Tue Jun 08 17:20:55 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
0.076345	105.317552	0.000000
-0.500213	93.039777	0.005005
-0.854183	60.221285	0.010010
-2.665614	18.558602	0.015014
-6.216349	-0.358552	0.020019
-11.202140	-0.173507	0.025024
-17.089058	2.097374	0.030029
-21.485906	-6.356935	0.035034
-25.336926	2.145099	0.040038
-29.198636	0.225445	0.045043
-32.821000	-6.233762	0.050048
-36.449557	0.009492	0.055053
-39.703776	-2.648616	0.060058
-43.837659	15.434996	0.065062
-47.626056	6.041959	0.070067
-51.196714	0.622250	0.075072
-55.334081	0.059932	0.080077
-58.735857	0.194061	0.085082
-62.539498	4.146853	0.090086
-66.419871	-1.381170	0.095091
-70.110542	-5.322220	0.100096
-74.012475	6.862943	0.105101
-77.366741	0.903290	0.110106
-81.510152	4.527543	0.115110
-84.970520	0.391102	0.120115
-88.754608	-3.430105	0.125120
-93.074923	14.067788	0.130125
-96.569478	-1.960942	0.135130
-100.636565	5.518009	0.140134
-104.254358	-3.507146	0.145139
-107.947265	-2.350095	0.150144
-111.467476	15.991860	0.155149
-115.055146	1.213768	0.160154
-118.941458	-1.361939	0.165158
-122.597890	1.516516	0.170163
-126.455032	3.986529	0.175168
-130.912035	7.511849	0.180173
-134.297049	-3.640031	0.185178
-137.677897	-5.316810	0.190182
-141.284956	1.152161	0.195187
-145.173602	-9.794136	0.200192
-148.919443	-5.049927	0.205197
-152.982065	-7.901662	0.210202
-157.004281	-7.329107	0.215206
-160.612547	1.743593	0.220211
-164.333729	-2.676454	0.225216
-168.547648	9.166389	0.230221
-172.196812	-0.087785	0.235226
-175.651960	7.601262	0.240230
-179.700787	-2.230504	0.245235
-183.494656	-0.708338	0.250240
-186.958794	8.464395	0.255245
-189.873851	1.910464	0.260250
-194.262609	2.780371	0.265254
-198.019688	3.292886	0.270259
-201.536676	2.100920	0.275264
-205.744067	12.156612	0.280269
-209.780156	0.265066	0.285274
-213.530038	-3.372043	0.290278
-217.236666	4.538175	0.295283
-220.576051	0.277286	0.300288
-224.450846	3.234321	0.305293
-228.227856	-1.688034	0.310298
-231.744326	-4.964922	0.315302
-236.020172	4.189962	0.320307
-239.762293	-7.933138	0.325312
-243.069847	4.231909	0.330317
-246.962467	-9.023054	0.335322
-250.891443	3.028725	0.340326
-254.538940	3.673666	0.345331
-258.168168	-2.291571	0.350336
-262.275348	4.236427	0.355341
-265.530156	4.321821	0.360346
-269.569607	-0.173800	0.365350
-273.210766	0.429019	0.370355
-276.972926	-4.725954	0.375360
-281.287620	5.026117	0.380365
-284.601169	-1.938178	0.385370
-288.611999	-0.173857	0.390374
-292.185914	4.709517	0.395379
-296.109815	-3.906931	0.400384
-299.825643	7.541130	0.405389
-303.484989	-3.462108	0.410394
-307.134469	3.649743	0.415398
-310.796660	2.313440	0.420403
-314.212285	-3.907845	0.425408
-318.691233	2.536347	0.430413
-322.346653	3.949623	0.435418
-326.569766	6.834657	0.440422
-330.075696	-1.026143	0.445427
-333.298427	-2.012707	0.450432
-337.210950	3.785697	0.455437
-341.034695	-8.718406	0.460442
-344.925033	4.824343	0.465446
-348.759604	2.751114	0.470451
-352.157755	4.942858	0.475456
-356.116025	7.973923	0.480461
-359.806132	-5.740769	0.485466
-363.728598	3.737657	0.490470
-367.708264	7.943506	0.495475
-371.229886	-2.668454	0.500480
-374.997730	8.228886	0.505485
-378.719225	0.497073	0.510490
-382.413853	3.010467	0.515494
-386.360109	0.093201	0.520499
-389.983915	-10.465684	0.525504
-393.776430	2.320239	0.530509
-397.311482	-3.745104	0.535514
-401.477159	-1.637170	0.540518
-405.185793	-3.363294	0.545523
-408.619030	-5.753194	0.550528
-412.431130	-7.411433	0.555533
-416.478774	-6.830733	0.560538
-419.662115	-2.373848	0.565542
-423.664970	-12.185222	0.570547
-427.548623	0.482157	0.575552
-431.649618	-0.649303	0.580557
-435.175088	-6.931373	0.585562
-438.890123	0.241160	0.590566
-442.869366	-3.112863	0.595571
-446.570149	-7.052247	0.600576
-450.477466	3.916832	0.605581
-454.199203	-7.967204	0.610586
-457.821913	-6.482069	0.615590
-461.254422	-1.009846	0.620595
-464.947074	-1.322840	0.625600
-469.525929	-0.440972	0.630605
-472.691821	1.134739	0.635610
-476.598541	-0.988757	0.640614
-480.433120	-0.775714	0.645619
-483.806215	1.313546	0.650624
-487.809808	2.270016	0.655629
-491.244149	-0.701431	0.660634
-495.307914	-6.066548	0.665638
-499.319168	-3.951073	0.670643
-502.833258	-9.684022	0.675648
-506.583387	-1.397866	0.680653
-510.541567	-12.848937	0.685658
-513.985602	-1.708264	0.690662
-517.980287	-9.332681	0.695667
-521.455894	-7.941807	0.700672
-525.306030	-10.723867	0.705677
-529.060568	-3.305691	0.710682
-533.111892	4.841127	0.715686
-537.217411	-3.762081	0.720691
-540.263708	-5.808952	0.725696
-544.402648	6.468139	0.730701
-548.215222	-2.929742	0.735706
-551.693878	1.469753	0.740710
-555.521856	1.609496	0.745715
-558.985704	3.600313	0.750720
-562.939793	10.808435	0.755725
-566.710111	-4.177858	0.760730
-570.624492	2.217065	0.765734
-574.734853	-6.284622	0.770739
-577.889920	-0.241413	0.775744
-581.918024	10.261031	0.780749
-585.361558	3.048910	0.785754
-589.396003	7.146329	0.790758
-593.177172	0.241211	0.795763
-596.607929	-2.034498	0.800768
-600.851327	6.501362	0.805773
-604.638489	2.363005	0.810778
-608.475412	2.876145	0.815782
-612.133149	-0.444473	0.820787
-615.589605	4.879219	0.825792
-619.551380	10.742751	0.830797
-623.061139	-1.582471	0.835802
-627.165719	0.976206	0.840806
-630.888505	7.133845	0.845811
-634.254668	3.277325	0.850816
-638.276958	4.139645	0.855821
-641.705667	-0.482920	0.860826
-645.540391	4.044847	0.865830
-649.654510	4.014317	0.870835
-653.582755	1.142756	0.875840
-657.485802	2.043443	0.880845
-660.628175	-5.286205	0.885850
-664.362302	-2.205320	0.890854
-668.264232	7.593879	0.895859
-672.542912	2.117798	0.900864
-675.949923	11.953643	0.905869
-679.607986	-5.875539	0.910874
-683.477797	3.343068	0.915878
-687.365108	2.515812	0.920883
-690.840448	-1.729658	0.925888
-694.971480	7.360907	0.930893
-698.381889	3.890558	0.935898
-701.967887	3.013579	0.940902
-705.775378	6.652577	0.945907
-709.693144	4.574211	0.950912
-713.844331	3.428344	0.955917
-717.510836	-0.353276	0.960922
-721.190563	-2.164214	0.965926
-724.681981	0.831651	0.970931
-728.282395	-3.192205	0.975936
-732.403451	2.708623	0.980941
-736.308489	-8.139147	0.985946
-739.967311	-2.717482	0.990950
-743.791271	-1.525183	0.995955
-746.859100	-14.714354	1.000960
-750.737925	1.901879	1.005965
-754.894111	-3.203587	1.010970
-758.554480	-1.520706	1.015974
-762.546545	-5.571253	1.020979
-766.019856	-15.307778	1.025984
-770.633463	-2.301328	1.030989
-773.626142	0.566347	1.035994
-777.032450	-6.047695	1.040998
-781.006592	-1.183675	1.046003
-785.036333	-8.249219	1.051008
-788.909505	0.502713	1.056013
-792.691141	0.176060	1.061018
-796.304526	-6.209412	1.066022
-800.250787	2.069980	1.071027
-803.396337	0.751989	1.076032
-807.674829	1.188737	1.081037
-811.601644	4.324526	1.086042
-815.036596	-6.498858	1.091046
-818.993299	-0.859041	1.096051
-822.721452	-6.578259	1.101056
-826.158860	0.377589	1.106061
-829.885064	5.021478	1.111066
-833.868550	-2.106034	1.116070
-837.845235	1.009129	1.121075
-841.185123	-6.693809	1.126080
-845.531231	-3.718503	1.131085
-849.036830	-1.758189	1.136090
-852.829308	3.338376	1.141094
-856.350223	-2.503615	1.146099
-859.903967	-3.119175	1.151104
-863.614702	-0.049244	1.156109
-867.564688	2.897165	1.161114
-871.618855	2.228575	1.166118
-875.471918	6.189725	1.171123
-878.820362	-3.660105	1.176128
-882.532961	7.972938	1.181133
-886.773028	3.948501	1.186138
-890.345880	1.078521	1.191142
-894.420752	2.027465	1.196147
-897.736439	-4.926873	1.201152
-901.620419	6.640478	1.206157
-905.445573	5.061095	1.211162
-909.048503	2.482851	1.216166
-912.892434	8.581777	1.221171
-916.304277	-7.630469	1.226176
-920.354853	-3.332637	1.231181
-924.327817	1.102258	1.236186
-927.901322	1.083786	1.241190
-931.974239	7.478596	1.246195
-935.239452	-9.492956	1.251200
-939.068822	6.687064	1.256205
-942.624214	-1.495860	1.261210
-946.795456	-0.739123	1.266214
-950.658059	8.212428	1.271219
-954.157573	-5.244677	1.276224
-958.205830	-2.742335	1.281229
-961.823395	1.707365	1.286234
-965.059722	1.436054	1.291238
-968.978553	6.389814	1.296243
-972.886791	3.716419	1.301248
-977.012540	8.053655	1.306253
-981.105180	-1.623327	1.311258
-984.735453	3.726531	1.316262
-988.469283	-0.488912	1.321267
-991.545427	-0.912036	1.326272
-995.198730	9.100903	1.331277
-999.309579	4.126837	1.336282
-1002.884477	1.026007	1.341286
-1007.069073	1.386047	1.346291
-1010.701509	1.002790	1.351296
-1014.772696	0.532638	1.356301
-1018.237129	2.224330	1.361306
-1021.729058	-7.814667	1.366310
-1025.889064	2.186214	1.371315
