Tue Jun 08 17:17:48 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
0.114387	105.332514	0.000000
0.003416	85.769053	0.005005
-0.804627	51.146876	0.010010
-2.718126	11.437036	0.015014
-7.034583	6.928317	0.020019
-12.268801	2.770378	0.025024
-17.327398	7.108085	0.030029
-21.435748	5.103661	0.035034
-25.571921	2.802848	0.040038
-29.186333	-2.621963	0.045043
-33.213824	11.010434	0.050048
-37.035352	4.169395	0.055053
-39.471080	1.292429	0.060058
-43.995166	2.274252	0.065062
-47.365264	0.363115	0.070067
-51.798708	-2.294039	0.075072
-55.560073	-2.631861	0.080077
-59.281384	-14.857326	0.085082
-63.406384	5.879620	0.090086
-66.780373	-1.248118	0.095091
-70.138112	-7.920773	0.100096
-74.048900	-5.877325	0.105101
-77.811938	-2.782835	0.110106
-81.566176	3.913066	0.115110
-85.306654	-2.111353	0.120115
-89.273820	-0.572532	0.125120
-93.036619	1.863553	0.130125
-96.915722	-5.371736	0.135130
-100.785811	6.043467	0.140134
-104.219873	2.205709	0.145139
-108.231449	2.864460	0.150144
-111.668482	2.634080	0.155149
-115.126683	-7.357007	0.160154
-118.988534	-1.720183	0.165158
-123.047041	-3.697930	0.170163
-127.322371	1.919027	0.175168
-131.387551	-0.693052	0.180173
-134.940617	4.017733	0.185178
-138.673280	6.961020	0.190182
-141.957029	-0.217262	0.195187
-145.680078	3.435650	0.200192
-149.603142	2.839473	0.205197
-153.014439	0.558929	0.210202
-157.071452	-5.023929	0.215206
-160.757032	-2.597876	0.220211
-164.480409	-0.229280	0.225216
-168.122316	0.432436	0.230221
-171.604843	-9.053541	0.235226
-175.894020	8.658562	0.240230
-179.503528	0.921221	0.245235
-183.230442	-0.334973	0.250240
-187.104193	2.934503	0.255245
-190.870066	-2.878638	0.260250
-194.734827	6.390473	0.265254
-198.324283	-7.927339	0.270259
-202.003809	-3.729650	0.275264
-206.266283	5.231128	0.280269
-209.556221	-1.160565	0.285274
-213.145505	4.569709	0.290278
-216.968502	-8.685336	0.295283
-220.647646	-2.378369	0.300288
-224.473086	2.881267	0.305293
-228.532748	-4.756322	0.310298
-232.511632	4.525286	0.315302
-236.134332	-2.844240	0.320307
-239.729684	1.408511	0.325312
-244.126569	6.079777	0.330317
-247.374488	1.584197	0.335322
-251.376020	4.101223	0.340326
-254.698935	-2.666461	0.345331
-258.824708	-4.842135	0.350336
-262.364033	-5.269970	0.355341
-265.712621	-9.916411	0.360346
-269.953578	-0.287083	0.365350
-273.587189	-8.628449	0.370355
-277.218539	-1.567059	0.375360
-281.115160	5.201965	0.380365
-284.804467	0.536221	0.385370
-288.949645	-5.512933	0.390374
-292.525084	4.314871	0.395379
-296.136870	-8.222034	0.400384
-300.123365	0.425053	0.405389
-303.684771	-4.738236	0.410394
-307.659810	-3.107487	0.415398
-311.176696	0.777014	0.420403
-315.214630	-8.670404	0.425408
-318.954248	3.262540	0.430413
-322.451067	-7.717197	0.435418
-326.324276	2.235912	0.440422
-329.712005	-7.223954	0.445427
-333.797506	-6.435884	0.450432
-338.027761	6.009497	0.455437
-341.351352	-0.205408	0.460442
-345.278670	2.706309	0.465446
-348.905947	3.832996	0.470451
-352.638454	-0.762124	0.475456
-356.603721	-1.014982	0.480461
-360.131330	-4.765042	0.485466
-364.082226	-7.027848	0.490470
-367.409035	-9.191277	0.495475
-370.832526	-17.561885	0.500480
-374.663695	0.524523	0.505485
-378.604332	-6.220768	0.510490
-382.780550	-4.920942	0.515494
-386.707656	-8.550738	0.520499
-390.670183	-4.397505	0.525504
-394.152028	-5.778450	0.530509
-397.778615	-8.270927	0.535514
-401.910959	-8.174183	0.540518
-405.318864	-19.607611	0.545523
-409.232657	-11.617474	0.550528
-412.776753	-6.941971	0.555533
-416.378218	-18.452307	0.560538
-420.301054	-6.279065	0.565542
-424.256621	-11.482383	0.570547
-427.864740	-20.528189	0.575552
-431.779327	-7.988882	0.580557
-435.446865	-12.077608	0.585562
-439.223256	-5.765635	0.590566
-442.967042	-3.355027	0.595571
-446.561559	-2.051921	0.600576
-450.430491	-0.843827	0.605581
-454.195199	-7.253332	0.610586
-457.942285	-7.009885	0.615590
-461.687507	-9.464982	0.620595
-465.767894	-9.691281	0.625600
-469.457050	-7.382386	0.630605
-472.854959	-7.618014	0.635610
-476.724694	-4.279518	0.640614
-480.568847	-8.901942	0.645619
-484.372095	-8.606603	0.650624
-488.423980	-5.830093	0.655629
-491.432738	-6.733616	0.660634
-495.754227	-1.185774	0.665638
-499.199963	-3.215416	0.670643
-503.337368	-11.180811	0.675648
-506.986057	-3.464614	0.680653
-510.411610	-6.024251	0.685658
-514.667067	3.689479	0.690662
-518.489783	-5.914652	0.695667
-521.973070	-2.721367	0.700672
-525.882455	1.719685	0.705677
-528.698378	-13.466658	0.710682
-532.564341	0.785316	0.715686
-536.882403	-6.845519	0.720691
-540.662984	-10.230728	0.725696
-544.929658	3.584392	0.730701
-548.282196	-4.976257	0.735706
-552.137565	-2.266170	0.740710
-555.822850	-5.515360	0.745715
-559.303870	-9.058525	0.750720
-563.475881	-0.984087	0.755725
-567.261302	-1.877439	0.760730
-571.049336	3.231989	0.765734
-574.645229	-0.421313	0.770739
-578.072643	-5.738006	0.775744
-582.807214	0.770075	0.780749
-585.931659	-1.710521	0.785754
-589.550205	1.667462	0.790758
-593.605213	-10.297743	0.795763
-596.981349	-8.765957	0.800768
-600.707381	6.521455	0.805773
-604.636582	-7.317695	0.810778
-608.884203	-4.277769	0.815782
-612.132918	-6.060885	0.820787
-615.630062	-9.259024	0.825792
-619.568526	2.956923	0.830797
-623.417647	-14.091500	0.835802
-627.808505	-5.550801	0.840806
-631.196292	-1.600983	0.845811
-634.383691	-9.460869	0.850816
-638.578090	-4.538214	0.855821
-642.268309	-14.353627	0.860826
-645.998508	-3.678030	0.865830
-649.807841	1.287495	0.870835
-653.582894	-5.347007	0.875840
-657.557616	1.563608	0.880845
-660.784830	-3.605808	0.885850
-664.967059	-2.401390	0.890854
-668.764958	-7.088021	0.895859
-671.957700	-15.979906	0.900864
-676.843716	-1.584745	0.905869
-680.212441	-15.126076	0.910874
-684.224271	-2.082423	0.915878
-687.760819	-7.108340	0.920883
-690.916977	-11.538795	0.925888
-694.794754	-5.009893	0.930893
-698.406725	-8.676115	0.935898
-702.230138	-2.585188	0.940902
-706.235197	-5.384659	0.945907
-710.029572	-7.928199	0.950912
-713.663357	-8.348537	0.955917
-717.618458	-12.738556	0.960922
-721.690895	-2.525574	0.965926
-725.186918	-0.128046	0.970931
-728.309598	-6.045557	0.975936
-732.622120	-0.078671	0.980941
-736.326185	-10.009244	0.985946
-740.214297	-2.813054	0.990950
-743.907271	-2.820211	0.995955
-747.463206	-4.942440	1.000960
-751.526922	-6.204282	1.005965
-755.372617	-5.335413	1.010970
-759.420087	-5.406835	1.015974
-762.664969	-8.571180	1.020979
-765.996769	-8.780824	1.025984
-770.469158	-0.518477	1.030989
-773.645446	-3.968119	1.035994
-777.451975	-1.081104	1.040998
-781.439646	-7.722015	1.046003
-785.484705	-5.067190	1.051008
-789.257755	3.621416	1.056013
-792.669676	-5.754557	1.061018
-796.639298	-1.565812	1.066022
-800.296008	-2.016087	1.071027
-804.092142	-5.668763	1.076032
-808.032332	-0.707882	1.081037
-811.411615	0.029667	1.086042
-815.385238	8.406566	1.091046
-818.989737	1.201008	1.096051
-822.871234	-5.404012	1.101056
-826.877871	11.329383	1.106061
-830.585695	2.621553	1.111066
-834.311734	-0.355549	1.116070
-838.090081	0.819177	1.121075
-841.453730	-2.718243	1.126080
-844.940699	3.151247	1.131085
-848.911546	-3.259214	1.136090
-853.019802	0.735893	1.141094
-856.922322	9.020891	1.146099
-860.392214	-1.887589	1.151104
-864.403993	5.198892	1.156109
-867.877593	-3.358857	1.161114
-871.886737	-4.453123	1.166118
-875.932330	-1.165409	1.171123
-879.109371	-8.388631	1.176128
-882.943569	5.338715	1.181133
-886.734752	-0.724422	1.186138
-890.385227	3.850902	1.191142
-894.600994	3.727187	1.196147
-898.022564	-2.724627	1.201152
-902.017147	1.031949	1.206157
-905.445162	1.710837	1.211162
-909.406150	2.949345	1.216166
-913.182656	8.065363	1.221171
-916.622814	4.232871	1.226176
-920.816941	2.599660	1.231181
-924.683589	-5.371522	1.236186
-928.358317	-5.155092	1.241190
-932.042378	-0.551866	1.246195
-935.600330	1.061519	1.251200
-939.355052	6.888633	1.256205
-942.987751	-8.298460	1.261210
-946.706848	5.285235	1.266214
-950.714417	2.781275	1.271219
-954.882518	5.388700	1.276224
-958.418718	7.278217	1.281229
-962.002067	0.770553	1.286234
-965.719771	-2.080370	1.291238
-969.640309	4.394924	1.296243
-973.405224	-0.556805	1.301248
-976.943352	4.535312	1.306253
-980.474130	-5.534900	1.311258
-984.505858	-1.085479	1.316262
-988.424759	1.672599	1.321267
-991.908578	-0.513116	1.326272
-996.048223	1.952104	1.331277
-999.698138	-1.817463	1.336282
-1003.389345	0.734181	1.341286
-1007.324627	-4.446403	1.346291
-1010.922559	-8.584460	1.351296
-1014.727145	1.509364	1.356301
-1018.111705	-5.028824	1.361306
-1022.308305	8.307728	1.366310
-1026.153267	6.423634	1.371315
-1029.654933	-4.765787	1.376320
-1033.447446	2.334503	1.381325
-1037.331299	-6.771945	1.386330
-1041.103469	-5.712568	1.391334
-1044.763068	-5.077484	1.396339
-1048.496251	-8.711139	1.401344
-1052.248153	-1.680962	1.406349
-1055.709234	-8.261236	1.411354
-1059.750577	-7.152467	1.416358
-1064.291921	-1.798430	1.421363
-1067.665043	7.391683	1.426368
-1071.446203	2.114439	1.431373
-1074.745723	-7.046124	1.436378
-1078.565005	-5.560631	1.441382
-1082.199418	-10.633339	1.446387
-1086.191268	-6.502098	1.451392
-1090.295191	3.668447	1.456397
-1093.814627	-3.033212	1.461402
-1097.586982	1.858446	1.466406
-1101.337312	3.424876	1.471411
-1104.588028	-10.347889	1.476416
-1108.553086	5.565478	1.481421
-1112.576344	2.242985	1.486426
-1116.034783	6.951687	1.491430
-1120.133907	7.477587	1.496435
-1123.854265	-3.448421	1.501440
-1127.757822	0.172736	1.506445
-1131.333185	-4.578911	1.511450
-1135.016394	-6.494230	1.516454
-1138.929407	-9.780761	1.521459
-1142.260123	-6.527546	1.526464
-1146.586780	-3.565896	1.531469
-1150.068895	-7.397691	1.536474
-1154.087459	-7.381737	1.541478
-1157.549950	-0.300524	1.546483
-1161.112444	-1.295968	1.551488
-1165.005442	2.939940	1.556493
-1168.705964	-7.864699	1.561498
-1172.832861	-6.210647	1.566502
-1176.775910	5.569979	1.571507
-1180.526247	-0.290302	1.576512
-1184.158283	-2.679330	1.581517
-1187.619043	-10.618511	1.586522
-1191.141272	-3.243222	1.591526
-1195.146417	0.868298	1.596531
-1198.814660	-1.511736	1.601536
-1202.908318	3.409535	1.606541
-1206.315021	0.358193	1.611546
-1210.296342	-6.258904	1.616550
-1214.208467	3.920252	1.621555
-1217.947628	-5.169812	1.626560
-1221.565376	6.717207	1.631565
-1225.598633	1.759305	1.636570
-1229.023290	-2.628563	1.641574
-1233.130537	-0.778107	1.646579
-1236.358251	-6.636913	1.651584
-1240.440416	1.691092	1.656589
-1244.008157	-2.293272	1.661594
-1247.765249	-6.074993	1.666598
-1252.023827	0.342950	1.671603
-1255.237272	-7.174080	1.676608
-1259.325415	-2.110823	1.681613
-1263.523327	-1.946340	1.686618
-1266.761741	2.323272	1.691622
-1270.461605	0.055699	1.696627
-1273.741430	-14.427901	1.701632
-1277.650082	0.099171	1.706637
-1281.575314	-2.711874	1.711642
-1285.313030	-7.518383	1.716646
-1289.707976	1.008243	1.721651
-1293.179472	0.965495	1.726656
-1296.979524	5.183581	1.731661
-1300.550181	-2.044708	1.736666
-1303.956281	1.210527	1.741670
-1308.233647	8.119609	1.746675
-1311.477591	-6.812591	1.751680
-1315.663809	2.142383	1.756685
-1319.600798	0.416464	1.761690
-1323.131870	-0.564107	1.766694
-1327.039623	2.947825	1.771699
-1330.512051	-7.825967	1.776704
-1334.475732	3.151552	1.781709
-1338.292089	3.025589	1.786714
-1341.837803	-0.897345	1.791718
-1345.730065	1.115223	1.796723
-1349.124934	-6.129794	1.801728
-1353.372128	-0.558379	1.806733
-1356.955981	-2.440044	1.811738
-1360.535497	-2.193809	1.816742
-1364.556526	7.494617	1.821747
-1367.809088	-1.251422	1.826752
-1372.097672	3.272077	1.831757
-1376.024754	1.632924	1.836762
-1379.532856	2.017291	1.841766
-1383.527465	0.027802	1.846771
-1386.938280	-3.463170	1.851776
-1391.281027	5.737824	1.856781
-1394.741864	3.629023	1.861786
-1398.608682	-6.529106	1.866790
-1401.826209	1.294093	1.871795
-1405.708679	-3.634268	1.876800
-1409.681262	-1.172485	1.881805
-1413.521599	-0.406964	1.886810
-1416.660662	1.106440	1.891814
-1420.810891	6.004871	1.896819
-1424.287127	-7.709122	1.901824
-1428.476229	-0.787858	1.906829
-1432.594726	-1.266796	1.911834
-1436.050827	-7.944682	1.916838
-1439.758627	0.026710	1.921843
-1443.014143	8.524701	1.926848
-1447.095433	10.983091	1.931853
-1450.721875	-1.672923	1.936858
-1454.720987	6.453126	1.941862
-1459.082772	-5.468307	1.946867
-1462.414219	1.169077	1.951872
-1466.140886	0.852969	1.956877
-1469.962068	-4.735145	1.961882
-1473.473831	1.101190	1.966886
-1477.495536	3.032310	1.971891
-1480.948522	8.330046	1.976896
-1485.199515	6.148670	1.981901
-1488.272710	5.851749	1.986906
-1491.887063	7.712897	1.991910
-1495.965802	3.410005	1.996915
-1500.343958	-3.845427	2.006912
-1501.347671	5.443754	2.016909
-1498.381830	0.007952	2.026906
-1495.616549	5.116418	2.036902
-1493.238067	5.701377	2.046899
-1491.941423	4.797700	2.056896
-1489.667392	2.547193	2.066893
-1487.955196	3.426842	2.076890
-1485.934594	5.021003	2.086886
-1484.097370	1.233879	2.096883
-1482.243499	-1.355852	2.106880
-1480.261979	-4.978459	2.116877
-1478.107123	-1.273623	2.126874
-1476.426307	-2.895392	2.136870
-1474.763880	7.793223	2.146867
-1472.528200	1.697994	2.156864
-1470.858040	-3.720303	2.166861
-1468.923582	4.719075	2.176858
-1466.623355	0.784833	2.186854
-1465.115045	-2.548589	2.196851
-1463.412429	-2.974243	2.206848
-1461.320351	-5.558253	2.216845
-1459.225573	-4.879086	2.226842
-1457.739591	-6.393077	2.236838
-1455.777544	-3.586614	2.246835
-1453.844999	-4.693980	2.256832
-1451.574389	-0.951710	2.266829
-1449.878214	-3.804815	2.276826
-1447.945697	-2.219610	2.286822
-1446.484142	-3.133820	2.296819
-1444.640845	-5.587347	2.306816
-1442.384854	-4.302345	2.316813
-1440.645567	0.810108	2.326810
-1438.732659	-1.118681	2.336806
-1436.842433	-1.717643	2.346803
-1434.679608	1.602890	2.356800
-1433.400248	-7.067228	2.366797
-1431.262383	-4.657712	2.376794
-1429.056783	3.294054	2.386790
-1427.142559	3.713381	2.396787
-1425.662835	-0.911011	2.406784
-1423.502498	1.634159	2.416781
-1421.836889	0.058496	2.426778
-1419.998481	6.391731	2.436774
-1418.176800	1.207469	2.446771
-1415.921272	-5.788662	2.456768
-1414.350685	-6.079770	2.466765
-1412.446430	-6.513562	2.476762
-1410.363306	-3.121229	2.486758
-1408.761486	-1.034585	2.496755
-1406.904594	-2.762060	2.506752
-1404.754323	-3.989010	2.516749
-1402.908122	-4.397412	2.526746
-1401.011323	-3.190983	2.536742
-1398.904803	0.917411	2.546739
-1397.631769	-4.101850	2.556736
-1396.061207	-0.905614	2.566733
-1393.558306	-0.215504	2.576730
-1391.579181	-0.475609	2.586726
-1389.896859	1.752136	2.596723
-1387.694331	-1.647557	2.606720
-1386.148863	-2.591969	2.616717
-1384.171161	-2.468077	2.626714
-1382.387377	-2.431808	2.636710
-1380.588185	-3.761264	2.646707
-1378.444755	0.497304	2.656704
-1376.673231	-4.655007	2.666701
-1374.792515	1.024813	2.676698
-1372.773407	-1.250609	2.686694
-1370.996785	-4.171252	2.696691
-1369.181120	-4.816658	2.706688
-1367.243239	-5.446697	2.716685
-1365.611648	-7.418818	2.726682
-1363.494995	-1.740396	2.736678
-1361.703131	-3.739652	2.746675
-1359.788670	-0.246786	2.756672
-1357.631459	0.090918	2.766669
-1356.037300	-3.878880	2.776666
-1353.947966	-1.163787	2.786662
-1352.335489	1.210739	2.796659
-1350.364922	-2.503990	2.806656
-1348.634686	-10.498266	2.816653
-1346.854909	-0.300442	2.826650
-1344.531946	-5.834780	2.836646
-1342.883787	3.073163	2.846643
-1340.912963	0.734121	2.856640
-1339.095619	2.826852	2.866637
-1337.111380	4.413502	2.876634
-1335.516451	2.125591	2.886630
-1333.473085	5.520845	2.896627
-1331.439152	-0.302537	2.906624
-1329.854497	-0.939862	2.916621
-1327.553280	-4.981700	2.926618
-1325.781188	0.663845	2.936614
-1324.350604	-2.895283	2.946611
-1322.061179	1.182132	2.956608
-1320.383166	-1.063134	2.966605
-1318.467732	-4.990486	2.976602
-1316.881650	2.264692	2.986598
-1314.864277	7.208509	2.996595
-1312.840095	0.281010	3.006592
-1311.002802	-2.872139	3.016589
-1308.952103	5.154524	3.026586
-1307.082188	5.472835	3.036582
-1305.317727	0.102816	3.046579
-1303.255692	1.246526	3.056576
-1301.356552	-6.651466	3.066573
-1299.870744	-2.530069	3.076570
-1298.264324	2.830544	3.086566
-1296.084322	-0.207570	3.096563
-1293.854167	-4.713018	3.106560
-1292.112578	-5.130673	3.116557
-1290.356674	-0.472333	3.126554
-1288.664629	-5.977715	3.136550
-1286.391458	0.888745	3.146547
-1284.636837	-3.238614	3.156544
-1282.861731	-4.316491	3.166541
-1280.717359	0.149455	3.176538
-1278.626846	-3.822575	3.186534
-1277.321964	0.349667	3.196531
-1275.270366	-1.891770	3.206528
-1273.460390	-7.897977	3.216525
-1271.681200	-5.428747	3.226522
-1269.934817	-1.610956	3.236518
-1267.779809	2.597075	3.246515
-1265.785690	-5.648403	3.256512
-1263.840021	-3.798997	3.266509
-1262.421208	7.160791	3.276506
-1260.170251	-1.742562	3.286502
-1258.417615	-4.027495	3.296499
-1256.537709	-0.140545	3.306496
-1254.449690	-3.366769	3.316493
-1252.763736	-9.269069	3.326490
-1250.882743	-6.294451	3.336486
-1249.585378	-1.220223	3.346483
-1247.102399	-3.545616	3.356480
-1245.052235	-5.267881	3.366477
-1243.406396	-2.141027	3.376474
-1241.403999	-3.374510	3.386470
-1239.520477	-5.308045	3.396467
-1237.746867	-2.737852	3.406464
-1235.801416	-9.603973	3.416461
-1233.874946	-2.004499	3.426458
-1231.828621	-2.434945	3.436454
-1230.393863	-5.022148	3.446451
-1228.507622	-1.967006	3.456448
-1226.486395	-5.026032	3.466445
-1224.960102	-2.622820	3.476442
-1222.744564	-1.660750	3.486438
-1221.122189	2.332099	3.496435
-1218.796367	-0.366241	3.506432
-1216.769381	-0.505646	3.516429
-1215.342239	-2.816469	3.526426
-1213.667160	-1.822834	3.536422
-1211.618737	-8.551312	3.546419
-1209.291615	-0.595385	3.556416
-1207.357639	-8.353492	3.566413
-1205.994641	0.982103	3.576410
-1203.941255	1.845564	3.586406
-1202.118614	-3.366444	3.596403
-1200.389374	1.439584	3.606400
-1198.397033	1.271755	3.616397
-1196.532074	3.692303	3.626394
-1194.603566	3.492756	3.636390
-1192.891369	4.304157	3.646387
-1190.683247	-4.814311	3.656384
-1188.817340	-3.378394	3.666381
-1187.072668	-3.905219	3.676378
-1185.269543	0.034078	3.686374
-1183.426024	8.093628	3.696371
-1181.347972	0.679516	3.706368
-1179.370013	-5.059098	3.716365
-1177.577774	-4.882313	3.726362
-1175.733921	2.483981	3.736358
-1174.281257	-4.191970	3.746355
-1172.097221	-2.557742	3.756352
-1170.022233	0.303374	3.766349
-1168.515684	0.293283	3.776346
-1166.554661	-1.847974	3.786342
-1164.322015	-2.036108	3.796339
-1162.588832	0.586906	3.806336
-1160.865474	-4.173304	3.816333
-1159.114114	-0.048052	3.826330
-1156.872028	-0.051659	3.836326
-1154.971150	-2.597554	3.846323
-1153.383130	2.861529	3.856320
-1151.155934	-6.956955	3.866317
-1149.633057	-1.180001	3.876314
-1147.934406	-3.979670	3.886310
-1145.880865	-2.566469	3.896307
-1143.783677	1.248050	3.906304
-1142.148004	-10.216078	3.916301
-1140.066876	-9.713040	3.926298
-1138.424895	-4.873821	3.936294
-1136.259356	-5.712000	3.946291
-1134.665816	-3.562960	3.956288
-1132.352934	3.095219	3.966285
-1130.558390	-1.991794	3.976282
-1129.161810	-6.881627	3.986278
-1126.889946	-0.404522	3.996275
-1125.287926	-5.869887	4.006272
-1123.365241	-0.119289	4.016269
-1121.621751	1.881097	4.026266
-1119.312564	1.354189	4.036262
-1117.648009	2.256401	4.046259
-1115.646238	0.795047	4.056256
-1114.055329	-2.008240	4.066253
-1111.973255	4.929875	4.076250
-1110.133855	6.142739	4.086246
-1108.382458	5.616768	4.096243
-1106.361641	2.234581	4.106240
-1104.568954	7.401655	4.116237
-1102.507634	3.586477	4.126234
-1100.437704	7.478025	4.136230
-1098.765921	6.323114	4.146227
-1097.095089	2.810931	4.156224
-1095.395598	-1.712774	4.166221
-1093.123584	-0.172653	4.176218
-1091.640887	-5.359050	4.186214
-1089.506584	1.272119	4.196211
-1087.808612	2.672500	4.206208
-1085.749261	0.883127	4.216205
-1083.502451	-1.254208	4.226202
-1081.774697	5.471278	4.236198
-1080.032784	-2.218236	4.246195
-1078.411939	-6.194500	4.256192
-1076.322189	-2.232836	4.266189
-1074.682534	-5.651523	4.276186
-1072.660843	-3.356238	4.286182
-1070.453451	-4.781741	4.296179
-1069.022138	-7.343798	4.306176
-1066.950812	-2.060146	4.316173
-1065.051099	-7.321695	4.326170
-1063.282847	-6.202115	4.336166
-1061.446140	-1.678872	4.346163
-1059.261263	-8.605402	4.356160
-1057.818717	-4.132252	4.366157
-1055.432755	-2.646849	4.376154
-1053.593140	2.067181	4.386150
-1051.890277	0.762305	4.396147
-1050.252239	2.074190	4.406144
-1048.220283	-1.803503	4.416141
-1046.210730	-6.127097	4.426138
-1044.629920	-1.220027	4.436134
-1042.425135	6.336906	4.446131
-1040.757611	-0.223350	4.456128
-1039.029874	-4.905623	4.466125
-1036.988926	-8.172275	4.476122
-1034.982090	-4.985590	4.486118
-1033.008970	-0.408294	4.496115
-1031.241676	-4.329459	4.506112
-1029.392394	-7.795584	4.516109
-1027.765334	-1.306907	4.526106
-1025.477621	-4.284341	4.536102
-1024.445671	-3.714926	4.546099
-1022.273269	-6.939723	4.556096
-1019.874863	-8.225288	4.566093
-1018.113194	1.052212	4.576090
-1016.245096	-9.021124	4.586086
-1014.265120	-0.781779	4.596083
-1012.655787	-2.596609	4.606080
-1010.906029	-3.851029	4.616077
-1008.775780	0.308043	4.626074
-1006.750568	-2.781607	4.636070
-1005.009438	-1.072037	4.646067
-1003.252774	-2.144657	4.656064
-1001.248062	0.100225	4.666061
-999.240397	6.199104	4.676058
-997.495034	4.485021	4.686054
-995.596288	-0.333305	4.696051
-993.775715	0.125223	4.706048
-992.234794	3.097886	4.716045
-990.025047	-1.222117	4.726042
-988.181395	-0.242313	4.736038
-986.526496	-3.746978	4.746035
-984.267559	-7.223740	4.756032
-982.572665	1.122268	4.766029
-980.364633	1.190602	4.776026
-978.689964	-1.854661	4.786022
-976.909648	-2.941212	4.796019
-975.220614	1.641020	4.806016
-973.227169	1.701144	4.816013
-971.139512	7.985492	4.826010
-969.073873	7.487436	4.836006
-967.752203	3.353898	4.846003
-965.867593	0.378513	4.856000
-963.650597	-1.633103	4.865997
-961.438913	3.172414	4.875994
-960.082279	-0.900333	4.885990
-958.357119	0.555902	4.895987
-956.481193	-1.219706	4.905984
-953.967214	-2.344070	4.915981
-952.325889	1.203793	4.925978
-950.730336	-5.931757	4.935974
-948.913041	-1.033233	4.945971
-946.705463	0.405396	4.955968
-945.220802	-0.344647	4.965965
-943.271439	2.621544	4.975962
-941.167613	4.438817	4.985958
-939.568525	1.680029	4.995955
-937.426279	1.177531	5.005952
-935.429486	-2.506350	5.015949
-933.848483	2.441838	5.025946
-931.645680	3.763917	5.035942
-929.923641	2.104847	5.045939
-928.379981	-0.404527	5.055936
-926.280508	1.914629	5.065933
-924.398750	2.060345	5.075930
-922.278745	0.462983	5.085926
-920.709367	-4.219331	5.095923
-918.586357	-1.684475	5.105920
-916.882235	-0.236863	5.115917
-915.344489	-1.577365	5.125914
-913.111751	3.572351	5.135910
-911.035944	5.991220	5.145907
-909.160132	-0.223372	5.155904
-907.468294	-4.263539	5.165901
-905.739783	4.432034	5.175898
-903.374108	3.612572	5.185894
-901.620305	4.999494	5.195891
-900.276958	1.381167	5.205888
-898.056795	-1.866393	5.215885
-896.106663	0.777195	5.225882
-894.569828	6.851434	5.235878
-892.413812	0.086827	5.245875
-890.495087	-4.144440	5.255872
-888.757356	-5.001930	5.265869
-887.064460	-1.076375	5.275866
-885.232889	4.949247	5.285862
-883.058973	-2.269365	5.295859
-881.191052	1.077198	5.305856
-879.247323	-1.912252	5.315853
-877.750897	-2.342193	5.325850
-875.512126	1.135156	5.335846
-873.308395	-2.242363	5.345843
-871.471708	-4.057044	5.355840
-870.429849	-3.322908	5.365837
-868.151740	3.565884	5.375834
-866.150657	-1.207514	5.385830
-864.059236	-1.768437	5.395827
-862.491751	-1.792436	5.405824
-860.650994	-0.975697	5.415821
-858.791231	8.094163	5.425818
-856.858061	2.989381	5.435814
-854.793579	9.592361	5.445811
-853.053275	9.869888	5.455808
-851.088856	-0.672452	5.465805
-849.609738	5.400647	5.475802
-847.141634	0.601628	5.485798
-845.462639	5.167067	5.495795
-843.736236	-0.154363	5.505792
-841.578295	-0.220822	5.515789
-840.064479	0.005875	5.525786
-838.072980	5.159104	5.535782
-836.167929	3.127192	5.545779
-834.617023	1.491606	5.555776
-832.599111	3.428412	5.565773
-830.472295	-2.562862	5.575770
-828.540158	-0.816842	5.585766
-826.548156	2.824619	5.595763
-825.082969	0.651242	5.605760
-823.166072	-0.589901	5.615757
-820.962478	-1.751811	5.625754
-819.009383	1.923206	5.635750
-817.385856	2.861432	5.645747
-815.944598	2.590767	5.655744
-813.790382	2.649058	5.665741
-811.648112	-0.536876	5.675738
-809.956237	-3.450264	5.685734
-808.167528	4.004332	5.695731
-805.940174	-0.294894	5.705728
-804.217374	3.973748	5.715725
-802.257775	9.268031	5.725722
-800.564736	3.457930	5.735718
-798.810711	2.003278	5.745715
-796.551916	0.695952	5.755712
-794.455038	-4.253129	5.765709
-792.891805	4.117153	5.775706
-791.678233	5.304390	5.785702
-789.270472	2.242443	5.795699
-787.355191	-3.270261	5.805696
-785.393449	-6.670622	5.815693
-783.404274	-2.752008	5.825690
-782.157447	-5.231330	5.835686
-780.114850	-8.442823	5.845683
-777.730757	0.343822	5.855680
-776.104486	-7.376331	5.865677
-774.199713	-2.485230	5.875674
-772.426316	-6.370197	5.885670
-770.477533	-4.238118	5.895667
-768.742308	-1.635044	5.905664
-766.684483	-11.704107	5.915661
-764.953467	-3.940020	5.925658
-763.169808	-3.427633	5.935654
-760.839078	-7.620087	5.945651
-758.864382	-3.351583	5.955648
-757.317889	-8.067858	5.965645
-755.732965	-3.932827	5.975642
-754.035580	-5.713671	5.985638
-751.799158	-10.202942	5.995635
-749.650659	-7.251472	6.005632
-747.726304	-14.967840	6.015629
-746.312483	-2.773114	6.025626
-744.207288	-6.914600	6.035622
-742.353835	-6.746557	6.045619
-740.460463	-5.713130	6.055616
-738.650546	-9.139582	6.065613
-736.455990	-8.008850	6.075610
-734.921029	-7.075154	6.085606
-733.065616	4.012289	6.095603
-730.876747	-3.375605	6.105600
-729.165405	-6.439324	6.115597
-727.621141	1.261985	6.125594
-725.654894	10.303762	6.135590
-723.729406	4.803160	6.145587
-721.353254	5.124954	6.155584
-719.707991	1.719258	6.165581
-718.060397	3.748921	6.175578
-715.984291	4.293737	6.185574
-714.415937	1.233220	6.195571
-712.201416	11.563473	6.205568
-710.378620	2.502636	6.215565
-708.463218	-0.866029	6.225562
-706.723096	4.558448	6.235558
-704.705672	1.596339	6.245555
-702.864543	-7.967186	6.255552
-701.153066	2.294872	6.265549
-699.137855	4.385155	6.275546
-697.249753	3.284170	6.285542
-695.116513	1.348317	6.295539
-693.701334	3.219481	6.305536
-691.945848	4.765078	6.315533
-689.963271	-1.992204	6.325530
-688.046866	-0.136711	6.335526
-685.905412	5.466699	6.345523
-683.966550	2.756790	6.355520
-682.272590	6.311148	6.365517
-680.603018	4.671848	6.375514
-678.537689	0.525769	6.385510
-676.618524	2.231404	6.395507
-674.662205	2.306732	6.405504
-672.804789	2.110529	6.415501
-671.268794	-1.149535	6.425498
-669.169102	5.115524	6.435494
-667.672001	0.449247	6.445491
-665.186236	5.233980	6.455488
-663.497653	-4.504124	6.465485
-661.273258	-2.358824	6.475482
-659.933909	0.773843	6.485478
-657.982232	4.982326	6.495475
-656.076269	2.125127	6.505472
-654.021607	2.777593	6.515469
-652.266220	2.547135	6.525466
-650.211979	4.227626	6.535462
-648.629450	7.780965	6.545459
-646.818956	5.942809	6.555456
-644.934750	7.163603	6.565453
-642.699148	4.524909	6.575450
-641.031973	8.392939	6.585446
-639.164310	6.337883	6.595443
-637.139265	3.605695	6.605440
-635.127771	5.145323	6.615437
-633.785588	6.536994	6.625434
-631.594053	7.618108	6.635430
-629.385382	3.550997	6.645427
-628.205563	4.948795	6.655424
-626.168815	1.622178	6.665421
-623.844973	5.960468	6.675418
-622.297101	3.598676	6.685414
-620.731276	0.263160	6.695411
-618.657925	4.893027	6.705408
-616.379839	3.933036	6.715405
-614.809307	5.693783	6.725402
-612.896881	7.847590	6.735398
-610.984055	6.233364	6.745395
-609.051643	3.101318	6.755392
-607.247097	10.283369	6.765389
-605.485212	7.340648	6.775386
-603.498675	5.399186	6.785382
-601.599649	6.316699	6.795379
-599.810487	0.810688	6.805376
-597.692321	3.456017	6.815373
-595.862160	7.811456	6.825370
-594.420879	9.120134	6.835366
-592.299798	10.329550	6.845363
-590.039590	6.950375	6.855360
-588.242778	4.743089	6.865357
-586.728230	5.740811	6.875354
-584.605733	4.312332	6.885350
-583.118599	1.503713	6.895347
-580.687511	-0.072172	6.905344
-578.932246	10.633774	6.915341
-577.334429	6.748572	6.925338
-575.501599	8.354851	6.935334
-573.199915	6.410307	6.945331
-571.666849	1.933122	6.955328
-569.860305	4.459229	6.965325
-568.150259	9.363298	6.975322
-566.210421	8.513937	6.985318
-564.015708	3.557253	6.995315
-562.218890	3.041096	7.005312
-559.575284	6.660201	7.015309
-558.513855	6.588377	7.025306
-556.856144	3.044250	7.035302
-554.640617	8.298301	7.045299
-552.915136	3.159715	7.055296
-550.848062	8.658981	7.065293
-548.885291	9.173132	7.075290
-547.197261	6.513431	7.085286
-545.379590	13.361282	7.095283
-543.450663	0.663708	7.105280
-541.459715	6.256268	7.115277
-539.867312	5.356267	7.125274
-538.162291	10.024479	7.135270
-535.776876	4.450960	7.145267
-534.066576	5.020689	7.155264
-532.067863	9.887495	7.165261
-530.170152	11.782630	7.175258
-528.654552	7.502109	7.185254
-526.481989	5.828728	7.195251
-524.589280	3.886800	7.205248
-522.820170	5.696900	7.215245
-521.131092	1.206003	7.225242
-518.803929	6.551579	7.235238
-517.086926	6.179951	7.245235
-515.316482	0.972801	7.255232
-513.463024	3.686119	7.265229
-512.236272	7.159070	7.275226
-509.797550	8.037772	7.285222
-507.748768	2.400696	7.295219
-505.840219	3.318592	7.305216
-503.726408	6.041389	7.315213
-502.020695	9.255900	7.325210
-500.640728	7.139138	7.335206
-498.742462	6.490593	7.345203
-496.244107	3.663424	7.355200
-494.475031	6.297563	7.365197
-492.878017	2.280130	7.375194
-490.745815	2.650230	7.385190
-489.026784	4.754280	7.395187
-487.256969	7.021932	7.405184
-485.334006	7.563098	7.415181
-483.309465	6.797647	7.425178
-481.530383	13.026921	7.435174
-479.644337	6.270468	7.445171
-477.544156	0.714299	7.455168
-475.851063	5.537926	7.465165
-473.955679	2.001266	7.475162
-472.435010	3.597517	7.485158
-470.162616	6.900962	7.495155
-468.356157	9.924704	7.505152
-466.441269	7.032061	7.515149
-464.680729	7.716899	7.525146
-462.886727	6.033012	7.535142
-460.820769	5.940234	7.545139
-458.773878	6.945473	7.555136
-457.423795	-3.740320	7.565133
-455.192595	0.863340	7.575130
-453.315256	7.742493	7.585126
-451.413138	0.463193	7.595123
-449.492565	0.764494	7.605120
-447.647111	-1.854202	7.615117
-445.910594	-5.104333	7.625114
-444.105203	3.131290	7.635110
-441.956228	7.492571	7.645107
-440.286679	2.460447	7.655104
-438.403277	6.804849	7.665101
-436.728357	9.684391	7.675098
-434.437132	-3.618724	7.685094
-432.831836	-1.088463	7.695091
-430.759892	1.502437	7.705088
-428.747769	1.346191	7.715085
-426.966865	-0.393137	7.725082
-425.494830	0.661732	7.735078
-423.418791	1.025296	7.745075
-421.701206	2.200078	7.755072
-419.513113	3.717416	7.765069
-417.534526	5.299153	7.775066
-416.155638	9.061812	7.785062
-413.751093	1.109436	7.795059
-412.014855	2.008719	7.805056
-410.201602	-0.480735	7.815053
-408.116730	6.302764	7.825050
-406.525525	2.082029	7.835046
-404.657471	2.410144	7.845043
-402.707277	-0.726054	7.855040
-400.872713	1.127012	7.865037
-398.871465	-1.375324	7.875034
-397.185778	-6.535483	7.885030
-395.251905	-1.132248	7.895027
-393.247219	-1.543301	7.905024
-391.459796	-0.113718	7.915021
-389.388252	-2.868400	7.925018
-387.655507	0.180668	7.935014
-385.664992	-3.265569	7.945011
-384.208346	-0.752471	7.955008
-382.096409	1.033259	7.965005
-379.861964	7.984770	7.975002
-378.600664	-0.371007	7.984998
-376.631766	0.613266	7.994995
-374.603361	-4.997337	8.004992
-372.493811	-6.135385	8.014989
-370.875870	-3.632168	8.024986
-368.848842	-7.691710	8.034982
-366.841038	-9.153371	8.044979
-365.116748	-5.107695	8.054976
-363.602773	-6.609923	8.064973
-361.485863	-0.447246	8.074970
-359.324005	1.827111	8.084966
-357.628588	-0.515640	8.094963
-355.918971	-1.942743	8.104960
-353.849334	-0.352884	8.114957
-351.970018	-4.205677	8.124954
-350.422438	-3.630886	8.134950
-348.216060	2.145346	8.144947
-346.446933	1.445508	8.154944
-344.464986	-6.853662	8.164941
-342.618185	-0.018621	8.174938
-341.006896	2.112272	8.184934
-338.782549	1.495991	8.194931
-337.225720	-0.396148	8.204928
-334.933831	3.649006	8.214925
-333.024123	1.442607	8.224922
-331.469178	5.366378	8.234918
-329.579566	0.212755	8.244915
-327.493154	3.605091	8.254912
-325.634939	3.191133	8.264909
-323.947917	0.470032	8.274906
-322.356779	4.587181	8.284902
-320.291768	3.080948	8.294899
-318.418367	-0.693752	8.304896
-316.358943	-4.867119	8.314893
-314.339370	-4.011657	8.324890
-312.498588	-6.770589	8.334886
-310.726889	-6.801756	8.344883
-308.942118	-6.601197	8.354880
-306.939158	1.788330	8.364877
-305.192512	0.420104	8.374874
-303.238242	-0.437548	8.384870
-301.323425	-3.922539	8.394867
-299.358157	-10.491347	8.404864
-297.853303	1.431873	8.414861
-295.890829	-3.724749	8.424858
-294.011771	-6.378790	8.434854
-291.815764	-7.313076	8.444851
-289.994717	-8.780610	8.454848
-288.440075	-6.203270	8.464845
-286.313169	-2.398142	8.474842
-284.601855	-0.987868	8.484838
-282.628727	-3.643417	8.494835
-280.640130	-5.204106	8.504832
-278.860113	0.435831	8.514829
-277.027328	-3.715244	8.524826
-275.158046	-3.570665	8.534822
-273.143368	0.957993	8.544819
-271.143449	-10.704744	8.554816
-269.591544	-8.042747	8.564813
-267.705550	-2.031301	8.574810
-265.994467	1.293047	8.584807
-263.902348	-4.060881	8.594803
-261.836187	-2.232462	8.604800
-259.854722	-3.187636	8.614797
-258.178601	0.383002	8.624794
-256.340514	-8.262173	8.634791
-254.503678	-6.495591	8.644787
-252.708290	-0.191156	8.654784
-250.457914	0.899029	8.664781
-249.017380	-5.491232	8.674778
-247.194246	-4.464511	8.684775
-244.991209	-10.010558	8.694771
-243.031870	-6.774628	8.704768
-241.609538	-5.189883	8.714765
-239.496662	-8.228634	8.724762
-237.773988	-2.978800	8.734759
-235.267703	-4.795439	8.744755
-233.886721	2.042881	8.754752
-232.155214	-2.160761	8.764749
-229.832789	3.249029	8.774746
-228.354401	-4.175674	8.784743
-226.450540	-5.964074	8.794739
-224.505848	-1.034102	8.804736
-222.381723	-8.143513	8.814733
-220.669095	-0.865286	8.824730
-218.999642	3.462955	8.834727
-216.982078	-0.980634	8.844723
-214.942861	-4.237942	8.854720
-212.749956	-8.861386	8.864717
-211.211754	-10.901656	8.874714
-209.526622	-12.250205	8.884711
-207.664725	-10.208090	8.894707
-205.768025	-10.569317	8.904704
-203.578305	-10.349641	8.914701
-201.921227	-5.440284	8.924698
-200.151402	-11.625374	8.934695
-198.182759	-10.171068	8.944691
-196.203210	-9.188542	8.954688
-194.172765	-8.711924	8.964685
-192.666485	-15.959598	8.974682
-190.816958	-14.601448	8.984679
-188.750088	-10.103439	8.994675
-186.906667	-11.124620	9.004672
-185.153986	-4.877250	9.014669
-183.249927	-0.790001	9.024666
-181.329893	1.552400	9.034663
-179.449940	-3.911731	9.044659
-177.596636	-3.573482	9.054656
-175.411806	-4.689966	9.064653
-173.939439	-3.563535	9.074650
-172.048343	-3.198567	9.084647
-170.208166	-1.914685	9.094643
-167.961413	-1.379905	9.104640
-166.106064	1.976258	9.114637
-164.554728	-0.103401	9.124634
-162.488045	-0.929289	9.134631
-160.629531	0.124994	9.144627
-158.729981	-8.091607	9.154624
-156.997115	-5.672042	9.164621
-155.228023	-1.552149	9.174618
-153.188217	1.019895	9.184615
-151.319123	-0.022669	9.194611
-149.173162	-5.675081	9.204608
-147.438785	-4.757194	9.214605
-145.751457	-10.243211	9.224602
-143.811676	-4.493472	9.234599
-141.893034	1.110108	9.244595
-140.126697	-3.979621	9.254592
-138.034797	-6.991807	9.264589
-136.078034	-2.160295	9.274586
-134.418395	-5.107835	9.284583
-132.780172	-8.434270	9.294579
-130.637189	-12.908419	9.304576
-128.748628	-7.017098	9.314573
-126.865899	-11.488112	9.324570
-125.172663	-7.030727	9.334567
-123.181874	-6.573360	9.344563
-121.120750	-9.760874	9.354560
-119.382500	-4.505361	9.364557
-117.553263	-8.548666	9.374554
-115.842170	-6.646244	9.384551
-113.453031	-4.241192	9.394547
-111.814350	-1.066403	9.404544
-110.069135	-8.625362	9.414541
-108.096600	-2.685195	9.424538
-106.205657	-1.147173	9.434535
-104.331974	-3.559928	9.444531
-102.545687	-10.243410	9.454528
-100.693080	-3.102165	9.464525
-98.737052	-3.562446	9.474522
-96.941565	-4.863483	9.484519
-94.983108	-3.169463	9.494515
-93.201965	-2.073032	9.504512
-90.902327	-3.037246	9.514509
-89.086093	-6.314360	9.524506
-87.662322	-6.414220	9.534503
-85.745941	1.484793	9.544499
-83.640100	3.840430	9.554496
-81.674710	2.633175	9.564493
-80.360652	0.060691	9.574490
-78.126437	-2.028543	9.584487
-76.436513	4.809819	9.594483
-74.390904	-0.149536	9.604480
-72.535316	-6.040631	9.614477
-70.442375	-0.086313	9.624474
-68.963346	5.939294	9.634471
-67.080345	4.132007	9.644467
-65.017094	4.031181	9.654464
-62.948016	2.513298	9.664461
-61.113210	4.088632	9.674458
-59.278760	5.111120	9.684455
-57.615436	7.483371	9.694451
-55.661650	2.824323	9.704448
-53.558698	2.741197	9.714445
-51.587578	3.633545	9.724442
-50.244719	0.900415	9.734439
-48.137348	2.719104	9.744435
-46.160214	1.969090	9.754432
-44.326374	2.714248	9.764429
-42.473321	-1.090849	9.774426
-40.753989	-1.880439	9.784423
-38.663018	3.958437	9.794419
-36.752842	-0.521206	9.804416
-34.925833	0.463442	9.814413
-32.765777	3.875706	9.824410
-31.093466	5.047340	9.834407
-29.567693	4.901157	9.844403
-27.699542	-4.381450	9.854400
-25.385638	-8.636669	9.864397
-23.797621	-1.349632	9.874394
-21.852272	-1.143690	9.884391
-20.169072	-6.208056	9.894387
-17.977460	-3.020543	9.904384
-16.205407	-2.177041	9.914381
-14.284077	-1.851970	9.924378
-12.434178	-5.039582	9.934375
-10.493211	-1.206777	9.944371
-8.485822	-4.004438	9.954368
-6.946933	-2.709929	9.964365
-5.056349	-6.641196	9.974362
-3.638623	14.697325	9.984359
-2.435197	48.662661	9.994355
-0.992454	105.422763	10.004352
0.000000	153.174116	10.009357
0.433724	183.337305	10.014362
1.091502	216.317512	10.019367
1.810001	251.962375	10.024371
2.003319	271.256584	10.029376
2.208348	293.629189	10.034381
2.379352	305.249210	10.039386
2.126722	331.815283	10.044391
2.777744	333.716349	10.049395
2.792408	361.013053	10.054400
3.002145	362.319948	10.059405
3.323436	377.206218	10.064410
3.030015	392.694463	10.069415
3.245702	401.164523	10.074419
3.536283	405.717955	10.079424
3.510652	398.604368	10.084429
3.518861	403.646330	10.089434
3.538323	411.340863	10.094439
3.703105	408.683392	10.099443
3.648329	425.705687	10.104448
3.745655	440.040706	10.109453
4.036193	444.661654	10.114458
4.038117	448.655932	10.119463
4.235080	454.902999	10.124467
4.189949	464.039897	10.129472
4.159893	454.979877	10.134477
4.618892	465.767114	10.139482
4.121985	464.247000	10.144487
4.352650	453.067221	10.149491
4.215717	463.385473	10.154496
4.368025	467.295946	10.159501
4.909420	467.766406	10.164506
4.403078	460.199183	10.169511
4.325392	438.412811	10.174515
4.488909	451.287861	10.179520
4.285039	466.439125	10.184525
4.432445	467.684878	10.189530
4.425080	480.467678	10.194535
4.841706	474.886721	10.199539
4.449962	481.573413	10.204544
4.484858	485.744804	10.209549
4.792664	481.822182	10.214554
4.792418	501.117498	10.219559
5.107750	491.239577	10.224563
5.225948	498.298693	10.229568
5.540107	488.598600	10.234573
5.288542	488.396632	10.239578
5.097855	492.862089	10.244583
5.457326	497.159008	10.249587
5.291219	492.092027	10.254592
5.017409	500.288059	10.259597
5.419842	500.197367	10.264602
5.362247	498.104571	10.269607
5.484679	496.666937	10.274611
5.353077	495.701925	10.279616
5.526224	499.113850	10.284621
5.386365	499.289030	10.289626
5.355304	509.211015	10.294631
5.558619	496.706860	10.299635
5.485333	506.214913	10.304640
5.319979	505.614097	10.309645
4.922123	513.069193	10.314650
4.772042	516.077085	10.319655
5.402856	536.439333	10.324659
5.231687	545.291189	10.329664
5.188809	542.684301	10.334669
5.844735	554.953181	10.339674
5.836727	576.878788	10.344679
6.148152	574.365483	10.349683
6.070653	586.891982	10.354688
5.928143	586.758153	10.359693
6.316005	589.366330	10.364698
6.163879	590.505956	10.369703
6.331229	584.601396	10.374707
6.420095	591.255464	10.379712
6.388314	594.259270	10.384717
6.522518	588.600386	10.389722
6.488383	593.570330	10.394727
6.475181	595.013758	10.399731
6.438069	607.696371	10.404736
6.392711	601.478550	10.409741
6.340903	595.422490	10.414746
6.272870	600.334697	10.419751
6.515382	592.674928	10.424755
6.324078	601.276458	10.429760
6.462807	607.823696	10.434765
6.474017	606.077105	10.439770
6.705513	629.364182	10.444775
6.765940	635.217507	10.449779
6.821467	640.647738	10.454784
6.892859	639.498309	10.459789
7.010450	639.310013	10.464794
6.563163	646.691545	10.469799
7.042101	642.173108	10.474803
6.990883	644.995130	10.479808
6.959011	645.732834	10.484813
7.112121	646.350007	10.489818
6.996887	647.973957	10.494823
6.849621	652.642799	10.499827
6.892272	671.813736	10.504832
6.572372	676.797179	10.509837
7.321818	683.850377	10.514842
7.074328	685.799764	10.519847
7.286098	691.081251	10.524851
7.162042	715.043222	10.529856
7.468576	726.032042	10.534861
7.714557	716.320604	10.539866
7.391128	727.449019	10.544871
7.641322	721.286261	10.549875
7.624572	721.058237	10.554880
7.525325	730.655745	10.559885
7.872163	728.952248	10.564890
7.863050	735.253316	10.569895
7.658330	726.057301	10.574899
7.917375	735.797452	10.579904
7.754302	759.928810	10.584909
8.492908	759.227855	10.589914
8.117311	765.942293	10.594919
8.038500	764.438485	10.599923
8.156197	763.290186	10.604928
8.146160	769.868921	10.609933
8.258907	766.769530	10.614938
8.797425	777.065330	10.619943
8.777995	762.477481	10.624947
8.959053	765.120358	10.629952
8.628588	766.883854	10.634957
8.841350	762.335629	10.639962
8.268332	754.218782	10.644967
8.358277	763.404535	10.649971
8.299236	771.349544	10.654976
8.415596	770.144633	10.659981
8.818663	777.915676	10.664986
8.137821	778.113750	10.669991
8.639902	778.744118	10.674995
8.543201	776.634701	10.680000
8.258422	795.032998	10.685005
8.742265	813.525706	10.690010
8.606416	814.188090	10.695015
8.852683	818.943055	10.700019
8.693067	816.532188	10.705024
8.589226	822.517169	10.710029
8.955908	837.362545	10.715034
9.078800	857.657174	10.720039
9.615627	852.739940	10.725043
9.667023	859.623570	10.730048
9.480127	869.551583	10.735053
9.600177	856.669843	10.740058
9.174633	863.773014	10.745063
9.526530	865.142024	10.750067
9.226077	862.437538	10.755072
9.156683	870.210296	10.760077
8.954761	863.500931	10.765082
9.241317	874.649990	10.770087
9.390789	874.854116	10.775091
9.373681	885.259863	10.780096
9.179834	898.191031	10.785101
9.356444	885.148782	10.790106
9.448732	896.712084	10.795111
9.729105	912.424559	10.800115
10.209241	921.804026	10.805120
9.724904	934.208720	10.810125
9.749727	929.457016	10.815130
10.004471	945.718652	10.820135
9.925066	926.372934	10.825139
10.148169	930.989012	10.830144
10.000688	937.418490	10.835149
10.403048	930.569169	10.840154
10.164402	938.972951	10.845159
10.189995	935.938207	10.850163
10.188724	943.491690	10.855168
10.269671	955.738686	10.860173
10.682183	956.895207	10.865178
10.484827	969.214012	10.870183
10.878994	970.775520	10.875187
10.851949	969.805971	10.880192
10.791003	976.792599	10.885197
11.107659	968.450068	10.890202
10.547891	964.753057	10.895207
10.684578	958.541775	10.900211
10.777498	966.744642	10.905216
10.662675	977.033784	10.910221
11.179411	974.532186	10.915226
10.839953	985.268796	10.920231
11.087993	972.765671	10.925235
10.827392	974.869315	10.930240
10.929203	976.489241	10.935245
10.952471	975.695801	10.940250
10.868671	975.500586	10.945255
11.054029	980.442886	10.950259
11.017636	985.307157	10.955264
11.102394	999.470766	10.960269
11.199198	1009.637986	10.965274
11.025569	1017.562899	10.970279
11.015830	1006.709735	10.975283
11.233055	1020.555387	10.980288
11.233493	1018.951913	10.985293
11.352285	1011.982231	10.990298
11.329503	1030.824565	10.995303
11.538769	1039.108574	11.000307
11.945875	1043.654056	11.005312
11.844803	1048.804964	11.010317
11.739272	1045.655313	11.015322
11.962146	1050.620413	11.020327
11.928931	1043.622702	11.025331
12.045630	1043.989555	11.030336
11.932973	1043.947313	11.035341
11.973566	1047.819061	11.040346
12.165135	1055.846770	11.045351
12.104491	1054.205213	11.050355
12.445329	1047.831785	11.055360
11.923455	1053.028793	11.060365
12.236381	1051.302657	11.065370
12.130225	1051.661932	11.070375
11.976326	1051.154656	11.075379
12.074064	1059.106877	11.080384
12.136677	1073.505666	11.085389
12.596547	1075.157367	11.090394
12.396449	1080.255395	11.095399
12.463368	1078.998543	11.100403
12.526140	1090.593497	11.105408
12.515554	1101.848536	11.110413
12.578032	1091.623592	11.115418
12.253028	1095.353563	11.120423
12.358078	1095.110571	11.125427
12.631685	1098.016716	11.130432
12.714195	1112.383314	11.135437
13.028117	1113.634910	11.140442
13.087147	1129.778322	11.145447
13.066815	1116.875438	11.150451
13.297938	1120.077426	11.155456
13.230329	1125.465386	11.160461
13.107786	1121.017182	11.165466
13.037929	1118.597982	11.170471
13.006305	1125.848072	11.175475
13.360769	1121.417553	11.180480
13.059178	1134.361074	11.185485
13.279704	1122.223735	11.190490
13.351270	1132.188913	11.195495
13.536673	1126.814743	11.200499
13.699098	1133.350639	11.205504
13.437394	1133.915008	11.210509
13.739500	1135.611925	11.215514
13.512427	1132.400990	11.220519
13.469779	1130.884235	11.225523
13.967120	1129.749368	11.230528
13.295826	1141.078643	11.235533
13.498836	1134.016703	11.240538
13.485759	1142.798761	11.245543
13.572224	1148.449260	11.250547
13.822197	1155.771476	11.255552
13.964329	1167.904727	11.260557
14.206076	1157.415315	11.265562
14.069671	1168.043023	11.270567
14.026260	1163.677949	11.275571
14.211951	1162.513622	11.280576
14.061111	1167.620996	11.285581
14.341913	1164.114156	11.290586
14.045585	1172.767165	11.295591
14.036621	1166.025769	11.300595
14.311028	1163.078188	11.305600
14.281048	1166.715749	11.310605
14.075539	1169.274975	11.315610
14.328301	1171.090094	11.320615
14.517833	1189.898189	11.325619
14.929472	1197.998372	11.330624
14.830169	1197.743837	11.335629
15.097488	1176.382812	11.340634
14.910592	1172.685371	11.345639
14.506645	1162.904305	11.350643
14.957695	1159.828147	11.355648
14.296925	1173.146709	11.360653
14.608792	1181.360701	11.365658
14.772783	1197.219736	11.370663
14.887880	1200.818613	11.375667
15.108206	1196.836208	11.380672
15.214466	1203.733478	11.385677
15.190291	1209.467313	11.390682
15.117418	1206.971247	11.395687
15.071890	1203.889830	11.400691
15.596648	1200.948264	11.405696
15.369809	1201.383104	11.410701
15.516074	1205.334274	11.415706
15.366298	1205.625241	11.420711
15.721316	1204.847540	11.425715
15.582434	1208.654968	11.430720
15.524874	1203.940595	11.435725
15.790543	1198.537243	11.440730
15.812086	1207.566036	11.445735
15.990852	1200.239010	11.450739
16.010567	1206.590982	11.455744
15.681819	1210.537151	11.460749
16.040428	1206.722484	11.465754
15.696799	1201.659262	11.470759
15.362734	1205.011071	11.475763
15.335604	1212.178719	11.480768
15.353519	1217.413886	11.485773
15.712417	1207.233964	11.490778
15.379559	1220.290681	11.495783
15.671455	1235.379789	11.500787
16.116163	1238.393599	11.505792
16.127741	1246.503191	11.510797
16.373572	1237.679233	11.515802
15.949633	1237.839970	11.520807
15.977676	1230.933514	11.525811
16.417603	1235.745404	11.530816
16.324292	1241.308339	11.535821
16.377349	1235.106944	11.540826
16.408403	1231.968178	11.545831
16.446530	1239.898344	11.550835
16.653452	1236.045730	11.555840
16.466163	1241.590436	11.560845
16.737053	1234.365625	11.565850
16.657601	1244.720721	11.570855
16.849806	1259.320886	11.575859
17.222930	1259.309431	11.580864
17.185193	1241.858837	11.585869
17.417065	1231.921339	11.590874
16.993868	1226.789646	11.595879
17.074119	1232.728218	11.600883
17.106153	1233.870655	11.605888
16.805970	1234.740841	11.610893
17.168923	1233.479403	11.615898
17.083421	1239.544294	11.620903
17.445012	1229.934692	11.625907
17.261851	1222.976821	11.630912
16.795058	1234.400968	11.635917
17.229716	1231.661559	11.640922
17.047971	1229.286790	11.645927
17.167082	1252.115639	11.650931
17.741246	1256.824386	11.655936
17.239651	1269.394936	11.660941
17.568512	1265.485091	11.665946
17.858737	1265.652063	11.670951
17.589714	1263.839762	11.675955
17.571414	1258.428631	11.680960
17.526437	1259.958885	11.685965
17.687609	1261.830378	11.690970
17.644594	1260.708415	11.695975
17.647769	1268.894065	11.700979
17.732558	1259.787439	11.705984
17.609721	1270.999872	11.710989
17.706532	1264.183060	11.715994
18.100480	1271.226825	11.720999
17.791040	1267.057338	11.726003
18.066020	1285.517341	11.731008
17.988028	1303.428402	11.736013
18.007477	1296.088383	11.741018
18.103376	1300.264137	11.746023
18.048478	1306.893817	11.751027
18.434380	1307.229125	11.756032
18.244402	1307.875546	11.761037
18.436251	1306.998709	11.766042
18.073192	1308.139026	11.771047
18.565430	1309.150455	11.776051
18.756063	1305.472726	11.781056
18.361780	1304.902445	11.786061
18.608806	1306.927777	11.791066
18.477093	1313.485366	11.796071
18.376632	1308.254492	11.801075
18.967015	1323.796200	11.806080
18.841683	1333.980402	11.811085
18.920044	1332.853018	11.816090
18.895486	1333.720556	11.821095
18.951987	1333.675756	11.826099
19.170532	1332.721314	11.831104
18.638721	1337.564453	11.836109
18.677676	1325.497958	11.841114
19.095735	1335.421620	11.846119
18.999048	1341.450968	11.851123
19.023802	1329.917442	11.856128
19.283937	1339.474623	11.861133
19.178860	1329.222594	11.866138
19.192976	1333.325536	11.871143
19.369968	1330.453444	11.876147
19.758192	1333.361299	11.881152
19.565179	1338.282929	11.886157
19.936233	1329.242051	11.891162
19.523013	1332.210740	11.896167
19.548024	1326.054382	11.901171
19.834485	1326.482137	11.906176
19.886411	1325.519947	11.911181
19.534449	1324.739905	11.916186
20.016651	1329.268649	11.921191
20.488449	1330.982677	11.926195
20.255312	1330.377659	11.931200
20.279470	1329.198384	11.936205
20.472989	1326.115824	11.941210
20.032262	1309.406500	11.946215
19.901691	1308.305073	11.951219
20.020514	1297.294267	11.956224
20.132604	1305.293496	11.961229
20.087240	1311.894700	11.966234
19.583840	1319.181165	11.971239
19.717967	1333.518589	11.976243
19.974304	1324.964759	11.981248
19.934811	1333.722244	11.986253
20.048216	1323.550785	11.991258
20.008007	1344.127439	11.996263
20.215128	1355.357569	12.001267
20.363638	1358.316398	12.006272
20.603399	1357.577400	12.011277
20.918631	1350.458226	12.016282
21.109330	1355.174330	12.021287
21.059043	1350.971834	12.026291
20.897679	1326.039823	12.031296
20.663080	1329.733032	12.036301
20.416924	1316.975284	12.041306
20.651323	1321.157692	12.046311
20.779361	1326.780995	12.051315
20.604786	1325.231182	12.056320
20.348637	1326.172376	12.061325
20.707546	1321.277215	12.066330
20.680637	1324.585463	12.071335
20.498221	1326.105341	12.076339
20.920101	1317.750504	12.081344
20.474139	1332.999379	12.086349
20.951231	1325.091396	12.091354
20.884788	1330.791075	12.096359
20.686791	1329.165144	12.101363
20.708526	1326.850999	12.106368
20.540307	1331.049547	12.111373
20.509852	1331.078869	12.116378
20.664089	1336.414257	12.121383
20.760453	1330.276848	12.126387
20.768597	1330.934301	12.131392
20.478520	1330.579840	12.136397
20.703983	1323.951341	12.141402
20.836946	1320.831401	12.146407
20.327650	1315.902338	12.151411
20.711425	1303.448706	12.156416
20.194558	1309.511400	12.161421
20.408017	1315.624537	12.166426
20.654146	1325.900967	12.171431
20.375484	1334.682091	12.176435
20.985623	1323.986901	12.181440
20.769417	1330.086080	12.186445
20.464054	1325.819166	12.191450
20.580606	1318.088665	12.196455
20.234634	1313.837797	12.201459
20.879265	1326.170017	12.206464
20.644428	1321.893381	12.211469
20.639902	1316.757767	12.216474
20.692307	1307.862328	12.221479
20.293603	1312.542503	12.226483
20.472656	1300.620956	12.231488
20.749598	1312.430805	12.236493
20.668456	1308.041765	12.241498
20.721274	1301.883412	12.246503
20.522922	1300.797160	12.251507
20.480965	1303.996666	12.256512
20.341529	1306.395373	12.261517
20.535675	1296.756413	12.266522
20.683909	1299.012240	12.271527
20.606173	1311.408700	12.276531
20.690411	1298.655108	12.281536
20.355022	1305.760388	12.286541
20.286876	1302.505983	12.291546
20.652511	1317.536737	12.296551
20.737898	1322.584316	12.301555
20.729939	1308.393076	12.306560
20.399808	1312.819515	12.311565
20.473923	1307.072384	12.316570
20.601472	1305.907752	12.321575
20.493937	1310.911430	12.326579
20.753400	1302.268260	12.331584
20.912906	1319.163601	12.336589
20.675121	1316.629871	12.341594
20.505472	1312.102056	12.346599
20.354521	1315.446176	12.351603
20.797896	1314.410947	12.356608
20.677716	1316.787406	12.361613
20.297213	1308.467912	12.366618
20.666248	1322.032010	12.371623
20.713316	1322.343308	12.376627
20.992023	1320.265767	12.381632
20.874970	1321.589302	12.386637
20.894918	1316.215410	12.391642
21.089703	1315.061354	12.396647
20.964156	1322.526195	12.401651
20.913131	1301.178530	12.406656
20.781957	1297.626244	12.411661
20.410789	1289.258975	12.416666
20.642884	1285.557562	12.421671
20.271953	1285.963030	12.426675
20.568851	1294.448074	12.431680
20.628873	1290.831822	12.436685
20.156498	1286.189733	12.441690
20.462058	1300.933135	12.446695
20.345711	1320.730957	12.451699
20.968171	1322.922845	12.456704
20.774354	1307.115811	12.461709
20.515950	1299.618955	12.466714
20.420780	1291.976480	12.471719
20.307456	1293.737539	12.476723
20.690342	1313.866207	12.481728
20.668813	1322.157965	12.486733
20.109870	1306.750648	12.491738
20.416811	1316.038076	12.496743
20.294667	1329.399418	12.501747
20.908564	1322.300101	12.506752
20.668067	1324.196260	12.511757
20.705488	1327.911513	12.516762
20.769948	1325.260037	12.521767
20.562246	1321.518758	12.526771
20.896122	1313.384674	12.531776
20.487247	1308.164838	12.536781
20.519132	1294.316522	12.541786
20.525329	1290.875686	12.546791
20.286282	1297.623780	12.551795
20.497045	1307.501650	12.556800
20.670610	1326.643444	12.561805
20.614139	1324.600872	12.566810
20.844657	1310.795853	12.571815
20.491400	1302.362347	12.576819
20.639108	1296.285228	12.581824
20.705686	1294.749728	12.586829
20.338645	1282.693273	12.591834
20.689763	1291.845214	12.596839
20.463326	1295.025823	12.601843
20.711391	1289.714275	12.606848
20.734641	1295.356718	12.611853
20.446552	1293.432418	12.616858
20.443096	1289.719285	12.621863
20.670554	1300.412591	12.626867
20.864630	1304.336246	12.631872
20.668210	1307.370786	12.636877
21.097556	1299.558241	12.641882
21.199617	1296.964271	12.646887
21.075554	1302.340655	12.651891
21.075739	1288.144879	12.656896
20.905915	1273.949054	12.661901
20.757817	1269.607032	12.666906
20.841293	1258.007832	12.671911
20.365757	1259.755991	12.676915
20.352355	1262.302031	12.681920
20.310613	1271.745140	12.686925
20.271031	1269.103617	12.691930
20.302189	1264.526385	12.696935
20.221632	1277.513442	12.701939
20.744993	1293.051611	12.706944
20.687396	1297.042100	12.711949
20.579493	1303.083225	12.716954
20.632101	1292.759182	12.721959
20.570941	1300.704823	12.726963
20.633461	1293.304525	12.731968
20.361030	1290.401734	12.736973
20.629526	1305.074915	12.741978
20.716024	1300.269890	12.746983
20.243691	1295.884769	12.751987
20.596093	1299.888251	12.756992
20.630048	1309.334983	12.761997
20.631116	1305.495937	12.767002
21.069728	1292.295134	12.772007
20.649400	1285.524349	12.777011
20.775363	1275.229188	12.782016
20.935596	1278.048227	12.787021
20.789631	1277.522213	12.792026
20.791155	1270.429231	12.797031
20.170029	1273.947908	12.802035
20.449270	1269.937226	12.807040
20.186475	1277.265707	12.812045
20.391383	1272.786183	12.817050
20.483606	1265.393437	12.822055
20.789697	1275.809161	12.827059
20.581871	1273.697414	12.832064
20.389827	1277.310681	12.837069
20.661716	1272.265848	12.842074
20.778800	1279.429326	12.847079
20.342614	1278.906494	12.852083
20.442829	1273.662145	12.857088
20.342635	1279.397592	12.862093
20.506871	1282.557793	12.867098
20.625886	1276.701920	12.872103
20.543363	1280.652862	12.877107
20.564294	1273.629579	12.882112
20.798261	1278.307057	12.887117
20.496748	1277.817188	12.892122
20.490024	1281.939874	12.897127
20.255436	1281.611427	12.902131
20.450589	1276.853701	12.907136
20.511973	1294.881778	12.912141
20.580545	1307.786448	12.917146
20.849391	1307.193257	12.922151
20.486533	1302.093825	12.927155
20.418736	1287.738387	12.932160
20.843595	1304.985327	12.937165
20.550397	1301.188447	12.942170
20.706167	1294.269537	12.947175
20.569223	1289.366640	12.952179
20.506569	1281.155297	12.957184
20.568517	1290.799721	12.962189
20.370502	1289.202614	12.967194
20.520349	1286.290579	12.972199
20.308183	1289.795981	12.977203
20.745008	1296.441610	12.982208
20.395348	1313.955967	12.987213
20.780133	1306.700148	12.992218
21.001460	1304.097175	12.997223
20.474704	1294.224975	13.002227
20.604514	1285.949049	13.007232
20.608948	1285.981073	13.012237
20.695262	1280.012778	13.017242
20.918209	1290.493294	13.022247
20.944696	1286.426470	13.027251
20.780822	1279.554873	13.032256
20.614221	1292.834595	13.037261
20.468426	1290.609971	13.042266
20.776094	1277.650715	13.047271
20.306577	1293.988739	13.052275
20.651641	1284.762076	13.057280
20.521745	1291.127104	13.062285
20.426845	1289.641003	13.067290
20.774186	1279.046956	13.072295
20.574465	1289.644944	13.077299
20.651678	1280.005912	13.082304
20.370592	1294.701867	13.087309
20.593691	1291.336342	13.092314
20.467703	1285.372472	13.097319
20.532802	1288.800729	13.102323
20.576094	1284.101408	13.107328
20.666887	1289.608714	13.112333
20.325276	1288.040965	13.117338
20.894042	1290.369557	13.122343
20.304039	1292.867622	13.127347
20.565268	1289.397269	13.132352
20.492182	1284.016049	13.137357
20.545466	1295.733968	13.142362
20.890402	1285.579285	13.147367
20.675609	1294.985762	13.152371
20.638778	1289.618061	13.157376
20.432741	1292.646748	13.162381
20.471539	1294.594490	13.167386
20.756925	1286.081886	13.172391
20.340652	1292.551676	13.177395
20.784219	1285.779217	13.182400
20.355750	1291.504242	13.187405
20.349986	1291.127877	13.192410
20.452290	1300.339064	13.197415
20.487559	1291.937238	13.202419
20.542938	1292.151977	13.207424
20.631030	1293.901791	13.212429
20.584348	1296.892103	13.217434
20.604708	1297.943782	13.222439
20.489226	1298.167291	13.227443
20.517476	1297.035870	13.232448
20.902725	1295.804158	13.237453
20.947262	1294.025328	13.242458
21.181197	1299.391250	13.247463
21.144107	1295.376773	13.252467
20.791517	1285.772747	13.257472
20.661357	1272.513164	13.262477
20.448761	1263.212391	13.267482
20.777103	1256.735231	13.272487
20.599177	1268.111847	13.277491
20.519420	1263.225601	13.282496
20.629111	1265.570928	13.287501
20.345394	1265.030638	13.292506
20.626290	1260.917042	13.297511
20.638716	1271.265086	13.302515
20.482867	1262.968283	13.307520
20.190887	1261.652951	13.312525
20.442488	1265.080410	13.317530
20.501775	1263.058262	13.322535
20.628102	1266.308250	13.327539
20.872367	1266.275073	13.332544
20.818469	1259.373575	13.337549
20.607833	1273.374525	13.342554
21.087262	1268.973856	13.347559
20.740276	1272.344079	13.352563
20.955390	1263.295238	13.357568
20.857380	1263.318774	13.362573
20.484482	1273.271434	13.367578
20.582774	1266.776082	13.372583
20.520692	1280.445247	13.377587
20.755863	1274.806699	13.382592
20.403211	1269.782897	13.387597
20.254943	1273.388658	13.392602
20.281843	1267.413975	13.397607
20.322930	1271.982020	13.402611
20.612685	1266.138324	13.407616
20.676777	1269.491748	13.412621
20.689804	1278.289540	13.417626
20.804188	1266.635690	13.422631
20.133885	1282.349304	13.427635
20.514701	1271.975315	13.432640
20.624187	1277.834286	13.437645
20.348077	1280.346424	13.442650
20.469570	1275.220797	13.447655
20.438728	1282.085161	13.452659
20.312059	1279.556070	13.457664
20.524566	1282.626677	13.462669
20.295533	1279.007094	13.467674
20.438215	1272.373863	13.472679
20.338495	1287.644250	13.477683
20.202747	1278.526873	13.482688
20.431689	1294.180657	13.487693
20.308723	1301.579518	13.492698
20.599175	1300.927358	13.497703
20.391876	1312.116013	13.502707
20.250683	1310.768113	13.507712
20.513286	1318.831938	13.512717
20.393984	1319.237684	13.517722
20.536218	1310.881456	13.522727
20.661545	1315.806524	13.527731
20.438199	1311.900558	13.532736
20.803740	1316.019820	13.537741
20.961289	1311.531431	13.542746
21.009217	1313.423926	13.547751
20.831202	1326.376812	13.552755
20.902939	1307.253790	13.557760
21.051625	1293.446238	13.562765
20.718423	1291.311775	13.567770
20.762592	1281.278138	13.572775
20.542282	1283.985581	13.577779
20.384882	1282.684673	13.582784
20.655707	1276.689875	13.587789
20.161340	1282.461328	13.592794
20.726747	1274.821654	13.597799
20.569374	1279.566626	13.602803
20.470404	1280.565342	13.607808
20.383089	1280.883102	13.612813
20.385514	1284.279077	13.617818
20.407561	1287.739189	13.622823
19.969784	1288.026643	13.627827
20.264209	1303.460389	13.632832
20.530047	1311.269046	13.637837
20.729042	1316.870311	13.642842
20.767733	1312.733886	13.647847
20.553963	1318.348687	13.652851
20.575663	1314.165438	13.657856
21.051190	1314.394587	13.662861
20.595326	1303.798108	13.667866
20.643358	1285.829460	13.672871
20.294899	1289.511787	13.677875
