Tue Jun 08 17:14:41 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-0.324335	107.415111	0.000000
-0.966174	101.554742	0.005005
-1.358794	61.491232	0.010010
-2.775706	12.881126	0.015014
-7.400151	-7.148114	0.020019
-12.723909	-6.046197	0.025024
-18.067692	7.228879	0.030029
-22.520622	-10.206499	0.035034
-26.826209	-1.688471	0.040038
-30.103618	-7.739858	0.045043
-33.679311	-6.774246	0.050048
-37.632327	-8.557032	0.055053
-40.934659	-12.722156	0.060058
-44.516938	-0.636809	0.065062
-48.516155	-1.533828	0.070067
-52.045500	-3.762251	0.075072
-56.240446	2.512638	0.080077
-59.865916	0.785408	0.085082
-63.691494	0.559633	0.090086
-67.451165	-0.931435	0.095091
-71.073663	-3.121766	0.100096
-75.387399	-2.674125	0.105101
-78.571141	-12.039338	0.110106
-82.567592	-5.841885	0.115110
-86.256758	-7.872754	0.120115
-89.795754	-14.795751	0.125120
-93.833960	3.196103	0.130125
-97.318010	-1.580803	0.135130
-101.181634	-4.365638	0.140134
-105.131653	-3.375645	0.145139
-108.484520	-10.002147	0.150144
-112.941515	3.086612	0.155149
-116.468645	-7.856551	0.160154
-120.304926	-0.359912	0.165158
-123.832463	1.228654	0.170163
-127.395477	-15.664121	0.175168
-131.515505	-1.520055	0.180173
-135.033069	-17.253851	0.185178
-139.198711	-4.778687	0.190182
-143.405567	-5.722112	0.195187
-146.710885	-4.041778	0.200192
-150.524178	5.975904	0.205197
-153.918377	-5.332238	0.210202
-157.701978	-5.335015	0.215206
-161.793087	-3.184407	0.220211
-165.424751	-9.750419	0.225216
-169.240652	-0.111201	0.230221
-172.746548	-5.306242	0.235226
-176.425452	-6.505563	0.240230
-180.195171	-9.347481	0.245235
-183.753271	-13.343506	0.250240
-188.406376	0.972944	0.255245
-191.784109	-15.583280	0.260250
-195.665417	-10.746312	0.265254
-198.837363	-6.757266	0.270259
-202.371090	-4.378159	0.275264
-206.836878	3.808314	0.280269
-210.586854	-1.855983	0.285274
-214.342515	-6.620152	0.290278
-218.114290	-5.080409	0.295283
-221.868432	-1.977083	0.300288
-225.462590	0.546607	0.305293
-229.096178	-10.169786	0.310298
-232.932891	-7.156100	0.315302
-236.778163	-7.199151	0.320307
-240.406686	-13.709191	0.325312
-244.781566	-3.246202	0.330317
-247.841497	-11.657976	0.335322
-251.354909	-11.975814	0.340326
-255.466508	-8.329212	0.345331
-259.416381	-10.162467	0.350336
-263.133807	-6.459923	0.355341
-266.924088	-13.788057	0.360346
-270.866954	-9.043883	0.365350
-274.282322	-3.198950	0.370355
-277.830039	-13.718066	0.375360
-282.112838	-10.037735	0.380365
-285.894379	-9.179502	0.385370
-289.823349	-13.152480	0.390374
-293.323751	-6.608524	0.395379
-297.174808	-12.290531	0.400384
-300.689456	-2.958661	0.405389
-304.347153	-8.289383	0.410394
-308.133447	-13.552650	0.415398
-312.172656	-7.837510	0.420403
-315.834752	-6.607794	0.425408
-319.347963	-7.343610	0.430413
-323.107357	-8.893319	0.435418
-327.011593	-1.880225	0.440422
-331.177537	8.540297	0.445427
-334.513047	-9.505177	0.450432
-338.319892	-10.904637	0.455437
-341.596647	-7.783640	0.460442
-345.791208	-13.883091	0.465446
-349.675076	-6.252598	0.470451
-353.248056	-16.227347	0.475456
-357.681882	-5.250502	0.480461
-361.448769	-10.464554	0.485466
-364.660511	-9.595455	0.490470
-368.825551	-5.538956	0.495475
-372.092352	-5.420617	0.500480
-375.941316	-0.219995	0.505485
-379.423801	-10.947960	0.510490
-383.328001	-6.824492	0.515494
-387.319287	-3.255251	0.520499
-390.954955	-7.494359	0.525504
-394.649210	-3.704902	0.530509
-398.842613	-5.416917	0.535514
-402.398851	-10.422744	0.540518
-406.466460	-3.344853	0.545523
-409.733230	-11.441564	0.550528
-413.870470	-4.369878	0.555533
-417.332219	-12.417739	0.560538
-421.196726	-3.841631	0.565542
-425.086382	4.306593	0.570547
-428.323829	-5.494753	0.575552
-432.460553	-11.298930	0.580557
-436.073864	-11.836309	0.585562
-439.798633	-14.322184	0.590566
-443.817342	-13.197752	0.595571
-447.267011	-10.821828	0.600576
-451.784769	-6.655010	0.605581
-454.940281	-3.405532	0.610586
-458.696886	-3.987383	0.615590
-462.574727	-0.295445	0.620595
-466.075222	-9.143402	0.625600
-470.178474	-11.232368	0.630605
-474.057346	-16.759052	0.635610
-477.632452	-7.391825	0.640614
-481.193094	-6.409102	0.645619
-485.048441	-12.378730	0.650624
-488.522035	-3.143769	0.655629
-492.427221	-12.241193	0.660634
-496.209598	-14.355188	0.665638
-500.259481	-7.722729	0.670643
-503.686509	-15.228615	0.675648
-507.524327	-10.248865	0.680653
-511.258341	-13.585662	0.685658
-514.856507	-9.286057	0.690662
-519.013361	-17.145095	0.695667
-522.522446	-21.421196	0.700672
-526.826301	-3.942373	0.705677
-530.240361	-7.604032	0.710682
-534.094157	-4.644792	0.715686
-537.925520	0.543863	0.720691
-541.436367	-10.044494	0.725696
-545.196034	-2.112283	0.730701
-548.740678	-11.393875	0.735706
-553.036708	-13.060501	0.740710
-556.655029	-9.759174	0.745715
-560.442362	-12.076721	0.750720
-564.034704	-0.644122	0.755725
-567.686694	-2.801743	0.760730
-571.575790	-0.291117	0.765734
-575.451547	-0.296673	0.770739
-579.235725	-11.541858	0.775744
-582.837549	-10.355423	0.780749
-586.534929	-8.565658	0.785754
-590.187436	-5.048848	0.790758
-594.495533	-4.706273	0.795763
-597.792458	-14.899077	0.800768
-601.701894	-3.180348	0.805773
-605.596874	-10.990691	0.810778
-609.723214	-4.230553	0.815782
-613.629561	-3.793489	0.820787
-616.639880	-18.053977	0.825792
-620.482273	-14.370754	0.830797
-624.306400	-14.932586	0.835802
-627.839795	-20.534591	0.840806
-631.800107	-13.332437	0.845811
-635.646157	-16.668053	0.850816
-639.412460	-5.067800	0.855821
-642.928909	-6.183693	0.860826
-646.760503	-1.358042	0.865830
-650.671228	-3.829980	0.870835
-654.319523	-5.222033	0.875840
-658.190045	-4.521492	0.880845
-661.760201	-4.396271	0.885850
-665.867817	-3.173493	0.890854
-669.587558	-0.469625	0.895859
-673.169142	-8.825491	0.900864
-676.786473	-5.019802	0.905869
-680.668973	-14.418541	0.910874
-684.085200	-10.376196	0.915878
-688.492246	-6.088024	0.920883
-692.307738	-9.405941	0.925888
-695.639232	-14.390088	0.930893
-698.951172	-17.636138	0.935898
-703.052825	-13.538907	0.940902
-707.129521	-3.715985	0.945907
-710.858937	-16.225604	0.950912
-714.785505	-12.520751	0.955917
-718.393180	-11.456351	0.960922
-722.476336	-14.567262	0.965926
-725.976877	-8.752784	0.970931
-729.576943	-14.385495	0.975936
-733.234148	-6.047995	0.980941
-736.970271	-19.950540	0.985946
-740.383635	-19.142875	0.990950
-744.844501	-3.140765	0.995955
-748.359180	-18.251613	1.000960
-752.409235	-3.110997	1.005965
-755.880104	-9.095046	1.010970
-759.534821	-5.569827	1.015974
-763.644436	-4.694747	1.020979
-766.962177	-13.053969	1.025984
-771.017521	-2.292099	1.030989
-774.820556	-2.812421	1.035994
-778.577511	-4.463197	1.040998
-782.598957	-9.240439	1.046003
-786.015752	-6.284943	1.051008
-789.568495	1.883895	1.056013
-793.288569	-3.809079	1.061018
-797.395180	-5.907022	1.066022
-801.520102	-10.076397	1.071027
-805.062532	-10.337499	1.076032
-808.541030	-0.230750	1.081037
-812.368508	2.831571	1.086042
-816.018253	-7.907942	1.091046
-820.059228	0.739822	1.096051
-823.319349	-2.043746	1.101056
-827.847821	-0.430445	1.106061
-831.196387	-4.452415	1.111066
-834.293121	-6.463158	1.116070
-838.946246	-6.464114	1.121075
-842.524345	-4.705268	1.126080
-846.367257	0.932431	1.131085
-849.756135	-8.697310	1.136090
-853.465656	-3.479578	1.141094
-857.495910	2.732221	1.146099
-861.142101	-6.789005	1.151104
-864.819004	-5.350260	1.156109
-868.549401	-8.148190	1.161114
-872.204613	-3.632476	1.166118
-876.580185	3.199100	1.171123
-880.367281	-11.441737	1.176128
-884.034149	0.612122	1.181133
-887.475385	-2.131622	1.186138
-890.705558	-6.223204	1.191142
-895.111964	-1.961780	1.196147
-898.911227	-7.085710	1.201152
-902.754061	-7.236746	1.206157
-906.815344	-7.639599	1.211162
-910.130090	-4.412996	1.216166
-913.914398	-5.228493	1.221171
-917.230611	-9.122139	1.226176
-921.375869	-5.049984	1.231181
-925.188945	-5.215581	1.236186
-928.845043	-5.432991	1.241190
-933.076973	1.696454	1.246195
-936.484613	-9.630384	1.251200
-940.424870	-6.113627	1.256205
-943.966623	-8.008025	1.261210
-947.594099	-5.411734	1.266214
-951.646037	-3.655131	1.271219
-955.356293	-13.620360	1.276224
-958.865196	0.175508	1.281229
-962.797552	-3.013160	1.286234
-966.245825	-8.540283	1.291238
-970.330004	-0.876083	1.296243
-973.836031	-7.837120	1.301248
-977.932196	5.531864	1.306253
-981.846064	3.680462	1.311258
-985.185887	3.547738	1.316262
-989.182373	-1.204380	1.321267
-992.854785	-10.227592	1.326272
-996.852922	-0.733680	1.331277
-1000.549382	0.826949	1.336282
-1004.283064	0.953688	1.341286
-1008.012179	2.886612	1.346291
-1011.551918	-10.054323	1.351296
-1015.756499	-5.814013	1.356301
-1020.024493	0.739116	1.361306
-1023.033008	6.687617	1.366310
-1027.265405	7.987023	1.371315
-1030.299263	-0.319280	1.376320
-1033.675652	-0.871575	1.381325
-1037.918693	4.234242	1.386330
-1041.340877	0.398755	1.391334
-1045.289144	5.511200	1.396339
-1049.520984	-0.172216	1.401344
-1053.396850	-2.272029	1.406349
-1056.848048	-1.452094	1.411354
-1060.352658	2.416252	1.416358
-1064.711446	9.814293	1.421363
-1068.044020	-0.988123	1.426368
-1072.073225	6.770932	1.431373
-1075.937193	1.134897	1.436378
-1079.090354	-2.971732	1.441382
-1083.063296	-2.706744	1.446387
-1086.894601	-1.425233	1.451392
-1090.790463	5.509294	1.456397
-1094.399560	1.059418	1.461402
-1097.979267	-3.243539	1.466406
-1102.315400	-3.201936	1.471411
-1105.799753	-4.056925	1.476416
-1109.518887	2.146667	1.481421
-1113.525808	2.819724	1.486426
-1116.854505	-5.990046	1.491430
-1121.135434	-2.919853	1.496435
-1124.483168	-0.789050	1.501440
-1128.196781	-1.992649	1.506445
-1132.309336	9.554949	1.511450
-1135.689900	-4.089730	1.516454
-1140.060530	2.001174	1.521459
-1143.393779	-10.866940	1.526464
-1146.899395	-1.408535	1.531469
-1150.460711	1.882297	1.536474
-1154.353748	-14.499260	1.541478
-1158.420058	-9.989689	1.546483
-1162.525887	-9.712464	1.551488
-1166.248363	4.453749	1.556493
-1169.701150	-3.042794	1.561498
-1173.385375	-3.642764	1.566502
-1177.156792	7.433031	1.571507
-1180.719236	-6.293649	1.576512
-1185.130015	-4.987532	1.581517
-1188.607615	3.450913	1.586522
-1192.261187	0.627845	1.591526
-1196.095517	-1.095709	1.596531
-1199.325510	-5.198521	1.601536
-1203.272338	-2.559805	1.606541
-1207.287437	-0.337616	1.611546
-1210.926239	-2.961903	1.616550
-1215.203670	9.342706	1.621555
-1218.418550	-5.002925	1.626560
-1222.406503	3.718965	1.631565
-1226.004238	1.393535	1.636570
-1229.572003	-10.605737	1.641574
-1233.529165	-7.739054	1.646579
-1237.478548	-12.063650	1.651584
-1241.320493	-5.093263	1.656589
-1245.046849	1.125494	1.661594
-1248.944795	-10.759030	1.666598
-1252.677991	-0.588490	1.671603
-1256.039489	-7.233858	1.676608
-1259.670047	3.777940	1.681613
-1264.136648	4.820196	1.686618
-1267.377347	-4.549642	1.691622
-1271.125657	-3.905460	1.696627
-1274.899560	-2.186044	1.701632
-1278.620644	-2.477246	1.706637
-1282.785615	-7.522210	1.711642
-1285.997346	-8.402952	1.716646
-1290.215159	9.365646	1.721651
-1293.897060	1.413999	1.726656
-1297.490526	-3.721611	1.731661
-1301.507185	-3.253925	1.736666
-1304.964087	-11.623116	1.741670
-1309.039528	1.585090	1.746675
-1312.201668	-0.547472	1.751680
-1316.258601	-5.254935	1.756685
-1320.151814	3.381693	1.761690
-1323.457731	-8.138691	1.766694
-1327.535845	-5.434684	1.771699
-1331.462484	-7.715761	1.776704
-1335.330094	-8.720236	1.781709
-1339.301787	-0.606913	1.786714
-1342.354304	-1.427335	1.791718
-1345.877532	1.130067	1.796723
-1350.005357	-1.342997	1.801728
-1354.118604	1.263658	1.806733
-1357.736728	0.553031	1.811738
-1361.558806	-8.756722	1.816742
-1365.692345	6.609101	1.821747
-1368.971053	-5.013409	1.826752
-1372.580621	-1.982113	1.831757
-1376.302121	9.047766	1.836762
-1380.256758	-2.719132	1.841766
-1384.403719	7.333922	1.846771
-1387.824650	-2.350613	1.851776
-1391.731190	4.609291	1.856781
-1395.627530	0.703991	1.861786
-1399.082128	-0.495310	1.866790
-1403.018655	1.801189	1.871795
-1406.645799	-0.427852	1.876800
-1410.768904	-1.994634	1.881805
-1414.126286	-2.299249	1.886810
-1417.767528	-4.388501	1.891814
-1421.742285	4.746128	1.896819
-1424.815039	-5.625368	1.901824
-1428.996712	-6.365426	1.906829
-1433.090263	1.508409	1.911834
-1436.832638	-3.277835	1.916838
-1440.514428	1.899697	1.921843
-1444.416948	-2.615101	1.926848
-1447.782008	-5.791422	1.931853
-1451.746016	2.778537	1.936858
-1455.753406	-13.278329	1.941862
-1459.602906	-3.572344	1.946867
-1462.727565	0.695218	1.951872
-1466.662734	-8.791167	1.956877
-1470.820117	1.027717	1.961882
-1474.202136	-7.372341	1.966886
-1478.583598	-0.344587	1.971891
-1482.100244	1.483961	1.976896
-1485.399317	-3.328663	1.981901
-1489.699929	-4.361620	1.986906
-1493.079976	-3.403566	1.991910
-1497.114744	7.385776	1.996915
-1500.986417	-2.163053	2.006912
-1501.542538	-4.854101	2.016909
-1499.357886	-6.220198	2.026906
-1496.079479	-5.070973	2.036902
-1493.882235	0.662289	2.046899
-1492.437200	-1.760388	2.056896
-1490.579878	-4.176435	2.066893
-1489.029541	1.112306	2.076890
-1486.943314	1.622982	2.086886
-1484.609193	-2.105266	2.096883
-1482.786990	-2.357827	2.106880
-1481.129651	-6.798950	2.116877
-1479.027624	-8.453966	2.126874
-1477.387754	-7.986746	2.136870
-1475.246108	-13.005870	2.146867
-1473.221162	-7.442184	2.156864
-1471.783226	-1.372952	2.166861
-1469.555469	-7.668379	2.176858
-1467.546713	-6.399019	2.186854
-1465.822447	-5.179191	2.196851
-1463.818800	-4.363443	2.206848
-1462.261062	-3.541831	2.216845
-1460.392427	-4.448923	2.226842
-1458.521986	0.205462	2.236838
-1456.528721	-1.553770	2.246835
-1454.145981	-2.288341	2.256832
-1452.838817	-9.272935	2.266829
-1451.033180	-0.418589	2.276826
-1448.811192	1.188017	2.286822
-1447.046503	-1.937308	2.296819
-1445.490947	-6.148705	2.306816
-1443.150038	-7.172095	2.316813
-1441.243552	-7.858435	2.326810
-1439.092930	-7.309792	2.336806
-1437.480916	-1.866823	2.346803
-1435.639455	-4.735008	2.356800
-1433.693974	-6.492343	2.366797
-1432.102754	-7.622089	2.376794
-1430.133484	-3.063316	2.386790
-1428.386545	-0.292216	2.396787
-1426.384112	-9.339490	2.406784
-1424.526921	-8.500539	2.416781
-1422.852096	-6.730367	2.426778
-1420.621122	-9.249303	2.436774
-1418.819168	-0.947600	2.446771
-1416.813740	0.276117	2.456768
-1414.663274	-0.672650	2.466765
-1413.006314	-7.938248	2.476762
-1411.168139	-8.906480	2.486758
-1409.486262	-3.617381	2.496755
-1407.759206	-5.688919	2.506752
-1405.789179	-3.418133	2.516749
-1404.030766	-3.002468	2.526746
-1401.757248	-6.930907	2.536742
-1399.920592	-8.901916	2.546739
-1397.999408	-5.959179	2.556736
-1396.363984	-5.783222	2.566733
-1394.448497	0.448248	2.576730
-1392.468090	-6.082486	2.586726
-1390.571139	-8.277262	2.596723
-1388.774244	-4.526306	2.606720
-1386.556603	-13.808926	2.616717
-1384.936398	-6.304347	2.626714
-1383.165132	-3.708928	2.636710
-1381.280746	-9.285723	2.646707
-1379.124213	-5.990170	2.656704
-1377.344539	-6.811992	2.666701
-1375.532911	-1.621439	2.676698
-1373.660632	-3.354317	2.686694
-1371.982149	-0.287672	2.696691
-1370.137523	-1.417055	2.706688
-1368.251407	-1.752474	2.716685
-1366.265839	-0.985739	2.726682
-1364.114834	5.577976	2.736678
-1362.063298	4.141150	2.746675
-1360.618402	-1.700424	2.756672
-1359.234591	-1.825856	2.766669
-1356.820389	-3.840328	2.776666
-1354.561846	0.969156	2.786662
-1353.117274	-1.417827	2.796659
-1351.208466	0.754425	2.806656
-1349.341104	1.167998	2.816653
-1347.353977	2.467217	2.826650
-1345.655320	3.061926	2.836646
-1343.201944	0.227389	2.846643
-1341.679022	-1.079898	2.856640
-1339.786628	-2.473174	2.866637
-1338.069494	2.065724	2.876634
-1336.184293	7.817112	2.886630
-1334.431242	6.043472	2.896627
-1332.465304	-1.324577	2.906624
-1330.370699	-1.862568	2.916621
-1328.533287	2.605879	2.926618
-1326.857041	-4.231436	2.936614
-1324.893195	-5.108978	2.946611
-1322.942643	-3.311428	2.956608
-1320.992634	-0.019495	2.966605
-1319.195178	2.775385	2.976602
-1317.305691	0.455059	2.986598
-1315.496567	0.591728	2.996595
-1313.177958	2.460437	3.006592
-1311.896227	-1.192483	3.016589
-1310.031923	5.174292	3.026586
-1308.211624	-2.905799	3.036582
-1306.205802	1.063827	3.046579
-1303.955764	-5.954632	3.056576
-1302.381990	-1.641264	3.066573
-1300.418287	-5.357961	3.076570
-1298.368836	-0.827907	3.086566
-1296.689142	-0.644497	3.096563
-1295.090232	-1.208781	3.106560
-1293.261400	-7.007990	3.116557
-1291.001639	-3.023087	3.126554
-1289.195459	-3.396513	3.136550
-1287.213785	-7.363692	3.146547
-1285.509250	-4.537820	3.156544
-1283.712912	-1.683846	3.166541
-1281.594608	-6.302479	3.176538
-1279.738602	-5.935931	3.186534
-1277.839854	-1.540043	3.196531
-1276.260120	-6.830114	3.206528
-1274.247149	-8.003388	3.216525
-1272.203019	2.221786	3.226522
-1270.372569	1.364018	3.236518
-1268.321205	-0.252159	3.246515
-1266.520344	-6.510532	3.256512
-1265.116271	-0.469386	3.266509
-1263.150634	-2.935558	3.276506
-1261.077892	-7.198571	3.286502
-1259.379495	-4.528137	3.296499
-1257.204952	-3.148823	3.306496
-1255.152527	-7.394906	3.316493
-1253.802924	-3.359976	3.326490
-1251.809731	-4.709663	3.336486
-1249.616909	-4.766913	3.346483
-1247.740529	-6.384249	3.356480
-1245.757585	-3.554007	3.366477
-1244.040086	-5.068570	3.376474
-1242.313351	1.736441	3.386470
-1240.384396	3.050446	3.396467
-1238.752621	-6.038226	3.406464
-1236.364939	-7.513753	3.416461
-1234.864455	-0.694385	3.426458
-1233.249111	-3.589655	3.436454
-1230.847425	-1.962809	3.446451
-1229.286123	-8.250768	3.456448
-1227.200463	-5.962602	3.466445
-1225.105032	-6.021293	3.476442
-1223.660306	-7.224210	3.486438
-1221.690981	-1.784808	3.496435
-1219.927753	-1.830312	3.506432
-1217.913835	-2.430667	3.516429
-1215.949527	-3.614526	3.526426
-1213.894699	-0.846805	3.536422
-1212.083093	-7.192763	3.546419
-1210.598014	-12.359454	3.556416
-1208.577766	0.232426	3.566413
-1206.773897	-3.854759	3.576410
-1204.553103	-0.477270	3.586406
-1202.888315	-6.500418	3.596403
-1201.050863	-8.511397	3.606400
-1199.050352	-14.241644	3.616397
-1197.369456	-17.197953	3.626394
-1195.323480	-9.262907	3.636390
-1193.457978	-7.467289	3.646387
-1191.380520	-12.760207	3.656384
-1189.740645	-11.091038	3.666381
-1188.010086	-7.296585	3.676378
-1186.017500	-14.475099	3.686374
-1184.197054	-14.320162	3.696371
-1182.117702	-7.655909	3.706368
-1180.429597	-13.945076	3.716365
-1178.237881	-9.602614	3.726362
-1176.614379	-2.673533	3.736358
-1174.746249	-8.038786	3.746355
-1173.084057	-12.855293	3.756352
-1171.091592	0.171766	3.766349
-1168.818097	1.198600	3.776346
-1167.172113	-5.406615	3.786342
-1165.359922	-7.079683	3.796339
-1163.331765	-4.666603	3.806336
-1161.613318	-1.211124	3.816333
-1159.858411	-7.099158	3.826330
-1157.941437	-5.272050	3.836326
-1156.140420	-5.468664	3.846323
-1154.019776	-6.673809	3.856320
-1152.232044	-4.515845	3.866317
-1150.209278	-5.156417	3.876314
-1148.487044	-9.140638	3.886310
-1146.297099	-0.192853	3.896307
-1144.528271	-7.175240	3.906304
-1142.926986	-4.305097	3.916301
-1141.243096	-1.049975	3.926298
-1139.148352	-5.410377	3.936294
-1137.040583	-5.251800	3.946291
-1135.173084	-8.025136	3.956288
-1133.522668	-3.313048	3.966285
-1131.701790	-4.203101	3.976282
-1129.528381	-2.996232	3.986278
-1127.811197	-7.603616	3.996275
-1125.704629	-3.492717	4.006272
-1123.937763	-0.157380	4.016269
-1122.223600	-0.099172	4.026266
-1120.476432	-1.910052	4.036262
-1118.652111	-6.523579	4.046259
-1116.090989	-7.179513	4.056256
-1114.725737	-1.536733	4.066253
-1112.878758	1.357234	4.076250
-1110.774974	-5.319460	4.086246
-1108.952055	-8.282735	4.096243
-1107.363308	-7.876542	4.106240
-1105.363141	-2.434866	4.116237
-1103.085411	0.566148	4.126234
-1101.717391	-4.193896	4.136230
-1099.676644	-5.003916	4.146227
-1097.714430	-3.100368	4.156224
-1095.729405	-2.900144	4.166221
-1093.969120	-0.894734	4.176218
-1092.466343	-1.304112	4.186214
-1089.879478	-2.743017	4.196211
-1088.310138	-7.706380	4.206208
-1086.620687	-0.874342	4.216205
-1084.743536	-6.885699	4.226202
-1082.733096	4.760625	4.236198
-1080.969496	-5.376607	4.246195
-1078.634692	-4.840828	4.256192
-1077.087648	-6.137541	4.266189
-1075.327951	-4.533162	4.276186
-1073.490623	-1.644238	4.286182
-1071.647403	-7.331224	4.296179
-1069.895073	-10.732114	4.306176
-1067.713567	-6.848257	4.316173
-1065.764118	-8.928602	4.326170
-1063.894408	-8.726348	4.336166
-1061.994243	-8.099332	4.346163
-1060.091280	-10.723012	4.356160
-1058.357968	-7.433263	4.366157
-1056.430451	-9.584929	4.376154
-1055.079055	-8.651062	4.386150
-1052.923190	-8.331947	4.396147
-1050.636557	-13.895080	4.406144
-1049.022503	-9.539517	4.416141
-1046.639058	-9.338121	4.426138
-1045.232218	0.472954	4.436134
-1043.496776	1.410047	4.446131
-1041.236870	-6.812221	4.456128
-1039.631435	-1.371897	4.466125
-1037.814299	-2.031255	4.476122
-1035.971365	0.330303	4.486118
-1034.236367	1.450854	4.496115
-1031.733536	-6.126241	4.506112
-1030.203762	-1.628939	4.516109
-1028.772323	1.409133	4.526106
-1026.393682	5.508153	4.536102
-1024.686933	-2.700550	4.546099
-1022.555159	-4.810995	4.556096
-1020.922876	-0.877867	4.566093
-1019.116854	4.137955	4.576090
-1017.180942	5.902598	4.586086
-1015.062561	2.551513	4.596083
-1013.328279	-3.836429	4.606080
-1011.229118	2.560918	4.616077
-1009.482272	-6.862034	4.626074
-1007.672288	-0.645446	4.636070
-1005.859475	-9.207489	4.646067
-1004.124348	-11.310293	4.656064
-1002.307847	-8.501941	4.666061
-1000.078292	-11.336987	4.676058
-998.316196	-6.380408	4.686054
-996.475582	-5.254656	4.696051
-994.451366	-6.147945	4.706048
-992.834031	-1.465684	4.716045
-990.590188	-1.519703	4.726042
-989.003407	-5.969093	4.736038
-987.063935	-5.555091	4.746035
-984.864341	-7.645150	4.756032
-983.450049	-2.583401	4.766029
-981.159362	-1.990197	4.776026
-979.354761	2.011379	4.786022
-977.805796	-3.655487	4.796019
-975.899497	-0.615136	4.806016
-974.115929	-4.202757	4.816013
-971.931462	-2.244429	4.826010
-970.024106	-4.210800	4.836006
-968.562785	-6.430992	4.846003
-966.422422	-5.786283	4.856000
-964.427007	-6.494792	4.865997
-962.594593	-3.854352	4.875994
-961.067212	-0.181022	4.885990
-959.063457	-3.859792	4.895987
-957.039843	-5.696330	4.905984
-954.898429	-12.159678	4.915981
-953.146462	-6.435024	4.925978
-951.581561	-7.171188	4.935974
-949.667746	-3.896964	4.945971
-947.690594	-6.609216	4.955968
-945.747029	-7.197365	4.965965
-943.952874	-6.876170	4.975962
-942.109864	-11.333962	4.985958
-940.119852	-8.515058	4.995955
-938.003884	-2.886873	5.005952
-936.438128	-4.382380	5.015949
-934.703617	-4.129194	5.025946
-932.783331	-3.345908	5.035942
-930.682924	-2.387241	5.045939
-928.640054	-3.528338	5.055936
-926.674391	-1.850966	5.065933
-925.320469	-3.134629	5.075930
-923.373902	-0.854440	5.085926
-921.493387	0.414676	5.095923
-919.465089	-5.590951	5.105920
-917.524888	-3.451943	5.115917
-915.997907	4.649036	5.125914
-913.717330	3.473067	5.135910
-911.878426	-4.143337	5.145907
-910.378150	-2.080566	5.155904
-907.893535	-2.827184	5.165901
-906.186655	-3.325679	5.175898
-904.517158	-4.584071	5.185894
-903.044335	-6.445388	5.195891
-900.619766	-5.062567	5.205888
-898.828748	-5.948582	5.215885
-897.142806	-11.591510	5.225882
-895.279328	-5.434638	5.235878
-893.114871	-6.677609	5.245875
-891.329644	-7.601358	5.255872
-889.655198	-10.386903	5.265869
-887.836970	-9.885648	5.275866
-885.479813	-12.913668	5.285862
-883.656990	-6.861263	5.295859
-881.673005	-14.904882	5.305856
-880.126803	-9.898937	5.315853
-878.237516	-7.456343	5.325850
-876.399178	-11.387676	5.335846
-874.384427	-5.925855	5.345843
-872.692316	-10.968321	5.355840
-870.804531	-8.036589	5.365837
-868.833787	-1.210051	5.375834
-866.769485	-5.906965	5.385830
-865.207574	-10.131517	5.395827
-863.194575	-6.916171	5.405824
-861.155380	-13.036277	5.415821
-859.451259	-1.605196	5.425818
-857.839343	-1.071676	5.435814
-855.586739	-1.097092	5.445811
-853.761391	-5.072428	5.455808
-851.934646	-8.581257	5.465805
-850.092010	-6.138941	5.475802
-848.176956	-9.986210	5.485798
-846.655096	-10.071148	5.495795
-844.664235	-8.396086	5.505792
-842.364448	-6.235771	5.515789
-840.584068	-5.051001	5.525786
-838.633926	-3.170945	5.535782
-837.042300	-5.099663	5.545779
-834.975401	-10.581505	5.555776
-833.338647	-9.338090	5.565773
-831.467868	-2.942940	5.575770
-829.273197	-3.063130	5.585766
-827.494567	-1.250456	5.595763
-825.533643	-6.534678	5.605760
-823.655202	-13.849963	5.615757
-821.883145	-7.094030	5.625754
-820.152951	-13.167800	5.635750
-818.592539	-10.308690	5.645747
-816.153016	-11.837940	5.655744
-814.307453	-12.271281	5.665741
-812.505442	-13.081686	5.675738
-810.862148	-11.198351	5.685734
-808.813130	-9.206019	5.695731
-807.145752	-8.962994	5.705728
-804.823825	-6.360264	5.715725
-803.208937	-1.865228	5.725722
-801.220039	2.613831	5.735718
-799.566664	-9.332254	5.745715
-797.710242	-8.060924	5.755712
-795.641720	-10.793930	5.765709
-793.554978	-2.462533	5.775706
-791.937607	-1.563562	5.785702
-790.094830	-11.735634	5.795699
-788.046221	-8.735035	5.805696
-786.221422	-7.566165	5.815693
-784.319644	-8.383012	5.825690
-782.686082	-6.977387	5.835686
-780.584274	-9.096407	5.845683
-778.655689	-6.372796	5.855680
-777.214603	-7.948420	5.865677
-774.790068	-7.881183	5.875674
-773.108374	-4.866605	5.885670
-771.465792	-8.340238	5.895667
-769.266774	-3.630460	5.905664
-767.552884	-2.376545	5.915661
-765.836531	0.601656	5.925658
-763.672001	-5.864395	5.935654
-761.910265	-5.491715	5.945651
-760.004017	-10.427434	5.955648
-757.814544	-3.160171	5.965645
-756.001469	-5.759209	5.975642
-754.403706	-10.363751	5.985638
-752.618824	-4.356541	5.995635
-750.405624	-5.430357	6.005632
-748.800759	-5.067107	6.015629
-747.056418	-12.908301	6.025626
-744.751964	-6.832967	6.035622
-743.123907	-4.162096	6.045619
-741.080385	-9.186579	6.055616
-739.573817	-10.167567	6.065613
-737.580035	-8.743916	6.075610
-735.609984	-7.734720	6.085606
-733.692139	-7.431504	6.095603
-731.649778	-13.395597	6.105600
-730.002670	-6.820920	6.115597
-728.103168	-0.664612	6.125594
-726.330670	5.370033	6.135590
-724.686303	5.637195	6.145587
-722.450311	-0.982987	6.155584
-720.522140	5.622111	6.165581
-718.743691	-1.709970	6.175578
-716.864424	1.763555	6.185574
-714.762430	1.896852	6.195571
-713.079549	-3.635229	6.205568
-711.462409	0.712442	6.215565
-709.520864	-4.769178	6.225562
-707.581248	-5.055787	6.235558
-705.301418	-4.924946	6.245555
-703.763994	-4.895521	6.255552
-701.462647	-6.622315	6.265549
-699.894179	-9.812482	6.275546
-698.205525	-5.977026	6.285542
-696.328011	-2.692894	6.295539
-694.329403	-6.520453	6.305536
-692.482193	-9.323721	6.315533
-690.589261	-6.940552	6.325530
-688.826600	-9.356623	6.335526
-686.706403	-13.588796	6.345523
-685.330630	-11.480469	6.355520
-682.918387	-7.379900	6.365517
-681.181179	-4.652250	6.375514
-679.330944	0.320970	6.385510
-677.375617	-1.517557	6.395507
-675.407901	-8.354888	6.405504
-673.643431	-8.477843	6.415501
-672.019178	-0.591849	6.425498
-669.856901	-1.167613	6.435494
-668.089949	-7.836905	6.445491
-666.174800	-4.511793	6.455488
-664.429625	-2.730062	6.465485
-662.213951	1.565107	6.475482
-660.390702	-1.139582	6.485478
-659.367765	-0.555894	6.495475
-657.052426	-2.429320	6.505472
-654.709605	-2.439287	6.515469
-652.960501	-2.593585	6.525466
-651.108866	-1.186600	6.535462
-649.493074	-2.194602	6.545459
-647.243486	-2.654522	6.555456
-645.481750	-1.060190	6.565453
-643.463216	-5.083617	6.575450
-641.469786	-1.390545	6.585446
-640.019332	-2.587933	6.595443
-638.033876	-5.922357	6.605440
-636.159738	-8.003032	6.615437
-634.410396	-1.515015	6.625434
-632.663227	0.304723	6.635430
-630.729752	-4.988151	6.645427
-628.707495	-5.116593	6.655424
-626.535906	-4.574295	6.665421
-624.966300	-3.314928	6.675418
-623.158155	-5.531293	6.685414
-620.871647	-3.871288	6.695411
-619.255769	-2.970413	6.705408
-617.317407	-1.053453	6.715405
-615.487097	-0.296081	6.725402
-613.548403	-0.413338	6.735398
-611.763480	0.781421	6.745395
-609.791605	-3.202764	6.755392
-608.033095	-6.353190	6.765389
-606.116434	-0.763735	6.775386
-604.515990	2.641891	6.785382
-602.456361	4.857778	6.795379
-600.519583	-2.995845	6.805376
-598.535036	-1.370169	6.815373
-596.676209	-2.596911	6.825370
-594.813473	-1.725740	6.835366
-592.979416	-4.035463	6.845363
-591.081071	-5.273331	6.855360
-589.437527	-5.263656	6.865357
-587.204067	-4.039936	6.875354
-585.648875	-3.717503	6.885350
-583.536922	0.440583	6.895347
-581.572602	-1.824697	6.905344
-579.554610	-9.617549	6.915341
-578.384289	-5.914024	6.925338
-576.201213	-2.611920	6.935334
-574.395729	-0.321979	6.945331
-572.462857	-4.006208	6.955328
-570.221266	0.264409	6.965325
-568.816939	-8.113581	6.975322
-566.580008	-7.578907	6.985318
-564.961639	-5.506237	6.995315
-562.722672	-10.854663	7.005312
-560.971676	-11.785053	7.015309
-559.236006	-9.928929	7.025306
-557.490060	-4.111761	7.035302
-555.309127	-10.897103	7.045299
-553.516348	-8.520004	7.055296
-551.803185	-13.047060	7.065293
-549.901685	-4.613787	7.075290
-548.186986	-13.970614	7.085286
-546.188702	-6.326195	7.095283
-544.293579	-16.269647	7.105280
-542.311572	-17.462567	7.115277
-540.350230	-10.332303	7.125274
-538.925905	-11.863478	7.135270
-536.436960	-5.362018	7.145267
-534.803002	-9.842676	7.155264
-532.852817	-9.334666	7.165261
-531.150342	-10.140526	7.175258
-529.260690	-8.022304	7.185254
-527.523356	-8.510860	7.195251
-525.342898	-17.187992	7.205248
-523.792054	-12.929256	7.215245
-521.847396	-12.807208	7.225242
-519.566295	-9.180034	7.235238
-518.028355	-14.388397	7.245235
-515.991494	-13.804748	7.255232
-514.228942	-8.804552	7.265229
-512.183001	-3.041996	7.275226
-510.580826	-6.339062	7.285222
-508.630292	-8.494051	7.295219
-506.692459	-2.244616	7.305216
-504.673441	-7.357672	7.315213
-502.980878	-7.104624	7.325210
-500.936034	-6.188382	7.335206
-498.868369	-1.114451	7.345203
-497.428165	-6.666873	7.355200
-495.726561	-4.011288	7.365197
-493.581115	-3.474318	7.375194
-491.603366	-4.029006	7.385190
-489.614173	-5.577644	7.395187
-487.918865	-3.498778	7.405184
-486.105271	-8.864297	7.415181
-484.303240	-12.991207	7.425178
-482.212488	-4.207012	7.435174
-480.679639	-6.945197	7.445171
-478.466026	-10.247561	7.455168
-476.643107	-10.076545	7.465165
-474.597201	-7.406909	7.475162
-472.620812	-11.002921	7.485158
-470.818743	-3.135487	7.495155
-469.526803	-5.991609	7.505152
-467.292176	-1.247855	7.515149
-465.395462	-7.465877	7.525146
-463.587989	-5.749291	7.535142
-461.879023	-7.975452	7.545139
-459.891424	-12.655873	7.555136
-457.821498	-1.928380	7.565133
-456.092309	-5.275674	7.575130
-454.057739	-8.725551	7.585126
-452.045247	-10.995482	7.595123
-450.305711	-11.697405	7.605120
-448.675293	-7.953026	7.615117
-446.482269	-8.537514	7.625114
-444.689213	-7.384392	7.635110
-442.900792	-12.297405	7.645107
-441.188542	-4.465135	7.655104
-439.025208	-6.946295	7.665101
-437.391587	-5.331874	7.675098
-435.228454	-5.195495	7.685094
-433.637824	-2.695135	7.695091
-431.450761	-1.310425	7.705088
-429.714207	-8.370429	7.715085
-427.848386	-9.695920	7.725082
-426.065409	-5.771006	7.735078
-424.050570	-4.695446	7.745075
-422.060040	-5.785045	7.755072
-420.211747	-9.223107	7.765069
-418.353786	-6.480097	7.775066
-416.583853	-3.118493	7.785062
-415.294971	-5.513255	7.795059
-413.142992	-3.088243	7.805056
-410.905416	-4.883388	7.815053
-408.872945	-4.649490	7.825050
-407.071227	-3.858669	7.835046
-405.293818	-2.685062	7.845043
-403.608292	-3.381259	7.855040
-401.805791	-8.171786	7.865037
-399.526745	-3.452610	7.875034
-397.943763	0.584089	7.885030
-395.769637	-9.411926	7.895027
-394.289726	-3.557345	7.905024
-392.288753	-5.858868	7.915021
-390.253725	-10.122147	7.925018
-388.576114	-0.522044	7.935014
-386.605617	-7.110760	7.945011
-384.599001	-2.784319	7.955008
-382.986633	-4.655182	7.965005
-381.163445	4.346103	7.975002
-378.917978	-0.123611	7.984998
-377.198238	-5.537414	7.994995
-375.331389	-5.305125	8.004992
-373.553137	0.857142	8.014989
-371.436873	0.910298	8.024986
-369.594205	-1.171195	8.034982
-367.942680	-1.343025	8.044979
-366.033710	4.996407	8.054976
-364.084885	-3.886757	8.064973
-362.341138	0.322356	8.074970
-360.323965	-0.670216	8.084966
-358.522635	2.931062	8.094963
-356.625476	5.563831	8.104960
-354.380757	-0.643898	8.114957
-352.741565	0.170083	8.124954
-350.826510	4.592083	8.134950
-349.184513	2.167195	8.144947
-347.135760	3.497815	8.154944
-345.240334	-1.935444	8.164941
-343.673639	-0.460082	8.174938
-341.587042	-1.789816	8.184934
-339.626177	-6.564409	8.194931
-337.575168	2.248032	8.204928
-335.926461	1.214339	8.214925
-334.257251	1.632310	8.224922
-332.206088	0.385329	8.234918
-329.867521	1.814450	8.244915
-328.324006	1.969430	8.254912
-326.683867	-1.313538	8.264909
-324.624650	5.063377	8.274906
-323.018453	9.403208	8.284902
-321.175707	6.879078	8.294899
-319.210286	3.240743	8.304896
-317.107389	6.804144	8.314893
-315.045650	3.933000	8.324890
-313.335658	4.181945	8.334886
-311.524806	-2.046195	8.344883
-309.665910	0.283705	8.354880
-307.734056	5.283020	8.364877
-306.050452	5.923015	8.374874
-304.245316	6.393168	8.384870
-301.922346	1.938254	8.394867
-300.291155	4.754600	8.404864
-298.573992	2.847214	8.414861
-296.313353	2.816359	8.424858
-294.771436	-0.229220	8.434854
-292.849357	2.706385	8.444851
-290.955820	4.411841	8.454848
-289.020166	8.458441	8.464845
-286.799678	2.851671	8.474842
-285.476273	9.999019	8.484838
-283.290802	5.802059	8.494835
-281.586133	3.551800	8.504832
-279.878886	5.907330	8.514829
-277.685073	2.149213	8.524826
-275.833151	3.917934	8.534822
-273.737789	-2.225806	8.544819
-272.233229	2.482428	8.554816
-270.180545	1.503564	8.564813
-268.220876	-0.054537	8.574810
-266.624044	-2.814696	8.584807
-264.851163	1.202131	8.594803
-262.604592	1.066207	8.604800
-260.948223	1.372982	8.614797
-259.034520	2.846954	8.624794
-257.046136	6.175904	8.634791
-255.138714	0.897519	8.644787
-253.136229	0.225266	8.654784
-251.619053	1.788198	8.664781
-249.764893	-4.209429	8.674778
-247.974503	3.650636	8.684775
-245.596515	-3.891227	8.694771
-243.891546	-4.104981	8.704768
-242.230943	-5.453690	8.714765
-240.151929	-2.538260	8.724762
-238.422765	2.312077	8.734759
-236.477243	-3.363702	8.744755
-234.602701	-0.596579	8.754752
-232.860518	-3.854729	8.764749
-230.495657	-4.803331	8.774746
-229.029083	-0.740276	8.784743
-227.137224	3.620946	8.794739
-225.040804	-9.146759	8.804736
-223.049328	-8.621981	8.814733
-221.555810	-7.165641	8.824730
-219.586160	-2.659674	8.834727
-217.740897	-7.303732	8.844723
-215.809427	-7.830601	8.854720
-214.143764	-13.067898	8.864717
-211.698607	-15.632857	8.874714
-210.402139	-8.911654	8.884711
-208.528928	-9.620208	8.894707
-206.679553	-10.223103	8.904704
-204.374784	-14.243271	8.914701
-202.610908	-18.347331	8.924698
-201.016827	-13.128002	8.934695
-198.777573	-7.151825	8.944691
-197.310327	-13.785765	8.954688
-195.483482	-12.748206	8.964685
-193.385558	-17.437561	8.974682
-191.277652	-19.109185	8.984679
-189.559737	-17.130116	8.994675
-187.575930	-17.333968	9.004672
-185.856126	-17.040022	9.014669
-183.708556	-20.835611	9.024666
-182.199427	-15.917483	9.034663
-180.397512	-10.185230	9.044659
-178.260531	-15.296650	9.054656
-176.418721	-19.001067	9.064653
-174.643713	-9.416384	9.074650
-172.592590	-11.700331	9.084647
-170.910687	-17.677869	9.094643
-168.678041	-15.830936	9.104640
-166.902575	-15.950833	9.114637
-165.276120	-16.659339	9.124634
-163.510279	-10.153384	9.134631
-161.406297	-9.649454	9.144627
-159.519971	-11.149876	9.154624
-157.697898	-11.884418	9.164621
-155.849816	-11.297473	9.174618
-153.877577	-8.285042	9.184615
-151.881609	-6.418456	9.194611
-150.159793	-11.833725	9.204608
-148.364178	-17.836290	9.214605
-146.362987	-13.532121	9.224602
-144.757760	-10.303797	9.234599
-142.546384	-3.274300	9.244595
-141.068009	-9.536657	9.254592
-139.298785	-19.635841	9.264589
-136.943074	-20.626299	9.274586
-135.025559	-20.741298	9.284583
-133.586425	-8.154248	9.294579
-131.457734	-8.955194	9.304576
-129.192170	-8.128007	9.314573
-127.543029	-3.885574	9.324570
-125.772645	-0.947592	9.334567
-123.992742	-1.347255	9.344563
-121.952244	-4.243920	9.354560
-120.229155	-2.638395	9.364557
-118.351100	-2.300027	9.374554
-116.155975	-4.909799	9.384551
-114.410875	-7.398528	9.394547
-113.036904	-3.195058	9.404544
-111.007554	3.785447	9.414541
-108.774702	3.137777	9.424538
-106.758225	5.015887	9.434535
-105.554325	6.227498	9.444531
-103.313983	2.512067	9.454528
-101.185339	4.434969	9.464525
-99.335715	8.256121	9.474522
-97.684216	8.080047	9.484519
-95.892871	3.287189	9.494515
-93.694816	4.047324	9.504512
-91.797426	5.022638	9.514509
-90.475696	5.302679	9.524506
-88.073376	5.236962	9.534503
-86.669073	2.272351	9.544499
-84.480047	6.952999	9.554496
-82.749145	3.060932	9.564493
-80.533270	1.922958	9.574490
-79.080001	7.094560	9.584487
-76.991942	6.683175	9.594483
-75.001793	7.339855	9.604480
-73.353384	4.345244	9.614477
-71.268583	3.205642	9.624474
-69.424658	-1.484770	9.634471
-67.732623	2.923438	9.644467
-65.559928	-0.310069	9.654464
-63.842083	0.799591	9.664461
-62.046159	-2.061828	9.674458
-60.451913	2.808165	9.684455
-58.515308	0.073990	9.694451
-56.388070	-2.887713	9.704448
-54.111076	2.481350	9.714445
-52.316034	-3.698543	9.724442
-50.792527	4.277334	9.734439
-49.331863	-2.656994	9.744435
-46.615525	-2.256827	9.754432
-44.983525	-2.104275	9.764429
-43.207793	-6.139573	9.774426
-41.273581	-0.946880	9.784423
-39.546163	4.784780	9.794419
-37.485002	1.441965	9.804416
-35.834640	0.681979	9.814413
-34.055994	5.040572	9.824410
-32.127059	2.190739	9.834407
-30.143095	3.223954	9.844403
-28.350660	-4.241121	9.854400
-26.165469	-2.245279	9.864397
-24.488072	-3.235169	9.874394
-22.684531	-2.423162	9.884391
-20.484833	0.312806	9.894387
-18.933296	-0.560254	9.904384
-16.813954	1.323972	9.914381
-15.408219	-6.297694	9.924378
-13.068845	-1.289863	9.934375
-11.262703	-1.030019	9.944371
-9.398389	-2.283155	9.954368
-7.569865	-11.342781	9.964365
-5.475060	-9.113273	9.974362
-4.091037	12.292668	9.984359
-2.923060	32.136239	9.994355
-2.020075	79.346283	10.004352
-0.868730	151.034102	10.014349
0.000000	212.804270	10.019354
1.075597	261.332640	10.024359
1.422040	306.751071	10.029363
2.198850	343.503983	10.034368
2.589345	380.321641	10.039373
2.608303	406.662063	10.044378
3.363575	436.014317	10.049383
3.426568	447.370336	10.054387
3.406497	471.659084	10.059392
4.004379	488.336254	10.064397
3.891369	494.070446	10.069402
4.308783	507.247386	10.074407
4.143233	525.152825	10.079411
4.226914	520.221021	10.084416
4.364221	524.854445	10.089421
4.214029	525.898204	10.094426
4.734623	540.512828	10.099431
4.666559	557.591220	10.104435
4.940799	562.177889	10.109440
5.170145	570.234389	10.114445
5.072729	568.996670	10.119450
5.227628	568.441193	10.124455
5.039703	578.282351	10.129459
5.307155	573.131131	10.134464
5.235678	575.519252	10.139469
4.907714	580.664693	10.144474
5.365118	575.861812	10.149479
5.217223	586.557008	10.154483
5.606120	582.239937	10.159488
5.466715	585.998351	10.164493
4.945219	595.100553	10.169498
5.361621	586.429677	10.174503
5.083622	595.637361	10.179507
5.166203	591.570172	10.184512
5.065148	605.137267	10.189517
5.549862	620.781643	10.194522
5.544188	624.698712	10.199527
5.520863	627.810013	10.204531
5.630172	634.181910	10.209536
5.690160	635.196349	10.214541
5.462815	636.049270	10.219546
6.049484	633.847958	10.224551
6.185605	646.687993	10.229555
6.034136	639.733231	10.234560
6.353587	644.695057	10.239565
5.983189	652.304579	10.244570
5.966149	644.449681	10.249575
6.137638	645.028172	10.254579
6.207658	645.257753	10.259584
6.123812	659.018124	10.264589
5.972476	656.667038	10.269594
6.798586	673.057385	10.274599
6.507455	676.850521	10.279603
6.390269	664.561045	10.284608
6.685811	671.313910	10.289613
6.366821	678.394379	10.294618
6.650008	691.372257	10.299623
6.829034	695.426618	10.304627
6.902467	691.287947	10.309632
6.324469	685.881397	10.314637
6.484766	692.365362	10.319642
6.671660	693.468964	10.324647
6.613607	704.507644	10.329651
6.750606	695.676198	10.334656
6.614773	697.544857	10.339661
6.734380	702.891091	10.344666
7.033580	696.252576	10.349671
7.066896	708.527276	10.354675
6.971149	708.605285	10.359680
6.784876	713.857130	10.364685
6.994777	733.280900	10.369690
7.243353	731.106755	10.374695
7.325377	746.145711	10.379699
7.475276	744.037430	10.384704
7.829234	748.618774	10.389709
7.498967	737.224708	10.394714
7.408433	719.471513	10.399719
7.413876	732.011136	10.404723
7.591007	736.856870	10.409728
7.760021	750.797778	10.414733
7.722335	754.363137	10.419738
7.692409	752.419107	10.424743
7.295735	751.141502	10.429747
7.559484	756.892110	10.434752
7.636582	754.087771	10.439757
7.745112	766.287252	10.444762
8.012163	762.712591	10.449767
7.894590	766.224941	10.454771
7.906860	769.863053	10.459776
7.782097	762.165906	10.464781
7.391881	771.126097	10.469786
7.820881	769.164165	10.474791
7.738159	792.433513	10.479795
8.056845	796.798291	10.484800
7.750147	804.471963	10.489805
8.055807	810.472770	10.494810
8.080303	796.387739	10.499815
8.034537	802.906687	10.504819
8.369735	803.397509	10.509824
8.295417	808.806240	10.514829
8.392209	825.657320	10.519834
9.058968	832.347395	10.524839
8.800952	821.359690	10.529843
8.839084	816.248104	10.534848
8.994734	809.593103	10.539853
8.657708	813.081513	10.544858
8.791177	806.876757	10.549863
9.090064	813.853318	10.554867
9.359476	810.228111	10.559872
9.176622	811.897612	10.564877
9.078866	820.302428	10.569882
9.101438	808.171637	10.574887
9.385746	815.132936	10.579891
9.068762	807.634907	10.584896
9.020411	812.462880	10.589901
8.955087	812.572777	10.594906
9.280588	812.222511	10.599911
9.241053	813.783361	10.604915
9.267371	812.636116	10.609920
9.206595	814.024557	10.614925
8.742666	820.779814	10.619930
8.887148	817.270761	10.624935
9.199237	831.793912	10.629939
9.274673	851.851930	10.634944
9.687649	842.300853	10.639949
9.522250	845.074588	10.644954
9.495849	853.004957	10.649959
9.124296	856.266799	10.654963
9.268955	846.723831	10.659968
9.459451	861.756141	10.664973
9.997689	877.213574	10.669978
10.287349	875.267627	10.674983
9.996918	866.778974	10.679987
10.076830	856.028168	10.684992
10.110685	856.595134	10.689997
10.166362	852.931564	10.695002
10.292697	857.698415	10.700007
10.220819	856.205244	10.705011
10.099909	857.564527	10.710016
10.682357	850.570280	10.715021
10.247002	860.318251	10.720026
10.140620	849.115055	10.725031
9.941660	859.009596	10.730035
10.389476	876.121856	10.735040
9.783368	881.892579	10.740045
10.123587	896.405046	10.745050
10.573190	890.948546	10.750055
10.223069	900.657059	10.755059
10.466702	904.538557	10.760064
10.423647	897.497592	10.765069
10.407361	904.997967	10.770074
10.430215	908.779163	10.775079
10.647658	925.432823	10.780083
10.597604	925.631287	10.785088
10.793004	926.668316	10.790093
11.126734	941.405357	10.795098
11.268703	934.338572	10.800103
11.287077	936.418449	10.805107
11.622941	935.428908	10.810112
11.712677	929.016473	10.815117
10.550055	913.494363	10.820122
11.308223	917.211458	10.825127
11.113765	934.058909	10.830131
11.016691	935.341086	10.835136
11.167785	934.311779	10.840141
10.745678	930.871032	10.845146
11.094284	939.247142	10.850151
10.909259	940.519531	10.855155
11.060129	937.745930	10.860160
11.348706	966.757236	10.865165
11.225877	975.827616	10.870170
11.788860	969.980202	10.875175
11.882681	967.149668	10.880179
11.378919	972.736298	10.885184
11.972793	963.655840	10.890189
11.883315	964.160667	10.895194
12.469055	961.158158	10.900199
11.918994	968.336797	10.905203
11.986844	965.450716	10.910208
12.315561	962.638328	10.915213
12.015994	975.835573	10.920218
11.964380	969.748145	10.925223
11.538344	971.296727	10.930227
11.864242	976.437554	10.935232
12.327389	980.742089	10.940237
12.214697	975.572628	10.945242
12.024187	970.739010	10.950247
12.120476	975.220523	10.955251
12.271017	973.428285	10.960256
12.455713	970.182301	10.965261
12.257498	979.423898	10.970266
12.170377	970.912566	10.975271
12.358403	991.613825	10.980275
12.336987	1005.286033	10.985280
12.905170	998.613903	10.990285
12.723006	1004.518824	10.995290
12.993929	1000.214368	11.000295
12.697120	1001.381586	11.005299
12.949544	1001.079373	11.010304
13.171598	1000.979735	11.015309
12.905469	1000.191697	11.020314
13.199655	991.876684	11.025319
13.258186	985.972074	11.030323
12.716214	976.724782	11.035328
12.938490	974.366430	11.040333
13.368202	996.815987	11.045338
13.484274	999.037016	11.050343
12.905500	994.452330	11.055347
12.910648	1005.517490	11.060352
13.328513	997.702715	11.065357
13.084339	1008.340891	11.070362
13.323847	1005.182213	11.075367
13.226660	1005.514285	11.080371
13.346784	1010.404616	11.085376
13.482870	1014.817738	11.090381
13.380972	1018.602588	11.095386
13.379640	1007.609818	11.100391
13.352323	1013.243850	11.105395
13.185524	1019.094431	11.110400
13.746104	1024.747271	11.115405
13.477948	1033.276945	11.120410
13.886091	1032.826059	11.125415
13.956960	1047.311428	11.130419
14.145691	1039.717893	11.135424
14.842095	1040.290476	11.140429
14.370789	1028.565904	11.145434
14.310826	1008.376745	11.150439
13.962144	1011.568776	11.155443
14.170512	1010.904643	11.160448
14.295110	1005.332513	11.165453
14.230608	1015.087257	11.170458
14.371222	1002.870154	11.175463
13.960554	1003.389396	11.180467
13.956956	1001.437267	11.185472
14.096305	1019.008758	11.190477
14.233181	1037.763719	11.195482
14.311161	1036.990099	11.200487
14.260393	1043.876716	11.205491
13.990490	1042.557217	11.210496
14.200553	1040.766213	11.215501
14.296048	1049.176308	11.220506
14.880585	1063.386908	11.225511
14.832102	1070.654461	11.230515
14.849480	1068.636754	11.235520
15.163766	1058.385230	11.240525
14.890222	1053.289506	11.245530
15.145710	1052.193345	11.250535
14.575982	1040.460771	11.255539
14.782419	1060.663175	11.260544
15.085192	1064.491152	11.265549
15.253786	1073.312674	11.270554
15.327019	1076.049087	11.275559
15.181155	1080.451755	11.280563
15.360094	1077.283316	11.285568
15.910960	1071.554785	11.290573
15.396765	1056.090300	11.295578
15.389346	1048.394209	11.300583
15.435916	1047.959132	11.305587
15.370125	1046.850952	11.310592
15.552063	1046.989508	11.315597
15.561638	1050.386568	11.320602
15.494505	1047.628617	11.325607
15.564480	1055.782169	11.330611
15.414504	1070.578979	11.335616
15.777245	1064.120073	11.340621
15.582069	1079.643459	11.345626
15.889841	1074.938321	11.350631
16.016208	1078.862469	11.355635
15.829747	1082.302227	11.360640
15.892059	1075.476406	11.365645
15.917426	1075.931151	11.370650
15.990400	1078.098001	11.375655
15.948822	1082.593316	11.380659
15.954758	1080.451253	11.385664
16.114097	1083.915800	11.390669
15.880304	1086.507882	11.395674
15.962754	1079.123210	11.400679
16.040225	1077.841253	11.405683
15.854105	1074.838434	11.410688
15.918857	1085.938827	11.415693
16.136909	1107.607332	11.420698
16.275482	1107.455691	11.425703
16.219310	1116.601962	11.430707
16.455495	1109.194863	11.435712
16.561520	1098.928099	11.440717
16.469742	1109.482976	11.445722
16.597062	1108.118654	11.450727
16.788480	1103.185562	11.455731
16.956337	1110.565251	11.460736
17.122977	1098.802692	11.465741
17.218779	1104.828939	11.470746
17.485898	1104.535652	11.475751
17.279543	1107.681193	11.480755
17.117512	1108.384387	11.485760
17.409963	1101.907518	11.490765
17.104091	1109.907250	11.495770
17.408802	1111.123710	11.500775
17.238765	1097.206762	11.505779
17.099992	1088.459089	11.510784
17.200153	1087.559689	11.515789
17.026020	1111.404135	11.520794
17.117013	1106.614577	11.525799
17.219336	1111.089964	11.530803
17.085495	1115.213473	11.535808
17.506489	1106.998238	11.540813
16.898379	1114.964530	11.545818
17.565823	1108.334546	11.550823
17.386504	1115.367579	11.555827
17.262099	1115.606819	11.560832
17.680106	1131.299069	11.565837
17.543042	1136.623145	11.570842
18.026043	1130.891229	11.575847
17.833226	1140.273707	11.580851
17.674895	1140.495474	11.585856
17.913887	1130.761290	11.590861
18.041155	1147.738941	11.595866
17.876645	1143.387130	11.600871
18.328832	1138.852213	11.605875
17.830293	1140.181136	11.610880
18.048822	1139.345123	11.615885
17.687824	1143.725484	11.620890
18.359610	1135.967763	11.625895
18.281707	1140.876299	11.630899
18.208219	1136.851517	11.635904
18.183670	1131.402021	11.640909
18.096810	1140.270539	11.645914
18.312974	1126.678929	11.650919
18.631052	1128.792314	11.655923
18.409508	1131.080328	11.660928
18.766621	1126.751191	11.665933
18.398958	1132.098224	11.670938
18.587579	1127.401263	11.675943
18.512053	1132.872287	11.680947
18.591512	1152.127497	11.685952
19.326989	1156.799471	11.690957
19.159132	1151.269143	11.695962
19.137241	1142.593374	11.700967
19.356499	1129.283075	11.705971
18.814426	1131.853416	11.710976
19.179704	1133.735287	11.715981
19.009593	1143.473481	11.720986
19.488228	1132.989648	11.725991
19.152913	1126.005795	11.730995
19.369532	1136.876501	11.736000
19.251228	1126.266468	11.741005
19.288372	1136.750707	11.746010
19.368624	1135.262214	11.751015
19.390028	1137.557126	11.756019
18.910971	1136.275849	11.761024
19.354613	1138.765209	11.766029
19.034239	1138.937391	11.771034
19.409417	1141.839151	11.776039
19.550270	1156.497361	11.781043
19.497266	1167.569449	11.786048
19.567458	1165.464516	11.791053
19.703616	1175.542984	11.796058
19.465170	1166.435775	11.801063
19.539516	1170.051099	11.806067
19.603074	1163.261342	11.811072
19.940283	1170.190441	11.816077
19.693912	1172.609824	11.821082
19.594796	1167.687841	11.826087
19.677104	1169.492312	11.831091
19.794657	1174.120633	11.836096
20.018755	1176.063820	11.841101
20.110434	1190.101672	11.846106
20.119231	1181.062589	11.851111
20.552188	1179.080983	11.856115
20.503017	1178.097840	11.861120
20.380881	1175.536403	11.866125
20.524616	1180.863664	11.871130
20.735785	1173.564247	11.876135
20.554412	1171.210337	11.881139
20.176966	1172.150207	11.886144
21.041828	1169.818625	11.891149
21.033376	1162.886871	11.896154
20.849705	1155.524501	11.901159
21.006564	1164.995067	11.906163
20.572086	1164.242200	11.911168
20.877557	1167.201312	11.916173
20.610961	1169.506924	11.921178
21.153408	1162.462951	11.926183
20.844006	1159.461516	11.931187
20.488263	1167.885884	11.936192
20.550988	1160.274817	11.941197
20.550537	1175.019641	11.946202
20.808060	1183.347948	11.951207
21.181888	1185.738758	11.956211
21.713158	1181.535669	11.961216
21.520329	1173.150509	11.966221
21.692303	1173.016036	11.971226
21.548411	1160.806537	11.976231
21.552124	1148.257922	11.981235
21.060373	1154.025320	11.986240
21.527625	1151.827046	11.991245
21.390959	1148.532704	11.996250
21.652389	1148.700659	12.001255
21.396446	1155.846716	12.006259
21.533005	1159.232291	12.011264
21.802986	1151.410427	12.016269
21.593025	1160.812436	12.021274
21.313996	1158.405009	12.026279
21.588300	1154.284275	12.031283
21.575509	1172.669136	12.036288
22.142537	1170.996915	12.041293
21.631400	1171.214042	12.046298
21.332305	1157.400485	12.051303
21.840048	1164.335474	12.056307
21.506795	1173.122308	12.061312
21.787395	1174.360276	12.066317
22.033150	1177.773711	12.071322
22.181780	1167.356701	12.076327
22.269418	1157.402527	12.081331
22.080284	1158.635374	12.086336
22.343613	1158.489975	12.091341
22.300423	1154.531441	12.096346
22.000121	1134.056087	12.101351
21.575151	1125.461280	12.106355
21.595034	1125.415253	12.111360
22.016503	1118.098751	12.116365
21.808359	1120.102227	12.121370
21.552620	1117.488706	12.126375
21.690976	1118.952770	12.131379
21.565114	1118.831073	12.136384
21.624164	1122.235851	12.141389
21.438852	1125.528183	12.146394
21.283572	1115.676081	12.151399
21.358130	1122.816378	12.156403
21.348500	1140.255654	12.161408
22.239728	1139.633515	12.166413
21.524449	1143.835408	12.171418
21.403432	1131.086349	12.176423
21.738977	1141.023240	12.181427
21.736382	1154.050900	12.186432
21.765319	1147.175901	12.191437
21.589208	1152.224833	12.196442
21.687881	1143.010887	12.201447
21.633921	1142.876468	12.206451
21.747523	1154.615513	12.211456
21.728212	1147.635100	12.216461
21.562983	1148.052263	12.221466
21.702843	1143.072735	12.226471
21.716251	1139.382003	12.231475
21.449505	1141.590531	12.236480
21.669696	1145.292950	12.241485
22.093749	1166.098843	12.246490
21.606806	1142.153344	12.251495
21.398879	1139.022013	12.256499
21.361163	1156.405333	12.261504
21.511808	1153.667655	12.266509
21.428426	1163.991785	12.271514
21.800300	1169.343875	12.276519
21.772868	1167.461339	12.281523
22.010198	1171.464776	12.286528
22.099982	1166.108954	12.291533
21.628767	1158.700357	12.296538
21.599767	1145.738139	12.301543
22.006041	1137.895677	12.306547
21.842907	1137.540369	12.311552
21.909070	1132.730587	12.316557
21.823090	1130.170063	12.321562
21.889029	1144.123076	12.326567
21.693251	1133.316321	12.331571
21.984581	1140.563933	12.336576
21.934906	1130.412660	12.341581
21.686788	1142.682271	12.346586
21.676183	1133.405357	12.351591
21.937965	1130.958103	12.356595
21.624897	1138.635397	12.361600
21.885802	1132.069582	12.366605
21.917440	1142.407530	12.371610
21.541529	1138.134993	12.376615
21.702279	1129.857392	12.381619
21.466837	1137.819405	12.386624
21.319296	1134.662721	12.391629
21.370355	1133.195814	12.396634
21.505862	1131.608242	12.401639
21.637286	1128.197280	12.406643
21.356264	1143.227024	12.411648
21.336018	1136.062039	12.416653
21.369285	1135.922533	12.421658
21.513247	1139.784864	12.426663
21.478043	1137.343134	12.431667
21.560318	1144.164747	12.436672
21.371744	1139.263638	12.441677
21.285010	1157.229709	12.446682
21.632248	1163.865768	12.451687
21.675144	1175.408134	12.456691
21.753606	1176.471941	12.461696
21.844995	1175.572068	12.466701
21.762875	1182.061881	12.471706
21.802866	1181.184635	12.476711
21.914038	1181.546907	12.481715
21.701604	1163.138311	12.486720
21.710147	1145.514091	12.491725
21.620541	1151.171485	12.496730
21.334889	1145.182931	12.501735
21.873869	1149.803331	12.506739
21.728416	1153.734630	12.511744
21.516912	1144.649261	12.516749
21.526372	1153.348507	12.521754
21.816730	1173.601802	12.526759
21.741660	1168.608196	12.531763
21.700175	1156.941278	12.536768
21.487175	1155.249247	12.541773
21.732324	1161.503332	12.546778
21.515383	1170.107194	12.551783
21.902322	1175.701836	12.556787
21.732132	1172.740872	12.561792
21.618729	1163.674988	12.566797
21.861349	1157.741907	12.571802
21.978562	1155.197462	12.576807
22.237236	1154.256275	12.581811
21.559687	1155.594970	12.586816
22.040486	1147.770120	12.591821
22.092813	1152.711989	12.596826
21.945669	1151.196563	12.601831
22.217516	1150.639963	12.606835
21.447986	1144.609636	12.611840
21.849220	1144.884279	12.616845
21.710608	1143.576603	12.621850
21.533352	1127.935457	12.626855
21.785051	1139.642524	12.631859
21.679133	1139.259248	12.636864
21.702930	1127.676291	12.641869
21.361569	1137.854768	12.646874
21.759395	1154.186033	12.651879
21.963597	1153.439319	12.656883
21.647260	1140.439134	12.661888
21.811243	1131.748869	12.666893
21.455138	1127.903205	12.671898
21.671552	1128.516644	12.676903
21.725471	1127.682803	12.681907
21.790085	1128.102794	12.686912
22.009041	1124.545771	12.691917
21.558405	1129.528475	12.696922
21.759049	1131.609890	12.701927
21.713898	1124.535628	12.706931
21.437603	1131.602269	12.711936
21.658383	1128.164144	12.716941
21.718832	1126.885891	12.721946
21.721171	1132.277643	12.726951
21.761687	1125.159483	12.731955
21.472216	1134.887742	12.736960
21.891692	1131.392259	12.741965
22.004741	1126.668387	12.746970
21.888627	1125.392776	12.751975
21.840111	1125.019396	12.756979
21.834608	1134.923573	12.761984
21.692082	1132.658141	12.766989
21.827613	1128.792130	12.771994
21.879374	1125.619829	12.776999
21.939335	1135.975023	12.782003
21.235351	1142.446705	12.787008
21.772335	1131.989579	12.792013
21.569752	1132.135644	12.797018
21.576264	1140.334860	12.802023
21.543320	1129.021369	12.807027
21.402457	1132.087002	12.812032
21.722993	1133.528120	12.817037
21.629677	1131.509647	12.822042
21.904741	1134.889232	12.827047
21.648165	1133.062173	12.832051
21.400174	1139.374354	12.837056
21.692882	1139.407077	12.842061
21.758332	1136.159005	12.847066
21.574226	1140.186928	12.852071
21.528473	1130.500776	12.857075
21.426983	1128.212914	12.862080
21.394958	1135.212016	12.867085
21.661718	1136.433800	12.872090
21.467809	1133.849544	12.877095
21.457199	1130.187407	12.882099
21.569163	1133.834563	12.887104
21.673522	1135.067613	12.892109
21.822015	1142.318006	12.897114
21.489677	1140.747096	12.902119
21.578365	1139.293078	12.907123
21.385452	1151.059412	12.912128
21.972577	1146.167802	12.917133
21.873871	1153.919667	12.922138
21.562132	1150.291787	12.927143
21.601376	1134.527461	12.932147
21.254776	1149.120426	12.937152
21.864632	1148.874164	12.942157
21.661146	1152.149486	12.947162
21.643033	1160.816754	12.952167
21.649510	1161.059607	12.957171
21.794713	1171.211522	12.962176
21.672157	1163.518930	12.967181
21.725331	1160.929411	12.972186
21.622778	1154.645379	12.977191
21.694236	1146.137946	12.982195
21.258114	1148.355384	12.987200
21.563710	1163.781939	12.992205
21.733852	1174.113530	12.997210
21.730075	1177.878042	13.002215
21.820790	1172.391794	13.007219
21.830777	1179.971482	13.012224
21.564629	1163.975275	13.017229
22.111042	1168.867961	13.022234
21.534577	1152.891024	13.027239
21.795127	1140.776408	13.032243
21.224189	1146.861331	13.037248
21.739550	1155.230678	13.042253
21.876196	1151.115784	13.047258
21.950479	1153.386237	13.052263
21.789549	1146.007736	13.057267
21.545946	1145.990307	13.062272
21.524625	1146.221741	13.067277
21.789811	1144.222720	13.072282
21.881012	1146.009479	13.077287
21.891067	1146.278560	13.082291
21.740653	1141.547751	13.087296
21.800627	1147.877002	13.092301
21.967283	1145.229738	13.097306
21.694485	1146.996801	13.102311
21.941667	1144.244151	13.107315
21.837335	1150.267624	13.112320
22.134753	1143.004354	13.117325
22.188630	1152.966652	13.122330
21.814802	1134.643394	13.127335
21.417336	1118.496853	13.132339
20.897493	1127.903421	13.137344
21.581143	1139.513531	13.142349
21.555541	1143.507568	13.147354
21.532219	1148.853199	13.152359
21.554123	1146.065753	13.157363
21.357300	1152.702326	13.162368
21.622512	1147.780252	13.167373
21.730973	1154.653433	13.172378
21.565998	1155.965032	13.177383
21.543656	1146.210909	13.182387
21.272314	1157.627139	13.187392
21.421823	1150.200934	13.192397
21.678738	1161.535673	13.197402
21.520926	1161.446296	13.202407
21.734725	1157.211198	13.207411
21.777147	1162.101873	13.212416
21.588292	1151.700106	13.217421
21.664315	1152.295379	13.222426
21.428470	1154.781639	13.227431
21.768703	1151.047105	13.232435
21.582150	1151.894638	13.237440
21.455229	1161.707544	13.242445
21.519701	1163.625204	13.247450
21.333968	1180.370766	13.252455
22.194719	1190.364481	13.257459
21.852855	1184.482657	13.262464
21.978054	1164.713525	13.267469
21.751981	1163.926110	13.272474
21.755681	1163.891147	13.277479
22.093636	1151.596276	13.282483
22.010507	1161.856809	13.287488
21.883988	1157.924799	13.292493
21.582198	1151.557297	13.297498
21.493793	1161.162281	13.302503
22.085302	1155.396358	13.307507
21.517163	1161.405015	13.312512
21.966350	1165.754629	13.317517
21.560078	1155.581191	13.322522
21.404929	1161.069825	13.327527
21.659762	1159.699424	13.332531
21.687982	1165.764124	13.337536
21.627726	1166.357896	13.342541
21.568743	1165.183802	13.347546
21.558405	1163.991500	13.352551
21.651349	1155.448798	13.357555
21.535208	1170.074900	13.362560
21.808004	1158.948574	13.367565
21.624325	1165.532767	13.372570
21.765633	1165.086970	13.377575
21.830107	1159.313119	13.382579
21.617540	1164.653702	13.387584
21.868847	1166.223536	13.392589
21.678874	1163.280966	13.397594
21.539839	1160.051765	13.402599
21.526639	1170.245840	13.407603
21.503029	1168.978838	13.412608
21.494826	1162.469414	13.417613
21.456767	1157.145779	13.422618
21.267696	1172.219785	13.427623
21.917358	1169.330622	13.432627
21.500118	1169.368227	13.437632
21.545773	1165.837357	13.442637
21.163324	1172.592609	13.447642
21.185362	1176.650328	13.452647
21.914476	1179.768519	13.457651
21.490943	1203.437180	13.462656
21.981343	1193.880906	13.467661
21.802068	1200.039617	13.472666
21.578058	1195.646282	13.477671
21.994323	1190.768559	13.482675
21.449992	1175.122015	13.487680
21.502100	1173.026102	13.492685
21.620269	1179.445651	13.497690
21.753051	1200.087975	13.502695
21.707742	1191.330929	13.507699
21.721350	1199.032375	13.512704
21.571047	1199.899353	13.517709
21.965745	1179.802149	13.522714
21.610150	1185.275422	13.527719
21.734113	1176.509098	13.532723
21.836604	1179.611568	13.537728
21.804645	1174.015695	13.542733
21.942238	1171.670649	13.547738
21.799170	1175.192199	13.552743
22.029173	1170.274575	13.557747
21.639576	1175.043931	13.562752
21.658556	1167.556019	13.567757
21.855041	1176.259133	13.572762
21.644985	1183.722996	13.577767
22.109217	1182.738669	13.582771
21.652082	1178.025701	13.587776
21.688980	1173.505137	13.592781
21.661945	1171.340293	13.597786
21.654177	1175.866153	13.602791
21.920589	1166.083824	13.607795
21.351116	1171.069942	13.612800
21.636539	1176.373698	13.617805
21.762385	1175.327784	13.622810
