188211	80971.244801	51.666829
3427.911003	78530.820103	51.671834
3426.875956	76081.248698	51.676839
3425.563430	73666.714827	51.681844
3424.415566	71256.993433	51.686849
3423.414757	68858.841145	51.691853
3422.133178	66468.089987	51.696858
3420.956806	64103.689568	51.701863
3419.407371	61754.701595	51.706868
3418.400012	59414.339654	51.711873
3416.938011	57085.080604	51.716877
3415.382751	54783.302271	51.721882
3413.875410	52504.603396	51.726887
3412.277386	50245.569819	51.731892
3410.602489	48006.493033	51.736897
3409.077895	45791.018863	51.741901
3407.468114	43601.243135	51.746906
3406.161257	41433.855133	51.751911
3404.054235	39304.885861	51.756916
3401.561760	37194.572300	51.761921
3399.571807	35130.849126	51.766925
3395.894274	33132.709970	51.771930
3390.876595	31224.987005	51.776935
3384.568446	29425.249096	51.781940
3377.754580	27708.048547	51.786945
3371.793092	26096.421453	51.791949
3365.830665	24613.812288	51.796954
3359.674012	23227.843497	51.801959
3353.681861	21994.876831	51.806964
3347.894062	20875.696330	51.811969
3342.767151	19872.307719	51.816973
3337.389005	18987.595517	51.821978
3332.998317	18199.619263	51.826983
3328.665227	17522.526956	51.831988
3324.967813	16937.527615	51.836993
3321.808507	16433.884071	51.841997
3318.617852	16018.924818	51.847002
3316.373202	15658.498634	51.852007
3314.317387	15372.696547	51.857012
3312.423926	15139.665735	51.862017
3311.232421	14945.044295	51.867021
3309.468664	14795.023839	51.872026
3308.875547	14676.362473	51.877031
3308.175170	14592.708711	51.882036
3307.289471	14526.353620	51.887041
3306.886694	14474.115442	51.892045
3306.153021	14446.792284	51.897050
3305.827343	14424.816785	51.902055
3305.667168	14424.377972	51.907060
3305.225893	14431.781280	51.912065
3305.195356	14431.238145	51.917069
3304.942311	14447.266263	51.922074
3304.823465	14454.974814	51.927079
3304.594357	14475.499608	51.932084
3304.599182	14485.947861	51.937089
3304.944256	14501.982899	51.942093
3304.413677	14518.494664	51.947098
3304.331804	14523.338129	51.952103
3304.302830	14537.711387	51.957108
3304.150877	14540.796868	51.962113
3304.397434	14536.525821	51.967117
3304.125579	14530.834126	51.972122
3304.096933	14511.448490	51.977127
3303.926815	14490.532011	51.982132
3303.718617	14454.918804	51.987137
3303.874288	14432.473890	51.992141
3303.424183	14394.888817	51.997146
3303.434891	14340.658771	52.002151
3302.918884	14303.466016	52.007156
3302.386046	14251.664798	52.012161
3302.578457	14193.118432	52.017165
3301.873928	14143.186340	52.022170
3301.894126	14092.514287	52.027175
3301.427347	14031.285583	52.032180
3300.573341	13963.266468	52.037185
3300.377758	13900.392689	52.042189
3299.974767	13827.308200	52.047194
3299.418334	13765.944089	52.052199
3298.843253	13699.250069	52.057204
3298.405201	13628.095606	52.062209
3297.887602	13542.467498	52.067213
3296.931574	13466.659951	52.072218
3297.041827	13389.760398	52.077223
3296.311589	13324.031465	52.082228
3295.924372	13244.995796	52.087233
3295.433868	13164.630246	52.092237
3294.320366	13096.570542	52.097242
3294.123550	12994.489739	52.102247
3293.855374	12913.793518	52.107252
3293.025651	12841.647481	52.112257
3292.775804	12740.681840	52.117261
3292.174688	12658.035375	52.122266
3291.253143	12561.984472	52.127271
3290.904254	12479.676627	52.132276
3290.448473	12392.048234	52.137281
3289.850338	12298.049923	52.142285
3288.587851	12204.047133	52.147290
3288.332233	12115.423740	52.152295
3287.450203	12028.661726	52.157300
3286.872444	11946.849131	52.162305
3286.435779	11854.402690	52.167309
3285.862230	11767.194345	52.172314
3285.556552	11677.801317	52.177319
3284.590966	11585.601592	52.182324
3283.694402	11496.108250	52.187329
3283.164856	11399.305135	52.192333
3282.436081	11311.560084	52.197338
3282.209445	11226.319353	52.202343
3281.181386	11141.746853	52.207348
3280.495828	11045.593420	52.212353
3280.043228	10955.147143	52.217357
3279.233460	10877.972524	52.222362
3279.210216	10790.741731	52.227367
3278.557844	10705.292050	52.232372
3277.705630	10615.165554	52.237377
3277.171462	10512.026576	52.242381
3276.290979	10433.115572	52.247386
3275.955084	10333.125831	52.252391
3275.319052	10242.176087	52.257396
3274.455612	10149.845366	52.262401
3274.131019	10054.584050	52.267405
3273.130744	9956.353207	52.272410
3272.493137	9864.544805	52.277415
3271.649610	9778.908297	52.282420
3271.018323	9688.618059	52.287425
3270.776114	9588.201384	52.292429
3269.529590	9506.087127	52.297434
3268.945209	9416.469720	52.302439
3268.857281	9330.415806	52.307444
3267.435533	9250.373909	52.312449
3267.148073	9152.669140	52.317453
3266.324827	9065.361499	52.322458
3265.438341	8980.305272	52.327463
3265.141659	8900.164535	52.332468
3264.123486	8808.916849	52.337473
3264.201968	8710.367083	52.342477
3262.903999	8641.063659	52.347482
3262.353175	8553.127732	52.352487
3261.703241	8466.692589	52.357492
3260.922267	8386.123715	52.362497
3260.342042	8301.664847	52.367501
3259.795887	8224.272980	52.372506
3258.995075	8135.303877	52.377511
3258.568670	8057.420810	52.382516
3257.840081	7963.033803	52.387521
3257.594418	7875.707370	52.392525
3256.531757	7797.814196	52.397530
3256.030029	7720.613034	52.402535
3255.311521	7628.898264	52.407540
3254.859028	7549.806559	52.412545
3254.493351	7460.127877	52.417549
3253.817263	7378.482232	52.422554
3253.468739	7280.097064	52.427559
3252.728403	7196.369530	52.432564
3251.961525	7102.003586	52.437569
3251.136618	7003.304222	52.442573
3250.101191	6918.763719	52.447578
3249.847910	6834.523636	52.452583
3249.030378	6754.332475	52.457588
3248.293506	6659.842376	52.462593
3247.551395	6575.902770	52.467597
3246.617143	6490.341066	52.472602
3246.280384	6401.539996	52.477607
3245.818305	6322.665255	52.482612
3244.980724	6237.021259	52.487617
3244.129660	6142.145414	52.492621
3243.394083	6064.632820	52.497626
3242.508459	5990.837516	52.502631
3241.835015	5906.561152	52.507636
3241.035616	5833.181466	52.512641
3240.738826	5750.015134	52.517645
3239.946979	5687.368921	52.522650
3239.421886	5600.983930	52.527655
3238.999930	5528.500682	52.532660
3238.014123	5453.969207	52.537665
3237.435279	5368.516261	52.542669
3237.021343	5287.472996	52.547674
3236.200632	5207.626550	52.552679
3235.133659	5142.330256	52.557684
3234.755246	5064.845996	52.562689
3234.305631	4978.870809	52.567693
3233.460222	4898.651867	52.572698
3232.810249	4820.918261	52.577703
3232.321696	4741.139810	52.582708
3231.299311	4664.062858	52.587713
3230.812193	4585.377074	52.592717
3230.287293	4519.279229	52.597722
3229.563696	4435.766239	52.602727
3228.806814	4360.313187	52.607732
3227.902837	4281.188420	52.612737
3227.410573	4211.618080	52.617741
3227.004251	4146.459386	52.622746
3226.394258	4067.187543	52.627751
3225.628039	3990.255668	52.632756
3224.955678	3917.151332	52.637761
3224.285328	3828.944316	52.642765
3223.479841	3764.259681	52.647770
3222.653934	3691.730626	52.652775
3222.017369	3621.450798	52.657780
3221.228384	3551.988528	52.662785
3220.775132	3486.247554	52.667789
3219.846702	3412.942931	52.672794
3219.368339	3338.644224	52.677799
3218.574252	3261.283993	52.682804
3217.773135	3203.055200	52.687809
3217.365901	3132.794425	52.692813
3216.632019	3066.900998	52.697818
3216.418513	3000.382806	52.702823
3215.187872	2940.743125	52.707828
3214.949087	2855.488801	52.712833
3214.483051	2774.918117	52.717837
3213.951159	2721.446592	52.722842
3212.755276	2646.653107	52.727847
3212.501458	2576.358331	52.732852
3211.484363	2517.515197	52.737857
3211.106023	2437.722407	52.742861
3210.337878	2368.047811	52.747866
3209.396761	2286.670943	52.752871
3208.709205	2224.950702	52.757876
3207.747250	2165.054877	52.762881
3207.633221	2087.983732	52.767885
3206.698464	2039.037225	52.772890
3205.992925	1963.188121	52.777895
3205.555187	1898.773600	52.782900
3204.642550	1840.773388	52.787905
3203.769863	1768.530403	52.792909
3203.120995	1713.736913	52.797914
3202.543605	1646.468641	52.802919
3201.591952	1586.657743	52.807924
3200.927277	1529.101485	52.812929
3200.467815	1466.333084	52.817933
3200.121920	1426.070932	52.822938
3199.472003	1356.264958	52.827943
3198.918043	1292.300304	52.832948
3197.702923	1242.240835	52.837953
3197.162180	1176.508654	52.842957
3196.369707	1118.366633	52.847962
3195.862515	1064.054913	52.852967
3195.115590	1004.697988	52.857972
3194.499494	949.510374	52.862977
3193.942320	884.573300	52.867981
3192.958648	837.495005	52.872986
3192.554882	770.544256	52.877991
3191.845182	713.796069	52.882996
3190.983423	663.547820	52.888001
3190.464153	607.354861	52.893005
3189.903686	567.956580	52.898010
3189.390924	513.314564	52.903015
3188.698424	461.484756	52.908020
3187.707606	404.745853	52.913025
3186.916610	347.034736	52.918029
3185.715797	307.193100	52.923034
3184.750870	273.658149	52.928039
3184.350450	231.324205	52.933044
3183.203950	200.300919	52.938049
3182.175390	161.846517	52.943053
3181.295476	147.485076	52.948058
3180.446057	132.385035	52.953063
3179.066274	137.445149	52.958068
3177.067988	147.134519	52.963073
3176.927039	138.265792	52.968077
3176.550757	144.927973	52.973082
3175.860989	152.578038	52.978087
3175.757417	148.669784	52.983092
3174.920777	152.859889	52.988097
3174.562565	148.768961	52.993101
3173.857058	149.480422	52.998106
3173.049752	152.906452	53.003111
3172.233717	149.520967	53.008116
3171.587330	148.492234	53.013121
3171.674333	153.195177	53.018125
3170.726705	151.561478	53.023130
3169.689091	149.410666	53.028135
3169.438841	151.043008	53.033140
3168.345405	162.768931	53.038145
3168.025476	149.571397	53.043149
3167.534858	152.550567	53.048154
3166.732290	151.441153	53.053159
3166.108265	139.369243	53.058164
3165.139671	150.152138	53.063169
3164.375465	140.954115	53.068173
3164.021180	150.819705	53.073178
3163.120388	151.921761	53.078183
3163.275271	143.218404	53.083188
3162.464498	155.545356	53.088193
3161.289229	145.172985	53.093197
3160.863050	150.415963	53.098202
3159.873757	153.986769	53.103207
3159.953625	146.683303	53.108212
3159.232219	150.056764	53.113217
3158.362255	144.561596	53.118221
3157.704213	152.462025	53.123226
3156.994848	149.172789	53.128231
3156.281363	147.240542	53.133236
3155.572639	152.761921	53.138241
3155.254788	150.784973	53.143245
3154.418633	152.090719	53.148250
3153.880691	150.902542	53.153255
3153.677921	144.165644	53.158260
3152.146254	163.439038	53.163265
3151.950735	151.256806	53.168269
3151.861560	153.088597	53.173274
3150.929018	155.783676	53.178279
3150.068444	152.409356	53.183284
3148.652822	150.669703	53.188289
3148.426940	146.701429	53.193293
3147.677630	148.755742	53.198298
3147.158940	154.428992	53.203303
3146.823836	148.473765	53.208308
3146.035922	147.934995	53.213313
3145.525693	147.312466	53.218317
3145.038253	143.604798	53.223322
3144.273928	143.991187	53.228327
3143.524104	138.376816	53.233332
3142.327902	148.323488	53.238337
3142.341322	141.987409	53.243341
3141.727428	147.263642	53.248346
3140.766930	145.471100	53.253351
3139.957003	138.571501	53.258356
3139.642856	140.795800	53.263361
3139.098569	142.926790	53.268365
3138.617061	145.732698	53.273370
3137.203354	150.826646	53.278375
3136.848680	144.574378	53.283380
3136.388030	151.297554	53.288385
3135.957985	150.750930	53.293389
3135.254014	142.826276	53.298394
3134.020544	150.018986	53.303399
3133.371321	136.859969	53.308404
3132.887953	141.526150	53.313409
3132.364246	143.781517	53.318413
3131.232151	143.200505	53.323418
3130.581591	140.713972	53.328423
3130.948146	138.532067	53.333428
3129.795118	150.294217	53.338433
3128.812267	142.546684	53.343437
3128.259234	148.037120	53.348442
3127.955192	146.055447	53.353447
3127.563622	142.463635	53.358452
3126.740849	145.498373	53.363457
3125.918982	136.740862	53.368461
3124.821393	136.223033	53.373466
3124.156350	140.401978	53.378471
3123.634082	136.113699	53.383476
3122.963262	145.466143	53.388481
3122.537195	135.677476	53.393485
3121.590438	139.758900	53.398490
3120.874558	141.812634	53.403495
3120.803925	134.954485	53.408500
3120.237747	140.522952	53.413505
3120.022728	146.044843	53.418509
3119.065607	143.367933	53.423514
3117.643470	145.320896	53.428519
3117.356167	132.497934	53.433524
3116.094965	139.362625	53.438529
3115.638466	134.494309	53.443533
3115.443142	141.946998	53.448538
3114.559549	140.452761	53.453543
3114.214999	135.211641	53.458548
3113.141938	147.473667	53.463553
3112.588833	137.991700	53.468557
3111.707856	133.855895	53.473562
3111.577590	134.936828	53.478567
3111.406217	129.886774	53.483572
3110.430631	141.567286	53.488577
3109.791548	133.687607	53.493581
3108.921223	130.534829	53.498586
3108.240370	139.202158	53.503591
3107.335956	139.985110	53.508596
3106.429579	144.727122	53.513601
3105.725329	134.453897	53.518605
3105.380196	137.937539	53.523610
3105.014506	135.921403	53.528615
3104.889272	132.804340	53.533620
3104.286231	132.400169	53.538625
3102.791878	139.850212	53.543629
3102.065814	134.308762	53.548634
3101.067982	143.117093	53.553639
3100.539731	139.842316	53.558644
3099.716534	137.338707	53.563649
3099.300243	133.499683	53.568653
3099.346532	133.875465	53.573658
3098.817402	130.963989	53.578663
3098.184788	123.274655	53.583668
3097.191075	138.574753	53.588673
3096.485367	130.562781	53.593677
3095.660340	127.598840	53.598682
3095.013030	136.490563	53.603687
3094.442959	132.758339	53.608692
3093.222482	141.658790	53.613697
3092.686391	128.795452	53.618701
3091.967639	134.218676	53.623706
3091.167269	131.710379	53.628711
3091.682759	135.359991	53.633716
3091.104904	134.477845	53.638721
3089.633481	135.513204	53.643725
3088.510601	130.460339	53.648730
3088.436562	136.112081	53.653735
3087.841609	138.023580	53.658740
3087.056300	135.847439	53.663745
3086.170459	132.415875	53.668749
3085.615114	129.862950	53.673754
3084.669925	135.254209	53.678759
3085.008792	129.455412	53.683764
3084.358882	138.592705	53.688769
3083.580243	128.937711	53.693773
3082.493909	134.198748	53.698778
3081.260052	138.238840	53.703783
3081.689786	130.905604	53.708788
3080.871093	139.448858	53.713793
3080.319800	128.335580	53.718797
3078.938842	133.461042	53.723802
3077.853557	136.519323	53.728807
3078.364115	123.323213	53.733812
3077.373357	131.364955	53.738817
3077.223280	131.226408	53.743821
3076.533626	128.637225	53.748826
3075.519184	131.211701	53.753831
3074.198219	130.175485	53.758836
3073.570779	135.775340	53.763841
3073.349988	133.506691	53.768845
3072.951469	139.630314	53.773850
3072.284533	136.192137	53.778855
3071.926090	128.825423	53.783860
3070.480991	134.976690	53.788865
3069.461214	128.255465	53.793869
3069.162758	132.116780	53.798874
3068.186157	134.736501	53.803879
3067.952908	130.345955	53.808884
3067.004171	145.638769	53.813889
3066.723001	133.573040	53.818893
3066.835797	129.739140	53.823898
3065.317389	135.633336	53.828903
3064.272184	133.934229	53.833908
3064.139352	139.273524	53.838913
3063.877641	136.652666	53.843917
3063.099450	131.978663	53.848922
3061.654854	130.950943	53.853927
3061.954323	130.233490	53.858932
3060.839742	141.016460	53.863937
3059.803448	133.342817	53.868941
3059.516299	138.820188	53.873946
3059.170934	132.192933	53.878951
3058.600367	130.672455	53.883956
3057.157451	129.266696	53.888961
3057.111290	126.239938	53.893965
3056.608053	131.003459	53.898970
3055.235543	140.025020	53.903975
3054.813182	135.429556	53.908980
3054.359600	139.384877	53.913985
3053.809226	132.204508	53.918989
3052.724762	129.830812	53.923994
3052.477464	131.937113	53.928999
3051.923074	132.803551	53.934004
3050.346076	130.266521	53.939009
3050.445076	127.781788	53.944013
3050.235961	130.659572	53.949018
3048.612086	141.687853	53.954023
3048.285603	134.161735	53.959028
3048.265465	137.140252	53.964033
3046.835716	125.343817	53.969037
3046.035931	127.762411	53.974042
3045.692586	132.275985	53.979047
3045.198478	135.789426	53.984052
3044.344341	134.431876	53.989057
3043.634290	137.520385	53.994061
3042.972615	135.380361	53.999066
3042.812172	139.589533	54.004071
3042.455354	130.494034	54.009076
3041.036434	139.966411	54.014081
3039.917284	133.264539	54.019085
3038.988329	133.927751	54.024090
3039.025945	137.491647	54.029095
3038.879642	126.143787	54.034100
3038.042755	134.676334	54.039105
3036.864646	129.893044	54.044109
3036.502635	135.684383	54.049114
3035.721055	140.054164	54.054119
3035.200667	131.971459	54.059124
3034.411324	131.014934	54.064129
3033.649378	131.701318	54.069133
3033.577343	130.274074	54.074138
3032.499472	135.339072	54.079143
3031.738092	128.176212	54.084148
3030.860560	139.722737	54.089153
3030.693424	135.200109	54.094157
3029.799902	133.694952	54.099162
3028.899319	130.193289	54.104167
3029.274822	136.149913	54.109172
3028.168623	139.232697	54.114177
3027.174245	137.346494	54.119181
3026.625641	123.691518	54.124186
3025.710642	141.404160	54.129191
3025.136777	135.747509	54.134196
3024.556917	136.896189	54.139201
3023.861499	132.575145	54.144205
3023.459788	125.774767	54.149210
3022.455506	128.347120	54.154215
3022.221953	128.570199	54.159220
3021.236408	128.161531	54.164225
3020.910744	126.954070	54.169229
3020.318416	126.987408	54.174234
3019.676583	135.277816	54.179239
3018.989583	128.973411	54.184244
3018.392367	132.350922	54.189249
3017.177860	130.145504	54.194253
3016.439212	118.425594	54.199258
3015.988963	132.441141	54.204263
3015.713792	126.377805	54.209268
3014.622673	129.684586	54.214273
3013.845744	122.742673	54.219277
3013.362744	123.058112	54.224282
3012.368128	132.227859	54.229287
3012.504963	125.301510	54.234292
3011.381980	128.884913	54.239297
3010.163846	124.264389	54.244301
3010.403768	127.527666	54.249306
3009.470934	134.442441	54.254311
3008.738816	127.198009	54.259316
3007.998396	142.469433	54.264321
3007.433717	131.601213	54.269325
3006.978687	135.308499	54.274330
3006.317440	135.147963	54.279335
3005.601565	128.707578	54.284340
3004.910865	137.526587	54.289345
3004.268422	130.374592	54.294349
3004.037278	126.004218	54.299354
3003.216160	138.053458	54.304359
3002.749870	129.696260	54.309364
3001.230714	133.234471	54.314369
3000.327663	130.089674	54.319373
3000.182942	123.879711	54.324378
2999.979617	130.111288	54.329383
2998.979006	125.348204	54.334388
2998.092744	122.991572	54.339393
2997.504418	126.343486	54.344397
2997.056431	128.369610	54.349402
2995.879142	124.344858	54.354407
2995.578680	119.527265	54.359412
2995.025615	123.838654	54.364417
2994.237873	121.188879	54.369421
2993.652989	116.250552	54.374426
2992.943907	124.821255	54.379431
2992.384807	118.263299	54.384436
2992.068055	123.485598	54.389441
2991.590285	127.840963	54.394445
2991.204886	117.426845	54.399450
2989.938082	124.390397	54.404455
2988.980248	120.656559	54.409460
2987.959521	127.574115	54.414465
2987.414932	124.447407	54.419469
2986.854114	113.353155	54.424474
2985.978428	125.820647	54.429479
2985.832816	119.348347	54.434484
2984.924474	119.443979	54.439489
2984.411560	124.822954	54.444493
2983.731552	126.179798	54.449498
2983.221434	121.465925	54.454503
2982.760481	122.024699	54.459508
2981.972832	118.656903	54.464513
2981.757434	129.047801	54.469517
2980.627980	121.865750	54.474522
2979.178372	123.975405	54.479527
2979.015117	121.616408	54.484532
2978.691148	125.923781	54.489537
2978.037374	125.163960	54.494541
2976.984174	120.002117	54.499546
2976.145983	119.185787	54.504551
2975.676585	118.241307	54.509556
2975.310968	127.384881	54.514561
2974.567377	124.208498	54.519565
2974.343361	124.716915	54.524570
2973.274224	132.013790	54.529575
2973.094847	126.255793	54.534580
2972.069902	119.666922	54.539585
2971.251389	124.063541	54.544589
2970.174469	115.832019	54.549594
2969.698905	123.924276	54.554599
2968.921195	115.017561	54.559604
2968.692875	118.639526	54.564609
2968.090584	116.589628	54.569613
2967.399535	117.997306	54.574618
2966.824314	130.767132	54.579623
2966.389163	124.192339	54.584628
2965.574680	126.099125	54.589633
2965.109226	123.773612	54.594637
2963.849822	119.289230	54.599642
2962.479577	124.389986	54.604647
2962.045826	120.102002	54.609652
2962.272597	128.553440	54.614657
2961.636443	117.780741	54.619661
2960.673660	116.547163	54.624666
2959.579542	123.719229	54.629671
2959.128743	114.347321	54.634676
2958.605218	120.441774	54.639681
2957.902500	121.838026	54.644685
2957.446845	114.457949	54.649690
2956.966254	119.146549	54.654695
2956.611936	113.826599	54.659700
2955.666582	122.517412	54.664705
2954.942988	113.081205	54.669709
2954.592493	120.366187	54.674714
2952.958187	127.228736	54.679719