20.359243	1292.320821	13.682880
21.147460	1306.083431	13.687885
20.559239	1297.869428	13.692890
20.765661	1284.849367	13.697895
20.712574	1285.528763	13.702899
20.604291	1280.774116	13.707904
20.889010	1285.284602	13.712909
20.620436	1281.824169	13.717914
20.670765	1283.763617	13.722919
20.642295	1292.800246	13.727923
20.489159	1278.791033	13.732928
20.806720	1292.651698	13.737933
20.479467	1293.518238	13.742938
20.487170	1282.509126	13.747943
20.679209	1293.684166	13.752947
20.415757	1289.190598	13.757952
20.431769	1289.781173	13.762957
20.338092	1297.016718	13.767962
20.622404	1288.367715	13.772967
20.512841	1289.235220	13.777971
20.628122	1290.639708	13.782976
20.850897	1283.118384	13.787981
20.722684	1291.418154	13.792986
20.832936	1285.864575	13.797991
20.428385	1288.832165	13.802995
20.743209	1296.907157	13.808000
20.862378	1286.334070	13.813005
20.694330	1297.160714	13.818010
20.737539	1284.738253	13.823015
20.839964	1287.197725	13.828019
20.509686	1284.638807	13.833024
20.402701	1278.075224	13.838029
20.443251	1279.133309	13.843034
20.419019	1286.553524	13.848039
20.678702	1287.989306	13.853043
20.362112	1291.441165	13.858048
20.461653	1298.752926	13.863053
20.275524	1296.927197	13.868058
20.714716	1298.065355	13.873063
20.646038	1297.377666	13.878067
20.251130	1297.909221	13.883072
20.709453	1295.689963	13.888077
20.669402	1304.331867	13.893082
20.493317	1297.542094	13.898087
20.295326	1294.786804	13.903091
20.460194	1297.790976	13.908096
20.814736	1297.110459	13.913101
20.512989	1304.504843	13.918106
20.441372	1299.139156	13.923111
20.694138	1300.963369	13.928115
20.375488	1297.925604	13.933120
20.729246	1285.297130	13.938125
20.745172	1294.507334	13.943130
20.585410	1293.580653	13.948135
20.413740	1290.193209	13.953139
20.471407	1290.464399	13.958144
20.651707	1293.795535	13.963149
20.800017	1297.699008	13.968154
20.736884	1289.091025	13.973159
20.455817	1300.874961	13.978163
20.659899	1299.410228	13.983168
20.694855	1299.971897	13.988173
20.378782	1300.077823	13.993178
20.931460	1300.032424	13.998183
20.623599	1307.718784	14.003187
20.688519	1299.405029	14.008192
20.891103	1294.003387	14.013210
20.360630	1282.079106	14.018227
20.467444	1274.932221	14.023245
20.792250	1282.785526	14.028263
20.273556	1289.764867	14.033280
20.600953	1300.882599	14.038298
20.286326	1299.540770	14.043315
20.675028	1305.014412	14.048333
20.566655	1299.388012	14.053351
20.528413	1313.092691	14.058368
20.836717	1297.214783	14.063386
20.355743	1303.126148	14.068403
20.443876	1303.352418	14.073421
20.516131	1305.105959	14.078439
20.452921	1306.948874	14.083456
20.890621	1304.333457	14.088474
20.707683	1311.819070	14.093491
21.066329	1310.903975	14.098509
20.762028	1309.254834	14.103527
20.668315	1314.651338	14.108544
20.744685	1315.284780	14.113562
20.798129	1339.467643	14.118579
20.919942	1338.836091	14.123597
21.265938	1345.103757	14.128615
20.877897	1342.825603	14.133632
21.154970	1341.992610	14.138650
21.023330	1347.651163	14.143667
21.658526	1339.805721	14.148685
21.385204	1318.061213	14.153703
20.831808	1320.892986	14.158720
21.361002	1311.472279	14.163738
20.809286	1312.079542	14.168755
21.012444	1313.787409	14.173773
21.293328	1311.653644	14.178791
20.903103	1319.555545	14.183808
21.314257	1318.016036	14.188826
21.507175	1351.538468	14.193843
21.438763	1319.718117	14.198861
21.258336	1321.641374	14.203879
21.185559	1321.360933	14.208896
21.498409	1303.392283	14.213914
21.337292	1312.009296	14.218931
21.241034	1314.230354	14.223949
21.224198	1313.557609	14.228967
21.066483	1314.464280	14.233984
21.327315	1315.550391	14.239002
21.487725	1336.170883	14.244019
21.754160	1335.638561	14.249037
21.412136	1316.365119	14.254055
21.102244	1324.464686	14.259072
21.269266	1329.633401	14.264090
21.417393	1348.093215	14.269107
21.015675	1345.605181	14.274125
20.949443	1346.752885	14.279143
21.217398	1348.230727	14.284160
21.216717	1345.610146	14.289178
20.841283	1349.955256	14.294195
21.520924	1366.004842	14.299213
21.620514	1379.709965	14.304231
21.328377	1374.170169	14.309248
21.585807	1368.108154	14.314266
21.403602	1376.240189	14.319283
21.202452	1381.758690	14.324301
21.741490	1380.594530	14.329319
21.617692	1383.798761	14.334336
21.706391	1375.977311	14.339354
21.230012	1378.917554	14.344371
21.580102	1374.669351	14.349389
21.836709	1373.050026	14.354407
21.759504	1378.200391	14.359424
22.090995	1370.656637	14.364442
21.485118	1373.428512	14.369459
21.617936	1384.564705	14.374477
22.218615	1393.867760	14.379495
22.021162	1407.525798	14.384512
21.970745	1394.618244	14.389530
21.944795	1391.296014	14.394547
21.761099	1398.011250	14.399565
22.183847	1403.674384	14.404583
21.974514	1412.004809	14.409600
22.261570	1411.068516	14.414618
21.914352	1398.224843	14.419635
22.164248	1394.790348	14.424653
22.075090	1385.455539	14.429671
21.928250	1406.633971	14.434688
22.232826	1413.986432	14.439706
22.295945	1410.409532	14.444723
22.011265	1407.469489	14.449741
22.034820	1403.280022	14.454759
22.250364	1417.220833	14.459776
22.132606	1405.839927	14.464794
22.208691	1411.539272	14.469811
21.928793	1407.267176	14.474829
22.182818	1414.514513	14.479847
22.092055	1419.753839	14.484864
22.093766	1406.158531	14.489882
22.175008	1404.204275	14.494899
22.333629	1414.434008	14.499917
22.351944	1398.050153	14.504935
22.149387	1414.968051	14.509952
22.343583	1405.649613	14.514970
22.286942	1410.960257	14.519987
22.056689	1412.158138	14.525005
22.297234	1411.868072	14.530023
22.570249	1429.330489	14.535040
22.299053	1425.774289	14.540058
22.625525	1442.453463	14.545075
22.619125	1434.436852	14.550093
22.661261	1429.737055	14.555111
22.527282	1440.376853	14.560128
22.618727	1433.507755	14.565146
22.830301	1437.487647	14.570163
22.801572	1435.020694	14.575181
23.035630	1437.210727	14.580199
23.113073	1421.997142	14.585216
23.079897	1415.243523	14.590234
22.938389	1415.079206	14.595251
22.739300	1399.257087	14.600269
23.272037	1397.901074	14.605287
22.942722	1410.658012	14.610304
23.103181	1408.835856	14.615322
22.828352	1405.029866	14.620339
22.793267	1405.642261	14.625357
23.336396	1407.713541	14.630375
22.895203	1401.754761	14.635392
23.068040	1402.271657	14.640410
22.829650	1400.298183	14.645427
22.703385	1400.526566	14.650445
22.842147	1403.937381	14.655463
22.787933	1403.012748	14.660480
22.987498	1400.580679	14.665498
23.007800	1403.397573	14.670515
22.697533	1398.639299	14.675533
22.957015	1404.970254	14.680551
22.882943	1404.094305	14.685568
23.239969	1404.841850	14.690586
23.472728	1404.845273	14.695603
23.417903	1406.924582	14.700621
23.352204	1403.108721	14.705639
23.329436	1403.593795	14.710656
23.046965	1412.005665	14.715674
23.247594	1408.760341	14.720691
23.081221	1414.472910	14.725709
23.140413	1416.367693	14.730727
23.230061	1416.856723	14.735744
23.033359	1411.000522	14.740762
23.291900	1406.773126	14.745779
23.159966	1417.828347	14.750797
23.457668	1408.915036	14.755815
23.282880	1418.588492	14.760832
22.956362	1414.963820	14.765850
23.083173	1409.638428	14.770867
22.732542	1423.533394	14.775885
22.966170	1435.802058	14.780903
22.916014	1443.430337	14.785920
23.143633	1444.031945	14.790938
23.199044	1441.108000	14.795955
23.076462	1460.204579	14.800973
23.249451	1462.408236	14.805991
23.775495	1467.679629	14.811008
24.016160	1464.654618	14.816026
24.002817	1455.332361	14.821043
24.048677	1447.707610	14.826061
24.103248	1432.794816	14.831079
24.203162	1429.714803	14.836096
24.003607	1423.544487	14.841114
23.966060	1412.867216	14.846131
23.780811	1426.247166	14.851149
23.931617	1427.548233	14.856167
23.828741	1425.093600	14.861184
23.903732	1421.906433	14.866202
23.986793	1420.551135	14.871219
24.009634	1417.763106	14.876237
23.877346	1425.199533	14.881255
24.100547	1430.261002	14.886272
23.811491	1426.756294	14.891290
23.960736	1425.788900	14.896307
23.693108	1427.847212	14.901325
24.348986	1420.636042	14.906343
24.121212	1430.697763	14.911360
23.957259	1434.180569	14.916378
24.256029	1429.083192	14.921395
24.005929	1434.623885	14.926413
23.901596	1419.677319	14.931431
24.102570	1428.055130	14.936448
24.174382	1423.612478	14.941466
24.531686	1419.627226	14.946483
24.027264	1426.217527	14.951501
24.232540	1420.886552	14.956519
24.181140	1422.409314	14.961536
24.065813	1418.847653	14.966554
23.936564	1421.999277	14.971571
24.027928	1423.084529	14.976589
24.034770	1417.852545	14.981607
24.170256	1421.594274	14.986624
23.956558	1418.318797	14.991642
24.565785	1418.356894	14.996659
23.922094	1420.408418	15.001677
24.387818	1417.688955	15.006695
24.181021	1416.738509	15.011712
24.130717	1436.895214	15.016730
24.348115	1445.315104	15.021747
24.199033	1451.511384	15.026765
24.326367	1455.301768	15.031783
24.692586	1458.103065	15.036800
24.407983	1458.714933	15.041818
24.755642	1456.881936	15.046835
24.764761	1462.740829	15.051853
24.460828	1457.807417	15.056871
24.836138	1458.499463	15.061888
24.239705	1461.809159	15.066906
24.683630	1454.889853	15.071923
24.535856	1459.104217	15.076941
24.301156	1458.088860	15.081959
24.399208	1463.102106	15.086976
24.333125	1463.224098	15.091994
24.594797	1480.461329	15.097011
24.840495	1495.378243	15.102029
24.845319	1490.328490	15.107047
25.164068	1493.790362	15.112064
24.919352	1495.165944	15.117082
24.959253	1492.893535	15.122099
24.922969	1490.208160	15.127117
25.273027	1493.689470	15.132135
24.983529	1493.728497	15.137152
24.916559	1489.280879	15.142170
25.375121	1486.392537	15.147187
24.770675	1471.639950	15.152205
25.175861	1478.517270	15.157223
25.545413	1474.034972	15.162240
24.661104	1468.349013	15.167258
25.210909	1472.938312	15.172275
25.040315	1473.539294	15.177293
25.251944	1479.197706	15.182311
25.373559	1477.751138	15.187328
25.128473	1471.856748	15.192346
25.367585	1460.802053	15.197363
25.271001	1473.260449	15.202381
25.369880	1468.074486	15.207399
25.348348	1458.856397	15.212416
24.957039	1469.825011	15.217434
25.339845	1472.583306	15.222451
25.348556	1487.689286	15.227469
25.616580	1491.311052	15.232487
25.804042	1491.242707	15.237504
25.430402	1490.777603	15.242522
25.415702	1469.290934	15.247539
25.433778	1475.160108	15.252557
25.199799	1477.363853	15.257575
25.443065	1483.025110	15.262592
25.379739	1502.936469	15.267610
26.012192	1493.518030	15.272627
25.551984	1487.757379	15.277645
25.375335	1500.567355	15.282663
25.566928	1490.564596	15.287680
25.420824	1494.486133	15.292698
25.584903	1489.579958	15.297715
25.590192	1494.051580	15.302733
25.509258	1490.948621	15.307751
25.580961	1485.233398	15.312768
25.492928	1490.168704	15.317786
25.769082	1488.503492	15.322803
25.549696	1493.681816	15.327821
25.837141	1500.634458	15.332839
25.717492	1488.440345	15.337856
25.549189	1494.197373	15.342874
26.049401	1507.300397	15.347891
26.087044	1514.043094	15.352909
26.254812	1520.645753	15.357927
26.110793	1497.597587	15.362944
25.907869	1496.209419	15.367962
26.195210	1488.300700	15.372979
26.120454	1493.253024	15.377997
26.202763	1492.240403	15.383015
26.392703	1483.306941	15.388032
26.191483	1495.953392	15.393050
26.012341	1475.789138	15.398067
26.011544	1481.493029	15.403085
25.623095	1481.893545	15.408103
25.970785	1493.119365	15.413120
25.806721	1516.262519	15.418138
26.090150	1518.913832	15.423155
26.303701	1514.950842	15.428173
26.081625	1512.701298	15.433191
26.427375	1514.722963	15.438208
26.513391	1518.480678	15.443226
26.306980	1522.374763	15.448243
26.310828	1522.480040	15.453261
26.013142	1522.458653	15.458279
26.319375	1521.079256	15.463296
26.261441	1511.248415	15.468314
26.232211	1518.168739	15.473331
26.256511	1521.957904	15.478349
26.720051	1537.578924	15.483367
26.748283	1531.895156	15.488384
26.409419	1540.414805	15.493402
26.608226	1537.539885	15.498419
26.472762	1543.234995	15.503437
26.531111	1549.283926	15.508455
27.105355	1538.586326	15.513472
26.787872	1540.275208	15.518490
26.969491	1537.238651	15.523507
26.659378	1524.565695	15.528525
26.601265	1531.464595	15.533543
26.905047	1529.805273	15.538560
26.878732	1537.101129	15.543578
27.233648	1530.671905	15.548595
27.047288	1518.565198	15.553613
26.842466	1518.772797	15.558631
26.899855	1509.978987	15.563648
26.792768	1518.377380	15.568666
27.122833	1526.590575	15.573683
26.812833	1524.931363	15.578701
27.132816	1537.555025	15.583719
27.311845	1526.458612	15.588736
27.191006	1524.694124	15.593754
26.906545	1511.663200	15.598771
27.554317	1515.313571	15.603789
27.323270	1514.189305	15.608807
27.481758	1496.505983	15.613824
27.261896	1499.526293	15.618842
26.983287	1501.757775	15.623859
26.974379	1504.409992	15.628877
26.873170	1503.583578	15.633895
27.507791	1512.779694	15.638912
27.077223	1520.585846	15.643930
27.210368	1525.959668	15.648947
27.639740	1528.319003	15.653965
27.156586	1529.835481	15.658983
27.317384	1532.139674	15.664000
27.346876	1534.614821	15.669018
27.171060	1535.295056	15.674035
27.126913	1538.450618	15.679053
27.600571	1536.346770	15.684071
27.944181	1531.230647	15.689088
27.728345	1535.820519	15.694106
27.741505	1533.959031	15.699123
27.965455	1526.068249	15.704141
27.846707	1536.792911	15.709159
28.143002	1521.874418	15.714176
27.567878	1514.770718	15.719194
27.649603	1505.056894	15.724211
27.817229	1504.526547	15.729229
27.587004	1514.939172	15.734247
27.566640	1510.023666	15.739264
27.659447	1520.430912	15.744282
27.696687	1524.907697	15.749299
28.210380	1532.296414	15.754317
27.943170	1534.670055	15.759335
27.828946	1537.102121	15.764352
27.615805	1531.377840	15.769370
27.592870	1532.754379	15.774387
27.953537	1534.710884	15.779405
27.791580	1532.766811	15.784423
27.935264	1523.131733	15.789440
28.208700	1536.456362	15.794458
27.736979	1537.585013	15.799475
27.971738	1542.557913	15.804493
27.663208	1539.307726	15.809511
27.974480	1538.766923	15.814528
28.022393	1536.500615	15.819546
28.021957	1549.807640	15.824563
28.339031	1556.774126	15.829581
28.357867	1573.957811	15.834599
28.389024	1560.327395	15.839616
28.518872	1547.209654	15.844634
28.008084	1550.323955	15.849651
28.234653	1554.124910	15.854669
28.057731	1569.741196	15.859687
28.047269	1570.276139	15.864704
28.309452	1568.371950	15.869722
28.053365	1571.630006	15.874739
28.656917	1568.944373	15.879757
28.504751	1575.654279	15.884775
28.328722	1573.139323	15.889792
28.432590	1562.953507	15.894810
28.330733	1575.250272	15.899827
28.789917	1568.716138	15.904845
28.317741	1572.448300	15.909863
28.735539	1568.858982	15.914880
28.483287	1568.861698	15.919898
28.668224	1582.531103	15.924915
28.859061	1584.545083	15.929933
28.939459	1594.580056	15.934951
29.259007	1582.621623	15.939968
28.775278	1564.069098	15.944986
28.940896	1558.273566	15.950003
29.113796	1560.780434	15.955021
28.485132	1559.371546	15.960039
28.561791	1554.778010	15.965056
28.946476	1568.444260	15.970074
28.829732	1584.920022	15.975091
29.155223	1578.178861	15.980109
29.305971	1588.362809	15.985127
28.899866	1575.876761	15.990144
29.182067	1574.164435	15.995162
29.048081	1575.378897	16.000179
29.080624	1567.798895	16.005197
29.142018	1579.783391	16.010215
29.034234	1587.638180	16.015232
29.076455	1583.929376	16.020250
29.066228	1583.946900	16.025267
28.730183	1588.987760	16.030285
29.113934	1591.125768	16.035303
28.873717	1591.587888	16.040320
28.971324	1581.781520	16.045338
28.766650	1595.822497	16.050355
29.058520	1603.748156	16.055373
29.098276	1617.836622	16.060391
29.393077	1621.803080	16.065408
29.561361	1618.841243	16.070426
29.188217	1626.880148	16.075443
29.576854	1617.782211	16.080461
29.546972	1623.290724	16.085479
29.542499	1625.137781	16.090496
29.517131	1618.854835	16.095514
29.445796	1632.522156	16.100531
29.599062	1633.619646	16.105549
29.761442	1627.617928	16.110567
29.380547	1626.787093	16.115584
29.820426	1623.781444	16.120602
29.870395	1627.510322	16.125619
30.201851	1628.990298	16.130637
29.607037	1626.302228	16.135655
29.889358	1621.055625	16.140672
30.169171	1627.758817	16.145690
29.914668	1630.369297	16.150707
29.947298	1624.095305	16.155725
30.299943	1627.667945	16.160743
30.063540	1632.894907	16.165760
30.052398	1627.109181	16.170778
29.814383	1630.464162	16.175795
30.423986	1622.455628	16.180813
30.094051	1635.171510	16.185831
30.052978	1631.911671	16.190848
30.054271	1619.747511	16.195866
30.000098	1624.190780	16.200883
30.723945	1618.378261	16.205901
31.084592	1601.199589	16.210919
30.762768	1603.702303	16.215936
30.663019	1593.788018	16.220954
30.784634	1584.199604	16.225971
30.623681	1569.065732	16.230989
30.706914	1575.764020	16.236007
30.654286	1573.393278	16.241024
30.503936	1564.405110	16.246042
30.094334	1566.479908	16.251059
30.617218	1561.870890	16.256077
30.587209	1563.258095	16.261095
30.586732	1571.034234	16.266112
30.541704	1561.620879	16.271130
30.409129	1563.412325	16.276147
30.781049	1552.483236	16.281165
30.749679	1566.478723	16.286183
30.610626	1561.786329	16.291200
30.738563	1557.000122	16.296218
30.531176	1561.086530	16.301235
30.714710	1562.184731	16.306253
30.672588	1559.553894	16.311271
30.430244	1570.107231	16.316288
30.657584	1565.073638	16.321306
30.829200	1569.848690	16.326323
30.664128	1567.347606	16.331341
30.544208	1571.856075	16.336359
31.119280	1584.211605	16.341376
31.150061	1581.219802	16.346394
30.923754	1578.978455	16.351411
30.702788	1587.979545	16.356429
30.763387	1595.577096	16.361447
30.831983	1600.643473	16.366464
31.008607	1600.067874	16.371482
30.775020	1610.935126	16.376499
30.909838	1600.995580	16.381517
31.140688	1597.355623	16.386535
31.026921	1606.124934	16.391552
30.999536	1601.458268	16.396570
30.597293	1604.046432	16.401587
30.835964	1617.638931	16.406605
30.908086	1624.556099	16.411623
31.121813	1634.236311	16.416640
31.553526	1633.703598	16.421658
31.281768	1639.923349	16.426675
31.424237	1629.898212	16.431693
31.594967	1630.423352	16.436711
31.375356	1644.879972	16.441728
31.782194	1628.187108	16.446746
31.311570	1641.699251	16.451763
31.462552	1639.388875	16.456781
31.327981	1638.770165	16.461799
31.333863	1650.174796	16.466816
31.873472	1659.218768	16.471834
31.651623	1675.948500	16.476851
31.488463	1663.997170	16.481869
32.054255	1669.965048	16.486887
31.849566	1679.069710	16.491904
31.894193	1669.480270	16.496922
31.777447	1666.142837	16.501939
31.576323	1672.723761	16.506957
31.942209	1672.698060	16.511975
31.631349	1678.399667	16.516992
31.812066	1666.191320	16.522010
32.584627	1673.668413	16.527027
32.350009	1668.197398	16.532045
32.716398	1667.730615	16.537063
32.031189	1657.218167	16.542080
32.287536	1635.723777	16.547098
32.061676	1636.318491	16.552115
32.128081	1634.958943	16.557133
32.070893	1636.299234	16.562151
32.276784	1633.087611	16.567168
32.210178	1631.759925	16.572186
32.351888	1647.332288	16.577203
32.358036	1644.271459	16.582221
32.148263	1644.461402	16.587239
32.058838	1671.315243	16.592256
32.765169	1664.570565	16.597274
32.767146	1674.699754	16.602291
32.240421	1659.276499	16.607309
32.612895	1662.054319	16.612327
32.344808	1672.618832	16.617344
32.451879	1671.485012	16.622362
32.412441	1668.461526	16.627379
32.351887	1670.268198	16.632397
32.694055	1673.103584	16.637415
32.344387	1665.217766	16.642432
32.602185	1669.967834	16.647450
32.276271	1671.312466	16.652467
32.205356	1673.476861	16.657485
32.735186	1667.940925	16.662503
32.599251	1677.058210	16.667520
32.715002	1695.690542	16.672538
32.772537	1700.900596	16.677555
32.757729	1705.781284	16.682573
33.104457	1696.595989	16.687591
32.672721	1705.511616	16.692608
32.792849	1703.769972	16.697626
32.994059	1700.302022	16.702643
32.514426	1701.412746	16.707661
32.705922	1700.197512	16.712679
32.672626	1711.838460	16.717696
32.883977	1716.174410	16.722714
33.147734	1732.990647	16.727731
32.937334	1738.283272	16.732749
33.137709	1727.611061	16.737767
33.288844	1730.023646	16.742784
33.553099	1727.869841	16.747802
33.549509	1737.166067	16.752819
33.822779	1730.622006	16.757837
33.617403	1730.537934	16.762855
33.505147	1723.911141	16.767872
33.640672	1722.810632	16.772890
33.637309	1703.159316	16.777907
33.437343	1695.998296	16.782925
33.274207	1688.960901	16.787943
33.534516	1710.842860	16.792960
33.795024	1714.525817	16.797978
33.749312	1707.746659	16.802995
33.482892	1705.874025	16.808013
33.927355	1710.319628	16.813031
33.860546	1714.251642	16.818048
33.710873	1682.981555	16.823066
33.874587	1685.032486	16.828083
33.630456	1688.379472	16.833101
34.241454	1688.822039	16.838119
33.848641	1694.849157	16.843136
33.841525	1688.394531	16.848154
33.772954	1682.373328	16.853171
33.706522	1707.146671	16.858189
33.794548	1715.214436	16.863207
33.946317	1722.740112	16.868224
34.181846	1716.492325	16.873242
34.025648	1720.356586	16.878259
34.199519	1727.631595	16.883277
34.023316	1725.211537	16.888295
34.058525	1730.371880	16.893312
34.273905	1726.689659	16.898330
34.220494	1721.347812	16.903347
34.111293	1716.163975	16.908365
34.276364	1717.117698	16.913383
34.150953	1727.544779	16.918400
34.407234	1720.057854	16.923418
34.238595	1717.841249	16.928435
34.047205	1729.164787	16.933453
34.366354	1716.706655	16.938471
34.225070	1727.374281	16.943488
34.249723	1744.854437	16.948506
34.379710	1747.032433	16.953523
34.177224	1751.996107	16.958541
34.324667	1749.297693	16.963559
34.339337	1750.423286	16.968576
34.565594	1744.642094	16.973594
34.772553	1744.930685	16.978611
34.274876	1754.837290	16.983629
35.100766	1767.181855	16.988647
35.043422	1767.318101	16.993664
34.651364	1758.774856	16.998682
34.904048	1763.609305	17.003699
35.124249	1768.443025	17.008717
35.056954	1750.899321	17.013735
35.022449	1754.623420	17.018752
35.121152	1745.076636	17.023770
35.302544	1738.881829	17.028787
35.277738	1745.328209	17.033805
35.248662	1736.032107	17.038823
35.010377	1738.827642	17.043840
34.932961	1735.341307	17.048858
34.994521	1745.958811	17.053875
34.638802	1761.455138	17.058893
35.280786	1763.054347	17.063911
35.534821	1774.312966	17.068928
35.014157	1769.987156	17.073946
35.512428	1766.578902	17.078963
35.419823	1777.314996	17.083981
35.563018	1776.740792	17.088999
35.582706	1779.371615	17.094016
35.441494	1770.912929	17.099034
35.731670	1773.754098	17.104051
35.493135	1776.767819	17.109069
35.580885	1765.919199	17.114087
35.638567	1770.109049	17.119104
35.292283	1765.235169	17.124122
35.977025	1758.143324	17.129139
35.623434	1776.804643	17.134157
35.829971	1770.863024	17.139175
35.805345	1771.444108	17.144192
35.788716	1773.331066	17.149210
36.078006	1764.410728	17.154227
35.824686	1772.246857	17.159245
35.809180	1769.076711	17.164263
36.012047	1771.093772	17.169280
35.525665	1765.639509	17.174298
35.605581	1768.899057	17.179315
35.668928	1770.735684	17.184333
35.910741	1763.120101	17.189351
36.122729	1783.116911	17.194368
36.160842	1801.135438	17.199386
36.600375	1802.196064	17.204403
36.372982	1784.491561	17.209421
36.428988	1772.843556	17.214439
36.030651	1772.049565	17.219456
36.056423	1772.494040	17.224474
36.299818	1786.291807	17.229491
36.296590	1795.998293	17.234509
36.437229	1797.221204	17.239527
36.402085	1799.515326	17.244544
36.344959	1801.559250	17.249562
36.648799	1791.849297	17.254579
36.418065	1798.381407	17.259597
36.388051	1798.495642	17.264615
36.756260	1792.409351	17.269632
36.170618	1804.233665	17.274650
36.655672	1781.385921	17.279667
36.616526	1793.100382	17.284685
36.969405	1797.936563	17.289703
36.776501	1780.708493	17.294720
36.663784	1795.390654	17.299738
36.736086	1788.613671	17.304755
36.376265	1789.226633	17.309773
36.917061	1805.287882	17.314791
37.230312	1807.685677	17.319808
37.455943	1807.492662	17.324826
37.529090	1787.611954	17.329843
37.248672	1779.774447	17.334861
37.015815	1780.572752	17.339879
37.389731	1771.754056	17.344896
36.941050	1778.523157	17.349914
37.297334	1769.732685	17.354931
36.950876	1777.103231	17.359949
37.056308	1773.662712	17.364967
37.241358	1777.906720	17.369984
36.792441	1782.317703	17.375002
37.424041	1786.560355	17.380019
37.391579	1805.405261	17.385037
37.365785	1805.518379	17.390055
37.777266	1802.105704	17.395072
37.841055	1807.269441	17.400090
37.815400	1785.438898	17.405107
37.463609	1779.474879	17.410125
37.167207	1783.871131	17.415143
37.766741	1792.595420	17.420160
37.610552	1799.156093	17.425178
38.127482	1804.721721	17.430195
37.678586	1796.632350	17.435213
37.566771	1805.952686	17.440231
37.783821	1800.224633	17.445248
38.035713	1808.981762	17.450266
38.290513	1802.947987	17.455283
37.913608	1803.234312	17.460301
38.056233	1795.855825	17.465319
38.079680	1787.837458	17.470336
37.648465	1781.403927	17.475354
37.957070	1792.921739	17.480371
37.928321	1807.259554	17.485389
38.043664	1816.927611	17.490407
38.178617	1805.033733	17.495424
38.149626	1814.625342	17.500442
37.995922	1808.471425	17.505459
38.224356	1810.745557	17.510477
38.195499	1810.384732	17.515495
38.358075	1806.336696	17.520512
38.250641	1811.575073	17.525530
38.380121	1809.092747	17.530547
38.370345	1806.828416	17.535565
38.119365	1807.918448	17.540583
38.473842	1813.853315	17.545600
38.513907	1836.107506	17.550618
38.656298	1834.358881	17.555635
38.802489	1839.156487	17.560653
38.395928	1837.233052	17.565671
38.580278	1830.395889	17.570688
38.640869	1835.931884	17.575706
38.570230	1839.271598	17.580723
38.685069	1846.828078	17.585741
38.367828	1842.524857	17.590759
38.764143	1834.129505	17.595776
38.661866	1842.101602	17.600794
38.865699	1836.586065	17.605811
38.812655	1848.903420	17.610829
38.893043	1842.021864	17.615847
39.323503	1842.137080	17.620864
39.125067	1842.235699	17.625882
38.901141	1838.286998	17.630899
38.781705	1842.214286	17.635917
39.041837	1860.541709	17.640935
39.572356	1862.464017	17.645952
39.616020	1860.248397	17.650970
39.533109	1862.366443	17.655987
39.625492	1842.744605	17.661005
39.260875	1834.475388	17.666023
39.572051	1825.483144	17.671040
39.371884	1828.682446	17.676058
39.385145	1832.262530	17.681075
39.865650	1840.291023	17.686093
39.621307	1842.187108	17.691111
39.605256	1837.285328	17.696128
39.505814	1840.480750	17.701146
39.493972	1847.099775	17.706163
39.901489	1851.777373	17.711181
39.969361	1857.788565	17.716199
39.778505	1848.476822	17.721216
39.809957	1843.511376	17.726234
39.805420	1847.371716	17.731251
40.017151	1860.095708	17.736269
39.962717	1864.131163	17.741287
40.339804	1859.624627	17.746304
39.790864	1857.050319	17.751322
40.193752	1854.041913	17.756339
40.188638	1860.054989	17.761357
40.014600	1855.144067	17.766375
40.223988	1850.482799	17.771392
40.221561	1861.533846	17.776410
40.175487	1863.768427	17.781427
40.530340	1868.342841	17.786445
40.118287	1864.505927	17.791463
40.258670	1853.656097	17.796480
40.125406	1856.321033	17.801498
40.343541	1857.104623	17.806515
40.156707	1857.040602	17.811533
40.069674	1868.280198	17.816551
40.238151	1869.515273	17.821568
39.922693	1865.064083	17.826586
40.191088	1876.148245	17.831603
40.658175	1883.415971	17.836621
40.262730	1900.119007	17.841639
40.606727	1886.144080	17.846656
40.493453	1886.805337	17.851674
40.646613	1889.517245	17.856691
40.363875	1893.336307	17.861709
40.640408	1907.751809	17.866727
41.340401	1917.375599	17.871744
41.033943	1922.774531	17.876762
41.127865	1912.807544	17.881779
41.003721	1887.749227	17.886797
41.036625	1888.414953	17.891815
40.965065	1893.308580	17.896832
40.960125	1909.765514	17.901850
41.418977	1916.569647	17.906867
41.856714	1921.649619	17.911885
41.478605	1899.776971	17.916903
41.752636	1888.582507	17.921920
41.388761	1892.126466	17.926938
41.201996	1891.317062	17.931955
41.429593	1887.353933	17.936973
41.448129	1879.904938	17.941991
41.037112	1876.253694	17.947008
41.269664	1875.010539	17.952026
41.525725	1892.001912	17.957043
41.870650	1900.275759	17.962061
41.490398	1899.069945	17.967079
41.604574	1907.953906	17.972096
41.924311	1921.950936	17.977114
41.810886	1924.119110	17.982131
41.899889	1916.970262	17.987149
41.730394	1921.634594	17.992167
41.887449	1920.522505	17.997184
41.865533	1913.320620	18.002202
41.539192	1920.559420	18.007219
41.617226	1914.049150	18.012237
41.559994	1921.046116	18.017255
41.438162	1917.574050	18.022272
41.515009	1925.167400	18.027290
41.341100	1929.807291	18.032307
41.842204	1935.237868	18.037325
41.750507	1928.135746	18.042343
42.138130	1937.236259	18.047360
42.004440	1941.023478	18.052378
42.319971	1953.565554	18.057395
42.741499	1960.356418	18.062413
42.446245	1969.070422	18.067431
42.921051	1948.192567	18.072448
43.277956	1935.443499	18.077466
42.895785	1932.824833	18.082483
43.002097	1927.098003	18.087501
42.594653	1924.899869	18.092519
42.906017	1915.950066	18.097536
43.173747	1920.858373	18.102554
42.810552	1928.640180	18.107571
43.055464	1915.864654	18.112589
42.692956	1931.714327	18.117607
42.780373	1919.299311	18.122624
43.059849	1918.875774	18.127642
42.751843	1914.470936	18.132659
43.192451	1917.922644	18.137677
43.045866	1930.220269	18.142695
43.027761	1929.227988	18.147712
43.220857	1922.890926	18.152730
43.090346	1922.499096	18.157747
42.612765	1914.545699	18.162765
42.661094	1924.120575	18.167783
42.794489	1922.423095	18.172800
43.262080	1918.870838	18.177818
43.077698	1939.536675	18.182835
43.223265	1946.244123	18.187853
43.345830	1948.811660	18.192871
43.267326	1953.678934	18.197888
43.966139	1953.441013	18.202906
43.335935	1959.875518	18.207923
43.669040	1948.349973	18.212941
43.665968	1952.068730	18.217959
43.385470	1965.110305	18.222976
43.860614	1956.988812	18.227994
43.351457	1963.794348	18.233011
43.868903	1957.098470	18.238029
43.895616	1956.436737	18.243047
43.793526	1953.412912	18.248064
43.635484	1956.542411	18.253082
43.710170	1960.860517	18.258099
43.814564	1956.760600	18.263117
43.697003	1954.965575	18.268135
43.499953	1968.776414	18.273152
43.832530	1981.383316	18.278170
43.897140	1985.627556	18.283187
44.146806	1979.872977	18.288205
43.896248	1986.223106	18.293223
43.877637	1982.642764	18.298240
44.440588	1985.627387	18.303258
44.114987	1983.747146	18.308275
44.454424	1991.713673	18.313293
44.574196	2015.455050	18.318311
44.912662	2011.791428	18.323328
44.710319	2000.219050	18.328346
44.176591	1988.637347	18.333363
44.426700	1994.997713	18.338381
44.543818	2017.645306	18.343399
44.707480	2018.831605	18.348416
44.903452	2019.806037	18.353434
44.863522	2015.926152	18.358451
45.031277	2017.623236	18.363469
45.082045	2021.266234	18.368487
44.964711	2017.847712	18.373504
44.995539	2013.188661	18.378522
45.184229	2020.242338	18.383539
44.846858	2010.944200	18.388557
45.249153	2017.001672	18.393575
45.233367	2012.017104	18.398592
45.205781	2012.445534	18.403610
44.959230	2017.996848	18.408627
44.944017	2010.065715	18.413645
44.859027	2009.897606	18.418663
44.880774	2025.551159	18.423680
44.857227	2013.787463	18.428698
45.028118	2019.203810	18.433715
45.007434	2031.068061	18.438733
45.070910	2041.346020	18.443751
45.002421	2038.229004	18.448768
45.318046	2043.765446	18.453786
45.416834	2042.568051	18.458803
45.540914	2043.322889	18.463821
45.651117	2051.678011	18.468839
45.521651	2062.325332	18.473856
45.773711	2059.659328	18.478874
45.478607	2074.212763	18.483891
45.651162	2074.071766	18.488909
46.105312	2067.564672	18.493927
45.819508	2076.974457	18.498944
45.779431	2066.444832	18.503962
45.938931	2072.660900	18.508979
46.096310	2065.310864	18.513997
45.954691	2071.679361	18.519015
46.017934	2073.521161	18.524032
46.263667	2057.110224	18.529050
46.250727	2070.666721	18.534067
46.005140	2064.366228	18.539085
46.414845	2074.702579	18.544103
46.481032	2096.054503	18.549120
46.671986	2093.767527	18.554138
46.379556	2088.125149	18.559155
46.748616	2085.895050	18.564173
46.726702	2078.369421	18.569191
46.557443	2068.445489	18.574208
46.847968	2069.347800	18.579226
46.440877	2065.640318	18.584243
46.482117	2078.926471	18.589261
46.772158	2089.032133	18.594279
46.682688	2094.690024	18.599296
46.784599	2088.123613	18.604314
46.637163	2094.036360	18.609331
46.974172	2093.864015	18.614349
46.829951	2089.630680	18.619367
46.793380	2089.130600	18.624384
46.743255	2082.000412	18.629402
46.759353	2093.748152	18.634419
46.989760	2106.154137	18.639437
47.317634	2111.355385	18.644455
47.488237	2119.128059	18.649472
47.386713	2115.084275	18.654490
47.638001	2121.422440	18.659507
47.798303	2114.600302	18.664525
48.041878	2102.582836	18.669543
47.578336	2099.065759	18.674560
47.933854	2082.999016	18.679578
48.014203	2082.416283	18.684595
47.752020	2079.522652	18.689613
48.166942	2070.773935	18.694631
47.546830	2083.309191	18.699648
47.241956	2074.305484	18.704666
47.443340	2083.863665	18.709683
47.345842	2085.065609	18.714701
47.524074	2092.466830	18.719719
47.588825	2112.479463	18.724736
47.731581	2109.549081	18.729754
47.699676	2121.955559	18.734771
47.663486	2116.883104	18.739789
47.770768	2118.000326	18.744807
47.776577	2140.223810	18.749824
47.902140	2144.966772	18.754842
47.957509	2150.747903	18.759859
48.128256	2141.365323	18.764877
48.246024	2144.174696	18.769895
47.986441	2144.853173	18.774912
47.992019	2142.976375	18.779930
48.538658	2148.802428	18.784947
48.569299	2160.887931	18.789965
48.927572	2154.872901	18.794983
48.840561	2140.983459	18.800000
48.942972	2121.995471	18.805018
49.127710	2131.048588	18.810035
49.164324	2125.935297	18.815053
49.516640	2126.869543	18.820071
49.209673	2127.265551	18.825088
49.504589	2121.680353	18.830106
49.348411	2114.625034	18.835123
49.476221	2104.778904	18.840141
49.533813	2093.129208	18.845159
49.117142	2092.742730	18.850176
49.371689	2085.517383	18.855194
49.185153	2089.460175	18.860211
49.347388	2086.583945	18.865229
49.667032	2085.403018	18.870247
49.325611	2099.326927	18.875264
48.897095	2090.838574	18.880282
49.318625	2088.860934	18.885299
49.232307	2087.984683	18.890317
49.292986	2085.084128	18.895335
49.376248	2099.104144	18.900352
49.626117	2102.323992	18.905370
49.395295	2112.320126	18.910387
49.337542	2119.301912	18.915405
49.648804	2112.124712	18.920423
49.822834	2122.539697	18.925440
49.834246	2115.498169	18.930458
49.750076	2112.006608	18.935475
49.746111	2120.593577	18.940493
49.548360	2111.802617	18.945511
49.582188	2113.468731	18.950528
49.942523	2123.988802	18.955546
50.374270	2144.731187	18.960563
50.070596	2154.038161	18.965581
50.354725	2151.375701	18.970599
50.016444	2152.388978	18.975616
50.149385	2148.193158	18.980634
50.381638	2145.183636	18.985651
50.238244	2151.039009	18.990669
50.086546	2145.984774	18.995687
50.501761	2145.270204	19.000704
50.677461	2143.728070	19.005722
50.295300	2150.337870	19.010739
50.287904	2151.657461	19.015757
50.547996	2139.390643	19.020775
50.324374	2150.461312	19.025792
50.657850	2161.726279	19.030810
51.009672	2167.569204	19.035827
50.599209	2176.148722	19.040845
50.940733	2169.947553	19.045863
50.742211	2180.702084	19.050880
51.063681	2174.042866	19.055898
51.170954	2178.214087	19.060915
50.686327	2178.983914	19.065933
51.469505	2172.423514	19.070951
51.060447	2175.354719	19.075968
51.290269	2170.438242	19.080986
51.667033	2165.980896	19.086003
51.585488	2166.339830	19.091021
51.649319	2166.335994	19.096039
51.781564	2167.510367	19.101056
51.610536	2168.727286	19.106074
51.656800	2166.733257	19.111091
51.646507	2164.931629	19.116109
51.729712	2165.296967	19.121127
51.490447	2170.181239	19.126144
51.896772	2170.317136	19.131162
52.094946	2167.327628	19.136179
51.550655	2169.637042	19.141197
51.853887	2165.841216	19.146215
51.711403	2167.760432	19.151232
51.798455	2165.653095	19.156250
51.791407	2164.368309	19.161267
51.873582	2167.732688	19.166285
51.941370	2175.475766	19.171303
51.602050	2188.446891	19.176320
51.776274	2202.567169	19.181338
52.367777	2199.247186	19.186355
51.991445	2203.570630	19.191373
52.348739	2200.808990	19.196391
52.219679	2200.605121	19.201408
51.995756	2200.941216	19.206426
52.524144	2210.467822	19.211443
52.323430	2229.815384	19.216461
52.714202	2230.506000	19.221479
52.588421	2228.688727	19.226496
52.543555	2232.125302	19.231514
52.998032	2229.784856	19.236531
52.988972	2230.589700	19.241549
52.946534	2216.762638	19.246567
53.133369	2218.330077	19.251584
52.882279	2222.910048	19.256602
53.081801	2225.710144	19.261619
52.515626	2221.698747	19.266637
52.930465	2225.558940	19.271655
53.021758	2225.816577	19.276672
52.749706	2221.405093	19.281690
53.220808	2237.345648	19.286707
53.219335	2248.708270	19.291725
53.541864	2252.917418	19.296743
53.661194	2251.128207	19.301760
53.747839	2237.652280	19.306778
53.892796	2229.797921	19.311795
53.622426	2220.277507	19.316813
53.598804	2214.219254	19.321831
53.607324	2209.962060	19.326848
53.292338	2233.044734	19.331866
53.546881	2234.784846	19.336883
53.767806	2238.557799	19.341901
53.491700	2243.323195	19.346919
53.768389	2239.476777	19.351936
54.061033	2242.940539	19.356954
53.894870	2238.381742	19.361971
54.159659	2240.580797	19.366989
53.933807	2233.448380	19.372007
53.988512	2239.761235	19.377024
53.986573	2246.556316	19.382042
54.205370	2256.910952	19.387059
54.025482	2266.914989	19.392077
54.433440	2265.863811	19.397095
54.045147	2279.834897	19.402112
54.211192	2271.192530	19.407130
54.811208	2268.409739	19.412147
54.571198	2274.097443	19.417165
54.378732	2269.757352	19.422183
54.644717	2270.144906	19.427200
54.728993	2269.049997	19.432218
54.847010	2273.246964	19.437235
54.599823	2288.849237	19.442253
54.993253	2297.987161	19.447271
54.920052	2305.838743	19.452288
54.749352	2306.874486	19.457306
55.336427	2302.129035	19.462323
55.225184	2307.687571	19.467341
55.357450	2304.199809	19.472359
55.536928	2297.420769	19.477376
55.509840	2308.120792	19.482394
55.555930	2303.194037	19.487411
55.187240	2307.596527	19.492429
55.597430	2300.290451	19.497447
55.720229	2296.603496	19.502464
55.503178	2300.265701	19.507482
55.680646	2292.695545	19.512499
55.371117	2299.513461	19.517517
55.676365	2293.952420	19.522535
55.808208	2289.029079	19.527552
55.793003	2297.864567	19.532570
55.711604	2291.288549	19.537587
55.791457	2300.251857	19.542605
55.930215	2300.832905	19.547623
55.951623	2296.226181	19.552640
55.713805	2300.987392	19.557658
55.931648	2302.083309	19.562675
55.847050	2304.668311	19.567693
55.676682	2315.429132	19.572711
56.264191	2320.098458	19.577728
56.231585	2323.335283	19.582746
56.686108	2322.538364	19.587763
56.601134	2322.177304	19.592781
56.547149	2324.885428	19.597799
56.761302	2324.542384	19.602816
56.739414	2332.797057	19.607834
56.577450	2307.327952	19.612851
56.941754	2320.169096	19.617869
56.729468	2319.644796	19.622887
56.968162	2316.958598	19.627904
56.801122	2311.487188	19.632922
56.680973	2321.909431	19.637939
56.543677	2316.121848	19.642957
56.273446	2321.567468	19.647975
56.274177	2322.239122	19.652992
56.420772	2343.389773	19.658010
56.865276	2348.504165	19.663027
56.520628	2355.310013	19.668045
57.005060	2367.850240	19.673063
57.251024	2374.287075	19.678080
57.438046	2382.609122	19.683098
57.570089	2374.987651	19.688115
57.436440	2373.260700	19.693133
57.735716	2369.081979	19.698151
57.837111	2367.463573	19.703168
57.698381	2371.516368	19.708186
57.797344	2367.188498	19.713203
57.724996	2367.194623	19.718221
57.634556	2363.606427	19.723239
58.061040	2362.786750	19.728256
57.474290	2365.792557	19.733274
58.054009	2370.287615	19.738291
58.012246	2375.093199	19.743309
58.132386	2394.935648	19.748327
58.186883	2389.579009	19.753344
58.126415	2394.118471	19.758362
58.152802	2400.667779	19.763379
58.256278	2398.772590	19.768397
58.261927	2399.344963	19.773415
58.546328	2397.409304	19.778432
58.464803	2391.660958	19.783450
58.525380	2390.196816	19.788467
58.521102	2393.664269	19.793485
58.605169	2393.049779	19.798503
58.873687	2385.933335	19.803520
58.885578	2388.715228	19.808538
58.953792	2388.786244	19.813555
58.953788	2384.658044	19.818573
59.111853	2380.922496	19.823591
59.085822	2378.671501	19.828608
58.988231	2392.950383	19.833626
58.943894	2376.244303	19.838643
59.162813	2383.388253	19.843661
59.083214	2401.411116	19.848679
59.428957	2404.824072	19.853696
59.594266	2419.360314	19.858714
59.325036	2416.889551	19.863731
59.357123	2420.875270	19.868749
59.260730	2421.350947	19.873767
59.763399	2415.541019	19.878784
59.614006	2411.136014	19.883802
59.366920	2413.791420	19.888819
59.891440	2410.354512	19.893837
59.514355	2416.114596	19.898855
59.843935	2402.305490	19.903872
59.627063	2412.241145	19.908890
59.797407	2410.996802	19.913907
59.952951	2411.560013	19.918925
59.937341	2438.749027	19.923943
59.973283	2435.616390	19.928960
59.982115	2438.398029	19.933978
59.803981	2438.863307	19.938995
60.124037	2443.002054	19.944013
60.131078	2444.821639	19.949031
60.503314	2434.947571	19.954048
60.531100	2445.290979	19.959066
60.353794	2435.231557	19.964083
60.574643	2449.522834	19.969101
60.417367	2470.965166	19.974119
60.640361	2470.338667	19.979136
60.966727	2473.230465	19.984154
60.580860	2479.028303	19.989171
61.012412	2470.381257	19.994189
60.873448	2477.981951	19.999207
60.804761	2470.520067	20.004224
60.964446	2469.765030	20.009242
60.804562	2463.034652	20.014259
61.145224	2466.000387	20.019277
61.050824	2476.721517	20.024295
61.492485	2487.920132	20.029312
61.234568	2499.949054	20.034330
61.236622	2505.329153	20.039347
61.630749	2496.491625	20.044365
61.820783	2509.528974	20.049383
62.230289	2494.333413	20.054400
61.661837	2505.552444	20.059418
61.758210	2500.198826	20.064435
62.119992	2501.374821	20.069453
61.840140	2509.877786	20.074471
62.005241	2501.556768	20.079488
61.896943	2503.128373	20.084506
61.669793	2500.344031	20.089523
62.227601	2495.705921	20.094541
61.832229	2500.239044	20.099559
62.132526	2500.757752	20.104576
61.639585	2499.054587	20.109594
61.845881	2502.315066	20.114611
62.146276	2497.412377	20.119629
62.118369	2512.387412	20.124647
62.330959	2523.054365	20.129664
62.407586	2523.804369	20.134682
62.408330	2526.535433	20.139699
62.502034	2526.184685	20.144717
62.537011	2532.984587	20.149735
62.710285	2529.062901	20.154752
62.787276	2526.067327	20.159770
62.891413	2526.690546	20.164787
63.291044	2523.104131	20.169805
62.438976	2532.838478	20.174823
62.569426	2541.219924	20.179840
63.112310	2552.487072	20.184858
63.251338	2555.385016	20.189875
62.911690	2549.639915	20.194893
63.275978	2554.535018	20.199911
63.516095	2544.912707	20.204928
63.500440	2557.626245	20.209946
63.257766	2555.344639	20.214963
63.304591	2541.476786	20.219981
63.682200	2555.118342	20.224999
63.551139	2571.038837	20.230016
63.954250	2572.251066	20.235034
63.677299	2572.997904	20.240051
64.362823	2580.555730	20.245069
63.979206	2584.052037	20.250087
63.730347	2576.916319	20.255104
64.026601	2574.615552	20.260122
63.858275	2583.228591	20.265139
64.334517	2573.209024	20.270157
63.962501	2577.187675	20.275175
64.205994	2573.159435	20.280192
64.064949	2569.685398	20.285210
64.133704	2571.336909	20.290227
64.369550	2578.096090	20.295245
64.627811	2602.836444	20.300263
64.431062	2604.488589	20.305280
64.499924	2604.700465	20.310298
64.398126	2606.488326	20.315315
64.628470	2602.885240	20.320333
64.836125	2602.494479	20.325351
64.949643	2604.888843	20.330368
64.866257	2602.913049	20.335386
64.456737	2608.894549	20.340403
65.056808	2618.709957	20.345421
64.842819	2631.299263	20.350439
64.732791	2625.419474	20.355456
64.959063	2630.065775	20.360474
65.263303	2634.208073	20.365491
65.853987	2626.925242	20.370509
65.625850	2635.537539	20.375527
65.661080	2636.682116	20.380544
65.906146	2632.351963	20.385562
65.965140	2627.696957	20.390579
66.401297	2626.796857	20.395597
65.718380	2626.347722	20.400615
66.173365	2630.803603	20.405632
66.617115	2620.957323	20.410650
66.102602	2631.300902	20.415667
66.079356	2620.833777	20.420685
66.202243	2624.376346	20.425703
66.142963	2631.906750	20.430720
66.179505	2622.431125	20.435738
65.995404	2621.699584	20.440755
65.982018	2622.185449	20.445773
65.861899	2626.478467	20.450791
65.725123	2626.123919	20.455808
66.174984	2641.858257	20.460826
66.121345	2654.587049	20.465843
66.231113	2658.508319	20.470861
66.306155	2660.703740	20.475879
66.508257	2675.602482	20.480896
67.100405	2688.004006	20.485914
66.417846	2696.439871	20.490931
66.387057	2685.573137	20.495949
66.791502	2691.967969	20.500967
66.699302	2693.117859	20.505984
67.475439	2695.898721	20.511002
67.015614	2718.634431	20.516019
67.315609	2715.789597	20.521037
67.710611	2714.758728	20.526055
67.965281	2717.298231	20.531072
68.047988	2704.525856	20.536090
67.692212	2685.643307	20.541107
68.186990	2674.087152	20.546125
68.241302	2670.292933	20.551143
67.785795	2668.742413	20.556160
68.065481	2665.824679	20.561178
68.176921	2663.219305	20.566195
68.187296	2660.628110	20.571213
68.426436	2669.117783	20.576231
68.136097	2665.524413	20.581248
68.155891	2661.766829	20.586266
67.560386	2667.756612	20.591283
67.475971	2667.977441	20.596301
68.144654	2679.978367	20.601319
68.542449	2692.617978	20.606336
68.538885	2696.442920	20.611354
68.207716	2703.567923	20.616371
68.425485	2702.243761	20.621389
68.427658	2698.013512	20.626407
68.431451	2697.563195	20.631424
68.459616	2707.174296	20.636442
68.401732	2713.227854	20.641459
68.591308	2717.699338	20.646477
68.727478	2722.377654	20.651495
68.537080	2723.990133	20.656512
68.892298	2734.494168	20.661530
69.207510	2752.071721	20.666547
69.365276	2748.481833	20.671565
69.486496	2748.321675	20.676583
69.349339	2745.022555	20.681600
69.716096	2741.403139	20.686618
69.747100	2741.598668	20.691635
69.878379	2740.421638	20.696653
69.829106	2742.537579	20.701671
69.714730	2742.761971	20.706688
70.016654	2732.046861	20.711706
70.280469	2738.476062	20.716723
69.783632	2741.201118	20.721741
69.727009	2741.347092	20.726759
69.748309	2740.103863	20.731776
70.085861	2738.699308	20.736794
69.800075	2744.665945	20.741811
70.134669	2741.990010	20.746829
69.985502	2747.616631	20.751847
70.123964	2763.049298	20.756864
70.582383	2758.323410	20.761882
70.300890	2772.327810	20.766899
70.575777	2773.171418	20.771917
70.683050	2770.169030	20.776935
70.658999	2771.789221	20.781952
70.794015	2763.672472	20.786970
70.918051	2770.115413	20.791987
70.630048	2776.081654	20.797005
70.666204	2784.935386	20.802023
70.766070	2806.580591	20.807040
71.039145	2801.220989	20.812058
71.111456	2804.999872	20.817075
71.092507	2818.389902	20.822093
71.176132	2800.550987	20.827111
71.037749	2806.779830	20.832128
71.456664	2820.836663	20.837146
71.843180	2822.608556	20.842163
72.084435	2825.822945	20.847181
72.091784	2827.977230	20.852199
71.959356	2821.825564	20.857216
71.622033	2813.490503	20.862234
71.696873	2824.947565	20.867251
71.866919	2825.931220	20.872269
71.699503	2816.690484	20.877287
71.682033	2829.596716	20.882304
72.146703	2834.586530	20.887322
72.052761	2831.017728	20.892339
72.027326	2847.522081	20.897357
72.491720	2852.771053	20.902375
72.058563	2865.608399	20.907392
72.097151	2855.751895	20.912410
72.430093	2859.901933	20.917427
72.065135	2863.867632	20.922445
72.359567	2870.424733	20.927463
72.551588	2887.343113	20.932480
72.787643	2879.577557	20.937498
73.000496	2888.747577	20.942515
72.951348	2884.759192	20.947533
73.326643	2883.078023	20.952551
73.071422	2886.200345	20.957568
73.567494	2879.258880	20.962586
73.491112	2884.406840	20.967603
73.496205	2888.860387	20.972621
74.430896	2865.792617	20.977639
74.833645	2852.089494	20.982656
74.574222	2836.319971	20.987674
74.883905	2829.526254	20.992691
74.640247	2809.371339	20.997709
74.235097	2790.315204	21.002727
74.303582	2783.430551	21.007744
73.826444	2782.504316	21.012762
73.869241	2776.020995	21.017779
73.720396	2773.803600	21.022797
74.171894	2782.774345	21.027815
74.026979	2806.090167	21.032832
74.135104	2804.676900	21.037850
73.854112	2810.561622	21.042867
73.998905	2809.053863	21.047885
74.316870	2807.610133	21.052903
74.205271	2824.241067	21.057920
74.178028	2833.572714	21.062938
74.143168	2839.742081	21.067955
74.215249	2855.220872	21.072973
74.680212	2854.502471	21.077991
74.752614	2873.010935	21.083008
74.768304	2870.358152	21.088026
75.099516	2876.817595	21.093043
75.228498	2891.753493	21.098061
75.185838	2880.970564	21.103079
75.196928	2889.282879	21.108096
74.891948	2881.643947	21.113114
75.024287	2883.980786	21.118131
74.711347	2902.467144	21.123149
75.326194	2906.573588	21.128167
75.119557	2920.471567	21.133184
75.567792	2928.638863	21.138202
75.562846	2934.556634	21.143219
75.833157	2947.461663	21.148237
76.198500	2938.331917	21.153255
76.013508	2940.691668	21.158272
76.074483	2944.228386	21.163290
76.630384	2935.838562	21.168307
76.565522	2932.320668	21.173325
76.816380	2918.279678	21.178343
76.655602	2923.908353	21.183360
76.654190	2922.235062	21.188378
77.001646	2920.868958	21.193395
76.938703	2921.956358	21.198413
77.022596	2924.814207	21.203431
77.130908	2923.122104	21.208448
76.690594	2904.429409	21.213466
76.758911	2899.879044	21.218483
76.843145	2920.920671	21.223501
77.081677	2910.531330	21.228519
77.183469	2919.516433	21.233536
77.043731	2918.040908	21.238554
76.929861	2915.892314	21.243571
76.807826	2930.750002	21.248589
77.095511	2921.169710	21.253607
77.167546	2937.518837	21.258624
77.658288	2945.224435	21.263642
77.552081	2948.087316	21.268659
77.484771	2959.307379	21.273677
77.739567	2947.452733	21.278695
77.393552	2950.832414	21.283712
77.685944	2954.420027	21.288730
78.100391	2976.708520	21.293747
77.838281	2985.623741	21.298765
77.946048	2983.797840	21.303783
78.268437	2985.572084	21.308800
78.322242	2982.871795	21.313818
78.085167	2990.296605	21.318835
78.063541	2986.002629	21.323853
78.235358	3000.295727	21.328871
78.272478	3005.773943	21.333888
78.512439	3011.603288	21.338906
78.858492	3014.927334	21.343923
78.708395	3013.000728	21.348941
78.730756	3011.749421	21.353959
78.929181	3028.406174	21.358976
78.697681	3043.367005	21.363994
79.235938	3049.416143	21.369011
78.916329	3044.268332	21.374029
79.445839	3042.153538	21.379047
79.503534	3038.994212	21.384064
79.231754	3038.260356	21.389082
79.578512	3037.482670	21.394099
79.306177	3037.429362	21.399117
79.522665	3048.776457	21.404135
79.590299	3070.518122	21.409152
79.582539	3070.309981	21.414170
79.725984	3070.212165	21.419187
79.640880	3073.545564	21.424205
79.862887	3065.343653	21.429223
80.183388	3090.124509	21.434240
80.086517	3099.617888	21.439258
80.393562	3093.479764	21.444275
79.963933	3104.297385	21.449293
80.394344	3097.932554	21.454311
80.701430	3096.207928	21.459328
80.188271	3098.522371	21.464346
81.106486	3099.673109	21.469363
80.922109	3097.416081	21.474381
81.057855	3098.435562	21.479399
81.054008	3091.659259	21.484416
81.115702	3099.383363	21.489434
81.246275	3091.778337	21.494451
81.236234	3100.299940	21.499469
81.352102	3093.236915	21.504487
81.300924	3093.758414	21.509504
80.733857	3107.418290	21.514522
81.066599	3108.859998	21.519539
81.010022	3114.204678	21.524557
81.160134	3116.794464	21.529575
81.338726	3133.935143	21.534592
80.992852	3151.155521	21.539610
81.314057	3155.852647	21.544627
81.676717	3160.077215	21.549645
82.081146	3168.789268	21.554663
82.552886	3173.020340	21.559680
82.256430	3179.297696	21.564698
82.546923	3165.315060	21.569715
82.511381	3171.717006	21.574733
82.587143	3167.717373	21.579751
82.693150	3170.002065	21.584768
82.386057	3168.099994	21.589786
82.678588	3165.096485	21.594803
82.708414	3168.199131	21.599821
82.817071	3166.788105	21.604839
82.820405	3163.676664	21.609856
82.870698	3174.290767	21.614874
83.108728	3168.351100	21.619891
82.944634	3160.135004	21.624909
83.263968	3185.413953	21.629927
83.376864	3185.892360	21.634944
83.515785	3200.166866	21.639962
83.679235	3198.373922	21.644979
83.870844	3200.591963	21.649997
83.634277	3197.804384	21.655015
84.089514	3196.196897	21.660032
83.668187	3199.378474	21.665050
84.192416	3200.651111	21.670067
84.215852	3198.571870	21.675085
83.906978	3198.085361	21.680103
84.191914	3198.281464	21.685120
83.966104	3194.539083	21.690138
83.773230	3198.438345	21.695155
84.109367	3207.533073	21.700173
83.911398	3226.663232	21.705191
84.301102	3226.205805	21.710208
84.115539	3233.732944	21.715226
84.302453	3225.801591	21.720243
84.578297	3241.052872	21.725261
84.671852	3257.409669	21.730279
84.846342	3254.717782	21.735296
84.617074	3265.165657	21.740314
84.810494	3258.245989	21.745331
84.981397	3253.156562	21.750349
85.325667	3268.952165	21.755367
85.758404	3268.355047	21.760384
85.912887	3268.803488	21.765402
86.005618	3249.485805	21.770419
85.980051	3238.854064	21.775437
85.711644	3239.388396	21.780455
85.789300	3232.201911	21.785472
85.702959	3234.369952	21.790490
85.907796	3233.651243	21.795507
85.896230	3254.874343	21.800525
86.129851	3260.735584	21.805543
85.990207	3262.782818	21.810560
86.275964	3274.048894	21.815578
86.123125	3265.558314	21.820595
86.149692	3267.047016	21.825613
86.148905	3259.788909	21.830631
86.223974	3276.343425	21.835648
86.082018	3300.436016	21.840666
86.737876	3304.646585	21.845683
86.843047	3299.729866	21.850701
86.787852	3295.945608	21.855719
86.864063	3298.142493	21.860736
86.778845	3320.027269	21.865754
86.892624	3323.325835	21.870771
87.501335	3339.195095	21.875789
87.476248	3338.544154	21.880807
87.340621	3321.556592	21.885824
87.612723	3333.694535	21.890842
87.780544	3328.162208	21.895859
87.799294	3325.191431	21.900877
87.785799	3334.791156	21.905895
88.005369	3322.303546	21.910912
88.186401	3332.402319	21.915930
88.014489	3318.600422	21.920947
88.433871	3317.307801	21.925965
88.294804	3327.908793	21.930983
88.592184	3326.845008	21.936000
88.069554	3333.882619	21.941018
87.866287	3346.966830	21.946035
88.167449	3355.996759	21.951053
88.151449	3364.276954	21.956071
88.526352	3365.958757	21.961088
88.968758	3384.450066	21.966106
88.614836	3379.954628	21.971123
89.073273	3374.477207	21.976141
89.127919	3373.065184	21.981159
89.457413	3368.103684	21.986176
89.590349	3382.341577	21.991194
89.531330	3378.116124	21.996211
89.831478	3376.858116	22.001229
89.645912	3373.830213	22.006247
89.670756	3370.257462	22.011264
89.788438	3368.126600	22.016282
89.880005	3372.314221	22.021299
89.912684	3372.856005	22.026317
89.433066	3366.508474	22.031335
89.634353	3367.179654	22.036352
89.876116	3381.331945	22.041370
89.860161	3396.737366	22.046387
90.278942	3397.959579	22.051405
89.687202	3408.198766	22.056423
90.474265	3401.617515	22.061440
90.272731	3397.686629	22.066458
90.323954	3410.891866	22.071475
90.656563	3417.519048	22.076493
90.583948	3425.100159	22.081511
90.890024	3414.542967	22.086528
91.074170	3420.247358	22.091546
90.657619	3417.604795	22.096563
91.238368	3421.671546	22.101581
91.055822	3426.214120	22.106599
91.393595	3435.250420	22.111616
91.364438	3446.999055	22.116634
91.424899	3453.242104	22.121651
91.809359	3453.562126	22.126669
91.511201	3456.959697	22.131687
91.841100	3451.711422	22.136704
91.740665	3458.763339	22.141722
91.602215	3451.320824	22.146739
92.229733	3447.671508	22.151757
92.206404	3464.817239	22.156775
92.371543	3473.587027	22.161792
92.236590	3476.511638	22.166810
92.563409	3474.173213	22.171827
92.675332	3469.262372	22.176845
92.454344	3467.467576	22.181863
93.234207	3465.260978	22.186880
92.984433	3467.119985	22.191898
93.004414	3463.242464	22.196915
93.141927	3457.763331	22.201933
93.144892	3464.961340	22.206951
93.260216	3464.328063	22.211968
93.263099	3460.622804	22.216986
92.967294	3460.130108	22.222003
93.403261	3457.225603	22.227021
93.267090	3461.675179	22.232039
93.529290	3480.039193	22.237056
93.262705	3486.905385	22.242074
93.274288	3486.801821	22.247091
94.201369	3486.135696	22.252109
93.594628	3503.736691	22.257127
93.695771	3500.292595	22.262144
93.949200	3507.809184	22.267162
93.582594	3518.199650	22.272179
94.135501	3512.833575	22.277197
94.423484	3517.871230	22.282215
94.318897	3511.868886	22.287232
94.288599	3523.909181	22.292250
94.642483	3537.156357	22.297267
94.796027	3530.887652	22.302285
94.719466	3544.445694	22.307303
94.745881	3540.092925	22.312320
94.981074	3536.716411	22.317338
95.201717	3539.242982	22.322355
95.127265	3528.343772	22.327373
94.853302	3538.552975	22.332391
95.164825	3551.405757	22.337408
95.464860	3563.921069	22.342426
95.095928	3568.558646	22.347443
95.852959	3557.324692	22.352461
95.531220	3566.548170	22.357479
95.591860	3567.085955	22.362496
95.670179	3577.285979	22.367514
95.798643	3591.913110	22.372531
96.086406	3595.690687	22.377549
96.349956	3595.869198	22.382567
96.472325	3599.592436	22.387584
96.433574	3590.070856	22.392602
96.259274	3595.858817	22.397619
96.793930	3596.897363	22.402637
96.614050	3609.541458	22.407655
96.812676	3624.008523	22.412672
97.094931	3615.351010	22.417690
96.803162	3627.437786	22.422707
97.236788	3624.098116	22.427725
97.000642	3622.882417	22.432743
97.340737	3624.900217	22.437760
97.555468	3622.001322	22.442778
97.143381	3625.359392	22.447795
97.626807	3625.215101	22.452813
97.928305	3648.629690	22.457831
97.914982	3647.896385	22.462848
97.831643	3652.379485	22.467866
97.272727	3650.411052	22.472883
97.760422	3654.509570	22.477901
97.790126	3662.278814	22.482919
97.899493	3662.843690	22.487936
98.093392	3672.805010	22.492954
98.094529	3687.409954	22.497971
98.438302	3681.780393	22.502989
98.077058	3687.069600	22.508007
98.496793	3712.933905	22.513024
98.693389	3712.096874	22.518042
98.504905	3712.357612	22.523059
98.628643	3718.963238	22.528077
98.697843	3726.517030	22.533095
98.851481	3746.967404	22.538112
99.350841	3742.989514	22.543130
99.000353	3745.566780	22.548147
99.227213	3735.642794	22.553165
99.332338	3753.187391	22.558183
99.426000	3770.674115	22.563200
100.116783	3761.852760	22.568218
100.351034	3757.836832	22.573235
100.688588	3753.644888	22.578253
100.751922	3757.138854	22.583271
100.484110	3733.716007	22.588288
100.352259	3716.744697	22.593306
100.312496	3724.739320	22.598323
100.771061	3722.792548	22.603341
100.865026	3718.082395	22.608359
100.899032	3728.924128	22.613376
100.977933	3712.188412	22.618394
100.718835	3719.844166	22.623411
100.911315	3736.916964	22.628429
100.670595	3750.936505	22.633447
100.730799	3753.577253	22.638464
101.141932	3760.034387	22.643482
101.135764	3759.330566	22.648499
101.615292	3753.279969	22.653517
101.792675	3755.022458	22.658535
101.632642	3752.134234	22.663552
101.406293	3766.918444	22.668570
101.449840	3782.807864	22.673587
101.634063	3790.332516	22.678605
101.763631	3790.346552	22.683623
101.561361	3788.629632	22.688640
101.934116	3806.559222	22.693658
101.651389	3822.199031	22.698675
101.910910	3824.978891	22.703693
102.085023	3837.431736	22.708711
102.110662	3849.761977	22.713728
102.402876	3843.772601	22.718746
102.633325	3852.236841	22.723763
103.220548	3862.542765	22.728781
103.625958	3870.167364	22.733799
103.030943	3872.189570	22.738816
103.492553	3864.520330	22.743834
103.308909	3873.424960	22.748851
103.414949	3872.481368	22.753869
103.626981	3873.683148	22.758887
103.120755	3878.337263	22.763904
103.870573	3871.690536	22.768922
103.820447	3868.050190	22.773939
103.838580	3869.533307	22.778957
103.986539	3887.724420	22.783975
103.572910	3899.469998	22.788992
104.062812	3898.654345	22.794010
103.920323	3900.513910	22.799027
104.179696	3910.717765	22.804045
104.063316	3928.171365	22.809063
104.100103	3939.438073	22.814080
104.307632	3939.790016	22.819098
104.577700	3951.694868	22.824115
104.809042	3962.647062	22.829133
105.134477	3966.438748	22.834151
105.137797	3961.591268	22.839168
105.434019	3963.125168	22.844186
105.374300	3967.304230	22.849203
105.510448	3968.065366	22.854221
105.647872	3958.738615	22.859239
105.562111	3955.855735	22.864256
105.795861	3953.249659	22.869274
105.673210	3964.375959	22.874291
105.767963	3981.336609	22.879309
106.135206	3984.610763	22.884327
106.226768	3980.827958	22.889344
106.614349	3979.507660	22.894362
106.420204	3977.301009	22.899379
106.321949	3977.201309	22.904397
106.642874	3970.884832	22.909415
106.701328	3979.058859	22.914432
106.497284	3982.578237	22.919450
106.553882	3984.131168	22.924467
106.869299	4001.028017	22.929485
107.189586	4001.755223	22.934503
107.150775	4009.425331	22.939520
107.108040	4006.415349	22.944538
107.729271	4007.101199	22.949555
107.701354	4006.099441	22.954573
108.057593	4007.189872	22.959591
107.812822	4007.668192	22.964608
108.005713	4007.345303	22.969626
107.815553	4017.003297	22.974643
107.570328	4035.276953	22.979661
108.199784	4025.742153	22.984679
108.020053	4041.979644	22.989696
107.992317	4034.786447	22.994714
108.021414	4037.242762	22.999731
107.906808	4050.245406	23.004749
108.541450	4052.519147	23.009767
108.333925	4062.748801	23.014784
108.445945	4078.168389	23.019802
108.950671	4085.767403	23.024819
108.889234	4093.987247	23.029837
109.250090	4089.204449	23.034855
109.045503	4100.896221	23.039872
109.150525	4108.693728	23.044890
109.545660	4113.044522	23.049907
109.400242	4115.177916	23.054925
110.258843	4107.456253	23.059943
110.170527	4113.395847	23.064960
110.415758	4115.146435	23.069978
110.335851	4109.464917	23.074995
110.453284	4109.170715	23.080013
110.554369	4106.789776	23.085031
110.606739	4109.954903	23.090048
110.526914	4113.421509	23.095066
110.591310	4108.756478	23.100083
110.451370	4135.042713	23.105101
110.594580	4141.415194	23.110119
110.550637	4163.253893	23.115136