22.162600	1177.947755	13.627815
22.348168	1160.101323	13.632819
21.988650	1150.212769	13.637824
21.281039	1146.961847	13.642829
21.516450	1142.981206	13.647834
21.542428	1141.549783	13.652839
21.955053	1128.409621	13.657843
21.553068	1140.575348	13.662848
21.751262	1138.198996	13.667853
22.179806	1135.061171	13.672858
21.645197	1140.566305	13.677863
21.844782	1138.004976	13.682867
21.526072	1143.978361	13.687872
21.488831	1137.573795	13.692877
21.743657	1132.369294	13.697882
21.513805	1138.590732	13.702887
21.930788	1136.307921	13.707891
21.201125	1142.442161	13.712896
21.101364	1146.987339	13.717901
21.766440	1149.415840	13.722906
21.792383	1155.085791	13.727911
21.848164	1140.055999	13.732915
21.777544	1141.936029	13.737920
21.677864	1139.469433	13.742925
21.841192	1146.508467	13.747930
21.638205	1148.227244	13.752935
21.607045	1151.192360	13.757939
21.571278	1149.443494	13.762944
21.678717	1148.573633	13.767949
22.058035	1142.647120	13.772954
21.540193	1141.971312	13.777959
21.854881	1141.700658	13.782963
21.289748	1149.563678	13.787968
21.953168	1156.584472	13.792973
21.761852	1142.221523	13.797978
21.687593	1146.411799	13.802983
22.085045	1147.450517	13.807987
21.727262	1144.706066	13.812992
21.453555	1144.486955	13.817997
21.521690	1146.941226	13.823002
21.629459	1150.217655	13.828007
21.499237	1141.003088	13.833011
21.478542	1146.533795	13.838016
21.763335	1148.787101	13.843021
22.216880	1151.019764	13.848026
21.553768	1145.703039	13.853031
21.687839	1144.848743	13.858035
21.497771	1151.662975	13.863040
21.513130	1152.544968	13.868045
21.536713	1145.131673	13.873050
21.368531	1151.624387	13.878055
21.596082	1148.498126	13.883059
21.604044	1151.777457	13.888064
21.820191	1152.795946	13.893069
21.764017	1148.326873	13.898074
21.680280	1157.106839	13.903079
21.811897	1143.631553	13.908083
21.532614	1146.413814	13.913088
21.587445	1149.804715	13.918093
21.515238	1145.119312	13.923098
21.481089	1157.897779	13.928103
21.571836	1155.087080	13.933107
21.387257	1157.748894	13.938112
21.856577	1165.713638	13.943117
21.653324	1173.923178	13.948122
21.692072	1172.046269	13.953127
21.926086	1160.730010	13.958131
21.789312	1160.802818	13.963136
21.677444	1155.498549	13.968141
21.644035	1154.822180	13.973146
22.002060	1158.251099	13.978151
21.732629	1152.193840	13.983155
21.717790	1153.336407	13.988160
21.856500	1149.138660	13.993165
21.857819	1147.264618	13.998170
21.511651	1160.881328	14.003175
21.840552	1156.696758	14.008179
21.552694	1159.497465	14.013184
21.745592	1158.577030	14.018189
21.891018	1153.756203	14.023207
21.951501	1153.956101	14.028224
21.734140	1145.478123	14.033242
21.908901	1152.602692	14.038259
21.755628	1147.523846	14.043277
21.792951	1152.295015	14.048295
21.482062	1157.064467	14.053312
21.928919	1154.249845	14.058330
21.928755	1165.648460	14.063347
21.891083	1156.063595	14.068365
21.782025	1150.142060	14.073383
21.897774	1160.555757	14.078400
22.007494	1156.297242	14.083418
22.077417	1158.011393	14.088435
21.852788	1159.427987	14.093453
21.919789	1160.296113	14.098471
21.646987	1160.245255	14.103488
22.026640	1160.030950	14.108506
22.050025	1154.123716	14.113523
21.820733	1162.764536	14.118541
22.355145	1154.478549	14.123559
22.153358	1165.066389	14.128576
21.805411	1162.228972	14.133594
21.844670	1158.794415	14.138611
22.219927	1161.885465	14.143629
22.125193	1150.879167	14.148647
21.717267	1157.112619	14.153664
21.610683	1151.757634	14.158682
21.671406	1161.977602	14.163699
21.926807	1165.637280	14.168717
21.919721	1178.736050	14.173735
22.025925	1188.592301	14.178752
22.121580	1190.943436	14.183770
21.706761	1200.910290	14.188787
22.046039	1196.200558	14.193805
22.195707	1200.440232	14.198823
22.146331	1208.428523	14.203840
22.195676	1200.097717	14.208858
22.420023	1201.117228	14.213875
22.402592	1203.206628	14.218893
22.325826	1197.890220	14.223911
22.134454	1199.567673	14.228928
22.109787	1202.394991	14.233946
22.567934	1221.303505	14.238963
22.257633	1223.421861	14.243981
22.750837	1235.551753	14.248999
22.225523	1235.413076	14.254016
22.678156	1238.869649	14.259034
22.608482	1224.087021	14.264051
22.861667	1234.620917	14.269069
22.973633	1227.279447	14.274087
22.746648	1208.775451	14.279104
22.670753	1205.655141	14.284122
22.680055	1207.184399	14.289139
22.662937	1203.047233	14.294157
22.612585	1185.991057	14.299175
22.417234	1201.206552	14.304192
22.368981	1200.782913	14.309210
22.698156	1205.790697	14.314227
22.787172	1237.694727	14.319245
22.738134	1227.755831	14.324263
22.906150	1227.684120	14.329280
22.742160	1214.875322	14.334298
22.573353	1211.282710	14.339315
22.646019	1228.815078	14.344333
22.737262	1225.547986	14.349351
22.937939	1223.765805	14.354368
22.685620	1227.669256	14.359386
23.079680	1235.669334	14.364403
23.065705	1238.273939	14.369421
22.972548	1227.274010	14.374439
22.661150	1236.484114	14.379456
22.806762	1228.495480	14.384474
22.980928	1224.379453	14.389491
22.882072	1230.961157	14.394509
23.170053	1224.087583	14.399527
22.990148	1233.314513	14.404544
22.930999	1235.818193	14.409562
23.327149	1235.378992	14.414579
22.885923	1231.344459	14.419597
23.022682	1232.295912	14.424615
23.217360	1237.845315	14.429632
22.924605	1236.865514	14.434650
22.975233	1232.023751	14.439667
23.007405	1235.811491	14.444685
23.359373	1227.057886	14.449703
23.031879	1235.411226	14.454720
22.845951	1224.843777	14.459738
23.415482	1239.248578	14.464755
23.593391	1244.960715	14.469773
23.665828	1239.190721	14.474791
23.383060	1237.937136	14.479808
23.358767	1235.883656	14.484826
23.822132	1234.747044	14.489843
23.124061	1234.634444	14.494861
23.461783	1231.968060	14.499879
23.476890	1230.134223	14.504896
23.349013	1235.309759	14.509914
23.473670	1231.588866	14.514931
23.239423	1237.668150	14.519949
23.535501	1235.623920	14.524967
23.536592	1241.286444	14.529984
23.097487	1237.872072	14.535002
23.626754	1246.334448	14.540019
23.569421	1270.692899	14.545037
23.982070	1262.675393	14.550055
23.617607	1253.220127	14.555072
23.386282	1243.048673	14.560090
23.704821	1253.308755	14.565107
23.705421	1266.426361	14.570125
23.868130	1259.217526	14.575143
23.921320	1259.123374	14.580160
24.084803	1249.622870	14.585178
23.961585	1236.393641	14.590195
23.714649	1227.185587	14.595213
24.201971	1221.070818	14.600231
24.081300	1224.913505	14.605248
23.564102	1223.657199	14.610266
24.040378	1224.052365	14.615283
23.902651	1229.291010	14.620301
23.704032	1216.380264	14.625319
24.057446	1230.203949	14.630336
24.021588	1231.771664	14.635354
24.315097	1216.843694	14.640371
23.635601	1236.998162	14.645389
23.701000	1226.552989	14.650407
23.903068	1225.700964	14.655424
23.454868	1231.111750	14.660442
23.763044	1235.344730	14.665459
23.923221	1254.181922	14.670477
24.453848	1267.779569	14.675495
24.237381	1260.339264	14.680512
24.242851	1257.289252	14.685530
24.415799	1256.139042	14.690547
23.872973	1260.317921	14.695565
24.056707	1261.198718	14.700583
24.159738	1260.525497	14.705600
23.366848	1264.425571	14.710618
23.733813	1259.315369	14.715635
23.840822	1262.201229	14.720653
24.170681	1259.145996	14.725671
24.027160	1262.457917	14.730688
23.859009	1278.961458	14.735706
24.307341	1278.875153	14.740723
23.943844	1289.685308	14.745741
24.292451	1287.305263	14.750759
24.690889	1289.317071	14.755776
24.675036	1289.973012	14.760794
24.460270	1284.909783	14.765811
24.370739	1285.510240	14.770829
24.474754	1281.909027	14.775847
24.859762	1269.596658	14.780864
24.766953	1272.128164	14.785882
24.902985	1268.270655	14.790899
24.792081	1269.618542	14.795917
24.843229	1262.711537	14.800935
25.251776	1265.545303	14.805952
24.782780	1264.113785	14.810970
24.872588	1241.612171	14.815987
24.574534	1239.548537	14.821005
24.279042	1240.314633	14.826023
24.614988	1244.655462	14.831040
24.521866	1251.016487	14.836058
25.316725	1260.210567	14.841075
24.847571	1255.821334	14.846093
24.857638	1250.918798	14.851111
25.039525	1247.411337	14.856128
25.057394	1242.831509	14.861146
24.951932	1238.969346	14.866163
24.830712	1240.606426	14.871181
24.969309	1236.539412	14.876199
25.131273	1246.279437	14.881216
24.800141	1243.841520	14.886234
24.970966	1229.929936	14.891251
25.057879	1243.452052	14.896269
25.055017	1243.120638	14.901287
25.538938	1242.643158	14.906304
24.964013	1243.043348	14.911322
24.984549	1243.850148	14.916339
25.049399	1243.186230	14.921357
25.090183	1242.713857	14.926375
25.970973	1247.145144	14.931392
25.529521	1249.993926	14.936410
25.428242	1235.478540	14.941427
25.078345	1239.901131	14.946445
24.981370	1242.991268	14.951463
24.923059	1241.827556	14.956480
25.241732	1240.386196	14.961498
25.436654	1239.338134	14.966515
25.190580	1245.756881	14.971533
25.008320	1248.003693	14.976551
25.225259	1249.866678	14.981568
25.025844	1248.225933	14.986586
25.121871	1244.585544	14.991603
25.075651	1259.455419	14.996621
25.336719	1274.988040	15.001639
25.546197	1264.029512	15.006656
25.454743	1274.733953	15.011674
25.482581	1276.460845	15.016691
25.414703	1271.098395	15.021709
25.168868	1267.408338	15.026727
25.723086	1267.636584	15.031744
25.443257	1278.701308	15.036762
25.462119	1271.659270	15.041779
25.337377	1278.793907	15.046797
25.653754	1277.315926	15.051815
25.620948	1278.092107	15.056832
25.793654	1275.233122	15.061850
25.720836	1273.200163	15.066867
25.906961	1275.735030	15.071885
25.590301	1276.772890	15.076903
25.893469	1272.940665	15.081920
25.450310	1274.541207	15.086938
25.142925	1270.154552	15.091955
25.658875	1292.574030	15.096973
25.435108	1296.671439	15.101991
25.893602	1300.688490	15.107008
25.725424	1307.323060	15.112026
25.884960	1306.362958	15.117043
25.893938	1301.513353	15.122061
25.978136	1298.697888	15.127079
25.706543	1299.840238	15.132096
25.778293	1299.906697	15.137114
26.014783	1299.951211	15.142131
26.186084	1297.304293	15.147149
25.764229	1299.222081	15.152167
26.467600	1317.456720	15.157184
25.809173	1307.751796	15.162202
26.254170	1319.597867	15.167219
26.412028	1321.339876	15.172237
26.598170	1313.145413	15.177255
26.520418	1301.171048	15.182272
25.935415	1307.246713	15.187290
25.715068	1302.966396	15.192307
26.052738	1307.575870	15.197325
26.569362	1329.136938	15.202343
26.766069	1332.098780	15.207360
26.838315	1315.435654	15.212378
26.782938	1305.511969	15.217395
26.768423	1307.017365	15.222413
26.866508	1307.289171	15.227431
26.783712	1294.967219	15.232448
26.726054	1306.236018	15.237466
27.189109	1295.196585	15.242483
26.784583	1275.648443	15.247501
26.498484	1272.561798	15.252519
26.605541	1265.312104	15.257536
26.609627	1266.437502	15.262554
26.416671	1267.630939	15.267571
26.293473	1264.753394	15.272589
26.360134	1282.597904	15.277607
26.556521	1291.955644	15.282624
26.885282	1299.360203	15.287642
26.814971	1298.801354	15.292659
26.948069	1291.243613	15.297677
26.281175	1295.003576	15.302695
26.733856	1296.326889	15.307712
26.804671	1304.362738	15.312730
26.107859	1296.251555	15.317747
26.445890	1299.036783	15.322765
26.487481	1309.966885	15.327783
26.880156	1299.306086	15.332800
26.799151	1306.641523	15.337818
27.150326	1323.387989	15.342835
27.036996	1318.181755	15.347853
26.797141	1319.969512	15.352871
26.771868	1323.553717	15.357888
26.917759	1336.718132	15.362906
26.822597	1326.035829	15.367923
26.900764	1325.327889	15.372941
26.528997	1330.764584	15.377959
27.056843	1323.820704	15.382976
26.780736	1331.161649	15.387994
26.761488	1330.090848	15.393011
27.135112	1335.833641	15.398029
27.173306	1357.342514	15.403047
27.456541	1352.876619	15.408064
27.556310	1359.865308	15.413082
27.174376	1335.804523	15.418099
27.361205	1335.197647	15.423117
27.383965	1329.918859	15.428135
27.520739	1326.058452	15.433152
27.283371	1320.400606	15.438170
27.244374	1324.007245	15.443187
27.509051	1328.324882	15.448205
27.500705	1343.652953	15.453223
27.684296	1332.292872	15.458240
27.739012	1331.486581	15.463258
27.505211	1337.679617	15.468275
27.515315	1323.773850	15.473293
27.544744	1326.287950	15.478311
27.734234	1317.495610	15.483328
27.493275	1321.112859	15.488346
27.647317	1322.247986	15.493363
28.202514	1322.763101	15.498381
28.089257	1331.985749	15.503399
27.949411	1331.483314	15.508416
28.110610	1328.006157	15.513434
27.948084	1333.264838	15.518451
28.245210	1327.406282	15.523469
27.718755	1329.132539	15.528487
27.641434	1335.199129	15.533504
27.636699	1329.555729	15.538522
27.265576	1333.854808	15.543539
27.605018	1323.960276	15.548557
27.310866	1329.558483	15.553575
27.667186	1338.830951	15.558592
27.829435	1361.085953	15.563610
28.018460	1361.149236	15.568627
28.352352	1357.108554	15.573645
28.259041	1356.083918	15.578663
28.374957	1360.818838	15.583680
28.028343	1345.875684	15.588698
27.752429	1336.782386	15.593715
28.254749	1351.263389	15.598733
28.235000	1362.615501	15.603751
28.046052	1357.095416	15.608768
28.212257	1359.935315	15.613786
28.271285	1362.341580	15.618803
28.334334	1365.207435	15.623821
28.362791	1367.595318	15.628839
28.274519	1369.323229	15.633856
28.528790	1364.962306	15.638874
28.009562	1359.091330	15.643891
27.926893	1352.009178	15.648909
28.058253	1361.946668	15.653927
28.259114	1363.248984	15.658944
28.103955	1363.577205	15.663962
28.369203	1363.356133	15.668979
28.019693	1347.209029	15.673997
27.977549	1367.407944	15.679015
28.408592	1380.430582	15.684032
28.489318	1381.119185	15.689050
28.540622	1394.750303	15.694067
28.661533	1383.768684	15.699085
28.520192	1386.167571	15.704103
28.691442	1386.158697	15.709120
28.736448	1384.565015	15.714138
28.381480	1381.001133	15.719155
28.897522	1383.482207	15.724173
28.560253	1386.655309	15.729191
28.771396	1380.849274	15.734208
28.943465	1382.636102	15.739226
28.673672	1383.280857	15.744243
29.084149	1369.783221	15.749261
29.196927	1381.190190	15.754279
28.857769	1381.154251	15.759296
29.026145	1384.541080	15.764314
28.859308	1380.350395	15.769331
28.793638	1380.747533	15.774349
28.577968	1382.798498	15.779367
29.195285	1389.702795	15.784384
29.429047	1377.430449	15.789402
28.782183	1385.342122	15.794419
29.338385	1382.902451	15.799437
28.874556	1387.525737	15.804455
28.842588	1396.939624	15.809472
28.859595	1410.604592	15.814490
29.399457	1414.387227	15.819507
29.549786	1417.635017	15.824525
29.402140	1420.478734	15.829543
29.291901	1414.581712	15.834560
29.468539	1416.476433	15.839578
28.978264	1425.536197	15.844595
29.379969	1422.135117	15.849613
29.756189	1421.076827	15.854631
29.638431	1413.629761	15.859648
29.491154	1412.558462	15.864666
29.503737	1433.565876	15.869683
29.440464	1417.867309	15.874701
29.576555	1416.961619	15.879719
29.796226	1416.453451	15.884736
29.739578	1407.972581	15.889754
29.067569	1415.153075	15.894771
29.611715	1414.682983	15.899789
29.341485	1412.473597	15.904807
29.427324	1412.926656	15.909824
29.578726	1413.750401	15.914842
29.354548	1407.757551	15.919859
29.580495	1403.650318	15.924877
29.738805	1417.495809	15.929895
29.523653	1413.486645	15.934912
29.623074	1417.808622	15.939930
29.599592	1437.054727	15.944947
29.622034	1447.437760	15.949965
29.494264	1433.589791	15.954983
29.847808	1437.648102	15.960000
30.197486	1427.591498	15.965018
30.284242	1430.170596	15.970035
30.587808	1427.345452	15.975053
30.536726	1430.404921	15.980071
30.717584	1410.408963	15.985088
30.507437	1397.854803	15.990106
30.280940	1404.002514	15.995123
30.429013	1388.458704	16.000141
30.595075	1388.163684	16.005159
30.579364	1393.718111	16.010176
30.748850	1398.302506	16.015194
30.493750	1376.999708	16.020211
30.265351	1361.102323	16.025229
30.234754	1351.659445	16.030247
30.661335	1354.355085	16.035264
30.787640	1350.540959	16.040282
30.572696	1358.199413	16.045299
30.143601	1354.930556	16.050317
30.400108	1358.210921	16.055335
30.871503	1357.081981	16.060352
30.460783	1352.496857	16.065370
30.222540	1355.509260	16.070387
30.284074	1356.036570	16.075405
30.563836	1356.200448	16.080423
30.256532	1357.271358	16.085440
30.495410	1370.326149	16.090458
30.360019	1381.924895	16.095475
30.199780	1389.306636	16.100493
30.634175	1387.512320	16.105511
30.544922	1388.806501	16.110528
30.717961	1389.603698	16.115546
30.338794	1395.853574	16.120563
30.817581	1390.395385	16.125581
31.188780	1395.991359	16.130599
30.636860	1392.983734	16.135616
30.803626	1393.059496	16.140634
30.353454	1397.916686	16.145651
30.638174	1402.872701	16.150669
30.786335	1415.159936	16.155687
31.196615	1429.132331	16.160704
31.446754	1423.849175	16.165722
31.195489	1431.409551	16.170739
31.269905	1429.516698	16.175757
31.537096	1409.581931	16.180775
30.906987	1403.760267	16.185792
31.149714	1398.841023	16.190810
31.079504	1400.043349	16.195827
30.884885	1397.997002	16.200845
31.469411	1411.614277	16.205863
31.642377	1440.008711	16.210880
31.409075	1420.192423	16.215898
30.940957	1404.939697	16.220915
31.358753	1417.112586	16.225933
31.472914	1424.988294	16.230951
31.275711	1437.242626	16.235968
31.288215	1430.726462	16.240986
31.300182	1436.849049	16.246003
31.193752	1436.203466	16.251021
31.313454	1436.963743	16.256039
31.066752	1428.822171	16.261056
31.567749	1434.296287	16.266074
31.276798	1432.638143	16.271091
31.381008	1431.942663	16.276109
31.567403	1431.361452	16.281127
31.312858	1435.261792	16.286144
31.753786	1441.629763	16.291162
31.898904	1454.375077	16.296179
31.883843	1454.309556	16.301197
31.855931	1432.649587	16.306215
31.441456	1444.456089	16.311232
31.850001	1453.869687	16.316250
32.228690	1462.020957	16.321267
31.642222	1461.978597	16.326285
32.137138	1462.768253	16.331303
31.796411	1467.335806	16.336320
32.011807	1459.247679	16.341338
32.167873	1454.924832	16.346355
32.159569	1453.890338	16.351373
32.062469	1456.365517	16.356391
32.027704	1460.110058	16.361408
31.972060	1452.505065	16.366426
31.930165	1460.499289	16.371443
32.197619	1448.797547	16.376461
32.432107	1455.724200	16.381479
32.256982	1467.921615	16.386496
32.242630	1464.863936	16.391514
32.134763	1465.277367	16.396531
32.264438	1466.267849	16.401549
31.969409	1459.919767	16.406567
31.954256	1465.747379	16.411584
31.850267	1458.846805	16.416602
32.046297	1465.878098	16.421619
31.970008	1485.239233	16.426637
32.584969	1483.589950	16.431655
32.567008	1496.866066	16.436672
32.756835	1488.530313	16.441690
32.383224	1488.592810	16.446707
32.869719	1493.995018	16.451725
32.618505	1491.088193	16.456743
32.572384	1497.177058	16.461760
32.693155	1491.523893	16.466778
32.610326	1495.866509	16.471795
32.589531	1499.694895	16.476813
32.801987	1492.387651	16.481831
32.725234	1491.677128	16.486848
32.878703	1482.663289	16.491866
32.575158	1491.773367	16.496883
32.359741	1496.468671	16.501901
32.964181	1486.951481	16.506919
32.762898	1502.029688	16.511936
32.984223	1492.789620	16.516954
32.971608	1500.203195	16.521971
32.968358	1499.500150	16.526989
33.203109	1499.797745	16.532007
33.210369	1498.671201	16.537024
33.372987	1484.422574	16.542042
33.225849	1479.302012	16.547059
33.022268	1475.969657	16.552077
33.483223	1477.566400	16.557095
33.379386	1480.021869	16.562112
33.304937	1484.770173	16.567130
33.219725	1482.655445	16.572147
33.255794	1482.460279	16.577165
32.948365	1479.717441	16.582183
33.140269	1493.003246	16.587200
33.836217	1499.360591	16.592218
33.966577	1485.732912	16.597235
33.760439	1486.592370	16.602253
33.784989	1469.975056	16.607271
33.815911	1470.707246	16.612288
33.478937	1471.181220	16.617306
33.257586	1464.891770	16.622323
33.064543	1469.882080	16.627341
33.553849	1468.470506	16.632359
33.344548	1478.439309	16.637376
33.678365	1492.904449	16.642394
33.782383	1502.569128	16.647411
33.545939	1506.203757	16.652429
34.006866	1499.375616	16.657447
33.778596	1500.373135	16.662464
33.699228	1498.670831	16.667482
33.669958	1500.161451	16.672499
33.605797	1507.217687	16.677517
33.884242	1492.287707	16.682535
33.971738	1504.614551	16.687552
33.828464	1506.901964	16.692570
34.321926	1499.036248	16.697587
33.979626	1507.580873	16.702605
34.179603	1498.888613	16.707623
34.162934	1500.461333	16.712640
34.166888	1494.754172	16.717658
34.545502	1487.688155	16.722675
34.187345	1493.571831	16.727693
34.405696	1487.082168	16.732711
34.091772	1492.419228	16.737728
34.154183	1494.497340	16.742746
34.437735	1490.206961	16.747763
34.426622	1500.139042	16.752781
34.337751	1492.062117	16.757799
34.332094	1496.124151	16.762816
34.511576	1496.913556	16.767834
34.544960	1496.951945	16.772851
34.105967	1510.582968	16.777869
34.512502	1490.453323	16.782887
34.437096	1508.635080	16.787904
34.412363	1525.941543	16.792922
34.908368	1526.211277	16.797939
34.988860	1528.697754	16.802957
35.009092	1514.147100	16.807975
34.566382	1510.398210	16.812992
34.604018	1506.230707	16.818010
34.426714	1500.473905	16.823027
34.276373	1526.090562	16.828045
35.022883	1521.362493	16.833063
34.836191	1529.509545	16.838080
34.528638	1531.106155	16.843098
34.647801	1533.804530	16.848115
34.402521	1536.124005	16.853133
35.084373	1524.858690	16.858151
34.939069	1527.821722	16.863168
34.851325	1531.619463	16.868186
34.880749	1535.101023	16.873203
34.870997	1556.393170	16.878221
34.997942	1554.012504	16.883239
35.257942	1567.193773	16.888256
35.340796	1562.586172	16.893274
35.813839	1553.867932	16.898291
35.728155	1560.456178	16.903309
35.548251	1540.580183	16.908327
35.551593	1536.600067	16.913344
35.499274	1533.062613	16.918362
35.533334	1526.324580	16.923379
35.001331	1538.180046	16.928397
35.135094	1530.422054	16.933415
35.402637	1539.844129	16.938432
35.233407	1561.001798	16.943450
35.543217	1540.420512	16.948467
35.576323	1550.466316	16.953485
35.755387	1558.123855	16.958503
35.810084	1557.988888	16.963520
35.678722	1552.130872	16.968538
35.755106	1544.864259	16.973555
35.735880	1546.634293	16.978573
35.908249	1543.502061	16.983591
35.928967	1545.952721	16.988608
35.728383	1548.301941	16.993626
35.626672	1554.246013	16.998643
35.628221	1557.457917	17.003661
35.820269	1552.472898	17.008679
36.157961	1546.532100	17.013696
36.256203	1551.048826	17.018714
36.624541	1544.539329	17.023731
36.367484	1554.471088	17.028749
36.558633	1555.964083	17.033767
36.541621	1556.296971	17.038784
36.410231	1554.955980	17.043802
36.507135	1529.381540	17.048819
36.197113	1516.656592	17.053837
35.818368	1518.893425	17.058855
35.938522	1535.910463	17.063872
36.238549	1547.891026	17.068890
36.264837	1546.696249	17.073907
36.005924	1551.291141	17.078925
36.183393	1546.025522	17.083943
36.516065	1553.446464	17.088960
36.223204	1555.946559	17.093978
36.309701	1551.254076	17.098995
35.934397	1557.384443	17.104013
36.162866	1564.010570	17.109031
35.990556	1580.247396	17.114048
36.338017	1583.155483	17.119066
36.747077	1576.307065	17.124083
36.501954	1586.055282	17.129101
36.501988	1586.607713	17.134119
36.537619	1577.808927	17.139136
36.599768	1583.480794	17.144154
36.657585	1593.640119	17.149171
36.818852	1615.001066	17.154189
36.865913	1602.945220	17.159207
37.242760	1605.117484	17.164224
36.980836	1610.437793	17.169242
37.509521	1607.384235	17.174259
37.273562	1604.045198	17.179277
36.910534	1600.840953	17.184295
37.405008	1601.204662	17.189312
37.103974	1595.952162	17.194330
37.102145	1581.270962	17.199347
37.065110	1586.055800	17.204365
37.368481	1592.171404	17.209383
37.614025	1604.249944	17.214400
37.097897	1601.151485	17.219418
37.230347	1596.504659	17.224435
37.202524	1602.032099	17.229453
37.233580	1597.609373	17.234471
37.423649	1599.141144	17.239488
37.228120	1601.977747	17.244506
37.255488	1596.430333	17.249523
37.522087	1600.895764	17.254541
37.441747	1603.379904	17.259559
37.373837	1597.578716	17.264576
37.492804	1601.535543	17.269594
37.547726	1595.148273	17.274611
37.496333	1610.821426	17.279629
37.272469	1630.861266	17.284647
38.029840	1632.708419	17.289664
37.661044	1633.447331	17.294682
37.794333	1631.365206	17.299699
37.831125	1627.837651	17.304717
37.898870	1632.702581	17.309735
38.095467	1627.541148	17.314752
37.631993	1631.589969	17.319770
38.063584	1636.309831	17.324787
38.180390	1636.989897	17.329805
37.729814	1631.402748	17.334823
38.207050	1635.675758	17.339840
38.158047	1640.217755	17.344858
37.982014	1630.452362	17.349875
38.153080	1630.895146	17.354893
38.088725	1628.016500	17.359911
38.225097	1627.974627	17.364928
37.885962	1649.447798	17.369946
38.432224	1653.484149	17.374963
38.711520	1667.479217	17.379981
38.445921	1661.586296	17.384999
38.351821	1665.103237	17.390016
38.506977	1671.436433	17.395034
38.344462	1663.879978	17.400051
38.695769	1665.284493	17.405069
38.622773	1668.785217	17.410087
39.252699	1659.837242	17.415104
38.788336	1655.481328	17.420122
38.626728	1643.034015	17.425139
38.249870	1644.320828	17.430157
38.729006	1659.300244	17.435175
38.720526	1668.759092	17.440192
38.614337	1660.710643	17.445210
38.734842	1661.860208	17.450227
38.721329	1663.443428	17.455245
38.657896	1656.610625	17.460263
38.885038	1655.825547	17.465280
38.779963	1666.544010	17.470298
38.727245	1660.574033	17.475315
38.905040	1668.400761	17.480333
38.727810	1684.895655	17.485351
39.363705	1685.601697	17.490368
39.061589	1692.210176	17.495386
39.128481	1686.542554	17.500403
39.464515	1691.914717	17.505421
39.074635	1683.206546	17.510439
39.218291	1683.794205	17.515456
39.354933	1684.303530	17.520474
39.090364	1687.075599	17.525491
39.253824	1673.956313	17.530509
39.410149	1689.226566	17.535527
39.908502	1676.053798	17.540544
39.710801	1677.063805	17.545562
39.345299	1681.754972	17.550579
39.723052	1671.535113	17.555597
39.333032	1683.332482	17.560615
39.665590	1679.908948	17.565632
39.746561	1697.173853	17.570650
39.511014	1708.705358	17.575667
39.589232	1706.492491	17.580685
39.393409	1706.574117	17.585703
39.828600	1704.248072	17.590720
39.881278	1711.487934	17.595738
39.849715	1712.615539	17.600755
39.456850	1712.263570	17.605773
39.554615	1719.263789	17.610791
39.707803	1706.689215	17.615808
39.964190	1719.761378	17.620826
40.211779	1736.577630	17.625843
40.777162	1725.237643	17.630861
40.173936	1716.824330	17.635879
40.453550	1706.531107	17.640896
40.258387	1704.332431	17.645914
40.382601	1703.059428	17.650931
40.541863	1695.345413	17.655949
40.313394	1700.625367	17.660967
40.354278	1695.053944	17.665984
40.526234	1700.543622	17.671002
40.502894	1697.042505	17.676019
40.594149	1693.133901	17.681037
40.419322	1694.799120	17.686055
40.796584	1700.349278	17.691072
40.901443	1698.840195	17.696090
40.697151	1698.168067	17.701107
40.768095	1695.471353	17.706125
40.588852	1701.590209	17.711143
40.873467	1703.696795	17.716160
40.579566	1707.601194	17.721178
40.918889	1723.493724	17.726195
41.352877	1721.078896	17.731213
40.974343	1719.623159	17.736231
40.951286	1708.340761	17.741248
41.049621	1714.000566	17.746266
40.730465	1704.395507	17.751283
41.044681	1714.543631	17.756301
40.922976	1737.034885	17.761319
41.205197	1725.989538	17.766336
41.232605	1739.238000	17.771354
41.191803	1743.496698	17.776371
41.487946	1729.895113	17.781389
41.111911	1732.961531	17.786407
41.264515	1732.299478	17.791424
41.715349	1732.327326	17.796442
41.752288	1729.377351	17.801459
41.448207	1724.254873	17.806477
41.160024	1738.990290	17.811495
41.295318	1733.554260	17.816512
41.350504	1731.083890	17.821530
41.195212	1735.270079	17.826547
41.526733	1735.820411	17.831565
41.380906	1732.856096	17.836583
41.170469	1739.416982	17.841600
41.507584	1753.063591	17.846618
41.293767	1767.623273	17.851635
41.816713	1763.856805	17.856653
41.702914	1769.734518	17.861671
41.739014	1762.303430	17.866688
41.976945	1758.600792	17.871706
42.072161	1765.150233	17.876723
42.419362	1765.276568	17.881741
42.342755	1762.102324	17.886759
42.667998	1757.305846	17.891776
42.474448	1758.892381	17.896794
42.363231	1751.427888	17.901811
42.769011	1735.669056	17.906829
42.134361	1728.993613	17.911847
42.393627	1716.616223	17.916864
42.104680	1711.732915	17.921882
42.148682	1726.207012	17.926899
42.177769	1729.882397	17.931917
42.495478	1754.878171	17.936935
42.487716	1753.819546	17.941952
42.638925	1747.602342	17.946970
42.324097	1754.605592	17.951987
42.377927	1746.359957	17.957005
42.699320	1749.315070	17.962023
42.636146	1746.401157	17.967040
43.203804	1745.528948	17.972058
43.194614	1753.505903	17.977075
43.329247	1745.078284	17.982093
42.836597	1729.391203	17.987111
42.765981	1722.732063	17.992128
42.617914	1720.763528	17.997146
42.406789	1740.350877	18.002163
42.971577	1739.989458	18.007181
42.641742	1749.915706	18.012199
42.836451	1751.777052	18.017216
42.926206	1747.106789	18.022234
42.625402	1755.713340	18.027251
42.832067	1747.928960	18.032269
43.145220	1758.417099	18.037287
43.043006	1772.945840	18.042304
43.263918	1769.304392	18.047322
43.089483	1780.600641	18.052339
43.206533	1774.204221	18.057357
42.887307	1792.663967	18.062375
43.045720	1785.599346	18.067392
43.358120	1773.737669	18.072410
43.286953	1783.254978	18.077427
43.702088	1800.465460	18.082445
43.775490	1809.705998	18.087463
43.943206	1812.517372	18.092480
43.782514	1790.524905	18.097498
43.435813	1788.929041	18.102515
43.339368	1788.644373	18.107533
43.783892	1808.307999	18.112551
44.037428	1810.688859	18.117568
43.873475	1808.179662	18.122586
43.505669	1808.197063	18.127603
44.091502	1799.287675	18.132621
43.942238	1801.527333	18.137639
44.026725	1812.829612	18.142656
43.731777	1813.998839	18.147674
43.824939	1819.507975	18.152691
44.304641	1806.487921	18.157709
44.141788	1814.774752	18.162727
44.105284	1812.840233	18.167744
44.185252	1807.498319	18.172762
44.048784	1815.440821	18.177779
44.177162	1816.011811	18.182797
44.034380	1832.881316	18.187815
44.311056	1843.347810	18.192832
44.321178	1836.765736	18.197850
44.252738	1836.876709	18.202867
44.463616	1834.537129	18.207885
44.671366	1835.341000	18.212903
44.849605	1833.714979	18.217920
45.111278	1822.330919	18.222938
45.430287	1829.865373	18.227955
45.103766	1824.855778	18.232973
45.163890	1819.218405	18.237991
45.183626	1810.534432	18.243008
45.217242	1796.960082	18.248026
44.976624	1798.426723	18.253043
45.259780	1788.690781	18.258061
44.951908	1793.617012	18.263079
44.946616	1797.127025	18.268096
45.141434	1788.120097	18.273114
45.107770	1790.032022	18.278131
45.328082	1788.741354	18.283149
45.423821	1794.502039	18.288167
45.329587	1792.944788	18.293184
45.342169	1793.821099	18.298202
45.032387	1793.012703	18.303219
45.253026	1783.396552	18.308237
45.241235	1788.122787	18.313255
45.101753	1806.702932	18.318272
45.384211	1820.717283	18.323290
45.275936	1830.525270	18.328307
45.308811	1824.625999	18.333325
45.451424	1827.761405	18.338343
45.275559	1827.955765	18.343360
45.567155	1824.929035	18.348378
45.462980	1825.169773	18.353395
45.935789	1837.142198	18.358413
46.054621	1836.518613	18.363431
45.831462	1835.501244	18.368448
46.175958	1821.838133	18.373466
46.117661	1829.751096	18.378483
45.911729	1827.401081	18.383501
45.852145	1830.072666	18.388519
45.936367	1839.060549	18.393536
45.968879	1846.017281	18.398554
46.051943	1854.203301	18.403571
45.808349	1854.263980	18.408589
46.183994	1854.291333	18.413607
46.225665	1848.328332	18.418624
46.064070	1844.480367	18.423642
45.845123	1851.461315	18.428659
45.921402	1858.741300	18.433677
46.010027	1871.446634	18.438695
46.417727	1883.312919	18.443712
46.713307	1880.005933	18.448730
46.348524	1885.342394	18.453747
46.294222	1883.846801	18.458765
46.554481	1879.402417	18.463783
46.411354	1884.326811	18.468800
46.743811	1875.323797	18.473818
46.685337	1877.592000	18.478835
46.832391	1883.588045	18.483853
46.960822	1873.375365	18.488871
47.058327	1883.493817	18.493888
47.099628	1881.606981	18.498906
46.749150	1886.203889	18.503923
46.943940	1894.821226	18.508941
47.249146	1901.061063	18.513959
46.913854	1912.690144	18.518976
47.066745	1908.245654	18.523994
46.976901	1917.932804	18.529011
47.118628	1909.948033	18.534029
47.352460	1914.223872	18.539047
47.150147	1915.177591	18.544064
47.605908	1902.330088	18.549082
47.355982	1914.376874	18.554099
47.421405	1908.064064	18.559117
47.529583	1902.489692	18.564135
47.387718	1914.449438	18.569152
47.429638	1902.517882	18.574170
47.638292	1917.296646	18.579187
47.373954	1930.566547	18.584205
47.750448	1941.298313	18.589223
47.487130	1943.754029	18.594240
48.034762	1936.492276	18.599258
47.772763	1934.390864	18.604275
47.671694	1938.872968	18.609293
48.329052	1934.915676	18.614311
48.129770	1935.268404	18.619328
48.247105	1930.044861	18.624346
48.151938	1934.691327	18.629363
47.781509	1936.114480	18.634381
48.225789	1931.235722	18.639399
47.830297	1940.587443	18.644416
48.295912	1935.825120	18.649434
48.217290	1939.055573	18.654451
48.181003	1934.552553	18.659469
48.228460	1947.789880	18.664487
48.047995	1961.183634	18.669504
48.206196	1973.303817	18.674522
48.602075	1972.246848	18.679539
48.482290	1964.493919	18.684557
48.741582	1967.753462	18.689575
48.625946	1971.452140	18.694592
48.719340	1959.833411	18.699610
48.869771	1960.396689	18.704627
48.823425	1971.615202	18.709645
49.134168	1959.562698	18.714663
48.657890	1965.387656	18.719680
48.723409	1966.120631	18.724698
48.789255	1968.115923	18.729715
48.780299	1973.501265	18.734733
48.795157	1972.687993	18.739751
49.065198	1988.906100	18.744768
49.078980	1994.677761	18.749786
49.105797	1990.765955	18.754803
49.267736	1994.828522	18.759821
49.346325	1997.491803	18.764839
49.303227	1996.756979	18.769856
49.591693	1997.364318	18.774874
49.244070	1994.271143	18.779891
49.318265	1996.721368	18.784909
49.660838	1988.380031	18.789927
49.267671	1995.163717	18.794944
49.530871	1986.430029	18.799962
49.624493	1986.932960	18.804979
49.593328	2001.677320	18.809997
49.792412	1990.210156	18.815015
49.546680	1996.057811	18.820032
49.546478	2000.165110	18.825050
50.114461	2016.254988	18.830067
50.007575	2022.835644	18.835085
50.054868	2024.496676	18.840103
50.093766	2020.498923	18.845120
50.280259	2018.521814	18.850138
50.049536	2019.046885	18.855155
49.974146	2020.095794	18.860173
50.138459	2019.762870	18.865191
50.057664	2020.372094	18.870208
50.155673	2019.980844	18.875226
50.069109	2020.221321	18.880243
49.778959	2023.853069	18.885261
50.114637	2025.799743	18.890279
50.077855	2050.973320	18.895296
50.100106	2054.620027	18.900314
50.573190	2045.740858	18.905331
50.328855	2058.099831	18.910349
50.545165	2047.223062	18.915367
50.527410	2054.592892	18.920384
50.668186	2055.084983	18.925402
51.238248	2064.353921	18.930419
51.343325	2051.176604	18.935437
51.445955	2036.753483	18.940455
51.440087	2033.624544	18.945472
51.745290	2032.689432	18.950490
51.619073	2029.086572	18.955507
51.190999	2033.937803	18.960525
51.677123	2036.468611	18.965543
51.447261	2021.463445	18.970560
51.539605	2009.680664	18.975578
51.736725	2005.826676	18.980595
51.824649	2008.092241	18.985613
51.751495	1997.602583	18.990631
51.338041	2008.587566	18.995648
51.424440	2005.492820	19.000666
51.383877	1998.359448	19.005683
51.339380	2002.940547	19.010701
51.450462	1999.521842	19.015719
51.289542	2002.154524	19.020736
51.713748	2013.321528	19.025754
52.050112	2018.870939	19.030771
51.952391	2025.625639	19.035789
51.845221	2005.947633	19.040807
51.944434	2018.276417	19.045824
52.017595	2030.924682	19.050842
51.696380	2036.233249	19.055859
51.501348	2045.323072	19.060877
52.082147	2033.534096	19.065895
51.922604	2041.590920	19.070912
51.804291	2044.387588	19.075930
51.810710	2043.097347	19.080947
51.921942	2049.361445	19.085965
52.482253	2064.621470	19.090983
52.184943	2078.775225	19.096000
52.148055	2079.977007	19.101018
52.392356	2072.238778	19.106035
52.067830	2074.412053	19.111053
52.032059	2076.478332	19.116071
52.420207	2074.522556	19.121088
52.280770	2080.400844	19.126106
52.155086	2098.042615	19.131123
52.257598	2090.031401	19.136141
52.406619	2092.575520	19.141159
52.730425	2098.615764	19.146176
52.599128	2108.140429	19.151194
53.102872	2114.344738	19.156211
53.165815	2123.617969	19.161229
53.138701	2117.040585	19.166247
53.068619	2120.593280	19.171264
53.139025	2121.754619	19.176282
53.242339	2117.164612	19.181299
53.178382	2117.668575	19.186317
53.418413	2104.575178	19.191335
53.383206	2106.745316	19.196352
53.433628	2110.059207	19.201370
53.541709	2110.710077	19.206387
53.507896	2115.083442	19.211405
53.799979	2099.674496	19.216423
53.809152	2104.278316	19.221440
53.698659	2107.372516	19.226458
54.017279	2101.617091	19.231475
53.777762	2103.152871	19.236493
53.867319	2103.584838	19.241511
53.771154	2099.992165	19.246528
53.521026	2101.305323	19.251546
53.960559	2095.171245	19.256563
53.514078	2102.334248	19.261581
54.090796	2118.154192	19.266599
54.186142	2117.325932	19.271616
54.088844	2128.393033	19.276634
54.047778	2127.774801	19.281651
54.220606	2131.485093	19.286669
54.424748	2128.663879	19.291687
54.402999	2128.980265	19.296704
54.431743	2130.302314	19.301722
54.962240	2118.033246	19.306739
54.854567	2128.838310	19.311757
54.809663	2130.358052	19.316775
54.812735	2128.065870	19.321792
54.582041	2123.584315	19.326810
55.089981	2131.110149	19.331827
54.685972	2112.750801	19.336845
55.151048	2113.787773	19.341863
55.040543	2109.386417	19.346880
54.645302	2101.873587	19.351898
54.846598	2110.076484	19.356915
54.908721	2122.671589	19.361933
54.932648	2124.418933	19.366951
55.043902	2114.511841	19.371968
55.054029	2128.857847	19.376986
55.044364	2114.381850	19.382003
55.370942	2122.461684	19.387021
55.096266	2130.601294	19.392039
55.153364	2120.605044	19.397056
55.022221	2135.007564	19.402074
55.420632	2133.973777	19.407091
55.331216	2159.466835	19.412109
55.142109	2156.536634	19.417127
55.313886	2158.486226	19.422144
55.436482	2164.476335	19.427162
55.349607	2162.306673	19.432179
55.086450	2168.175492	19.437197
55.400301	2182.755342	19.442215
55.429957	2188.926774	19.447232
55.869320	2174.747807	19.452250
56.353474	2167.659061	19.457267
56.207019	2168.663856	19.462285
56.144031	2174.249503	19.467303
56.319464	2169.063564	19.472320
56.303480	2169.435664	19.477338
56.977580	2167.330049	19.482355
57.039822	2166.640552	19.487373
56.805378	2161.921798	19.492391
56.834668	2159.540853	19.497408
56.818735	2161.911661	19.502426
57.079650	2145.310988	19.507443
57.115284	2136.832013	19.512461
56.468072	2130.411340	19.517479
56.940849	2125.698134	19.522496
56.950453	2131.887944	19.527514
56.993034	2136.217504	19.532531
56.792422	2133.616100	19.537549
56.541661	2133.804797	19.542567
56.939943	2136.488104	19.547584
56.555629	2137.023368	19.552602
56.893323	2143.448313	19.557619
56.972674	2158.707021	19.562637
57.016445	2167.146435	19.567655
57.400820	2162.774406	19.572672
56.937135	2167.542794	19.577690
56.928068	2159.670771	19.582707
57.036285	2164.594686	19.587725
57.118218	2166.034408	19.592743
57.054947	2168.852768	19.597760
57.003482	2189.102380	19.602778
57.581957	2200.519094	19.607795
57.314129	2200.995800	19.612813
57.175740	2208.635635	19.617831
57.526214	2200.173523	19.622848
57.445454	2211.751310	19.627866
57.727771	2222.014700	19.632883
57.752771	2236.521271	19.637901
57.597593	2241.630548	19.642919
57.770995	2238.405074	19.647936
57.801642	2243.077706	19.652954
58.024014	2229.261926	19.657971
58.180553	2231.449608	19.662989
58.155113	2232.084788	19.668007
58.495553	2237.550101	19.673024
58.326536	2250.522784	19.678042
58.400720	2255.392710	19.683059
58.505632	2273.954738	19.688077
58.793300	2274.676416	19.693095
59.026643	2258.623742	19.698112
58.757136	2249.333898	19.703130
58.222258	2237.149745	19.708147
58.470204	2246.753589	19.713165
58.338621	2265.816066	19.718183
58.382344	2262.341914	19.723200
58.411524	2270.354685	19.728218
58.626127	2268.151432	19.733235
58.585666	2281.796694	19.738253
58.500196	2293.317860	19.743271
59.006695	2288.821693	19.748288
59.181346	2292.336405	19.753306
59.312594	2282.822690	19.758323
59.140379	2284.497366	19.763341
59.464007	2285.233354	19.768359
59.339279	2279.843685	19.773376
59.375641	2287.682766	19.778394
59.597074	2285.680734	19.783411
59.761817	2291.903073	19.788429
59.377230	2288.847283	19.793447
59.721068	2299.716019	19.798464
59.543937	2313.954120	19.803482
59.568955	2315.167358	19.808499
59.650738	2315.397483	19.813517
59.529420	2316.186920	19.818535
59.656914	2312.843299	19.823552
59.673343	2317.482164	19.828570
60.018248	2317.465571	19.833587
60.078335	2322.279659	19.838605
60.065742	2324.545178	19.843623
60.395562	2334.599678	19.848640
60.102469	2340.266574	19.853658
60.069819	2345.591922	19.858675
60.815551	2338.219633	19.863693
60.674561	2344.841710	19.868711
60.745335	2340.336756	19.873728
60.632088	2347.116307	19.878746
60.780719	2337.316857	19.883763
60.716794	2342.244354	19.888781
60.663854	2347.946468	19.893799
60.950050	2336.360163	19.898816
60.964254	2345.968705	19.903834
60.796920	2339.127822	19.908851
60.910074	2346.163091	19.913869
60.435538	2346.423232	19.918887
60.490316	2343.619713	19.923904
60.811902	2335.467254	19.928922
60.687023	2343.409611	19.933939
61.289132	2360.750098	19.938957
61.236976	2371.657639	19.943975
61.344750	2368.785964	19.948992
61.520920	2369.043222	19.954010
61.412867	2374.665017	19.959027
61.788653	2365.103027	19.964045
61.200838	2359.115453	19.969063
61.448797	2361.834023	19.974080
61.721443	2367.424409	19.979098
61.843297	2358.563544	19.984115
62.025653	2359.198541	19.989133
62.014669	2361.262183	19.994151
62.405702	2347.459122	19.999168
62.263369	2348.442745	20.004186
62.281680	2355.824253	20.009203
62.501328	2353.016879	20.014221
62.358199	2357.124756	20.019239
62.654633	2348.889975	20.024256
62.750714	2352.389820	20.029274
62.701548	2354.609637	20.034291
62.838134	2347.401633	20.039309
62.714514	2349.598776	20.044327
62.902681	2331.521168	20.049344
62.766289	2317.590414	20.054362
62.777604	2320.069191	20.059379
62.887712	2311.745883	20.064397
62.587401	2315.557813	20.069415
62.536120	2313.951407	20.074432
63.017354	2330.012382	20.079450
62.925674	2343.588515	20.084467
63.177159	2336.974299	20.089485
62.991868	2349.504902	20.094503
63.180997	2344.514227	20.099520
63.158194	2343.389626	20.104538
62.882214	2354.126047	20.109555
63.148801	2351.479944	20.114573
63.015265	2351.280770	20.119591
62.951661	2348.687341	20.124608
62.975650	2351.941237	20.129626
63.157074	2373.486803	20.134643
62.833050	2378.225796	20.139661
63.036715	2390.047123	20.144679
63.256166	2376.991679	20.149696
63.377222	2396.989110	20.154714
62.855400	2405.913874	20.159731
63.271715	2408.465770	20.164749
63.015443	2419.068126	20.169767
63.148054	2432.425537	20.174784
63.653561	2437.764967	20.179802
63.811244	2444.300439	20.184819
64.768644	2448.511042	20.189837
64.363273	2456.153457	20.194855
64.249152	2449.390818	20.199872
64.344493	2457.848322	20.204890
63.977581	2455.805384	20.209907
64.577273	2464.200048	20.214925
64.720376	2474.130720	20.219943
64.694694	2479.764418	20.224960
64.719614	2483.686010	20.229978
65.210824	2476.012356	20.234995
65.449037	2474.169655	20.240013
65.151184	2464.979835	20.245031
64.553952	2446.871368	20.250048
64.834282	2444.183516	20.255066
64.707606	2472.105914	20.260083
65.008559	2477.806467	20.265101
64.716099	2478.985944	20.270119
65.274763	2479.705273	20.275136
64.904986	2475.129331	20.280154
64.666295	2479.706455	20.285171
64.883048	2486.084549	20.290189
64.883755	2501.120026	20.295207
65.040486	2504.306307	20.300224
65.471306	2499.272571	20.305242
65.354999	2513.880016	20.310259
65.580901	2532.768122	20.315277
65.777921	2527.812263	20.320295
66.084820	2524.507141	20.325312
66.218064	2524.444147	20.330330
65.511214	2531.455493	20.335347
66.195897	2531.430261	20.340365
66.680843	2532.615064	20.345383
66.426780	2536.664828	20.350400
66.498889	2525.346625	20.355418
66.427658	2532.068650	20.360435
66.446965	2522.440102	20.365453
66.141989	2531.231679	20.370471
65.908293	2528.876866	20.375488
66.308571	2524.573678	20.380506
66.081673	2527.420942	20.385523
66.589807	2521.920324	20.390541
66.910037	2528.625634	20.395559
66.079569	2523.633303	20.400576
66.251535	2527.550171	20.405594
66.449706	2553.296187	20.410611
66.818132	2555.861044	20.415629
66.406516	2557.934334	20.420647
66.617448	2560.030046	20.425664
66.852727	2581.013813	20.430682
66.870445	2590.094251	20.435699
67.122505	2584.216181	20.440717
67.108963	2584.561884	20.445735
67.186659	2592.746848	20.450752
67.345991	2579.209332	20.455770
67.364778	2587.469759	20.460787
68.005574	2596.894636	20.465805
68.138259	2588.730331	20.470823
67.943223	2572.226281	20.475840
68.298359	2565.683978	20.480858
67.716560	2570.045891	20.485875
67.808540	2559.785856	20.490893
68.383554	2560.362204	20.495911
68.229188	2570.619575	20.500928
68.254045	2561.531877	20.505946
68.234862	2576.817337	20.510963
67.939674	2571.253607	20.515981
68.076934	2572.299564	20.520999
68.211258	2587.064929	20.526016
68.803515	2593.321985	20.531034
68.649844	2595.655045	20.536051
68.734444	2596.257198	20.541069
68.553408	2593.542104	20.546087
68.568564	2595.636734	20.551104
68.592385	2591.954073	20.556122
68.525439	2592.503453	20.561139
68.763231	2590.826194	20.566157
68.874529	2595.727666	20.571175
68.615559	2592.824324	20.576192
68.852037	2588.183784	20.581210
68.680442	2612.717482	20.586227
69.208435	2614.858072	20.591245
69.201219	2627.355215	20.596263
69.023752	2630.260176	20.601280
69.035461	2621.595244	20.606298
69.085663	2625.409370	20.611315
69.169764	2632.842731	20.616333
69.462579	2647.529003	20.621351
69.391749	2653.802900	20.626368
69.582060	2656.620398	20.631386
69.147253	2656.103515	20.636403
69.640912	2654.646996	20.641421
69.838550	2663.465880	20.646439
69.721902	2671.233731	20.651456
70.336279	2677.708328	20.656474
70.160555	2685.961990	20.661491
70.322264	2684.010313	20.666509
70.858140	2679.167995	20.671527
70.247629	2666.445979	20.676544
70.428192	2669.651047	20.681562
70.241309	2675.632195	20.686579
70.381038	2680.613086	20.691597
70.647333	2682.422108	20.696615
70.545059	2684.873164	20.701632
70.604923	2681.400876	20.706650
70.744005	2678.889986	20.711667
70.777104	2675.375824	20.716685
70.827245	2674.808086	20.721703
70.818244	2678.022029	20.726720
71.239322	2665.235770	20.731738
71.084587	2673.492127	20.736755
71.186346	2677.187170	20.741773
71.216594	2677.991592	20.746791
70.912780	2679.896782	20.751808
70.925489	2700.562111	20.756826
70.835487	2709.671324	20.761843
71.180333	2710.898275	20.766861
71.022967	2710.833914	20.771879
71.041500	2734.662642	20.776896
71.653081	2742.184394	20.781914
71.300766	2741.975471	20.786931
71.469933	2753.019378	20.791949
71.788039	2744.894869	20.796967
71.719197	2770.691746	20.801984
72.268494	2769.496594	20.807002
72.454159	2770.088514	20.812019
72.532074	2762.124096	20.817037
72.550849	2763.850344	20.822055
72.425896	2773.809837	20.827072
72.669443	2759.264632	20.832090
72.849397	2761.957917	20.837107
72.833310	2749.537145	20.842125
73.004771	2730.895697	20.847143
72.742409	2726.248499	20.852160
72.560217	2708.817526	20.857178
73.263617	2724.429720	20.862195
73.026209	2725.926607	20.867213
73.341298	2723.976980	20.872231
72.705122	2725.192565	20.877248
72.782764	2724.992619	20.882266
73.199658	2749.401222	20.887283
73.397661	2750.321008	20.892301
73.451796	2747.059175	20.897319
73.145878	2758.058531	20.902336
73.341838	2754.083279	20.907354
73.395032	2754.804228	20.912371
73.276107	2760.265790	20.917389
73.155368	2758.566503	20.922407
73.328759	2760.015802	20.927424
73.631046	2780.021241	20.932442
73.820801	2791.201829	20.937459
73.923364	2786.648770	20.942477
74.094424	2782.840802	20.947495
74.022029	2791.003562	20.952512
73.984970	2787.821935	20.957530
74.101844	2783.002594	20.962547
74.278568	2782.599800	20.967565
74.322424	2787.881467	20.972583
74.242547	2795.073677	20.977600
74.019212	2778.441166	20.982618
74.323927	2798.286339	20.987635
74.367692	2810.896958	20.992653
74.471843	2807.454852	20.997671
75.002007	2824.394728	21.002688
74.631625	2819.582522	21.007706
74.654640	2810.409941	21.012723
74.933947	2816.328542	21.017741
74.931917	2816.493502	21.022759
74.903519	2819.847046	21.027776
75.152367	2833.877126	21.032794
75.249934	2838.013954	21.037811
75.286641	2846.934562	21.042829
75.399781	2846.655287	21.047847
75.281518	2851.270938	21.052864
75.231131	2851.021274	21.057882
75.148192	2855.978179	21.062899
75.444210	2852.722896	21.067917
75.566638	2867.619723	21.072935
75.667170	2876.534919	21.077952
75.787705	2880.235454	21.082970
76.054128	2877.708213	21.087987
75.831415	2887.780619	21.093005
75.888632	2878.891954	21.098023
75.688842	2883.164042	21.103040
75.643864	2891.021308	21.108058
75.826995	2905.847123	21.113075
76.075291	2906.171568	21.118093
76.462491	2912.928567	21.123111
76.011543	2909.187831	21.128128
76.813811	2924.786426	21.133146
77.136293	2922.195225	21.138163
76.953648	2927.338572	21.143181
77.398749	2918.295177	21.148199
77.246567	2917.240757	21.153216
77.235845	2899.406873	21.158234
77.241302	2897.337837	21.163251
77.188688	2895.665444	21.168269
77.331674	2894.761247	21.173287
77.185285	2905.068659	21.178304
77.114622	2917.317017	21.183322
77.409129	2921.950915	21.188339
77.407206	2921.313339	21.193357
77.425935	2919.593273	21.198375
77.122512	2927.122353	21.203392
77.338123	2930.779822	21.208410
77.508726	2932.144560	21.213427
77.374688	2950.749931	21.218445
77.839204	2952.729766	21.223463
77.726335	2959.878879	21.228480
77.673967	2958.473420	21.233498
77.914150	2957.667538	21.238515
77.980898	2975.576180	21.243533
78.387931	2971.949014	21.248551
78.457669	2980.532473	21.253568
78.654874	2973.719383	21.258586
79.105010	2977.672942	21.263603
78.801734	2975.863953	21.268621
79.125447	2964.060479	21.273639
78.973214	2950.134242	21.278656
79.188917	2935.913395	21.283674
79.280747	2926.369823	21.288691
78.992483	2928.506279	21.293709
79.218031	2926.222305	21.298727
79.155086	2928.854094	21.303744
78.941274	2935.665315	21.308762
79.057847	2951.285414	21.313779
79.375613	2958.564674	21.318797
79.331491	2957.451560	21.323815
79.379502	2966.028498	21.328832
79.701339	2962.024525	21.333850
79.704909	2968.887486	21.338867
79.309403	2965.844457	21.343885
79.429527	2964.258214	21.348903
79.813184	2980.231055	21.353920
79.790493	2992.359414	21.358938
80.124341	2997.010216	21.363955
80.047121	2999.212882	21.368973
79.979410	2990.844883	21.373991
80.325752	2988.393705	21.379008
80.123670	2991.175368	21.384026
80.757979	2988.285765	21.389043
80.342445	2997.361962	21.394061
80.497752	2986.904141	21.399079
80.691670	3006.813464	21.404096
80.339010	3022.762950	21.409114
80.581544	3016.642211	21.414131
80.245933	3026.259951	21.419149
80.618926	3023.228492	21.424167
80.827722	3037.697992	21.429184
80.766002	3049.343223	21.434202
81.407745	3050.376753	21.439219
80.994540	3057.521484	21.444237
81.047436	3055.980623	21.449255
81.116265	3053.636080	21.454272
81.107315	3058.210998	21.459290
81.297688	3069.267244	21.464307
81.425105	3080.129525	21.469325
82.057079	3078.387786	21.474343
81.988208	3086.320126	21.479360
81.707711	3086.751773	21.484378
81.824328	3087.764289	21.489395
81.758412	3086.105183	21.494413
81.848655	3082.483475	21.499431
82.377224	3085.253297	21.504448
82.324241	3087.175386	21.509466
82.528361	3100.261209	21.514483
82.414062	3106.535651	21.519501
82.644793	3107.433309	21.524519
82.926675	3098.442997	21.529536
82.952583	3100.392514	21.534554
83.193690	3076.620342	21.539571
82.994024	3072.218249	21.544589
82.690698	3068.397036	21.549607
83.003977	3072.734000	21.554624
82.591375	3093.983891	21.559642
83.052751	3084.597384	21.564659
83.148751	3101.184348	21.569677
83.353799	3090.648625	21.574695
83.478866	3088.929999	21.579712
83.286920	3095.049210	21.584730
83.607772	3086.154607	21.589747
83.214667	3089.050155	21.594765
83.065441	3103.329076	21.599783
83.437819	3115.785155	21.604800
83.401754	3120.523828	21.609818
83.378734	3126.117924	21.614835
83.953604	3146.971771	21.619853
84.579656	3159.812043	21.624871
84.661039	3156.349350	21.629888
84.313505	3163.241087	21.634906
84.800056	3151.841930	21.639923
84.744136	3160.132005	21.644941
84.918780	3142.918170	21.649959
85.062330	3123.266659	21.654976
84.805016	3119.094166	21.659994
84.908925	3104.039402	21.665011
84.596360	3108.775859	21.670029
84.794432	3122.399857	21.675047
85.072484	3132.003810	21.680064
84.838232	3149.792566	21.685082
85.376826	3139.464248	21.690099
84.652634	3142.739470	21.695117
84.854829	3146.599333	21.700135
84.908439	3144.938630	21.705152
84.993333	3170.203400	21.710170
85.467787	3156.516067	21.715187
85.128825	3175.352940	21.720205
85.285170	3180.111410	21.725223
85.986141	3192.452148	21.730240
85.651004	3202.455034	21.735258
86.232412	3203.024803	21.740275
86.294508	3198.257256	21.745293
86.586243	3202.638903	21.750311
86.831013	3202.734778	21.755328
86.045879	3206.908839	21.760346
86.157636	3202.021730	21.765363
86.216708	3196.241889	21.770381
86.320538	3203.846192	21.775399
86.354672	3197.808365	21.780416
85.988982	3211.264471	21.785434
86.403541	3210.488537	21.790451
86.166074	3224.514135	21.795469
86.631409	3233.122056	21.800487
86.690329	3228.370796	21.805504
86.786475	3248.575988	21.810522
86.904589	3252.280964	21.815539
87.197829	3263.814307	21.820557
86.781505	3262.556276	21.825575
87.174209	3261.970741	21.830592
87.389669	3283.139987	21.835610
87.601590	3287.452646	21.840627
87.360292	3289.537781	21.845645
87.491508	3300.884708	21.850663
87.656381	3293.204392	21.855680
88.164466	3290.113495	21.860698
88.606546	3284.890928	21.865715
88.826379	3288.728112	21.870733
88.503461	3280.528149	21.875751
88.588906	3275.710110	21.880768
88.602752	3268.603061	21.885786
88.886703	3265.763239	21.890803
89.262765	3273.295700	21.895821
88.880488	3273.351802	21.900839
89.048175	3259.012885	21.905856
89.032585	3269.811607	21.910874
89.225272	3269.543890	21.915891
89.050214	3264.451549	21.920909
88.803959	3267.970124	21.925927
89.283759	3258.826866	21.930944
89.193561	3265.821805	21.935962
88.848161	3262.273169	21.940979
89.007560	3258.893950	21.945997
88.902494	3274.989472	21.951015
89.413014	3295.387520	21.956032
89.365264	3298.487734	21.961050
89.510992	3300.477377	21.966067
89.448796	3301.649726	21.971085
89.525855	3317.050929	21.976103
89.502384	3323.325636	21.981120
89.567269	3337.512144	21.986138
89.776602	3324.971150	21.991155
90.080536	3347.642972	21.996173
90.300611	3360.705800	22.001191
90.458601	3352.749409	22.006208
90.421815	3355.221631	22.011226
90.735328	3342.122486	22.016243
90.580683	3350.057063	22.021261
90.329298	3351.754085	22.026279
90.706747	3358.629511	22.031296
90.427973	3382.482626	22.036314
90.431662	3380.695782	22.041331
90.870608	3377.514336	22.046349
90.519210	3384.485589	22.051367
91.034962	3395.686326	22.056384
91.024595	3405.764399	22.061402
91.220526	3406.019076	22.066419
91.431323	3406.129441	22.071437
91.737792	3414.574892	22.076455
91.816412	3413.545450	22.081472
91.703844	3418.787202	22.086490
91.894284	3430.239844	22.091507
92.003443	3436.807678	22.096525
92.500194	3430.128906	22.101543
92.413956	3435.916668	22.106560
92.210318	3434.479607	22.111578
92.394202	3425.016823	22.116595
92.550299	3430.321205	22.121613
92.203452	3432.630800	22.126631
92.484350	3434.265716	22.131648
92.610905	3432.860254	22.136666
92.673705	3429.905527	22.141683
92.896674	3435.073221	22.146701
92.441446	3452.778126	22.151719
92.966291	3452.447160	22.156736
93.324138	3464.894195	22.161754
93.406916	3457.886292	22.166771
93.579111	3456.543886	22.171789
93.556010	3460.340854	22.176807
93.659794	3456.511968	22.181824
93.847871	3453.165595	22.186842
93.594502	3461.059660	22.191859
93.816358	3451.610040	22.196877
93.690779	3464.095061	22.201895
93.644246	3462.632638	22.206912
93.699788	3486.021414	22.211930
93.318559	3488.791347	22.216947
93.753503	3484.490623	22.221965
94.055171	3515.401981	22.226983
94.306947	3513.371755	22.232000
94.310907	3523.002461	22.237018
94.239018	3520.795387	22.242035
94.425119	3519.645125	22.247053
94.276330	3539.161016	22.252071
94.372351	3540.701625	22.257088
94.699638	3549.743721	22.262106
94.460532	3552.647603	22.267123
94.839185	3565.865348	22.272141
94.849126	3578.902952	22.277159
95.389341	3582.469483	22.282176
95.570213	3572.140782	22.287194
95.549573	3588.671861	22.292211
95.869101	3587.413661	22.297229
95.769234	3582.038970	22.302247
95.540314	3585.652304	22.307264
95.727072	3588.784828	22.312282
95.415585	3607.842755	22.317299
96.343606	3606.166772	22.322317
96.067629	3619.855146	22.327335
96.074682	3607.376174	22.332352
96.321518	3609.476900	22.337370
96.213175	3616.783839	22.342387
96.822824	3614.263010	22.347405
96.551079	3611.308110	22.352423
96.658828	3602.753763	22.357440
96.655241	3614.547750	22.362458
97.066238	3630.239336	22.367475
97.271676	3626.490642	22.372493
97.359048	3636.343395	22.377511
97.445295	3624.721119	22.382528
97.601225	3624.371489	22.387546
97.804949	3622.581039	22.392563
97.952996	3597.089765	22.397581
97.470016	3596.557475	22.402599
97.732403	3592.203610	22.407616
97.555456	3596.353834	22.412634
97.749644	3620.201831	22.417651
97.982488	3623.205961	22.422669
98.012549	3623.981323	22.427687
97.815366	3629.698391	22.432704
98.361181	3629.111799	22.437722
98.079066	3632.913046	22.442739
98.716811	3628.915393	22.447757
98.408941	3623.782696	22.452775
98.586141	3629.411952	22.457792
98.288407	3640.413667	22.462810
98.145411	3648.111694	22.467827
98.474563	3660.891441	22.472845
98.456117	3663.069158	22.477863
98.887986	3680.552138	22.482880
98.934560	3684.282870	22.487898
98.893347	3688.505147	22.492915
99.023605	3682.614475	22.497933
99.238040	3700.246592	22.502951
99.513884	3710.835771	22.507968
99.776034	3718.835330	22.512986
99.490091	3714.525031	22.518003
100.183760	3711.325054	22.523021
99.832394	3726.852088	22.528039
100.015057	3713.176498	22.533056
100.409860	3706.258333	22.538074
100.433470	3714.252318	22.543091
100.120013	3701.913280	22.548109
100.210536	3706.993507	22.553127
100.501804	3723.149915	22.558144
100.649785	3732.450471	22.563162
100.779952	3740.927112	22.568179
101.153062	3732.191734	22.573197
100.901672	3741.866352	22.578215
101.242414	3732.457616	22.583232
101.431899	3734.024751	22.588250
100.744082	3728.922503	22.593267
101.121345	3735.474427	22.598285
101.278489	3729.934334	22.603303
101.542957	3724.513672	22.608320
101.156252	3719.248754	22.613338
101.285034	3735.738619	22.618355
101.714107	3743.402412	22.623373
102.053230	3757.710828	22.628391
101.890986	3755.402646	22.633408
102.271442	3747.210230	22.638426
101.845754	3750.652560	22.643443
102.242212	3747.947733	22.648461
101.933952	3748.032100	22.653479
102.172620	3760.124905	22.658496
102.820829	3769.868990	22.663514
102.554663	3778.747540	22.668531
102.938350	3772.696034	22.673549
102.715404	3775.078160	22.678567
102.664802	3776.099699	22.683584
102.639779	3777.052271	22.688602
102.851503	3789.526190	22.693619
102.983142	3793.857479	22.698637
102.986969	3809.124437	22.703655
102.850555	3810.520623	22.708672
102.934745	3813.688892	22.713690
102.932258	3835.166392	22.718707
103.220208	3828.541366	22.723725
103.761730	3838.482570	22.728743
103.878961	3860.008100	22.733760
104.289593	3859.814850	22.738778
103.609049	3860.459229	22.743795
103.976604	3862.068308	22.748813
104.302420	3864.094096	22.753831
104.178423	3867.137396	22.758848
104.353474	3872.835630	22.763866
104.453448	3887.578177	22.768883
104.465284	3892.310444	22.773901
104.675176	3900.210367	22.778919
104.710938	3897.625636	22.783936
105.034131	3905.067441	22.788954
105.039151	3918.527537	22.793971
105.068421	3927.378361	22.798989
104.933347	3925.941312	22.804007
105.312597	3927.101034	22.809024
105.446306	3919.505306	22.814042
105.407397	3936.540010	22.819059
105.739301	3956.043315	22.824077
105.804197	3956.955278	22.829095
105.848511	3968.430213	22.834112
106.262766	3960.674528	22.839130
106.152311	3963.500509	22.844147
106.010603	3962.202425	22.849165
106.163914	3959.918088	22.854183
105.993782	3983.143087	22.859200
106.522254	3987.292193	22.864218
106.360280	3990.643682	22.869235
106.567277	3991.104402	22.874253
106.681235	3990.576085	22.879271
106.599300	3995.748979	22.884288
106.868836	4014.636113	22.889306
107.311771	4022.419746	22.894323
107.484286	4023.171493	22.899341
107.677971	4017.106000	22.904359
107.514783	4017.819999	22.909376
108.163880	4011.382655	22.914394
107.705555	4018.530825	22.919411
107.533522	4011.384424	22.924429
107.568557	4015.975707	22.929447
107.404405	4017.829542	22.934464
107.531044	4028.143647	22.939482
107.764047	4045.154693	22.944499
107.790834	4051.532914	22.949517
108.321942	4067.842310	22.954535
108.162718	4082.371927	22.959552
108.640519	4082.094699	22.964570
108.481248	4083.426305	22.969587
108.652274	4077.962472	22.974605
108.697086	4082.609594	22.979623
109.252948	4101.223274	22.984640
109.433593	4106.127507	22.989658
109.609383	4105.757922	22.994675
109.562090	4111.354165	22.999693
109.244206	4110.493469	23.004711
109.029631	4107.853170	23.009728
109.617692	4099.903010	23.014746
109.541629	4115.201287	23.019763
109.487034	4126.905950	23.024781
109.601876	4134.313485	23.029799
109.410344	4141.519937	23.034816
109.881016	4152.209907	23.039834
110.334192	4161.435554	23.044851
110.391719	4160.564841	23.049869
110.743182	4156.364889	23.054887
110.994138	4167.443026	23.059904
111.175249	4150.540458	23.064922
111.083969	4154.682442	23.069939