-1029.495643	-6.494247	1.376320
-1033.226552	1.682841	1.381325
-1036.944344	-4.472134	1.386330
-1041.191015	1.768669	1.391334
-1044.982289	4.371432	1.396339
-1047.968861	-10.131204	1.401344
-1051.600332	-6.791328	1.406349
-1055.769694	-1.217420	1.411354
-1059.438246	-2.248068	1.416358
-1063.640637	5.277029	1.421363
-1066.938085	2.893163	1.426368
-1071.340481	1.425279	1.431373
-1074.509901	-2.096791	1.436378
-1078.291278	-0.594956	1.441382
-1082.093533	5.294864	1.446387
-1085.386890	-0.499556	1.451392
-1089.487593	6.435780	1.456397
-1093.251785	-3.891509	1.461402
-1097.653340	-5.249386	1.466406
-1101.075878	2.766263	1.471411
-1104.764816	-3.725946	1.476416
-1108.664586	10.787999	1.481421
-1112.514539	6.298551	1.486426
-1115.979360	3.095241	1.491430
-1119.804831	-2.262412	1.496435
-1123.165680	-2.676814	1.501440
-1127.478626	7.729733	1.506445
-1131.133561	0.900155	1.511450
-1134.725133	-5.701105	1.516454
-1138.746257	7.588006	1.521459
-1142.114159	0.307735	1.526464
-1145.791093	3.436434	1.531469
-1150.002357	2.601681	1.536474
-1153.816948	12.507842	1.541478
-1157.420461	8.523181	1.546483
-1161.015576	6.254054	1.551488
-1164.765140	11.249571	1.556493
-1168.532487	1.318786	1.561498
-1172.006846	1.949361	1.566502
-1176.204715	7.928511	1.571507
-1180.084151	1.195158	1.576512
-1183.801963	0.418585	1.581517
-1187.426026	1.208686	1.586522
-1191.064265	0.058088	1.591526
-1195.147390	5.346550	1.596531
-1198.878658	-0.292842	1.601536
-1202.676520	7.616429	1.606541
-1206.471150	0.265034	1.611546
-1209.368235	3.184868	1.616550
-1213.565020	6.742346	1.621555
-1217.052292	8.662312	1.626560
-1221.167648	6.194445	1.631565
-1225.153723	2.978121	1.636570
-1228.910672	-1.197999	1.641574
-1232.740146	11.134271	1.646579
-1236.524006	-3.846235	1.651584
-1240.197564	3.416109	1.656589
-1244.107835	15.171393	1.661594
-1247.733349	12.548379	1.666598
-1251.874881	9.249050	1.671603
-1255.151645	2.561861	1.676608
-1258.876162	1.487715	1.681613
-1262.605871	9.046673	1.686618
-1266.436187	5.086459	1.691622
-1270.466015	8.147592	1.696627
-1273.647426	0.003763	1.701632
-1277.657621	8.881068	1.706637
-1281.250257	3.358458	1.711642
-1285.189908	1.020335	1.716646
-1289.042860	15.943978	1.721651
-1292.506952	6.799584	1.726656
-1296.529258	14.699330	1.731661
-1300.058308	7.250703	1.736666
-1303.554061	2.242747	1.741670
-1308.058987	2.339179	1.746675
-1311.551187	5.878753	1.751680
-1315.495598	10.589335	1.756685
-1319.431358	2.654839	1.761690
-1323.168864	6.954919	1.766694
-1326.903889	12.710646	1.771699
-1330.066804	4.596446	1.776704
-1333.699750	8.180737	1.781709
-1337.817750	6.225375	1.786714
-1341.947682	5.661428	1.791718
-1345.708837	15.108601	1.796723
-1349.281507	6.080403	1.801728
-1353.016801	8.701842	1.806733
-1356.831598	13.049173	1.811738
-1360.348445	20.237337	1.816742
-1364.369412	15.928676	1.821747
-1368.100557	8.019865	1.826752
-1371.722048	10.151680	1.831757
-1375.353240	2.635808	1.836762
-1378.949003	-1.875333	1.841766
-1383.107534	12.604725	1.846771
-1386.778830	4.911030	1.851776
-1390.510531	13.876769	1.856781
-1394.437566	4.688451	1.861786
-1397.982243	4.754232	1.866790
-1401.784720	10.142295	1.871795
-1405.421747	6.766725	1.876800
-1409.532250	3.829700	1.881805
-1413.622110	4.719350	1.886810
-1416.673725	4.942403	1.891814
-1420.807861	4.569110	1.896819
-1424.141645	-0.158296	1.901824
-1427.938333	13.587855	1.906829
-1432.064020	11.965854	1.911834
-1435.377702	1.591513	1.916838
-1439.416822	2.825337	1.921843
-1442.984292	-0.472547	1.926848
-1446.668472	2.926838	1.931853
-1450.780654	10.152607	1.936858
-1454.446845	7.208373	1.941862
-1458.547323	9.704365	1.946867
-1461.810824	1.615453	1.951872
-1465.969123	6.883528	1.956877
-1469.858228	1.115995	1.961882
-1473.241437	7.383329	1.966886
-1477.033540	15.918631	1.971891
-1480.683517	6.777138	1.976896
-1484.445458	9.889152	1.981901
-1488.501679	6.178733	1.986906
-1491.980986	12.882953	1.991910
-1496.167854	21.012842	1.996915
-1499.837460	9.853561	2.006912
-1500.763104	10.323233	2.016909
-1498.229508	12.038703	2.026906
-1495.397154	12.321194	2.036902
-1493.367590	13.489342	2.046899
-1491.423183	9.226127	2.056896
-1489.434728	11.390156	2.066893
-1487.171189	4.746702	2.076890
-1485.777952	8.665757	2.086886
-1484.076704	0.937623	2.096883
-1482.050906	0.077811	2.106880
-1479.866032	5.619551	2.116877
-1477.856673	0.493113	2.126874
-1476.404405	9.217663	2.136870
-1474.388712	6.641613	2.146867
-1472.133181	6.724831	2.156864
-1470.335153	-1.143625	2.166861
-1468.804089	6.592013	2.176858
-1466.712179	7.613117	2.186854
-1464.879587	5.342802	2.196851
-1462.844760	6.748373	2.206848
-1461.015934	-6.603768	2.216845
-1459.060375	2.081750	2.226842
-1457.157901	1.551400	2.236838
-1455.426390	8.531351	2.246835
-1453.769582	5.965191	2.256832
-1451.357927	4.323382	2.266829
-1449.562503	4.246552	2.276826
-1447.991849	1.274295	2.286822
-1446.087998	1.400158	2.296819
-1444.228529	4.877122	2.306816
-1442.405756	0.057028	2.316813
-1440.675682	2.773311	2.326810
-1438.595536	2.132220	2.336806
-1436.282879	6.745818	2.346803
-1434.444856	0.584135	2.356800
-1432.906390	2.073803	2.366797
-1431.066835	7.961816	2.376794
-1429.068608	3.439610	2.386790
-1426.721694	5.340534	2.396787
-1425.032769	3.541108	2.406784
-1423.321602	5.603809	2.416781
-1421.993271	8.182418	2.426778
-1419.881114	10.615712	2.436774
-1417.441091	8.109861	2.446771
-1415.888436	11.566828	2.456768
-1414.063900	13.463830	2.466765
-1411.916992	10.163374	2.476762
-1410.070006	9.288468	2.486758
-1408.716571	6.762581	2.496755
-1406.746960	5.612888	2.506752
-1404.434962	0.143224	2.516749
-1402.804037	7.996505	2.526746
-1400.556088	11.849396	2.536742
-1399.173196	9.032714	2.546739
-1396.994092	8.787245	2.556736
-1394.930148	3.954196	2.566733
-1393.270699	3.411871	2.576730
-1391.529928	0.896522	2.586726
-1389.532859	4.911470	2.596723
-1387.934885	5.329399	2.606720
-1385.917867	4.639105	2.616717
-1383.923279	9.335037	2.626714
-1382.014485	6.927175	2.636710
-1379.947644	5.311043	2.646707
-1378.223944	7.559335	2.656704
-1376.351293	3.378843	2.666701
-1374.824153	13.635458	2.676698
-1372.864181	7.985592	2.686694
-1370.962601	10.976760	2.696691
-1368.578849	5.428392	2.706688
-1367.039871	6.132714	2.716685
-1365.026719	9.464757	2.726682
-1363.509914	6.585959	2.736678
-1361.282510	11.844608	2.746675
-1359.193665	5.926001	2.756672
-1357.666771	5.344806	2.766669
-1356.189989	8.795068	2.776666
-1353.649002	9.100434	2.786662
-1351.625008	2.619914	2.796659
-1350.304591	9.804507	2.806656
-1348.608295	9.496159	2.816653
-1345.962853	14.336810	2.826650
-1344.417577	6.778970	2.836646
-1342.726970	2.134561	2.846643
-1340.738414	6.272723	2.856640
-1338.751824	5.150576	2.866637
-1336.980143	8.560468	2.876634
-1335.203778	14.132941	2.886630
-1333.288009	8.388719	2.896627
-1331.067371	-0.935909	2.906624
-1329.151784	3.535307	2.916621
-1327.702739	10.891073	2.926618
-1325.949187	4.713507	2.936614
-1324.003424	16.389375	2.946611
-1321.736215	11.492593	2.956608
-1319.937981	1.687224	2.966605
-1318.252617	-1.630342	2.976602
-1316.731809	4.090366	2.986598
-1314.673865	3.204166	2.996595
-1312.214693	1.447172	3.006592
-1310.752515	2.503006	3.016589
-1308.896867	3.931921	3.026586
-1306.704304	7.088136	3.036582
-1305.149220	3.057067	3.046579
-1303.351359	-2.403678	3.056576
-1301.540786	2.509254	3.066573
-1299.457998	7.881699	3.076570
-1297.382496	7.781728	3.086566
-1295.756359	8.283778	3.096563
-1293.785957	6.415902	3.106560
-1291.661386	6.251781	3.116557
-1290.126181	5.498058	3.126554
-1288.146746	2.779720	3.136550
-1286.241666	9.927551	3.146547
-1284.473103	8.739329	3.156544
-1282.318595	7.017684	3.166541
-1280.758735	7.562344	3.176538
-1278.751025	6.429087	3.186534
-1276.872959	3.415553	3.196531
-1275.061615	-1.308848	3.206528
-1273.212635	7.654341	3.216525
-1271.383781	1.612856	3.226522
-1269.708597	10.976211	3.236518
-1267.349956	7.507459	3.246515
-1265.773169	6.500781	3.256512
-1264.106668	7.774871	3.266509
-1261.628331	6.472268	3.276506
-1259.574043	5.491082	3.286502
-1258.163748	3.403644	3.296499
-1256.132322	11.017087	3.306496
-1254.478557	10.083744	3.316493
-1252.638300	9.372493	3.326490
-1250.619002	14.133020	3.336486
-1249.070253	12.547436	3.346483
-1246.518455	3.458029	3.356480
-1244.887354	5.486341	3.366477
-1243.142859	7.688437	3.376474
-1241.171302	11.400373	3.386470
-1239.372970	15.525414	3.396467
-1237.410811	9.979562	3.406464
-1235.692733	2.968296	3.416461
-1233.739813	11.168291	3.426458
-1231.903100	8.855867	3.436454
-1229.790639	2.782685	3.446451