110.510174	4144.810153	23.120154
110.758690	4159.490476	23.125171
110.704976	4174.711739	23.130189
111.533127	4164.214979	23.135207
111.745410	4160.735146	23.140224
112.192123	4161.925069	23.145242
112.258542	4158.512775	23.150259
112.117642	4157.314571	23.155277
112.548334	4141.213555	23.160295
112.467175	4143.662797	23.165312
112.413153	4139.366972	23.170330
112.425596	4143.236778	23.175347
112.352650	4150.827745	23.180365
112.986888	4142.386842	23.185383
112.857208	4150.406547	23.190400
112.725801	4141.699162	23.195418
113.176080	4135.732198	23.200435
112.759054	4138.841546	23.205453
112.796477	4135.879230	23.210471
112.854375	4137.864355	23.215488
112.794524	4136.643593	23.220506
112.930156	4152.263198	23.225523
113.079936	4165.790846	23.230541
113.313557	4167.872654	23.235559
113.122423	4176.599949	23.240576
113.063679	4187.131037	23.245594
113.613905	4191.678947	23.250611
113.371193	4208.848920	23.255629
113.413253	4221.401894	23.260647
113.931834	4246.560176	23.265664
113.972555	4241.319476	23.270682
114.248166	4249.485556	23.275699
114.179092	4270.712792	23.280717
114.630338	4266.961194	23.285735
114.484646	4276.218699	23.290752
114.098240	4281.051656	23.295770
114.336411	4294.468170	23.300787
114.677394	4305.584534	23.305805
114.792378	4310.605635	23.310823
115.084008	4334.470306	23.315840
114.905766	4333.573849	23.320858
115.255155	4336.911786	23.325875
115.027328	4358.225428	23.330893
115.435531	4354.947464	23.335911
115.740061	4361.986277	23.340928
115.710258	4366.557279	23.345946
116.342612	4380.335544	23.350963
116.096519	4384.078817	23.355981
116.501928	4373.685901	23.360999
116.821935	4374.864484	23.366016
116.643926	4371.372754	23.371034
117.145828	4366.341219	23.376051
117.084434	4372.733119	23.381069
117.116181	4374.215525	23.386087
116.902390	4380.972234	23.391104
117.209311	4377.838438	23.396122
117.372071	4369.468008	23.401139
117.062127	4387.138027	23.406157
117.312323	4400.725848	23.411175
117.347258	4407.929045	23.416192
117.005710	4415.129841	23.421210
117.534837	4410.417341	23.426227
117.738548	4428.089922	23.431245
118.086059	4431.086370	23.436263
118.003171	4435.350653	23.441280
117.892316	4437.545114	23.446298
118.222764	4450.086635	23.451315
118.143867	4472.125510	23.456333
118.550635	4476.148331	23.461351
118.743099	4469.615816	23.466368
118.538777	4472.255564	23.471386
118.788993	4474.946559	23.476403
118.815618	4485.147369	23.481421
119.376285	4482.378044	23.486439
119.358159	4494.035776	23.491456
119.488845	4496.692920	23.496474
119.671814	4484.245327	23.501491
120.219575	4477.692065	23.506509
120.399736	4469.977847	23.511527
120.453342	4453.210241	23.516544
120.177633	4464.085886	23.521562
120.634898	4461.951007	23.526579
120.560030	4470.849925	23.531597
120.798865	4466.165910	23.536615
120.914340	4466.772301	23.541632
120.630895	4469.063303	23.546650
120.931697	4465.938415	23.551667
120.982564	4473.624092	23.556685
120.918546	4472.318954	23.561703
121.235986	4482.355699	23.566720
121.225344	4497.862100	23.571738
121.649539	4502.351370	23.576755
120.876770	4519.076171	23.581773
121.140534	4514.194898	23.586791
121.479899	4526.504962	23.591808
121.451250	4545.313111	23.596826
121.477862	4542.585713	23.601843
121.351254	4547.701079	23.606861
121.681926	4574.942316	23.611879
122.073352	4577.602032	23.616896
122.111258	4582.223711	23.621914
122.423727	4595.799449	23.626931
122.493400	4604.569693	23.631949
122.618032	4606.490664	23.636967
122.944425	4603.766997	23.641984
123.005974	4613.016735	23.647002
122.957692	4623.040655	23.652019
123.171503	4641.089811	23.657037
122.987856	4637.016134	23.662055
123.367189	4634.822131	23.667072
123.720774	4638.224000	23.672090
123.995742	4651.386402	23.677107
123.807057	4650.949337	23.682125
124.135715	4650.872534	23.687143
124.387848	4657.705437	23.692160
124.396015	4669.016166	23.697178
124.351719	4662.287868	23.702195
124.139805	4660.432304	23.707213
124.456794	4661.889465	23.712231
124.450907	4656.281701	23.717248
124.292191	4675.827481	23.722266
124.511508	4686.814534	23.727283
124.586941	4687.339582	23.732301
124.620243	4691.262656	23.737319
124.990180	4710.664288	23.742336
125.109955	4718.348510	23.747354
125.321887	4711.910226	23.752371
125.373667	4728.606520	23.757389
125.488484	4746.522327	23.762407
125.929992	4751.815250	23.767424
125.684097	4745.004908	23.772442
125.911267	4749.854113	23.777459
126.110580	4774.845068	23.782477
126.523593	4779.508830	23.787495
126.602152	4772.419949	23.792512
126.668151	4782.443280	23.797530
126.781581	4775.760358	23.802547
126.968452	4785.071416	23.807565
127.223227	4804.375547	23.812583
127.536309	4805.365528	23.817600
127.323086	4818.758266	23.822618
127.599604	4808.795167	23.827635
127.875055	4810.365009	23.832653
127.466878	4804.170048	23.837671
127.908777	4807.759240	23.842688
127.620408	4813.816883	23.847706
128.073419	4815.120778	23.852723
128.009246	4816.284131	23.857741
127.724554	4830.039635	23.862759
128.116481	4826.525709	23.867776
128.074026	4843.707719	23.872794
128.184638	4848.650976	23.877811
128.310636	4856.663436	23.882829
128.380403	4874.887994	23.887847
128.895629	4877.221716	23.892864
128.948446	4891.711003	23.897882
129.081579	4893.709317	23.902899
129.361881	4912.713834	23.907917
129.447252	4918.490051	23.912935
129.920055	4915.235558	23.917952
130.058979	4924.929053	23.922970
129.862937	4915.802262	23.927987
130.426964	4919.988064	23.933005
130.251914	4930.219009	23.938023
130.402250	4933.974788	23.943040
130.253368	4944.847921	23.948058
130.375432	4945.871447	23.953075
130.631988	4942.019957	23.958093
130.222291	4946.431772	23.963111
130.668060	4959.999149	23.968128
130.929835	4979.257396	23.973146
131.081959	4972.471664	23.978163
131.154954	4980.851658	23.983181
130.896022	4983.548899	23.988199
131.373118	4990.263825	23.993216
131.300890	5013.063973	23.998234
131.425946	5006.838166	24.003251
131.913645	5020.195190	24.008269
131.352642	5042.002442	24.013287
131.876542	5043.358004	24.018304
131.981686	5052.433542	24.023322
132.000417	5065.326728	24.028339
132.225919	5073.675111	24.033357
132.569411	5077.849141	24.038375
133.587963	5088.572642	24.043392
133.197277	5101.903886	24.048410
133.540482	5103.157316	24.053427
133.664521	5103.752812	24.058445
133.375487	5104.886208	24.063463
133.554675	5087.315041	24.068480
133.728054	5095.176145	24.073498
133.734054	5094.421343	24.078515
133.724197	5088.752669	24.083533
133.584416	5113.972427	24.088551
134.468242	5116.181557	24.093568
134.106533	5122.540175	24.098586
133.791852	5127.034996	24.103603
134.193235	5142.153173	24.108621
134.583516	5166.098281	24.113639
134.675000	5153.502801	24.118656
134.699925	5165.326144	24.123674
134.517844	5182.205575	24.128691
134.709854	5182.624012	24.133709
134.888033	5201.759807	24.138727
135.150813	5211.513374	24.143744
135.359529	5225.634390	24.148762
135.225508	5233.331652	24.153779
135.999604	5240.960666	24.158797
136.033787	5255.065945	24.163815
136.138845	5247.966007	24.168832
136.454628	5248.405761	24.173850
136.463846	5245.174752	24.178867
136.639124	5260.875298	24.183885
136.707317	5278.292438	24.188903
136.934961	5272.851578	24.193920
137.317923	5267.764539	24.198938
137.187994	5282.530477	24.203955
137.407547	5281.354672	24.208973
137.121632	5281.270592	24.213991
137.075941	5293.759905	24.219008
137.505767	5304.647497	24.224026
137.443816	5310.753944	24.229043
137.305693	5313.470700	24.234061
137.215889	5328.519665	24.239079
137.725521	5330.895376	24.244096
138.149136	5353.276244	24.249114
138.304542	5352.878628	24.254131
138.870024	5356.022991	24.259149
138.816265	5349.875754	24.264167
138.897928	5347.685427	24.269184
138.915198	5348.562321	24.274202
139.252878	5365.081880	24.279219
139.534993	5370.332236	24.284237
139.447467	5388.964797	24.289255
139.571371	5384.014291	24.294272
139.690156	5377.064752	24.299290
139.856217	5379.233923	24.304307
140.069339	5386.369209	24.309325
139.728984	5390.414014	24.314343
139.823279	5407.620450	24.319360
139.979437	5407.844181	24.324378
140.010057	5423.032490	24.329395
140.421163	5439.270940	24.334413
140.269100	5451.752619	24.339431
140.341048	5449.094486	24.344448
140.711886	5469.583106	24.349466
140.817932	5476.660383	24.354483
141.479350	5468.933283	24.359501
141.809069	5493.523352	24.364519
142.086640	5495.114168	24.369536
142.047655	5492.962621	24.374554
142.064964	5498.258417	24.379571
142.518456	5489.458682	24.384589
142.518470	5498.893565	24.389607
142.506396	5496.422331	24.394624
142.870389	5493.072163	24.399642
142.703967	5490.850304	24.404659
142.553122	5484.534553	24.409677
143.044414	5492.977013	24.414695
143.168237	5507.659486	24.419712
142.905278	5522.188517	24.424730
142.806366	5529.606576	24.429747
143.341399	5519.265526	24.434765
143.455663	5548.912529	24.439783
143.781904	5557.673187	24.444800
143.679812	5552.960656	24.449818
143.658564	5557.193404	24.454835
143.751829	5570.846943	24.459853
143.966564	5578.104130	24.464871
144.186650	5586.688444	24.469888
144.197832	5599.988229	24.474906
144.488989	5623.693448	24.479923
144.679331	5617.861871	24.484941
144.684459	5629.622000	24.489959
144.829853	5651.118361	24.494976
145.139275	5647.150515	24.499994
144.917276	5659.096112	24.505011
145.426479	5666.154772	24.510029
145.286774	5680.694324	24.515047
145.560360	5678.415912	24.520064
145.999034	5676.890589	24.525082
145.730729	5684.962400	24.530099
145.829092	5708.962311	24.535117
146.169254	5711.668033	24.540135
146.426447	5715.522258	24.545152
146.651278	5723.956170	24.550170
146.646995	5740.062128	24.555187
146.949898	5745.336615	24.560205
146.973743	5738.812008	24.565223
146.884043	5745.222702	24.570240
147.281406	5753.686130	24.575258
147.354070	5763.698699	24.580275
147.880206	5762.541982	24.585293
148.055364	5765.330352	24.590311
147.823583	5770.345197	24.595328
148.021783	5787.792596	24.600346
148.344072	5790.881853	24.605363
148.391811	5786.530327	24.610381
148.711590	5786.227402	24.615399
148.726785	5809.599750	24.620416
149.338487	5808.486651	24.625434
149.396566	5812.454592	24.630451
149.314341	5806.738203	24.635469
149.560284	5809.255293	24.640487
149.748720	5806.800049	24.645504
149.862262	5809.565119	24.650522
149.718569	5813.191918	24.655539
150.188641	5817.357837	24.660557
150.100967	5822.775714	24.665575
150.055885	5841.532286	24.670592
150.371680	5852.707624	24.675610
149.849764	5856.297659	24.680627
149.988184	5862.784297	24.685645
150.703673	5879.522409	24.690663
150.233088	5888.486806	24.695680
150.794059	5896.286588	24.700698
151.004227	5917.833646	24.705715
150.709268	5923.421790	24.710733
151.188630	5934.145360	24.715751
151.229026	5948.276970	24.720768
151.556478	5963.701633	24.725786
151.695543	5983.603635	24.730803
151.635211	5985.170508	24.735821
152.006664	6000.289122	24.740839
151.901357	6021.707655	24.745856
152.064413	6029.246455	24.750874
152.117628	6046.344043	24.755891
152.487790	6052.546841	24.760909
152.839338	6058.809547	24.765927
152.707839	6077.855334	24.770944
153.301744	6085.819710	24.775962
153.191107	6088.609081	24.780979
153.410898	6105.333157	24.785997
153.439169	6113.212552	24.791015
153.740671	6116.149470	24.796032
153.978381	6107.645549	24.801050
154.329571	6136.682724	24.806067
154.336514	6136.899751	24.811085
154.596797	6134.011502	24.816103
154.787217	6138.472790	24.821120
154.785054	6140.813482	24.826138
154.978125	6149.093159	24.831155
154.914698	6172.618155	24.836173
155.494492	6177.508964	24.841191
155.064053	6178.555605	24.846208
155.270338	6173.532441	24.851226
155.524562	6197.897077	24.856243
155.673197	6203.625106	24.861261
155.723318	6211.819830	24.866279
155.794159	6227.798394	24.871296
156.073469	6227.746594	24.876314
156.141321	6234.501490	24.881331
156.809310	6245.372534	24.886349
157.304619	6245.713800	24.891367
157.052585	6250.532186	24.896384
157.633474	6240.822442	24.901402
157.905030	6246.768094	24.906419
158.012795	6245.021383	24.911437
157.956033	6246.931902	24.916455
157.750963	6248.715817	24.921472
158.058761	6236.848063	24.926490
157.961651	6258.315134	24.931507
158.147416	6269.356300	24.936525
158.496255	6268.068462	24.941543
158.419613	6278.511050	24.946560
158.610295	6280.024680	24.951578
158.638610	6299.351333	24.956595
158.538189	6303.446609	24.961613
158.887615	6317.421590	24.966631
159.344465	6335.903643	24.971648
159.569154	6345.699098	24.976666
159.654406	6345.603369	24.981683
159.134416	6347.509812	24.986701
159.724597	6362.910304	24.991719
159.869445	6371.344094	24.996736
159.982222	6369.201859	25.001754
160.181398	6400.064741	25.006771
160.259821	6404.399574	25.011789
160.382079	6410.440202	25.016807
160.685286	6433.522256	25.021824
160.817834	6438.525267	25.026842
160.697332	6446.817894	25.031859
160.991480	6467.475343	25.036877
161.255976	6460.457817	25.041895
161.496229	6486.176246	25.046912
161.628142	6492.142778	25.051930
161.857117	6496.409290	25.056947
161.933814	6496.802632	25.061965
162.491431	6499.189993	25.066983
162.875089	6499.690623	25.072000
163.372083	6507.421327	25.077018
163.650803	6511.481594	25.082035
163.756181	6497.204801	25.087053
163.883010	6478.413005	25.092071
163.566219	6473.549527	25.097088
163.979322	6462.864056	25.102106
164.126580	6460.615069	25.107123
164.214003	6463.628927	25.112141
164.701397	6463.201156	25.117159
164.479328	6458.744455	25.122176
164.668320	6455.951082	25.127194
164.465699	6458.808276	25.132211
164.544358	6482.618161	25.137229
164.701348	6485.453885	25.142247
164.724850	6494.484375	25.147264
164.941791	6493.961962	25.152282
165.322961	6510.075090	25.157299
165.205046	6530.756786	25.162317
165.420314	6530.051117	25.167335
165.826203	6537.978633	25.172352
166.047834	6558.978694	25.177370
165.729236	6571.238508	25.182387
165.696363	6576.930831	25.187405
165.746286	6573.754806	25.192423
166.386165	6591.612615	25.197440
166.142595	6596.861333	25.202458
166.612213	6621.295248	25.207475
166.612920	6628.562823	25.212493
166.784373	6628.199451	25.217511
167.204506	6663.804964	25.222528
166.879869	6666.342807	25.227546
167.381775	6672.884838	25.232563
167.405972	6702.931480	25.237581
168.037443	6694.517295	25.242599
168.009815	6704.575219	25.247616
167.920790	6709.306716	25.252634
168.561638	6710.675470	25.257651
168.663682	6715.049664	25.262669
168.785651	6724.576224	25.267687
169.014290	6744.239314	25.272704
169.056413	6730.495432	25.277722
169.513194	6744.327133	25.282739
169.597305	6769.955414	25.287757
170.039680	6758.279259	25.292775
170.264153	6758.829245	25.297792
170.517810	6761.220702	25.302810
170.725133	6755.611097	25.307827
170.424894	6754.915805	25.312845
170.857762	6752.689501	25.317863
171.346626	6751.023137	25.322880
171.360167	6750.199219	25.327898
171.751484	6735.127989	25.332915
171.309830	6740.311454	25.337933
171.973359	6747.315787	25.342951
171.747768	6750.419595	25.347968
171.508607	6756.812201	25.352986
172.215016	6760.899259	25.358003
172.317540	6765.828746	25.363021
172.459475	6755.982826	25.368039
172.201993	6768.223648	25.373056
172.238584	6771.177744	25.378074
172.880212	6778.105495	25.383091
172.732815	6797.869351	25.388109
172.688874	6793.142545	25.393127
173.059931	6813.569841	25.398144
172.627133	6824.361369	25.403162
172.895730	6831.948628	25.408179
172.914395	6855.346332	25.413197
173.150215	6857.421035	25.418215
173.611341	6890.436208	25.423232
173.476698	6902.389814	25.428250
174.072287	6912.231534	25.433267
174.290936	6921.135068	25.438285
174.564796	6931.625920	25.443303
174.761960	6952.932403	25.448320
175.180562	6956.825434	25.453338
175.262431	6947.471800	25.458355
175.355802	6962.753226	25.463373
175.514238	6971.571005	25.468391
175.841049	6980.682905	25.473408
175.702388	6989.605979	25.478426
176.293351	6998.953047	25.483443
176.320614	7009.643775	25.488461
176.517512	7011.525081	25.493479
176.698982	7016.950791	25.498496
176.785149	7032.433608	25.503514
177.042300	7038.660107	25.508531
177.137164	7037.128217	25.513549
177.342982	7041.168032	25.518567
177.395891	7057.144198	25.523584
177.729104	7070.954828	25.528602
178.083725	7072.961929	25.533619
177.859361	7078.672289	25.538637
178.655696	7097.364082	25.543655
178.615314	7105.474734	25.548672
178.376397	7114.521411	25.553690
178.796990	7109.653433	25.558707
179.039139	7134.617906	25.563725
179.285716	7140.399595	25.568743
179.194355	7143.864108	25.573760
179.352781	7144.545170	25.578778
179.627178	7150.558423	25.583795
179.565192	7167.249991	25.588813
179.609994	7170.401270	25.593831
180.000861	7178.750774	25.598848
180.099617	7199.951565	25.603866
180.052730	7197.444284	25.608883
179.905415	7224.431686	25.613901
180.474549	7226.732108	25.618919
180.574380	7239.268107	25.623936
180.425393	7257.752677	25.628954
181.143698	7268.663068	25.633971
180.947750	7289.849112	25.638989
181.380957	7302.664389	25.644007
181.789157	7317.065023	25.649024
181.399145	7330.807640	25.654042
181.768630	7335.895572	25.659059
182.162941	7348.150357	25.664077
182.302907	7360.013112	25.669095
182.585254	7384.695363	25.674112
182.443173	7392.074418	25.679130
182.808426	7400.858555	25.684148
182.940107	7422.715729	25.689165
182.807317	7431.211065	25.694183
183.151960	7450.113051	25.699200
183.582360	7466.390443	25.704218
184.184972	7477.961276	25.709236
184.453618	7484.703550	25.714253
184.530915	7485.002281	25.719271
184.906350	7477.726599	25.724288
184.818700	7497.955318	25.729306
185.269407	7503.142821	25.734324
185.361380	7509.356067	25.739341
185.358536	7514.966372	25.744359
185.991677	7513.079044	25.749376
185.928562	7522.043820	25.754394
185.987734	7526.134894	25.759412
186.184647	7541.124974	25.764429
186.445349	7547.432992	25.769447
186.651339	7545.633065	25.774464
186.552797	7570.046875	25.779482
187.178171	7567.299824	25.784500
187.011209	7572.226125	25.789517
187.094458	7581.423450	25.794535
187.373297	7597.518981	25.799552
187.611174	7601.946549	25.804570
187.521953	7603.281407	25.809588
187.781636	7625.851132	25.814605
187.686600	7632.957535	25.819623
188.122204	7640.566970	25.824640
188.030691	7669.526054	25.829658
188.384868	7659.283179	25.834676
188.705751	7692.609228	25.839693
188.947356	7695.709543	25.844711
189.292626	7701.365015	25.849728
189.782582	7710.919677	25.854746
190.114911	7712.992918	25.859764
190.229881	7721.794141	25.864781
190.262956	7718.404923	25.869799
190.963135	7711.739152	25.874816
190.384455	7716.535188	25.879834
190.641727	7734.447265	25.884852
190.869927	7744.427322	25.889869
190.839311	7756.448811	25.894887
191.139432	7751.984950	25.899904
191.427422	7760.144418	25.904922
191.431673	7771.638421	25.909940
191.493848	7778.060918	25.914957
191.225971	7784.097255	25.919975
191.570854	7790.664305	25.924992
191.903880	7812.160559	25.930010
191.929124	7829.275088	25.935028
192.091464	7839.558768	25.940045
192.061186	7856.346454	25.945063
192.656592	7875.364303	25.950080
192.368105	7885.752868	25.955098
193.708201	7885.362454	25.960116
194.099722	7886.852841	25.965133
194.420251	7883.784579	25.970151
194.801966	7870.385648	25.975168
194.960477	7873.519937	25.980186
194.900225	7873.982484	25.985204
195.621040	7863.589184	25.990221
195.662460	7874.111047	25.995239
195.965615	7856.265072	26.000256
196.096309	7859.961101	26.005274
196.200007	7864.413319	26.010292
196.526779	7852.852304	26.015309
196.360068	7851.947361	26.020327
196.703100	7842.301069	26.025344
196.597871	7851.249613	26.030362
196.672803	7848.743406	26.035380
197.014476	7844.515826	26.040397
196.841828	7845.887851	26.045415
196.981464	7854.430459	26.050432
197.194458	7867.629785	26.055450
197.141170	7874.974144	26.060468
197.541175	7886.334214	26.065485
197.535617	7907.893365	26.070503
197.984084	7911.568021	26.075520
197.655856	7925.694453	26.080538
197.809219	7950.228734	26.085556
198.331169	7961.890165	26.090573
197.965030	7972.675758	26.095591
198.323905	7983.177938	26.100608
198.682208	7999.825897	26.105626
198.464870	8016.442563	26.110644
198.688673	8032.301383	26.115661
198.865921	8052.157662	26.120679
199.725488	8068.448759	26.125696
200.103608	8087.546651	26.130714
200.197687	8091.540500	26.135732
200.347783	8099.114802	26.140749
200.432534	8103.327689	26.145767
200.633621	8115.059991	26.150784
200.795393	8129.895932	26.155802
200.859304	8139.452983	26.160820
201.341234	8149.062857	26.165837
201.300867	8170.258053	26.170855
201.642872	8173.221504	26.175872
201.380933	8192.788484	26.180890
201.854148	8210.648320	26.185908
201.907039	8206.030548	26.190925
202.417404	8224.547372	26.195943
202.991592	8229.061635	26.200960
202.657841	8242.105254	26.205978
202.926486	8257.531976	26.210996
203.556760	8259.287146	26.216013
203.449053	8271.183579	26.221031
203.213492	8276.054101	26.226048
203.599117	8297.387577	26.231066
203.954443	8320.163262	26.236084
204.315952	8329.413369	26.241101
203.797673	8336.678507	26.246119
204.383125	8353.246141	26.251136
204.819265	8369.228036	26.256154
204.987772	8386.663667	26.261172
205.587280	8392.977756	26.266189
205.485695	8395.754943	26.271207
206.185471	8407.390945	26.276224
206.129415	8416.365250	26.281242
206.232355	8424.694648	26.286260
206.461683	8430.918583	26.291277
206.556104	8451.676647	26.296295
206.607583	8456.557893	26.301312
207.140105	8463.920276	26.306330
207.172581	8480.319698	26.311348
207.453634	8478.877082	26.316365
207.676079	8495.212442	26.321383
207.976843	8510.133628	26.326400
207.910628	8511.145545	26.331418
207.833755	8525.427947	26.336436
208.093428	8542.303728	26.341453
208.186150	8557.478850	26.346471
208.506734	8579.802340	26.351488
208.889258	8594.176225	26.356506
208.893324	8613.951800	26.361524
209.143917	8618.833628	26.366541
209.116379	8646.344125	26.371559
209.237274	8660.744010	26.376576
209.274725	8672.165211	26.381594
209.115883	8703.947917	26.386612
209.594503	8720.369585	26.391629
209.653976	8744.333440	26.396647
210.306173	8765.699839	26.401664
211.628826	8780.275143	26.406682
211.634044	8785.987717	26.411700
211.927735	8802.679099	26.416717
212.217121	8804.619611	26.421735
212.341238	8804.062620	26.426752
212.703500	8803.401780	26.431770
212.599766	8801.111196	26.436788
213.030490	8808.695240	26.441805
213.447144	8826.722240	26.446823
213.709507	8822.739630	26.451840
214.009731	8809.063178	26.456858
214.484408	8813.083355	26.461876
214.161069	8816.876343	26.466893
214.600872	8814.390165	26.471911
214.707092	8813.278448	26.476928
214.643617	8809.495083	26.481946
214.786293	8806.897543	26.486964
214.606558	8803.622574	26.491981
214.900443	8823.867128	26.496999
215.003089	8827.691093	26.502016
215.460057	8831.834064	26.507034
215.453567	8852.886477	26.512052
215.790733	8862.905278	26.517069
215.800915	8863.656736	26.522087
215.919488	8898.219860	26.527104
216.135212	8900.121013	26.532122
216.216153	8921.795111	26.537140
216.263074	8936.467915	26.542157
216.462184	8956.344410	26.547175
216.453816	8981.681657	26.552192
216.985217	9000.708665	26.557210
217.153456	9029.928203	26.562228
217.322716	9046.242512	26.567245
217.437642	9072.255232	26.572263
217.790159	9091.974813	26.577280
218.190294	9103.854925	26.582298
218.295588	9120.786926	26.587316
218.494757	9134.177960	26.592333
218.537895	9156.024304	26.597351
218.914449	9167.161611	26.602368
219.209219	9186.237279	26.607386
219.502664	9212.760099	26.612404
219.945655	9215.222686	26.617421
220.239018	9239.793234	26.622439
220.499324	9254.300538	26.627456
220.736696	9256.204326	26.632474
220.635091	9270.037813	26.637492
221.044638	9275.826219	26.642509
221.532049	9302.656297	26.647527
221.604015	9310.100382	26.652544
221.968050	9321.019338	26.657562
222.417886	9333.597033	26.662580
222.341680	9343.020453	26.667597
222.968346	9354.833556	26.672615
222.857327	9370.929937	26.677632
223.088863	9364.245348	26.682650
223.381823	9377.436145	26.687668
223.366629	9389.441238	26.692685
223.737669	9395.672770	26.697703
223.589823	9408.376612	26.702720
223.986016	9420.170967	26.707738
223.771731	9438.194926	26.712756
223.745127	9450.688927	26.717773
223.961632	9458.941878	26.722791
224.147839	9482.705469	26.727808
224.696716	9504.886319	26.732826
224.988360	9525.515047	26.737844
225.153174	9549.698404	26.742861
225.683764	9551.438511	26.747879
225.187748	9573.505474	26.752896
225.750409	9597.844464	26.757914
226.175062	9615.959219	26.762932
226.295044	9623.124186	26.767949
226.344808	9638.293506	26.772967
226.599242	9660.912682	26.777984
227.242899	9666.683161	26.783002
227.515811	9692.983377	26.788020
228.020772	9707.650851	26.793037
228.197005	9694.860010	26.798055
228.134305	9719.810630	26.803072
228.711333	9729.755764	26.808090
228.623854	9738.976495	26.813108
229.277196	9751.522785	26.818125
229.578313	9759.570717	26.823143
229.320993	9771.436380	26.828160
229.674715	9778.011400	26.833178
229.861553	9796.668223	26.838196
229.856858	9801.884906	26.843213
230.131668	9810.277743	26.848231
229.844736	9836.133662	26.853248
230.458073	9858.105399	26.858266
230.411416	9882.744663	26.863284
230.680208	9908.097306	26.868301
230.600153	9931.505368	26.873319
230.651307	9951.290263	26.878336
231.079140	9966.525875	26.883354
230.944011	10003.788501	26.888372
231.187728	10032.097123	26.893389
231.976986	10061.421654	26.898407
231.985706	10072.868467	26.903424
232.501504	10103.933950	26.908442
232.516357	10126.246589	26.913460
233.028997	10149.142079	26.918477
233.579824	10163.453848	26.923495
233.434076	10182.886700	26.928512
233.970337	10201.832351	26.933530
234.482914	10211.229413	26.938548
234.452043	10235.787715	26.943565
235.376086	10233.382209	26.948583
235.306920	10240.289918	26.953600
235.324542	10247.688596	26.958618
235.967889	10267.098171	26.963636
236.098565	10265.591358	26.968653
236.400292	10271.932814	26.973671
236.702791	10291.345691	26.978688
236.824251	10291.164156	26.983706
237.078495	10290.258614	26.988724
237.409259	10312.284134	26.993741
237.477075	10319.945284	26.998759
237.744336	10321.718011	27.003776
238.439582	10314.504434	27.008794
238.263316	10319.372492	27.013812
238.603025	10332.649030	27.018829
238.952306	10339.422021	27.023847
238.772875	10347.325698	27.028864
238.965654	10339.879920	27.033882
239.156648	10360.418233	27.038900
239.350023	10381.827605	27.043917
239.728441	10385.413992	27.048935
239.530014	10410.098981	27.053952
239.965396	10417.771238	27.058970
239.896373	10436.619209	27.063988
239.668009	10449.547253	27.069005
240.510446	10462.835427	27.074023
240.709024	10474.284648	27.079040
241.278210	10505.296051	27.084058
241.927808	10513.190074	27.089076
241.878106	10519.081290	27.094093
242.209071	10537.777295	27.099111
242.135425	10554.508240	27.104128
242.554877	10564.088513	27.109146
242.819881	10591.852368	27.114164
242.751328	10598.785338	27.119181
242.944763	10614.832339	27.124199
243.492571	10632.169132	27.129216
243.790221	10647.268538	27.134234
243.755993	10660.592109	27.139252
243.888466	10671.729746	27.144269
244.083318	10683.071017	27.149287
244.074295	10704.923660	27.154304
244.959685	10716.044157	27.159322
245.118020	10731.197464	27.164340
245.118514	10750.470400	27.169357
245.381518	10766.549751	27.174375
245.397666	10787.863967	27.179392
245.693453	10811.391673	27.184410
245.879793	10818.993346	27.189428
246.061700	10853.472562	27.194445
247.017086	10866.232698	27.199463
247.334318	10872.631617	27.204480
247.366290	10881.971198	27.209498
247.967231	10896.744645	27.214516
248.274798	10913.150592	27.219533
248.225055	10913.822591	27.224551
248.283905	10933.315822	27.229568
248.349340	10945.232600	27.234586
248.679975	10944.769364	27.239604
248.726343	10973.576771	27.244621
249.121421	10987.312399	27.249639
249.127732	11012.811041	27.254656
249.264024	11020.249614	27.259674
249.831539	11046.479464	27.264692
249.624388	11062.286693	27.269709
250.457990	11076.557106	27.274727
250.363227	11096.798631	27.279744
250.640779	11115.329530	27.284762
251.351955	11116.540873	27.289780
250.886938	11140.008778	27.294797
251.354894	11149.092550	27.299815
251.575878	11170.933183	27.304832
252.255537	11183.422497	27.309850
252.418139	11198.041270	27.314868
252.414589	11212.723207	27.319885
252.974399	11224.082671	27.324903
253.379016	11238.581200	27.329920
253.394320	11251.896763	27.334938
253.907459	11269.173992	27.339956
253.755982	11287.340518	27.344973
253.734295	11299.740541	27.349991
254.112986	11320.882995	27.355008
254.243333	11348.855608	27.360026
254.580076	11366.836101	27.365044
254.645370	11397.212224	27.370061
255.111411	11420.572945	27.375079
255.229367	11435.640849	27.380096
255.609542	11460.459912	27.385114
255.863471	11477.195540	27.390132
256.064863	11502.809649	27.395149
256.143781	11518.944937	27.400167
256.153512	11547.423958	27.405184
256.463400	11572.178017	27.410202
257.401072	11587.226903	27.415220
258.008278	11598.004857	27.420237
258.562198	11604.557339	27.425255
258.659791	11616.239005	27.430272
259.233622	11630.869628	27.435290
259.245594	11648.113391	27.440308
259.508180	11649.181035	27.445325
260.194100	11653.512438	27.450343
260.211212	11653.689186	27.455360
260.357813	11673.844350	27.460378
260.721695	11670.724619	27.465396
260.729180	11678.926276	27.470413
260.749632	11691.963945	27.475431
261.104845	11701.020073	27.480448
261.286458	11715.650236	27.485466
262.075000	11719.396717	27.490484
262.001032	11736.924795	27.495501
262.269663	11739.080408	27.500519
262.416037	11760.862126	27.505536
262.811391	11779.189200	27.510554
262.767753	11782.444794	27.515572
262.554683	11817.758102	27.520589
263.308108	11810.236046	27.525607
263.874981	11829.351712	27.530624
263.957540	11841.096003	27.535642
264.431504	11837.451480	27.540660
264.717760	11848.272006	27.545677
265.069742	11852.635488	27.550695
265.236064	11853.798446	27.555712
265.160949	11854.659222	27.560730
266.104574	11864.922654	27.565748
266.031604	11875.655053	27.570765
266.270424	11881.544585	27.575783
266.542570	11877.904703	27.580800
266.245745	11888.897695	27.585818
266.615876	11905.292344	27.590836
266.700104	11917.550177	27.595853
266.909824	11944.169036	27.600871
267.411365	11957.319878	27.605888
267.606238	11986.593753	27.610906
267.896372	11990.906410	27.615924
267.827220	12016.175274	27.620941
268.063378	12032.183254	27.625959
268.010006	12051.465383	27.630976
268.277678	12073.009237	27.635994
268.532507	12097.053296	27.641012
268.709489	12119.832588	27.646029
268.899060	12155.061847	27.651047
269.180549	12184.798763	27.656064
269.442775	12212.357821	27.661082
269.792915	12240.010602	27.666100
270.259815	12268.217090	27.671117
270.727133	12295.632388	27.676135
271.356398	12302.183273	27.681152
271.300848	12324.444793	27.686170
272.314449	12333.709934	27.691188
272.175586	12346.023664	27.696205
272.740652	12360.243527	27.701223
273.302057	12370.249709	27.706240
273.256231	12381.136966	27.711258
273.813101	12383.136090	27.716276
274.181710	12405.063394	27.721293
274.116752	12407.972886	27.726311
274.832382	12421.308053	27.731328
275.590948	12420.320686	27.736346
276.213093	12405.682977	27.741364
276.259075	12400.365439	27.746381
276.572264	12397.292087	27.751399
276.714079	12400.878506	27.756416
276.971733	12402.897398	27.761434
277.470965	12398.789797	27.766452
277.647773	12392.564104	27.771469
277.434220	12396.737829	27.776487
277.838195	12395.177675	27.781504
278.350327	12399.212831	27.786522
278.589508	12390.019799	27.791540
278.786382	12393.878890	27.796557
278.898721	12385.317528	27.801575
279.041603	12390.810767	27.806592
279.281161	12410.331525	27.811610
279.650224	12422.307662	27.816628
279.810372	12416.842891	27.821645
279.569649	12419.612299	27.826663
279.835334	12420.512405	27.831680
280.072372	12447.374841	27.836698
280.023178	12449.440030	27.841716
280.138929	12465.956071	27.846733
280.307593	12482.475668	27.851751
280.139166	12514.769425	27.856768
280.059382	12543.979475	27.861786
280.581878	12566.567780	27.866804
280.476568	12604.048723	27.871821
280.982811	12634.622647	27.876839
281.185395	12660.559884	27.881856
281.361546	12695.822553	27.886874
281.788315	12728.553726	27.891892
281.935794	12753.490294	27.896909
282.356889	12794.979236	27.901927
282.979593	12826.420887	27.906944
283.289389	12850.592175	27.911962
283.968981	12879.382664	27.916980
284.509452	12907.081178	27.921997
284.728084	12926.636084	27.927015
285.447326	12935.367299	27.932032
285.595835	12948.185431	27.937050
286.541144	12955.751003	27.942068
287.207669	12954.107970	27.947085
286.855792	12950.839597	27.952103
287.379614	12958.168500	27.957120
287.708722	12972.776084	27.962138
288.263756	12967.386871	27.967156
288.245395	12978.104327	27.972173
288.115456	12988.241997	27.977191
288.857976	13000.933139	27.982208
288.624576	13014.193470	27.987226
288.985726	13027.147012	27.992244
289.200316	13040.191881	27.997261
289.033430	13054.295090	28.002279
289.422894	13069.962589	28.007296
289.260284	13092.790409	28.012314
289.670956	13106.091725	28.017332
289.987300	13130.924270	28.022349
289.881685	13168.059808	28.027367
290.672399	13187.282128	28.032384
291.002966	13211.212395	28.037402
290.988940	13230.244866	28.042420
291.493982	13258.846861	28.047437
291.769160	13279.161642	28.052455
292.258805	13299.567354	28.057472
292.150345	13319.566518	28.062490
292.701056	13342.034424	28.067508
293.385608	13368.489100	28.072525
293.513073	13391.278647	28.077543
293.800101	13409.328230	28.082560
293.636375	13421.678548	28.087578
294.128820	13451.134150	28.092596
294.414214	13460.617751	28.097613
294.742419	13485.898000	28.102631
295.515873	13492.577543	28.107648
294.980021	13516.923128	28.112666
295.443003	13535.331999	28.117684
295.776222	13552.538463	28.122701
296.083795	13583.476047	28.127719
296.256134	13598.293893	28.132736
296.370126	13637.820125	28.137754
296.571082	13649.130889	28.142772
296.853660	13683.532615	28.147789
296.950079	13710.314039	28.152807
297.413583	13746.024624	28.157824
297.777582	13752.771303	28.162842
298.392226	13781.470482	28.167860
299.224513	13791.541443	28.172877
299.809476	13815.283979	28.177895
300.368105	13816.832202	28.182912
300.496942	13842.032109	28.187930
300.737937	13843.420416	28.192948
301.139197	13847.019426	28.197965
301.048613	13872.734571	28.202983
301.655617	13871.896052	28.208000
301.599409	13898.502191	28.213018
302.116568	13905.755432	28.218036
302.268932	13911.635297	28.223053
302.544316	13939.188697	28.228071
302.561300	13954.769570	28.233088
302.921272	13975.797301	28.238106
303.049834	13995.816555	28.243124
303.502524	14020.089592	28.248141
303.421414	14050.175752	28.253159
303.700530	14074.477044	28.258176
304.211220	14092.340878	28.263194
304.233745	14132.337919	28.268212
304.762996	14152.011272	28.273229
304.703392	14178.802861	28.278247
305.304357	14202.658277	28.283264
305.618218	14241.062535	28.288282
305.654490	14265.192941	28.293300
306.148555	14296.411991	28.298317
306.401050	14327.443953	28.303335
306.500611	14349.634337	28.308352
306.536101	14378.952403	28.313370
306.607820	14421.879801	28.318388
307.289272	14447.999433	28.323405
307.288635	14487.558380	28.328423
307.780542	14519.334634	28.333440
308.232197	14560.882687	28.338458
308.690119	14597.097319	28.343476
309.326237	14620.212783	28.348493
309.480359	14648.409193	28.353511
309.849929	14673.324787	28.358528
310.189759	14698.645886	28.363546
310.678458	14730.974788	28.368564
311.331433	14742.965434	28.373581
310.569282	14768.710380	28.378599
311.026245	14789.103051	28.383616
311.990798	14812.227119	28.388634
312.759331	14833.206409	28.393652
313.715538	14824.172861	28.398669
313.917988	14820.928895	28.403687
314.469407	14827.710099	28.408704
314.840789	14843.814287	28.413722
315.238691	14860.394709	28.418740
315.757219	14854.112676	28.423757
315.473465	14860.379732	28.428775
315.643128	14861.356336	28.433792
315.984881	14861.534223	28.438810
316.411491	14870.795824	28.443828
316.175043	14890.538247	28.448845
316.254675	14895.876081	28.453863
316.462008	14908.766047	28.458880
316.857041	14931.459844	28.463898
316.798513	14963.017615	28.468916
317.230837	14983.793059	28.473933
317.236381	15007.108568	28.478951
317.765061	15032.352099	28.483968
318.314535	15060.667453	28.488986
318.291122	15078.236132	28.494004
318.534083	15102.135296	28.499021
318.494080	15139.717989	28.504039
318.958929	15166.443353	28.509056
319.289355	15194.837464	28.514074
319.472202	15230.588331	28.519092
319.954868	15256.573075	28.524109
319.974043	15290.767931	28.529127
320.296192	15328.665719	28.534144
320.952697	15357.614256	28.539162
321.430768	15391.689683	28.544180
322.348844	15409.611229	28.549197
322.460390	15428.545891	28.554215
322.742625	15458.897055	28.559232
323.602577	15481.660097	28.564250
323.512175	15503.564590	28.569268
323.647877	15523.355899	28.574285
324.629677	15543.829794	28.579303
324.285520	15551.953354	28.584320
325.596605	15569.418359	28.589338
325.993417	15577.446461	28.594356
326.450978	15585.312826	28.599373
325.893060	15601.487177	28.604391
326.233202	15611.821744	28.609408
326.817893	15618.354816	28.614426
326.599869	15647.939264	28.619444
327.119145	15662.185609	28.624461
327.362458	15691.014809	28.629479
327.503855	15714.828224	28.634496
327.656993	15742.303116	28.639514
328.027175	15773.558800	28.644532
328.634680	15792.437248	28.649549
328.719319	15813.248102	28.654567
328.837318	15840.659820	28.659584
329.133564	15854.443271	28.664602
329.141678	15893.715594	28.669620
329.473217	15919.334762	28.674637
329.900328	15953.662840	28.679655
330.063780	15984.883416	28.684672
330.440346	16001.031982	28.689690
330.441851	16043.434909	28.694708
331.223117	16075.667425	28.699725
331.168353	16112.242802	28.704743
331.653982	16149.638374	28.709760
331.983468	16173.415479	28.714778
332.447318	16210.677774	28.719796
333.296198	16249.173121	28.724813
333.294470	16270.382416	28.729831
333.793433	16306.954748	28.734848
334.012816	16328.996400	28.739866
334.360570	16369.122798	28.744884
335.069758	16391.652824	28.749901
335.319550	16419.809046	28.754919
335.764341	16447.383298	28.759936
336.318644	16460.309588	28.764954
336.371471	16486.105089	28.769972
336.703597	16513.580529	28.774989
337.035626	16535.120760	28.780007
337.203161	16558.725965	28.785024
337.961094	16579.135469	28.790042
338.694821	16597.006351	28.795060
338.949984	16613.031287	28.800077
339.326899	16630.922372	28.805095
339.357093	16650.991642	28.810112
339.858658	16660.277660	28.815130
339.884172	16690.798035	28.820148
340.218197	16716.208337	28.825165
340.452027	16740.705744	28.830183
340.694727	16774.178001	28.835200
340.932277	16806.167761	28.840218
341.296244	16839.682424	28.845236
341.946767	16857.012932	28.850253
342.677338	16877.290340	28.855271
343.052963	16901.792058	28.860288
343.890380	16902.668529	28.865306
343.862852	16915.103719	28.870324
344.247990	16934.961155	28.875341
344.544030	16942.375028	28.880359
344.849397	16971.517410	28.885376
344.962065	16993.579807	28.890394
345.100594	17019.202219	28.895412
345.566297	17032.101576	28.900429
345.528830	17059.114715	28.905447
345.707795	17089.109773	28.910464
346.350277	17113.045824	28.915482
346.414679	17141.480970	28.920500
346.414317	17173.750259	28.925517
346.869652	17196.121517	28.930535
346.695430	17230.222646	28.935552
347.102076	17265.692014	28.940570
347.678515	17307.733184	28.945588
347.922967	17329.442372	28.950605
348.206859	17363.756911	28.955623
348.361828	17412.184506	28.960640
348.894323	17443.809633	28.965658
349.396538	17485.614881	28.970676
349.905344	17519.517557	28.975693
350.158955	17544.964973	28.980711
350.211031	17583.114396	28.985728
351.002728	17617.457510	28.990746
351.499491	17639.516414	28.995764
352.516461	17657.544844	29.000781
353.365355	17669.601788	29.005799
353.502515	17690.426475	29.010816
354.228218	17693.341693	29.015834
354.907583	17708.194552	29.020852
354.955456	17720.535436	29.025869
355.628068	17718.086895	29.030887
355.777966	17726.018046	29.035904
355.828119	17745.150315	29.040922
356.249500	17762.011815	29.045940
356.241714	17770.788241	29.050957
356.397125	17795.663240	29.055975
356.370601	17811.058110	29.060992
356.740324	17831.582984	29.066010
357.186192	17869.302960	29.071028
357.415494	17901.660414	29.076045
357.873105	17925.593055	29.081063
357.526093	17955.391298	29.086080
358.144987	17984.076532	29.091098
358.664077	18022.772813	29.096116
358.405393	18055.147979	29.101133
359.173923	18089.589054	29.106151
359.284298	18132.593481	29.111168
359.916253	18164.554502	29.116186
360.699615	18200.710166	29.121204
361.068461	18230.904906	29.126221
361.360281	18248.599469	29.131239
361.647006	18277.539209	29.136256
362.061497	18306.783458	29.141274
362.949716	18322.733070	29.146292
362.857966	18356.259503	29.151309
363.517149	18375.646000	29.156327
364.031471	18402.060641	29.161344
364.729518	18421.010117	29.166362
365.168181	18439.419146	29.171380
365.141093	18469.116168	29.176397
365.546762	18478.436983	29.181415
365.835666	18505.686611	29.186432
366.336162	18526.640837	29.191450
366.405619	18559.761658	29.196468
366.504065	18566.730825	29.201485
366.892218	18588.987755	29.206503
366.873183	18624.734762	29.211520
366.839627	18643.896590	29.216538
367.182564	18664.375046	29.221556
367.144132	18713.180091	29.226573
368.086325	18744.742189	29.231591
368.362059	18786.669905	29.236608
368.750049	18822.309734	29.241626
369.171372	18852.758321	29.246644
369.121373	18884.184856	29.251661
369.526946	18917.203051	29.256679
370.045218	18961.038382	29.261696
371.031790	19008.003658	29.266714
371.296866	19034.545573	29.271732
371.596851	19075.282620	29.276749
372.142738	19101.625155	29.281767
372.263530	19123.737835	29.286784
373.085478	19158.842038	29.291802
373.273338	19191.901237	29.296820
373.720590	19222.472184	29.301837
374.182472	19243.366124	29.306855
374.100357	19283.101742	29.311872
374.299739	19312.635299	29.316890
375.116057	19346.038028	29.321908
374.935752	19396.682564	29.326925
375.478088	19421.056907	29.331943
375.839206	19460.770587	29.336960
376.376327	19494.011757	29.341978
376.929819	19531.431631	29.346996
377.060656	19567.793517	29.352013
377.791430	19599.369804	29.357031
378.164424	19641.913665	29.362048
378.003225	19681.700036	29.367066
378.543189	19711.764040	29.372084
378.940299	19757.482748	29.377101
379.886709	19782.758055	29.382119
379.938842	19816.358907	29.387136
380.553708	19852.237959	29.392154
380.941894	19880.901324	29.397172
381.352702	19909.716959	29.402189
381.992127	19932.254258	29.407207
382.267190	19972.193595	29.412224
382.343425	20000.021335	29.417242
382.808932	20031.312773	29.422260
383.146841	20056.418421	29.427277
383.728881	20075.120021	29.432295
383.982444	20116.575501	29.437312
384.489249	20138.304846	29.442330
385.731059	20150.485465	29.447348
386.053794	20169.767712	29.452365
386.724767	20178.477944	29.457383
386.865586	20202.772436	29.462400
387.411525	20205.893941	29.467418
387.861368	20211.300898	29.472436
388.073329	20236.534043	29.477453
388.296945	20242.028661	29.482471
388.345065	20247.126049	29.487488
389.041729	20261.601363	29.492506
390.174942	20254.379459	29.497524
390.730599	20255.763273	29.502541
391.644948	20260.538766	29.507559
391.664287	20251.755954	29.512576
391.750387	20253.754768	29.517594
392.190678	20265.804784	29.522612
392.155161	20283.929706	29.527629
392.554715	20277.795365	29.532647
392.489902	20282.178914	29.537664
392.742143	20312.368986	29.542682
392.996548	20330.631910	29.547700
393.049320	20355.906706	29.552717
393.194992	20373.015178	29.557735
393.699382	20409.975531	29.562752
393.653102	20439.764450	29.567770
394.095682	20466.289232	29.572788
394.890438	20507.047430	29.577805
394.554629	20540.580598	29.582823
395.039585	20584.093145	29.587840
395.375882	20622.248033	29.592858
395.707133	20655.719142	29.597876
396.378406	20702.948162	29.602893
396.860394	20731.910683	29.607911
397.565347	20766.070112	29.612928
397.328023	20807.152551	29.617946
398.535925	20835.300191	29.622964
399.317668	20857.055878	29.627981
399.841847	20880.555566	29.632999
400.469069	20895.106401	29.638016
400.536659	20917.310961	29.643034
401.087101	20943.622477	29.648052
400.791990	20973.447090	29.653069
401.623623	20992.493261	29.658087
401.648069	21021.935209	29.663104
401.474928	21063.772041	29.668122
402.459152	21084.957190	29.673140
402.579769	21124.827947	29.678157
402.862272	21164.760934	29.683175
403.201652	21202.915021	29.688192
403.220595	21247.582980	29.693210
403.747354	21291.536431	29.698228
403.926331	21338.753820	29.703245
404.415927	21379.602680	29.708263
404.679482	21424.388447	29.713280
404.787886	21477.963721	29.718298
405.509302	21514.296372	29.723316
406.555921	21558.850527	29.728333
407.093426	21587.981606	29.733351
407.775961	21630.229832	29.738368
408.031898	21669.911520	29.743386
408.650883	21685.618746	29.748404
408.920114	21711.246379	29.753421
409.324134	21742.767551	29.758439
409.956949	21765.393579	29.763456
409.716455	21791.237994	29.768474
410.325374	21822.686353	29.773492
410.787326	21852.600373	29.778509
410.773970	21889.354633	29.783527
411.110559	21928.881177	29.788544
411.426610	21964.131519	29.793562
411.633907	22008.493224	29.798580
412.259747	22047.626699	29.803597
412.475932	22088.934121	29.808615
413.011192	22119.413210	29.813632
413.226675	22168.031702	29.818650
413.891650	22220.269702	29.823668
414.395334	22264.164960	29.828685
414.797022	22303.085119	29.833703
415.170146	22344.766814	29.838720
415.271580	22391.938901	29.843738
415.697107	22429.016505	29.848756
416.162958	22477.391115	29.853773
416.457004	22530.624053	29.858791
417.082141	22575.016547	29.863808
417.298393	22627.603933	29.868826
417.614076	22673.200925	29.873844
418.318445	22721.838135	29.878861
418.616370	22765.836175	29.883879
419.487028	22802.929772	29.888896
419.845352	22858.082979	29.893914
420.458527	22895.154667	29.898932
420.743169	22935.421024	29.903949
421.241868	22980.016018	29.908967
421.729077	23013.993333	29.913984
422.643781	23039.151199	29.919002
423.386122	23071.930516	29.924020
423.986211	23104.024604	29.929037
424.172419	23131.193594	29.934055
424.491855	23151.586872	29.939072
424.930278	23188.383195	29.944090
425.800303	23208.868279	29.949108
425.854036	23241.355894	29.954125
425.827407	23283.326012	29.959143
426.651924	23308.862455	29.964160
426.508825	23351.597072	29.969178
426.648480	23391.324755	29.974196
427.358789	23428.939235	29.979213
427.480700	23472.328958	29.984231
428.038177	23501.097149	29.989248
428.187200	23554.503205	29.994266
428.797622	23591.308766	29.999284
429.408021	23620.304651	30.004301
430.511696	23660.012842	30.009319
431.470969	23671.373888	30.014336
432.161859	23692.312912	30.019354
432.841449	23697.221108	30.024372
433.798575	23686.547324	30.029389
434.376810	23687.258881	30.034407
434.894190	23678.625526	30.039424
435.013910	23682.257587	30.044442
435.394900	23679.416626	30.049460
436.030252	23692.426066	30.054477
436.152067	23714.348970	30.059495
436.593319	23705.580399	30.064512
436.621725	23714.940371	30.069530
436.689010	23721.937496	30.074548
437.210840	23747.898664	30.079565
437.110312	23761.520010	30.084583
437.703085	23784.109843	30.089600
438.060891	23824.094485	30.094618
437.934067	23842.798698	30.099636
438.380049	23865.634589	30.104653
438.338284	23914.040311	30.109671
438.883216	23944.571462	30.114688
439.213191	23999.335757	30.119706
439.835055	24027.037123	30.124724
440.436866	24058.053947	30.129741
440.386163	24101.099478	30.134759
440.805201	24150.833702	30.139776
441.401798	24194.882002	30.144794
441.574444	24225.493220	30.149812
442.306794	24272.098666	30.154829
442.905902	24333.495562	30.159847
442.829173	24367.758302	30.164864
443.265084	24419.329376	30.169882
443.216448	24466.611728	30.174900
443.790685	24528.534044	30.179917
444.503142	24586.874778	30.184935
444.742601	24624.865920	30.189952
444.585767	24673.495366	30.194970
445.410056	24733.318913	30.199988
446.014449	24787.366796	30.205005
446.451388	24854.695210	30.210023
447.082375	24899.051699	30.215040
447.506892	24949.963881	30.220058
447.759370	25004.277786	30.225076
448.079863	25065.270787	30.230093
448.404974	25130.001243	30.235111
449.108291	25178.033615	30.240128
449.992240	25232.400900	30.245146
450.279870	25281.839139	30.250164
450.984765	25324.770845	30.255181
451.562714	25376.787297	30.260199
452.756351	25415.619793	30.265216
453.376249	25460.796642	30.270234
453.232027	25506.486249	30.275252
454.075943	25531.193033	30.280269
454.001377	25571.624890	30.285287
454.801891	25608.433728	30.290304
455.037429	25655.273149	30.295322
455.255968	25697.112473	30.300340
455.958627	25722.960453	30.305357
455.988992	25768.926825	30.310375
456.426775	25809.549039	30.315392
456.944013	25850.735022	30.320410
457.189400	25890.027611	30.325428
458.321095	25934.663728	30.330445
458.436344	25980.180776	30.335463
458.966073	26016.708805	30.340480
459.388328	26065.331240	30.345498
459.433121	26100.172798	30.350516
459.945711	26132.877436	30.355533
460.481342	26205.008158	30.360551
460.884379	26247.990722	30.365568
461.589596	26291.145592	30.370586
461.784407	26332.744447	30.375604
462.461787	26379.633134	30.380621
462.932861	26420.626479	30.385639
463.509918	26462.847865	30.390656
463.923032	26509.318446	30.395674
464.434979	26557.277016	30.400692
464.779814	26599.226209	30.405709
465.137647	26649.356654	30.410727
466.130183	26696.655936	30.415744
466.384260	26742.990347	30.420762
466.469305	26792.306701	30.425780
467.002599	26833.407081	30.430797
468.074481	26883.863816	30.435815
468.694722	26923.965219	30.440832
469.109158	26968.133805	30.445850
469.610370	27015.240525	30.450868
470.204598	27042.856812	30.455885
469.909285	27090.917324	30.460903
470.352497	27139.072250	30.465920
470.689107	27174.758761	30.470938
470.813401	27220.845363	30.475956
471.423081	27265.429230	30.480973
472.390953	27325.644076	30.485991
472.809483	27370.033816	30.491008
473.282778	27417.480820	30.496026
473.938970	27474.118330	30.501044
474.500416	27505.126155	30.506061
474.871163	27561.440585	30.511079
475.405977	27602.523585	30.516096
476.055186	27647.003849	30.521114
476.882067	27686.484780	30.526132
477.888212	27705.743556	30.531149
478.656877	27733.788509	30.536167
479.114498	27757.586633	30.541184
479.806024	27786.998357	30.546202
479.864193	27818.730278	30.551220
480.354974	27845.002626	30.556237
480.502555	27876.328116	30.561255
480.650180	27916.560110	30.566272
481.592629	27949.686670	30.571290
481.543301	27989.359446	30.576308
481.986626	28012.879575	30.581325
482.524904	28048.751004	30.586343
482.671424	28082.487453	30.591360
482.962517	28113.476430	30.596378
483.482519	28152.689190	30.601396
484.038846	28192.624622	30.606413
484.364824	28243.503366	30.611431
484.576862	28274.749111	30.616448
485.423108	28314.597280	30.621466
485.839676	28354.481308	30.626484
486.145829	28389.579210	30.631501
486.840736	28441.953903	30.636519
487.681085	28479.699036	30.641536
488.599093	28510.341502	30.646554
488.396641	28555.455893	30.651572
489.244985	28592.155568	30.656589
489.357384	28630.975446	30.661607
489.474767	28678.906478	30.666624
490.325601	28722.897434	30.671642
490.422782	28768.112470	30.676660
490.961637	28820.937817	30.681677
491.553063	28875.350813	30.686695
491.972600	28931.270039	30.691712
492.292032	28977.510810	30.696730
492.453580	29027.590191	30.701748
493.317410	29083.320180	30.706765
493.461367	29130.891353	30.711783
493.696914	29198.643329	30.716800
494.587552	29245.171855	30.721818
494.981772	29313.824713	30.726836
495.475307	29372.689091	30.731853
495.889921	29436.404162	30.736871
496.415256	29487.791883	30.741888
497.046730	29550.940126	30.746906
497.349595	29612.043497	30.751924
497.811277	29672.873753	30.756941
498.547328	29727.242507	30.761959
498.932469	29788.998156	30.766976
499.937530	29828.850940	30.771994
500.393060	29883.792025	30.777012
501.365364	29928.743326	30.782029
501.952398	29988.748582	30.787047
502.602558	30030.830351	30.792064
503.084386	30067.889354	30.797082
503.492049	30118.772129	30.802100
504.082808	30164.653977	30.807117
504.851177	30199.423848	30.812135
505.093510	30246.826550	30.817152
505.573960	30283.902018	30.822170
506.086871	30336.054780	30.827188
506.703283	30374.971979	30.832205
507.268210	30413.538370	30.837223
507.582491	30455.454669	30.842240
508.374713	30486.639621	30.847258
508.531038	30538.251394	30.852276
509.033994	30574.253923	30.857293
509.953617	30617.537312	30.862311
510.037494	30664.182574	30.867328
510.365715	30688.991336	30.872346
510.530725	30737.863264	30.877364
511.045097	30779.174902	30.882381
511.370419	30831.294998	30.887399
511.767921	30871.165888	30.892416
512.065985	30914.430287	30.897434
512.602539	30972.459559	30.902452
513.257847	31016.581244	30.907469
513.943433	31075.566681	30.912487
514.249696	31141.991800	30.917504
514.561247	31188.706712	30.922522
515.218332	31255.469739	30.927540
515.505178	31310.453610	30.932557
516.092909	31377.336266	30.937575
516.708760	31428.859258	30.942592
517.493313	31486.797223	30.947610
517.827056	31545.891840	30.952628
518.083905	31598.256272	30.957645
519.259472	31641.488834	30.962663
520.042798	31697.458584	30.967680
521.117971	31740.897929	30.972698
521.411959	31793.250259	30.977716
521.876342	31828.943217	30.982733
522.494287	31873.963327	30.987751
522.342393	31929.762710	30.992768
523.063077	31979.060356	30.997786
523.451392	32037.544514	31.002804
524.229270	32086.573890	31.007821
525.127510	32127.289567	31.012839
525.330633	32173.893098	31.017856
526.361464	32214.854491	31.022874
526.535782	32265.679248	31.027892
527.110261	32310.875161	31.032909
527.795173	32348.535268	31.037927
527.886128	32392.488824	31.042944
528.586394	32449.361932	31.047962
528.979920	32497.407423	31.052980
529.340122	32548.185352	31.057997
529.760055	32604.302261	31.063015
529.728713	32668.960542	31.068032
530.457404	32735.186656	31.073050
530.644855	32803.784263	31.078068
530.852411	32864.517486	31.083085
531.457014	32927.240497	31.088103
532.028850	33013.010310	31.093120
532.296779	33075.870425	31.098138
532.678068	33156.895576	31.103156
533.187932	33232.874859	31.108173
534.134209	33297.367886	31.113191
535.492295	33354.970624	31.118208
537.064104	33392.007570	31.123226
537.853168	33425.312688	31.128244
538.757467	33462.732411	31.133261
538.958857	33488.589321	31.138279
539.487364	33531.063135	31.143296
539.897649	33559.368093	31.148314
540.294893	33595.732517	31.153332
540.407361	33639.319343	31.158349
540.939353	33675.237939	31.163367
541.261506	33726.006780	31.168384
541.570344	33777.879490	31.173402
542.251905	33833.052792	31.178420
542.033330	33880.392612	31.183437
542.346837	33933.688334	31.188455
542.799946	34000.499699	31.193472
543.397297	34058.253980	31.198490
543.509282	34130.947190	31.203508
544.510168	34192.612552	31.208525
545.907109	34242.204524	31.213543
546.353714	34299.092234	31.218560
546.970929	34358.106508	31.223578
547.397606	34424.033949	31.228596
548.059785	34475.835497	31.233613
548.511736	34524.873727	31.238631
548.465278	34605.704096	31.243648
549.150941	34658.556297	31.248666
549.531258	34719.641749	31.253684
549.799163	34792.285651	31.258701
550.530543	34860.510669	31.263719
550.756393	34940.134393	31.268736
551.258801	35018.445437	31.273754
551.907165	35097.454587	31.278772
552.005391	35173.534661	31.283789
553.076993	35242.425603	31.288807
554.333041	35302.435029	31.293824
555.513959	35355.510564	31.298842
556.838288	35406.585849	31.303860
557.543346	35452.868819	31.308877
558.234721	35492.235641	31.313895
558.834844	35535.219531	31.318912
559.540300	35573.056464	31.323930
560.229401	35606.584746	31.328948
560.106226	35644.399678	31.333965
560.879765	35686.489380	31.338983
561.771556	35733.116674	31.344000
562.601125	35747.872492	31.349018
563.162315	35775.650052	31.354036
563.769291	35816.212515	31.359053
564.162947	35840.793084	31.364071
564.542014	35885.876784	31.369088
565.015051	35915.942248	31.374106
565.502199	35944.427155	31.379124
565.450843	35989.398633	31.384141
566.242005	36031.034752	31.389159
566.956036	36077.248338	31.394176
567.060539	36121.476934	31.399194
567.145922	36157.644272	31.404212
567.208545	36218.678727	31.409229
567.708680	36269.976575	31.414247
568.153628	36325.463154	31.419264
568.186365	36392.986649	31.424282
568.838656	36458.939638	31.429300
569.264696	36546.446200	31.434317
570.073401	36602.089092	31.439335
570.601694	36662.117232	31.444352
571.536232	36715.475698	31.449370
573.024072	36766.441572	31.454388
573.523503	36818.435517	31.459405
574.070485	36859.300984	31.464423
574.924515	36927.664261	31.469440
575.390366	36977.322255	31.474458
576.033379	37020.504324	31.479476
576.313125	37073.038528	31.484493
577.235275	37122.533507	31.489511
577.535840	37178.315725	31.494528
577.996076	37228.316274	31.499546
578.823324	37276.208594	31.504564
578.959159	37335.261351	31.509581
579.524353	37397.779313	31.514599
579.841797	37449.316955	31.519616
580.266909	37517.276117	31.524634
581.085063	37577.282850	31.529652
581.386411	37651.930582	31.534669
581.769064	37718.177376	31.539687
582.493982	37792.970919	31.544704
582.797594	37860.825902	31.549722
583.565241	37928.440636	31.554740
583.948368	38025.962108	31.559757
584.636388	38088.701291	31.564775
585.164694	38161.130891	31.569792
585.500631	38240.939547	31.574810
585.988177	38308.114369	31.579828
586.477037	38397.670911	31.584845
587.466739	38470.278375	31.589863
588.000838	38546.209403	31.594880
588.982237	38614.175168	31.599898
590.371641	38671.117017	31.604916
591.146792	38728.622030	31.609933
591.994270	38790.619679	31.614951
592.857112	38846.099110	31.619968
592.803025	38896.725831	31.624986
593.776338	38939.631687	31.630004
593.889354	39002.017908	31.635021
594.426059	39064.975757	31.640039
594.726916	39121.890836	31.645056
595.145102	39187.101353	31.650074
596.266819	39241.423222	31.655092
596.730022	39311.863837	31.660109
597.268261	39383.014811	31.665127
597.931879	39422.770530	31.670144
598.390722	39486.036753	31.675162
599.047499	39543.700337	31.680180
599.719847	39607.037731	31.685197
600.100967	39653.071122	31.690215
600.855290	39726.652023	31.695232
600.948215	39786.941750	31.700250
601.688988	39834.161001	31.705268
602.028476	39897.584831	31.710285
602.792580	39965.580174	31.715303
603.298778	40025.102155	31.720320
603.902154	40099.973232	31.725338
604.705075	40156.549746	31.730356
604.708289	40233.475274	31.735373
605.261916	40304.361950	31.740391
605.662563	40373.421867	31.745408
606.175021	40460.834340	31.750426
607.157234	40530.543445	31.755444
607.737968	40604.148095	31.760461
608.289860	40675.996266	31.765479
608.981401	40750.400221	31.770496
609.624997	40832.112167	31.775514
610.174139	40910.623438	31.780532
610.717026	40992.441743	31.785549
611.208865	41068.308256	31.790567
611.695983	41148.365580	31.795584
611.841740	41237.574705	31.800602
612.786339	41319.350876	31.805620
613.337090	41412.520161	31.810637
613.779301	41501.458742	31.815655
614.651440	41585.445993	31.820672
615.199191	41670.824761	31.825690
616.004395	41763.958515	31.830708
616.494397	41850.251003	31.835725
617.524809	41930.013362	31.840743
619.227195	41992.816142	31.845760
620.216038	42050.758973	31.850778
621.284428	42107.090697	31.855796
622.114531	42172.487379	31.860813
622.413962	42224.192937	31.865831
623.267455	42275.086969	31.870848
623.716786	42334.439773	31.875866
624.753386	42377.955287	31.880884
625.056570	42429.114524	31.885901
625.541214	42482.759333	31.890919
626.280175	42526.724030	31.895936
626.085406	42587.400466	31.900954
626.780663	42650.842161	31.905972
627.520581	42717.500259	31.910989
627.856570	42778.297932	31.916007
628.595614	42844.925056	31.921024
628.699995	42917.717361	31.926042
629.499141	42983.251633	31.931060
629.670373	43059.313754	31.936077
630.387668	43144.875424	31.941095
630.681137	43211.652810	31.946112
631.314256	43298.713680	31.951130
631.932276	43371.530254	31.956148
632.433980	43439.371629	31.961165
632.738914	43521.740645	31.966183
633.514723	43602.298938	31.971200
633.613866	43697.868351	31.976218
634.338622	43776.724663	31.981236
634.886446	43864.746911	31.986253
635.136620	43958.488705	31.991271
636.103964	44039.293927	31.996288
637.098892	44130.114365	32.001306
637.881056	44217.836013	32.006324
638.901950	44283.605223	32.011341
639.862877	44367.671792	32.016359
640.699852	44445.820109	32.021376
641.309790	44522.760301	32.026394
642.296043	44590.289110	32.031412
642.941425	44654.352393	32.036429
643.743442	44725.510046	32.041447
644.355766	44781.934228	32.046464
645.104719	44865.341431	32.051482
645.829228	44921.317335	32.056500
646.763995	44977.964754	32.061517
647.730699	45041.001657	32.066535
648.583991	45093.848614	32.071552
649.025399	45154.414809	32.076570
649.759333	45197.420264	32.081588
650.357229	45256.573636	32.086605
651.049393	45300.887560	32.091623
651.871767	45336.450651	32.096640
652.508980	45394.426111	32.101658
653.254961	45453.204190	32.106676
653.937177	45504.429971	32.111693
653.971203	45572.706486	32.116711
654.688842	45623.755987	32.121728