111.119515	4149.708868	23.074957
111.186183	4157.531083	23.079975
111.434770	4158.131963	23.084992
111.183361	4149.427025	23.090010
111.104692	4167.873114	23.095027
111.333365	4174.506616	23.100045
111.059779	4186.615896	23.105063
111.334525	4193.302943	23.110080
111.756790	4178.547793	23.115098
111.709866	4197.972997	23.120115
111.929837	4201.967119	23.125133
112.379481	4195.769464	23.130151
111.842598	4205.065630	23.135168
112.200246	4197.732248	23.140186
112.524633	4200.830274	23.145203
112.325803	4204.700866	23.150221
112.892364	4213.837007	23.155239
112.951981	4231.544305	23.160256
113.260446	4237.026044	23.165274
113.196917	4234.928490	23.170291
113.182046	4231.207973	23.175309
113.219918	4225.748014	23.180327
113.184013	4230.555515	23.185344
113.214731	4226.982344	23.190362
113.374255	4233.679710	23.195379
112.971533	4235.535088	23.200397
113.349148	4252.467220	23.205415
113.463351	4262.445721	23.210432
113.823582	4266.231510	23.215450
113.895896	4279.089660	23.220467
113.556254	4287.042244	23.225485
114.204999	4290.286312	23.230503
114.317517	4294.026362	23.235520
114.075333	4298.035941	23.240538
114.289659	4317.941061	23.245555
114.211529	4319.261926	23.250573
114.547544	4311.940864	23.255591
114.676262	4338.297151	23.260608
115.210812	4344.789286	23.265626
114.783148	4351.814991	23.270643
115.084345	4354.883944	23.275661
115.099416	4345.284939	23.280679
115.184172	4370.784792	23.285696
115.606343	4382.246444	23.290714
115.534504	4370.676715	23.295731
115.887716	4376.470608	23.300749
115.852696	4376.899582	23.305767
116.161161	4396.298757	23.310784
116.403836	4397.555180	23.315802
116.634599	4407.108949	23.320819
116.628678	4405.333087	23.325837
116.657749	4402.179178	23.330855
116.480744	4403.829690	23.335872
116.800266	4403.598497	23.340890
117.101502	4396.382600	23.345907
116.875923	4405.123794	23.350925
117.053641	4413.354780	23.355943
117.390007	4414.303719	23.360960
117.760413	4414.036236	23.365978
117.934388	4422.345057	23.370995
117.709418	4415.612389	23.376013
117.951573	4414.783260	23.381031
117.817568	4425.781077	23.386048
118.101258	4412.218310	23.391066
118.200839	4415.420293	23.396083
117.887414	4415.932440	23.401101
118.254495	4420.385002	23.406119
118.259219	4432.216769	23.411136
118.416235	4447.037486	23.416154
118.470728	4448.690847	23.421171
118.524317	4461.305827	23.426189
118.759493	4447.390613	23.431207
118.903141	4452.569090	23.436224
118.552916	4447.126756	23.441242
118.571565	4466.478037	23.446259
118.740588	4481.651162	23.451277
119.028841	4482.760367	23.456295
118.769082	4505.235917	23.461312
119.036731	4516.141309	23.466330
119.367491	4511.361178	23.471347
119.574912	4536.303101	23.476365
119.673271	4542.955950	23.481383
119.634004	4546.620475	23.486400
120.085337	4546.048480	23.491418
120.208481	4556.235932	23.496435
120.363265	4573.642961	23.501453
120.554737	4577.026920	23.506471
120.365819	4575.139062	23.511488
120.892156	4572.678843	23.516506
121.219203	4560.899604	23.521523
121.423659	4565.717196	23.526541
121.636778	4559.168495	23.531559
121.686623	4551.877480	23.536576
121.229252	4552.569472	23.541594
121.657552	4557.325846	23.546611
121.537324	4585.654932	23.551629
122.112272	4579.731800	23.556647
122.162527	4591.804774	23.561664
121.974213	4594.434702	23.566682
121.968731	4583.841139	23.571699
121.929157	4595.484500	23.576717
122.158384	4592.827895	23.581735
122.395229	4610.765154	23.586752
122.284783	4616.757557	23.591770
122.526903	4621.745928	23.596787
122.236401	4633.397679	23.601805
122.884834	4629.171110	23.606823
123.218998	4640.348735	23.611840
123.052755	4637.194395	23.616858
123.210537	4641.428494	23.621875
123.362165	4643.155802	23.626893
123.414842	4643.086137	23.631911
123.232252	4648.711277	23.636928
123.516099	4665.141660	23.641946
123.837494	4673.604923	23.646963
123.683939	4672.329289	23.651981
123.863586	4675.089909	23.656999
123.871632	4697.877410	23.662016
123.866781	4715.266278	23.667034
124.063872	4703.908548	23.672051
123.936624	4727.522682	23.677069
124.249190	4732.257993	23.682087
124.638157	4745.138637	23.687104
124.759870	4752.704390	23.692122
124.954512	4762.645788	23.697139
124.950095	4778.097040	23.702157
125.224469	4764.438690	23.707175
125.274430	4768.484945	23.712192
125.134590	4774.086260	23.717210
125.858046	4786.986786	23.722227
125.542268	4800.314379	23.727245
125.925708	4798.392171	23.732263
126.001613	4804.699264	23.737280
126.272629	4793.733648	23.742298
126.727249	4798.439900	23.747315
126.404617	4800.406846	23.752333
126.526197	4795.704236	23.757351
126.414696	4816.722079	23.762368
126.283443	4822.260502	23.767386
126.368396	4821.093621	23.772403
126.359356	4836.993896	23.777421
126.586416	4851.860483	23.782439
126.924063	4854.412888	23.787456
127.040007	4878.236815	23.792474
127.043997	4889.742960	23.797491
127.211147	4901.373160	23.802509
127.408294	4907.843031	23.807527
127.887650	4917.604179	23.812544
127.835346	4924.072713	23.817562
128.474133	4919.464135	23.822579
128.344036	4923.408971	23.827597
128.045389	4918.768127	23.832615
128.491927	4920.378744	23.837632
128.877456	4943.442151	23.842650
129.092585	4946.651213	23.847667
129.023095	4947.021524	23.852685
129.303184	4938.624374	23.857703
129.590006	4939.370748	23.862720
128.990784	4941.673411	23.867738
129.498322	4926.487857	23.872755
129.600861	4938.808907	23.877773
129.281581	4940.804439	23.882791
129.703725	4958.915117	23.887808
129.882713	4966.842927	23.892826
129.750326	4965.781821	23.897843
129.844417	4979.710383	23.902861
130.027543	4994.479090	23.907879
130.182616	4994.833746	23.912896
130.020542	5007.735032	23.917914
130.136634	5017.747555	23.922931
130.299632	5037.272489	23.927949
130.172748	5036.026910	23.932967
130.621118	5055.015381	23.937984
130.671877	5074.004299	23.943002
131.236543	5070.437073	23.948019
131.467214	5098.388702	23.953037
131.765951	5106.350402	23.958055
132.076013	5108.664978	23.963072
132.046657	5116.496252	23.968090
131.963584	5109.145851	23.973107
132.290746	5108.894438	23.978125
132.430746	5099.473627	23.983143
132.701904	5101.099365	23.988160
132.679869	5100.234364	23.993178
133.013371	5101.253153	23.998195
132.858250	5102.336804	24.003213
132.943588	5104.109397	24.008231
132.848404	5088.886024	24.013248
132.990189	5093.549113	24.018266
133.056072	5088.184088	24.023283
132.893698	5102.496207	24.028301
133.241493	5107.279940	24.033319
133.374291	5104.776048	24.038336
133.289271	5117.961952	24.043354
133.660514	5127.351082	24.048371
133.569867	5139.150102	24.053389
133.752493	5150.205199	24.058407
134.357514	5148.505682	24.063424
134.166920	5170.718262	24.068442
134.368310	5166.774562	24.073459
134.409657	5183.076919	24.078477
134.306684	5173.578780	24.083495
134.677753	5191.390503	24.088512
135.101595	5206.309544	24.093530
135.292705	5202.914239	24.098547
135.027615	5208.967246	24.103565
134.798475	5214.914845	24.108583
135.112346	5229.533755	24.113600
135.489084	5240.676939	24.118618
135.152822	5252.717430	24.123635
135.558185	5272.933638	24.128653
135.747471	5277.579973	24.133671
135.974962	5286.215622	24.138688
135.860260	5307.598566	24.143706
136.226820	5317.217037	24.148723
135.871897	5321.394282	24.153741
135.987969	5344.555665	24.158759
136.421647	5348.574094	24.163776
136.654711	5365.076923	24.168794
137.295702	5361.177540	24.173811
137.824247	5362.967916	24.178829
137.560997	5363.029601	24.183847
138.167935	5357.327552	24.188864
138.244342	5353.447767	24.193882
138.331195	5349.411020	24.198899
138.292859	5347.501979	24.203917
137.937080	5358.566815	24.208935
138.427627	5345.340365	24.213952
138.283849	5371.601728	24.218970
138.465005	5381.535587	24.223987
138.220742	5385.125961	24.229005
138.327722	5391.684743	24.234023
138.883887	5402.476697	24.239040
138.742516	5421.412323	24.244058
138.915135	5421.737201	24.249075
139.227712	5415.943812	24.254093
139.612530	5412.141108	24.259111
140.002513	5396.037137	24.264128
139.900707	5414.824191	24.269146
139.976137	5424.419384	24.274163
140.032130	5432.763927	24.279181
140.142810	5441.074682	24.284199
140.227524	5447.314355	24.289216
140.438946	5451.526874	24.294234
140.537359	5449.003617	24.299251
140.274872	5448.062454	24.304269
140.327922	5459.268372	24.309287
140.900907	5462.812396	24.314304
140.872561	5472.627841	24.319322
140.956360	5471.461899	24.324339
141.236681	5491.202795	24.329357
141.102586	5510.943868	24.334375
141.320493	5507.890486	24.339392
141.597869	5511.468656	24.344410
142.095931	5529.084910	24.349427
142.429951	5536.222374	24.354445
141.916044	5542.222851	24.359463
142.194856	5533.553070	24.364480
142.330830	5539.197953	24.369498
142.229070	5543.683162	24.374515
142.853311	5555.760869	24.379533
142.620690	5568.243838	24.384551
142.972863	5561.310129	24.389568
142.951713	5575.892269	24.394586
143.038894	5584.632479	24.399603
143.348979	5589.503168	24.404621
143.091653	5593.688170	24.409639
142.996717	5602.863694	24.414656
143.142812	5615.719731	24.419674
143.545086	5633.770785	24.424691
143.834457	5646.202139	24.429709
143.964608	5654.276512	24.434727
144.134962	5658.359068	24.439744
144.418683	5677.434801	24.444762
144.428238	5691.704583	24.449779
144.492303	5691.499055	24.454797
144.584136	5701.987996	24.459815
144.935668	5708.661736	24.464832
145.190650	5711.161500	24.469850
145.248416	5715.384677	24.474867
145.505296	5723.802849	24.479885
145.529615	5745.444543	24.484903
145.846162	5744.208748	24.489920
145.852998	5751.405550	24.494938
145.960299	5751.089421	24.499955
146.392669	5760.807158	24.504973
146.161059	5773.030962	24.509991
146.458135	5773.157281	24.515008
146.483055	5779.816149	24.520026
146.550145	5783.503687	24.525043
146.773730	5805.276717	24.530061
146.579180	5823.548456	24.535079
146.992807	5811.298164	24.540096
147.284293	5814.619559	24.545114
147.448119	5838.033415	24.550131
147.922411	5835.886772	24.555149
147.919388	5853.864196	24.560167
147.744519	5853.186832	24.565184
147.810569	5844.220947	24.570202
147.438908	5860.610554	24.575219
147.832220	5865.712825	24.580237
148.125179	5884.391797	24.585255
148.133644	5907.189623	24.590272
148.316474	5911.085783	24.595290
148.445699	5928.402579	24.600307
148.944156	5936.338337	24.605325
149.001461	5943.019291	24.610343
149.255885	5947.333273	24.615360
149.239677	5956.666436	24.620378
149.238038	5977.663825	24.625395
150.001416	5974.207277	24.630413
149.944008	5987.600270	24.635431
149.965963	6004.989103	24.640448
150.152089	6004.533423	24.645466
150.344503	6003.665481	24.650483
150.418522	6010.288459	24.655501
150.538482	6033.491139	24.660519
150.670185	6036.982548	24.665536
150.799834	6033.033605	24.670554
150.997619	6040.818518	24.675571
151.300811	6054.075705	24.680589
151.421257	6071.906174	24.685607
151.687491	6059.772335	24.690624
151.793858	6064.395307	24.695642
152.181392	6076.508477	24.700659
152.164527	6078.520835	24.705677
151.941335	6084.375574	24.710695
152.104164	6081.163743	24.715712
152.482824	6091.692783	24.720730
152.656901	6111.255734	24.725747
152.688022	6112.999136	24.730765
152.342064	6115.534241	24.735783
152.751056	6116.405460	24.740800
153.393040	6133.320279	24.745818
153.171137	6151.131542	24.750835
153.707948	6134.874836	24.755853
153.823469	6147.697947	24.760871
153.587315	6161.675493	24.765888
154.156588	6182.425614	24.770906
153.507937	6180.495852	24.775923
153.861101	6194.160504	24.780941
153.987094	6205.508047	24.785959
154.019587	6210.609267	24.790976
154.253651	6221.798081	24.795994
154.108437	6246.699164	24.801011
154.630174	6244.333227	24.806029
154.861520	6264.917674	24.811047
155.107481	6275.512121	24.816064
155.422779	6273.637661	24.821082
155.521829	6287.431817	24.826099
155.730093	6307.651622	24.831117
155.538705	6318.080028	24.836135
155.887793	6316.500680	24.841152
155.938112	6316.659853	24.846170
155.633885	6338.148350	24.851187
156.266498	6340.336921	24.856205
156.620757	6352.032210	24.861223
157.148546	6360.335747	24.866240
157.615745	6352.986541	24.871258
157.528761	6354.899885	24.876275
157.905454	6346.360978	24.881293
157.886641	6346.686396	24.886311
157.950746	6346.587984	24.891328
158.430624	6344.337127	24.896346
157.949879	6352.789132	24.901363
158.459372	6345.484669	24.906381
158.189260	6345.820870	24.911399
158.198289	6353.533527	24.916416
158.306172	6365.141087	24.921434
158.543675	6376.884768	24.926451
158.444956	6376.110041	24.931469
158.858930	6403.674125	24.936487
159.171867	6413.222896	24.941504
159.407543	6410.306514	24.946522
158.677925	6421.163614	24.951539
159.137172	6434.664558	24.956557
159.251197	6447.521251	24.961575
158.844789	6470.787231	24.966592
159.756115	6478.622551	24.971610
160.105367	6498.075598	24.976627
161.052605	6503.961440	24.981645
161.016838	6510.305683	24.986663
160.793203	6507.538918	24.991680
161.070703	6501.702314	24.996698
160.732036	6519.231513	25.001715
161.095448	6531.305052	25.006733
161.728805	6543.270882	25.011751
161.181369	6544.334443	25.016768
161.402799	6555.650908	25.021786
161.324031	6570.697569	25.026803
161.116795	6572.346392	25.031821
161.365262	6597.229372	25.036839
161.810721	6605.885879	25.041856
162.134081	6621.078704	25.046874
162.023116	6624.941117	25.051891
162.331918	6646.361173	25.056909
162.451873	6659.192600	25.061927
162.898328	6678.818262	25.066944
163.123097	6677.562685	25.071962
163.090085	6693.323976	25.076979
163.685685	6691.506974	25.081997
163.208924	6698.537390	25.087015
163.761187	6718.406493	25.092032
163.978310	6718.982939	25.097050
164.236272	6734.922836	25.102067
164.182595	6731.781076	25.107085
164.389725	6749.258712	25.112103
164.387223	6757.332752	25.117120
164.562753	6754.565262	25.122138
164.858396	6761.868196	25.127155
165.169550	6780.052759	25.132173
165.229960	6786.037166	25.137191
165.192450	6784.464967	25.142208
166.036347	6801.768119	25.147226
165.702678	6811.067974	25.152243
166.044340	6813.415988	25.157261
166.496661	6808.815215	25.162279
166.633925	6808.219006	25.167296
166.855929	6808.121882	25.172314
166.706264	6816.563850	25.177331
167.217635	6825.325765	25.182349
167.009285	6841.925490	25.187367
166.967693	6843.820081	25.192384
167.236115	6836.401537	25.197402
167.298590	6849.492687	25.202419
167.446889	6870.237885	25.207437
167.874309	6872.987927	25.212455
167.482448	6874.341513	25.217472
168.047072	6893.253962	25.222490
167.893590	6902.360704	25.227507
168.141199	6906.170380	25.232525
167.723607	6927.798051	25.237543
168.142039	6943.367974	25.242560
168.513635	6960.817648	25.247578
168.573173	6972.763219	25.252595
168.508089	6985.462775	25.257613
169.134951	6999.476654	25.262631
169.078661	7018.523264	25.267648
169.511831	7033.837091	25.272666
169.551460	7044.123958	25.277683
170.121699	7046.063364	25.282701
170.842346	7049.762837	25.287719
170.830134	7051.119891	25.292736
171.626497	7046.612112	25.297754
171.502618	7044.764010	25.302771
171.151398	7056.172694	25.307789
171.403522	7044.032654	25.312807
171.381497	7048.264348	25.317824
171.797029	7041.054456	25.322842
171.534636	7057.488785	25.327859
171.578322	7066.266410	25.332877
171.763480	7082.026133	25.337895
171.927872	7092.948636	25.342912
172.006993	7093.135179	25.347930
172.058475	7106.894082	25.352947
171.880511	7113.748202	25.357965
172.271626	7134.580524	25.362983
172.391224	7145.245265	25.368000
172.342038	7156.884264	25.373018
172.748018	7178.385271	25.378035
172.645356	7196.043331	25.383053
173.089460	7214.475802	25.388071
172.952613	7238.192188	25.393088
173.464709	7245.243966	25.398106
173.657602	7252.006998	25.403123
173.785746	7274.512114	25.408141
174.143303	7284.787174	25.413159
174.150912	7289.855190	25.418176
174.671188	7306.588092	25.423194
174.590028	7325.731498	25.428211
174.862921	7326.271623	25.433229
175.770622	7332.856223	25.438247
175.887283	7339.178603	25.443264
176.159293	7330.663424	25.448282
176.368548	7341.265660	25.453299
176.610154	7338.517467	25.458317
176.728363	7326.501793	25.463335
176.594315	7332.060468	25.468352
176.836487	7331.012194	25.473370
176.947451	7343.409285	25.478387
177.130601	7366.058716	25.483405
177.427125	7363.264867	25.488423
177.036372	7366.584588	25.493440
177.461943	7372.013471	25.498458
177.242199	7376.751022	25.503475
177.335767	7389.757718	25.508493
177.729970	7395.056489	25.513511
177.834836	7414.134237	25.518528
177.937381	7430.971965	25.523546
178.040669	7441.405729	25.528563
178.009049	7467.210148	25.533581
178.491320	7462.859299	25.538599
178.564515	7497.298772	25.543616
179.013997	7494.492860	25.548634
179.187881	7508.316994	25.553651
179.259328	7531.491563	25.558669
179.817612	7524.565797	25.563687
179.553259	7527.799284	25.568704
179.664598	7548.427227	25.573722
180.334463	7555.562388	25.578739
180.300628	7547.778594	25.583757
180.916626	7560.888092	25.588775
180.940312	7572.784323	25.593792
181.242649	7577.346568	25.598810
181.306411	7576.021626	25.603827
181.349682	7569.919129	25.608845
181.513245	7573.155686	25.613863
181.813091	7595.887850	25.618880
181.897432	7595.369223	25.623898
182.018355	7597.159629	25.628915
182.202868	7599.522096	25.633933
182.479145	7595.752460	25.638951
182.428363	7615.403065	25.643968
182.417309	7621.242479	25.648986
183.129241	7626.230830	25.654003
183.107155	7635.829888	25.659021
183.267539	7631.569623	25.664039
183.831784	7653.378161	25.669056
183.500579	7657.934015	25.674074
183.716023	7663.491190	25.679092
183.623055	7664.534419	25.684109
183.821164	7685.164207	25.689127
184.175973	7697.234592	25.694144
184.088148	7704.559577	25.699162
184.290458	7717.064195	25.704180
184.227842	7736.253755	25.709197
185.101615	7728.107099	25.714215
185.205946	7744.484779	25.719232
185.365535	7752.147879	25.724250
185.710343	7751.549147	25.729268
185.794454	7769.134855	25.734285
185.849728	7770.118803	25.739303
186.405052	7777.147653	25.744320
186.151184	7778.392573	25.749338
186.819605	7788.715507	25.754356
186.660751	7814.892864	25.759373
187.181057	7819.805411	25.764391
187.018573	7819.493737	25.769408
186.926678	7826.105732	25.774426
187.344859	7835.732639	25.779444
187.076915	7847.906739	25.784461
187.540499	7864.712182	25.789479
187.614029	7885.057917	25.794496
187.586058	7898.614474	25.799514
187.818068	7902.432579	25.804532
187.877730	7927.315330	25.809549
188.237489	7952.212851	25.814567
188.324238	7960.525870	25.819584
188.453549	7984.482128	25.824602
188.915443	7993.617137	25.829620
189.197451	8025.164577	25.834637
189.397170	8030.088027	25.839655
189.229498	8048.991875	25.844672
189.508194	8057.087692	25.849690
189.653978	8069.680267	25.854708
189.480083	8083.776434	25.859725
190.017573	8104.570747	25.864743
190.095229	8111.308992	25.869760
190.393795	8138.402681	25.874778
190.993465	8146.239479	25.879796
191.182787	8159.882694	25.884813
191.209056	8177.146307	25.889831
191.525342	8184.911954	25.894848
191.638983	8194.547952	25.899866
191.898435	8209.736699	25.904884
191.716555	8222.812559	25.909901
191.821267	8226.944843	25.914919
192.218773	8246.803776	25.919936
192.060203	8264.545859	25.924954
192.403168	8288.672355	25.929972
192.321755	8312.345369	25.934989
192.771421	8318.592932	25.940007
193.429035	8334.935456	25.945024
193.539618	8352.244677	25.950042
193.764498	8358.561514	25.955060
194.235177	8368.963628	25.960077
194.170882	8368.139570	25.965095
194.664425	8382.449321	25.970112
194.526119	8392.517812	25.975130
194.838822	8393.886247	25.980148
194.899093	8418.012551	25.985165
195.124119	8421.551512	25.990183
195.640069	8425.425851	25.995200
195.792937	8442.968996	26.000218
195.994209	8452.750844	26.005236
195.961476	8458.005769	26.010253
196.041987	8459.783504	26.015271
196.068845	8478.074666	26.020288
196.026107	8494.010349	26.025306
196.853250	8505.106977	26.030324
196.802329	8524.163902	26.035341
197.216377	8519.777199	26.040359
197.699031	8538.603231	26.045376
197.710835	8547.074361	26.050394
198.313012	8538.196272	26.055412
198.431866	8547.298225	26.060429
198.362241	8547.190424	26.065447
198.567548	8550.063924	26.070464
198.534139	8564.179758	26.075482
198.727959	8567.663438	26.080500
198.693390	8579.058307	26.085517
198.852001	8597.341200	26.090535
199.087589	8601.359758	26.095552
199.198506	8622.328708	26.100570
199.467796	8622.470067	26.105588
199.605525	8649.520494	26.110605
200.066581	8657.573538	26.115623
200.282642	8665.748943	26.120640
200.668936	8670.476737	26.125658
201.137352	8674.740600	26.130676
201.508964	8688.921049	26.135693
202.074073	8679.923183	26.140711
202.281607	8676.389616	26.145728
201.952750	8673.653901	26.150746
202.179010	8676.296934	26.155764
202.480019	8679.091025	26.160781
202.197558	8670.838786	26.165799
202.827731	8676.348069	26.170816
202.728162	8700.974112	26.175834
202.937944	8707.470939	26.180852
202.651449	8707.888773	26.185869
202.929737	8710.239271	26.190887
203.176340	8716.931477	26.195904
203.228937	8740.853954	26.200922
203.308359	8739.806704	26.205940
203.494052	8752.413457	26.210957
203.448292	8776.285092	26.215975
203.575307	8787.743800	26.220992
203.793794	8812.884317	26.226010
204.206992	8827.246842	26.231028
204.283861	8855.501635	26.236045
204.115821	8871.582074	26.241063
204.687856	8883.134741	26.246080
204.605349	8911.179021	26.251098
205.167939	8923.929293	26.256116
205.316877	8948.880254	26.261133
205.719940	8962.927921	26.266151
206.183906	8976.355362	26.271168
206.159625	8987.038112	26.276186
207.241382	8987.208805	26.281204
208.097236	8987.038476	26.286221
208.082078	8982.296630	26.291239
208.650061	8970.258572	26.296256
208.833235	8945.740720	26.301274
209.096385	8936.491939	26.306292
209.132880	8935.548154	26.311309
209.134174	8940.270330	26.316327
209.140041	8942.223211	26.321344
208.993670	8937.141460	26.326362
209.368518	8925.491074	26.331380
209.023382	8930.924972	26.336397
209.014942	8946.396693	26.341415
209.144613	8953.197282	26.346432
209.344924	8967.019717	26.351450
210.043355	8982.880833	26.356468
209.993535	8994.026496	26.361485
209.981158	9001.068903	26.366503
210.183429	9013.521750	26.371520
210.256833	9041.273236	26.376538
210.172426	9043.079305	26.381556
210.721568	9059.437226	26.386573
210.632816	9083.663342	26.391591
211.022828	9094.472111	26.396608
210.976402	9126.068553	26.401626
211.143597	9136.323073	26.406644
211.416133	9155.728683	26.411661
211.444575	9175.623664	26.416679
212.048652	9202.011272	26.421696
211.980623	9220.110756	26.426714
212.426868	9221.704552	26.431732
212.930391	9241.128973	26.436749
213.156943	9265.427371	26.441767
213.753505	9252.823244	26.446784
213.993354	9263.533384	26.451802
214.364560	9279.813304	26.456820
214.283375	9285.532980	26.461837
214.321950	9292.636111	26.466855
214.477248	9287.488356	26.471872
214.747585	9307.994392	26.476890
215.077149	9317.144964	26.481908
215.417280	9325.324649	26.486925
214.941669	9332.151941	26.491943
215.490285	9344.372344	26.496960
215.023681	9359.147730	26.501978
215.534728	9385.100922	26.506996
216.076627	9398.702872	26.512013
216.156613	9422.246635	26.517031
216.390607	9417.198803	26.522048
216.439903	9449.170254	26.527066
216.398774	9467.621523	26.532084
216.824934	9480.628838	26.537101
216.696601	9504.994732	26.542119
217.253208	9519.512931	26.547136
217.494701	9542.138878	26.552154
217.672830	9555.672528	26.557172
217.944733	9573.014498	26.562189
218.066494	9589.890584	26.567207
218.108276	9609.733387	26.572224
218.418833	9635.855290	26.577242
218.681048	9654.760598	26.582260
219.137609	9662.186186	26.587277
219.417330	9685.923006	26.592295
219.652198	9700.354698	26.597312
219.693264	9713.124086	26.602330
219.704456	9731.484747	26.607348
220.227042	9752.455508	26.612365
220.439243	9770.198718	26.617383
220.656833	9781.856912	26.622400
220.664262	9803.839456	26.627418
221.127497	9820.997620	26.632436
221.493799	9838.013262	26.637453
221.921926	9851.258483	26.642471
222.319770	9872.956739	26.647488
222.298822	9867.708221	26.652506
222.850919	9874.531336	26.657524
223.230073	9887.277576	26.662541
223.051301	9907.913357	26.667559
223.359760	9904.754599	26.672576
223.447910	9920.094084	26.677594
223.755809	9937.302635	26.682612
223.880521	9938.836588	26.687629
224.120681	9961.737540	26.692647
224.195649	9970.494051	26.697664
224.019804	9984.293590	26.702682
223.821282	10000.298430	26.707700
224.432923	10021.693927	26.712717
224.864416	10048.728645	26.717735
225.194987	10049.346443	26.722752
225.137789	10074.545633	26.727770
225.094861	10086.762419	26.732788
225.234815	10106.957744	26.737805
225.297468	10126.216125	26.742823
225.719573	10137.403018	26.747840
225.907344	10164.497040	26.752858
226.446638	10178.418412	26.757876
226.936057	10194.002962	26.762893
227.107529	10209.960345	26.767911
227.406733	10202.759545	26.772928
227.966041	10217.400825	26.777946
228.292835	10218.150071	26.782964
228.909728	10221.854695	26.787981
229.107504	10248.353055	26.792999
228.950998	10256.842112	26.798016
229.656260	10242.961077	26.803034
229.487868	10253.938830	26.808052
229.727500	10241.497554	26.813069
229.703191	10256.697476	26.818087
230.083635	10268.153189	26.823104
230.589975	10267.234371	26.828122
230.500913	10263.760757	26.833140
231.122855	10284.143152	26.838157
230.954810	10304.672017	26.843175
231.168449	10308.740466	26.848192
231.534116	10302.595071	26.853210
231.483913	10323.912164	26.858228
231.776023	10336.109529	26.863245
231.545781	10344.168459	26.868263
231.923438	10358.253216	26.873280
232.092490	10374.526345	26.878298
232.246431	10397.215770	26.883316
232.692318	10399.273049	26.888333
232.916210	10428.444590	26.893351
232.992912	10434.900316	26.898368
233.479051	10453.084255	26.903386
233.488912	10468.183966	26.908404
233.534234	10479.311189	26.913421
233.833185	10511.546079	26.918439
233.934732	10518.593254	26.923456
234.343302	10534.322788	26.928474
234.719052	10559.145952	26.933492
235.108291	10570.252107	26.938509
235.090330	10583.032297	26.943527
235.114289	10600.131061	26.948544
235.572063	10614.905144	26.953562
235.805006	10643.167819	26.958580
236.229833	10644.032656	26.963597
236.373158	10666.495776	26.968615
236.476387	10672.917108	26.973632
236.472391	10691.576146	26.978650
236.793051	10713.484167	26.983668
237.099035	10738.272288	26.988685
236.949230	10756.274038	26.993703
237.489172	10778.707149	26.998720
237.726697	10794.113257	27.003738
237.949470	10808.191860	27.008756
238.220732	10815.038301	27.013773
238.628975	10851.598275	27.018791
238.945916	10849.071392	27.023808
239.266866	10874.547394	27.028826
238.978220	10886.769078	27.033844
239.144187	10898.927028	27.038861
239.404345	10927.880503	27.043879
239.371928	10946.724356	27.048896
239.561090	10973.975503	27.053914
239.532292	10999.976544	27.058932
239.640121	11019.110046	27.063949
240.274589	11056.244728	27.068967
240.641168	11084.105468	27.073984
240.825675	11115.053164	27.079002
240.676147	11141.109793	27.084020
241.408104	11165.251914	27.089037
241.362358	11188.452598	27.094055
242.069794	11198.395193	27.099072
242.843764	11213.927224	27.104090
243.304755	11220.660944	27.109108
243.670968	11229.407610	27.114125
243.567535	11249.456962	27.119143
243.905990	11261.864557	27.124160
244.339784	11267.892214	27.129178
244.161215	11289.949622	27.134196
244.506848	11293.403144	27.139213
244.727534	11311.778533	27.144231
244.817467	11326.994541	27.149248
245.291813	11346.300418	27.154266
245.311866	11361.320412	27.159284
245.577063	11375.455273	27.164301
245.946114	11400.868697	27.169319
246.149926	11418.095084	27.174336
246.125765	11424.908896	27.179354
246.061317	11448.924767	27.184372
246.486564	11475.111920	27.189389
247.352947	11491.931689	27.194407
247.612753	11515.037913	27.199424
247.737222	11515.848695	27.204442
248.025771	11542.926163	27.209460
247.973113	11545.877514	27.214477
248.237581	11571.521884	27.219495
248.249268	11581.779392	27.224512
248.717181	11611.807946	27.229530
248.423058	11629.743988	27.234548
249.038757	11649.290758	27.239565
248.999568	11682.233647	27.244583
249.000196	11704.126939	27.249600
249.064218	11729.805916	27.254618
249.339209	11757.749697	27.259636
249.560968	11782.350543	27.264653
249.947118	11813.389502	27.269671
250.216155	11846.996962	27.274688
250.389109	11866.347236	27.279706
250.603051	11901.034346	27.284724
251.036542	11915.388259	27.289741
251.471479	11946.913970	27.294759
251.563986	11968.635844	27.299776
252.002486	11989.644401	27.304794
251.933107	12015.209579	27.309812
252.149821	12036.100187	27.314829
252.376483	12067.997521	27.319847
252.396259	12100.718383	27.324864
252.852474	12131.690776	27.329882
252.947034	12163.584147	27.334900
253.058169	12194.683576	27.339917
253.664905	12231.997477	27.344935
253.667487	12260.211029	27.349952
253.970007	12286.297589	27.354970
254.498271	12314.832472	27.359988
254.947634	12340.834060	27.365005
255.209359	12359.933297	27.370023
254.994307	12398.690242	27.375040
255.261081	12417.979382	27.380058
256.272073	12446.171706	27.385076
256.265254	12474.549570	27.390093
256.838091	12497.482171	27.395111
257.084472	12515.834021	27.400128
257.524099	12535.158289	27.405146
257.606743	12547.349086	27.410164
257.871553	12570.101330	27.415181
258.371034	12583.544593	27.420199
258.545976	12609.175990	27.425216
259.024928	12634.046091	27.430234
258.575080	12645.012221	27.435252
258.964504	12667.286183	27.440269
259.289219	12690.159139	27.445287
259.477891	12712.590506	27.450304
259.584702	12736.649831	27.455322
259.628755	12756.431453	27.460340
259.836592	12782.467262	27.465357
260.484382	12808.021073	27.470375
260.507123	12840.413501	27.475392
261.141107	12858.566907	27.480410
261.265941	12881.241130	27.485428
261.349229	12908.460061	27.490445
261.653583	12927.470696	27.495463
262.090861	12956.933275	27.500480
262.714263	12968.568325	27.505498
262.552680	13002.143214	27.510516
262.465286	13025.396190	27.515533
262.961214	13047.764317	27.520551
263.228429	13078.406816	27.525568
263.536658	13105.311699	27.530586
264.374745	13113.617570	27.535604
265.233716	13131.891903	27.540621
265.739269	13131.047155	27.545639
265.543688	13140.285171	27.550656
266.006660	13142.514831	27.555674
266.070150	13147.571157	27.560692
266.182936	13164.023777	27.565709
266.508448	13168.110020	27.570727
266.514992	13178.482887	27.575744
266.705987	13188.767405	27.580762
266.802110	13210.145133	27.585780
266.873788	13229.679868	27.590797
267.417449	13241.350848	27.595815
266.899264	13263.336722	27.600832
267.399513	13285.578343	27.605850
267.764862	13319.238510	27.610868
267.688574	13336.221766	27.615885
267.797545	13361.496831	27.620903
268.256340	13401.108380	27.625920
268.624486	13428.452721	27.630938
268.421369	13455.184184	27.635956
268.676620	13480.606158	27.640973
269.321997	13510.027755	27.645991
269.597745	13549.201345	27.651008
269.775096	13581.444215	27.656026
269.946031	13605.966666	27.661044
269.888850	13637.364046	27.666061
271.112234	13663.763076	27.671079
271.558793	13692.645356	27.676096
271.892355	13708.234770	27.681114
271.969885	13728.026007	27.686132
272.004301	13755.215311	27.691149
272.620359	13764.752732	27.696167
272.830805	13789.743112	27.701184
272.803289	13806.436357	27.706202
273.621988	13831.388744	27.711220
273.751860	13856.366240	27.716237
274.160974	13869.824474	27.721255
274.107841	13896.686985	27.726272
274.368951	13909.565366	27.731290
274.620831	13939.948875	27.736308
274.596485	13966.880648	27.741325
274.939811	13984.167780	27.746343
275.351900	14024.647859	27.751360
275.545700	14041.420047	27.756378
275.988205	14065.740591	27.761396
276.004277	14087.921277	27.766413
276.625838	14109.627804	27.771431
277.218677	14119.486230	27.776448
278.131389	14132.127003	27.781466
278.511067	14137.394241	27.786484
278.093284	14144.985939	27.791501
278.980819	14164.575816	27.796519
279.242444	14179.886409	27.801536
279.227069	14185.864468	27.806554
278.936929	14190.485220	27.811572
279.230612	14226.514383	27.816589
279.382378	14222.007211	27.821607
279.507271	14262.218704	27.826624
279.507027	14281.755979	27.831642
279.608023	14298.484438	27.836660
279.322224	14335.574657	27.841677
279.485360	14363.928219	27.846695
279.847974	14396.495578	27.851712
280.185591	14433.490195	27.856730
280.939645	14470.991997	27.861748
280.644258	14505.961048	27.866765
281.514521	14538.780568	27.871783
281.503783	14567.498445	27.876800
281.986258	14596.735539	27.881818
282.423643	14624.361602	27.886836
282.680057	14653.656458	27.891853
283.137432	14684.122758	27.896871
283.543988	14716.695826	27.901888
283.557771	14744.747778	27.906906
284.045575	14755.677534	27.911924
283.988357	14785.206074	27.916941
284.446060	14810.381024	27.921959
284.515442	14860.611219	27.926976
284.712943	14881.395242	27.931994
285.274916	14912.621139	27.937012
285.236600	14953.196454	27.942029
285.565486	14981.834769	27.947047
286.031469	15012.875543	27.952064
286.075095	15041.799299	27.957082
286.687446	15074.478088	27.962100
286.547156	15121.690153	27.967117
287.295207	15147.687544	27.972135
287.427999	15177.381251	27.977152
287.617139	15206.677581	27.982170
288.470335	15230.847482	27.987188
288.589354	15267.487352	27.992205
288.777391	15286.776009	27.997223
289.334277	15319.009233	28.002240
289.701034	15340.530912	28.007258
290.339579	15356.429011	28.012276
290.624099	15384.768244	28.017293
291.363141	15400.598719	28.022311
291.746911	15416.835316	28.027328
291.423005	15436.415239	28.032346
291.963522	15450.574201	28.037364
291.670752	15471.309007	28.042381
291.942024	15492.519373	28.047399
292.165194	15519.236269	28.052416
292.334768	15543.779166	28.057434
292.889134	15561.764777	28.062452
292.425262	15607.446308	28.067469
293.115292	15623.450913	28.072487
293.449080	15664.372460	28.077504
293.373947	15702.156317	28.082522
293.590139	15719.123410	28.087540
294.283327	15755.158359	28.092557
294.775022	15769.683795	28.097575
294.897540	15795.750012	28.102592
295.752401	15818.095060	28.107610
296.345702	15837.921796	28.112628
296.277192	15855.907293	28.117645
297.392056	15858.339300	28.122663
297.823093	15872.760149	28.127680
297.578369	15868.377239	28.132698
298.403223	15884.032680	28.137716
298.455046	15907.905847	28.142733
298.762252	15907.496947	28.147751
299.221602	15910.555213	28.152768
299.222375	15911.589196	28.157786
299.363066	15930.612427	28.162804
299.305609	15944.332030	28.167821
299.369957	15957.871553	28.172839
299.436939	15983.745807	28.177856
300.044642	16016.501342	28.182874
300.134030	16038.675222	28.187892
300.415759	16071.111555	28.192909
300.444972	16101.396895	28.197927
300.363273	16128.159142	28.202944
300.837307	16163.390746	28.207962
301.244121	16189.400970	28.212980
301.070077	16238.605098	28.217997
301.642710	16262.569218	28.223015
301.998794	16298.065666	28.228032
301.877567	16341.664791	28.233050
302.097321	16375.340365	28.238068
302.153829	16411.484286	28.243085
302.350423	16452.401333	28.248103
302.884101	16488.660689	28.253120
303.305042	16529.605684	28.258138
304.271909	16573.890688	28.263156
304.811272	16614.989004	28.268173
304.721024	16641.258536	28.273191
305.558087	16667.440112	28.278208
305.218430	16707.325691	28.283226
305.853496	16735.947657	28.288244
306.168537	16767.544116	28.293261
306.060329	16797.176395	28.298279
306.864472	16828.912998	28.303296
306.879364	16864.253154	28.308314
307.686905	16883.003954	28.313332
307.797905	16911.813786	28.318349
308.165093	16946.032770	28.323367
308.571898	16968.082540	28.328384
308.648557	16995.786988	28.333402
309.248955	17014.535605	28.338420
309.512485	17050.724250	28.343437
309.646313	17076.959213	28.348455
309.974966	17102.347359	28.353472
310.222124	17134.372339	28.358490
310.496703	17164.065779	28.363508
310.756139	17193.173835	28.368525
310.996370	17218.090175	28.373543
311.439908	17246.919260	28.378560
311.201136	17286.464165	28.383578
312.047487	17317.510263	28.388596
312.442205	17344.125010	28.393613
312.613392	17372.501238	28.398631
313.110350	17399.625105	28.403648
312.793849	17428.572157	28.408666
313.400876	17456.987337	28.413684
313.856024	17487.761849	28.418701
314.143429	17518.839484	28.423719
314.827851	17538.679434	28.428736
315.080976	17564.716567	28.433754
315.507191	17584.435290	28.438772
315.789697	17610.614077	28.443789
315.740817	17629.258682	28.448807
316.332665	17653.800099	28.453824
316.306939	17682.820722	28.458842
316.853998	17712.001777	28.463860
317.029237	17749.130918	28.468877
317.386850	17787.966241	28.473895
317.978915	17801.464108	28.478912
318.494262	17838.845736	28.483930
318.819328	17850.489655	28.488948
319.233557	17877.978473	28.493965
319.416148	17903.813810	28.498983
319.730183	17924.329406	28.504000
319.598518	17953.318203	28.509018
319.849272	17977.037255	28.514036
320.112050	18006.229709	28.519053
320.731748	18038.698647	28.524071
321.068706	18062.421964	28.529088
321.211953	18102.573360	28.534106
321.035223	18137.573814	28.539124
321.624057	18169.272616	28.544141
321.778568	18197.320438	28.549159
321.899174	18228.558832	28.554176
321.894628	18279.270767	28.559194
322.322581	18321.034043	28.564212
323.055530	18354.318203	28.569229
322.964152	18398.773653	28.574247
323.840944	18432.291878	28.579264
324.082273	18476.225410	28.584282
324.399013	18508.023514	28.589300
325.005493	18543.418744	28.594317
324.497127	18584.354609	28.599335
325.200102	18618.569909	28.604352
325.555775	18668.857077	28.609370
325.776070	18699.043410	28.614388
326.174621	18744.234076	28.619405
326.975373	18783.981151	28.624423
327.469598	18810.833435	28.629440
328.528284	18819.306213	28.634458
329.471486	18829.886270	28.639476
330.026135	18847.315673	28.644493
330.413820	18850.236993	28.649511
330.829007	18855.510692	28.654528
330.915899	18861.807145	28.659546
331.069641	18858.859276	28.664564
330.894234	18864.949999	28.669581
330.812813	18877.827868	28.674599
331.141808	18887.396961	28.679616
331.192364	18911.449631	28.684634
331.366140	18942.978226	28.689652
331.514646	18971.496635	28.694669
331.527687	19006.769087	28.699687
331.950868	19031.629960	28.704704
332.002948	19075.305806	28.709722
332.491463	19096.423598	28.714740
332.860580	19124.286399	28.719757
333.173948	19160.581416	28.724775
333.791849	19190.886533	28.729792
334.144388	19229.784394	28.734810
334.489113	19264.995808	28.739828
334.811197	19290.650121	28.744845
335.044205	19326.087357	28.749863
335.421672	19356.035076	28.754880
335.385237	19395.356317	28.759898
335.719283	19420.658750	28.764916
336.126964	19459.257575	28.769933
336.238913	19514.036924	28.774951
336.631780	19535.062866	28.779968
337.042477	19575.818385	28.784986
337.795553	19609.604555	28.790004
338.538102	19643.335835	28.795021
338.127180	19688.330345	28.800039
338.813627	19723.184570	28.805056
338.757055	19757.638004	28.810074
339.318412	19792.966334	28.815092
339.356934	19825.814258	28.820109
340.209713	19859.030404	28.825127
341.034929	19887.111146	28.830144
341.071911	19910.926322	28.835162
341.073769	19951.779621	28.840180
341.714999	19971.598321	28.845197
342.122636	20009.807376	28.850215
342.396388	20029.632362	28.855232
342.683684	20062.077029	28.860250
342.896470	20099.354702	28.865268
343.549403	20120.023025	28.870285
343.943926	20154.256468	28.875303
344.226703	20175.461330	28.880320
344.587629	20211.132356	28.885338
344.902746	20248.336055	28.890356
345.019363	20269.318803	28.895373
345.358451	20307.824099	28.900391
345.852310	20338.838440	28.905408
345.975627	20373.684874	28.910426
345.866907	20412.065325	28.915444
346.471440	20442.688765	28.920461
346.413336	20491.948514	28.925479
346.773249	20518.116974	28.930496
347.111171	20551.511022	28.935514
347.282655	20607.513610	28.940532
347.898931	20631.560069	28.945549
348.228446	20683.139662	28.950567
348.717255	20719.737509	28.955584
348.848663	20753.375488	28.960602
348.873594	20796.573182	28.965620
349.658918	20841.938114	28.970637
349.997253	20876.318252	28.975655
350.371537	20905.859280	28.980672
350.865949	20949.667557	28.985690
351.052324	20987.117274	28.990708
351.618311	21022.862087	28.995725
351.599942	21062.185667	29.000743
352.155346	21086.752529	29.005760
352.767374	21119.663926	29.010778
353.174061	21168.322457	29.015796
353.877757	21191.548950	29.020813
354.009253	21224.099806	29.025831
354.362495	21260.401947	29.030848
355.001358	21282.445983	29.035866
355.057192	21309.724283	29.040884
355.645099	21342.857857	29.045901
356.033074	21378.731694	29.050919
356.161304	21407.268712	29.055936
356.447534	21442.647633	29.060954
356.758235	21491.061772	29.065972
357.481249	21522.185653	29.070989
357.447150	21553.163389	29.076007
357.830099	21581.770582	29.081024
358.063740	21617.262953	29.086042
358.243999	21653.426849	29.091060
358.905747	21678.764796	29.096077
359.268246	21720.430988	29.101095
359.701603	21757.363840	29.106112
360.257618	21792.894366	29.111130
360.359365	21823.298964	29.116148
361.090142	21844.925861	29.121165
361.544506	21881.098456	29.126183
361.644958	21908.343258	29.131200
362.160679	21942.332453	29.136218
362.322267	21980.536067	29.141236
362.602720	22008.034029	29.146253
362.832169	22042.684339	29.151271
363.067965	22077.806716	29.156288
362.939798	22117.299776	29.161306
362.999583	22164.853657	29.166324
364.230032	22207.548697	29.171341
364.309633	22244.612616	29.176359
365.176625	22280.671185	29.181376
365.770926	22315.861922	29.186394
366.006778	22346.102539	29.191412
366.212329	22375.821693	29.196429
366.808621	22413.604839	29.201447
367.058146	22438.661321	29.206464
367.155822	22467.074455	29.211482
367.220483	22501.160989	29.216500
368.034993	22530.460650	29.221517
368.162320	22575.913007	29.226535
368.287009	22603.908566	29.231552
368.564080	22637.347093	29.236570
368.851915	22667.607755	29.241588
369.459906	22706.733151	29.246605
369.540243	22748.292503	29.251623
370.154952	22791.012525	29.256640
370.609847	22831.864467	29.261658
370.881395	22880.563651	29.266676
371.383104	22903.647318	29.271693
371.449225	22947.852684	29.276711
371.925981	22987.291385	29.281728
372.308665	23032.206000	29.286746
372.290077	23072.023116	29.291764
372.827503	23106.484017	29.296781
373.409779	23155.133882	29.301799
373.903464	23192.308667	29.306816
374.977838	23223.101028	29.311834
375.237471	23252.556950	29.316852
375.767539	23294.658756	29.321869
376.304971	23307.672047	29.326887
376.716481	23331.664367	29.331904
377.161708	23359.492676	29.336922
377.342872	23384.713655	29.341940
378.062357	23401.789889	29.346957
378.124999	23428.535770	29.351975
378.638879	23461.714530	29.356992
379.060306	23477.573951	29.362010
379.301758	23519.375661	29.367028
379.842124	23543.813010	29.372045
380.202590	23576.144579	29.377063
379.754434	23605.993665	29.382080
380.427149	23643.350075	29.387098
380.427393	23664.722822	29.392116
381.057175	23696.197834	29.397133
381.015350	23744.322332	29.402151
381.435046	23782.510958	29.407168
381.953656	23819.427338	29.412186
382.213032	23868.825336	29.417204
382.622359	23899.830671	29.422221
383.069911	23945.458875	29.427239
383.152352	23991.528280	29.432256
384.281472	24016.966238	29.437274
384.844293	24048.560616	29.442292
385.511661	24078.358129	29.447309
385.876845	24103.561241	29.452327
385.854418	24136.385307	29.457344
386.326791	24154.028252	29.462362
386.487516	24198.062901	29.467380
387.017239	24234.981422	29.472397
387.543875	24262.005514	29.477415
387.561229	24291.082058	29.482432
388.094607	24310.777624	29.487450
388.374182	24348.483674	29.492468
388.498625	24380.560696	29.497485
388.507213	24420.196473	29.502503
388.649082	24454.854040	29.507520
389.514943	24493.627035	29.512538
389.408329	24544.155855	29.517556
389.833186	24589.130392	29.522573
390.439685	24625.194377	29.527591
390.389047	24680.426623	29.532608
390.727227	24724.141998	29.537626
391.316061	24774.646939	29.542644
391.645759	24822.729695	29.547661
391.863002	24869.216800	29.552679
391.970231	24927.059864	29.557696
392.649978	24972.256686	29.562714
392.743915	25024.137329	29.567732
393.280760	25082.964024	29.572749
394.225718	25137.247956	29.577767
394.279109	25189.391554	29.582784
394.706851	25238.023310	29.587802
395.413749	25289.821783	29.592820
395.994894	25328.941970	29.597837
396.530034	25361.865228	29.602855
397.230013	25409.425600	29.607872
397.991730	25434.070595	29.612890
398.259802	25481.386576	29.617908
399.210572	25510.734218	29.622925
399.604759	25530.634839	29.627943
399.645384	25557.125959	29.632960
400.003091	25586.821420	29.637978
400.447314	25625.558806	29.642996
400.770766	25651.427474	29.648013
401.041155	25678.425141	29.653031
401.370922	25720.832176	29.658048
402.113061	25754.029854	29.663066
402.317157	25794.837158	29.668084
402.720635	25814.925789	29.673101
403.337591	25842.586718	29.678119
403.663319	25879.909642	29.683136
404.372316	25905.526496	29.688154
404.630104	25941.697150	29.693172
404.766689	25970.292349	29.698189
405.396743	26002.301496	29.703207
405.438048	26044.260326	29.708224
406.042645	26066.800625	29.713242
405.980159	26109.392551	29.718260
406.589447	26143.566442	29.723277
407.064824	26173.564514	29.728295
407.353180	26209.228897	29.733312
407.657403	26250.802465	29.738330
408.147633	26280.082068	29.743348
408.634624	26315.551740	29.748365
409.209133	26341.738045	29.753383
409.520040	26386.481242	29.758400
409.794172	26413.757023	29.763418
410.206003	26444.119777	29.768436
410.647499	26472.938007	29.773453
411.426115	26501.222152	29.778471
411.594488	26539.478858	29.783488
412.223700	26556.469592	29.788506
412.590443	26583.086205	29.793524
413.076569	26606.114406	29.798541
413.453472	26628.391602	29.803559
413.478763	26665.950673	29.808576
413.913498	26707.909928	29.813594
413.949002	26731.277362	29.818612
414.024677	26771.935452	29.823629
414.641405	26814.100380	29.828647
414.879217	26859.743806	29.833664
415.239716	26906.561988	29.838682
415.691204	26950.692597	29.843700
416.034683	26999.277470	29.848717
416.624385	27047.328132	29.853735
416.811120	27094.930594	29.858752
417.091784	27140.996466	29.863770
417.365690	27186.091929	29.868788
417.621521	27243.358817	29.873805
418.311636	27288.869065	29.878823
419.016935	27346.933159	29.883840
419.369265	27395.252606	29.888858
419.452173	27446.577631	29.893876
419.746884	27494.112196	29.898893
420.501771	27542.558667	29.903911
420.502712	27610.448794	29.908928
420.969192	27656.553586	29.913946
421.562851	27716.095607	29.918964
422.256286	27775.661746	29.923981
423.092206	27818.271085	29.928999
423.311561	27868.356153	29.934016
423.326417	27909.557337	29.939034
424.162142	27955.353551	29.944052
424.455005	28019.475528	29.949069
424.969279	28055.168062	29.954087
425.101925	28103.053858	29.959104
425.677507	28152.211067	29.964122
426.122953	28206.183177	29.969140
426.549627	28261.051540	29.974157
427.103324	28300.129466	29.979175
427.072083	28366.649281	29.984192
427.618713	28412.594038	29.989210
428.456075	28465.073699	29.994228
428.503111	28512.618760	29.999245
429.265643	28572.772071	30.004263
429.304169	28624.723381	30.009280
429.954828	28669.707612	30.014298
430.975839	28710.959107	30.019316
431.360533	28760.579824	30.024333
432.152726	28795.674092	30.029351
433.000348	28816.788049	30.034368
433.286309	28850.549374	30.039386
433.678289	28876.966377	30.044404
434.057176	28910.087176	30.049421
434.666885	28933.854499	30.054439
435.048212	28966.485938	30.059456
435.261105	28994.192711	30.064474
435.509171	29024.670039	30.069492
435.740648	29077.880080	30.074509
436.141083	29095.019770	30.079527
436.138624	29146.443262	30.084544
436.388781	29189.291983	30.089562
437.150112	29233.542463	30.094580
437.316682	29279.702907	30.099597
437.920657	29314.899882	30.104615
437.808212	29371.028363	30.109632
438.421578	29424.675686	30.114650
438.977339	29471.262153	30.119668
439.037061	29530.027811	30.124685
439.371797	29583.130176	30.129703
439.881649	29640.654776	30.134720
440.356116	29701.817352	30.139738
441.106845	29745.821667	30.144756
441.042728	29816.183094	30.149773
442.020651	29857.630825	30.154791
442.369695	29924.466820	30.159808
442.367791	29978.095045	30.164826
443.272564	30034.919030	30.169844
443.508318	30096.726547	30.174861
444.271035	30147.258226	30.179879
444.766225	30206.838161	30.184896
445.065272	30257.970249	30.189914
445.894496	30315.391826	30.194932
445.850347	30374.080264	30.199949
446.136372	30414.508768	30.204967
446.211749	30478.235185	30.209984
447.064426	30533.772821	30.215002
447.893270	30589.223208	30.220020
448.016599	30652.222591	30.225037
448.758162	30699.436784	30.230055
449.319639	30751.355207	30.235072
449.738149	30808.119847	30.240090
450.276308	30856.767190	30.245108
450.687669	30921.803946	30.250125
451.232566	30958.005139	30.255143
451.900551	31003.787529	30.260160
451.976782	31052.129592	30.265178
453.021005	31106.803141	30.270196
453.138179	31161.834518	30.275213
453.584919	31206.279528	30.280231
454.512490	31255.732164	30.285248
454.832244	31300.028769	30.290266
455.183398	31349.937021	30.295284
455.453552	31392.973816	30.300301
455.535439	31432.268896	30.305319
456.052364	31480.599713	30.310336
456.317456	31529.866852	30.315354
457.305033	31563.238578	30.320372
457.749475	31615.507761	30.325389
458.232355	31653.756372	30.330407
458.540060	31704.786998	30.335424
459.195855	31751.144570	30.340442
459.533812	31789.664447	30.345460
459.520616	31847.910641	30.350477
459.722537	31888.290636	30.355495
460.216023	31937.551318	30.360512
460.159485	32001.072262	30.365530
461.133641	32059.140484	30.370548
461.173702	32125.927242	30.375565
461.776791	32179.748745	30.380583
461.978547	32242.169116	30.385600
462.566672	32316.584741	30.390618
463.665912	32361.539341	30.395636
464.204837	32406.536423	30.400653
465.343000	32453.251811	30.405671
466.330424	32485.015851	30.410688
466.466115	32525.307647	30.415706
467.006516	32560.392564	30.420724
467.393908	32600.616152	30.425741
467.968672	32651.569002	30.430759
468.329628	32681.064424	30.435776
468.590394	32733.876436	30.440794
469.596568	32760.010934	30.445812
469.852599	32804.618834	30.450829
470.605753	32844.199621	30.455847
470.427216	32881.888850	30.460864
470.688914	32938.579835	30.465882
470.885853	32977.719733	30.470900
471.203927	33034.227787	30.475917
471.728187	33092.190261	30.480935
472.001962	33137.316667	30.485952
472.254649	33201.098146	30.490970
473.120466	33244.147777	30.495988
474.047132	33293.221192	30.501005
474.372286	33342.937477	30.506023
475.015321	33393.186432	30.511040
475.512376	33450.091174	30.516058
475.807297	33488.663105	30.521076
475.861479	33547.524989	30.526093
476.519334	33608.335002	30.531111
477.237396	33668.289101	30.536128
477.293739	33720.832910	30.541146
478.141878	33775.649220	30.546164
478.245383	33834.282668	30.551181
478.708613	33892.946190	30.556199
478.818149	33948.050545	30.561216
479.156339	34018.327997	30.566234
479.922392	34069.514040	30.571252
480.325552	34144.697978	30.576269
480.858109	34201.352835	30.581287
481.293361	34254.833745	30.586304
481.420977	34316.355597	30.591322
481.874731	34370.805755	30.596340
482.142281	34438.370073	30.601357
482.702836	34504.846070	30.606375
483.522657	34563.838871	30.611392
483.688794	34637.496873	30.616410
484.150667	34689.431149	30.621428
484.666352	34751.481340	30.626445
485.139148	34822.439521	30.631463
485.541415	34889.543728	30.636480
485.813856	34961.565704	30.641498
486.458968	35023.641992	30.646516
486.716175	35094.234183	30.651533
487.183794	35166.315058	30.656551
488.435752	35230.254406	30.661568
488.641046	35305.802163	30.666586
489.383234	35365.019191	30.671604
490.105844	35429.068885	30.676621
490.265302	35487.063680	30.681639
491.116269	35553.885143	30.686656
491.676648	35622.120175	30.691674
492.099374	35683.091082	30.696692
492.638394	35741.551913	30.701709
492.875796	35804.354096	30.706727
493.661234	35860.882432	30.711744
494.175238	35930.016660	30.716762
494.685020	35979.591765	30.721780
495.319512	36042.112092	30.726797
495.570693	36109.360323	30.731815
496.103599	36149.222831	30.736832
496.968515	36218.512660	30.741850
497.767737	36273.095560	30.746868
498.618768	36312.641931	30.751885
498.762104	36358.543635	30.756903
499.933064	36398.723479	30.761920
500.782540	36447.051668	30.766938
501.038793	36492.208374	30.771956
501.725155	36523.608164	30.776973
501.646412	36564.362350	30.781991
502.064567	36613.071065	30.787008
502.441436	36654.631201	30.792026
503.075114	36706.093579	30.797044
503.555889	36748.223234	30.802061
503.767739	36801.854088	30.807079
504.418611	36855.637143	30.812096
504.484073	36917.784496	30.817114
504.846736	36964.852785	30.822132
505.464243	37029.614247	30.827149
505.474616	37092.863805	30.832167
506.133877	37143.401311	30.837184
506.214697	37212.406287	30.842202
506.885672	37275.486462	30.847220
507.664929	37335.877803	30.852237
507.861265	37399.563733	30.857255
508.718500	37449.982935	30.862272
509.099839	37520.689509	30.867290
509.654905	37570.153848	30.872308
510.423254	37621.292686	30.877325
510.625570	37685.379479	30.882343
510.963007	37742.646998	30.887360
511.134229	37801.123779	30.892378
511.559537	37857.303322	30.897396
512.501430	37928.518348	30.902413
512.427310	38000.242356	30.907431
512.997511	38069.580229	30.912448
513.599843	38136.551606	30.917466
514.333494	38213.049941	30.922484
514.707286	38280.471382	30.927501
514.697808	38351.847907	30.932519
515.444327	38420.235106	30.937536
516.085701	38491.529061	30.942554
516.667470	38565.636767	30.947572
517.200039	38635.766113	30.952589
517.286915	38707.307442	30.957607
518.118913	38783.062061	30.962624
518.597542	38863.612856	30.967642
518.640279	38936.166521	30.972660
519.471751	39008.080219	30.977677
520.103049	39097.391535	30.982695
520.828150	39168.301242	30.987712
521.287519	39248.238255	30.992730
521.794234	39318.624023	30.997748
522.608472	39391.034650	31.002765
523.206952	39472.394687	31.007783
523.803704	39534.740805	31.012800
524.436282	39600.664192	31.017818
524.747613	39670.289210	31.022836
525.468273	39733.858631	31.027853
526.105164	39813.290955	31.032871
526.325073	39875.437598	31.037888
526.735966	39952.402544	31.042906
527.419146	40024.531870	31.047924
528.400515	40091.533787	31.052941
528.130987	40166.516744	31.057959
528.714177	40240.144719	31.062976
529.335779	40322.890497	31.067994
529.949514	40396.242345	31.073012
530.730709	40462.528501	31.078029
530.951491	40543.238119	31.083047
531.654669	40613.465692	31.088064
532.396632	40691.927146	31.093082
532.485931	40746.032462	31.098100
533.530180	40809.486977	31.103117
534.084973	40891.233266	31.108135
534.884822	40949.321814	31.113152
535.516644	41019.345296	31.118170
535.781270	41089.892918	31.123188
536.512822	41137.997887	31.128205
536.782739	41201.974760	31.133223
537.304110	41271.228795	31.138240
537.598238	41329.777740	31.143258
538.519343	41387.692171	31.148276
538.770196	41449.144155	31.153293
539.225328	41519.878613	31.158311
539.572525	41586.820922	31.163328
540.685048	41648.359564	31.168346
540.960629	41715.627184	31.173364
541.782907	41763.506678	31.178381
542.235601	41836.986507	31.183399
543.115687	41888.329537	31.188416
543.655219	41942.683228	31.193434
543.891975	42004.991951	31.198452
544.948094	42062.916917	31.203469
545.050477	42129.189536	31.208487
545.845908	42185.561888	31.213504
546.309023	42242.310252	31.218522
546.021310	42303.134260	31.223540
547.446597	42363.301849	31.228557
547.558618	42433.167091	31.233575
547.946738	42493.354932	31.238592
548.686001	42566.889560	31.243610
549.078857	42636.334853	31.248628
549.855506	42690.018580	31.253645
550.490330	42761.759447	31.258663
551.038178	42824.949060	31.263680
551.475373	42890.939655	31.268698
551.770262	42966.092873	31.273716
552.625385	43029.691532	31.278733
553.067181	43105.148523	31.283751
553.676869	43175.079655	31.288768
554.335381	43236.439224	31.293786
554.383966	43305.131306	31.298804
555.389451	43366.466582	31.303821
555.941616	43439.493565	31.308839
556.674432	43500.733903	31.313856
557.150828	43563.938239	31.318874
557.636448	43631.925094	31.323892
558.479704	43692.152461	31.328909
558.920027	43761.852700	31.333927
559.442623	43825.359450	31.338944
560.050990	43903.743559	31.343962
560.356177	43974.860295	31.348980
560.835537	44026.138888	31.353997
561.602622	44101.935689	31.359015
561.799505	44175.411637	31.364032
562.645300	44238.078111	31.369050
563.141707	44307.862328	31.374068
563.831449	44376.066351	31.379085
564.419568	44450.129996	31.384103
564.981312	44511.257660	31.389120
565.595223	44577.830173	31.394138
565.641364	44651.677997	31.399156
565.938689	44721.339953	31.404173
567.071484	44795.245308	31.409191
567.729647	44853.853360	31.414208
568.778953	44911.121945	31.419226
569.031591	44967.065090	31.424244
569.809239	45021.870020	31.429261
570.068846	45080.401794	31.434279
570.434294	45145.051481	31.439296
571.071534	45199.233602	31.444314
571.128765	45284.336896	31.449332
571.577793	45350.362461	31.454349
572.158830	45418.850967	31.459367
572.666657	45488.211236	31.464384
573.190910	45575.329559	31.469402
573.405850	45650.649231	31.474420
574.201533	45729.302478	31.479437
574.776581	45806.399039	31.484455
575.516574	45894.413479	31.489472
576.286557	45965.369600	31.494490
576.875985	46053.233717	31.499508
577.038603	46122.150143	31.504525
577.886721	46215.168909	31.509543
577.813513	46290.625741	31.514560
578.560385	46383.068943	31.519578
579.280721	46470.274602	31.524596
580.106003	46558.555405	31.529613
581.132976	46617.882602	31.534631
582.080906	46688.043480	31.539648
583.217617	46757.875400	31.544666
583.417855	46829.522927	31.549684
584.303998	46885.423157	31.554701
584.412226	46957.241678	31.559719
584.920896	47031.240529	31.564736
585.055898	47097.603855	31.569754
585.691679	47176.773663	31.574772
586.367208	47255.043194	31.579789
586.894462	47334.001690	31.584807
587.171983	47418.587187	31.589824
587.801132	47493.230419	31.594842
588.461287	47569.716255	31.599860
589.092509	47655.815044	31.604877
589.774281	47743.247862	31.609895
589.726763	47819.619059	31.614912
591.048237	47904.037301	31.619930
591.395634	47991.787523	31.624948
592.732851	48051.732424	31.629965
593.339393	48119.616638	31.634983
593.754176	48194.340374	31.640000
594.567487	48266.084030	31.645018
595.256934	48337.435416	31.650036
596.004718	48409.307695	31.655053
597.228060	48464.756779	31.660071
597.947362	48514.379688	31.665088
598.539132	48565.073195	31.670106
599.153212	48625.819697	31.675124
599.837786	48675.884845	31.680141
600.640240	48723.478913	31.685159
601.046561	48780.029074	31.690176
601.934954	48817.678229	31.695194
602.110810	48860.490572	31.700212
602.662904	48904.059773	31.705229
603.375691	48942.907923	31.710247
603.899371	48999.470204	31.715264
604.512875	49043.484032	31.720282
604.911806	49097.376867	31.725300
605.194157	49154.094654	31.730317
605.688933	49205.716134	31.735335
606.137677	49267.358432	31.740352
606.605612	49328.707046	31.745370
606.722470	49395.258254	31.750388
607.409758	49459.538813	31.755405
608.213869	49518.872073	31.760423
608.443385	49593.838263	31.765440
609.509072	49666.861037	31.770458
609.988499	49734.545268	31.775476
610.471152	49804.478175	31.780493
610.933910	49878.502113	31.785511
611.711193	49951.411115	31.790528
612.591132	50020.398607	31.795546
613.097146	50096.639712	31.800564
613.322949	50162.012457	31.805581
613.986073	50243.546565	31.810599
614.443375	50319.038779	31.815616
614.944332	50395.174518	31.820634
615.266691	50478.296845	31.825652
615.849683	50571.173537	31.830669
616.373289	50655.013936	31.835687
616.804722	50757.204457	31.840704
617.636687	50839.432345	31.845722
618.138372	50931.320158	31.850740
618.568209	51023.189122	31.855757
619.295561	51115.525606	31.860775
619.609501	51219.356030	31.865792
620.574653	51308.594842	31.870810
620.964790	51415.565873	31.875828
621.602673	51500.116871	31.880845
622.492041	51599.725104	31.885863
623.050684	51693.938065	31.890880
623.888646	51783.889493	31.895898
624.739513	51869.207981	31.900916
625.290443	51964.295451	31.905933
626.331975	52044.584425	31.910951
626.580108	52129.798808	31.915968
628.123455	52203.734860	31.920986
628.475544	52278.178553	31.926004
629.093301	52353.341517	31.931021
630.404204	52430.780630	31.936039
630.629535	52507.976388	31.941056
631.344537	52575.250979	31.946074
632.086857	52654.462729	31.951092
632.572695	52723.527259	31.956109
633.216021	52778.336112	31.961127
634.364609	52848.450114	31.966144
634.561008	52903.980358	31.971162
635.416119	52969.406274	31.976180
636.347879	53032.247672	31.981197
636.935290	53088.002093	31.986215
637.232840	53152.898611	31.991232
637.415202	53214.548415	31.996250
638.234467	53284.511875	32.001268
638.376659	53359.956018	32.006285
639.153305	53423.374946	32.011303
639.521305	53498.692472	32.016320
640.434834	53575.401696	32.021338
641.171189	53646.315793	32.026356
641.344030	53719.993156	32.031373
642.384496	53789.787814	32.036391
642.738048	53881.474645	32.041408
643.552772	53959.244868	32.046426
644.132288	54039.513687	32.051444
644.477547	54122.280968	32.056461
645.291157	54207.685444	32.061479
645.954444	54282.127587	32.066496
646.964599	54348.978510	32.071514
647.858050	54423.615549	32.076532
648.212376	54496.588577	32.081549