2952.107418	117.469268	54.684724
2952.671638	120.623438	54.689729
2951.267978	127.969190	54.694733
2950.991834	123.355465	54.699738
2949.998483	128.804307	54.704743
2949.444427	124.718457	54.709748
2949.134525	123.734486	54.714753
2948.365405	123.745939	54.719757
2947.991600	118.842598	54.724762
2946.438644	120.199811	54.729767
2945.967634	121.479497	54.734772
2945.255517	123.351424	54.739777
2945.122354	126.544640	54.744781
2943.749023	123.335750	54.749786
2943.144710	127.069337	54.754791
2942.926970	122.842728	54.759796
2942.249372	128.252216	54.764801
2941.620143	128.244502	54.769805
2941.255317	117.080845	54.774810
2940.523894	130.002096	54.779815
2940.246442	114.538358	54.784820
2938.824886	117.560177	54.789825
2937.818179	125.761754	54.794829
2937.546334	127.031484	54.799834
2936.465811	125.517644	54.804839
2936.356152	123.539874	54.809844
2935.730388	122.705406	54.814849
2935.069065	118.139746	54.819853
2935.020252	118.200603	54.824858
2933.861424	124.848876	54.829863
2933.436592	115.118860	54.834868
2931.997684	114.238225	54.839873
2931.018418	116.717107	54.844877
2931.213283	113.730087	54.849882
2930.198992	115.254585	54.854887
2929.782057	106.590170	54.859892
2929.287476	122.324020	54.864897
2928.609787	121.433296	54.869901
2928.377586	117.011009	54.874906
2927.020414	131.318504	54.879911
2926.166168	118.860101	54.884916
2925.600370	121.439242	54.889921
2924.896142	117.328141	54.894925
2924.468265	121.842739	54.899930
2923.783199	126.946801	54.904935
2923.328541	124.687341	54.909940
2922.724331	128.034475	54.914945
2922.176947	129.579050	54.919949
2921.390203	120.001668	54.924954
2920.022755	125.867328	54.929959
2919.604479	114.874254	54.934964
2918.796801	114.737568	54.939969
2917.989845	117.091876	54.944973
2917.849277	116.725136	54.949978
2917.050057	121.521083	54.954983
2916.589160	115.557396	54.959988
2916.111877	117.987598	54.964993
2915.299619	118.464311	54.969997
2915.400826	110.257650	54.975002
2914.085501	123.944584	54.980007
2913.474108	116.250084	54.985012
2912.503653	122.767091	54.990017
2911.742553	121.095250	54.995021
2911.305015	117.509744	55.000026
2910.589387	121.312091	55.005031
2910.083859	117.256243	55.010036
2908.984190	114.875705	55.015041
2907.962262	116.917025	55.020045
2908.249254	112.133257	55.025050
2907.108267	118.349020	55.030055
2906.237404	111.513186	55.035060
2905.778109	112.110364	55.040065
2904.947939	117.175277	55.045069
2904.624691	121.385818	55.050074
2903.964283	126.170677	55.055079
2903.427745	118.844690	55.060084
2903.102393	124.457659	55.065089
2902.508892	127.782833	55.070093
2901.850895	117.697547	55.075098
2900.124461	122.112363	55.080103
2899.533026	118.414215	55.085108
2899.235878	109.941300	55.090113
2898.669885	114.722651	55.095117
2898.424549	116.587834	55.100122
2897.545675	115.439005	55.105127
2897.379548	108.261295	55.110132
2896.298323	114.817362	55.115137
2895.201906	116.087883	55.120141
2894.530255	111.107955	55.125146
2893.701714	111.172201	55.130151
2893.459474	109.658396	55.135156
2892.924080	106.175274	55.140161
2892.189382	114.892453	55.145165
2891.844555	109.202217	55.150170
2890.532064	117.693282	55.155175
2889.674312	110.953498	55.160180
2889.067341	115.875271	55.165185
2888.270802	119.226459	55.170189
2888.411666	108.347044	55.175194
2887.435431	111.605786	55.180199
2887.257754	115.758291	55.185204
2886.366004	112.556326	55.190209
2885.670978	114.891508	55.195213
2885.638762	116.669745	55.200218
2883.963454	118.841678	55.205223
2883.360350	113.375181	55.210228
2882.696564	112.809315	55.215233
2882.136174	114.543610	55.220237
2882.054444	112.109110	55.225242
2881.069964	112.126984	55.230247
2880.466343	117.869215	55.235252
2879.579780	114.339926	55.240257
2878.845918	111.615834	55.245261
2878.326457	108.456428	55.250266
2877.855953	112.795946	55.255271
2877.396901	103.852168	55.260276
2876.085667	110.259655	55.265281
2875.056323	115.011250	55.270285
2874.241091	104.472469	55.275290
2873.777667	116.481878	55.280295
2873.910879	118.808538	55.285300
2872.805568	112.920254	55.290305
2871.987520	119.840679	55.295309
2871.605458	116.933704	55.300314
2871.134661	115.231993	55.305319
2870.703076	116.267716	55.310324
2870.181010	108.467964	55.315329
2869.094297	111.037057	55.320333
2868.152761	109.534610	55.325338
2867.686218	112.300864	55.330343
2867.564727	108.462410	55.335348
2867.042498	106.289898	55.340353
2865.539232	113.044014	55.345357
2864.925960	102.409538	55.350362
2864.046512	114.072426	55.355367
2863.357250	108.607238	55.360372
2862.881041	101.471872	55.365377
2861.802186	108.140032	55.370381
2861.798589	109.834826	55.375386
2860.858249	111.289856	55.380391
2860.574572	107.874241	55.385396
2860.244168	103.028233	55.390401
2859.413541	116.723116	55.395405
2858.738221	109.843216	55.400410
2857.677967	118.782217	55.405415
2856.714640	118.982001	55.410420
2856.518997	98.666950	55.415425
2855.811305	110.267719	55.420429
2855.290821	111.680994	55.425434
2854.925800	106.916688	55.430439
2854.225859	110.686752	55.435444
2853.223666	108.961786	55.440449
2852.038283	115.907096	55.445453
2851.644722	114.053244	55.450458
2851.152216	112.619712	55.455463
2850.990456	107.997111	55.460468
2850.571670	103.534883	55.465473
2849.069160	105.267566	55.470477
2848.445676	105.303484	55.475482
2847.248144	111.180373	55.480487
2846.644338	106.136757	55.485492
2846.343213	104.138033	55.490497
2845.913856	112.616717	55.495501
2845.523971	107.487594	55.500506
2844.868714	105.743993	55.505511
2844.538072	97.233003	55.510516
2843.299533	101.349713	55.515521
2842.026608	119.190993	55.520525
2841.814072	108.065279	55.525530
2841.228539	108.705747	55.530535
2840.836974	109.064387	55.535540
2840.514852	110.752832	55.540545
2839.370853	115.134038	55.545549
2838.487159	106.564016	55.550554
2837.621675	111.235506	55.555559
2837.320171	118.778158	55.560564
2837.014187	108.710491	55.565569
2836.155666	114.229847	55.570573
2835.890634	106.204205	55.575578
2834.457303	115.036051	55.580583
2833.492339	110.245997	55.585588
2833.066964	108.505345	55.590593
2832.444424	120.037490	55.595597
2831.946017	107.776458	55.600602
2831.462372	105.518806	55.605607
2831.142623	107.862879	55.610612
2830.626289	101.460671	55.615617
2829.415968	112.890773	55.620621
2828.576739	104.519597	55.625626
2827.771620	106.116122	55.630631
2827.419657	105.555389	55.635636
2827.199107	103.669998	55.640641
2826.217041	110.043733	55.645645
2825.789858	99.030106	55.650650
2824.456466	108.140519	55.655655
2823.515193	107.867211	55.660660
2823.598889	107.906606	55.665665
2822.673505	109.099751	55.670669
2822.345321	104.078109	55.675674
2821.784092	110.272160	55.680679
2821.082533	104.148707	55.685684
2820.285796	107.404805	55.690689
2819.152072	120.793477	55.695693
2818.420590	104.885152	55.700698
2818.212281	108.865263	55.705703
2817.458622	106.233378	55.710708
2817.286299	110.827453	55.715713
2816.518588	108.998473	55.720717
2815.706017	98.053479	55.725722
2814.538186	106.234833	55.730727
2814.005255	109.596234	55.735732
2813.519083	102.939012	55.740737
2812.695916	111.645261	55.745741
2812.568641	102.960965	55.750746
2811.998096	111.113658	55.755751
2811.154401	107.834023	55.760756
2810.161610	101.631274	55.765761
2809.411860	108.086091	55.770765
2808.702573	105.771483	55.775770
2808.403267	109.398868	55.780775
2808.066591	109.149725	55.785780
2807.615451	105.383800	55.790785
2806.241364	110.147747	55.795789
2805.567125	104.186991	55.800794
2805.007441	111.202992	55.805799
2804.735975	114.779042	55.810804
2803.778962	113.452536	55.815809
2802.943394	114.338237	55.820813
2802.215970	103.434740	55.825818
2801.331849	111.867600	55.830823
2800.535744	107.131981	55.835828
2800.204792	105.222435	55.840833
2799.319050	109.945547	55.845837
2799.349973	106.500641	55.850842
2798.664117	108.256781	55.855847
2798.328323	109.785726	55.860852
2797.362143	104.832078	55.865857
2796.114142	102.433500	55.870861
2795.879161	103.115502	55.875866
2794.999393	100.442019	55.880871
2794.141384	104.650406	55.885876
2794.149742	105.633439	55.890881
2792.857627	109.447484	55.895885
2792.543225	104.599142	55.900890
2791.566163	110.322309	55.905895
2790.737266	110.122954	55.910900
2790.757385	102.393179	55.915905
2789.792271	105.313331	55.920909
2789.881243	91.970247	55.925914
2788.344227	98.394228	55.930919
2787.846264	106.772532	55.935924
2787.652956	105.960087	55.940929
2786.661455	110.507072	55.945933
2786.102830	98.760808	55.950938
2784.943138	107.073403	55.955943
2784.182137	111.046139	55.960948
2783.532192	103.517729	55.965953
2783.212809	106.563956	55.970957
2782.466125	100.237442	55.975962
2781.993793	107.692051	55.980967
2781.370027	99.700497	55.985972
2780.568896	98.637872	55.990977
2779.072158	109.190116	55.995981
2778.577967	100.831425	56.000986
2778.587425	97.220064	56.005991
2778.406391	105.956292	56.010996
2777.158788	103.625937	56.016001
2776.599138	98.190325	56.021005
2776.279930	100.989029	56.026010
2775.879316	109.239778	56.031015
2774.566949	111.725485	56.036020
2774.151508	104.395408	56.041025
2773.209544	110.902029	56.046029
2772.796396	98.965119	56.051034
2772.285362	106.231348	56.056039
2770.731953	108.434184	56.061044
2770.350636	112.341632	56.066049
2769.446217	110.770887	56.071053
2769.277392	106.548567	56.076058
2769.060161	104.450644	56.081063
2768.391998	105.902587	56.086068
2767.745129	102.410905	56.091073
2766.682165	110.509608	56.096077
2765.921660	105.220032	56.101082
2765.267053	106.636106	56.106087
2765.025633	109.161788	56.111092
2764.655705	106.725632	56.116097
2763.460445	109.935382	56.121101
2762.273346	105.831056	56.126106
2761.896596	98.943174	56.131111
2761.009545	108.512159	56.136116
2760.661197	103.146218	56.141121
2760.096975	108.449098	56.146125
2759.963434	105.574657	56.151130
2759.253492	100.296178	56.156135
2758.277824	109.525058	56.161140
2757.547643	97.688128	56.166145
2756.766267	105.703175	56.171149
2756.201392	102.095640	56.176154
2755.755707	105.041881	56.181159
2754.275956	104.450897	56.186164
2753.433020	100.561690	56.191169
2753.290799	113.609579	56.196173
2752.852109	111.821869	56.201178
2752.366175	116.581649	56.206183
2751.614135	102.941005	56.211188
2751.357717	98.138415	56.216193
2750.293482	107.321645	56.221197
2749.639692	103.189720	56.226202
2748.880848	104.914525	56.231207
2748.348623	103.411216	56.236212
2748.121009	101.959656	56.241217
2746.353823	109.042315	56.246221
2745.719685	101.167800	56.251226
2745.053202	106.698942	56.256231
2744.865455	102.565120	56.261236
2744.465528	102.879802	56.266241
2743.661919	104.338715	56.271245
2743.132136	107.124467	56.276250
2743.090879	99.873331	56.281255
2741.835281	100.895963	56.286260
2740.837869	101.906831	56.291265
2740.052541	116.171847	56.296269
2739.844279	104.597803	56.301274
2739.185034	102.769243	56.306279
2738.161288	107.120040	56.311284
2737.491408	107.594940	56.316289
2736.682136	102.882900	56.321293
2736.085842	100.472809	56.326298
2735.933250	106.653066	56.331303
2735.394695	105.365571	56.336308
2734.847131	96.432610	56.341313
2733.581538	111.216277	56.346317
2732.847403	100.797485	56.351322
2732.324538	104.200590	56.356327
2731.696510	106.647094	56.361332
2731.555084	102.743375	56.366337
2729.819582	118.946671	56.371341
2729.547412	103.589452	56.376346
2728.365093	98.083836	56.381351
2727.679128	99.408961	56.386356
2727.917094	96.329316	56.391361
2727.239668	107.964382	56.396365
2726.500164	102.465574	56.401370
2726.185044	100.007029	56.406375
2725.531304	107.626852	56.411380
2724.893080	103.608713	56.416385
2723.637921	110.321236	56.421389
2723.034299	103.630815	56.426394
2722.547751	106.668513	56.431399
2721.749050	109.120113	56.436404
2720.851950	102.328677	56.441409
2719.914614	113.103858	56.446413
2719.276795	104.273557	56.451418
2719.266295	104.562728	56.456423
2718.400231	104.409210	56.461428
2718.336081	107.956533	56.466433
2717.655595	106.560673	56.471437
2716.967666	101.326990	56.476442
2715.888065	105.952592	56.481447
2714.982260	112.228834	56.486452
2715.390017	100.744101	56.491457
2714.076695	107.731031	56.496461
2712.498393	107.875698	56.501466
2711.792890	106.214122	56.506471
2711.596643	108.018420	56.511476
2711.509273	101.399229	56.516481
2710.650474	105.571050	56.521485
2710.325902	104.467633	56.526490
2710.180802	108.106159	56.531495
2708.679405	102.798767	56.536500
2707.715587	107.459447	56.541505
2706.991158	104.915344	56.546509
2706.671450	101.327882	56.551514
2705.955376	101.411615	56.556519
2705.341629	106.080744	56.561524
2704.660873	98.498015	56.566529
2703.655647	107.733923	56.571533
2703.029549	106.095881	56.576538
2702.796007	101.027682	56.581543
2702.243157	100.244725	56.586548
2701.813636	96.605380	56.591553
2700.781521	98.653997	56.596557
2699.972385	99.496904	56.601562
2699.648820	105.671648	56.606567
2698.850788	109.201919	56.611572
2698.402966	99.818901	56.616577
2697.058807	101.851386	56.621581
2696.505493	101.145875	56.626586
2696.034388	96.488932	56.631591
2695.222793	95.884805	56.636596
2695.399206	99.047990	56.641601
2694.242848	108.813797	56.646605
2692.919293	98.524978	56.651610
2692.245108	91.941758	56.656615
2691.575687	109.514878	56.661620
2691.510845	101.445960	56.666625
2690.672096	110.644336	56.671629
2690.454293	100.930299	56.676634
2690.043211	95.561277	56.681639
2688.888440	104.270132	56.686644
2688.223329	93.061950	56.691649
2687.414217	91.671898	56.696653
2686.863667	90.720792	56.701658
2686.228850	86.284859	56.706663
2685.491501	99.212620	56.711668
2684.476251	94.692507	56.716673
2684.018811	98.957561	56.721677
2683.552821	92.611509	56.726682
2683.152221	97.712741	56.731687
2682.375431	95.652843	56.736692
2681.796032	96.988571	56.741697
2680.583195	96.720656	56.746701
2680.040739	98.487820	56.751706
2679.488926	94.282031	56.756711
2678.982896	106.036214	56.761716
2678.486171	90.043214	56.766721
2677.360037	92.683809	56.771725
2676.375487	91.447296	56.776730
2676.066383	106.651656	56.781735
2675.239306	104.603117	56.786740
2675.124725	99.581295	56.791745
2674.239186	99.167437	56.796749
2674.036923	99.742406	56.801754
2673.611188	98.588392	56.806759
2672.298104	99.139695	56.811764
2671.788861	101.002232	56.816769
2670.931789	104.772327	56.821773
2670.557921	96.388354	56.826778
2669.525121	94.851020	56.831783
2668.670246	104.571213	56.836788
2668.104130	93.806757	56.841793
2667.698748	102.138444	56.846797
2667.449461	104.739285	56.851802
2666.735409	101.328574	56.856807
2665.190852	104.231743	56.861812
2664.299549	106.118933	56.866817
2663.682921	105.113204	56.871821
2663.393334	105.565737	56.876826
2663.113047	104.115290	56.881831
2662.482231	108.361432	56.886836
2662.239482	93.753923	56.891841
2661.637077	103.223333	56.896845
2660.384459	102.801569	56.901850
2659.749478	103.134728	56.906855
2658.907409	102.617128	56.911860
2658.671410	93.552770	56.916865
2658.049117	99.696077	56.921869
2656.776738	101.949189	56.926874
2656.129498	98.772183	56.931879
2655.491227	97.933967	56.936884
2655.177412	97.735792	56.941889
2654.814088	102.512901	56.946893
2654.174896	98.526519	56.951898
2653.126220	101.999378	56.956903
2652.487910	102.374947	56.961908
2652.085998	93.796831	56.966913
2651.241881	106.021687	56.971917
2650.607125	101.344173	56.976922
2649.630561	101.213896	56.981927
2648.586855	98.819510	56.986932
2648.455495	91.458266	56.991937
2647.829944	97.872912	56.996941
2647.167620	95.821083	57.001946
2647.058191	100.408347	57.006951
2645.870477	100.915331	57.011956
2645.047822	93.011489	57.016961
2644.437673	102.757741	57.021965
2643.607044	101.420319	57.026970
2643.541813	101.604376	57.031975
2642.730469	98.678444	57.036980
2642.593624	92.159296	57.041985
2641.163179	96.653439	57.046989
2640.113609	90.862665	57.051994
2639.807399	90.066369	57.056999
2639.425028	92.383651	57.062004
2639.175690	95.441985	57.067009
2638.243329	97.808681	57.072013
2637.394931	92.397979	57.077018
2636.812195	97.530741	57.082023
2636.248323	100.409166	57.087028
2634.765662	100.730526	57.092033
2633.688834	100.219904	57.097037
2633.800077	99.346721	57.102042
2633.656993	91.240664	57.107047
2632.726455	106.158893	57.112052
2632.550854	93.376565	57.117057
2631.637904	100.016389	57.122061
2630.574736	102.720042	57.127066
2629.846969	97.872122	57.132071
2629.211545	98.376670	57.137076
2629.022341	90.610461	57.142081
2628.054715	97.412783	57.147085
2627.251111	91.957322	57.152090
2626.256960	97.203833	57.157095
2625.345134	106.572592	57.162100
2625.400747	85.015099	57.167105
2624.856595	93.647205	57.172109
2624.244669	91.232302	57.177114
2623.872591	88.398648	57.182119
2622.872656	105.034342	57.187124
2622.026693	88.888303	57.192129
2621.130724	91.646661	57.197133
2620.848170	101.360595	57.202138
2620.417647	89.115651	57.207143
2619.816586	98.043662	57.212148
2619.002843	92.078768	57.217153
2617.848172	91.198969	57.222157
2617.300879	96.986442	57.227162
2616.872363	90.485579	57.232167
2616.273750	89.872291	57.237172
2616.201386	88.043685	57.242177
2614.824280	91.952417	57.247181
2613.589901	98.149046	57.252186
2613.365066	90.289065	57.257191
2612.764876	94.844567	57.262196
2612.611837	84.299638	57.267201
2611.828895	90.365015	57.272205
2610.644277	90.407676	57.277210
2610.244464	89.831060	57.282215
2609.175723	97.907866	57.287220
2609.175909	87.377004	57.292225
2608.559074	96.374024	57.297229
2607.367276	89.942068	57.302234
2606.688019	83.374340	57.307239
2606.103835	91.977368	57.312244
2605.626816	89.794398	57.317249
2605.243316	93.273548	57.322253
2604.638266	90.770239	57.327258
2603.435668	89.528385	57.332263
2602.472415	102.244511	57.337268
2602.138907	90.749540	57.342273
2601.796712	99.077527	57.347277
2601.140601	96.298745	57.352282
2600.693775	92.251068	57.357287
2599.481062	100.847867	57.362292
2598.794722	91.733007	57.367297
2598.301127	99.095724	57.372301
2597.884407	94.119245	57.377306
2597.433209	95.408198	57.382311
2595.915547	100.799074	57.387316
2595.564053	95.452641	57.392321
2594.718522	98.492898	57.397325
2594.309519	99.705561	57.402330
2594.093888	94.993907	57.407335
2593.399683	98.311444	57.412340
2592.580556	91.737627	57.417345
2591.545855	91.273890	57.422349
2590.731784	94.434686	57.427354
2590.463963	80.755539	57.432359
2590.192326	91.052184	57.437364
2588.913844	90.555519	57.442369
2587.905743	94.816819	57.447373
2587.247010	95.107468	57.452378
2586.980430	94.337557	57.457383
2586.425721	100.608652	57.462388
2585.952529	96.437198	57.467393
2585.631628	91.226453	57.472397
2585.486373	91.500767	57.477402
2584.391833	92.088148	57.482407
2583.081331	97.766102	57.487412
2581.919981	93.198755	57.492417
2581.373606	94.985937	57.497421
2580.597117	96.826274	57.502426
2580.599425	95.102530	57.507431
2579.776305	100.347046	57.512436
2579.677878	97.417273	57.517441
2579.238607	95.967959	57.522445
2578.046158	92.583392	57.527450
2577.679422	94.137766	57.532455
2576.656644	99.608644	57.537460
2576.142006	88.419768	57.542465
2575.035647	93.349161	57.547469
2574.192526	94.660117	57.552474
2573.954161	83.980180	57.557479
2572.966135	87.831878	57.562484
2572.801690	94.130593	57.567489
2571.992415	97.128735	57.572493
2570.588301	96.303036	57.577498
2570.409302	87.295658	57.582503
2569.433907	96.078459	57.587508
2569.137036	94.458755	57.592513
2568.568210	92.307667	57.597517
2568.013594	95.106358	57.602522
2567.862003	96.717502	57.607527
2566.676278	95.109231	57.612532
2565.928375	89.623340	57.617537
2565.385630	89.877979	57.622541
2564.591613	95.306592	57.627546
2564.610040	87.515554	57.632551
2563.219692	98.724614	57.637556
2562.854151	86.652516	57.642561
2562.148192	89.430897	57.647565
2561.390974	87.041237	57.652570
2560.781600	87.237006	57.657575
2559.764673	101.032010	57.662580
2558.988475	89.568125	57.667585
2558.266994	91.848255	57.672589
2557.796579	92.668406	57.677594
2557.576612	91.015030	57.682599
2556.927323	99.242758	57.687604
2556.407269	101.538189	57.692609
2555.626402	102.041558	57.697613
2554.323475	99.299151	57.702618
2554.123387	98.554979	57.707623
2553.621716	107.605342	57.712628
2553.490888	96.939777	57.717633
2552.314892	100.053114	57.722637
2550.872309	100.070812	57.727642
2550.605448	98.015729	57.732647
2550.335695	103.429716	57.737652
2549.675454	99.702730	57.742657
2548.710709	103.874523	57.747661
2547.747369	106.900588	57.752666
2547.314933	96.992353	57.757671
2546.728482	105.564594	57.762676
2546.101029	111.297491	57.767681
2546.036898	97.034059	57.772685
2544.929476	108.869342	57.777690