-1227.836487	7.630290	3.456448
-1226.432951	5.051194	3.466445
-1224.460443	6.034831	3.476442
-1222.449914	7.729248	3.486438
-1220.862292	4.338788	3.496435
-1218.698338	3.586981	3.506432
-1216.835396	5.422543	3.516429
-1214.900228	4.552338	3.526426
-1213.224904	5.028583	3.536422
-1211.313386	6.932872	3.546419
-1209.206875	8.047241	3.556416
-1207.285610	4.171870	3.566413
-1205.498483	10.549973	3.576410
-1203.567116	11.184205	3.586406
-1201.763162	7.736840	3.596403
-1200.073053	8.311331	3.606400
-1198.406238	5.663318	3.616397
-1195.911935	3.019826	3.626394
-1194.152758	6.065570	3.636390
-1192.552290	4.969486	3.646387
-1190.408535	2.259333	3.656384
-1188.579659	2.681950	3.666381
-1187.091210	9.250862	3.676378
-1184.929571	9.496192	3.686374
-1183.007999	9.409669	3.696371
-1181.139237	-0.143369	3.706368
-1179.392923	7.659377	3.716365
-1177.347250	11.100148	3.726362
-1175.692887	-3.549864	3.736358
-1173.608615	4.873820	3.746355
-1171.702324	3.929947	3.756352
-1169.884315	7.433529	3.766349
-1168.637103	6.386655	3.776346
-1166.059851	6.183988	3.786342
-1164.119066	9.181962	3.796339
-1162.363015	10.790478	3.806336
-1160.633937	9.011132	3.816333
-1158.688299	12.398745	3.826330
-1156.752576	7.905962	3.836326
-1155.001413	3.020812	3.846323
-1152.795943	7.911456	3.856320
-1151.029078	1.603221	3.866317
-1149.383511	5.777062	3.876314
-1147.661241	5.916061	3.886310
-1145.579062	7.218414	3.896307
-1143.609039	-0.578290	3.906304
-1141.872954	4.211162	3.916301
-1139.676415	6.969996	3.926298
-1137.960103	3.862569	3.936294
-1136.158813	7.772549	3.946291
-1134.468757	8.814216	3.956288
-1132.328326	-1.093720	3.966285
-1130.392514	7.813139	3.976282
-1128.814927	6.636037	3.986278
-1126.672174	6.067342	3.996275
-1124.786554	3.170347	4.006272
-1123.222324	-2.225317	4.016269
-1121.101438	9.415853	4.026266
-1119.437343	8.279230	4.036262
-1117.498626	2.497165	4.046259
-1115.210387	6.396655	4.056256
-1113.574385	4.572447	4.066253
-1111.662679	8.270616	4.076250
-1109.820468	9.895978	4.086246
-1108.178835	6.633816	4.096243
-1105.991680	7.718977	4.106240
-1104.270470	2.504639	4.116237
-1102.114844	1.719937	4.126234
-1100.310997	13.826186	4.136230
-1098.658916	1.251045	4.146227
-1096.946659	-0.800849	4.156224
-1094.798492	4.443500	4.166221
-1092.886539	6.822419	4.176218
-1091.036908	2.304530	4.186214
-1089.132792	1.325498	4.196211
-1087.640870	5.277159	4.206208
-1085.624067	2.554865	4.216205
-1083.736569	-2.156851	4.226202
-1081.695354	0.599832	4.236198
-1079.741537	5.125472	4.246195
-1077.960701	7.206790	4.256192
-1076.251586	7.690726	4.266189
-1074.137833	0.776774	4.276186
-1072.558095	-0.610929	4.286182
-1070.654882	3.289090	4.296179
-1068.112032	-2.075003	4.306176
-1066.833356	2.017219	4.316173
-1065.246259	7.437754	4.326170
-1062.684024	7.259465	4.336166
-1060.784649	3.439685	4.346163
-1059.190174	2.550190	4.356160
-1057.481628	4.829678	4.366157
-1055.428083	1.831555	4.376154
-1053.597331	10.294889	4.386150
-1051.781509	5.385236	4.396147
-1049.647290	2.687063	4.406144
-1047.737378	0.027404	4.416141
-1046.195706	1.539986	4.426138
-1044.210764	5.457603	4.436134
-1042.429402	8.277892	4.446131
-1040.160104	6.110618	4.456128
-1038.639863	-0.927477	4.466125
-1036.745941	-0.848336	4.476122
-1034.645337	0.172285	4.486118
-1032.842158	-1.528439	4.496115
-1031.136597	0.585188	4.506112
-1029.232839	-0.397709	4.516109
-1027.236748	-1.586160	4.526106
-1025.781402	7.934017	4.536102
-1023.532326	4.864398	4.546099
-1021.293021	0.702906	4.556096
-1020.028879	-3.562671	4.566093
-1018.399827	2.429269	4.576090
-1015.861913	6.719103	4.586086
-1014.230826	3.950823	4.596083
-1012.098079	-1.840008	4.606080
-1010.010549	1.286978	4.616077
-1008.563911	2.228605	4.626074
-1006.849818	6.464648	4.636070
-1004.927026	7.680615	4.646067
-1003.087511	3.717398	4.656064
-1001.093205	2.205587	4.666061
-999.039246	4.106863	4.676058
-997.412112	3.752433	4.686054
-995.426453	3.326175	4.696051
-993.732498	-0.308919	4.706048
-991.624762	3.491606	4.716045
-989.622805	9.093490	4.726042
-987.868585	5.134647	4.736038
-986.098589	10.471649	4.746035
-984.016361	4.269391	4.756032
-982.266846	7.210576	4.766029
-980.339019	11.757330	4.776026
-978.593689	5.469450	4.786022
-976.721602	11.285711	4.796019
-974.367951	-1.219743	4.806016
-972.563763	1.331075	4.816013
-971.118383	4.355304	4.826010
-969.617715	2.097122	4.836006
-967.550506	3.334158	4.846003
-965.449116	5.773096	4.856000
-963.436423	6.753910	4.865997
-961.552192	1.449192	4.875994
-959.693563	6.258398	4.885990
-957.703795	6.352738	4.895987
-955.772898	0.940023	4.905984
-954.397279	4.614897	4.915981
-951.935187	5.650174	4.925978
-950.231265	4.813857	4.935974
-948.230569	2.878096	4.945971
-946.915343	0.533588	4.955968
-944.849230	-1.561211	4.965965
-942.599538	1.525720	4.975962
-940.930656	1.605596	4.985958
-939.458558	9.230265	4.995955
-937.277460	6.931166	5.005952
-935.241332	1.636741	5.015949
-933.475911	6.144606	5.025946
-931.784180	9.071626	5.035942
-929.804474	8.009338	5.045939
-927.811449	2.117246	5.055936
-925.439331	11.176568	5.065933
-924.469049	7.853847	5.075930
-922.396700	6.304566	5.085926
-920.078699	9.095628	5.095923
-918.255679	0.919939	5.105920
-916.688744	4.276642	5.115917
-915.157751	3.720194	5.125914
-912.597163	2.862117	5.135910
-910.824051	5.017158	5.145907
-909.306518	5.472791	5.155904
-907.420114	0.039672	5.165901
-905.245299	2.152632	5.175898
-903.365686	1.973054	5.185894
-901.443733	5.324941	5.195891
-899.628049	2.511971	5.205888
-898.027788	0.953237	5.215885
-895.812931	4.492369	5.225882
-893.774429	5.944227	5.235878
-892.453384	5.967639	5.245875
-890.407559	2.450420	5.255872
-888.450271	4.828373	5.265869
-886.407956	3.511906	5.275866
-884.806507	8.006443	5.285862
-883.170484	0.988037	5.295859
-880.748548	2.235758	5.305856
-878.796751	7.360990	5.315853
-877.038437	3.122860	5.325850
-875.391105	5.256429	5.335846
-873.545179	3.330668	5.345843
-871.424845	0.255953	5.355840
-869.889398	4.754711	5.365837
-867.750284	4.574868	5.375834
-865.785707	6.207790	5.385830
-864.054320	4.994898	5.395827
-862.524731	-5.146381	5.405824
-860.450571	0.668842	5.415821
-858.307101	8.436378	5.425818
-856.273328	4.344627	5.435814
-854.617231	-3.297699	5.445811
-853.133817	-1.759236	5.455808
-850.991112	-3.224128	5.465805
-849.000224	-0.616774	5.475802
-847.232390	3.222411	5.485798
-845.139965	0.167121	5.495795
-843.477915	2.505663	5.505792
-841.196103	6.254258	5.515789
-839.861846	7.641273	5.525786
-837.663427	10.446189	5.535782
-836.304780	10.676184	5.545779
-833.978620	4.840373	5.555776
-831.856330	-0.753351	5.565773
-830.354438	3.743674	5.575770
-828.524614	2.389011	5.585766
-826.905306	4.295025	5.595763
-824.307537	-2.313800	5.605760
-822.450301	4.383247	5.615757
-820.771730	0.870209	5.625754
-819.113800	2.797261	5.635750
-817.080876	12.210098	5.645747
-815.845496	7.582352	5.655744
-813.152294	7.016951	5.665741
-811.620298	3.192746	5.675738
-809.598286	9.482511	5.685734
-807.752877	4.336671	5.695731
-806.082417	5.354169	5.705728
-803.895281	1.664924	5.715725
-802.099287	9.222203	5.725722
-800.252230	4.260252	5.735718
-798.633568	7.560699	5.745715
-796.210205	1.804260	5.755712
-794.359706	7.689922	5.765709
-792.580011	5.614710	5.775706
-790.841893	3.977417	5.785702
-789.297574	0.313143	5.795699
-787.018531	2.675440	5.805696
-785.244852	4.724126	5.815693
-783.785899	5.622221	5.825690
-781.503957	1.472495	5.835686
-779.302535	12.390256	5.845683
-777.776466	9.394655	5.855680
-776.131581	13.213083	5.865677
-773.997408	14.678617	5.875674
-772.138729	9.822969	5.885670
-770.311727	6.047738	5.895667
-767.921952	8.371282	5.905664
-765.981430	10.232466	5.915661
-764.479452	11.666206	5.925658
-762.942494	1.639876	5.935654
-761.139717	5.020188	5.945651
-758.676521	7.762314	5.955648
-756.934117	-2.389777	5.965645
-755.381950	7.760076	5.975642
-753.677529	6.663700	5.985638
-751.309266	11.919080	5.995635
-749.558311	6.174915	6.005632
-748.030144	-0.545919	6.015629
-745.691023	6.187028	6.025626
-743.781651	3.252913	6.035622
-742.097464	2.968224	6.045619
-740.198270	1.783096	6.055616
-738.286917	2.970322	6.065613
-736.462707	-1.126119	6.075610
-734.631939	3.398681	6.085606
-732.931420	4.382594	6.095603
-730.662703	3.432833	6.105600
-728.775336	6.309369	6.115597
-727.446459	13.377351	6.125594
-725.197045	7.927844	6.135590
-723.434472	7.353851	6.145587
-721.212310	4.942285	6.155584
-719.316308	7.036007	6.165581
-717.721817	5.662100	6.175578
-716.215699	7.869370	6.185574
-714.095682	6.068158	6.195571