649.360703	54562.531901	32.086567
649.346302	54646.626761	32.091584
650.495519	54722.219497	32.096602
651.404083	54791.231442	32.101620
651.860145	54872.144029	32.106637
653.204019	54933.833979	32.111655
653.614987	54996.467506	32.116672
654.581428	55057.609551	32.121690
655.048358	55126.401319	32.126708
655.574083	55181.976293	32.131725
656.606123	55250.324124	32.136743
657.247313	55319.826044	32.141760
657.631886	55372.266148	32.146778
658.600178	55442.508673	32.151796
658.612972	55512.188426	32.156813
659.351693	55575.317389	32.161831
659.762261	55643.153746	32.166848
660.463865	55720.905986	32.171866
660.988999	55784.944263	32.176884
661.425406	55854.059726	32.181901
662.206289	55936.734618	32.186919
662.435542	56032.048328	32.191936
663.176204	56107.501438	32.196954
663.824116	56190.920570	32.201972
664.273120	56277.451700	32.206989
665.138533	56363.924506	32.212007
665.500923	56441.263686	32.217024
666.043292	56534.794589	32.222042
666.745570	56615.899536	32.227060
667.184520	56706.371324	32.232077
667.874346	56799.454782	32.237095
668.569594	56889.219922	32.242112
669.018880	56973.181893	32.247130
669.846645	57059.310232	32.252148
670.397062	57156.312158	32.257165
671.044576	57240.380315	32.262183
671.833154	57329.998712	32.267200
672.057569	57419.916388	32.272218
672.927489	57514.463767	32.277236
673.350087	57620.596720	32.282253
674.154972	57698.598017	32.287271
674.879006	57805.027892	32.292288
675.449993	57896.796934	32.297306
676.397433	57977.947509	32.302324
676.951731	58083.061762	32.307341
677.472936	58173.513379	32.312359
678.314481	58266.666076	32.317376
679.411020	58369.698096	32.322394
679.993356	58460.500764	32.327412
680.874848	58549.293336	32.332429
681.935345	58628.998789	32.337447
682.482050	58717.495517	32.342464
682.947560	58806.537441	32.347482
683.875849	58891.588223	32.352500
684.250125	58980.027146	32.357517
685.310513	59069.315926	32.362535
686.153335	59159.957003	32.367552
686.665408	59245.845329	32.372570
687.463033	59324.764248	32.377588
688.355887	59418.305291	32.382605
688.833371	59499.100013	32.387623
689.634348	59592.208839	32.392640
689.804337	59680.894368	32.397658
690.792065	59756.963438	32.402676
691.255486	59858.196316	32.407693
691.664396	59950.337361	32.412711
692.429259	60051.102392	32.417728
693.044036	60133.418332	32.422746
694.029228	60228.521105	32.427764
694.651835	60329.785927	32.432781
695.250756	60427.155402	32.437799
695.928750	60537.077508	32.442816
696.927548	60638.386860	32.447834
697.205941	60722.229213	32.452852
697.825355	60822.416145	32.457869
698.512377	60926.378202	32.462887
699.318541	61023.177719	32.467904
700.113942	61125.541983	32.472922
700.868301	61223.596546	32.477940
701.310021	61328.639297	32.482957
701.921226	61434.310938	32.487975
703.213356	61537.578239	32.492992
703.304459	61637.600467	32.498010
703.832248	61735.064158	32.503028
704.375767	61849.769802	32.508045
705.349931	61944.686430	32.513063
706.429087	62041.216390	32.518080
706.869499	62131.421165	32.523098
708.033500	62216.698191	32.528116
708.508460	62305.987540	32.533133
709.293181	62398.934843	32.538151
710.120069	62488.569258	32.543168
710.611351	62580.493007	32.548186
711.518356	62666.998013	32.553204
712.199294	62752.998461	32.558221
713.273668	62847.219338	32.563239
713.999430	62938.320637	32.568256
714.545206	63020.141535	32.573274
715.583156	63101.221000	32.578292
715.798738	63204.156331	32.583309
716.725884	63280.406811	32.588327
717.927428	63369.241212	32.593344
718.418172	63462.743039	32.598362
719.280051	63539.467130	32.603380
719.898290	63619.109622	32.608397
720.461907	63704.097331	32.613415
721.360747	63795.678468	32.618432
721.998529	63889.770230	32.623450
722.809229	63973.787404	32.628468
723.844638	64059.681945	32.633485
724.447921	64140.270941	32.638503
725.477419	64219.895849	32.643520
726.148071	64297.344567	32.648538
727.122198	64366.206954	32.653556
728.136709	64460.059731	32.658573
728.470979	64545.184971	32.663591
729.293618	64610.280910	32.668608
729.854964	64701.329552	32.673626
730.533899	64783.747779	32.678644
730.624529	64868.960319	32.683661
731.138320	64958.817023	32.688679
732.097002	65052.252106	32.693696
732.798997	65144.998201	32.698714
733.432199	65225.320705	32.703732
734.244919	65323.378240	32.708749
734.595733	65425.100079	32.713767
735.748153	65523.100352	32.718784
736.473282	65623.987710	32.723802
737.108056	65710.937593	32.728820
738.072376	65810.811229	32.733837
738.786238	65902.869484	32.738855
739.729790	66002.210177	32.743872
739.734406	66105.828102	32.748890
740.789786	66203.999898	32.753908
741.066587	66299.055738	32.758925
741.702713	66405.892602	32.763943
742.544174	66512.625283	32.768960
742.863691	66621.679794	32.773978
743.893157	66730.904094	32.778996
744.169306	66845.170726	32.784013
744.507792	66955.500883	32.789031
745.549911	67063.384308	32.794048
746.321192	67170.163926	32.799066
746.957440	67281.184531	32.804084
747.772934	67386.143010	32.809101
748.029719	67489.079545	32.814119
749.810796	67595.542896	32.819136
750.508353	67706.694318	32.824154
751.457581	67805.568250	32.829172
752.380106	67913.375297	32.834189
752.892383	68018.401471	32.839207
753.571316	68111.170803	32.844224
754.347450	68230.480890	32.849242
754.900178	68322.292674	32.854260
755.655385	68435.284360	32.859277
756.069448	68540.842094	32.864295
756.729834	68659.409289	32.869312
757.376829	68775.639824	32.874330
758.320377	68876.846636	32.879348
759.459271	68996.250601	32.884365
759.969036	69108.168642	32.889383
761.157014	69226.408303	32.894400
761.761327	69334.473026	32.899418
762.979861	69428.584715	32.904436
763.803737	69535.417703	32.909453
764.829837	69634.628366	32.914471
765.877913	69741.158384	32.919488
766.135479	69847.539774	32.924506
767.074928	69950.143519	32.929524
768.057331	70049.546959	32.934541
768.840827	70158.217477	32.939559
769.639663	70257.697583	32.944576
770.070161	70361.769025	32.949594
770.739113	70465.926597	32.954612
771.404979	70577.091953	32.959629
772.025360	70685.192294	32.964647
772.839090	70801.133249	32.969664
773.238336	70915.975900	32.974682
774.560395	71017.968988	32.979700
775.345360	71127.757121	32.984717
775.718555	71243.718979	32.989735
776.352442	71344.705808	32.994752
777.184734	71470.841460	32.999770
778.304365	71578.633058	33.004788
779.278699	71691.174188	33.009805
780.076931	71806.338962	33.014823
781.178491	71893.467920	33.019840
781.977799	72013.117437	33.024858
782.592436	72120.435357	33.029876
783.189460	72219.212740	33.034893
783.632163	72337.198587	33.039911
784.828482	72451.103276	33.044928
785.698510	72555.286986	33.049946
786.430959	72663.188200	33.054964
787.327923	72767.267113	33.059981
787.947477	72879.369170	33.064999
788.854081	72986.192282	33.070016
789.492506	73079.584312	33.075034
789.869151	73178.017964	33.080052
790.644304	73272.374021	33.085069
791.420908	73382.276090	33.090087
792.141438	73488.052005	33.095104
792.614443	73597.652971	33.100122
793.405127	73720.108764	33.105140
794.131489	73833.917702	33.110157
794.889553	73945.691548	33.115175
795.955301	74054.573427	33.120192
796.498872	74176.308776	33.125210
797.284885	74290.862502	33.130228
798.483378	74402.917413	33.135245
798.852186	74526.828760	33.140263
799.572983	74645.658491	33.145280
800.175410	74768.860728	33.150298
800.979316	74896.146733	33.155316
802.038204	75022.390432	33.160333
802.469402	75152.682899	33.165351
803.462472	75278.249888	33.170368
804.164291	75420.812619	33.175386
805.465232	75541.154362	33.180404
806.258001	75664.006366	33.185421
806.781611	75792.686457	33.190439
807.904651	75900.055828	33.195456
809.188279	76019.384742	33.200474
809.978880	76137.122514	33.205492
811.071601	76250.729266	33.210509
811.873474	76368.902780	33.215527
812.995792	76488.818468	33.220544
813.799847	76599.769129	33.225562
814.342588	76704.641972	33.230580
815.385769	76821.751805	33.235597
816.321975	76937.994986	33.240615
817.193375	77028.574112	33.245632
818.299755	77137.938521	33.250650
818.913866	77236.893455	33.255668
819.995765	77344.352704	33.260685
820.550967	77455.508356	33.265703
821.384211	77566.686517	33.270720
821.996454	77677.321104	33.275738
822.593718	77771.157360	33.280756
823.842134	77875.383419	33.285773
824.450544	77990.315462	33.290791
825.399135	78110.035489	33.295808
825.995477	78223.193194	33.300826
826.353467	78343.698819	33.305844
827.338043	78460.536206	33.310861
828.605519	78572.226933	33.315879
829.862167	78666.542288	33.320896
830.753293	78785.472315	33.325914
831.508282	78882.436571	33.330932
833.500666	78948.988152	33.335949
835.072472	79028.523718	33.340967
836.161446	79088.341222	33.345984
837.329515	79159.115013	33.351002
838.167721	79210.966788	33.356020
838.919222	79262.447631	33.361037
840.073594	79324.778734	33.366055
840.827508	79369.806609	33.371072
841.109326	79425.859930	33.376090
841.512815	79487.282574	33.381108
842.770989	79541.378606	33.386125
842.877276	79623.976160	33.391143
843.397647	79689.440850	33.396160
844.192228	79779.417833	33.401178
844.334459	79860.226039	33.406196
844.757534	79947.705114	33.411213
845.480951	80052.543536	33.416231
845.647359	80137.429156	33.421248
846.405363	80258.034561	33.426266
846.568152	80371.928836	33.431284
847.569923	80495.745595	33.436301
848.075911	80626.303554	33.441319
848.658024	80752.085235	33.446336
849.579815	80879.157015	33.451354
850.067146	81008.929504	33.456372
851.398261	81140.336031	33.461389
852.696425	81281.618780	33.466407
853.580081	81402.113767	33.471424
854.636537	81533.955521	33.476442
855.479016	81661.291949	33.481460
856.476017	81771.627407	33.486477
857.268765	81906.641967	33.491495
857.942002	82020.716372	33.496512
859.388044	82142.941085	33.501530
860.009854	82272.640701	33.506548
861.242015	82386.285845	33.511565
862.223287	82508.465547	33.516583
863.199718	82626.666926	33.521600
863.885316	82744.697265	33.526618
864.164985	82877.065668	33.531636
865.107768	82992.870317	33.536653
865.944137	83124.094451	33.541671
867.095785	83247.381447	33.546688
868.130145	83374.460305	33.551706
868.942986	83493.257241	33.556724
869.999562	83622.750719	33.561741
870.492902	83752.600808	33.566759
871.436216	83873.762795	33.571776
872.312056	83989.963512	33.576794
872.062554	84123.442017	33.581812
873.422370	84260.233418	33.586829
873.794654	84405.686471	33.591847
874.578812	84545.185122	33.596864
875.874232	84680.484010	33.601882
876.804555	84820.016209	33.606900
877.898903	84964.558083	33.611917
878.858052	85104.118669	33.616935
879.402107	85225.836930	33.621952
880.464201	85343.467856	33.626970
880.934237	85478.729183	33.631988
881.882591	85597.735036	33.637005
883.145820	85725.205070	33.642023
883.952828	85851.760423	33.647040
884.780272	85975.547580	33.652058
885.364912	86117.722184	33.657076
886.656106	86228.724376	33.662093
887.927809	86366.302470	33.667111
888.701792	86495.872807	33.672128
889.996563	86604.306888	33.677146
890.513516	86734.466775	33.682164
891.777014	86860.189933	33.687181
892.734466	86982.460262	33.692199
893.056735	87111.256985	33.697216
893.923499	87230.076161	33.702234
895.049127	87373.108549	33.707252
895.847875	87495.490959	33.712269
896.938417	87631.310099	33.717287
897.565448	87756.476161	33.722304
898.609264	87882.875185	33.727322
899.257886	88024.974262	33.732340
900.138520	88149.738213	33.737357
901.557868	88287.783081	33.742375
902.335292	88431.685171	33.747392
903.299857	88559.822751	33.752410
904.136475	88692.280183	33.757428
905.219775	88815.709149	33.762445
905.935278	88951.213930	33.767463
906.729607	89083.351652	33.772480
907.820859	89203.192752	33.777498
909.017373	89331.908621	33.782516
910.327627	89457.219681	33.787533
911.150294	89577.058003	33.792551
912.355428	89699.660509	33.797568
913.491390	89826.357751	33.802586
914.528376	89942.787770	33.807604
915.539187	90052.058223	33.812621
916.587768	90162.025239	33.817639
917.550261	90277.615182	33.822656
918.415584	90387.101936	33.827674
919.197076	90498.546627	33.832692
919.965638	90618.101880	33.837709
920.741892	90737.333607	33.842727
921.307531	90859.121074	33.847744
922.254076	90971.849842	33.852762
923.243495	91104.212004	33.857780
923.709690	91232.740221	33.862797
924.284171	91362.434184	33.867815
924.928450	91501.408633	33.872832
925.662931	91638.748053	33.877850
926.350328	91789.837881	33.882868
927.003334	91928.617038	33.887885
928.156868	92073.678919	33.892903
928.817650	92222.136485	33.897920
929.770445	92370.051217	33.902938
930.158960	92504.650642	33.907956
931.203327	92649.753603	33.912973
932.043553	92807.748338	33.917991
932.617045	92960.763816	33.923008
934.001552	93109.235707	33.928026
934.827358	93265.647022	33.933044
936.349155	93401.342237	33.938061
937.555928	93548.271026	33.943079
938.567372	93695.696234	33.948096
939.628268	93842.835322	33.953114
940.576311	93982.550329	33.958132
941.490925	94115.403574	33.963149
942.778694	94247.965737	33.968167
943.537820	94389.475186	33.973184
944.948724	94519.067798	33.978202
945.741767	94656.040453	33.983220
946.601857	94792.179429	33.988237
948.550975	94919.048513	33.993255
949.332972	95057.683828	33.998272
950.345241	95184.214591	34.003290
951.092956	95310.614044	34.008308
952.011541	95443.853506	34.013325
952.529755	95579.998335	34.018343
953.138904	95718.280736	34.023360
954.723217	95852.763110	34.028378
955.575161	95993.126208	34.033396
956.443303	96139.083663	34.038413
957.662916	96272.541854	34.043431
957.817422	96412.969747	34.048448
958.942072	96555.992520	34.053466
959.846736	96709.835220	34.058484
960.581316	96847.532551	34.063501
961.854156	96997.572395	34.068519
962.687100	97152.164451	34.073536
963.700569	97292.880630	34.078554
964.987049	97446.839686	34.083572
965.944888	97587.541700	34.088589
967.711578	97715.823628	34.093607
967.927355	97855.438626	34.098624
969.197565	97993.367000	34.103642
970.034660	98129.597551	34.108660
970.826797	98276.384381	34.113677
972.002675	98419.111300	34.118695
972.387379	98566.982573	34.123712
973.748512	98714.168319	34.128730
974.329592	98866.591593	34.133748
975.061906	99022.978673	34.138765
976.038698	99170.175870	34.143783
977.206980	99334.518489	34.148800
978.197387	99483.165061	34.153818
979.004272	99636.560944	34.158836
979.761799	99804.642888	34.163853
981.299277	99938.540702	34.168871
982.375343	100082.155056	34.173888
983.402551	100217.484016	34.178906
984.324196	100351.730035	34.183924
985.272840	100486.864909	34.188941
986.398232	100619.469152	34.193959
987.964847	100749.054205	34.198976
988.901550	100874.752355	34.203994
989.560556	101010.452437	34.209012
990.590994	101143.411207	34.214029
991.888828	101271.550555	34.219047
992.563933	101415.867818	34.224064
993.363861	101553.604503	34.229082
994.298261	101688.266823	34.234100
994.772522	101833.583264	34.239117
996.594869	101961.002969	34.244135
997.629331	102101.678489	34.249152
998.640003	102243.853241	34.254170
999.638863	102390.995270	34.259188
1000.049104	102535.376727	34.264205
1000.956066	102681.294991	34.269223
1001.650064	102841.333695	34.274240
1002.119944	103001.766362	34.279258
1003.277788	103162.981405	34.284276
1003.859486	103331.451789	34.289293
1005.111824	103505.748307	34.294311
1005.711438	103684.134594	34.299328
1006.983165	103856.403683	34.304346
1007.653559	104030.993288	34.309364
1008.317723	104210.043318	34.314381
1009.555705	104395.341689	34.319399
1010.410422	104575.944734	34.324416
1011.370299	104759.811395	34.329434
1012.229659	104946.938960	34.334452
1013.367198	105141.493030	34.339469
1014.386634	105332.560284	34.344487
1015.454524	105519.060846	34.349504
1016.472558	105707.091173	34.354522
1017.349764	105892.183048	34.359540
1018.462808	106086.013530	34.364557
1020.200935	106257.711597	34.369575
1021.315673	106450.898434	34.374592
1022.699834	106623.090101	34.379610
1024.360716	106793.462160	34.384628
1025.437818	106968.165926	34.389645
1026.551819	107129.412412	34.394663
1027.414704	107297.631610	34.399680
1028.007579	107468.532802	34.404698
1029.754907	107638.629373	34.409716
1030.667322	107797.583622	34.414733
1031.685495	107954.455947	34.419751
1032.716637	108122.955451	34.424768
1033.944382	108288.382183	34.429786
1035.570357	108444.988580	34.434804
1036.489613	108605.770467	34.439821
1037.224807	108758.756297	34.444839
1038.302041	108904.261215	34.449856
1038.881511	109048.838726	34.454874
1040.393109	109190.483162	34.459892
1041.130183	109341.293072	34.464909
1042.449285	109471.697604	34.469927
1043.564156	109625.345315	34.474944
1044.322729	109771.821480	34.479962
1045.229165	109921.642802	34.484980
1046.175281	110075.258575	34.489997
1047.072833	110227.464681	34.495015
1047.778775	110382.529453	34.500032
1049.287494	110542.854339	34.505050
1050.318712	110695.990256	34.510068
1051.120283	110853.498954	34.515085
1052.919726	111001.462966	34.520103
1053.448730	111160.654316	34.525120
1055.043360	111301.674595	34.530138
1056.837918	111459.396757	34.535156
1057.306354	111618.854469	34.540173
1058.118128	111765.585418	34.545191
1058.845975	111922.593356	34.550208
1059.923522	112084.698587	34.555226
1061.116773	112238.727400	34.560244
1061.750720	112403.811654	34.565261
1063.095364	112568.901880	34.570279
1064.409970	112733.656147	34.575296
1064.925322	112889.641652	34.580314
1066.332442	113049.073451	34.585332
1067.312950	113219.804403	34.590349
1068.366211	113379.564719	34.595367
1069.686509	113551.924554	34.600384
1070.497111	113724.372711	34.605402
1071.426757	113892.493788	34.610420
1072.030631	114070.250094	34.615437
1072.921509	114238.392525	34.620455
1074.138339	114425.916021	34.625472
1075.407502	114607.286767	34.630490
1076.390758	114787.896724	34.635508
1077.147656	114982.838696	34.640525
1078.314043	115158.440203	34.645543
1079.467085	115336.908598	34.650560
1080.710436	115517.617999	34.655578
1081.688160	115699.869153	34.660596
1082.555887	115887.500008	34.665613
1084.007893	116069.304844	34.670631
1085.330986	116256.492680	34.675648
1086.328855	116436.109498	34.680666
1087.679212	116618.404022	34.685684
1089.048216	116792.726370	34.690701
1089.761050	116963.069323	34.695719
1090.933126	117138.884656	34.700736
1091.759887	117314.772850	34.705754
1092.913347	117500.806661	34.710772
1093.945692	117687.508645	34.715789
1095.006149	117865.881779	34.720807
1095.749048	118038.924921	34.725824
1096.723398	118221.053104	34.730842
1097.815372	118392.112461	34.735860
1098.728310	118586.012866	34.740877
1099.635007	118762.681738	34.745895
1100.644408	118944.897113	34.750912
1101.299956	119147.525640	34.755930
1102.342117	119331.347156	34.760948
1103.294209	119535.689010	34.765965
1104.259114	119731.843720	34.770983
1105.620086	119931.353482	34.776000
1106.688490	120137.098886	34.781018
1108.348058	120332.631729	34.786036
1109.025465	120534.163473	34.791053
1110.160121	120737.113682	34.796071
1111.724039	120943.045943	34.801088
1112.688659	121141.769921	34.806106
1113.888830	121342.685348	34.811124
1114.688344	121546.065946	34.816141
1115.985987	121743.317499	34.821159
1117.226147	121948.906561	34.826176
1117.967108	122162.300602	34.831194
1119.346340	122370.644207	34.836212
1120.269762	122578.826491	34.841229
1121.504953	122795.017285	34.846247
1122.984923	123001.092069	34.851264
1123.510221	123222.046046	34.856282
1124.702108	123437.779899	34.861300
1125.720048	123663.177329	34.866317
1126.919862	123868.697601	34.871335
1128.340942	124085.423397	34.876352
1129.699792	124298.777344	34.881370
1131.071245	124509.342253	34.886388
1132.015670	124712.884013	34.891405
1133.539287	124921.511850	34.896423
1135.048084	125117.950633	34.901440
1136.287122	125332.561708	34.906458
1137.605565	125529.872236	34.911476
1138.689328	125730.038028	34.916493
1139.722883	125945.601126	34.921511
1140.611040	126143.673679	34.926528
1141.402193	126360.840191	34.931546
1142.385547	126562.410125	34.936564
1143.330973	126781.238956	34.941581
1144.240068	126995.803927	34.946599
1145.074381	127219.116586	34.951616
1146.292309	127439.259639	34.956634
1147.460899	127666.967382	34.961652
1147.995778	127900.666825	34.966669
1148.993742	128134.466176	34.971687
1150.372231	128376.390778	34.976704
1151.769943	128614.789996	34.981722
1153.214210	128837.451938	34.986740
1154.345060	129065.112832	34.991757
1155.823977	129302.159627	34.996775
1156.996445	129507.658345	35.001792
1158.031841	129727.835882	35.006810
1159.422093	129937.064997	35.011828
1159.774613	130148.336612	35.016845
1161.114634	130363.953475	35.021863
1162.138585	130579.435744	35.026880
1162.872240	130816.900228	35.031898
1164.094971	131046.968089	35.036916
1165.191223	131270.669980	35.041933
1166.428456	131502.044335	35.046951
1167.894174	131734.015088	35.051968
1168.717678	131967.327151	35.056986
1169.893965	132201.429878	35.062004
1171.092982	132437.672900	35.067021
1172.025392	132678.831490	35.072039
1173.464974	132912.856202	35.077056
1174.314596	133156.225726	35.082074
1175.535244	133394.284867	35.087092
1177.009373	133635.091497	35.092109
1178.090221	133888.759432	35.097127
1179.372877	134128.474086	35.102144
1180.321932	134392.729392	35.107162
1181.647103	134632.884152	35.112180
1183.131785	134884.626838	35.117197
1184.325171	135121.283058	35.122215
1185.518232	135348.913794	35.127232
1187.295901	135598.304181	35.132250
1189.515750	135828.741904	35.137268
1190.917396	136050.446027	35.142285
1192.435658	136265.246939	35.147303
1193.881850	136477.208760	35.152320
1194.935087	136707.028074	35.157338
1195.855240	136907.417801	35.162356
1197.386159	137114.322763	35.167373
1198.467519	137336.090148	35.172391
1199.517078	137544.297358	35.177408
1200.613014	137762.933190	35.182426
1202.123706	137986.457163	35.187444
1202.844488	138213.262402	35.192461
1203.229518	138432.886437	35.197479
1204.733474	138657.164045	35.202496
1205.667374	138897.593576	35.207514
1206.847649	139123.096188	35.212532
1208.162011	139362.994663	35.217549
1209.214144	139605.995633	35.222567
1210.129299	139841.096539	35.227584
1210.881380	140089.909134	35.232602
1212.019226	140341.218928	35.237620
1213.062672	140593.142680	35.242637
1214.080075	140857.740728	35.247655
1215.144776	141107.458093	35.252672
1216.304591	141377.881527	35.257690
1217.589205	141636.631840	35.262708
1218.901947	141908.187127	35.267725
1219.876061	142170.481799	35.272743
1221.224003	142418.270444	35.277760
1222.926408	142659.139521	35.282778
1223.775179	142905.051398	35.287796
1225.452252	143141.755877	35.292813
1226.420404	143397.580339	35.297831
1228.217970	143630.665843	35.302848
1228.876197	143880.840038	35.307866
1229.951434	144125.871832	35.312884
1231.617598	144375.166721	35.317901
1232.842055	144623.625837	35.322919
1234.370599	144872.935030	35.327936
1235.508505	145131.101585	35.332954
1236.134523	145370.296086	35.337972
1237.711450	145619.957213	35.342989
1238.567679	145885.533108	35.348007
1240.154632	146141.511950	35.353024
1241.605115	146393.761869	35.358042
1243.052577	146632.481544	35.363060
1244.481889	146888.137443	35.368077
1245.374767	147145.535716	35.373095
1246.749935	147394.507797	35.378112
1248.430417	147645.154178	35.383130
1249.389254	147897.447761	35.388148
1251.094051	148146.875766	35.393165
1251.973820	148397.740366	35.398183
1253.194815	148655.029459	35.403200
1254.463057	148918.945703	35.408218
1255.557098	149163.069142	35.413236
1256.720923	149421.324517	35.418253
1257.659861	149697.377434	35.423271
1258.880166	149959.913922	35.428288
1259.889826	150230.035230	35.433306
1260.754246	150517.002356	35.438324
1262.216473	150790.791946	35.443341
1263.203888	151077.691475	35.448359
1264.518096	151359.641049	35.453376
1265.607747	151651.106384	35.458394
1267.266484	151934.345720	35.463412
1268.677215	152218.301861	35.468429
1269.794600	152503.375803	35.473447
1270.772981	152773.520253	35.478464
1272.498699	153058.646327	35.483482
1273.805596	153356.683362	35.488500
1275.458998	153630.358747	35.493517
1276.603341	153920.195263	35.498535
1278.126333	154195.101972	35.503552
1279.437296	154475.184442	35.508570
1280.775595	154753.133053	35.513588
1282.302201	155027.994157	35.518605
1283.590700	155308.289288	35.523623
1285.022603	155585.326979	35.528640
1286.197830	155859.645016	35.533658
1287.072992	156140.168924	35.538676
1288.665035	156412.021735	35.543693
1289.556419	156682.220259	35.548711
1291.164275	156939.725997	35.553728
1292.765060	157206.330573	35.558746
1293.822427	157464.428612	35.563764
1295.057948	157727.090241	35.568781
1296.312189	157990.638393	35.573799
1297.560330	158259.251195	35.578816
1299.037472	158519.466075	35.583834
1300.096334	158780.020609	35.588852
1301.346445	159047.851610	35.593869
1302.204191	159325.456930	35.598887
1303.727086	159586.076627	35.603904
1304.937447	159861.265375	35.608922
1305.961518	160138.631929	35.613940
1307.717968	160396.552389	35.618957
1308.897741	160688.955577	35.623975
1310.244845	160970.636713	35.628992
1311.211136	161259.921228	35.634010
1312.659661	161544.709907	35.639028
1313.847392	161824.964903	35.644045
1314.955296	162118.126071	35.649063
1316.435648	162403.587452	35.654080
1317.442865	162705.689348	35.659098
1318.781475	163006.188698	35.664116
1320.582660	163286.627313	35.669133
1321.819831	163594.608646	35.674151
1322.850832	163889.660102	35.679168
1324.490121	164178.328725	35.684186
1325.949803	164475.302798	35.689204
1327.158706	164784.997556	35.694221
1328.646432	165077.758310	35.699239
1330.028401	165378.393351	35.704256
1331.342600	165661.531609	35.709274
1332.659102	165950.596926	35.714292
1334.621019	166238.297436	35.719309
1335.922837	166538.598697	35.724327
1337.531859	166831.895783	35.729344
1338.853583	167106.565573	35.734362
1339.619973	167411.075536	35.739380
1341.029431	167708.104991	35.744397
1341.890314	168004.037471	35.749415
1343.078586	168314.876671	35.754432
1344.409166	168614.082694	35.759450
1345.563175	168934.639420	35.764468
1346.864655	169249.018615	35.769485
1348.360588	169559.179021	35.774503
1349.899966	169874.663795	35.779520
1351.283271	170181.979695	35.784538
1352.762802	170493.544984	35.789556
1353.926260	170809.950603	35.794573
1355.616572	171114.199774	35.799591
1357.206312	171424.927459	35.804608
1358.584940	171725.223749	35.809626
1359.789234	172032.455362	35.814644
1361.009835	172331.488067	35.819661
1362.511308	172645.906325	35.824679
1363.551993	172934.719546	35.829696
1364.603735	173224.281345	35.834714
1365.776210	173535.868177	35.839732
1367.345888	173830.268961	35.844749
1368.940901	174125.403251	35.849767
1370.200741	174429.746934	35.854784
1372.063678	174722.719528	35.859802
1373.245736	175028.691975	35.864820
1374.536437	175333.365884	35.869837
1376.022643	175620.849449	35.874855
1377.192213	175915.356456	35.879872
1378.838944	176217.360352	35.884890
1380.045424	176531.054214	35.889908
1381.598173	176829.067296	35.894925
1382.977427	177135.412217	35.899943
1383.787458	177445.333956	35.904960
1385.387803	177752.342771	35.909978
1386.434295	178072.762093	35.914996
1387.746677	178385.383041	35.920013
1389.584032	178704.769770	35.925031
1390.663057	179029.517434	35.930048
1391.990973	179347.624519	35.935066
1393.303530	179677.260824	35.940084
1394.693086	180002.189799	35.945101
1396.325732	180322.014840	35.950119
1397.740426	180650.573534	35.955136
1399.445092	180969.768188	35.960154
1401.151388	181289.624482	35.965172
1402.910366	181598.875145	35.970189
1404.713363	181910.607847	35.975207
1405.967443	182230.293228	35.980224
1407.493373	182539.627200	35.985242
1408.961802	182851.130584	35.990260
1410.063148	183153.191359	35.995277
1412.439599	183451.113333	36.000295
1413.963262	183754.298267	36.005312
1415.591100	184050.092159	36.010330
1416.823076	184357.328699	36.015348
1418.125022	184657.992387	36.020365
1419.687674	184955.312722	36.025383
1420.729707	185271.510331	36.030400
1422.148821	185570.254747	36.035418
1422.932705	185882.374454	36.040436
1424.078670	186206.721547	36.045453
1425.194781	186544.670780	36.050471
1426.320246	186912.133970	36.055488
1427.442697	187234.282063	36.060506
1428.822809	187578.488366	36.065524
1430.098139	187917.357643	36.070541
1431.905248	188243.481621	36.075559
1433.373549	188596.742485	36.080576
1434.397881	188946.209607	36.085594
1435.764243	189293.627181	36.090612
1437.088996	189633.741783	36.095629
1438.855007	189978.695608	36.100647
1440.460655	190306.832904	36.105664
1441.839133	190625.426252	36.110682
1442.827672	190960.870605	36.115700
1444.287575	191280.595933	36.120717
1446.149307	191602.983560	36.125735
1447.010621	191943.431418	36.130752
1448.703361	192280.641212	36.135770
1450.098079	192618.855947	36.140788
1451.238453	192945.639480	36.145805
1452.408408	193289.190167	36.150823
1453.863118	193643.510449	36.155840
1454.985529	193995.363141	36.160858
1456.556938	194353.374412	36.165876
1457.851337	194718.671556	36.170893
1459.331072	195080.193781	36.175911
1460.997416	195442.955623	36.180928
1462.263465	195809.139648	36.185946
1463.601264	196181.216990	36.190964
1465.004393	196543.471223	36.195981
1466.846140	196907.874135	36.200999
1467.978282	197302.274376	36.206016
1469.778058	197670.827469	36.211034
1470.912048	198052.916403	36.216052
1471.876607	198439.175431	36.221069
1473.837430	198826.675395	36.226087
1475.146304	199211.280002	36.231104
1476.428339	199596.348362	36.236122
1478.144593	199988.162562	36.241140
1479.452446	200380.747106	36.246157
1481.273792	200775.785249	36.251175
1482.565074	201172.122442	36.256192
1484.259988	201562.348990	36.261210
1485.967570	201950.340769	36.266228
1487.660816	202347.186834	36.271245
1489.892397	202724.338601	36.276263
1491.101615	203112.942262	36.281280
1493.103029	203484.144154	36.286298
1494.173997	203879.885806	36.291316
1496.257187	204248.169722	36.296333
1498.564423	204617.382045	36.301351
1500.111336	204978.853813	36.306368
1501.751292	205335.295805	36.311386
1503.668230	205695.247315	36.316404
1505.427426	206049.691283	36.321421
1507.290945	206391.776832	36.326439
1508.234679	206745.995173	36.331456
1510.375005	207080.011293	36.336474
1511.462444	207425.535406	36.341492
1513.041907	207767.129308	36.346509
1514.213826	208123.155707	36.351527
1515.345412	208479.800022	36.356544
1516.582274	208823.120286	36.361562
1517.929351	209183.082961	36.366580
1519.346566	209544.914470	36.371597
1521.261171	209901.786271	36.376615
1522.677053	210238.961017	36.381632
1524.230639	210575.732545	36.386650
1525.583356	210910.533393	36.391668
1526.653138	211268.367997	36.396685
1528.339694	211603.292090	36.401703
1529.767385	211965.538068	36.406720
1531.385062	212302.762258	36.411738
1532.753628	212643.611314	36.416756
1533.938949	213004.912378	36.421773
1535.947617	213362.924676	36.426791
1537.133789	213717.777415	36.431808
1538.741322	214074.489592	36.436826
1540.203890	214443.240991	36.441844
1541.505091	214807.551410	36.446861
1543.095520	215175.902752	36.451879
1544.593842	215548.893662	36.456896
1546.165414	215924.540233	36.461914
1547.888101	216285.025080	36.466932
1549.180469	216673.878457	36.471949
1550.610972	217046.505560	36.476967
1551.954729	217433.016385	36.481984
1553.722143	217818.135432	36.487002
1555.263979	218200.932425	36.492020
1556.663800	218597.927568	36.497037
1557.947907	218978.460179	36.502055
1559.118927	219387.333215	36.507072
1560.804237	219788.322297	36.512090
1562.651917	220184.738621	36.517108
1564.118000	220585.488706	36.522125
1566.148580	220994.576166	36.527143
1567.297213	221406.432136	36.532160
1568.422953	221818.674483	36.537178
1570.016768	222228.095043	36.542196
1571.100785	222644.233547	36.547213
1573.049253	223060.784372	36.552231
1574.123002	223499.253905	36.557248
1575.763853	223930.744604	36.562266
1577.598812	224357.910996	36.567284
1578.899561	224801.934266	36.572301
1580.560044	225240.385698	36.577319
1581.973434	225685.865951	36.582336
1583.108311	226116.282197	36.587354
1584.662398	226552.851192	36.592372
1586.052665	227012.665646	36.597389
1587.583454	227470.755758	36.602407
1589.185939	227939.173161	36.607424
1591.006078	228404.557588	36.612442
1592.712419	228849.820164	36.617460
1594.319851	229305.997991	36.622477
1596.131181	229771.362870	36.627495
1597.818780	230223.745030	36.632512
1599.298174	230683.886077	36.637530
1600.914017	231141.033192	36.642548
1602.593326	231607.035792	36.647565
1604.499091	232047.904485	36.652583
1606.724663	232464.105702	36.657600
1608.886289	232887.863118	36.662618
1610.882247	233299.939841	36.667636
1612.291969	233714.886617	36.672653
1613.692157	234127.524448	36.677671
1615.540375	234542.347313	36.682688
1617.140100	234943.090270	36.687706
1618.802983	235353.044126	36.692724
1620.488305	235766.906907	36.697741
1622.122283	236182.074851	36.702759
1623.512131	236595.608905	36.707776
1624.820503	237016.397313	36.712794
1626.782989	237433.061135	36.717812
1628.146146	237867.787606	36.722829
1629.392288	238286.684033	36.727847
1630.988259	238718.654332	36.732864
1632.552908	239148.090590	36.737882
1634.248837	239594.550119	36.742900
1635.515244	240038.340524	36.747917
1637.229168	240482.080568	36.752935
1638.903862	240920.137965	36.757952
1640.340526	241362.250423	36.762970
1642.323264	241805.972155	36.767988
1643.569621	242270.701500	36.773005
1645.284483	242720.516335	36.778023
1646.758489	243176.596720	36.783040
1648.287408	243640.721049	36.788058
1650.041235	244098.482315	36.793076
1651.643759	244563.382886	36.798093
1653.447662	245034.422523	36.803111
1655.547493	245497.867530	36.808128
1656.677199	245968.668117	36.813146
1658.488532	246436.863186	36.818164
1660.058314	246911.019013	36.823181
1661.510141	247387.075381	36.828199
1663.232264	247858.234058	36.833216
1664.759232	248339.968847	36.838234
1667.193619	248804.249414	36.843252
1668.964856	249275.426469	36.848269
1671.045509	249739.717572	36.853287
1673.097320	250202.642214	36.858304
1674.366948	250679.901353	36.863322
1676.018189	251134.461370	36.868340
1677.526425	251608.403319	36.873357
1679.264400	252070.824028	36.878375
1681.230649	252538.642201	36.883392
1682.383894	253018.844020	36.888410
1684.075121	253494.000390	36.893428
1685.641945	253970.677011	36.898445
1687.473523	254436.791571	36.903463
1689.555064	254914.447348	36.908480
1691.053829	255394.743252	36.913498
1692.932784	255863.441135	36.918516
1694.597227	256338.297938	36.923533
1696.221105	256797.081474	36.928551
1698.017129	257250.450078	36.933568
1699.944017	257701.230545	36.938586
1701.602944	258138.567710	36.943604
1703.991449	258584.417079	36.948621
1705.148985	259013.151981	36.953639
1707.388748	259432.531082	36.958656
1709.473501	259868.880508	36.963674
1711.487962	260293.683373	36.968692
1713.211526	260713.531427	36.973709
1714.520935	261141.452156	36.978727
1716.469667	261574.089909	36.983744
1717.859970	262008.652001	36.988762
1719.710905	262445.522939	36.993780
1721.501391	262882.556372	36.998797
1723.392181	263314.009085	37.003815
1725.257532	263754.737967	37.008832
1726.661680	264199.381277	37.013850
1728.121841	264627.477282	37.018868
1729.749582	265080.693227	37.023885
1731.243474	265517.876977	37.028903
1732.832250	265962.131506	37.033920
1734.206300	266416.253253	37.038938
1736.252256	266878.159865	37.043956
1737.566066	267335.364657	37.048973
1739.298476	267806.976908	37.053991
1741.245725	268280.736444	37.059008
1742.446085	268750.457069	37.064026
1743.766664	269226.811993	37.069044
1745.530703	269711.015998	37.074061
1747.063436	270197.570470	37.079079
1749.172275	270686.489661	37.084096
1750.336175	271180.726409	37.089114
1752.514235	271679.335851	37.094132
1754.256353	272179.568513	37.099149
1755.677221	272690.752824	37.104167
1757.632907	273192.217127	37.109184
1758.961895	273712.026491	37.114202
1760.999629	274219.088565	37.119220
1762.553682	274729.331352	37.124237
1763.689850	275252.777390	37.129255
1765.811083	275769.499937	37.134272
1767.303798	276301.061932	37.139290
1769.211127	276833.415315	37.144308
1770.927284	277368.797431	37.149325
1772.809268	277895.055884	37.154343
1774.553407	278429.134820	37.159360
1776.250906	278969.392829	37.164378
1778.121163	279499.967091	37.169396
1779.750110	280038.049113	37.174413
1781.327034	280581.980716	37.179431
1783.158262	281134.732166	37.184448
1784.426951	281695.681030	37.189466
1786.186616	282258.322068	37.194484
1787.864526	282823.083406	37.199501
1789.340654	283386.149959	37.204519
1791.542552	283921.631909	37.209536
1793.297906	284459.372809	37.214554
1795.103721	284995.401269	37.219572
1796.911702	285536.583700	37.224589
1798.494420	286079.733042	37.229607
1799.967777	286621.908357	37.234624
1801.676713	287187.104725	37.239642
1803.422357	287742.513350	37.244660
1805.454907	288297.387954	37.249677
1806.831600	288869.999973	37.254695
1809.205435	289433.193286	37.259712
1811.018879	289998.867500	37.264730
1812.212365	290562.333791	37.269748
1814.572087	291142.209255	37.274765
1816.724094	291715.538973	37.279783
1818.987557	292285.316313	37.284800
1820.530564	292857.220600	37.289818
1821.979212	293428.985743	37.294836
1823.908461	294013.822369	37.299853
1825.824724	294586.873074	37.304871
1827.696034	295162.239700	37.309888
1829.334172	295751.815452	37.314906
1831.506718	296326.540039	37.319924
1833.503364	296909.241149	37.324941
1835.695624	297490.711753	37.329959
1837.288823	298078.732521	37.334976
1838.916846	298664.432641	37.339994
1840.706049	299247.104754	37.345012
1842.786720	299833.990248	37.350029
1844.261486	300424.582164	37.355047
1846.577001	301003.775617	37.360064
1848.385634	301600.474450	37.365082
1850.310641	302184.654247	37.370100
1852.837204	302773.146364	37.375117
1854.457534	303361.916571	37.380135
1856.344929	303946.015018	37.385152
1857.950976	304535.084491	37.390170
1859.959682	305126.138102	37.395188
1862.444859	305710.706345	37.400205
1863.870810	306294.892964	37.405223
1866.292601	306879.616181	37.410240
1868.056542	307459.927374	37.415258
1870.480225	308042.381697	37.420276
1872.523613	308620.605078	37.425293
1874.358988	309192.765072	37.430311
1876.289817	309757.870266	37.435328
1878.788464	310329.019610	37.440346
1880.688310	310891.709283	37.445364
1883.132742	311453.565187	37.450381
1885.065226	311998.008154	37.455399
1887.015192	312544.450209	37.460416
1888.870818	313108.857410	37.465434
1890.239851	313666.842797	37.470452
1892.137887	314219.350060	37.475469
1893.725867	314771.093491	37.480487
1895.574385	315308.999880	37.485504
1897.155847	315848.217413	37.490522
1899.032240	316393.906076	37.495540
1901.234012	316916.758156	37.500557
1902.875557	317458.796626	37.505575
1905.555080	317978.232453	37.510592
1907.322360	318509.347935	37.515610
1909.211566	319038.584741	37.520628
1911.869087	319557.427922	37.525645
1913.703701	320078.464355	37.530663
1915.706646	320600.305674	37.535680
1917.448827	321124.954877	37.540698
1919.931694	321637.235019	37.545716
1922.062698	322158.203738	37.550733
1923.566540	322683.997856	37.555751
1925.407797	323204.423398	37.560768
1926.798379	323739.977442	37.565786
1928.683733	324274.248872	37.570804
1930.171345	324817.799742	37.575821
1931.608175	325378.263160	37.580839
1933.210895	325940.495494	37.585856
1934.750076	326499.280558	37.590874
1936.238301	327074.672646	37.595892
1938.073970	327653.147667	37.600909
1938.992161	328265.234273	37.605927
1941.220084	328857.923098	37.610944
1943.105593	329465.033191	37.615962
1944.430747	330084.341910	37.620980
1946.226731	330706.634943	37.625997
1947.906530	331338.790564	37.631015
1949.621452	331984.945733	37.636032
1951.371361	332614.104446	37.641050
1953.398191	333260.368708	37.646068
1955.626694	333911.566046	37.651085
1957.223617	334575.377882	37.656103
1959.201757	335221.093431	37.661120
1961.517878	335885.298674	37.666138
1963.954691	336552.977627	37.671156
1966.283902	337192.135673	37.676173
1968.331078	337853.848409	37.681191
1970.766950	338489.342059	37.686208
1972.867531	339146.815097	37.691226
1975.186242	339789.825253	37.696244
1977.031160	340429.836866	37.701261
1978.825897	341092.310928	37.706279
1980.931406	341737.743047	37.711296
1982.716142	342390.226334	37.716314
1984.455119	343050.627086	37.721332
1986.478666	343707.822858	37.726349
1988.419529	344376.165091	37.731367
1991.078346	345027.878608	37.736384
1993.255591	345670.935039	37.741402
1994.898916	346332.295353	37.746420
1997.137658	346967.506512	37.751437
1999.435823	347618.838695	37.756455
2001.453507	348247.826722	37.761472
2003.475819	348865.563146	37.766490
2005.696297	349479.653598	37.771508
2007.813750	350091.063222	37.776525
2009.529280	350711.084650	37.781543
2011.342367	351326.639841	37.786560
2013.450886	351939.268338	37.791578
2015.250521	352557.091951	37.796596
2017.816985	353173.938102	37.801613
2019.588644	353792.991832	37.806631
2021.590954	354412.986562	37.811648
2024.369077	355031.469255	37.816666
2025.956725	355654.459679	37.821684
2028.280675	356272.570130	37.826701
2029.904738	356889.801426	37.831719
2032.079713	357518.092670	37.836736
2033.743107	358153.134270	37.841754
2035.676650	358796.517381	37.846772
2037.617524	359426.975327	37.851789
2039.742261	360082.152946	37.856807
2041.375552	360723.729512	37.861824
2043.622589	361369.960023	37.866842
2045.561921	362036.425946	37.871860
2047.794869	362685.021631	37.876877
2049.622520	363343.797465	37.881895
2051.566021	363996.479316	37.886912
2053.904694	364655.246554	37.891930
2055.193847	365330.467090	37.896948
2057.726101	365993.414007	37.901965
2059.986922	366671.767124	37.906983
2061.421872	367350.604158	37.912000
2063.556697	368030.323587	37.917018
2065.899372	368710.857231	37.922036
2068.190466	369387.404852	37.927053
2070.174339	370064.778607	37.932071
2072.231297	370751.206973	37.937088
2074.784385	371437.765568	37.942106
2076.635183	372112.384115	37.947124
2078.930954	372796.043753	37.952141
2080.683143	373477.272296	37.957159
2082.655688	374176.633205	37.962176
2084.441668	374862.089373	37.967194
2086.257030	375572.328279	37.972212
2087.723018	376274.852421	37.977229
2089.909414	376989.081183	37.982247
2091.731629	377712.688780	37.987264
2094.123955	378429.615827	37.992282
2096.513778	379158.166611	37.997300
2098.622489	379872.829028	38.002317
2100.992080	380590.727596	38.007335
2103.021313	381317.162580	38.012352
2105.017786	382031.619745	38.017370
2106.749767	382769.761525	38.022388
2108.655600	383495.560387	38.027405
2111.137645	384217.669586	38.032423
2113.189531	384930.100794	38.037440
2114.988154	385632.190540	38.042458
2117.116197	386344.247321	38.047476
2119.775578	387037.463155	38.052493
2122.013359	387733.093215	38.057511
2123.951464	388432.358523	38.062528
2126.365196	389136.520361	38.067546
2128.238319	389849.199405	38.072564
2130.647661	390552.036699	38.077581
2132.538888	391269.596839	38.082599
2134.133504	391981.411703	38.087616
2136.554847	392695.045323	38.092634
2138.210653	393428.840769	38.097652
2140.706017	394154.440370	38.102669
2142.872698	394879.343399	38.107687
2144.681837	395610.828251	38.112704
2146.844084	396344.008429	38.117722
2148.526524	397091.088871	38.122740
2151.139427	397833.657593	38.127757
2153.450074	398572.533777	38.132775
2155.437887	399317.831773	38.137792
2157.948885	400069.457003	38.142810
2159.694852	400835.306711	38.147828
2161.901790	401589.882784	38.152845
2163.807915	402353.104647	38.157863
2166.257363	403118.898408	38.162880
2169.099009	403867.578293	38.167898
2171.841996	404617.192140	38.172916
2174.215600	405358.386967	38.177933
2176.866233	406086.974099	38.182951
2179.492425	406826.439119	38.187968
2182.155681	407551.438112	38.192986
2184.016013	408286.535562	38.198004
2186.184451	409019.913650	38.203021
2188.141536	409756.676635	38.208039
2190.082965	410504.414895	38.213056
2192.558667	411246.873536	38.218074
2194.057827	412005.890816	38.223092
2195.802175	412741.289619	38.228109
2197.757420	413502.287555	38.233127
2199.446645	414273.514970	38.238144
2201.842065	415039.102993	38.243162
2204.343461	415816.501867	38.248180
2206.002573	416592.197749	38.253197
2208.617008	417358.944877	38.258215
2210.544044	418141.612574	38.263232
2213.496394	418904.405931	38.268250
2215.447447	419685.780577	38.273268
2218.232440	420459.037717	38.278285
2220.412869	421233.437473	38.283303
2222.060256	422018.487032	38.288320
2224.204174	422797.451693	38.293338
2226.185437	423594.697853	38.298356
2228.370199	424382.668155	38.303373
2230.458223	425163.389266	38.308391
2232.226254	425936.748057	38.313408
2234.209605	426706.248090	38.318426
2236.352021	427494.123548	38.323444
2238.614324	428273.245175	38.328461
2240.943144	429054.506462	38.333479
2242.674966	429850.726078	38.338496
2245.058689	430624.889540	38.343514
2247.243333	431414.347466	38.348532
2250.048454	432211.264642	38.353549
2252.323535	432994.883115	38.358567
2254.521456	433790.331076	38.363584
2256.762274	434580.784326	38.368602
2259.168499	435391.880382	38.373620
2261.468833	436184.949852	38.378637
2264.017001	436981.035927	38.383655
2265.701055	437788.728224	38.388672
2268.737402	438596.058971	38.393690
2271.140916	439404.632387	38.398708
2273.377988	440202.984219	38.403725
2275.768748	441000.066614	38.408743
2277.699620	441816.424055	38.413760
2280.030344	442621.147890	38.418778
2282.278832	443439.059834	38.423796
2284.496231	444257.148577	38.428813
2286.919645	445075.069914	38.433831
2288.859954	445921.470589	38.438848
2291.242725	446733.366747	38.443866
2293.521315	447572.410955	38.448884
2295.400731	448414.170794	38.453901
2298.137573	449248.518190	38.458919
2299.903038	450109.094387	38.463936
2302.083318	450952.622868	38.468954
2304.377039	451803.885451	38.473972
2306.723458	452659.958513	38.478989
2309.296968	453514.288589	38.484007
2311.362240	454374.636443	38.489024
2313.523164	455239.532791	38.494042
2315.900339	456113.607667	38.499060
2318.162188	456993.124661	38.504077
2320.242626	457865.405071	38.509095
2322.691880	458753.963423	38.514112
2324.934740	459637.968094	38.519130
2326.867002	460537.201411	38.524148
2329.475309	461418.688630	38.529165
2331.703556	462313.190976	38.534183
2333.990375	463213.505292	38.539200
2336.614799	464110.991380	38.544218
2339.359288	465008.668248	38.549236
2341.510208	465896.601476	38.554253
2344.355964	466780.079914	38.559271
2346.579385	467686.513732	38.564288
2348.945241	468571.558042	38.569306
2351.313759	469465.604614	38.574324
2353.635691	470355.575258	38.579341
2356.516221	471230.050552	38.584359
2358.703109	472101.875818	38.589376
2361.171246	472961.337324	38.594394
2364.464414	473798.847291	38.599412
2366.810305	474645.421729	38.604429
2369.297029	475480.518559	38.609447
2371.448726	476318.614652	38.614464
2374.588724	477150.897675	38.619482
2376.930149	477992.521006	38.624500
2379.143080	478834.177913	38.629517
2381.375102	479665.289267	38.634535
2382.909978	480507.943723	38.639552
2385.641426	481349.041437	38.644570
2388.038663	482192.832761	38.649588
2390.339600	483050.131182	38.654605
2392.790253	483888.683461	38.659623
2395.546774	484740.420583	38.664640
2397.951811	485588.239288	38.669658
2400.168668	486445.589491	38.674676
2402.915374	487290.541831	38.679693
2405.451575	488142.858207	38.684711
2407.522837	489008.738185	38.689728
2410.055376	489862.686715	38.694746
2412.438426	490727.367537	38.699764
2414.623258	491598.598842	38.704781
2416.936176	492465.071201	38.709799
2419.052232	493353.381101	38.714816
2421.139789	494235.140844	38.719834
2423.211056	495126.392835	38.724852
2425.563586	496026.832286	38.729869
2428.015594	496920.143998	38.734887
2430.453717	497838.783529	38.739904
2432.463000	498751.695492	38.744922
2434.711702	499670.720231	38.749940
2437.214646	500598.880096	38.754957
2439.390630	501526.034914	38.759975
2441.742315	502460.823036	38.764992
2444.260727	503394.470255	38.770010
2446.963917	504349.109431	38.775028
2449.346581	505293.461390	38.780045
2451.604487	506234.048563	38.785063
2454.063501	507189.217076	38.790080
2456.654597	508141.583864	38.795098
2459.576884	509098.172381	38.800116
2462.172630	510051.936444	38.805133
2464.745408	510997.431378	38.810151
2467.105066	511954.447590	38.815168
2469.834881	512912.148616	38.820186
2472.502985	513861.234723	38.825204
2474.629240	514820.887268	38.830221
2477.553046	515767.193166	38.835239
2480.286819	516722.643598	38.840256
2482.475824	517670.167722	38.845274
2485.436280	518619.617430	38.850292
2487.799956	519570.168087	38.855309
2490.191795	520503.427552	38.860327
2492.615199	521424.787655	38.865344
2495.054695	522334.655926	38.870362
2497.832946	523239.022606	38.875380
2499.979366	524161.169389	38.880397
2502.287868	525074.368957	38.885415
2504.944363	525995.509689	38.890432
2507.139322	526919.592533	38.895450
2509.850676	527828.677102	38.900468
2511.876345	528773.617389	38.905485
2514.104666	529706.732978	38.910503
2516.504322	530649.525340	38.915520
2518.983876	531593.199533	38.920538
2521.869988	532543.940359	38.925556
2523.841387	533494.171228	38.930573
2526.533201	534443.461624	38.935591
2529.533209	535405.921462	38.940608
2532.774460	536360.325311	38.945626
2535.511179	537306.449797	38.950644
2537.588687	538260.975679	38.955661
2540.468602	539211.829024	38.960679
2543.195874	540163.751200	38.965696
2545.722800	541119.214650	38.970714
2548.679049	542069.107618	38.975732
2550.344531	543037.815668	38.980749
2552.898178	544004.142173	38.985767
2555.375145	544986.254890	38.990784
2557.932187	545955.059791	38.995802
2560.322042	546935.238700	39.000820
2562.796863	547934.790000	39.005837
2565.048945	548931.993906	39.010855
2567.751629	549923.920561	39.015872
2569.973435	550942.949813	39.020890
2572.142061	551948.793394	39.025908
2574.211108	552975.385597	39.030925
2576.661973	553992.185566	39.035943
2579.572829	555026.718664	39.040960
2582.198415	556064.184867	39.045978
2584.619548	557102.408994	39.050996
2587.456145	558154.597647	39.056013
2589.727083	559199.917130	39.061031
2592.667718	560249.208232	39.066048
2595.584070	561297.565685	39.071066
2598.024510	562345.418129	39.076084
2600.692260	563414.088144	39.081101
2603.174037	564456.942383	39.086119
2605.279914	565522.571801	39.091136
2608.001750	566590.718882	39.096154
2611.001333	567646.329921	39.101172
2613.697638	568722.335754	39.106189
2616.305160	569792.493721	39.111207
2619.157458	570858.353998	39.116224
2621.534773	571923.653583	39.121242
2624.229003	572986.751590	39.126260
2626.737749	574074.076293	39.131277
2629.605306	575129.035235	39.136295
2632.536906	576168.091318	39.141312
2634.864784	577193.067862	39.146330
2637.827878	578216.095466	39.151348
2640.277504	579262.197131	39.156365
2642.840988	580283.165322	39.161383
2645.559266	581313.449512	39.166400
2647.608173	582353.839717	39.171418
2650.459511	583393.652950	39.176436
2652.789674	584445.899184	39.181453
2655.668253	585503.574588	39.186471
2658.143318	586549.847837	39.191488
2660.302955	587621.444619	39.196506
2663.184612	588679.591580	39.201524
2666.137657	589749.709253	39.206541
2668.667827	590825.214353	39.211559
2671.531931	591899.362306	39.216576
2673.969062	592984.106139	39.221594
2676.567235	594051.039679	39.226612
2679.251190	595141.753583	39.231629
2681.605826	596249.550506	39.236647
2684.217072	597360.603557	39.241664
2686.420060	598469.917479	39.246682
2689.373042	599581.900860	39.251700
2692.343841	600708.743082	39.256717
2694.304432	601833.995379	39.261735
2697.208760	602965.232590	39.266752
2699.589039	604116.767123	39.271770
2702.174341	605254.237660	39.276788
2705.077116	606413.456834	39.281805
2706.843481	607572.400841	39.286823
2710.450892	608736.013789	39.291840
2713.198237	609909.407392	39.296858
2715.969768	611081.022928	39.301876
2719.015482	612244.816232	39.306893
2721.429615	613417.546635	39.311911
2724.601816	614587.322889	39.316928
2727.279743	615768.558581	39.321946
2730.005660	616938.760679	39.326964
2732.563655	618128.510786	39.331981
2735.065527	619315.791423	39.336999
2737.954693	620505.424749	39.342016
2740.262948	621713.715140	39.347034
2742.948916	622917.758438	39.352052
2745.732700	624134.739131	39.357069
2748.300095	625335.633481	39.362087
2751.127161	626552.231399	39.367104
2753.976498	627774.029918	39.372122
2757.070724	628980.165534	39.377140
2759.586569	630201.191089	39.382157
2762.022412	631433.321397	39.387175
2764.851949	632661.944918	39.392192
2766.966101	633902.175580	39.397210
2769.922169	635140.816965	39.402228
2772.580522	636391.137618	39.407245
2774.940106	637631.628558	39.412263
2778.100433	638844.244949	39.417280
2780.857115	640071.352540	39.422298
2783.865093	641276.723229	39.427316
2786.406701	642490.808123	39.432333
2789.160105	643711.144121	39.437351
2792.294802	644911.773049	39.442368
2795.268423	646130.283249	39.447386
2797.804527	647346.576981	39.452404
2800.585445	648568.213413	39.457421
2803.265436	649781.594513	39.462439
2806.450681	651019.655323	39.467456
2809.003349	652246.011180	39.472474
2811.787689	653469.684394	39.477492
2815.004387	654702.695043	39.482509
2817.881785	655945.569296	39.487527
2821.289840	657165.288295	39.492544
2824.428461	658398.593044	39.497562
2827.611031	659624.614471	39.502580
2830.674978	660845.771916	39.507597
2833.179565	662069.010496	39.512615
2836.682090	663289.633757	39.517632
2839.028071	664530.600758	39.522650
2841.683544	665768.766526	39.527668
2844.369805	666999.403565	39.532685
2847.161359	668250.455161	39.537703
2850.374221	669476.999567	39.542720
2852.545355	670726.038661	39.547738
2855.276737	671980.732643	39.552756
2857.866021	673247.860157	39.557773
2860.502475	674517.441974	39.562791
2863.117454	675794.607254	39.567808
2865.551086	677086.734055	39.572826
2868.627255	678374.098654	39.577844
2871.433150	679669.675376	39.582861
2874.253186	680983.941887	39.587879
2877.720258	682290.608291	39.592896
2880.155393	683599.796080	39.597914
2882.894571	684918.474597	39.602932
2885.873157	686236.920072	39.607949
2888.720271	687566.313593	39.612967
2891.835432	688877.151933	39.617984
2894.568662	690216.643734	39.623002
2897.252306	691548.401802	39.628020
2900.604234	692879.548730	39.633037
2903.382267	694222.398224	39.638055
2906.284793	695566.410919	39.643072
2909.003763	696915.009818	39.648090
2911.373895	698260.585685	39.653108
2914.694451	699613.177825	39.658125
2917.501317	700961.336050	39.663143
2920.564114	702318.804951	39.668160
2923.750560	703674.850785	39.673178
2926.882945	705039.064424	39.678196
2929.955664	706392.274468	39.683213
2932.894482	707735.983686	39.688231
2935.919025	709041.688001	39.693248
2938.857368	710359.979305	39.698266
2941.585054	711660.727846	39.703284
2945.107659	712956.092496	39.708301
2947.988244	714258.740724	39.713319
2951.187325	715553.117590	39.718336
2953.513211	716865.202513	39.723354
2956.402986	718172.137886	39.728372
2959.729267	719480.474849	39.733389
2961.859408	720802.011417	39.738407
2965.064296	722117.764694	39.743424
2967.674596	723446.260910	39.748442
2970.640961	724783.821992	39.753460
2973.706432	726115.860584	39.758477
2976.355308	727471.812835	39.763495
2979.439077	728820.944612	39.768512
2982.421832	730174.807993	39.773530
2985.041979	731545.295562	39.778548
2988.577863	732903.791487	39.783565
2990.969337	734278.493350	39.788583
2993.571016	735654.798737	39.793600
2996.660474	737051.656555	39.798618
2999.760366	738450.734078	39.803636
3002.701025	739847.668062	39.808653
3005.322630	741259.303934	39.813671
3008.670758	742663.215442	39.818688
3011.675865	744090.796265	39.823706
3014.319851	745516.699454	39.828724
3017.193825	746948.807977	39.833741
3020.023354	748387.804891	39.838759
3022.812692	749841.567079	39.843776
3025.719709	751298.828019	39.848794
3028.694998	752759.888645	39.853812
3031.645736	754228.306685	39.858829
3034.371652	755710.215273	39.863847
3037.230380	757192.895541	39.868864
3040.113077	758691.471389	39.873882
3042.913417	760196.406052	39.878900
3046.294225	761691.792024	39.883917
3049.222127	763205.596152	39.888935
3052.622693	764718.865844	39.893952
3056.107126	766216.919130	39.898970
3059.715094	767725.314571	39.903988
3063.350117	769218.607488	39.909005
3066.458919	770725.395020	39.914023
3069.483139	772219.756118	39.919040
3073.125097	773715.033074	39.924058
3075.881988	775215.359598	39.929076
3079.642366	776710.002320	39.934093
3082.585883	778202.071887	39.939111
3086.014534	779683.986311	39.944128
3089.390929	781150.102697	39.949146
3092.312273	782630.859229	39.954164
3095.667041	784105.253016	39.959181
3098.761546	785564.629373	39.964199
3102.113255	786998.320275	39.969216
3105.364464	788415.663896	39.974234
3108.350133	789842.568419	39.979252
3111.566271	791241.956175	39.984269
3114.587635	792646.290256	39.989287
3118.136023	794055.345588	39.994304
3121.313859	795456.787074	39.999322
3124.080766	796867.121175	40.004340
3126.727363	798285.851499	40.009357
3129.693040	799710.303676	40.014375
3132.517333	801136.638290	40.019392
3135.403598	802564.329396	40.024410
3138.314020	804019.395550	40.029428
3141.265976	805467.691619	40.034445
3143.861258	806928.937624	40.039463
3146.891348	808406.360852	40.044480
3149.825050	809882.647554	40.049498
3152.497935	811386.302273	40.054516
3155.531134	812878.913488	40.059533
3158.477803	814400.745328	40.064551
3161.825662	815929.483946	40.069568
3164.979250	817462.980173	40.074586
3167.640051	818999.182529	40.079604
3171.268744	820523.253838	40.084621
3175.030342	822065.140336	40.089639
3178.369478	823600.301627	40.094656
3182.154548	825128.787913	40.099674
3185.138786	826681.419514	40.104692
3188.593349	828224.002571	40.109709
3191.670023	829772.761804	40.114727
3194.876338	831308.418029	40.119744
3197.902061	832857.371422	40.124762
3200.531707	834417.506245	40.129780
3203.724209	835982.615213	40.134797
3207.067838	837555.877173	40.139815
3210.373667	839132.112688	40.144832
3213.802207	840699.912270	40.149850
3216.958934	842276.411681	40.154868
3220.688957	843846.100597	40.159885
3223.800520	845425.123561	40.164903
3227.301914	847002.127266	40.169920
3230.890867	848571.821249	40.174938
3233.655023	850140.288870	40.179956
3237.218884	851717.640065	40.184973
3240.591241	853299.668264	40.189991
3243.518403	854881.075085	40.195008
3247.079911	856449.064515	40.200026
3250.247200	858038.637277	40.205044
3253.778579	859610.184698	40.210061
3256.811908	861195.272100	40.215079
3259.749888	862772.984114	40.220096
3262.856024	864355.293231	40.225114
3266.128992	865957.594433	40.230132
3269.330576	867542.632004	40.235149
3272.804717	869123.815088	40.240167
3275.733437	870678.348649	40.245184
3279.206618	872224.739411	40.250202
3282.064021	873775.378034	40.255220
3285.206696	875321.499588	40.260237
3288.090782	876880.214109	40.265255
3290.995732	878443.633831	40.270272
3294.587915	880010.673552	40.275290
3297.516778	881591.605655	40.280308
3300.416890	883162.069545	40.285325
3303.513343	884751.576887	40.290343
3306.457554	886367.022818	40.295360
3309.551345	887980.060506	40.300378
3312.348924	889613.049746	40.305396
3315.294493	891251.912790	40.310413
3318.128340	892913.365918	40.315431
3320.679651	894585.754855	40.320448
3323.724908	896269.995507	40.325466
3326.681218	897980.815899	40.330484
3329.616863	899706.430633	40.335501
3332.578169	901446.142383	40.340519
3335.269506	903204.798095	40.345536
3338.396800	904975.811802	40.350554
3341.603175	906759.615113	40.355572
3344.819308	908553.897976	40.360589
3348.168797	910363.912789	40.365607
3350.996848	912186.871233	40.370624
3354.101585	914011.672889	40.375642
3357.506261	915862.504434	40.380660
3360.991180	917709.717008	40.385677
3364.381330	919582.221347	40.390695
3367.573785	921456.795540	40.395712
3371.407643	923316.225210	40.400730
3374.413322	925196.045454	40.405748
3378.426503	927077.523177	40.410765
3382.094680	928958.107155	40.415783
3384.970936	930858.552583	40.420800
3388.671018	932741.711868	40.425818
3392.070951	934652.568223	40.430836
3395.507403	936541.872743	40.435853
3399.080637	938442.134604	40.440871
3402.590999	940351.652875	40.445888
3406.306775	942247.153902	40.450906
3409.641826	944164.753605	40.455924
3413.184463	946059.169910	40.460941
3416.756205	947965.478415	40.465959
3420.079733	949885.999770	40.470976
3423.887187	951807.671688	40.475994
3427.597983	953767.921034	40.481012
3431.307884	955716.651312	40.486029
3434.892589	957662.300783	40.491047
3438.420232	959604.469297	40.496064
3442.000889	961541.577903	40.501082
3445.461904	963493.287508	40.506100
3449.418789	965416.429512	40.511117
3453.287948	967330.062298	40.516122
3456.817873	969191.382161	40.521127
3461.083011	970961.633591	40.526132
3464.934347	972656.832656	40.531136
3468.665710	974285.496400	40.536141
3472.424145	975801.938772	40.541146
3475.786992	977244.116244	40.546151
3478.987836	978596.617933	40.551156
3481.920025	979869.092022	40.556160
3484.847435	981039.880246	40.561165
3488.213055	982141.755885	40.566170
3490.760450	983164.241496	40.571175
3493.253312	984093.593141	40.576180
3495.226871	984958.804673	40.581184
3497.583270	985735.177127	40.586189
3499.636221	986458.258164	40.591194
3501.408523	987119.679797	40.596199
3503.438260	987698.900259	40.601204
3505.110915	988236.306423	40.606208
3507.127655	988699.724251	40.611213