2543.864583	97.368366	57.782695
2543.296137	98.652499	57.787700
2542.630145	103.837394	57.792705
2542.252225	96.776460	57.797709
2541.874722	104.676684	57.802714
2541.074231	104.142916	57.807719
2539.890847	104.922331	57.812724
2539.281519	102.877640	57.817729
2538.960299	97.132891	57.822733
2538.276849	110.763923	57.827738
2538.061927	100.364174	57.832743
2537.151053	99.170747	57.837748
2536.106038	102.929174	57.842753
2535.737402	98.873662	57.847757
2534.851871	99.575710	57.852762
2534.529697	93.663368	57.857767
2533.417549	106.912571	57.862772
2532.966398	105.109250	57.867777
2532.534126	108.808711	57.872781
2531.684097	108.198943	57.877786
2531.596912	107.437047	57.882791
2529.943028	115.215630	57.887796
2529.435452	101.313395	57.892801
2529.010056	101.427190	57.897805
2527.970222	109.906818	57.902810
2528.054338	90.928332	57.907815
2527.107619	99.620975	57.912820
2526.506522	99.293903	57.917825
2525.443817	102.497215	57.922829
2524.747111	100.232209	57.927834
2524.779830	96.441229	57.932839
2523.932121	101.949288	57.937844
2522.620394	108.316653	57.942849
2522.113928	100.233257	57.947853
2521.399655	102.842150	57.952858
2521.234542	96.902168	57.957863
2520.936560	102.763861	57.962868
2520.174382	101.800402	57.967873
2519.447876	99.896138	57.972877
2518.208237	97.768954	57.977882
2518.325881	85.796621	57.982887
2516.765900	95.838673	57.987892
2515.509351	97.272817	57.992897
2515.604454	97.691165	57.997901
2514.695741	105.565368	58.002906
2514.423672	89.067046	58.007911
2513.730410	99.183941	58.012916
2513.493661	101.762114	58.017921
2513.438021	93.814009	58.022925
2512.000869	95.461393	58.027930
2511.338637	93.651139	58.032935
2510.334433	101.553113	58.037940
2509.788676	91.668210	58.042945
2509.216703	93.250965	58.047949
2508.314023	97.713326	58.052954
2507.655705	92.752507	58.057959
2507.097095	100.403831	58.062964
2507.030061	96.084003	58.067969
2506.044367	94.158925	58.072973
2504.913921	99.006004	58.077978
2504.381658	100.364083	58.082983
2503.893433	99.302081	58.087988
2503.587998	100.907951	58.092993
2503.498560	106.664520	58.097997
2501.833914	101.886010	58.103002
2500.948082	97.433810	58.108007
2500.694403	101.492724	58.113012
2499.901444	102.310394	58.118017
2499.384860	99.579611	58.123021
2498.135977	101.750187	58.128026
2498.100252	100.820027	58.133031
2497.323760	110.477885	58.138036
2496.352879	98.849537	58.143041
2496.088814	99.980191	58.148045
2495.295760	94.961885	58.153050
2494.659460	96.327884	58.158055
2493.654572	104.908114	58.163060
2493.182984	96.379829	58.168065
2492.613061	100.614385	58.173069
2492.232911	103.253785	58.178074
2491.893690	100.870430	58.183079
2490.787178	97.831574	58.188084
2490.101456	97.463713	58.193089
2489.858263	95.073415	58.198093
2488.481479	99.044090	58.203098
2487.186717	99.231526	58.208103
2486.985936	101.916835	58.213108
2486.679836	99.212040	58.218113
2486.135193	94.885452	58.223117
2485.506713	101.820852	58.228122
2485.337529	92.516945	58.233127
2484.020815	98.070851	58.238132
2482.971225	91.660798	58.243137
2482.688091	96.219335	58.248141
2482.060036	94.572579	58.253146
2481.335875	87.872819	58.258151
2481.255736	104.234020	58.263156
2480.333938	102.140132	58.268161
2479.309960	96.245157	58.273165
2478.486861	98.375307	58.278170
2478.344534	87.679358	58.283175
2477.749026	95.190547	58.288180
2477.038688	90.462831	58.293185
2476.432749	92.839659	58.298189
2475.141805	93.046180	58.303194
2474.706486	88.568672	58.308199
2474.173275	90.028754	58.313204
2473.661787	88.287467	58.318209
2472.397138	88.134242	58.323213
2471.783654	99.204175	58.328218
2471.205926	91.657959	58.333223
2470.645777	93.683155	58.338228
2470.431462	96.119734	58.343233
2470.491389	91.678337	58.348237
2469.229989	99.783756	58.353242
2468.434839	97.461777	58.358247
2467.954366	99.242438	58.363252
2467.048004	93.338804	58.368257
2466.229611	90.691601	58.373261
2465.075686	95.586908	58.378266
2464.652539	97.865777	58.383271
2464.203455	98.533082	58.388276
2463.602685	98.496478	58.393281
2463.466694	96.239032	58.398285
2462.253056	100.881664	58.403290
2461.832477	99.442587	58.408295
2461.151489	104.395586	58.413300
2460.901155	104.113151	58.418305
2459.584846	89.498981	58.423309
2458.313880	101.006186	58.428314
2458.231388	91.559570	58.433319
2457.736528	98.619751	58.438324
2457.364403	96.994369	58.443329
2456.722730	93.053837	58.448333
2455.292861	90.801305	58.453338
2454.956417	91.129625	58.458343
2454.033571	93.899312	58.463348
2453.564377	100.074082	58.468353
2453.571945	96.548317	58.473357
2452.462053	93.282688	58.478362
2451.768831	96.530993	58.483367
2451.419196	103.866731	58.488372
2450.844606	98.639376	58.493377
2449.640216	86.957032	58.498381
2448.395596	101.824356	58.503386
2447.999325	94.442901	58.508391
2447.621056	101.993527	58.513396
2447.147553	93.291900	58.518401
2446.618820	83.698964	58.523405
2446.180296	97.812298	58.528410
2445.680532	96.439259	58.533415
2444.631578	100.909664	58.538420
2444.140742	97.866206	58.543425
2442.693700	96.452243	58.548429
2441.794248	97.629169	58.553434
2441.563130	99.762316	58.558439
2441.242004	92.825895	58.563444
2440.210506	102.862076	58.568449
2440.212471	97.598116	58.573453
2439.479880	98.878746	58.578458
2439.073928	89.311392	58.583463
2437.750624	93.641210	58.588468
2437.051771	96.897583	58.593473
2436.747434	93.915395	58.598477
2436.268161	104.547531	58.603482
2435.313486	88.965254	58.608487
2434.138256	91.521919	58.613492
2433.578660	96.606525	58.618497
2433.564540	85.197108	58.623501
2433.033285	89.221376	58.628506
2431.678040	91.203315	58.633511
2430.690611	87.786495	58.638516
2429.900892	88.189160	58.643521
2429.757046	84.073125	58.648525
2429.050293	89.604059	58.653530
2428.831940	85.079198	58.658535
2428.677966	90.465884	58.663540
2427.555609	95.917491	58.668545
2426.657547	89.740485	58.673549
2425.709312	92.390178	58.678554
2425.502223	90.932759	58.683559
2425.124552	88.717033	58.688564
2423.721428	94.342563	58.693569
2422.962342	95.933635	58.698573
2422.495241	96.616655	58.703578
2421.932360	78.973655	58.708583
2421.775072	88.577733	58.713588
2420.422951	96.171713	58.718593
2419.706150	89.710698	58.723597
2418.977312	90.941742	58.728602
2418.811263	89.477307	58.733607
2418.133709	87.996517	58.738612
2417.804540	91.358624	58.743617
2416.903228	83.682229	58.748621
2416.075592	97.799331	58.753626
2415.588992	91.369216	58.758631
2415.032334	92.083338	58.763636
2414.132714	91.602854	58.768641
2413.521947	86.174860	58.773645
2412.578256	98.106092	58.778650
2412.282783	94.900161	58.783655
2411.766174	91.105616	58.788660
2410.206467	88.238213	58.793665
2409.803606	85.932063	58.798669
2408.900047	93.891042	58.803674
2408.975281	79.538691	58.808679
2408.385390	92.169267	58.813684
2407.820896	97.322604	58.818689
2407.429531	81.500743	58.823693
2406.029889	88.701413	58.828698
2405.752645	86.616540	58.833703
2405.271915	89.509577	58.838708
2404.449723	90.909738	58.843713
2403.381129	88.635710	58.848717
2402.467714	92.908081	58.853722
2402.243485	84.999870	58.858727
2401.963127	86.830393	58.863732
2400.781262	89.363332	58.868737
2399.511484	73.201035	58.873741
2398.652893	84.670881	58.878746
2398.316183	87.011944	58.883751
2397.874370	86.472131	58.888756
2397.624721	81.870127	58.893761
2397.470712	78.907635	58.898765
2396.935582	87.330965	58.903770
2396.155228	86.738121	58.908775
2394.966261	87.913243	58.913780
2394.067615	82.204488	58.918785
2393.988656	83.517434	58.923789
2392.459009	94.397053	58.928794
2391.717135	87.298512	58.933799
2391.009209	87.515098	58.938804
2390.438762	91.054640	58.943809
2390.368601	86.180375	58.948813
2389.896545	88.810229	58.953818
2389.869683	85.193254	58.958823
2389.123457	81.781779	58.963828
2387.778774	89.326333	58.968833
2387.344064	80.171265	58.973837
2385.873929	88.431193	58.978842
2385.111800	84.797445	58.983847
2384.775138	90.348388	58.988852
2384.422627	80.965326	58.993857
2384.213407	82.480538	58.998861
2383.454471	84.242109	59.003866
2382.463065	84.631900	59.008871
2381.432950	85.096597	59.013876
2380.982047	85.082927	59.018881
2380.644030	82.148345	59.023885
2380.133804	88.772613	59.028890
2379.153707	87.469477	59.033895
2378.087040	98.068233	59.038900
2377.472309	91.195445	59.043905
2377.464042	81.314194	59.048909
2376.411002	90.752893	59.053914
2375.494112	79.390487	59.058919
2374.906160	90.534597	59.063924
2374.448887	89.647310	59.068929
2373.971056	87.780283	59.073933
2373.481316	89.841998	59.078938
2372.623333	84.175635	59.083943
2371.978691	92.466910	59.088948
2370.929815	86.392281	59.093953
2370.545110	82.179282	59.098957
2370.008206	85.290340	59.103962
2369.431426	84.238364	59.108967
2368.669446	88.754044	59.113972
2368.006008	86.438772	59.118977
2367.600551	75.705343	59.123981
2366.013025	88.110989	59.128986
2365.533227	83.253089	59.133991
2364.914332	81.776487	59.138996
2363.703423	91.989787	59.144001
2363.750494	86.534972	59.149005
2363.115880	88.601329	59.154010
2363.037477	86.657320	59.159015
2362.605743	85.898689	59.164020
2361.009049	81.590574	59.169025
2360.325415	85.412751	59.174029
2359.923129	95.862772	59.179034
2359.787850	87.446741	59.184039
2358.784028	83.143430	59.189044
2357.693875	90.880905	59.194049
2357.253598	83.126876	59.199053
2356.433793	90.955882	59.204058
2355.866740	91.129437	59.209063
2355.518284	84.934652	59.214068
2354.824379	83.255359	59.219073
2354.003850	81.651006	59.224077
2353.238239	80.240150	59.229082
2352.706931	78.515687	59.234087
2352.690135	81.884377	59.239092
2351.209685	92.059298	59.244097
2351.007633	80.170863	59.249101
2350.368789	85.465593	59.254106
2349.081240	81.974983	59.259111
2348.238172	86.327695	59.264116
2347.469400	90.389819	59.269121
2347.317011	82.439333	59.274125
2346.479700	92.518886	59.279130
2346.507378	89.347307	59.284135
2345.995768	80.519596	59.289140
2344.825517	89.340467	59.294145
2344.116152	83.724879	59.299149
2343.375379	82.707658	59.304154
2342.913633	87.737640	59.309159
2341.817650	80.271389	59.314164
2340.944693	87.287671	59.319169
2340.459184	81.443550	59.324173
2340.007450	89.648549	59.329178
2339.684516	81.656966	59.334183
2339.462713	85.599114	59.339188
2337.907758	87.294708	59.344193
2337.495586	82.454063	59.349197
2336.678793	87.632386	59.354202
2336.262348	81.969080	59.359207
2335.838741	80.343435	59.364212
2334.791620	86.838071	59.369217
2334.114695	81.611267	59.374221
2333.414899	86.217366	59.379226
2332.585049	81.840498	59.384231
2332.569407	81.678196	59.389236
2331.616267	83.055759	59.394241
2330.767831	79.918737	59.399245
2329.623744	82.982840	59.404250
2329.541733	85.553500	59.409255
2329.286300	93.095351	59.414260
2328.546727	88.237272	59.419265
2327.710624	78.603768	59.424269
2326.958663	85.710672	59.429274
2326.049695	81.524960	59.434279
2325.754232	77.695771	59.439284
2325.151327	83.823141	59.444289
2324.705364	84.798201	59.449293
2323.490019	87.352667	59.454298
2323.002074	79.264967	59.459303
2322.598873	80.996503	59.464308
2321.364691	90.374211	59.469313
2320.568700	74.357499	59.474317
2319.775273	86.257111	59.479322
2319.097320	87.210659	59.484327
2318.985870	87.022899	59.489332
2318.328555	83.964509	59.494337
2318.252461	78.388659	59.499341
2317.155004	82.130029	59.504346
2316.298708	84.187720	59.509351
2315.709921	79.837132	59.514356
2315.313718	78.288511	59.519361
2314.638723	76.082589	59.524365
2313.323832	77.399650	59.529370
2312.710790	74.448556	59.534375
2312.364866	77.839579	59.539380
2311.656987	83.620176	59.544385
2311.407828	82.990587	59.549389
2310.397437	94.217594	59.554394
2309.049310	89.483713	59.559399
2308.971038	87.376269	59.564404
2308.306176	96.291903	59.569409
2308.135910	82.870066	59.574413
2307.391642	88.819909	59.579418
2306.144723	97.528773	59.584423
2305.670504	85.907138	59.589428
2305.429809	89.496083	59.594433
2304.931516	80.936092	59.599437
2303.759459	78.922535	59.604442
2302.794173	89.024366	59.609447
2302.679694	83.059173	59.614452
2301.724303	95.859220	59.619457
2301.584060	82.376200	59.624461
2300.428757	91.344121	59.629466
2299.372723	79.842511	59.634471
2299.363471	82.979786	59.639476
2298.815903	89.897800	59.644481
2298.087686	78.879718	59.649485
2297.308376	87.698476	59.654490
2296.776700	95.038891	59.659495
2296.115729	88.390334	59.664500
2295.632342	95.401187	59.669505
2294.395759	82.402084	59.674509
2293.304779	87.567695	59.679514
2292.698954	89.350855	59.684519
2292.598528	87.730341	59.689524
2291.880946	90.481131	59.694529
2291.557112	81.707764	59.699533
2290.625334	90.928767	59.704538
2289.917700	88.836188	59.709543
2289.298061	78.316628	59.714548
2288.685677	83.407501	59.719553
2288.335217	86.924034	59.724557
2286.970727	82.078885	59.729562
2285.985927	81.408128	59.734567
2285.779543	75.867983	59.739572
2285.118247	84.936155	59.744577
2285.099182	71.799911	59.749581
2284.356843	77.556403	59.754586
2283.456693	78.079416	59.759591
2282.639528	75.491641	59.764596
2281.938657	78.281809	59.769601
2281.722980	74.908306	59.774605
2280.401429	83.578220	59.779610
2279.351889	82.517102	59.784615
2279.217025	80.699590	59.789620
2278.425814	84.552407	59.794625
2278.429119	78.233930	59.799629
2277.949379	83.921834	59.804634
2276.613190	84.886507	59.809639
2276.023700	80.408155	59.814644
2275.354879	85.277373	59.819649
2274.935623	78.319078	59.824653
2274.451920	80.132275	59.829658
2273.344417	82.770542	59.834663
2273.117908	77.172262	59.839668
2272.187892	80.290948	59.844673
2271.788203	74.349272	59.849677
2270.546405	84.246556	59.854682
2270.149412	85.984138	59.859687
2269.325370	73.225151	59.864692
2268.904021	79.514493	59.869697
2268.362629	70.232833	59.874701
2267.234490	79.782269	59.879706
2265.945059	78.860464	59.884711
2265.944119	76.864925	59.889716
2265.084814	88.045963	59.894721
2264.833257	76.464422	59.899725
2264.777084	83.796540	59.904730
2263.574703	80.908736	59.909735
2262.988752	82.401142	59.914740
2261.911089	89.068373	59.919745
2261.759000	78.093878	59.924750
2260.858181	81.332305	59.929754
2260.097581	82.383674	59.934759
2259.337068	76.901584	59.939764
2258.788723	73.816281	59.944769
2258.200750	70.610654	59.949774
2257.983808	73.492533	59.954778
2257.622647	85.524268	59.959783
2256.351829	79.607227	59.964788
2255.524735	73.671148	59.969793
2254.901028	74.838049	59.974798
2253.893026	79.894739	59.979802
2253.225610	78.292640	59.984807
2252.732373	72.660638	59.989812
2251.853012	85.371890	59.994817
2251.605797	67.805229	59.999822
2250.978002	70.725001	60.004826
2250.953884	70.766246	60.009831
2249.745066	73.467235	60.014836
2248.343483	82.514378	60.019841
2248.049756	75.507780	60.024846
2247.837619	81.828844	60.029850
2247.150495	83.929847	60.034855
2246.971304	82.010185	60.039860
2245.718446	83.854660	60.044865
2245.016400	76.873287	60.049870
2244.613874	79.372051	60.054874
2243.993276	85.611789	60.059879
2243.442584	75.286102	60.064884
2242.492582	86.041745	60.069889
2242.017146	82.831478	60.074894
2240.438776	79.775487	60.079898
2239.746571	83.290861	60.084903
2239.480355	82.540250	60.089908
2238.747869	91.391267	60.094913
2238.507937	83.492473	60.099918
2238.323936	81.251935	60.104922
2237.270976	91.157194	60.109927
2236.325461	80.810608	60.114932
2235.293162	89.994334	60.119937
2235.217538	84.730633	60.124942
2234.883982	88.647289	60.129946
2233.920350	83.632949	60.134951
2233.097433	83.110564	60.139956
2232.306668	85.605464	60.144961
2232.008180	80.662105	60.149966
2231.739399	83.895075	60.154970
2230.463630	92.228368	60.159975
2229.807157	83.088358	60.164980
2229.127909	92.730374	60.169985
2228.635780	87.703686	60.174990
2227.101423	82.422227	60.179994
2226.893036	87.555326	60.184999
2226.495043	77.973630	60.190004
2225.311880	91.167089	60.195009
2224.987122	84.211191	60.200014
2224.387365	85.805037	60.205018
2223.912678	88.014182	60.210023
2223.834224	81.208787	60.215028
2222.899792	92.355706	60.220033
2221.939446	79.780294	60.225038
2221.524167	81.326802	60.230042
2220.375517	87.429883	60.235047
2219.863397	78.353609	60.240052
2218.758141	83.661403	60.245057
2218.454517	79.236010	60.250062
2218.121842	79.592120	60.255066
2217.425173	84.157036	60.260071
2217.573238	85.660096	60.265076
2215.739459	84.902052	60.270081
2215.316002	80.943979	60.275086
2215.082173	79.571669	60.280090
2213.595974	84.501733	60.285095
2212.620823	79.999350	60.290100
2211.840588	89.043263	60.295105
2212.141271	82.720903	60.300110
2211.862433	86.640832	60.305114
2210.901947	81.497281	60.310119
2210.654227	83.912338	60.315124
2208.580017	84.940481	60.320129
2208.351468	76.390825	60.325134
2207.923671	78.951542	60.330138
2207.487034	73.832085	60.335143
2207.514867	69.909332	60.340148
2206.235241	85.224731	60.345153
2205.698546	85.067464	60.350158
2205.341595	75.952026	60.355162
2203.802730	80.540585	60.360167
2203.231384	78.179985	60.365172
2202.377100	76.827342	60.370177
2201.860946	79.368830	60.375182
2201.479420	79.207920	60.380186
2200.878303	79.812038	60.385191
2200.163347	77.160221	60.390196
2198.784656	82.471755	60.395201
2198.248156	74.594481	60.400206
2197.932870	70.299373	60.405210
2197.490420	69.076818	60.410215
2197.243640	67.257137	60.415220
2196.549746	78.999596	60.420225
2195.892435	69.039118	60.425230
2195.092503	72.605679	60.430234
2194.128970	82.745107	60.435239
2193.649810	73.526236	60.440244
2192.125567	74.262178	60.445249
2191.875281	66.497402	60.450254
2191.453688	69.036926	60.455258
2190.956259	73.405142	60.460263
2190.663784	72.988223	60.465268
2189.632289	80.921726	60.470273
2188.553036	73.276220	60.475278
2187.954482	73.302422	60.480282
2187.405309	86.295088	60.485287
2187.213491	77.169173	60.490292
2186.785723	77.811932	60.495297
2185.483050	76.056786	60.500302
2184.606680	79.839704	60.505306
2184.392183	78.493694	60.510311
2183.974809	77.746438	60.515316
2182.536969	74.778535	60.520321
2182.109452	72.626226	60.525326
2181.189384	85.093397	60.530330
2180.582473	84.441318	60.535335
2180.411251	71.516238	60.540340
2180.077660	90.787192	60.545345
2179.227056	80.775298	60.550350
2178.423874	78.430668	60.555354
2177.431724	79.129689	60.560359
2177.295198	77.831132	60.565364
2176.363448	81.367743	60.570369
2175.246078	71.695548	60.575374
2174.863497	77.023033	60.580378
2173.976823	82.064510	60.585383
2173.884015	69.969937	60.590388
2173.508587	79.053162	60.595393
2172.413890	73.389438	60.600398
2171.365891	72.356895	60.605402
2170.355237	80.398541	60.610407
2170.771371	76.469770	60.615412
2169.840232	77.913067	60.620417
2169.585584	75.101612	60.625422
2168.670861	67.322980	60.630426
2167.646727	77.088707	60.635431
2167.475011	67.686610	60.640436
2166.216027	74.256178	60.645441
2165.449745	68.522869	60.650446
2164.666029	75.837307	60.655450
2164.076778	76.630839	60.660455
2163.886328	74.871391	60.665460
2163.254914	80.388666	60.670465
2163.156616	76.377357	60.675470
2162.041238	71.098870	60.680474
2161.039355	83.514510	60.685479
2160.727281	72.744626	60.690484
2160.066005	82.515795	60.695489
2158.263220	77.213563	60.700494
2158.042453	68.637719	60.705498
2157.306953	71.100675	60.710503
2157.102728	66.719474	60.715508
2156.385454	63.129415	60.720513
2156.470935	70.886091	60.725518
2155.692050	67.289200	60.730522
2154.848726	74.131878	60.735527
2154.164724	73.792975	60.740532
2153.348893	81.048569	60.745537
2152.419012	84.443160	60.750542
2151.874155	71.518437	60.755546
2150.802668	68.643802	60.760551
2150.706333	69.447764	60.765556
2150.068519	74.599437	60.770561
2149.411146	73.487063	60.775566
2148.391620	79.184003	60.780570
2147.581125	70.775334	60.785575
2147.119180	67.744346	60.790580
2146.777240	80.624591	60.795585
2146.361401	69.005256	60.800590
2145.537959	78.687320	60.805594
2144.166909	81.448050	60.810599
2143.916993	83.269427	60.815604
2143.730284	84.866055	60.820609
2142.454423	79.319766	60.825614
2141.699587	72.679406	60.830618
2140.579274	85.604364	60.835623
2140.785470	75.762644	60.840628
2139.989889	83.055433	60.845633
2139.188532	76.981165	60.850638
2139.040581	73.831739	60.855642
2138.020473	76.036676	60.860647
2137.373396	69.437097	60.865652
2137.031021	76.762891	60.870657
2136.240077	77.296065	60.875662
2135.353357	83.977624	60.880666
2134.299211	77.982906	60.885671
2134.045267	69.882459	60.890676
2133.597269	69.918837	60.895681
2133.134878	82.039318	60.900686
2132.545013	75.404295	60.905690
2131.218409	79.761180	60.910695
2131.184353	74.868130	60.915700
2130.289775	73.961322	60.920705
2128.890958	79.498540	60.925710
2128.545640	71.371879	60.930714
2127.706130	85.258114	60.935719
2127.317847	78.463091	60.940724