-711.690232	0.874852	6.205568
-709.971475	6.205758	6.215565
-708.478309	0.350530	6.225562
-706.604788	8.291345	6.235558
-704.444505	1.573491	6.245555
-702.701006	2.755156	6.255552
-700.912266	3.788757	6.265549
-698.810382	3.556104	6.275546
-697.055190	6.598800	6.285542
-694.983318	7.183464	6.295539
-693.218902	3.979812	6.305536
-691.541842	4.081303	6.315533
-689.497963	1.492071	6.325530
-687.718254	2.363214	6.335526
-685.822124	0.365680	6.345523
-683.778127	1.856218	6.355520
-681.990898	0.052454	6.365517
-680.206539	4.543352	6.375514
-678.460913	-3.824484	6.385510
-676.391071	4.976232	6.395507
-674.500869	7.999722	6.405504
-672.758034	2.991283	6.415501
-670.667394	1.796648	6.425498
-668.851934	-1.667900	6.435494
-667.037372	-1.184506	6.445491
-665.202011	3.603541	6.455488
-663.126549	-5.129553	6.465485
-661.443016	-1.914880	6.475482
-659.574208	-3.291576	6.485478
-657.386074	0.799643	6.495475
-655.587448	-0.269784	6.505472
-654.160554	-7.245513	6.515469
-652.161669	0.223666	6.525466
-650.134417	2.781008	6.535462
-648.475085	4.190159	6.545459
-646.211993	-0.246749	6.555456
-644.247246	2.203154	6.565453
-642.505968	4.823802	6.575450
-641.366539	2.427341	6.585446
-638.992047	-0.622905	6.595443
-636.495623	-0.117786	6.605440
-635.222007	-1.534220	6.615437
-633.274033	1.275049	6.625434
-631.479974	5.599501	6.635430
-629.434605	-7.408580	6.645427
-627.512946	-0.104377	6.655424
-625.494629	-1.139167	6.665421
-623.664338	-6.517889	6.675418
-622.495096	0.766432	6.685414
-620.172127	-0.209181	6.695411
-617.728947	3.399213	6.705408
-616.685271	2.176374	6.715405
-614.907664	2.607639	6.725402
-612.617135	-1.160912	6.735398
-610.553343	-4.335675	6.745395
-608.860405	-4.663311	6.755392
-606.994943	-1.043122	6.765389
-605.207978	1.988234	6.775386
-603.212041	2.982765	6.785382
-601.125926	6.758357	6.795379
-599.555258	1.621796	6.805376
-597.640851	-3.543709	6.815373
-595.789905	3.718106	6.825370
-593.921332	4.444805	6.835366
-591.930713	2.510138	6.845363
-589.890147	0.701276	6.855360
-588.388338	-4.806426	6.865357
-586.271659	2.173458	6.875354
-584.499264	-0.520116	6.885350
-582.693392	-5.312089	6.895347
-580.879776	3.770169	6.905344
-578.788137	3.751561	6.915341
-576.592700	-0.348050	6.925338
-575.022499	1.004494	6.935334
-573.372639	7.338084	6.945331
-571.329420	4.729652	6.955328
-569.420226	-0.365391	6.965325
-567.702959	1.759462	6.975322
-565.925052	7.318203	6.985318
-563.878093	0.457420	6.995315
-561.692061	0.988966	7.005312
-560.072184	-5.884690	7.015309
-558.167662	7.483096	7.025306
-556.387470	0.457835	7.035302
-554.273204	1.471607	7.045299
-552.183305	-3.083350	7.055296
-550.951133	1.062477	7.065293
-549.118724	5.852667	7.075290
-546.940647	-5.256232	7.085286
-544.804703	3.384220	7.095283
-542.991358	0.065126	7.105280
-541.502934	1.718639	7.115277
-539.751317	4.996379	7.125274
-537.612151	5.056583	7.135270
-535.670575	-1.513014	7.145267
-533.793280	4.277277	7.155264
-531.832763	3.615253	7.165261
-529.907651	10.577058	7.175258
-528.120807	10.235317	7.185254
-526.447846	5.611208	7.195251
-524.440814	1.443167	7.205248
-522.549913	-1.357268	7.215245
-520.576718	6.154727	7.225242
-518.715457	1.631502	7.235238
-516.612944	1.658879	7.245235
-515.352698	1.083812	7.255232
-513.393629	3.579410	7.265229
-511.212937	8.075896	7.275226
-509.248624	0.140104	7.285222
-507.622738	-2.603395	7.295219
-505.624888	-0.517961	7.305216
-503.756433	3.501326	7.315213
-501.910430	4.465509	7.325210
-500.105776	7.655124	7.335206
-498.013725	2.454039	7.345203
-496.206652	2.361381	7.355200
-494.452383	0.413558	7.365197
-492.474309	1.991380	7.375194
-490.658703	3.135072	7.385190
-488.791854	1.521257	7.395187
-486.798801	-0.622849	7.405184
-485.192180	0.878403	7.415181
-483.224803	2.512604	7.425178
-481.166867	-1.228626	7.435174
-479.133698	-8.354962	7.445171
-477.382929	0.069032	7.455168
-475.533171	-2.621570	7.465165
-473.687715	1.558576	7.475162
-471.948545	6.846565	7.485158
-470.020784	3.153756	7.495155
-468.362385	0.029634	7.505152
-466.196828	-0.774641	7.515149
-463.985532	-1.732201	7.525146
-462.683424	0.127593	7.535142
-460.872134	-7.383154	7.545139
-458.768537	-0.229433	7.555136
-456.784067	-3.230855	7.565133
-454.831138	-0.642091	7.575130
-453.139533	1.819193	7.585126
-451.218636	-0.109380	7.595123
-449.588426	-0.880295	7.605120
-447.445893	-2.591976	7.615117
-445.470967	-1.172074	7.625114
-443.643804	7.863274	7.635110
-441.844577	-1.539664	7.645107
-440.003818	0.075177	7.655104
-438.128726	-6.143488	7.665101
-436.025576	-2.042708	7.675098
-434.475329	0.806036	7.685094
-432.660135	-9.922416	7.695091
-430.376852	-8.247931	7.705088
-428.731080	-2.854190	7.715085
-426.989000	3.045901	7.725082
-424.950224	-5.510077	7.735078
-423.136151	0.653129	7.745075
-421.132586	-5.046916	7.755072
-419.257751	-5.439674	7.765069
-417.553332	-0.412471	7.775066
-415.771882	-3.906264	7.785062
-413.432241	-0.867671	7.795059
-411.920604	1.588538	7.805056
-409.784442	0.968365	7.815053
-408.071866	0.500691	7.825050
-406.460904	0.398634	7.835046
-404.191986	6.130107	7.845043
-402.372334	2.898115	7.855040
-400.618122	0.908839	7.865037
-398.492967	6.300984	7.875034
-396.968416	0.594196	7.885030
-394.661703	-2.735572	7.895027
-393.121974	0.939014	7.905024
-391.136080	-1.455575	7.915021
-389.165339	-1.342694	7.925018
-387.311541	1.068266	7.935014
-385.560867	-0.606201	7.945011
-383.933890	-2.083578	7.955008
-381.872540	-7.091223	7.965005
-379.762443	-1.416281	7.975002
-377.973146	-0.352210	7.984998
-375.989621	1.910428	7.994995
-374.731010	-3.245648	8.004992
-372.458386	-7.766267	8.014989
-370.347259	0.207467	8.024986
-368.853339	-4.323431	8.034982
-366.514844	-2.410582	8.044979
-364.761862	-0.852976	8.054976
-362.982135	0.543142	8.064973
-361.227577	-0.392535	8.074970
-359.429161	-0.204236	8.084966
-357.267094	-4.978978	8.094963
-355.395863	-7.805613	8.104960
-353.740934	-5.736374	8.114957
-351.986898	1.784846	8.124954
-349.951810	-2.064256	8.134950
-348.193223	-3.618340	8.144947
-345.914872	-4.114668	8.154944
-344.271283	-15.300559	8.164941
-342.920152	-5.642859	8.174938
-340.730562	-1.533540	8.184934
-338.490849	-4.488191	8.194931
-336.370541	-6.263194	8.204928
-334.761264	-7.585754	8.214925
-333.004245	-6.526799	8.224922
-331.048257	-9.614577	8.234918
-329.637429	-6.997189	8.244915
-327.286448	-7.975876	8.254912
-325.299712	-10.002241	8.264909
-323.668049	-4.418703	8.274906
-321.899942	-0.293197	8.284902
-319.832428	-6.939250	8.294899
-317.907085	-12.839251	8.304896
-316.452846	-9.066188	8.314893
-313.976623	-12.841548	8.324890
-312.256137	-11.183101	8.334886
-310.879596	-7.455201	8.344883
-308.477500	-7.992101	8.354880
-306.940358	-1.295226	8.364877
-304.704455	-9.332460	8.374874
-303.050735	-1.483768	8.384870
-301.119876	-4.085457	8.394867
-299.008859	1.077568	8.404864
-297.306514	1.309246	8.414861
-296.026153	-4.856365	8.424858
-293.602760	5.569913	8.434854
-291.827579	-0.871066	8.444851
-289.839450	-4.702602	8.454848
-287.951301	-4.496862	8.464845
-286.019339	0.136072	8.474842
-284.236572	-0.543968	8.484838
-282.372012	1.707106	8.494835
-280.369353	-2.514625	8.504832
-278.241881	0.045469	8.514829
-276.695152	-1.282153	8.524826
-275.120026	-1.894167	8.534822
-273.359331	-2.430511	8.544819
-271.109694	-3.066129	8.554816
-269.077157	0.973339	8.564813
-267.281213	3.499403	8.574810
-265.661672	3.948831	8.584807
-263.597727	5.503731	8.594803
-261.487408	-0.223259	8.604800
-259.770885	-3.129636	8.614797
-258.014456	-1.126380	8.624794
-256.327321	4.031514	8.634791
-254.187118	6.977144	8.644787
-252.283969	3.792145	8.654784
-250.373618	0.937498	8.664781
-248.591511	3.584508	8.674778
-246.707578	3.820235	8.684775
-244.874566	1.314392	8.694771
-242.678886	-1.733442	8.704768
-240.884084	0.861200	8.714765
-239.168457	0.107722	8.724762
-237.305641	2.382038	8.734759
-235.582932	-3.440500	8.744755
-233.568378	-4.510434	8.754752
-231.769737	-4.062861	8.764749
-229.700977	-4.538202	8.774746
-227.826030	-1.583031	8.784743
-226.082276	-9.672965	8.794739
-224.220412	-6.059493	8.804736
-222.258613	-13.341060	8.814733
-220.236370	-7.720921	8.824730
-218.417633	-3.066165	8.834727
-216.604097	-1.397553	8.844723
-214.889450	-10.389907	8.854720
-213.132670	-9.340743	8.864717
-211.194506	-7.052860	8.874714
-209.020866	-8.413281	8.884711
-207.317120	-12.310227	8.894707
-205.617823	-10.721219	8.904704
-203.599245	-8.702038	8.914701
-201.457848	-9.129355	8.924698
-199.839782	-5.017981	8.934695
-198.151513	-2.791176	8.944691
-196.006510	1.516758	8.954688