654.927183	45687.766169	32.126746
655.627314	45750.753197	32.131764
656.046424	45821.396317	32.136781
656.655184	45892.193533	32.141799
657.511079	45949.908996	32.146816
657.837412	46034.581161	32.151834
658.059239	46102.770550	32.156852
658.677329	46179.652884	32.161869
659.130144	46271.258583	32.166887
660.153449	46346.328882	32.171904
660.441996	46433.488422	32.176922
661.032510	46518.003773	32.181940
662.270734	46578.627469	32.186957
663.012132	46663.108137	32.191975
663.812593	46735.574739	32.196992
664.101016	46819.164131	32.202010
664.747253	46894.819127	32.207028
665.313537	46979.580690	32.212045
665.677660	47070.782201	32.217063
666.460524	47146.114747	32.222080
666.905932	47237.590526	32.227098
667.068812	47312.107719	32.232116
667.922724	47400.343360	32.237133
668.072429	47493.541760	32.242151
668.864063	47581.829961	32.247168
669.757670	47678.669711	32.252186
670.003855	47769.171472	32.257204
671.260159	47864.585605	32.262221
671.571179	47966.813747	32.267239
672.371932	48055.348912	32.272256
672.835489	48158.092023	32.277274
673.204226	48256.449047	32.282292
673.988523	48355.894536	32.287309
674.576540	48453.257980	32.292327
675.734931	48556.803292	32.297344
676.143787	48649.485939	32.302362
676.772587	48735.037296	32.307380
678.540531	48822.333223	32.312397
679.715013	48900.659846	32.317415
680.929733	48982.599610	32.322432
681.686647	49045.552968	32.327450
682.317169	49113.209211	32.332468
683.132954	49181.699408	32.337485
683.403595	49265.501430	32.342503
684.124997	49323.805980	32.347520
684.573561	49406.251508	32.352538
684.969520	49487.872513	32.357556
685.996300	49571.009346	32.362573
686.475613	49656.603013	32.367591
687.356817	49736.537327	32.372608
687.450944	49831.926519	32.377626
687.778947	49913.131365	32.382644
688.433531	50010.863950	32.387661
688.745533	50113.027423	32.392679
689.312546	50201.716672	32.397696
689.899587	50309.873617	32.402714
690.984921	50414.313179	32.407732
691.649535	50503.126064	32.412749
692.419208	50611.878840	32.417767
693.244707	50696.615422	32.422784
694.404316	50789.861962	32.427802
695.354447	50876.605962	32.432820
696.711620	50962.680428	32.437837
697.178061	51044.327459	32.442855
698.216283	51113.778240	32.447872
699.068722	51190.469759	32.452890
699.943811	51274.322169	32.457908
700.830982	51339.554017	32.462925
701.221755	51411.132178	32.467943
701.957910	51468.385522	32.472960
702.790622	51538.416360	32.477978
703.395257	51613.901032	32.482996
704.219824	51680.079800	32.488013
704.914657	51763.624010	32.493031
705.201283	51821.347111	32.498048
705.766986	51892.701200	32.503066
705.868352	51973.618560	32.508084
707.113351	52045.122194	32.513101
707.299555	52115.663884	32.518119
708.142142	52182.649980	32.523136
709.050930	52254.906971	32.528154
709.504794	52331.923958	32.533172
710.347981	52402.992270	32.538189
710.666739	52489.219735	32.543207
711.355255	52565.691975	32.548224
712.086112	52633.772856	32.553242
712.962988	52727.702553	32.558260
713.602550	52798.781901	32.563277
714.249413	52888.726968	32.568295
714.946807	52971.909396	32.573312
715.899047	53056.609173	32.578330
716.073320	53131.528902	32.583348
716.984031	53227.015838	32.588365
717.661052	53323.516321	32.593383
718.202260	53409.589640	32.598400
718.985602	53500.322883	32.603418
719.333642	53590.992101	32.608436
720.305775	53680.088897	32.613453
720.865043	53785.988675	32.618471
721.465239	53883.389658	32.623488
721.994812	53977.725989	32.628506
722.820781	54089.104274	32.633524
723.686631	54181.943288	32.638541
723.946780	54289.065964	32.643559
724.732494	54393.097720	32.648576
726.001613	54486.045999	32.653594
726.778298	54591.900183	32.658612
728.783404	54662.638546	32.663629
730.305539	54732.916465	32.668647
731.559056	54790.918598	32.673664
732.402653	54863.550140	32.678682
733.195624	54911.881272	32.683700
734.296826	54953.979689	32.688717
735.311252	55020.617359	32.693735
735.390559	55070.410771	32.698752
736.232805	55133.647050	32.703770
736.390641	55201.417839	32.708788
737.275426	55262.871565	32.713805
737.929429	55331.398248	32.718823
738.203908	55386.441839	32.723840
738.473537	55457.019020	32.728858
739.035980	55538.472242	32.733876
739.674423	55610.446528	32.738893
740.183388	55695.024941	32.743911
740.708932	55779.600871	32.748928
741.474393	55865.102918	32.753946
742.111834	55968.138224	32.758964
742.104814	56058.070591	32.763981
742.759616	56161.445161	32.768999
743.283641	56271.364350	32.774016
744.378650	56364.275359	32.779034
744.663240	56462.109502	32.784052
745.502682	56559.198159	32.789069
745.929325	56656.844605	32.794087
746.347575	56768.895370	32.799104
747.541116	56870.057901	32.804122
748.344745	56981.873203	32.809140
748.537811	57091.373261	32.814157
749.323650	57192.038470	32.819175
749.844853	57304.504315	32.824192
750.555818	57416.559089	32.829210
751.064301	57541.965112	32.834228
752.426239	57661.582045	32.839245
753.202881	57771.478768	32.844263
753.755851	57883.657990	32.849280
754.528646	57991.932335	32.854298
754.974555	58123.179714	32.859316
755.982714	58241.805227	32.864333
757.306584	58353.286183	32.869351
757.809205	58454.069377	32.874368
759.411783	58563.614023	32.879386
759.760281	58675.807363	32.884404
761.068882	58775.322768	32.889421
762.041443	58884.711614	32.894439
762.054957	59001.558971	32.899456
763.230241	59098.949888	32.904474
763.873335	59201.830035	32.909492
765.053807	59311.362526	32.914509
766.108066	59399.320276	32.919527
766.755732	59506.606521	32.924544
767.474473	59606.037409	32.929562
768.288791	59707.196875	32.934580
769.218604	59807.433217	32.939597
769.969510	59907.580605	32.944615
770.371185	60013.717051	32.949632
771.436070	60109.785404	32.954650
771.935155	60217.524307	32.959668
772.631453	60326.361404	32.964685
773.182453	60435.217644	32.969703
773.903062	60548.558453	32.974720
774.559118	60644.870003	32.979738
775.265202	60757.917374	32.984756
776.085461	60871.887623	32.989773
776.914503	60988.606600	32.994791
777.483271	61103.954926	32.999808
779.079795	61200.183829	33.004826
779.825059	61312.405803	33.009844
780.831304	61419.653257	33.014861
781.975332	61511.245613	33.019879
782.430058	61622.526629	33.024896
783.181648	61719.572726	33.029914
783.803985	61829.713623	33.034932
784.642209	61932.024067	33.039949
785.069819	62029.828769	33.044967
785.618164	62148.397613	33.049984
786.434394	62251.863876	33.055002
787.092125	62348.208366	33.060020
788.254562	62449.941160	33.065037
789.252013	62545.716346	33.070055
790.500628	62646.600918	33.075072
791.160007	62734.134842	33.080090
791.905756	62834.556497	33.085108
792.362803	62921.582218	33.090125
792.985576	63004.395056	33.095143
793.484573	63112.300771	33.100160
794.755057	63216.300899	33.105178
795.583750	63317.652595	33.110196
795.701223	63421.648953	33.115213
796.636347	63528.135601	33.120231
797.077604	63632.526388	33.125248
797.499411	63748.730083	33.130266
798.040253	63885.403004	33.135284
798.808348	64006.840170	33.140301
800.015750	64120.281478	33.145319
800.625057	64251.799053	33.150336
801.422362	64376.356386	33.155354
802.527603	64493.155205	33.160372
803.364185	64616.651464	33.165389
804.509003	64746.228056	33.170407
805.228645	64869.290642	33.175424
806.153734	64981.438356	33.180442
806.952762	65093.317441	33.185460
807.732117	65210.125487	33.190477
808.476781	65331.340403	33.195495
809.368135	65442.857806	33.200512
810.421138	65563.357403	33.205530
811.888550	65678.235685	33.210548
812.143185	65787.158004	33.215565
812.765295	65893.495299	33.220583
813.583254	66019.607802	33.225600
814.243950	66141.341221	33.230618
815.328708	66258.570618	33.235636
815.962284	66375.972783	33.240653
816.785612	66495.100776	33.245671
817.454504	66619.048441	33.250688
818.100612	66739.953207	33.255706
819.167018	66863.435882	33.260724
819.853697	66988.546031	33.265741
820.796829	67111.943778	33.270759
821.070058	67243.215072	33.275776
822.017456	67374.529770	33.280794
822.814365	67503.234409	33.285812
823.160513	67646.610352	33.290829
824.401039	67774.696871	33.295847
824.538058	67913.911975	33.300864
825.742244	68052.761829	33.305882
827.053711	68184.739978	33.310900
827.536374	68316.772377	33.315917
828.508650	68452.844432	33.320935
829.537311	68600.232564	33.325952
830.349478	68715.833867	33.330970
831.333693	68841.390786	33.335988
832.224617	68956.334919	33.341005
833.338048	69062.667093	33.346023
834.282845	69178.292430	33.351040
834.883897	69292.434352	33.356058
835.749133	69404.021220	33.361076
836.750663	69516.401051	33.366093
837.966382	69637.281527	33.371111
838.497039	69742.414232	33.376128
839.475398	69848.824012	33.381146
840.368601	69971.304552	33.386164
840.715529	70091.653428	33.391181
841.310585	70199.022218	33.396199
842.438617	70325.321987	33.401216
842.487808	70450.080891	33.406234
843.609106	70589.568384	33.411252
844.168562	70717.656277	33.416269
845.496369	70852.171177	33.421287
845.958608	70986.101589	33.426304
846.891240	71122.526105	33.431322
847.605321	71258.103550	33.436340
847.862683	71401.140207	33.441357
849.058178	71540.753899	33.446375
849.578323	71680.022498	33.451392
850.430904	71839.175104	33.456410
851.068750	71982.858707	33.461428
852.305308	72128.300035	33.466445
853.340108	72271.854306	33.471463
853.824747	72432.908291	33.476480
854.650348	72578.941595	33.481498
856.282087	72708.356386	33.486516
856.940488	72863.008764	33.491533
857.876154	73005.781612	33.496551
859.138365	73138.133549	33.501568
860.311672	73275.769876	33.506586
861.676801	73402.609727	33.511604
862.848347	73517.087167	33.516621
864.384863	73624.210345	33.521639
865.419791	73733.488132	33.526656
866.419802	73856.895575	33.531674
867.788119	73957.705473	33.536692
868.226048	74066.511605	33.541709
868.825975	74170.686051	33.546727
869.574193	74278.630503	33.551744
870.069701	74396.966284	33.556762
870.575173	74511.689458	33.561780
871.231941	74645.627839	33.566797
871.986797	74765.135557	33.571815
872.473612	74905.809112	33.576832
872.921617	75038.318207	33.581850
873.650910	75180.349809	33.586868
874.048086	75336.879532	33.591885
874.788535	75481.049043	33.596903
875.358670	75633.054005	33.601920
875.977583	75794.912768	33.606938
877.131989	75940.184525	33.611956
878.098429	76085.508395	33.616973
879.154386	76238.794222	33.621991
879.936871	76380.185478	33.627008
880.353443	76524.701834	33.632026
881.205126	76668.303303	33.637044
882.180754	76832.752544	33.642061
882.963632	76986.583647	33.647079
884.013639	77144.279314	33.652096
885.025901	77287.060199	33.657114
886.198888	77435.204001	33.662132
886.760242	77595.364998	33.667149
888.095675	77743.223645	33.672167
889.383100	77890.275444	33.677184
890.002278	78036.487436	33.682202
891.140581	78183.111214	33.687220
892.116636	78342.757339	33.692237
892.664811	78486.782949	33.697255
894.005552	78624.107258	33.702272
894.428038	78774.507608	33.707290
895.442389	78920.094592	33.712308
896.038127	79088.851188	33.717325
897.209102	79239.531298	33.722343
898.214830	79386.084331	33.727360
898.946287	79541.738266	33.732378
900.122940	79689.149660	33.737396
900.810395	79855.428933	33.742413
901.874176	80005.860427	33.747431
902.997823	80151.936348	33.752448
903.566340	80308.819120	33.757466
905.154692	80453.912683	33.762484
905.972928	80615.721159	33.767501
906.982431	80753.431348	33.772519
907.679734	80911.586824	33.777536
908.486821	81063.884987	33.782554
909.992946	81200.633383	33.787572
910.295464	81355.936544	33.792589
911.112049	81508.805436	33.797607
912.338327	81658.359466	33.802624
913.173715	81812.315378	33.807642
914.018876	81955.647605	33.812660
914.921360	82110.448155	33.817677
915.603413	82263.977784	33.822695
916.962987	82416.126971	33.827712
917.752180	82568.064810	33.832730
919.364995	82712.782442	33.837748
920.217411	82856.903571	33.842765
921.095011	83004.241868	33.847783
922.352348	83142.202241	33.852800
922.941209	83286.776117	33.857818
924.058460	83424.066140	33.862836
924.532843	83574.058673	33.867853
925.642833	83719.716557	33.872871
926.063508	83864.499980	33.877888
926.507813	84026.579802	33.882906
927.393798	84167.374974	33.887924
928.438708	84330.701818	33.892941
929.251229	84472.935126	33.897959
930.190896	84620.380547	33.902976
930.911338	84773.534113	33.907994
932.405390	84915.893839	33.913012
933.135988	85066.529108	33.918029
934.170149	85218.809223	33.923047
934.964811	85366.701792	33.928064
935.490983	85518.937955	33.933082
936.583260	85684.809921	33.938100
937.583774	85839.105777	33.943117
938.067079	85998.547359	33.948135
939.010592	86161.619486	33.953152
939.552260	86340.449112	33.958170
940.409746	86504.221768	33.963188
941.320909	86690.787128	33.968205
942.084309	86860.558571	33.973223
942.632819	87039.164455	33.978240
943.828719	87230.558121	33.983258
944.538256	87411.828795	33.988276
945.804194	87603.896932	33.993293
947.102586	87776.374142	33.998311
948.177730	87954.921992	34.003328
949.185637	88147.544967	34.008346
950.598093	88310.412238	34.013364
951.524189	88488.831367	34.018381
952.679791	88651.251293	34.023399
953.976592	88806.464905	34.028416
955.286289	88976.942562	34.033434
956.796890	89142.355525	34.038452
957.935779	89294.605743	34.043469
959.076685	89445.179391	34.048487
960.319214	89588.901210	34.053504
961.038594	89725.897058	34.058522
962.167589	89872.215935	34.063540
963.575064	90009.506941	34.068557
964.035902	90161.150874	34.073575
964.873541	90294.591665	34.078592
965.895929	90445.843733	34.083610
967.183722	90592.779013	34.088628
968.021713	90728.323450	34.093645
969.213810	90869.624691	34.098663
970.883389	90999.540662	34.103680
971.956476	91121.122333	34.108698
973.042419	91252.443462	34.113716
973.704089	91379.546549	34.118733
974.217781	91512.226641	34.123751
975.098514	91647.673915	34.128768
976.204494	91794.229807	34.133786
977.049529	91930.267080	34.138804
977.703019	92078.269359	34.143821
978.222764	92218.073124	34.148839
979.781552	92359.389794	34.153856
980.529843	92507.606292	34.158874
981.501965	92643.454839	34.163892
982.103599	92780.823449	34.168909
982.845826	92924.144172	34.173927
983.570100	93055.017815	34.178944
984.068135	93215.213344	34.183962
984.624843	93367.512660	34.188980
985.796671	93532.329704	34.193997
986.298524	93697.522109	34.199015
987.251742	93856.928530	34.204032
988.102776	94037.331696	34.209050
988.911236	94206.349046	34.214068
990.247069	94377.746039	34.219085
990.782836	94559.643945	34.224103
992.367472	94723.227076	34.229120
993.538649	94900.334187	34.234138
994.542909	95065.607877	34.239156
996.935958	95209.171833	34.244173
998.334381	95361.263224	34.249191
999.373947	95502.262548	34.254208
1000.140850	95664.383902	34.259226
1001.292513	95807.378873	34.264244
1002.157629	95957.488752	34.269261
1002.759250	96114.538789	34.274279
1003.938372	96260.481741	34.279296
1004.868663	96421.003629	34.284314
1005.930640	96580.636663	34.289332
1007.002347	96731.766688	34.294349
1007.942818	96896.905054	34.299367
1009.110883	97033.864482	34.304384
1010.074430	97197.854957	34.309402
1011.072455	97348.634081	34.314420
1012.368441	97498.521046	34.319437
1013.627918	97648.927966	34.324455
1014.893394	97787.729790	34.329472
1015.751057	97941.176542	34.334490
1017.245212	98086.113720	34.339508
1018.249197	98232.395574	34.344525
1018.700580	98379.197088	34.349543
1019.881530	98524.525944	34.354560
1020.161979	98686.673933	34.359578
1021.168172	98844.792203	34.364596
1022.189001	99002.041536	34.369613
1022.915724	99158.595081	34.374631
1024.718189	99319.802641	34.379648
1025.306604	99472.975434	34.384666
1026.430291	99638.030499	34.389684
1027.783883	99781.412104	34.394701
1028.868063	99945.627467	34.399719
1030.189798	100093.784002	34.404736
1031.152982	100249.005679	34.409754
1032.629546	100379.908703	34.414772
1033.447922	100530.901921	34.419789
1034.025941	100678.942217	34.424807
1035.112047	100834.279319	34.429824
1035.746471	100991.879204	34.434842
1036.925578	101139.116350	34.439860
1038.039128	101286.865781	34.444877
1037.971842	101445.304080	34.449895
1038.922246	101590.385725	34.454912
1040.025857	101747.751535	34.459930
1040.851771	101916.285076	34.464948
1041.781491	102075.493625	34.469965
1042.301008	102255.353089	34.474983
1043.134860	102419.797894	34.480000
1044.222739	102602.133306	34.485018
1045.106766	102790.090020	34.490036
1046.362019	102963.749293	34.495053
1047.263284	103150.971073	34.500071
1048.452547	103343.489479	34.505088
1049.254754	103531.136194	34.510106
1050.204876	103725.230800	34.515124
1051.438574	103911.235845	34.520141
1052.044395	104126.112670	34.525159
1052.847046	104318.223076	34.530176
1054.271054	104523.970565	34.535194
1054.895109	104736.886042	34.540212
1056.299379	104929.037159	34.545229
1057.061184	105141.349651	34.550247
1058.179008	105351.829637	34.555264
1059.212019	105557.094736	34.560282
1060.289323	105771.714079	34.565300
1061.483696	105984.389826	34.570317
1062.513896	106199.818624	34.575335
1064.411125	106399.242334	34.580352
1066.178165	106579.208738	34.585370
1067.958446	106763.341381	34.590388
1070.457227	106904.728952	34.595405
1071.900971	107074.152033	34.600423
1073.211920	107225.789391	34.605440
1074.763488	107372.864326	34.610458
1075.697531	107521.705165	34.615476
1076.831280	107653.234835	34.620493
1077.867080	107810.369383	34.625511
1078.608933	107939.560798	34.630528
1080.226467	108072.517048	34.635546
1081.486989	108221.749167	34.640564
1082.355325	108346.385974	34.645581
1083.494691	108487.127852	34.650599
1084.477719	108625.832430	34.655616
1085.703332	108758.821131	34.660634
1086.684507	108885.480544	34.665652
1087.834701	109033.241210	34.670669
1088.531511	109180.016215	34.675687
1089.422116	109324.123926	34.680704
1090.283572	109461.384084	34.685722
1090.974062	109610.556688	34.690740
1092.030230	109756.196464	34.695757
1093.097661	109915.377212	34.700775
1093.923397	110077.361912	34.705792
1094.680222	110231.631764	34.710810
1095.410263	110374.746331	34.715828
1096.563898	110524.249950	34.720845
1097.654881	110695.922121	34.725863
1098.818668	110844.222229	34.730880
1099.662016	111003.092878	34.735898
1099.831701	111175.217131	34.740916
1101.012012	111345.750511	34.745933
1101.729315	111527.272025	34.750951
1102.350151	111710.496192	34.755968
1103.654369	111904.170448	34.760986
1104.383309	112090.596505	34.766004
1105.465122	112287.428071	34.771021
1106.134213	112497.925746	34.776039
1107.040889	112702.683128	34.781056
1108.375282	112909.687264	34.786074
1108.993996	113125.646094	34.791092
1109.745065	113341.153146	34.796109
1111.013312	113569.445693	34.801127
1111.698758	113798.308648	34.806144
1112.569283	114034.857727	34.811162
1113.384839	114285.621264	34.816180
1114.857835	114516.572406	34.821197
1115.944142	114749.340116	34.826215
1117.198068	114997.526148	34.831232
1118.425620	115237.635109	34.836250
1120.339736	115468.455059	34.841268
1122.183771	115683.932057	34.846285
1123.905874	115890.042542	34.851303
1125.189071	116096.875861	34.856320
1127.047286	116295.781596	34.861338
1128.351698	116500.751556	34.866356
1130.897240	116656.942264	34.871373
1133.264806	116808.590015	34.876391
1135.770361	116952.890990	34.881408
1137.492382	117078.877503	34.886426
1138.568420	117221.447855	34.891444
1139.679592	117346.868538	34.896461
1140.513800	117474.339265	34.901479
1141.353196	117596.931146	34.906496
1142.274473	117733.169426	34.911514
1142.807162	117879.827560	34.916532
1143.531594	118024.084002	34.921549
1144.466940	118178.961957	34.926567
1144.919894	118344.694344	34.931584
1146.044522	118503.609253	34.936602
1146.366117	118671.190720	34.941620
1147.487113	118842.703988	34.946637
1147.895584	119033.741207	34.951655
1148.852053	119222.899064	34.956672
1150.044983	119408.963637	34.961690
1150.604237	119602.209033	34.966708
1151.612443	119795.695634	34.971725
1152.639388	120005.363072	34.976743
1153.308893	120232.315246	34.981760
1153.981720	120442.857445	34.986778
1155.086107	120646.483943	34.991796
1155.795644	120852.016999	34.996813
1157.013237	121075.992342	35.001831
1158.359814	121302.760696	35.006848
1159.129347	121500.975584	35.011866
1160.037990	121737.352401	35.016884
1161.019544	121954.771961	35.021901
1162.315534	122191.174737	35.026919
1163.534451	122418.416930	35.031936
1164.681347	122639.399720	35.036954
1165.884546	122888.979056	35.041972
1167.268574	123122.902665	35.046989
1168.321650	123360.243323	35.052007
1169.339454	123597.781980	35.057024
1170.775686	123833.045554	35.062042
1171.808106	124073.627198	35.067060
1173.107397	124312.314592	35.072077
1174.275767	124560.671486	35.077095
1175.342518	124805.067987	35.082112
1176.567877	125037.258972	35.087130
1177.699380	125289.164269	35.092148
1178.955218	125544.776730	35.097165
1179.864554	125797.459342	35.102183
1181.601494	126048.899595	35.107200
1182.951708	126280.622229	35.112218
1183.376927	126538.603220	35.117236
1184.904887	126787.398070	35.122253
1186.515035	127030.502240	35.127271
1187.532662	127288.704882	35.132288
1188.734206	127539.437568	35.137306
1190.043269	127792.055205	35.142324
1191.962763	128043.112640	35.147341
1193.871412	128270.812202	35.152359
1195.294756	128494.045803	35.157376
1197.144944	128713.810708	35.162394
1198.558532	128931.395521	35.167412
1200.320371	129128.120452	35.172429
1202.767129	129306.830356	35.177447
1203.827205	129503.867896	35.182464
1205.863176	129673.954170	35.187482
1206.923469	129846.236633	35.192500
1208.457134	130019.478466	35.197517
1209.872618	130185.122782	35.202535
1210.652996	130362.526614	35.207552
1211.919259	130533.509833	35.212570
1212.824771	130707.395343	35.217588
1213.456428	130888.326354	35.222605
1214.591819	131080.302573	35.227623
1215.126257	131268.389525	35.232640
1216.082763	131461.526893	35.237658
1216.615594	131660.949798	35.242676
1217.667806	131872.911642	35.247693
1218.497189	132076.076850	35.252711
1219.544141	132303.534208	35.257728
1220.484774	132515.455943	35.262746
1221.396587	132733.494624	35.267764
1222.274323	132954.164884	35.272781
1223.843580	133162.420735	35.277799
1224.962499	133366.964303	35.282816
1226.451031	133577.442559	35.287834
1227.886125	133780.971042	35.292852
1228.842364	134003.954985	35.297869
1230.247988	134220.220095	35.302887
1231.456417	134428.482314	35.307904
1233.149976	134645.436247	35.312922
1234.147287	134860.165266	35.317940
1235.032587	135081.063951	35.322957
1236.336924	135296.681433	35.327975
1237.733960	135536.703693	35.332992
1238.959794	135750.258219	35.338010
1240.017255	135972.401191	35.343028
1241.149025	136201.886725	35.348045
1242.288474	136430.878023	35.353063
1243.240787	136662.413384	35.358080
1244.273766	136911.015481	35.363098
1245.485429	137152.463014	35.368116
1246.235271	137406.011435	35.373133
1247.629540	137648.927404	35.378151
1248.875213	137909.736141	35.383168
1249.531549	138164.358607	35.388186
1251.342034	138429.626636	35.393204
1252.043140	138692.335083	35.398221
1253.332420	138959.332131	35.403239
1254.422688	139227.633324	35.408256
1255.081528	139509.413444	35.413274
1256.706775	139788.988883	35.418292
1257.295161	140079.699958	35.423309
1258.665342	140362.658620	35.428327
1260.061696	140654.377414	35.433344
1261.533811	140943.232501	35.438362
1263.993480	141199.090212	35.443380
1265.749822	141464.238497	35.448397
1267.642626	141714.477895	35.453415
1269.002607	141978.645371	35.458432
1270.518071	142233.087076	35.463450
1271.731243	142476.993471	35.468468
1273.425879	142733.741448	35.473485
1274.835961	142974.295018	35.478503
1275.635602	143226.469557	35.483520
1276.863294	143477.875106	35.488538
1278.272284	143727.006712	35.493556
1279.282499	143973.583168	35.498573
1280.779708	144226.482311	35.503591
1281.924888	144484.009003	35.508608
1283.573982	144728.616992	35.513626
1285.563012	144960.093123	35.518644
1287.180002	145194.855706	35.523661
1288.900034	145422.779070	35.528679
1290.114862	145650.168899	35.533696
1291.554944	145859.728060	35.538714
1292.829896	146073.945817	35.543732
1293.956343	146277.498791	35.548749
1295.407212	146486.349454	35.553767
1296.180524	146685.640332	35.558784
1297.599362	146896.540724	35.563802
1299.131468	147098.544894	35.568820
1300.455979	147296.603247	35.573837
1301.668607	147493.806678	35.578855
1303.101383	147702.299486	35.583872
1303.870518	147912.441724	35.588890
1305.434182	148115.612867	35.593908
1306.800289	148327.177238	35.598925
1307.920345	148533.026660	35.603943
1309.287648	148755.488274	35.608960
1310.383065	148971.846226	35.613978
1311.644625	149184.828504	35.618996
1312.519213	149412.388357	35.624013
1313.783705	149638.398833	35.629031
1314.622959	149873.856801	35.634048
1315.571930	150115.068627	35.639066
1316.765662	150360.616061	35.644084
1317.957825	150614.625624	35.649101
1318.985425	150857.135130	35.654119
1320.430908	151116.863267	35.659136
1321.444730	151366.582997	35.664154
1323.166946	151628.195228	35.669172
1324.507536	151888.847106	35.674189
1325.859455	152135.748703	35.679207
1327.257805	152398.410962	35.684224
1328.031565	152670.226134	35.689242
1329.637519	152929.507654	35.694260
1330.932223	153197.089369	35.699277
1332.397024	153464.986286	35.704295
1333.748055	153730.633865	35.709312
1335.079539	153991.123706	35.714330
1336.910995	154259.546771	35.719348
1338.152253	154530.000848	35.724365
1339.535912	154784.359937	35.729383
1340.010839	155057.029171	35.734400
1341.262072	155334.184945	35.739418
1342.640670	155611.409631	35.744436
1343.865272	155902.959468	35.749453
1345.028417	156190.982569	35.754471
1346.288414	156487.706403	35.759488
1347.260612	156776.717796	35.764506
1348.735068	157065.061706	35.769524
1349.804107	157372.874314	35.774541
1351.034376	157678.263918	35.779559
1352.272903	157989.198350	35.784576
1353.525081	158306.780534	35.789594
1355.074872	158610.282802	35.794612
1356.188101	158919.545665	35.799629
1357.827762	159222.466119	35.804647
1358.945945	159539.750803	35.809664
1360.471821	159854.963559	35.814682
1361.607476	160146.634783	35.819700
1362.761014	160449.875674	35.824717
1363.695513	160753.955529	35.829735
1364.751143	161069.600396	35.834752
1366.052257	161388.681951	35.839770
1367.374829	161704.184325	35.844788
1368.809648	162025.810634	35.849805
1370.642675	162344.770202	35.854823
1371.832414	162653.768090	35.859840
1373.241010	162982.955287	35.864858
1375.215231	163291.696570	35.869876
1376.480979	163609.645995	35.874893
1377.964546	163916.927732	35.879911
1380.002150	164229.433188	35.884928
1381.351647	164551.473423	35.889946
1383.316747	164856.255818	35.894964
1384.947719	165157.696964	35.899981
1386.042904	165462.175624	35.904999
1387.907475	165751.260130	35.910016
1389.329455	166056.131009	35.915034
1390.674346	166353.746412	35.920052
1392.323546	166662.173466	35.925069
1394.011833	166944.354940	35.930087
1396.024132	167214.783324	35.935104
1397.436257	167513.016609	35.940122
1398.916991	167791.825464	35.945140
1400.493550	168065.061668	35.950157
1401.679480	168359.380094	35.955175
1402.988181	168639.822412	35.960192
1404.576978	168919.698218	35.965210
1406.239310	169196.581050	35.970228
1407.868737	169478.978520	35.975245
1408.629558	169764.432338	35.980263
1410.027007	170050.768746	35.985280
1410.712040	170344.906280	35.990298
1412.494791	170627.588983	35.995316
1413.914330	170924.485059	36.000333
1415.367004	171205.781028	36.005351
1417.280953	171493.382934	36.010368
1418.292239	171799.339073	36.015386
1419.838548	172073.162177	36.020404
1421.285105	172371.572784	36.025421
1422.281789	172676.090274	36.030439
1423.841648	172961.274197	36.035456
1425.218529	173262.925654	36.040474
1426.490465	173560.764300	36.045492
1427.686591	173854.455109	36.050509
1429.067361	174158.509999	36.055527
1430.765253	174469.847932	36.060544
1431.830605	174773.668694	36.065562
1432.890291	175077.225766	36.070580
1434.660402	175389.521633	36.075597
1436.180907	175696.100275	36.080615
1437.784991	176002.679174	36.085632
1438.778642	176329.988176	36.090650
1440.167188	176617.671900	36.095668
1441.387862	176923.623952	36.100685
1442.960683	177217.143089	36.105703
1443.977224	177514.058992	36.110720
1445.391358	177833.703252	36.115738
1446.934946	178126.052229	36.120756
1448.540340	178434.193904	36.125773
1449.556143	178738.617973	36.130791
1451.193157	179052.304356	36.135808
1452.277150	179369.526874	36.140826
1454.761119	179664.871213	36.145844
1456.385006	179973.894543	36.150861
1457.900838	180278.191164	36.155879
1459.905492	180573.901832	36.160896
1461.357546	180869.594475	36.165914
1463.531148	181160.659342	36.170932
1465.155298	181456.071901	36.175949
1466.265537	181750.457051	36.180967
1467.813360	182037.889340	36.185984
1469.065549	182335.947004	36.191002
1470.390043	182638.169934	36.196020
1472.126212	182927.504004	36.201037
1473.365971	183227.447210	36.206055
1474.728841	183518.371440	36.211072
1475.519739	183832.776206	36.216090
1476.846397	184153.171194	36.221108
1478.236471	184462.755001	36.226125
1478.845718	184789.381951	36.231143
1480.407491	185122.524619	36.236160
1481.482257	185466.834186	36.241178
1482.853747	185808.657838	36.246196
1484.237430	186159.494075	36.251213
1485.594219	186510.273576	36.256231
1487.102619	186858.261955	36.261248
1488.365692	187216.589300	36.266266
1489.715009	187649.444272	36.271284
1491.220925	188024.440524	36.276301
1492.786537	188400.139812	36.281319
1493.803603	188766.414525	36.286336
1495.277080	189147.262818	36.291354
1496.630139	189517.889596	36.296372
1497.992321	189915.340892	36.301389
1499.530283	190301.897993	36.306407
1501.013966	190685.191554	36.311424
1502.358275	191082.424957	36.316442
1504.294031	191457.597367	36.321460
1506.652715	191825.679290	36.326477
1508.364567	192198.253883	36.331495
1510.617730	192558.791854	36.336512
1512.325083	192909.878433	36.341530
1514.485316	193266.437304	36.346548
1516.191508	193614.595322	36.351565
1517.929116	193968.754800	36.356583
1519.844905	194299.272003	36.361600
1520.885123	194637.316863	36.366618
1522.240034	194962.144196	36.371636
1524.286184	195278.488350	36.376653
1525.553939	195598.801346	36.381671
1527.159704	195910.577209	36.386688
1528.826772	196221.531492	36.391706
1530.118474	196533.440164	36.396724
1531.688852	196847.549780	36.401741
1533.279552	197174.353456	36.406759
1534.890440	197478.175211	36.411776
1536.185719	197802.607468	36.416794
1537.727860	198120.333464	36.421812
1539.789268	198435.089987	36.426829
1541.237384	198765.518637	36.431847
1542.254950	199093.102334	36.436864
1543.085734	199421.163888	36.441882
1544.587670	199755.612739	36.446900
1546.075366	200092.592217	36.451917
1547.299705	200436.131734	36.456935
1548.959818	200775.192540	36.461952
1550.224054	201128.797015	36.466970
1551.835769	201483.181725	36.471988
1553.833910	201832.651789	36.477005
1555.242103	202184.560693	36.482023
1557.018660	202526.593409	36.487040
1558.640139	202877.427910	36.492058
1560.319271	203235.085239	36.497076
1562.117906	203592.507945	36.502093
1562.820996	203951.503786	36.507111
1564.435549	204305.152117	36.512128
1565.633240	204678.833685	36.517146
1566.767971	205061.555696	36.522164
1568.388323	205432.819491	36.527181
1569.669683	205826.922473	36.532199
1570.879292	206216.976427	36.537216
1572.334702	206607.815553	36.542234
1573.760883	206998.648860	36.547252
1575.915409	207394.070288	36.552269
1577.243291	207802.117076	36.557287
1578.963775	208184.563120	36.562304
1580.866848	208576.020636	36.567322
1582.469709	208974.921601	36.572340
1584.431399	209371.959895	36.577357
1585.890536	209766.927324	36.582375
1587.831123	210159.071348	36.587392
1589.441261	210557.191075	36.592410
1590.887064	210942.439197	36.597428
1592.537422	211328.390489	36.602445
1594.253433	211733.303697	36.607463
1595.752289	212125.074815	36.612480
1597.216417	212522.948865	36.617498
1598.676456	212921.155494	36.622516
1599.896292	213321.563701	36.627533
1601.292267	213732.508815	36.632551
1603.465977	214131.715943	36.637568
1605.249584	214522.864232	36.642586
1606.800678	214910.447407	36.647604
1608.652949	215282.767264	36.652621
1610.515975	215666.414181	36.657639
1612.255802	216030.577951	36.662656
1613.730977	216391.410375	36.667674
1614.989005	216764.573989	36.672692
1616.823091	217155.571624	36.677709
1618.228666	217541.869158	36.682727
1619.614044	217916.437462	36.687744
1621.675179	218292.694777	36.692762
1623.243598	218667.132829	36.697780
1625.733663	219034.810807	36.702797
1627.037794	219417.551296	36.707815
1628.213217	219791.577903	36.712832
1629.803148	220185.447709	36.717850
1631.074747	220577.443037	36.722868
1632.884176	220963.759871	36.727885
1634.665334	221370.478502	36.732903
1636.040020	221763.958827	36.737920
1637.781064	222165.480230	36.742938
1639.245489	222562.376808	36.747956
1641.069783	222950.170851	36.752973
1642.368762	223355.708843	36.757991
1644.248462	223759.421628	36.763008
1645.668145	224161.563447	36.768026
1647.042237	224574.712552	36.773044
1648.769742	224991.510944	36.778061
1649.852160	225414.644100	36.783079
1650.926266	225833.563611	36.788096
1653.028290	226274.991061	36.793114
1654.527377	226715.075304	36.798132
1656.174570	227138.396711	36.803149
1658.177283	227586.220933	36.808167
1659.892398	228018.372797	36.813184
1662.067999	228445.392444	36.818202
1663.385700	228889.731076	36.823220
1664.813277	229323.714101	36.828237
1667.133027	229756.250295	36.833255
1669.227813	230179.554847	36.838272
1671.659394	230590.712026	36.843290
1673.426295	230999.647107	36.848308
1675.132220	231414.131139	36.853325
1676.971959	231836.848759	36.858343
1678.909432	232252.463772	36.863360
1680.669989	232647.179334	36.868378
1682.204189	233048.284909	36.873396
1684.132609	233460.373632	36.878413
1685.634049	233868.319714	36.883431
1687.094957	234292.022680	36.888448
1688.304676	234694.508388	36.893466
1689.928214	235116.712135	36.898484
1691.896143	235530.195887	36.903501
1693.237517	235957.961965	36.908519
1694.800873	236382.820579	36.913536
1696.705543	236795.885987	36.918554
1697.922416	237213.413649	36.923572
1699.500634	237610.025222	36.928589
1700.976598	238018.492414	36.933607
1702.342300	238428.020723	36.938624
1704.196475	238839.701608	36.943642
1705.407614	239272.399310	36.948660
1707.747920	239690.806348	36.953677
1708.770500	240126.179711	36.958695
1710.211177	240563.082664	36.963712
1711.577260	240989.533332	36.968730
1713.195039	241440.175605	36.973748
1714.749517	241887.069894	36.978765
1716.557323	242340.119796	36.983783
1718.152308	242786.805376	36.988800
1719.996391	243243.965715	36.993818
1721.681444	243716.014519	36.998836
1723.250805	244167.228198	37.003853
1724.915302	244639.485107	37.008871
1726.427678	245113.648510	37.013888
1728.225968	245581.997198	37.018906
1729.547057	246067.702065	37.023924
1731.080991	246558.527921	37.028941
1732.802957	247056.638248	37.033959
1734.612096	247552.676612	37.038976
1736.469745	248045.811292	37.043994
1737.995214	248547.970578	37.049012
1740.099027	249041.826251	37.054029
1742.516415	249545.256492	37.059047
1744.610685	250022.348673	37.064064
1747.076891	250507.633602	37.069082
1748.547839	250981.733971	37.074100
1750.601467	251450.298706	37.079117
1752.445123	251930.000817	37.084135
1754.478966	252411.271061	37.089152
1756.435727	252889.557166	37.094170
1757.712339	253371.795723	37.099188
1759.664407	253847.009253	37.104205
1761.265637	254330.869241	37.109223
1762.766088	254820.741762	37.114240
1764.841039	255287.678638	37.119258
1766.199308	255791.420423	37.124276
1768.190998	256280.345450	37.129293
1769.678072	256770.906426	37.134311
1771.404766	257254.770768	37.139328
1773.314537	257745.919885	37.144346
1775.011018	258236.953011	37.149364
1777.069153	258727.466924	37.154381
1779.084698	259210.849710	37.159399
1780.748512	259706.105005	37.164416
1782.881601	260188.806888	37.169434
1784.023276	260690.324094	37.174452
1785.799179	261185.508789	37.179469
1787.933508	261670.165812	37.184487
1789.994979	262158.823306	37.189504
1792.200159	262637.980544	37.194522
1793.869568	263103.765471	37.199540
1795.623712	263564.759790	37.204557
1797.362057	264030.100377	37.209575
1798.597124	264504.189102	37.214592
1800.374955	264974.856760	37.219610
1801.629588	265451.811797	37.224628
1803.253862	265932.132515	37.229645
1804.668524	266412.107527	37.234663
1806.031106	266902.607698	37.239680
1808.360029	267389.715802	37.244698
1810.243903	267888.660926	37.249716
1811.833972	268389.306812	37.254733
1813.902546	268885.272231	37.259751
1815.115201	269406.811448	37.264768
1816.948297	269910.385613	37.269786
1818.348736	270433.542187	37.274804
1819.980006	270960.519550	37.279821
1822.101498	271483.601710	37.284839
1823.599931	272020.887841	37.289856
1825.476702	272549.903189	37.294874
1826.965950	273102.861978	37.299892
1828.618757	273641.236037	37.304909
1830.530849	274192.773718	37.309927
1832.394509	274741.803569	37.314944
1834.455410	275289.858472	37.319962
1836.209903	275844.187934	37.324980
1837.780350	276407.438144	37.329997
1840.157458	276969.939195	37.335015
1842.017870	277531.688803	37.340032
1843.915390	278084.108001	37.345050
1845.868018	278640.402641	37.350068
1847.736114	279199.275648	37.355085
1850.746681	279733.007178	37.360103
1852.987679	280278.121603	37.365120
1855.656845	280804.795859	37.370138
1857.594775	281337.156453	37.375156
1859.651861	281871.044435	37.380173
1861.780945	282388.077379	37.385191
1863.486253	282909.372310	37.390208
1865.603823	283428.588304	37.395226
1867.027265	283964.076244	37.400244
1868.740907	284485.288180	37.405261
1870.725259	285004.318305	37.410279
1872.209709	285547.486471	37.415296
1873.922441	286071.715514	37.420314
1875.882374	286603.215626	37.425332
1877.336781	287144.807875	37.430349
1879.256498	287679.866692	37.435367
1881.112977	288229.412229	37.440384
1883.038504	288763.830617	37.445402
1885.020627	289320.817607	37.450420
1886.395154	289863.682164	37.455437
1888.652336	290408.349132	37.460455
1890.080414	290959.429163	37.465472
1892.697273	291490.948933	37.470490
1894.425288	292022.567534	37.475508
1896.416421	292541.591472	37.480525
1898.760975	293043.179609	37.485543
1900.389837	293561.905250	37.490560
1902.356847	294068.150578	37.495578
1903.971614	294592.944107	37.500596
1906.013108	295115.477813	37.505613
1907.627398	295634.678624	37.510631
1909.471342	296159.526825	37.515648
1911.211408	296690.511112	37.520666
1913.209103	297222.997861	37.525684
1915.221925	297749.256708	37.530701
1917.780210	298282.861045	37.535719
1919.439919	298815.981236	37.540736
1921.578782	299335.200268	37.545754
1923.878062	299866.173458	37.550772
1926.300176	300377.592148	37.555789
1928.532569	300875.122854	37.560807
1930.732732	301390.662878	37.565824
1932.976619	301897.151233	37.570842
1934.907057	302406.890349	37.575860
1936.027026	302921.031805	37.580877
1937.835816	303430.531894	37.585895
1939.077118	303961.179591	37.590912
1941.295142	304493.968026	37.595930
1943.164123	305040.501261	37.600948
1944.237379	305582.773587	37.605965
1946.280681	306146.640535	37.610983
1947.121653	306703.166827	37.616000
1948.628358	307281.694749	37.621018
1950.409329	307868.856739	37.626036
1951.548529	308475.017975	37.631053
1952.951093	309071.809661	37.636071
1955.072982	309677.691958	37.641088
1956.980995	310297.649120	37.646106
1958.559691	310914.661062	37.651124
1960.416734	311551.859263	37.656141
1962.969686	312181.391078	37.661159
1965.086530	312804.618346	37.666176
1967.250542	313435.094672	37.671194
1969.427786	314068.051728	37.676212
1971.457715	314705.649837	37.681229
1973.836802	315331.146396	37.686247
1975.901123	315969.615856	37.691264
1978.063003	316600.191174	37.696282
1979.918733	317225.328386	37.701300
1981.551044	317861.721104	37.706317
1983.803214	318491.958605	37.711335
1985.803087	319134.116284	37.716352
1987.799852	319768.092335	37.721370
1990.081066	320399.119003	37.726388
1991.888951	321031.109073	37.731405
1994.014774	321665.044295	37.736423
1995.878062	322305.035418	37.741440
1998.454345	322914.455906	37.746458
2000.663852	323528.173117	37.751476
2002.082109	324132.600134	37.756493
2004.686946	324724.809268	37.761511
2006.700419	325325.009544	37.766528
2008.612915	325910.368861	37.771546
2011.056140	326510.356690	37.776564
2013.259046	327103.575528	37.781581
2015.722209	327684.557759	37.786599
2018.030056	328259.848539	37.791616
2020.222935	328841.576101	37.796634
2022.747854	329407.297995	37.801652
2024.556222	329987.480120	37.806669
2026.698127	330569.198496	37.811687
2028.958346	331140.659958	37.816704
2031.118501	331699.845879	37.821722
2032.909292	332275.208996	37.826740
2034.889844	332849.492740	37.831757
2036.488848	333421.754015	37.836775
2038.365434	334014.929385	37.841792
2040.178791	334590.060622	37.846810
2042.588522	335187.446933	37.851828
2044.023081	335793.369793	37.856845
2046.026269	336387.156527	37.861863
2047.871582	337003.249809	37.866880
2049.577884	337612.658317	37.871898
2051.494750	338236.009245	37.876916
2052.830379	338861.913884	37.881933
2054.321194	339500.805020	37.886951
2056.024321	340159.246146	37.891968
2057.790212	340828.759268	37.896986
2059.775715	341484.773729	37.902004
2061.317300	342174.687396	37.907021
2063.406111	342850.614573	37.912039
2065.426281	343521.544021	37.917056
2067.211380	344215.548603	37.922074
2069.857664	344909.192552	37.927092
2072.076984	345596.148387	37.932109
2074.115707	346282.211201	37.937127
2076.481353	346974.907537	37.942144
2078.989872	347669.472131	37.947162
2081.490052	348355.221534	37.952180
2083.611795	349041.608746	37.957197
2085.863756	349724.765606	37.962215
2088.072086	350412.436195	37.967232
2089.979278	351091.037599	37.972250
2092.164679	351763.389239	37.977268
2094.052790	352452.223998	37.982285
2096.536404	353127.573521	37.987303
2099.813548	353805.491570	37.992320
2102.594608	354475.034122	37.997338
2104.677017	355128.801829	38.002356
2106.746962	355782.891192	38.007373
2108.887273	356440.789340	38.012391
2110.638319	357103.158170	38.017408
2112.321382	357751.395909	38.022426
2114.708422	358392.145243	38.027444
2116.996362	359028.385299	38.032461
2119.113908	359656.449731	38.037479
2121.244742	360283.208063	38.042496
2122.992680	360915.907597	38.047514
2124.974778	361546.375117	38.052532
2126.723006	362188.262915	38.057549
2128.209973	362842.107776	38.062567
2130.608585	363501.848513	38.067584
2132.204710	364165.672361	38.072602
2133.753930	364825.814412	38.077620
2135.551225	365516.240716	38.082637
2137.114969	366207.861059	38.087655
2139.332766	366912.927230	38.092672
2140.627844	367624.656525	38.097690
2142.700719	368331.191504	38.102708
2144.576772	369069.705064	38.107725
2146.087426	369813.617745	38.112743
2148.565796	370566.049070	38.117760
2150.171814	371328.403603	38.122778
2152.063867	372083.160413	38.127796
2153.912808	372864.106650	38.132813
2155.863866	373651.129959	38.137831
2158.234782	374441.842348	38.142848
2160.091844	375237.341393	38.147866
2162.813238	376019.259347	38.152884
2164.852689	376822.323420	38.157901
2167.504231	377621.181211	38.162919
2170.288095	378406.304556	38.167936
2172.603285	379208.022077	38.172954
2175.043336	379994.510696	38.177972
2177.541454	380789.261844	38.182989
2179.528544	381587.503996	38.188007
2182.061214	382367.276945	38.193024
2183.976315	383171.399994	38.198042
2186.726230	383957.156868	38.203060
2189.194243	384752.525770	38.208077
2191.277478	385535.239404	38.213095
2194.174845	386313.662232	38.218112
2196.423107	387086.599658	38.223130
2199.364254	387861.199297	38.228148
2201.710350	388629.189168	38.233165
2204.100970	389400.548988	38.238183
2206.676817	390155.939297	38.243200
2208.197041	390922.339962	38.248218
2210.364380	391681.741693	38.253236
2213.068681	392461.157117	38.258253
2214.808836	393234.710281	38.263271
2217.138090	393999.170656	38.268288
2218.787047	394779.973060	38.273306
2221.027912	395540.480339	38.278324
2223.779841	396323.055249	38.283341
2225.972140	397090.550346	38.288359
2228.264519	397865.027508	38.293376
2230.169897	398626.499622	38.298394
2232.081441	399371.226111	38.303412
2234.279491	400118.240696	38.308429
2236.162253	400881.404811	38.313447
2238.507718	401636.791784	38.318464
2240.172457	402400.610716	38.323482
2242.269359	403163.574750	38.328500
2244.624783	403924.776105	38.333517
2247.083558	404691.917868	38.338535
2249.528326	405453.137676	38.343552
2251.236519	406230.397062	38.348570
2253.591182	407005.471719	38.353588
2256.127665	407791.689887	38.358605
2258.196530	408572.746724	38.363623
2260.608211	409346.832186	38.368640
2262.701120	410141.466889	38.373658
2264.857664	410923.655546	38.378676
2266.970452	411717.276900	38.383693
2269.635984	412513.945666	38.388711
2272.184935	413305.721909	38.393728
2274.339080	414111.065603	38.398746
2276.760301	414903.068019	38.403764
2278.842080	415699.257239	38.408781
2281.014211	416514.626894	38.413799
2283.634196	417305.558473	38.418816
2286.411830	418113.378844	38.423834
2288.817698	418906.297228	38.428852
2291.292468	419718.675489	38.433869
2293.232853	420513.799923	38.438887
2295.318862	421312.418576	38.443904
2297.790395	422129.731425	38.448922
2300.227198	422942.212699	38.453940
2302.356112	423746.972744	38.458957
2304.016254	424573.051273	38.463975
2306.442049	425399.476958	38.468992
2308.911845	426241.459968	38.474010
2310.496507	427065.693776	38.479028
2313.127580	427910.729090	38.484045
2314.920261	428762.610304	38.489063
2317.321137	429609.446582	38.494080
2319.339685	430467.301823	38.499098
2321.509222	431318.620782	38.504116
2323.775327	432185.582557	38.509133
2325.424034	433069.319531	38.514151
2327.828608	433948.135889	38.519168
2329.923445	434841.394920	38.524186
2332.696699	435729.796457	38.529204
2334.637112	436620.532091	38.534221
2337.186242	437536.024999	38.539239
2339.422866	438425.727537	38.544256
2341.652480	439335.837626	38.549274
2344.059579	440227.513446	38.554292
2347.144586	441126.069985	38.559309
2349.561503	442033.658810	38.564327
2352.413239	442921.304157	38.569344
2354.626871	443813.676455	38.574362
2356.877715	444683.444101	38.579380
2359.689696	445538.360663	38.584397
2361.668734	446402.844375	38.589415
2364.399175	447243.998868	38.594432
2366.345546	448115.297509	38.599450
2368.808864	448971.299038	38.604468
2371.803283	449816.857840	38.609485
2374.226193	450671.987726	38.614503
2376.804962	451525.134236	38.619520
2379.324612	452371.631391	38.624538
2381.660381	453229.148636	38.629556
2384.136599	454086.960072	38.634573
2386.404616	454944.316112	38.639591
2388.553521	455806.459604	38.644608
2390.850267	456677.641509	38.649626
2392.669610	457548.463024	38.654644
2395.120438	458427.075703	38.659661
2398.115480	459310.207470	38.664679
2400.391493	460173.506965	38.669696
2402.602386	461053.814110	38.674714
2405.128964	461933.067756	38.679732
2407.852119	462824.580667	38.684749
2410.602917	463711.752440	38.689767
2413.118861	464584.975783	38.694784
2415.245235	465463.633671	38.699802
2417.507574	466362.390834	38.704820
2419.914067	467242.738994	38.709837
2421.653323	468145.089810	38.714855
2423.812703	469057.481748	38.719872
2426.197562	469978.582315	38.724890
2428.415550	470894.412441	38.729908
2430.953626	471815.245637	38.734925
2433.187189	472750.583582	38.739943
2436.033089	473674.505639	38.744960
2438.462874	474610.928944	38.749978
2440.370378	475555.576391	38.754996
2443.093448	476512.258252	38.760013
2444.991990	477475.141939	38.765031
2447.275161	478432.051141	38.770048
2449.701916	479402.923632	38.775066
2452.359961	480359.010632	38.780084
2454.871595	481323.403055	38.785101
2456.936636	482303.723988	38.790119
2459.368688	483269.943706	38.795136
2462.021477	484256.367529	38.800154
2464.322468	485237.697964	38.805172
2467.237893	486221.493579	38.810189
2469.548723	487209.476301	38.815207
2472.197613	488189.320298	38.820224
2474.722551	489165.799296	38.825242
2477.288333	490155.741236	38.830260
2480.047877	491140.294546	38.835277
2482.857960	492113.580485	38.840295
2485.908333	493081.572775	38.845312
2488.738669	494041.071182	38.850330
2491.400672	494968.557405	38.855348
2494.395831	495891.849320	38.860365
2496.467847	496810.556761	38.865383
2498.855782	497729.109366	38.870400
2501.173688	498646.917179	38.875418
2503.613785	499568.184086	38.880436
2506.391639	500489.997640	38.885453
2508.662460	501428.085591	38.890471
2511.313918	502336.805650	38.895488
2514.715251	503254.171772	38.900506
2517.188019	504172.250013	38.905524
2519.878176	505070.625294	38.910541
2522.104615	505997.465913	38.915559
2524.195187	506926.091382	38.920576
2526.715819	507844.305444	38.925594
2528.887872	508771.952945	38.930612
2531.845064	509712.366750	38.935629
2533.770529	510663.082662	38.940647
2536.449324	511598.190032	38.945664
2539.229677	512538.869028	38.950682
2540.851595	513485.384158	38.955700
2543.904346	514430.085670	38.960717
2546.503065	515405.695533	38.965735
2548.519727	516369.855627	38.970752
2551.073162	517342.327980	38.975770
2553.179670	518333.102753	38.980788
2555.648109	519320.729070	38.985805
2557.750096	520333.086883	38.990823
2559.736679	521340.360111	38.995840
2562.341072	522359.498108	39.000858
2564.414066	523391.298915	39.005876
2566.783366	524416.028721	39.010893
2569.313932	525462.363824	39.015911
2572.184256	526505.949095	39.020928
2575.032958	527549.766743	39.025946
2577.540200	528588.031123	39.030964
2581.034222	529635.064648	39.035981
2583.847591	530682.391380	39.040999
2586.492252	531724.235782	39.046016
2589.303977	532771.966276	39.051034
2591.710120	533831.215036	39.056052
2593.799925	534880.375566	39.061069
2596.437061	535936.058408	39.066087
2598.681698	537016.032719	39.071104
2601.208057	538080.129628	39.076122
2603.551076	539141.713062	39.081140
2606.055476	540227.385389	39.086157
2608.613057	541318.447657	39.091175
2610.840224	542408.525933	39.096192
2614.172991	543485.958419	39.101210
2616.436409	544574.201612	39.106228
2619.095239	545664.655192	39.111245
2621.847662	546775.923228	39.116263
2624.343969	547872.162980	39.121280
2626.966281	548956.831454	39.126298
2629.812578	550018.855310	39.131316
2632.957830	551066.771639	39.136333
2635.766802	552122.706012	39.141351
2638.557117	553171.927083	39.146368
2641.777540	554214.258921	39.151386
2644.313396	555263.209182	39.156404
2647.152847	556283.737325	39.161421
2649.851974	557325.663975	39.166439
2652.758098	558367.322596	39.171456
2655.504765	559398.628503	39.176474
2657.773919	560451.433141	39.181492
2660.314473	561494.413422	39.186509
2662.553092	562551.072293	39.191527
2664.582651	563604.919153	39.196544
2667.290592	564662.330387	39.201562
2670.150932	565740.515756	39.206580
2672.669289	566818.819832	39.211597
2675.213260	567905.010651	39.216615
2677.394480	569001.963178	39.221632
2680.319151	570099.497194	39.226650
2682.636744	571199.348535	39.231668
2685.124998	572301.082272	39.236685
2687.783196	573436.661145	39.241703
2690.156646	574573.289644	39.246720
2692.782470	575712.280049	39.251738
2695.384524	576854.882425	39.256756
2697.940490	577993.324430	39.261773
2700.744377	579146.264412	39.266791
2703.228771	580309.983407	39.271808
2706.108967	581468.359298	39.276826
2708.741724	582639.453456	39.281844
2711.619942	583803.624579	39.286861
2714.169428	584983.280646	39.291879
2716.813083	586166.564805	39.296896
2719.530588	587343.003677	39.301914
2722.051132	588547.275396	39.306932
2724.740358	589745.132886	39.311949
2727.880811	590944.596397	39.316967
2730.381603	592136.983464	39.321984
2733.076448	593345.297643	39.327002
2735.754443	594559.250900	39.332020
2738.012899	595784.819872	39.337037
2740.729482	597000.766724	39.342055
2743.520582	598235.852414	39.347072
2746.677180	599456.924655	39.352090
2749.292792	600699.237269	39.357108
2751.674371	601941.155138	39.362125
2754.380375	603181.731546	39.367143
2756.614236	604428.559605	39.372160
2759.108774	605695.072989	39.377178
2761.763092	606968.722583	39.382196
2764.799259	608238.910925	39.387213
2767.349407	609516.842450	39.392231
2769.786593	610799.749161	39.397248
2772.792958	612062.905463	39.402266
2775.451569	613320.776473	39.407284
2777.846789	614571.798964	39.412301
2780.565309	615831.723457	39.417319
2783.527057	617085.362746	39.422336
2786.388562	618337.875597	39.427354
2789.254143	619590.493513	39.432372
2792.472641	620835.160512	39.437389
2795.426382	622096.818362	39.442407
2798.187738	623348.368783	39.447424
2801.477846	624601.930836	39.452442
2804.653901	625858.062600	39.457460
2807.527962	627102.061108	39.462477
2811.094455	628353.086447	39.467495
2813.866139	629597.658134	39.472512
2816.995694	630849.610448	39.477530
2820.078654	632089.689926	39.482548
2823.086355	633320.999869	39.487565
2826.249767	634548.344571	39.492583
2828.990277	635786.046141	39.497600
2832.732993	636998.280216	39.502618
2835.940517	638230.369754	39.507636
2839.238595	639439.199108	39.512653
2842.093940	640647.412649	39.517671
2844.470085	641879.005504	39.522688
2847.272957	643088.534320	39.527706
2850.200664	644326.268590	39.532724
2852.785796	645546.859113	39.537741
2855.188905	646768.180103	39.542759
2857.596838	648008.939898	39.547776
2860.891446	649248.945638	39.552794
2863.948790	650488.189682	39.557812
2866.489627	651728.214216	39.562829
2869.327668	652974.359425	39.567847
2872.394969	654215.426341	39.572864
2875.473860	655466.046545	39.577882
2878.180545	656723.193828	39.582900
2880.993104	657979.414126	39.587917
2883.803154	659228.801152	39.592935
2886.979945	660498.075474	39.597952
2889.861206	661746.477931	39.602970
2892.949952	663006.577253	39.607988
2895.634262	664276.432602	39.613005
2898.727865	665540.128623	39.618023
2900.775762	666812.441830	39.623040
2903.565864	668089.829691	39.628058
2905.758509	669385.349583	39.633076
2908.545400	670686.656595	39.638093
2911.660559	671972.861072	39.643111
2914.271537	673298.844644	39.648128
2917.302530	674606.077496	39.653146
2919.907370	675937.651080	39.658164
2922.124625	677267.310605	39.663181
2925.106835	678609.069054	39.668199
2927.204388	679954.309986	39.673216
2930.440410	681284.605855	39.678234
2933.308113	682617.303692	39.683252
2936.476401	683932.673681	39.688269
2939.778668	685236.510292	39.693287
2942.492831	686550.634287	39.698304
2945.641799	687855.607943	39.703322
2948.645881	689175.205403	39.708340
2951.795805	690491.010816	39.713357
2954.975403	691804.285301	39.718375
2957.922728	693120.728949	39.723392
2961.064649	694430.793722	39.728410
2964.157049	695752.871659	39.733428
2966.922528	697066.576180	39.738445
2969.832998	698389.180959	39.743463
2972.870775	699718.850288	39.748480
2976.109377	701060.077584	39.753498
2979.387141	702380.180088	39.758516
2982.121070	703713.253845	39.763533
2985.655902	705041.873250	39.768551
2988.684331	706376.862109	39.773568
2991.373472	707710.413375	39.778586
2994.092666	709057.119951	39.783604
2996.975982	710412.100408	39.788621
3000.015993	711751.790369	39.793639
3003.007382	713108.944252	39.798656
3006.214562	714466.436491	39.803674
3009.457240	715839.287490	39.808692
3012.142908	717203.896086	39.813709
3015.295357	718570.773555	39.818727
3018.076099	719942.929231	39.823744
3021.306657	721325.509619	39.828762
3024.496149	722695.556778	39.833780
3027.536408	724076.620780	39.838797
3030.888031	725447.417020	39.843815
3034.175715	726839.684457	39.848832
3037.070932	728217.504600	39.853850
3040.434971	729597.233556	39.858868
3043.708198	730979.557668	39.863885
3047.306389	732336.606050	39.868903
3050.214329	733713.536526	39.873920
3052.929425	735089.029494	39.878938
3055.847615	736467.902816	39.883956
3058.797433	737859.212457	39.888973
3061.771171	739247.610237	39.893991
3064.871972	740644.867409	39.899008
3067.553772	742037.460962	39.904026
3070.684675	743437.866479	39.909044
3073.554350	744840.432493	39.914061
3076.456102	746252.155032	39.919079
3079.317150	747671.266629	39.924096
3082.351338	749093.932054	39.929114
3085.180238	750520.607132	39.934132
3088.135538	751952.611124	39.939149
3091.618540	753376.379233	39.944167
3095.127489	754810.167732	39.949184
3098.095240	756230.193421	39.954202
3101.460210	757620.504955	39.959220
3104.365231	759001.930579	39.964237
3107.832267	760367.510660	39.969255
3110.330934	761755.339769	39.974272
3113.639969	763137.413497	39.979290
3116.948662	764504.825334	39.984308
3119.869363	765897.272171	39.989325
3123.180844	767282.215480	39.994343
3126.429194	768664.552011	39.999360
3129.330466	770054.206584	40.004378
3132.781066	771438.248998	40.009396
3135.402233	772832.879137	40.014413
3138.146948	774237.534571	40.019431
3141.377414	775657.350857	40.024448
3144.329315	777078.704689	40.029466
3147.538349	778491.491241	40.034484
3150.343458	779933.461447	40.039501
3153.639910	781354.161096	40.044519
3156.535997	782798.632008	40.049536
3159.726639	784247.272601	40.054554
3162.988418	785700.362593	40.059572
3165.697862	787160.749650	40.064589
3169.249246	788619.810065	40.069607
3172.349858	790100.106676	40.074624
3175.630920	791574.036144	40.079642
3178.991285	793042.989979	40.084660
3181.620662	794532.374814	40.089677
3184.739126	796027.183851	40.094695
3187.918958	797528.219630	40.099712
3191.420034	799024.716113	40.104730
3194.660451	800537.224304	40.109748
3197.345136	802042.451788	40.114765
3200.675209	803555.943457	40.119783
3203.965221	805078.445220	40.124800
3207.389026	806604.054618	40.129818
3210.884247	808129.504796	40.134836
3213.425550	809664.790111	40.139853
3216.760740	811189.137626	40.144871
3220.345703	812725.403693	40.149888
3223.147186	814290.941356	40.154906
3225.769914	815840.864597	40.159924
3228.909071	817414.007694	40.164941
3232.512130	818975.574873	40.169959
3235.449442	820543.130829	40.174976
3238.781679	822112.343799	40.179994
3242.305934	823683.879674	40.185012
3244.789795	825271.106447	40.190029
3248.206895	826869.629775	40.195047
3251.512299	828440.594317	40.200064
3255.186699	830039.219465	40.205082
3258.204876	831619.154570	40.210100
3261.194361	833214.967386	40.215117
3264.454497	834818.222170	40.220135
3267.578157	836430.781748	40.225152
3270.238856	838030.753854	40.230170
3273.351424	839601.989677	40.235188
3276.132335	841189.618616	40.240205
3279.437758	842766.648080	40.245223
3283.083504	844341.183264	40.250240
3285.948004	845941.790093	40.255258
3288.854210	847534.111364	40.260276
3292.288481	849133.025609	40.265293
3295.660967	850731.441819	40.270311
3299.251128	852339.406594	40.275328
3302.053650	853950.386474	40.280346
3305.829300	855559.420098	40.285364
3308.775519	857178.648473	40.290381
3311.761218	858807.331922	40.295399
3315.394135	860427.907871	40.300416
3318.786333	862065.634220	40.305434
3322.382680	863695.615653	40.310452
3325.808470	865334.290858	40.315469
3329.345044	866976.858084	40.320487
3332.650903	868626.275133	40.325504
3335.687628	870280.702391	40.330522
3339.182034	871928.882912	40.335540
3342.741380	873594.973033	40.340557
3345.376874	875264.909488	40.345575
3348.698305	876946.243256	40.350592
3351.529127	878634.331228	40.355610
3354.710975	880329.698499	40.360628
3357.903117	882043.213200	40.365645
3360.793583	883755.501747	40.370663
3364.663764	885481.886506	40.375680
3367.631697	887209.549504	40.380698
3371.275606	888941.691459	40.385716
3374.559778	890694.975320	40.390733
3377.267602	892438.274312	40.395751
3380.785468	894199.985799	40.400768
3384.177760	895960.882597	40.405786
3387.583512	897727.971493	40.410804
3391.200195	899509.492293	40.415821
3394.078897	901298.371227	40.420839
3398.054252	903072.344567	40.425856
3401.420582	904863.558817	40.430874
3404.981846	906637.332090	40.435892
3408.357906	908444.795054	40.440909
3411.619364	910241.305564	40.445927
3415.033583	912038.259804	40.450944
3418.355173	913843.188598	40.455962
3421.762707	915647.313943	40.460980
3424.941847	917467.293029	40.465997
3428.107538	919278.411657	40.471015
3431.707618	921100.071367	40.476032
3434.774142	922935.396717	40.481050
3438.493588	924762.601998	40.486068
3442.262789	926582.179239	40.491085
3445.379829	928422.702445	40.496103
3449.063215	930252.819607	40.501120
3452.112231	932074.522478	40.506125
3455.207925	933845.124614	40.511130
3458.246268	935565.270961	40.516135
3461.665224	937231.962343	40.521140
3465.092110	938812.150282	40.526144
3468.139176	940336.159557	40.531149
3471.048685	941776.697518	40.536154
3474.325567	943157.016554	40.541159
3477.607406	944453.674239	40.546164
3480.523770	945655.980232	40.551168
3483.102481	946788.205983	40.556173
3485.389544	947838.238820	40.561178
3488.132726	948819.967042	40.566183
3490.337353	949722.313958	40.571188
3493.081726	950564.548967	40.576192
3494.543768	951365.321228	40.581197
3496.580164	952087.261326	40.586202
3498.493320	952756.954166	40.591207
3500.030017	953363.183184	40.596212
3502.020317	953910.827728	40.601216
3503.278173	954407.852955	40.606221
3505.304006	954851.956922	40.611226
3506.749737	955244.460340	40.616231
3508.005782	955577.954757	40.621236
3509.546223	955865.309012	40.626240
3510.380816	956117.677537	40.631245
3511.910907	956320.220945	40.636250
3513.202963	956482.317348	40.641255
3514.194654	956612.606033	40.646260