3508.545886	989105.608405	40.616218
3509.714687	989475.838541	40.621223
3511.116230	989774.088966	40.626228
3512.478922	990042.805207	40.631232
3513.800816	990254.806297	40.636237
3515.339291	990433.731710	40.641242
3516.314945	990559.938536	40.646247
3517.929948	990640.629987	40.651252
3518.348483	990698.920415	40.656256
3519.160958	990709.206923	40.661261
3520.604642	990683.043685	40.666266
3520.982686	990649.754793	40.671271
3522.208464	990553.573776	40.676276
3523.212237	990452.849548	40.681280
3523.931045	990298.873575	40.686285
3524.907111	990130.428216	40.691290
3525.516180	989937.387058	40.696295
3525.926115	989720.206179	40.701300
3526.643812	989481.135146	40.706304
3526.784203	989222.368871	40.711309
3527.629630	988954.504013	40.716314
3528.099503	988674.020027	40.721319
3528.856014	988348.636361	40.726324
3529.245543	988028.755456	40.731328
3529.654996	987671.809525	40.736333
3530.166267	987320.088248	40.741338
3530.326172	986941.691337	40.746343
3530.988261	986543.877991	40.751348
3531.223422	986142.501844	40.756352
3531.599916	985732.004201	40.761357
3531.962779	985306.460583	40.766362
3532.017952	984884.351266	40.771367
3532.677997	984441.819342	40.776372
3532.875809	983984.699940	40.781376
3532.996240	983515.460271	40.786381
3533.173142	983041.879536	40.791386
3533.154066	982573.756856	40.796391
3533.973431	982080.765078	40.801396
3534.187957	981586.858037	40.806400
3534.283962	981083.559185	40.811405
3534.464007	980566.244025	40.816410
3534.348342	980056.155855	40.821415
3534.536372	979531.326800	40.826420
3534.880417	979014.428655	40.831424
3535.149053	978488.318343	40.836429
3535.526757	977940.072029	40.841434
3535.721094	977408.308823	40.846439
3535.690988	976849.480214	40.851444
3535.524463	976300.192693	40.856448
3535.368602	975748.506037	40.861453
3535.952397	975185.697785	40.866458
3535.916263	974628.802369	40.871463
3536.103330	974062.531559	40.876468
3536.078629	973490.279541	40.881472
3536.097267	972924.413457	40.886477
3536.378061	972342.220885	40.891482
3536.263738	971755.442027	40.896487
3536.405322	971170.319134	40.901492
3536.456147	970589.747421	40.906496
3536.367878	970000.828825	40.911501
3536.798285	969410.392026	40.916506
3536.281284	968808.221601	40.921511
3536.507395	968214.566726	40.926516
3536.733377	967629.948277	40.931520
3536.683047	967021.543169	40.936525
3537.011519	966416.237842	40.941530
3536.607146	965815.690928	40.946535
3537.007366	965203.199743	40.951540
3536.925427	964601.100613	40.956544
3536.717703	963992.107668	40.961549
3537.290878	963370.385842	40.966554
3536.855307	962766.686367	40.971559
3536.814969	962150.028567	40.976564
3537.121387	961544.409477	40.981568
3536.796755	960920.323619	40.986573
3537.260434	960304.361348	40.991578
3536.974037	959686.208091	40.996583
3537.109810	959054.886095	41.001588
3537.083369	958432.243068	41.006592
3536.889641	957821.712474	41.011597
3537.286499	957187.789468	41.016602
3537.435636	956567.659114	41.021607
3537.391161	955935.339986	41.026612
3537.492464	955299.593419	41.031616
3537.095800	954664.155936	41.036621
3537.499040	954023.510983	41.041626
3537.481362	953391.202623	41.046631
3537.643721	952753.007607	41.051636
3537.715968	952115.444092	41.056640
3537.602016	951475.095174	41.061645
3538.000888	950812.904980	41.066650
3537.608583	950191.180433	41.071655
3537.958086	949550.739928	41.076660
3537.850847	948918.236247	41.081664
3537.894250	948277.879512	41.086669
3538.034316	947648.907405	41.091674
3537.666773	947003.103210	41.096679
3537.948937	946362.848806	41.101684
3538.091597	945717.178320	41.106688
3538.010310	945071.560609	41.111693
3538.237105	944427.436784	41.116698
3537.774905	943783.924479	41.121703
3537.739701	943129.725100	41.126708
3537.803574	942488.163837	41.131712
3537.657592	941840.045290	41.136717
3537.570577	941200.169896	41.141722
3537.314219	940553.920910	41.146727
3537.623222	939912.956716	41.151732
3537.601477	939283.565705	41.156736
3537.103714	938641.240675	41.161741
3537.530134	937989.380475	41.166746
3536.950649	937347.101489	41.171751
3537.235856	936713.704479	41.176756
3537.628270	936070.143702	41.181760
3537.315202	935422.404398	41.186765
3537.441908	934773.742572	41.191770
3537.449653	934127.514940	41.196775
3537.686194	933479.441798	41.201780
3537.750569	932835.827875	41.206784
3537.433619	932184.811170	41.211789
3537.251414	931530.043968	41.216794
3537.145757	930876.526260	41.221799
3537.474203	930224.773586	41.226804
3537.551581	929579.800236	41.231808
3537.611053	928924.957115	41.236813
3537.587925	928271.487746	41.241818
3537.207504	927625.298440	41.246823
3537.297859	926964.925775	41.251828
3537.503992	926319.054019	41.256832
3537.125181	925663.883963	41.261837
3537.578322	924996.095409	41.266842
3537.081223	924346.933923	41.271847
3537.333407	923685.647263	41.276852
3537.264571	923030.389883	41.281856
3537.175293	922374.671377	41.286861
3537.148226	921717.035292	41.291866
3537.450433	921062.147488	41.296871
3537.111299	920396.325485	41.301876
3537.541929	919733.175467	41.306880
3537.117200	919082.114914	41.311885
3537.136898	918404.057181	41.316890
3536.938119	917759.052499	41.321895
3537.180382	917104.945962	41.326900
3537.207421	916437.707852	41.331904
3536.695580	915779.816789	41.336909
3536.958788	915123.446685	41.341914
3537.037012	914468.376998	41.346919
3537.281025	913805.400627	41.351924
3537.123884	913142.508548	41.356928
3536.673074	912487.773075	41.361933
3537.049648	911817.790953	41.366938
3536.775246	911161.325578	41.371943
3537.035481	910498.331264	41.376948
3536.943777	909845.338735	41.381952
3536.931808	909178.280902	41.386957
3537.261443	908507.710502	41.391962
3536.853819	907848.462938	41.396967
3536.934032	907180.569443	41.401972
3537.155605	906517.874297	41.406976
3536.915145	905846.017701	41.411981
3536.857994	905170.479994	41.416986
3536.553101	904508.502602	41.421991
3537.012352	903840.624412	41.426996
3536.820112	903172.005504	41.432000
3536.838825	902505.296681	41.437005
3537.069084	901832.392526	41.442010
3536.757485	901166.834864	41.447015
3536.491088	900491.730920	41.452020
3536.985164	899828.386321	41.457024
3536.860848	899149.524719	41.462029
3536.605503	898464.230541	41.467034
3536.302908	897800.106597	41.472039
3536.517462	897126.447592	41.477044
3536.644599	896467.695126	41.482048
3536.888488	895798.702384	41.487053
3537.022527	895123.272585	41.492058
3536.665567	894449.198854	41.497063
3536.354335	893771.654801	41.502068
3536.718719	893099.520345	41.507072
3536.166728	892431.522712	41.512077
3536.485187	891753.340698	41.517082
3536.151401	891096.556822	41.522087
3536.351155	890417.172736	41.527092
3536.144932	889755.378069	41.532096
3536.030036	889090.106134	41.537101
3536.271261	888415.990464	41.542106
3536.036078	887755.517525	41.547111
3536.058759	887078.573443	41.552116
3536.152914	886405.311342	41.557120
3536.248497	885746.583428	41.562125
3536.439686	885073.633183	41.567130
3535.897151	884415.249469	41.572135
3536.181606	883737.191092	41.577140
3536.246770	883066.933234	41.582144
3535.999228	882391.809753	41.587149
3536.046794	881709.584755	41.592154
3535.872461	881049.594018	41.597159
3535.986182	880374.852740	41.602164
3536.057635	879706.531319	41.607168
3535.874057	879034.689024	41.612173
3536.019925	878358.062186	41.617178
3535.924112	877686.825363	41.622183
3535.987990	877015.581364	41.627188
3535.961902	876350.673474	41.632192
3536.051165	875676.655051	41.637197
3536.114417	874994.904566	41.642202
3535.722230	874319.940543	41.647207
3535.564538	873646.216973	41.652212
3535.969674	872974.551246	41.657216
3535.654450	872310.013141	41.662221
3535.522318	871634.892323	41.667226
3535.717144	870965.945193	41.672231
3535.372942	870290.319676	41.677236
3535.852862	869610.109892	41.682240
3535.469233	868941.519198	41.687245
3535.634547	868261.306366	41.692250
3535.410868	867600.497467	41.697255
3535.619741	866925.658547	41.702260
3535.696561	866256.106483	41.707264
3535.451751	865581.485045	41.712269
3535.483920	864906.254987	41.717274
3535.429166	864237.665898	41.722279
3535.295347	863559.884978	41.727284
3535.864923	862886.571080	41.732288
3535.731513	862221.269410	41.737293
3535.827976	861526.217789	41.742298
3535.580609	860854.177614	41.747303
3535.636801	860163.835856	41.752308
3536.054214	859484.046581	41.757312
3535.553838	858797.921772	41.762317
3535.791745	858113.149282	41.767322
3535.530331	857441.123341	41.772327
3535.227430	856764.848867	41.777332
3535.431884	856079.367899	41.782336
3535.104692	855406.837933	41.787341
3535.324566	854720.910647	41.792346
3535.285881	854049.933846	41.797351
3535.066892	853378.136223	41.802356
3535.140048	852703.685331	41.807360
3534.866945	852032.042193	41.812365
3534.918024	851353.067963	41.817370
3534.750589	850682.720195	41.822375
3534.795366	850010.024487	41.827380
3535.157800	849330.386001	41.832384
3535.153778	848665.829069	41.837389
3534.898773	847981.182295	41.842394
3535.110153	847300.276559	41.847399
3534.746479	846624.459898	41.852404
3534.973625	845947.495068	41.857408
3534.746224	845271.119156	41.862413
3535.023643	844598.189301	41.867418
3534.928628	843938.601501	41.872423
3534.574878	843257.254952	41.877428
3534.973583	842581.261992	41.882432
3534.741288	841900.527627	41.887437
3534.558014	841229.655604	41.892442
3534.571172	840556.436245	41.897447
3534.476643	839876.484006	41.902452
3534.734142	839207.223751	41.907456
3534.322453	838541.664629	41.912461
3535.068302	837849.062433	41.917466
3534.405178	837177.209336	41.922471
3534.375438	836504.835765	41.927476
3534.704964	835827.597623	41.932480
3534.169651	835161.462443	41.937485
3534.268150	834490.221133	41.942490
3534.322633	833822.821226	41.947495
3534.185720	833141.962419	41.952500
3534.031387	832472.114971	41.957504
3534.507457	831808.534137	41.962509
3534.289281	831121.177820	41.967514
3534.251729	830454.762426	41.972519
3534.100259	829786.149076	41.977524
3534.411877	829110.843240	41.982528
3534.293958	828447.702358	41.987533
3533.834867	827766.282633	41.992538
3533.693407	827100.516898	41.997543
3533.883647	826437.264772	42.002548
3534.030197	825766.232173	42.007552
3533.604631	825098.844502	42.012557
3533.579957	824425.699768	42.017562
3533.804612	823761.045838	42.022567
3533.588842	823106.078593	42.027572
3533.978565	822426.351785	42.032576
3533.833203	821766.838989	42.037581
3533.849963	821093.443109	42.042586
3534.098300	820422.041729	42.047591
3533.904966	819753.386309	42.052596
3533.514202	819079.120827	42.057600
3533.491365	818425.465116	42.062605
3534.078424	817749.527649	42.067610
3533.687270	817093.210598	42.072615
3533.368251	816418.270891	42.077620
3533.542600	815750.959616	42.082624
3533.396512	815089.949835	42.087629
3533.159571	814418.317446	42.092634
3533.434825	813750.984800	42.097639
3533.015246	813080.473068	42.102644
3533.168539	812420.519172	42.107648
3533.817856	811762.521305	42.112653
3533.998627	811081.228476	42.117658
3533.418871	810424.288991	42.122663
3533.454405	809751.604336	42.127668
3533.696287	809071.665420	42.132672
3533.460018	808409.180665	42.137677
3533.338360	807732.451655	42.142682
3533.409502	807071.939514	42.147687
3533.159618	806402.596906	42.152692
3533.640277	805736.641472	42.157696
3533.412053	805084.564248	42.162701
3533.534561	804402.854758	42.167706
3533.379052	803730.292359	42.172711
3533.362593	803052.933230	42.177716
3533.273740	802379.540318	42.182720
3533.153310	801716.679197	42.187725
3533.155511	801037.891932	42.192730
3533.189541	800380.270453	42.197735
3532.973723	799712.033288	42.202740
3532.989221	799044.525905	42.207744
3533.034908	798392.158430	42.212749
3532.954143	797720.271176	42.217754
3532.890083	797059.406302	42.222759
3532.567822	796392.731474	42.227764
3532.888606	795721.563712	42.232768
3532.701010	795060.333511	42.237773
3532.539274	794392.654310	42.242778
3532.986594	793730.404203	42.247783
3532.911502	793067.935053	42.252788
3532.915590	792406.273591	42.257792
3532.539146	791745.449514	42.262797
3532.764517	791083.674666	42.267802
3532.581875	790422.152789	42.272807
3532.761346	789751.369945	42.277812
3533.027134	789086.944383	42.282816
3532.574291	788433.879569	42.287821
3532.753551	787749.345943	42.292826
3532.827247	787092.529571	42.297831
3532.158911	786426.244591	42.302836
3532.169089	785753.735649	42.307840
3531.973369	785108.774794	42.312845
3532.351271	784454.169678	42.317850
3532.314486	783795.543790	42.322855
3532.001985	783142.607918	42.327860
3532.362330	782481.875643	42.332864
3532.579366	781828.483698	42.337869
3532.068154	781159.811513	42.342874
3532.084648	780505.890845	42.347879
3531.816327	779845.269288	42.352884
3531.749961	779186.963336	42.357888
3531.718570	778542.761251	42.362893
3531.942613	777892.504323	42.367898
3531.664851	777239.322086	42.372903
3531.593966	776596.380651	42.377908
3531.898829	775943.129921	42.382912
3531.551912	775292.294487	42.387917
3531.716285	774642.445826	42.392922
3531.851167	773985.898025	42.397927
3531.546290	773341.084480	42.402932
3531.551147	772678.631606	42.407936
3531.288534	772047.681206	42.412941
3531.618193	771385.991737	42.417946
3531.680957	770743.152367	42.422951
3531.670621	770090.959584	42.427956
3531.479624	769435.291563	42.432960
3531.342796	768801.627449	42.437965
3531.441273	768152.791982	42.442970
3531.254832	767506.264207	42.447975
3531.247725	766862.606183	42.452980
3531.550908	766215.833073	42.457984
3531.248976	765569.205577	42.462989
3531.186507	764921.396602	42.467994
3531.198015	764271.793333	42.472999
3531.043165	763627.486436	42.478004
3531.134815	762986.385375	42.483008
3530.890341	762347.949513	42.488013
3531.047026	761698.640485	42.493018
3530.939606	761063.967766	42.498023
3531.066130	760418.794652	42.503028
3531.240465	759773.508798	42.508032
3530.732472	759137.706316	42.513037
3530.915635	758497.045558	42.518042
3530.703679	757853.536373	42.523047
3530.774777	757207.259702	42.528052
3530.443860	756572.839896	42.533056
3530.631876	755944.792868	42.538061
3530.940277	755296.339152	42.543066
3530.810537	754662.120570	42.548071
3530.574996	754024.905549	42.553076
3530.584528	753388.138613	42.558080
3530.282465	752758.777652	42.563085
3530.382655	752118.828710	42.568090
3530.539586	751492.396189	42.573095
3530.314833	750865.681497	42.578100
3530.286646	750227.819373	42.583104
3529.963390	749605.710873	42.588109
3530.301782	748970.398802	42.593114
3530.385710	748338.733596	42.598119
3529.980225	747706.062951	42.603124
3530.005444	747069.759207	42.608128
3529.699557	746455.052905	42.613133
3530.243356	745833.481843	42.618138
3530.103668	745204.218983	42.623143
3530.026316	744571.484492	42.628148
3529.974688	743940.028931	42.633152
3529.819756	743317.833233	42.638157
3529.658113	742690.101926	42.643162
3529.676997	742074.204545	42.648167
3529.425129	741455.882402	42.653172
3529.967389	740823.876983	42.658176
3529.636731	740208.437233	42.663181
3529.758053	739575.760847	42.668186
3529.760394	738957.446772	42.673191
3529.631305	738335.050893	42.678196
3529.615407	737714.268717	42.683200
3529.298085	737102.196322	42.688205
3529.325935	736484.179902	42.693210
3529.464765	735870.797032	42.698215
3529.062408	735251.768944	42.703220
3529.541637	734629.523735	42.708224
3529.265049	734018.246937	42.713229
3528.829042	733403.090215	42.718234
3529.268776	732789.964202	42.723239
3529.199783	732178.957317	42.728244
3529.386461	731561.474264	42.733248
3529.070706	730952.941244	42.738253
3528.885041	730337.754979	42.743258
3528.838250	729730.420771	42.748263
3528.905574	729127.874460	42.753268
3529.436946	728512.030885	42.758272
3529.321367	727900.609460	42.763277
3529.012320	727281.596831	42.768282
3529.376392	726673.815233	42.773287
3529.119910	726054.353662	42.778292
3529.177198	725437.565903	42.783296
3528.770502	724833.990070	42.788301
3528.698236	724213.564888	42.793306
3528.586324	723610.344123	42.798311
3528.373889	723008.582934	42.803316
3528.753021	722398.598362	42.808321
3529.025661	721801.077012	42.813325
3528.451436	721191.859834	42.818330
3528.340022	720584.947725	42.823335
3527.991299	719989.433892	42.828340
3528.297560	719382.858142	42.833345
3528.150186	718794.115547	42.838349
3528.779686	718178.471884	42.843354
3528.501885	717587.087668	42.848359
3528.620848	716985.179246	42.853364
3528.450458	716374.051872	42.858369
3528.117437	715770.794024	42.863373
3528.100679	715166.744268	42.868378
3528.175710	714570.870145	42.873383
3527.739108	713979.605285	42.878388
3527.979614	713385.950617	42.883393
3527.823382	712802.791185	42.888397
3527.887494	712201.541336	42.893402
3528.126380	711610.342305	42.898407
3527.772352	711026.498524	42.903412
3527.900796	710432.159142	42.908417
3527.612535	709841.274091	42.913421
3527.704009	709247.652278	42.918426
3527.711245	708662.889349	42.923431
3527.461567	708072.123072	42.928436
3527.685049	707479.398117	42.933441
3527.554349	706899.453147	42.938445
3527.508930	706307.437679	42.943450
3527.533655	705714.177534	42.948455
3527.548427	705137.961965	42.953460
3527.641053	704547.837749	42.958465
3527.279161	703964.158007	42.963469
3527.327771	703387.720193	42.968474
3527.419065	702797.327392	42.973479
3527.001885	702210.061206	42.978484
3527.389735	701634.640934	42.983489
3526.970314	701069.754326	42.988493
3526.824635	700476.858991	42.993498
3526.886897	699900.683798	42.998503
3526.808493	699337.067519	43.003508
3526.981158	698767.358401	43.008513
3527.047662	698196.536814	43.013517
3526.952531	697626.202634	43.018522
3526.829372	697046.640019	43.023527
3526.825944	696475.767976	43.028532
3526.857761	695902.864225	43.033537
3526.693897	695335.574757	43.038541
3526.722329	694769.110927	43.043546
3527.290282	694190.087450	43.048551
3526.942142	693623.564718	43.053556
3527.164212	693047.061603	43.058561
3526.972336	692467.906010	43.063565
3526.577404	691888.200181	43.068570
3526.876421	691320.425111	43.073575
3526.617660	690750.022887	43.078580
3526.493582	690174.486958	43.083585
3526.511843	689606.103446	43.088589
3526.317435	689042.247691	43.093594
3526.543255	688471.517779	43.098599
3526.495126	687912.442129	43.103604
3526.413462	687340.050697	43.108609
3526.599503	686780.516327	43.113613
3526.060369	686205.343939	43.118618
3526.502346	685639.523674	43.123623
3526.100889	685082.821334	43.128628
3526.614719	684513.483841	43.133633
3526.107380	683957.875313	43.138637
3526.122301	683389.000434	43.143642
3526.023829	682817.221609	43.148647
3525.937278	682266.317017	43.153652
3526.075481	681710.560540	43.158657
3526.041028	681148.774272	43.163661
3525.842092	680592.459560	43.168666
3526.023690	680046.205881	43.173671
3525.753062	679479.426988	43.178676
3525.903774	678923.698403	43.183681
3525.951783	678376.023317	43.188685
3525.719231	677820.592412	43.193690
3526.104963	677265.719944	43.198695
3525.839741	676716.604869	43.203700
3526.231279	676149.009832	43.208705
3526.022612	675601.562781	43.213709
3525.991975	675040.549102	43.218714
3526.129121	674483.459533	43.223719
3525.817059	673922.874941	43.228724
3525.984416	673360.579915	43.233729
3525.730203	672806.247849	43.238733
3525.791589	672251.729321	43.243738
3525.823434	671692.896062	43.248743
3525.480376	671145.260066	43.253748
3525.518998	670592.192600	43.258753
3525.212727	670049.023083	43.263757
3525.077404	669501.704552	43.268762
3525.294067	668950.753918	43.273767
3525.230480	668416.124922	43.278772
3525.041205	667869.419072	43.283777
3524.887872	667326.166482	43.288781
3524.574530	666789.144305	43.293786
3524.810892	666258.731242	43.298791
3524.635755	665727.909934	43.303796
3524.806807	665183.581623	43.308801
3524.864477	664651.064352	43.313805
3524.400978	664114.515565	43.318810
3524.517549	663588.613997	43.323815
3524.442715	663069.401926	43.328820
3524.419580	662527.150863	43.333825
3524.477114	662005.313930	43.338829
3524.288916	661476.953542	43.343834
3524.476920	660952.093046	43.348839
3524.336643	660430.953151	43.353844
3524.362320	659907.660601	43.358849
3524.410565	659382.888432	43.363853
3524.264393	658854.327484	43.368858
3524.780849	658327.122141	43.373863
3524.527294	657808.156688	43.378868
3524.493182	657278.292767	43.383873
3524.516586	656746.343249	43.388877
3524.424667	656215.083418	43.393882
3525.075489	655695.301880	43.398887
3524.260071	655164.308201	43.403892
3524.510900	654640.444382	43.408897
3524.046940	654111.830525	43.413901
3523.927466	653587.324539	43.418906
3523.945999	653063.416317	43.423911
3523.876125	652554.379614	43.428916
3523.813483	652039.621147	43.433921
3523.918254	651526.705479	43.438925
3523.842428	651002.154551	43.443930
3523.897257	650486.396061	43.448935
3523.700917	649970.403854	43.453940
3523.575931	649452.623980	43.458945
3523.509641	648950.596212	43.463949
3523.458495	648423.006970	43.468954
3523.371542	647906.489431	43.473959
3523.282037	647415.431914	43.478964
3523.252742	646906.098968	43.483969
3523.224566	646404.886382	43.488973
3523.801137	645895.848521	43.493978
3523.832952	645393.375705	43.498983
3523.356530	644884.666398	43.503988
3523.252662	644371.868761	43.508993
3522.858155	643871.542372	43.513997
3522.834319	643374.227509	43.519002
3523.414931	642873.785293	43.524007
3522.959848	642380.844914	43.529012
3523.118660	641872.425653	43.534017
3523.179349	641377.898546	43.539021
3523.325437	640889.083455	43.544026
3523.197365	640374.037663	43.549031
3522.944463	639884.892534	43.554036
3523.074569	639379.404500	43.559041
3523.064373	638886.619314	43.564045
3522.950138	638391.177282	43.569050
3522.985522	637886.582172	43.574055
3522.989492	637397.524630	43.579060
3523.059301	636907.832327	43.584065
3522.865559	636413.459220	43.589069
3522.481320	635914.942517	43.594074
3522.854394	635422.426412	43.599079
3522.453608	634935.572816	43.604084
3522.726199	634445.479126	43.609089
3522.610854	633959.581779	43.614093
3522.272058	633469.096079	43.619098
3522.795318	632978.990579	43.624103
3522.463534	632503.070960	43.629108
3522.822029	632005.491035	43.634113
3522.683372	631523.187730	43.639117
3522.269604	631034.101978	43.644122
3522.380683	630541.750323	43.649127
3522.412619	630068.561175	43.654132
3522.335983	629582.904369	43.659137
3522.152444	629095.991865	43.664141
3521.882773	628620.185902	43.669146
3522.330609	628135.424258	43.674151
3521.732036	627668.593553	43.679156
3521.706827	627180.914887	43.684161
3521.914076	626727.674747	43.689165
3521.762091	626251.842429	43.694170
3522.147577	625781.405624	43.699175
3521.715051	625313.241146	43.704180
3521.762977	624835.458449	43.709185
3522.008012	624366.185180	43.714189
3521.626370	623897.799701	43.719194
3521.801552	623421.184262	43.724199
3521.417515	622958.067537	43.729204
3521.685040	622487.756445	43.734209
3521.511916	622024.663668	43.739213
3521.405020	621565.246888	43.744218
3521.337947	621088.018324	43.749223
3521.448458	620635.137995	43.754228
3521.513308	620170.973092	43.759233
3521.191088	619707.104908	43.764237
3521.220432	619246.363783	43.769242
3521.307953	618791.355872	43.774247
3520.934190	618351.942540	43.779252
3520.978891	617886.580933	43.784257
3521.015623	617435.584309	43.789261
3521.028901	616985.124362	43.794266
3520.965943	616535.360558	43.799271
3520.802480	616090.357099	43.804276
3521.059551	615630.326559	43.809281
3520.958718	615182.017431	43.814285
3520.835719	614730.986832	43.819290
3521.051254	614276.320643	43.824295
3520.861125	613835.742228	43.829300
3520.597310	613385.131778	43.834305
3520.707561	612941.157464	43.839309
3520.642170	612495.089478	43.844314
3520.766608	612049.572816	43.849319
3520.206039	611606.361516	43.854324
3520.422197	611160.893818	43.859329
3520.460896	610724.916397	43.864333
3520.873788	610288.506982	43.869338
3520.818029	609838.970768	43.874343
3520.933364	609397.762822	43.879348
3520.633074	608948.132217	43.884353
3520.769851	608511.399628	43.889357
3520.649095	608065.815847	43.894362
3520.395470	607619.735457	43.899367
3520.554792	607185.806644	43.904372
3520.778261	606733.840931	43.909377
3520.690737	606296.458628	43.914381
3520.470677	605859.383021	43.919386
3520.703475	605411.928169	43.924391
3520.452217	604983.854814	43.929396
3520.157847	604532.792627	43.934401
3520.152591	604095.060341	43.939405
3519.687361	603666.722953	43.944410
3520.114011	603235.959046	43.949415
3519.817099	602811.976653	43.954420
3519.687831	602375.052528	43.959425
3519.781530	601955.187110	43.964429
3519.761780	601537.784866	43.969434
3519.989644	601110.236989	43.974439
3519.543974	600680.077821	43.979444
3519.323253	600272.150065	43.984449
3519.536530	599852.639019	43.989453
3519.619974	599439.811081	43.994458
3519.408787	599012.862565	43.999463
3519.183337	598601.312340	44.004468
3519.425132	598179.476568	44.009473
3519.498417	597765.034247	44.014477
3519.204985	597360.982188	44.019482
3519.621312	596943.891449	44.024487
3519.399492	596526.844488	44.029492
3519.093226	596114.767938	44.034497
3519.368201	595695.648140	44.039501
3519.331928	595286.609450	44.044506
3519.315213	594866.254305	44.049511
3519.217221	594474.522551	44.054516
3519.142927	594049.829120	44.059521
3519.282928	593639.296599	44.064525
3518.649306	593238.826138	44.069530
3518.911605	592828.445304	44.074535
3518.679449	592428.380966	44.079540
3518.630223	592022.947540	44.084545
3518.813048	591637.804011	44.089549
3518.924034	591232.969116	44.094554
3518.998155	590823.153488	44.099559
3518.805862	590431.052186	44.104564
3519.106941	590024.385293	44.109569
3518.974023	589619.185278	44.114573
3518.704960	589219.772410	44.119578
3518.735650	588824.414859	44.124583
3518.759785	588425.578466	44.129588
3518.876496	588026.461717	44.134593
3518.690832	587620.398850	44.139597
3518.580453	587227.826421	44.144602
3518.578516	586825.323180	44.149607
3518.506104	586436.386685	44.154612
3518.463208	586044.266545	44.159617
3518.325424	585644.159138	44.164621
3518.049609	585256.626397	44.169626
3518.260789	584864.173180	44.174631
3518.200353	584486.530251	44.179636
3518.311111	584090.550809	44.184641
3518.184529	583709.778665	44.189645
3517.930165	583324.090354	44.194650
3518.196918	582929.855929	44.199655
3518.248218	582549.720765	44.204660
3518.092958	582169.558724	44.209665
3518.104031	581778.749048	44.214669
3517.811777	581414.171131	44.219674
3518.277301	581020.645377	44.224679
3517.600932	580641.178279	44.229684
3517.890521	580268.271768	44.234689
3517.755039	579888.236496	44.239693
3517.423484	579517.474683	44.244698
3517.849064	579138.024345	44.249703
3517.743753	578770.821752	44.254708
3517.639959	578395.763373	44.259713
3517.820853	578022.053030	44.264717
3517.520042	577649.519979	44.269722
3517.831624	577268.472654	44.274727
3517.591075	576891.631812	44.279732
3517.500422	576513.999518	44.284737
3517.758625	576146.455757	44.289741
3517.457707	575781.612003	44.294746
3517.571082	575399.987904	44.299751
3517.335773	575029.276336	44.304756
3517.334072	574667.970440	44.309761
3517.374688	574296.837901	44.314765
3517.228844	573935.133007	44.319770
3517.334404	573565.678025	44.324775
3517.374696	573211.063803	44.329780
3517.140181	572846.022373	44.334785
3517.259298	572480.557792	44.339789
3517.198347	572128.898586	44.344794
3517.164670	571753.578009	44.349799
3517.168729	571393.686236	44.354804
3517.096292	571038.828810	44.359809
3517.271057	570681.604643	44.364813
3517.226499	570321.137152	44.369818
3517.146793	569952.765210	44.374823
3517.101103	569604.807161	44.379828
3516.950688	569238.590376	44.384833
3516.909612	568881.352376	44.389837
3516.714473	568546.273818	44.394842
3516.933109	568174.578612	44.399847
3516.616449	567820.528525	44.404852
3516.377012	567473.098944	44.409857
3516.791941	567125.145557	44.414861
3516.591424	566778.596441	44.419866
3516.695227	566432.086668	44.424871
3516.778127	566097.299163	44.429876
3516.637696	565733.295672	44.434881
3516.563024	565391.318592	44.439885
3516.344291	565045.229231	44.444890
3516.332850	564701.964596	44.449895
3516.328836	564360.854264	44.454900
3516.526668	564019.700472	44.459905
3516.577416	563673.780089	44.464909
3516.615549	563333.239622	44.469914
3516.371515	562987.552649	44.474919
3516.054008	562646.249331	44.479924
3515.944935	562309.634339	44.484929
3516.164356	561969.127885	44.489933
3515.958068	561638.201809	44.494938
3516.309209	561306.114744	44.499943
3516.224098	560980.941982	44.504948
3516.348943	560638.856001	44.509953
3516.296958	560307.970625	44.514957
3516.324707	559965.178635	44.519962
3516.456792	559624.223204	44.524967
3516.183961	559291.436234	44.529972
3516.054178	558950.558410	44.534977
3516.147738	558612.051101	44.539981
3515.853986	558281.206374	44.544986
3515.964438	557954.061825	44.549991
3515.796051	557620.660834	44.554996
3515.761467	557295.791315	44.560001
3515.974584	556972.684865	44.565005
3515.663059	556645.227444	44.570010
3516.110944	556304.888012	44.575015
3515.798611	555984.869608	44.580020
3515.775828	555659.454313	44.585025
3515.758950	555328.035280	44.590029
3515.444657	555010.663762	44.595034
3515.460473	554693.480234	44.600039
3515.402604	554374.790366	44.605044
3515.314092	554051.513459	44.610049
3515.595913	553719.802049	44.615053
3515.413847	553410.733502	44.620058
3515.689729	553083.441141	44.625063
3515.378014	552767.074132	44.630068
3515.487995	552454.054016	44.635073
3515.600883	552144.805260	44.640077
3515.454034	551829.143913	44.645082
3515.467956	551499.136784	44.650087
3514.931788	551186.348775	44.655092
3514.861156	550869.996932	44.660097
3515.115143	550573.588777	44.665101
3515.039974	550269.671058	44.670106
3515.128122	549944.602543	44.675111
3515.253918	549649.153645	44.680116
3514.748238	549333.999457	44.685121
3515.168406	549025.181491	44.690125
3514.679692	548722.912649	44.695130
3514.852352	548422.842691	44.700135
3515.031973	548109.609717	44.705140
3515.076742	547806.775908	44.710145
3514.967235	547497.661061	44.715149
3514.662840	547193.764409	44.720154
3514.719018	546887.379896	44.725159
3514.700412	546595.871937	44.730164
3514.620039	546293.631040	44.735169
3514.823673	545990.125159	44.740173
3514.652445	545692.776475	44.745178
3514.922510	545397.513810	44.750183
3514.629961	545101.836759	44.755188
3514.614187	544798.190919	44.760193
3514.686151	544496.993854	44.765197
3514.500273	544207.783233	44.770202
3514.563006	543899.970089	44.775207
3514.428673	543613.107964	44.780212
3514.233087	543318.334326	44.785217
3514.730085	543030.444832	44.790221
3514.478131	542738.996404	44.795226
3514.441099	542440.748391	44.800231
3514.390182	542158.632376	44.805236
3514.288901	541860.282101	44.810241
3514.560285	541572.501956	44.815245
3514.265720	541288.392928	44.820250
3514.291350	540993.633364	44.825255
3514.197487	540708.570611	44.830260
3513.993079	540424.226992	44.835265
3514.267898	540139.089756	44.840269
3514.119004	539855.330362	44.845274
3513.976192	539560.720858	44.850279
3514.026624	539283.976741	44.855284
3514.033661	539014.446997	44.860289
3513.995520	538717.229799	44.865293
3513.871382	538445.341068	44.870298
3513.905840	538158.792669	44.875303
3514.197515	537879.508409	44.880308
3513.676632	537593.648711	44.885313
3514.079499	537311.358275	44.890317
3513.808615	537041.737649	44.895322
3514.307321	536762.043019	44.900327
3513.977144	536488.083849	44.905332
3513.980231	536210.480846	44.910337
3514.049216	535918.382870	44.915341
3514.039255	535652.374116	44.920346
3514.118871	535361.826868	44.925351
3513.827359	535083.243337	44.930356
3513.419930	534811.888697	44.935361
3513.912279	534535.279650	44.940365
3513.722638	534259.639435	44.945370
3514.009680	533989.008406	44.950375
3513.890366	533711.125719	44.955380
3513.745592	533438.792177	44.960385
3513.558096	533160.557347	44.965389
3513.689951	532902.042091	44.970394
3513.885862	532628.222304	44.975399
3513.782969	532351.622623	44.980404
3513.770688	532089.787155	44.985409
3514.293930	531807.570000	44.990413
3513.860304	531548.773957	44.995418
3513.709396	531253.692306	45.000423
3513.951654	530978.319621	45.005428
3513.540594	530707.897962	45.010433
3514.029948	530433.532583	45.015437
3513.562657	530164.927259	45.020442
3513.853018	529886.649155	45.025447
3514.060286	529614.587657	45.030452
3513.359364	529353.678649	45.035457
3513.391400	529077.347153	45.040461
3513.402837	528814.893753	45.045466
3513.094248	528538.660761	45.050471
3513.169592	528279.114317	45.055476
3512.984483	528027.683709	45.060481
3513.243064	527761.585648	45.065485
3513.326614	527512.169882	45.070490
3513.196599	527247.895592	45.075495
3512.847775	526991.427574	45.080500
3513.207707	526735.591284	45.085505
3513.320776	526476.763940	45.090509
3513.127842	526215.611733	45.095514
3513.287355	525957.373175	45.100519
3512.668574	525704.462716	45.105524
3512.821904	525451.668544	45.110529
3513.274711	525189.832760	45.115533
3512.838140	524944.349950	45.120538
3512.909439	524686.356851	45.125543
3512.761368	524434.404683	45.130548
3512.603325	524187.751175	45.135553
3512.842032	523933.452592	45.140557
3512.777839	523692.076188	45.145562
3512.758980	523441.852389	45.150567
3512.736518	523192.836818	45.155572
3512.655422	522941.756969	45.160577
3512.839025	522685.931917	45.165581
3512.480450	522448.827194	45.170586
3512.651580	522203.397731	45.175591
3512.788965	521948.931411	45.180596
3512.408991	521708.284042	45.185601
3512.611246	521461.473820	45.190605
3512.504378	521226.882269	45.195610
3512.691251	520978.854866	45.200615
3512.466587	520739.630032	45.205620
3512.293560	520494.433613	45.210625
3512.397189	520248.276983	45.215629
3511.873422	520021.464599	45.220634
3512.070612	519788.212945	45.225639
3512.148782	519554.473011	45.230644
3511.875119	519323.769295	45.235649
3512.031663	519088.342210	45.240653
3511.988300	518851.379961	45.245658
3511.906069	518616.087380	45.250663
3511.789164	518391.151032	45.255668
3511.794368	518161.695345	45.260673
3511.881797	517929.949304	45.265677
3511.722808	517712.535944	45.270682
3511.852582	517485.624848	45.275687
3511.835563	517256.816061	45.280692
3511.468868	517033.013695	45.285697
3511.735798	516813.443935	45.290701
3511.585779	516592.578391	45.295706
3511.844364	516366.032910	45.300711
3511.811422	516142.059600	45.305716
3511.454114	515932.484699	45.310721
3512.084976	515702.329878	45.315725
3511.699950	515479.164821	45.320730
3511.700824	515253.657385	45.325735
3511.347442	515026.691617	45.330740
3511.147185	514818.186222	45.335745
3511.575440	514605.630208	45.340749
3511.992159	514393.224820	45.345754
3512.015888	514167.748242	45.350759
3512.090716	513943.977407	45.355764
3511.863652	513725.408171	45.360769
3512.113340	513495.993090	45.365773
3511.630951	513278.117984	45.370778
3511.575200	513058.297594	45.375783
3511.800109	512828.169605	45.380788
3511.620815	512623.218572	45.385793
3511.786869	512406.079548	45.390797
3511.773335	512189.978726	45.395802
3512.151628	511947.179831	45.400807
3511.720296	511738.925441	45.405812
3511.493698	511516.384074	45.410817
3511.545765	511295.712123	45.415821
3511.117574	511089.570865	45.420826
3511.076213	510872.799809	45.425831
3511.493479	510664.790580	45.430836
3511.176273	510455.286973	45.435841
3511.073337	510239.932665	45.440845
3511.055538	510041.085528	45.445850
3510.955302	509829.161486	45.450855
3511.187398	509626.072094	45.455860
3511.292539	509417.847107	45.460865
3511.388126	509201.535150	45.465869
3511.205424	509004.370890	45.470874
3510.916272	508801.410495	45.475879
3511.213136	508594.354903	45.480884
3511.103189	508391.914617	45.485889
3511.124848	508178.734824	45.490893
3510.900491	507984.850158	45.495898
3510.963279	507776.054996	45.500903
3510.755565	507586.054323	45.505908
3510.772956	507386.207725	45.510913
3511.077555	507172.662954	45.515917
3511.022794	506984.701301	45.520922
3510.582402	506776.787725	45.525927
3510.757241	506580.341219	45.530932
3511.115456	506381.687540	45.535937
3510.985328	506183.670798	45.540941
3510.906287	505989.989928	45.545946
3510.827301	505779.878785	45.550951
3510.976308	505575.488467	45.555956
3510.781034	505384.954158	45.560961
3510.963325	505192.583907	45.565965
3510.737738	504997.298562	45.570970
3510.881016	504795.376302	45.575975
3510.852678	504594.845709	45.580980
3510.809981	504399.724132	45.585985
3510.687286	504198.294811	45.590989
3510.815538	504013.907074	45.595994
3510.337131	503829.924149	45.600999
3510.542480	503631.717773	45.606004
3510.513234	503437.795644	45.611009
3510.970008	503247.731543	45.616013
3510.441414	503045.952807	45.621018
3509.957589	502851.545199	45.626023
3510.082501	502676.141962	45.631028
3510.091183	502501.919516	45.636033
3510.186465	502316.153138	45.641037
3510.104851	502132.588887	45.646042
3510.425818	501951.785167	45.651047
3510.492945	501771.730634	45.656052
3510.258588	501587.124591	45.661057
3510.227344	501405.060407	45.666061
3510.226018	501227.691330	45.671066
3510.338186	501044.132371	45.676071
3510.610445	500865.195805	45.681076
3510.522960	500678.430840	45.686081
3510.540084	500486.184991	45.691085
3510.462122	500306.897648	45.696090
3510.431685	500120.015485	45.701095
3509.854076	499939.545335	45.706100
3509.937380	499761.792070	45.711105
3510.129221	499575.877123	45.716109
3510.141174	499393.429378	45.721114
3510.079530	499217.212031	45.726119
3509.996732	499042.311199	45.731124
3509.718410	498875.280082	45.736129
3509.646206	498700.677253	45.741133
3509.705551	498536.012398	45.746138
3509.915185	498358.121374	45.751143
3510.009113	498183.889315	45.756148
3509.784828	498019.014916	45.761153
3509.668414	497841.426900	45.766157
3509.637380	497674.088635	45.771162
3509.736053	497506.726545	45.776167
3509.666270	497335.649100	45.781172
3509.910083	497156.323361	45.786177
3509.862352	496984.530521	45.791181
3509.756029	496824.024166	45.796186
3509.589994	496653.613655	45.801191
3509.853828	496480.245175	45.806196
3509.071322	496320.557515	45.811201
3509.703693	496154.759811	45.816205
3509.756515	495994.420651	45.821210
3509.883236	495823.142478	45.826215
3509.810446	495651.390841	45.831220
3509.989530	495489.052738	45.836225
3510.366643	495319.952174	45.841229
3509.923292	495141.733840	45.846234
3509.778555	494975.349088	45.851239
3510.087652	494797.807935	45.856244
3509.806799	494628.408135	45.861249
3509.681784	494458.625954	45.866253
3509.256415	494295.671430	45.871258
3509.213146	494130.525603	45.876263
3509.455200	493965.632951	45.881268
3509.131177	493813.582551	45.886273
3509.516306	493656.199493	45.891277
3509.513956	493501.966824	45.896282
3509.221292	493341.964991	45.901287
3509.584856	493189.791603	45.906292
3509.362511	493026.891398	45.911297
3509.454165	492862.317237	45.916301
3509.526388	492708.874036	45.921306
3509.356859	492544.746104	45.926311
3509.149555	492387.503058	45.931316
3508.948745	492234.152793	45.936321
3509.075115	492083.021804	45.941325
3509.025742	491933.993663	45.946330
3509.133353	491778.917192	45.951335
3509.130118	491620.468672	45.956340
3509.103385	491477.351791	45.961345
3509.230895	491324.493815	45.966349
3509.073959	491177.905852	45.971354
3509.358591	491031.544796	45.976359
3509.220946	490876.653818	45.981364
3508.937950	490720.319056	45.986369
3509.228376	490561.254090	45.991373
3509.091719	490413.694864	45.996378
3509.186386	490264.172280	46.001383
3509.550965	490111.111254	46.006388
3509.045386	489964.420691	46.011393
3509.017688	489802.822673	46.016397
3509.063175	489656.541361	46.021402
3508.851873	489503.725067	46.026407
3508.868307	489354.056166	46.031412
3508.863993	489208.032549	46.036417
3509.285810	489056.520939	46.041421
3509.025598	488914.383997	46.046426
3508.760310	488775.687487	46.051431
3509.148671	488621.900838	46.056436
3508.816613	488484.326585	46.061441
3508.884197	488326.797107	46.066445
3508.831080	488194.232956	46.071450
3508.740210	488045.633700	46.076455
3508.771337	487901.819489	46.081460
3508.678506	487766.981795	46.086465
3508.597988	487616.757849	46.091469
3508.690574	487481.177852	46.096474
3508.620826	487344.713663	46.101479
3508.872776	487201.766829	46.106484
3508.471841	487071.125853	46.111489
3508.481337	486924.777084	46.116493
3508.315105	486793.587914	46.121498
3508.547645	486656.510085	46.126503
3508.874350	486517.998150	46.131508
3508.256123	486389.970068	46.136513
3508.611817	486246.441053	46.141517
3508.485480	486119.541559	46.146522
3508.355569	485981.710634	46.151527
3508.637927	485849.577485	46.156532
3508.695550	485720.872439	46.161537
3508.831961	485575.452287	46.166541
3508.689518	485437.973496	46.171546
3508.548052	485301.303208	46.176551
3508.733815	485160.881498	46.181556
3508.508590	485035.053862	46.186561
3508.409469	484891.439622	46.191565
3508.707741	484758.080924	46.196570
3508.756167	484630.887805	46.201575
3508.815822	484489.621902	46.206580
3508.482022	484350.446521	46.211585
3508.648157	484208.704688	46.216589
3508.487236	484077.646198	46.221594
3508.546750	483939.210227	46.226599
3508.644008	483802.436971	46.231604
3508.268991	483688.114544	46.236609
3508.247856	483547.310442	46.241613
3508.164238	483418.460899	46.246618
3508.236015	483294.139218	46.251623
3508.348315	483161.711327	46.256628
3508.579131	483039.992702	46.261633
3508.266050	482902.776428	46.266637
3508.284161	482778.359075	46.271642
3508.089507	482653.622866	46.276647
3508.649245	482523.948364	46.281652
3508.483001	482397.687005	46.286657
3508.537769	482269.058602	46.291661
3508.794800	482135.737878	46.296666
3508.805724	482007.823733	46.301671
3508.796584	481862.904181	46.306676
3508.389067	481734.401483	46.311681
3508.516747	481605.806480	46.316685
3508.434637	481475.980876	46.321690
3508.449046	481337.228678	46.326695
3508.514408	481205.300501	46.331700
3508.494086	481079.612374	46.336705
3508.183970	480962.426619	46.341709
3507.672108	480830.847355	46.346714
3507.826650	480714.188103	46.351719
3507.871296	480594.357648	46.356724
3507.805794	480479.911213	46.361729
3507.965325	480345.885118	46.366733
3507.606610	480228.449762	46.371738
3507.380237	480114.180342	46.376743
3508.056189	479990.846288	46.381748
3507.436051	479890.260561	46.386753
3507.583762	479776.431372	46.391757
3507.435385	479672.473274	46.396762
3507.448134	479555.526987	46.401767
3507.888995	479436.279318	46.406772
3507.397042	479329.137867	46.411777
3507.390777	479218.115882	46.416781
3507.601135	479105.486805	46.421786
3507.395805	478997.585679	46.426791
3507.774616	478882.445737	46.431796
3507.435255	478790.615082	46.436801
3507.675465	478669.371530	46.441805
3507.483491	478555.947066	46.446810
3507.373456	478454.051181	46.451815
3507.518523	478342.592972	46.456820
3507.253221	478246.443479	46.461825
3507.555217	478129.337351	46.466829
3507.348444	478037.682768	46.471834
3507.411809	477925.780291	46.476839
3507.695109	477813.788944	46.481844
3507.088572	477715.163399	46.486849
3507.184125	477611.050582	46.491853
3507.407113	477504.130706	46.496858
3507.575798	477394.485384	46.501863
3507.461254	477292.229351	46.506868
3507.354620	477192.047304	46.511873
3507.340971	477078.481929	46.516877
3507.604274	476977.172262	46.521882
3507.631319	476877.471992	46.526887
3507.798413	476767.620653	46.531892
3507.737405	476662.060806	46.536897
3507.300053	476550.336669	46.541901
3507.610322	476444.560275	46.546906
3507.587375	476339.852852	46.551911
3507.619088	476217.058955	46.556916
3507.447403	476117.034040	46.561921
3507.755034	476007.407328	46.566925
3507.546993	475900.349150	46.571930
3507.235540	475795.991702	46.576935
3507.619341	475691.920037	46.581940
3507.446772	475600.753771	46.586945
3507.332320	475494.436795	46.591949
3507.166593	475384.077010	46.596954
3506.904396	475287.151889	46.601959
3507.142135	475179.456395	46.606964
3507.101521	475084.517872	46.611969
3507.162372	474988.194311	46.616973
3507.440131	474888.845555	46.621978
3507.248722	474790.589144	46.626983
3507.520752	474688.151338	46.631988
3507.003255	474590.304012	46.636993
3507.300627	474500.469964	46.641997
3507.128213	474397.954521	46.647002
3507.143524	474307.205544	46.652007
3507.190594	474208.550844	46.657012
3507.037359	474116.209227	46.662017
3507.643269	474008.747901	46.667021
3507.768929	473908.710890	46.672026
3507.399220	473804.352138	46.677031
3507.412368	473696.939578	46.682036
3507.365736	473608.831122	46.687041
3507.260648	473500.424780	46.692045
3507.216569	473405.832742	46.697050
3507.365037	473310.143854	46.702055
3507.240028	473209.690100	46.707060
3507.223866	473108.761431	46.712065
3507.296095	473019.718314	46.717069
3507.441387	472921.647736	46.722074
3507.204050	472817.463419	46.727079
3507.336882	472729.117583	46.732084
3507.153599	472634.899910	46.737089
3506.890014	472527.983661	46.742093
3506.809199	472434.456507	46.747098
3506.787733	472358.239399	46.752103
3507.053578	472259.283791	46.757108
3506.626442	472173.613857	46.762113
3506.372575	472080.418354	46.767117
3506.631462	471993.313665	46.772122
3506.522578	471910.930832	46.777127
3506.451881	471819.728610	46.782132
3506.754267	471737.983847	46.787137
3506.818796	471656.684518	46.792141
3506.711065	471576.477841	46.797146
3506.611359	471498.497941	46.802151
3506.542097	471402.178049	46.807156
3506.349766	471320.363996	46.812161
3506.481849	471237.076046	46.817165
3506.682984	471161.626436	46.822170
3506.252097	471077.066396	46.827175
3506.529413	470996.690202	46.832180
3506.428122	470924.380857	46.837185
3506.713320	470841.216958	46.842189
3506.755721	470746.039574	46.847194
3506.763933	470678.471640	46.852199
3506.474279	470582.944932	46.857204
3506.279793	470511.916165	46.862209
3506.568344	470432.498000	46.867213
3506.563476	470347.152836	46.872218
3506.232581	470267.687795	46.877223
3506.382249	470187.177996	46.882228
3506.634453	470117.388400	46.887233
3506.347169	470037.560386	46.892237
3506.642076	469955.049395	46.897242
3506.314089	469882.622811	46.902247
3506.466041	469800.287510	46.907252
3506.390533	469727.817223	46.912257
3506.240671	469649.331716	46.917261
3506.491314	469572.752952	46.922266
3506.432861	469502.558260	46.927271
3506.569015	469422.908617	46.932276
3506.533254	469349.062463	46.937281
3506.438401	469253.597084	46.942285
3506.536557	469177.903872	46.947290
3506.180313	469110.696491	46.952295
3506.342883	469026.329863	46.957300
3506.081649	468956.724972	46.962305
3505.741187	468887.184007	46.967309
3506.813137	468821.909887	46.972314
3506.741371	468748.675403	46.977319
3506.635929	468667.290925	46.982324
3506.502349	468589.963325	46.987329
3506.603074	468501.552510	46.992333
3506.499511	468430.399105	46.997338
3506.273241	468352.934402	47.002343
3506.315020	468271.776376	47.007348
3506.095016	468196.589492	47.012353
3506.048237	468129.629742	47.017357
3506.251630	468062.525728	47.022362
3506.350178	467988.853990	47.027367
3506.287866	467917.640972	47.032372
3506.074883	467849.796793	47.037377
3506.243458	467773.984666	47.042381
3506.126420	467709.517654	47.047386
3505.956054	467647.389787	47.052391
3506.092878	467570.974384	47.057396
3505.878458	467505.307519	47.062401
3506.096425	467438.350801	47.067405
3506.118515	467358.256082	47.072410
3506.059285	467306.239834	47.077415
3506.382952	467237.035384	47.082420
3505.837389	467171.930506	47.087425
3505.859059	467103.587683	47.092429
3505.895007	467045.323393	47.097434
3505.613364	466986.049303	47.102439
3505.742091	466923.209444	47.107444
3506.073491	466861.246651	47.112449
3506.088581	466797.969846	47.117453
3506.341174	466727.914477	47.122458
3506.223891	466656.300876	47.127463
3506.142138	466583.161124	47.132468
3506.260958	466516.370101	47.137473
3506.112811	466446.078166	47.142477
3506.183383	466370.986483	47.147482
3506.198370	466315.712566	47.152487
3506.170400	466232.024748	47.157492
3506.182958	466177.814742	47.162497
3506.013768	466110.311564	47.167501
3506.381535	466045.553536	47.172506
3506.312581	465979.501982	47.177511
3506.153964	465901.863834	47.182516
3506.158029	465839.599010	47.187521
3506.179702	465771.251454	47.192525
3505.900438	465704.778905	47.197530
3505.517279	465642.072932	47.202535
3505.846372	465587.199263	47.207540
3506.114849	465524.786950	47.212545
3505.884074	465461.345084	47.217549
3505.727048	465401.892848	47.222554
3505.746018	465347.122114	47.227559
3505.910318	465274.188703	47.232564
3505.616037	465220.991019	47.237569
3505.764689	465160.979207	47.242573
3505.766055	465094.304649	47.247578
3505.742555	465051.902460	47.252583
3505.822445	464983.288857	47.257588
3505.850423	464929.579364	47.262593
3505.773656	464863.272005	47.267597
3505.919914	464800.675568	47.272602
3505.760757	464749.682787	47.277607
3505.824469	464683.350828	47.282612
3505.990485	464626.779656	47.287617
3505.695306	464567.095118	47.292621
3506.122889	464500.953735	47.297626
3506.037688	464448.731551	47.302631
3506.100996	464383.665291	47.307636
3506.418465	464323.520733	47.312641
3506.321350	464260.254779	47.317645
3506.295173	464191.504489	47.322650
3506.136847	464126.829882	47.327655
3506.055633	464057.125841	47.332660
3506.173138	464005.729199	47.337665
3506.024698	463935.884201	47.342669
3506.312517	463869.663203	47.347674
3505.864083	463816.285319	47.352679
3505.738176	463748.259842	47.357684
3506.099773	463686.636412	47.362689
3505.701123	463632.692174	47.367693
3505.664751	463565.005448	47.372698
3505.447226	463512.550004	47.377703
3505.813343	463456.498622	47.382708
3505.476124	463406.900781	47.387713
3505.522164	463346.748888	47.392717
3505.504526	463294.157389	47.397722
3505.167205	463241.772342	47.402727
3505.226868	463199.554594	47.407732
3505.433754	463146.113650	47.412737
3505.243973	463102.620876	47.417741
3505.660154	463053.096175	47.422746
3505.350834	463004.708624	47.427751
3505.446508	462947.485883	47.432756
3505.209230	462912.209344	47.437761
3505.430454	462862.869461	47.442765
3505.690215	462811.698739	47.447770
3505.266571	462767.839789	47.452775
3505.282462	462708.907175	47.457780
3505.542270	462671.721183	47.462785
3505.371133	462617.633953	47.467789
3505.579817	462569.967614	47.472794
3505.227857	462521.130109	47.477799
3505.328551	462469.377600	47.482804
3505.314741	462418.505920	47.487809
3505.337760	462388.656508	47.492813
3505.505047	462330.811681	47.497818
3505.230948	462289.865083	47.502823
3505.546828	462232.450640	47.507828
3505.343715	462179.735804	47.512833
3505.158654	462142.168722	47.517837
3505.470912	462088.605560	47.522842
3505.192126	462052.473133	47.527847
3505.586527	462000.314533	47.532852
3505.383632	461960.672575	47.537857
3505.218233	461911.294971	47.542861
3505.730064	461860.686805	47.547866
3505.579457	461810.799695	47.552871
3505.116061	461763.752888	47.557876
3505.642376	461707.871851	47.562881
3505.159493	461660.929472	47.567885
3505.418545	461612.137398	47.572890
3505.100029	461581.280933	47.577895
3505.270412	461528.551252	47.582900
3505.295742	461481.470995	47.587905
3505.057913	461450.955265	47.592909
3505.243187	461391.026975	47.597914
3504.953764	461361.533398	47.602919
3504.939996	461325.962475	47.607924
3505.140937	461270.085082	47.612929
3505.177637	461239.775523	47.617933
3505.252830	461199.527131	47.622938
3505.189759	461158.238097	47.627943
3505.254863	461113.987953	47.632948
3505.300676	461073.794997	47.637953
3504.965162	461036.656894	47.642957
3505.355201	460993.719224	47.647962
3504.817798	460959.098526	47.652967
3505.206861	460908.812936	47.657972
3505.240435	460869.837862	47.662977
3505.011837	460828.931131	47.667981
3505.285914	460793.006047	47.672986
3504.916110	460755.518540	47.677991
3505.229933	460704.485143	47.682996
3505.217838	460676.514140	47.688001
3505.083762	460634.273293	47.693005
3505.244546	460589.549556	47.698010
3505.092298	460556.534700	47.703015
3505.029832	460500.598758	47.708020
3505.380959	460468.562009	47.713025
3504.797722	460428.525827	47.718029
3505.170858	460389.947919	47.723034
3504.753523	460370.863412	47.728039
3505.406002	460332.389724	47.733044
3505.199290	460286.765194	47.738049
3505.177885	460245.112402	47.743053
3505.710203	460197.131690	47.748058
3505.199653	460157.133225	47.753063
3505.415174	460110.219940	47.758068
3505.358010	460069.789143	47.763073
3505.496060	460017.010279	47.768077
3505.648157	459976.948983	47.773082
3505.435722	459940.649328	47.778087
3505.318695	459888.268421	47.783092
3504.996860	459844.791004	47.788097
3505.037979	459810.728329	47.793101
3505.404178	459778.738574	47.798106
3505.017012	459734.866647	47.803111
3504.876289	459697.794128	47.808116
3504.972820	459662.809527	47.813121
3504.869826	459625.781111	47.818125
3504.941142	459587.810647	47.823130
3504.894595	459562.023140	47.828135
3505.032088	459527.740810	47.833140
3504.883167	459487.071101	47.838145
3504.828924	459463.463975	47.843149
3504.740879	459437.784750	47.848154
3504.841957	459396.565379	47.853159
3504.949630	459354.179173	47.858164
3504.558383	459326.625763	47.863169
3504.774478	459297.802986	47.868173
3504.936915	459271.168548	47.873178
3504.664911	459241.111364	47.878183
3504.780220	459201.865663	47.883188
3505.085648	459180.223975	47.888193
3505.099176	459143.833604	47.893197
3505.074270	459105.523892	47.898202
3505.026502	459071.779211	47.903207
3504.870354	459032.579528	47.908212
3505.320775	459000.472785	47.913217
3504.868901	458984.687053	47.918221
3505.144162	458931.273722	47.923226
3504.989735	458889.792849	47.928231
3504.781524	458862.460946	47.933236
3504.963089	458831.362769	47.938241
3504.914063	458796.908309	47.943245
3504.948222	458757.371507	47.948250
3504.800947	458739.709062	47.953255
3504.865166	458697.126158	47.958260
3504.609748	458659.919251	47.963265
3504.794537	458627.857266	47.968269
3505.005713	458603.544948	47.973274
3504.795567	458568.357388	47.978279
3504.734100	458539.023417	47.983284
3504.805921	458516.305909	47.988289
3504.885719	458494.904732	47.993293
3504.899900	458454.255750	47.998298
3504.741972	458416.119475	48.003303
3505.123552	458381.742820	48.008308
3504.924729	458355.878393	48.013313
3504.707944	458323.884490	48.018317
3504.810411	458283.828270	48.023322
3504.963680	458268.141371	48.028327
3504.856437	458244.744582	48.033332
3505.010145	458197.989404	48.038337
3504.596406	458167.904123	48.043341
3505.394003	458143.288389	48.048346
3505.099164	458105.985818	48.053351
3505.045867	458069.503538	48.058356
3504.597750	458049.661819	48.063361
3504.483894	458011.111787	48.068365
3504.876349	457969.738358	48.073370
3504.609252	457947.939684	48.078375
3504.657705	457924.667985	48.083380
3504.873175	457907.905843	48.088385
3504.661357	457875.251497	48.093389
3504.655121	457834.807478	48.098394
3504.647740	457820.617471	48.103399
3504.683973	457788.072679	48.108404
3504.684277	457777.277106	48.113409
3504.618988	457745.560512	48.118413
3504.972358	457693.448314	48.123418
3504.673793	457677.483319	48.128423
3504.811379	457651.560542	48.133428
3504.967105	457632.476926	48.138433
3504.493689	457603.566711	48.143437
3504.674383	457570.844849	48.148442
3504.882638	457559.456131	48.153447
3504.684895	457533.590458	48.158452
3504.620992	457516.774324	48.163457
3504.464411	457475.290890	48.168461
3504.608269	457436.594383	48.173466
3504.755789	457418.829753	48.178471
3504.329672	457398.020633	48.183476
3504.476171	457385.071150	48.188481
3504.695549	457363.695619	48.193485
3504.685050	457322.845823	48.198490
3504.530742	457301.128557	48.203495
3504.560164	457276.288138	48.208500
3504.757509	457252.990240	48.213505
3504.588347	457240.702777	48.218509
3504.686290	457212.404025	48.223514
3504.695759	457178.240906	48.228519
3504.670045	457146.060447	48.233524
3504.968570	457123.758820	48.238529
3504.780685	457108.129268	48.243533
3504.915372	457081.040497	48.248538
3504.656755	457046.720190	48.253543
3504.267504	457016.476946	48.258548
3504.467025	456995.763324	48.263553
3504.416097	456980.211658	48.268557
3504.413299	456959.076376	48.273562
3504.388480	456943.520223	48.278567
3504.272312	456932.338602	48.283572
3504.724232	456908.743411	48.288577
3504.357482	456873.174135	48.293581
3504.615576	456834.000796	48.298586
3504.582235	456829.394109	48.303591
3504.473835	456808.732871	48.308596
3504.774902	456789.116784	48.313601
3504.601851	456774.548841	48.318605
3504.539330	456731.121754	48.323610
3504.465072	456704.169526	48.328615
3504.343110	456683.459790	48.333620
3504.388941	456673.314771	48.338625
3504.370431	456657.351832	48.343629
3504.486433	456642.227578	48.348634
3504.588431	456626.091980	48.353639
3504.565089	456610.586005	48.358644
3504.782448	456578.211077	48.363649
3504.680983	456545.079554	48.368653
3504.735071	456517.192807	48.373658
3504.480179	456501.422167	48.378663
3504.369176	456483.396738	48.383668
3504.433080	456467.115458	48.388673
3504.471143	456456.971656	48.393677
3504.467714	456423.062895	48.398682
3504.191225	456391.633666	48.403687
3504.242437	456377.584698	48.408692
3504.395794	456360.781191	48.413697
3504.152411	456347.187999	48.418701
3504.584799	456325.724313	48.423706
3504.634731	456305.441021	48.428711
3504.242456	456295.471992	48.433716
3504.472826	456279.669007	48.438721
3504.161988	456272.169726	48.443725
3504.519714	456254.317494	48.448730
3504.467164	456247.433033	48.453735
3504.711805	456216.218672	48.458740
3504.853412	456173.414467	48.463745
3504.868285	456156.887873	48.468749
3504.678738	456132.336874	48.473754
3504.267284	456130.176896	48.478759
3504.206133	456101.346193	48.483764
3504.439322	456082.906825	48.488769
3504.181937	456058.164568	48.493773
3504.331776	456021.846648	48.498778
3504.307807	456008.925391	48.503783
3504.202058	455998.957979	48.508788
3504.419467	455976.314125	48.513793
3504.287494	455962.600275	48.518797
3504.425498	455945.849733	48.523802
3504.471421	455933.930252	48.528807
3504.080065	455922.896436	48.533812
3504.178237	455911.576275	48.538817
3503.950745	455900.058274	48.543821
3504.253372	455883.634388	48.548826
3504.218324	455878.672959	48.553831
3504.445141	455856.483558	48.558836
3504.556505	455836.290684	48.563841
3504.630382	455830.398257	48.568845
3504.887310	455801.816946	48.573850
3504.678040	455774.785157	48.578855
3504.978986	455743.256325	48.583860
3505.079194	455733.101550	48.588865
3504.610653	455712.500687	48.593869
3504.730367	455672.791159	48.598874
3504.631774	455652.633952	48.603879
3504.294157	455643.212842	48.608884
3504.349991	455617.909680	48.613889
3504.385815	455601.024235	48.618893
3504.310766	455589.327962	48.623898
3504.275934	455584.366424	48.628903
3504.314033	455566.973675	48.633908
3504.462731	455552.654047	48.638913
3504.084539	455522.001166	48.643917
3504.543172	455503.269334	48.648922
3504.328505	455486.375875	48.653927
3504.485061	455457.861908	48.658932
3504.673469	455442.217505	48.663937
3504.421978	455433.389860	48.668941
3504.622925	455413.130581	48.673946
3504.901132	455403.959033	48.678951
3504.423480	455373.627046	48.683956
3504.257458	455341.873190	48.688961
3503.991727	455333.047934	48.693965
3504.368382	455310.376148	48.698970
3504.350561	455309.061279	48.703975
3504.444899	455300.934869	48.708980
3504.442960	455274.576666	48.713985
3503.749788	455267.750568	48.718989
3504.153735	455244.263016	48.723994
3504.064836	455240.476487	48.728999
3504.288839	455229.742737	48.734004
3504.492334	455217.390413	48.739009
3504.357317	455214.828307	48.744013
3504.664904	455183.044025	48.749018
3504.501049	455178.408557	48.754023
3504.403835	455167.932381	48.759028
3504.752304	455152.006976	48.764033
3504.435771	455119.467436	48.769037
3504.274079	455094.555595	48.774042
3504.032722	455081.163966	48.779047
3504.003983	455066.316703	48.784052
3503.982103	455041.076783	48.789057
3503.910316	455040.784914	48.794061
3504.406541	455044.856789	48.799066
3503.794976	455020.629954	48.804071
3504.071398	455032.140128	48.809076
3504.290850	455028.300909	48.814081
3503.970274	455029.673605	48.819085
3504.307016	455012.229389	48.824090
3503.883682	455009.767176	48.829095
3503.963570	454993.786127	48.834100
3504.207708	454976.408383	48.839105
3503.883403	454973.625115	48.844109
3504.226035	454959.677479	48.849114
3504.040600	454949.165563	48.854119
3503.861236	454945.799949	48.859124
3504.191374	454927.900575	48.864129
3504.106819	454915.242420	48.869133
3504.073820	454905.870334	48.874138
3503.899381	454893.734418	48.879143
3504.368820	454881.184410	48.884148
3504.197850	454872.292082	48.889153
3504.350856	454875.307403	48.894157
3504.674535	454854.773160	48.899162
3504.500090	454846.895226	48.904167
3504.321887	454827.713916	48.909172
3504.828754	454815.664384	48.914177
3504.585172	454779.816949	48.919181
3504.378038	454750.857184	48.924186
3504.419859	454742.536755	48.929191
3504.384740	454735.395352	48.934196
3504.422806	454715.112500	48.939201
3504.372697	454708.125719	48.944205
3504.361284	454700.371964	48.949210
3504.628715	454691.506082	48.954215
3504.432153	454682.161822	48.959220
3504.319829	454643.909257	48.964225
3504.241118	454627.955002	48.969229
3503.938044	454605.753336	48.974234
3503.805446	454594.623921	48.979239
3503.901144	454608.953211	48.984244
3504.245660	454596.728506	48.989249
3503.959265	454600.579264	48.994253
3503.928860	454586.948526	48.999258