-193.993814	-7.888724	8.964685
-192.117049	-1.488757	8.974682
-190.592996	-3.649132	8.984679
-188.846674	-9.608890	8.994675
-186.535432	-4.160811	9.004672
-184.944065	-0.723436	9.014669
-182.947352	0.184603	9.024666
-181.072268	-1.581078	9.034663
-179.114951	-2.444355	9.044659
-177.340585	-7.294017	9.054656
-175.488848	-9.004708	9.064653
-173.703331	-6.496183	9.074650
-171.452949	-8.677568	9.084647
-169.605957	-3.262499	9.094643
-167.941332	2.390150	9.104640
-165.984322	-1.145912	9.114637
-164.173891	-4.185739	9.124634
-162.403988	-4.603474	9.134631
-160.598050	-3.823166	9.144627
-158.587619	0.125691	9.154624
-156.750124	-1.333170	9.164621
-154.767000	-1.774820	9.174618
-152.864707	4.580479	9.184615
-151.060226	0.508582	9.194611
-149.139836	-8.311549	9.204608
-147.240450	-2.424477	9.214605
-145.402339	-4.474286	9.224602
-143.423740	-0.585173	9.234599
-141.696242	1.707253	9.244595
-139.840045	-1.369265	9.254592
-137.726435	-0.960649	9.264589
-136.119916	4.569187	9.274586
-133.812660	0.786927	9.284583
-132.329017	4.699271	9.294579
-130.490664	-0.198895	9.304576
-128.611470	3.255541	9.314573
-126.514804	0.374526	9.324570
-124.872491	4.404312	9.334567
-123.078404	8.191100	9.344563
-120.865143	3.310455	9.354560
-119.038938	-1.590366	9.364557
-117.299230	4.053383	9.374554
-115.242544	6.494091	9.384551
-113.444452	0.197447	9.394547
-111.648495	1.492082	9.404544
-109.780357	5.500935	9.414541
-107.959673	2.090237	9.424538
-106.099626	7.358057	9.434535
-104.135325	2.979352	9.444531
-102.167528	-0.731245	9.454528
-100.545793	-3.804692	9.464525
-98.411496	0.298430	9.474522
-96.594340	3.538641	9.484519
-94.691181	9.240135	9.494515
-92.895621	-1.551651	9.504512
-90.681696	6.454808	9.514509
-89.089608	3.736608	9.524506
-87.591487	6.178260	9.534503
-85.442497	7.022686	9.544499
-83.440927	3.127271	9.554496
-81.501172	4.905904	9.564493
-79.607575	9.155044	9.574490
-77.910128	8.891649	9.584487
-76.016383	3.356795	9.594483
-74.274372	0.560724	9.604480
-72.202972	2.331805	9.614477
-70.269062	1.293949	9.624474
-68.815530	9.010694	9.634471
-66.441800	6.732325	9.644467
-64.493293	0.352203	9.654464
-62.802360	-0.238889	9.664461
-60.926606	0.570986	9.674458
-58.951624	6.604018	9.684455
-57.220248	4.469392	9.694451
-55.352341	2.026800	9.704448
-53.340734	-1.313068	9.714445
-51.533365	-0.161853	9.724442
-49.966173	-0.532138	9.734439
-47.922640	1.570971	9.744435
-46.077575	4.063017	9.754432
-44.050284	-3.632447	9.764429
-42.070267	-0.926015	9.774426
-40.414021	-1.387054	9.784423
-38.443898	-4.634436	9.794419
-36.495246	3.677590	9.804416
-34.633620	11.894674	9.814413
-32.953777	7.059288	9.824410
-30.854747	7.974356	9.834407
-28.842830	2.993505	9.844403
-27.217282	3.848667	9.854400
-25.428811	3.896528	9.864397
-23.323594	2.953812	9.874394
-21.545439	-4.883097	9.884391
-19.770957	-1.193290	9.894387
-17.731505	2.822985	9.904384
-15.877438	3.874518	9.914381
-14.112951	-4.148563	9.924378
-12.390336	1.577205	9.934375
-10.265963	-4.250501	9.944371
-8.208157	1.479055	9.954368
-6.891870	0.921789	9.964365
-4.483697	4.529826	9.974362
-3.518682	17.512442	9.984359
-1.958279	54.074806	9.994355
-0.690271	107.492493	10.004352
0.000000	147.315614	10.009357
0.646514	185.375304	10.014362
1.329791	214.837779	10.019367
2.186474	232.600375	10.024371
2.540519	261.883349	10.029376
2.716502	275.157931	10.034381
3.076929	288.043286	10.039386
3.200111	310.032070	10.044391
3.225943	311.308114	10.049395
3.461151	325.845159	10.054400
3.470865	318.381334	10.059405
3.649625	326.329541	10.064410
3.390873	324.967132	10.069415
3.958702	341.290105	10.074419
3.793982	342.759079	10.079424
3.980663	352.962949	10.084429
4.500038	358.117363	10.089434
3.576876	358.648267	10.094439
4.190304	355.546382	10.099443
4.107910	366.206904	10.104448
4.341173	362.544962	10.109453
4.493477	368.925952	10.114458
4.357339	364.254496	10.119463
4.013960	358.467177	10.124467
4.236833	369.427057	10.129472
4.427526	380.602059	10.134477
4.389402	388.107109	10.139482
4.350632	389.382789	10.144487
4.643529	384.119498	10.149491
4.567970	390.992310	10.154496
4.585027	394.029531	10.159501
4.127408	391.998215	10.164506
4.276211	398.237718	10.169511
4.159029	399.768412	10.174515
3.928430	407.655801	10.179520
4.668641	426.010147	10.184525
4.615506	425.020222	10.189530
4.460832	428.246756	10.194535
4.597013	434.225553	10.199539
4.775850	439.015635	10.204544
4.990688	440.683609	10.209549
5.177918	438.523565	10.214554
4.944566	444.331655	10.219559
5.125399	446.258082	10.224563
5.174494	464.193753	10.229568
5.308554	470.183980	10.234573
5.402851	468.974175	10.239578
5.266924	470.871630	10.244583
5.739969	469.650963	10.249587
5.567179	475.814194	10.254592
5.227978	465.454042	10.259597
5.614770	464.674070	10.264602
5.706822	477.921376	10.269607
5.850511	474.929612	10.274611
5.224486	471.246824	10.279616
5.330510	479.665459	10.284621
5.544047	486.669924	10.289626
5.519991	491.603359	10.294631
5.727834	485.767663	10.299635
5.342033	492.025052	10.304640
5.771424	487.259359	10.309645
5.856258	481.964606	10.314650
5.789347	496.399668	10.319655
6.299127	507.929775	10.324659
6.382727	519.726376	10.329664
6.305922	507.978750	10.334669
6.521234	503.323965	10.339674
6.213959	505.146596	10.344679
6.349650	494.567638	10.349683
6.304814	501.188529	10.354688
6.172068	502.428622	10.359693
6.523019	499.886037	10.364698
6.244823	505.549474	10.369703
6.558558	491.947590	10.374707
6.389285	508.962760	10.379712
6.531953	524.339645	10.384717
6.515235	528.727903	10.389722
6.360600	533.336383	10.394727
6.411857	539.506222	10.399731
6.592100	542.809168	10.404736
6.438949	539.400143	10.409741
6.470885	543.124821	10.414746
6.317840	546.925424	10.419751
6.965344	554.686803	10.424755
6.736664	571.036062	10.429760
6.860998	584.714095	10.434765
6.845156	583.771054	10.439770
6.894621	584.646763	10.444775
7.294286	584.554560	10.449779
7.028135	585.422806	10.454784
7.175788	585.078162	10.459789
7.397647	579.316211	10.464794
7.137971	585.113866	10.469799
7.367366	581.231491	10.474803
7.169047	583.778718	10.479808
7.361794	593.609874	10.484813
7.786562	580.796879	10.489818
7.412281	588.335584	10.494823
7.525972	587.061263	10.499827
7.770664	596.369581	10.504832
7.624023	593.509677	10.509837
7.965678	598.647671	10.514842
7.718868	598.405791	10.519847
7.979396	589.007700	10.524851
7.698422	599.357439	10.529856
7.577797	592.804753	10.534861
7.796775	609.512286	10.539866
8.380616	615.215851	10.544871
8.322633	605.228168	10.549875
7.986146	601.481100	10.554880
7.790920	601.583260	10.559885
8.061194	604.493424	10.564890
8.149606	622.776211	10.569895
8.466681	619.660351	10.574899
8.367373	624.063586	10.579904
8.456392	618.998590	10.584909
8.584220	627.546985	10.589914
8.320939	621.340054	10.594919
8.301585	624.595926	10.599923
8.546689	628.636171	10.604928
8.522187	632.642513	10.609933
8.766186	633.070803	10.614938
8.451927	635.374634	10.619943
8.829627	627.234557	10.624947
8.714076	631.736892	10.629952
8.817441	634.093852	10.634957
8.711774	621.858864	10.639962
8.817992	633.830090	10.644967
8.782974	627.497575	10.649971
9.076852	632.935081	10.654976
8.990266	635.844465	10.659981
9.327078	631.183415	10.664986
9.288158	647.582716	10.669991
9.412606	644.270148	10.674995
9.738693	642.242186	10.680000
9.047299	639.375019	10.685005
8.956746	632.274806	10.690010
8.847959	639.345656	10.695015
9.040125	633.558382	10.700019
8.950672	644.017809	10.705024
8.951864	643.538016	10.710029
9.143996	642.289320	10.715034
9.121833	650.602529	10.720039
9.642407	651.079712	10.725043
9.509433	657.469472	10.730048
9.567617	665.801281	10.735053
9.741039	663.263846	10.740058
9.839997	675.183061	10.745063
10.445738	669.183157	10.750067
9.840019	670.913690	10.755072
10.012668	669.388074	10.760077
9.807143	665.386042	10.765082
9.751239	676.758270	10.770087
9.878320	671.861201	10.775091
10.162598	671.019851	10.780096
9.974885	674.474332	10.785101
10.111467	672.482806	10.790106
9.731845	674.649036	10.795111
10.181497	683.579247	10.800115
9.956896	686.051261	10.805120
9.944085	689.806145	10.810125
9.908639	682.679093	10.815130
9.798578	700.169834	10.820135
10.407450	705.606251	10.825139
10.810728	706.621827	10.830144
10.745645	713.477590	10.835149
11.008749	701.144181	10.840154
10.470551	703.261816	10.845159
10.852560	700.295462	10.850163
10.753660	709.045009	10.855168
10.755753	703.836998	10.860173
11.014505	706.908628	10.865178
10.496950	709.309693	10.870183
10.966058	713.116952	10.875187
10.771919	719.576827	10.880192
10.825347	714.289354	10.885197