3515.382048	956698.850959	40.651264
3515.985430	956759.319333	40.656269
3517.313610	956773.402281	40.661274
3518.342449	956754.114479	40.666279
3518.932517	956723.434121	40.671284
3520.104768	956640.119287	40.676288
3520.278394	956542.271477	40.681293
3521.150212	956420.680752	40.686298
3522.021124	956267.721401	40.691303
3522.212584	956093.407054	40.696308
3523.035884	955893.394840	40.701312
3523.436896	955694.330048	40.706317
3523.733639	955461.356727	40.711322
3524.320551	955229.500920	40.716327
3524.871025	954964.111805	40.721332
3525.681436	954684.743523	40.726336
3525.883566	954394.385747	40.731341
3526.283419	954084.760518	40.736346
3526.732692	953754.615247	40.741351
3526.854237	953434.411908	40.746356
3527.400783	953085.578875	40.751360
3527.497929	952727.680076	40.756365
3527.851883	952352.354034	40.761370
3528.557507	951968.801897	40.766375
3528.541745	951575.341322	40.771380
3528.755967	951181.520384	40.776384
3528.949355	950796.015753	40.781389
3528.948541	950391.370543	40.786394
3529.288060	949981.918781	40.791399
3529.280793	949570.676114	40.796404
3529.644595	949148.337207	40.801408
3529.873752	948722.064361	40.806413
3529.943827	948286.312161	40.811418
3530.175842	947842.936897	40.816423
3529.776541	947411.686965	40.821428
3530.433547	946958.689984	40.826432
3530.735275	946508.584592	40.831437
3530.821095	946049.958564	40.836442
3530.914175	945584.590165	40.841447
3531.213505	945116.176921	40.846452
3531.188052	944635.235287	40.851456
3531.248186	944167.063655	40.856461
3531.420274	943691.361732	40.861466
3531.450179	943206.447168	40.866471
3531.305632	942718.643720	40.871476
3531.651530	942218.642335	40.876480
3531.779494	941730.220172	40.881485
3531.536020	941231.852405	40.886490
3531.931463	940728.824708	40.891495
3531.877853	940232.915239	40.896500
3532.018114	939726.192884	40.901504
3531.747972	939225.337054	40.906509
3531.930003	938719.180227	40.911514
3532.148618	938215.555964	40.916519
3532.125545	937694.669051	40.921524
3532.563364	937179.499626	40.926528
3532.235810	936668.053510	40.931533
3532.063021	936141.188357	40.936538
3532.296352	935621.489248	40.941543
3532.169311	935101.608250	40.946548
3532.232883	934572.243009	40.951552
3532.067074	934053.799448	40.956557
3532.221703	933524.984547	40.961562
3532.606988	933003.944851	40.966567
3532.316034	932480.282181	40.971572
3532.522760	931931.147011	40.976576
3532.522018	931400.993663	40.981581
3532.485280	930865.129957	40.986586
3532.709314	930330.703338	40.991591
3532.864490	929798.442630	40.996596
3532.818801	929246.671353	41.001600
3532.540441	928714.087642	41.006605
3532.516735	928161.431471	41.011610
3532.666485	927620.693954	41.016615
3532.789954	927080.482263	41.021620
3532.688477	926530.071177	41.026624
3532.778373	925978.513721	41.031629
3532.907837	925428.237672	41.036634
3532.720368	924889.586554	41.041639
3532.654400	924337.117369	41.046644
3532.975347	923785.197893	41.051648
3532.791320	923236.095376	41.056653
3532.527367	922681.374435	41.061658
3532.705687	922129.116569	41.066663
3532.770293	921576.917510	41.071668
3533.086025	921012.598313	41.076672
3532.836362	920454.567859	41.081677
3532.959883	919899.878572	41.086682
3532.921904	919336.117549	41.091687
3532.543260	918774.760957	41.096692
3533.228200	918219.803338	41.101696
3532.841993	917657.466191	41.106701
3532.478891	917096.798960	41.111706
3532.854064	916528.536932	41.116711
3532.637746	915970.423155	41.121716
3532.792007	915405.835381	41.126720
3532.751445	914843.051522	41.131725
3532.906637	914283.931213	41.136730
3532.688580	913721.254435	41.141735
3532.557105	913163.609012	41.146740
3533.026172	912587.986113	41.151744
3532.707085	912025.152014	41.156749
3532.732437	911451.893559	41.161754
3532.870077	910881.060977	41.166759
3532.642975	910323.913591	41.171764
3532.884904	909755.836935	41.176768
3532.563143	909189.532600	41.181773
3532.701667	908612.778421	41.186778
3533.005158	908044.418436	41.191783
3532.737750	907480.242772	41.196788
3532.890116	906897.908530	41.201792
3532.640363	906326.959667	41.206797
3532.644817	905754.269197	41.211802
3532.793464	905172.332840	41.216807
3533.261670	904606.195817	41.221812
3532.961940	904019.296116	41.226816
3532.890566	903446.573658	41.231821
3532.695009	902865.226484	41.236826
3532.546093	902289.503887	41.241831
3532.566622	901712.438464	41.246836
3532.954692	901133.803039	41.251840
3532.869553	900564.261797	41.256845
3532.739876	899982.314001	41.261850
3533.196696	899399.047199	41.266855
3532.561676	898818.899376	41.271860
3532.585712	898234.233820	41.276864
3532.621653	897655.106770	41.281869
3532.422065	897074.318501	41.286874
3532.740976	896494.058088	41.291879
3532.603502	895915.748049	41.296884
3532.594823	895332.526229	41.301888
3532.749101	894759.748418	41.306893
3532.702592	894176.220774	41.311898
3532.820976	893590.382194	41.316903
3532.623247	893009.079847	41.321908
3532.767792	892420.603287	41.326912
3532.769977	891834.023673	41.331917
3532.506442	891247.332382	41.336922
3532.748999	890657.690304	41.341927
3532.855769	890074.392934	41.346932
3532.892732	889482.924178	41.351936
3532.589920	888893.870404	41.356941
3532.634859	888298.505882	41.361946
3533.083256	887704.752115	41.366951
3532.758846	887126.162297	41.371956
3532.722831	886529.370577	41.376960
3532.795232	885936.272644	41.381965
3533.017260	885335.829532	41.386970
3532.966917	884730.627675	41.391975
3532.697098	884132.853718	41.396980
3532.865355	883534.652808	41.401984
3532.541994	882938.120062	41.406989
3532.608712	882346.107338	41.411994
3532.705682	881742.311236	41.416999
3532.441475	881151.104890	41.422004
3532.341067	880547.121641	41.427008
3532.334872	879963.112227	41.432013
3532.494191	879369.618625	41.437018
3532.685975	878777.028134	41.442023
3532.377143	878186.982522	41.447028
3532.579394	877578.861681	41.452032
3532.609796	876987.862170	41.457037
3532.468869	876387.333210	41.462042
3532.743131	875787.641441	41.467047
3532.254566	875191.315126	41.472052
3532.510124	874590.826056	41.477056
3532.420941	873997.025682	41.482061
3532.420912	873397.137644	41.487066
3532.462023	872794.175057	41.492071
3532.420153	872207.267188	41.497076
3532.774639	871602.577877	41.502080
3532.579527	871013.443866	41.507085
3532.291582	870403.891250	41.512090
3532.374686	869799.841101	41.517095
3532.449712	869204.756609	41.522100
3532.330081	868605.375422	41.527104
3532.398475	868002.989942	41.532109
3532.266227	867396.209529	41.537114
3532.472025	866786.979804	41.542119
3532.422407	866185.305377	41.547124
3532.324409	865581.636746	41.552128
3532.384974	864985.552637	41.557133
3532.317441	864378.941671	41.562138
3532.322190	863772.160139	41.567143
3532.142510	863169.817768	41.572148
3532.046586	862561.377347	41.577152
3532.500687	861964.538838	41.582157
3532.070778	861361.573196	41.587162
3532.121047	860754.578191	41.592167
3532.105377	860159.099876	41.597172
3531.935868	859554.452281	41.602176
3532.030934	858958.157008	41.607181
3531.787354	858358.361133	41.612186
3532.151205	857747.998654	41.617191
3531.848698	857152.372539	41.622196
3531.949391	856549.520163	41.627200
3532.234824	855947.646754	41.632205
3532.080761	855348.415585	41.637210
3532.256055	854731.072744	41.642215
3531.614472	854126.065920	41.647220
3531.838203	853521.435654	41.652224
3531.755617	852926.529267	41.657229
3531.428919	852322.069913	41.662234
3531.807907	851718.890831	41.667239
3531.836239	851125.835893	41.672244
3532.129484	850509.510275	41.677248
3532.058962	849911.391209	41.682253
3532.236194	849300.611945	41.687258
3532.073795	848689.148984	41.692263
3532.020525	848078.970677	41.697268
3532.314601	847463.024384	41.702272
3531.658728	846848.932708	41.707277
3531.552835	846234.686730	41.712282
3531.926573	845630.625440	41.717287
3531.981768	845029.288373	41.722292
3531.610929	844423.971201	41.727296
3531.809015	843823.176196	41.732301
3531.493888	843207.109955	41.737306
3531.780594	842604.624011	41.742311
3531.304620	841999.188766	41.747316
3531.259768	841384.457789	41.752320
3531.624404	840795.824233	41.757325
3531.313653	840187.213334	41.762330
3531.491542	839582.653745	41.767335
3531.401521	838971.547956	41.772340
3531.467723	838365.330990	41.777344
3531.489869	837763.014298	41.782349
3531.320205	837155.063954	41.787354
3531.578394	836554.543744	41.792359
3531.500803	835954.073114	41.797364
3531.516457	835338.356088	41.802368
3531.843087	834725.796017	41.807373
3531.437521	834117.157583	41.812378
3531.579881	833509.148705	41.817383
3531.616782	832890.703781	41.822388
3531.522204	832276.371029	41.827392
3531.787490	831677.540290	41.832397
3531.527266	831061.801850	41.837402
3531.595453	830434.913385	41.842407
3531.399779	829831.693149	41.847412
3531.535774	829216.639041	41.852416
3531.608683	828604.858578	41.857421
3531.328801	827991.419847	41.862426
3531.443308	827367.352783	41.867431
3531.264379	826760.375557	41.872436
3531.255563	826141.488436	41.877440
3531.211130	825534.667232	41.882445
3531.338305	824924.143964	41.887450
3531.618932	824307.965806	41.892455
3531.100873	823697.633709	41.897460
3530.863626	823088.027838	41.902464
3531.159078	822477.541075	41.907469
3530.738976	821864.137304	41.912474
3531.096544	821256.753510	41.917479
3530.995667	820653.304114	41.922484
3531.048328	820044.393632	41.927488
3531.170950	819432.920632	41.932493
3531.263614	818823.303902	41.937498
3531.360287	818207.613255	41.942503
3531.074694	817601.226287	41.947508
3531.279135	816973.807732	41.952512
3531.134215	816364.103462	41.957517
3530.843698	815754.710762	41.962522
3531.016736	815144.106479	41.967527
3530.518663	814536.595594	41.972532
3531.115259	813921.548882	41.977536
3531.065138	813314.535822	41.982541
3530.781681	812699.037515	41.987546
3530.969306	812082.374058	41.992551
3530.664527	811473.328261	41.997556
3530.911564	810854.044577	42.002560
3531.035570	810247.361280	42.007565
3530.548848	809634.457933	42.012570
3530.793638	809026.762618	42.017575
3530.305652	808412.181043	42.022580
3530.308342	807800.448643	42.027584
3530.679896	807194.135086	42.032589
3530.606499	806589.999544	42.037594
3530.776422	805980.524837	42.042599
3530.549896	805369.788899	42.047604
3530.779721	804762.841730	42.052608
3530.638966	804150.462422	42.057613
3530.274253	803536.350546	42.062618
3530.744051	802931.749162	42.067623
3530.247551	802324.856687	42.072628
3530.340152	801711.434834	42.077632
3530.484137	801100.352585	42.082637
3530.436748	800508.867931	42.087642
3530.597152	799886.982718	42.092647
3530.134214	799271.476174	42.097652
3530.079223	798663.694896	42.102656
3530.286412	798057.336473	42.107661
3530.134723	797449.759486	42.112666
3530.271333	796834.473577	42.117671
3530.130326	796229.045284	42.122676
3530.213958	795618.421332	42.127680
3530.410759	795007.184552	42.132685
3530.234320	794405.039767	42.137690
3530.120322	793796.990026	42.142695
3529.940120	793189.095088	42.147700
3529.877754	792586.283144	42.152704
3530.266689	791977.203789	42.157709
3530.296449	791371.619881	42.162714
3530.110862	790753.888731	42.167719
3529.922271	790157.078506	42.172724
3530.110782	789542.370065	42.177728
3530.598689	788929.964306	42.182733
3530.482126	788324.831314	42.187738
3530.640320	787700.091913	42.192743
3530.108166	787088.044830	42.197748
3530.131853	786474.326498	42.202752
3530.334871	785856.297570	42.207757
3530.272117	785254.088211	42.212762
3530.226176	784622.477064	42.217767
3530.105438	784024.991363	42.222772
3530.069930	783394.597190	42.227776
3530.316872	782788.242655	42.232781
3530.132581	782181.664528	42.237786
3529.614414	781559.256056	42.242791
3529.253356	780954.424034	42.247796
3529.563344	780341.900724	42.252800
3529.567844	779739.265214	42.257805
3529.114524	779143.643442	42.262810
3529.609089	778529.655578	42.267815
3529.102023	777941.176384	42.272820
3529.458378	777335.967717	42.277824
3529.509924	776741.587462	42.282829
3529.076585	776139.268140	42.287834
3529.385196	775536.033919	42.292839
3529.233816	774940.162813	42.297844
3529.200584	774327.287918	42.302848
3529.363108	773733.972303	42.307853
3529.302615	773138.184728	42.312858
3529.250552	772534.862507	42.317863
3529.484007	771937.499073	42.322868
3529.303433	771332.524020	42.327872
3529.275495	770723.089526	42.332877
3528.988975	770121.874734	42.337882
3529.121316	769511.130388	42.342887
3529.090996	768915.783445	42.347892
3529.324953	768302.606309	42.352896
3529.227413	767717.471737	42.357901
3528.743057	767117.869362	42.362906
3529.171612	766509.635497	42.367911
3528.836793	765922.379291	42.372916
3528.587056	765318.796642	42.377920
3528.770719	764728.153882	42.382925
3528.579403	764129.985866	42.387930
3529.062800	763542.402458	42.392935
3528.714828	762946.286413	42.397940
3528.556968	762338.995884	42.402944
3528.815195	761752.543245	42.407949
3528.626563	761159.808531	42.412954
3528.706894	760558.497981	42.417959
3528.519298	759962.561568	42.422964
3528.594478	759371.022109	42.427968
3528.803306	758773.345589	42.432973
3528.556490	758182.705400	42.437978
3528.752477	757584.197107	42.442983
3528.607359	756997.542417	42.447988
3528.643310	756400.645793	42.452992
3528.751896	755803.986021	42.457997
3528.480938	755206.406527	42.463002
3528.691277	754597.937610	42.468007
3528.080120	754016.414227	42.473012
3528.079015	753412.181591	42.478016
3528.344567	752829.035989	42.483021
3528.552151	752239.140943	42.488026
3528.698679	751634.743018	42.493031
3528.772469	751047.939596	42.498036
3528.645279	750454.754915	42.503040
3528.618437	749856.469652	42.508045
3528.626926	749254.723796	42.513050
3528.472446	748657.404729	42.518055
3528.379744	748067.933286	42.523060
3527.965501	747461.674054	42.528064
3528.203541	746870.474172	42.533069
3527.798803	746284.181538	42.538074
3528.047920	745690.271184	42.543079
3528.129916	745103.806608	42.548084
3528.105041	744507.134828	42.553088
3528.092028	743921.289629	42.558093
3528.109663	743340.387942	42.563098
3528.106367	742742.441024	42.568103
3527.826315	742161.305089	42.573108
3527.860502	741570.381759	42.578112
3527.799986	740977.650158	42.583117
3527.816099	740400.042089	42.588122
3527.832775	739810.127123	42.593127
3527.717393	739233.445260	42.598132
3527.879320	738645.001230	42.603136
3527.880051	738056.343172	42.608141
3527.748987	737475.282079	42.613146
3528.090455	736872.676439	42.618151
3527.728063	736291.964157	42.623156
3527.647555	735696.812416	42.628160
3527.832922	735114.090111	42.633165
3527.390475	734522.475419	42.638170
3527.637662	733938.370246	42.643175
3527.715713	733358.557349	42.648180
3527.786440	732778.060347	42.653184
3527.670982	732191.365572	42.658189
3527.221923	731603.892901	42.663194
3527.505054	731011.796651	42.668199
3527.385635	730441.907002	42.673204
3527.274937	729857.170593	42.678208
3527.886691	729283.212275	42.683213
3527.427550	728699.244049	42.688218
3527.647782	728105.262129	42.693223
3527.556329	727528.674911	42.698228
3527.250008	726944.851690	42.703232
3527.249665	726357.516370	42.708237
3527.059959	725778.295708	42.713242
3527.436556	725194.131571	42.718247
3527.515686	724620.876924	42.723252
3527.322906	724035.191374	42.728256
3527.232179	723456.532860	42.733261
3527.176728	722880.057678	42.738266
3527.441857	722293.971635	42.743271
3527.095713	721718.802953	42.748276
3526.961472	721129.183230	42.753280
3527.143860	720539.863962	42.758285
3526.808850	719964.521715	42.763290
3526.987255	719394.654261	42.768295
3526.937200	718821.464693	42.773300
3526.732045	718243.749799	42.778304
3526.902270	717670.244953	42.783309
3526.738586	717095.468257	42.788314
3526.962824	716518.006776	42.793319
3526.857028	715941.256138	42.798324
3526.876510	715355.317495	42.803329
3527.251404	714780.934644	42.808333
3526.901689	714216.111599	42.813338
3526.572839	713627.532136	42.818343
3526.583614	713055.772674	42.823348
3526.551337	712494.600364	42.828353
3526.836623	711925.099148	42.833357
3526.378722	711350.128318	42.838362
3526.772382	710776.759715	42.843367
3526.575194	710215.464374	42.848372
3526.683966	709636.260294	42.853377
3526.694726	709066.167176	42.858381
3526.323873	708496.746393	42.863386
3526.454607	707921.244396	42.868391
3526.390839	707357.404459	42.873396
3526.349833	706781.656432	42.878401
3526.316902	706213.962266	42.883405
3526.332179	705646.520241	42.888410
3526.520581	705067.737724	42.893415
3526.531951	704505.236945	42.898420
3526.367741	703941.437999	42.903425
3526.576533	703363.828887	42.908429
3526.227862	702800.086209	42.913434
3526.239255	702236.245305	42.918439
3526.040346	701669.074882	42.923444
3526.028881	701097.661776	42.928449
3526.375118	700528.087874	42.933453
3526.043630	699969.077408	42.938458
3526.271557	699405.015727	42.943463
3526.102641	698832.983869	42.948468
3525.954408	698271.497483	42.953473
3526.025907	697709.191968	42.958477
3525.949513	697147.820062	42.963482
3525.599271	696576.665861	42.968487
3525.616867	696016.199770	42.973492
3525.489899	695467.654879	42.978497
3525.845180	694905.320308	42.983501
3525.652654	694350.750627	42.988506
3525.496931	693787.537077	42.993511
3525.612753	693241.845786	42.998516
3525.521838	692684.817015	43.003521
3525.602344	692127.525061	43.008525
3525.627858	691571.102855	43.013530
3525.335671	691019.326149	43.018535
3525.368585	690464.126811	43.023540
3525.326270	689915.920341	43.028545
3525.256436	689355.097738	43.033549
3525.108047	688807.289178	43.038554
3525.246091	688253.128730	43.043559
3525.443266	687707.532619	43.048564
3525.215863	687159.039799	43.053569
3525.490465	686597.886545	43.058573
3525.061690	686062.002116	43.063578
3525.306841	685508.500467	43.068583
3525.397207	684951.656349	43.073588
3525.315304	684401.278680	43.078593
3525.561433	683851.857013	43.083597
3524.868181	683304.454307	43.088602
3524.922592	682750.069993	43.093607
3524.896419	682211.449491	43.098612
3524.838639	681663.789819	43.103617
3525.310344	681121.036405	43.108621
3525.161616	680577.360698	43.113626
3525.259793	680017.524153	43.118631
3524.800363	679474.782313	43.123636
3524.941700	678925.131785	43.128641
3524.906076	678381.206994	43.133645
3525.005091	677843.005614	43.138650
3524.943607	677293.441756	43.143655
3524.971022	676743.979472	43.148660
3524.662065	676212.428691	43.153665
3524.824069	675660.587211	43.158669
3524.728889	675121.513179	43.163674
3524.634681	674585.547130	43.168679
3524.299934	674039.424850	43.173684
3524.219015	673501.649869	43.178689
3524.504432	672966.323232	43.183693
3524.091057	672440.206655	43.188698
3524.239212	671899.209974	43.193703
3524.540763	671365.284358	43.198708
3524.223463	670832.979433	43.203713
3524.433462	670297.413430	43.208717
3523.878066	669761.399171	43.213722
3524.063548	669235.499265	43.218727
3524.157884	668704.399779	43.223732
3524.056501	668178.340366	43.228737
3524.360819	667650.038055	43.233741
3524.183450	667124.930461	43.238746
3524.457552	666582.210654	43.243751
3524.853945	666048.865855	43.248756
3524.189874	665509.038108	43.253761
3524.202018	664965.722131	43.258765
3523.989357	664438.476934	43.263770
3524.193820	663908.686873	43.268775
3523.992559	663375.294661	43.273780
3523.766816	662847.265531	43.278785
3523.955621	662325.822781	43.283789
3523.859356	661806.745700	43.288794
3524.108537	661271.363322	43.293799
3524.057348	660750.075781	43.298804
3523.697195	660217.633442	43.303809
3524.006595	659690.138350	43.308813
3523.683453	659162.472940	43.313818
3523.945659	658621.750566	43.318823
3523.667005	658117.631067	43.323828
3523.703466	657591.466172	43.328833
3523.815412	657059.219117	43.333837
3523.509611	656537.349203	43.338842
3523.500992	656006.862686	43.343847
3523.936645	655499.090590	43.348852
3523.398861	654967.539552	43.353857
3523.692468	654442.709137	43.358861
3523.616816	653934.294114	43.363866
3523.650469	653407.155524	43.368871
3523.500527	652893.854964	43.373876
3523.530321	652371.256598	43.378881
3523.507999	651846.491592	43.383885
3523.523417	651334.879988	43.388890
3523.447488	650808.570496	43.393895
3523.393180	650276.983721	43.398900
3523.466371	649771.076789	43.403905
3523.433529	649249.823342	43.408909
3523.206441	648731.723665	43.413914
3523.176824	648223.906945	43.418919
3523.336349	647701.040651	43.423924
3523.150958	647189.450106	43.428929
3523.108152	646666.614303	43.433933
3523.019875	646162.951070	43.438938
3522.996114	645637.759390	43.443943
3522.895348	645134.046745	43.448948
3522.546264	644632.000877	43.453953
3522.828384	644123.923515	43.458957
3522.829961	643617.268280	43.463962
3522.996996	643103.310240	43.468967
3522.777489	642600.241461	43.473972
3522.541872	642097.050491	43.478977
3522.612208	641584.032002	43.483981
3522.622054	641091.349756	43.488986
3522.530989	640589.959745	43.493991
3522.405650	640066.896934	43.498996
3522.263217	639570.716633	43.504001
3522.456815	639068.203131	43.509005
3522.181919	638568.595929	43.514010
3522.504635	638064.110563	43.519015
3522.247829	637572.755001	43.524020
3522.173071	637077.743180	43.529025
3522.573944	636570.970248	43.534029
3522.311588	636079.194251	43.539034
3522.034914	635578.691882	43.544039
3522.158620	635085.902188	43.549044
3522.060009	634603.484458	43.554049
3522.441873	634095.742999	43.559053
3522.330034	633612.430856	43.564058
3522.495484	633108.080914	43.569063
3522.070835	632616.869184	43.574068
3521.749776	632123.764884	43.579073
3521.856739	631627.561239	43.584077
3522.053722	631149.037288	43.589082
3521.718077	630655.465901	43.594087
3522.471504	630164.738856	43.599092
3521.994469	629673.748462	43.604097
3522.355755	629182.792288	43.609101
3522.260527	628692.642164	43.614106
3522.407262	628191.463421	43.619111
3522.019792	627697.912529	43.624116
3521.610616	627214.356563	43.629121
3521.768642	626717.662615	43.634125
3521.523828	626233.032402	43.639130
3521.602362	625752.431295	43.644135
3521.524662	625275.641276	43.649140
3521.424630	624791.471628	43.654145
3521.297103	624310.690490	43.659149
3521.349465	623839.323468	43.664154
3521.604682	623354.677520	43.669159
3521.337774	622876.710895	43.674164
3520.989149	622399.237887	43.679169
3521.547652	621922.841202	43.684173
3521.195315	621444.124155	43.689178
3521.125004	620966.289614	43.694183
3521.286538	620489.145890	43.699188
3521.383631	620019.357523	43.704193
3521.649828	619535.740504	43.709197
3521.172787	619064.104696	43.714202
3520.984589	618585.634060	43.719207
3521.103482	618116.511291	43.724212
3520.763631	617646.694908	43.729217
3520.935711	617175.818647	43.734221
3520.709185	616707.997345	43.739226
3520.726939	616246.880812	43.744231
3520.824238	615788.889113	43.749236
3520.763758	615314.814686	43.754241
3520.857359	614849.014823	43.759245
3520.843727	614388.026082	43.764250
3521.331324	613919.613103	43.769255
3521.237763	613451.830946	43.774260
3520.769438	612989.257068	43.779265
3521.135684	612508.772126	43.784269
3520.676661	612055.333081	43.789274
3520.374867	611579.885910	43.794279
3520.692981	611110.179564	43.799284
3520.655623	610656.360692	43.804289
3520.604224	610194.050461	43.809293
3520.465409	609730.732964	43.814298
3520.694160	609263.622122	43.819303
3520.666722	608811.130851	43.824308
3520.408130	608353.644992	43.829313
3520.769140	607894.830852	43.834317
3520.439288	607443.590051	43.839322
3520.494214	606976.213005	43.844327
3520.464346	606514.650304	43.849332
3520.068376	606059.251725	43.854337
3520.313216	605605.380989	43.859341
3520.172329	605152.410829	43.864346
3519.978414	604702.592574	43.869351
3520.205808	604251.931911	43.874356
3520.029869	603800.720101	43.879361
3520.089246	603340.668715	43.884365
3520.249391	602904.568547	43.889370
3519.793185	602447.228777	43.894375
3519.857214	602004.335795	43.899380
3519.940106	601553.141449	43.904385
3519.737127	601105.290672	43.909389
3520.132808	600665.902993	43.914394
3520.314249	600211.928720	43.919399
3520.023154	599755.306643	43.924404
3519.568273	599321.484173	43.929409
3519.703250	598878.709556	43.934413
3519.475116	598440.196889	43.939418
3519.460037	598001.380203	43.944423
3519.865685	597556.701455	43.949428
3519.753486	597126.352918	43.954433
3519.821860	596674.920013	43.959437
3519.570033	596234.369838	43.964442
3519.513536	595791.259003	43.969447
3519.687114	595358.034582	43.974452
3519.156429	594927.877117	43.979457
3519.468058	594486.311072	43.984461
3519.714538	594049.912207	43.989466
3519.759031	593600.976024	43.994471
3519.457421	593166.194772	43.999476
3519.081505	592731.811938	44.004481
3519.045478	592302.176923	44.009485
3518.960595	591866.105197	44.014490
3519.025316	591439.184197	44.019495
3519.326988	591015.321797	44.024500
3518.975962	590584.773925	44.029505
3519.263130	590152.795293	44.034509
3518.864326	589732.824659	44.039514
3518.608980	589306.785829	44.044519
3518.927707	588881.940039	44.049524
3518.918343	588465.224432	44.054529
3518.895580	588039.703542	44.059533
3518.516379	587622.418730	44.064538
3518.502525	587200.735543	44.069543
3519.027118	586782.211916	44.074548
3518.561310	586364.998616	44.079553
3518.817342	585934.078823	44.084557
3518.743433	585518.678931	44.089562
3518.824843	585104.092592	44.094567
3518.592680	584677.935510	44.099572
3518.278252	584264.242341	44.104577
3518.642202	583842.829432	44.109581
3518.645621	583436.844554	44.114586
3518.547826	583022.971489	44.119591
3518.635560	582592.262955	44.124596
3518.316406	582188.352448	44.129601
3518.440106	581771.181687	44.134605
3518.477099	581359.792940	44.139610
3518.314388	580948.776365	44.144615
3518.340820	580535.400940	44.149620
3518.263408	580129.571106	44.154625
3518.348845	579713.794801	44.159629
3518.123339	579314.198062	44.164634
3517.960713	578907.638451	44.169639
3518.396215	578499.153022	44.174644
3518.060351	578094.406433	44.179649
3518.538578	577673.515770	44.184653
3518.380528	577283.245689	44.189658
3518.326088	576871.068613	44.194663
3518.490597	576458.790158	44.199668
3517.846732	576053.677379	44.204673
3518.043362	575649.313234	44.209677
3518.170687	575249.877050	44.214682
3517.851358	574849.196523	44.219687
3518.147384	574430.943333	44.224692
3517.672143	574039.518987	44.229697
3517.891351	573634.632993	44.234701
3517.871039	573232.239842	44.239706
3517.918889	572832.538799	44.244711
3517.949560	572431.067129	44.249716
3517.584995	572042.026751	44.254721
3517.732209	571641.566551	44.259725
3517.515358	571241.960833	44.264730
3517.460027	570842.264581	44.269735
3517.871104	570459.332520	44.274740
3517.452283	570060.277450	44.279745
3517.531005	569671.692257	44.284749
3517.314663	569275.899126	44.289754
3517.268989	568887.411837	44.294759
3517.631416	568493.156235	44.299764
3517.414136	568104.674383	44.304769
3517.573870	567711.083479	44.309773
3517.184436	567323.110538	44.314778
3516.772213	566934.676742	44.319783
3517.261760	566555.489508	44.324788
3517.169764	566165.568417	44.329793
3517.016747	565785.360797	44.334797
3517.178135	565407.252781	44.339802
3516.782009	565024.849356	44.344807
3517.229463	564645.663385	44.349812
3516.664138	564275.650440	44.354817
3517.123499	563886.271067	44.359821
3517.224810	563512.850162	44.364826
3517.054148	563127.331439	44.369831
3517.519954	562748.791668	44.374836
3517.000223	562366.280495	44.379841
3517.124135	561983.144677	44.384845
3516.904817	561599.401622	44.389850
3516.955672	561230.153426	44.394855
3516.862538	560848.834115	44.399860
3516.820071	560476.106051	44.404865
3516.738241	560099.244736	44.409869
3516.594563	559724.196104	44.414874
3516.573910	559341.964489	44.419879
3516.785099	558975.395294	44.424884
3516.676327	558607.309250	44.429889
3516.568893	558235.233847	44.434893
3516.642756	557874.953186	44.439898
3516.322457	557501.634306	44.444903
3516.904632	557127.949334	44.449908
3516.652619	556767.593448	44.454913
3516.641088	556389.203807	44.459917
3516.795631	556015.258306	44.464922
3516.463906	555649.445350	44.469927
3516.326660	555274.470994	44.474932
3516.254109	554908.089686	44.479937
3516.606282	554550.945987	44.484941
3516.672927	554186.234032	44.489946
3516.327306	553821.532158	44.494951
3516.464923	553451.649135	44.499956
3516.163204	553087.474036	44.504961
3516.183597	552723.183691	44.509965
3516.220677	552366.640316	44.514970
3516.228092	552008.933638	44.519975
3516.281232	551646.372221	44.524980
3515.805859	551284.344842	44.529985
3515.921921	550928.808259	44.534989
3515.670375	550572.014867	44.539994
3515.761424	550218.076537	44.544999
3515.960084	549860.028475	44.550004
3515.697165	549519.487543	44.555009
3515.666599	549168.969753	44.560013
3515.719599	548814.799840	44.565018
3515.659372	548464.420222	44.570023
3515.955092	548113.668433	44.575028
3515.557895	547768.268039	44.580033
3515.589525	547420.315838	44.585037
3515.609395	547066.963265	44.590042
3515.407623	546720.444582	44.595047
3515.581633	546377.835371	44.600052
3515.535846	546027.491893	44.605057
3515.590584	545681.155327	44.610061
3515.620226	545344.392911	44.615066
3515.262397	545014.242350	44.620071
3515.336162	544658.046062	44.625076
3515.131277	544325.080088	44.630081
3515.570103	543981.509204	44.635085
3515.344322	543638.345823	44.640090
3515.219517	543296.871045	44.645095
3515.268065	542957.627291	44.650100
3515.173728	542624.601747	44.655105
3515.159891	542283.083204	44.660109
3515.360326	541950.798066	44.665114
3515.075022	541618.033283	44.670119
3515.252274	541273.129305	44.675124
3515.516191	540948.323359	44.680129
3515.408245	540600.930105	44.685133
3515.302227	540266.640202	44.690138
3515.192597	539930.628264	44.695143
3515.356002	539591.989561	44.700148
3514.978215	539262.009151	44.705153
3515.134810	538920.934636	44.710157
3514.904811	538582.540676	44.715162
3514.445078	538266.522299	44.720167
3514.792001	537937.597830	44.725172
3514.968263	537604.659591	44.730177
3514.968984	537275.425830	44.735181
3515.154794	536947.968825	44.740186
3514.928251	536626.577627	44.745191
3514.903492	536293.441308	44.750196
3514.956236	535974.661391	44.755201
3514.998821	535638.572399	44.760205
3514.919268	535305.069296	44.765210
3514.476565	534986.150188	44.770215
3514.626875	534650.675521	44.775220
3514.162420	534338.556725	44.780225
3514.191338	534008.788982	44.785229
3514.202946	533703.941422	44.790234
3514.174328	533390.062663	44.795239
3514.478054	533078.189087	44.800244
3514.120825	532754.362123	44.805249
3513.981637	532442.550480	44.810253
3514.299508	532129.190743	44.815258
3514.526322	531819.069331	44.820263
3514.194322	531501.820567	44.825268
3514.103563	531200.672077	44.830273
3514.459168	530874.612498	44.835277
3514.743905	530560.770482	44.840282
3514.719057	530252.626883	44.845287
3514.767925	529917.160994	44.850292
3514.623553	529603.068891	44.855297
3514.290986	529280.472717	44.860301
3514.167836	528977.719411	44.865306
3514.194573	528666.303500	44.870311
3514.478091	528346.458560	44.875316
3513.966369	528041.884826	44.880321
3513.889848	527729.962009	44.885325
3514.114934	527417.880154	44.890330
3513.727824	527104.028565	44.895335
3514.203270	526797.493908	44.900340
3513.826480	526499.074236	44.905345
3513.983895	526185.211175	44.910349
3513.952657	525889.698625	44.915354
3513.948191	525585.997406	44.920359
3513.882127	525276.545341	44.925364
3513.765029	524980.978934	44.930369
3513.706489	524674.188791	44.935373
3513.911137	524379.666241	44.940378
3513.234217	524079.835712	44.945383
3513.726398	523782.273524	44.950388
3513.366639	523483.891588	44.955393
3513.464928	523195.523707	44.960397
3513.540847	522896.904248	44.965402
3513.556058	522602.631624	44.970407
3513.965348	522302.479163	44.975412
3513.944783	522009.766389	44.980417
3513.622527	521702.960589	44.985421
3513.805012	521402.778478	44.990426
3513.642179	521113.405439	44.995431
3513.705359	520814.140996	45.000436
3513.694766	520505.995258	45.005441
3513.713273	520214.251108	45.010445
3513.577786	519917.780476	45.015450
3513.386886	519639.545064	45.020455
3513.274891	519333.968547	45.025460
3512.964372	519043.722768	45.030465
3513.147102	518758.538842	45.035469
3513.087148	518467.633273	45.040474
3512.860739	518188.922940	45.045479
3513.097263	517894.824402	45.050484
3512.883819	517619.687620	45.055489
3513.323573	517336.807310	45.060493
3513.119669	517060.295107	45.065498
3513.488295	516774.335415	45.070503
3513.184478	516487.020354	45.075508
3512.836773	516209.961804	45.080513
3512.856959	515920.257225	45.085517
3513.066740	515634.960257	45.090522
3512.689767	515355.163528	45.095527
3512.675948	515082.321716	45.100532
3512.620583	514812.917472	45.105537
3512.944290	514532.885244	45.110541
3512.891833	514259.075703	45.115546
3512.584347	513978.636072	45.120551
3512.653599	513702.876164	45.125556
3512.431094	513428.070616	45.130561
3512.718605	513154.486777	45.135565
3512.862739	512881.023686	45.140570
3512.487540	512615.223362	45.145575
3512.900122	512337.864997	45.150580
3512.702285	512070.155665	45.155585
3512.630846	511791.101824	45.160589
3512.751941	511515.597740	45.165594
3512.040960	511249.124220	45.170599
3512.731096	510973.361905	45.175604
3512.416510	510700.090794	45.180609
3512.043417	510445.168342	45.185613
3512.629994	510186.035236	45.190618
3512.297411	509922.051926	45.195623
3512.292295	509647.800180	45.200628
3512.154281	509395.397993	45.205633
3512.149234	509139.027212	45.210637
3512.006155	508867.160778	45.215642
3512.288575	508602.595688	45.220647
3512.322263	508337.563282	45.225652
3512.036617	508075.057471	45.230657
3512.132153	507826.835929	45.235661
3512.375311	507559.632123	45.240666
3512.184326	507296.591947	45.245671
3512.257141	507032.440994	45.250676
3511.866258	506778.979187	45.255681
3512.296013	506524.311809	45.260685
3512.145557	506264.280500	45.265690
3511.634829	506006.682201	45.270695
3511.935365	505755.866283	45.275700
3512.154411	505513.097569	45.280705
3511.860797	505250.900770	45.285709
3511.827024	504994.569697	45.290714
3511.888108	504746.559240	45.295719
3511.950467	504490.405971	45.300724
3511.782230	504247.836049	45.305729
3511.649197	503988.877292	45.310733
3511.849486	503734.963436	45.315738
3511.498433	503493.424539	45.320743
3511.842530	503240.691728	45.325748
3512.002358	503004.922785	45.330753
3511.739580	502749.960405	45.335757
3511.904324	502490.067502	45.340762
3511.663046	502241.767140	45.345767
3511.923162	502000.202903	45.350772
3511.830836	501753.790959	45.355777
3511.567493	501493.803655	45.360781
3511.719080	501249.921099	45.365786
3511.561466	501008.919208	45.370791
3511.579175	500751.754225	45.375796
3511.349559	500512.274247	45.380801
3511.068772	500275.125497	45.385805
3511.121895	500034.275622	45.390810
3511.235987	499796.850316	45.395815
3511.329215	499563.571637	45.400820
3511.441550	499321.942775	45.405825
3511.308841	499081.464730	45.410829
3511.529375	498839.709228	45.415834
3511.232349	498603.297825	45.420839
3511.205116	498363.549915	45.425844
3510.760542	498136.209161	45.430849
3510.704861	497909.810336	45.435853
3510.996220	497684.664064	45.440858
3510.821339	497454.789913	45.445863
3511.052331	497217.459511	45.450868
3510.561887	496993.904059	45.455873
3510.659311	496773.886659	45.460877
3510.921946	496547.465598	45.465882
3510.508463	496326.973230	45.470887
3510.834586	496091.330233	45.475892
3510.959593	495875.949456	45.480897
3510.885946	495656.502974	45.485901
3511.055021	495426.339962	45.490906
3510.983540	495201.323456	45.495911
3511.262490	494961.626304	45.500916
3510.816191	494739.196666	45.505921
3511.063487	494512.801437	45.510925
3511.178674	494271.756748	45.515930
3511.226919	494046.148005	45.520935
3511.059207	493813.592527	45.525940
3510.715108	493589.663392	45.530945
3510.684501	493360.265132	45.535949
3510.748024	493135.703973	45.540954
3510.348281	492917.289365	45.545959
3510.367301	492692.477023	45.550964
3510.497589	492479.885036	45.555969
3510.782142	492262.104012	45.560973
3510.859880	492038.891874	45.565978
3510.570239	491823.024514	45.570983
3510.611295	491599.155230	45.575988
3510.775930	491389.123941	45.580993
3510.634242	491165.533152	45.585997
3510.518786	490946.336527	45.591002
3510.319746	490722.345017	45.596007
3510.809316	490510.426143	45.601012
3510.567795	490291.293287	45.606017
3510.473369	490075.218832	45.611021
3510.807938	489854.565393	45.616026
3510.690585	489635.301807	45.621031
3510.563964	489409.155814	45.626036
3510.262222	489199.531632	45.631041
3510.499871	488985.461354	45.636045
3510.446954	488762.077232	45.641050
3510.279538	488565.375782	45.646055
3510.283182	488338.687578	45.651060
3510.314339	488136.684942	45.656065
3509.879989	487929.851105	45.661069
3510.354241	487712.688658	45.666074
3510.128130	487512.392573	45.671079
3510.212813	487302.527712	45.676084
3510.280215	487093.017506	45.681089
3510.378189	486889.825126	45.686093
3510.303987	486676.133933	45.691098
3509.924181	486470.690432	45.696103
3510.131205	486260.842789	45.701108
3510.313766	486057.980560	45.706113
3509.865771	485851.883562	45.711117
3510.510652	485645.597540	45.716122
3509.945998	485441.337535	45.721127
3510.128161	485231.886721	45.726132
3509.945758	485024.874327	45.731137
3509.945755	484817.119814	45.736141
3509.967123	484620.797291	45.741146
3509.919771	484422.662305	45.746151
3510.082259	484211.633789	45.751156
3510.037374	484015.973823	45.756161
3509.830108	483810.672285	45.761165
3509.853120	483611.858241	45.766170
3509.938776	483411.310383	45.771175
3509.927363	483203.842578	45.776180
3509.899809	483014.293028	45.781185
3510.092004	482820.047256	45.786189
3510.179412	482610.632252	45.791194
3509.916975	482413.726376	45.796199
3509.981705	482197.477062	45.801204
3509.886803	481997.500916	45.806209
3509.817910	481814.677930	45.811213
3510.024349	481602.446741	45.816218
3509.990054	481408.072431	45.821223
3509.910792	481204.996936	45.826228
3510.005867	481011.102442	45.831233
3509.824294	480816.898740	45.836237
3510.062519	480611.433723	45.841242
3509.837988	480416.929302	45.846247
3509.525924	480222.640220	45.851252
3509.595717	480030.106306	45.856257
3509.736247	479841.557598	45.861261
3509.674954	479640.030739	45.866266
3509.496184	479449.102451	45.871271
3509.340802	479255.434340	45.876276
3509.595691	479068.528709	45.881281
3509.451889	478873.335736	45.886285
3509.295679	478683.863718	45.891290
3509.322870	478510.761965	45.896295
3509.372333	478308.492591	45.901300
3509.711021	478127.030872	45.906305
3509.476468	477940.197203	45.911309
3509.697781	477742.043839	45.916314
3509.117118	477565.340866	45.921319
3509.249516	477376.362897	45.926324
3509.518325	477197.789854	45.931329
3509.653513	477001.314010	45.936333
3509.543931	476816.067735	45.941338
3509.081850	476628.398735	45.946343
3509.349279	476440.147544	45.951348
3509.441204	476264.431107	45.956353
3509.318385	476085.509019	45.961357
3509.252716	475889.308732	45.966362
3509.011058	475710.302011	45.971367
3509.196976	475523.928887	45.976372
3509.175401	475350.501741	45.981377
3509.065485	475168.378404	45.986381
3508.930660	474992.283441	45.991386
3509.026215	474819.894707	45.996391
3509.145975	474632.409831	46.001396
3509.085616	474461.512909	46.006401
3509.146739	474283.098961	46.011405
3509.239645	474095.106833	46.016410
3508.960142	473918.519953	46.021415
3509.042296	473741.261943	46.026420
3508.875169	473567.032677	46.031425
3508.925651	473390.029936	46.036429
3508.919258	473206.350369	46.041434
3508.530215	473041.421711	46.046439
3508.797157	472866.655984	46.051444
3508.616839	472699.662912	46.056449
3508.460344	472540.058399	46.061453
3508.494560	472367.758684	46.066458
3508.450350	472204.435039	46.071463
3508.553448	472027.157160	46.076468
3508.788387	471867.530719	46.081473
3508.846240	471703.881404	46.086477
3508.790392	471527.132407	46.091482
3508.551821	471366.670903	46.096487
3508.229633	471199.840625	46.101492
3508.507335	471030.019458	46.106497
3508.303044	470870.256946	46.111501
3508.697441	470705.072647	46.116506
3508.123562	470536.101528	46.121511
3508.167432	470386.118647	46.126516
3508.253471	470220.628205	46.131521
3508.432887	470066.010406	46.136525
3508.307378	469904.250862	46.141530
3508.284277	469749.158535	46.146535
3508.424094	469589.478387	46.151540
3508.518633	469424.840629	46.156545
3508.284293	469260.916094	46.161549
3508.561041	469102.018918	46.166554
3507.995035	468942.048609	46.171559
3508.193927	468784.073847	46.176564
3508.103766	468626.299094	46.181569
3508.178155	468487.288148	46.186573
3508.057963	468323.032102	46.191578
3508.155700	468179.050636	46.196583
3508.309845	468013.681300	46.201588
3508.321359	467863.684020	46.206593
3507.935007	467703.520663	46.211597
3508.146373	467541.683506	46.216602
3507.939280	467396.633718	46.221607
3507.705026	467245.660388	46.226612
3507.708071	467111.109589	46.231617
3507.886961	466958.594338	46.236621
3507.989288	466810.599687	46.241626
3507.902481	466662.129587	46.246631
3508.069939	466505.357220	46.251636
3508.520335	466356.995682	46.256641
3508.144882	466207.456813	46.261645
3508.160015	466045.437908	46.266650
3507.604617	465900.790933	46.271655
3507.826918	465748.866633	46.276660
3507.772538	465603.574591	46.281665
3507.509969	465464.447290	46.286669
3507.789759	465312.053769	46.291674
3507.545798	465176.771677	46.296679
3507.525471	465030.557560	46.301684
3507.436274	464894.537765	46.306689
3507.343848	464753.603028	46.311693
3507.641531	464612.347328	46.316698
3507.353081	464478.435933	46.321703
3507.739179	464333.008486	46.326708
3507.906879	464193.849264	46.331713
3507.548936	464058.325503	46.336717
3507.679740	463904.781030	46.341722
3507.704189	463775.726126	46.346727
3507.629215	463631.233521	46.351732
3507.518088	463493.788963	46.356737
3507.655552	463356.959687	46.361741
3507.578829	463217.733896	46.366746
3507.393717	463080.907098	46.371751
3507.352432	462935.390199	46.376756
3507.726042	462799.074071	46.381761
3507.367713	462672.965458	46.386765
3507.381796	462526.270640	46.391770
3507.093362	462401.820496	46.396775
3507.406481	462276.405428	46.401780
3507.399180	462144.456895	46.406785
3507.290285	462006.900177	46.411789
3507.187042	461867.973365	46.416794
3507.347498	461739.135184	46.421799
3507.659903	461604.341414	46.426804
3507.642035	461468.133575	46.431809
3507.455828	461332.967023	46.436813
3507.698590	461200.057329	46.441818
3507.617508	461068.418234	46.446823
3507.409645	460942.526212	46.451828
3507.282206	460793.511592	46.456833
3507.305106	460674.977101	46.461837
3507.638082	460536.473193	46.466842
3507.248433	460405.845227	46.471847
3507.070710	460268.288149	46.476852
3507.438775	460143.965050	46.481857
3507.261792	460021.305245	46.486861
3507.401032	459877.863418	46.491866
3507.081139	459763.486926	46.496871
3506.986522	459637.972710	46.501876
3506.986002	459506.866957	46.506881
3507.291937	459379.255559	46.511885
3507.074767	459247.526263	46.516890
3506.708530	459130.468031	46.521895
3507.053684	459000.972363	46.526900
3507.347780	458874.626765	46.531905
3507.085327	458756.585690	46.536909
3507.222035	458625.805483	46.541914
3507.237666	458505.536155	46.546919
3506.573560	458388.321709	46.551924
3507.000452	458265.091855	46.556929
3506.725586	458143.957680	46.561933
3507.090405	458012.779745	46.566938
3506.812553	457898.131977	46.571943
3506.904653	457769.229068	46.576948
3506.788159	457652.018179	46.581953
3506.743228	457544.069535	46.586957
3506.982464	457408.651656	46.591962
3506.700209	457298.714851	46.596967
3506.722441	457183.809033	46.601972
3506.704408	457077.931372	46.606977
3506.621816	456956.757213	46.611981
3506.851565	456830.156314	46.616986
3506.850362	456718.394357	46.621991
3506.754463	456596.460018	46.626996
3506.910798	456479.094350	46.632001
3506.694093	456366.606946	46.637005
3506.956383	456245.623068	46.642010
3506.463103	456133.739153	46.647015
3506.741992	456016.045750	46.652020
3506.523071	455908.878389	46.657025
3506.255772	455803.746251	46.662029
3506.326301	455687.911299	46.667034
3506.476497	455593.249992	46.672039
3506.521802	455476.404366	46.677044
3506.530207	455372.642213	46.682049
3506.409766	455256.837412	46.687053
3506.665726	455140.866301	46.692058
3506.821245	455041.081839	46.697063
3506.819049	454917.093803	46.702068
3507.148340	454805.416951	46.707073
3506.666825	454689.112978	46.712077
3506.730929	454571.245131	46.717082
3506.465340	454470.059732	46.722087
3506.526770	454352.647304	46.727092
3506.733833	454239.822318	46.732097
3506.391284	454137.229033	46.737101
3506.650393	454025.965445	46.742106
3506.589701	453925.553448	46.747111
3506.708984	453813.653575	46.752116
3506.725121	453689.350806	46.757121
3506.188953	453592.110665	46.762125
3506.372025	453471.174549	46.767130
3506.255815	453363.672118	46.772135
3506.462622	453262.349398	46.777140
3506.487675	453156.900241	46.782145
3506.437109	453063.376790	46.787149
3506.291470	452952.734144	46.792154
3506.250092	452854.442816	46.797159
3506.059834	452747.659548	46.802164
3506.224723	452644.465202	46.807169
3506.063004	452546.091560	46.812173
3506.243756	452437.823842	46.817178
3506.326123	452336.416426	46.822183
3506.320892	452239.586204	46.827188
3506.772362	452130.104617	46.832193
3506.624083	452023.462528	46.837197
3507.009835	451911.557523	46.842202
3506.039458	451806.626323	46.847207
3506.162820	451706.526971	46.852212
3506.636649	451603.376077	46.857217
3506.171856	451501.956604	46.862221
3506.305202	451394.249212	46.867226
3506.294024	451295.641126	46.872231
3506.206947	451198.921416	46.877236
3506.454854	451085.666607	46.882241
3506.423314	450992.738945	46.887245
3506.397466	450881.050769	46.892250
3506.345468	450789.697405	46.897255
3506.360719	450681.448781	46.902260
3506.202319	450581.645629	46.907265
3505.940840	450488.298668	46.912269
3506.187101	450385.383401	46.917274
3506.158984	450288.902906	46.922279
3505.995467	450190.315599	46.927284
3506.066097	450090.673800	46.932289
3506.041876	449992.213881	46.937293
3506.297817	449895.226743	46.942298
3506.136525	449793.595020	46.947303
3506.200944	449697.805839	46.952308
3505.980799	449592.177631	46.957313
3505.783089	449503.226587	46.962317
3506.377145	449406.534380	46.967322
3506.520716	449318.639767	46.972327
3506.014233	449230.703669	46.977332
3506.468475	449128.456576	46.982337
3506.083008	449032.386244	46.987341
3506.148382	448925.996062	46.992346
3505.824732	448832.703043	46.997351
3505.403777	448746.271473	47.002356
3505.712550	448649.979440	47.007361
3505.803257	448567.972585	47.012365
3506.021020	448471.948810	47.017370
3505.776322	448383.254581	47.022375
3505.821730	448298.617679	47.027380
3505.888921	448197.649118	47.032385
3505.736132	448105.692789	47.037389
3505.600882	448014.950041	47.042394
3505.321997	447928.693690	47.047399
3505.386997	447843.138883	47.052404
3505.572041	447766.284992	47.057409
3505.104763	447698.720366	47.062413
3505.561655	447610.105927	47.067418
3505.339188	447527.286467	47.072423
3505.146736	447449.988802	47.077428
3505.427431	447374.334164	47.082433
3505.038287	447293.976277	47.087437
3505.271538	447207.173157	47.092442
3505.559307	447137.145190	47.097447
3505.553967	447060.422669	47.102452
3505.486130	446972.148713	47.107457
3505.292698	446901.238649	47.112461
3505.359546	446809.289902	47.117466
3505.546645	446733.243283	47.122471
3505.180684	446648.162929	47.127476
3505.385373	446567.041657	47.132481
3505.123788	446490.208700	47.137485
3505.679871	446405.274202	47.142490
3505.212980	446337.451621	47.147495
3505.109021	446265.662070	47.152500
3505.380927	446188.939780	47.157505
3505.430267	446111.748099	47.162509
3505.271798	446024.804201	47.167514
3505.294257	445955.324774	47.172519
3505.111110	445874.064243	47.177524
3505.301381	445795.173845	47.182529
3505.391329	445719.545904	47.187533
3505.413041	445647.276402	47.192538
3505.449247	445577.235558	47.197543
3505.168595	445500.199443	47.202548
3505.289426	445417.008880	47.207553
3505.211914	445350.587369	47.212557
3505.333262	445266.939713	47.217562
3505.312313	445192.292410	47.222567
3505.262292	445112.984106	47.227572
3505.289664	445043.906598	47.232577
3505.247759	444967.994235	47.237581
3505.523679	444901.206698	47.242586
3505.241203	444827.262074	47.247591
3504.855477	444751.864088	47.252596
3504.957079	444664.464544	47.257601
3504.913411	444610.510916	47.262605
3504.864806	444536.576074	47.267610
3504.900517	444472.516147	47.272615
3504.977978	444410.578967	47.277620
3505.341124	444334.544490	47.282625
3505.037766	444273.280534	47.287629
3505.063971	444196.491645	47.292634
3505.062765	444132.792027	47.297639
3504.890690	444061.564614	47.302644
3505.289707	443988.058626	47.307649
3504.929462	443918.840829	47.312653
3504.933024	443854.784558	47.317658
3504.966410	443788.034987	47.322663
3504.409878	443733.456695	47.327668
3505.051693	443654.278478	47.332673
3504.756183	443593.873453	47.337677
3505.031320	443530.885642	47.342682
3505.090416	443473.564243	47.347687
3504.774881	443411.792741	47.352692
3504.857309	443337.425675	47.357697
3504.547292	443283.311338	47.362701
3504.785623	443215.612075	47.367706
3504.718423	443155.471155	47.372711
3504.864581	443088.497297	47.377716
3504.794839	443025.668346	47.382721
3504.982888	442962.237284	47.387725
3505.393735	442895.978426	47.392730
3504.753987	442828.225011	47.397735
3504.688656	442772.444593	47.402740
3504.855877	442690.554317	47.407745
3504.652746	442640.883477	47.412749
3504.545133	442574.306407	47.417754
3504.962464	442509.008948	47.422759
3504.671962	442453.113998	47.427764
3504.539312	442387.859365	47.432769
3504.226318	442332.373711	47.437773
3504.542461	442273.940121	47.442778
3504.547715	442216.472438	47.447783
3504.238350	442165.297022	47.452788
3504.892927	442104.370578	47.457793
3504.561693	442051.676992	47.462797
3504.421358	441998.392746	47.467802
3504.494348	441947.151531	47.472807
3504.458997	441905.768710	47.477812
3504.620511	441838.737667	47.482817
3504.693095	441782.880445	47.487821
3504.710493	441723.684844	47.492826
3504.607023	441664.560443	47.497831
3504.342562	441600.594020	47.502836
3504.966164	441543.120427	47.507841
3505.100227	441496.432757	47.512845
3505.033893	441436.286945	47.517850
3505.047147	441367.352308	47.522855
3504.979891	441303.047005	47.527860
3505.005084	441245.116857	47.532865
3504.965919	441179.436867	47.537869
3505.198168	441113.761059	47.542874
3505.026409	441049.574304	47.547879
3504.614482	440993.290564	47.552884
3504.644232	440924.858958	47.557889
3504.074664	440879.253877	47.562893
3504.137410	440817.055362	47.567898
3504.233140	440771.894424	47.572903
3504.590728	440719.637981	47.577908
3504.249517	440670.950007	47.582913
3504.249521	440617.841339	47.587917
3504.878596	440578.878796	47.592922
3504.706973	440514.487555	47.597927
3504.129723	440465.484355	47.602932
3504.629570	440407.876752	47.607937
3504.294201	440362.433509	47.612941
3504.656693	440308.957849	47.617946
3504.505558	440249.482698	47.622951
3504.278936	440210.564166	47.627956
3504.253855	440146.755535	47.632961
3504.052357	440106.057126	47.637965
3504.179814	440062.512544	47.642970
3504.471185	440002.707539	47.647975
3504.166881	439967.403395	47.652980
3504.372107	439899.192270	47.657985
3504.881500	439867.654955	47.662989
3504.602040	439815.302243	47.667994
3504.649933	439755.994684	47.672999
3504.715999	439699.879652	47.678004
3504.400234	439642.713683	47.683009
3504.190470	439596.232875	47.688013
3504.325424	439539.040404	47.693018
3504.641885	439501.042432	47.698023
3504.034852	439439.309491	47.703028
3504.449579	439400.178564	47.708033
3504.039514	439350.231243	47.713037
3504.218534	439296.226460	47.718042
3504.742396	439253.880793	47.723047
3504.432021	439212.083317	47.728052
3504.736326	439149.027212	47.733057
3504.566186	439113.445155	47.738061
3504.558787	439043.441489	47.743066
3504.647949	438994.828515	47.748071
3504.485337	438946.207698	47.753076
3504.548461	438893.895767	47.758081
3504.669167	438849.791940	47.763085
3504.488047	438795.543061	47.768090
3504.437969	438747.054779	47.773095
3504.135551	438692.877091	47.778100
3504.647101	438646.626230	47.783105
3504.423504	438601.819763	47.788109
3504.276439	438551.216983	47.793114
3504.559047	438494.554634	47.798119
3504.842964	438452.907899	47.803124
3504.481782	438394.275308	47.808129
3504.752437	438343.955840	47.813133
3504.259321	438284.838189	47.818138
3504.094846	438237.078550	47.823143
3504.300567	438195.901259	47.828148
3504.274050	438146.037928	47.833153
3504.250598	438102.971844	47.838157
3504.240257	438054.424539	47.843162
3504.389077	438007.929908	47.848167
3504.219001	437958.851632	47.853172
3504.228436	437911.721101	47.858177
3504.323127	437868.786585	47.863181
3504.244829	437818.271862	47.868186
3504.379044	437780.504998	47.873191
3504.102171	437729.465938	47.878196
3504.322517	437693.916399	47.883201
3504.070953	437646.373292	47.888205
3504.302593	437606.458777	47.893210
3504.410243	437558.600489	47.898215
3504.143984	437515.016683	47.903220
3504.282094	437469.385202	47.908225
3504.244518	437426.472422	47.913229
3504.323451	437376.031317	47.918234
3504.169268	437337.196844	47.923239
3504.044113	437304.394487	47.928244
3504.278358	437258.898359	47.933249
3504.205740	437216.447751	47.938253
3503.959781	437164.336742	47.943258
3504.127646	437122.656615	47.948263
3503.956145	437084.890049	47.953268
3504.365497	437039.515774	47.958273
3504.230532	437003.924346	47.963277
3504.437478	436960.563058	47.968282
3504.112505	436918.662308	47.973287
3503.982634	436874.698836	47.978292
3504.291006	436817.571244	47.983297
3504.572830	436793.475517	47.988301
3504.159306	436743.218545	47.993306
3504.362075	436696.052446	47.998311
3504.378100	436654.955449	48.003316
3504.287173	436610.173070	48.008321
3504.188505	436560.775136	48.013325
3504.434554	436520.602562	48.018330
3504.350773	436482.972207	48.023335
3503.919213	436440.429221	48.028340
3504.368795	436395.554122	48.033345
3504.130191	436354.855197	48.038349
3504.253551	436311.303993	48.043354
3504.588824	436260.816615	48.048359
3504.221512	436218.668117	48.053364
3504.103333	436165.163135	48.058369
3503.818545	436140.503908	48.063373
3504.094973	436096.469540	48.068378
3504.269238	436056.206926	48.073383
3504.072351	436022.907597	48.078388
3503.881638	435961.296892	48.083393
3504.100515	435944.313946	48.088397
3503.965047	435904.256155	48.093402
3504.276521	435850.271179	48.098407
3503.953083	435833.177809	48.103412
3503.954099	435790.306055	48.108417
3503.928313	435752.410900	48.113421
3503.744916	435722.863270	48.118426
3504.092505	435680.845375	48.123431
3503.527584	435652.732669	48.128436
3504.152040	435613.559324	48.133441
3503.630635	435580.314754	48.138445
3503.737349	435533.872935	48.143450
3504.157096	435504.780131	48.148455
3503.855207	435478.245857	48.153460
3504.060217	435428.336964	48.158465
3504.020070	435402.721901	48.163469
3503.873946	435374.232919	48.168474
3503.727165	435318.955037	48.173479
3503.554873	435298.080935	48.178484
3503.892331	435274.024826	48.183489
3503.720447	435240.111233	48.188493
3503.718192	435200.232397	48.193498
3503.556589	435170.680325	48.198503
3503.436436	435148.934653	48.203508
3503.830170	435123.295925	48.208513
3503.899908	435087.767994	48.213517
3503.845411	435049.572142	48.218522
3503.871916	435016.131712	48.223527
3503.641860	434978.828254	48.228532
3503.771423	434939.281614	48.233537
3503.889286	434922.365889	48.238541
3503.846743	434894.822633	48.243546
3504.248097	434849.140905	48.248551
3504.000638	434827.416662	48.253556
3503.773713	434782.755362	48.258561
3503.665683	434742.640094	48.263565
3503.809494	434704.714229	48.268570
3504.099442	434684.978349	48.273575
3503.845103	434653.411913	48.278580
3504.071291	434615.218142	48.283585
3504.015806	434589.959949	48.288589
3503.915128	434547.204687	48.293594
3504.008264	434501.067505	48.298599
3504.016873	434485.590791	48.303604
3504.013888	434437.338873	48.308609
3503.997648	434410.805313	48.313613
3503.683468	434374.783697	48.318618
3504.084780	434333.413743	48.323623
3503.750988	434310.435275	48.328628
3504.029502	434281.872415	48.333633
3503.803790	434237.006880	48.338637
3503.743304	434201.347584	48.343642
3503.755715	434182.724183	48.348647
3503.612591	434158.190826	48.353652
3503.873753	434113.749307	48.358657
3503.874091	434082.037113	48.363661
3503.882651	434066.306426	48.368666
3503.938075	434029.257102	48.373671
3503.705440	434007.631024	48.378676
3504.055079	433978.193066	48.383681
3503.820453	433939.315753	48.388685
3503.726172	433895.695600	48.393690
3503.993639	433868.504087	48.398695
3503.630708	433850.451906	48.403700
3503.534936	433803.533731	48.408705
3503.461379	433780.814733	48.413709
3503.799558	433758.279109	48.418714
3504.077718	433730.578204	48.423719
3503.678196	433694.417865	48.428724
3503.842635	433659.886345	48.433729
3503.668325	433635.205530	48.438733
3503.605769	433613.144114	48.443738
3503.912678	433568.034096	48.448743
3503.509371	433557.548930	48.453748
3503.899182	433518.564277	48.458753
3503.798639	433498.488125	48.463757
3503.728313	433451.260438	48.468762
3503.679130	433415.800950	48.473767
3503.552567	433400.498805	48.478772
3503.882599	433377.558270	48.483777
3503.950244	433345.529116	48.488781
3503.566121	433307.285149	48.493786
3503.655707	433286.465969	48.498791
3503.543672	433270.400138	48.503796
3503.631666	433218.324515	48.508801
3503.557122	433202.658166	48.513805
3503.358012	433176.002174	48.518810
3503.941940	433158.345923	48.523815
3503.621270	433128.564658	48.528820
3503.719475	433095.667330	48.533825
3503.763823	433068.208517	48.538829
3503.639437	433049.607553	48.543834
3503.895359	433015.719086	48.548839
3503.367387	432988.510128	48.553844
3503.712844	432944.813077	48.558849
3503.613740	432931.383385	48.563853
3503.572790	432912.869547	48.568858
3503.988967	432886.564836	48.573863
3503.451158	432847.128533	48.578868
3503.462749	432824.191079	48.583873
3503.693843	432804.057691	48.588877
3503.626237	432774.283496	48.593882
3503.745154	432736.155651	48.598887
3503.556463	432712.998572	48.603892
3503.775083	432680.384544	48.608897
3503.716721	432670.601208	48.613901
3503.675984	432646.860631	48.618906
3503.785335	432615.381507	48.623911
3503.486983	432589.705892	48.628916
3503.484476	432562.305219	48.633921
3503.512480	432553.724914	48.638925
3503.626082	432527.572945	48.643930
3503.763739	432483.606044	48.648935
3503.473730	432461.633103	48.653940
3503.570159	432440.253815	48.658945
3503.775732	432421.849717	48.663949
3503.309470	432386.459858	48.668954
3503.657993	432354.787309	48.673959
3503.414819	432341.940049	48.678964
3503.540674	432320.758599	48.683969
3503.173437	432307.272840	48.688973
3503.675129	432291.304502	48.693978
3503.884677	432251.841051	48.698983
3503.656975	432224.376941	48.703988
3504.000631	432199.098702	48.708993
3503.688828	432183.015478	48.713997
3503.541737	432158.937352	48.719002
3503.697633	432121.005150	48.724007
3503.728869	432116.026942	48.729012
3503.821896	432086.072198	48.734017
3503.758160	432055.991952	48.739021
3503.577080	432025.880958	48.744026
3503.551846	432002.187814	48.749031
3503.286193	431981.884810	48.754036
3503.531902	431965.756981	48.759041
3504.069145	431933.188980	48.764045
3504.184213	431906.122661	48.769050
3504.177140	431873.546031	48.774055
3504.214532	431843.549728	48.779060
3503.983347	431807.306929	48.784065
3504.088479	431779.278012	48.789069
3503.752354	431750.360259	48.794074
3503.565502	431713.957510	48.799079
3503.397612	431707.338639	48.804084
3503.589542	431663.513145	48.809089
3503.695112	431628.937889	48.814093
3503.432780	431614.063698	48.819098
3503.643833	431595.201302	48.824103
3503.508082	431584.669546	48.829108
3503.596326	431549.538934	48.834113
3503.615021	431521.067758	48.839117
3503.625925	431496.556003	48.844122
3504.286354	431475.434735	48.849127
3504.360433	431449.998729	48.854132
3504.336992	431401.033495	48.859137
3504.391740	431369.257525	48.864141
3504.076632	431336.935720	48.869146
3504.372700	431298.115562	48.874151
3504.147788	431262.175312	48.879156
3503.625673	431230.345416	48.884161
3504.051325	431187.392538	48.889165
3504.021784	431162.379877	48.894170
3504.106916	431140.138637	48.899175
3503.966113	431102.610653	48.904180
3504.010289	431081.949478	48.909185
3503.984556	431047.243536	48.914189
3503.958147	431011.928703	48.919194
3504.274574	430990.967229	48.924199
3504.171721	430952.163864	48.929204
3503.744421	430910.371046	48.934209
3504.013373	430895.963886	48.939213
3503.673364	430861.818796	48.944218
3503.824365	430812.670295	48.949223
3503.697538	430802.999352	48.954228
3503.826589	430780.242802	48.959233
3503.853788	430742.482562	48.964237
3503.853815	430719.088274	48.969242
3503.700684	430695.009657	48.974247
3503.680666	430684.660718	48.979252
3503.569617	430648.141858	48.984257
3503.390689	430630.461706	48.989261
3503.356848	430605.753663	48.994266
3503.858733	430587.855734	48.999271
3503.495820	430575.992134	49.004276
3503.587661	430536.393622	49.009281
3503.550589	430505.139624	49.014285
3503.886882	430481.535437	49.019290
3503.847068	430461.953749	49.024295
3503.560510	430432.467666	49.029300