2126.792048	79.719046	60.945729
2126.401170	82.775145	60.950734
2126.149919	78.470668	60.955738
2124.899858	77.850048	60.960743
2124.370406	71.201537	60.965748
2123.508935	81.358643	60.970753
2122.091611	73.767426	60.975758
2121.993898	73.035763	60.980762
2120.991746	83.502710	60.985767
2120.990323	74.625284	60.990772
2120.294334	76.590453	60.995777
2119.784721	81.387846	61.000782
2118.977906	76.422895	61.005786
2118.028823	81.697281	61.010791
2117.676896	75.351156	61.015796
2117.149856	79.339193	61.020801
2116.393510	78.866622	61.025806
2115.764980	78.794542	61.030810
2114.844737	84.718840	61.035815
2114.282929	77.305365	61.040820
2114.048704	85.554472	61.045825
2112.629072	76.869087	61.050830
2111.902939	73.914077	61.055834
2111.358659	78.930154	61.060839
2111.069297	74.387471	61.065844
2110.310899	76.737117	61.070849
2109.679515	76.886965	61.075854
2108.625040	71.770174	61.080858
2107.862971	83.504956	61.085863
2107.393415	78.948094	61.090868
2107.058171	74.738904	61.095873
2106.897084	78.324888	61.100878
2106.351579	77.521005	61.105882
2104.895164	77.581843	61.110887
2104.541136	76.562849	61.115892
2103.990330	78.940934	61.120897
2102.935702	80.990736	61.125902
2102.072603	71.237180	61.130906
2101.172018	71.459125	61.135911
2100.876608	71.405067	61.140916
2100.695095	76.535537	61.145921
2100.126858	77.227196	61.150926
2098.951769	75.159735	61.155930
2098.143367	76.054307	61.160935
2097.815859	64.201991	61.165940
2097.323837	72.981086	61.170945
2096.608461	80.390416	61.175950
2095.681555	73.783838	61.180954
2094.726080	81.304890	61.185959
2094.027397	78.423736	61.190964
2093.893373	83.636477	61.195969
2093.438155	75.797423	61.200974
2092.315027	75.512323	61.205978
2091.048627	75.277385	61.210983
2090.760194	71.886343	61.215988
2090.264073	75.480291	61.220993
2089.870178	75.767540	61.225998
2089.636350	74.142222	61.231002
2088.812328	76.079953	61.236007
2088.250910	76.863206	61.241012
2087.442733	78.945853	61.246017
2086.562027	87.228959	61.251022
2085.646296	75.674213	61.256026
2084.677281	84.991988	61.261031
2084.079069	75.111816	61.266036
2083.697852	79.540289	61.271041
2083.298370	83.534141	61.276046
2083.140619	75.127518	61.281050
2081.778495	78.090411	61.286055
2081.354442	79.703558	61.291060
2080.710899	89.430253	61.296065
2080.057900	85.945651	61.301070
2079.309604	72.285640	61.306074
2078.170009	80.553027	61.311079
2077.792751	75.193308	61.316084
2077.024789	74.250248	61.321089
2076.343957	74.072650	61.326094
2076.252904	68.875156	61.331098
2075.553008	75.631731	61.336103
2074.474347	74.156048	61.341108
2073.969640	75.107622	61.346113
2073.768699	82.415148	61.351118
2073.291897	70.575736	61.356122
2071.746623	84.714524	61.361127
2071.278930	75.770808	61.366132
2070.631486	78.337524	61.371137
2069.880351	80.781455	61.376142
2068.852631	74.023582	61.381146
2068.290519	84.695914	61.386151
2067.893576	77.681732	61.391156
2067.284302	82.780374	61.396161
2066.936712	73.410738	61.401166
2066.603903	72.184441	61.406170
2065.411246	83.847222	61.411175
2064.719828	80.249989	61.416180
2064.051324	78.308247	61.421185
2063.215879	85.166956	61.426190
2062.944298	77.773319	61.431194
2061.707182	85.875030	61.436199
2060.955133	79.147369	61.441204
2061.102298	91.306086	61.446209
2060.504281	75.169151	61.451214
2059.523615	78.439419	61.456218
2058.166532	79.124701	61.461223
2057.657656	86.216489	61.466228
2057.147854	82.563719	61.471233
2056.869017	85.934591	61.476238
2056.493761	83.276400	61.481242
2055.859845	83.080122	61.486247
2055.270898	75.341709	61.491252
2054.447404	82.295080	61.496257
2053.884742	78.961209	61.501262
2052.732326	73.514619	61.506266
2051.820606	84.725548	61.511271
2051.420345	79.713173	61.516276
2050.995835	80.663663	61.521281
2050.172993	79.854331	61.526286
2049.585211	80.420264	61.531290
2048.202468	75.220695	61.536295
2048.315447	74.443917	61.541300
2047.918436	71.160264	61.546305
2046.972542	79.432414	61.551310
2046.109527	67.836302	61.556314
2044.991175	76.049927	61.561319
2044.780438	81.558408	61.566324
2044.215596	77.765456	61.571329
2043.656308	73.416577	61.576334
2043.203442	75.646077	61.581338
2041.989310	79.491129	61.586343
2041.463822	74.074669	61.591348
2040.969923	80.409580	61.596353
2040.032862	82.154688	61.601358
2040.198180	71.885382	61.606362
2039.152406	82.035730	61.611367
2037.761129	79.514623	61.616372
2037.272518	80.606731	61.621377
2036.902112	80.946017	61.626382
2036.419949	68.950827	61.631386
2035.995550	81.203747	61.636391
2035.104488	76.381903	61.641396
2034.153865	75.069057	61.646401
2033.612649	77.724181	61.651406
2033.143626	73.045271	61.656410
2032.263463	75.541275	61.661415
2031.423292	69.283022	61.666420
2030.639676	67.238218	61.671425
2030.288002	79.547378	61.676430
2030.030276	78.366265	61.681434
2029.128165	75.425975	61.686439
2028.583155	76.074985	61.691444
2028.191714	82.557760	61.696449
2027.353585	77.767124	61.701454
2026.524983	80.981782	61.706458
2025.608535	76.870439	61.711463
2024.808266	75.717790	61.716468
2024.104676	70.460872	61.721473
2023.794929	72.471294	61.726478
2023.580622	69.981359	61.731482
2022.391050	74.544158	61.736487
2021.570818	70.618061	61.741492
2020.941056	68.436025	61.746497
2020.285362	78.013220	61.751502
2020.288062	74.152796	61.756506
2019.393388	83.419571	61.761511
2018.399072	67.850162	61.766516
2018.172192	70.246656	61.771521
2017.189972	75.312781	61.776526
2016.462916	70.102114	61.781530
2015.297180	78.866591	61.786535
2015.204270	76.448649	61.791540
2014.786851	68.399471	61.796545
2014.268893	81.005090	61.801550
2013.556065	76.928785	61.806554
2012.421328	72.117051	61.811559
2011.706289	73.020138	61.816564
2011.034998	78.015711	61.821569
2010.537652	76.007990	61.826574
2009.651338	71.463225	61.831578
2008.512640	72.769953	61.836583
2007.892222	70.019500	61.841588
2007.816729	76.445069	61.846593
2007.539034	72.202759	61.851598
2006.908493	67.060450	61.856602
2006.783930	73.658616	61.861607
2005.410275	63.019833	61.866612
2004.743814	68.990721	61.871617
2004.040830	67.546315	61.876622
2003.015157	62.846978	61.881626
2001.946766	72.027021	61.886631
2001.236597	74.924196	61.891636
2001.144328	71.383954	61.896641
2000.465002	76.626418	61.901646
2000.166875	65.299204	61.906650
2000.083485	71.143119	61.911655
1999.055102	68.153388	61.916660
1998.478297	64.555511	61.921665
1997.627521	68.683004	61.926670
1996.674013	68.627452	61.931674
1995.347343	73.879206	61.936679
1994.650557	68.278907	61.941684
1994.650930	77.579277	61.946689
1993.921618	79.400167	61.951694
1994.030684	72.357465	61.956698
1992.981743	72.712169	61.961703
1991.951943	87.880644	61.966708
1991.291736	81.288860	61.971713
1990.443627	92.193269	61.976718
1990.513910	83.342662	61.981722
1989.886642	80.861003	61.986727
1988.441551	85.043588	61.991732
1987.903482	77.217935	61.996737
1986.990264	84.368232	62.001742
1987.238804	81.619919	62.006746
1986.263771	77.578604	62.011751
1985.573252	80.751488	62.016756
1984.613223	79.494733	62.021761
1984.038918	78.897492	62.026766
1983.837366	71.482022	62.031770
1982.570479	81.346526	62.036775
1981.954586	79.805912	62.041780
1981.577026	73.659184	62.046785
1980.923487	75.076733	62.051790
1980.703263	70.534475	62.056794
1979.294808	84.575269	62.061799
1978.708804	75.737463	62.066804
1977.970720	76.046099	62.071809
1977.179158	81.034619	62.076814
1976.932884	70.223120	62.081818
1976.685858	79.820010	62.086823
1975.715608	77.359132	62.091828
1975.326739	71.121186	62.096833
1974.204399	81.394764	62.101838
1973.336494	77.474857	62.106842
1972.704001	78.785785	62.111847
1972.026185	71.207455	62.116852
1971.653306	74.839535	62.121857
1970.895996	75.982349	62.126862
1970.590136	69.077336	62.131866
1969.762548	85.868257	62.136871
1968.667089	76.190008	62.141876
1968.460861	73.050957	62.146881
1967.785901	82.543428	62.151886
1967.051608	74.339258	62.156890
1966.124852	76.165506	62.161895
1965.866881	74.677741	62.166900
1965.436539	75.770149	62.171905
1964.571973	81.587441	62.176910
1963.676864	71.186135	62.181914
1962.768625	80.279976	62.186919
1962.323045	80.749358	62.191924
1961.684409	83.408128	62.196929
1960.474302	80.573826	62.201934
1959.751966	71.702114	62.206938
1959.320849	85.486120	62.211943
1959.017496	79.182231	62.216948
1958.627554	76.727475	62.221953
1958.178739	85.757333	62.226958
1957.340087	76.404615	62.231962
1956.186827	76.856511	62.236967
1955.467616	72.100416	62.241972
1955.232628	74.672766	62.246977
1954.821863	74.392538	62.251982
1953.969393	68.837432	62.256986
1952.855062	73.645123	62.261991
1951.946354	73.085751	62.266996
1952.005791	66.075227	62.272001
1951.191489	79.697419	62.277006
1950.997725	71.304870	62.282010
1949.429357	77.822799	62.287015
1949.113262	76.359583	62.292020
1948.789797	71.168304	62.297025
1947.631953	79.698949	62.302030
1946.678621	71.988948	62.307034
1945.807988	81.056227	62.312039
1945.302329	73.530158	62.317044
1945.173157	68.308012	62.322049
1944.573876	77.483600	62.327054
1944.328319	70.102898	62.332058
1943.926817	76.386874	62.337063
1942.903575	77.812017	62.342068
1942.509647	74.890596	62.347073
1940.463105	69.051096	62.352078
1939.818257	77.267413	62.357082
1939.309710	72.198584	62.362087
1939.082042	70.348809	62.367092
1938.576007	69.409119	62.372097
1937.694478	79.500193	62.377102
1937.645594	70.176188	62.382106
1937.087240	78.655593	62.387111
1935.880913	89.680491	62.392116
1935.436514	87.404388	62.397121
1934.856318	88.351126	62.402126
1934.070819	75.928654	62.407130
1933.029568	79.465478	62.412135
1932.146166	81.909553	62.417140
1931.821363	73.206278	62.422145
1931.165058	71.871129	62.427150
1931.133587	67.250008	62.432154
1929.987524	77.276998	62.437159
1928.960426	76.565390	62.442164
1928.460319	76.319396	62.447169
1928.023527	77.032793	62.452174
1928.050160	69.288175	62.457178
1926.986705	73.007211	62.462183
1925.954510	76.723664	62.467188
1925.438623	71.663197	62.472193
1924.589680	80.635191	62.477198
1924.079529	66.241361	62.482202
1923.474414	74.563375	62.487207
1922.900907	77.168770	62.492212
1922.419328	72.265849	62.497217
1921.160809	87.234647	62.502222
1920.309278	75.956719	62.507226
1919.666518	75.932490	62.512231
1919.117601	83.873068	62.517236
1918.735788	73.598690	62.522241
1918.360234	80.230319	62.527246
1918.051082	77.472811	62.532250
1916.607440	79.971285	62.537255
1916.043417	83.535810	62.542260
1915.731610	80.112467	62.547265
1914.569723	83.664012	62.552270
1914.035207	74.095073	62.557274
1913.155333	79.019367	62.562279
1912.400579	77.780795	62.567284
1912.429163	71.851954	62.572289
1911.821430	77.720439	62.577294
1911.498556	76.670079	62.582298
1910.074523	71.631165	62.587303
1909.217997	77.547345	62.592308
1909.041181	72.842541	62.597313
1908.089111	87.394587	62.602318
1907.193479	71.802411	62.607322
1906.487491	71.415595	62.612327
1905.698740	81.016740	62.617332
1905.936560	64.160578	62.622337
1905.331745	84.174959	62.627342
1904.619791	76.569719	62.632346
1903.721486	76.950774	62.637351
1903.079113	82.173899	62.642356
1902.687925	75.876361	62.647361
1901.665641	78.617346	62.652366
1900.800400	77.077954	62.657370
1900.202057	79.946537	62.662375
1899.479498	76.784511	62.667380
1899.010560	72.810182	62.672385
1897.980719	78.777329	62.677390
1897.506692	73.779570	62.682394
1897.540945	82.647443	62.687399
1896.223317	74.932674	62.692404
1895.148159	79.336586	62.697409
1894.225670	81.952742	62.702414
1894.264910	73.065619	62.707418
1893.284219	78.168208	62.712423
1893.014573	77.527936	62.717428
1892.797127	73.060996	62.722433
1892.281878	78.179875	62.727438
1891.259873	77.832520	62.732442
1890.504955	73.253459	62.737447
1889.692172	74.209598	62.742452
1888.857346	69.238436	62.747457
1887.686241	75.515923	62.752462
1887.646342	72.588807	62.757466
1886.786516	67.880466	62.762471
1886.766153	72.255890	62.767476
1886.007734	68.153464	62.772481
1884.567306	73.601141	62.777486
1884.048490	71.938542	62.782490
1883.964464	72.749875	62.787495
1882.891552	84.053122	62.792500
1882.865373	73.532390	62.797505
1882.414057	79.905018	62.802510
1880.922249	68.236535	62.807514
1880.264596	77.469476	62.812519
1879.602757	82.204900	62.817524
1879.481836	68.273416	62.822529
1878.259189	79.092693	62.827534
1877.402685	72.733061	62.832538
1876.725158	76.976189	62.837543
1876.396921	74.513254	62.842548
1876.288412	74.957344	62.847553
1875.273477	74.550758	62.852558
1874.408213	70.236490	62.857562
1873.745970	70.436249	62.862567
1873.213730	71.759245	62.867572
1873.025441	72.432106	62.872577
1871.458200	77.824117	62.877582
1870.982249	74.386627	62.882586
1870.498736	79.091543	62.887591
1870.073895	80.433664	62.892596
1869.521135	69.814744	62.897601
1868.862862	78.508604	62.902606
1867.944681	68.157851	62.907610
1867.363063	78.209855	62.912615
1866.683742	75.192011	62.917620
1865.726049	61.526846	62.922625
1864.638381	83.693348	62.927630
1864.243397	77.525144	62.932634
1863.427509	73.891217	62.937639
1862.995023	82.389747	62.942644
1862.967905	72.164431	62.947649
1862.712849	76.510142	62.952654
1861.744249	70.419946	62.957658
1861.511147	72.251874	62.962663
1859.834968	83.039015	62.967668
1859.489974	75.585733	62.972673
1858.491039	87.001454	62.977678
1857.801548	78.564651	62.982682
1857.400123	75.865960	62.987687
1856.477704	79.709295	62.992692
1855.877348	74.917094	62.997697
1854.724247	78.096109	63.002702
1854.307346	83.968660	63.007706
1853.924373	80.267379	63.012711
1853.435575	84.468748	63.017716
1853.145439	69.730988	63.022721
1852.071754	69.930881	63.027726
1850.996029	78.327493	63.032730
1850.463656	66.195680	63.037735
1849.769967	86.335785	63.042740
1849.920293	82.113018	63.047745
1849.033584	79.804445	63.052750
1847.727436	81.672332	63.057754
1847.351391	77.204109	63.062759
1846.883966	80.198713	63.067764
1846.612454	69.945347	63.072769
1845.295829	80.754655	63.077774
1844.243395	83.209900	63.082778
1844.132943	78.699000	63.087783
1843.610123	74.210103	63.092788
1843.145070	70.308140	63.097793
1842.019361	74.255332	63.102798
1841.274963	77.176932	63.107802
1841.281752	76.587259	63.112807
1840.065260	81.854537	63.117812
1840.047520	70.288332	63.122817
1838.813815	77.376635	63.127822
1838.206827	73.819074	63.132826
1837.871651	76.308703	63.137831
1836.483445	72.366927	63.142836
1836.176449	70.958607	63.147841
1835.254917	74.708243	63.152846
1834.217255	74.607910	63.157850
1833.942744	72.285781	63.162855
1833.687329	71.853859	63.167860
1833.830397	72.623576	63.172865
1832.140700	73.278982	63.177870
1831.245599	72.245613	63.182874
1830.972006	71.167091	63.187879
1830.327804	77.029584	63.192884
1829.205574	71.697098	63.197889
1828.356670	77.140290	63.202894
1827.587178	75.449536	63.207898
1827.306983	67.555720	63.212903
1827.036327	76.679425	63.217908
1826.965267	71.881143	63.222913
1826.356321	71.633255	63.227918
1825.531786	73.462955	63.232922
1824.711427	76.334793	63.237927
1823.195665	84.390663	63.242932
1822.556792	73.077171	63.247937
1821.850851	78.765894	63.252942
1821.316728	76.288849	63.257946
1820.835879	66.269455	63.262951
1820.367932	74.158678	63.267956
1820.276682	72.611610	63.272961
1819.479419	71.870569	63.277966
1818.485784	77.923895	63.282970
1818.014450	74.692850	63.287975
1816.726163	83.115968	63.292980
1816.496708	74.613098	63.297985
1815.334459	74.667895	63.302990
1815.091612	68.500907	63.307994
1814.865170	79.988134	63.312999
1813.976104	81.543495	63.318004
1813.035902	71.599138	63.323009
1811.983060	80.731547	63.328014
1811.775549	75.068489	63.333018
1811.583423	78.331769	63.338023
1810.248675	75.190425	63.343028
1809.547959	69.512680	63.348033
1808.814012	69.091189	63.353038
1808.620148	77.136801	63.358042
1808.273942	74.173283	63.363047
1807.144850	78.709984	63.368052
1806.312870	73.182586	63.373057
1805.867468	77.221405	63.378062
1805.335608	72.276185	63.383066
1804.712575	69.089649	63.388071
1803.694329	76.715016	63.393076
1803.154537	72.470992	63.398081
1802.370467	82.106077	63.403086
1801.992937	73.637229	63.408090
1801.281233	71.227280	63.413095
1799.902097	84.976906	63.418100
1799.538680	75.112675	63.423105
1799.047925	76.507918	63.428110
1798.547426	73.982889	63.433114
1798.200359	77.691082	63.438119
1797.507559	72.666824	63.443124
1796.481098	70.392042	63.448129
1795.610829	73.892923	63.453134
1795.434984	75.565457	63.458138
1794.993100	72.290693	63.463143
1793.954208	75.647143	63.468148
1793.153827	70.176314	63.473153
1792.480049	81.656397	63.478158
1792.051996	70.095669	63.483162
1791.629069	74.954424	63.488167
1789.923245	75.387218	63.493172
1789.727727	78.080707	63.498177
1789.219160	82.479663	63.503182
1788.865079	81.796610	63.508186
1788.439836	73.675782	63.513191
1787.202011	79.350911	63.518196
1786.401553	73.191308	63.523201
1785.707803	77.436824	63.528206
1785.534126	71.108404	63.533210
1785.182109	79.157787	63.538215
1784.054204	81.743976	63.543220
1783.472447	77.758176	63.548225
1782.551547	76.291484	63.553230
1782.203271	76.173862	63.558234
1781.043349	76.423259	63.563239
1780.149802	78.985929	63.568244
1779.815567	71.715153	63.573249
1779.074329	78.918539	63.578254
1778.951277	74.672290	63.583258
1778.701313	69.290437	63.588263
1777.570586	75.523533	63.593268
1776.715317	72.282794	63.598273
1776.069068	70.123744	63.603278
1775.578345	67.439158	63.608282
1774.663714	60.173356	63.613287
1773.794405	66.295803	63.618292
1773.098765	70.160342	63.623297
1772.692365	72.365724	63.628302
1772.291202	76.300664	63.633306
1771.985691	68.071727	63.638311
1770.441558	73.377706	63.643316
1770.142789	63.307829	63.648321
1769.810969	75.575282	63.653326
1769.166344	80.698937	63.658330
1768.121091	72.236190	63.663335
1767.180509	79.475264	63.668340
1766.944121	70.209411	63.673345
1766.789757	74.031073	63.678350
1765.535010	73.253059	63.683354
1764.697441	68.227528	63.688359
1763.842371	81.636839	63.693364
1763.503208	68.896089	63.698369
1762.604887	72.956749	63.703374
1762.132144	74.259312	63.708378
1761.860315	71.552668	63.713383
1760.624061	74.102928	63.718388
1760.140662	74.657346	63.723393
1759.311276	73.605246	63.728398
1758.916582	81.733376	63.733402
1758.658981	68.677500	63.738407
1757.533218	75.821947	63.743412
1756.556865	74.180415	63.748417
1756.088053	69.914781	63.753422
1755.777998	69.946534	63.758426
1755.343849	72.198506	63.763431
1753.973585	82.843329	63.768436
1753.700911	75.166907	63.773441
1752.965970	79.415527	63.778446
1752.649313	78.661339	63.783450
1751.874436	74.120061	63.788455
1750.739208	78.280468	63.793460
1749.715840	78.987671	63.798465
1749.562771	77.109355	63.803470
1749.071428	77.815522	63.808474
1748.978903	73.238013	63.813479
1747.434908	84.566616	63.818484
1746.940367	67.685395	63.823489
1746.365541	75.411336	63.828494
1745.782412	74.452885	63.833498
1745.195516	67.357580	63.838503
1744.083264	80.474594	63.843508
1743.424254	75.626530	63.848513
1743.065075	72.004084	63.853518
1742.776203	74.580920	63.858522
1742.286606	68.423794	63.863527
1740.829846	68.997927	63.868532
1740.506962	68.572028	63.873537
1739.865383	77.602494	63.878542
1738.868136	73.068480	63.883546
1737.886301	64.195044	63.888551
1737.221680	68.730434	63.893556
1736.896924	72.402837	63.898561
1736.447314	69.967393	63.903566
1736.263495	77.782740	63.908570
1735.927373	69.610360	63.913575
1734.417335	77.036475	63.918580
1733.544469	78.156858	63.923585
1733.252266	72.543431	63.928590
1732.674738	72.903967	63.933594
1732.202046	67.169854	63.938599
1731.026852	72.109173	63.943604
1730.332024	65.644550	63.948609
1729.652472	65.837025	63.953614
1728.841278	74.905591	63.958618
1729.106174	70.470602	63.963623
1727.633575	73.650627	63.968628
1727.163443	66.280357	63.973633
1726.851653	70.185399	63.978638
1725.794395	70.894853	63.983642
1724.991154	67.048406	63.988647
1723.944137	75.179998	63.993652
1723.511003	70.427494	63.998657
1722.975853	71.270233	64.003662
1722.284877	72.922759	64.008666
1722.495985	63.051422	64.013671
1721.851556	62.747646	64.018676
1720.898432	63.428230	64.023681
1719.821145	65.711307	64.028686
1719.257280	68.234149	64.033690
1719.143099	57.884420	64.038695
1717.922535	67.209338	64.043700
1717.662817	67.151563	64.048705
1717.171351	75.124545	64.053710
1715.861849	71.990751	64.058714
1715.418090	66.912845	64.063719
1714.718992	72.263312	64.068724
1714.256876	62.743215	64.073729
1713.189202	60.099337	64.078734
1712.365878	61.741748	64.083738
1711.732568	58.752374	64.088743
1711.138299	65.457340	64.093748
1710.615023	70.960871	64.098753
1709.991592	66.878405	64.103758