10.982998	716.263211	10.890202
10.985877	713.709220	10.895207
11.087993	712.833971	10.900211
10.922602	718.191570	10.905216
11.124364	717.895672	10.910221
11.033762	714.232336	10.915226
10.629538	723.232789	10.920231
11.263739	726.023343	10.925235
11.007776	723.301367	10.930240
11.228674	732.301221	10.935245
11.339792	738.774291	10.940250
11.181757	751.250381	10.945255
11.605749	746.997106	10.950259
11.707830	749.539827	10.955264
11.505374	738.000672	10.960269
11.907631	750.018729	10.965274
11.799405	747.105236	10.970279
12.088672	740.151821	10.975283
12.122095	737.939557	10.980288
12.159224	741.166032	10.985293
12.181530	727.441809	10.990298
12.098513	721.097354	10.995303
12.266559	709.405882	11.000307
12.256301	713.137835	11.005312
12.174930	712.309834	11.010317
12.485475	708.524038	11.015322
12.329035	701.440616	11.020327
12.186858	710.394948	11.025331
12.208807	707.303226	11.030336
11.925232	707.966050	11.035341
12.073639	711.610799	11.040346
12.061712	722.358165	11.045351
12.451197	716.239798	11.050355
12.448181	716.850571	11.055360
12.368566	730.343442	11.060365
12.773192	726.920056	11.065370
12.642772	741.931487	11.070375
12.784741	725.053385	11.075379
12.967131	720.787857	11.080384
12.668751	719.688386	11.085389
13.123605	705.367792	11.090394
12.832622	714.848552	11.095399
12.678795	710.373837	11.100403
12.503573	715.083791	11.105408
12.848800	729.724322	11.110413
13.309963	739.330737	11.115418
13.087634	740.916992	11.120423
13.304846	739.002815	11.125427
13.379858	725.687181	11.130432
12.951251	721.156156	11.135437
12.988251	711.761975	11.140442
12.896230	736.362287	11.145447
13.180502	742.747646	11.150451
13.099909	746.186934	11.155456
13.106345	748.817105	11.160461
13.557319	746.946530	11.165466
13.593176	748.255627	11.170471
13.097900	754.379524	11.175475
13.191613	753.420057	11.180480
13.415084	746.350817	11.185485
13.246576	749.378872	11.190490
13.158174	763.047353	11.195495
13.765653	768.531400	11.200499
14.229226	774.649191	11.205504
13.685524	782.206774	11.210509
14.054397	777.685445	11.215514
13.697093	781.911121	11.220519
13.730351	779.148624	11.225523
14.293000	777.900731	11.230528
14.172427	779.432833	11.235533
14.186201	770.303516	11.240538
14.125688	786.095623	11.245543
14.011809	775.562422	11.250547
14.354286	778.193797	11.255552
14.113699	784.050620	11.260557
13.887067	775.652113	11.265562
14.406757	787.905456	11.270567
14.616029	777.839471	11.275571
14.869291	782.989130	11.280576
14.312311	791.277272	11.285581
14.622756	785.246640	11.290586
14.473319	795.904740	11.295591
14.519090	782.034737	11.300595
14.664331	783.109954	11.305600
14.416467	786.213200	11.310605
14.439645	784.625965	11.315610
14.316905	781.910741	11.320615
14.807332	784.993190	11.325619
14.490820	786.849015	11.330624
15.109101	799.364142	11.335629
15.410079	793.419997	11.340634
14.910242	788.823008	11.345639
15.023601	790.943019	11.350643
14.974162	798.605731	11.355648
14.945252	803.523518	11.360653
15.053150	805.426575	11.365658
14.985557	807.911556	11.370663
14.960230	805.798565	11.375667
15.009374	803.639253	11.380672
15.103050	808.825756	11.385677
15.461952	803.074963	11.390682
15.174824	812.476963	11.395687
15.048523	809.389718	11.400691
15.522225	813.303582	11.405696
15.133753	829.983663	11.410701
15.963275	827.485682	11.415706
15.507794	836.266833	11.420711
15.666979	834.640880	11.425715
16.100274	828.165226	11.430720
15.789885	836.601373	11.435725
15.930001	832.627270	11.440730
15.789124	842.491707	11.445735
15.934439	839.612489	11.450739
16.184335	840.573057	11.455744
15.775441	842.211046	11.460749
15.887144	834.183967	11.465754
15.871577	838.270935	11.470759
16.032936	827.583930	11.475763
16.017844	834.154074	11.480768
15.915205	840.395024	11.485773
16.530080	833.404688	11.490778
16.263780	838.323319	11.495783
15.960276	837.768658	11.500787
16.287277	834.214482	11.505792
16.491137	837.477915	11.510797
16.151653	827.992296	11.515802
16.171420	851.278901	11.520807
16.560426	862.883664	11.525811
17.148238	863.577878	11.530816
16.726514	862.542569	11.535821
17.379338	857.657931	11.540826
17.063469	847.157341	11.545831
16.658404	837.384147	11.550835
16.958150	839.078660	11.555840
16.903319	837.928737	11.560845
16.770012	826.708052	11.565850
16.709327	838.113980	11.570855
17.052513	849.130544	11.575859
17.007368	845.961088	11.580864
16.838324	863.574229	11.585869
17.500062	860.886329	11.590874
17.282651	860.460984	11.595879
17.341072	853.858147	11.600883
17.683300	855.595509	11.605888
17.031297	846.186750	11.610893
17.946250	852.367312	11.615898
18.046224	840.485311	11.620903
17.501402	830.655952	11.625907
17.334272	827.104394	11.630912
17.202527	832.904284	11.635917
17.316947	831.014431	11.640922
17.442870	843.420198	11.645927
17.453769	862.680494	11.650931
17.678250	857.612326	11.655936
17.403709	867.163779	11.660941
17.804148	862.731355	11.665946
17.909785	867.743724	11.670951
17.982945	854.992370	11.675955
17.617505	857.914080	11.680960
17.672263	860.387170	11.685965
17.832638	857.923388	11.690970
17.445575	865.410338	11.695975
18.072805	877.680840	11.700979
18.283267	888.408348	11.705984
18.298051	891.527766	11.710989
18.375001	877.679963	11.715994
18.384239	890.805241	11.720999
18.390163	881.874177	11.726003
18.580119	870.160276	11.731008
18.150227	866.595735	11.736013
18.853248	872.020413	11.741018
18.499727	871.619982	11.746023
18.014158	873.909008	11.751027
18.394374	887.463305	11.756032
18.296260	885.723569	11.761037
19.029924	885.414628	11.766042
19.015807	893.711588	11.771047
19.381796	893.098189	11.776051
19.256737	878.510554	11.781056
18.547373	873.171839	11.786061
18.504718	869.273669	11.791066
18.818669	895.111192	11.796071
18.890237	898.391005	11.801075
18.889083	895.699124	11.806080
18.746238	895.404281	11.811085
18.879263	895.128060	11.816090
18.678618	896.852321	11.821095
18.778858	897.224742	11.826099
19.066654	898.767364	11.831104
18.811197	916.729720	11.836109
19.507893	907.229420	11.841114
19.571276	912.496546	11.846119
19.716872	910.958967	11.851123
20.280259	913.428543	11.856128
19.647810	899.211697	11.861133
19.461332	883.153941	11.866138
19.142555	890.993534	11.871143
19.427690	904.418491	11.876147
19.775885	912.019399	11.881152
19.787994	917.910708	11.886157
19.961107	905.121649	11.891162
19.842722	913.266762	11.896167
19.674396	912.485238	11.901171
19.776905	911.822277	11.906176
19.783588	916.962548	11.911181
20.228593	910.224723	11.916186
20.186282	924.069389	11.921191
20.171786	910.990784	11.926195
20.229232	909.071611	11.931200
20.184250	912.063518	11.936205
20.165598	910.248971	11.941210
20.353916	906.304874	11.946215
20.079121	921.522415	11.951219
20.072380	918.482543	11.956224
19.773738	924.011084	11.961229
19.942567	910.021580	11.966234
20.046703	938.458156	11.971239
20.600141	939.501687	11.976243
20.960833	936.984600	11.981248
20.930287	945.500719	11.986253
20.795895	930.312270	11.991258
20.635321	919.706057	11.996263
20.597667	931.300735	12.001267
20.795394	932.168018	12.006272
21.291774	935.552240	12.011277
21.336761	918.705556	12.016282
20.910977	906.502334	12.021287
21.289756	897.249177	12.026291
21.212962	897.490900	12.031296
21.052329	908.923096	12.036301
21.350700	898.132815	12.041306
20.985350	907.157498	12.046311
20.794936	898.984818	12.051315
21.272790	890.864538	12.056320
20.972984	889.659509	12.061325
21.031772	877.857961	12.066330
21.467766	883.654476	12.071335
21.325285	879.921444	12.076339
21.247817	880.062625	12.081344
20.630223	875.856058	12.086349
20.867093	871.569307	12.091354
21.085301	871.848476	12.096359
21.274314	871.340026	12.101363
21.013333	853.768247	12.106368
20.472764	855.103948	12.111373
20.840228	846.010654	12.116378
21.115113	851.739255	12.121383
20.868544	844.535827	12.126387
20.964750	839.325055	12.131392
20.788169	846.082363	12.136397
20.779340	846.687428	12.141402
20.926306	840.511516	12.146407
20.649073	849.328428	12.151411
20.915453	849.195920	12.156416
20.906526	858.922483	12.161421
21.072082	852.778115	12.166426
21.063958	855.359880	12.171431
20.806891	860.057069	12.176435
21.286274	849.138683	12.181440
21.004876	848.563258	12.186445
20.794537	855.999377	12.191450
20.730399	854.209609	12.196455
21.039642	861.232176	12.201459
20.904742	850.177929	12.206464
20.776054	866.882981	12.211469
20.903908	865.951995	12.216474
20.873924	859.998254	12.221479
20.908216	864.803383	12.226483
21.259361	860.569674	12.231488
21.149913	864.464720	12.236493
20.955254	851.187319	12.241498
20.770169	836.542910	12.246503