3503.722252	430391.233052	49.034305
3503.593186	430381.359326	49.039309
3503.592208	430373.544378	49.044314
3503.801717	430343.618245	49.049319
3503.402737	430312.527280	49.054324
3503.795067	430282.468356	49.059329
3503.495289	430259.936765	49.064333
3503.632056	430248.698146	49.069338
3503.520312	430225.982171	49.074343
3503.446069	430196.459537	49.079348
3503.472746	430173.872119	49.084353
3503.565749	430153.760013	49.089357
3503.191729	430142.710058	49.094362
3503.538744	430127.375629	49.099367
3503.732833	430119.831776	49.104372
3503.639399	430074.275830	49.109377
3503.904102	430048.653499	49.114381
3503.465424	430033.909903	49.119386
3503.537794	430005.833695	49.124391
3503.366191	429990.130996	49.129396
3503.398468	429952.520855	49.134401
3503.306965	429920.057402	49.139405
3503.097221	429912.785434	49.144410
3503.823557	429896.726351	49.149415
3503.567895	429888.092001	49.154420
3503.532150	429865.616442	49.159425
3503.497449	429832.077444	49.164429
3503.248423	429807.506797	49.169434
3503.095951	429787.334794	49.174439
3502.881231	429784.986279	49.179444
3503.099219	429763.786769	49.184449
3503.393023	429750.947879	49.189453
3503.272734	429738.890175	49.194458
3503.159820	429723.177275	49.199463
3502.967433	429719.353218	49.204468
3503.382073	429697.003588	49.209473
3503.263616	429681.190108	49.214477
3503.167009	429672.477770	49.219482
3503.380004	429650.670020	49.224487
3502.962049	429645.717235	49.229492
3502.958442	429622.271720	49.234497
3503.255408	429610.853193	49.239501
3503.339286	429609.468660	49.244506
3503.239758	429589.490442	49.249511
3502.785654	429590.278493	49.254516
3503.045002	429566.229779	49.259521
3503.515109	429555.289154	49.264525
3503.391431	429543.790173	49.269530
3503.739438	429506.683648	49.274535
3503.653519	429487.007517	49.279540
3503.463852	429469.582067	49.284545
3503.762661	429463.542611	49.289549
3503.131770	429440.610021	49.294554
3503.531273	429396.085077	49.299559
3503.325052	429379.880381	49.304564
3503.416575	429357.433353	49.309569
3503.529162	429342.950438	49.314573
3503.490342	429334.938606	49.319578
3503.368669	429315.826685	49.324583
3503.238722	429317.422142	49.329588
3503.343659	429297.205762	49.334593
3503.461391	429274.601930	49.339597
3503.420229	429250.198205	49.344602
3503.558082	429229.468646	49.349607
3503.694152	429212.748636	49.354612
3503.888203	429205.915000	49.359617
3503.728262	429163.718150	49.364621
3503.780402	429127.067548	49.369626
3503.724219	429111.040048	49.374631
3503.347516	429107.653366	49.379636
3503.526249	429086.764450	49.384641
3503.645219	429054.111607	49.389645
3503.378742	429033.755419	49.394650
3503.305368	429019.913066	49.399655
3503.371934	429004.879545	49.404660
3503.497663	428985.522108	49.409665
3503.378119	428973.971390	49.414669
3503.273017	428978.455416	49.419674
3503.382517	428944.789025	49.424679
3503.487070	428916.655268	49.429684
3503.367699	428887.189440	49.434689
3503.477071	428877.578870	49.439693
3503.181566	428865.246131	49.444698
3503.378270	428847.855747	49.449703
3503.344338	428841.263937	49.454708
3503.456020	428831.094694	49.459713
3503.733445	428806.788361	49.464717
3503.615454	428779.808964	49.469722
3503.652226	428754.021137	49.474727
3503.665597	428744.731412	49.479732
3503.465534	428725.733898	49.484737
3503.810730	428695.173480	49.489741
3503.520633	428666.802304	49.494746
3503.799103	428642.546376	49.499751
3503.396609	428639.011775	49.504756
3503.350232	428618.262384	49.509761
3503.879006	428602.439163	49.514765
3503.520351	428573.013800	49.519770
3503.668396	428546.648479	49.524775
3503.240779	428544.894459	49.529780
3503.329193	428531.734715	49.534785
3503.439517	428521.007302	49.539789
3503.236386	428490.641750	49.544794
3503.475204	428455.531530	49.549799
3503.402184	428451.940642	49.554804
3503.383087	428429.410114	49.559809
3503.346310	428413.074314	49.564813
3503.225009	428414.972867	49.569818
3503.344206	428402.569073	49.574823
3503.360423	428391.908422	49.579828
3503.285343	428377.710719	49.584833
3503.255136	428367.108735	49.589837
3503.135922	428350.482457	49.594842
3503.175817	428310.483042	49.599847
3503.231876	428290.121889	49.604852
3503.295878	428279.300771	49.609857
3503.315769	428262.092403	49.614861
3503.146746	428256.538542	49.619866
3503.277336	428248.446659	49.624871
3503.122249	428241.063334	49.629876
3502.971968	428226.726124	49.634881
3503.405053	428208.787384	49.639885
3503.081848	428202.143285	49.644890
3503.302454	428189.722063	49.649895
3503.050399	428194.586597	49.654900
3503.306028	428176.170610	49.659905
3503.244916	428165.979832	49.664909
3503.191728	428162.740780	49.669914
3503.374566	428146.418048	49.674919
3503.614813	428130.390017	49.679924
3503.349164	428096.684969	49.684929
3503.399708	428079.775750	49.689933
3503.130536	428066.118527	49.694938
3503.304898	428046.295242	49.699943
3503.337486	428037.306473	49.704948
3503.294130	428016.556038	49.709953
3503.379841	428008.471737	49.714957
3503.066793	427999.186704	49.719962
3503.416667	427990.955784	49.724967
3503.103589	427981.061715	49.729972
3502.970812	427973.217721	49.734977
3503.543042	427959.213753	49.739981
3503.103416	427934.470681	49.744986
3503.303144	427908.248082	49.749991
3503.240551	427895.722804	49.754996
3503.275961	427892.265575	49.760001
3503.452318	427869.092102	49.765005
3503.291028	427866.531258	49.770010
3503.506435	427852.182131	49.775015
3503.610399	427847.495115	49.780020
3503.338794	427832.620098	49.785025
3503.686855	427803.276113	49.790029
3503.365431	427779.223240	49.795034
3503.572944	427763.758836	49.800039
3503.311890	427746.953339	49.805044
3503.491663	427740.832265	49.810049
3503.669303	427719.637807	49.815053
3503.380740	427701.365127	49.820058
3503.403223	427667.153486	49.825063
3503.615350	427660.062550	49.830068
3503.253524	427642.309869	49.835073
3503.475681	427631.461450	49.840077
3503.510382	427624.502306	49.845082
3503.623203	427601.491682	49.850087
3503.230611	427577.400002	49.855092
3503.070125	427557.278209	49.860097
3503.247641	427537.250945	49.865101
3502.970279	427530.446567	49.870106
3503.333637	427515.513683	49.875111
3503.369091	427512.969959	49.880116
3503.221762	427501.677033	49.885121
3502.982316	427485.476707	49.890125
3502.917287	427483.508430	49.895130
3503.196947	427468.234530	49.900135
3502.992633	427469.081500	49.905140
3502.998900	427446.038166	49.910145
3503.077340	427443.740864	49.915149
3503.043926	427436.691789	49.920154
3503.080994	427425.164324	49.925159
3502.860431	427409.772786	49.930164
3502.757728	427399.182748	49.935169
3502.942006	427391.791963	49.940173
3502.922334	427384.842034	49.945178
3502.706165	427367.368799	49.950183
3502.905733	427383.880582	49.955188
3502.611694	427387.635858	49.960193
3503.450747	427386.122247	49.965197
3502.518018	427386.433797	49.970202
3502.689709	427371.635058	49.975207
3503.046831	427358.631796	49.980212
3502.745950	427362.946540	49.985217
3503.202749	427348.302120	49.990221
3502.689580	427348.694291	49.995226
3502.556525	427332.120413	50.000231
3502.718084	427332.346618	50.005236
3502.634638	427345.861500	50.010241
3503.242132	427351.645272	50.015245
3502.863585	427343.538510	50.020250
3502.779982	427338.984929	50.025255
3502.987143	427329.610805	50.030260
3502.806834	427324.160159	50.035265
3503.222250	427310.436358	50.040269
3502.786398	427304.166520	50.045274
3503.195620	427291.002062	50.050279
3503.174023	427286.640901	50.055284
3502.997404	427274.946834	50.060289
3503.393693	427265.032847	50.065293
3502.909223	427259.532614	50.070298
3503.009851	427252.054560	50.075303
3503.122271	427237.824157	50.080308
3503.011347	427236.421995	50.085313
3503.062401	427231.490120	50.090317
3502.842825	427220.158642	50.095322
3503.297315	427200.185309	50.100327
3503.259048	427208.008052	50.105332
3503.142699	427200.770050	50.110337
3503.118302	427195.749543	50.115341
3502.903947	427191.218260	50.120346
3503.154387	427180.009525	50.125351
3502.945816	427168.676143	50.130356
3502.708360	427152.729022	50.135361
3502.846948	427153.111415	50.140365
3502.654420	427153.753365	50.145370
3503.338034	427131.152366	50.150375
3503.076700	427130.790974	50.155380
3503.075806	427125.461910	50.160385
3503.060401	427110.085900	50.165389
3502.867117	427104.028363	50.170394
3502.762070	427085.876136	50.175399
3503.180737	427091.742969	50.180404
3503.133595	427076.727640	50.185409
3503.129287	427070.688581	50.190413
3503.129491	427065.004033	50.195418
3503.155766	427048.910299	50.200423
3503.225407	427038.696711	50.205428
3503.198278	427046.314586	50.210433
3503.090563	427022.072188	50.215437
3503.151294	427030.588653	50.220442
3503.213484	427020.224065	50.225447
3503.084697	427008.623209	50.230452
3503.124953	426996.841218	50.235457
3503.506265	426988.046281	50.240461
3503.025642	426983.255896	50.245466
3503.036063	426973.204656	50.250471
3503.151549	426976.230254	50.255476
3502.901260	426966.325039	50.260481
3503.366097	426950.613147	50.265485
3503.272386	426948.954254	50.270490
3503.107230	426932.639354	50.275495
3502.761077	426928.079771	50.280500
3502.672384	426920.126391	50.285505
3502.765432	426909.096668	50.290509
3502.707002	426908.243829	50.295514
3502.643972	426894.093934	50.300519
3502.969514	426888.404546	50.305524
3502.889214	426886.692603	50.310529
3503.007426	426872.511748	50.315533
3502.760322	426879.355155	50.320538
3502.501271	426891.225360	50.325543
3502.769271	426904.731237	50.330548
3502.979028	426894.036865	50.335553
3502.929320	426880.950545	50.340557
3502.904381	426880.345762	50.345562
3502.983145	426876.576451	50.350567
3502.975616	426867.898621	50.355572
3502.746079	426865.450831	50.360577
3503.138488	426854.877519	50.365581
3502.804929	426853.462594	50.370586
3502.888906	426846.697830	50.375591
3503.054110	426839.766928	50.380596
3502.774694	426838.038226	50.385601
3503.158259	426821.578799	50.390605
3503.087667	426822.809000	50.395610
3502.926277	426804.057116	50.400615
3503.020194	426813.938386	50.405620
3502.701665	426830.285243	50.410625
3502.812231	426817.882095	50.415629
3503.058032	426824.489087	50.420634
3502.779111	426812.203198	50.425639
3503.001137	426812.013040	50.430644
3502.901737	426804.264470	50.435649
3502.871918	426795.691931	50.440653
3502.578928	426782.494832	50.445658
3502.817026	426778.546033	50.450663
3502.280727	426772.800758	50.455668
3502.515966	426788.545533	50.460673
3502.583157	426799.040437	50.465677
3502.713259	426800.185615	50.470682
3502.792245	426789.868813	50.475687
3502.529857	426785.548676	50.480692
3502.628881	426796.190412	50.485697
3502.662250	426798.113438	50.490701
3502.482513	426813.370746	50.495706
3502.926561	426807.255061	50.500711
3502.883019	426798.228068	50.505716
3502.863635	426795.744387	50.510721
3502.788789	426795.249634	50.515725
3502.734114	426782.823928	50.520730
3502.838490	426778.491919	50.525735
3502.936290	426747.514438	50.530740
3502.941500	426718.227658	50.535745
3502.888644	426671.338568	50.540749
3502.742698	426612.842220	50.545754
3502.603877	426537.341295	50.550759
3503.003540	426466.417739	50.555764
3502.716248	426381.501046	50.560769
3502.963328	426278.626543	50.565773
3502.719229	426154.416148	50.570778
3502.603153	426031.705957	50.575783
3502.920527	425889.988669	50.580788
3502.407831	425742.575160	50.585793
3502.967346	425581.120751	50.590797
3502.711727	425414.221034	50.595802
3502.582371	425240.699976	50.600807
3502.944125	425034.354224	50.605812
3502.612355	424825.282594	50.610817
3502.900440	424602.093555	50.615821
3502.853194	424374.442032	50.620826
3502.769839	424119.129802	50.625831
3502.964080	423873.056838	50.630836
3502.355250	423601.635952	50.635841
3502.897350	423307.375352	50.640845
3502.682007	423019.636708	50.645850
3502.571326	422713.551022	50.650855
3503.054047	422389.947920	50.655860
3502.323414	422056.293136	50.660865
3502.704122	421708.128031	50.665869
3502.418770	421356.822654	50.670874
3502.170815	420981.543623	50.675879
3502.591171	420603.377896	50.680884
3502.412929	420204.518661	50.685889
3502.493176	419794.160251	50.690893
3502.236886	419369.408241	50.695898
3502.161652	418929.538884	50.700903
3502.368553	418473.391758	50.705908
3502.438293	418003.449343	50.710913
3502.118947	417517.672149	50.715917
3502.175888	417026.591462	50.720922
3502.105534	416505.133204	50.725927
3502.271434	415989.844150	50.730932
3502.158758	415444.912100	50.735937
3501.926594	414877.061745	50.740941
3501.935145	414310.579579	50.745946
3502.175059	413715.835983	50.750951
3502.179684	413097.123758	50.755956
3502.203667	412466.078216	50.760961
3502.220057	411820.062259	50.765965
3501.679665	411157.035563	50.770970
3501.823556	410482.904989	50.775975
3502.016378	409784.318977	50.780980
3501.856878	409075.337147	50.785985
3501.978064	408333.959095	50.790989
3501.953086	407584.915583	50.795994
3501.680950	406811.918001	50.800999
3501.861429	406015.352882	50.806004
3501.626369	405210.047261	50.811009
3501.699513	404375.099739	50.816013
3501.235293	403538.846979	50.821018
3501.260117	402671.216146	50.826023
3501.160190	401782.114582	50.831028
3501.061616	400892.273254	50.836033
3501.329121	399964.514796	50.841037
3501.423346	399026.060139	50.846042
3501.174012	398066.241718	50.851047
3500.749917	397075.425105	50.856052
3500.639669	396079.744375	50.861057
3501.052350	395054.924065	50.866061
3500.788651	394015.242881	50.871066
3500.690109	392950.849161	50.876071
3500.561329	391871.811273	50.881076
3500.218257	390768.401187	50.886081
3500.240713	389649.793258	50.891085
3500.152210	388514.974736	50.896090
3499.920102	387355.562883	50.901095
3500.139224	386179.535956	50.906100
3499.465411	384983.436597	50.911105
3499.624404	383768.772901	50.916109
3499.214114	382543.382800	50.921114
3499.224377	381291.310910	50.926119
3499.350889	380024.884757	50.931124
3498.918179	378728.253768	50.936129
3498.673533	377423.506672	50.941133
3498.552689	376091.001623	50.946138
3498.285456	374752.189576	50.951143
3498.667908	373392.136764	50.956148
3497.946916	372003.563565	50.961153
3498.187071	370612.050828	50.966157
3497.835032	369189.994420	50.971162
3497.645479	367753.791785	50.976167
3497.415185	366308.410225	50.981172
3497.168768	364833.220187	50.986177
3497.101824	363337.748193	50.991181
3496.556856	361831.591681	50.996186
3496.598316	360319.604508	51.001191
3496.693443	358777.942975	51.006196
3496.274596	357221.581840	51.011201
3496.529888	355636.606599	51.016205
3496.443113	354055.876944	51.021210
3495.672599	352441.547858	51.026215
3495.700655	350810.383053	51.031220
3495.367487	349156.295712	51.036225
3495.446222	347487.904496	51.041229
3495.107360	345813.059919	51.046234
3494.952685	344119.929855	51.051239
3494.674549	342403.756889	51.056244
3494.250087	340679.582287	51.061249
3494.325692	338930.043004	51.066253
3493.991773	337174.913305	51.071258
3493.824089	335398.953587	51.076263
3493.763515	333609.070014	51.081268
3493.498225	331799.996662	51.086273
3493.356105	329975.214788	51.091277
3492.953272	328136.037031	51.096282
3492.829129	326287.640165	51.101287
3492.227182	324413.303628	51.106292
3491.818327	322538.544778	51.111297
3491.804538	320630.493303	51.116301
3491.273699	318734.742798	51.121306
3490.872637	316810.658280	51.126311
3491.016561	314872.806236	51.131316
3490.438935	312931.688714	51.136321
3490.278929	310964.912513	51.141325
3489.857051	308989.778708	51.146330
3489.526555	306996.120504	51.151335
3489.511874	305000.016835	51.156340
3489.159040	302994.171876	51.161345
3488.634502	300955.107982	51.166349
3488.436880	298926.178961	51.171354
3488.062398	296867.598348	51.176359
3488.031711	294799.444685	51.181364
3487.212717	292732.887918	51.186369
3487.003148	290637.847159	51.191373
3486.826987	288537.620084	51.196378
3486.499683	286423.021741	51.201383
3486.199546	284288.191640	51.206388
3485.555476	282158.966338	51.211393
3485.788207	280011.328829	51.216397
3485.357507	277857.462297	51.221402
3484.889221	275678.569282	51.226407
3484.543777	273490.643024	51.231412
3484.063866	271290.215246	51.236417
3483.861184	269082.693477	51.241421
3482.929809	266863.998845	51.246426
3482.757972	264646.053347	51.251431
3482.439370	262410.397276	51.256436
3481.827689	260167.041654	51.261441
3481.864767	257900.165409	51.266445
3481.573492	255643.428809	51.271450
3480.858524	253360.329618	51.276455
3480.683333	251060.384171	51.281460
3480.011733	248772.398543	51.286465
3479.530703	246458.005469	51.291469
3479.110184	244136.560576	51.296474
3478.674741	241819.463916	51.301479
3478.355621	239486.857001	51.306484
3477.562243	237151.959724	51.311489
3477.103885	234802.387571	51.316493
3476.561432	232444.709732	51.321498
3476.381762	230083.513696	51.326503
3475.999924	227708.891328	51.331508
3475.396023	225339.235799	51.336513
3474.929034	222947.037862	51.341517
3474.270284	220556.039953	51.346522
3473.733989	218156.235407	51.351527
3473.176682	215743.884154	51.356532
3472.665300	213342.328094	51.361537
3472.366675	210927.734604	51.366541
3472.003130	208498.857061	51.371546
3471.072928	206065.066124	51.376551
3470.791707	203627.787567	51.381556
3469.909294	201182.745297	51.386561
3469.667905	198728.611369	51.391565
3468.789494	196278.566157	51.396570
3468.118093	193811.772993	51.401575
3467.573172	191342.467780	51.406580
3466.871288	188887.973430	51.411585
3466.534710	186411.346780	51.416589
3466.182385	183939.014750	51.421594
3465.104914	181454.469633	51.426599
3464.604494	178970.168312	51.431604
3463.911902	176487.747329	51.436609
3463.420331	173996.315324	51.441613
3462.879847	171508.821101	51.446618
3462.237216	169012.860081	51.451623
3461.658213	166513.268736	51.456628
3460.842442	164022.085792	51.461633
3460.187914	161501.823269	51.466637
3459.598852	159003.549065	51.471642
3458.479205	156504.357098	51.476647
3457.745068	153988.274071	51.481652
3457.221201	151492.890100	51.486657
3457.057228	148953.111199	51.491661
3456.339906	146406.768695	51.496666
3455.603625	143888.868382	51.501671
3454.807267	141373.556171	51.506676
3453.773185	138849.538918	51.511681
3452.980320	136340.130079	51.516685
3452.367791	133828.511824	51.521690
3451.290031	131322.831366	51.526695
3450.332923	128810.371458	51.531700
3449.716322	126313.541879	51.536705
3448.659828	123809.095769	51.541709
3448.126677	121315.843903	51.546714
3447.068085	118827.080612	51.551719
3446.646751	116333.920862	51.556724
3445.481427	113847.008791	51.561729
3444.830919	111360.670102	51.566733
3443.658250	108886.299810	51.571738
3442.676325	106401.109046	51.576743
3441.708522	103921.667330	51.581748
3440.538354	101473.381765	51.586753
3440.075280	99014.038333	51.591757
3438.644922	96575.227487	51.596762
3437.473179	94138.961094	51.601767
3436.561274	91703.039809	51.606772
3435.302252	89295.324980	51.611777
3434.449603	86878.091183	51.616781
3433.504040	84479.280177	51.621786
3432.462532	82092.064955	51.626791
3431.403678	79712.905456	51.631796
3430.027939	77344.904273	51.636801
3429.016125	74980.747578	51.641805
3427.815821	72643.085669	51.646810
3426.838385	70308.537249	51.651815
3425.636136	67981.111391	51.656820
3424.160456	65665.945280	51.661825
3422.682751	63377.740172	51.666829
3421.698090	61109.181293	51.671834
3420.117033	58849.108788	51.676839
3418.808651	56612.618516	51.681844
3417.495399	54394.988899	51.686849
3416.583325	52180.805025	51.691853
3415.480094	49991.964172	51.696858
3413.681979	47814.050234	51.701863
3412.400252	45660.811847	51.706868
3410.757958	43529.217741	51.711873
3409.181639	41414.878938	51.716877
3407.343246	39329.935675	51.721882
3405.484898	37269.104586	51.726887
3404.193151	35237.731962	51.731892
3402.262926	33242.549774	51.736897
3400.243027	31258.673028	51.741901
3397.901254	29323.714177	51.746906
3394.888893	27427.362978	51.751911
3391.154379	25597.237487	51.756916
3385.712397	23892.402186	51.761921
3378.498726	22291.972187	51.766925
3370.536830	20829.090983	51.771930
3362.712744	19486.837020	51.776935
3356.072182	18271.655261	51.781940
3349.348759	17195.810702	51.786945
3342.914312	16226.614361	51.791949
3337.561074	15389.734876	51.796954
3332.510433	14684.016487	51.801959
3328.649651	14056.977404	51.806964
3325.094742	13531.851631	51.811969
3322.118976	13094.413284	51.816973
3319.575779	12738.723277	51.821978
3316.986048	12443.490138	51.826983
3315.909255	12200.226112	51.831988
3314.253675	12019.898053	51.836993
3313.152142	11857.196206	51.841997
3311.893459	11748.676050	51.847002
3311.058063	11677.817456	51.852007
3310.502416	11611.956463	51.857012
3309.806094	11577.265509	51.862017
3309.478293	11551.339350	51.867021
3309.319176	11543.123492	51.872026
3308.559593	11551.131343	51.877031
3308.642263	11552.262769	51.882036
3308.397434	11581.296772	51.887041
3308.094532	11600.809921	51.892045
3308.429871	11624.153117	51.897050
3307.905734	11657.314646	51.902055
3308.153469	11670.224013	51.907060
3308.046145	11691.806906	51.912065
3308.087140	11715.644510	51.917069
3307.981196	11725.027614	51.922074
3307.220875	11737.747407	51.927079
3307.477840	11742.214593	51.932084
3307.238987	11761.868677	51.937089
3307.432477	11756.847398	51.942093
3307.418533	11754.675640	51.947098
3307.245803	11753.716051	51.952103
3307.005191	11742.120051	51.957108
3306.615953	11716.670243	51.962113
3306.586766	11695.199161	51.967117
3306.726952	11664.299456	51.972122
3306.626091	11640.217807	51.977127
3306.571237	11602.195505	51.982132
3306.566587	11555.939028	51.987137
3306.620926	11494.333634	51.992141
3306.166158	11425.008529	51.997146
3306.016477	11353.907798	52.002151
3305.566920	11292.016360	52.007156
3304.305349	11219.911665	52.012161
3303.883901	11147.069691	52.017165
3303.713206	11081.724931	52.022170
3302.640834	11021.364488	52.027175
3302.819955	10942.555916	52.032180
3301.660217	10873.699594	52.037185
3301.053715	10796.234615	52.042189
3300.525888	10715.988477	52.047194
3300.125201	10648.556535	52.052199
3299.837206	10572.780892	52.057204
3299.582049	10506.929898	52.062209
3298.842681	10402.842273	52.067213
3297.903376	10319.614377	52.072218
3297.118768	10250.821418	52.077223
3297.010744	10166.186787	52.082228
3295.919032	10082.038199	52.087233
3295.315687	9997.212580	52.092237
3295.073293	9923.121067	52.097242
3294.049753	9849.833203	52.102247
3293.995698	9760.715675	52.107252
3293.273528	9700.391939	52.112257
3292.379097	9589.654778	52.117261
3291.993433	9515.469529	52.122266
3291.151833	9436.544011	52.127271
3290.858208	9342.259410	52.132276
3290.003316	9272.395681	52.137281
3289.638875	9177.149389	52.142285
3288.949026	9097.555035	52.147290
3288.440836	9012.397603	52.152295
3287.587711	8919.005678	52.157300
3286.760283	8838.857898	52.162305
3286.243160	8753.550114	52.167309
3285.733159	8674.408945	52.172314
3284.846114	8591.997718	52.177319
3284.501415	8501.421771	52.182324
3283.595400	8422.001946	52.187329
3283.194204	8333.882019	52.192333
3282.958938	8250.975731	52.197338
3282.203580	8161.444159	52.202343
3281.493157	8064.483973	52.207348
3280.315968	7994.563138	52.212353
3279.915034	7903.125000	52.217357
3279.572494	7818.749613	52.222362
3278.446784	7744.540936	52.227367
3278.151684	7651.875326	52.232372
3277.572410	7577.956344	52.237377
3276.889335	7491.758688	52.242381
3276.542786	7401.404058	52.247386
3275.441526	7312.352529	52.252391
3275.240244	7221.015260	52.257396
3274.368306	7136.337403	52.262401
3273.688646	7059.331651	52.267405
3272.961254	6965.311932	52.272410
3272.209990	6884.642748	52.277415
3271.813377	6796.469628	52.282420
3270.774323	6726.353010	52.287425
3270.036272	6635.133673	52.292429
3269.662581	6552.342700	52.297434
3269.178152	6475.616777	52.302439
3268.658986	6378.487970	52.307444
3268.005954	6302.906829	52.312449
3267.319716	6208.192682	52.317453
3266.734153	6122.991078	52.322458
3265.520575	6042.493565	52.327463
3265.167225	5952.699492	52.332468
3264.651176	5874.994664	52.337473
3263.578170	5794.762641	52.342477
3263.201103	5710.262072	52.347482
3262.202259	5627.551878	52.352487
3261.582385	5548.065002	52.357492
3260.906015	5476.584907	52.362497
3260.480592	5395.264213	52.367501
3259.759418	5312.775139	52.372506
3258.558836	5241.023176	52.377511
3258.759184	5149.569075	52.382516
3258.052245	5074.539954	52.387521
3257.298630	4999.162216	52.392525
3256.802349	4916.320893	52.397530
3255.524621	4838.249780	52.402535
3255.168354	4759.756295	52.407540
3254.649496	4679.181727	52.412545
3253.968995	4604.874443	52.417549
3253.053080	4523.742280	52.422554
3252.414774	4443.216953	52.427559
3251.984502	4355.909572	52.432564
3251.259655	4292.079953	52.437569
3250.658699	4222.135610	52.442573
3249.606690	4133.038116	52.447578
3249.086591	4065.455937	52.452583
3248.761704	3989.318007	52.457588
3247.991867	3917.714798	52.462593
3246.988469	3836.166790	52.467597
3246.262388	3759.568653	52.472602
3245.300495	3699.586393	52.477607
3245.171869	3618.851043	52.482612
3244.292807	3554.976513	52.487617
3244.036090	3479.236044	52.492621
3243.446894	3404.224704	52.497626
3242.784974	3329.215880	52.502631
3241.945472	3254.971299	52.507636
3241.591455	3183.220621	52.512641
3240.576471	3095.810823	52.517645
3239.966330	3021.582637	52.522650
3239.047304	2951.794575	52.527655
3238.747370	2878.629766	52.532660
3237.638327	2809.553847	52.537665
3236.906165	2733.427578	52.542669
3236.098756	2663.410904	52.547674
3235.368443	2603.399561	52.552679
3234.936538	2530.694759	52.557684
3234.242075	2465.922195	52.562689
3233.538899	2408.161982	52.567693
3232.535405	2332.752769	52.572698
3232.106624	2274.884580	52.577703
3231.608151	2215.363326	52.582708
3231.211635	2160.443793	52.587713
3230.173701	2096.487036	52.592717
3230.126718	2018.229061	52.597722
3229.694304	1964.570941	52.602727
3228.893858	1877.861578	52.607732
3228.048008	1815.618830	52.612737
3227.404456	1747.421815	52.617741
3226.893029	1668.430912	52.622746
3225.646798	1602.940581	52.627751
3225.210179	1533.829207	52.632756
3224.328399	1476.178727	52.637761
3223.749697	1406.557680	52.642765
3223.167410	1344.978786	52.647770
3222.181861	1282.563062	52.652775
3221.814404	1202.227472	52.657780
3220.884629	1153.758120	52.662785
3220.631592	1086.517302	52.667789
3220.038352	1026.556461	52.672794
3218.959589	972.731094	52.677799
3218.415236	898.358392	52.682804
3217.832996	842.277140	52.687809
3216.473921	781.616743	52.692813
3215.889609	729.987781	52.697818
3215.102981	676.546953	52.702823
3214.712567	624.174285	52.707828
3213.869675	572.218966	52.712833
3212.945428	525.864841	52.717837
3212.803333	478.949726	52.722842
3211.887923	435.838701	52.727847
3210.990756	385.954191	52.732852
3210.549405	333.197255	52.737857
3209.075447	290.227849	52.742861
3208.526694	250.926226	52.747866
3207.502773	232.753302	52.752871
3206.667327	213.240852	52.757876
3206.075445	176.715424	52.762881
3205.040156	157.533629	52.767885
3204.255384	133.619292	52.772890
3201.867101	137.448456	52.777895
3201.255492	137.028770	52.782900
3200.725957	145.887361	52.787905
3199.924908	157.416895	52.792909
3199.614975	142.534130	52.797914
3199.020036	153.044390	52.802919
3198.750842	141.623541	52.807924
3198.148245	140.926795	52.812929
3197.013574	143.319310	52.817933
3196.883866	148.057706	52.822938
3195.959673	145.422526	52.827943
3195.651041	150.414118	52.832948
3195.013236	145.714131	52.837953
3194.223317	152.473442	52.842957
3193.852270	138.943595	52.847962
3192.901987	144.570195	52.852967
3192.136507	136.475651	52.857972
3191.930851	146.782822	52.862977
3190.916897	147.860794	52.867981
3190.266692	139.809316	52.872986
3189.755949	149.246527	52.877991
3189.639851	145.754089	52.882996
3188.604450	150.013685	52.888001
3187.445477	152.808636	52.893005
3187.228777	143.027995	52.898010
3186.447417	149.576637	52.903015
3186.101255	140.731913	52.908020
3185.341893	145.243550	52.913025
3184.458749	139.482612	52.918029
3184.270149	146.445099	52.923034
3183.504409	153.787636	52.928039
3182.957711	153.525016	52.933044
3182.006383	155.925684	52.938049
3181.105314	151.274229	52.943053
3180.916439	137.801285	52.948058
3180.040684	147.272043	52.953063
3179.531809	143.489879	52.958068
3178.817316	145.234700	52.963073
3177.969238	148.307317	52.968077
3177.704664	142.152938	52.973082
3176.325415	144.104097	52.978087
3175.762359	140.630000	52.983092
3175.733352	143.698462	52.988097
3174.418270	147.681771	52.993101
3174.372776	145.585663	52.998106
3173.410950	137.884266	53.003111
3172.835240	142.514917	53.008116
3172.793720	149.552932	53.013121
3172.073332	145.112974	53.018125
3171.480934	140.653913	53.023130
3170.357577	147.154804	53.028135
3170.213017	134.989923	53.033140
3169.362415	134.121611	53.038145
3168.205430	138.962493	53.043149
3167.371513	135.637701	53.048154
3166.957149	142.845991	53.053159
3166.028259	140.858580	53.058164
3165.609216	135.118614	53.063169
3164.970379	141.905793	53.068173
3165.014870	143.434888	53.073178
3164.100486	139.034394	53.078183
3163.237243	140.576084	53.083188
3162.726637	136.549488	53.088193
3161.734587	138.230025	53.093197
3161.277579	141.798708	53.098202
3160.502592	139.984340	53.103207
3160.290942	136.773884	53.108212
3159.622969	139.014827	53.113217
3158.470897	140.895595	53.118221
3157.800748	137.155201	53.123226
3157.341042	142.709038	53.128231
3156.462399	136.181960	53.133236
3156.128495	144.527925	53.138241
3155.362695	148.377127	53.143245
3154.831181	140.703657	53.148250
3154.531873	145.188403	53.153255
3153.743476	137.174754	53.158260
3153.315046	141.624720	53.163265
3151.855071	141.831556	53.168269
3151.140769	136.432165	53.173274
3150.340772	144.385275	53.178279
3150.555556	140.262768	53.183284
3149.750240	140.148941	53.188289
3148.684477	149.831372	53.193293
3147.874406	141.945371	53.198298
3147.568626	150.387584	53.203303
3147.103931	147.242071	53.208308
3146.493938	147.561046	53.213313
3145.699326	143.635869	53.218317
3145.090921	142.045273	53.223322
3143.927993	143.233967	53.228327
3143.809295	143.885438	53.233332
3143.449375	141.665031	53.238337
3142.599779	145.963542	53.243341
3141.899038	140.594991	53.248346
3141.021031	152.596739	53.253351
3140.450975	140.005623	53.258356
3139.576370	144.744580	53.263361
3138.341616	152.661059	53.268365
3138.772275	135.372616	53.273370
3138.011543	139.951988	53.278375
3137.566117	141.205982	53.283380
3137.187812	137.371517	53.288385
3136.136151	144.524094	53.293389
3134.664490	139.494891	53.298394
3133.726039	143.749769	53.303399
3132.775847	144.786462	53.308404
3132.862484	148.427652	53.313409
3132.427004	148.151165	53.318413
3131.734144	139.530684	53.323418
3131.204096	132.177491	53.328423
3130.928559	140.284538	53.333428
3130.302298	137.470575	53.338433
3129.018015	141.670860	53.343437
3128.872697	139.011955	53.348442
3128.094393	139.482054	53.353447
3127.053112	142.709658	53.358452
3126.110685	135.125352	53.363457
3125.512944	145.486482	53.368461
3125.168157	129.836034	53.373466
3124.644726	133.498169	53.378471
3124.478486	146.904713	53.383476
3123.726138	133.812658	53.388481
3122.981246	140.381516	53.393485
3122.271217	138.276983	53.398490
3121.371464	140.351483	53.403495
3120.632913	134.068104	53.408500
3119.897158	128.600545	53.413505
3118.987980	140.248804	53.418509
3118.425518	137.913405	53.423514
3117.976410	150.188045	53.428519
3118.038951	147.486124	53.433524
3116.894159	134.793091	53.438529
3115.956349	137.226980	53.443533
3115.797164	141.583970	53.448538
3114.811960	135.201817	53.453543
3114.710632	140.511661	53.458548
3113.794281	138.955134	53.463553
3112.831504	145.194520	53.468557
3111.935011	132.947739	53.473562
3110.977957	134.114683	53.478567
3110.101725	140.537039	53.483572
3109.939470	135.868707	53.488577
3109.645064	149.154258	53.493581
3109.432810	135.701508	53.498586
3108.639631	137.324388	53.503591
3107.474346	141.756971	53.508596
3107.371534	140.525639	53.513601
3105.992890	138.390881	53.518605
3105.751411	139.904891	53.523610
3105.306280	138.541791	53.528615
3104.669562	137.033800	53.533620
3103.614689	132.373910	53.538625
3103.049034	145.041083	53.543629
3102.364336	128.284273	53.548634
3101.798606	131.950479	53.553639
3101.156731	133.875526	53.558644
3100.629798	133.818743	53.563649
3099.517265	138.369809	53.568653
3098.697285	127.887026	53.573658
3097.870668	133.980384	53.578663
3096.836977	136.046984	53.583668
3096.736980	140.168864	53.588673
3096.431543	137.946258	53.593677
3096.203532	127.703372	53.598682
3095.838571	133.741138	53.603687
3093.694365	138.814266	53.608692
3093.584455	121.474133	53.613697
3093.130601	135.649000	53.618701
3092.804663	126.220199	53.623706
3092.168479	129.990809	53.628711
3091.390114	134.682536	53.633716
3090.475715	134.076973	53.638721
3089.678850	135.374441	53.643725
3089.188196	131.211818	53.648730
3088.376076	133.968437	53.653735
3087.919218	133.167462	53.658740
3087.329091	135.422345	53.663745
3086.285444	135.718715	53.668749
3085.496897	133.883387	53.673754
3084.914488	134.391466	53.678759
3084.016918	138.138454	53.683764
3083.834662	137.259374	53.688769
3083.503300	137.212595	53.693773
3082.788714	138.971652	53.698778
3081.773041	135.844112	53.703783
3081.289138	137.769800	53.708788
3080.831573	132.364053	53.713793
3079.911830	142.047982	53.718797
3079.646805	129.773837	53.723802
3078.396861	123.973763	53.728807
3077.785806	133.388236	53.733812
3078.112486	121.658373	53.738817
3076.484382	133.476049	53.743821
3075.939880	133.753841	53.748826
3075.127802	135.876917	53.753831
3075.025023	143.416035	53.758836
3073.758081	134.586564	53.763841
3073.231313	137.484291	53.768845
3073.271187	133.764691	53.773850
3072.277860	139.197739	53.778855
3070.985964	139.216406	53.783860
3070.848576	136.821012	53.788865
3069.925140	139.302582	53.793869
3069.775523	129.218011	53.798874
3068.607835	140.241775	53.803879
3068.264804	138.370980	53.808884
3067.517110	127.187844	53.813889
3066.322180	135.211200	53.818893
3066.176326	126.757003	53.823898
3066.019356	127.490801	53.828903
3065.499030	132.546981	53.833908
3064.532507	137.001262	53.838913
3063.473169	136.824671	53.843917
3062.670487	132.932469	53.848922
3061.704551	132.282429	53.853927
3061.296187	136.593969	53.858932
3060.707201	126.004623	53.863937
3059.937496	137.303793	53.868941
3059.675103	132.971516	53.873946
3059.167353	123.558394	53.878951
3058.184240	134.304701	53.883956
3057.432988	126.290653	53.888961
3056.640500	133.208295	53.893965
3056.706889	129.043649	53.898970
3055.569383	135.816961	53.903975
3054.768670	136.806019	53.908980
3054.579512	125.255481	53.913985
3053.550335	129.293373	53.918989
3052.711813	122.768152	53.923994
3052.446128	123.440003	53.928999
3051.523059	132.661481	53.934004
3051.085377	128.827305	53.939009
3050.129162	131.448685	53.944013
3049.581674	127.077496	53.949018
3049.132239	127.542331	53.954023
3048.285635	126.940980	53.959028
3048.069267	120.151955	53.964033
3047.457909	124.303973	53.969037
3046.797481	121.875196	53.974042
3046.101020	118.029980	53.979047
3045.843937	120.010461	53.984052
3044.063902	115.564500	53.989057
3043.164598	125.640050	53.994061
3043.399982	125.464852	53.999066
3042.700142	120.732867	54.004071
3041.204857	126.010509	54.009076
3041.138926	121.384541	54.014081
3040.977484	122.899479	54.019085
3039.553479	118.548600	54.024090
3038.800190	120.729920	54.029095
3038.073726	132.588132	54.034100
3038.425405	119.358381	54.039105
3036.746519	129.473989	54.044109
3036.162165	122.724951	54.049114
3036.189385	131.002092	54.054119
3035.169597	120.306373	54.059124
3034.139233	120.759163	54.064129
3033.749022	134.451056	54.069133
3033.483413	127.392950	54.074138
3032.625436	124.422814	54.079143
3031.889185	121.508850	54.084148
3031.469274	117.193628	54.089153
3030.536871	122.794287	54.094157
3030.029309	115.653982	54.099162
3029.375229	118.513859	54.104167
3028.528270	124.603195	54.109172
3028.259024	124.368178	54.114177
3026.983497	123.143036	54.119181
3026.835741	123.803026	54.124186
3026.335354	121.925969	54.129191
3025.711997	117.656170	54.134196
3024.462037	113.049772	54.139201
3023.434381	123.486719	54.144205
3023.579546	118.970335	54.149210
3022.541380	117.333591	54.154215
3021.598737	131.185404	54.159220
3021.845236	121.296440	54.164225
3020.637623	125.345879	54.169229
3019.687043	121.605273	54.174234
3019.192196	121.617617	54.179239
3018.446534	128.318052	54.184244
3018.343817	113.011534	54.189249
3017.657161	121.815250	54.194253
3016.968028	122.814850	54.199258
3016.685517	115.838980	54.204263
3015.915932	115.816169	54.209268
3014.978149	109.817122	54.214273
3013.491928	111.772380	54.219277
3013.280228	110.832812	54.224282
3013.088887	120.888038	54.229287
3011.681142	122.325427	54.234292
3011.503145	114.769608	54.239297
3010.772482	123.371640	54.244301
3009.776437	118.256472	54.249306
3009.282772	122.865605	54.254311
3008.991595	117.640647	54.259316
3008.616859	118.866778	54.264321
3007.687392	120.183362	54.269325
3006.597732	118.546341	54.274330
3006.436068	119.137657	54.279335
3005.671206	119.997834	54.284340
3004.973560	108.888672	54.289345
3004.303973	121.693579	54.294349
3003.774496	122.463008	54.299354
3003.117438	123.127926	54.304359
3001.577366	123.620060	54.309364
3001.375306	122.418324	54.314369
3001.246841	130.184841	54.319373
3000.203561	117.426359	54.324378
2999.380788	125.643090	54.329383
2998.445650	132.849183	54.334388
2998.210031	122.101181	54.339393
2997.478378	122.510038	54.344397
2997.104979	119.301185	54.349402
2996.514613	122.330174	54.354407
2995.562999	118.378571	54.359412
2995.295464	120.016243	54.364417
2994.447323	127.303781	54.369421
2993.956243	132.285887	54.374426
2993.490377	123.651523	54.379431
2992.392817	137.521919	54.384436
2991.902178	121.820646	54.389441
2991.233029	127.029360	54.394445
2990.373355	119.258063	54.399450
2989.947493	122.629195	54.404455
2989.570766	124.648280	54.409460
2988.836294	119.120532	54.414465
2987.350619	123.151968	54.419469
2986.362577	116.020358	54.424474
2986.458199	117.831228	54.429479
2986.275731	124.573181	54.434484
2985.050545	117.158813	54.439489
2983.988632	123.321990	54.444493
2983.231855	122.807533	54.449498
2983.092875	122.756305	54.454503
2982.248446	124.172437	54.459508
2982.358836	111.092085	54.464513
2981.709450	119.450101	54.469517
2981.315466	116.711336	54.474522
2979.659155	111.424409	54.479527
2978.402365	123.959804	54.484532
2978.660263	120.648599	54.489537
2977.548307	113.317120	54.494541
2977.071933	114.639962	54.499546
2976.351149	115.790628	54.504551
2975.471592	119.199028	54.509556
2975.226911	115.550956	54.514561
2974.607333	120.127135	54.519565
2973.790861	123.352259	54.524570
2973.450908	113.651150	54.529575
2972.792949	121.206574	54.534580
2972.540950	121.488468	54.539585
2971.642686	119.408626	54.544589
2970.654308	121.045932	54.549594
2969.598312	114.616317	54.554599
2969.037093	115.440119	54.559604
2968.870491	110.212036	54.564609
2967.958616	120.479597	54.569613
2967.678567	123.228590	54.574618
2967.021400	111.057019	54.579623
2966.286542	123.821766	54.584628
2965.601891	117.162907	54.589633
2964.283215	117.472746	54.594637
2963.388296	115.916532	54.599642
2963.291456	119.585902	54.604647
2962.288181	118.954892	54.609652
2961.834556	111.418551	54.614657
2961.265571	113.787456	54.619661
2960.882481	119.833446	54.624666
2960.075875	115.197088	54.629671
2959.350988	119.728897	54.634676
2959.266075	112.166256	54.639681
2958.286937	121.870592	54.644685
2957.381487	121.989425	54.649690
2956.471612	117.586235	54.654695
2955.507014	122.860439	54.659700
2955.769028	108.873941	54.664705
2954.883897	122.982754	54.669709
2954.018145	121.569579	54.674714
2953.508303	119.975980	54.679719
2952.570033	112.398912	54.684724
2952.587943	116.206957	54.689729
2951.841717	115.513864	54.694733
2950.840839	111.500430	54.699738
2950.007911	119.463903	54.704743
2949.171107	124.028655	54.709748
2948.667749	114.745069	54.714753
2947.790097	117.731972	54.719757
2947.171914	132.368712	54.724762
2946.863236	117.017666	54.729767
2945.971315	118.525600	54.734772
2945.956131	111.929177	54.739777
2945.179308	119.711356	54.744781
2944.466458	125.619101	54.749786
2944.370383	113.821767	54.754791
2942.724145	117.508028	54.759796
2942.035107	114.204311	54.764801
2941.505574	109.778760	54.769805
2940.620855	117.826476	54.774810
2940.365327	114.078421	54.779815
2939.437357	126.958670	54.784820
2939.313811	114.472890	54.789825
2938.619219	119.928315	54.794829
2937.821164	119.724858	54.799834
2936.808841	109.726172	54.804839
2935.854056	118.179009	54.809844
2935.418222	117.633001	54.814849
2934.863403	123.553607	54.819853
2934.195118	119.281631	54.824858
2934.059387	115.824938	54.829863
2933.321451	113.744942	54.834868
2932.753152	109.177994	54.839873
2931.921887	107.738405	54.844877
2930.589128	115.732034	54.849882
2930.241828	116.137187	54.854887
2929.100120	125.009199	54.859892
2928.784777	113.127764	54.864897
2928.067238	117.442008	54.869901
2927.692966	110.874586	54.874906
2927.329713	113.164915	54.879911
2926.576222	116.464541	54.884916
2926.464964	111.086086	54.889921
2925.544123	123.517495	54.894925
2924.370246	120.957803	54.899930
2923.780510	109.364047	54.904935
2922.776219	119.852661	54.909940
2922.106257	112.976570	54.914945
2921.826305	116.653548	54.919949
2921.287564	115.196731	54.924954
2921.147795	110.385634	54.929959
2919.986038	120.909843	54.934964
2919.151446	103.763085	54.939969
2918.223854	111.339717	54.944973
2917.575348	113.801556	54.949978
2917.006853	108.134542	54.954983
2916.668294	116.000108	54.959988
2916.207170	112.502713	54.964993
2915.837319	114.081689	54.969997
2914.469411	117.399873	54.975002
2913.942987	114.073502	54.980007
2912.837856	113.882660	54.985012
2912.442987	111.393126	54.990017
2911.857666	104.230214	54.995021
2911.176700	114.083717	55.000026
2910.614256	113.598821	55.005031
2909.830605	116.803737	55.010036
2909.508287	106.915292	55.015041
2908.442449	118.012829	55.020045
2907.159931	113.749517	55.025050
2907.096598	112.580919	55.030055
2906.554660	110.496641	55.035060
2906.019832	114.726373	55.040065
2905.198845	110.578788	55.045069
2904.685704	121.172936	55.050074
2904.609769	117.782602	55.055079
2903.744458	121.733693	55.060084
2902.554503	112.326673	55.065089
2901.486189	111.775472	55.070093
2900.949283	114.619281	55.075098
2900.654199	109.213036	55.080103
2899.812183	116.296245	55.085108
2899.367225	105.125769	55.090113
2898.644162	117.157462	55.095117
2898.496648	111.576790	55.100122
2898.116790	109.817304	55.105127
2896.783226	119.213933	55.110132
2895.812789	115.390303	55.115137
2895.302525	107.342616	55.120141
2894.416376	120.962140	55.125146
2894.141135	112.027597	55.130151
2893.856702	112.628055	55.135156
2893.464039	109.132383	55.140161
2892.166814	110.215788	55.145165
2891.165371	117.445847	55.150170
2890.841791	105.122949	55.155175
2890.060127	111.132450	55.160180
2889.342548	112.302315	55.165185
2889.106533	102.033215	55.170189
2888.340394	104.380162	55.175194
2887.423848	103.575664	55.180199
2886.202717	106.737719	55.185204
2886.013899	106.479885	55.190209
2885.477177	99.997867	55.195213
2884.625776	113.914202	55.200218
2884.438672	99.509094	55.205223
2883.855271	109.416181	55.210228
2883.373872	105.842521	55.215233
2882.203814	108.618096	55.220237
2881.129690	113.620504	55.225242
2880.646441	112.370913	55.230247
2879.766454	114.312199	55.235252
2879.222814	106.623894	55.240257
2878.904748	99.480840	55.245261
2878.268703	111.080036	55.250266
2878.394387	105.496492	55.255271
2877.333696	112.467472	55.260276
2876.134884	111.356358	55.265281
2875.276178	103.210336	55.270285
2874.895018	115.044650	55.275290
2874.737776	104.869849	55.280295
2874.153955	111.226054	55.285300
2872.951847	108.792382	55.290305
2872.103778	109.118916	55.295309
2871.114212	112.338501	55.300314
2871.034542	115.766124	55.305319
2870.239342	110.678638	55.310324
2869.920099	108.594593	55.315329
2869.862476	105.301789	55.320333
2867.981185	117.424064	55.325338
2867.545000	101.207103	55.330343
2866.774671	108.239376	55.335348
2866.500982	115.560973	55.340353
2866.045282	112.159364	55.345357
2865.115224	110.510097	55.350362
2864.765459	108.481794	55.355367
2863.312271	110.913403	55.360372
2862.376214	112.516521	55.365377
2862.115327	102.889947	55.370381
2861.770666	117.377688	55.375386
2861.149792	107.374885	55.380391
2860.826448	110.225617	55.385396
2860.042881	105.469294	55.390401
2859.476678	111.716308	55.395405
2858.274289	118.955846	55.400410
2857.269784	109.774903	55.405415
2856.110299	114.010346	55.410420
2856.573782	117.660922	55.415425
2855.901961	111.505142	55.420429
2854.870824	113.413845	55.425434
2854.599516	103.811947	55.430439
2854.059325	108.085622	55.435444
2853.865043	102.000201	55.440449
2852.739004	104.558263	55.445453
2851.437049	109.637506	55.450458
2851.315318	103.600868	55.455463
2850.624482	114.897203	55.460468
2849.964018	104.091587	55.465473
2849.768457	109.711981	55.470477
2848.342307	113.314072	55.475482
2847.861003	101.596416	55.480487
2846.699169	105.081886	55.485492
2846.232963	104.330688	55.490497
2845.961594	107.040698	55.495501
2845.469418	112.942307	55.500506
2844.949688	109.189681	55.505511
2843.982967	108.096143	55.510516
2842.809888	107.019716	55.515521
2842.490276	106.540692	55.520525
2841.662449	110.558405	55.525530
2841.259470	101.053618	55.530535
2840.507879	117.590850	55.535540
2840.136340	108.604092	55.540545
2839.742626	108.327991	55.545549
2838.939019	113.241540	55.550554
2838.085254	101.438337	55.555559
2836.629943	105.597635	55.560564
2836.217920	108.022614	55.565569
2836.026774	100.466701	55.570573
2835.320831	112.447307	55.575578
2835.089461	104.351176	55.580583
2834.406878	109.735869	55.585588
2833.436402	106.765263	55.590593
2832.560730	112.738732	55.595597
2831.992388	114.374531	55.600602
2831.547756	108.639784	55.605607
2831.229319	114.052633	55.610612
2830.217299	105.896904	55.615617
2828.985571	106.461116	55.620621
2828.511550	120.215855	55.625626
2828.025472	114.340957	55.630631
2827.022999	114.192980	55.635636
2826.970857	111.722243	55.640641
2826.349732	100.643473	55.645645
2825.853192	105.422831	55.650650
2824.631718	101.389105	55.655655
2823.956844	99.378084	55.660660
2823.310349	113.088481	55.665665
2822.928088	104.456840	55.670669
2822.311306	106.497223	55.675674
2822.217324	105.289262	55.680679
2820.573761	107.612501	55.685684
2819.597185	111.712085	55.690689
2819.415078	99.757383	55.695693
2818.693035	106.782590	55.700698
2818.363003	106.373636	55.705703
2817.626630	111.532267	55.710708
2817.135712	101.810415	55.715713
2816.303800	102.907858	55.720717
2815.325504	111.761024	55.725722
2814.627414	110.003437	55.730727
2814.151217	111.494018	55.735732
2814.068142	110.843518	55.740737
2813.386937	101.401289	55.745741
2811.742319	106.899884	55.750746
2811.278679	103.849762	55.755751
2810.454023	102.448141	55.760756
2809.566841	108.450025	55.765761
2809.474751	101.457431	55.770765
2808.701492	109.208608	55.775770
2808.533407	104.487228	55.780775
2807.771244	108.442801	55.785780
2807.325392	108.217849	55.790785
2807.124915	100.043815	55.795789
2805.651156	102.088568	55.800794
2804.770668	103.185631	55.805799
2804.085521	108.548264	55.810804
2803.523496	106.918603	55.815809
2803.869837	106.198262	55.820813
2802.503756	110.209689	55.825818
2801.393327	106.638949	55.830823
2801.291841	107.708259	55.835828
2800.366128	101.569442	55.840833
2800.100286	100.716899	55.845837
2798.845775	110.066868	55.850842
2798.007416	103.973908	55.855847
2797.372691	107.786914	55.860852
2796.784846	107.902407	55.865857
2796.609849	106.349488	55.870861
2795.843010	111.443856	55.875866
2795.627415	102.449403	55.880871
2794.363736	104.915740	55.885876
2793.100562	107.768033	55.890881
2792.864296	102.939100	55.895885
2792.384833	106.204137	55.900890
2791.982740	96.652633	55.905895
2791.365933	102.945004	55.910900
2790.563575	110.169462	55.915905
2790.214004	107.074978	55.920909
2788.998242	106.108092	55.925914
2788.279673	104.299537	55.930919
2787.750377	107.302705	55.935924
2787.176774	108.162586	55.940929
2787.265110	99.071979	55.945933
2785.590691	111.677181	55.950938
2785.159763	105.667344	55.955943
2784.212035	99.500322	55.960948
2783.095044	98.549713	55.965953
2783.354830	105.977089	55.970957
2782.193399	106.507192	55.975962
2782.101345	97.528731	55.980967
2781.589056	109.102825	55.985972
2780.270375	106.252928	55.990977
2780.029116	98.767954	55.995981
2779.115430	111.149187	56.000986
2778.657768	98.346354	56.005991
2778.394176	100.308609	56.010996
2777.756877	101.124905	56.016001
2776.649010	99.416049	56.021005
2775.461077	98.854925	56.026010
2775.207413	104.647083	56.031015
2774.624179	105.682291	56.036020
2774.091563	102.064112	56.041025
2773.596603	92.454673	56.046029
2772.000189	105.102196	56.051034
2771.557104	104.061665	56.056039
2771.121119	106.250750	56.061044
2770.585933	103.289044	56.066049
2770.211674	99.277099	56.071053
2769.910287	110.227794	56.076058
2769.081806	103.180285	56.081063
2767.947476	105.542021	56.086068
2767.326034	105.311559	56.091073
2766.625583	103.488859	56.096077
2766.017915	104.510086	56.101082
2765.346426	103.855954	56.106087
2764.962501	107.026902	56.111092
2763.406937	107.480695	56.116097
2763.188126	104.391100	56.121101
2762.409519	117.918822	56.126106
2761.967491	115.310261	56.131111
2761.874802	113.001190	56.136116
2761.365034	107.013515	56.141121
2760.489415	94.043319	56.146125
2759.027621	107.598598	56.151130
2758.536101	88.444906	56.156135
2758.070289	91.805105	56.161140
2757.472037	114.696458	56.166145
2757.315437	97.193487	56.171149
2755.970096	114.012192	56.176154
2755.516398	98.864015	56.181159
2754.723779	96.270384	56.186164
2754.099261	106.294230	56.191169
2753.682616	100.862994	56.196173
2753.023912	111.144126	56.201178
2751.863686	102.316666	56.206183
2751.136777	103.433274	56.211188
2750.436586	100.167811	56.216193
2750.388444	99.960540	56.221197
2749.807320	99.212810	56.226202
2749.323502	93.790690	56.231207
2748.382560	95.003879	56.236212
2747.190683	93.852137	56.241217
2746.811233	102.001778	56.246221
2746.179115	107.481267	56.251226
2745.720734	100.439581	56.256231
2745.268969	100.935624	56.261236
2744.484770	99.467890	56.266241
2743.758238	95.013677	56.271245
2742.569884	103.362370	56.276250
2742.225996	91.136533	56.281255
2741.758155	90.963502	56.286260
2741.179641	103.209284	56.291265
2740.456471	89.939890	56.296269
2739.557743	107.088422	56.301274
2738.881328	98.752597	56.306279
2738.650139	99.175807	56.311284
2737.501273	95.865463	56.316289
2736.670592	95.936814	56.321293
2735.749835	103.241113	56.326298
2735.346840	101.576779	56.331303
2734.844215	101.779551	56.336308
2734.295644	111.609635	56.341313
2733.719042	95.790125	56.346317
2733.320054	104.805976	56.351322
2732.597116	96.109038	56.356327
2731.612217	96.739235	56.361332
2730.630574	102.847266	56.366337
2730.168894	98.258971	56.371341
2729.703921	106.465467	56.376346
2728.944555	99.494573	56.381351
2728.877409	104.193038	56.386356
2728.196937	103.361637	56.391361
2727.445300	93.305831	56.396365
2726.355093	95.997915	56.401370
2725.709645	101.127587	56.406375
2725.229014	98.933777	56.411380
2724.004936	103.378826	56.416385
2723.484224	89.900362	56.421389
2722.289807	96.403961	56.426394
2722.603267	100.092396	56.431399
2721.777644	94.710152	56.436404
2721.031688	94.943072	56.441409
2720.678127	93.856851	56.446413
2720.442277	98.937035	56.451418
2719.284936	89.284124	56.456423
2718.452125	92.701926	56.461428
2717.301658	104.026688	56.466433
2717.060957	88.501475	56.471437
2716.684809	94.826129	56.476442
2716.423472	93.173897	56.481447
2715.097919	91.651076	56.486452
2714.522314	108.061108	56.491457
2713.963325	101.085175	56.496461
2713.290337	99.722380	56.501466
2712.653279	104.559707	56.506471
2711.870868	95.868203	56.511476
2710.580305	108.352934	56.516481
2710.335764	97.359028	56.521485
2709.497245	104.931107	56.526490
2709.425808	106.548291	56.531495
2708.917112	103.047212	56.536500
2708.110466	104.275741	56.541505
2707.551033	94.586547	56.546509
2706.699758	99.884820	56.551514
2706.229003	92.877626	56.556519
2705.712469	98.338147	56.561524
2704.289105	101.914528	56.566529
2703.775844	97.222951	56.571533
2703.244399	106.754454	56.576538
2702.578299	109.966533	56.581543
2702.356006	108.844454	56.586548
2701.362736	104.833723	56.591553
2700.725315	105.890436	56.596557
2699.476798	106.797009	56.601562
2698.738232	98.075118	56.606567
2698.501993	98.583270	56.611572
2697.832152	97.572823	56.616577
2697.676104	99.143682	56.621581
2696.958909	96.412830	56.626586
2696.353847	106.005468	56.631591
2695.899105	97.857149	56.636596
2694.251585	108.924259	56.641601
2694.162100	99.047369	56.646605
2693.459555	101.447411	56.651610
2693.074191	104.411376	56.656615
2692.060885	100.758932	56.661620
2691.001807	114.615243	56.666625
2690.532340	102.138118	56.671629
2690.019207	106.248101	56.676634
2689.325059	109.764572	56.681639
2689.329962	99.428666	56.686644
2688.078488	101.026121	56.691649
2687.326141	95.207424	56.696653
2686.202521	100.918163	56.701658
2685.975810	103.591332	56.706663
2685.844307	102.931746	56.711668
2685.444613	109.751863	56.716673
2685.268893	105.871378	56.721677
2684.014643	106.512890	56.726682
2683.220247	109.654930	56.731687
2682.159522	104.622739	56.736692
2680.913750	112.279042	56.741697
2680.313301	100.003912	56.746701
2679.734843	109.023600	56.751706
2679.120817	109.198053	56.756711
2679.090296	102.475201	56.761716
2678.379264	108.553166	56.766721
2678.340805	100.366847	56.771725
2676.844332	93.441443	56.776730
2675.865520	106.081300	56.781735
2675.398247	102.688010	56.786740
2674.882547	106.034639	56.791745
2674.563461	107.289168	56.796749
2673.739854	101.600281	56.801754
2672.341746	99.769356	56.806759
2672.334553	107.273540	56.811764
2671.054078	109.906979	56.816769
2670.833527	98.560435	56.821773
2670.258579	102.466649	56.826778
2669.784374	100.983435	56.831783
2669.663810	106.033651	56.836788
2668.273655	107.637054	56.841793
2667.718443	105.056141	56.846797
2667.037545	107.632087	56.851802
2666.397562	106.402994	56.856807
2665.986022	108.640009	56.861812
2664.798586	102.824638	56.866817
2664.092582	93.399318	56.871821
2663.559195	105.061087	56.876826
2663.233354	110.727035	56.881831
2662.732653	100.659923	56.886836
2661.279601	101.750674	56.891841
2660.947010	99.446303	56.896845
2660.376336	106.022892	56.901850
2659.460713	97.316672	56.906855
2659.384742	101.605339	56.911860
2658.869738	108.674107	56.916865
2657.856388	104.059732	56.921869
2656.764983	104.283819	56.926874
2656.141350	102.710100	56.931879
2655.793261	91.074323	56.936884
2655.276725	106.490992	56.941889
2654.984109	102.141033	56.946893
2654.027773	99.741979	56.951898
2653.419809	101.907575	56.956903
2652.762444	101.081311	56.961908
2651.206584	106.268332	56.966913
2650.559389	95.893909	56.971917
2650.660467	100.237965	56.976922
2649.297769	100.747633	56.981927
2649.130563	94.907073	56.986932
2648.319423	102.832095	56.991937
2647.848263	100.230896	56.996941
2647.725487	102.964849	57.001946
2646.694222	102.669857	57.006951
2645.905227	92.658351	57.011956
2645.254980	100.262193	57.016961
2644.496857	96.623768	57.021965
2644.099389	101.009628	57.026970
2643.443521	106.087800	57.031975
2642.443117	98.718405	57.036980
2641.303798	105.044448	57.041985
2640.971172	97.645766	57.046989
2640.758559	95.776401	57.051994
2639.610416	100.861357	57.056999
2639.879160	94.745360	57.062004
2638.683823	104.230487	57.067009
2637.690112	98.458191	57.072013
2637.192972	105.035235	57.077018
2636.663801	108.794684	57.082023
2636.487717	104.071133	57.087028
2635.055361	107.088557	57.092033
2634.303582	100.399403	57.097037
2633.670387	100.749238	57.102042
2632.963553	95.191185	57.107047
2632.759387	93.536291	57.112052
2632.329290	98.647706	57.117057
2631.808509	92.965483	57.122061
2631.084602	98.662765	57.127066
2629.949022	106.411154	57.132071
2629.381133	96.879731	57.137076
2629.147126	99.657960	57.142081
2627.871132	92.358972	57.147085
2627.161275	94.825795	57.152090
2626.197598	98.397028	57.157095
2625.922239	101.438897	57.162100
2625.485196	108.485260	57.167105
2624.814330	100.310742	57.172109
2624.613088	99.276249	57.177114
2623.038329	99.479553	57.182119
2622.415273	97.359837	57.187124
2621.836592	98.039817	57.192129
2621.390120	96.963171	57.197133
2620.597652	91.884746	57.202138
2620.734653	105.306853	57.207143
2619.636937	98.996962	57.212148
2618.647012	99.172525	57.217153
2618.117369	102.587460	57.222157
2617.231157	96.742715	57.227162
2616.626401	102.832513	57.232167
2616.545952	95.408094	57.237172
2615.416781	107.547885	57.242177
2614.722817	95.427309	57.247181
2613.765826	98.059930	57.252186
2613.683302	93.944844	57.257191
2613.358948	94.883311	57.262196
2612.256776	99.937519	57.267201
2611.624404	94.275559	57.272205
2610.748921	101.953432	57.277210
2609.964990	96.842365	57.282215
2609.869122	97.023769	57.287220
2608.692955	106.989557	57.292225
2607.738597	101.940385	57.297229
2607.519145	98.302640	57.302234
2606.733905	106.567833	57.307239
2606.886439	103.587657	57.312244
2605.681791	103.603357	57.317249
2604.703918	97.162461	57.322253
2604.047116	100.284143	57.327258
2603.028554	104.651449	57.332263
2603.026342	101.036170	57.337268
2602.126473	107.215498	57.342273
2601.590492	97.393240	57.347277
2601.656304	102.977232	57.352282
2600.545300	103.318361	57.357287
2599.715841	95.927254	57.362292
2599.140781	104.708736	57.367297
2598.850211	97.874826	57.372301
2597.540868	104.527563	57.377306
2596.968836	102.069532	57.382311
2596.865332	96.122564	57.387316
2595.720438	104.474897	57.392321
2594.656499	100.817709	57.397325
2594.213703	92.642501	57.402330
2593.195601	112.963317	57.407335
2593.235203	98.956075	57.412340
2592.826481	105.604844	57.417345
2592.127134	93.967943	57.422349
2591.041353	95.164867	57.427354
2589.868732	96.680574	57.432359
2589.944134	98.613301	57.437364
2589.180033	98.674871	57.442369
2588.675303	96.630849	57.447373
2587.843776	94.399545	57.452378
2586.863772	102.210153	57.457383
2586.378089	93.572555	57.462388
2585.897267	99.339991	57.467393
2585.412799	94.226681	57.472397
2583.880920	96.387998	57.477402
2582.646686	103.434068	57.482407
2583.191414	96.874586	57.487412
2582.091935	96.809551	57.492417
2581.518415	100.737630	57.497421
2581.132516	93.311752	57.502426
2580.739815	99.606080	57.507431
2580.250663	95.759847	57.512436
2580.037497	100.516425	57.517441
2578.644097	101.998828	57.522445
2577.851799	108.299106	57.527450
2577.250148	107.757792	57.532455
2575.975022	101.937701	57.537460
2575.245460	100.596833	57.542465
2574.999041	102.299192	57.547469
2574.655282	95.699768	57.552474
2573.588184	104.963644	57.557479
2573.449297	94.653915	57.562484
2572.607325	105.424255	57.567489
2572.156717	101.527618	57.572493
2571.470424	102.715854	57.577498
2570.336570	104.964651	57.582503
2569.908598	96.180614	57.587508
2569.488954	99.796606	57.592513
2568.677862	95.644635	57.597517
2567.986398	93.151371	57.602522
2566.946808	106.600150	57.607527
2566.956627	94.178485	57.612532
2566.556716	95.196581	57.617537
2565.825122	96.501505	57.622541
2565.400839	101.149706	57.627546
2564.211559	104.751228	57.632551
2562.980094	96.908610	57.637556
2562.040291	100.037231	57.642561
2561.351880	103.026168	57.647565
2561.039734	99.570057	57.652570
2560.244456	100.424042	57.657575
2560.250641	97.081268	57.662580
2559.457209	99.205555	57.667585
2559.059061	97.899607	57.672589
2558.422550	92.601512	57.677594
2556.970368	99.080521	57.682599
2556.641816	92.229430	57.687604
2556.058155	93.931024	57.692609
2555.341764	90.778492	57.697613
2555.090010	85.658561	57.702618
2553.896645	99.605319	57.707623
2553.507555	99.048589	57.712628
2552.312260	107.812954	57.717633
2551.915141	96.200575	57.722637
2551.945461	101.282620	57.727642
2550.832642	103.343883	57.732647
2550.127994	106.142972	57.737652
2549.579607	94.385145	57.742657
2549.093002	99.957393	57.747661
2548.578165	101.691037	57.752666
2546.820164	113.609932	57.757671
2546.260835	101.391354	57.762676
2545.932264	106.616070	57.767681
2545.202684	105.799403	57.772685
2544.992331	107.325471	57.777690
2544.358130	104.445062	57.782695
2543.654465	105.302334	57.787700
2542.756140	102.576814	57.792705
2541.780189	100.365866	57.797709
2541.501625	95.776289	57.802714
2541.094512	105.025621	57.807719
2540.364921	100.193425	57.812724
2539.728006	96.899811	57.817729
2538.585299	102.611860	57.822733
2538.254637	97.868958	57.827738
2537.625984	99.447593	57.832743
2537.178349	98.804955	57.837748
2536.485792	102.686680	57.842753
2535.290640	100.997930	57.847757
2535.132934	97.482657	57.852762
2533.920187	98.104080	57.857767
2533.610335	102.771796	57.862772
2533.336785	93.689006	57.867777
2532.027071	101.736771	57.872781
2531.538932	91.021380	57.877786
2530.702278	98.232370	57.882791
2530.386263	94.217601	57.887796
2529.765029	94.662899	57.892801
2529.338257	94.919035	57.897805
2528.187758	87.194427	57.902810
2527.325587	97.196926	57.907815
2526.909741	85.778413	57.912820
2526.847706	101.184860	57.917825