1709.301035	78.722131	64.108762
1708.750694	63.754208	64.113767
1707.412056	71.665712	64.118772
1707.293966	69.554844	64.123777
1706.934307	65.310407	64.128782
1706.403539	69.206737	64.133786
1705.804680	62.074412	64.138791
1704.879456	68.549839	64.143796
1704.396438	62.884206	64.148801
1703.721168	71.688734	64.153806
1702.459849	71.406839	64.158810
1701.641039	70.243997	64.163815
1701.127421	74.816707	64.168820
1700.714414	76.920597	64.173825
1700.650021	74.747647	64.178830
1699.288409	67.998065	64.183834
1698.405580	64.091430	64.188839
1697.256728	73.420266	64.193844
1697.338815	66.098002	64.198849
1696.999430	68.756900	64.203854
1696.537997	72.377695	64.208858
1696.419699	57.495319	64.213863
1695.144491	64.831125	64.218868
1694.092499	59.815462	64.223873
1693.659189	63.601172	64.228878
1692.295370	69.207088	64.233882
1691.956897	58.654963	64.238887
1691.389382	64.734064	64.243892
1690.618746	63.453249	64.248897
1690.478985	67.515162	64.253902
1689.768835	72.048084	64.258906
1689.266036	69.251105	64.263911
1688.209119	68.715563	64.268916
1687.688537	63.686332	64.273921
1687.025353	60.009341	64.278926
1686.299051	69.511781	64.283930
1685.197587	68.794791	64.288935
1684.490302	71.967414	64.293940
1684.286011	68.072560	64.298945
1684.303726	60.861573	64.303950
1683.068532	71.074752	64.308954
1682.400616	64.770132	64.313959
1681.365107	65.688626	64.318964
1681.302250	59.541776	64.323969
1680.558766	65.969923	64.328974
1679.271604	63.856221	64.333978
1678.945585	54.357451	64.338983
1678.009861	64.980413	64.343988
1677.917164	70.824720	64.348993
1677.308746	70.029283	64.353998
1675.820207	69.567996	64.359002
1675.248347	73.170190	64.364007
1674.809947	73.053392	64.369012
1674.831828	64.825683	64.374017
1674.623660	61.242139	64.379022
1673.429344	69.998914	64.384026
1672.447895	64.260689	64.389031
1671.942884	76.162264	64.394036
1670.999414	63.128648	64.399041
1670.029779	67.114684	64.404046
1669.349509	70.101509	64.409050
1669.069377	61.549710	64.414055
1668.307175	62.018430	64.419060
1668.031803	66.950221	64.424065
1667.085851	69.186361	64.429070
1666.436849	73.030299	64.434074
1665.689151	59.500576	64.439079
1665.410638	69.196773	64.444084
1664.680461	59.803081	64.449089
1663.851311	67.809767	64.454094
1662.752866	68.782059	64.459098
1662.784608	61.089879	64.464103
1662.183184	66.383372	64.469108
1660.992605	63.213457	64.474113
1660.508968	57.770560	64.479118
1659.666304	67.246335	64.484122
1659.227222	54.558635	64.489127
1658.652684	57.930769	64.494132
1657.354898	68.184264	64.499137
1656.869406	60.797691	64.504142
1655.910899	80.000236	64.509146
1655.996893	67.782386	64.514151
1654.982556	69.984049	64.519156
1654.794435	69.078799	64.524161
1654.037562	58.893529	64.529166
1653.155790	72.382400	64.534170
1652.427642	61.643948	64.539175
1651.682043	65.914134	64.544180
1651.672183	67.140257	64.549185
1650.972665	57.364366	64.554190
1649.522483	68.171680	64.559194
1649.763130	69.716499	64.564199
1648.626259	70.035004	64.569204
1648.215723	69.136633	64.574209
1647.095217	68.356202	64.579214
1646.071454	69.273088	64.584218
1645.485995	58.784158	64.589223
1645.200146	71.355955	64.594228
1644.619197	66.646521	64.599233
1644.437169	76.730403	64.604238
1643.269946	76.372423	64.609242
1642.910701	62.354274	64.614247
1642.025192	64.815327	64.619252
1641.760580	61.139213	64.624257
1640.790745	66.346153	64.629262
1640.007925	72.124224	64.634266
1639.561730	72.266120	64.639271
1638.917865	69.321980	64.644276
1637.640445	69.088249	64.649281
1637.082125	61.809664	64.654286
1636.373316	63.931414	64.659290
1635.725403	59.054635	64.664295
1635.593134	63.707737	64.669300
1635.055247	64.514243	64.674305
1634.474334	63.677396	64.679310
1633.289416	63.352445	64.684314
1633.064224	63.570990	64.689319
1632.274502	67.208495	64.694324
1631.412823	65.239089	64.699329
1630.706180	70.174029	64.704334
1629.856927	70.764621	64.709338
1629.550787	65.465028	64.714343
1629.297694	66.709092	64.719348
1627.441667	61.848407	64.724353
1627.206949	62.247785	64.729358
1626.011304	68.225575	64.734362
1626.097331	60.262014	64.739367
1625.599557	61.184019	64.744372
1624.971646	64.365563	64.749377
1624.951745	61.856598	64.754382
1623.553413	64.878286	64.759386
1622.838523	64.291726	64.764391
1622.481790	65.844434	64.769396
1621.297668	70.732802	64.774401
1620.371266	64.639396	64.779406
1619.245856	71.826430	64.784410
1618.966436	66.230962	64.789415
1618.640016	71.282802	64.794420
1618.799691	67.204884	64.799425
1618.196510	61.153267	64.804430
1617.426942	64.329844	64.809434
1616.499465	63.449680	64.814439
1615.941706	62.125342	64.819444
1614.769961	62.102470	64.824449
1614.127403	57.611208	64.829454
1613.076849	75.032343	64.834458
1613.038822	58.899193	64.839463
1612.706445	62.406330	64.844468
1611.780559	60.726193	64.849473
1611.185194	56.160149	64.854478
1610.145846	71.537876	64.859482
1609.664492	56.656466	64.864487
1609.304143	69.705987	64.869492
1608.264488	66.292767	64.874497
1607.793460	67.934901	64.879502
1607.039527	74.559047	64.884506
1606.556466	60.862478	64.889511
1605.272203	65.739960	64.894516
1604.461234	62.902973	64.899521
1604.052835	62.168049	64.904526
1603.566740	66.474747	64.909530
1603.398698	57.972458	64.914535
1602.688849	62.391260	64.919540
1601.911070	60.471842	64.924545
1601.172184	65.926225	64.929550
1600.217128	64.150429	64.934554
1599.971748	57.789702	64.939559
1599.164035	72.940298	64.944564
1598.277876	61.854313	64.949569
1597.709048	55.992604	64.954574
1597.458849	62.290155	64.959578
1596.995895	61.276027	64.964583
1595.388746	63.459944	64.969588
1594.740341	62.900693	64.974593
1594.375100	63.608976	64.979598
1593.625382	69.785577	64.984602
1593.372536	65.963775	64.989607
1592.658854	71.479765	64.994612
1591.052200	73.860171	64.999617
1590.831640	67.966882	65.004622
1590.101694	72.184662	65.009626
1590.109085	61.943611	65.014631
1589.295283	68.345511	65.019636
1588.981789	68.414572	65.024641
1588.431973	64.471890	65.029646
1587.172413	69.501063	65.034650
1586.393960	64.155601	65.039655
1585.233334	67.364371	65.044660
1584.646627	54.293813	65.049665
1584.679287	52.061632	65.054670
1583.848629	70.528238	65.059674
1583.782271	57.882946	65.064679
1583.282590	62.291438	65.069684
1581.891970	62.669173	65.074689
1581.358884	59.184662	65.079694
1580.749914	55.787740	65.084698
1579.323110	58.947331	65.089703
1578.713375	59.466546	65.094708
1577.972750	65.617118	65.099713
1577.883188	60.017585	65.104718
1577.277222	55.298631	65.109722
1577.087616	53.309348	65.114727
1576.223888	56.631905	65.119732
1575.424964	65.609957	65.124737
1574.580118	58.209113	65.129742
1574.070142	63.207499	65.134746
1573.747272	55.242479	65.139751
1572.495400	60.932280	65.144756
1571.634272	59.862751	65.149761
1571.522917	50.184770	65.154766
1570.854007	61.309549	65.159770
1570.294768	56.074201	65.164775
1569.163030	62.342232	65.169780
1568.339956	67.259209	65.174785
1567.988533	59.531959	65.179790
1567.144148	63.523414	65.184794
1567.395134	60.267860	65.189799
1565.950365	61.839022	65.194804
1564.892241	65.127749	65.199809
1564.783733	65.724599	65.204814
1564.229017	68.690737	65.209818
1563.774866	55.130941	65.214823
1562.729523	59.269677	65.219828
1561.687100	54.833044	65.224833
1561.579635	51.812119	65.229838
1560.432482	64.187904	65.234842
1560.303778	65.337264	65.239847
1559.654911	60.938666	65.244852
1558.766083	61.698271	65.249857
1558.523267	58.160534	65.254862
1558.116488	62.679438	65.259866
1556.513601	59.967729	65.264871
1556.216556	60.824993	65.269876
1555.361807	61.212072	65.274881
1555.241700	64.810771	65.279886
1553.261497	65.302836	65.284890
1552.910607	58.688605	65.289895
1552.237512	61.150026	65.294900
1551.646661	63.405933	65.299905
1551.674357	59.920579	65.304910
1550.809892	61.126390	65.309914
1551.004964	57.493581	65.314919
1550.005518	65.084571	65.319924
1549.118463	62.926112	65.324929
1548.647319	64.266310	65.329934
1547.453781	65.616858	65.334938
1546.540675	61.406373	65.339943
1546.035363	57.576077	65.344948
1545.469462	58.611191	65.349953
1544.880030	55.478156	65.354958
1544.948293	57.816250	65.359962
1543.851932	54.981937	65.364967
1542.681536	56.838106	65.369972
1541.976457	62.358546	65.374977
1541.561245	46.811794	65.379982
1540.765796	67.007550	65.384986
1540.172416	59.176457	65.389991
1539.395986	58.641493	65.394996
1538.758907	65.128803	65.400001
1538.714348	60.900324	65.405006
1537.849134	60.726723	65.410010
1537.185979	60.367363	65.415015
1536.308108	55.473120	65.420020
1535.575326	65.624800	65.425025
1535.495490	56.892697	65.430030
1534.612552	67.664524	65.435034
1533.848407	52.549312	65.440039
1533.037817	55.349251	65.445044
1532.237167	61.064460	65.450049
1531.320449	56.464222	65.455054
1530.275460	62.566234	65.460058
1530.149332	59.379959	65.465063
1529.460024	62.500574	65.470068
1528.711485	68.015034	65.475073
1528.699643	58.239894	65.480078
1528.042029	66.880359	65.485082
1527.696058	61.146695	65.490087
1526.880846	52.270862	65.495092
1526.068029	61.923498	65.500097
1525.050240	58.115786	65.505102
1524.058375	56.289862	65.510106
1523.770930	55.018741	65.515111
1522.755851	56.978984	65.520116
1522.347845	60.344336	65.525121
1522.224390	55.358082	65.530126
1520.931750	58.689715	65.535130
1520.361929	57.885325	65.540135
1519.169101	59.548768	65.545140
1518.867182	61.482082	65.550145
1518.904441	57.312230	65.555150
1518.115377	64.748801	65.560154
1517.446403	64.306759	65.565159
1516.109100	62.934677	65.570164
1515.682231	59.628171	65.575169
1515.692688	60.852789	65.580174
1514.476316	62.757489	65.585178
1514.084860	57.592903	65.590183
1513.308843	60.373903	65.595188
1512.977371	69.845483	65.600193
1511.791026	60.506613	65.605198
1510.851758	65.070868	65.610202
1510.406859	62.347685	65.615207
1510.103940	63.172406	65.620212
1508.956430	61.467856	65.625217
1508.934188	57.944474	65.630222
1507.716542	58.979039	65.635226
1506.967050	55.916429	65.640231
1506.662819	57.284112	65.645236
1506.151829	59.254788	65.650241
1505.845317	52.229173	65.655246
1504.517169	61.945933	65.660250
1504.025997	54.391423	65.665255
1503.608030	56.498144	65.670260
1502.617446	56.562707	65.675265
1501.794251	60.323974	65.680270
1501.078410	58.734220	65.685274
1500.402177	59.915717	65.690279
1500.336931	57.891337	65.695284
1499.414173	59.586716	65.700289
1498.373953	56.302694	65.705294
1497.254561	65.496251	65.710298
1496.983243	56.440100	65.715303
1496.848592	56.702362	65.720308
1496.028434	67.521469	65.725313
1496.205541	55.074117	65.730318
1494.566483	66.261528	65.735322
1493.908547	65.194734	65.740327
1493.734421	63.563972	65.745332
1492.669381	63.179460	65.750337
1492.518878	49.893357	65.755342
1491.132130	49.679165	65.760346
1490.410875	63.268842	65.765351
1490.011743	60.585194	65.770356
1489.325804	61.514944	65.775361
1489.260193	58.254369	65.780366
1488.003005	63.688529	65.785370
1487.261643	60.319412	65.790375
1487.201676	61.872252	65.795380
1486.099475	61.918029	65.800385
1485.229058	65.400817	65.805390
1484.456319	65.407572	65.810394
1484.105946	62.925964	65.815399
1483.667514	62.303949	65.820404
1483.007830	57.757618	65.825409
1482.569151	63.598765	65.830414
1481.427633	61.856882	65.835418
1481.179202	59.070867	65.840423
1480.612134	53.897267	65.845428
1479.173308	60.940206	65.850433
1478.547135	61.026476	65.855438
1477.829540	61.766260	65.860442
1477.290872	59.343723	65.865447
1477.083235	56.417706	65.870452
1476.466475	60.918081	65.875457
1475.894597	59.592625	65.880462
1474.638596	59.248695	65.885466
1474.327237	60.778251	65.890471
1473.996754	57.187634	65.895476
1473.044791	57.357298	65.900481
1472.241340	58.635174	65.905486
1471.599357	63.798257	65.910490
1470.815180	52.891431	65.915495
1470.052916	49.118548	65.920500
1469.036097	66.597055	65.925505
1468.397980	58.390363	65.930510
1467.750551	63.186107	65.935514
1467.746632	68.787851	65.940519
1466.985861	60.491630	65.945524
1466.654700	63.147944	65.950529
1466.403314	57.187716	65.955534
1465.053434	60.374824	65.960538
1464.030836	57.794734	65.965543
1463.630001	51.702201	65.970548
1463.104349	63.675184	65.975553
1462.619298	57.765213	65.980558
1461.273970	55.792180	65.985562
1460.824528	56.068851	65.990567
1460.494850	56.816447	65.995572
1459.767525	59.435968	66.000577
1459.235309	65.192079	66.005582
1457.989067	63.919289	66.010586
1457.655280	63.998147	66.015591
1457.108748	52.467650	66.020596
1456.618557	64.086816	66.025601
1455.834140	56.183840	66.030606
1455.383630	63.307479	66.035610
1454.669133	62.669168	66.040615
1454.183275	59.175803	66.045620
1452.782780	60.700340	66.050625
1451.917000	57.514755	66.055630
1451.642203	61.482938	66.060634
1451.006853	55.605011	66.065639
1450.981575	54.471777	66.070644
1449.640329	62.953741	66.075649
1449.390028	59.442556	66.080654
1448.563116	60.042772	66.085658
1447.730160	57.807578	66.090663
1447.500341	54.400252	66.095668
1446.156219	61.743946	66.100673
1446.029447	47.545545	66.105678
1445.234627	60.853351	66.110682
1445.024016	60.495093	66.115687
1443.963073	51.766731	66.120692
1442.827634	60.281755	66.125697
1442.424203	60.556473	66.130702
1441.738688	57.877247	66.135706
1441.232928	59.699013	66.140711
1440.813160	51.069712	66.145716
1439.558731	62.038146	66.150721
1439.546913	55.873502	66.155726
1439.010611	53.977909	66.160730
1437.887272	52.989206	66.165735
1436.775853	55.421459	66.170740
1436.193226	63.299519	66.175745
1435.646810	55.838946	66.180750
1435.161051	51.039840	66.185754
1434.796673	56.495654	66.190759
1434.729720	56.640940	66.195764
1433.518770	58.658803	66.200769
1432.722428	57.661102	66.205774
1431.759764	59.902507	66.210778
1430.916547	62.022025	66.215783
1430.312358	50.916647	66.220788
1429.349606	56.553827	66.225793
1429.199983	53.434340	66.230798
1428.744615	57.843938	66.235802
1428.018445	61.658077	66.240807
1428.007834	52.475608	66.245812
1426.720000	52.358182	66.250817
1426.149427	54.250251	66.255822
1425.599024	62.790659	66.260826
1424.772319	63.616622	66.265831
1423.999253	57.319793	66.270836
1423.040011	64.238420	66.275841
1422.753296	46.153375	66.280846
1422.540952	54.886954	66.285850
1421.783347	55.133485	66.290855
1420.632206	47.828137	66.295860
1419.842926	61.553397	66.300865
1419.754312	51.142892	66.305870
1418.649084	61.372929	66.310874
1417.263296	61.739618	66.315879
1416.825711	54.758160	66.320884
1416.353630	61.040004	66.325889
1415.895224	58.879645	66.330894
1415.230002	54.922010	66.335898
1414.808333	56.333088	66.340903
1414.955703	57.377170	66.345908
1413.904723	55.421659	66.350913
1413.397477	55.040760	66.355918
1412.523944	48.634034	66.360922
1411.454253	51.353213	66.365927
1410.694065	56.201811	66.370932
1409.597300	60.481605	66.375937
1409.547262	56.487745	66.380942
1409.279718	59.686961	66.385946
1407.899566	58.220011	66.390951
1407.107096	53.936413	66.395956
1406.390861	56.298264	66.400961
1406.142656	55.885262	66.405966
1405.723133	53.199194	66.410970
1405.453215	53.985510	66.415975
1404.750992	52.157005	66.420980
1403.957528	63.717560	66.425985
1403.356307	49.663927	66.430990
1401.941217	63.497494	66.435994
1401.049932	62.544469	66.440999
1400.878444	52.913905	66.446004
1399.974443	58.937724	66.451009
1399.684119	55.503260	66.456014
1399.472956	63.290107	66.461018
1398.163596	62.025374	66.466023
1397.675355	53.268859	66.471028
1396.907562	64.551877	66.476033
1396.533214	54.620131	66.481038
1395.666093	58.067629	66.486042
1394.824049	54.549983	66.491047
1394.295134	61.458896	66.496052
1393.314292	53.809417	66.501057
1393.217386	60.951471	66.506062
1392.362669	65.977694	66.511066
1391.192970	61.335926	66.516071
1391.072323	58.697773	66.521076
1390.050781	62.327225	66.526081
1389.935301	58.207601	66.531086
1389.557219	54.844210	66.536090
1388.205750	60.798186	66.541095
1387.671330	59.924992	66.546100
1386.655418	67.380668	66.551105
1386.580644	58.620084	66.556110
1385.968026	60.117137	66.561114
1384.859411	54.397204	66.566119
1384.151432	57.565632	66.571124
1383.494653	60.500308	66.576129
1382.992570	59.976035	66.581134
1382.636487	70.959646	66.586138
1382.078496	68.679763	66.591143
1381.695020	53.892181	66.596148
1380.747268	61.055544	66.601153
1379.719116	64.577187	66.606158
1378.671135	59.756700	66.611162
1378.000537	62.554801	66.616167
1377.462428	60.406115	66.621172
1377.180946	67.325174	66.626177
1376.715905	60.498018	66.631182
1376.341347	64.263816	66.636186
1374.810086	63.230091	66.641191
1374.202603	55.088832	66.646196
1373.633714	65.849142	66.651201
1373.129719	61.069742	66.656206
1372.964356	61.406340	66.661210
1371.907876	58.394724	66.666215
1371.331757	58.733743	66.671220
1370.441985	58.710815	66.676225
1370.283825	59.013419	66.681230
1369.127450	50.577324	66.686234
1368.291557	63.719279	66.691239
1367.933864	51.269546	66.696244
1367.110750	58.111588	66.701249
1367.048094	50.118242	66.706254
1366.111060	60.122528	66.711258
1365.016593	56.602310	66.716263
1364.770916	55.814290	66.721268
1364.113079	61.859131	66.726273
1363.400485	62.689648	66.731278
1362.495730	62.043658	66.736282
1361.321195	58.803976	66.741287
1361.176937	53.387107	66.746292
1360.402517	55.915231	66.751297
1360.363211	59.089982	66.756302
1359.748407	57.091790	66.761306
1358.474738	58.323865	66.766311
1358.133138	54.970021	66.771316
1357.780791	61.102299	66.776321
1356.542895	55.238722	66.781326
1355.647694	56.792835	66.786330
1354.834788	60.394866	66.791335
1354.704716	51.607836	66.796340
1354.136319	56.932005	66.801345
1354.339098	55.552506	66.806350
1352.918257	56.790829	66.811354
1352.128225	64.990962	66.816359
1351.563209	60.282403	66.821364
1350.104002	70.178330	66.826369
1349.127419	62.002760	66.831374
1349.041023	59.529265	66.836378
1348.509686	64.183966	66.841383
1348.158581	56.358412	66.846388
1347.390637	73.909583	66.851393
1347.149956	62.945665	66.856398
1346.234640	65.027803	66.861402
1345.304484	75.340777	66.866407
1344.858436	64.419908	66.871412
1344.128706	74.059523	66.876417
1344.019384	62.308155	66.881422
1342.775864	64.705017	66.886426
1341.744737	64.956938	66.891431
1341.388411	53.664683	66.896436
1340.977482	58.939793	66.901441
1340.254237	64.445596	66.906446
1339.379375	66.467918	66.911450
1338.367137	70.324329	66.916455
1338.444219	59.403909	66.921460
1337.561241	63.409498	66.926465
1337.126624	60.411036	66.931470
1335.920675	62.394514	66.936474
1334.925157	66.845270	66.941479
1334.853112	59.541524	66.946484
1334.262143	69.693409	66.951489
1333.942237	69.323473	66.956494
1333.205706	60.588550	66.961498
1332.106381	68.217583	66.966503
1331.516342	60.065055	66.971508
1331.006684	68.964001	66.976513
1330.613157	62.471567	66.981518
1329.637615	60.563157	66.986522
1328.708811	64.396207	66.991527
1328.646794	61.870778	66.996532
1327.588940	63.567207	67.001537
1326.596761	57.523030	67.006542
1325.887048	59.352089	67.011546
1325.021600	66.276776	67.016551
1324.916385	58.448209	67.021556
1324.502462	55.184114	67.026561
1324.327863	59.678672	67.031566
1323.326118	63.716437	67.036570
1322.053515	67.730705	67.041575
1321.821763	58.700173	67.046580
1321.278407	63.370748	67.051585
1320.215200	59.083384	67.056590
1319.180620	65.163514	67.061594
1318.428899	73.423408	67.066599
1318.373148	56.992969	67.071604
1317.748598	60.918796	67.076609
1317.738541	54.804778	67.081614
1316.519937	67.946335	67.086618
1315.538485	65.786714	67.091623
1315.273612	61.571095	67.096628
1314.400819	67.053558	67.101633
1313.696609	66.809014	67.106638
1312.951670	66.643677	67.111642
1312.024804	72.265260	67.116647
1311.858196	70.398758	67.121652
1311.261455	68.446029	67.126657
1311.092947	61.592592	67.131662
1310.232645	59.797873	67.136666
1309.279923	66.336864	67.141671
1308.213680	61.995156	67.146676
1307.239905	64.005601	67.151681
1306.370196	56.301200	67.156686
1306.231693	63.247092	67.161690
1305.725404	64.787921	67.166695
1305.615645	62.389082	67.171700
1305.220176	70.599039	67.176705
1303.813656	56.101473	67.181710
1303.171473	62.114824	67.186714
1302.459031	65.292710	67.191719
1302.179389	63.535950	67.196724
1301.304089	72.165141	67.201729
1300.518887	65.840809	67.206734
1300.025782	63.099457	67.211738
1299.472511	69.762295	67.216743
1298.461942	57.930762	67.221748
1297.335229	62.056236	67.226753
1296.713495	64.909135	67.231758
1296.424545	57.445167	67.236762
1296.282882	71.852162	67.241767
1295.628006	56.115187	67.246772
1294.297009	65.507222	67.251777
1293.666557	64.121162	67.256782
1293.714415	66.334852	67.261786
1293.265081	63.974804	67.266791
1292.109971	56.985945	67.271796