3504.303338	454580.649572	49.004263
3503.729565	454570.102387	49.009268
3503.837801	454560.858101	49.014273
3503.777660	454555.343029	49.019277
3503.999415	454536.245227	49.024282
3504.112063	454534.046276	49.029287
3504.053481	454512.765898	49.034292
3504.158595	454510.213392	49.039297
3504.129351	454503.324361	49.044301
3504.150013	454484.564996	49.049306
3504.272325	454478.511834	49.054311
3504.040230	454468.413170	49.059316
3504.178618	454454.347989	49.064321
3504.097277	454455.781257	49.069325
3503.689706	454441.859981	49.074330
3503.975231	454461.479581	49.079335
3504.176088	454464.892325	49.084340
3504.414350	454444.321564	49.089345
3504.168681	454446.289807	49.094349
3504.226996	454432.593125	49.099354
3504.237630	454433.605156	49.104359
3504.163444	454421.908065	49.109364
3503.912544	454414.803393	49.114369
3504.137553	454408.428525	49.119373
3504.143584	454381.763657	49.124378
3504.234748	454374.195030	49.129383
3503.741936	454368.145484	49.134388
3503.968697	454353.558227	49.139393
3503.637558	454356.554909	49.144397
3503.764142	454345.989405	49.149402
3504.036364	454335.094877	49.154407
3503.907422	454329.540800	49.159412
3503.888867	454316.262701	49.164417
3503.680131	454327.653346	49.169421
3503.986762	454332.619501	49.174426
3504.177387	454334.209106	49.179431
3503.644689	454328.115667	49.184436
3503.915799	454310.732751	49.189441
3504.180651	454309.369552	49.194445
3503.971432	454298.607902	49.199450
3504.136225	454294.879263	49.204455
3503.781553	454287.437422	49.209460
3503.933400	454270.632449	49.214465
3504.059154	454266.555627	49.219469
3504.080705	454255.602474	49.224474
3504.209114	454239.004246	49.229479
3504.016381	454237.262944	49.234484
3504.008284	454249.329064	49.239489
3503.874526	454256.955730	49.244493
3503.864785	454253.206193	49.249498
3503.983760	454247.305609	49.254503
3503.884508	454236.322381	49.259508
3503.827400	454225.230567	49.264513
3503.817278	454227.614841	49.269517
3503.615537	454215.331106	49.274522
3504.194328	454205.448699	49.279527
3503.987851	454210.147651	49.284532
3504.057868	454209.121866	49.289537
3503.711532	454207.356097	49.294541
3504.176693	454199.977007	49.299546
3504.114056	454195.628185	49.304551
3503.892615	454198.808928	49.309556
3504.100237	454181.183283	49.314561
3504.317170	454176.583951	49.319565
3504.091054	454168.866654	49.324570
3504.073982	454160.860199	49.329575
3503.847366	454147.364055	49.334580
3504.058008	454142.816483	49.339585
3504.044995	454142.717334	49.344589
3503.919832	454128.494161	49.349594
3504.153889	454121.813505	49.354599
3503.839877	454115.530584	49.359604
3503.822981	454108.892774	49.364609
3503.838279	454116.240579	49.369613
3503.765928	454128.571203	49.374618
3504.231847	454128.542354	49.379623
3503.858553	454124.145176	49.384628
3503.907178	454106.495923	49.389633
3504.126649	454105.241844	49.394637
3503.876461	454098.694557	49.399642
3504.124548	454087.753327	49.404647
3504.171611	454086.528685	49.409652
3504.409105	454079.543274	49.414657
3503.932611	454082.767584	49.419661
3504.079000	454065.405757	49.424666
3504.268277	454048.442133	49.429671
3503.813741	454052.068239	49.434676
3504.018046	454037.180436	49.439681
3503.751037	454038.138509	49.444685
3503.988578	454028.466363	49.449690
3504.039531	454032.462395	49.454695
3503.596499	454054.944188	49.459700
3503.976145	454041.141685	49.464705
3503.903092	454047.997674	49.469709
3503.625338	454030.911010	49.474714
3504.111756	454021.399136	49.479719
3503.838885	454016.528554	49.484724
3504.243086	454004.749541	49.489729
3503.582814	453998.424321	49.494733
3504.164467	454009.376028	49.499738
3504.140726	454022.915040	49.504743
3504.120210	454026.010809	49.509748
3504.370675	454014.410129	49.514753
3504.120325	454022.817180	49.519757
3504.275751	453997.647082	49.524762
3504.357091	453983.388548	49.529767
3503.952135	453958.314086	49.534772
3504.477297	453948.288635	49.539777
3504.305617	453938.838399	49.544781
3504.098241	453921.688934	49.549786
3503.915726	453914.927262	49.554791
3503.776825	453918.905041	49.559796
3503.899580	453929.833761	49.564801
3504.035921	453939.137984	49.569805
3503.998564	453928.194715	49.574810
3504.139224	453920.820241	49.579815
3503.689885	453921.150444	49.584820
3503.609327	453909.302069	49.589825
3503.568682	453908.244471	49.594829
3504.053490	453901.825087	49.599834
3503.667515	453910.103263	49.604839
3503.720834	453921.956316	49.609844
3503.899207	453914.321936	49.614849
3503.717576	453913.085640	49.619853
3503.687712	453900.924447	49.624858
3503.511941	453893.097063	49.629863
3503.741236	453924.031312	49.634868
3503.926645	453926.331541	49.639873
3503.786350	453923.922251	49.644877
3503.890479	453922.535777	49.649882
3503.874533	453911.842308	49.654887
3503.779029	453904.660232	49.659892
3503.901575	453888.772422	49.664897
3503.551460	453902.215162	49.669901
3503.782238	453922.402251	49.674906
3503.836387	453918.286893	49.679911
3503.789959	453921.741953	49.684916
3503.728134	453920.738665	49.689921
3503.774375	453911.606058	49.694925
3503.802055	453903.135624	49.699930
3503.771808	453916.726510	49.704935
3503.832337	453939.882840	49.709940
3504.104132	453931.269350	49.714945
3503.895778	453923.447542	49.719949
3503.642922	453916.038873	49.724954
3504.036836	453912.980744	49.729959
3503.477734	453912.569294	49.734964
3503.891568	453902.866988	49.739969
3503.754556	453923.268954	49.744973
3503.849118	453926.243703	49.749978
3504.079972	453919.512836	49.754983
3503.875746	453909.358443	49.759988
3504.240065	453906.356059	49.764993
3503.752737	453899.190191	49.769997
3503.827369	453901.306567	49.775002
3503.937371	453887.752774	49.780007
3503.827758	453886.909723	49.785012
3504.150531	453899.781334	49.790017
3503.664036	453917.505559	49.795021
3503.877164	453907.229210	49.800026
3504.059102	453900.405303	49.805031
3503.543374	453896.387246	49.810036
3503.947916	453882.783158	49.815041
3504.089189	453881.998655	49.820045
3503.643630	453883.139300	49.825050
3503.646842	453884.608863	49.830055
3503.739064	453897.012912	49.835060
3503.909671	453901.799626	49.840065
3503.620930	453906.918238	49.845069
3503.954183	453902.603141	49.850074
3504.014239	453898.689543	49.855079
3503.786679	453894.470203	49.860084
3504.166805	453874.381576	49.865089
3504.051891	453881.244769	49.870093
3503.823056	453879.610987	49.875098
3503.815129	453890.764814	49.880103
3503.856653	453907.739881	49.885108
3503.854575	453895.320475	49.890113
3503.944679	453893.936394	49.895117
3504.083209	453881.290199	49.900122
3503.855713	453880.568663	49.905127
3503.744432	453875.062139	49.910132
3504.063164	453870.191892	49.915137
3503.972889	453859.663167	49.920141
3504.205660	453857.545020	49.925146
3504.310375	453852.001609	49.930151
3504.385649	453848.896492	49.935156
3504.645021	453847.990436	49.940161
3504.257750	453837.309638	49.945165
3504.277587	453827.319719	49.950170
3503.997320	453814.694299	49.955175
3503.618230	453817.445780	49.960180
3503.859882	453808.735999	49.965185
3503.827650	453811.276176	49.970189
3503.756662	453816.965947	49.975194
3503.763552	453825.937473	49.980199
3503.950660	453833.509509	49.985204
3503.736747	453822.342864	49.990209
3503.684671	453823.568406	49.995213
3503.830978	453815.483226	50.000218
3503.985847	453811.097183	50.005223
3503.742964	453835.978313	50.010228
3503.922311	453832.754037	50.015233
3504.092754	453837.135250	50.020237
3504.012354	453820.470950	50.025242
3503.990660	453817.179613	50.030247
3504.194549	453821.555118	50.035252
3503.904132	453807.309246	50.040257
3503.787293	453810.877733	50.045261
3503.806767	453803.726682	50.050266
3504.048954	453794.205712	50.055271
3503.771429	453787.561607	50.060276
3504.144642	453800.830213	50.065281
3504.264262	453814.547657	50.070285
3504.073483	453816.709359	50.075290
3504.311448	453814.894480	50.080295
3503.913508	453813.188181	50.085300
3504.055106	453797.854672	50.090305
3504.022255	453795.122862	50.095309
3503.954231	453792.397057	50.100314
3503.985976	453781.036364	50.105319
3504.045553	453776.869358	50.110324
3504.095925	453771.284512	50.115329
3504.248989	453766.036982	50.120333
3503.738349	453773.271940	50.125338
3503.912604	453749.973974	50.130343
3503.928747	453757.676616	50.135348
3503.644689	453743.277534	50.140353
3503.433115	453745.240021	50.145357
3503.477794	453764.952107	50.150362
3503.694628	453775.864846	50.155367
3503.932517	453779.068610	50.160372
3503.878648	453764.376771	50.165377
3504.095489	453755.012192	50.170381
3503.855182	453757.030277	50.175386
3504.245405	453771.005705	50.180391
3503.637869	453789.713880	50.185396
3503.959071	453775.870485	50.190401
3503.705855	453780.121276	50.195405
3503.907111	453777.045330	50.200410
3504.205527	453765.689789	50.205415
3503.912306	453770.403652	50.210420
3503.996061	453757.716041	50.215425
3503.734042	453759.940607	50.220429
3503.328956	453756.968190	50.225434
3503.724642	453776.721718	50.230439
3503.607883	453784.092191	50.235444
3503.847082	453781.060460	50.240449
3503.841625	453789.780644	50.245453
3503.530148	453784.561745	50.250458
3503.944527	453791.030433	50.255463
3503.625808	453805.937979	50.260468
3503.765843	453807.029332	50.265473
3503.525941	453807.780014	50.270477
3503.499397	453798.761171	50.275482
3503.614861	453813.543882	50.280487
3503.512236	453822.382030	50.285492
3503.661693	453818.351765	50.290497
3503.608524	453822.213538	50.295501
3503.477293	453822.742891	50.300506
3503.461798	453840.133294	50.305511
3503.763386	453850.778056	50.310516
3503.476844	453847.988184	50.315521
3503.779447	453848.595539	50.320525
3503.632436	453860.939072	50.325530
3503.466105	453873.133817	50.330535
3503.297631	453876.153486	50.335540
3503.461469	453877.139386	50.340545
3503.528431	453892.183787	50.345549
3503.496918	453912.922601	50.350554
3503.876820	453900.691440	50.355559
3503.526087	453905.263014	50.360564
3503.612398	453918.124296	50.365569
3503.630723	453930.693020	50.370573
3503.274143	453939.219630	50.375578
3503.484739	453933.759548	50.380583
3503.198398	453937.204877	50.385588
3503.594184	453947.326575	50.390593
3504.076749	453950.843384	50.395597
3503.851035	453958.536555	50.400602
3503.799351	453954.591354	50.405607
3504.158804	453952.096736	50.410612
3503.818091	453954.233332	50.415617
3503.593016	453973.382965	50.420621
3503.539576	453978.309303	50.425626
3503.607400	453974.394392	50.430631
3503.549821	453983.630321	50.435636
3503.575470	453976.275505	50.440641
3504.029941	453991.304360	50.445645
3503.743120	454006.916012	50.450650
3503.741474	454001.035954	50.455655
3503.473970	454001.436492	50.460660
3503.718470	453997.237956	50.465665
3503.913795	454010.993034	50.470669
3503.837046	454029.661053	50.475674
3504.200790	454031.778742	50.480679
3503.570779	454031.582173	50.485684
3504.213436	454022.347778	50.490689
3503.854528	454015.768336	50.495693
3503.732840	454026.029046	50.500698
3503.707415	454015.641405	50.505703
3503.740976	454012.644821	50.510708
3503.734672	454024.609381	50.515713
3503.568931	454025.448778	50.520717
3503.437683	454029.273151	50.525722
3503.895548	454023.466716	50.530727
3503.224982	454030.779584	50.535732
3503.547419	454009.180160	50.540737
3503.614437	453991.122124	50.545741
3503.166981	453964.736916	50.550746
3503.384648	453905.084942	50.555751
3503.383420	453860.323243	50.560756
3503.675861	453781.851010	50.565761
3503.845776	453699.749469	50.570765
3503.648423	453603.668163	50.575770
3504.053001	453490.957399	50.580775
3503.957000	453378.939822	50.585780
3504.067267	453235.202311	50.590785
3503.988968	453086.882753	50.595789
3503.933412	452928.621954	50.600794
3504.069915	452748.730746	50.605799
3503.974035	452579.321071	50.610804
3504.104081	452368.350845	50.615809
3503.617176	452164.733514	50.620813
3503.479451	451955.427106	50.625818
3503.668145	451725.225851	50.630823
3503.359467	451495.766051	50.635828
3503.491211	451238.090308	50.640833
3503.553526	450980.676726	50.645837
3503.359082	450714.126964	50.650842
3503.659453	450413.113708	50.655847
3503.146992	450118.775490	50.660852
3503.294117	449811.644765	50.665857
3503.391522	449503.351839	50.670861
3503.301012	449169.227180	50.675866
3503.646713	448809.010875	50.680871
3503.490422	448461.449271	50.685876
3503.444836	448084.757163	50.690881
3503.375453	447695.740348	50.695885
3503.408306	447296.962800	50.700890
3503.438733	446881.596008	50.705895
3503.400279	446457.814837	50.710900
3503.447991	446009.719456	50.715905
3503.253299	445561.148937	50.720909
3502.957800	445082.259119	50.725914
3502.944666	444595.601664	50.730919
3502.967592	444108.572035	50.735924
3502.887016	443598.573957	50.740929
3502.718659	443071.537275	50.745933
3502.713761	442530.562540	50.750938
3502.947879	441971.983901	50.755943
3502.742672	441409.255997	50.760948
3502.776025	440821.770221	50.765953
3502.880220	440223.705726	50.770957
3502.631117	439604.582908	50.775962
3502.941837	438960.997512	50.780967
3502.654813	438304.863771	50.785972
3502.670007	437635.063070	50.790977
3502.843863	436946.494731	50.795981
3502.394485	436240.203845	50.800986
3502.498513	435517.205581	50.805991
3502.243264	434767.506692	50.810996
3502.507335	434016.781098	50.816001
3502.220769	433224.973624	50.821005
3502.366525	432431.238248	50.826010
3502.353641	431604.924392	50.831015
3502.236252	430769.921200	50.836020
3502.528939	429917.005263	50.841025
3502.470781	429026.258246	50.846029
3502.490917	428141.097639	50.851034
3502.185415	427217.183119	50.856039
3501.910194	426285.309505	50.861044
3501.707574	425316.333489	50.866049
3501.728308	424339.412389	50.871053
3501.182549	423348.081208	50.876058
3501.643702	422324.911273	50.881063
3501.302721	421299.195665	50.886068
3501.314327	420250.480320	50.891073
3501.290034	419169.867822	50.896077
3500.875182	418094.301796	50.901082
3500.655523	416968.794738	50.906087
3500.875574	415847.453273	50.911092
3500.606630	414688.441696	50.916097
3500.829664	413522.057285	50.921101
3500.238210	412336.588102	50.926106
3500.589414	411117.866994	50.931111
3499.698669	409894.958931	50.936116
3499.733365	408644.611914	50.941121
3499.965878	407388.382040	50.946125
3499.310845	406093.055475	50.951130
3499.246263	404797.693326	50.956135
3499.192660	403475.571866	50.961140
3498.675979	402133.424096	50.966145
3498.793888	400780.891338	50.971149
3498.240384	399411.870014	50.976154
3498.733135	398020.882293	50.981159
3498.327862	396603.125459	50.986164
3498.158831	395179.110268	50.991169
3498.016476	393730.374243	50.996173
3497.569705	392270.616582	51.001178
3497.790983	390773.928080	51.006183
3497.539628	389271.070970	51.011188
3497.466277	387750.827958	51.016193
3497.159705	386204.194159	51.021197
3496.607854	384661.211487	51.026202
3496.387677	383088.612117	51.031207
3495.825149	381512.816888	51.036212
3495.782592	379904.140216	51.041217
3495.847855	378283.748900	51.046221
3495.739860	376662.469703	51.051226
3495.482730	375000.815366	51.056231
3495.283152	373339.884507	51.061236
3494.928495	371655.762608	51.066241
3494.910575	369943.150779	51.071245
3494.530354	368223.932994	51.076250
3494.427947	366498.178269	51.081255
3494.173399	364756.550675	51.086260
3493.845718	362987.184109	51.091265
3493.884210	361210.399120	51.096269
3493.337958	359424.857784	51.101274
3493.470450	357596.844929	51.106279
3492.774475	355765.329465	51.111284
3492.493902	353915.193000	51.116289
3492.229684	352056.958481	51.121293
3492.115649	350193.071331	51.126298
3492.089944	348303.850948	51.131303
3491.384662	346403.216962	51.136308
3491.054052	344490.429810	51.141313
3490.958230	342560.450017	51.146317
3490.775950	340636.004586	51.151322
3490.431754	338670.006203	51.156327
3489.959797	336700.898049	51.161332
3489.716603	334728.620754	51.166337
3489.527418	332724.523469	51.171341
3488.954646	330733.091299	51.176346
3488.943718	328712.501344	51.181351
3488.683045	326673.657609	51.186356
3488.239493	324630.599258	51.191361
3487.629130	322580.550654	51.196365
3487.540206	320512.220752	51.201370
3487.296442	318415.492008	51.206375
3486.925297	316330.123117	51.211380
3486.788866	314233.194437	51.216385
3486.897253	312108.081038	51.221389
3485.799353	309970.586197	51.226394
3485.350621	307819.248684	51.231399
3484.879522	305669.155335	51.236404
3484.747850	303503.697067	51.241409
3484.296322	301335.107650	51.246413
3483.806343	299152.927130	51.251418
3483.709170	296948.655177	51.256423
3483.011391	294746.831257	51.261428
3482.993657	292528.090415	51.266433
3482.869778	290296.388255	51.271437
3482.058753	288074.464420	51.276442
3481.867066	285813.892823	51.281447
3481.113670	283560.256259	51.286452
3480.966064	281292.399742	51.291457
3480.625001	279015.173323	51.296461
3479.815512	276716.606095	51.301466
3479.404336	274415.652626	51.306471
3479.155700	272119.665229	51.311476
3478.249339	269795.169817	51.316481
3478.118491	267474.955739	51.321485
3477.665728	265152.846561	51.326490
3477.390173	262814.778113	51.331495
3476.898613	260485.524550	51.336500
3476.054855	258114.048610	51.341505
3475.771192	255755.030540	51.346509
3475.223153	253385.361933	51.351514
3474.657894	251005.233080	51.356519
3474.248652	248634.380932	51.361524
3473.511547	246245.869874	51.366529
3473.221558	243833.866406	51.371533
3472.779120	241443.503325	51.376538
3472.234845	239034.358293	51.381543
3471.324529	236618.067851	51.386548
3471.045906	234192.555298	51.391553
3470.291722	231767.105022	51.396557
3469.562191	229352.356229	51.401562
3469.261712	226912.693012	51.406567
3468.954142	224473.023037	51.411572
3468.232764	222021.858435	51.416577
3467.751009	219575.745331	51.421581
3466.894926	217123.002288	51.426586
3466.786092	214661.252038	51.431591
3465.966445	212201.391044	51.436596
3465.155870	209719.009705	51.441601
3464.710254	207248.361072	51.446605
3464.117860	204773.164510	51.451610
3463.724431	202287.191286	51.456615
3462.832045	199811.364740	51.461620
3461.714974	197321.367199	51.466625
3461.576684	194821.211451	51.471629
3460.707964	192333.824173	51.476634
3460.026495	189838.382016	51.481639
3459.225773	187334.267587	51.486644
3458.466208	184844.250892	51.491649
3458.292965	182345.614782	51.496653
3457.357513	179858.979922	51.501658
3456.720437	177349.048102	51.506663
3456.113132	174845.315115	51.511668
3454.999379	172331.831683	51.516673
3454.177289	169831.990647	51.521677
3453.706156	167339.524491	51.526682
3452.888095	164835.295389	51.531687
3452.244147	162335.044244	51.536692
3451.055014	159836.442199	51.541697
3450.628863	157336.051557	51.546701
3449.640505	154852.009771	51.551706
3448.968550	152343.103684	51.556711
3448.060604	149863.023125	51.561716
3447.344782	147398.138419	51.566721
3447.014354	144821.460928	51.571725
3445.949423	142330.590872	51.576730
3445.356707	139840.258778	51.581735
3444.221644	137367.929942	51.586740
3443.576601	134878.612317	51.591745
3443.048741	132397.543163	51.596749
3442.037720	129925.462412	51.601754
3440.939772	127446.723901	51.606759
3440.185618	124979.583133	51.611764
3438.480501	122525.786964	51.616769
3438.236502	120063.045738	51.621773
3436.873207	117617.684186	51.626778
3436.307751	115170.370582	51.631783
3435.070932	112737.186545	51.636788
3433.986806	110302.839286	51.641793
3433.185738	107888.176028	51.646797
3431.786302	105481.218527	51.651802
3431.161335	103073.366176	51.656807
3430.067177	100670.421446	51.661812
3428.836289	98297.459648	51.666817
3428.045116	95916.346452	51.671821
3426.901222	93559.214843	51.676826
3425.969476	91202.200034	51.681831
3425.004629	88864.376257	51.686836
3424.135669	86520.030168	51.691841
3422.698060	84183.833337	51.696845
3421.491791	81875.130165	51.701850
3420.543581	79564.519214	51.706855
3419.621895	77277.735167	51.711860
3418.284702	74994.912117	51.716865
3417.232921	72723.230336	51.721869
3415.852608	70461.798833	51.726874
3414.699412	68219.866763	51.731879
3413.254944	65989.836902	51.736884
3411.907940	63792.012561	51.741889
3410.780515	61582.339470	51.746893
3409.014258	59407.336669	51.751898
3407.850189	57254.929086	51.756903
3406.859199	55120.642894	51.761908
3405.053516	52996.110650	51.766913
3403.781250	50889.019048	51.771917
3402.379211	48810.232245	51.776922
3401.177564	46743.415223	51.781927
3399.911161	44705.913982	51.786932
3398.162125	42677.959724	51.791937
3396.837375	40672.852520	51.796941
3394.928831	38698.117946	51.801946
3393.804784	36745.004829	51.806951
3392.076177	34823.725775	51.811956
3390.309358	32924.519317	51.816961
3388.132141	31040.341402	51.821965
3385.816001	29190.233485	51.826970
3383.894480	27389.277983	51.831975
3381.487707	25639.151894	51.836980
3376.467571	23983.444493	51.841985
3370.774673	22399.657472	51.846989
3365.259927	20923.069445	51.851994
3360.172682	19520.317838	51.856999
3355.571114	18201.052043	51.862004
3350.698531	16990.261915	51.867009
3346.362776	15849.639202	51.872013
3341.465283	14820.569967	51.877018
3337.721116	13878.626082	51.882023
3334.172129	13022.052467	51.887028
3330.073512	12246.271923	51.892033
3326.381065	11554.824580	51.897037
3322.655093	10952.786684	51.902042
3319.519738	10423.964444	51.907047
3316.425853	9954.699590	51.912052
3313.779130	9571.128936	51.917057
3311.459426	9235.125443	51.922061
3309.404341	8961.641618	51.927066
3307.783349	8728.358008	51.932071
3306.018312	8523.553559	51.937076
3304.794242	8379.941701	51.942081
3303.703769	8252.088104	51.947085
3302.838956	8152.134894	51.952090
3302.075802	8070.995757	51.957095
3301.181328	8015.670346	51.962100
3300.635862	7966.680093	51.967105
3300.398649	7931.965092	51.972109
3299.687580	7927.473101	51.977114
3299.222455	7913.613417	51.982119
3299.060986	7909.576483	51.987124
3298.476021	7917.182304	51.992129
3298.557910	7918.127199	51.997133
3298.573695	7933.467228	52.002138
3298.347797	7936.395871	52.007143
3298.011806	7942.433983	52.012148
3297.693573	7943.740264	52.017153
3298.199636	7947.664658	52.022157
3297.937652	7951.465138	52.027162
3297.641124	7937.167494	52.032167
3297.680704	7929.172265	52.037172
3297.109333	7914.229689	52.042177
3297.496174	7899.222166	52.047181
3297.316102	7888.155662	52.052186
3297.175190	7854.931395	52.057191
3297.223405	7816.569373	52.062196
3297.055623	7775.468066	52.067201
3296.509536	7725.807292	52.072205
3296.238166	7686.113227	52.077210
3295.808186	7637.605001	52.082215
3295.352876	7587.692986	52.087220
3294.268013	7535.884889	52.092225
3293.981263	7476.455476	52.097229
3293.597323	7440.697971	52.102234
3293.227104	7379.259658	52.107239
3292.965027	7321.255382	52.112244
3292.459387	7265.112647	52.117249
3291.957567	7196.663455	52.122253
3291.401036	7142.307700	52.127258
3290.550118	7080.741767	52.132263
3290.587175	7015.588750	52.137268
3290.146425	6951.463797	52.142273
3289.813731	6892.854718	52.147277
3288.664553	6835.503677	52.152282
3288.360549	6754.623664	52.157287
3287.654129	6681.202797	52.162292
3287.230588	6610.252547	52.167297
3286.777600	6531.423313	52.172301
3286.239196	6472.779040	52.177306
3285.925900	6392.944146	52.182311
3285.620028	6320.773046	52.187316
3284.666848	6233.220902	52.192321
3283.924619	6155.712862	52.197325
3283.324263	6080.412013	52.202330
3282.946878	5982.260746	52.207335
3282.108987	5914.386983	52.212340
3281.517823	5844.733138	52.217345
3280.786335	5754.556971	52.222349
3280.208584	5680.237366	52.227354
3279.564450	5605.747809	52.232359
3279.080556	5522.585309	52.237364
3278.321122	5454.877785	52.242369
3277.905021	5353.128752	52.247373
3277.045273	5291.346933	52.252378
3276.675541	5208.033896	52.257383
3276.577482	5121.644782	52.262388
3275.619668	5046.734440	52.267393
3274.422881	4966.447946	52.272397
3273.625481	4886.846997	52.277402
3273.281309	4813.726607	52.282407
3272.807225	4728.771603	52.287412
3272.257862	4655.170539	52.292417
3271.687915	4564.506011	52.297421
3270.821390	4491.845114	52.302426
3270.222636	4416.142795	52.307431
3269.526290	4332.135210	52.312436
3268.514330	4261.396992	52.317441
3268.335744	4180.633346	52.322445
3267.566532	4104.662350	52.327450
3266.429022	4025.610244	52.332455
3265.999122	3954.597867	52.337460
3265.293812	3876.698202	52.342465
3264.890773	3806.723438	52.347469
3264.004498	3736.975250	52.352474
3263.540082	3660.886401	52.357479
3262.818674	3588.483593	52.362484
3262.224817	3519.423922	52.367489
3261.970530	3433.389673	52.372493
3260.956065	3370.751857	52.377498
3260.074835	3292.738249	52.382503
3259.716009	3219.042600	52.387508
3258.715127	3148.230872	52.392513
3258.204057	3076.994674	52.397517
3257.705325	2999.455679	52.402522
3257.181664	2932.303729	52.407527
3256.024657	2859.095118	52.412532
3255.824876	2792.535898	52.417537
3255.196732	2713.845503	52.422541
3254.558851	2638.173368	52.427546
3253.843408	2562.331663	52.432551
3253.003784	2495.338196	52.437556
3252.261787	2418.987705	52.442561
3251.686275	2345.986122	52.447565
3250.988491	2275.681598	52.452570
3250.507967	2212.316041	52.457575
3249.854972	2134.468138	52.462580
3249.022420	2082.543133	52.467585
3248.583399	2003.901349	52.472589
3247.826354	1938.641840	52.477594
3246.907962	1862.591839	52.482599
3246.444673	1795.951567	52.487604
3245.538047	1741.205107	52.492609
3245.192155	1669.150409	52.497613
3244.500124	1609.726868	52.502618
3243.680246	1538.636834	52.507623
3243.169930	1465.674385	52.512628
3242.232489	1412.329821	52.517633
3241.848212	1345.307282	52.522637
3241.116289	1291.905910	52.527642
3240.183287	1224.026268	52.532647
3239.673388	1163.161263	52.537652
3238.927762	1104.130126	52.542657
3238.633481	1040.286276	52.547661
3237.739173	983.234619	52.552666
3237.132393	913.999890	52.557671
3236.084662	857.642421	52.562676
3235.122084	819.945217	52.567681
3234.469539	754.216459	52.572685
3234.084154	708.785387	52.577690
3232.458442	663.355949	52.582695
3232.022708	623.153002	52.587700
3230.791140	588.510631	52.592705
3230.344129	542.907806	52.597709
3229.353176	520.214273	52.602714
3228.839561	480.347500	52.607719
3228.359692	440.857168	52.612724
3227.367357	410.494315	52.617729
3226.940887	371.920689	52.622733
3225.996016	347.886518	52.627738
3225.430911	326.722740	52.632743
3224.771286	283.834865	52.637748
3223.948168	263.751029	52.642753
3223.474735	240.931202	52.647757
3222.686303	226.647980	52.652762
3221.835068	198.328641	52.657767
3220.964048	174.567118	52.662772
3219.567128	170.217850	52.667777
3218.961052	159.334128	52.672781
3217.999472	160.023806	52.677786
3217.318880	159.373926	52.682791
3216.615324	157.014453	52.687796
3215.876919	165.412951	52.692801
3215.286720	157.543828	52.697805
3214.748786	158.820720	52.702810
3214.051972	163.535214	52.707815
3213.893109	157.618148	52.712820
3213.240545	163.740185	52.717825
3212.463143	158.232734	52.722829
3211.527546	158.388643	52.727834
3211.166199	170.154892	52.732839
3210.009369	163.283345	52.737844
3209.514699	171.063112	52.742849
3209.396774	169.289229	52.747853
3208.442472	169.453071	52.752858
3207.765603	160.603247	52.757863
3206.952601	160.501770	52.762868
3206.550823	168.026854	52.767873
3206.134112	157.762087	52.772877
3205.716818	164.027083	52.777882
3204.588246	160.018416	52.782887
3203.762798	153.697746	52.787892
3203.207631	161.250218	52.792897
3203.001119	149.643782	52.797901
3202.587394	164.527068	52.802906
3201.301720	163.257818	52.807911
3200.546674	159.147047	52.812916
3200.115862	165.705269	52.817921
3199.916264	158.294799	52.822925
3199.097074	162.728629	52.827930
3197.834964	163.271896	52.832935
3197.722045	160.768490	52.837940
3196.868120	161.787930	52.842945
3196.511360	153.606961	52.847949
3195.865031	162.753133	52.852954
3194.868566	160.410152	52.857959
3194.413062	147.688915	52.862964
3193.320848	158.434914	52.867969
3193.132788	160.604514	52.872973
3192.310897	161.025994	52.877978
3192.157791	161.079402	52.882983
3191.582826	158.589017	52.887988
3190.364301	158.023941	52.892993
3189.358956	159.073198	52.897997
3189.316350	162.155428	52.903002
3188.014486	153.608178	52.908007
3188.197634	154.560170	52.913012
3187.295417	156.784679	52.918017
3186.210362	158.373729	52.923021
3186.091487	157.083158	52.928026
3185.079659	155.930939	52.933031
3184.857334	150.713916	52.938036
3183.998787	160.122918	52.943041
3183.780776	154.564507	52.948045
3182.858313	165.007963	52.953050
3181.882529	153.590193	52.958055
3181.481294	155.805292	52.963060
3180.991635	166.202041	52.968065
3179.736256	156.884234	52.973069
3179.669337	152.322751	52.978074
3178.967727	169.704515	52.983079
3178.007506	146.792354	52.988084
3176.889115	155.949308	52.993089
3176.824621	156.677563	52.998093
3175.985672	158.767713	53.003098
3175.285933	164.371639	53.008103
3175.509808	150.851844	53.013108
3174.560735	156.863095	53.018113
3174.133733	148.281247	53.023117
3173.168628	152.358303	53.028122
3171.633748	151.104402	53.033127
3171.243409	148.084725	53.038132
3170.488021	161.448650	53.043137
3170.309923	152.305602	53.048141
3170.133378	151.562901	53.053146
3169.132194	153.468800	53.058151
3168.673372	147.820881	53.063156
3166.986697	148.827473	53.068161
3167.136345	146.901697	53.073165
3166.654491	156.116473	53.078170
3165.334089	156.982726	53.083175
3165.098837	146.131193	53.088180
3164.548694	154.055821	53.093185
3164.406869	153.504158	53.098189
3163.654068	157.612443	53.103194
3162.542427	153.077879	53.108199
3161.903734	150.658386	53.113204
3160.751529	155.951202	53.118209
3159.957000	162.530118	53.123213
3160.031592	152.446285	53.128218
3159.076437	165.665532	53.133223
3158.598731	153.308478	53.138228
3157.698572	156.528144	53.143233
3157.447199	148.448385	53.148237
3157.102302	155.477045	53.153242
3156.460953	156.293200	53.158247
3155.736516	156.084232	53.163252
3154.697126	154.565287	53.168257
3153.633772	148.633033	53.173261
3152.844185	151.676310	53.178266
3151.765789	156.331662	53.183271
3151.819945	142.666799	53.188276
3151.385864	154.987422	53.193281
3150.611419	155.630927	53.198285
3150.553758	152.698882	53.203290
3149.937950	153.134498	53.208295
3149.118442	141.743729	53.213300
3147.673980	154.965649	53.218305
3147.577497	147.316130	53.223309
3146.907580	144.870001	53.228314
3146.016442	157.473581	53.233319
3145.273458	153.491416	53.238324
3144.455411	152.460829	53.243329
3144.393901	156.014039	53.248333
3143.967990	152.559530	53.253338
3143.581233	150.874215	53.258343
3142.789635	146.926015	53.263348
3141.507211	156.958480	53.268353
3140.698010	152.649742	53.273357
3140.000755	151.418521	53.278362
3138.934935	154.556364	53.283367
3138.209051	135.618980	53.288372
3138.282770	140.694442	53.293377
3138.013840	145.894764	53.298381
3137.394658	152.479638	53.303386
3136.166938	145.008007	53.308391
3135.319192	149.771974	53.313396
3134.571356	151.410781	53.318401
3134.216098	149.108651	53.323405
3134.181466	140.289647	53.328410
3133.014750	148.588034	53.333415
3132.770078	149.301680	53.338420
3131.986969	142.819457	53.343425
3131.284599	141.728451	53.348429
3130.564198	137.985587	53.353434
3129.770341	152.200794	53.358439
3129.419884	146.873041	53.363444
3128.340693	149.991854	53.368449
3127.168847	147.544647	53.373453
3126.867416	145.158717	53.378458
3125.936547	152.934848	53.383463
3126.227004	143.851092	53.388468
3125.509051	146.527666	53.393473
3124.686788	150.379405	53.398477
3124.104639	143.922451	53.403482
3122.486595	150.659834	53.408487
3122.268440	140.373404	53.413492
3121.373177	150.597080	53.418497
3120.752641	149.700509	53.423501
3120.484653	138.360383	53.428506
3120.415150	149.801227	53.433511
3119.758831	141.225416	53.438516
3118.075910	151.996952	53.443521
3118.080448	148.503636	53.448525
3117.669518	145.078940	53.453530
3116.508153	146.231443	53.458535
3115.925438	143.275036	53.463540
3115.181567	146.508658	53.468545
3114.344894	145.707833	53.473549
3114.067666	148.381340	53.478554
3113.033573	158.551770	53.483559
3112.493822	147.525303	53.488564
3111.601270	155.174102	53.493569
3111.541238	142.495839	53.498573
3111.551316	141.358894	53.503578
3109.819303	138.657675	53.508583
3109.101248	141.742020	53.513588
3108.492151	145.562470	53.518593
3108.295837	146.350746	53.523597
3108.036960	138.661484	53.528602
3107.111142	147.387649	53.533607
3106.053529	142.265989	53.538612
3105.173890	140.329770	53.543617
3105.122543	139.742518	53.548621
3104.358539	144.712041	53.553626
3103.258040	144.324577	53.558631
3103.242889	142.810240	53.563636
3101.619234	144.786586	53.568641
3101.319622	140.029218	53.573645
3101.158322	136.642003	53.578650
3100.114811	144.407773	53.583655
3099.763426	132.747964	53.588660
3098.954691	134.181263	53.593665
3098.323076	137.311233	53.598669
3097.577248	134.162442	53.603674
3096.666971	142.708718	53.608679
3096.150153	125.833617	53.613684
3095.202407	136.106119	53.618689
3094.578894	132.516835	53.623693
3094.258096	137.235369	53.628698
3093.126179	138.931911	53.633703
3092.482472	129.301613	53.638708
3092.161525	140.603046	53.643713
3092.025843	126.426313	53.648717
3092.016270	131.771783	53.653722
3089.958929	137.052289	53.658727
3089.471724	126.153045	53.663732
3088.769156	139.435690	53.668737
3088.692102	134.317410	53.673741
3087.623958	132.597741	53.678746
3086.819665	134.542245	53.683751
3086.664138	132.361516	53.688756
3086.262295	138.720966	53.693761
3084.735616	135.669283	53.698765
3084.124316	137.565812	53.703770
3083.845131	145.222696	53.708775
3083.078403	131.154180	53.713780
3082.349465	133.446588	53.718785
3081.955068	130.980631	53.723789
3081.124576	126.563841	53.728794
3079.943214	137.819266	53.733799
3079.999745	133.886028	53.738804
3079.716551	136.550685	53.743809
3078.257018	136.398648	53.748813
3077.453507	136.890816	53.753818
3077.458022	138.643834	53.758823
3076.671111	133.694609	53.763828
3075.510353	136.897231	53.768833
3075.068650	135.445911	53.773837
3075.185808	130.201688	53.778842
3073.699573	139.126633	53.783847
3072.701526	123.011121	53.788852
3072.649094	134.503898	53.793857
3071.836633	131.816093	53.798861
3071.729317	131.031568	53.803866
3070.036184	141.118419	53.808871
3069.705353	129.993514	53.813876
3069.358111	133.964610	53.818881
3068.909963	138.389123	53.823885
3068.210723	132.570729	53.828890
3066.600643	139.330836	53.833895
3066.682875	133.744430	53.838900
3066.589111	139.791113	53.843905
3065.107143	135.344724	53.848909
3064.464881	133.761100	53.853914
3063.709872	135.760736	53.858919
3063.429133	131.484480	53.863924
3062.733917	132.788258	53.868929
3061.951949	130.862199	53.873933
3061.205581	127.437989	53.878938
3060.235950	132.853558	53.883943
3060.561169	125.836590	53.888948
3059.800311	130.043751	53.893953
3059.034309	138.142621	53.898957
3057.604922	129.023546	53.903962
3056.284803	133.818100	53.908967
3056.806836	136.040043	53.913972
3057.258342	136.830913	53.918977
3055.790753	133.829931	53.923981
3054.895238	121.925623	53.928986
3053.833965	129.613901	53.933991
3053.322650	130.954544	53.938996
3052.646312	128.136511	53.944001
3052.131219	125.598815	53.949005
3051.735543	124.835143	53.954010
3050.778992	131.997515	53.959015
3050.068794	132.945836	53.964020
3049.328048	126.772180	53.969025
3048.701634	133.496045	53.974029
3048.487615	128.468672	53.979034
3047.858529	140.873519	53.984039
3047.110444	135.899507	53.989044
3045.799207	129.296371	53.994049
3045.594364	131.376469	53.999053
3045.216375	122.562077	54.004058
3043.566297	129.633748	54.009063
3043.611848	125.386608	54.014068
3043.387194	126.224727	54.019073
3042.055875	125.824612	54.024077
3041.361091	123.819319	54.029082
3040.391770	127.771188	54.034087
3040.375227	115.835903	54.039092
3039.627830	126.145612	54.044097
3039.016483	128.323987	54.049101
3038.405070	126.696807	54.054106
3037.323635	122.081334	54.059111
3037.227754	118.164671	54.064116
3036.446339	126.463534	54.069121
3035.818928	129.711996	54.074125
3035.097990	131.545553	54.079130
3034.185654	130.455309	54.084135
3033.653032	122.799024	54.089140
3032.699267	122.777676	54.094145
3032.341634	127.772890	54.099149
3031.712293	126.149959	54.104154
3031.370927	131.085553	54.109159
3030.669283	122.598040	54.114164
3030.224095	126.253906	54.119169
3028.936585	122.785989	54.124173
3027.830880	113.827145	54.129178
3027.399870	115.060121	54.134183
3027.693887	115.998291	54.139188
3026.300292	119.425831	54.144193
3025.314873	122.155218	54.149197
3024.695473	122.925794	54.154202
3024.454875	136.391988	54.159207
3024.399159	128.943545	54.164212
3023.432617	130.764994	54.169217
3022.496321	123.725571	54.174221
3021.895568	123.936395	54.179226
3021.082259	125.617978	54.184231
3020.781221	121.255201	54.189236
3020.114824	125.035311	54.194241
3019.175744	130.868022	54.199245
3018.743587	129.308106	54.204250
3017.067004	131.611667	54.209255
3016.818266	122.909401	54.214260
3016.950995	123.002389	54.219265
3015.730231	123.062193	54.224269
3015.343203	122.494805	54.229274
3014.534531	137.055150	54.234279
3013.599535	127.296229	54.239284
3013.051695	134.804808	54.244289
3012.372176	129.525016	54.249293
3012.136103	122.320154	54.254298
3011.136039	133.832358	54.259303
3010.822659	134.843530	54.264308
3010.512958	133.534657	54.269313
3009.694120	127.059755	54.274317
3009.662577	131.833069	54.279322
3007.986695	129.935036	54.284327
3006.901654	123.872327	54.289332
3006.563919	123.697559	54.294337
3005.359365	134.621037	54.299341
3005.181525	126.783344	54.304346
3004.171154	121.732194	54.309351
3004.472898	123.282053	54.314356
3002.970082	127.038913	54.319361
3002.283050	129.450876	54.324365
3002.092683	116.992680	54.329370
3001.287394	134.323822	54.334375
3000.506078	130.801779	54.339380
3000.086003	127.441029	54.344385
2999.481237	133.508318	54.349389
2998.988969	112.878366	54.354394
2998.513317	122.099164	54.359399
2998.303143	127.122073	54.364404
2997.012104	127.690062	54.369409
2995.784251	133.466729	54.374413
2995.385711	116.865132	54.379418
2994.599399	126.809265	54.384423
2994.136452	124.936858	54.389428
2993.511080	126.276074	54.394433
2993.033620	126.046633	54.399437
2992.556998	122.433449	54.404442
2991.904839	123.669482	54.409447
2990.833184	119.761279	54.414452
2989.934184	121.240015	54.419457
2988.700257	126.518389	54.424461
2988.962887	120.879060	54.429466
2988.095981	123.231368	54.434471
2987.458907	125.074678	54.439476
2986.640446	116.871212	54.444481
2986.068931	125.038289	54.449485
2985.982132	117.330699	54.454490
2985.065429	121.409368	54.459495
2984.453889	120.555882	54.464500
2984.133420	126.021970	54.469505
2983.471642	124.455903	54.474509
2982.298668	117.369307	54.479514
2981.531710	119.881374	54.484519
2980.767390	122.632589	54.489524
2980.303900	124.887541	54.494529
2979.075214	121.828390	54.499533
2978.902416	118.597095	54.504538
2977.877570	126.078238	54.509543
2977.678986	122.526489	54.514548
2976.981452	119.823404	54.519553
2976.355520	122.908199	54.524557
2976.231681	117.937661	54.529562
2975.165885	122.535612	54.534567
2974.190524	121.807455	54.539572
2973.277127	120.798321	54.544577
2972.559955	121.341274	54.549581
2971.894180	122.471481	54.554586
2972.089277	125.362292	54.559591
2971.733668	116.550406	54.564596
2970.515775	120.658836	54.569601
2969.782005	120.647665	54.574605
2969.592199	121.387070	54.579610
2968.506232	122.420534	54.584615
2967.013487	125.654641	54.589620
2967.077926	115.878893	54.594625
2966.384716	124.098344	54.599629
2965.613891	125.889514	54.604634
2964.822948	124.960111	54.609639
2964.184843	126.363478	54.614644
2963.594397	129.619049	54.619649
2962.921208	125.915120	54.624653
2962.687744	122.172363	54.629658
2961.800021	128.895490	54.634663
2961.761047	128.498359	54.639668
2960.908024	132.784435	54.644673
2960.138426	132.259138	54.649677
2958.870706	123.427860	54.654682
2957.687618	132.053521	54.659687
2958.243013	124.184084	54.664692
2957.200472	129.503968	54.669697
2956.117116	132.706013	54.674701
2955.969605	128.628049	54.679706
2954.966604	127.115559	54.684711
2954.886102	124.375321	54.689716
2954.293336	126.631446	54.694721
2953.627741	133.603977	54.699725
2952.420934	121.737106	54.704730
2951.406033	123.634722	54.709735
2951.367697	127.319746	54.714740
2950.744987	129.226524	54.719745
2949.804225	121.830654	54.724749
2949.524178	119.845288	54.729754
2948.971248	129.637834	54.734759
2948.102617	122.662654	54.739764
2947.682082	127.167709	54.744769
2946.080494	131.988278	54.749773
2945.454074	123.103069	54.754778
2945.541245	122.004267	54.759783
2944.594609	116.547513	54.764788
2943.745593	117.478517	54.769793
2943.165963	125.922500	54.774797
2942.713180	115.018201	54.779802
2942.022164	126.714820	54.784807
2941.632140	124.559569	54.789812
2941.237016	117.437950	54.794817
2940.699991	124.322587	54.799821
2939.590316	113.344630	54.804826
2938.528537	115.575908	54.809831
2937.864440	112.384760	54.814836
2937.425993	121.603541	54.819841
2936.880202	119.327282	54.824845
2936.591517	109.790304	54.829850
2935.370807	125.656150	54.834855
2934.192126	114.472492	54.839860
2933.564217	115.223610	54.844865
2933.403877	119.543676	54.849869
2933.052908	114.712217	54.854874
2932.025472	124.849526	54.859879
2931.572145	124.573335	54.864884
2931.240548	116.921796	54.869889
2930.435137	122.989031	54.874893
2929.859478	115.710377	54.879898
2928.368489	119.659041	54.884903
2927.780752	113.437951	54.889908
2927.195000	121.463385	54.894913
2926.363822	126.563998	54.899917
2925.965694	117.695044	54.904922
2925.941133	119.067378	54.909927
2925.070219	126.285779	54.914932
2924.879456	120.892481	54.919937
2923.997774	116.603285	54.924941
2922.891290	114.604422	54.929946
2922.091574	114.374008	54.934951
2921.464088	118.610883	54.939956
2921.337960	117.325118	54.944961
2920.314471	125.481412	54.949965
2920.117569	119.632860	54.954970
2918.603880	124.889188	54.959975
2917.631428	124.734477	54.964980
2917.665641	114.680486	54.969985
2916.713107	125.524977	54.974989
2916.166016	125.143631	54.979994
2915.368970	125.628005	54.984999
2915.037232	123.764761	54.990004
2914.881401	122.414995	54.995009
2914.042713	119.607756	55.000013
2913.715476	113.369386	55.005018
2912.083123	123.238241	55.010023
2911.641276	126.466842	55.015028
2910.777217	120.300868	55.020033
2909.974289	123.710778	55.025037
2909.606532	120.132683	55.030042
2908.850377	126.230976	55.035047
2908.167001	123.113387	55.040052
2907.707489	124.480712	55.045057
2906.933858	130.872118	55.050061
2907.253324	113.155498	55.055066
2905.428956	121.465237	55.060071
2904.756515	118.883793	55.065076
2904.375754	118.101401	55.070081
2903.416443	125.318331	55.075085
2903.265581	118.893507	55.080090
2902.557184	120.684277	55.085095
2901.969948	122.284214	55.090100
2901.417884	119.085372	55.095105
2900.555575	122.540560	55.100109
2899.767591	113.296541	55.105114
2898.937129	119.114249	55.110119
2898.146439	120.975529	55.115124
2897.865396	120.123992	55.120129
2897.243646	121.807589	55.125133
2896.430385	117.526047	55.130138
2896.558761	126.370073	55.135143
2895.694435	127.869738	55.140148
2894.886151	123.866415	55.145153
2893.779122	125.708734	55.150157
2893.450260	120.031154	55.155162
2892.078112	119.898177	55.160167
2891.772742	123.052533	55.165172
2890.873351	120.764475	55.170177
2890.438068	117.698831	55.175181
2889.612719	111.599275	55.180186
2889.048307	120.166178	55.185191
2888.340607	120.165562	55.190196
2887.980538	127.455343	55.195201
2887.347839	116.326019	55.200205
2887.210054	112.723231	55.205210
2886.531407	114.433130	55.210215
2885.582789	118.107143	55.215220
2884.300634	115.283333	55.220225
2883.559596	119.938686	55.225229
2883.251723	121.209836	55.230234
2882.589603	123.606105	55.235239
2882.016481	125.714013	55.240244
2881.615258	120.532341	55.245249
2881.031888	130.036412	55.250253
2879.735292	121.154044	55.255258
2879.102754	123.489206	55.260263
2878.343957	119.938471	55.265268
2878.068122	117.910155	55.270273
2877.524940	126.736716	55.275277
2877.142038	115.450234	55.280282
2876.515025	126.671715	55.285287
2875.408411	130.319446	55.290292
2874.565772	122.529467	55.295297
2873.840556	122.465532	55.300301
2873.120203	118.616920	55.305306
2872.705399	116.306442	55.310311
2872.118395	120.619690	55.315316
2872.015115	110.306976	55.320321
2870.571212	114.836141	55.325325
2869.713640	113.433022	55.330330
2869.013801	119.198804	55.335335
2868.067580	116.765601	55.340340
2867.622895	120.702036	55.345345
2867.795941	128.699632	55.350349
2867.273103	112.602854	55.355354
2866.552052	117.494390	55.360359
2865.967484	124.324788	55.365364
2865.050794	116.866408	55.370369
2863.925339	110.115140	55.375373
2863.250763	118.304170	55.380378
2862.884326	119.205998	55.385383
2862.164145	115.808531	55.390388
2862.173090	112.303033	55.395393
2860.488641	115.369799	55.400397
2859.952619	114.233823	55.405402
2859.288374	120.293515	55.410407
2858.421490	118.923173	55.415412
2858.119600	114.605557	55.420417
2857.472177	123.168492	55.425421
2857.199147	122.464004	55.430426
2856.779947	125.890836	55.435431
2856.010750	118.057523	55.440436
2854.729056	108.485406	55.445441
2854.019334	121.659123	55.450445
2853.507133	111.462481	55.455450
2853.066925	117.449936	55.460455
2852.571544	123.254987	55.465460
2852.356082	112.446328	55.470465
2850.825277	115.308422	55.475469
2850.004145	116.737949	55.480474
2848.959681	124.049961	55.485479
2848.706095	113.262028	55.490484
2848.140033	120.764243	55.495489
2847.764945	118.222775	55.500493
2847.507298	114.566265	55.505498
2846.695559	123.583587	55.510503
2845.740566	115.411384	55.515508
2844.992921	113.053586	55.520513
2844.189491	118.606160	55.525517
2843.769444	120.429758	55.530522
2843.544738	118.111266	55.535527
2842.806689	111.964037	55.540532
2841.680830	108.133028	55.545537
2840.506581	117.280590	55.550541
2840.094522	112.056963	55.555546
2839.508616	111.925014	55.560551
2838.742517	117.231609	55.565556
2838.670332	115.301908	55.570561
2837.996697	119.431022	55.575565
2837.805041	114.057228	55.580570
2836.189042	117.832677	55.585575
2835.496171	111.268793	55.590580
2834.859174	108.050926	55.595585
2834.170789	122.347939	55.600589
2834.242596	117.615941	55.605594
2833.622842	109.260530	55.610599
2832.529188	114.785339	55.615604
2831.285413	114.358470	55.620609
2830.269132	118.807850	55.625613
2830.779436	111.375981	55.630618
2830.353183	113.701547	55.635623
2829.593318	120.839001	55.640628
2828.945920	114.053798	55.645633
2827.631780	118.289223	55.650637
2826.858632	106.369999	55.655642
2826.071284	110.764461	55.660647
2825.578458	114.266241	55.665652
2825.293797	102.625891	55.670657
2824.579687	118.540937	55.675661
2824.349430	107.751788	55.680666
2823.741543	113.996447	55.685671
2822.584219	118.807029	55.690676
2822.322010	106.498515	55.695681
2821.321899	118.072302	55.700685
2820.400748	108.421996	55.705690
2820.232852	111.314836	55.710695
2819.065312	110.167198	55.715700
2818.407563	110.821588	55.720705
2817.765840	123.306729	55.725709
2817.578629	112.530747	55.730714
2816.874334	113.454401	55.735719
2816.398861	121.274677	55.740724
2815.668127	105.338581	55.745729
2814.302056	108.047399	55.750733
2813.641869	102.662113	55.755738
2813.266228	99.595366	55.760743
2812.595629	110.480874	55.765748
2812.411290	107.069991	55.770753
2811.905615	111.712751	55.775757
2810.853981	107.424602	55.780762
2809.840102	113.274453	55.785767
2808.855208	119.778546	55.790772
2808.716889	108.774743	55.795777
2808.054270	107.917772	55.800781
2807.234093	107.683371	55.805786
2806.483712	115.713257	55.810791
2806.244105	116.195922	55.815796
2805.788086	111.656768	55.820801
2804.119372	113.083536	55.825805
2803.902791	99.662395	55.830810
2803.051705	111.646484	55.835815
2802.616896	111.575160	55.840820
2802.597342	106.686285	55.845825
2802.133008	109.066517	55.850829
2801.036301	110.536439	55.855834
2799.891878	112.429768	55.860839
2799.313141	113.328017	55.865844
2798.673113	107.401275	55.870849
2797.965299	116.524777	55.875853
2797.708997	107.678583	55.880858
2797.428350	109.209548	55.885863
2796.181440	108.505337	55.890868
2795.468829	102.630476	55.895873
2794.425658	106.470259	55.900877
2793.750063	106.645347	55.905882
2793.568846	110.241102	55.910887
2792.912824	115.402573	55.915892
2792.743870	108.714021	55.920897
2791.226495	113.724299	55.925901
2791.017974	112.183023	55.930906
2790.505763	106.809553	55.935911
2789.657390	116.233386	55.940916
2789.331229	111.936111	55.945921
2787.990774	112.212994	55.950925
2787.136658	109.702487	55.955930
2786.486975	120.253252	55.960935
2786.133141	114.798632	55.965940
2785.558574	104.236494	55.970945
2785.119044	108.287308	55.975949
2784.529891	105.518363	55.980954
2784.086346	106.549818	55.985959
2782.797221	111.720027	55.990964
2782.457580	103.308859	55.995969
2781.580063	115.638512	56.000973
2781.322173	109.231602	56.005978
2780.824943	112.744399	56.010983
2779.483884	110.773030	56.015988
2778.482219	108.770888	56.020993
2777.549543	111.196829	56.025997
2777.219120	102.168315	56.031002
2777.047648	100.942410	56.036007
2776.371472	108.428310	56.041012
2776.083618	111.495597	56.046017
2775.183542	113.979912	56.051021
2774.536740	110.305847	56.056026
2773.677228	111.507081	56.061031
2772.963304	111.650040	56.066036
2772.679653	105.916200	56.071041
2771.773932	109.009752	56.076045
2771.611418	105.275809	56.081050
2770.631532	104.807797	56.086055
2769.216191	103.616869	56.091060
2768.891228	108.289925	56.096065
2768.259192	114.145961	56.101069
2767.779504	106.415950	56.106074
2767.451449	108.783548	56.111079
2766.764451	109.954507	56.116084
2765.953760	105.204410	56.121089
2764.993767	113.013157	56.126093
2764.220182	109.614968	56.131098
2763.939752	113.817006	56.136103
2763.441759	109.122800	56.141108
2762.998502	99.221891	56.146113
2761.690337	111.823695	56.151117
2760.913909	113.402692	56.156122
2760.306670	116.035504	56.161127
2759.476914	117.936635	56.166132
2759.326503	111.326624	56.171137
2759.208221	110.995549	56.176141
2758.526313	107.911682	56.181146
2757.424980	110.096066	56.186151
2756.165893	113.105944	56.191156
2755.766499	109.613799	56.196161
2755.422014	104.388109	56.201165
2754.887839	115.200172	56.206170
2753.875847	106.922479	56.211175
2752.890650	110.247111	56.216180
2752.085456	103.760469	56.221185
2751.865550	114.167510	56.226189
2751.611802	112.600810	56.231194
2750.942164	102.836092	56.236199
2749.845599	113.469550	56.241204
2749.530095	105.971603	56.246209
2748.466949	106.955416	56.251213
2748.014878	110.297080	56.256218
2747.914436	113.350491	56.261223
2746.496431	102.301361	56.266228
2745.641351	102.014121	56.271233
2744.707602	100.613386	56.276237
2744.566762	108.785395	56.281242
2743.975124	109.481386	56.286247
2743.282653	107.037598	56.291252
2742.974590	97.060692	56.296257
2742.192971	99.626996	56.301261
2741.686078	103.625774	56.306266
2740.956003	102.241147	56.311271
2739.662768	107.402985	56.316276
2739.582652	110.068064	56.321281
2738.717267	102.841735	56.326285
2738.309896	106.449303	56.331290
2737.294324	110.392927	56.336295
2736.410531	116.603832	56.341300
2735.557906	102.096584	56.346305
2735.330759	108.381952	56.351309
2735.133835	101.390699	56.356314
2734.759095	102.717887	56.361319
2733.572642	114.906535	56.366324
2733.476168	105.779224	56.371329
2732.642244	111.241887	56.376333
2730.804407	113.645714	56.381338
2730.408103	106.038032	56.386343
2730.511601	111.272176	56.391348
2729.370606	100.794634	56.396353
2728.314006	100.967751	56.401357
2728.003013	101.157892	56.406362
2727.392453	97.271991	56.411367
2726.504924	107.259867	56.416372
2726.686862	108.905971	56.421377
2726.200307	114.175843	56.426381
2725.107809	116.094257	56.431386
2724.132711	99.296832	56.436391
2723.440916	111.054358	56.441396
2723.408188	102.405219	56.446401
2722.085357	108.691955	56.451405
2721.263283	106.677680	56.456410
2720.688478	101.159794	56.461415
2719.674928	106.405667	56.466420
2719.808310	99.352037	56.471425
2718.899422	98.675326	56.476429
2718.701035	103.030307	56.481434
2717.664764	105.002266	56.486439
2716.754766	108.461282	56.491444
2716.485473	102.556843	56.496449
2715.741103	103.466437	56.501453
2715.257324	103.109420	56.506458
2714.386580	93.600532	56.511463
2713.266890	101.868404	56.516468
2712.843175	91.468789	56.521473
2711.782972	99.188088	56.526477
2711.524886	100.861247	56.531482
2711.276248	102.198854	56.536487
2710.662788	109.288391	56.541492
2710.290855	104.970924	56.546497
2709.301834	104.669875	56.551501
2708.595051	96.462000	56.556506
2707.696062	97.121717	56.561511
2706.691632	106.532356	56.566516
2706.336756	102.066322	56.571521
2705.794153	100.815439	56.576525
2705.260150	98.078527	56.581530
2704.523384	93.385280	56.586535
2703.901402	101.714917	56.591540
2703.189568	95.502454	56.596545
2701.708631	104.390219	56.601549
2701.064505	102.397240	56.606554
2700.845892	103.613666	56.611559
2700.146555	102.215106	56.616564
2700.011933	93.536814	56.621569
2699.567905	100.141873	56.626573
2699.067962	88.575854	56.631578
2698.067549	100.256655	56.636583
2697.132068	102.315596	56.641588
2697.083101	87.231673	56.646593
2695.653847	98.504607	56.651597
2694.742257	96.565637	56.656602
2694.345107	93.602840	56.661607
2693.315436	100.400371	56.666612
2692.796863	88.640964	56.671617
2692.297640	99.092577	56.676621
2691.745623	96.073754	56.681626
2691.463440	92.848944	56.686631
2691.154448	99.849329	56.691636
2690.380733	93.679814	56.696641
2689.369898	94.074845	56.701645
2688.600709	91.462213	56.706650
2688.151642	79.898559	56.711655
2686.872219	95.545480	56.716660
2686.321755	86.945775	56.721665
2685.684678	94.341307	56.726669
2685.012786	92.889508	56.731674
2684.666357	90.638415	56.736679
2684.128409	96.568364	56.741684
2683.862250	100.125347	56.746689
2682.291965	93.454121	56.751693
2681.594399	95.160957	56.756698
2681.104374	87.655756	56.761703
2680.448953	101.742249	56.766708
2680.400461	93.748294	56.771713
2679.677188	92.320673	56.776717
2678.691827	97.274370	56.781722
2677.845394	92.301858	56.786727
2676.673010	99.299043	56.791732
2676.724505	96.814145	56.796737
2676.168768	96.898498	56.801741
2675.587125	98.692885	56.806746
2675.203712	102.769633	56.811751
2673.624461	99.224978	56.816756
2673.298023	94.018716	56.821761
2672.897418	100.097289	56.826765
2672.012898	95.661798	56.831770
2671.931643	90.991897	56.836775
2670.602232	100.138755	56.841780
2669.988704	100.048650	56.846785
2669.585233	97.639945	56.851789
2668.661015	94.704879	56.856794
2668.586009	94.383383	56.861799
2666.817087	103.476297	56.866804
2665.924846	94.366610	56.871809
2666.009287	98.517721	56.876813
2665.123698	99.486986	56.881818
2664.370237	94.967122	56.886823
2664.199273	104.335157	56.891828
2664.357339	96.718775	56.896833
2663.573591	101.038820	56.901837
2661.856468	97.861937	56.906842
2661.207683	86.877143	56.911847
2660.813628	97.532217	56.916852
2660.430073	94.554073	56.921857
2659.744321	99.121042	56.926861
2658.125703	95.934032	56.931866
2657.942481	96.256278	56.936871
2657.261825	102.865079	56.941876
2657.058939	90.566598	56.946881
2656.284525	105.976815	56.951885
2656.235256	96.732900	56.956890
2655.483674	94.782374	56.961895
2654.336236	96.362437	56.966900
2653.840721	89.317243	56.971905
2653.371157	99.994700	56.976909
2652.282481	98.690727	56.981914
2651.141814	87.603707	56.986919
2650.561670	95.853166	56.991924
2650.060845	92.479030	56.996929
2649.780356	99.455200	57.001933
2649.182787	94.461467	57.006938
2647.992588	90.522301	57.011943
2646.802339	93.333724	57.016948
2646.443240	90.719680	57.021953
2645.827643	83.479892	57.026957
2645.705741	83.863101	57.031962
2645.207920	88.470967	57.036967
2644.655584	91.989240	57.041972
2643.981417	85.910875	57.046977
2642.849896	85.579331	57.051981
2642.201972	93.699064	57.056986
2641.893902	91.456417	57.061991
2641.263397	91.551975	57.066996
2640.820656	85.522469	57.072001
2639.725845	100.121029	57.077005
2638.681933	92.857748	57.082010
2638.133226	88.306047	57.087015
2637.834331	104.183642	57.092020
2637.364733	91.247094	57.097025
2636.724926	97.170378	57.102029
2635.259537	95.127146	57.107034
2634.824321	94.940250	57.112039
2633.882759	99.687131	57.117044
2633.808871	89.567194	57.122049
2633.132937	83.137435	57.127053
2633.052507	94.467949	57.132058
2632.122235	92.195485	57.137063
2630.580646	92.402975	57.142068
2630.643022	92.426667	57.147073
2629.880724	95.325196	57.152077
2629.400756	94.554653	57.157082
2628.613019	89.369624	57.162087
2627.326437	100.041487	57.167092
2627.285292	86.950783	57.172097
2626.684624	86.269951	57.177101
2625.808408	88.420214	57.182106
2625.702905	87.049228	57.187111
2624.181444	93.396771	57.192116
2623.842353	93.677376	57.197121
2623.395672	91.728417	57.202125
2622.788123	94.341948	57.207130
2621.854371	82.629852	57.212135
2620.506533	96.817731	57.217140
2620.024614	86.201515	57.222145
2619.726252	96.438004	57.227149
2619.020911	94.181562	57.232154
2618.830812	87.106664	57.237159
2617.930657	95.037024	57.242164
2617.786953	93.707699	57.247169
2616.555971	85.562619	57.252173
2615.604803	93.623669	57.257178
2615.304133	99.244251	57.262183
2614.592756	99.657575	57.267188
2614.365069	96.410824	57.272193
2613.400173	98.966632	57.277197
2612.345763	100.189758	57.282202
2611.870827	94.134968	57.287207
2611.203508	94.266032	57.292212
2610.715250	94.914759	57.297217
2610.500783	98.128574	57.302221
2609.056829	99.490922	57.307226
2608.658568	96.529507	57.312231
2607.808087	97.667642	57.317236
2607.806681	89.687357	57.322241
2607.645898	98.650630	57.327245
2605.877118	103.493534	57.332250
2605.215862	94.956199	57.337255
2604.919777	88.453613	57.342260
2604.081696	102.510937	57.347265
2602.845367	98.050340	57.352269
2601.958625	102.665489	57.357274
2601.899509	93.092880	57.362279
2601.120351	105.298744	57.367284
2600.639915	102.420848	57.372289
2600.573983	103.663674	57.377293
2600.003697	106.952529	57.382298
2599.210111	95.538958	57.387303
2598.350205	105.333833	57.392308
2597.680189	104.098033	57.397313
2596.968773	90.535749	57.402317
2595.036121	96.387163	57.407322
2595.056439	89.772069	57.412327
2594.275408	96.409476	57.417332
2594.243547	95.257210	57.422337
2593.462610	96.071231	57.427341
2593.080376	92.432890	57.432346
2593.162738	89.772986	57.437351
2591.420953	93.392367	57.442356
2590.756396	90.257802	57.447361
2590.009344	92.224547	57.452365
2589.049007	95.205486	57.457370
2588.981828	88.271020	57.462375
2588.217459	90.818997	57.467380
2587.715318	91.633514	57.472385
2586.384316	90.254144	57.477389
2585.842745	92.497594	57.482394
2585.956872	89.628977	57.487399
2584.969142	97.430238	57.492404
2584.884514	88.993670	57.497409
2583.316282	91.151324	57.502413
2582.638173	95.432789	57.507418
2582.338331	86.717235	57.512423
2581.684090	98.539776	57.517428
2581.092310	94.353461	57.522433
2580.079128	95.756643	57.527437
2579.189463	92.612011	57.532442
2578.585588	94.092059	57.537447
2577.887232	92.201129	57.542452
2577.842371	94.343876	57.547457
2577.603111	89.204431	57.552461
2576.470804	90.650478	57.557466
2576.030261	88.501928	57.562471
2574.832049	98.685414	57.567476
2574.282979	88.948684	57.572481
2573.934137	86.105928	57.577485
2572.773876	101.350002	57.582490
2572.282896	89.538538	57.587495
2571.204336	86.106475	57.592500
2570.794332	80.914515	57.597505
2570.375616	93.307820	57.602509
2569.958248	96.351855	57.607514
2569.625289	91.547365	57.612519
2568.575681	94.140160	57.617524
2567.522939	93.531093	57.622529
2567.203005	84.592011	57.627533
2566.676456	89.497677	57.632538
2565.972628	82.318382	57.637543
2564.779027	90.969941	57.642548
2564.633957	88.198134	57.647553
2564.315255	92.994060	57.652557
2562.694536	93.712844	57.657562
2562.182728	86.047577	57.662567
2561.070733	97.950347	57.667572
2560.920479	91.179291	57.672577
2560.636505	88.035323	57.677581
2559.733415	97.895997	57.682586
2559.849706	83.442645	57.687591
2558.163533	91.291863	57.692596
2557.464666	92.398954	57.697601
2557.227743	92.204217	57.702605
2556.748672	100.742706	57.707610
2556.276104	87.736031	57.712615
2555.475922	86.592358	57.717620
2554.455159	95.624097	57.722625
2553.929583	89.037202	57.727629
2553.153827	89.394042	57.732634
2552.869299	82.720942	57.737639
2551.477805	88.410378	57.742644
2550.603393	78.760463	57.747649
2550.253486	86.530046	57.752653
2549.988270	92.345478	57.757658
2549.641005	89.616529	57.762663
2548.910369	85.468169	57.767668
2548.041350	91.378538	57.772673
2547.352102	85.599603	57.777677
2546.361790	91.925827	57.782682
2546.125984	88.921647	57.787687
2545.528204	88.469270	57.792692
2544.944939	92.177567	57.797697
2544.052918	93.499255	57.802701
2543.072482	88.783357	57.807706
2543.030051	87.094102	57.812711
2541.568998	92.874772	57.817716
2540.839310	92.695992	57.822721
2540.635367	98.433453	57.827725
2539.973158	89.894719	57.832730
2539.761128	92.293406	57.837735
2538.614992	93.427625	57.842740
2537.479784	91.493757	57.847745
2536.629232	83.306164	57.852749
2536.235819	92.879181	57.857754
2536.004479	83.776147	57.862759
2535.037756	92.290242	57.867764
2534.870791	80.338533	57.872769
2534.422553	85.769609	57.877773
2534.113429	88.308838	57.882778
2533.006579	86.975631	57.887783
2531.694839	94.172704	57.892788
2531.652592	89.447199	57.897793
2530.932782	85.078315	57.902797
2529.512935	96.287689	57.907802
2529.200954	89.200086	57.912807