2525.862886	101.166941	57.922829
2524.947418	95.307483	57.927834
2523.898677	103.156690	57.932839
2523.411980	95.159913	57.937844
2523.165472	97.908307	57.942849
2522.561578	108.657290	57.947853
2522.349138	95.029853	57.952858
2520.810400	101.357095	57.957863
2520.608825	92.546203	57.962868
2519.946813	98.471324	57.967873
2518.689755	90.534417	57.972877
2517.797134	90.060620	57.977882
2517.455526	102.606143	57.982887
2516.918803	95.891695	57.987892
2516.273205	95.966962	57.992897
2515.699190	92.980746	57.997901
2515.688580	88.612985	58.002906
2514.997751	97.464386	58.007911
2513.911049	90.645423	58.012916
2512.930186	95.450753	58.017921
2512.494864	95.562304	58.022925
2512.067738	99.010241	58.027930
2510.682216	92.709326	58.032935
2509.965694	92.448178	58.037940
2509.392557	93.356950	58.042945
2508.836567	101.416772	58.047949
2508.856205	88.245044	58.052954
2508.071087	101.312825	58.057959
2507.534481	91.212416	58.062964
2506.841836	86.131949	58.067969
2505.724017	87.394362	58.072973
2505.627798	93.545634	58.077978
2504.754848	94.536848	58.082983
2503.663210	98.045899	58.087988
2503.039554	103.265014	58.092993
2502.229896	103.859763	58.097997
2502.215291	96.615539	58.103002
2501.699307	97.029424	58.108007
2500.882970	94.923823	58.113012
2499.868967	88.659260	58.118017
2499.089232	98.821741	58.123021
2498.696819	86.905426	58.128026
2498.297696	96.198384	58.133031
2497.249594	89.657818	58.138036
2496.259000	100.077790	58.143041
2495.392024	109.619687	58.148045
2494.724680	88.515802	58.153050
2494.564649	91.659924	58.158055
2494.213245	98.162710	58.163060
2493.855709	96.095507	58.168065
2492.612679	99.962801	58.173069
2492.019350	91.762033	58.178074
2491.363438	99.470660	58.183079
2490.854453	99.066271	58.188084
2490.461260	101.510151	58.193089
2488.837464	103.787468	58.198093
2488.367559	93.380405	58.203098
2487.705597	100.856785	58.208103
2487.429715	103.202453	58.213108
2487.126829	94.343362	58.218113
2486.200284	96.615938	58.223117
2485.559867	97.439509	58.228122
2484.771948	96.382965	58.233127
2484.258846	91.525215	58.238132
2483.813633	91.135976	58.243137
2482.609327	100.402001	58.248141
2481.960526	85.532386	58.253146
2481.210288	92.840705	58.258151
2480.899602	93.702239	58.263156
2480.491450	81.822174	58.268161
2479.197563	94.196172	58.273165
2478.757910	97.739012	58.278170
2477.999035	94.609545	58.283175
2477.454630	96.941519	58.288180
2477.139741	93.140109	58.293185
2476.004851	99.096742	58.298189
2475.311416	98.633499	58.303194
2474.886656	97.322241	58.308199
2473.981648	92.218482	58.313204
2473.775631	89.401847	58.318209
2472.970700	95.685736	58.323213
2472.262285	90.008779	58.328218
2471.462348	92.793771	58.333223
2470.833128	91.989561	58.338228
2470.557341	91.954237	58.343233
2469.764477	98.482767	58.348237
2468.348193	89.897332	58.353242
2467.710540	91.817764	58.358247
2467.348635	103.102454	58.363252
2466.911007	88.030951	58.368257
2466.282226	92.753590	58.373261
2465.988848	89.020738	58.378266
2465.326549	93.065445	58.383271
2464.454019	99.866536	58.388276
2463.463665	90.856974	58.393281
2462.970027	94.748901	58.398285
2462.239304	87.049249	58.403290
2460.553536	86.173852	58.408295
2460.193176	93.027103	58.413300
2460.251371	91.729584	58.418305
2460.005772	101.826005	58.423309
2459.539725	91.526443	58.428314
2459.017177	91.666727	58.433319
2457.395037	92.000543	58.438324
2456.654718	84.910803	58.443329
2455.966538	92.176144	58.448333
2455.866361	86.339540	58.453338
2455.270110	91.018328	58.458343
2454.691414	87.447547	58.463348
2453.857838	89.197406	58.468353
2453.089815	87.577747	58.473357
2452.713435	89.988359	58.478362
2451.587807	97.876374	58.483367
2450.625541	86.997339	58.488372
2450.404645	91.501822	58.493377
2449.695943	95.154610	58.498381
2449.267379	79.399487	58.503386
2448.680514	88.720987	58.508391
2447.256168	83.819320	58.513396
2446.677788	81.104247	58.518401
2446.195710	92.058961	58.523405
2445.758576	88.002939	58.528410
2445.152668	92.100372	58.533415
2444.989161	82.714980	58.538420
2444.358101	84.503632	58.543425
2443.038783	88.860013	58.548429
2442.461085	71.982542	58.553434
2442.162262	90.678814	58.558439
2441.120063	92.867359	58.563444
2440.242244	85.444696	58.568449
2439.298053	91.743713	58.573453
2439.165357	87.466697	58.578458
2438.690923	91.738224	58.583463
2438.177743	82.640375	58.588468
2437.117235	90.038060	58.593473
2435.986993	100.672171	58.598477
2435.815034	90.469168	58.603482
2435.533098	98.041224	58.608487
2434.898213	90.413212	58.613492
2434.078514	81.170808	58.618497
2433.006092	91.233335	58.623501
2432.624697	91.075154	58.628506
2432.122334	89.962688	58.633511
2431.133842	84.393233	58.638516
2430.451868	82.230726	58.643521
2429.734493	94.590231	58.648525
2429.461281	83.925352	58.653530
2428.410072	95.323946	58.658535
2428.107188	93.097014	58.663540
2427.018354	87.982464	58.668545
2425.947262	89.920170	58.673549
2425.789748	83.166956	58.678554
2425.583760	91.585336	58.683559
2424.930419	90.383427	58.688564
2424.712637	83.723016	58.693569
2423.612790	88.993553	58.698573
2422.951505	91.071971	58.703578
2422.037719	83.895850	58.708583
2420.943434	80.436917	58.713588
2420.267260	84.475314	58.718593
2419.348146	86.689788	58.723597
2419.244184	84.507790	58.728602
2418.349375	88.047537	58.733607
2418.052325	84.634650	58.738612
2417.852810	82.122424	58.743617
2416.994492	87.678889	58.748621
2415.876493	80.427166	58.753626
2414.673774	84.685854	58.758631
2414.648114	93.555753	58.763636
2414.486803	87.863021	58.768641
2413.844037	88.711868	58.773645
2413.091297	84.304039	58.778650
2411.838991	87.434404	58.783655
2411.466447	83.019592	58.788660
2411.037564	74.211672	58.793665
2410.170109	91.223782	58.798669
2409.202007	74.570962	58.803674
2408.107006	86.591228	58.808679
2407.498040	92.094008	58.813684
2407.744830	88.247090	58.818689
2407.070904	94.467138	58.823693
2406.792648	84.839668	58.828698
2405.208903	88.531952	58.833703
2404.550562	89.653454	58.838708
2404.091999	85.911749	58.843713
2403.529137	89.746438	58.848717
2403.449222	88.959624	58.853722
2402.508007	89.562276	58.858727
2401.435493	91.264580	58.863732
2400.956885	90.152398	58.868737
2400.165810	87.424359	58.873741
2399.365660	82.547024	58.878746
2398.567003	85.637321	58.883751
2397.993579	94.624564	58.888756
2397.744720	92.250244	58.893761
2397.233328	88.889402	58.898765
2396.640785	87.088174	58.903770
2395.856536	82.971911	58.908775
2395.053979	87.447959	58.913780
2394.670339	81.394182	58.918785
2393.259166	87.977913	58.923789
2392.588153	88.074907	58.928794
2392.129884	89.449559	58.933799
2391.103377	79.796491	58.938804
2391.013369	81.487897	58.943809
2390.393034	84.823219	58.948813
2390.013745	82.414364	58.953818
2388.772081	82.307366	58.958823
2387.951047	85.450435	58.963828
2387.737043	81.730861	58.968833
2386.936516	99.411644	58.973837
2386.584928	89.285941	58.978842
2385.233157	84.178074	58.983847
2384.625642	91.487255	58.988852
2384.272478	83.592803	58.993857
2383.172129	91.921354	58.998861
2383.110228	90.954624	59.003866
2382.673275	81.001808	59.008871
2382.164449	83.226654	59.013876
2381.279067	82.806509	59.018881
2380.503100	89.767137	59.023885
2380.296531	87.940569	59.028890
2378.676943	89.470773	59.033895
2377.646219	87.777630	59.038900
2377.215944	84.601072	59.043905
2376.691955	86.616940	59.048909
2376.435294	90.100862	59.053914
2376.279651	83.659560	59.058919
2375.382789	86.069176	59.063924
2374.811952	81.179477	59.068929
2373.923855	83.951529	59.073933
2373.395457	83.248113	59.078938
2372.995174	87.871291	59.083943
2371.282500	87.083415	59.088948
2370.715315	80.735774	59.093953
2370.105907	85.626808	59.098957
2369.892151	89.352464	59.103962
2369.765845	85.203435	59.108967
2368.958008	86.810751	59.113972
2368.216788	82.254914	59.118977
2366.985630	84.618276	59.123981
2366.400926	79.845025	59.128986
2366.062410	78.042600	59.133991
2364.489622	89.656693	59.138996
2364.088351	77.793242	59.144001
2363.266470	84.325946	59.149005
2363.309658	84.141746	59.154010
2363.069973	85.298633	59.159015
2362.025106	94.612798	59.164020
2361.629876	80.094587	59.169025
2360.002187	89.109343	59.174029
2359.894287	82.233973	59.179034
2359.132258	78.916786	59.184039
2358.682964	80.444636	59.189044
2358.704343	83.607074	59.194049
2357.364526	89.569553	59.199053
2356.617343	76.268463	59.204058
2355.745104	79.317269	59.209063
2355.324097	96.573557	59.214068
2354.144963	84.980083	59.219073
2353.651849	89.636898	59.224077
2352.651211	87.507577	59.229082
2352.494631	86.572827	59.234087
2352.384611	88.594881	59.239092
2352.283926	77.286328	59.244097
2351.238474	83.842658	59.249101
2350.168698	81.669505	59.254106
2349.477526	81.062213	59.259111
2347.991291	85.217819	59.264116
2347.651758	76.731329	59.269121
2346.899771	79.204198	59.274125
2346.868878	80.437089	59.279130
2346.176325	77.885629	59.284135
2345.425953	82.949578	59.289140
2345.481862	81.819025	59.294145
2343.520066	83.734981	59.299149
2343.233569	77.165276	59.304154
2342.741028	78.724205	59.309159
2342.054091	85.858289	59.314164
2342.275709	83.354577	59.319169
2341.449535	82.579720	59.324173
2340.653275	78.345922	59.329178
2339.065763	80.622204	59.334183
2338.279009	80.334800	59.339188
2337.961109	79.335271	59.344193
2337.488563	79.337152	59.349197
2337.126296	79.528194	59.354202
2336.506150	89.817721	59.359207
2335.272997	88.210121	59.364212
2334.613729	81.366276	59.369217
2333.630728	82.193973	59.374221
2333.486064	84.319842	59.379226
2333.256980	82.776196	59.384231
2332.158982	82.629644	59.389236
2331.200633	74.842245	59.394241
2330.245536	87.281078	59.399245
2330.054338	77.985304	59.404250
2329.742532	75.073880	59.409255
2328.969499	89.585849	59.414260
2328.683688	76.981108	59.419265
2327.642946	88.602512	59.424269
2326.705410	80.462616	59.429274
2326.207880	83.319065	59.434279
2326.023419	88.482028	59.439284
2325.474460	83.277949	59.444289
2323.792546	80.818703	59.449293
2323.476883	94.312235	59.454298
2323.062343	91.978094	59.459303
2321.942309	91.889784	59.464308
2321.780201	85.253810	59.469313
2320.469212	87.351368	59.474317
2319.917345	85.116893	59.479322
2319.459525	88.021815	59.484327
2318.577122	88.394168	59.489332
2318.293601	83.699680	59.494337
2317.868463	90.627161	59.499341
2317.295323	83.485969	59.504346
2316.517421	82.251298	59.509351
2315.565252	79.007684	59.514356
2315.056878	80.331306	59.519361
2314.720857	84.133918	59.524365
2313.524475	73.424043	59.529370
2312.877148	78.776283	59.534375
2312.088526	86.350110	59.539380
2311.853654	84.854427	59.544385
2311.308038	80.486197	59.549389
2310.350336	85.341666	59.554394
2309.277113	80.627490	59.559399
2308.914495	82.241571	59.564404
2308.396502	68.154887	59.569409
2308.007886	81.098403	59.574413
2307.177112	82.650835	59.579418
2306.541503	75.148502	59.584423
2305.591472	84.639468	59.589428
2305.223664	74.824052	59.594433
2304.843645	74.102375	59.599437
2303.653570	74.856938	59.604442
2302.938802	75.866920	59.609447
2302.212136	76.901041	59.614452
2302.155925	80.493967	59.619457
2301.295319	83.162252	59.624461
2300.217692	76.924018	59.629466
2299.439217	82.989847	59.634471
2298.597327	73.540889	59.639476
2298.342054	73.133000	59.644481
2297.988553	78.971028	59.649485
2297.744253	74.591930	59.654490
2296.758828	74.675600	59.659495
2295.546320	80.946304	59.664500
2295.292485	74.796927	59.669505
2294.501875	75.110957	59.674509
2294.131727	76.821848	59.679514
2293.023238	67.446511	59.684519
2292.103175	71.048613	59.689524
2291.592388	69.633273	59.694529
2291.547364	72.176296	59.699533
2290.938139	69.709671	59.704538
2290.167248	65.638121	59.709543
2289.331085	77.095065	59.714548
2289.122429	75.499773	59.719553
2287.878905	76.931745	59.724557
2286.585397	79.982734	59.729562
2286.600305	82.555772	59.734567
2285.685001	85.806155	59.739572
2285.574616	76.112109	59.744577
2285.087831	78.421610	59.749581
2283.889744	77.876147	59.754586
2283.225149	74.184298	59.759591
2282.180661	76.444703	59.764596
2281.858709	69.561348	59.769601
2281.475739	75.653484	59.774605
2281.064035	82.461037	59.779610
2280.457625	81.293752	59.784615
2279.259399	79.543620	59.789620
2278.874932	77.367758	59.794625
2278.104049	82.199571	59.799629
2277.042915	78.662768	59.804634
2276.497623	76.146528	59.809639
2275.629911	83.512837	59.814644
2275.036748	68.138800	59.819649
2274.829526	73.881550	59.824653
2274.381882	85.129170	59.829658
2273.712384	77.563167	59.834663
2272.642336	87.164263	59.839668
2271.790213	81.965854	59.844673
2271.465283	78.161843	59.849677
2271.044948	82.671613	59.854682
2269.776317	81.938487	59.859687
2268.602848	80.082284	59.864692
2268.201009	71.742249	59.869697
2268.071688	77.943372	59.874701
2267.602561	84.542464	59.879706
2267.543346	77.131430	59.884711
2266.252207	81.586441	59.889716
2265.348934	81.595675	59.894721
2264.817614	80.423446	59.899725
2264.570554	89.129487	59.904730
2263.855779	78.207006	59.909735
2262.740184	79.378693	59.914740
2261.597721	70.669545	59.919745
2261.426364	74.560045	59.924750
2260.702781	82.677730	59.929754
2260.940825	79.147694	59.934759
2259.541466	73.781963	59.939764
2258.519209	91.289473	59.944769
2258.360062	76.684733	59.949774
2257.688961	83.633749	59.954778
2257.538229	76.226919	59.959783
2255.993665	81.616555	59.964788
2255.665372	81.651798	59.969793
2254.802537	73.418232	59.974798
2254.131586	78.375056	59.979802
2253.268132	69.874766	59.984807
2252.339893	85.263109	59.989812
2252.070049	78.646359	59.994817
2251.299665	75.587190	59.999822
2250.956497	81.955538	60.004826
2250.750461	76.128768	60.009831
2250.010994	76.588395	60.014836
2248.899622	78.295791	60.019841
2248.069520	85.057665	60.024846
2247.441476	74.258907	60.029850
2247.721554	73.506450	60.034855
2246.579406	75.645409	60.039860
2245.552232	75.815172	60.044865
2245.031283	76.851223	60.049870
2244.646345	84.900734	60.054874
2243.602935	82.927561	60.059879
2242.793392	88.575172	60.064884
2241.798827	74.396719	60.069889
2241.468782	77.285711	60.074894
2241.272427	78.861493	60.079898
2241.295348	79.909923	60.084903
2239.807753	84.397748	60.089908
2239.013014	73.964987	60.094913
2238.785387	75.492829	60.099918
2237.643692	71.675747	60.104922
2236.954632	76.270155	60.109927
2236.141938	74.572518	60.114932
2235.254730	73.079459	60.119937
2235.202648	78.553318	60.124942
2234.640867	79.715165	60.129946
2234.214675	76.924755	60.134951
2232.709724	81.362261	60.139956
2232.479847	73.826476	60.144961
2231.638268	73.275711	60.149966
2231.119326	80.083841	60.154970
2230.828302	77.551357	60.159975
2229.512577	79.176473	60.164980
2229.237143	75.809249	60.169985
2228.274811	71.519800	60.174990
2227.676025	80.782942	60.179994
2227.388085	76.343817	60.184999
2226.139583	81.629934	60.190004
2225.827805	75.936116	60.195009
2225.324334	74.893334	60.200014
2224.814660	82.361435	60.205018
2224.237057	77.058854	60.210023
2223.306634	78.456240	60.215028
2222.165924	71.098334	60.220033
2222.364141	71.250764	60.225038
2221.142747	86.348204	60.230042
2220.149199	78.422383	60.235047
2219.387174	78.296946	60.240052
2219.035405	82.054491	60.245057
2218.709622	84.382645	60.250062
2218.255227	86.761610	60.255066
2218.033060	82.729641	60.260071
2216.838122	89.645491	60.265076
2215.930434	87.133999	60.270081
2215.395426	84.704819	60.275086
2214.087689	78.117555	60.280090
2213.440305	78.146980	60.285095
2212.971361	90.182951	60.290100
2212.451346	91.316342	60.295105
2212.049953	81.753779	60.300110
2211.489540	74.218080	60.305114
2211.344805	75.049271	60.310119
2209.520669	87.986853	60.315124
2208.802477	88.313773	60.320129
2208.774310	80.341268	60.325134
2207.951161	87.128799	60.330138
2208.004945	76.673291	60.335143
2206.739815	81.323200	60.340148
2206.158961	73.248255	60.345153
2206.175227	72.374737	60.350158
2204.989293	74.272517	60.355162
2204.055814	76.064362	60.360167
2203.239822	81.280066	60.365172
2202.577936	79.586246	60.370177
2201.988210	75.649904	60.375182
2200.778343	74.937533	60.380186
2200.513394	73.014781	60.385191
2199.664595	80.131947	60.390196
2199.420921	73.133770	60.395201
2199.185928	81.598144	60.400206
2198.048373	87.108442	60.405210
2197.288689	79.112632	60.410215
2196.441851	74.445029	60.415220
2195.315818	77.357661	60.420225
2195.453683	70.581195	60.425230
2194.590356	75.424876	60.430234
2194.541426	73.057827	60.435239
2193.537513	82.183423	60.440244
2193.073537	86.766184	60.445249
2192.218881	81.327051	60.450254
2191.348991	80.249837	60.455258
2190.896072	77.975958	60.460263
2190.258849	73.672755	60.465268
2189.612850	76.833277	60.470273
2188.636896	79.220920	60.475278
2187.871996	88.913120	60.480282
2187.611785	78.704729	60.485287
2187.302153	82.581775	60.490292
2186.589706	83.003632	60.495297
2185.502712	68.519707	60.500302
2184.886199	86.200966	60.505306
2184.244479	70.665921	60.510311
2183.739483	80.370111	60.515316
2182.529373	82.797407	60.520321
2182.318932	78.814751	60.525326
2181.246266	74.189722	60.530330
2181.163873	72.354166	60.535335
2180.604356	76.569200	60.540340
2179.442947	78.349901	60.545345
2178.915084	74.572318	60.550350
2178.108418	77.006006	60.555354
2178.260059	70.250079	60.560359
2177.372835	72.675834	60.565364
2175.730532	74.189059	60.570369
2175.802206	70.495248	60.575374
2174.850594	83.443469	60.580378
2174.525671	77.125875	60.585383
2173.797769	76.236742	60.590388
2172.396519	78.031623	60.595393
2172.052142	75.664974	60.600398
2171.589835	78.445936	60.605402
2171.447792	65.599548	60.610407
2170.711124	73.308565	60.615412
2169.528092	66.929720	60.620417
2169.092058	65.414771	60.625422
2168.279157	80.923116	60.630426
2168.072973	69.137656	60.635431
2166.850837	78.264656	60.640436
2166.005474	80.890089	60.645441
2165.801846	69.287739	60.650446
2165.323651	78.333289	60.655450
2165.067076	69.147406	60.660455
2163.676978	81.539065	60.665460
2162.403176	71.084449	60.670465
2162.632274	69.252459	60.675470
2161.867167	72.850575	60.680474
2161.570379	74.108021	60.685479
2160.264160	86.287583	60.690484
2159.515303	80.436034	60.695489
2159.020662	68.307164	60.700494
2158.131901	81.221345	60.705498
2158.027479	75.580094	60.710503
2157.609682	82.051201	60.715508
2155.909733	76.908618	60.720513
2155.173170	80.171867	60.725518
2154.667303	90.096466	60.730522
2154.478933	77.844157	60.735527
2153.984250	79.821083	60.740532
2153.421615	79.804442	60.745537
2153.522500	74.064527	60.750542
2151.967100	83.048011	60.755546
2150.991131	74.728429	60.760551
2150.954074	79.512109	60.765556
2149.737008	81.854552	60.770561
2149.225494	74.421024	60.775566
2148.063022	75.185109	60.780570
2148.256635	74.577694	60.785575
2147.771917	76.068592	60.790580
2146.198244	85.335851	60.795585
2145.825412	80.122203	60.800590
2144.947393	73.935922	60.805594
2144.907498	71.109057	60.810599
2144.206227	81.665075	60.815604
2142.680032	76.254761	60.820609
2142.397266	75.680668	60.825614
2141.775620	78.818478	60.830618
2141.440677	70.993582	60.835623
2141.261869	75.232710	60.840628
2140.058457	81.454122	60.845633
2138.957274	73.802120	60.850638
2137.947809	80.274954	60.855642
2137.564653	68.848572	60.860647
2137.456207	72.562527	60.865652
2137.079041	71.916557	60.870657
2136.487966	73.170261	60.875662
2135.292438	73.893425	60.880666
2134.906571	67.879542	60.885671
2134.651473	74.995425	60.890676
2133.352456	72.977974	60.895681
2132.593719	68.967134	60.900686
2132.124571	75.775826	60.905690
2131.397134	70.619280	60.910695
2130.900436	69.500748	60.915700
2129.349646	70.238494	60.920705
2128.863062	56.154389	60.925710
2128.486669	75.189113	60.930714
2128.008004	68.962163	60.935719
2127.596758	68.443598	60.940724
2127.591631	70.234953	60.945729
2126.891344	69.509650	60.950734
2125.578209	72.188647	60.955738
2124.956958	65.573603	60.960743
2123.859289	67.884576	60.965748
2122.675522	72.058757	60.970753
2122.477935	62.639777	60.975758
2122.078055	67.849442	60.980762
2121.739507	69.836373	60.985767
2121.152584	68.355525	60.990772
2120.129038	72.158500	60.995777
2119.890987	70.006162	61.000782
2118.611196	69.478264	61.005786
2118.715252	70.008361	61.010791
2117.741022	70.334481	61.015796
2116.567967	67.493020	61.020801
2115.719541	64.805633	61.025806
2114.824875	75.465776	61.030810
2114.871286	69.016393	61.035815
2114.577460	64.680917	61.040820
2114.272169	71.316323	61.045825
2113.018051	65.006889	61.050830
2112.152235	76.295231	61.055834
2111.457367	73.441847	61.060839
2110.808990	69.915406	61.065844
2109.905930	75.663884	61.070849
2109.219616	75.338415	61.075854
2108.452697	82.088703	61.080858
2107.850199	76.153714	61.085863
2107.243102	70.221093	61.090868
2107.026883	77.065073	61.095873
2106.731251	71.191279	61.100878
2106.190216	65.153812	61.105882
2105.442073	72.804797	61.110887
2104.653863	71.893227	61.115892
2103.376135	70.016611	61.120897
2102.414813	71.160363	61.125902
2101.581259	74.799797	61.130906
2101.689828	75.932256	61.135911
2101.499576	74.798810	61.140916
2100.543051	71.524805	61.145921
2100.674320	65.324190	61.150926
2099.083869	74.756552	61.155930
2098.268216	68.552512	61.160935
2098.056841	72.529588	61.165940
2096.653050	78.700414	61.170945
2096.084822	73.884523	61.175950
2095.367869	68.528437	61.180954
2094.903679	74.203035	61.185959
2094.457143	70.387082	61.190964
2093.852697	69.333955	61.195969
2093.484967	58.088497	61.200974
2092.439740	73.415921	61.205978
2091.563185	66.684689	61.210983
2091.386421	65.223686	61.215988
2090.660181	68.455569	61.220993
2089.994643	66.004526	61.225998
2089.025726	80.380257	61.231002
2088.010601	68.770676	61.236007
2087.892335	75.333832	61.241012
2087.457678	71.773601	61.246017
2086.854015	74.672295	61.251022
2085.783631	77.212678	61.256026
2085.186476	73.176972	61.261031
2084.513891	61.421179	61.266036
2083.245648	73.086631	61.271041
2082.432197	65.918703	61.276046
2081.893507	69.073904	61.281050
2081.745723	70.380469	61.286055
2081.438999	62.981795	61.291060
2080.794611	79.411802	61.296065
2080.430266	65.263373	61.301070
2079.198651	67.568845	61.306074
2078.491313	74.963389	61.311079
2077.862027	61.963923	61.316084
2077.159918	72.540605	61.321089
2077.121256	60.982688	61.326094
2075.974397	62.659081	61.331098
2074.940535	66.988806	61.336103
2074.683596	61.053929	61.341108
2074.039994	66.120159	61.346113
2073.637036	67.398137	61.351118
2072.680281	69.548442	61.356122
2072.033219	65.527986	61.361127
2071.528429	62.729726	61.366132
2070.401892	72.711927	61.371137
2069.549991	64.750084	61.376142
2068.715015	71.978572	61.381146
2068.487065	70.011213	61.386151
2068.337777	68.913786	61.391156
2067.826828	70.844949	61.396161
2066.904470	70.419339	61.401166
2065.992225	67.637092	61.406170
2065.531226	63.967296	61.411175
2064.729221	66.629927	61.416180
2063.658726	69.285986	61.421185
2063.037070	70.804654	61.426190
2062.501922	70.377153	61.431194
2061.972394	67.512864	61.436199
2061.851326	68.218830	61.441204
2060.793338	72.444136	61.446209
2059.939663	67.640371	61.451214
2059.309814	73.247387	61.456218
2058.526248	79.441599	61.461223
2058.132838	72.864958	61.466228
2057.804724	78.089588	61.471233
2057.039376	63.088872	61.476238
2056.127405	71.305098	61.481242
2055.046188	73.269862	61.486247
2055.192806	66.689663	61.491252
2054.199361	73.215814	61.496257
2053.315929	66.482610	61.501262
2052.390857	70.356379	61.506266
2052.149702	70.686980	61.511271
2051.385011	64.690937	61.516276
2050.897630	76.260326	61.521281
2050.312268	66.672823	61.526286
2049.009792	67.939279	61.531290
2048.596287	70.050346	61.536295
2048.322926	75.042197	61.541300
2047.981123	76.651150	61.546305
2047.404880	66.545004	61.551310
2045.969627	69.355823	61.556314
2045.207688	74.859914	61.561319
2044.835365	68.208225	61.566324
2044.406671	80.064014	61.571329
2043.884087	61.651645	61.576334
2042.406536	71.245092	61.581338
2042.075789	73.776197	61.586343
2041.699841	71.411409	61.591348
2041.163284	69.565917	61.596353
2040.156586	62.751175	61.601358
2039.540835	64.593296	61.606362
2038.128628	66.918614	61.611367
2038.226080	60.053157	61.616372
2037.329849	73.149000	61.621377
2037.288032	58.853446	61.626382
2036.863901	62.363643	61.631386
2035.874544	68.348327	61.636391
2035.459262	68.255574	61.641396
2034.201435	75.974408	61.646401
2033.353925	72.704664	61.651406
2032.850742	69.327865	61.656410
2032.056796	75.783975	61.661415
2031.715507	67.345206	61.666420
2031.403974	70.031308	61.671425
2030.382770	65.675005	61.676430
2029.590857	67.364110	61.681434
2029.325590	73.981618	61.686439
2028.734063	72.380784	61.691444
2026.839991	69.530053	61.696449
2026.367029	70.280819	61.701454
2025.844137	77.521453	61.706458
2025.999206	72.276335	61.711463
2025.306482	71.757376	61.716468
2025.011594	76.289506	61.721473
2023.540767	64.660799	61.726478
2022.920163	68.753663	61.731482
2022.381946	77.440809	61.736487
2021.653764	67.495652	61.741492
2021.439393	72.495964	61.746497
2021.209916	76.412982	61.751502
2020.148606	76.133513	61.756506
2019.346653	72.125349	61.761511
2018.337942	74.693482	61.766516
2017.650317	78.963992	61.771521
2016.905709	79.113094	61.776526
2016.065428	81.043361	61.781530
2015.851668	85.127818	61.786535
2015.654724	71.102731	61.791540
2014.348816	77.607735	61.796545
2013.709516	67.879867	61.801550
2013.023101	74.553232	61.806554
2012.277618	77.109101	61.811559
2012.296474	70.748513	61.816564
2011.094781	78.115920	61.821569
2010.250367	73.470836	61.826574
2009.649488	73.172606	61.831578
2009.408965	78.054634	61.836583
2009.584433	75.651573	61.841588
2007.729431	82.083147	61.846593
2006.958947	75.824031	61.851598
2006.610962	79.543435	61.856602
2006.103231	79.605441	61.861607
2004.864009	78.298161	61.866612
2003.500232	81.491487	61.871617
2004.082661	75.986166	61.876622
2003.082961	82.110386	61.881626
2002.644156	83.107538	61.886631
2002.259980	76.728658	61.891636
2001.517881	79.566176	61.896641
2000.890396	73.949284	61.901646
1999.949491	71.429705	61.906650
1999.102553	70.603590	61.911655
1999.150270	64.159914	61.916660
1997.831949	72.073039	61.921665
1997.096139	69.132734	61.926670
1996.770692	71.042037	61.931674
1995.719438	72.012515	61.936679
1995.896249	60.915492	61.941684
1994.297525	74.660039	61.946689
1993.881756	73.580965	61.951694
1993.179209	71.282313	61.956698
1992.615385	73.792109	61.961703
1992.708301	68.016857	61.966708
1991.162933	77.237854	61.971713
1989.851395	72.042707	61.976718
1989.819860	78.382215	61.981722
1989.240413	74.456384	61.986727
1989.236790	58.344508	61.991732
1988.702870	72.407016	61.996737
1988.003403	67.656225	62.001742
1987.264479	68.359731	62.006746
1986.285809	69.397133	62.011751
1985.048654	58.597648	62.016756
1984.415501	70.316699	62.021761
1983.792868	60.431261	62.026766
1983.888027	63.882232	62.031770
1982.948426	71.823333	62.036775
1982.281247	72.353521	62.041780
1981.188968	75.767633	62.046785
1980.825038	77.240644	62.051790
1980.201441	64.057078	62.056794
1979.313685	77.601458	62.061799
1978.778114	69.186459	62.066804
1977.713101	72.209080	62.071809
1977.119310	69.992086	62.076814
1977.002850	65.742330	62.081818
1976.541267	70.090221	62.086823
1975.797589	64.866226	62.091828
1974.922035	66.674247	62.096833
1974.494232	67.618205	62.101838
1973.564680	68.825225	62.106842
1972.714410	66.587768	62.111847
1971.627914	68.530160	62.116852
1970.998168	69.891544	62.121857
1970.465107	62.568314	62.126862
1970.174181	66.651756	62.131866
1969.485158	71.848917	62.136871
1969.288790	63.424842	62.141876
1968.693008	61.915925	62.146881
1967.579157	58.380719	62.151886
1966.801773	69.385919	62.156890
1966.299048	64.047683	62.161895
1966.475866	64.722428	62.166900
1965.282353	71.713849	62.171905
1964.368609	66.445136	62.176910
1963.608189	64.719656	62.181914
1962.474012	67.413862	62.186919
1961.950303	60.936895	62.191924
1961.192708	64.742552	62.196929
1960.755163	64.464543	62.201934
1960.337449	60.858406	62.206938
1960.011967	70.041635	62.211943
1959.426917	57.660663	62.216948
1958.355289	63.504304	62.221953
1957.282850	58.279716	62.226958
1956.779532	63.190511	62.231962
1956.179244	69.056149	62.236967
1956.214724	59.035636	62.241972
1955.600010	64.822033	62.246977
1954.507111	66.980647	62.251982
1953.842955	70.775058	62.256986
1953.008501	70.778098	62.261991
1952.233374	66.714441	62.266996
1951.445506	76.536488	62.272001
1950.542100	76.025949	62.277006
1950.116070	74.773772	62.282010
1949.948420	74.357622	62.287015
1949.564280	65.011629	62.292020
1948.693868	64.718860	62.297025
1947.870874	70.870482	62.302030
1947.687600	62.638372	62.307034
1946.274411	68.302825	62.312039
1945.385672	60.342581	62.317044
1944.626752	69.252208	62.322049
1944.130626	72.384743	62.327054
1943.749055	58.273244	62.332058
1943.074380	70.940017	62.337063
1943.250673	64.928277	62.342068
1942.189967	72.656820	62.347073
1941.384916	73.685448	62.352078
1940.818316	66.792284	62.357082
1939.939464	71.090381	62.362087
1938.486523	67.778577	62.367092
1937.763762	70.192414	62.372097
1937.767570	74.479638	62.377102
1937.162313	64.812673	62.382106
1936.762002	63.900295	62.387111
1936.652900	68.859701	62.392116
1935.699447	75.639147	62.397121
1934.784586	75.843437	62.402126
1934.284137	69.212498	62.407130
1932.594564	79.732337	62.412135
1931.487561	62.421782	62.417140
1931.706012	62.296409	62.422145
1931.393382	57.989827	62.427150
1930.786006	57.473253	62.432154
1930.023275	60.994408	62.437159
1929.950790	55.892829	62.442164
1928.825161	63.831415	62.447169
1927.946365	64.244660	62.452174
1927.715684	60.280097	62.457178
1926.319812	63.732733	62.462183
1925.863620	67.141451	62.467188
1924.903828	62.400868	62.472193
1924.351793	63.951058	62.477198
1924.202193	65.120967	62.482202
1923.616185	71.118370	62.487207
1923.127904	63.580258	62.492212
1921.910805	68.599353	62.497217
1921.305966	62.667171	62.502222
1920.705906	63.339825	62.507226
1919.991190	63.541455	62.512231
1919.344264	53.232315	62.517236
1918.402360	61.749708	62.522241
1917.723511	66.223976	62.527246
1917.426143	64.892163	62.532250
1917.042841	64.012006	62.537255
1916.621785	59.384910	62.542260
1915.646351	71.697759	62.547265
1914.920088	61.661124	62.552270
1914.510211	58.882171	62.557274
1913.045705	71.043435	62.562279
1912.624643	60.531842	62.567284
1912.168736	71.976238	62.572289
1911.632077	65.503862	62.577294
1911.308586	64.995958	62.582298
1909.453168	68.586031	62.587303
1909.094760	69.186161	62.592308
1908.721592	65.683720	62.597313
1908.029253	65.641534	62.602318
1907.749905	60.745074	62.607322
1906.884064	66.445757	62.612327
1906.214744	63.102926	62.617332
1905.301359	60.153941	62.622337
1904.506782	59.878203	62.627342
1904.556126	58.869165	62.632346
1903.676913	63.808747	62.637351
1902.748930	62.764023	62.642356
1902.306792	62.690875	62.647361
1901.595152	66.351314	62.652366
1901.141181	67.780524	62.657370
1900.106140	64.501445	62.662375
1899.154125	55.622867	62.667380
1898.873174	64.830049	62.672385
1898.243613	72.107878	62.677390
1898.032584	59.142296	62.682394
1896.696070	59.593592	62.687399
1895.987749	59.067056	62.692404
1895.079252	56.477617	62.697409
1894.435792	65.085266	62.702414
1894.123070	57.047410	62.707418
1893.699767	61.649268	62.712423
1893.297695	62.007801	62.717428
1893.196743	64.528805	62.722433
1891.931932	60.875371	62.727438
1891.702420	57.311648	62.732442
1890.424590	61.987072	62.737447
1889.431625	55.421461	62.742452
1888.866053	55.950855	62.747457
1888.593458	63.526410	62.752462
1887.692268	55.585286	62.757466
1886.588751	61.966474	62.762471
1886.347175	64.147999	62.767476
1885.819481	58.368410	62.772481
1884.907597	62.603876	62.777486
1884.333423	62.185833	62.782490
1883.230640	65.218878	62.787495
1882.446900	66.146372	62.792500
1881.900540	58.963982	62.797505
1881.405994	61.247205	62.802510
1881.324228	59.553258	62.807514
1880.766332	65.485064	62.812519
1880.309928	61.450574	62.817524
1879.574144	71.553040	62.822529
1878.724272	68.225708	62.827534
1878.100382	59.810449	62.832538
1876.339539	72.985142	62.837543
1875.848951	60.229622	62.842548
1875.577425	62.167991	62.847553
1875.069611	64.024424	62.852558
1874.543791	55.776329	62.857562
1874.649498	64.363171	62.862567
1873.454883	66.459863	62.867572
1872.360975	63.668868	62.872577
1871.733155	72.650805	62.877582
1871.775184	62.966268	62.882586
1870.008147	64.656047	62.887591
1869.508204	60.031006	62.892596
1868.947377	66.733019	62.897601
1868.252319	66.987739	62.902606
1868.079252	65.584533	62.907610
1867.774243	55.798724	62.912615
1867.018928	57.210810	62.917620
1866.330272	68.006234	62.922625
1864.714060	70.499913	62.927630
1864.127289	62.639993	62.932634
1863.252922	64.083895	62.937639
1863.035245	58.098118	62.942644
1862.624851	54.898883	62.947649
1862.145148	59.772880	62.952654
1861.941678	50.713356	62.957658
1860.492625	60.390765	62.962663
1859.991965	56.567527	62.967668
1859.388474	51.649956	62.972673
1859.110421	52.670138	62.977678
1857.930016	49.247003	62.982682
1856.987792	52.967813	62.987687
1856.501428	50.882452	62.992692
1856.406659	58.146935	62.997697
1855.436550	49.914862	63.002702
1854.344483	49.833708	63.007706
1853.570705	56.807799	63.012711
1853.271009	50.661198	63.017716
1852.932505	54.604758	63.022721
1852.433019	56.801199	63.027726
1851.539280	51.024642	63.032730
1850.538004	58.658157	63.037735
1849.978260	50.374033	63.042740
1849.786515	55.935705	63.047745
1848.071017	61.087843	63.052750
1847.416112	56.369324	63.057754
1847.047485	65.351909	63.062759
1846.740688	66.905936	63.067764
1846.323092	59.462716	63.072769
1846.002811	63.890641	63.077774
1845.116552	55.160690	63.082778
1843.852373	53.874695	63.087783
1843.100366	54.870578	63.092788
1842.886774	47.585084	63.097793
1842.037748	51.563887	63.102798
1841.837160	50.308281	63.107802
1840.011881	59.760337	63.112807
1839.648513	56.184390	63.117812
1839.046955	50.055491	63.122817
1838.691772	54.549382	63.127822
1838.623170	50.983002	63.132826
1837.988844	54.862312	63.137831
1836.867048	55.884360	63.142836
1836.735799	55.163972	63.147841
1836.074527	63.795195	63.152846
1835.060227	52.289773	63.157850
1834.073677	58.941864	63.162855
1833.561061	51.900548	63.167860
1832.822193	54.167946	63.172865
1831.610045	50.871821	63.177870
1830.956259	53.608589	63.182874
1830.411836	57.556199	63.187879
1830.152831	52.919547	63.192884
1829.732663	54.162985	63.197889
1829.439113	47.986521	63.202894
1828.571966	58.153691	63.207898
1827.899478	52.996493	63.212903
1827.300701	47.363679	63.217908
1826.224606	50.032181	63.222913
1824.453796	52.830597	63.227918
1824.602473	46.992138	63.232922
1823.830656	53.768534	63.237927
1823.200050	51.763117	63.242932
1823.064164	52.338206	63.247937
1822.154639	58.559111	63.252942
1822.139849	52.509418	63.257946
1821.422020	55.733966	63.262951
1820.340820	55.305185	63.267956
1819.551922	51.946910	63.272961
1819.147738	57.525983	63.277966
1818.870555	46.397720	63.282970
1817.638887	54.935487	63.287975
1816.872236	49.113116	63.292980
1816.388516	50.178357	63.297985
1815.684790	51.321108	63.302990
1814.625583	50.022155	63.307994
1813.800894	57.323893	63.312999
1813.396824	52.353658	63.318004
1813.506407	54.607332	63.323009
1812.155415	57.278663	63.328014
1812.242684	61.872505	63.333018
1811.566739	58.563190	63.338023
1810.528073	53.358126	63.343028
1810.034636	48.987368	63.348033
1809.081791	65.605905	63.353038
1808.021481	59.642337	63.358042
1807.616254	60.044045	63.363047
1807.067543	52.146447	63.368052
1806.712873	55.550034	63.373057
1806.092112	62.013233	63.378062
1804.739209	51.322040	63.383066
1803.928454	53.190047	63.388071
1803.862616	53.625657	63.393076
1803.223803	53.358020	63.398081
1803.089677	58.973382	63.403086
1801.903271	47.787935	63.408090
1801.112599	64.061367	63.413095
1800.474513	55.506062	63.418100
1800.214983	58.444576	63.423105
1799.110349	62.483304	63.428110
1798.499063	57.218537	63.433114
1797.874804	52.965686	63.438119
1797.279694	59.597778	63.443124
1796.169254	55.230752	63.448129
1795.189557	57.028592	63.453134
1794.994500	56.203866	63.458138
1794.402130	54.371113	63.463143
1793.754451	65.442539	63.468148
1793.360970	58.974108	63.473153
1793.179248	54.248451	63.478158
1792.486033	54.077356	63.483162
1791.574723	55.622322	63.488167
1790.632242	53.483174	63.493172
1789.732737	55.841217	63.498177
1788.396071	58.543654	63.503182
1788.352293	49.385373	63.508186
1787.840199	57.194130	63.513191
1787.312068	57.473980	63.518196
1787.270522	50.394308	63.523201
1786.029651	63.847921	63.528206
1785.380329	62.446869	63.533210
1784.599300	58.067691	63.538215
1784.131718	60.731948	63.543220
1783.689487	55.965604	63.548225
1782.200228	56.460431	63.553230
1781.653671	53.865137	63.558234
1780.917603	61.340787	63.563239
1780.653430	59.625162	63.568244
1780.390409	57.016089	63.573249
1779.228741	59.322679	63.578254
1778.612493	47.155117	63.583258
1777.890360	48.619165	63.588263
1777.524797	57.651743	63.593268
1777.389027	45.323027	63.598273
1776.104242	56.014796	63.603278
1774.826089	52.789188	63.608282
1774.613829	59.055786	63.613287
1774.339529	46.978131	63.618292
1774.028385	54.327390	63.623297
1772.646711	57.170551	63.628302
1772.177932	58.863608	63.633306
1771.580194	60.097566	63.638311
1771.073287	60.035906	63.643316
1769.913328	46.576306	63.648321
1768.909087	50.911266	63.653326
1768.605143	49.427833	63.658330
1768.248787	55.738821	63.663335
1767.781400	56.067488	63.668340
1767.066411	43.576972	63.673345
1765.647573	52.742797	63.678350
1765.697383	48.506847	63.683354
1764.976256	48.724200	63.688359
1764.410000	60.080099	63.693364
1763.736469	49.374120	63.698369
1762.365042	56.339168	63.703374
1762.046254	51.483026	63.708378
1761.840026	54.777929	63.713383
1760.801754	65.652121	63.718388
1759.711204	49.109724	63.723393
1758.860711	66.961221	63.728398
1758.681579	67.581999	63.733402
1758.415338	56.432526	63.738407
1757.765786	54.313917	63.743412
1757.576408	57.237665	63.748417
1756.043563	69.779707	63.753422
1755.665747	56.883348	63.758426
1754.805382	66.872926	63.763431
1754.345509	58.940397	63.768436
1753.898485	62.151773	63.773441
1752.523210	60.417067	63.778446
1752.481466	54.014770	63.783450
1751.618076	57.085424	63.788455
1750.794573	62.404288	63.793460
1750.117928	53.781780	63.798465
1749.321466	56.431263	63.803470
1748.727404	62.314790	63.808474
1748.275499	56.849479	63.813479
1747.557046	60.275055	63.818484
1747.625277	56.061607	63.823489
1746.395061	59.671457	63.828494
1745.524044	60.957310	63.833498
1744.868363	58.609630	63.838503
1744.695319	65.999208	63.843508
1744.065114	55.787111	63.848513
1742.911922	68.801800	63.853518
1742.484434	57.497165	63.858522
1741.663337	60.968330	63.863527
1741.140850	64.216697	63.868532
1740.307239	58.557764	63.873537
1739.637734	52.922856	63.878542
1739.008137	61.304329	63.883546
1738.655881	56.919290	63.888551
1737.850394	52.939422	63.893556
1736.859500	55.062068	63.898561
1735.859571	55.881713	63.903566
1735.650795	53.093632	63.908570
1734.870656	55.808611	63.913575
1734.773949	55.989777	63.918580
1734.482451	48.510004	63.923585
1733.358008	61.966592	63.928590
1732.400835	50.391036	63.933594
1731.792110	51.079402	63.938599
1730.819203	59.273709	63.943604
1729.891954	44.467783	63.948609
1728.982217	57.880918	63.953614
1728.887032	51.998930	63.958618
1728.570307	52.272610	63.963623
1727.753292	59.314501	63.968628
1728.092222	53.049954	63.973633
1726.635623	57.816784	63.978638
1725.698633	50.443912	63.983642
1725.377403	53.265883	63.988647
1724.882523	56.800829	63.993652
1723.932583	40.357942	63.998657
1722.760990	50.675492	64.003662
1722.613537	48.631624	64.008666
1722.299356	51.211611	64.013671
1721.330385	54.931886	64.018676
1720.505795	51.708021	64.023681
1720.036537	49.757112	64.028686
1719.635031	47.275158	64.033690
1718.832064	55.651954	64.038695
1717.568796	58.607889	64.043700
1716.827872	55.669694	64.048705
1716.418328	50.864217	64.053710
1716.135798	52.359625	64.058714
1715.747902	55.266028	64.063719
1714.146372	56.770436	64.068724
1713.853547	55.516015	64.073729
1713.462236	62.310598	64.078734
1713.145833	56.110821	64.083738
1712.489916	56.598063	64.088743
1710.818747	56.811419	64.093748
1710.241934	54.250126	64.098753
1709.774315	59.031275	64.103758
1709.382462	57.765379	64.108762
1709.116179	51.517951	64.113767
1708.291587	61.641138	64.118772
1707.371756	48.987932	64.123777
1706.577411	56.750255	64.128782
1706.375894	50.777521	64.133786
1705.678136	53.248679	64.138791
1704.342078	56.830465	64.143796
1704.039089	58.184118	64.148801
1703.256872	56.810555	64.153806
1703.036645	59.786554	64.158810
1702.450267	51.703587	64.163815
1700.834683	53.210404	64.168820
1700.356371	51.591032	64.173825
1699.903650	59.344633	64.178830
1699.582316	55.396788	64.183834
1699.307445	53.977855	64.188839
1697.681392	57.402434	64.193844
1697.523531	47.308859	64.198849
1696.842472	51.694312	64.203854
1696.464937	51.170015	64.208858
1695.630608	53.370872	64.213863
1694.528299	57.492900	64.218868
1694.279593	51.609554	64.223873
1693.453050	60.703647	64.228878
1693.046702	57.642285	64.233882
1692.245369	50.498039	64.238887
1690.877639	52.817408	64.243892
1690.751911	45.019553	64.248897
1690.253094	50.536664	64.253902
1689.910949	52.559356	64.258906
1689.152806	52.231631	64.263911
1687.882694	52.238608	64.268916
1687.584189	49.750084	64.273921
1686.904965	61.960541	64.278926
1686.354753	52.676571	64.283930
1685.515246	46.300275	64.288935
1684.715491	53.345134	64.293940
1684.363191	56.865157	64.298945
1683.592904	62.116109	64.303950
1683.511324	56.879924	64.308954
1682.138801	51.805441	64.313959
1681.295225	51.661671	64.318964
1681.186715	54.933932	64.323969
1680.192255	54.953739	64.328974
1679.392957	63.645689	64.333978
1678.667400	58.108011	64.338983
1677.327449	58.827963	64.343988
1677.001537	54.641704	64.348993
1677.061572	62.646627	64.353998
1676.936089	57.282171	64.359002
1676.669493	55.298954	64.364007
1674.832269	62.131370	64.369012
1674.365046	52.057184	64.374017
1674.390516	60.129991	64.379022
1672.906296	52.170278	64.384026
1671.887347	52.944639	64.389031
1671.013800	59.926738	64.394036
1670.784095	54.807872	64.399041
1670.558117	58.350883	64.404046
1669.671364	58.835396	64.409050
1669.797702	65.564292	64.414055
1668.566468	67.412699	64.419060
1667.744388	60.943817	64.424065
1666.995306	72.932168	64.429070
1666.649149	64.000497	64.434074
1665.781922	58.169315	64.439079
1664.591773	64.981395	64.444084
1664.159824	52.669824	64.449089
1663.768693	56.397010	64.454094
1663.547275	60.116469	64.459098
1662.745721	63.201027	64.464103
1661.242855	57.121794	64.469108
1660.988384	61.698320	64.474113
1660.554458	65.772685	64.479118
1660.268006	66.913125	64.484122
1659.431871	61.951716	64.489127
1658.299931	68.492533	64.494132
1658.231032	62.571313	64.499137
1657.519848	68.724352	64.504142
1655.995056	70.589051	64.509146
1655.440182	58.366011	64.514151
1655.158888	67.101946	64.519156
1654.929878	61.607187	64.524161
1654.464342	68.048964	64.529166
1653.171714	73.351022	64.534170
1652.817801	67.239373	64.539175
1651.607725	65.087232	64.544180
1651.536671	59.482947	64.549185
1650.397526	65.375289	64.554190
1649.072867	67.442179	64.559194
1649.067273	68.340355	64.564199
1648.264407	58.230059	64.569204
1648.382456	63.632929	64.574209
1648.029388	64.459915	64.579214
1646.945844	61.712200	64.584218
1646.215017	57.845882	64.589223
1645.093329	56.654365	64.594228
1644.425794	58.096061	64.599233
1643.552025	68.478318	64.604238
1643.002041	60.177561	64.609242
1642.598185	53.791058	64.614247
1642.090089	68.430547	64.619252
1641.614647	53.841390	64.624257
1640.486370	62.393071	64.629262
1639.423624	64.490533	64.634266
1638.966778	59.318964	64.639271
1638.710502	62.474415	64.644276
1638.580159	58.976633	64.649281
1637.935890	48.074239	64.654286
1636.735091	60.421713	64.659290
1635.993539	51.125896	64.664295
1635.532116	58.155887	64.669300
1634.492120	51.770491	64.674305
1633.407904	54.970920	64.679310
1632.959720	53.144302	64.684314
1632.733770	44.793235	64.689319
1631.841192	46.094241	64.694324
1631.832176	55.571433	64.699329
1631.278481	53.917996	64.704334
1630.470281	56.694234	64.709338
1630.057656	50.019117	64.714343
1628.894208	57.776324	64.719348
1627.916342	45.322149	64.724353
1627.384179	46.500296	64.729358
1626.651179	51.943412	64.734362
1626.282812	54.312422	64.739367
1625.204450	56.918588	64.744372
1624.367872	47.656800	64.749377
1623.923616	56.601398	64.754382
1623.053723	58.224957	64.759386
1623.248030	56.475091	64.764391
1622.448468	58.945524	64.769396
1622.171878	50.041436	64.774401
1620.957326	56.186278	64.779406
1619.906831	53.751453	64.784410
1619.496505	48.558115	64.789415
1618.868251	63.393810	64.794420
1617.844740	57.872398	64.799425
1617.323998	54.961669	64.804430
1616.727691	64.721336	64.809434
1616.620306	56.889161	64.814439
1615.806350	61.049088	64.819444
1614.870713	50.822192	64.824449
1613.556438	53.056251	64.829454
1613.058415	54.571174	64.834458
1613.098043	53.461172	64.839463
1612.222315	56.325150	64.844468
1611.612319	47.212082	64.849473
1611.360259	55.997082	64.854478
1610.078810	56.332452	64.859482
1609.597984	54.471951	64.864487
1608.663066	53.870556	64.869492
1608.604340	52.765150	64.874497
1607.612698	50.195921	64.879502
1606.408828	44.321322	64.884506
1606.405963	51.186785	64.889511
1605.755692	58.075418	64.894516
1605.442893	48.596109	64.899521
1604.470841	49.502186	64.904526
1603.435480	53.470277	64.909530
1603.667936	49.099264	64.914535
1602.562335	58.791751	64.919540
1601.861533	44.184342	64.924545
1601.315175	55.770898	64.929550
1600.514436	56.087552	64.934554
1599.707426	52.718603	64.939559
1598.552327	63.042431	64.944564
1598.022906	50.436124	64.949569
1597.529748	55.471504	64.954574
1596.978392	52.104986	64.959578
1596.720283	48.711965	64.964583
1595.772767	60.993203	64.969588
1594.680321	59.673935	64.974593
1594.295034	60.341839	64.979598
1593.775247	53.338897	64.984602
1593.727718	45.779894	64.989607
1592.956006	60.102529	64.994612
1591.619509	55.639249	64.999617
1591.233545	58.030219	65.004622
1590.495151	58.610535	65.009626
1589.606962	54.175134	65.014631
1588.453836	58.575075	65.019636
1588.076291	59.471776	65.024641
1587.751702	54.186797	65.029646
1587.185911	64.757126	65.034650
1587.062997	53.190411	65.039655
1586.390337	66.046692	65.044660
1585.170119	51.557383	65.049665
1584.334033	49.240208	65.054670
1583.464106	49.500420	65.059674
1583.569696	53.678232	65.064679
1582.018749	49.695323	65.069684
1581.239300	49.977548	65.074689
1581.379722	47.594302	65.079694
1580.599483	58.228168	65.084698
1580.515172	49.969702	65.089703
1579.349417	52.339791	65.094708
1578.513627	59.934356	65.099713
1578.030488	54.251400	65.104718
1577.803347	63.846444	65.109722
1576.939574	54.787469	65.114727
1575.519767	54.484187	65.119732
1575.239025	58.987843	65.124737
1574.999465	57.854573	65.129742
1573.760138	53.446509	65.134746
1572.935053	55.767770	65.139751
1572.049943	53.865942	65.144756
1571.772472	56.268738	65.149761
1571.348760	54.998440	65.154766
1570.792463	50.733996	65.159770
1570.464367	50.829245	65.164775
1569.356208	55.204125	65.169780
1568.786423	55.995182	65.174785
1568.321130	50.819546	65.179790
1567.152744	58.847990	65.184794
1566.271060	53.353240	65.189799
1565.718777	54.037490	65.194804
1564.950706	52.454697	65.199809
1564.872506	48.601435	65.204814
1564.336396	55.851830	65.209818
1564.046559	55.216617	65.214823
1562.683768	53.442726	65.219828
1561.795155	52.842889	65.224833
1561.458028	48.912367	65.229838
1560.205688	48.707923	65.234842
1560.003670	51.211879	65.239847
1558.622001	51.689539	65.244852
1558.456618	56.028984	65.249857
1558.079491	51.516388	65.254862
1557.272041	56.408595	65.259866
1557.172545	55.299510	65.264871
1556.736561	56.818819	65.269876
1555.607024	49.882743	65.274881
1555.176627	55.808132	65.279886
1554.200172	54.533755	65.284890
1553.952502	50.886331	65.289895
1552.720274	57.243806	65.294900
1552.034410	58.685098	65.299905
1551.603044	47.894308	65.304910
1550.226507	59.473745	65.309914
1549.628605	54.928279	65.314919
1549.090694	57.844575	65.319924
1548.308729	55.383940	65.324929
1548.415310	54.676935	65.329934
1547.813154	51.295435	65.334938
1547.872486	48.199389	65.339943
1546.685390	52.620543	65.344948
1545.600199	50.280092	65.349953
1544.994082	47.198468	65.354958
1543.680769	51.473864	65.359962
1543.266552	45.931087	65.364967
1542.756621	57.475095	65.369972
1542.295872	53.431133	65.374977
1542.012811	48.619821	65.379982
1541.378104	50.847321	65.384986
1540.289418	47.427519	65.389991
1539.863858	52.257524	65.394996
1539.208273	44.932063	65.400001
1537.804805	45.231494	65.405006
1536.764378	55.076640	65.410010
1536.051760	46.577967	65.415015
1536.604966	52.356721	65.420020
1536.081330	52.280580	65.425025
1534.888976	44.567799	65.430030
1534.693598	60.195414	65.435034
1533.719712	51.033724	65.440039
1532.723180	54.969130	65.445044
1532.123934	57.554493	65.450049
1532.005717	53.571903	65.455054
1531.421738	59.240960	65.460058
1530.967332	49.123955	65.465063
1529.991986	63.448289	65.470068
1528.940945	65.875726	65.475073
1528.376161	58.772341	65.480078
1527.461961	64.013598	65.485082
1527.230124	57.411362	65.490087
1526.337239	55.343908	65.495092
1525.519846	58.325013	65.500097
1524.251837	52.827711	65.505102
1524.166174	59.239207	65.510106
1523.586221	53.495465	65.515111
1523.103868	61.419131	65.520116
1522.356446	58.300907	65.525121
1522.404839	58.984981	65.530126
1521.190758	65.022005	65.535130
1520.355831	60.135022	65.540135
1519.535390	52.165176	65.545140
1519.105084	55.676450	65.550145
1518.929835	53.449858	65.555150
1517.762732	60.956272	65.560154
1516.620534	54.847335	65.565159
1516.302837	58.656690	65.570164
1515.777310	56.283216	65.575169
1515.603090	51.472619	65.580174
1514.601802	53.835887	65.585178
1513.869118	56.849072	65.590183
1513.339136	61.054351	65.595188
1512.688200	52.967472	65.600193
1512.120447	46.197352	65.605198
1510.557464	57.324779	65.610202
1510.213791	45.403910	65.615207
1509.566952	45.844230	65.620212
1509.610041	44.929418	65.625217
1508.978645	50.989466	65.630222
1507.521976	50.310030	65.635226
1507.026166	45.874594	65.640231
1506.297335	51.616993	65.645236
1506.086368	54.907183	65.650241
1505.831036	51.214103	65.655246
1505.007726	59.462166	65.660250
1504.376544	57.126118	65.665255
1503.430994	59.165653	65.670260
1502.203169	55.141280	65.675265
1501.126810	58.089742	65.680270
1500.660835	54.914667	65.685274
1500.509477	58.675422	65.690279
1500.192112	57.279565	65.695284
1499.993703	52.657048	65.700289
1499.431761	54.486458	65.705294
1497.873392	57.048494	65.710298
1497.458484	53.700476	65.715303
1496.972754	54.829243	65.720308
1496.012056	61.968769	65.725313
1495.194227	48.672938	65.730318
1494.298620	52.055441	65.735322
1494.081367	57.360167	65.740327
1493.805233	56.572225	65.745332
1492.671382	58.352688	65.750337
1492.068705	53.837259	65.755342
1491.200637	61.195789	65.760346
1490.849931	56.786830	65.765351
1489.997788	57.662142	65.770356
1489.188164	60.683368	65.775361
1488.853086	55.456246	65.780366
1488.083125	61.774479	65.785370
1487.423861	56.800993	65.790375
1487.024647	54.855093	65.795380
1486.229614	57.402528	65.800385
1485.740231	49.767983	65.805390
1484.526307	55.426053	65.810394
1483.988506	54.959991	65.815399
1482.750096	48.104148	65.820404
1482.529790	61.971238	65.825409
1482.342310	54.013057	65.830414
1481.318566	59.552923	65.835418
1480.933908	53.581560	65.840423
1480.628188	56.607324	65.845428
1479.198838	58.146670	65.850433
1478.526140	54.710152	65.855438
1477.760749	69.513269	65.860442
1477.446308	56.133645	65.865447
1477.208130	58.116448	65.870452
1476.340638	70.623597	65.875457
1475.515084	62.906462	65.880462
1474.429782	58.463773	65.885466
1474.012237	56.566404	65.890471
1473.519074	56.213488	65.895476
1473.385297	57.443455	65.900481
1472.638552	52.039309	65.905486
1471.314751	57.359758	65.910490
1471.009918	56.502918	65.915495
1470.477882	54.618831	65.920500
1469.612125	51.351932	65.925505
1468.637919	59.561091	65.930510
1467.798616	55.692060	65.935514
1467.470878	57.107193	65.940519
1466.982392	55.488009	65.945524
1466.698843	57.195565	65.950529
1465.802735	47.900590	65.955534
1464.991481	54.613109	65.960538
1464.660292	51.262607	65.965543
1463.991839	51.881098	65.970548
1462.633231	56.589376	65.975553
1461.831507	50.588751	65.980558
1461.248188	55.108672	65.985562
1461.201907	66.215709	65.990567
1460.538101	59.408351	65.995572
1460.013202	60.140818	66.000577
1459.191721	60.344207	66.005582
1458.347717	54.215824	66.010586
1457.876453	51.377565	66.015591
1456.954710	56.513940	66.020596
1456.019539	53.863239	66.025601
1455.413107	51.232451	66.030606
1454.799841	56.769162	66.035610
1454.441225	50.443231	66.040615
1454.474392	57.315149	66.045620
1453.012343	61.169204	66.050625
1452.449747	53.175370	66.055630
1451.706642	56.254290	66.060634
1451.448264	55.012149	66.065639
1450.292298	55.018593	66.070644
1449.326455	55.313402	66.075649
1449.324653	55.954359	66.080654
1448.519820	56.559881	66.085658
1448.317357	53.553251	66.090663
1447.068341	52.262395	66.095668
1445.882183	54.658503	66.100673
1445.931224	48.295558	66.105678
1445.208804	47.735976	66.110682
1444.613454	54.991382	66.115687
1443.641214	54.093658	66.120692
1442.631141	57.745225	66.125697
1442.144518	51.616066	66.130702
1441.562965	58.802010	66.135706
1441.233253	52.036153	66.140711
1441.074327	43.801529	66.145716
1440.026016	53.254498	66.150721
1439.281037	46.210794	66.155726
1438.819242	58.279824	66.160730
1438.612480	55.341427	66.165735
1437.500465	56.537533	66.170740
1436.541561	61.437126	66.175745
1435.958742	54.189223	66.180750
1434.805820	65.806585	66.185754
1433.511737	59.137116	66.190759
1433.966370	56.379573	66.195764
1432.896211	56.315285	66.200769
1432.433045	53.451170	66.205774
1431.824501	64.143679	66.210778
1431.660422	57.433150	66.215783
1431.070064	55.005261	66.220788
1429.997875	57.220030	66.225793
1429.802468	49.145194	66.230798
1429.048520	51.297199	66.235802
1427.605328	57.191093	66.240807
1426.919504	48.181830	66.245812
1426.277968	52.193058	66.250817
1426.037903	48.500136	66.255822
1425.432575	54.307451	66.260826
1424.910824	52.303589	66.265831
1423.872868	52.705083	66.270836
1422.965180	56.076639	66.275841
1423.057714	50.953166	66.280846
1422.484223	53.591758	66.285850
1421.258701	58.973944	66.290855
1420.473103	59.466052	66.295860
1419.636024	53.574508	66.300865
1419.453441	49.518474	66.305870
1418.890176	52.553982	66.310874
1418.322584	52.112763	66.315879
1417.301770	48.328891	66.320884
1416.515898	55.654409	66.325889
1416.126879	45.841616	66.330894
1415.826195	52.524371	66.335898
1415.105972	46.839002	66.340903
1414.307624	48.853747	66.345908
1413.439359	54.405690	66.350913
1413.361853	52.255527	66.355918
1412.053356	53.115814	66.360922
1411.104782	54.753662	66.365927
1410.819540	45.110204	66.370932
1410.173793	55.172790	66.375937
1409.535484	49.512870	66.380942
1408.772975	52.422624	66.385946
1407.857364	52.080055	66.390951
1407.415640	49.330295	66.395956
1406.663448	55.237352	66.400961
1406.283866	50.732695	66.405966
1405.914273	54.474360	66.410970
1404.256217	47.093166	66.415975
1404.075223	48.936319	66.420980
1403.219598	58.895103	66.425985
1403.088678	53.288851	66.430990
1402.451645	55.223883	66.435994
1401.124741	43.303193	66.440999
1400.902893	43.060149	66.446004
1400.249235	50.319615	66.451009
1399.657274	53.052156	66.456014
1399.072056	46.217155	66.461018
1398.413578	50.800864	66.466023
1397.834816	44.177906	66.471028
1397.155392	47.915371	66.476033
1396.773625	55.117246	66.481038
1395.584800	54.669876	66.486042
1394.609280	60.931334	66.491047
1394.405368	55.318630	66.496052
1393.427663	50.240996	66.501057
1393.297459	46.931490	66.506062
1392.101967	55.611935	66.511066
1391.265716	52.613935	66.516071
1390.892055	50.386185	66.521076
1390.416400	56.491421	66.526081
1390.183534	55.893044	66.531086
1388.923136	57.019828	66.536090
1388.072973	55.085213	66.541095
1387.892798	48.013517	66.546100
1387.181176	47.540907	66.551105
1386.573865	50.723293	66.556110
1386.063690	51.258255	66.561114
1385.347966	45.804611	66.566119
1384.577672	45.673608	66.571124
1383.362051	47.649659	66.576129
1382.159211	41.925734	66.581134
1381.902110	45.939049	66.586138
1381.196064	55.112789	66.591143
1381.380746	49.514486	66.596148
1380.737648	57.211075	66.601153
1380.435997	49.248375	66.606158
1379.051993	48.647718	66.611162
1378.316403	52.702681	66.616167
1378.077552	46.596250	66.621172
1376.955442	47.125443	66.626177
1376.224404	47.918071	66.631182
1375.354104	45.269310	66.636186
1374.559077	49.878368	66.641191
1374.451194	41.200432	66.646196
1373.923103	46.141539	66.651201
1373.921362	51.352925	66.656206
1372.673822	48.409546	66.661210
1371.562893	48.804202	66.666215
1371.687886	52.055038	66.671220
1370.871130	57.662113	66.676225
1369.586507	51.175778	66.681230
1368.977058	47.354655	66.686234
1368.220324	51.448368	66.691239
1368.016411	46.608528	66.696244
1367.400318	44.278603	66.701249
1366.376116	39.607605	66.706254
1365.767307	38.818597	66.711258
1364.759759	41.572152	66.716263
1364.568741	39.171042	66.721268
1364.090292	46.788523	66.726273
1363.649778	40.933317	66.731278
1362.581986	42.055949	66.736282
1361.603627	44.229010	66.741287
1361.588566	42.596293	66.746292
1361.092493	43.255152	66.751297
1360.201736	46.491192	66.756302
1359.282956	54.345494	66.761306
1358.540050	51.751107	66.766311
1358.172141	50.321680	66.771316
1356.928035	60.657217	66.776321
1355.952125	51.418956	66.781326
1355.815929	50.218271	66.786330
1355.405967	53.906851	66.791335
1355.257193	46.828600	66.796340
1354.092823	51.639433	66.801345
1353.404312	38.259152	66.806350
1352.975036	41.421719	66.811354
1352.015422	44.160361	66.816359
1351.485159	42.777279	66.821364
1350.443510	51.017727	66.826369
1349.594785	36.039032	66.831374
1349.506472	35.245394	66.836378
1349.031894	50.998135	66.841383
1348.040665	49.600810	66.846388
1346.842315	50.851580	66.851393
1346.157199	54.419508	66.856398
1345.885966	58.072104	66.861402
1345.139531	54.896114	66.866407
1345.278780	47.887369	66.871412
1344.674423	57.385135	66.876417
1343.488879	61.759487	66.881422
1342.569147	63.435435	66.886426
1342.034190	55.608593	66.891431
1341.943238	48.046784	66.896436
1340.562521	51.257760	66.901441
1339.497542	55.542791	66.906446
1339.039968	58.176942	66.911450
1338.284958	60.812671	66.916455
1338.471990	55.433034	66.921460
1338.149051	57.359301	66.926465
1337.140789	49.482836	66.931470
1336.042269	48.376237	66.936474
1335.557579	52.650740	66.941479
1335.040408	49.296565	66.946484
1334.032875	61.703349	66.951489
1333.264520	57.114864	66.956494
1332.714032	53.799944	66.961498
1332.151091	58.885175	66.966503
1331.733657	47.447470	66.971508
1331.063080	58.402820	66.976513
1330.167732	54.372499	66.981518
1329.372970	49.456581	66.986522
1328.654985	56.369451	66.991527
1328.476894	50.839173	66.996532
1327.516669	53.124788	67.001537
1327.079960	48.906223	67.006542
1326.630638	59.376876	67.011546
1325.495126	59.892981	67.016551
1325.453004	47.203322	67.021556
1323.941730	56.346763	67.026561
1323.128566	46.736855	67.031566
1322.778866	49.453981	67.036570
1322.226759	54.266580	67.041575
1321.885564	52.128800	67.046580
1320.976930	54.501107	67.051585
1320.199564	54.612891	67.056590
1319.348980	54.445908	67.061594
1318.790450	53.637641	67.066599
1319.115334	45.182055	67.071604
1317.797076	54.709671	67.076609
1316.660544	54.230474	67.081614
1316.291142	41.393963	67.086618
1315.727817	51.979254	67.091623
1315.457595	43.296353	67.096628
1314.016415	56.852582	67.101633
1313.289167	59.172524	67.106638
1313.025984	51.650068	67.111642
1312.276359	60.166964	67.116647
1312.189698	50.523074	67.121652
1311.595428	56.318240	67.126657
1310.249188	49.531040	67.131662
1309.734641	53.502776	67.136666
1309.210158	55.104749	67.141671
1308.970524	56.667431	67.146676
1307.544543	56.347915	67.151681
1307.326406	57.632982	67.156686
1306.655511	52.967823	67.161690
1305.121185	55.562900	67.166695
1304.750988	57.540678	67.171700
1303.692501	55.349652	67.176705
1303.952603	51.929123	67.181710
1303.125237	53.990692	67.186714
1302.673180	56.430094	67.191719
1302.306235	49.354463	67.196724
1301.601366	55.795375	67.201729
1300.351685	50.511707	67.206734
1300.095315	57.139510	67.211738
1299.340897	63.195768	67.216743
1298.342101	50.358457	67.221748
1297.386121	53.047148	67.226753
1297.250224	59.607355	67.231758
1296.829345	53.149612	67.236762
1296.376266	63.051331	67.241767
1295.429167	56.553811	67.246772
1294.385427	57.795887	67.251777
1294.133124	57.004273	67.256782
1293.165835	55.139462	67.261786
1291.920813	58.797330	67.266791
1291.578860	50.007504	67.271796
1291.414503	46.555831	67.276801
1290.660083	56.985560	67.281806
1290.413652	54.624332	67.286810
1289.174276	59.255398	67.291815
1288.385741	45.639633	67.296820
1287.676154	51.121794	67.301825
1286.928762	44.916523	67.306830
1286.690711	53.784762	67.311834
1286.476217	46.239767	67.316839
1285.715221	46.093767	67.321844
1284.412066	52.744863	67.326849
1283.955653	46.326759	67.331854
1283.814436	43.801475	67.336858
1282.532653	47.008947	67.341863
1282.094028	38.491851	67.346868