1291.249572	63.640572	67.276801
1290.563226	59.958535	67.281806
1289.973115	61.821595	67.286810
1288.917304	69.513840	67.291815
1288.433757	66.232457	67.296820
1287.748909	65.602121	67.301825
1287.092660	68.185813	67.306830
1286.825085	60.705159	67.311834
1286.341378	68.969694	67.316839
1285.413732	66.438912	67.321844
1284.584630	72.385588	67.326849
1283.826692	71.304366	67.331854
1283.536602	66.566907	67.336858
1282.891302	62.606673	67.341863
1281.991285	59.742363	67.346868
1281.006554	59.445985	67.351873
1280.579895	65.022987	67.356878
1280.121102	61.174107	67.361882
1279.292250	67.121133	67.366887
1279.105153	61.356356	67.371892
1278.043119	66.795434	67.376897
1277.314006	63.902656	67.381902
1277.262143	64.552573	67.386906
1275.874847	73.745844	67.391911
1275.264794	65.524517	67.396916
1274.407733	71.294805	67.401921
1273.806889	71.329793	67.406926
1273.669227	66.068501	67.411930
1272.768305	70.733193	67.416935
1272.491506	63.711598	67.421940
1271.082158	71.628179	67.426945
1270.520132	65.251832	67.431950
1270.036523	63.107250	67.436954
1269.644921	70.311989	67.441959
1269.366272	59.223935	67.446964
1268.031678	64.534027	67.451969
1267.407437	64.925504	67.456974
1267.042891	61.330083	67.461978
1266.307442	65.442656	67.466983
1265.645788	63.085804	67.471988
1264.539895	66.137247	67.476993
1264.094801	69.075957	67.481998
1263.730844	58.973514	67.487002
1263.057694	67.333241	67.492007
1261.814420	66.824957	67.497012
1261.046573	64.768509	67.502017
1260.702765	63.646785	67.507022
1260.574501	62.631049	67.512026
1259.540187	65.532481	67.517031
1259.104315	62.622660	67.522036
1257.974044	63.028933	67.527041
1257.417497	69.603916	67.532046
1257.379029	62.608227	67.537050
1256.747319	65.237455	67.542055
1255.781966	56.654617	67.547060
1254.492539	58.162164	67.552065
1253.962140	59.934482	67.557070
1254.010849	57.032092	67.562074
1252.916267	63.275258	67.567079
1252.023123	59.456536	67.572084
1251.208621	57.787007	67.577089
1250.615609	57.280289	67.582094
1250.547192	53.869030	67.587098
1250.139880	64.032099	67.592103
1249.472169	55.677767	67.597108
1248.469461	56.452973	67.602113
1247.574598	57.832974	67.607118
1247.581751	57.446917	67.612122
1245.710141	65.310015	67.617127
1245.423162	62.887442	67.622132
1245.167942	57.023023	67.627137
1244.609900	65.136869	67.632142
1243.871327	55.490129	67.637146
1243.125207	65.830408	67.642151
1242.129004	60.532168	67.647156
1241.442582	60.795353	67.652161
1241.324722	59.520086	67.657166
1240.802959	58.811312	67.662170
1239.899686	62.163974	67.667175
1239.235470	60.124918	67.672180
1238.405533	58.338830	67.677185
1237.951170	51.406062	67.682190
1237.109854	57.032739	67.687194
1235.692323	53.325903	67.692199
1235.574071	60.191353	67.697204
1235.347959	61.332922	67.702209
1234.342461	69.336281	67.707214
1234.106408	63.284640	67.712218
1233.562477	64.584038	67.717223
1232.384383	53.520518	67.722228
1231.780793	58.610731	67.727233
1231.266891	62.523542	67.732238
1230.795846	59.484359	67.737242
1229.698306	65.581991	67.742247
1228.856013	58.713664	67.747252
1228.535237	60.083008	67.752257
1227.844635	52.886755	67.757262
1227.838255	50.284705	67.762266
1226.510436	64.577804	67.767271
1225.881420	55.524912	67.772276
1225.597162	63.462022	67.777281
1224.145454	52.810464	67.782286
1223.498925	57.565019	67.787290
1222.463382	58.331642	67.792295
1222.348237	57.760086	67.797300
1222.008654	62.684712	67.802305
1221.516418	53.728399	67.807310
1221.440308	53.483301	67.812314
1219.766400	55.514555	67.817319
1219.642138	56.986432	67.822324
1218.793488	59.578992	67.827329
1218.161454	62.438398	67.832334
1217.121348	52.547254	67.837338
1215.886258	65.471388	67.842343
1215.741074	56.315137	67.847348
1215.272113	55.984938	67.852353
1214.748895	60.213540	67.857358
1214.453968	52.007357	67.862362
1213.279271	65.134694	67.867367
1212.455513	54.166823	67.872372
1211.975533	52.886453	67.877377
1211.345889	66.551231	67.882382
1211.181443	56.912775	67.887386
1209.981355	67.784706	67.892391
1209.515205	60.354640	67.897396
1208.919309	59.506201	67.902401
1208.153357	60.683358	67.907406
1207.064008	55.341078	67.912410
1206.132384	63.079960	67.917415
1205.788686	59.207832	67.922420
1205.368648	62.879586	67.927425
1204.998054	62.550309	67.932430
1204.556370	64.352441	67.937434
1203.700999	67.842163	67.942439
1202.752823	55.372776	67.947444
1202.200226	68.369923	67.952449
1201.589537	59.777295	67.957454
1200.557000	53.719537	67.962458
1199.550736	60.231391	67.967463
1199.372174	55.992324	67.972468
1198.978677	63.293695	67.977473
1198.517531	58.563825	67.982478
1198.003318	53.334647	67.987482
1196.974173	64.219939	67.992487
1196.449379	56.041271	67.997492
1195.585253	60.154961	68.002497
1194.760761	57.516543	68.007502
1194.270577	59.795114	68.012506
1193.391304	56.761885	68.017511
1193.325536	54.046062	68.022516
1192.312164	55.061908	68.027521
1191.058660	60.827449	68.032526
1190.543871	62.549735	68.037530
1190.132824	64.382936	68.042535
1189.576358	59.234409	68.047540
1189.382090	55.951274	68.052545
1187.797957	61.318316	68.057550
1187.519850	60.465994	68.062554
1186.866658	60.316149	68.067559
1186.686955	65.363395	68.072564
1186.001618	68.854007	68.077569
1184.665224	64.191102	68.082574
1184.455787	70.757182	68.087578
1183.588599	71.213554	68.092583
1182.627349	61.420224	68.097588
1181.915469	62.906663	68.102593
1181.071230	62.146930	68.107598
1180.964061	58.599421	68.112602
1179.906647	58.487999	68.117607
1179.389995	67.070394	68.122612
1179.437988	62.422687	68.127617
1178.857768	67.881124	68.132622
1178.042692	61.048015	68.137626
1177.222866	66.374984	68.142631
1176.607183	68.781618	68.147636
1174.938184	63.072825	68.152641
1174.553064	69.974100	68.157646
1174.232560	60.313422	68.162650
1173.308413	69.391884	68.167655
1173.222946	59.693727	68.172660
1173.023611	62.261169	68.177665
1172.147811	67.544041	68.182670
1171.496294	56.836411	68.187674
1170.450322	64.020562	68.192679
1169.790270	60.329308	68.197684
1168.618258	64.662683	68.202689
1167.460009	62.867692	68.207694
1167.518283	59.405930	68.212698
1167.324905	68.412952	68.217703
1166.572218	55.964181	68.222708
1165.866972	58.175371	68.227713
1165.337767	59.478174	68.232718
1164.644875	51.685120	68.237722
1164.198422	60.738232	68.242727
1163.738146	60.106171	68.247732
1162.467622	60.641869	68.252737
1161.613623	61.102697	68.257742
1161.378478	54.225560	68.262746
1160.453479	61.145457	68.267751
1160.067125	61.659235	68.272756
1159.286352	64.848046	68.277761
1158.235877	68.278027	68.282766
1157.865495	59.915039	68.287770
1157.045914	66.419410	68.292775
1156.452306	60.147567	68.297780
1155.687078	52.703199	68.302785
1154.828581	58.536896	68.307790
1154.614579	50.065826	68.312794
1153.702404	57.236541	68.317799
1153.352467	52.449351	68.322804
1153.160926	63.754491	68.327809
1151.650051	59.317648	68.332814
1151.368018	53.939387	68.337818
1150.581792	60.892758	68.342823
1149.998379	60.042979	68.347828
1149.410416	59.480938	68.352833
1148.265208	57.618592	68.357838
1148.064535	56.852877	68.362842
1147.352539	59.808082	68.367847
1146.701464	59.328291	68.372852
1146.039296	52.365597	68.377857
1145.112615	61.187135	68.382862
1144.960397	49.638537	68.387866
1144.604387	60.729480	68.392871
1143.235010	56.409722	68.397876
1142.674624	57.299465	68.402881
1141.318374	64.909755	68.407886
1141.422811	54.600829	68.412890
1140.880709	61.326095	68.417895
1139.661426	59.585770	68.422900
1139.183474	57.176960	68.427905
1138.186132	58.540186	68.432910
1138.010281	56.252140	68.437914
1137.509447	65.669811	68.442919
1137.361141	56.585943	68.447924
1136.138074	55.657805	68.452929
1135.101644	54.010114	68.457934
1134.771607	54.387941	68.462938
1134.205853	54.142215	68.467943
1133.424230	60.276552	68.472948
1132.900772	58.656284	68.477953
1131.913572	60.705372	68.482958
1131.523371	57.266720	68.487962
1131.337871	61.910372	68.492967
1129.856202	57.220260	68.497972
1129.126429	54.337491	68.502977
1128.514115	59.824711	68.507982
1128.049764	47.611573	68.512986
1127.550259	61.424578	68.517991
1127.081331	63.484394	68.522996
1126.172770	57.650151	68.528001
1125.054867	62.592791	68.533006
1124.961302	57.422643	68.538010
1124.662464	59.760029	68.543015
1123.743901	56.486450	68.548020
1122.741589	53.944807	68.553025
1122.270537	61.458789	68.558030
1121.782167	58.020764	68.563034
1120.752819	60.595334	68.568039
1119.504761	64.861612	68.573044
1119.340515	62.343828	68.578049
1118.488858	63.432652	68.583054
1118.333414	57.573267	68.588058
1117.810896	58.623889	68.593063
1117.243002	63.836677	68.598068
1116.303854	63.683703	68.603073
1115.217672	69.612049	68.608078
1115.126910	61.574196	68.613082
1114.626639	66.124517	68.618087
1113.804229	58.229707	68.623092
1112.930062	59.657895	68.628097
1111.984305	64.032667	68.633102
1112.164022	52.261455	68.638106
1110.728090	63.973079	68.643111
1109.817519	54.097680	68.648116
1109.322819	50.228528	68.653121
1108.574773	67.580891	68.658126
1108.677216	56.198283	68.663130
1108.224250	59.088218	68.668135
1107.171235	54.284850	68.673140
1106.625075	51.234863	68.678145
1106.106590	60.854096	68.683150
1105.119443	61.269841	68.688154
1104.086201	56.067580	68.693159
1103.391994	53.968949	68.698164
1102.867449	59.929012	68.703169
1102.173300	59.884476	68.708174
1102.165756	52.325381	68.713178
1101.131764	56.867227	68.718183
1100.372717	61.365942	68.723188
1100.194774	58.958263	68.728193
1099.018478	60.994738	68.733198
1098.076322	49.990337	68.738202
1096.929644	55.119081	68.743207
1096.458982	57.306688	68.748212
1096.132155	56.997951	68.753217
1095.664179	59.390351	68.758222
1095.740309	60.225973	68.763226
1095.393729	55.881876	68.768231
1094.271083	59.031345	68.773236
1093.560560	63.217031	68.778241
1092.599104	60.750499	68.783246
1091.680446	47.956379	68.788250
1091.103157	64.181791	68.793255
1090.670065	59.669754	68.798260
1090.418306	53.409650	68.803265
1088.917016	53.051376	68.808270
1087.992032	49.187226	68.813274
1086.882719	53.717893	68.818279
1086.893925	55.741282	68.823284
1086.391653	57.396698	68.828289
1085.965384	57.187880	68.833294
1085.539462	46.867154	68.838298
1084.462439	61.275996	68.843303
1083.974097	49.409984	68.848308
1083.999343	51.472808	68.853313
1082.511873	56.001129	68.858318
1081.866362	49.256638	68.863322
1080.774901	52.136308	68.868327
1080.234293	57.877291	68.873332
1080.132792	54.738534	68.878337
1079.729841	61.280904	68.883342
1078.520489	47.251369	68.888346
1077.757555	48.798270	68.893351
1077.191339	60.924231	68.898356
1077.133518	48.207303	68.903361
1076.022222	59.064829	68.908366
1075.208148	50.492062	68.913370
1074.665254	48.562120	68.918375
1074.178690	46.975410	68.923380
1073.331022	49.391383	68.928385
1071.940538	49.872648	68.933390
1071.640146	44.664903	68.938394
1070.713263	52.230095	68.943399
1070.416399	45.105003	68.948404
1070.424296	45.173138	68.953409
1069.783282	50.050699	68.958414
1069.568556	42.470644	68.963418
1068.608795	55.998133	68.968423
1067.422771	58.140485	68.973428
1066.333122	44.185587	68.978433
1065.358959	52.772508	68.983438
1065.135727	48.742803	68.988442
1064.434514	56.680255	68.993447
1063.943176	49.637802	68.998452
1064.185969	55.947231	69.003457
1062.926707	52.600961	69.008462
1062.353442	46.391182	69.013466
1061.597943	48.136144	69.018471
1060.976573	60.318125	69.023476
1060.001867	45.116371	69.028481
1059.209548	51.022818	69.033486
1058.853361	45.309918	69.038490
1058.432718	48.720476	69.043495
1057.356026	51.348950	69.048500
1056.723035	48.693162	69.053505
1055.041544	57.708694	69.058510
1055.253783	49.307536	69.063514
1054.707463	50.847346	69.068519
1054.280448	53.614820	69.073524
1054.257808	53.867385	69.078529
1052.933798	50.607992	69.083534
1052.068063	48.445590	69.088538
1051.708632	55.443902	69.093543
1050.563917	56.389903	69.098548
1050.568815	55.521100	69.103553
1049.357222	57.391138	69.108558
1049.021889	54.189010	69.113562
1048.262664	49.619150	69.118567
1047.925016	54.196489	69.123572
1047.001619	45.989013	69.128577
1045.926049	53.910443	69.133582
1045.450311	49.166519	69.138586
1044.920887	49.722172	69.143591
1044.333593	62.802221	69.148596
1043.602474	57.808752	69.153601
1042.608729	60.523284	69.158606
1042.510093	56.941956	69.163610
1041.896304	54.029868	69.168615
1041.318429	56.155317	69.173620
1040.559966	51.246266	69.178625
1039.435924	59.481905	69.183630
1039.090551	52.347753	69.188634
1038.461777	48.031069	69.193639
1036.985200	56.799157	69.198644
1036.671922	46.636774	69.203649
1035.952576	63.404771	69.208654
1035.619368	54.723614	69.213658
1035.324040	57.040271	69.218663
1034.818077	58.543569	69.223668
1033.939521	57.210690	69.228673
1032.636800	57.323272	69.233678
1032.133023	45.537676	69.238682
1032.047889	60.373475	69.243687
1030.737155	61.490799	69.248692
1030.238071	48.604718	69.253697
1029.484747	63.085626	69.258702
1029.466302	52.879461	69.263706
1028.957625	50.906957	69.268711
1027.907084	63.597018	69.273716
1027.127571	58.730255	69.278721
1026.185959	56.213369	69.283726
1025.917419	55.097327	69.288730
1024.745741	56.910407	69.293735
1023.779132	52.416722	69.298740
1023.429469	54.968856	69.303745
1022.737479	60.008304	69.308750
1022.692628	57.433372	69.313754
1022.278567	58.609107	69.318759
1021.550678	57.838161	69.323764
1020.661879	56.860310	69.328769
1019.654844	61.778061	69.333774
1019.306576	50.227137	69.338778
1018.813295	51.109744	69.343783
1017.371511	54.120072	69.348788
1016.994201	57.462822	69.353793
1016.348797	61.948401	69.358798
1016.648640	57.471904	69.363802
1015.414434	51.422287	69.368807
1014.171182	62.231371	69.373812
1014.122679	47.834917	69.378817
1013.401848	54.664604	69.383822
1012.658265	61.498190	69.388826
1011.229382	52.446939	69.393831
1010.506122	52.906717	69.398836
1010.436480	51.532417	69.403841
1009.764702	52.682816	69.408846
1009.756961	43.780942	69.413850
1009.243885	53.431611	69.418855
1008.025558	51.588532	69.423860
1007.514428	46.056112	69.428865
1006.731184	60.265446	69.433870
1005.609599	54.424296	69.438874
1004.487779	61.595801	69.443879
1003.660644	56.067760	69.448884
1004.070749	52.903365	69.453889
1003.500791	53.486094	69.458894
1003.023746	52.626802	69.463898
1002.505079	52.173302	69.468903
1001.348205	53.208628	69.473908
1000.535214	49.307557	69.478913
999.815638	48.437697	69.483918
999.599464	50.509496	69.488922
998.862495	50.711111	69.493927
997.684121	56.573158	69.498932
997.131625	51.827781	69.503937
996.984064	58.428251	69.508942
996.264167	50.013446	69.513946
995.237594	51.881809	69.518951
994.276609	52.072055	69.523956
994.043006	47.543633	69.528961
993.243758	52.505138	69.533966
993.004909	57.538035	69.538970
992.422498	58.356570	69.543975
991.506862	58.634966	69.548980
990.881519	53.479718	69.553985
990.521563	60.489569	69.558990
989.194505	48.745898	69.563994
988.065315	57.574894	69.568999
987.384354	56.577244	69.574004
987.124893	52.746372	69.579009
986.602602	54.954275	69.584014
986.428744	51.240578	69.589018
986.017001	50.962574	69.594023
985.289956	54.491922	69.599028
984.239320	44.998165	69.604033
983.913074	55.390088	69.609038
982.993320	55.451307	69.614042
982.279574	51.008270	69.619047
981.177097	57.115072	69.624052
980.817587	56.311044	69.629057
980.025629	61.107498	69.634062
979.711558	58.862079	69.639066
978.963820	56.820791	69.644071
978.252250	57.640922	69.649076
977.958300	58.897137	69.654081
976.835306	63.919223	69.659086
975.775590	60.125141	69.664090
975.101708	50.889740	69.669095
974.660005	58.841567	69.674100
974.447268	54.865332	69.679105
974.009579	57.544644	69.684110
972.968966	51.324920	69.689114
972.190079	57.707867	69.694119
971.414515	57.449936	69.699124
971.237159	50.039929	69.704129
970.338062	57.390387	69.709134
969.552397	53.849754	69.714138
968.847594	54.860164	69.719143
967.792656	57.507429	69.724148
967.676088	51.890074	69.729153
967.440455	52.743955	69.734158
966.404283	55.232488	69.739162
965.769656	45.193438	69.744167
965.047034	52.611955	69.749172
964.506416	49.671166	69.754177
963.364718	52.158825	69.759182
962.687958	52.105410	69.764186
962.201460	45.441076	69.769191
961.578073	49.716054	69.774196
961.703550	47.119060	69.779201
960.300127	50.352164	69.784206
959.709079	51.535320	69.789210
958.949952	53.025142	69.794215
958.239812	54.375923	69.799220
958.050479	46.371554	69.804225
956.953335	52.675197	69.809230
956.056694	52.063814	69.814234
955.727101	51.257428	69.819239
954.590015	56.745720	69.824244
954.676030	45.411737	69.829249
954.248386	58.949939	69.834254
953.264634	54.917866	69.839258
952.476011	45.584893	69.844263
951.722209	57.330892	69.849268
951.219462	47.634370	69.854273
950.185995	51.721831	69.859278
949.679066	48.529366	69.864282
948.843195	50.341790	69.869287
948.102459	53.746388	69.874292
948.121107	52.935623	69.879297
947.700363	55.800708	69.884302
946.344018	55.498176	69.889306
945.753432	61.204701	69.894311
945.147045	56.796965	69.899316
945.031117	44.917336	69.904321
943.553799	55.562443	69.909326
942.955006	49.159698	69.914330
942.451725	48.844088	69.919335
941.784455	56.914279	69.924340
941.886724	60.797759	69.929345
941.003316	63.358025	69.934350
940.192035	62.754130	69.939354
939.748756	58.248200	69.944359
938.191105	61.777315	69.949364
937.765528	49.135628	69.954369
936.965499	58.799130	69.959374
936.580807	56.190436	69.964378
936.238916	52.012915	69.969383
934.878013	59.875078	69.974388
934.166080	46.133418	69.979393
933.116503	59.562225	69.984398
932.796687	63.489575	69.989402
932.500992	63.636545	69.994407
932.398543	63.873570	69.999412
931.957240	57.611605	70.004417
930.969840	53.494905	70.009422
929.970189	50.478008	70.014426
929.238802	52.393718	70.019431
928.688593	62.619932	70.024436
928.086984	58.707933	70.029441
927.153521	59.684883	70.034446
926.623340	58.814174	70.039450
926.241637	59.439271	70.044455
925.642992	62.399561	70.049460
924.831091	58.494369	70.054465
923.676155	64.353207	70.059470
923.140423	68.045578	70.064474
922.560314	56.864753	70.069479
922.336647	58.515097	70.074484
921.875940	49.810405	70.079489
920.961481	55.208866	70.084494
920.529136	59.727431	70.089498
919.445047	53.760287	70.094503
918.045780	56.106158	70.099508
918.045617	49.176177	70.104513
917.417259	52.278521	70.109518
917.019417	53.637791	70.114522
916.655414	53.878957	70.119527
915.281581	62.479089	70.124532
914.742380	54.558326	70.129537
914.150724	56.406688	70.134542
913.622368	53.151585	70.139546
912.655621	62.491953	70.144551
911.427965	65.230782	70.149556
911.187684	54.642645	70.154561
910.254438	62.347494	70.159566
909.684914	58.295800	70.164570
909.362020	55.035900	70.169575
908.992474	61.928189	70.174580
908.978416	53.190025	70.179585
908.118464	57.161333	70.184590
906.881294	53.997237	70.189594
906.514202	57.179171	70.194599
905.422051	52.929636	70.199604
904.627039	49.974796	70.204609
903.931265	60.230282	70.209614
903.394459	53.805479	70.214618
903.492900	48.081047	70.219623
902.613825	57.241012	70.224628
901.753584	58.073985	70.229633
900.710025	65.728655	70.234638
900.472418	60.771868	70.239642
899.598335	50.557144	70.244647
898.679693	57.877406	70.249652
898.110989	51.833443	70.254657
897.398464	54.505360	70.259662
896.599550	52.124318	70.264666
896.490895	52.940665	70.269671
896.011294	60.972796	70.274676
894.934925	63.978596	70.279681
894.486518	62.261034	70.284686
893.580031	58.769133	70.289690
893.327664	57.598228	70.294695
891.818093	57.626281	70.299700
891.681165	59.350975	70.304705
890.943852	56.718211	70.309710
890.716767	55.799541	70.314714
889.862310	47.150850	70.319719
888.917940	58.918834	70.324724
888.390266	51.041496	70.329729
887.982738	57.756747	70.334734
887.435415	52.610260	70.339738
886.481561	51.802648	70.344743
885.491601	62.248251	70.349748
885.274568	55.767498	70.354753
884.374704	53.016926	70.359758
883.186970	57.936437	70.364762
882.647169	49.866977	70.369767
881.977087	49.734277	70.374772
881.796907	47.624611	70.379777
881.434100	54.855594	70.384782
881.159936	56.795230	70.389786
880.062146	58.829358	70.394791
879.000858	57.237296	70.399796
878.732520	54.379350	70.404801
878.043167	59.644925	70.409806
876.686642	63.713922	70.414810
876.459423	55.058056	70.419815
875.501658	61.713612	70.424820
875.339011	58.481923	70.429825
874.821690	60.330189	70.434830
873.764193	59.159430	70.439834
873.057508	58.682492	70.444839
872.306977	54.786142	70.449844
872.008520	54.439799	70.454849
871.528833	55.457847	70.459854
870.372123	62.029064	70.464858
869.627698	54.048728	70.469863