2528.091084	83.065974	57.917812
2527.609431	86.693349	57.922817
2527.435392	82.544964	57.927821
2527.154605	81.144346	57.932826
2527.079150	79.312321	57.937831
2525.789174	99.719062	57.942836
2524.852014	96.809131	57.947841
2524.649669	90.892483	57.952845
2523.532052	98.808715	57.957850
2522.548628	86.924354	57.962855
2521.860108	92.849655	57.967860
2521.570403	94.740586	57.972865
2521.136914	94.924050	57.977869
2520.070982	99.587999	57.982874
2519.171701	93.245783	57.987879
2518.270100	97.406389	57.992884
2518.078249	99.635843	57.997889
2517.339968	90.687764	58.002893
2517.081129	96.977750	58.007898
2516.808705	87.475175	58.012903
2516.069394	85.941772	58.017908
2514.712440	89.228152	58.022913
2514.410467	83.416564	58.027917
2513.999578	91.117234	58.032922
2512.868288	79.244346	58.037927
2511.751202	88.082954	58.042932
2510.919472	84.352924	58.047937
2510.818301	84.957979	58.052941
2510.051906	92.992184	58.057946
2509.516453	83.366823	58.062951
2509.109548	92.678470	58.067956
2508.990814	87.904467	58.072961
2507.899626	93.425732	58.077965
2506.711804	95.811649	58.082970
2506.676438	89.276343	58.087975
2505.918894	91.880791	58.092980
2504.768551	89.300593	58.097985
2504.150129	86.055921	58.102989
2503.603524	99.035547	58.107994
2503.366447	91.217926	58.112999
2502.310625	92.566440	58.118004
2501.401012	91.610426	58.123009
2500.881305	87.718108	58.128013
2500.184489	89.442203	58.133018
2499.870728	84.313136	58.138023
2499.336520	90.057323	58.143028
2498.526411	84.989432	58.148033
2497.510537	91.777517	58.153037
2496.703820	92.135315	58.158042
2496.704623	82.437617	58.163047
2495.875079	88.484130	58.168052
2494.919604	92.762498	58.173057
2494.113730	89.099495	58.178061
2493.006700	94.557158	58.183066
2492.838973	90.635845	58.188071
2492.329339	93.274882	58.193076
2491.940336	92.728792	58.198081
2491.647994	83.258048	58.203085
2490.830347	90.472885	58.208090
2490.184526	89.351777	58.213095
2489.396469	93.959931	58.218100
2488.454470	87.771865	58.223105
2487.598754	91.960154	58.228109
2486.366088	93.799548	58.233114
2486.231494	90.832145	58.238119
2485.446354	93.967876	58.243124
2485.261065	93.933650	58.248129
2485.090957	87.462040	58.253133
2484.375652	98.612938	58.258138
2483.610338	84.547159	58.263143
2482.457135	94.295865	58.268148
2481.746021	90.343119	58.273153
2481.627447	90.224463	58.278157
2479.975984	100.258881	58.283162
2479.313197	97.135081	58.288167
2478.669011	96.194083	58.293172
2478.353947	91.956920	58.298177
2478.025059	95.351740	58.303181
2477.378158	99.506304	58.308186
2477.337147	92.115413	58.313191
2476.313482	91.717701	58.318196
2475.208430	94.006185	58.323201
2474.899362	90.272060	58.328205
2474.164870	89.636625	58.333210
2473.244346	83.334370	58.338215
2472.096069	87.173613	58.343220
2471.298422	89.050735	58.348225
2471.166599	83.688072	58.353229
2470.670126	91.800467	58.358234
2470.571108	86.578242	58.363239
2469.905195	86.940785	58.368244
2468.804231	87.314950	58.373249
2468.127161	83.972551	58.378253
2467.522210	90.856165	58.383258
2467.006241	85.336951	58.388263
2465.890464	96.002125	58.393268
2465.249217	91.001286	58.398273
2464.540657	92.204779	58.403277
2464.002455	95.705647	58.408282
2463.513766	83.122924	58.413287
2462.071545	87.095318	58.418292
2461.446268	87.789983	58.423297
2461.010044	82.418578	58.428301
2460.248429	90.812744	58.433306
2460.278497	81.584899	58.438311
2459.862849	85.627687	58.443316
2459.199123	86.630100	58.448321
2458.254931	88.049927	58.453325
2457.398346	88.887163	58.458330
2457.016475	89.654681	58.463335
2456.562524	98.819248	58.468340
2455.384413	89.081939	58.473345
2454.780045	92.870032	58.478349
2453.633333	98.889074	58.483354
2453.533003	90.146530	58.488359
2452.988200	89.085915	58.493364
2452.163394	85.478262	58.498369
2451.575909	85.291363	58.503373
2450.693896	87.363696	58.508378
2450.372426	86.245950	58.513383
2450.023925	92.156144	58.518388
2448.732007	92.252709	58.523393
2447.871511	88.689840	58.528397
2447.313323	93.159620	58.533402
2446.962148	87.384477	58.538407
2446.649476	83.984514	58.543412
2445.543293	86.298458	58.548417
2444.723852	78.993699	58.553421
2444.234262	86.681770	58.558426
2443.805803	81.131021	58.563431
2443.159301	89.236304	58.568436
2441.792796	81.474440	58.573441
2441.369636	81.701932	58.578445
2440.346804	88.773044	58.583450
2440.299899	82.210115	58.588455
2439.569056	88.906840	58.593460
2439.037560	94.041508	58.598465
2438.842844	94.560720	58.603469
2437.501831	94.971987	58.608474
2436.867878	93.511762	58.613479
2435.952717	92.990114	58.618484
2435.746795	91.989582	58.623489
2435.251911	81.761268	58.628493
2434.042266	86.724525	58.633498
2433.540825	85.787942	58.638503
2432.693328	94.773487	58.643508
2432.119145	91.406001	58.648513
2432.134849	84.780657	58.653517
2431.182678	91.347469	58.658522
2430.523449	84.225705	58.663527
2430.145011	89.125394	58.668532
2429.230142	90.157724	58.673537
2428.501210	86.069882	58.678541
2427.168598	97.236330	58.683546
2426.394401	90.322899	58.688551
2425.864200	86.894212	58.693556
2425.359021	93.277233	58.698561
2425.487879	94.730692	58.703565
2424.585202	90.471642	58.708570
2424.458717	79.831407	58.713575
2423.488873	85.638239	58.718580
2422.667706	82.229305	58.723585
2422.112185	85.041579	58.728589
2420.922429	86.939568	58.733594
2420.103684	89.777509	58.738599
2419.467108	80.529052	58.743604
2418.939003	78.985208	58.748609
2418.574204	84.029400	58.753613
2417.785208	88.716665	58.758618
2417.322093	84.799289	58.763623
2416.377151	80.849433	58.768628
2415.242749	82.520466	58.773633
2415.109160	80.867326	58.778637
2414.607747	90.351439	58.783642
2414.523261	89.775392	58.788647
2413.225204	84.925156	58.793652
2412.176170	82.743697	58.798657
2411.896528	83.757808	58.803661
2411.339376	91.361122	58.808666
2410.733046	80.477287	58.813671
2409.542472	85.993848	58.818676
2408.490470	89.637831	58.823681
2408.271270	89.484673	58.828685
2407.832012	93.926621	58.833690
2407.380963	85.234974	58.838695
2407.028107	84.389431	58.843700
2406.316888	88.162245	58.848705
2405.731221	82.999552	58.853709
2404.723290	83.523606	58.858714
2404.296456	77.104983	58.863719
2403.252068	86.460100	58.868724
2402.169823	88.263134	58.873729
2402.057563	91.960771	58.878733
2401.244209	93.568624	58.883738
2400.622099	86.193421	58.888743
2400.068279	91.393879	58.893748
2398.846525	91.992388	58.898753
2398.569623	90.184153	58.903757
2398.055888	85.780846	58.908762
2397.486100	81.591590	58.913767
2396.896519	91.488660	58.918772
2395.998894	78.805753	58.923777
2395.079280	75.751541	58.928781
2394.523049	80.896752	58.933786
2394.393341	87.505298	58.938791
2393.596076	85.233032	58.943796
2392.823349	96.585977	58.948801
2392.062759	86.955715	58.953805
2391.244055	85.212887	58.958810
2390.825956	82.969733	58.963815
2390.604222	88.473000	58.968820
2389.215099	90.881517	58.973825
2388.021833	80.717367	58.978829
2387.748841	83.881584	58.983834
2387.132988	83.158378	58.988839
2386.920056	83.769912	58.993844
2386.857044	88.486987	58.998849
2385.845071	78.244869	59.003853
2384.621525	89.648843	59.008858
2384.303619	83.299618	59.013863
2383.576298	82.710732	59.018868
2382.864680	77.968645	59.023873
2382.030770	80.986018	59.028877
2381.161018	88.818434	59.033882
2380.475701	80.104486	59.038887
2380.210255	81.264193	59.043892
2379.741224	83.202368	59.048897
2379.025274	80.015049	59.053901
2377.661306	84.358146	59.058906
2377.430294	85.928792	59.063911
2376.760993	79.094543	59.068916
2376.504504	78.536461	59.073921
2375.766825	79.568501	59.078925
2374.638175	83.760049	59.083930
2373.972299	73.862560	59.088935
2373.505563	72.671374	59.093940
2373.133745	83.611955	59.098945
2372.648649	79.572822	59.103949
2371.360825	93.240475	59.108954
2371.114917	82.177392	59.113959
2370.439453	81.145444	59.118964
2369.993705	83.867507	59.123969
2368.829416	80.285157	59.128973
2367.610050	87.953152	59.133978
2367.529733	82.551297	59.138983
2367.294125	84.612975	59.143988
2366.289555	80.350048	59.148993
2366.017900	81.047412	59.153997
2364.493736	85.175544	59.159002
2363.819973	82.575861	59.164007
2363.744469	84.649240	59.169012
2362.994371	90.130358	59.174017
2362.458695	76.602835	59.179021
2361.974795	87.181676	59.184026
2361.004060	79.725969	59.189031
2360.304058	87.043456	59.194036
2359.634514	85.699850	59.199041
2359.749997	79.603354	59.204045
2357.849084	79.584608	59.209050
2357.356414	76.857254	59.214055
2356.597856	82.376131	59.219060
2356.181177	89.293474	59.224065
2356.017750	84.558307	59.229069
2355.592582	81.298770	59.234074
2354.718619	84.173395	59.239079
2353.606344	78.020402	59.244084
2352.542699	87.113958	59.249089
2352.678520	84.919770	59.254093
2352.237969	78.855987	59.259098
2351.329541	88.702975	59.264103
2350.382475	83.111448	59.269108
2349.863428	87.765190	59.274113
2349.586314	85.735555	59.279117
2348.388779	92.150918	59.284122
2347.284429	89.299217	59.289127
2346.429269	90.025309	59.294132
2346.364170	89.648836	59.299137
2346.070998	80.318781	59.304141
2345.567368	83.210605	59.309146
2344.824477	80.475514	59.314151
2344.151389	84.745873	59.319156
2343.014399	89.362787	59.324161
2342.507170	82.631088	59.329165
2341.820925	84.133136	59.334170
2340.870046	80.334307	59.339175
2340.013948	87.392707	59.344180
2339.125671	87.399750	59.349185
2339.519255	85.167011	59.354189
2338.903721	90.198820	59.359194
2338.556169	85.564216	59.364199
2337.577735	88.170140	59.369204
2336.510373	88.427273	59.374209
2336.254300	82.453126	59.379213
2335.371027	92.590279	59.384218
2334.287661	83.529946	59.389223
2333.504656	85.343004	59.394228
2333.171913	82.946713	59.399233
2332.678740	76.373662	59.404237
2332.322600	82.173057	59.409242
2331.166175	72.539455	59.414247
2330.011930	77.296682	59.419252
2329.160525	76.993090	59.424257
2329.156067	70.407523	59.429261
2328.622754	80.377066	59.434266
2328.178105	77.524271	59.439271
2328.208752	73.558395	59.444276
2326.795634	77.317821	59.449281
2326.366084	72.846845	59.454285
2325.287924	83.394673	59.459290
2324.862101	75.878165	59.464295
2323.767436	77.864118	59.469300
2322.614976	81.120306	59.474305
2322.415507	79.937104	59.479309
2321.502296	85.562558	59.484314
2321.373518	87.913460	59.489319
2321.072516	85.152938	59.494324
2320.505412	85.357292	59.499329
2319.921171	83.300840	59.504333
2318.548857	81.620325	59.509338
2318.255769	86.506209	59.514343
2317.823860	81.421050	59.519348
2316.981259	89.922621	59.524353
2316.357980	79.544978	59.529357
2315.543488	92.026077	59.534362
2315.117514	80.229217	59.539367
2313.949342	83.848869	59.544372
2312.774464	91.799388	59.549377
2312.646372	87.278832	59.554381
2312.118306	84.663320	59.559386
2311.716864	87.458334	59.564391
2310.916067	79.705958	59.569396
2309.496532	84.457636	59.574401
2308.741453	77.366895	59.579405
2308.381752	89.277606	59.584410
2308.425562	85.479209	59.589415
2308.019053	82.011230	59.594420
2307.161901	87.643284	59.599425
2306.543261	70.448387	59.604429
2305.332691	80.312698	59.609434
2304.952200	81.232747	59.614439
2304.428985	84.276734	59.619444
2303.350923	84.155979	59.624449
2302.411103	78.327182	59.629453
2301.697387	79.008566	59.634458
2301.248800	82.380042	59.639463
2301.004968	81.776380	59.644468
2300.645629	75.966736	59.649473
2300.423460	73.848767	59.654477
2299.361560	83.500559	59.659482
2298.369593	84.043612	59.664487
2297.863425	75.559567	59.669492
2296.875098	85.521662	59.674497
2296.158338	74.788580	59.679501
2295.485861	81.311125	59.684506
2295.127684	78.459730	59.689511
2294.684532	79.621013	59.694516
2292.920521	92.458293	59.699521
2292.288925	90.584804	59.704525
2291.900062	88.981637	59.709530
2292.041269	85.211583	59.714535
2291.628413	91.739471	59.719540
2291.053492	84.941595	59.724545
2289.805482	80.959123	59.729549
2288.733240	83.825033	59.734554
2288.496077	84.656628	59.739559
2287.633238	80.223435	59.744564
2287.145065	84.096269	59.749569
2286.517506	91.219800	59.754573
2285.389466	88.633472	59.759578
2284.880250	84.173358	59.764583
2284.719206	79.328848	59.769588
2284.062107	86.292040	59.774593
2282.850725	83.815093	59.779597
2282.264158	80.105551	59.784602
2281.567403	90.399091	59.789607
2281.230231	81.874700	59.794612
2280.646809	87.923746	59.799617
2280.011251	82.059894	59.804621
2278.684242	79.076557	59.809626
2278.166388	81.485309	59.814631
2277.847342	79.325488	59.819636
2277.366203	77.606267	59.824641
2276.761691	81.243215	59.829645
2275.293317	86.337582	59.834650
2274.847367	82.806486	59.839655
2275.004927	79.300470	59.844660
2274.180101	86.375237	59.849665
2273.277999	86.627804	59.854669
2272.137374	83.280238	59.859674
2271.676173	89.730738	59.864679
2271.124985	79.017896	59.869684
2270.839271	83.542135	59.874689
2270.115025	79.839955	59.879693
2268.876523	81.284879	59.884698
2268.230413	78.412860	59.889703
2267.992194	86.235176	59.894708
2267.443277	85.234494	59.899713
2267.020728	79.847358	59.904718
2265.779106	84.023113	59.909722
2265.028749	86.745564	59.914727
2264.679291	84.555814	59.919732
2264.021481	83.295080	59.924737
2263.265001	71.545679	59.929742
2262.292867	79.705070	59.934746
2261.453308	84.859663	59.939751
2261.502378	82.237432	59.944756
2260.658374	77.913520	59.949761
2260.459149	70.863914	59.954766
2258.841487	79.509868	59.959770
2258.136332	74.846040	59.964775
2257.850422	75.968199	59.969780
2257.481487	78.657789	59.974785
2257.363815	80.382733	59.979790
2255.855310	78.233307	59.984794
2254.950562	79.138806	59.989799
2255.070633	75.892219	59.994804
2253.852008	75.829854	59.999809
2253.644363	68.654589	60.004814
2252.223923	72.909869	60.009818
2251.401682	78.243072	60.014823
2251.176948	74.910193	60.019828
2250.970080	80.346573	60.024833
2250.569942	72.602273	60.029838
2250.141669	77.892180	60.034842
2249.016889	83.099102	60.039847
2248.240497	81.988119	60.044852
2247.488378	77.998615	60.049857
2246.464527	80.636001	60.054862
2245.031400	83.112862	60.059866
2245.275193	71.267403	60.064871
2244.581312	75.543296	60.069876
2244.298885	81.148119	60.074881
2243.984301	75.555820	60.079886
2243.392473	84.702113	60.084890
2242.277799	86.658347	60.089895
2241.797039	80.284100	60.094900
2240.553574	80.447425	60.099905
2239.945289	77.003699	60.104910
2238.543915	83.091974	60.109914
2238.615691	83.598378	60.114919
2237.918658	74.607005	60.119924
2237.180483	81.578536	60.124929
2236.730909	82.862891	60.129934
2236.327630	86.653712	60.134938
2236.026965	82.532137	60.139943
2235.289882	68.400436	60.144948
2234.120980	85.459736	60.149953
2233.338165	67.173507	60.154958
2233.035152	74.968214	60.159962
2232.187095	76.328610	60.164967
2231.641610	70.121353	60.169972
2230.607011	72.389935	60.174977
2230.784450	77.219426	60.179982
2229.998236	87.374323	60.184986
2228.891445	84.963579	60.189991
2227.848788	81.789132	60.194996
2227.009931	84.405542	60.200001
2226.864208	82.366868	60.205006
2226.308661	84.536552	60.210010
2225.697080	80.805243	60.215015
2225.832477	76.280687	60.220020
2224.494667	85.045759	60.225025
2223.691696	76.687089	60.230030
2222.976806	91.266471	60.235034
2221.931414	82.151522	60.240039
2221.488696	85.913169	60.245044
2220.475252	88.153663	60.250049
2220.163590	81.032500	60.255054
2219.515518	89.328314	60.260058
2219.234415	81.227354	60.265063
2218.848282	76.849224	60.270068
2217.862347	85.667011	60.275073
2216.919509	89.106835	60.280078
2216.321457	93.135829	60.285082
2215.826959	81.411101	60.290087
2215.014252	82.995972	60.295092
2214.169425	81.528422	60.300097
2213.724826	81.519606	60.305102
2213.314038	81.925387	60.310106
2212.699030	89.286370	60.315111
2211.704248	76.779209	60.320116
2210.939794	86.997093	60.325121
2210.327345	82.304391	60.330126
2209.886829	85.689886	60.335130
2209.168758	82.468615	60.340135
2208.003639	83.901792	60.345140
2207.188878	89.053729	60.350145
2206.650690	86.411541	60.355150
2206.413308	90.809890	60.360154
2205.658518	89.254313	60.365159
2206.022746	80.742606	60.370164
2204.768578	90.503080	60.375169
2203.744883	86.199251	60.380174
2203.308069	89.022818	60.385178
2202.800478	83.650233	60.390183
2202.413270	82.735583	60.395188
2200.724291	85.396338	60.400193
2200.249286	79.056244	60.405198
2200.033657	82.609717	60.410202
2199.275823	82.218304	60.415207
2198.756209	70.841686	60.420212
2197.411184	77.369128	60.425217
2197.038410	81.189073	60.430222
2196.856097	86.717172	60.435226
2196.146687	84.066770	60.440231
2195.423582	75.014342	60.445236
2194.248492	83.900794	60.450241
2194.001884	75.633289	60.455246
2193.161724	82.557925	60.460250
2192.287278	78.209629	60.465255
2192.230014	74.797590	60.470260
2191.073643	90.937814	60.475265
2190.479162	86.841230	60.480270
2189.888280	84.022537	60.485274
2189.071406	87.385955	60.490279
2189.002762	82.007774	60.495284
2188.188541	84.679973	60.500289
2187.274795	77.822439	60.505294
2186.501280	84.488188	60.510298
2185.641946	85.820916	60.515303
2185.299908	81.446695	60.520308
2184.913879	81.959555	60.525313
2184.197066	83.541451	60.530318
2183.392877	79.718752	60.535322
2182.735929	85.035141	60.540327
2182.556496	82.571987	60.545332
2181.160721	79.681356	60.550337
2180.789434	83.808931	60.555342
2180.179330	86.249651	60.560346
2179.535414	87.724347	60.565351
2178.740378	83.762325	60.570356
2177.598236	84.139247	60.575361
2177.090531	79.773230	60.580366
2176.650368	87.440219	60.585370
2175.942741	84.634390	60.590375
2175.722789	76.298778	60.595380
2175.009815	84.437539	60.600385
2174.432249	85.508534	60.605390
2173.537018	87.251204	60.610394
2172.951788	88.269038	60.615399
2171.697636	80.422527	60.620404
2170.757965	84.597182	60.625409
2170.109979	80.371600	60.630414
2170.478137	80.068658	60.635418
2169.862548	80.739197	60.640423
2169.721759	82.799662	60.645428
2168.073217	86.150590	60.650433
2167.485987	84.550968	60.655438
2167.065102	77.710984	60.660442
2166.418964	71.516215	60.665447
2165.467365	66.407863	60.670452
2164.584129	74.760864	60.675457
2163.955730	77.281289	60.680462
2163.435568	68.827297	60.685466
2162.947216	79.854898	60.690471
2162.627490	77.315875	60.695476
2160.973836	86.073004	60.700481
2160.680666	83.179320	60.705486
2159.945958	74.730836	60.710490
2159.670377	88.143278	60.715495
2159.508447	77.348886	60.720500
2158.263402	84.204226	60.725505
2157.644017	82.824439	60.730510
2156.928593	76.622574	60.735514
2156.212417	85.422254	60.740519
2155.986737	73.564335	60.745524
2154.854896	76.127445	60.750529
2153.933729	76.624863	60.755534
2153.680032	78.530171	60.760538
2153.106150	75.090048	60.765543
2152.483031	70.154851	60.770548
2151.305592	71.736192	60.775553
2150.701920	79.486798	60.780558
2150.468933	77.250692	60.785562
2149.578037	80.133765	60.790567
2149.536098	70.216061	60.795572
2148.509499	78.382804	60.800577
2147.646673	80.890038	60.805582
2146.924233	82.944198	60.810586
2146.235322	76.423207	60.815591
2146.231230	77.076397	60.820596
2144.998011	77.572320	60.825601
2144.180496	83.415102	60.830606
2143.486328	83.659363	60.835610
2142.579153	82.649314	60.840615
2142.721906	73.779980	60.845620
2141.982254	78.603297	60.850625
2141.070892	77.951188	60.855630
2140.436069	79.544722	60.860634
2139.586232	81.878427	60.865639
2139.469099	80.221695	60.870644
2138.220677	86.153966	60.875649
2137.550146	73.954518	60.880654
2137.065876	82.705850	60.885658
2136.436178	79.471057	60.890663
2136.109227	80.329856	60.895668
2135.034450	86.158221	60.900673
2134.103600	84.859338	60.905678
2133.765418	80.536567	60.910682
2132.811833	88.736221	60.915687
2132.957169	82.991852	60.920692
2132.462695	86.636833	60.925697
2131.408156	81.604509	60.930702
2130.473003	82.638777	60.935706
2129.913794	82.436420	60.940711
2129.485105	76.447614	60.945716
2128.265254	83.109182	60.950721
2127.563760	76.066945	60.955726
2126.891646	70.133592	60.960730
2126.566500	87.973813	60.965735
2126.099063	75.717526	60.970740
2125.083273	87.793727	60.975745
2124.269624	78.669960	60.980750
2124.136818	75.169796	60.985754
2123.326511	85.703802	60.990759
2123.202707	76.181795	60.995764
2121.623534	78.757082	61.000769
2121.075006	80.643743	61.005774
2120.596385	75.711860	61.010778
2120.130311	78.509645	61.015783
2119.693518	75.758553	61.020788
2118.223817	77.648037	61.025793
2117.727436	81.890557	61.030798
2116.988726	81.949816	61.035802
2116.704254	87.371443	61.040807
2116.296688	70.895210	61.045812
2115.397859	77.371613	61.050817
2114.384486	73.879170	61.055822
2114.261029	78.993002	61.060826
2113.200274	75.835099	61.065831
2112.738849	73.480574	61.070836
2112.336988	83.459211	61.075841
2111.333427	89.351976	61.080846
2110.262141	80.703314	61.085850
2109.768566	76.594223	61.090855
2109.969690	74.047827	61.095860
2109.015597	84.249992	61.100865
2108.043746	80.690055	61.105870
2107.178015	73.942351	61.110874
2106.734772	82.063005	61.115879
2106.234336	82.043223	61.120884
2104.897357	84.419596	61.125889
2104.200125	82.961555	61.130894
2103.753017	85.604131	61.135898
2102.973929	80.648644	61.140903
2102.912950	78.937311	61.145908
2102.091717	75.859227	61.150913
2102.088850	77.655321	61.155918
2100.971677	80.925248	61.160922
2099.957223	76.432373	61.165927
2099.615286	77.569647	61.170932
2099.262885	80.707188	61.175937
2098.530294	79.300984	61.180942
2097.386159	84.078625	61.185946
2096.765553	83.553628	61.190951
2096.222988	84.697194	61.195956
2095.966964	80.117225	61.200961
2094.562228	81.481281	61.205966
2093.974252	70.421105	61.210970
2093.080697	80.732120	61.215975
2092.881659	73.669868	61.220980
2092.615799	80.679828	61.225985
2091.540946	81.648000	61.230990
2090.404656	69.742961	61.235994
2089.760101	80.586101	61.240999
2089.669033	71.161920	61.246004
2088.911373	76.521589	61.251009
2088.758855	70.276352	61.256014
2087.902274	81.477457	61.261018
2086.750185	84.954667	61.266023
2086.340337	73.009845	61.271028
2085.897801	78.754940	61.276033
2084.588095	79.155807	61.281038
2083.913458	73.145921	61.286042
2083.240474	81.810324	61.291047
2083.220083	74.025175	61.296052
2082.650687	75.211618	61.301057
2081.960228	69.934676	61.306062
2081.301253	71.641290	61.311066
2080.377122	75.955001	61.316071
2079.948885	68.966692	61.321076
2078.356918	73.569890	61.326081
2077.571771	74.711924	61.331086
2077.180993	65.579792	61.336090
2076.553354	74.920883	61.341095
2076.696640	76.674610	61.346100
2075.939421	69.456004	61.351105
2075.378789	75.541813	61.356110
2075.083035	71.903740	61.361114
2073.710803	79.421479	61.366119
2073.112060	79.266152	61.371124
2072.469554	85.635169	61.376129
2071.686669	80.145490	61.381134
2070.977653	78.338562	61.386138
2070.575508	81.021999	61.391143
2070.465808	78.862702	61.396148
2069.073663	76.664220	61.401153
2068.394860	79.644443	61.406158
2067.655799	79.472856	61.411162
2067.184487	90.486099	61.416167
2066.691453	72.037466	61.421172
2065.250270	83.914861	61.426177
2064.253305	79.380320	61.431182
2064.132985	78.492265	61.436186
2063.420140	77.506620	61.441191
2063.130802	65.067924	61.446196
2062.821987	79.628752	61.451201
2062.602875	70.953554	61.456206
2061.318048	75.540534	61.461210
2060.147143	76.424093	61.466215
2060.100098	68.525486	61.471220
2059.664223	78.365863	61.476225
2058.314408	79.871317	61.481230
2057.504103	77.540554	61.486234
2056.862055	90.748050	61.491239
2056.427095	79.933271	61.496244
2056.290581	74.914856	61.501249
2055.625572	75.045987	61.506254
2054.631607	77.464747	61.511258
2053.433108	79.072210	61.516263
2053.180117	74.603829	61.521268
2053.120272	74.357511	61.526273
2051.987542	74.500753	61.531278
2051.364255	78.588543	61.536282
2050.942675	73.198511	61.541287
2050.192778	75.939852	61.546292
2048.788573	79.525716	61.551297
2048.165274	76.438258	61.556302
2048.100379	74.451292	61.561306
2047.139533	79.964532	61.566311
2047.268770	65.955483	61.571316
2045.782239	77.834712	61.576321
2045.340538	74.276078	61.581326
2044.467169	74.759417	61.586330
2043.687792	78.551024	61.591335
2042.990459	65.680823	61.596340
2042.680574	78.751758	61.601345
2041.984204	79.413630	61.606350
2041.059144	70.846162	61.611354
2040.700454	80.032704	61.616359
2040.334909	75.388980	61.621364
2039.641348	75.856562	61.626369
2038.859516	71.490485	61.631374
2038.458875	67.300381	61.636378
2037.342026	71.054190	61.641383
2036.925128	71.737334	61.646388
2035.761673	74.279032	61.651393
2035.084939	75.194509	61.656398
2034.826557	73.423791	61.661402
2033.839841	68.103195	61.666407
2033.644684	72.752858	61.671412
2033.068911	74.431035	61.676417
2032.368619	66.915740	61.681422
2031.837247	76.406149	61.686426
2030.757180	71.705839	61.691431
2029.375778	65.823572	61.696436
2028.443743	69.052762	61.701441
2028.825569	65.764169	61.706446
2028.175495	65.685915	61.711450
2026.649891	69.691216	61.716455
2026.532691	63.547311	61.721460
2026.283832	65.344824	61.726465
2025.818712	73.934591	61.731470
2025.679236	65.338933	61.736474
2024.619905	69.606700	61.741479
2023.582803	67.899716	61.746484
2023.250740	78.986627	61.751489
2022.213991	72.950277	61.756494
2021.358035	71.913332	61.761498
2020.826197	79.808753	61.766503
2020.286354	64.523554	61.771508
2019.752173	77.186818	61.776513
2019.034760	70.580734	61.781518
2018.153058	67.515774	61.786522
2017.740989	68.802411	61.791527
2016.874522	68.336059	61.796532
2015.261190	74.611414	61.801537
2015.329930	70.843895	61.806542
2014.674949	75.840231	61.811546
2014.034813	70.252731	61.816551
2013.401490	65.683237	61.821556
2013.205467	72.729796	61.826561
2012.671434	75.561711	61.831566
2011.948235	64.724812	61.836570
2011.080790	71.206116	61.841575
2010.405450	68.200986	61.846580
2010.098913	72.715365	61.851585
2009.266013	74.565023	61.856590
2008.391892	69.962907	61.861594
2007.496177	78.649622	61.866599
2006.940600	69.851599	61.871604
2005.804349	68.137896	61.876609
2005.359932	75.316546	61.881614
2004.809504	73.626575	61.886618
2004.097285	70.413815	61.891623
2003.750693	72.954729	61.896628
2002.938727	77.060587	61.901633
2002.666169	77.725359	61.906638
2002.341644	72.261891	61.911642
2001.111408	77.190453	61.916647
2000.610364	66.936056	61.921652
1999.804064	69.765994	61.926657
1998.303837	74.700084	61.931662
1997.629768	69.352461	61.936666
1997.530752	74.147514	61.941671
1996.981972	77.688899	61.946676
1996.480360	75.681906	61.951681
1996.183784	76.878529	61.956686
1995.773839	70.728255	61.961690
1994.440562	80.583199	61.966695
1993.729602	78.356238	61.971700
1993.394240	80.753133	61.976705
1992.811340	71.634930	61.981710
1991.760359	68.874053	61.986714
1990.473667	70.374646	61.991719
1990.673247	76.373834	61.996724
1989.953022	74.197799	62.001729
1989.217961	72.318370	62.006734
1988.135766	73.318210	62.011738
1987.273428	81.862251	62.016743
1986.906897	73.202411	62.021748
1986.523491	76.670509	62.026753
1985.953786	74.798319	62.031758
1985.898493	74.004534	62.036762
1984.576745	80.989463	62.041767
1983.847071	65.392154	62.046772
1983.455539	75.433354	62.051777
1982.802247	73.179163	62.056782
1982.187025	68.145543	62.061786
1981.049570	77.712790	62.066791
1980.474803	78.516887	62.071796
1980.081328	76.289300	62.076801
1979.537463	76.104466	62.081806
1978.546811	71.032441	62.086810
1977.731444	80.374072	62.091815
1977.390739	66.053463	62.096820
1977.156617	70.315464	62.101825
1975.725205	79.429728	62.106830
1974.886611	72.244800	62.111834
1974.290480	80.589361	62.116839
1973.801765	78.159786	62.121844
1973.680135	67.928512	62.126849
1973.019219	79.625864	62.131854
1971.956705	75.560435	62.136858
1970.861661	78.528979	62.141863
1970.537646	70.596447	62.146868
1970.583685	78.043685	62.151873
1969.436410	76.282140	62.156878
1968.525282	74.515330	62.161882
1967.642845	83.528187	62.166887
1967.444887	68.558710	62.171892
1966.932019	63.402195	62.176897
1966.300462	83.844703	62.181902
1965.401959	77.463414	62.186906
1964.862926	85.242442	62.191911
1964.598250	75.425226	62.196916
1963.824751	81.010239	62.201921
1962.146886	78.069643	62.206926
1961.822662	76.063097	62.211930
1961.326283	77.522445	62.216935
1961.068505	75.963198	62.221940
1960.408340	76.630333	62.226945
1959.066106	75.093187	62.231950
1958.639919	75.865159	62.236954
1957.859031	79.081136	62.241959
1957.822840	75.020528	62.246964
1957.239554	77.018143	62.251969
1956.094918	78.830745	62.256974
1955.624147	76.648751	62.261978
1954.841294	87.555816	62.266983
1954.201068	72.780017	62.271988
1953.194639	70.525059	62.276993
1952.039713	75.253648	62.281998
1952.081950	71.373433	62.287002
1951.144909	81.307042	62.292007
1951.115509	71.736939	62.297012
1950.613421	75.978073	62.302017
1949.879651	77.476058	62.307022
1949.388756	70.188632	62.312026
1948.224754	75.428359	62.317031
1948.000182	65.519031	62.322036
1946.530570	73.587900	62.327041
1945.636680	71.451450	62.332046
1945.319810	70.408741	62.337050
1944.523551	78.945031	62.342055
1944.726582	80.286311	62.347060
1944.587003	72.104344	62.352065
1943.270790	76.808029	62.357070
1942.381860	76.247640	62.362074
1941.758042	78.610598	62.367079
1940.597701	74.893478	62.372084
1939.773553	78.197380	62.377089
1939.598371	80.007160	62.382094
1939.105334	66.697054	62.387098
1938.590288	82.848353	62.392103
1937.926037	71.369435	62.397108
1936.665857	77.700838	62.402113
1935.758526	73.173889	62.407118
1935.270396	70.656986	62.412122
1934.828170	76.141120	62.417127
1934.716695	74.848941	62.422132
1934.359161	76.918460	62.427137
1932.916394	90.049784	62.432142
1932.288618	72.634727	62.437146
1931.628392	90.221997	62.442151
1931.086002	80.243879	62.447156
1930.355748	76.367136	62.452161
1929.202654	82.743378	62.457166
1928.870172	78.926872	62.462170
1928.035307	88.427366	62.467175
1927.903023	80.867809	62.472180
1927.746070	78.953829	62.477185
1926.357643	78.065621	62.482190
1925.835243	79.266933	62.487194
1924.952008	82.425032	62.492199
1924.663531	84.877065	62.497204
1924.322825	80.177790	62.502209
1922.751290	82.845767	62.507214
1922.333272	76.059408	62.512218
1921.149279	78.573460	62.517223
1921.226190	75.326761	62.522228
1920.725262	80.359905	62.527233
1919.930686	78.974596	62.532238
1918.857988	79.060230	62.537242
1918.387026	87.345095	62.542247
1917.887242	78.758189	62.547252
1917.763684	78.629742	62.552257
1916.500188	81.932628	62.557262
1916.146882	77.811408	62.562266
1915.277709	75.758757	62.567271
1914.834839	77.998790	62.572276
1913.748686	76.417058	62.577281
1912.909737	80.308077	62.582286
1912.868433	74.782353	62.587290
1912.014984	80.738270	62.592295
1911.331935	76.113354	62.597300
1910.377735	80.624066	62.602305
1909.612334	80.102154	62.607310
1909.292539	77.350410	62.612314
1908.608262	72.172701	62.617319
1908.332373	78.171911	62.622324
1907.136659	67.985061	62.627329
1905.996445	80.879891	62.632334
1905.867386	76.227697	62.637338
1905.463100	76.536471	62.642343
1904.818935	80.936910	62.647348
1904.208737	73.375044	62.652353
1902.661893	78.626988	62.657358
1902.341491	70.742793	62.662362
1901.889519	80.345536	62.667367
1901.585900	73.500138	62.672372
1901.190127	77.110875	62.677377
1900.104242	75.971187	62.682382
1899.336295	71.925644	62.687386
1898.429527	75.235790	62.692391
1898.378424	72.178750	62.697396
1897.322932	81.829876	62.702401
1896.363467	72.330870	62.707406
1895.803516	77.946458	62.712410
1895.320522	79.217607	62.717415
1894.897682	76.998605	62.722420
1894.743779	72.045149	62.727425
1893.252178	80.067664	62.732430
1892.739263	72.702701	62.737434
1891.855281	78.766471	62.742439
1891.565731	76.851101	62.747444
1890.695130	73.978863	62.752449
1889.754303	77.403781	62.757454
1889.132109	71.339569	62.762458
1888.750911	80.664161	62.767463
1888.425161	64.896731	62.772468
1887.864293	68.619787	62.777473
1886.311227	77.838558	62.782478
1886.252793	72.621281	62.787482
1885.328265	69.999445	62.792487
1884.964910	59.908619	62.797492
1884.501506	73.866686	62.802497
1883.493270	66.012544	62.807502
1882.860725	65.304887	62.812506
1882.025630	75.380128	62.817511
1881.785557	66.663940	62.822516
1880.404191	62.471121	62.827521
1879.612663	75.663517	62.832526
1879.345437	72.890152	62.837530
1878.737018	71.416952	62.842535
1878.474490	64.684526	62.847540
1878.087869	72.062095	62.852545
1876.975880	71.427385	62.857550
1876.222284	69.654956	62.862554
1875.306000	77.842325	62.867559
1874.934363	71.427762	62.872564
1874.470795	67.625007	62.877569
1873.394813	75.182881	62.882574
1872.614463	60.721604	62.887578
1872.101038	70.641552	62.892583
1871.749871	72.631434	62.897588
1871.032202	81.355592	62.902593
1870.548342	81.284051	62.907598
1869.947457	70.624803	62.912602
1868.815675	78.689574	62.917607
1868.270112	72.340292	62.922612
1867.808453	67.531858	62.927617
1866.595964	77.084717	62.932622
1866.234090	71.684496	62.937626
1865.686380	77.015370	62.942631
1864.988483	72.325506	62.947636
1864.749995	65.691596	62.952641
1863.342611	67.285494	62.957646
1863.268296	66.723509	62.962650
1862.087557	65.114553	62.967655
1861.909580	70.944251	62.972660
1861.777525	74.198041	62.977665
1860.673671	79.106191	62.982670
1860.094701	67.737832	62.987674
1858.899666	69.776171	62.992679
1857.816617	81.055502	62.997684
1857.214553	73.620932	63.002689
1856.681639	72.351123	63.007694
1856.470761	78.520387	63.012698
1856.294317	86.972354	63.017703
1855.298226	70.738977	63.022708
1854.234106	71.332742	63.027713
1853.145956	67.564218	63.032718
1853.097746	73.980770	63.037722
1852.782263	65.489453	63.042727
1852.382062	67.548906	63.047732
1851.380813	71.139686	63.052737
1850.300796	71.418421	63.057742
1849.745880	74.467858	63.062746
1849.455110	72.396785	63.067751
1848.311548	79.240335	63.072756
1847.591048	71.835899	63.077761
1846.657688	76.898821	63.082766
1846.483850	77.289351	63.087770
1846.070077	80.836858	63.092775
1845.414337	69.101914	63.097780
1844.757379	74.103336	63.102785
1843.230392	69.268757	63.107790
1843.041641	75.267267	63.112794
1842.583975	75.182957	63.117799
1841.950742	73.056797	63.122804
1841.786730	66.413305	63.127809
1840.457396	67.654396	63.132814
1839.867617	68.956449	63.137818
1839.278040	71.899322	63.142823
1838.587265	73.071030	63.147828
1838.147156	71.807450	63.152833
1837.037453	69.202701	63.157838
1837.024713	66.057394	63.162842
1836.320202	71.467987	63.167847
1834.716193	73.809978	63.172852
1834.483419	70.956121	63.177857
1833.395290	81.125579	63.182862
1833.249663	72.286266	63.187866
1833.085088	76.823331	63.192871
1832.290352	67.182878	63.197876
1831.310006	74.216390	63.202881
1830.176257	78.008257	63.207886
1829.957070	69.181927	63.212890
1829.379955	76.669849	63.217895
1828.939962	80.480384	63.222900
1828.108322	76.743370	63.227905
1826.635153	83.934622	63.232910
1826.755254	77.486060	63.237914
1826.228968	82.041988	63.242919
1825.669069	81.868597	63.247924
1824.872946	70.818438	63.252929
1823.722533	71.967345	63.257934
1823.257383	67.112543	63.262938
1823.041459	73.418845	63.267943
1822.518865	75.590817	63.272948
1821.622863	73.547905	63.277953
1820.464073	69.459516	63.282958
1820.402167	61.569004	63.287962
1819.218221	69.759539	63.292967
1818.096327	69.534677	63.297972
1817.480004	78.439646	63.302977
1816.737767	85.261510	63.307982
1816.928836	69.043709	63.312986
1816.636587	73.660246	63.317991
1815.975774	71.144088	63.322996
1815.534754	67.902328	63.328001
1814.017382	74.546954	63.333006
1813.589847	69.285075	63.338010
1813.059394	70.826049	63.343015
1811.866120	74.654155	63.348020
1811.310018	66.447555	63.353025
1810.139348	75.643149	63.358030
1810.224695	68.445832	63.363034
1809.758548	73.889458	63.368039
1809.264770	72.421914	63.373044
1808.509938	66.786185	63.378049
1807.681975	73.188915	63.383054
1807.205265	62.248716	63.388058
1805.963223	71.346392	63.393063
1804.880296	77.968398	63.398068
1804.432684	68.818801	63.403073
1803.853138	69.267695	63.408078
1803.410842	67.680822	63.413082
1803.005546	75.273158	63.418087
1802.545095	69.202604	63.423092
1802.415698	61.938616	63.428097
1800.776249	67.818241	63.433102
1800.090260	68.143643	63.438106
1799.654999	72.614130	63.443111
1799.203872	73.097103	63.448116
1798.240654	63.296812	63.453121
1797.457984	77.906319	63.458126
1796.936987	73.198042	63.463130
1796.457406	69.643552	63.468135
1795.515817	76.558336	63.473140
1794.601937	66.894465	63.478145
1793.859503	76.054289	63.483150
1793.777890	65.155828	63.488154
1793.073014	65.056981	63.493159
1792.768205	74.037326	63.498164
1792.305590	64.610443	63.503169
1791.083967	75.679022	63.508174
1790.144832	69.088423	63.513178
1789.750337	62.582264	63.518183
1789.047222	69.424666	63.523188
1788.450745	67.411431	63.528193
1787.446526	79.051867	63.533198
1787.002963	66.460013	63.538202
1786.357046	75.465566	63.543207
1785.811840	68.336272	63.548212
1785.080822	65.063611	63.553217
1783.881761	67.294094	63.558222
1783.768025	70.212394	63.563226
1783.500912	70.065488	63.568231
1782.715396	64.005559	63.573236
1782.118080	71.018931	63.578241
1781.067220	74.880304	63.583246
1780.566591	70.440902	63.588250
1779.905472	69.714859	63.593255
1778.767497	72.496579	63.598260
1778.200867	70.241011	63.603265
1777.670699	73.160303	63.608270
1777.396126	65.160530	63.613274
1776.876508	63.462948	63.618279
1775.721547	71.789051	63.623284
1775.300136	71.455791	63.628289
1774.342202	71.590500	63.633294
1774.085032	65.659242	63.638298
1773.474253	74.509183	63.643303
1771.788521	73.822276	63.648308
1771.522490	66.480224	63.653313
1771.003073	76.028978	63.658318
1771.032032	70.572950	63.663322
1770.439514	77.812073	63.668327
1769.292723	71.393977	63.673332
1768.942206	66.827055	63.678337
1767.920704	81.032975	63.683342
1767.265944	72.682215	63.688346
1766.063213	70.051166	63.693351
1765.216586	77.438370	63.698356
1765.087557	68.402814	63.703361
1764.334909	78.616319	63.708366
1764.143177	74.490365	63.713370
1763.758961	69.278710	63.718375
1762.818935	64.771606	63.723380
1762.043172	62.548272	63.728385
1761.094799	74.221386	63.733390
1760.745485	59.564819	63.738394
1760.356744	70.114719	63.743399
1758.798798	74.456791	63.748404
1758.612649	66.854768	63.753409
1757.610511	71.621190	63.758414
1757.608226	62.429748	63.763418
1756.931640	71.959209	63.768423
1756.098554	75.024672	63.773428
1755.235474	67.415717	63.778433
1754.749844	79.053866	63.783438
1754.417866	67.992203	63.788442
1753.603236	71.375021	63.793447
1752.344806	72.643473	63.798452
1751.902568	70.787791	63.803457
1751.207661	71.392214	63.808462
1750.964430	71.238854	63.813466
1750.424076	70.542676	63.818471
1749.369298	66.419930	63.823476
1748.831823	67.230695	63.828481
1747.891895	66.855902	63.833486
1747.730490	56.149520	63.838490
1746.644031	60.708931	63.843495
1745.817614	75.654723	63.848500
1745.580921	70.902544	63.853505
1744.578850	72.883417	63.858510
1744.481756	66.552945	63.863514
1743.599364	71.750440	63.868519
1742.346140	72.873931	63.873524
1741.816677	67.076105	63.878529
1741.232672	76.518284	63.883534
1741.107289	69.707541	63.888538
1740.480626	73.675540	63.893543
1739.811047	75.956349	63.898548
1738.917956	73.097069	63.903553
1737.952979	68.579634	63.908558
1737.832756	75.182178	63.913562
1736.864423	73.050611	63.918567
1735.884487	69.178735	63.923572
1735.617389	65.756836	63.928577
1735.063979	75.894013	63.933582
1734.554286	69.122189	63.938586
1733.499313	76.750693	63.943591
1732.444861	77.292303	63.948596
1731.826140	69.392078	63.953601
1731.515431	76.706529	63.958606
1731.532010	76.779098	63.963610
1730.540114	74.373286	63.968615
1729.352979	69.172318	63.973620
1729.010132	66.158102	63.978625
1728.234828	73.357846	63.983630
1728.196107	67.059228	63.988634
1726.892541	68.000686	63.993639
1726.142254	77.657627	63.998644
1725.346844	68.279016	64.003649
1725.168040	69.290504	64.008654
1724.416580	65.372432	64.013658
1723.291700	74.052986	64.018663
1722.595153	71.644005	64.023668
1722.266606	63.072843	64.028673
1721.681127	69.503558	64.033678
1721.443561	63.776180	64.038682
1720.474381	65.806294	64.043687
1719.704508	67.862698	64.048692
1719.024720	66.683561	64.053697
1718.541145	63.865919	64.058702
1717.813568	64.795659	64.063706
1716.934855	71.967311	64.068711
1716.339573	76.134408	64.073716
1715.876515	54.935887	64.078721
1715.447771	70.445178	64.083726
1714.468676	66.643424	64.088730
1713.463654	75.693848	64.093735
1712.845873	76.370338	64.098740
1712.759103	67.764909	64.103745
1711.707818	72.256339	64.108750
1710.854635	65.327384	64.113754
1709.972508	69.312257	64.118759
1709.096946	72.977863	64.123764
1708.749561	62.261860	64.128769
1708.540508	76.424279	64.133774
1708.407121	67.141988	64.138778
1707.711617	70.474033	64.143783
1706.720742	73.384142	64.148788
1706.138470	66.053977	64.153793
1705.123292	68.205250	64.158798
1704.318515	69.397271	64.163802
1703.537267	73.750920	64.168807
1703.129584	76.958325	64.173812
1702.837030	77.655346	64.178817
1702.041568	74.813312	64.183822
1701.126647	72.279077	64.188826
1700.233105	72.083058	64.193831
1699.609347	80.264991	64.198836
1699.247150	73.261098	64.203841
1698.589416	77.708082	64.208846
1698.284875	72.607533	64.213850
1696.927253	65.543855	64.218855
1696.173944	74.747384	64.223860
1695.889756	64.078988	64.228865
1695.248615	76.832775	64.233870
1694.942396	71.655148	64.238874
1693.899950	69.049188	64.243879
1692.910535	73.983568	64.248884
1692.823067	63.216381	64.253889
1692.115168	74.380212	64.258894
1691.472731	71.251087	64.263898
1690.303821	67.393796	64.268903
1690.043275	72.738298	64.273908
1689.123914	72.695509	64.278913
1688.674252	77.062285	64.283918
1688.521530	70.744099	64.288922
1687.509342	72.107002	64.293927
1686.403318	68.602489	64.298932
1686.317486	64.577628	64.303937
1685.766876	73.884623	64.308942
1684.584973	71.903293	64.313946
1683.877228	66.349528	64.318951
1683.009491	60.850774	64.323956
1682.781926	57.994066	64.328961
1682.368318	72.429102	64.333966
1681.272732	67.262218	64.338970
1680.520888	66.824070	64.343975
1679.778301	71.885942	64.348980
1679.785668	57.373220	64.353985
1679.045399	59.897041	64.358990
1677.809534	65.773948	64.363994
1677.132474	62.228401	64.368999
1676.479453	67.818080	64.374004
1676.251804	63.685652	64.379009
1675.699494	66.317830	64.384014
1674.785326	63.039821	64.389018
1673.604392	61.272267	64.394023
1672.706681	68.766501	64.399028
1672.565773	56.894962	64.404033
1671.824382	65.325954	64.409038
1672.042458	66.501625	64.414042
1671.653871	62.340686	64.419047
1670.694976	68.782805	64.424052
1670.030205	59.631321	64.429057
1668.282146	68.669165	64.434062
1667.848554	62.102218	64.439066
1667.591048	58.443038	64.444071
1666.563353	68.398092	64.449076
1666.346448	60.212424	64.454081
1665.846889	65.169553	64.459086
1664.851505	60.699971	64.464090
1663.505683	58.723804	64.469095
1662.884485	64.423690	64.474100
1662.824433	62.660505	64.479105
1662.187493	59.601890	64.484110
1661.948719	63.541804	64.489114
1661.786238	60.363315	64.494119
1660.445996	69.848852	64.499124
1659.744274	68.687687	64.504129
1658.724667	62.412856	64.509134
1658.040013	59.365564	64.514138
1657.536097	55.317914	64.519143
1656.532027	70.988018	64.524148
1656.404463	55.245156	64.529153
1655.787154	68.871925	64.534158
1655.283934	63.132780	64.539162
1654.502471	70.588571	64.544167
1653.437977	69.768159	64.549172
1653.117497	62.620171	64.554177
1652.580446	70.525958	64.559182
1651.675121	66.470816	64.564186
1651.496085	55.411429	64.569191
1650.786581	63.263043	64.574196
1649.870516	60.217854	64.579201
1648.554795	66.870635	64.584206
1648.471518	69.791616	64.589210
1648.036826	64.274813	64.594215
1646.642526	72.525843	64.599220
1645.875620	62.104265	64.604225
1645.220878	62.140932	64.609230
1644.905175	59.011953	64.614234
1644.716607	60.183791	64.619239
1643.739907	64.957716	64.624244
1643.735955	60.563205	64.629249
1642.630863	69.054861	64.634254
1641.167315	66.471636	64.639258
1641.119274	65.513597	64.644263
1640.391601	65.512221	64.649268
1639.960966	66.526150	64.654273
1638.607534	63.421999	64.659278
1637.986833	56.654589	64.664282
1637.756021	62.883301	64.669287
1637.110866	68.523346	64.674292
1636.926048	59.659589	64.679297
1635.986702	68.353398	64.684302
1634.672169	55.249874	64.689306
1634.258842	56.205186	64.694311
1633.545211	68.791379	64.699316
1633.357525	62.784303	64.704321
1633.127199	56.041664	64.709326
1632.313994	60.130797	64.714330
1631.456262	71.761959	64.719335
1630.663969	65.715065	64.724340
1629.780981	53.396604	64.729345
1628.781934	53.640213	64.734350
1627.958724	57.277921	64.739354
1627.339130	54.182004	64.744359
1627.235094	67.679094	64.749364
1627.272616	56.896846	64.754369
1626.348308	56.132973	64.759374
1625.453060	62.098039	64.764378
1625.093392	60.293764	64.769383
1624.116733	61.284299	64.774388
1623.003772	52.135322	64.779393
1622.136731	65.976133	64.784398
1621.599222	67.477280	64.789402
1621.441966	60.759239	64.794407
1620.744412	65.467635	64.799412
1620.234495	54.867096	64.804417
1619.152338	71.489602	64.809422
1618.404028	61.955731	64.814426
1618.274934	66.151601	64.819431
1617.445294	66.228859	64.824436
1616.477106	57.111550	64.829441
1615.636150	66.749664	64.834446
1614.858254	60.932011	64.839450
1614.620815	59.546143	64.844455
1613.970013	63.316579	64.849460
1613.562558	59.969631	64.854465
1612.909898	63.126202	64.859470
1611.896142	67.531095	64.864474
1611.437122	68.378576	64.869479
1610.931830	65.679132	64.874484
1610.543095	63.393539	64.879489
1609.216944	61.523753	64.884494
1608.465337	66.501520	64.889498
1608.098247	58.962455	64.894503
1607.546084	63.193226	64.899508
1607.144912	59.903228	64.904513
1605.769974	58.172049	64.909518
1605.074775	63.581458	64.914522
1604.634126	52.357650	64.919527
1603.790163	68.330733	64.924532
1603.834294	51.528680	64.929537
1602.909253	60.254380	64.934542
1601.986359	61.754378	64.939546
1601.726869	49.058845	64.944551
1600.956889	68.384641	64.949556
1600.094421	59.008861	64.954561
1599.427014	58.157213	64.959566
1598.903812	63.978879	64.964570
1598.436767	55.823004	64.969575
1597.456638	72.586334	64.974580
1596.512747	60.711702	64.979585
1595.788427	57.875674	64.984590
1595.102694	60.958173	64.989594
1595.329175	57.018023	64.994599
1594.609015	59.420391	64.999604
1593.799400	52.345863	65.004609
1592.879396	62.565109	65.009614
1592.317682	62.690067	65.014618
1591.709128	52.379957	65.019623
1590.867594	60.033125	65.024628
1589.642087	54.234454	65.029633
1589.230992	58.485292	65.034638
1588.523401	53.655045	65.039642
1588.498615	58.368300	65.044647
1588.014697	64.103115	65.049652
1587.294920	58.756686	65.054657
1586.223184	50.606806	65.059662
1585.373842	63.462525	65.064666
1585.656716	59.908627	65.069671
1583.905474	58.347639	65.074676
1583.240681	57.947895	65.079681
1582.653767	60.162074	65.084686
1581.954466	55.961170	65.089690
1582.100722	63.585416	65.094695
1581.172724	67.299089	65.099700
1580.916917	56.907295	65.104705
1579.753597	55.072016	65.109710
1579.235927	66.370649	65.114714
1578.542353	58.945092	65.119719
1576.914397	61.423483	65.124724
1576.801913	59.684274	65.129729
1575.988208	68.419741	65.134734
1575.537353	66.220568	65.139738
1575.565184	61.524976	65.144743
1574.855809	67.315350	65.149748
1573.701676	58.344345	65.154753
1573.142966	63.620271	65.159758
1572.280205	69.024810	65.164762
1572.140583	61.427480	65.169767
1570.848755	60.605730	65.174772
1570.215324	61.677265	65.179777
1569.952320	63.344980	65.184782
1568.896519	64.066056	65.189786
1568.801751	59.708011	65.194791
1567.686770	64.952829	65.199796
1566.967341	59.685287	65.204801
1566.384992	53.304074	65.209806
1565.757345	63.408949	65.214810
1565.577694	67.672678	65.219815
1563.775227	55.186349	65.224820
1563.491677	56.771532	65.229825
1562.963681	65.181798	65.234830
1562.375679	70.111834	65.239834
1562.381741	64.870123	65.244839
1561.508083	74.175961	65.249844
1560.525095	63.813885	65.254849
1559.815255	66.458034	65.259854
1558.913416	70.373277	65.264858
1559.134787	60.435847	65.269863
1557.974365	66.879311	65.274868
1557.159522	59.386096	65.279873
1556.815987	65.292273	65.284878
1555.974056	65.524795	65.289882
1555.168875	59.806163	65.294887
1554.188175	71.051812	65.299892
1553.440123	60.943993	65.304897
1553.288493	62.211744	65.309902
1552.180978	58.527135	65.314906
1552.386725	54.336336	65.319911
1551.371001	66.243209	65.324916
1550.644982	56.576076	65.329921
1550.085981	65.245453	65.334926
1549.182488	66.144536	65.339930
1549.283298	51.806497	65.344935
1548.058651	60.856228	65.349940
1547.295188	63.815068	65.354945
1547.178845	57.731453	65.359950
1546.049670	62.504645	65.364954
1545.274929	64.510984	65.369959
1544.324829	64.752942	65.374964
1543.522436	60.056553	65.379969
1543.473108	68.721989	65.384974
1542.507894	61.584892	65.389978
1542.134443	49.629236	65.394983
1541.194099	63.164053	65.399988
1540.490487	55.474578	65.404993
1540.151750	59.729612	65.409998
1539.746559	61.398769	65.415002
1539.241840	61.037553	65.420007
1537.771320	59.010135	65.425012
1537.063239	59.423033	65.430017
1536.800250	55.484553	65.435022
1535.955168	58.873001	65.440026
1535.243475	68.667410	65.445031
1534.408721	68.515830	65.450036
1533.934347	67.211568	65.455041
1533.593394	61.474670	65.460046
1532.800706	69.446315	65.465050
1532.644836	68.280164	65.470055
1531.175892	70.425448	65.475060
1530.487841	65.143858	65.480065
1530.200437	68.628696	65.485070
1529.797100	65.765373	65.490074
1529.293904	61.824190	65.495079
1527.797620	60.969947	65.500084
1527.657516	63.908545	65.505089
1527.112132	66.750724	65.510094
1526.165043	62.109102	65.515098
1525.269055	58.314485	65.520103
1524.466336	63.144303	65.525108
1524.166932	71.800042	65.530113
1523.433923	60.751803	65.535118
1523.096644	70.781330	65.540122
1522.607066	52.817795	65.545127
1521.455365	62.668956	65.550132
1521.048383	60.349787	65.555137
1520.891455	56.378157	65.560142
1519.174128	58.113606	65.565146
1518.705424	60.474525	65.570151
1517.981404	62.593365	65.575156
1517.834424	51.287737	65.580161
1516.993449	55.511497	65.585166
1515.834230	58.734643	65.590170
1515.087862	51.601943	65.595175
1514.250264	61.631835	65.600180
1514.023074	61.491925	65.605185
1513.612723	59.820277	65.610190
1513.310745	66.384443	65.615194
1512.688032	55.070634	65.620199
1511.617206	60.153172	65.625204
1510.913013	56.140610	65.630209
1510.710309	51.375143	65.635214
1509.736539	56.231473	65.640218
1509.269939	47.424257	65.645223
1508.407790	65.072476	65.650228
1507.811109	52.339147	65.655233
1507.410934	50.655891	65.660238
1506.106362	64.054900	65.665242
1505.566122	47.975356	65.670247
1504.781206	52.872781	65.675252
1504.449560	61.222993	65.680257
1504.041749	57.289567	65.685262
1502.810942	56.096619	65.690266
1501.770801	55.154446	65.695271
1501.566504	53.382404	65.700276
1500.994569	56.049136	65.705281
1500.765537	55.049845	65.710286
1500.141115	63.046766	65.715290
1499.221236	56.878853	65.720295
1498.269887	57.556803	65.725300
1497.949339	49.977032	65.730305
1497.160947	58.413706	65.735310
1496.103757	65.665262	65.740314
1496.332494	59.820996	65.745319
1495.203451	67.055642	65.750324
1494.627658	55.992742	65.755329
1493.183505	57.729995	65.760334
1492.359140	54.915055	65.765338
1492.599286	60.941583	65.770343
1491.622272	57.725290	65.775348
1491.271219	51.199114	65.780353
1490.992084	53.582059	65.785358
1490.067429	64.704042	65.790362
1489.123686	56.552806	65.795367
1488.263403	50.092869	65.800372
1487.633688	55.543179	65.805377
1487.568306	52.535575	65.810382
1486.739299	56.450200	65.815386
1485.498339	43.490068	65.820391
1485.084674	54.465376	65.825396
1484.989939	46.078443	65.830401
1484.463437	52.652612	65.835406
1483.122304	63.611415	65.840410
1482.782542	58.362983	65.845415
1481.978319	52.112915	65.850420
1481.379375	56.901937	65.855425
1480.621739	58.010529	65.860430
1479.429938	62.395391	65.865434
1479.438506	49.800835	65.870439
1478.930235	53.778585	65.875444
1477.424511	59.408042	65.880449
1476.788991	60.708487	65.885454
1476.235012	56.200505	65.890458
1475.762263	54.014566	65.895463
1475.626501	62.697945	65.900468
1475.038668	48.482523	65.905473
1474.830730	51.010775	65.910478
1473.554315	52.508147	65.915482
1473.158792	50.147156	65.920487
1471.970616	49.979898	65.925492
1470.513217	57.307058	65.930497
1470.307308	49.987920	65.935502
1469.835379	50.326066	65.940506
1469.210414	53.095820	65.945511
1468.287979	50.067552	65.950516
1468.439074	46.342403	65.955521
1468.113254	47.305643	65.960526
1466.811260	55.955351	65.965530
1466.384856	46.678653	65.970535
1465.530467	50.921293	65.975540
1464.523560	48.351542	65.980545
1463.688257	46.417125	65.985550
1463.053100	55.435833	65.990554
1462.533692	57.463607	65.995559
1462.112901	60.621160	66.000564
1461.603976	53.873731	66.005569
1461.003732	46.318947	66.010574
1459.892901	56.665198	66.015578
1459.243277	46.758450	66.020583
1458.773146	57.808948	66.025588
1458.321349	54.142782	66.030593
1457.779123	51.309162	66.035598
1456.609919	57.306926	66.040602
1456.349646	47.249066	66.045607
1455.524172	47.585756	66.050612
1454.929106	56.952849	66.055617
1453.942259	48.642039	66.060622
1453.294524	57.008458	66.065626
1452.819573	46.752091	66.070631
1452.149461	50.424005	66.075636
1451.798611	49.893574	66.080641
1451.274278	54.231689	66.085646
1449.969634	53.716098	66.090650
1449.675862	48.205209	66.095655
1448.535756	50.733154	66.100660
1448.472130	52.282670	66.105665
1447.737523	53.785201	66.110670
1447.001554	55.841360	66.115674
1446.636126	43.381089	66.120679
1445.810856	64.537959	66.125684
1444.869550	60.589282	66.130689
1444.238307	57.791030	66.135694
1443.116013	54.333575	66.140698
1443.030833	53.785695	66.145703
1442.642546	58.565109	66.150708
1441.573810	49.935571	66.155713
1440.824925	54.215811	66.160718
1439.963641	56.464334	66.165722
1439.932587	57.111476	66.170727
1439.121980	52.252314	66.175732
1438.183405	58.809787	66.180737
1437.800625	50.854643	66.185742
1436.971403	52.603490	66.190746
1436.744926	48.787451	66.195751
1435.365320	55.868813	66.200756
1434.567867	48.657643	66.205761
1433.954177	45.479435	66.210766
1433.593374	50.105728	66.215770
1433.265731	44.164476	66.220775
1432.577860	55.209217	66.225780
1431.812666	48.886168	66.230785
1431.181480	49.837339	66.235790
1430.616137	59.135007	66.240794
1430.070494	48.833115	66.245799
1428.663953	53.058960	66.250804
1427.849657	51.589090	66.255809
1427.316740	51.765581	66.260814
1426.886987	58.068996	66.265818
1426.938559	49.616762	66.270823
1426.453578	47.659492	66.275828
1425.430420	52.272061	66.280833
1424.389049	46.435215	66.285838
1423.871186	48.374310	66.290842
1423.513075	44.769874	66.295847
1422.002937	52.091070	66.300852
1421.402876	51.566195	66.305857
1421.211998	47.347766	66.310862
1420.360204	54.019853	66.315866
1420.520178	46.587176	66.320871
1419.469075	45.785838	66.325876
1418.394825	43.741943	66.330881
1417.858851	40.566225	66.335886
1417.155044	54.779726	66.340890
1416.421849	46.592082	66.345895
1415.419628	49.504964	66.350900
1414.578200	49.031667	66.355905
1414.413320	41.532631	66.360910
1414.046425	51.744438	66.365914
1413.682241	53.812354	66.370919
1412.741801	44.669048	66.375924
1411.862805	54.243022	66.380929
1411.953975	57.303471	66.385934
1410.914603	56.318161	66.390938
1409.684761	51.424193	66.395943
1408.698972	53.974282	66.400948
1408.235875	45.867900	66.405953
1408.351152	46.373157	66.410958
1407.765662	47.407688	66.415962
1406.486758	53.175169	66.420967
1405.956534	51.500369	66.425972
1405.235650	56.461050	66.430977
1404.781812	49.898405	66.435982
1403.874444	54.417345	66.440986
1402.793865	52.028763	66.445991
1402.180909	50.457726	66.450996
1401.413679	59.352999	66.456001
1400.885750	42.185908	66.461006
1400.712228	52.960640	66.466010
1400.446172	53.160136	66.471015
1400.118454	55.111684	66.476020
1399.152874	54.871210	66.481025
1398.894463	54.941903	66.486030
1397.648017	53.812840	66.491034
1396.461964	47.404348	66.496039
1396.008563	50.619982	66.501044
1395.394477	44.711977	66.506049
1394.902539	47.267923	66.511054
1393.194112	52.038848	66.516058
1392.741946	45.969712	66.521063
1392.099471	51.199196	66.526068
1392.114197	55.739106	66.531073
1391.341712	44.813323	66.536078
1390.883640	63.882035	66.541082
1390.655413	44.962801	66.546087
1389.958350	54.198150	66.551092
1388.811503	55.402981	66.556097
1387.990714	49.132483	66.561102
1387.215755	53.322854	66.566106
1386.916362	50.348208	66.571111
1385.899163	54.633332	66.576116
1385.056392	58.816366	66.581121
1384.814133	49.103969	66.586126
1384.045481	56.680732	66.591130
1383.664591	50.005739	66.596135
1383.338321	49.930162	66.601140
1382.004848	58.687901	66.606145
1381.459661	49.666407	66.611150
1381.100506	53.349044	66.616154
1380.264183	53.002373	66.621159
1379.322117	60.077532	66.626164
1378.566681	53.112590	66.631169
1378.113597	51.111972	66.636174
1377.723289	55.760686	66.641178
1377.416686	46.503364	66.646183
1376.198952	52.886402	66.651188
1375.147566	53.241646	66.656193
1374.715692	63.667073	66.661198
1374.278764	52.566223	66.666202
1373.652766	52.933119	66.671207
1373.435426	55.374171	66.676212
1372.509549	61.387136	66.681217
1371.797518	55.231043	66.686222
1371.145322	56.475146	66.691226
1369.917904	53.614757	66.696231
1369.104011	48.776699	66.701236
1368.291470	58.157732	66.706241
1368.089531	49.105510	66.711246
1367.616471	52.756727	66.716250
1367.476170	50.104175	66.721255
1367.071353	51.439346	66.726260
1365.554258	54.558000	66.731265
1365.040651	48.656483	66.736270
1364.550027	41.869234	66.741274
1363.963758	45.028275	66.746279
1362.815682	50.440620	66.751284
1361.848332	56.438186	66.756289
1361.495533	47.369554	66.761294
1361.120802	60.879786	66.766298
1360.836605	49.895684	66.771303
1359.774602	51.018107	66.776308
1358.628395	49.965443	66.781313
1358.598145	47.041434	66.786318
1357.437206	55.248218	66.791322
1357.227165	49.877341	66.796327
1356.639338	57.085668	66.801332
1355.518895	48.136208	66.806337
1355.262573	53.294855	66.811342
1354.294847	59.236042	66.816346
1353.995576	46.455005	66.821351
1353.110902	52.516571	66.826356
1352.411246	62.121825	66.831361
1351.700441	56.224855	66.836366
1351.293804	61.762904	66.841370
1350.623085	50.008957	66.846375
1349.750847	49.820011	66.851380
1348.714856	48.624541	66.856385
1348.330245	57.616547	66.861390
1347.740340	59.967042	66.866394
1347.366993	52.862492	66.871399
1346.884099	56.526052	66.876404
1345.606950	55.568829	66.881409
1345.397886	49.201912	66.886414
1344.890949	58.174597	66.891418
1344.013527	52.003009	66.896423
1343.103402	50.624555	66.901428
1342.251756	62.440197	66.906433
1342.115144	46.823291	66.911438
1341.463821	61.955005	66.916442
1340.611021	50.435905	66.921447
1339.914846	54.173079	66.926452
1339.215498	57.780145	66.931457
1338.927361	49.591326	66.936462
1337.907380	52.916584	66.941466
1336.854465	53.843255	66.946471
1336.186418	50.831069	66.951476
1335.543676	57.106606	66.956481
1335.237311	54.276046	66.961486
1334.953402	58.409992	66.966490
1334.355664	53.652563	66.971495
1333.072854	55.897870	66.976500
1332.492533	61.210664	66.981505
1332.527404	51.850682	66.986510
1331.357944	57.766408	66.991514
1330.564387	62.599020	66.996519
1329.634562	60.475554	67.001524
1328.898871	57.864929	67.006529
1329.218572	47.502157	67.011534
1328.326082	61.430610	67.016538
1327.278712	53.899500	67.021543
1326.319427	62.685163	67.026548
1325.973801	63.105117	67.031553
1325.657820	61.554299	67.036558
1324.850726	57.607542	67.041562
1324.003765	55.432394	67.046567
1322.993373	51.837794	67.051572
1322.569336	52.187491	67.056577
1322.587452	47.838166	67.061582
1321.810510	69.992896	67.066586
1320.502472	54.926243	67.071591
1319.917107	56.081547	67.076596
1318.799514	55.238721	67.081601
1318.928003	50.908788	67.086606
1318.787270	61.232269	67.091610
1317.674048	62.509909	67.096615
1316.869242	57.024940	67.101620
1315.436978	66.474180	67.106625
1315.856393	53.243680	67.111630
1315.353216	59.950437	67.116634
1313.788561	54.111624	67.121639
1313.338825	55.814867	67.126644
1313.066417	60.363667	67.131649
1312.650288	51.528899	67.136654
1311.423349	56.786606	67.141658
1310.627494	58.274773	67.146663
1310.275418	52.216143	67.151668
1309.910348	50.961086	67.156673
1309.084193	52.985730	67.161678
1308.010937	58.562507	67.166682
1307.757805	48.116624	67.171687
1307.176579	58.854969	67.176692
1305.284471	55.046990	67.181697
1305.034464	48.505517	67.186702
1304.323220	57.711326	67.191706
1303.602765	50.828041	67.196711
1303.504287	57.368020	67.201716
1302.844258	52.658364	67.206721
1302.632105	54.797359	67.211726
1302.268543	62.757129	67.216730
1301.342689	56.200307	67.221735
1300.389366	49.017826	67.226740
1299.763538	60.209443	67.231745
1299.355524	57.237216	67.236750
1297.927990	53.131430	67.241754
1297.153791	49.161681	67.246759
1296.999302	51.390273	67.251764
1296.377276	64.623512	67.256769
1296.163039	58.234194	67.261774
1294.712241	60.777861	67.266778
1294.177428	54.375534	67.271783
1293.748779	60.926645	67.276788
1293.359766	56.168225	67.281793
1292.572312	52.165221	67.286798
1291.265486	62.141646	67.291802
1291.073520	60.396319	67.296807
1290.563515	59.380802	67.301812
1289.583081	64.421850	67.306817
1289.036926	48.386010	67.311822
1288.264279	58.013233	67.316826
1287.827155	53.003326	67.321831
1287.391155	57.141996	67.326836
1286.702703	60.253805	67.331841
1285.727002	52.265987	67.336846
1284.628661	56.187273	67.341850
1284.265841	57.410661	67.346855