20.576396	831.537778	12.251507
20.792439	836.696995	12.256512
21.099699	850.890209	12.261517
20.800280	846.377654	12.266522
21.143561	836.595362	12.271527
20.898231	829.597384	12.276531
21.033377	827.711083	12.281536
20.518568	834.558745	12.286541
20.697514	830.077071	12.291546
20.663978	834.310406	12.296551
20.653093	838.831565	12.301555
20.957417	838.086638	12.306560
20.820266	847.746363	12.311565
20.454215	840.371583	12.316570
20.627380	845.449339	12.321575
21.063263	865.671762	12.326579
21.172279	858.035128	12.331584
20.831733	855.113684	12.336589
20.707976	833.424630	12.341594
20.590398	850.600254	12.346599
20.510270	861.180200	12.351603
21.295934	849.230364	12.356608
21.061049	866.780588	12.361613
21.134582	854.747978	12.366618
21.081420	843.056439	12.371623
20.725745	843.989784	12.376627
20.711173	834.872395	12.381632
20.251563	839.476411	12.386637
20.976356	840.124639	12.391642
20.712216	838.874815	12.396647
20.649149	848.759862	12.401651
20.818287	861.382049	12.406656
20.732525	866.078684	12.411661
20.699542	870.757193	12.416666
20.888930	874.646400	12.421671
20.894139	876.893517	12.426675
20.926735	876.097678	12.431680
20.599354	880.144566	12.436685
20.783187	873.705743	12.441690
21.005867	877.461744	12.446695
20.826630	884.877940	12.451699
20.795792	871.887036	12.456704
20.791800	876.058476	12.461709
20.726400	872.174468	12.466714
20.913914	871.853773	12.471719
20.812916	876.885389	12.476723
20.804151	868.740791	12.481728
20.331391	879.971089	12.486733
20.885289	881.921239	12.491738
20.607937	883.387469	12.496743
20.407325	888.103802	12.501747
20.637995	879.591702	12.506752
20.364988	889.855399	12.511757
20.837768	887.499495	12.516762
20.767273	887.970662	12.521767
20.559473	886.753806	12.526771
20.805776	879.230201	12.531776
20.784185	887.957120	12.536781
20.845657	879.297583	12.541786
21.044450	889.125522	12.546791
20.656486	884.187220	12.551795
20.940554	880.808946	12.556800
20.381701	883.092775	12.561805
20.967505	884.605222	12.566810
21.109617	886.425451	12.571815
21.022222	887.507799	12.576819
21.313858	886.762677	12.581824
21.036709	885.835998	12.586829
20.899445	883.170219	12.591834
20.789960	889.846175	12.596839
20.336329	888.914623	12.601843
20.818871	884.744430	12.606848
20.694349	894.176231	12.611853
21.131175	893.583451	12.616858
20.631918	881.993630	12.621863
20.558148	888.869117	12.626867
20.931447	880.387825	12.631872
20.587043	888.598518	12.636877
20.610719	888.499728	12.641882
20.764304	889.118395	12.646887
20.622859	894.549316	12.651891
21.627953	894.920937	12.656896
21.206153	892.222627	12.661901
21.238048	894.730432	12.666906
21.206166	891.332511	12.671911
20.984176	895.913960	12.676915
21.217191	891.061028	12.681920
20.734817	900.193006	12.686925
20.807992	894.950244	12.691930
21.088843	886.351379	12.696935
20.738865	887.466906	12.701939
20.845469	871.788382	12.706944
20.926786	872.635358	12.711949
21.005349	875.092133	12.716954
20.682584	873.267363	12.721959
20.709077	873.385588	12.726963
20.691013	872.602382	12.731968
20.909110	892.915075	12.736973
20.777240	885.922486	12.741978
20.992889	886.391566	12.746983
20.845284	881.930339	12.751987
20.897748	874.903387	12.756992
20.866942	873.078692	12.761997
20.664023	865.748560	12.767002
20.850277	868.138713	12.772007
21.063126	865.961588	12.777011
21.082416	866.581174	12.782016
20.324648	874.649182	12.787021
20.747572	866.920434	12.792026
20.966844	865.426280	12.797031
20.966548	865.758700	12.802035
20.801167	864.999569	12.807040
21.029230	865.565992	12.812045
20.671949	864.287925	12.817050
20.876467	871.368716	12.822055
20.726700	860.089644	12.827059
21.114902	858.349424	12.832064
20.952504	878.224445	12.837069
20.998987	867.761581	12.842074
20.844109	873.840187	12.847079
20.725973	868.147871	12.852083
21.082864	870.267585	12.857088
20.548458	878.448876	12.862093
20.852162	872.554365	12.867098
20.913432	868.367590	12.872103
20.723298	872.427261	12.877107
21.227853	872.396415	12.882112
20.875183	876.308298	12.887117
21.087309	870.740144	12.892122
20.877811	875.782073	12.897127
20.458598	882.783890	12.902131
21.354645	874.219290	12.907136
21.122906	881.555670	12.912141
21.134218	873.754993	12.917146
21.186332	872.865808	12.922151
20.781454	865.517409	12.927155
20.757631	859.520771	12.932160
20.895245	857.741410	12.937165
20.674288	855.791031	12.942170
20.789345	854.544085	12.947175
20.759194	865.825195	12.952179
20.988508	878.915494	12.957184
20.657717	879.799576	12.962189
20.947901	874.523166	12.967194
20.994951	876.981397	12.972199
20.648481	862.046479	12.977203
21.002041	856.396055	12.982208
20.731046	858.003296	12.987213
21.099587	855.129222	12.992218
20.803108	852.890216	12.997223
20.650418	850.846818	13.002227
20.983557	839.927460	13.007232
21.016673	852.602960	13.012237
20.884008	837.041283	13.017242
21.011481	840.373077	13.022247
20.542187	847.472280	13.027251
21.055952	835.408810	13.032256
20.855759	846.218146	13.037261
20.334324	843.398375	13.042266
20.726450	846.925582	13.047271
20.559219	859.864383	13.052275
21.141039	870.939520	13.057280
20.725202	862.091438	13.062285
20.587614	853.028287	13.067290
20.851884	866.826653	13.072295
20.529352	881.312215	13.077299
21.185658	875.340670	13.082304
20.759021	875.805004	13.087309
20.887361	880.547829	13.092314
20.989123	875.571354	13.097319
20.739842	869.272712	13.102323
20.776404	852.053338	13.107328
20.968606	875.711859	13.112333
20.800930	869.135939	13.117338
20.728199	860.178900	13.122343
21.116806	866.956155	13.127347
20.672175	846.460507	13.132352
20.650364	850.552495	13.137357
20.612152	855.143081	13.142362
20.962564	860.831499	13.147367
20.901708	876.658493	13.152371
21.121496	871.338496	13.157376
20.922505	858.376435	13.162381
20.552750	854.849742	13.167386
20.832842	856.692888	13.172391
20.793293	856.899409	13.177395
20.957345	840.858570	13.182400
20.558216	854.440277	13.187405
20.588257	856.072877	13.192410
20.899263	878.528415	13.197415
20.913363	881.724131	13.202419
21.227882	872.100695	13.207424
20.806076	852.910454	13.212429
21.023640	845.031402	13.217434
20.881785	844.033767	13.222439
20.477001	841.030577	13.227443
21.044566	841.659974	13.232448
21.012627	852.767304	13.237453
20.761273	852.172122	13.242458
20.558650	842.792500	13.247463
20.623526	859.256332	13.252467
20.756998	848.371991	13.257472
20.925129	852.584965	13.262477
20.760389	862.710872	13.267482
21.239518	862.752675	13.272487
21.203173	865.314412	13.277491
21.100596	851.268073	13.282496
21.010137	857.474574	13.287501
20.843033	859.165449	13.292506
21.067742	855.680911	13.297511
20.786702	859.850900	13.302515
20.682201	852.886791	13.307520
20.393106	859.327874	13.312525
20.614890	862.517978	13.317530
20.988197	851.942247	13.322535
20.620352	857.537498	13.327539
20.644836	849.645759	13.332544
20.977930	854.655835	13.337549
20.645476	859.180425	13.342554
20.565774	856.458993	13.347559
20.999339	857.442545	13.352563
21.225393	854.965529	13.357568
20.784558	854.992565	13.362573
20.915778	859.857257	13.367578
20.891619	858.214185	13.372583
20.669530	867.593225	13.377587
21.034284	867.413456	13.382592
21.105728	859.987340	13.387597
20.637589	856.042915	13.392602
20.720840	859.246902	13.397607
21.035962	861.687194	13.402611
20.844052	856.904364	13.407616
21.130779	861.191742	13.412621
20.969747	856.245725	13.417626
21.232451	860.082490	13.422631
20.898302	867.654709	13.427635
20.768609	854.640112	13.432640
20.770670	863.899404	13.437645
21.053649	857.202013	13.442650
21.028095	859.276377	13.447655
21.100574	861.337882	13.452659
21.228201	848.734297	13.457664
20.633435	836.537998	13.462669
20.592204	838.171763	13.467674
21.013448	835.233000	13.472679
20.523397	833.246261	13.477683
20.650816	843.069041	13.482688
20.935680	850.980379	13.487693
20.634808	865.652079	13.492698
20.937903	866.127480	13.497703
21.008274	865.935422	13.502707
20.852762	852.466179	13.507712
20.705158	849.285474	13.512717
20.962580	855.997585	13.517722
20.815480	851.732068	13.522727
20.688466	851.320039	13.527731
20.822383	857.065706	13.532736
20.883033	868.237303	13.537741
20.814393	859.487982	13.542746
20.918538	862.436942	13.547751
20.563459	854.459096	13.552755
20.692930	856.685694	13.557760
20.604789	861.302605	13.562765
20.808724	868.625071	13.567770
20.835532	861.537788	13.572775
21.026017	878.666150	13.577779
21.157085	873.187287	13.582784
21.255729	865.565454	13.587789
21.169258	861.563484	13.592794
21.367273	848.217181	13.597799
21.066482	845.461421	13.602803
21.361555	835.021088	13.607808
21.358422	845.581112	13.612813