868.713723	62.576421	70.474868
868.409949	55.166367	70.479873
868.217592	56.881214	70.484878
867.409379	57.842643	70.489882
867.079925	51.438777	70.494887
865.948049	65.251933	70.499892
865.666471	50.777403	70.504897
864.597074	52.105260	70.509902
863.403061	54.665845	70.514906
863.179267	51.709881	70.519911
862.408597	63.502589	70.524916
862.278589	56.547089	70.529921
861.610286	51.339227	70.534926
860.449329	60.015007	70.539930
859.549498	54.265779	70.544935
858.844256	64.160541	70.549940
858.838982	51.618581	70.554945
858.385234	55.716889	70.559950
857.412886	54.516551	70.564954
856.564630	56.189012	70.569959
855.649899	60.411672	70.574964
855.678901	56.451275	70.579969
854.905696	45.254604	70.584974
853.977355	51.843543	70.589978
853.189692	45.424223	70.594983
852.587040	53.858327	70.599988
852.276800	53.793857	70.604993
851.627581	49.822926	70.609998
850.423578	57.028264	70.615002
850.174237	52.652147	70.620007
849.281119	57.891840	70.625012
848.796971	49.747332	70.630017
848.474957	64.714071	70.635022
847.419692	60.155880	70.640026
846.920564	50.413366	70.645031
846.247026	60.144414	70.650036
845.492219	55.333456	70.655041
844.713794	63.621631	70.660046
843.720821	54.596037	70.665050
843.024252	47.903366	70.670055
842.498118	56.084773	70.675060
842.319059	51.614519	70.680065
842.041674	52.891586	70.685070
841.066915	57.169526	70.690074
840.243254	51.143983	70.695079
839.433657	55.036811	70.700084
838.777213	48.808557	70.705089
837.904215	54.789632	70.710094
837.261624	52.766278	70.715098
836.898172	46.866372	70.720103
836.214751	66.317407	70.725108
835.818664	55.313098	70.730113
834.724364	52.642024	70.735118
834.027368	53.649931	70.740122
833.512949	51.763693	70.745127
833.009304	58.901965	70.750132
832.485434	48.248743	70.755137
831.623407	57.849848	70.760142
830.954760	58.808692	70.765146
830.608869	49.091642	70.770151
829.572553	57.662001	70.775156
828.861290	54.487973	70.780161
827.813369	54.990363	70.785166
827.124214	61.215857	70.790170
827.011985	52.063882	70.795175
826.510532	57.677387	70.800180
826.170775	49.863790	70.805185
824.952891	54.945571	70.810190
824.209076	48.341124	70.815194
824.047953	55.986746	70.820199
822.795850	63.133228	70.825204
821.955483	62.032257	70.830209
821.588752	55.193884	70.835214
820.539733	58.630383	70.840218
820.514918	57.516816	70.845223
819.897363	63.112318	70.850228
819.402347	58.843018	70.855233
818.737332	59.277059	70.860238
817.629239	64.144654	70.865242
817.212129	61.725067	70.870247
815.838680	63.571965	70.875252
815.318860	55.789999	70.880257
814.716077	61.315868	70.885262
814.225223	59.612297	70.890266
814.144362	63.527928	70.895271
813.411570	69.093042	70.900276
812.478734	64.472048	70.905281
811.829636	58.528312	70.910286
811.329173	59.327304	70.915290
810.652551	58.325780	70.920295
809.529679	59.516370	70.925300
808.725253	62.380478	70.930305
808.451346	54.283643	70.935310
808.108442	60.060245	70.940314
807.516769	61.340231	70.945319
806.378379	61.936670	70.950324
805.572310	59.266753	70.955329
804.887724	51.620377	70.960334
804.410860	61.503650	70.965338
804.248712	51.339889	70.970343
803.099007	60.826863	70.975348
802.390614	52.498944	70.980353
801.820073	57.026976	70.985358
801.147823	60.879310	70.990362
800.924015	57.259440	70.995367
799.791428	62.402404	71.000372
799.046009	53.962018	71.005377
798.803917	57.536206	71.010382
798.064753	67.460861	71.015386
797.495699	56.160547	71.020391
796.316061	64.727834	71.025396
795.631679	51.114905	71.030401
794.978435	54.521507	71.035406
794.478252	57.301529	71.040410
794.286028	48.637711	71.045415
793.078590	55.436300	71.050420
792.531371	52.907564	71.055425
791.901336	63.399675	71.060430
791.307323	58.974846	71.065434
790.889945	45.149223	71.070439
789.768763	54.825509	71.075444
788.923061	56.975544	71.080449
788.580544	55.223279	71.085454
788.078979	59.400436	71.090458
787.845571	49.115077	71.095463
786.698683	57.549653	71.100468
786.104480	57.541723	71.105473
786.158070	55.727527	71.110478
784.525249	54.994795	71.115482
783.756240	49.574870	71.120487
783.143933	57.464742	71.125492
782.899909	51.932785	71.130497
782.136178	55.741583	71.135502
781.099877	59.322350	71.140506
780.375752	54.293004	71.145511
779.994372	57.473838	71.150516
779.333905	50.595794	71.155521
778.925672	51.270839	71.160526
778.117203	55.964752	71.165530
777.495641	50.237350	71.170535
776.706365	56.669066	71.175540
776.444492	53.902384	71.180545
775.742576	56.273304	71.185550
774.318906	55.546982	71.190554
774.036063	57.932559	71.195559
773.322628	65.062958	71.200564
773.181503	58.402249	71.205569
772.439279	62.907985	71.210574
771.016592	64.269935	71.215578
770.684478	54.851306	71.220583
770.179214	59.721824	71.225588
769.731070	60.251740	71.230593
768.625561	55.069844	71.235598
767.713186	63.882258	71.240602
767.382978	68.796997	71.245607
766.458848	68.162729	71.250612
766.288090	64.021432	71.255617
766.187343	57.559849	71.260622
765.006472	65.251479	71.265626
764.476900	57.591580	71.270631
763.475965	63.079873	71.275636
762.890211	56.821366	71.280641
762.041656	51.905703	71.285646
760.695175	64.526880	71.290650
760.489501	56.593616	71.295655
759.876124	55.366936	71.300660
759.831486	53.738899	71.305665
759.456486	54.477328	71.310670
758.745737	53.603625	71.315674
757.733204	48.965908	71.320679
756.879530	58.277446	71.325684
756.388948	46.751745	71.330689
755.619036	50.445952	71.335694
755.161955	52.347852	71.340698
754.515377	52.634672	71.345703
753.751481	60.254872	71.350708
753.059284	54.630357	71.355713
751.672615	51.035625	71.360718
750.670684	57.418513	71.365722
750.664646	52.238533	71.370727
750.125555	58.985401	71.375732
749.922926	55.706100	71.380737
749.707039	53.777417	71.385742
748.457782	59.168520	71.390746
748.080961	52.568322	71.395751
747.421719	53.986987	71.400756
746.300087	51.246411	71.405761
745.459392	43.708895	71.410766
744.593369	46.888675	71.415770
744.036884	48.251845	71.420775
743.363652	52.311181	71.425780
743.873472	55.276590	71.430785
743.339261	51.765950	71.435790
741.931032	50.794638	71.440794
741.576339	45.431243	71.445799
739.666338	52.970290	71.450804
739.308483	57.470180	71.455809
738.775218	45.631287	71.460814
738.012533	54.815534	71.465818
738.079664	50.237198	71.470823
737.285224	59.045986	71.475828
736.670458	52.003420	71.480833
735.658926	52.472360	71.485838
734.886848	53.551165	71.490842
734.565856	47.649921	71.495847
733.655554	53.262024	71.500852
733.718742	46.212659	71.505857
732.479858	52.380364	71.510862
731.542901	52.557466	71.515866
731.372153	45.959075	71.520871
730.774078	53.544946	71.525876
729.515729	49.431294	71.530881
729.005392	43.186720	71.535886
728.211948	44.837970	71.540890
727.944295	44.584644	71.545895
727.185671	51.946979	71.550900
727.059680	49.914877	71.555905
726.128798	49.614913	71.560910
724.945976	57.607653	71.565914
724.487879	44.362938	71.570919
724.382968	56.229874	71.575924
723.197540	55.402363	71.580929
722.242559	45.650343	71.585934
721.793546	63.361568	71.590938
721.384471	57.069249	71.595943
720.661854	52.777380	71.600948
720.197108	54.367192	71.605953
719.480370	44.069520	71.610958
718.443406	45.748279	71.615962
718.462933	46.464516	71.620967
717.319997	58.026934	71.625972
716.512518	57.382955	71.630977
715.891512	49.852412	71.635982
714.853668	56.836292	71.640986
714.805678	49.609799	71.645991
713.968730	54.231630	71.650996
712.971032	50.257661	71.656001
712.677478	53.984342	71.661006
711.726270	62.645132	71.666010
712.037705	52.625241	71.671015
711.263279	48.491848	71.676020
710.164260	51.878908	71.681025
709.257215	57.165606	71.686030
708.364454	54.407146	71.691034
708.155892	46.602276	71.696039
707.052759	47.486365	71.701044
706.355247	47.619295	71.706049
705.781621	52.378373	71.711054
705.042539	56.567805	71.716058
705.071693	51.217992	71.721063
704.215952	53.185823	71.726068
704.054145	56.559558	71.731073
702.743192	50.262678	71.736078
702.121693	59.956002	71.741082
701.556957	46.201431	71.746087
700.598395	55.400684	71.751092
699.480752	47.466569	71.756097
699.002282	42.354898	71.761102
698.632716	57.407126	71.766106
698.545752	46.524359	71.771111
698.366075	56.077652	71.776116
697.261765	55.459661	71.781121
696.478236	52.835639	71.786126
695.814251	56.021078	71.791130
694.756363	50.938803	71.796135
693.829031	45.677463	71.801140
692.869494	48.214887	71.806145
692.820823	47.658800	71.811150
692.255096	58.605261	71.816154
692.082362	38.432976	71.821159
690.541526	45.879977	71.826164
689.997052	45.459747	71.831169
689.593412	49.374619	71.836174
689.202892	51.018818	71.841178
688.656197	41.508690	71.846183
687.354978	50.383771	71.851188
686.334506	42.713657	71.856193
686.179217	38.889443	71.861198
685.477516	40.830491	71.866202
685.313938	43.536669	71.871207
684.440564	50.416194	71.876212
683.405842	42.414989	71.881217
683.401371	42.182890	71.886222
682.618685	51.558448	71.891226
681.933992	43.669768	71.896231
680.893583	50.738953	71.901236
680.124763	50.538332	71.906241
680.023300	45.561012	71.911246
678.646248	48.839797	71.916250
678.297620	43.163153	71.921255
677.189420	57.793267	71.926260
677.097771	55.715812	71.931265
676.589269	44.186886	71.936270
675.594140	53.842775	71.941274
674.810454	47.904366	71.946279
673.953699	48.171944	71.951284
673.539372	42.930479	71.956289
673.097782	42.903128	71.961294
672.611786	47.134066	71.966298
671.945814	48.399954	71.971303
671.053524	46.981478	71.976308
670.071276	51.558341	71.981313
669.860895	54.617126	71.986318
669.112153	47.541085	71.991322
668.860635	45.161828	71.996327
667.669835	48.775002	72.001332
666.846942	52.935772	72.006337
666.450126	46.509926	72.011342
665.935048	51.261345	72.016346
665.249106	42.147293	72.021351
664.530728	46.812758	72.026356
663.883653	54.702274	72.031361
663.255779	54.482245	72.036366
662.181244	47.587145	72.041370
661.267017	39.609118	72.046375
660.672098	51.771559	72.051380
660.358863	49.434059	72.056385
659.644881	49.880457	72.061390
659.387099	50.663543	72.066394
659.083141	50.190270	72.071399
658.589617	51.013349	72.076404
657.916355	49.899174	72.081409
656.804216	43.439575	72.086414
654.984680	44.540354	72.091418
654.861780	52.130867	72.096423
654.698604	48.402735	72.101428
653.908392	51.044177	72.106433
653.660473	44.532827	72.111438
652.228505	50.623501	72.116442
651.899218	48.355853	72.121447
651.096082	57.576639	72.126452
650.787727	52.052561	72.131457
650.707695	43.004038	72.136462
649.148024	48.986729	72.141466
648.574794	39.439318	72.146471
647.731622	40.860297	72.151476
647.192434	57.066121	72.156481
646.449254	57.703434	72.161486
645.458691	53.463012	72.166490
645.087696	53.802889	72.171495
644.874221	53.959078	72.176500
643.712550	51.135788	72.181505
643.875707	48.824823	72.186510
642.861003	54.820330	72.191514
642.212091	55.162825	72.196519
641.387551	42.465622	72.201524
640.800697	46.283602	72.206529
640.149504	46.638329	72.211534
638.778445	48.779715	72.216538
638.828962	37.973666	72.221543
638.150142	44.993141	72.226548
637.722682	48.685924	72.231553
636.860837	43.514821	72.236558
635.973016	52.551968	72.241562
635.326052	48.132688	72.246567
634.651571	49.883169	72.251572
634.377375	44.567967	72.256577
634.261079	48.842930	72.261582
633.170781	43.433879	72.266586
632.017946	43.413525	72.271591
630.713631	51.176448	72.276596
630.219140	40.965454	72.281601
629.997174	47.986392	72.286606
629.621021	52.654014	72.291610
628.843767	40.010292	72.296615
628.721476	39.954291	72.301620
627.676665	43.234189	72.306625
626.755684	43.991172	72.311630
626.073812	56.106544	72.316634
625.379616	48.723947	72.321639
624.303725	45.919518	72.326644
623.189699	61.928191	72.331649
623.661789	52.902302	72.336654
622.474028	56.307347	72.341658
622.021864	53.767480	72.346663
621.365317	46.666181	72.351668
621.026453	48.067469	72.356673
621.092897	47.599417	72.361678
619.618527	50.988044	72.366682
619.073809	47.168583	72.371687
618.549421	48.231020	72.376692
617.436472	51.571540	72.381697
616.517419	46.516026	72.386702
615.459437	55.313529	72.391706
615.212305	51.470318	72.396711
615.183403	44.297011	72.401716
614.607867	44.439843	72.406721
614.432653	46.630940	72.411726
613.119256	48.258798	72.416730
612.605134	50.348102	72.421735
611.147222	47.631232	72.426740
610.145817	42.356948	72.431745
609.823078	45.636681	72.436750
609.308042	54.188801	72.441754
609.069405	44.638145	72.446759
608.471265	49.566420	72.451764
608.056965	54.321101	72.456769
607.309400	49.396066	72.461774
606.540479	53.689298	72.466778
605.512962	46.391445	72.471783
605.270441	50.609487	72.476788
604.437247	51.126841	72.481793
603.850907	42.057315	72.486798
602.688584	55.897804	72.491802
602.356350	51.565519	72.496807
602.197576	45.018378	72.501812
601.037137	50.396658	72.506817
600.210310	44.832349	72.511822
599.376789	45.077802	72.516826
599.042557	43.943837	72.521831
598.720249	51.582327	72.526836
597.558165	58.201085	72.531841
596.991275	46.695600	72.536846
596.190617	54.705770	72.541850
595.880512	49.487902	72.546855
595.491081	50.035799	72.551860
594.303205	53.258116	72.556865
593.432550	52.676691	72.561870
592.936212	53.701563	72.566874
592.620648	56.119987	72.571879
592.608083	59.075411	72.576884
591.386667	57.380597	72.581889
590.785000	42.029057	72.586894
589.723751	56.892697	72.591898
589.064529	47.278322	72.596903
588.180450	50.362541	72.601908
587.453019	50.010378	72.606913
586.833812	48.480792	72.611918
586.410998	56.811072	72.616922
586.448605	51.404557	72.621927
585.755733	54.064460	72.626932
584.318402	51.353940	72.631937
583.881894	44.203897	72.636942
583.250820	54.164504	72.641946
583.181975	50.714277	72.646951
582.527928	56.275783	72.651956
581.261999	51.020381	72.656961
580.714582	48.819323	72.661966
579.192352	63.925761	72.666970
578.632434	54.641717	72.671975
578.011192	49.330723	72.676980
577.636187	55.238343	72.681985
577.478564	37.339423	72.686990
577.040246	52.885362	72.691994
576.789662	46.880107	72.696999
575.069135	46.004195	72.702004
574.742727	51.484301	72.707009
574.366856	46.179817	72.712014
573.284033	53.145370	72.717018
572.737556	45.619852	72.722023
572.333628	54.390948	72.727028
571.199112	51.236991	72.732033
570.760445	50.623393	72.737038
569.513268	55.729585	72.742042
568.648813	48.830884	72.747047
567.929599	53.104157	72.752052
567.621805	51.209391	72.757057
567.948868	48.791004	72.762062
567.244277	49.551973	72.767066
566.328415	45.520603	72.772071
565.407192	54.279285	72.777076
564.604282	58.124821	72.782081
564.157400	51.021159	72.787086
563.584105	53.723335	72.792090
562.655106	54.200668	72.797095
561.883031	53.602752	72.802100
561.423614	52.004740	72.807105
561.418530	48.931199	72.812110
560.340206	52.652223	72.817114
559.065853	45.862046	72.822119
558.619800	40.255399	72.827124
558.394999	50.819773	72.832129
557.653694	48.619573	72.837134
556.532413	53.673803	72.842138
555.946190	53.347184	72.847143
555.636837	51.757406	72.852148
555.025524	49.602429	72.857153
554.340576	44.779171	72.862158
553.391367	48.959228	72.867162
552.190897	44.215619	72.872167
551.712375	48.626851	72.877172
551.325816	52.041068	72.882177
551.135984	49.320875	72.887182
550.740448	61.357191	72.892186
549.473398	46.819497	72.897191
548.828420	51.038607	72.902196
548.163435	59.065007	72.907201
548.155741	39.701273	72.912206
546.789333	49.130280	72.917210
546.451865	46.622478	72.922215
545.856921	52.811717	72.927220
544.889518	56.831089	72.932225
543.903863	53.969378	72.937230
543.455123	53.136468	72.942234
542.750732	44.100997	72.947239
542.546470	55.869680	72.952244
541.724447	62.321240	72.957249
541.299196	51.772755	72.962254
540.149226	59.323737	72.967258
539.808302	56.287609	72.972263
539.476888	60.052359	72.977268
538.227795	66.466578	72.982273
537.092907	44.448907	72.987278
536.584015	54.613171	72.992282
536.074541	41.723077	72.997287
535.631435	53.267040	73.002292
535.126366	52.664823	73.007297
534.680191	51.192038	73.012302
533.428502	50.666045	73.017306
532.683898	51.855824	73.022311
532.631485	52.215328	73.027316
531.745905	58.803692	73.032321
530.722070	52.535432	73.037326
529.666528	57.204609	73.042330
529.274278	53.569024	73.047335
528.834972	46.208297	73.052340
528.385774	48.697776	73.057345
528.449928	44.176798	73.062350
528.052966	58.287577	73.067354
527.105342	57.065705	73.072359
526.080516	56.194543	73.077364
524.692123	58.869032	73.082369
524.271634	53.537857	73.087374
523.363925	50.023358	73.092378
522.848344	52.226993	73.097383
522.205340	49.264734	73.102388
522.228474	66.089427	73.107393
521.295497	48.666766	73.112398
520.555714	60.138813	73.117402
519.929147	52.364540	73.122407
519.524433	58.491189	73.127412
518.274633	56.872702	73.132417
517.912168	54.572858	73.137422
516.699763	61.693252	73.142426
516.340771	55.260550	73.147431
516.090025	49.153098	73.152436
514.786391	56.369644	73.157441
513.999608	47.533022	73.162446
513.496655	52.171063	73.167450
512.850124	57.334204	73.172455
512.403839	54.185089	73.177460
512.072833	57.569660	73.182465
511.968804	50.846970	73.187470
510.754126	61.152307	73.192474
510.327471	59.111343	73.197479
509.795541	48.234588	73.202484
508.227122	63.165803	73.207489
507.464443	59.615008	73.212494
506.832645	54.215839	73.217498
506.598770	55.817025	73.222503
506.265443	52.452778	73.227508
505.783634	53.680420	73.232513
504.871741	47.332596	73.237518
504.059330	66.951754	73.242522
503.207336	53.870496	73.247527
502.647628	53.311986	73.252532
501.389195	53.551718	73.257537
500.704766	45.368182	73.262542
500.208555	49.324975	73.267546
499.885732	52.551836	73.272551
499.703503	50.926859	73.277556
498.917777	53.360328	73.282561
498.731806	50.660002	73.287566
497.454142	57.431206	73.292570
496.428113	53.344127	73.297575
496.584909	45.931784	73.302580
495.012709	53.114620	73.307585
493.999763	47.856948	73.312590
493.934430	47.412266	73.317594
493.186352	45.604399	73.322599
493.116640	44.727466	73.327604
492.235072	50.837540	73.332609
491.738625	45.389528	73.337614
490.547915	52.195170	73.342618
489.925513	54.013715	73.347623
489.923694	50.975140	73.352628
488.442345	48.764798	73.357633
487.692688	49.706780	73.362638
487.012685	48.069212	73.367642
486.794942	48.234428	73.372647
486.494784	51.046508	73.377652
485.718761	56.454065	73.382657
485.331675	51.408077	73.387662
484.143587	43.062577	73.392666
483.777137	52.688514	73.397671
483.057316	47.481662	73.402676
481.889701	49.256273	73.407681
481.107467	43.065440	73.412686
480.865620	56.154165	73.417690
480.119232	53.958401	73.422695
480.195956	48.837278	73.427700
478.871496	55.407305	73.432705
478.364394	48.173856	73.437710
477.803336	60.059725	73.442714
476.658935	55.622299	73.447719
476.091881	55.400162	73.452724
475.274378	56.754407	73.457729
475.009525	56.050642	73.462734
474.494338	60.441718	73.467738
473.557268	65.507030	73.472743
472.558871	49.474334	73.477748
471.974806	57.703174	73.482753
471.780658	48.163070	73.487758
470.851953	53.103794	73.492762
470.538111	55.650604	73.497767
469.573930	53.967794	73.502772
468.525792	56.163620	73.507777
468.167188	52.665558	73.512782
467.698832	51.493011	73.517786
467.241474	53.893503	73.522791
466.636997	57.583870	73.527796
465.324656	60.880436	73.532801
464.956682	47.019584	73.537806
464.502586	58.619507	73.542810
463.759014	57.080067	73.547815
463.064633	53.439820	73.552820
462.156072	56.672325	73.557825
461.706801	51.338198	73.562830
460.853074	55.167192	73.567834
460.334893	47.616716	73.572839
459.606237	46.627715	73.577844
458.491265	55.270804	73.582849
458.381756	56.741739	73.587854
457.763648	56.562299	73.592858
457.060388	55.812090	73.597863
457.004813	56.339890	73.602868
455.682164	55.933440	73.607873
455.749543	56.926852	73.612878
454.532322	54.808224	73.617882
452.991542	53.171335	73.622887
452.709395	47.889488	73.627892
452.072953	60.905710	73.632897
451.835424	54.824418	73.637902
451.566738	55.164540	73.642906
451.353695	53.414196	73.647911
450.044916	55.500752	73.652916
448.955329	48.896831	73.657921
448.666908	53.612579	73.662926
447.588834	51.093157	73.667930
446.639635	51.790672	73.672935
446.257732	47.693878	73.677940
445.650487	52.956864	73.682945
445.377280	54.059164	73.687950
444.514505	55.016984	73.692954
443.751140	53.567382	73.697959
442.960761	49.057853	73.702964
442.133348	43.180674	73.707969
442.111230	45.209361	73.712974
441.458279	51.342629	73.717978
440.780589	51.128404	73.722983
440.537434	41.392246	73.727988
439.367531	46.898879	73.732993
438.510561	40.872434	73.737998
437.244047	43.613684	73.743002