1281.276552	48.364766	67.351873
1280.812571	48.363698	67.356878
1280.019722	50.959334	67.361882
1278.576908	55.332349	67.366887
1278.550010	56.238509	67.371892
1277.856960	47.772466	67.376897
1277.341744	53.360687	67.381902
1277.298298	50.219878	67.386906
1275.994047	54.608642	67.391911
1275.226894	45.586894	67.396916
1274.714526	48.322003	67.401921
1274.331797	50.163776	67.406926
1274.057653	41.427871	67.411930
1272.812473	50.907456	67.416935
1272.467735	53.007581	67.421940
1271.840612	54.609367	67.426945
1270.785712	45.437945	67.431950
1270.023751	45.704197	67.436954
1268.995367	54.549856	67.441959
1269.213879	49.642441	67.446964
1268.435218	54.309496	67.451969
1266.820367	55.423969	67.456974
1266.651321	48.725364	67.461978
1265.601199	49.338963	67.466983
1265.396087	42.097483	67.471988
1265.025445	49.973206	67.476993
1264.346779	44.755599	67.481998
1263.169763	44.134932	67.487002
1262.204441	48.471988	67.492007
1261.730556	42.921706	67.497012
1261.297556	52.252377	67.502017
1260.920516	45.960417	67.507022
1260.725276	43.488987	67.512026
1260.255373	48.043973	67.517031
1259.236472	37.825131	67.522036
1258.473333	46.481699	67.527041
1257.698702	51.161880	67.532046
1256.579603	40.039315	67.537050
1255.906304	53.677627	67.542055
1255.497119	50.657063	67.547060
1254.630718	55.032052	67.552065
1254.426935	47.165900	67.557070
1254.024184	40.976236	67.562074
1252.543082	51.268676	67.567079
1252.368921	47.037539	67.572084
1251.650692	41.668427	67.577089
1251.290110	49.990432	67.582094
1250.376391	40.031859	67.587098
1249.249478	50.698245	67.592103
1249.097171	45.015938	67.597108
1248.816209	51.911224	67.602113
1247.853146	45.923666	67.607118
1246.817130	38.899442	67.612122
1245.965420	42.891801	67.617127
1246.135170	44.845029	67.622132
1245.213458	42.278120	67.627137
1244.028287	46.620450	67.632142
1243.645021	43.646371	67.637146
1242.857557	51.473068	67.642151
1242.755836	45.628951	67.647156
1242.003286	44.857858	67.652161
1240.943601	47.131701	67.657166
1240.722387	44.166586	67.662170
1239.951417	44.583983	67.667175
1239.312526	42.350345	67.672180
1238.347597	44.609545	67.677185
1237.440412	38.842151	67.682190
1237.324878	47.419422	67.687194
1236.639988	48.664014	67.692199
1235.496344	34.666595	67.697204
1234.564556	42.529445	67.702209
1234.051861	44.984758	67.707214
1233.734894	42.758370	67.712218
1232.927227	40.636520	67.717223
1233.035099	45.237053	67.722228
1232.029533	48.090155	67.727233
1231.211736	50.925321	67.732238
1230.938470	40.314761	67.737242
1230.006093	44.951296	67.742247
1228.817478	44.258022	67.747252
1228.025954	51.700566	67.752257
1227.504194	56.326011	67.757262
1227.193906	44.924457	67.762266
1226.441209	51.247646	67.767271
1226.348508	42.940134	67.772276
1224.826423	39.099247	67.777281
1223.875416	43.422803	67.782286
1223.776707	43.536035	67.787290
1223.206373	50.692038	67.792295
1223.205744	49.125138	67.797300
1222.576765	47.929095	67.802305
1221.211227	49.667969	67.807310
1220.946598	31.356583	67.812314
1220.233302	43.942313	67.817319
1219.044307	36.947054	67.822324
1218.131597	41.753898	67.827329
1217.661773	41.797254	67.832334
1217.629913	40.295700	67.837338
1216.896105	48.539901	67.842343
1216.009498	37.560696	67.847348
1215.441120	33.444821	67.852353
1214.549272	45.818767	67.857358
1214.025769	40.162126	67.862362
1212.549873	47.572246	67.867367
1212.593390	44.069594	67.872372
1211.985237	45.040538	67.877377
1211.334559	51.501385	67.882382
1210.975721	45.607349	67.887386
1210.148940	45.223558	67.892391
1209.042019	45.527172	67.897396
1208.594087	43.923968	67.902401
1208.003961	52.919191	67.907406
1207.397724	43.470456	67.912410
1206.577082	47.516314	67.917415
1206.290577	52.909860	67.922420
1205.267760	48.824029	67.927425
1204.484279	55.523132	67.932430
1204.272154	41.273865	67.937434
1203.680854	54.043179	67.942439
1202.662062	32.551611	67.947444
1201.961012	44.066351	67.952449
1201.259278	46.744681	67.957454
1200.640682	41.664032	67.962458
1199.990580	39.250751	67.967463
1199.944175	39.998021	67.972468
1198.841003	39.955618	67.977473
1198.135686	49.128448	67.982478
1197.628721	38.200294	67.987482
1196.541884	50.840513	67.992487
1195.840627	44.120152	67.997492
1195.567462	47.589140	68.002497
1195.086196	48.689537	68.007502
1194.934999	48.370068	68.012506
1194.087794	51.145145	68.017511
1193.271687	44.178409	68.022516
1191.961630	38.621709	68.027521
1190.682389	44.842035	68.032526
1190.280105	40.820481	68.037530
1189.721646	49.412405	68.042535
1189.248721	45.034674	68.047540
1188.855908	46.623586	68.052545
1188.459113	49.086294	68.057550
1188.124236	37.072021	68.062554
1186.929056	45.893350	68.067559
1186.027211	47.019182	68.072564
1185.655199	50.559961	68.077569
1184.600208	47.951939	68.082574
1184.892120	40.683393	68.087578
1183.482122	54.262324	68.092583
1182.395485	46.409982	68.097588
1182.194656	45.240107	68.102593
1181.449375	49.031893	68.107598
1181.289085	42.432453	68.112602
1180.730160	56.608128	68.117607
1179.504051	47.949971	68.122612
1179.295264	52.512357	68.127617
1178.420902	54.662118	68.132622
1177.574292	44.599315	68.137626
1176.371924	52.887433	68.142631
1175.565378	49.211399	68.147636
1175.509326	47.856480	68.152641
1174.675418	52.751283	68.157646
1174.708483	57.089900	68.162650
1174.302156	55.944158	68.167655
1173.134082	49.308859	68.172660
1172.248856	46.680851	68.177665
1171.521897	62.236419	68.182670
1171.108419	54.723137	68.187674
1170.954707	63.443915	68.192679
1169.731843	54.564160	68.197684
1169.222111	48.473345	68.202689
1168.429167	55.716807	68.207694
1167.934655	40.799093	68.212698
1166.784312	54.238835	68.217703
1166.002461	54.808099	68.222708
1165.724189	59.915252	68.227713
1164.839568	61.222473	68.232718
1164.820410	51.131669	68.237722
1163.589281	60.117446	68.242727
1162.936806	59.081347	68.247732
1162.395565	49.370844	68.252737
1161.863593	49.075523	68.257742
1161.546216	47.461022	68.262746
1160.155423	56.397561	68.267751
1159.469103	48.479839	68.272756
1158.935600	52.652977	68.277761
1158.419052	48.874400	68.282766
1158.335886	50.923427	68.287770
1157.399566	56.253774	68.292775
1156.310490	50.238869	68.297780
1155.953767	47.191968	68.302785
1155.363535	56.643504	68.307790
1154.693687	51.304807	68.312794
1153.611433	63.716109	68.317799
1152.982638	62.324263	68.322804
1152.682318	54.155719	68.327809
1152.039077	56.117103	68.332814
1151.717501	46.542667	68.337818
1150.336012	57.093192	68.342823
1149.900010	52.263901	68.347828
1149.031652	49.117509	68.352833
1148.509244	57.647215	68.357838
1148.125534	46.826245	68.362842
1146.908349	55.289003	68.367847
1146.574078	54.404070	68.372852
1145.927733	50.702979	68.377857
1145.151221	54.320126	68.382862
1145.278937	50.214536	68.387866
1144.353558	51.804645	68.392871
1143.433567	47.896607	68.397876
1142.963729	44.708426	68.402881
1141.655065	55.002941	68.407886
1141.315871	50.024056	68.412890
1140.524644	52.673114	68.417895
1139.739465	54.305925	68.422900
1139.446872	47.761509	68.427905
1139.059549	58.969134	68.432910
1137.974886	51.956028	68.437914
1136.917368	47.149482	68.442919
1136.656128	49.167819	68.447924
1136.382284	45.818980	68.452929
1135.322847	55.177971	68.457934
1134.393814	44.689184	68.462938
1133.511125	45.355452	68.467943
1133.009463	48.753046	68.472948
1132.947614	46.286809	68.477953
1132.209807	58.283883	68.482958
1131.872290	44.787115	68.487962
1130.872064	53.010629	68.492967
1129.723643	46.803800	68.497972
1129.296735	48.864319	68.502977
1128.776743	49.144027	68.507982
1128.616181	49.355478	68.512986
1127.063030	59.491345	68.517991
1126.655543	56.274725	68.522996
1126.590967	48.997748	68.528001
1125.566005	51.221854	68.533006
1124.624313	46.247065	68.538010
1123.894046	51.947901	68.543015
1123.283278	48.343349	68.548020
1123.117741	47.879503	68.553025
1122.113694	50.278046	68.558030
1122.032561	45.927574	68.563034
1120.844704	51.724526	68.568039
1120.130595	53.316356	68.573044
1120.007029	48.501858	68.578049
1118.714700	50.535707	68.583054
1118.143350	51.627853	68.588058
1117.516912	46.972880	68.593063
1116.953491	56.607317	68.598068
1115.834379	45.376253	68.603073
1114.653951	53.074864	68.608078
1114.707176	42.808264	68.613082
1113.937618	62.727614	68.618087
1113.513219	53.588793	68.623092
1113.068326	48.545911	68.628097
1112.369985	46.078536	68.633102
1112.210473	47.058322	68.638106
1111.122398	45.016481	68.643111
1110.515335	44.930988	68.648116
1109.993692	42.675319	68.653121
1108.589217	49.326823	68.658126
1107.804683	45.435071	68.663130
1107.416741	49.379218	68.668135
1106.745389	49.530512	68.673140
1106.631189	44.803223	68.678145
1106.015820	44.470875	68.683150
1104.893419	41.709820	68.688154
1103.963266	40.691675	68.693159
1103.996404	40.024082	68.698164
1103.721312	47.627664	68.703169
1102.792685	54.701743	68.708174
1101.823546	47.816097	68.713178
1101.385852	41.054573	68.718183
1099.413565	49.569666	68.723188
1098.516138	46.716011	68.728193
1098.861659	44.320932	68.733198
1099.234268	45.652078	68.738202
1098.433323	51.899465	68.743207
1097.138568	52.765372	68.748212
1096.329704	39.679311	68.753217
1094.600801	54.145714	68.758222
1094.946419	42.970538	68.763226
1094.355197	45.074985	68.768231
1093.760687	49.100686	68.773236
1093.522923	51.501827	68.778241
1092.427360	45.827116	68.783246
1091.742303	42.854997	68.788250
1091.104647	49.895827	68.793255
1090.741871	47.796105	68.798260
1090.326265	43.870787	68.803265
1089.063586	54.968183	68.808270
1088.490250	51.273151	68.813274
1088.114730	42.785149	68.818279
1087.291494	49.682504	68.823284
1086.428141	43.960927	68.828289
1085.297660	52.982763	68.833294
1085.065893	47.724978	68.838298
1085.008967	52.934745	68.843303
1084.077134	56.267460	68.848308
1083.251914	44.886614	68.853313
1082.406016	47.719111	68.858318
1081.944019	50.617310	68.863322
1081.519355	40.665432	68.868327
1080.417204	50.159234	68.873332
1079.655651	48.820132	68.878337
1078.957847	41.383979	68.883342
1078.646958	45.832406	68.888346
1078.129607	46.278631	68.893351
1077.202413	49.363459	68.898356
1076.608922	45.163487	68.903361
1075.695604	48.911037	68.908366
1075.195997	43.394792	68.913370
1075.159800	47.577112	68.918375
1073.700341	53.261117	68.923380
1073.010694	49.415094	68.928385
1072.332253	48.937637	68.933390
1071.986974	45.361049	68.938394
1071.469498	50.576657	68.943399
1070.680297	43.164840	68.948404
1069.993829	41.045554	68.953409
1068.918070	43.570459	68.958414
1068.451938	45.817689	68.963418
1068.013205	51.752013	68.968423
1067.655689	51.581162	68.973428
1067.444241	41.193321	68.978433
1066.150694	49.669165	68.983438
1065.430717	42.631528	68.988442
1064.732153	45.213414	68.993447
1063.529847	50.991930	68.998452
1063.352750	45.445326	69.003457
1062.810300	47.891933	69.008462
1062.276492	50.701383	69.013466
1061.178551	42.471693	69.018471
1060.016567	46.249591	69.023476
1059.580844	46.164366	69.028481
1058.902876	46.737961	69.033486
1058.706859	45.494641	69.038490
1058.576721	43.531128	69.043495
1058.315388	49.526252	69.048500
1057.341392	39.848045	69.053505
1056.305228	52.548674	69.058510
1055.295597	45.921411	69.063514
1054.310700	48.233796	69.068519
1053.739824	56.206963	69.073524
1053.159734	40.358193	69.078529
1052.758394	45.081437	69.083534
1052.549490	51.047058	69.088538
1051.861482	46.006346	69.093543
1050.736794	52.256285	69.098548
1050.215437	47.533990	69.103553
1049.529912	51.152540	69.108558
1049.096273	52.942258	69.113562
1048.215451	42.829697	69.118567
1047.290918	54.603364	69.123572
1046.776156	45.381356	69.128577
1045.963511	52.225194	69.133582
1045.858166	44.251034	69.138586
1045.488467	43.594402	69.143591
1044.460315	42.605287	69.148596
1043.855911	47.006878	69.153601
1042.742414	47.210607	69.158606
1041.580325	44.720824	69.163610
1041.273004	42.086243	69.168615
1040.575359	55.017443	69.173620
1040.328230	39.368224	69.178625
1039.697692	41.657820	69.183630
1039.505443	35.823700	69.188634
1038.678270	39.233623	69.193639
1037.837589	53.367149	69.198644
1037.225800	40.312880	69.203649
1036.255914	47.580335	69.208654
1035.070799	48.905879	69.213658
1034.613242	38.935565	69.218663
1033.900430	56.195849	69.223668
1033.722696	41.188002	69.228673
1033.170726	44.779734	69.233678
1032.457555	46.963883	69.238682
1031.973262	43.520048	69.243687
1031.105138	47.121318	69.248692
1030.839381	39.296206	69.253697
1029.585845	45.906877	69.258702
1028.474852	45.714281	69.263706
1027.607632	42.373520	69.268711
1027.386713	45.884483	69.273716
1027.239010	38.388478	69.278721
1026.493777	42.104091	69.283726
1026.177631	39.911527	69.288730
1025.895791	38.986442	69.293735
1024.511801	46.356390	69.298740
1023.908455	43.859738	69.303745
1022.505392	54.616860	69.308750
1021.851276	43.588817	69.313754
1020.948483	34.909298	69.318759
1020.916352	45.955035	69.323764
1020.171563	41.063389	69.328769
1019.876900	50.358128	69.333774
1019.522581	47.743438	69.338778
1019.317869	40.528367	69.343783
1017.926656	54.730123	69.348788
1017.325238	45.397836	69.353793
1016.844860	43.613903	69.358798
1015.723013	44.077608	69.363802
1015.118088	49.372139	69.368807
1014.266932	54.734101	69.373812
1014.223211	43.068265	69.378817
1012.885185	49.798405	69.383822
1011.957510	43.851031	69.388826
1011.652761	36.872162	69.393831
1011.225215	43.503216	69.398836
1010.936894	40.914724	69.403841
1010.470553	46.886142	69.408846
1009.359562	47.149841	69.413850
1008.930070	47.112499	69.418855
1007.829576	52.910299	69.423860
1007.350059	36.933406	69.428865
1006.116504	50.325439	69.433870
1005.615594	52.754674	69.438874
1005.228669	44.291926	69.443879
1004.448133	52.383099	69.448884
1004.278558	37.985675	69.453889
1003.278995	52.067467	69.458894
1002.354779	43.731468	69.463898
1001.824218	42.616098	69.468903
1001.504975	47.195423	69.473908
1001.055028	43.626900	69.478913
999.379039	48.236481	69.483918
998.918813	45.913075	69.488922
998.764541	46.837100	69.493927
998.188374	45.975843	69.498932
997.909626	40.834662	69.503937
996.863698	45.243188	69.508942
995.810598	50.621183	69.513946
995.390550	49.852789	69.518951
994.721798	53.018101	69.523956
994.021515	50.240831	69.528961
992.864607	54.027743	69.533966
992.081673	48.114002	69.538970
992.060497	42.607805	69.543975
991.208671	45.886965	69.548980
990.974010	47.976539	69.553985
990.407342	48.465559	69.558990
989.319474	43.278614	69.563994
988.974344	38.147224	69.568999
988.547883	47.443217	69.574004
987.556588	42.765101	69.579009
986.586305	39.924343	69.584014
986.026817	49.124705	69.589018
985.751988	46.771917	69.594023
985.012200	50.027944	69.599028
983.974375	43.156858	69.604033
983.109338	43.800788	69.609038
982.541605	46.021217	69.614042
982.219165	36.892599	69.619047
982.050810	45.081417	69.624052
980.910437	40.924203	69.629057
979.972237	41.389225	69.634062
979.768036	42.285883	69.639066
979.281503	34.397542	69.644071
977.972158	40.987781	69.649076
977.302148	37.619179	69.654081
976.812771	44.035835	69.659086
976.537052	46.516500	69.664090
975.906058	47.982409	69.669095
974.720000	53.993805	69.674100
974.125706	44.556892	69.679105
973.297104	50.141562	69.684110
972.685146	48.712915	69.689114
972.508333	43.397575	69.694119
971.224556	49.331369	69.699124
970.532677	45.878490	69.704129
969.807248	46.555746	69.709134
969.347847	37.380327	69.714138
969.363639	42.543686	69.719143
968.600420	49.029347	69.724148
967.784705	43.742905	69.729153
966.833744	40.213221	69.734158
965.992187	43.412471	69.739162
965.817891	40.012260	69.744167
965.173554	40.975613	69.749172
964.397817	46.485706	69.754177
963.499353	49.038685	69.759182
962.722025	45.212830	69.764186
962.708473	38.468685	69.769191
961.647003	40.725914	69.774196
961.261727	47.787076	69.779201
960.670481	46.039900	69.784206
959.545734	47.239470	69.789210
958.691144	47.046790	69.794215
957.995295	51.775875	69.799220
957.348651	43.232886	69.804225
957.048519	48.042216	69.809230
956.304664	48.217394	69.814234
956.037660	40.278432	69.819239
955.199584	54.141923	69.824244
954.281285	44.062252	69.829249
953.670987	44.724529	69.834254
953.260684	49.954944	69.839258
952.499114	41.807015	69.844263
951.684156	52.956821	69.849268
951.255030	45.244560	69.854273
951.163734	55.648357	69.859278
949.387464	52.348043	69.864282
948.772557	44.398800	69.869287
947.980090	52.334528	69.874292
947.746878	47.886173	69.879297
947.150477	54.741931	69.884302
946.312584	54.301274	69.889306
946.290952	49.334339	69.894311
945.576248	51.383374	69.899316
945.036955	50.225692	69.904321
944.030505	45.363875	69.909326
942.705220	52.256050	69.914330
942.145492	48.900930	69.919335
941.229546	50.736945	69.924340
940.646345	49.298246	69.929345
940.253780	52.655854	69.934350
939.734739	54.331529	69.939354
939.418392	42.369783	69.944359
939.224634	44.423144	69.949364
938.481602	43.783094	69.954369
937.234398	47.406673	69.959374
936.776526	49.809201	69.964378
935.969963	52.533936	69.969383
935.030350	57.667518	69.974388
934.812121	43.989318	69.979393
934.358957	49.492718	69.984398
932.769696	43.114361	69.989402
932.383499	50.294492	69.994407
931.683732	53.062906	69.999412
931.129201	56.779422	70.004417
930.879569	52.607418	70.009422
930.130792	52.513851	70.014426
929.138898	46.495395	70.019431
927.841078	51.550991	70.024436
927.960215	45.281858	70.029441
927.361693	47.800444	70.034446
926.881370	53.827154	70.039450
926.615963	46.674984	70.044455
925.304791	46.870756	70.049460
924.841838	49.932541	70.054465
924.363082	55.606502	70.059470
922.518218	50.693295	70.064474
922.089325	48.210197	70.069479
921.282307	43.511588	70.074484
921.174588	48.306910	70.079489
920.876672	45.422453	70.084494
920.848883	53.331816	70.089498
919.946654	46.060570	70.094503
918.447175	39.733944	70.099508
917.811389	43.937640	70.104513
917.923391	51.368346	70.109518
917.187268	52.871609	70.114522
916.111660	51.517249	70.119527
915.410715	51.899808	70.124532
915.071521	53.207595	70.129537
914.218020	51.765065	70.134542
913.013865	52.966799	70.139546
913.067970	50.305851	70.144551
912.558116	49.852040	70.149556
911.598448	47.561293	70.154561
910.666724	44.556851	70.159566
909.667091	54.373757	70.164570
909.621908	50.804599	70.169575
908.550175	52.019968	70.174580
908.624051	53.450417	70.179585
907.837448	52.124714	70.184590
906.519457	48.289240	70.189594
906.431856	50.872286	70.194599
905.414566	61.796637	70.199604
904.540205	55.163216	70.204609
904.233571	57.480637	70.209614
902.745948	59.550750	70.214618
902.973609	50.545407	70.219623
902.390312	49.844059	70.224628
902.121512	45.555349	70.229633
901.125951	52.814983	70.234638
899.741401	54.916388	70.239642
899.305867	44.868514	70.244647
899.033845	51.344653	70.249652
898.751377	49.983128	70.254657
897.652780	52.316199	70.259662
896.209546	51.527283	70.264666
896.285908	52.645875	70.269671
895.652640	48.323674	70.274676
895.327922	53.029854	70.279681
894.410338	54.165537	70.284686
893.537513	59.453861	70.289690
892.834290	50.299291	70.294695
892.195328	45.931095	70.299700
892.005376	57.103323	70.304705
890.949173	46.941111	70.309710
890.548671	55.565986	70.314714
890.056326	42.768387	70.319719
889.285354	55.793458	70.324724
887.787383	49.421978	70.329729
886.839473	51.168745	70.334734
886.456009	53.149212	70.339738
885.970237	50.451267	70.344743
885.648612	52.992296	70.349748
885.402051	53.439131	70.354753
885.072732	50.897931	70.359758
883.918607	57.644757	70.364762
883.643530	49.386674	70.369767
882.444177	47.568017	70.374772
881.015186	38.746175	70.379777
880.655123	44.648475	70.384782
880.047177	45.748098	70.389786
879.974909	42.663557	70.394791
879.469086	50.895175	70.399796
879.036576	47.207239	70.404801
878.183466	50.664652	70.409806
877.309821	50.714448	70.414810
876.945117	45.388670	70.419815
875.405590	46.602858	70.424820
874.567404	43.814101	70.429825
874.306810	43.171951	70.434830
873.608954	50.952145	70.439834
873.298750	42.177875	70.444839
872.786934	43.420103	70.449844
871.439631	42.938430	70.454849
870.864633	52.111848	70.459854
870.265127	54.478644	70.464858
870.040295	48.192642	70.469863
869.594377	47.631574	70.474868
868.568430	53.315975	70.479873
867.871809	50.244827	70.484878
866.886504	55.450977	70.489882
866.675008	46.349157	70.494887
866.116127	50.118919	70.499892
865.355914	50.296912	70.504897
864.453333	37.384073	70.509902
863.628185	61.676508	70.514906
863.073030	49.113078	70.519911
862.806541	50.909308	70.524916
861.825230	56.623959	70.529921
860.926710	52.072473	70.534926
860.192993	62.357367	70.539930
860.096360	50.812710	70.544935
859.659495	53.311903	70.549940
858.868877	51.634809	70.554945
858.079337	49.215465	70.559950
857.460895	51.123688	70.564954
857.283361	45.225092	70.569959
855.923578	53.046433	70.574964
854.900053	48.902789	70.579969
854.509504	46.993363	70.584974
853.781022	51.559109	70.589978
853.663170	42.635058	70.594983
852.273839	43.360920	70.599988
851.630434	39.424523	70.604993
851.065875	44.707412	70.609998
850.693417	49.280067	70.615002
850.576721	40.137148	70.620007
849.975111	51.347513	70.625012
848.724040	43.653303	70.630017
848.182114	47.247275	70.635022
847.153154	51.406224	70.640026
846.768664	42.596133	70.645031
845.747037	47.405106	70.650036
844.701481	49.932775	70.655041
845.009760	40.745088	70.660046
844.293080	48.490614	70.665050
843.995737	40.425424	70.670055
842.874743	43.483881	70.675060
841.342718	50.271363	70.680065
841.514379	45.530654	70.685070
840.636465	45.478562	70.690074
840.838580	36.760223	70.695079
839.698483	48.031245	70.700084
838.515623	49.350527	70.705089
837.942935	47.134819	70.710094
837.409451	57.301733	70.715098
837.101910	47.727710	70.720103
836.055835	50.715314	70.725108
834.948624	47.288208	70.730113
835.053639	40.519422	70.735118
834.369730	46.387199	70.740122
833.900298	45.941867	70.745127
832.617735	47.027978	70.750132
831.832016	47.524144	70.755137
831.377920	43.404936	70.760142
830.910614	42.726359	70.765146
830.816898	34.834704	70.770151
829.804742	42.892537	70.775156
828.864268	46.630958	70.780161
828.469917	41.798530	70.785166
827.917144	42.770687	70.790170
826.673379	40.977020	70.795175
825.819887	45.873242	70.800180
825.490331	47.719748	70.805185
825.167643	46.886143	70.810190
824.754524	46.444981	70.815194
823.929805	52.014003	70.820199
823.143671	49.012272	70.825204
822.427184	51.286221	70.830209
821.301274	48.720433	70.835214
820.342973	54.111823	70.840218
819.555188	41.808904	70.845223
819.407405	43.190480	70.850228
818.920211	51.050244	70.855233
819.044143	48.915729	70.860238
817.732341	53.751519	70.865242
817.052898	42.252235	70.870247
816.123678	47.143274	70.875252
815.532292	45.770332	70.880257
815.435582	48.622555	70.885262
814.510080	44.514628	70.890266
813.685767	39.643752	70.895271
812.730526	40.781557	70.900276
812.130456	48.479875	70.905281
812.152780	34.389076	70.910286
811.574687	50.950909	70.915290
810.791881	44.599055	70.920295
810.284970	46.163326	70.925300
808.752712	46.162144	70.930305
808.259584	40.126968	70.935310
807.231399	41.366080	70.940314
806.875083	41.570417	70.945319
806.791808	36.303807	70.950324
806.261693	38.848184	70.955329
805.313317	39.460632	70.960334
804.319060	46.280339	70.965338
803.567531	45.203633	70.970343
802.887761	40.717714	70.975348
802.122998	44.496695	70.980353
802.076245	36.190836	70.985358
800.929235	51.146532	70.990362
800.053949	45.163002	70.995367
799.588998	39.271414	71.000372
799.051648	41.387581	71.005377
799.100803	40.302398	71.010382
797.597861	49.206503	71.015386
796.922796	44.545314	71.020391
796.534008	41.045285	71.025396
795.780466	35.587586	71.030401
795.863830	34.959940	71.035406
795.008041	38.089022	71.040410
794.189110	39.600170	71.045415
793.290134	41.806702	71.050420
792.549451	45.685370	71.055425
791.483284	43.712087	71.060430
790.558776	43.354187	71.065434
790.413719	40.238306	71.070439
789.616696	36.020753	71.075444
789.215871	33.487078	71.080449
788.929064	32.125122	71.085454
788.687244	41.440003	71.090458
787.310882	41.299235	71.095463
787.006160	46.733397	71.100468
786.248844	47.456402	71.105473
784.937629	39.539636	71.110478
784.236227	44.045882	71.115482
783.726245	39.114064	71.120487
783.332234	41.722360	71.125492
782.691405	48.258515	71.130497
782.402252	38.319403	71.135502
781.607344	44.145016	71.140506
780.696881	50.738807	71.145511
780.647446	49.642882	71.150516
779.240098	52.381742	71.155521
778.447453	44.904273	71.160526
777.743385	51.961234	71.165530
777.531864	42.739440	71.170535
776.987895	44.848849	71.175540
775.754077	47.184977	71.180545
775.038679	41.820609	71.185550
774.327381	43.120307	71.190554
774.300258	45.304591	71.195559
774.119333	45.958465	71.200564
773.149928	48.606516	71.205569
771.978214	41.346741	71.210574
771.082078	46.175674	71.215578
770.527229	43.724828	71.220583
770.444121	37.104713	71.225588
769.476764	44.241904	71.230593
768.906383	35.730106	71.235598
767.902087	35.302988	71.240602
767.690513	39.934130	71.245607
767.013352	40.391579	71.250612
766.119409	44.588986	71.255617
765.802570	34.251618	71.260622
764.851064	42.505505	71.265626
764.229916	42.567722	71.270631
763.105523	40.753229	71.275636
762.574203	47.251679	71.280641
762.222800	45.456340	71.285646
761.325565	41.809743	71.290650
760.690427	44.988266	71.295655
760.772701	41.403599	71.300660
759.216580	45.709706	71.305665
758.688520	27.980777	71.310670
758.215300	36.954394	71.315674
757.852789	47.579486	71.320679
757.560490	36.196261	71.325684
756.096364	41.911529	71.330689
755.617118	37.182860	71.335694
755.035074	40.701610	71.340698
754.161438	38.270248	71.345703
753.244639	37.624866	71.350708
752.346376	43.888165	71.355713
751.710987	35.592364	71.360718
751.664719	36.466710	71.365722
751.215451	45.531355	71.370727
750.663585	42.273993	71.375732
749.689524	40.668211	71.380737
749.073804	30.011807	71.385742
748.426334	38.350181	71.390746
748.219621	40.236037	71.395751
746.529709	36.138295	71.400756
745.788209	44.122537	71.405761
745.522944	37.330746	71.410766
744.772659	43.351207	71.415770
744.274811	35.084738	71.420775
744.113437	33.346449	71.425780
743.251490	33.554915	71.430785
742.746685	28.196322	71.435790
741.616301	38.399955	71.440794
741.286102	40.570240	71.445799
740.538235	41.988700	71.450804
739.351331	41.903906	71.455809
739.044591	40.224859	71.460814
738.574278	41.653795	71.465818
737.963667	41.009645	71.470823
737.131067	33.711132	71.475828
736.415935	43.702325	71.480833
736.182236	36.313055	71.485838
735.337696	33.607123	71.490842
734.015485	39.221115	71.495847
733.571388	31.187797	71.500852
733.297994	38.912251	71.505857
732.926515	32.238127	71.510862
731.951286	35.203348	71.515866
730.985872	39.068417	71.520871
730.710685	41.714383	71.525876
729.747622	47.093968	71.530881
729.339899	38.489578	71.535886
728.106300	44.772040	71.540890
727.268661	36.171437	71.545895
726.917916	35.736572	71.550900
726.457011	42.662670	71.555905
726.192599	35.669431	71.560910
725.706383	40.256838	71.565914
724.572963	41.553071	71.570919
724.098107	43.169092	71.575924
723.138614	45.042207	71.580929
723.017885	39.810437	71.585934
721.389764	38.711426	71.590938
721.209104	41.940771	71.595943
721.017003	32.509623	71.600948
720.297640	43.298865	71.605953
719.263035	44.820131	71.610958
718.357069	40.739275	71.615962
718.002372	47.524819	71.620967
717.476445	47.260089	71.625972
716.130355	47.359273	71.630977
715.461899	38.301029	71.635982
715.193669	40.574771	71.640986
714.389505	45.275462	71.645991
713.952839	35.708589	71.650996
712.991284	40.386112	71.656001
712.954166	38.508912	71.661006
712.321872	47.932527	71.666010
711.269490	45.982164	71.671015
710.745475	32.236411	71.676020
710.003213	46.423335	71.681025
709.629589	34.228703	71.686030
708.408920	49.351357	71.691034
707.784798	39.743179	71.696039
707.438981	44.121809	71.701044
706.842428	53.538120	71.706049
706.448758	35.542241	71.711054
705.238081	44.482736	71.716058
704.201930	44.859992	71.721063
704.190294	44.822140	71.726068
703.154838	47.613354	71.731073
703.200365	40.647934	71.736078
701.825776	33.917519	71.741082
701.185571	40.511986	71.746087
701.558737	37.011295	71.751092
700.617016	48.404261	71.756097
699.508631	39.267843	71.761102
698.459013	43.215234	71.766106
698.009228	40.078542	71.771111
697.610243	40.215991	71.776116
696.801445	39.515015	71.781121
695.698318	34.427869	71.786126
694.839960	42.337402	71.791130
694.519604	44.197732	71.796135
693.944299	36.358992	71.801140
693.326093	46.086097	71.806145
693.342539	31.802520	71.811150
692.674768	41.455223	71.816154
691.210610	42.398016	71.821159
690.953950	39.899255	71.826164
690.182949	41.393129	71.831169
689.658409	32.879416	71.836174
689.024263	38.078319	71.841178
687.845008	36.251930	71.846183
687.679187	43.017350	71.851188
686.611152	47.478266	71.856193
686.479795	41.263507	71.861198
685.802728	33.603643	71.866202
685.106655	35.127309	71.871207
684.293219	34.062414	71.876212
683.737307	41.995523	71.881217
682.778973	39.226601	71.886222
681.813374	40.316865	71.891226
681.123863	34.976899	71.896231
680.940107	32.104485	71.901236
680.463854	43.812025	71.906241
680.123936	29.525166	71.911246
679.025273	45.407661	71.916250
678.381794	47.759903	71.921255
678.224565	35.090861	71.926260
677.079679	49.715034	71.931265
676.205707	41.701688	71.936270
675.532481	43.315779	71.941274
675.151923	40.692990	71.946279
674.466139	36.337594	71.951284
673.322723	49.735532	71.956289
672.856656	38.805621	71.961294
672.028154	38.062632	71.966298
671.706584	40.940745	71.971303
671.393964	35.001372	71.976308
670.681232	50.355542	71.981313
669.843079	35.469604	71.986318
669.385266	40.665929	71.991322
668.492261	39.038779	71.996327
667.588650	40.383674	72.001332
666.455091	46.551119	72.006337
666.215960	37.002514	72.011342
665.230033	37.677867	72.016346
665.094449	44.403767	72.021351
665.178002	44.927074	72.026356
663.825745	46.689473	72.031361
662.852777	39.968020	72.036366
662.529889	45.591600	72.041370
661.744466	49.991472	72.046375
661.465394	42.446176	72.051380
660.532688	43.473970	72.056385
659.678489	45.177092	72.061390
659.104972	46.055327	72.066394
658.575429	45.745436	72.071399
658.497526	35.985274	72.076404
657.272479	43.960003	72.081409
656.784830	35.407609	72.086414
655.997394	39.036157	72.091418
654.484406	42.556525	72.096423
654.300367	34.929823	72.101428
653.977401	44.795414	72.106433
653.373875	40.365931	72.111438
652.791900	40.908924	72.116442
651.617023	41.333246	72.121447
651.198207	45.793854	72.126452
650.314928	46.689242	72.131457
649.729770	42.906313	72.136462
649.370223	44.143394	72.141466
648.465143	41.752570	72.146471
648.144478	38.660470	72.151476
647.060328	38.398235	72.156481
646.553953	41.621809	72.161486
646.181424	39.228556	72.166490
645.736449	39.936356	72.171495
644.626907	36.128015	72.176500
643.552415	42.646111	72.181505
643.015082	42.313480	72.186510
642.620025	38.133661	72.191514
642.267862	44.763253	72.196519
641.003634	35.268710	72.201524
640.248431	45.867923	72.206529
640.043730	39.588765	72.211534
639.700821	37.670016	72.216538
638.750420	40.604160	72.221543
638.024081	38.911753	72.226548
637.148059	41.371337	72.231553
636.571680	31.666586	72.236558
636.477797	36.568861	72.241562
635.435785	35.262494	72.246567
634.790884	28.353801	72.251572
633.804108	39.742643	72.256577
633.302296	33.619386	72.261582
633.045733	40.505344	72.266586
631.848666	52.084558	72.271591
630.989445	37.572483	72.276596
630.675954	36.198532	72.281601
630.289481	33.201784	72.286606
629.801246	35.456384	72.291610
629.292184	42.022467	72.296615
628.572267	35.883292	72.301620
627.838175	39.411524	72.306625
626.672024	46.075980	72.311630
625.347507	37.516587	72.316634
624.771128	43.785143	72.321639
624.316982	31.544725	72.326644
623.504587	38.888263	72.331649
623.552869	36.401994	72.336654
623.106464	35.663808	72.341658
622.887642	38.354985	72.346663
621.849759	32.359496	72.351668
620.889323	34.408438	72.356673
620.466364	27.813412	72.361678
619.549375	31.474422	72.366682
618.424705	38.299522	72.371687
617.941313	37.767399	72.376692
617.534947	36.261344	72.381697
616.968519	37.856749	72.386702
616.922411	36.371070	72.391706
615.574898	37.450602	72.396711
615.130939	37.216443	72.401716
614.116278	41.996233	72.406721
613.442729	43.250012	72.411726
612.492232	36.817603	72.416730
611.581860	43.454419	72.421735
611.363376	33.277454	72.426740
610.779119	43.191363	72.431745
610.628841	39.291696	72.436750
610.316310	41.661448	72.441754
609.081834	48.511683	72.446759
608.728257	38.981116	72.451764
607.828686	49.854134	72.456769
606.571337	33.846425	72.461774
605.698416	33.690500	72.466778
604.883410	35.395598	72.471783
604.925427	44.160552	72.476788
604.163947	49.794942	72.481793
603.952034	43.578992	72.486798
603.690889	34.809390	72.491802
602.383848	47.287659	72.496807
601.782557	41.025932	72.501812
601.248536	37.393321	72.506817
600.737434	35.440634	72.511822
599.642403	38.682969	72.516826
598.617253	44.782116	72.521831
598.163123	37.764955	72.526836
597.463205	41.616923	72.531841
597.430208	33.533322	72.536846
596.732891	30.314327	72.541850
595.600764	40.861285	72.546855
594.976055	25.035310	72.551860
594.276621	41.352267	72.556865
593.968910	33.328367	72.561870
592.819522	33.492167	72.566874
591.953696	45.509597	72.571879
591.652538	36.804875	72.576884
591.066345	40.347242	72.581889
590.316519	42.476940	72.586894
590.398658	38.097346	72.591898
589.115325	45.336064	72.596903
588.154519	36.480697	72.601908
587.941410	39.258127	72.606913
587.285288	41.419530	72.611918
587.345715	39.077225	72.616922
585.697925	45.398709	72.621927
585.331492	45.775312	72.626932
584.763433	46.301719	72.631937
583.528799	37.990611	72.636942
582.926846	28.491955	72.641946
582.330374	41.465410	72.646951
581.881091	37.613426	72.651956
581.532865	42.877420	72.656961
580.562435	44.247990	72.661966
579.764485	37.963520	72.666970
578.845888	41.808356	72.671975
578.552808	39.699506	72.676980
578.292513	37.896469	72.681985
577.409875	36.040996	72.686990
576.915855	38.684990	72.691994
576.143347	41.041194	72.696999
575.345213	36.834139	72.702004
574.145161	43.238373	72.707009
573.325803	45.007772	72.712014
573.405409	37.142101	72.717018
572.616556	44.923691	72.722023
572.489658	35.379555	72.727028
571.767673	45.018660	72.732033
570.445057	48.186320	72.737038
570.051264	36.955117	72.742042
569.292178	43.205642	72.747047
568.963991	35.580756	72.752052
568.009917	48.911132	72.757057
567.272339	47.896808	72.762062
566.847618	35.971866	72.767066
565.926949	44.343642	72.772071
565.470994	35.639397	72.777076
564.160306	41.613404	72.782081
563.596488	49.556165	72.787086
563.217087	46.270068	72.792090
562.866485	53.020968	72.797095
562.639921	35.416474	72.802100
561.760759	46.972403	72.807105
560.537702	40.808932	72.812110
559.986597	41.880300	72.817114
559.266404	45.426291	72.822119
559.122226	41.029032	72.827124
558.098605	43.961525	72.832129
557.402522	48.748709	72.837134
557.200676	36.124435	72.842138
555.904008	44.488010	72.847143
554.815855	39.657270	72.852148
554.061107	38.389721	72.857153
553.456723	47.107940	72.862158
553.553435	39.100399	72.867162
552.943964	47.333596	72.872167
552.802342	40.196977	72.877172
551.819991	39.141708	72.882177
550.842305	35.523945	72.887182
550.594648	42.511791	72.892186
549.849076	39.419091	72.897191
548.748036	35.050009	72.902196
548.096535	41.274206	72.907201
547.441162	39.712147	72.912206
547.112935	42.652980	72.917210
546.006631	42.912034	72.922215
544.993661	36.569685	72.927220
544.712686	37.654765	72.932225
544.072203	37.652038	72.937230
543.874938	34.015809	72.942234
543.471129	41.266450	72.947239
542.533491	35.524185	72.952244
541.607421	32.024284	72.957249
540.838931	38.489172	72.962254
540.357241	35.217450	72.967258
539.396775	43.200938	72.972263
538.614586	32.357595	72.977268
538.154678	38.507911	72.982273
537.700878	41.028577	72.987278
537.404758	36.641567	72.992282
536.096890	42.754037	72.997287
535.367412	39.308076	73.002292
534.407521	38.589600	73.007297
534.172624	50.858906	73.012302
533.735042	37.659669	73.017306
533.097578	39.567632	73.022311
532.658820	29.438689	73.027316
531.518795	33.371601	73.032321
531.090049	43.263205	73.037326
530.997546	43.506037	73.042330
529.922542	39.711149	73.047335
528.824160	34.716391	73.052340
528.246162	43.749411	73.057345
527.824112	42.221579	73.062350
527.266318	43.138975	73.067354
525.943863	54.599171	73.072359
525.864754	44.351754	73.077364
525.388832	40.596309	73.082369
525.026434	54.407115	73.087374
523.299702	44.820950	73.092378
522.742892	38.484911	73.097383
521.986764	40.159013	73.102388
521.661111	47.464550	73.107393
521.210159	40.111350	73.112398
520.782100	37.592238	73.117402
519.411899	47.730031	73.122407
518.966587	40.033647	73.127412
518.244362	40.484643	73.132417
517.806137	49.845800	73.137422
517.825140	36.336632	73.142426
516.761922	51.753622	73.147431
515.506159	43.569306	73.152436
515.258809	46.630485	73.157441
514.162391	50.847625	73.162446
513.827037	40.584125	73.167450
513.009753	57.065756	73.172455
511.936818	39.538804	73.177460
511.800944	42.056305	73.182465
511.055617	47.194938	73.187470
511.282200	39.807345	73.192474
509.787606	42.229270	73.197479
509.041365	42.017710	73.202484
508.595632	38.211703	73.207489
507.653596	50.981106	73.212494
507.577954	35.977587	73.217498
506.950554	46.554116	73.222503
506.211944	48.774662	73.227508
505.608371	49.120464	73.232513
504.539046	50.448392	73.237518
503.671935	45.787407	73.242522
502.914932	42.163810	73.247527
502.498103	39.083072	73.252532
501.703471	47.502334	73.257537
501.495201	49.048219	73.262542
501.060695	45.127795	73.267546
499.832593	48.050342	73.272551
498.966352	45.639079	73.277556
498.813617	38.701728	73.282561
498.409722	48.967213	73.287566
497.519639	35.948546	73.292570
496.496501	50.094793	73.297575
495.833782	45.174982	73.302580
495.440941	40.308395	73.307585
494.930594	45.949494	73.312590
494.015963	34.975313	73.317594
493.531195	51.016690	73.322599
492.966575	37.865283	73.327604
491.929792	31.766228	73.332609
490.731845	46.197018	73.337614
490.267841	36.414228	73.342618
489.868155	47.238300	73.347623
489.536708	44.779210	73.352628
488.982396	39.800170	73.357633
488.288805	41.223969	73.362638
487.336030	39.911029	73.367642
486.716190	46.369003	73.372647
486.175598	46.155757	73.377652
485.455818	44.069116	73.382657
484.626174	51.204850	73.387662
483.889033	41.061519	73.392666
483.444840	53.972575	73.397671
482.854845	43.339449	73.402676
482.196718	50.172649	73.407681
481.773506	50.733453	73.412686
480.682206	38.194114	73.417690
480.042106	44.387549	73.422695
479.677984	43.923418	73.427700
479.251311	46.685741	73.432705
477.896328	53.043919	73.437710
477.260379	47.341542	73.442714
476.404241	49.867610	73.447719
475.855688	44.739566	73.452724
476.018174	42.052555	73.457729
475.061005	56.490644	73.462734
474.610046	40.336512	73.467738
473.841120	44.527536	73.472743
473.312414	48.528195	73.477748
471.957772	46.890988	73.482753
470.793791	43.227014	73.487758
470.435261	45.560052	73.492762
469.911360	49.684618	73.497767
469.766708	46.760913	73.502772
469.443683	39.789987	73.507777
468.273263	48.154839	73.512782
467.949360	39.467847	73.517786
467.096368	57.851802	73.522791
466.791907	47.975358	73.527796
465.602870	50.367828	73.532801
464.686917	46.767924	73.537806
464.289245	47.239490	73.542810
463.872143	50.814469	73.547815
462.900781	43.174296	73.552820
461.990014	45.067133	73.557825
461.357185	50.301749	73.562830
461.088114	52.342765	73.567834
460.433666	53.401855	73.572839
460.094601	50.847763	73.577844
458.923833	58.870070	73.582849
458.037599	64.414154	73.587854
457.641015	55.391078	73.592858
457.198535	45.087525	73.597863
456.629250	52.833870	73.602868
455.426334	49.379059	73.607873
454.381809	57.113301	73.612878
454.221910	50.652413	73.617882
454.154063	49.089151	73.622887
453.315180	48.766378	73.627892
452.990426	43.336712	73.632897
451.634683	48.100775	73.637902
451.531010	38.353342	73.642906
450.225507	49.874585	73.647911
449.309241	51.527591	73.652916
449.050953	45.447888	73.657921
447.912912	46.388548	73.662926
448.166478	41.838273	73.667930
447.553682	50.678721	73.672935
446.958302	42.447967	73.677940
445.722976	36.813975	73.682945
445.101085	49.972965	73.687950
444.412433	37.110048	73.692954
443.616372	40.703392	73.697959
442.494083	44.809722	73.702964
442.199116	42.452142	73.707969
441.052701	37.522084	73.712974
441.010525	42.192874	73.717978
440.676730	38.454136	73.722983
440.399293	32.664677	73.727988
439.894503	47.468104	73.732993
438.438239	41.705801	73.737998
437.881965	37.857961	73.743002
437.477333	41.581189	73.748007
436.703662	47.908038	73.753012
435.937342	51.452871	73.758017
434.837180	51.330789	73.763022
434.774914	38.914311	73.768026
434.188523	46.995540	73.773031
433.195540	41.856831	73.778036
432.413385	44.689154	73.783041
431.832407	52.930897	73.788046
431.640307	50.010983	73.793050
430.841619	59.116963	73.798055
429.941295	52.985849	73.803060
429.483666	49.525290	73.808065
428.740293	47.732817	73.813070
428.067894	39.243705	73.818074
426.860948	44.600789	73.823079
425.815931	50.444436	73.828084
425.656740	44.558136	73.833089
424.732152	50.021561	73.838094
425.235774	37.768618	73.843098
424.432511	40.362205	73.848103
423.836600	40.281597	73.853108
422.877226	42.753132	73.858113
422.165835	47.616763	73.863118
421.330308	44.687125	73.868122
420.286547	44.183166	73.873127
419.776637	47.241978	73.878132
419.320326	36.847657	73.883137
418.478231	49.190223	73.888142
418.175126	45.417017	73.893146
417.940652	45.551558	73.898151
416.525521	47.103758	73.903156
415.853507	45.968493	73.908161
415.003623	60.183346	73.913166
415.092198	45.289841	73.918170
414.493289	48.354038	73.923175
413.453475	50.601743	73.928180
412.637241	49.007670	73.933185
412.221668	50.931697	73.938190
412.017484	53.028300	73.943194
410.367752	56.258771	73.948199
409.266265	60.474040	73.953204
409.363613	46.734359	73.958209
408.519523	53.660616	73.963214
408.441039	41.108375	73.968218
407.929519	49.549385	73.973223
407.248734	50.676939	73.978228
406.402057	42.433606	73.983233
405.435384	56.589529	73.988238
404.993190	46.857878	73.993242
404.064778	51.055719	73.998247
403.629413	50.246588	74.003252
403.181449	53.277419	74.008257
402.554893	45.313711	74.013262
401.739673	43.866695	74.018266
400.561228	48.536441	74.023271
399.955309	46.723968	74.028276
399.554233	43.906579	74.033281
399.047767	48.098420	74.038286
397.761505	45.664431	74.043290
397.165964	40.182502	74.048295
396.605365	44.051271	74.053300
396.495734	45.629199	74.058305
395.886766	52.953293	74.063310
395.559030	49.958344	74.068314
394.325097	41.640075	74.073319
393.593293	41.808142	74.078324
393.216336	39.389624	74.083329
392.350924	46.473866	74.088334
391.601402	45.567402	74.093338
390.511722	42.184384	74.098343
389.878516	44.366355	74.103348
389.995617	33.912057	74.108353
389.296337	44.386044	74.113358
388.136239	38.880485	74.118362
387.305498	46.284030	74.123367
386.619315	43.831276	74.128372
386.369006	37.201959	74.133377
385.591582	38.639744	74.138382
385.521498	39.864335	74.143386
384.559102	42.735844	74.148391
383.710031	47.115868	74.153396
383.469635	43.130616	74.158401
382.820201	50.192845	74.163406
382.072170	44.682187	74.168410
380.898961	48.680816	74.173415
380.084548	44.879593	74.178420
379.953646	40.658484	74.183425
378.649001	55.694518	74.188430
377.972250	39.324915	74.193434
377.779025	42.374056	74.198439
377.019072	40.832710	74.203444
377.008719	38.402281	74.208449
375.808123	46.707585	74.213454
374.969072	43.192807	74.218458
374.281294	45.639512	74.223463
373.585552	39.288630	74.228468
373.287566	39.435241	74.233473
372.586580	42.801919	74.238478
372.159043	38.117338	74.243482
371.477082	53.435444	74.248487
370.330552	51.628397	74.253492
370.422434	46.943998	74.258497
369.036528	47.329166	74.263502
368.180761	40.299568	74.268506
368.048057	44.442351	74.273511
367.145396	40.737173	74.278516
367.235674	41.528515	74.283521
365.332625	50.571152	74.288526
365.119462	49.180816	74.293530
364.554219	47.239412	74.298535
364.098178	40.347347	74.303540
363.155549	40.733514	74.308545
362.361016	42.728019	74.313550
361.836147	36.605207	74.318554
361.215807	38.709980	74.323559
361.202548	46.943232	74.328564
360.504022	36.865946	74.333569
359.153558	44.500664	74.338574
358.858759	45.794557	74.343578
358.032798	39.263113	74.348583
356.648769	44.336369	74.353588
355.958450	34.210314	74.358593
355.265550	49.343986	74.363598
355.342627	47.498536	74.368602
354.825063	48.957707	74.373607
354.118729	44.970608	74.378612
354.083107	42.790021	74.383617
352.566534	40.571956	74.388622
352.125163	47.774174	74.393626
351.655387	44.089538	74.398631
350.530019	41.068679	74.403636
349.658811	38.796056	74.408641
349.028693	51.286627	74.413646
348.590612	44.850537	74.418650
348.333417	44.404009	74.423655
347.929112	41.040502	74.428660
346.966237	37.888775	74.433665
345.887387	44.196494	74.438670
345.486790	36.346830	74.443674
344.929897	40.305356	74.448679
343.931472	44.660854	74.453684
343.499984	37.883000	74.458689
342.537762	47.259362	74.463694
342.305257	41.836399	74.468698
341.765025	39.181412	74.473703
340.554701	44.938147	74.478708
339.699397	31.962125	74.483713
339.145024	44.006313	74.488718
338.652300	48.343425	74.493722
338.252358	36.958992	74.498727
337.745957	45.170584	74.503732
337.029734	42.632203	74.508737
336.190771	42.475244	74.513742
336.020072	45.806693	74.518746
335.035333	49.562252	74.523751
333.531967	46.841038	74.528756
333.264369	47.909231	74.533761
332.206964	48.330470	74.538766
331.902849	45.513838	74.543770
331.746572	41.602194	74.548775
331.034320	44.637274	74.553780
330.517977	39.060079	74.558785
329.327972	48.648369	74.563790
329.201220	43.494238	74.568794
328.539602	38.028385	74.573799
327.619538	40.620296	74.578804
326.982648	46.962789	74.583809
326.018583	54.613392	74.588814
325.807805	45.188652	74.593818
325.424969	41.951723	74.598823
323.952695	46.486725	74.603828
323.127232	28.057764	74.608833
322.551017	42.945260	74.613838
322.128910	36.156724	74.618842
322.071691	37.343191	74.623847
321.243423	46.606207	74.628852
320.458307	42.964966	74.633857
320.087437	46.326777	74.638862
318.966123	41.324561	74.643866
317.770367	42.735774	74.648871
316.737993	46.933684	74.653876
316.960853	38.397332	74.658881
316.123314	48.104411	74.663886
316.010506	45.265648	74.668890
315.513933	43.177094	74.673895
314.401910	43.397711	74.678900
313.762875	37.978909	74.683905
313.067046	48.333501	74.688910
312.804054	44.394757	74.693914
311.948459	47.150480	74.698919
311.049218	53.785822	74.703924
310.603758	46.319222	74.708929
309.487703	41.945280	74.713934
308.997896	43.272205	74.718938
308.100374	37.056574	74.723943
307.305181	49.896340	74.728948
307.231883	44.164266	74.733953
306.604416	52.386351	74.738958
306.117346	47.492520	74.743962
305.708299	36.540681	74.748967
304.590647	47.630297	74.753972
303.838703	40.855272	74.758977
302.855839	54.077318	74.763982
302.170915	47.331459	74.768986
301.334670	44.274478	74.773991
300.412276	40.345343	74.778996
300.177178	39.898979	74.784001
299.897492	49.892131	74.789006
299.318624	45.969637	74.794010
299.150955	44.281788	74.799015
298.120294	43.483524	74.804020
297.483021	38.051397	74.809025
296.823443	41.711362	74.814030
295.956334	41.976842	74.819034
294.782462	41.113525	74.824039
294.116492	46.771046	74.829044
293.949866	37.575181	74.834049
293.510888	44.741069	74.839054
292.904972	34.503464	74.844058
291.760467	42.601810	74.849063
290.773767	45.535130	74.854068
290.969527	41.109623	74.859073
290.221473	43.289581	74.864078
289.498451	44.127171	74.869082
288.541885	34.793172	74.874087
287.752932	45.692640	74.879092
287.569254	37.153345	74.884097
286.871327	41.376429	74.889102
285.729755	46.696680	74.894106
284.683855	36.859733	74.899111
284.195512	44.896531	74.904116
284.109764	43.123198	74.909121
283.236549	38.456998	74.914126
282.808705	43.874768	74.919130
282.471762	37.184134	74.924135
280.783007	36.892598	74.929140
280.821193	35.206175	74.934145
280.550157	42.568262	74.939150
279.488983	41.642609	74.944154
278.438895	33.555753	74.949159
277.579998	43.174525	74.954164
277.542560	40.561252	74.959169
276.681521	38.993043	74.964174
276.148507	46.887902	74.969178
275.623057	39.152012	74.974183
274.610299	39.673763	74.979188
274.268669	38.984360	74.984193
273.766917	42.196905	74.989198
272.734574	37.434833	74.994202
271.979745	32.032731	74.999207
271.229991	39.317014	75.004212
271.142044	34.309388	75.009217
270.117958	42.247368	75.014222
269.497651	36.932727	75.019226
269.020781	41.125026	75.024231
268.318229	54.715845	75.029236
267.834232	41.478442	75.034241
266.642648	40.467389	75.039246
265.993982	48.462989	75.044250
265.888947	41.916935	75.049255
264.754106	49.437351	75.054260
263.851071	43.257804	75.059265
262.776363	46.471067	75.064270
262.297122	45.140951	75.069274
262.032437	33.136151	75.074279
261.440508	50.638159	75.079284
261.254768	35.801179	75.084289
260.831255	37.786572	75.089294
259.234549	46.404120	75.094298
258.986629	37.397053	75.099303
258.298914	43.805494	75.104308
257.903027	34.903524	75.109313
256.791267	44.584193	75.114318
255.449582	40.127766	75.119322
255.412685	37.984899	75.124327
254.717654	43.950938	75.129332
254.519481	43.632843	75.134337
254.190818	38.756078	75.139342
252.770109	36.807784	75.144346
252.638294	47.593431	75.149351
251.793267	41.199088	75.154356
251.329077	43.255004	75.159361
250.596828	44.842952	75.164366
249.543313	40.610667	75.169370
249.132577	33.865981	75.174375
247.999497	51.552717	75.179380
246.932668	45.862275	75.184385
246.206585	37.655156	75.189390
246.222720	42.902486	75.194394
246.030932	29.556988	75.199399
245.144777	48.797218	75.204404
245.018759	40.219624	75.209409
244.042085	45.844359	75.214414
243.129108	44.947387	75.219418
242.635386	39.015035	75.224423
241.186711	45.577994	75.229428
240.763403	32.730442	75.234433
239.794701	40.586699	75.239438
239.297771	39.047263	75.244442
238.885170	43.024482	75.249447
238.535429	50.240994	75.254452
238.499840	43.075180	75.259457
237.335189	50.158632	75.264462
235.977030	56.454649	75.269466
235.760265	43.760752	75.274471
235.077452	43.361927	75.279476
234.876306	44.855286	75.284481
233.571777	46.427262	75.289486
232.701766	50.282770	75.294490
232.582292	48.324179	75.299495
231.799717	54.911904	75.304500
231.670211	39.767674	75.309505
230.926275	40.263483	75.314510
229.860636	43.192188	75.319514
229.829123	47.496429	75.324519
228.156121	51.535371	75.329524
227.483099	42.601570	75.334529
226.506605	42.487547	75.339534
226.473027	42.704890	75.344538
226.021206	46.649756	75.349543
225.444913	55.718417	75.354548
225.024145	44.533349	75.359553
223.762925	47.796353	75.364558
223.304310	47.291603	75.369562
222.990511	36.022683	75.374567
221.951827	49.024576	75.379572
221.171364	36.927417	75.384577
220.500315	40.280690	75.389582
219.948890	43.451626	75.394586
219.644192	42.456704	75.399591
218.380629	52.054069	75.404596
217.978068	39.932389	75.409601
217.127803	36.437332	75.414606
216.760648	43.963517	75.419610
216.304579	35.941423	75.424615
215.179353	33.871046	75.429620
214.495490	36.306836	75.434625
214.438616	39.108803	75.439630
212.781293	45.593858	75.444634
212.402696	31.822520	75.449639
211.387006	47.765027	75.454644
211.281477	38.171882	75.459649
211.103982	35.144490	75.464654
210.318011	44.938650	75.469658
209.687095	40.145674	75.474663
208.398754	43.936719	75.479668
207.966006	38.137992	75.484673
207.726237	42.232813	75.489678
206.845622	47.757014	75.494682
206.089407	44.085976	75.499687
205.306172	46.239216	75.504692
204.727244	44.008092	75.509697
204.266675	37.721138	75.514702
203.233026	45.828916	75.519706
202.580215	39.451766	75.524711
201.668842	47.358989	75.529716
201.414127	38.513349	75.534721
201.129340	43.319265	75.539726
199.902360	54.617891	75.544730
199.415709	49.383762	75.549735
198.905530	48.529453	75.554740
198.678142	36.128294	75.559745
197.644445	35.057038	75.564750
196.397015	42.902270	75.569754
195.605665	42.183788	75.574759
195.025610	41.549867	75.579764
194.395023	39.710868	75.584769
194.403363	44.092743	75.589774
193.792486	39.973662	75.594778
193.219777	40.405391	75.599783
192.288115	48.500819	75.604788
191.716996	41.236956	75.609793
191.039262	37.413136	75.614798
190.122582	40.785626	75.619802
189.420218	34.683406	75.624807
188.605105	41.798123	75.629812
188.656768	37.299431	75.634817
187.307163	42.914293	75.639822
186.036832	43.718623	75.644826
186.346334	35.302812	75.649831
185.159021	41.973733	75.654836
185.063206	38.693540	75.659841
184.195896	36.896701	75.664846
184.062354	40.110470	75.669850
183.336863	31.887874	75.674855
182.676090	39.614382	75.679860
181.581214	32.934886	75.684865
180.564863	41.009701	75.689870
179.678974	51.364515	75.694874
179.393242	44.349344	75.699879
178.963919	46.940044	75.704884
178.564410	36.105801	75.709889
178.154755	38.241578	75.714894
176.904557	48.085325	75.719898
176.047488	39.972909	75.724903
175.489245	46.792162	75.729908
175.055373	33.041754	75.734913
174.949348	38.986557	75.739918
174.142720	42.966594	75.744922
173.104159	31.369591	75.749927
172.523044	34.699162	75.754932
171.563129	31.257253	75.759937
170.578661	40.334698	75.764942
169.686753	38.881532	75.769946
169.450971	35.891765	75.774951
168.803456	33.228750	75.779956
168.382739	28.432118	75.784961
168.225833	33.715025	75.789966
167.858963	40.642776	75.794970
167.041850	35.870283	75.799975
165.743982	33.891880	75.804980
164.504913	41.597535	75.809985
164.043355	35.528639	75.814990
163.290375	37.338823	75.819994
163.014082	33.698411	75.824999
162.986798	42.192979	75.830004
162.560978	30.880519	75.835009
161.508992	36.684348	75.840014
160.632347	41.675801	75.845018
160.348515	37.921030	75.850023
158.798624	40.963946	75.855028
158.257245	32.575592	75.860033
157.408366	31.593838	75.865038
156.773061	38.232891	75.870042
156.615058	32.370101	75.875047
155.882169	27.836579	75.880052
155.233743	28.073279	75.885057
154.345437	29.940213	75.890062
153.731445	38.450100	75.895066
153.765857	30.739438	75.900071
152.710726	39.143778	75.905076
151.677311	31.487104	75.910081
151.494061	31.820495	75.915086
150.567046	43.793572	75.920090
150.180447	35.302109	75.925095
148.814542	37.209476	75.930100
147.927173	30.332586	75.935105
147.717600	35.609128	75.940110
146.973987	44.494902	75.945114
146.972917	37.801178	75.950119
146.764246	41.072824	75.955124
145.334838	42.252178	75.960129
144.565903	39.345524	75.965134
143.540174	46.887514	75.970138
143.366327	40.202490	75.975143
143.151334	46.165580	75.980148
142.453488	36.231516	75.985153
142.013841	31.519048	75.990158
140.573801	41.494810	75.995162
139.881399	40.479919	76.000167
138.803924	44.875843	76.005172
138.609353	40.742636	76.010177
138.393734	42.854624	76.015182
137.216123	46.701699	76.020186
136.424094	35.560569	76.025191
135.426991	44.204819	76.030196
134.618293	40.698311	76.035201
134.701485	33.930147	76.040206
133.913787	33.074875	76.045210
133.906714	33.073740	76.050215
133.310575	39.167693	76.055220
132.496299	28.419174	76.060225
132.037768	32.961998	76.065230
130.366258	37.927496	76.070234
129.554102	28.315781	76.075239
128.720048	38.104371	76.080244
128.266645	36.816417	76.085249
128.095985	35.103041	76.090254
127.557665	45.628386	76.095258
127.227075	32.818646	76.100263
126.611032	40.574197	76.105268
125.636136	46.751243	76.110273
125.456471	40.092874	76.115278
124.265033	39.538121	76.120282
123.089626	33.779893	76.125287
122.468680	40.489903	76.130292
121.940776	44.396506	76.135297
121.780652	38.749988	76.140302
120.974681	42.268895	76.145306
120.418318	43.782104	76.150311
119.523890	51.667883	76.155316
118.944026	40.068828	76.160321
118.741783	37.016871	76.165326
116.957583	38.375078	76.170330
116.445465	34.094222	76.175335
115.804187	38.469443	76.180340
115.497318	38.318007	76.185345
115.027476	40.351614	76.190350
114.330260	44.703666	76.195354
113.893393	45.665107	76.200359
112.528804	43.606190	76.205364
112.173472	44.608518	76.210369
112.027083	33.873386	76.215374
111.011237	32.019928	76.220378
110.032730	39.474881	76.225383
109.136321	41.467943	76.230388
108.953220	40.202330	76.235393
108.706346	33.790342	76.240398
107.775908	39.753726	76.245402
106.862889	40.166445	76.250407
106.176795	40.216201	76.255412
105.494605	38.682886	76.260417
105.051931	43.347724	76.265422
104.731252	49.244466	76.270426
104.115852	39.636911	76.275431
103.022614	43.570179	76.280436
102.291303	49.811252	76.285441
101.665298	39.779227	76.290446
100.271557	42.451991	76.295450
99.814353	46.875389	76.300455
99.721361	36.825401	76.305460
98.599393	37.694708	76.310465
98.536921	36.213427	76.315470
97.864556	42.916467	76.320474
97.825224	39.870131	76.325479
96.405846	44.894251	76.330484
95.701787	44.501853	76.335489
95.575736	29.575737	76.340494
94.285568	44.306172	76.345498
93.328325	39.236424	76.350503
92.861313	50.214912	76.355508
92.467149	55.787170	76.360513
92.103592	41.427520	76.365518
91.324150	47.106880	76.370522
90.236334	40.543033	76.375527
89.721441	44.113876	76.380532
89.124114	46.148423	76.385537
89.116022	47.852619	76.390542
87.940312	45.158996	76.395546
86.796040	38.273273	76.400551
85.778876	40.404665	76.405556
85.720145	39.030894	76.410561
85.448713	35.745292	76.415566
84.885158	37.911802	76.420570
84.469793	44.866421	76.425575
83.115114	34.073204	76.430580
82.031643	41.035400	76.435585
82.211204	35.164476	76.440590
80.911969	41.989201	76.445594
80.301562	47.221187	76.450599
79.753418	36.318505	76.455604
78.996969	41.856168	76.460609
78.873493	31.542219	76.465614
78.396101	43.723195	76.470618
77.466644	42.195965	76.475623
76.706505	45.646629	76.480628
75.730400	38.698526	76.485633
75.361002	34.685689	76.490638
73.915448	36.705806	76.495642
73.605443	30.681202	76.500647
73.338813	39.859782	76.505652
72.768916	35.669754	76.510657
72.716515	36.730271	76.515662
71.772700	47.709195	76.520666
71.117576	36.619212	76.525671
69.858465	39.979778	76.530676
68.844174	41.273102	76.535681
68.199926	37.595923	76.540686
67.490662	37.733730	76.545690
67.237981	27.552063	76.550695
67.199422	43.214153	76.555700
66.451007	38.423983	76.560705
65.423773	39.971749	76.565710
64.358338	44.609555	76.570714
64.207561	30.492107	76.575719
63.819330	33.102214	76.580724
62.934483	33.801408	76.585729
62.144923	41.068456	76.590734
60.830149	40.420399	76.595738
60.845496	36.736310	76.600743
60.264131	35.564640	76.605748
59.307044	47.848784	76.610753
58.587590	38.646689	76.615758
57.933947	36.283540	76.620762
57.155635	32.151353	76.625767
56.905446	32.638715	76.630772
56.251177	46.134806	76.635777
55.415403	31.020532	76.640782
54.138919	36.042659	76.645786
54.028425	31.241403	76.650791
53.224216	32.566601	76.655796
52.904499	38.111091	76.660801
52.636986	30.890333	76.665806
51.812353	37.535407	76.670810
50.974959	33.081004	76.675815
50.437717	34.640676	76.680820
49.462252	32.715182	76.685825
48.770755	38.733916	76.690830
47.963992	41.882334	76.695834
47.603388	40.659394	76.700839
47.164126	36.051471	76.705844
46.071893	37.243698	76.710849
45.503741	38.717097	76.715854
44.684125	52.391928	76.720858
44.359333	36.811118	76.725863
43.756658	42.057172	76.730868
43.026135	34.825410	76.735873
41.984424	39.453625	76.740878
41.164817	46.570708	76.745882
40.882889	44.075542	76.750887
40.712000	40.918353	76.755892
39.359693	46.761067	76.760897
38.578018	36.796405	76.765902
38.077026	46.932086	76.770906
37.820361	38.208771	76.775911
37.748298	41.840656	76.780916
36.595617	34.903500	76.785921
35.769288	32.379318	76.790926
35.097330	49.246914	76.795930
34.024540	43.523218	76.800935
33.120061	31.745785	76.805940
32.421659	34.388155	76.810945
32.300343	28.543166	76.815950
31.453178	33.590759	76.820954
30.999219	35.774008	76.825959
30.898987	40.278693	76.830964
30.078431	40.742674	76.835969
29.276150	42.039127	76.840974
28.151445	45.344687	76.845978
27.894506	45.709268	76.850983
27.303813	48.907874	76.855988
26.041445	49.355641	76.860993
25.740711	44.154003	76.865998
25.008324	56.202273	76.871002
24.720243	47.691960	76.876007
23.997205	43.819099	76.881012
22.918956	50.637133	76.886017
22.411038	43.141428	76.891022
22.025144	46.836991	76.896026
20.960310	30.463797	76.901031
20.559893	47.357854	76.906036
19.176304	50.856217	76.911041
19.179663	41.463490	76.916046
18.444598	50.562139	76.921050
18.025972	36.907041	76.926055
17.053243	48.253667	76.931060
16.292966	49.752907	76.936065
16.216148	37.535161	76.941070
15.225878	45.039906	76.946074
14.468508	39.263318	76.951079
13.633027	33.947729	76.956084
12.846671	47.432524	76.961089
12.944965	42.847295	76.966094
12.540741	46.635995	76.971098
11.578931	43.247339	76.976103
10.787955	49.328923	76.981108
9.634510	49.109902	76.986113
9.416521	34.870572	76.991118
8.040176	49.953277	76.996122
7.593102	35.871640	77.001127
7.551984	40.528415	77.006132
6.848172	43.354469	77.011137
6.733827	29.218945	77.016142
5.282821	37.163848	77.021147
4.227409	40.791063	77.026151
4.229019	39.494968	77.031156
3.263379	45.983056	77.036161