1284.056004	51.253082	67.351860
1283.537968	55.638679	67.356865
1282.402443	45.056117	67.361870
1281.666299	60.279713	67.366874
1281.224612	59.646824	67.371879
1280.273446	57.946607	67.376884
1279.021205	57.021452	67.381889
1279.305892	46.908218	67.386894
1278.480519	57.375347	67.391898
1277.832325	54.089390	67.396903
1277.284000	50.389250	67.401908
1276.645910	50.090761	67.406913
1276.109317	53.545238	67.411918
1275.369109	64.034501	67.416922
1274.281131	52.168858	67.421927
1273.960623	59.105646	67.426932
1273.239848	58.131345	67.431937
1272.112937	49.558001	67.436942
1271.350895	58.268849	67.441946
1270.645086	59.014930	67.446951
1270.437786	52.567195	67.451956
1269.770105	54.672077	67.456961
1270.218586	48.808357	67.461966
1268.900479	57.991752	67.466970
1267.837851	56.573108	67.471975
1267.378508	46.728167	67.476980
1266.568928	58.330959	67.481985
1265.393707	46.714721	67.486990
1264.973064	53.032365	67.491994
1264.508902	50.963791	67.496999
1264.019142	51.103702	67.502004
1263.340353	58.944944	67.507009
1263.550357	48.344389	67.512014
1262.184633	48.183893	67.517018
1261.579882	52.538944	67.522023
1260.798781	42.848561	67.527028
1259.428270	49.991552	67.532033
1259.102707	49.444175	67.537038
1258.754417	51.895411	67.542042
1258.392073	55.277823	67.547047
1257.789196	52.498034	67.552052
1256.305887	55.542252	67.557057
1255.915838	55.822585	67.562062
1255.232076	57.856016	67.567066
1254.079143	50.285373	67.572071
1254.224926	49.911103	67.577076
1253.388655	54.195271	67.582081
1252.624804	45.904366	67.587086
1251.482713	41.975509	67.592090
1251.188588	51.076353	67.597095
1250.793666	42.607031	67.602100
1250.334470	54.361403	67.607105
1250.079073	48.157553	67.612110
1248.815736	53.914899	67.617114
1248.159866	48.688252	67.622119
1248.149987	48.194982	67.627124
1246.256216	60.296800	67.632129
1245.492396	56.036349	67.637134
1244.976661	52.746272	67.642138
1244.647510	58.035014	67.647143
1244.343600	53.148353	67.652148
1243.738458	61.309735	67.657153
1243.370403	53.852602	67.662158
1242.109824	55.299952	67.667162
1241.464320	64.363861	67.672167
1241.232141	50.299181	67.677172
1240.041495	52.021123	67.682177
1239.418336	55.991321	67.687182
1238.316618	61.056297	67.692186
1237.946875	55.992626	67.697191
1237.915061	46.658677	67.702196
1237.288672	57.388174	67.707201
1236.317031	58.087803	67.712206
1235.764252	58.987285	67.717210
1235.359204	49.641449	67.722215
1234.295973	56.470538	67.727220
1233.257397	59.862943	67.732225
1232.703084	55.077571	67.737230
1232.536615	63.442522	67.742234
1231.827933	56.833142	67.747239
1230.528832	58.302090	67.752244
1229.295503	62.223210	67.757249
1229.371954	49.816005	67.762254
1228.682862	59.508659	67.767258
1228.475671	63.897882	67.772263
1228.327815	59.549344	67.777268
1227.416725	58.491982	67.782273
1226.843634	47.428689	67.787278
1225.893431	64.195177	67.792282
1224.517476	61.818919	67.797287
1223.684673	54.624901	67.802292
1223.037895	65.757349	67.807297
1223.042711	57.981390	67.812302
1222.846404	54.879378	67.817306
1222.013767	58.492304	67.822311
1221.110213	54.208811	67.827316
1220.303036	68.164506	67.832321
1219.980342	51.299410	67.837326
1218.768510	66.704317	67.842330
1218.500614	59.105700	67.847335
1217.755282	61.019025	67.852340
1216.533815	54.596912	67.857345
1216.198584	48.229901	67.862350
1215.613324	63.482137	67.867354
1215.450727	58.140646	67.872359
1214.649934	55.203705	67.877364
1213.293501	61.438029	67.882369
1213.263518	55.224007	67.887374
1212.576963	59.432419	67.892378
1212.185628	62.045757	67.897383
1210.792016	50.577843	67.902388
1210.000192	59.079462	67.907393
1209.777530	50.091201	67.912398
1209.095549	61.095863	67.917402
1209.183911	62.116883	67.922407
1207.975798	51.715313	67.927412
1207.050867	47.956512	67.932417
1206.803293	47.893525	67.937422
1206.084354	54.881553	67.942426
1204.798531	52.999451	67.947431
1204.265917	45.544846	67.952436
1203.507778	55.743506	67.957441
1203.699411	44.455742	67.962446
1203.355785	53.949910	67.967450
1201.843396	47.905230	67.972455
1201.021371	44.414588	67.977460
1200.328548	50.892511	67.982465
1199.975321	41.240197	67.987470
1198.850633	54.540147	67.992474
1197.997188	51.144879	67.997479
1197.476935	50.026527	68.002484
1197.220234	57.521571	68.007489
1197.087938	55.680775	68.012494
1196.643276	53.113105	68.017498
1195.182285	51.558614	68.022503
1194.571442	53.023409	68.027508
1194.010542	66.701686	68.032513
1193.348543	53.566352	68.037518
1192.168186	58.555198	68.042522
1191.385447	61.074112	68.047527
1190.691851	44.146619	68.052532
1190.117511	63.534804	68.057537
1189.891645	50.932666	68.062542
1189.638729	50.935327	68.067546
1188.769655	52.058302	68.072551
1189.016352	47.212370	68.077556
1187.403035	52.173902	68.082561
1186.742041	45.897407	68.087566
1186.190390	55.354565	68.092570
1185.190042	53.039136	68.097575
1184.703047	52.418356	68.102580
1183.958655	61.259208	68.107585
1184.031893	45.832973	68.112590
1182.564849	53.199736	68.117594
1181.770579	58.013932	68.122599
1180.978764	52.665316	68.127604
1180.309703	55.341600	68.132609
1180.147574	52.202162	68.137614
1179.916291	56.494460	68.142618
1178.970610	61.213403	68.147623
1178.306955	57.847219	68.152628
1177.393584	58.810420	68.157633
1177.057809	53.661604	68.162638
1175.814856	57.717401	68.167642
1174.957256	57.356251	68.172647
1174.678976	51.159880	68.177652
1173.756430	63.674476	68.182657
1173.591761	54.639185	68.187662
1173.437410	64.190946	68.192666
1172.080440	58.038745	68.197671
1171.434222	56.626979	68.202676
1170.664048	62.412004	68.207681
1170.371798	53.409215	68.212686
1169.834976	60.141867	68.217690
1168.553451	54.474095	68.222695
1167.831741	50.451571	68.227700
1167.456110	58.922193	68.232705
1166.909917	50.805608	68.237710
1166.432373	57.219046	68.242714
1165.354543	59.165230	68.247719
1164.760886	53.404549	68.252724
1164.005130	52.461123	68.257729
1163.901080	52.558291	68.262734
1163.291561	47.702257	68.267738
1162.171548	48.113109	68.272743
1161.950964	51.504803	68.277748
1161.014909	49.035484	68.282753
1160.279786	47.324354	68.287758
1159.517883	51.490409	68.292762
1158.631055	54.782637	68.297767
1158.546875	40.820135	68.302772
1157.642552	59.060135	68.307777
1156.735811	49.571673	68.312782
1156.052144	54.119051	68.317786
1154.847758	53.038505	68.322791
1154.836282	42.580879	68.327796
1154.044315	57.308395	68.332801
1153.931520	53.817502	68.337806
1153.301229	56.787136	68.342810
1152.186638	56.915233	68.347815
1151.628303	56.141285	68.352820
1150.719198	54.875582	68.357825
1150.951354	45.344480	68.362830
1150.312671	50.605303	68.367834
1148.781638	57.601735	68.372839
1148.317804	53.069688	68.377844
1147.724680	49.567097	68.382849
1147.360044	49.823747	68.387854
1146.307918	56.118077	68.392858
1145.484529	58.864604	68.397863
1145.251031	52.754905	68.402868
1144.626137	60.528508	68.407873
1144.154294	58.957816	68.412878
1142.904684	61.753245	68.417882
1142.207938	61.451396	68.422887
1142.258029	58.223520	68.427892
1140.802351	66.005962	68.432897
1139.676558	60.211273	68.437902
1139.329020	49.093591	68.442906
1138.538924	53.955231	68.447911
1138.516913	55.391837	68.452916
1137.818711	62.439478	68.457921
1137.727225	60.127114	68.462926
1137.168834	62.165932	68.467930
1135.620905	58.820513	68.472935
1135.444299	52.088474	68.477940
1134.857081	63.237168	68.482945
1133.720433	53.111532	68.487950
1133.326219	57.239106	68.492954
1132.614045	54.658830	68.497959
1132.177220	48.154497	68.502964
1131.003464	58.653657	68.507969
1130.296688	49.881716	68.512974
1129.894259	57.602226	68.517978
1129.088857	45.860745	68.522983
1128.934326	45.505528	68.527988
1127.540124	60.647993	68.532993
1127.102557	57.342573	68.537998
1126.169392	54.756324	68.543002
1125.826936	64.308714	68.548007
1125.494471	54.451544	68.553012
1124.839325	60.290294	68.558017
1123.780339	47.961080	68.563022
1123.300108	51.323816	68.568026
1122.461653	53.602817	68.573031
1122.005899	51.193757	68.578036
1121.255405	61.608210	68.583041
1120.397915	57.763671	68.588046
1119.587766	56.745491	68.593050
1119.034907	60.117507	68.598055
1118.603623	52.763979	68.603060
1118.375814	58.196019	68.608065
1117.765761	57.726179	68.613070
1116.825322	52.937078	68.618074
1115.800453	63.735207	68.623079
1115.792058	55.304317	68.628084
1114.429084	56.768836	68.633089
1113.765269	49.892868	68.638094
1113.029906	52.704847	68.643098
1112.283961	61.077834	68.648103
1112.037805	52.895673	68.653108
1111.319112	59.473163	68.658113
1111.054695	52.447887	68.663118
1110.473155	53.500721	68.668122
1109.479822	49.814835	68.673127
1109.163675	54.808471	68.678132
1108.294084	51.576636	68.683137
1107.473500	55.289348	68.688142
1106.746559	51.180104	68.693146
1106.132696	57.188618	68.698151
1105.423782	48.701245	68.703156
1104.031044	54.886940	68.708161
1103.494329	46.119043	68.713166
1103.625937	55.433944	68.718170
1102.642460	58.347223	68.723175
1102.346449	44.454551	68.728180
1101.929902	53.231765	68.733185
1101.131653	52.720341	68.738190
1100.330149	50.660605	68.743194
1099.666755	48.585510	68.748199
1098.819250	44.070619	68.753204
1097.797461	55.514368	68.758209
1097.115059	56.263964	68.763214
1096.656220	54.920381	68.768218
1096.499185	57.595047	68.773223
1095.907434	48.002143	68.778228
1094.659300	61.634676	68.783233
1094.143415	54.146830	68.788238
1093.806225	51.578926	68.793242
1093.354894	57.203969	68.798247
1092.357387	52.249392	68.803252
1090.972925	60.026752	68.808257
1090.691807	53.897584	68.813262
1089.936531	53.177497	68.818266
1089.660052	59.481117	68.823271
1089.421008	53.424872	68.828276
1088.387999	57.531575	68.833281
1087.503568	50.707599	68.838286
1087.058808	54.659891	68.843290
1086.080710	57.214639	68.848295
1085.332780	49.825738	68.853300
1084.482544	52.975928	68.858305
1083.855679	51.683223	68.863310
1083.591842	48.434505	68.868314
1082.890868	53.836256	68.873319
1083.022333	48.760595	68.878324
1082.005774	58.094085	68.883329
1080.956754	46.397492	68.888334
1080.282583	47.100682	68.893338
1079.915613	60.363655	68.898343
1079.428730	51.904184	68.903348
1078.065198	57.648723	68.908353
1077.659209	51.479363	68.913358
1077.226966	54.753757	68.918362
1076.567865	58.106471	68.923367
1075.763009	48.640058	68.928372
1074.479396	54.318808	68.933377
1074.591108	47.133611	68.938382
1074.089287	48.961046	68.943386
1073.086314	51.400850	68.948391
1072.142737	50.109489	68.953396
1071.233560	50.322423	68.958401
1070.865694	56.147901	68.963406
1070.672697	54.849189	68.968410
1070.235882	60.886991	68.973415
1069.356425	51.777545	68.978420
1068.518523	61.047684	68.983425
1067.503705	58.358199	68.988430
1067.349862	48.460589	68.993434
1066.341525	61.300127	68.998439
1065.334240	53.903143	69.003444
1064.446045	57.182988	69.008449
1064.061971	53.144901	69.013454
1063.578062	55.551477	69.018458
1063.280077	57.478213	69.023463
1063.221261	51.487420	69.028468
1062.370264	54.820102	69.033473
1061.618536	54.302297	69.038478
1061.162653	49.382474	69.043482
1059.347706	52.834043	69.048487
1059.198269	45.736985	69.053492
1058.341031	46.751381	69.058497
1058.096080	56.193913	69.063502
1057.473234	52.173821	69.068506
1056.284503	61.197342	69.073511
1056.211182	45.082577	69.078516
1055.435462	49.293244	69.083521
1054.701995	43.668628	69.088526
1053.599227	51.415121	69.093530
1052.676188	54.888819	69.098535
1052.402026	49.871172	69.103540
1051.920923	55.524997	69.108545
1051.344219	53.687288	69.113550
1051.074881	48.575267	69.118554
1049.981912	59.996082	69.123559
1049.771714	53.173098	69.128564
1048.970017	55.496733	69.133569
1047.573042	52.243912	69.138574
1046.486886	47.655038	69.143578
1045.646387	51.956532	69.148583
1046.504755	50.677508	69.153588
1045.598770	47.298375	69.158593
1045.372900	48.681078	69.163598
1044.593956	52.449032	69.168602
1043.346651	51.744924	69.173607
1042.537830	47.827337	69.178612
1042.400156	56.241418	69.183617
1040.792191	55.025549	69.188622
1040.082548	53.351520	69.193626
1039.337089	55.680920	69.198631
1039.367717	51.611687	69.203636
1038.484867	48.718436	69.208641
1038.406305	60.293944	69.213646
1037.606004	48.696080	69.218650
1036.767130	58.292422	69.223655
1036.084224	48.514625	69.228660
1035.272923	55.574137	69.233665
1034.898030	52.541798	69.238670
1034.823419	54.546724	69.243674
1033.112435	52.846419	69.248679
1032.897452	44.200275	69.253684
1031.809360	52.989862	69.258689
1031.606992	50.003765	69.263694
1031.199101	50.177835	69.268698
1030.101375	54.729818	69.273703
1029.723858	45.862835	69.278708
1029.281208	57.788043	69.283713
1027.778166	51.871292	69.288718
1027.312490	51.328190	69.293722
1026.276334	57.073516	69.298727
1026.182617	54.041182	69.303732
1025.292049	52.829959	69.308737
1024.855162	57.933479	69.313742
1024.608466	55.104570	69.318746
1022.854720	56.598534	69.323751
1022.727070	50.289154	69.328756
1022.278853	47.839345	69.333761
1021.808433	55.108101	69.338766
1021.363606	44.786670	69.343770
1019.863816	57.966935	69.348775
1019.821502	50.434714	69.353780
1019.111524	50.077915	69.358785
1018.039433	58.550967	69.363790
1017.181497	58.662378	69.368794
1015.965287	53.459498	69.373799
1015.685345	50.237621	69.378804
1015.688965	63.685010	69.383809
1015.137172	62.458402	69.388814
1014.815936	46.575168	69.393818
1014.095472	60.566138	69.398823
1013.038729	58.595520	69.403828
1012.506298	57.402305	69.408833
1012.037278	57.112395	69.413838
1011.248920	54.903589	69.418842
1010.243351	53.751140	69.423847
1009.608148	51.790040	69.428852
1008.954412	56.568346	69.433857
1008.180134	46.577269	69.438862
1007.296031	50.849526	69.443866
1006.526811	58.979807	69.448871
1006.318970	42.744019	69.453876
1005.646306	47.788445	69.458881
1005.309174	49.128627	69.463886
1004.849792	49.647815	69.468890
1003.436098	54.806516	69.473895
1003.077805	50.522850	69.478900
1002.389354	55.503670	69.483905
1002.022645	52.216525	69.488910
1001.161903	48.843469	69.493914
1000.171351	53.212506	69.498919
999.765861	55.613947	69.503924
999.378343	47.138267	69.508929
998.152857	52.788525	69.513934
997.485246	41.121774	69.518938
996.977239	55.745793	69.523943
996.584579	50.398727	69.528948
996.140963	47.761037	69.533953
995.483301	54.050595	69.538958
994.631056	50.897520	69.543962
993.489635	52.367942	69.548967
993.224494	53.874208	69.553972
992.876435	57.792183	69.558977
991.365292	61.511863	69.563982
990.931666	55.192124	69.568986
989.902821	65.076783	69.573991
989.868187	54.699708	69.578996
989.160943	54.164034	69.584001
988.983638	59.504139	69.589006
988.300715	51.599285	69.594010
986.994672	59.667167	69.599015
986.412921	55.039684	69.604020
985.778511	49.588765	69.609025
985.331282	49.727735	69.614030
984.261799	50.926905	69.619034
983.313814	55.607586	69.624039
983.023721	51.858135	69.629044
982.827695	53.601237	69.634049
982.212172	58.852582	69.639054
981.850086	55.547674	69.644058
980.383889	55.973645	69.649063
980.037958	55.659106	69.654068
979.357762	53.901495	69.659073
978.465908	54.104769	69.664078
977.938159	49.919203	69.669082
977.123710	55.660117	69.674087
976.936966	48.825233	69.679092
976.432456	51.392045	69.684097
975.058594	58.624482	69.689102
974.716953	51.664553	69.694106
973.989870	56.394637	69.699111
973.665845	58.904885	69.704116
972.734222	58.768805	69.709121
971.538791	46.534852	69.714126
971.126544	52.911059	69.719130
970.445245	63.989028	69.724135
970.541874	46.710362	69.729140
969.616109	55.842007	69.734145
968.466307	51.245896	69.739150
968.031633	45.954580	69.744154
967.339792	55.227733	69.749159
966.956699	51.668281	69.754164
966.176149	51.778289	69.759169
965.166369	61.737442	69.764174
964.823829	47.551202	69.769178
964.297529	54.839790	69.774183
963.753651	49.389160	69.779188
962.462541	52.974851	69.784193
961.611638	55.675986	69.789198
961.171076	52.728713	69.794202
960.629319	64.693001	69.799207
960.126489	52.785277	69.804212
960.048945	53.403277	69.809217
958.892021	54.617822	69.814222
958.251532	45.883516	69.819226
957.271032	55.829757	69.824231
956.840111	49.323257	69.829236
955.830319	49.635940	69.834241
954.707538	50.369400	69.839246
954.463285	41.731045	69.844250
953.792349	51.936882	69.849255
953.351350	49.923585	69.854260
952.976045	52.806938	69.859265
952.717443	49.085648	69.864270
952.392471	46.887094	69.869274
950.640415	54.695857	69.874279
950.273558	46.157835	69.879284
949.772434	47.893587	69.884289
948.729987	49.433115	69.889294
947.989360	54.070394	69.894298
947.418767	51.167497	69.899303
947.215726	48.944114	69.904308
946.566408	54.536757	69.909313
945.338675	54.955843	69.914318
944.727344	49.700310	69.919322
943.964772	59.594627	69.924327
943.582809	55.606716	69.929332
943.337238	61.065875	69.934337
942.448880	52.861890	69.939342
941.972171	45.012517	69.944346
941.188962	53.745163	69.949351
940.513995	49.522056	69.954356
939.148818	54.394976	69.959361
938.356105	62.973343	69.964366
938.164729	54.846162	69.969370
937.657347	62.170197	69.974375
937.449823	54.034731	69.979380
936.837669	61.015939	69.984385
935.445682	53.577911	69.989390
935.103636	54.834075	69.994394
934.334459	53.783649	69.999399
933.759362	48.431128	70.004404
932.947263	51.396790	70.009409
932.035473	59.208485	70.014414
931.545122	57.259296	70.019418
930.888568	57.636611	70.024423
931.001337	55.968582	70.029428
930.065680	50.766625	70.034433
928.510871	57.520877	70.039438
928.101196	45.818648	70.044442
927.492359	51.283969	70.049447
927.386128	58.838493	70.054452
926.829255	53.523112	70.059457
925.924079	49.348119	70.064462
925.412727	43.981131	70.069466
924.813947	57.409707	70.074471
923.799388	53.622901	70.079476
922.852318	50.475424	70.084481
922.294526	62.192600	70.089486
921.776962	49.588763	70.094490
921.318266	56.072396	70.099495
920.922241	52.371487	70.104500
919.374480	52.512250	70.109505
918.929405	54.949684	70.114510
918.549416	43.706560	70.119514
917.960718	54.209351	70.124519
917.791691	49.928804	70.129524
916.432948	58.516486	70.134529
915.568963	61.484329	70.139534
915.059648	47.763219	70.144538
914.981765	51.419012	70.149543
914.051406	51.037213	70.154548
913.102470	52.405610	70.159553
912.142623	57.753825	70.164558
912.142152	48.449673	70.169562
911.272426	51.051016	70.174567
910.603179	49.762833	70.179572
910.050820	52.095490	70.184577
908.899821	56.895817	70.189582
908.974639	56.439356	70.194586
907.828629	51.194488	70.199591
906.659285	53.544402	70.204596
906.212909	44.155185	70.209601
905.493486	46.392120	70.214606
905.647361	43.676580	70.219610
904.893567	54.283828	70.224615
904.577749	56.137049	70.229620
903.383669	52.771370	70.234625
902.536962	46.317146	70.239630
902.235449	52.906087	70.244634
901.337705	57.299505	70.249639
900.160470	53.074803	70.254644
900.235403	52.439121	70.259649
899.149120	54.020508	70.264654
898.979122	44.799866	70.269658
898.423881	58.154671	70.274663
897.502053	50.127739	70.279668
896.624121	54.000687	70.284673
896.103439	54.526436	70.289678
895.483700	53.331217	70.294682
894.227137	66.328542	70.299687
893.695116	57.643558	70.304692
893.037755	59.533568	70.309697
892.434618	47.287406	70.314702
892.383628	53.354253	70.319706
891.811457	59.791406	70.324711
891.097672	54.297653	70.329716
890.166980	54.124721	70.334721
889.572932	58.063516	70.339726
888.916525	54.587593	70.344730
887.670859	61.767699	70.349735
887.260990	58.229419	70.354740
886.624084	57.738552	70.359745
886.179620	59.131070	70.364750
885.769766	50.988427	70.369754
885.051723	56.570741	70.374759
884.155459	53.217608	70.379764
883.599955	52.229272	70.384769
883.062418	57.584102	70.389774
882.276992	50.504023	70.394778
880.947296	63.216652	70.399783
880.559103	53.902728	70.404788
880.455367	54.256018	70.409793
879.620354	60.350579	70.414798
879.334588	53.037296	70.419802
878.312827	53.551771	70.424807
877.235222	52.729830	70.429812
877.092060	51.089452	70.434817
876.660239	53.484358	70.439822
875.978826	46.278315	70.444826
875.018407	52.793411	70.449831
874.571699	47.893755	70.454836
873.450102	40.439442	70.459841
872.173580	52.280897	70.464846
871.705965	41.080818	70.469850
870.968624	54.981914	70.474855
870.780194	46.928054	70.479860
870.563695	50.740607	70.484865
870.019225	55.392451	70.489870
869.492450	51.584082	70.494874
868.491572	53.541221	70.499879
867.751975	57.761513	70.504884
867.570462	53.558499	70.509889
866.146978	68.664572	70.514894
865.856264	58.578859	70.519898
864.828885	61.606272	70.524903
864.007262	56.858062	70.529908
863.678283	54.216146	70.534913
863.086728	59.740484	70.539918
862.185846	52.848334	70.544922
861.322147	54.410156	70.549927
860.918944	54.463837	70.554932
860.719516	58.584504	70.559937
859.758177	57.603712	70.564942
859.022725	50.286144	70.569946
858.324594	52.176430	70.574951
857.530908	54.958958	70.579956
857.260212	52.068258	70.584961
856.715259	58.074851	70.589966
855.608932	58.397774	70.594970
854.844981	54.531746	70.599975
854.436507	60.824816	70.604980
854.298633	52.729929	70.609985
852.668768	53.970245	70.614990
852.158249	48.786273	70.619994
851.460067	57.230825	70.624999
851.016909	52.512526	70.630004
851.009021	47.045895	70.635009
850.129343	61.634104	70.640014
849.425707	50.108548	70.645018
848.359199	51.969570	70.650023
847.629856	49.066644	70.655028
847.382883	52.341288	70.660033
846.278998	61.603714	70.665038
845.522649	49.016325	70.670042
844.904631	55.296340	70.675047
844.496452	59.084098	70.680052
843.998199	58.929073	70.685057
843.289542	55.531183	70.690062
842.912047	59.183034	70.695066
841.946446	56.999487	70.700071
841.132781	50.815129	70.705076
841.004692	54.143617	70.710081
840.070373	54.951000	70.715086
839.367633	43.497137	70.720090
838.314991	48.661133	70.725095
837.793716	51.790139	70.730100
837.210857	53.763310	70.735105
836.611447	61.665186	70.740110
836.127548	48.484451	70.745114
834.942392	59.084674	70.750119
834.335908	53.495585	70.755124
834.314866	58.304473	70.760129
833.229541	58.075543	70.765134
832.663648	56.331928	70.770138
831.874395	54.098047	70.775143
831.684269	56.403400	70.780148
831.141570	48.894543	70.785153
829.550620	56.264845	70.790158
829.080728	56.249430	70.795162
828.203309	54.056703	70.800167
827.794890	53.759194	70.805172
827.867029	49.586943	70.810177
827.076995	56.937289	70.815182
826.181624	50.500891	70.820186
825.495554	52.412404	70.825191
824.731043	57.558234	70.830196
824.096453	56.468195	70.835201
823.154902	54.368160	70.840206
822.713619	47.720175	70.845210
822.391801	55.262279	70.850215
821.647886	56.094680	70.855220
820.652026	50.450324	70.860225
819.645696	57.701543	70.865230
819.642556	57.031078	70.870234
818.861201	55.471206	70.875239
818.610141	48.824583	70.880244
817.576579	45.941407	70.885249
816.639362	52.935274	70.890254
816.039975	47.549832	70.895258
815.771915	56.206878	70.900263
814.665591	49.023897	70.905268
814.037010	48.699763	70.910273
813.283877	55.746568	70.915278
812.811823	49.416469	70.920282
812.242844	51.319374	70.925287
811.272357	47.297692	70.930292
810.561892	60.513305	70.935297
809.731362	54.836683	70.940302
809.454328	54.336680	70.945306
809.104281	56.976517	70.950311
808.805637	52.614370	70.955316
807.882774	50.560872	70.960321
806.552570	58.518062	70.965326
806.066269	53.367841	70.970330
805.619156	57.146481	70.975335
804.757778	50.053380	70.980340
804.358561	44.582340	70.985345
803.264868	51.837077	70.990350
803.119441	50.260641	70.995354
802.296153	59.326989	71.000359
801.607851	60.174339	71.005364
800.682267	42.992257	71.010369
799.828764	49.907446	71.015374
799.704978	51.909346	71.020378
799.029446	52.489655	71.025383
798.788421	54.655315	71.030388
797.815866	52.751244	71.035393
796.913871	51.504920	71.040398
796.648804	44.326651	71.045402
796.182895	50.957960	71.050407
795.089189	53.077847	71.055412
794.403241	50.481692	71.060417
793.644586	63.043229	71.065422
792.687848	51.856685	71.070426
791.827419	51.384383	71.075431
791.403788	53.346072	71.080436
790.960303	47.500532	71.085441
790.154942	57.001942	71.090446
789.577924	54.783027	71.095450
789.117955	57.832067	71.100455
788.722138	54.261790	71.105460
787.820756	47.250148	71.110465
786.713715	56.780737	71.115470
786.486759	50.525889	71.120474
785.997296	45.261353	71.125479
785.180314	53.499690	71.130484
784.345337	50.397382	71.135489
783.562357	57.888227	71.140494
783.290902	51.329571	71.145498
782.707380	45.806425	71.150503
781.908394	48.199497	71.155508
780.880085	51.031303	71.160513
780.244377	54.849749	71.165518
779.629262	46.693737	71.170522
779.470430	50.172745	71.175527
779.132973	56.510883	71.180532
778.426121	52.779556	71.185537
777.267593	53.373530	71.190542
776.101789	47.869212	71.195546
775.464681	58.015976	71.200551
774.660090	61.307989	71.205556
774.400554	55.775130	71.210561
773.717365	52.014094	71.215566
773.632165	50.115912	71.220570
773.014984	59.927309	71.225575
771.951451	58.855100	71.230580
771.662531	49.185132	71.235585
770.417429	54.892476	71.240590
769.388370	53.010327	71.245594
768.877615	54.017126	71.250599
768.208637	56.747516	71.255604
767.876124	57.636944	71.260609
767.427809	59.278802	71.265614
766.852240	57.390414	71.270618
766.318632	52.173702	71.275623
764.926197	60.057092	71.280628
764.374957	48.504270	71.285633
763.919396	60.576146	71.290638
763.613082	51.622409	71.295642
762.760935	62.461241	71.300647
761.154953	59.344571	71.305652
761.374681	56.481572	71.310657
760.735506	64.208694	71.315662
760.639804	45.495854	71.320666
759.558653	51.121827	71.325671
758.880205	57.074718	71.330676
758.266992	53.630101	71.335681
756.932606	54.489060	71.340686
756.392195	50.454109	71.345690
755.619469	60.690419	71.350695
754.857735	56.851267	71.355700
754.868518	48.440023	71.360705
754.487648	57.245069	71.365710
753.569047	52.296799	71.370714
752.349002	53.768901	71.375719
751.645663	55.172224	71.380724
751.075958	50.749551	71.385729
750.592573	53.072380	71.390734
750.296137	45.996196	71.395738
750.040245	49.071853	71.400743
749.134699	49.953268	71.405748
748.469909	48.060431	71.410753
747.646274	55.217997	71.415758
746.783657	48.014999	71.420762
745.966430	51.908355	71.425767
745.316812	50.610124	71.430772
744.934882	47.460609	71.435777
744.201540	55.681859	71.440782
743.255277	42.782057	71.445786
742.578033	49.257343	71.450791
741.641951	51.424446	71.455796
741.560411	49.072110	71.460801
740.638301	48.735904	71.465806
740.545941	48.784501	71.470810
739.467196	46.364191	71.475815
738.956884	50.367989	71.480820
738.494095	42.686393	71.485825
737.640814	51.564469	71.490830
736.865880	41.302806	71.495834
735.890628	45.764782	71.500839
734.649868	49.132700	71.505844
734.848870	46.260622	71.510849
734.407384	47.894207	71.515854
734.239901	44.598227	71.520858
733.155165	48.819632	71.525863
732.066756	48.002338	71.530868
731.953914	51.184536	71.535873
731.012948	57.541196	71.540878
730.061130	47.857698	71.545882
728.909436	52.323852	71.550887
728.534383	49.584454	71.555892
728.535247	47.917043	71.560897
728.306690	48.384477	71.565902
727.792296	40.447265	71.570906
726.444973	47.018000	71.575911
725.830250	48.764942	71.580916
725.002855	49.634946	71.585921
723.938825	51.035725	71.590926
723.469550	42.064129	71.595930
722.838778	49.245889	71.600935
722.253743	50.579216	71.605940
722.004251	45.948938	71.610945
720.798227	52.961235	71.615950
720.115577	48.293852	71.620954
719.727952	48.307773	71.625959
719.077091	44.856194	71.630964
719.029448	49.941984	71.635969
717.443002	51.755531	71.640974
716.510165	50.976323	71.645978
716.327412	52.105743	71.650983
715.967548	51.241009	71.655988
715.869317	50.554074	71.660993
714.079957	49.389128	71.665998
713.811479	48.372957	71.671002
713.281944	43.660005	71.676007
712.338845	51.546552	71.681012
711.533866	50.227970	71.686017
710.832776	51.924187	71.691022
710.396479	47.797597	71.696026
709.777439	46.520184	71.701031
709.360583	54.752346	71.706036
708.740370	40.222577	71.711041
707.425767	50.264361	71.716046
707.026219	45.226394	71.721050
706.585108	37.230452	71.726055
706.192498	39.774956	71.731060
705.227252	47.664506	71.736065
704.164452	51.161804	71.741070
703.833989	48.965002	71.746074
703.312114	49.173230	71.751079
703.102407	49.833214	71.756084
702.268374	51.111311	71.761089
701.198436	55.478206	71.766094
700.847909	51.046412	71.771098
699.441905	47.858011	71.776103
698.432227	53.172162	71.781108
698.000517	50.744035	71.786113
697.419125	53.194179	71.791118
697.276381	59.423965	71.796122
696.945435	54.922899	71.801127
696.500876	56.048225	71.806132
695.732228	48.675992	71.811137
694.485895	53.031267	71.816142
694.128502	51.785607	71.821146
693.894256	46.225929	71.826151
692.133940	52.363770	71.831156
691.994651	40.661850	71.836161
691.057775	57.620647	71.841166
690.758577	47.164603	71.846170
690.291600	49.638170	71.851175
689.164229	53.740580	71.856180
688.714451	50.501647	71.861185
687.928699	49.800267	71.866190
687.612169	41.574180	71.871194
686.734923	43.150585	71.876199
685.390573	45.446453	71.881204
685.089880	47.078815	71.886209
684.190675	48.500308	71.891214
684.072524	44.818138	71.896218
683.656512	48.485670	71.901223
682.750164	56.318955	71.906228
682.191016	48.055091	71.911233
681.369817	53.270248	71.916238
681.023870	45.414310	71.921242
680.469630	44.433678	71.926247
679.187101	56.038572	71.931252
678.743078	42.993936	71.936257
677.715526	45.741161	71.941262
677.505468	43.120732	71.946266
676.977226	41.436212	71.951271
675.470468	52.352059	71.956276
674.986215	46.573913	71.961281
674.414121	46.786800	71.966286
673.959095	51.717395	71.971290
673.966702	52.616451	71.976295
673.060461	50.073056	71.981300
672.296341	42.184952	71.986305
671.403016	49.186314	71.991310
670.736549	48.425819	71.996314
670.537662	48.506878	72.001319
669.612326	50.644127	72.006324
668.756344	43.289233	72.011329
668.039886	56.789670	72.016334
667.762449	52.894011	72.021338
667.346744	46.507709	72.026343
665.918650	45.839016	72.031348
665.492371	48.567308	72.036353
664.849915	51.252114	72.041358
664.386976	52.051005	72.046362
664.036504	51.102171	72.051367
662.563619	51.296500	72.056372
662.306762	46.216726	72.061377
661.743123	52.893201	72.066382
660.835374	45.976232	72.071386
659.673581	40.538762	72.076391
659.188631	48.662987	72.081396
658.729385	43.164361	72.086401
658.012654	48.538453	72.091406
657.508466	45.303716	72.096410
657.524874	44.119538	72.101415
656.512057	55.837297	72.106420
655.341364	44.151041	72.111425
654.698140	57.058306	72.116430
654.557409	42.040637	72.121434
654.134787	48.995303	72.126439
652.861448	53.473628	72.131444
652.299253	45.950779	72.136449
651.755837	46.391243	72.141454
651.426081	42.226279	72.146458
650.257242	53.827091	72.151463
649.640700	55.834076	72.156468
649.148472	44.401827	72.161473
648.207180	48.053965	72.166478
647.633536	47.290991	72.171482
646.866639	50.047248	72.176487
646.212552	54.461321	72.181492
645.579491	39.401302	72.186497
644.857286	51.138739	72.191502
644.593981	45.739169	72.196506
643.937416	49.500018	72.201511
643.031409	54.470382	72.206516
642.168506	45.097713	72.211521
641.472119	44.905607	72.216526
641.117616	51.258899	72.221530
641.047578	54.939393	72.226535
639.466934	50.383246	72.231540
639.398552	42.715011	72.236545
638.185469	53.150708	72.241550
637.637623	45.337657	72.246554
637.379408	52.658872	72.251559
636.415640	47.941384	72.256564
635.721241	35.930000	72.261569
635.125197	48.270653	72.266574
634.895673	47.812650	72.271578
633.859521	48.943423	72.276583
632.751677	51.569421	72.281588
632.310962	48.319471	72.286593
631.796525	51.641915	72.291598
631.167515	43.622916	72.296602
630.883257	40.746797	72.301607
629.712095	43.451929	72.306612
629.087154	46.721073	72.311617
628.281017	45.398757	72.316622
628.057750	49.217601	72.321626
627.435502	52.431814	72.326631
626.514378	55.357384	72.331636
625.683348	42.824305	72.336641
625.121281	48.420177	72.341646
624.986776	47.234620	72.346650
624.193349	38.577910	72.351655
623.137402	44.801130	72.356660
622.429629	32.879670	72.361665
621.653252	49.602551	72.366670
621.479426	48.043226	72.371674
621.067604	35.938434	72.376679
619.742303	43.557726	72.381684
619.259085	33.951475	72.386689
618.408488	39.865579	72.391694
617.954053	41.624936	72.396698
617.989396	41.242732	72.401703
616.721431	49.462432	72.406708
616.418450	44.048743	72.411713
615.284137	47.965655	72.416718
614.164523	46.821780	72.421722
613.733318	44.502914	72.426727
613.310971	47.489863	72.431732
613.465583	45.207987	72.436737
612.655063	50.072393	72.441742
611.200066	47.598165	72.446746
610.841045	45.376662	72.451751
610.062784	42.849248	72.456756
609.428531	42.490194	72.461761
608.287703	50.561015	72.466766
607.790074	44.112185	72.471770
606.871772	44.845818	72.476775
606.283780	47.300258	72.481780
606.283609	38.122006	72.486785
605.707726	42.081390	72.491790
604.987008	41.281651	72.496794
604.172528	48.427396	72.501799
602.976000	47.642867	72.506804
602.910654	37.567939	72.511809
602.597690	46.028992	72.516814
601.323570	47.106996	72.521818
600.720612	45.424629	72.526823
599.970020	49.257247	72.531828
599.906258	39.033240	72.536833
599.246132	40.965595	72.541838
598.150419	44.985232	72.546842
597.526046	41.775438	72.551847
596.748589	47.762274	72.556852
596.519044	46.125660	72.561857
595.067158	47.816326	72.566862
594.561034	43.528832	72.571866
593.954615	46.001429	72.576871
593.412825	50.114834	72.581876
592.969358	42.987686	72.586881
592.781500	48.346953	72.591886
591.664800	44.931398	72.596890
590.877089	48.494077	72.601895
590.286600	45.893049	72.606900
589.938013	44.720095	72.611905
588.311461	44.443041	72.616910
587.638607	45.959182	72.621914
587.183391	39.701237	72.626919
586.758165	45.055781	72.631924
586.713641	39.922269	72.636929
585.867013	45.442169	72.641934
584.867385	48.959847	72.646938
584.314331	48.084807	72.651943
583.789957	49.639452	72.656948
583.243450	42.144324	72.661953
582.388943	44.199587	72.666958
581.481357	46.814967	72.671962
580.785247	42.385563	72.676967
580.288938	50.045974	72.681972
580.009484	43.390039	72.686977
579.163871	50.714401	72.691982
578.123178	46.443901	72.696986
577.712286	38.630293	72.701991
577.265386	56.530605	72.706996
576.825551	45.409113	72.712001
575.568189	46.125062	72.717006
574.824898	44.439508	72.722010
574.318459	42.886258	72.727015
573.600930	47.090561	72.732020
573.496910	43.081916	72.737025
572.392236	45.332799	72.742030
571.551114	46.631472	72.747034
571.023965	41.037922	72.752039
570.551651	43.798578	72.757044
569.689055	46.069559	72.762049
568.956494	50.501821	72.767054
568.160151	48.734969	72.772058
567.725673	40.619499	72.777063
567.149003	45.318322	72.782068
566.672787	49.506935	72.787073
565.572229	54.502750	72.792078
565.114977	44.908633	72.797082
564.435761	52.341452	72.802087
564.013720	58.978279	72.807092
563.506092	46.982270	72.812097
562.091025	52.107363	72.817102
561.543109	50.384783	72.822106
561.306419	44.700810	72.827111
560.450950	54.559746	72.832116
560.290627	40.987741	72.837121
559.324607	52.210015	72.842126
558.192041	54.838292	72.847130
557.757828	45.715070	72.852135
557.175246	49.137217	72.857140
557.113186	45.758847	72.862145
555.994684	46.541793	72.867150
555.362673	53.361822	72.872154
554.906725	45.046754	72.877159
553.570406	67.053721	72.882164
552.648456	48.835768	72.887169
551.927834	50.630083	72.892174
551.332623	51.523486	72.897178
551.362796	54.616050	72.902183
550.613136	54.783591	72.907188
550.278537	45.148331	72.912193
549.881390	46.734860	72.917198
548.722208	52.506468	72.922202
548.339979	51.899777	72.927207
547.406230	61.240846	72.932212
546.650928	48.612315	72.937217
545.674411	51.911711	72.942222
545.023170	48.722317	72.947226
544.793646	46.191674	72.952231
543.866618	50.841986	72.957236
544.098378	45.411675	72.962241
542.713168	50.843087	72.967246
541.829017	47.901616	72.972250
541.417381	45.923596	72.977255
540.734733	51.301333	72.982260
539.829441	46.988300	72.987265
538.867362	56.586049	72.992270
538.595124	50.504769	72.997274
538.246610	45.600968	73.002279
537.175514	52.497419	73.007284
537.250550	46.574518	73.012289
536.034812	43.852489	73.017294
535.024324	48.587362	73.022298
534.856638	36.889546	73.027303
534.284893	47.140759	73.032308
533.959897	42.123594	73.037313
532.687802	47.548256	73.042318
532.010823	46.798267	73.047322
531.350192	42.167805	73.052327
530.695805	49.288099	73.057332
530.033377	39.836116	73.062337
529.062428	42.871679	73.067342
528.360059	48.480940	73.072346
528.165063	41.865012	73.077351
527.525198	52.383281	73.082356
527.174117	49.956358	73.087361
526.130650	44.329319	73.092366
525.374232	54.898745	73.097370
525.013223	42.620271	73.102375
524.268213	49.405193	73.107380
524.152725	41.691361	73.112385
522.747591	44.935527	73.117390
521.745977	44.371816	73.122394
521.538294	38.032390	73.127399
520.994030	47.515519	73.132404
520.565254	49.572444	73.137409
519.570832	46.002542	73.142414
518.420144	50.929589	73.147418
518.312696	47.587023	73.152423
517.667728	47.737420	73.157428
517.449165	39.095518	73.162433
515.931470	47.666298	73.167438
515.237029	46.965090	73.172442
515.241308	44.783576	73.177447
514.541601	46.442477	73.182452
513.915439	42.697376	73.187457
513.571092	49.708101	73.192462
512.876080	56.472618	73.197466
511.724634	49.924269	73.202471
510.679516	51.918264	73.207476
510.577192	48.691261	73.212481
509.509477	56.018166	73.217486
508.068939	45.453800	73.222490
508.252082	48.237138	73.227495
507.062116	54.318353	73.232500
506.747455	50.102662	73.237505
506.225911	55.749227	73.242510
505.673742	51.739224	73.247514
505.388951	43.069988	73.252519
504.525472	51.659320	73.257524
504.052513	50.845561	73.262529
503.327530	51.194397	73.267534
502.603681	57.055619	73.272538
501.975681	55.677934	73.277543
500.674516	60.361973	73.282548
500.195992	54.664577	73.287553
499.766152	52.949007	73.292558
499.439322	57.553714	73.297562
498.610101	47.047614	73.302567
497.445855	52.646819	73.307572
496.990278	53.313418	73.312577
496.678956	57.719294	73.317582
495.963144	53.051715	73.322586
495.081380	42.191881	73.327591
493.941324	55.104941	73.332596
493.622428	44.973607	73.337601
493.449874	54.046090	73.342606
492.663714	52.065546	73.347610
492.145330	40.297179	73.352615
490.711182	49.017455	73.357620
490.320490	46.486804	73.362625
490.020655	48.123369	73.367630
489.150206	46.505012	73.372634
488.732082	47.477018	73.377639
487.780362	57.217858	73.382644
487.366718	48.676879	73.387649
487.303875	47.808633	73.392654
485.885361	48.962328	73.397658
485.069532	46.530975	73.402663
484.579863	43.972683	73.407668
483.607466	42.191018	73.412673
483.705130	50.616835	73.417678
482.639371	58.439171	73.422682
482.078964	45.500965	73.427687
481.453283	54.372823	73.432692
480.444755	42.313864	73.437697
479.115186	42.251994	73.442702
478.170613	39.796128	73.447706
478.894930	41.996888	73.452711
477.995683	34.788796	73.457716
477.796328	42.251090	73.462721
477.146918	51.765265	73.467726
475.558071	46.605886	73.472730
474.935752	41.584023	73.477735
474.226709	48.958409	73.482740
474.027058	39.852640	73.487745
473.829926	43.149929	73.492750
472.611093	44.336511	73.497754
471.943376	39.377294	73.502759
470.924818	48.543039	73.507764
470.642964	44.665527	73.512769
470.617430	42.525041	73.517774
469.632333	50.788658	73.522778
468.993438	41.686321	73.527783
468.331783	47.155985	73.532788
467.616005	49.037503	73.537793
466.561524	43.129359	73.542798
465.730631	52.898832	73.547802
465.306758	46.285421	73.552807
464.791323	52.175269	73.557812
464.133155	48.372111	73.562817
463.245443	46.605147	73.567822
462.458672	54.426252	73.572826
462.225497	44.103008	73.577831
461.326547	47.656346	73.582836
461.320571	51.053503	73.587841
460.299634	52.031318	73.592846
459.190324	46.721089	73.597850
458.864918	50.887813	73.602855
458.062699	53.558574	73.607860
457.322753	46.674084	73.612865
456.430794	51.717060	73.617870
455.705071	57.337043	73.622874
455.621584	47.779548	73.627879
455.008680	62.323235	73.632884
454.730005	46.762430	73.637889
454.121595	52.093902	73.642894
453.168391	51.678612	73.647898
452.352373	47.996843	73.652903
451.039416	50.547508	73.657908
450.210559	48.188653	73.662913
449.676661	48.718292	73.667918
449.219085	49.229721	73.672922
449.029339	43.947429	73.677927
448.547180	51.357537	73.682932
447.998167	42.519654	73.687937
447.128960	48.328029	73.692942
446.149157	51.499328	73.697946
445.785271	50.254012	73.702951
445.013762	53.856958	73.707956
444.328059	44.996317	73.712961
443.337097	48.720154	73.717966
442.515880	52.182811	73.722970
442.434197	42.951834	73.727975
442.001937	55.876231	73.732980
441.021152	44.681296	73.737985
440.068893	42.619890	73.742990
439.421600	51.061660	73.747994
439.116832	41.356182	73.752999
438.502294	50.111662	73.758004
437.920853	49.508726	73.763009
436.777992	40.654594	73.768014
436.027146	40.948271	73.773018
435.657781	40.651209	73.778023
435.045818	44.560346	73.783028
434.607569	43.624601	73.788033
433.570078	48.563842	73.793038
432.813290	54.026527	73.798042
432.672499	46.370720	73.803047
431.565955	42.111939	73.808052
430.125140	46.264954	73.813057
430.331807	40.257928	73.818062
429.463001	42.217382	73.823066
428.883033	40.071260	73.828071
428.309009	44.335453	73.833076
427.948051	44.009321	73.838081
427.680671	43.836880	73.843086
426.462912	41.311007	73.848090
426.004440	38.613964	73.853095
425.378775	47.118338	73.858100
424.412623	48.414384	73.863105
423.524402	40.177369	73.868110
422.896419	42.895244	73.873114
422.417239	42.689630	73.878119
421.934368	53.857537	73.883124
421.217381	38.107405	73.888129
420.347020	38.157107	73.893134
419.266207	53.952087	73.898138
419.257675	36.498929	73.903143
418.514155	45.714643	73.908148
418.519737	34.331345	73.913153
417.633172	43.701433	73.918158
416.242329	47.930357	73.923162
416.207725	42.847652	73.928167
415.075822	52.445305	73.933172
414.144693	38.490324	73.938177
413.134794	47.401974	73.943182
412.699216	46.354069	73.948186
412.375132	39.977764	73.953191
411.913759	46.869998	73.958196
411.766081	43.093833	73.963201
411.080205	41.116644	73.968206
409.975108	43.541702	73.973210
409.920773	42.508194	73.978215
408.792084	50.829187	73.983220
407.477089	47.486742	73.988225
406.906527	43.078485	73.993230
406.309983	48.340429	73.998234
406.580815	49.744997	74.003239
405.567157	51.572973	74.008244
405.228589	42.920468	74.013249
404.352261	50.846918	74.018254
403.156362	60.075041	74.023258
401.990240	49.243043	74.028263
401.536423	65.598439	74.033268
401.514749	50.401339	74.038273
400.998689	47.566149	74.043278
400.286236	52.528241	74.048282
399.468062	50.561489	74.053287
398.256664	60.527226	74.058292
397.912826	48.963422	74.063297
397.393263	44.549585	74.068302
397.156965	54.341892	74.073306
396.408978	47.028556	74.078311
395.246366	42.503884	74.083316
394.294643	48.195757	74.088321
393.948645	46.017436	74.093326
393.422921	48.225976	74.098330
393.113104	41.957747	74.103335
392.160495	49.812013	74.108340
391.023698	45.386333	74.113345
390.895642	43.529456	74.118350
389.984002	50.326368	74.123354
389.987855	39.797922	74.128359
388.496356	41.961593	74.133364
387.722696	41.817897	74.138369
387.530922	49.182188	74.143374
386.824727	45.709757	74.148378
386.540187	52.689707	74.153383
385.111195	47.833342	74.158388
384.515240	40.756836	74.163393
383.988416	41.786951	74.168398
383.494677	46.784187	74.173402
383.327296	42.559454	74.178407
382.371679	44.295386	74.183412
381.569697	47.457535	74.188417
381.124507	43.274097	74.193422
380.112112	49.834083	74.198426
379.340157	40.421038	74.203431
378.386530	49.930513	74.208436
378.246231	46.252553	74.213441
377.646340	39.877340	74.218446
377.037711	46.906910	74.223450
376.270458	38.737199	74.228455
375.230493	48.105953	74.233460
374.870289	53.223982	74.238465
374.426496	54.495642	74.243470
373.569380	48.632641	74.248474
373.246514	47.261494	74.253479
372.091406	48.134039	74.258484
371.420102	52.885410	74.263489
371.095110	55.062708	74.268494
370.480208	55.097453	74.273498
369.147765	47.168279	74.278503
368.516254	60.178530	74.283508
368.273814	45.629504	74.288513
367.388010	44.917697	74.293518
367.186158	49.928854	74.298522
366.774064	45.573966	74.303527
365.913695	49.994208	74.308532
365.265893	51.432667	74.313537
364.385797	49.157606	74.318542
363.592242	50.269356	74.323546
363.061337	46.502034	74.328551
362.387120	49.618606	74.333556
361.348953	34.879933	74.338561
361.209450	46.870381	74.343566
360.577936	49.336251	74.348570
359.604380	48.908285	74.353575
358.898188	50.577002	74.358580
358.567023	48.340093	74.363585
358.354686	45.178135	74.368590
356.757507	45.766865	74.373594
356.237231	47.754225	74.378599
355.537067	48.335658	74.383604
355.493399	47.857658	74.388609
355.068939	46.231967	74.393614
353.281027	50.497382	74.398618
353.014260	42.346497	74.403623
352.356477	48.548096	74.408628
352.089067	50.520538	74.413633
351.384461	45.979746	74.418638
350.154599	47.510070	74.423642
349.684489	42.848963	74.428647
348.586153	48.775563	74.433652
348.431766	41.284720	74.438657
348.186881	49.579767	74.443662
347.324642	52.316880	74.448666
346.723998	51.417660	74.453671
345.658351	48.767454	74.458676
345.204973	52.636791	74.463681
344.617346	43.420306	74.468686
343.085127	49.607969	74.473690
342.771524	41.510110	74.478695
342.009921	46.034209	74.483700
341.615303	49.634147	74.488705
341.644546	58.411527	74.493710
340.909748	50.733201	74.498714
340.847573	49.736562	74.503719
339.486952	53.228528	74.508724
338.806847	42.134060	74.513729
338.098081	41.250215	74.518734
336.950077	49.683469	74.523738
336.366552	43.601098	74.528743
335.609921	49.459267	74.533748
335.455332	40.365135	74.538753
334.903459	41.699135	74.543758
333.759384	45.173327	74.548762
333.437607	43.869098	74.553767
332.819965	53.711762	74.558772
332.331934	42.896988	74.563777
331.649246	49.239428	74.568782
330.325797	54.449134	74.573786
329.677934	39.328987	74.578791
329.122520	47.660282	74.583796
328.835022	51.398563	74.588801
328.442483	41.462240	74.593806
327.153886	47.018844	74.598810
326.712995	42.311288	74.603815
326.189225	49.246586	74.608820
325.558922	40.920790	74.613825
324.781948	39.320392	74.618830
323.424140	49.651469	74.623834
323.084072	40.145866	74.628839
322.926740	45.013609	74.633844
322.534698	42.209673	74.638849
321.446704	44.597083	74.643854
320.452728	51.528898	74.648858
320.059876	40.653213	74.653863
319.547370	46.919119	74.658868
318.607883	46.564266	74.663873
317.434996	46.839907	74.668878
317.099410	54.149903	74.673882
316.841038	45.718126	74.678887
316.132824	54.082323	74.683892
315.679005	47.823786	74.688897
315.546000	39.108435	74.693902
314.065134	47.942538	74.698906
313.726541	40.723258	74.703911
312.944767	50.967845	74.708916
311.969759	38.218770	74.713921
311.254412	40.892817	74.718926
310.633658	38.720547	74.723930
310.202046	44.887330	74.728935
309.979399	51.979821	74.733940
309.376723	42.640801	74.738945
308.224743	47.756387	74.743950
307.614171	53.919901	74.748954
307.207643	39.099036	74.753959
305.968287	46.178296	74.758964
304.887534	39.195163	74.763969
304.534228	51.086077	74.768974
303.966987	55.634103	74.773978
303.866000	43.990016	74.778983
302.878265	46.589575	74.783988
303.043864	50.116783	74.788993
301.878965	43.581466	74.793998
300.630296	48.141292	74.799002
300.688375	42.736412	74.804007
299.502525	45.988838	74.809012
298.774103	43.520437	74.814017
298.645998	47.457963	74.819022
297.752253	49.846030	74.824026
297.229623	51.333302	74.829031
296.058445	51.001981	74.834036
295.411314	51.654855	74.839041
294.805037	43.836890	74.844046
294.213463	49.203379	74.849050
294.319165	44.960660	74.854055
292.939021	51.947222	74.859060
291.869025	39.699537	74.864065
291.265633	43.893384	74.869070
290.745285	44.680833	74.874074
290.849899	39.517042	74.879079
290.248712	38.931720	74.884084
288.934740	49.508696	74.889089
288.345396	44.626076	74.894094
287.604300	51.645991	74.899098
287.410413	46.009182	74.904103
286.117145	48.832813	74.909108
285.475779	44.976680	74.914113
284.941912	38.839628	74.919118
284.203147	36.091969	74.924122
283.835856	43.565278	74.929127
283.113760	41.879302	74.934132
282.471370	39.912048	74.939137
281.675630	29.976566	74.944142
281.128502	42.185676	74.949146
280.828066	38.693453	74.954151
279.757677	43.356532	74.959156
278.481995	48.175978	74.964161
278.003261	37.946170	74.969166
277.533175	50.550609	74.974170
277.147595	41.318456	74.979175
276.409458	45.529875	74.984180
276.273501	36.201653	74.989185
275.790398	33.403858	74.994190
274.372945	48.051484	74.999194
274.216148	38.057794	75.004199
273.717610	46.141329	75.009204
272.413460	43.949236	75.014209
271.888731	38.142968	75.019214
271.825128	43.358175	75.024218
270.590720	42.194986	75.029223
269.708596	51.415918	75.034228
268.758455	46.595932	75.039233
268.345984	44.931093	75.044238
267.723141	45.194172	75.049242
267.674313	43.264120	75.054247
266.674613	42.807105	75.059252
265.392620	48.991763	75.064257
265.121273	38.842061	75.069262
264.400986	52.659316	75.074266
264.270239	48.125568	75.079271
263.510714	41.353027	75.084276
262.416020	49.476384	75.089281
261.863879	38.412108	75.094286
261.358132	39.344286	75.099290
261.301923	38.334786	75.104295
259.717263	38.140660	75.109300
258.978771	44.606741	75.114305
258.825922	39.077765	75.119310
257.819997	48.290313	75.124314
257.855223	41.401284	75.129319
256.394567	49.544741	75.134324
255.895257	38.664030	75.139329
255.917047	43.469492	75.144334
254.981791	44.601599	75.149338
253.692836	49.914743	75.154343
253.183680	47.226409	75.159348
252.335192	45.075026	75.164353
252.125944	36.307231	75.169358
251.545675	42.888683	75.174362
251.097595	42.145683	75.179367
249.922651	41.092695	75.184372
249.006762	40.036354	75.189377
248.880127	40.518309	75.194382
248.622070	43.796834	75.199386
247.398575	31.479568	75.204391
246.498181	42.094595	75.209396
246.080643	34.232847	75.214401
245.685689	33.857693	75.219406
245.169315	35.885047	75.224410
244.380216	27.695832	75.229415
243.686705	40.529206	75.234420
242.905549	42.448404	75.239425
242.103147	36.467121	75.244430
240.810137	47.265496	75.249434
240.291029	35.174443	75.254439
239.880724	42.679992	75.259444
239.195072	45.716436	75.264449
238.755895	49.497296	75.269454
238.103227	48.114801	75.274458
238.078715	34.857061	75.279463
237.374237	41.889646	75.284468
236.146727	43.956799	75.289473
235.662663	39.575980	75.294478
234.967220	45.283151	75.299482
234.133717	40.127807	75.304487
233.392374	52.039051	75.309492
232.783870	45.519297	75.314497
232.705625	43.588763	75.319502
232.080576	52.197640	75.324506
231.227271	41.942841	75.329511
230.417265	48.045418	75.334516
229.754059	50.327668	75.339521
228.547022	44.231019	75.344526
227.748038	50.331312	75.349530
227.381809	36.327328	75.354535
226.884843	45.917607	75.359540
226.008890	50.132131	75.364545
225.938825	40.784329	75.369550
225.194799	50.396040	75.374554
224.368593	49.332224	75.379559
223.478746	45.588165	75.384564
222.686451	48.807093	75.389569
222.778606	36.319176	75.394574
222.252837	45.468762	75.399578
221.113843	42.040553	75.404583
220.147557	41.076930	75.409588
219.752919	35.178904	75.414593
219.228390	34.925430	75.419598
217.853460	45.334849	75.424602
217.139557	43.997589	75.429607
216.938058	43.120752	75.434612
216.438959	41.394193	75.439617
216.389666	32.814500	75.444622
214.774143	48.249198	75.449626
214.399087	36.916567	75.454631
213.677562	36.084269	75.459636
212.998873	35.623157	75.464641
212.824382	33.441113	75.469646
211.636160	36.700279	75.474650
210.764117	30.134927	75.479655
210.252247	35.919175	75.484660
209.867595	46.838146	75.489665
209.681910	26.020482	75.494670
208.550854	44.847969	75.499674
207.955161	40.377348	75.504679
207.168614	41.087287	75.509684
206.492143	39.547441	75.514689
206.019526	34.626278	75.519694
205.235534	40.778471	75.524698
205.045430	39.493127	75.529703
204.611384	40.760366	75.534708
203.197601	47.031967	75.539713
202.342083	42.912577	75.544718
201.560211	47.640681	75.549722
201.098331	35.130115	75.554727
200.203070	40.892460	75.559732
199.576934	38.816256	75.564737
199.105106	30.802782	75.569742
198.203383	37.553410	75.574746
197.865112	37.727061	75.579751
197.486517	35.179767	75.584756
196.807470	37.281587	75.589761
195.751028	24.638887	75.594766
194.954078	38.307439	75.599770
194.610326	35.731279	75.604775
193.992164	39.402697	75.609780
193.394969	28.945736	75.614785
192.790513	36.390228	75.619790
191.687411	45.897317	75.624794
191.316842	38.265143	75.629799
191.078518	39.512252	75.634804
189.840380	43.585194	75.639809
188.535879	36.623481	75.644814
187.906895	39.728369	75.649818
188.303013	33.901230	75.654823
187.599046	40.943203	75.659828
187.051407	36.729992	75.664833
186.492726	38.986827	75.669838
185.331979	44.982569	75.674842
184.846720	38.618137	75.679847
184.563681	38.363532	75.684852
182.878639	30.023199	75.689857
182.172037	38.525269	75.694862
181.471971	40.336634	75.699866
181.097547	42.746610	75.704871
180.914164	40.137433	75.709876
180.555407	42.863257	75.714881
180.270459	29.476896	75.719886
179.089487	41.487574	75.724890
178.268816	34.935921	75.729895
177.024453	37.516340	75.734900
176.135712	37.435036	75.739905
175.747482	38.976248	75.744910
175.513391	41.538604	75.749914
175.220430	34.212847	75.754919
174.512659	41.166269	75.759924
173.098858	48.316115	75.764929
172.835567	39.331819	75.769934
172.156838	43.660951	75.774938
171.801099	43.764972	75.779943
171.212815	47.179840	75.784948
170.005060	49.040741	75.789953
169.375305	32.411323	75.794958
168.795259	58.627327	75.799962
168.259356	42.654006	75.804967
167.592111	38.908510	75.809972
166.361896	50.148475	75.814977
166.070661	33.018947	75.819982
165.289604	37.239707	75.824986
165.168082	36.478628	75.829991
164.775189	33.098183	75.834996
163.360355	43.855482	75.840001
163.053087	33.711960	75.845006
162.453956	44.948335	75.850010
161.869419	32.793918	75.855015
160.607386	36.514141	75.860020
159.738902	33.441791	75.865025
159.462147	34.307882	75.870030
159.024453	38.548723	75.875034
158.681254	35.244228	75.880039
157.520635	34.913896	75.885044
156.473720	35.934908	75.890049
156.157808	32.814802	75.895054
155.645041	44.849875	75.900058
155.406488	37.220337	75.905063
154.229195	42.147670	75.910068
153.285382	43.606507	75.915073
153.058034	36.799603	75.920078
152.508865	34.427994	75.925082
152.305580	36.851261	75.930087
150.760630	29.774084	75.935092
150.147134	41.839841	75.940097
149.671009	35.893825	75.945102
148.899544	44.289001	75.950106
148.501732	33.990882	75.955111
148.033893	35.375227	75.960116
146.700992	40.180826	75.965121
146.443197	34.954440	75.970126
146.070678	38.119176	75.975130
144.975902	40.588306	75.980135
144.178479	41.696016	75.985140
143.141698	41.111578	75.990145
142.761926	34.597238	75.995150
142.184534	38.649673	76.000154
141.680283	42.972580	76.005159
141.356171	42.539109	76.010164
140.815401	42.886813	76.015169
140.322183	38.834005	76.020174
139.291250	41.124440	76.025178
138.347403	36.346041	76.030183
137.944519	39.058510	76.035188
136.978464	49.667046	76.040193
136.421373	35.652779	76.045198
135.707465	47.653655	76.050202
135.308816	41.395560	76.055207
134.465241	37.962519	76.060212
133.391917	45.385562	76.065217
133.069095	35.487853	76.070222
132.625545	39.885611	76.075226
132.556909	31.801449	76.080231
131.135818	35.765644	76.085236
130.363137	40.837157	76.090241
129.747097	31.379694	76.095246
129.115460	40.747546	76.100250
128.941985	39.559218	76.105255
127.681552	40.256074	76.110260
126.646219	37.625598	76.115265
126.701543	39.839147	76.120270
126.180448	38.655153	76.125274
125.763829	38.338983	76.130279
124.802319	39.598372	76.135284
123.720826	45.705662	76.140289
123.231972	35.595643	76.145294
122.682706	42.010349	76.150298
122.155862	48.112548	76.155303
121.640088	42.253853	76.160308
120.768710	42.259578	76.165313
119.991156	37.153877	76.170318
118.811426	37.802560	76.175322
118.279351	43.513705	76.180327
117.671297	37.409138	76.185332
117.463094	37.087237	76.190337
116.991223	37.815081	76.195342
116.215742	41.934635	76.200346
115.175320	35.419092	76.205351
114.618255	32.051800	76.210356
113.839615	36.646338	76.215361
113.394497	28.267931	76.220366
112.484744	36.797333	76.225370
111.411956	34.959548	76.230375
111.098832	27.259127	76.235380
110.396679	46.768962	76.240385
110.097193	41.005418	76.245390
109.593933	44.929103	76.250394
109.065282	46.136785	76.255399
108.366410	30.877048	76.260404
107.356180	38.468869	76.265409
107.175664	40.129202	76.270414
106.331877	44.757017	76.275418
105.065372	39.196757	76.280423
104.498518	46.382591	76.285428
103.634040	45.199446	76.290433
103.786544	36.865018	76.295438
102.952430	41.765893	76.300442
102.308228	41.152053	76.305447
101.894285	47.765785	76.310452
100.888863	49.250193	76.315457
100.765296	43.162824	76.320462
99.195799	43.045885	76.325466
98.530297	43.313932	76.330471
98.355045	41.660939	76.335476
97.795688	40.725861	76.340481
97.194460	37.687832	76.345486
96.192932	39.724565	76.350490
95.397863	38.246909	76.355495
95.113668	38.041452	76.360500
93.625761	43.066258	76.365505
92.939338	38.206634	76.370510
92.319826	39.020972	76.375514
92.447605	37.043676	76.380519
91.866421	32.831890	76.385524
91.214530	42.005861	76.390529
90.542387	34.436065	76.395534
89.214137	44.560810	76.400538
88.582644	38.388430	76.405543
88.506482	32.441745	76.410548
87.821526	37.569270	76.415553
87.080831	46.067722	76.420558
85.822298	46.750054	76.425562
85.663421	38.573214	76.430567
85.111629	40.821379	76.435572
84.578343	48.524058	76.440577
83.910506	32.064213	76.445582
82.694027	43.735618	76.450586
82.057100	35.418122	76.455591
81.960026	33.757648	76.460596
80.947077	35.765948	76.465601
80.041549	41.835182	76.470606
79.182009	41.367599	76.475610
78.597532	44.455000	76.480615
78.347807	35.169598	76.485620
77.614703	45.848717	76.490625
77.475984	37.266211	76.495630
76.662704	48.930070	76.500634
75.891185	40.589466	76.505639
75.812168	40.578555	76.510644
74.033434	45.048135	76.515649
73.329415	32.197429	76.520654
72.272812	38.091655	76.525658
72.116436	37.522070	76.530663
71.795762	32.878412	76.535668
71.315704	41.232315	76.540673
71.182300	32.296818	76.545678
69.840470	41.909978	76.550682
69.018959	45.910334	76.555687
68.418421	42.460111	76.560692
67.856468	35.670325	76.565697
67.340343	34.436543	76.570702
66.013890	42.747676	76.575706
65.826930	41.578636	76.580711
65.060399	42.578042	76.585716
64.541757	46.933026	76.590721
64.108318	35.955020	76.595726
63.200362	42.791203	76.600730
62.469232	39.681114	76.605735
62.103207	43.854020	76.610740
60.895038	49.254797	76.615745
60.189629	46.602505	76.620750
59.438999	47.420382	76.625754
59.026716	42.060632	76.630759
58.865444	47.965955	76.635764
57.714570	52.308949	76.640769
57.542921	38.369531	76.645774
56.729453	43.408180	76.650778
56.161436	33.848163	76.655783
56.026784	40.601102	76.660788
54.819327	41.622031	76.665793
53.652131	33.406904	76.670798
52.662453	41.901469	76.675802
52.123536	48.031397	76.680807
51.995678	35.202299	76.685812
51.533562	39.844808	76.690817
50.440525	36.418243	76.695822
49.763189	45.767885	76.700826
49.130552	37.863713	76.705831
48.690642	42.198092	76.710836
48.207463	45.923351	76.715841
47.984562	36.116676	76.720846
46.770566	33.512906	76.725850
46.038913	35.145769	76.730855
45.162686	35.385614	76.735860
43.644254	47.257210	76.740865
43.650988	37.178678	76.745870
42.708055	45.907584	76.750874
42.547255	39.904363	76.755879
42.470171	38.430714	76.760884
41.951729	45.947307	76.765889
41.302449	39.433007	76.770894
40.245648	32.947137	76.775898
39.387315	30.629735	76.780903
39.349414	35.474230	76.785908
37.753257	46.958520	76.790913
36.915465	37.888417	76.795918
36.701442	41.085189	76.800922
36.057783	40.662701	76.805927
35.705067	43.177509	76.810932
34.590064	37.458675	76.815937
34.005792	41.745574	76.820942
33.344214	39.813622	76.825946
33.165719	43.974506	76.830951
32.331471	39.821907	76.835956
31.063220	44.297128	76.840961
30.659595	44.664748	76.845966
29.897976	41.983418	76.850970
29.709183	31.475813	76.855975
29.271459	38.177693	76.860980
28.123162	40.677340	76.865985
27.385342	40.879643	76.870990
26.640834	36.962696	76.875994
26.295756	42.832034	76.880999
25.575396	37.737074	76.886004
24.813599	39.523914	76.891009
24.129479	40.241188	76.896014
23.574858	39.222419	76.901018
23.210936	44.018215	76.906023
22.473252	38.119435	76.911028
21.127956	51.792421	76.916033
20.908447	31.935014	76.921038
20.546762	41.198168	76.926042
19.368578	45.016937	76.931047
18.714218	35.757109	76.936052
17.896804	41.765061	76.941057
17.594792	35.269774	76.946062
17.293396	39.854334	76.951066
16.685043	40.350210	76.956071
15.462312	37.540328	76.961076
14.644324	41.237342	76.966081
14.494259	35.029403	76.971086
13.739018	40.251482	76.976090
12.988650	50.909489	76.981095
12.221502	37.981601	76.986100
11.431258	45.317049	76.991105
11.187906	35.655588	76.996110
10.546716	40.445638	77.001114
9.579498	33.543784	77.006119
8.673380	39.949421	77.011124
7.581706	45.921117	77.016129
7.627981	44.486708	77.021134
7.301979	50.180290	77.026139
6.700299	38.376590	77.031143
5.820308	37.734513	77.036148
4.821115	42.158869	77.041153
4.597562	35.669472	77.046158