436.454952	50.369062	73.748007
436.927185	47.766328	73.753012
435.725656	57.071584	73.758017
435.181245	52.447277	73.763022
434.934297	50.075544	73.768026
434.121652	49.336190	73.773031
433.529281	43.045730	73.778036
432.398289	50.840957	73.783041
432.091930	50.343244	73.788046
431.738667	54.762228	73.793050
430.250214	43.186175	73.798055
430.059197	53.700940	73.803060
429.466766	48.484110	73.808065
429.110016	45.991466	73.813070
428.283017	52.110748	73.818074
427.107582	54.723111	73.823079
427.073696	46.969260	73.828084
425.951310	51.742666	73.833089
425.557622	47.266996	73.838094
424.217775	35.386028	73.843098
423.799405	53.702186	73.848103
423.585009	50.520844	73.853108
423.109106	50.686885	73.858113
422.213555	42.226936	73.863118
421.298937	49.658656	73.868122
420.761894	49.191793	73.873127
420.156607	37.010873	73.878132
418.991457	41.622669	73.883137
418.172563	42.756910	73.888142
417.641464	42.128775	73.893146
417.267597	54.046898	73.898151
417.190874	44.573518	73.903156
416.904655	53.096295	73.908161
416.054717	39.631458	73.913166
414.527735	51.955995	73.918170
413.978042	49.334191	73.923175
413.827976	57.069471	73.928180
412.357016	51.489283	73.933185
411.562087	45.097363	73.938190
411.163131	47.688364	73.943194
410.591768	51.105048	73.948199
410.852013	47.864471	73.953204
410.233182	53.528500	73.958209
409.334856	47.927148	73.963214
408.010995	54.878776	73.968218
407.181251	51.338706	73.973223
406.975656	48.820161	73.978228
405.545083	55.339313	73.983233
405.197448	45.852365	73.988238
404.760244	56.329983	73.993242
403.738662	57.885387	73.998247
403.887682	45.436651	74.003252
403.221226	48.006789	74.008257
402.843103	45.711221	74.013262
401.705471	53.109326	74.018266
400.967789	54.125843	74.023271
400.509654	50.580508	74.028276
399.205312	64.498648	74.033281
398.667347	51.081784	74.038286
398.091334	58.877431	74.043290
397.605359	53.379087	74.048295
397.165173	50.103819	74.053300
396.075296	56.797863	74.058305
395.265646	53.720114	74.063310
394.811670	60.751602	74.068314
393.784911	48.726196	74.073319
394.190053	41.333664	74.078324
393.369990	55.812581	74.083329
392.742442	50.858339	74.088334
391.963960	48.737956	74.093338
391.221059	48.734640	74.098343
390.502566	44.018999	74.103348
389.607886	44.445486	74.108353
389.311174	46.780559	74.113358
388.199140	49.236809	74.118362
387.620971	51.520651	74.123367
386.919776	55.611261	74.128372
385.534281	61.496680	74.133377
385.398693	49.738918	74.138382
384.918849	52.983219	74.143386
384.512188	43.905842	74.148391
384.531039	41.175159	74.153396
383.044877	48.245782	74.158401
382.573189	41.069439	74.163406
381.791159	49.048011	74.168410
381.318520	50.219227	74.173415
380.427413	37.919154	74.178420
379.394449	46.018884	74.183425
379.039521	43.809732	74.188430
378.762711	55.663066	74.193434
377.833320	53.235410	74.198439
377.537430	46.330103	74.203444
376.390122	54.191291	74.208449
375.908125	47.252356	74.213454
375.594438	47.254031	74.218458
374.298031	55.205111	74.223463
373.571780	45.978834	74.228468
372.921512	55.815243	74.233473
372.555314	54.971362	74.238478
372.407334	47.078000	74.243482
371.183118	51.780453	74.248487
370.048252	51.284612	74.253492
369.573074	60.204096	74.258497
369.321941	55.325864	74.263502
369.128062	45.716261	74.268506
368.043268	60.380281	74.273511
367.144131	44.941241	74.278516
366.415190	55.565166	74.283521
366.085052	58.528039	74.288526
365.356421	49.267435	74.293530
364.116525	44.097245	74.298535
363.690964	49.926299	74.303540
363.160100	53.043565	74.308545
362.974543	54.108348	74.313550
362.083755	46.924495	74.318554
361.363856	57.200313	74.323559
360.824106	43.137626	74.328564
359.535887	57.465872	74.333569
359.230769	56.563764	74.338574
359.091935	55.214367	74.343578
357.670772	59.781246	74.348583
356.998219	54.200813	74.353588
356.260666	52.577076	74.358593
355.928735	51.546546	74.363598
355.669210	57.967637	74.368602
354.770516	57.844193	74.373607
353.682568	57.037964	74.378612
353.350380	55.761177	74.383617
352.731094	52.951582	74.388622
352.384137	51.105387	74.393626
351.693643	52.196319	74.398631
350.867490	47.632945	74.403636
349.993053	48.989072	74.408641
349.567157	53.131181	74.413646
348.947050	49.499935	74.418650
348.010692	59.633654	74.423655
347.145356	45.776761	74.428660
346.614083	56.651398	74.433665
346.144041	53.228892	74.438670
345.740976	47.185460	74.443674
344.657924	54.293185	74.448679
343.941117	43.301325	74.453684
343.299392	47.259384	74.458689
342.873551	50.218922	74.463694
342.308312	45.655041	74.468698
341.211626	52.909962	74.473703
340.784377	49.988120	74.478708
339.726819	55.261981	74.483713
339.841814	55.935801	74.488718
339.261247	53.107337	74.493722
338.056171	57.885460	74.498727
337.492254	42.677122	74.503732
336.471393	55.445822	74.508737
336.180226	49.034285	74.513742
335.876684	55.756191	74.518746
334.943419	59.384112	74.523751
334.348358	53.988548	74.528756
333.771598	54.405949	74.533761
333.012848	57.286765	74.538766
332.114667	55.439920	74.543770
331.338438	59.620761	74.548775
330.983755	49.807419	74.553780
330.510801	47.169711	74.558785
329.292635	48.764743	74.563790
328.388456	45.603349	74.568794
327.612698	48.293670	74.573799
327.030629	45.716899	74.578804
327.098838	51.955508	74.583809
326.269717	46.129171	74.588814
326.378568	52.407785	74.593818
325.380482	55.798937	74.598823
324.699627	53.357510	74.603828
324.081888	57.345013	74.608833
323.375213	61.457884	74.613838
322.311364	56.525936	74.618842
321.752474	53.355490	74.623847
321.055748	52.999291	74.628852
319.489194	54.965465	74.633857
319.010621	56.076919	74.638862
318.816213	55.699359	74.643866
318.031797	56.971778	74.648871
317.917161	57.034861	74.653876
316.950225	53.738180	74.658881
316.756333	51.782074	74.663886
316.370455	52.535029	74.668890
315.265994	58.016264	74.673895
314.498335	57.508812	74.678900
313.751482	60.620868	74.683905
312.504143	52.681869	74.688910
312.133432	49.402203	74.693914
311.497587	55.055341	74.698919
311.015234	51.657450	74.703924
310.684656	49.668723	74.708929
310.028262	52.451082	74.713934
309.280009	47.284665	74.718938
308.268289	54.313857	74.723943
308.216984	42.666791	74.728948
308.052432	49.700378	74.733953
306.570740	46.166289	74.738958
305.695303	52.261126	74.743962
305.045579	56.355948	74.748967
304.135688	47.760337	74.753972
303.035591	50.115881	74.758977
302.549272	54.366633	74.763982
302.447157	44.460671	74.768986
301.761430	52.583789	74.773991
301.127369	45.003867	74.778996
300.744192	47.972278	74.784001
299.961702	41.153543	74.789006
299.482950	54.328641	74.794010
298.385340	56.329308	74.799015
298.192185	46.067525	74.804020
297.516157	52.518161	74.809025
296.667126	47.069432	74.814030
295.541654	41.094964	74.819034
294.906137	45.862703	74.824039
294.652180	47.674167	74.829044
294.453118	51.181382	74.834049
293.128874	46.065538	74.839054
292.586482	38.254790	74.844058
291.915117	47.458141	74.849063
291.432069	43.591060	74.854068
290.917652	44.419729	74.859073
289.763515	44.553620	74.864078
289.240148	49.163199	74.869082
288.557454	48.438702	74.874087
288.161633	45.581345	74.879092
287.122035	44.819737	74.884097
286.210524	55.023800	74.889102
285.816228	41.841281	74.894106
285.108166	51.980473	74.899111
284.996810	48.231252	74.904116
284.437149	53.628980	74.909121
283.554091	48.657373	74.914126
283.217829	47.821001	74.919130
281.983434	54.771134	74.924135
281.417136	40.400803	74.929140
280.458162	48.609436	74.934145
279.495138	51.250157	74.939150
278.953963	49.842233	74.944154
278.340918	53.858143	74.949159
278.335687	45.569295	74.954164
278.046442	48.426877	74.959169
276.932680	43.501527	74.964174
276.210362	42.569099	74.969178
275.431456	54.228238	74.974183
274.990657	44.167976	74.979188
274.084577	56.504928	74.984193
273.232573	51.724568	74.989198
273.471429	52.029018	74.994202
272.214165	52.026257	74.999207
271.663252	52.573833	75.004212
270.821492	48.971909	75.009217
270.463077	48.852976	75.014222
269.323355	48.365097	75.019226
268.180826	49.574571	75.024231
267.927155	40.102332	75.029236
267.061211	50.874470	75.034241
266.764853	53.628278	75.039246
266.782842	42.241693	75.044250
265.608558	51.648480	75.049255
264.897096	43.480291	75.054260
264.171575	59.025704	75.059265
263.918366	49.826523	75.064270
263.318665	44.772803	75.069274
261.799781	55.658440	75.074279
261.481374	53.174635	75.079284
260.821291	49.154360	75.084289
260.284142	54.725852	75.089294
259.954059	40.905923	75.094298
258.424710	54.699624	75.099303
258.127085	46.080787	75.104308
257.412084	51.183451	75.109313
257.168411	51.769939	75.114318
256.490041	57.034868	75.119322
255.020886	56.182301	75.124327
254.727407	48.669133	75.129332
254.097969	42.846087	75.134337
253.525048	49.557718	75.139342
253.238176	52.088861	75.144346
252.553607	56.823965	75.149351
251.537834	49.639065	75.154356
250.737289	53.350821	75.159361
250.233737	51.692520	75.164366
250.100769	49.445335	75.169370
249.337885	60.262179	75.174375
248.447320	46.405696	75.179380
247.702930	48.297673	75.184385
246.861904	54.988556	75.189390
246.595864	50.190653	75.194394
245.516308	51.805760	75.199399
244.818949	50.142392	75.204404
244.137475	47.673062	75.209409
243.590303	54.555929	75.214414
243.167063	51.214622	75.219418
242.444300	50.044263	75.224423
241.686638	56.368380	75.229428
241.106120	51.395053	75.234433
240.386948	47.365175	75.239438
240.460400	47.049068	75.244442
239.058055	58.886124	75.249447
238.282401	48.706827	75.254452
237.708145	57.359889	75.259457
237.348199	55.653291	75.264462
236.926757	45.280658	75.269466
235.627448	59.342021	75.274471
234.837695	54.670596	75.279476
234.105694	57.767485	75.284481
233.641909	55.910538	75.289486
233.422265	50.773519	75.294490
232.134313	57.128143	75.299495
231.503690	51.942762	75.304500
230.970775	54.121763	75.309505
230.472156	48.283795	75.314510
229.987053	50.035020	75.319514
229.607325	55.230998	75.324519
228.790648	52.103571	75.329524
227.704153	57.503194	75.334529
227.333526	52.446131	75.339534
226.949800	47.671166	75.344538
225.491969	56.819874	75.349543
225.030074	47.484771	75.354548
224.573661	52.937826	75.359553
224.147609	52.003567	75.364558
223.835690	47.492593	75.369562
222.530181	60.190501	75.374567
222.086675	55.238688	75.379572
221.628755	55.770329	75.384577
220.483062	53.106644	75.389582
219.349865	49.642315	75.394586
218.289079	54.985035	75.399591
218.091818	53.168846	75.404596
218.035121	49.577223	75.409601
217.489697	51.367998	75.414606
217.165561	52.718234	75.419610
216.460681	49.312715	75.424615
215.514598	43.498166	75.429620
214.668933	50.236028	75.434625
214.390233	56.036756	75.439630
213.388041	40.318223	75.444634
212.235469	47.999164	75.449639
212.050532	45.961798	75.454644
211.468116	44.817517	75.459649
211.216381	50.982283	75.464654
209.965154	45.719353	75.469658
208.980441	51.825038	75.474663
208.733432	46.184325	75.479668
208.468335	53.196856	75.484673
207.018136	55.825579	75.489678
206.540011	49.187966	75.494682
205.611815	51.310787	75.499687
205.271937	49.125123	75.504692
205.054325	48.821016	75.509697
204.586341	49.115977	75.514702
203.756977	45.023685	75.519706
202.620849	56.589337	75.524711
202.430747	49.885773	75.529716
201.186436	46.747188	75.534721
200.201658	45.650961	75.539726
200.150252	45.917537	75.544730
199.296630	49.109087	75.549735
198.776426	44.364627	75.554740
198.703462	44.906066	75.559745
197.880330	50.656443	75.564750
196.944303	50.605742	75.569754
196.219638	46.996394	75.574759
195.524972	52.456346	75.579764
194.255318	47.064746	75.584769
193.431232	49.802841	75.589774
193.298356	49.568283	75.594778
192.883547	57.048558	75.599783
192.193855	43.128454	75.604788
191.922760	48.042141	75.609793
191.723018	47.143692	75.614798
190.429112	35.408885	75.619802
189.689560	48.946028	75.624807
189.059439	49.485482	75.629812
187.981212	44.175537	75.634817
187.223430	47.189618	75.639822
186.826201	47.455873	75.644826
186.482747	52.188162	75.649831
185.892660	37.623003	75.654836
184.866201	53.314333	75.659841
183.894094	45.504245	75.664846
183.631446	48.381348	75.669850
182.853434	52.734605	75.674855
182.310579	46.952383	75.679860
182.040759	52.363585	75.684865
180.403932	51.424924	75.689870
179.629636	46.161164	75.694874
179.243012	56.199475	75.699879
179.497202	54.239193	75.704884
178.775267	50.773450	75.709889
177.754550	56.705324	75.714894
177.200117	44.279708	75.719898
176.792943	47.944959	75.724903
176.004290	54.679369	75.729908
174.529878	52.240195	75.734913
173.773654	51.698835	75.739918
173.659746	41.344547	75.744922
172.897819	47.526907	75.749927
172.773416	42.173846	75.754932
172.257070	48.700530	75.759937
171.086491	45.758513	75.764942
170.644888	47.743060	75.769946
170.341196	48.229716	75.774951
169.513502	43.138524	75.779956
168.496025	40.876008	75.784961
167.842446	53.668595	75.789966
167.221028	42.746479	75.794970
166.043432	44.876536	75.799975
165.969333	52.127886	75.804980
165.238467	44.163561	75.809985
164.310287	47.558150	75.814990
163.886258	44.585256	75.819994
162.786334	50.262304	75.824999
162.037155	36.720285	75.830004
161.605540	49.577444	75.835009
160.720310	52.050122	75.840014
160.694019	51.795319	75.845018
160.285049	51.508230	75.850023
159.494519	43.885299	75.855028
159.193709	45.484944	75.860033
157.849449	43.883544	75.865038
156.876570	45.329602	75.870042
155.820128	50.758818	75.875047
155.225056	38.937773	75.880052
155.048638	45.727479	75.885057
154.616862	52.280324	75.890062
154.428923	39.495855	75.895066
153.804485	48.612226	75.900071
152.603727	39.324862	75.905076
151.839314	46.048010	75.910081
151.145995	47.811254	75.915086
151.465518	50.996294	75.920090
150.155337	52.353738	75.925095
149.298661	49.483433	75.930100
148.819527	45.898710	75.935105
147.514273	47.355567	75.940110
146.893608	40.373742	75.945114
146.335284	45.376140	75.950119
145.791623	43.714861	75.955124
145.462520	41.890887	75.960129
144.384330	51.363318	75.965134
144.221030	40.857249	75.970138
143.040314	45.547159	75.975143
142.128150	41.684984	75.980148
141.973970	47.981830	75.985153
141.466800	57.091918	75.990158
141.349743	49.459317	75.995162
140.156950	48.433497	76.000167
139.572209	56.467082	76.005172
138.876367	50.425716	76.010177
138.186118	58.836972	76.015182
137.385060	44.558236	76.020186
136.660712	47.738686	76.025191
135.952259	43.031245	76.030196
135.480731	43.687587	76.035201
135.130574	54.239085	76.040206
133.841223	41.212806	76.045210
133.223219	48.867245	76.050215
132.451636	41.256073	76.055220
132.033881	38.672084	76.060225
131.539520	54.063395	76.065230
130.981136	39.677146	76.070234
129.972567	47.341307	76.075239
129.197400	45.343162	76.080244
128.636066	36.079209	76.085249
128.660593	44.907493	76.090254
127.595456	40.368564	76.095258
126.352434	55.163926	76.100263
126.067796	55.748364	76.105268
125.615220	53.696100	76.110273
124.886579	42.779351	76.115278
124.566804	44.675520	76.120282
123.493678	45.226590	76.125287
122.634076	49.714228	76.130292
122.223001	42.975538	76.135297
121.459123	44.119342	76.140302
120.594646	45.911142	76.145306
120.089193	48.346349	76.150311
119.426272	46.075952	76.155316
119.495270	43.776784	76.160321
118.403974	52.032594	76.165326
117.537419	42.250212	76.170330
116.842730	50.304617	76.175335
116.429067	42.699978	76.180340
115.729248	41.383217	76.185345
114.367029	47.790855	76.190350
113.907727	43.633563	76.195354
113.589049	54.956457	76.200359
113.105782	50.892476	76.205364
112.386998	43.233969	76.210369
111.649401	44.850081	76.215374
111.235122	40.441139	76.220378
109.928114	39.696209	76.225383
109.705641	44.052910	76.230388
109.258530	38.593348	76.235393
108.146042	52.933332	76.240398
107.453873	48.569661	76.245402
106.553152	48.970002	76.250407
106.271966	53.828188	76.255412
106.222990	53.501491	76.260417
105.359090	56.135511	76.265422
104.473809	53.191177	76.270426
103.702051	51.008910	76.275431
103.020585	55.136823	76.280436
102.716789	49.868596	76.285441
101.435439	48.325897	76.290446
100.818986	42.744982	76.295450
100.329547	48.408558	76.300455
100.010419	47.949371	76.305460
99.086960	35.583890	76.310465
98.018778	48.115205	76.315470
97.362136	34.856535	76.320474
96.840972	41.166559	76.325479
96.532430	50.799923	76.330484
96.237181	48.625960	76.335489
95.739681	53.541757	76.340494
94.688983	46.984170	76.345498
93.802750	44.281961	76.350503
92.928791	45.426090	76.355508
92.107637	43.005995	76.360513
91.267796	42.466355	76.365518
90.522835	38.230154	76.370522
90.284703	52.410370	76.375527
89.851081	43.254387	76.380532
89.534589	43.477205	76.385537
89.006759	48.706076	76.390542
88.085612	43.183321	76.395546
87.079930	47.170251	76.400551
86.707025	38.332657	76.405556
86.443576	39.440404	76.410561
85.304281	49.427759	76.415566
84.548572	48.056642	76.420570
83.839120	40.859541	76.425575
83.244259	45.283243	76.430580
82.215072	46.468591	76.435585
81.336197	54.026848	76.440590
81.072689	47.224971	76.445594
80.477444	42.950473	76.450599
80.043121	43.387692	76.455604
80.061012	43.188470	76.460609
79.015873	49.022708	76.465614
78.224100	41.125293	76.470618
77.235491	38.399590	76.475623
76.251842	43.228611	76.480628
75.305953	36.680695	76.485633
74.361246	41.007676	76.490638
74.162827	42.155588	76.495642
74.023043	43.873674	76.500647
73.514191	37.564231	76.505652
73.287936	40.993218	76.510657
72.374889	47.038874	76.515662
71.555800	42.601057	76.520666
71.057415	47.201235	76.525671
70.107551	50.565217	76.530676
69.033612	43.086024	76.535681
68.622660	47.251633	76.540686
68.456117	40.810876	76.545690
67.713356	39.319129	76.550695
66.495956	40.614507	76.555700
66.410465	46.281849	76.560705
65.516487	53.932296	76.565710
65.389609	46.520455	76.570714
63.904473	42.048420	76.575719
63.133872	47.840328	76.580724
62.851452	44.420826	76.585729
62.189889	47.635518	76.590734
61.335380	43.744137	76.595738
60.040017	41.305884	76.600743
59.532799	36.750263	76.605748
59.107514	46.322723	76.610753
58.156331	47.618642	76.615758
58.119216	39.754863	76.620762
57.966274	42.843276	76.625767
57.234454	48.395656	76.630772
56.777106	45.515719	76.635777
55.594038	58.514346	76.640782
55.168652	49.830608	76.645786
53.516162	51.368339	76.650791
52.669471	48.354641	76.655796
52.645688	46.406885	76.660801
51.862857	51.259900	76.665806
51.604361	43.501176	76.670810
51.116380	47.645258	76.675815
50.699726	46.414951	76.680820
49.519850	41.022219	76.685825
48.610917	47.752787	76.690830
48.309693	47.066338	76.695834
48.033210	43.980141	76.700839
46.735293	39.955984	76.705844
46.222989	43.325469	76.710849
45.316526	47.782075	76.715854
45.081632	46.252202	76.720858
44.667905	50.380791	76.725863
43.230504	44.984452	76.730868
42.870660	50.305306	76.735873
42.335604	51.478175	76.740878
41.901636	46.074391	76.745882
41.318347	40.392282	76.750887
40.206974	48.252096	76.755892
39.975649	43.726932	76.760897
38.961389	49.920597	76.765902
38.422309	39.746588	76.770906
37.208494	49.059928	76.775911
36.381228	38.520093	76.780916
36.255834	41.389849	76.785921
35.676853	58.043350	76.790926
35.240747	46.134290	76.795930
34.724025	41.030468	76.800935
33.478575	47.852681	76.805940
33.067875	45.835484	76.810945
32.011943	48.588092	76.815950
32.142586	42.543987	76.820954
30.831697	49.065204	76.825959
29.798852	52.421711	76.830964
29.349372	48.303007	76.835969
28.909176	52.867161	76.840974
28.601709	45.192621	76.845978
28.098628	42.837602	76.850983
27.239455	38.099978	76.855988
26.362791	38.243988	76.860993
25.776614	43.905996	76.865998
25.542799	41.741242	76.871002
24.624342	44.672373	76.876007
23.200721	42.998180	76.881012
22.771172	36.418982	76.886017
22.223486	50.094537	76.891022
22.059450	38.002662	76.896026
21.599731	43.181964	76.901031
20.529956	37.862727	76.906036
19.891593	37.566037	76.911041
19.002371	46.222974	76.916046
18.987716	45.989861	76.921050
17.833010	45.879986	76.926055
17.000427	48.183407	76.931060
16.809641	40.750954	76.936065
16.055509	55.063055	76.941070
15.215222	43.264352	76.946074
14.051200	41.610779	76.951079
13.607323	46.684347	76.956084
13.168318	50.465189	76.961089
12.326387	46.304836	76.966094
12.349152	43.675722	76.971098
11.286031	42.777695	76.976103
10.229824	39.581656	76.981108
9.780412	37.841083	76.986113
9.613955	47.695985	76.991118
9.115751	32.910272	76.996122
7.619005	38.596176	77.001127
6.914013	41.460710	77.006132
7.098273	39.682536	77.011137
5.972782	48.603787	77.016142
5.249507	41.861413	77.021147
4.294760	45.322552	77.026151
3.516403	49.652601	77.031156
3.216512	35.373245	77.036161