20.910884	842.145521	13.617818
21.048468	821.666528	13.622823
20.522144	823.049520	13.627827
20.651390	816.164560	13.632832
20.575860	826.828957	13.637837
20.802959	842.794439	13.642842
20.602599	843.763522	13.647847
20.732280	850.318324	13.652851
20.786809	848.334529	13.657856
20.924614	848.507483	13.662861
21.014420	851.073247	13.667866
20.879236	842.211398	13.672871
20.953698	853.124435	13.677875
20.784879	851.324589	13.682880
20.990157	856.453290	13.687885
20.731489	859.089460	13.692890
21.179301	846.179141	13.697895
20.886142	840.671973	13.702899
20.756865	817.574298	13.707904
20.625519	820.521390	13.712909
20.794670	840.332807	13.717914
21.041894	838.303343	13.722919
20.859222	840.030438	13.727923
20.889269	823.870093	13.732928
20.859768	814.460016	13.737933
20.627751	810.843008	13.742938
20.627611	809.659238	13.747943
21.019849	839.293195	13.752947
20.665075	843.830291	13.757952
20.349517	850.472484	13.762957
21.069874	853.196582	13.767962
21.288131	847.791988	13.772967
20.706690	835.272487	13.777971
21.259071	834.715948	13.782976
20.838478	827.785519	13.787981
20.999512	818.238562	13.792986
20.542178	814.908077	13.797991
20.302705	823.870867	13.802995
20.980757	838.781670	13.808000
20.661702	845.274462	13.813005
20.564442	853.134082	13.818010
20.956787	857.451113	13.823015
20.851038	860.068565	13.828019
20.696068	855.711633	13.833024
21.072336	861.156015	13.838029
20.984643	850.354592	13.843034
21.207302	835.236858	13.848039
20.893961	830.347752	13.853043
20.924812	818.896823	13.858048
20.658250	818.113990	13.863053
20.467718	824.540527	13.868058
20.474429	823.230451	13.873063
20.882013	838.263415	13.878067
20.636990	854.193015	13.883072
21.048316	854.746569	13.888077
20.632611	853.068393	13.893082
21.090017	845.327033	13.898087
20.794263	866.022263	13.903091
21.114218	854.891999	13.908096
21.019305	831.638018	13.913101
20.592915	830.607458	13.918106
20.641565	827.436530	13.923111
20.814729	853.024573	13.928115
20.861784	856.596340	13.933120
20.831424	847.205732	13.938125
20.921693	854.996885	13.943130
21.103142	832.143147	13.948135
20.727173	834.025354	13.953139
20.606086	813.417830	13.958144
20.403588	828.041840	13.963149
20.509270	854.616048	13.968154
21.054857	852.337271	13.973159
20.807125	860.033222	13.978163
21.168018	853.206817	13.983168
21.033097	856.924258	13.988173
20.712876	857.493502	13.993178
21.035461	854.233760	13.998183
20.800723	848.169868	14.003187
20.577419	826.705519	14.008192
20.795698	846.719383	14.013210
20.618029	854.512937	14.018227
21.121281	849.551547	14.023245
20.892453	858.309052	14.028263
20.962779	853.918377	14.033280
21.194445	865.562080	14.038298
20.988762	856.032176	14.043315
20.798843	836.359967	14.048333
20.689441	840.918775	14.053351
20.745225	850.570450	14.058368
20.921586	863.548127	14.063386
20.878588	862.901132	14.068403
21.146414	859.230184	14.073421
21.038799	868.271656	14.078439
20.901073	866.365230	14.083456
20.926367	861.966130	14.088474
20.756074	869.449745	14.093491
20.865970	860.398836	14.098509
20.869707	862.931826	14.103527
20.957053	864.395296	14.108544
21.503998	856.679388	14.113562
20.934577	858.588555	14.118579
21.589065	856.527797	14.123597
21.483662	866.852828	14.128615
21.551347	856.874847	14.133632
21.855717	866.234682	14.138650
21.093404	865.235002	14.143667
20.960001	863.490050	14.148685
21.167720	866.830641	14.153703
21.236578	863.865502	14.158720
21.286822	856.181602	14.163738
20.814206	871.386831	14.168755
21.248718	872.136800	14.173773
21.150254	873.066738	14.178791
21.145555	881.509432	14.183808
21.499964	889.204295	14.188826
21.054760	891.001611	14.193843
21.151414	888.430153	14.198861
20.822142	891.483659	14.203879
20.925040	891.598314	14.208896
21.245444	901.912177	14.213914
21.049416	926.813204	14.218931
21.683948	922.707689	14.223949
21.474257	924.043735	14.228967
21.995649	935.070061	14.233984
22.028633	925.252720	14.239002
21.770404	930.931634	14.244019
21.716072	925.722490	14.249037
21.462681	931.103310	14.254055
21.438423	927.791501	14.259072
21.351187	920.177995	14.264090
21.439056	926.602740	14.269107
21.361932	921.248283	14.274125
21.627098	928.960435	14.279143
21.433446	923.094031	14.284160
22.014317	924.385483	14.289178
21.702183	936.308708	14.294195
21.632369	917.959991	14.299213
22.016160	934.833923	14.304231
21.726794	937.030932	14.309248
21.947706	931.729710	14.314266
21.680809	933.922472	14.319283
22.101489	948.441115	14.324301
22.124394	949.898318	14.329319
21.933200	943.344429	14.334336
22.049996	935.025809	14.339354
22.009021	941.860472	14.344371
22.199051	938.604447	14.349389
22.141052	924.886690	14.354407
21.895494	933.262434	14.359424
22.055141	931.453843	14.364442
21.981876	944.862209	14.369459
22.372267	943.427075	14.374477
22.118457	930.424036	14.379495
22.026036	948.886033	14.384512
22.134578	946.201890	14.389530
22.196365	956.347911	14.394547
22.305194	956.106800	14.399565
22.572630	955.107737	14.404583
22.088920	955.155240	14.409600
22.504178	952.159042	14.414618
21.989207	950.990560	14.419635
22.334323	945.919631	14.424653
22.290180	959.152137	14.429671
22.082025	961.035598	14.434688
22.518969	951.711225	14.439706
22.455933	956.013674	14.444723
22.352504	958.392995	14.449741
22.560993	957.532393	14.454759
22.143861	954.827739	14.459776
22.524041	946.491910	14.464794
22.409060	962.218232	14.469811
22.347405	955.638191	14.474829
22.343664	960.233646	14.479847
22.112256	952.282613	14.484864
22.317081	954.256695	14.489882
22.226736	962.062497	14.494899
22.389769	967.748336	14.499917
22.418946	981.277761	14.504935
22.612472	988.067120	14.509952
22.688436	987.121751	14.514970
22.481193	991.777305	14.519987
23.137980	986.401726	14.525005
23.104182	983.799465	14.530023
22.725600	982.294189	14.535040
23.041715	970.985260	14.540058
22.725399	966.868733	14.545075
22.399491	956.190794	14.550093
22.997690	973.422129	14.555111
23.138288	978.742502	14.560128
23.482553	970.170281	14.565146
22.717599	955.901219	14.570163
22.941706	955.350953	14.575181
22.925159	963.846514	14.580199
22.755208	953.550528	14.585216
23.207784	944.835333	14.590234
23.240158	952.403145	14.595251
23.182287	952.874128	14.600269
23.420696	951.909965	14.605287
23.066707	952.454161	14.610304
23.185792	951.215948	14.615322
23.421902	958.528738	14.620339
23.083473	954.834144	14.625357
23.020034	955.592716	14.630375
22.826770	950.573538	14.635392
22.980656	946.787844	14.640410
23.041791	952.009225	14.645427
22.951573	950.352929	14.650445
23.319771	951.702502	14.655463
22.857543	950.521040	14.660480
23.296542	954.388177	14.665498
23.123015	950.787761	14.670515
22.903114	950.968392	14.675533
23.250966	959.015620	14.680551
23.313564	982.955401	14.685568
23.662145	980.469483	14.690586
23.350507	984.603526	14.695603
23.294059	980.842468	14.700621
23.530895	979.863611	14.705639
23.508761	988.514879	14.710656
23.406698	984.827787	14.715674
23.659811	983.798498	14.720691
23.554390	988.716141	14.725709
23.772966	972.574375	14.730727
23.491704	972.235962	14.735744
23.710853	972.168076	14.740762
23.468191	967.042000	14.745779
23.752515	980.570201	14.750797
23.699045	974.214749	14.755815
23.479360	982.537654	14.760832
23.721477	981.389375	14.765850
23.079957	981.459998	14.770867
23.557347	977.658204	14.775885
23.662841	977.996446	14.780903
23.244477	983.387064	14.785920
23.557186	979.157566	14.790938
23.511400	980.177304	14.795955
23.813736	983.035917	14.800973
24.127419	974.295696	14.805991
23.763787	984.813908	14.811008
24.175469	979.413028	14.816026
24.079549	976.964737	14.821043
23.955294	977.975880	14.826061
24.209137	978.557998	14.831079
23.872062	983.037764	14.836096
24.021245	972.156697	14.841114
24.120079	980.027323	14.846131
24.216889	981.058049	14.851149
24.684507	975.288893	14.856167
24.581827	979.567041	14.861184
24.218725	965.308605	14.866202
24.266129	956.336470	14.871219
23.968448	947.953070	14.876237
23.867513	943.674415	14.881255
24.002757	960.305537	14.886272
23.923488	960.277004	14.891290
24.023819	970.036084	14.896307
24.022532	986.093749	14.901325
24.177673	976.733025	14.906343
24.271357	974.190018	14.911360
24.175242	977.950468	14.916378
24.040272	979.054006	14.921395
23.908370	973.113605	14.926413
24.189457	971.092049	14.931431
23.912050	980.253648	14.936448
24.275073	988.968417	14.941466
24.470819	995.593607	14.946483
24.618972	995.383158	14.951501
25.039030	989.119753	14.956519
24.670082	984.196832	14.961536
24.666187	968.889727	14.966554
24.447431	964.296991	14.971571
24.258134	971.642959	14.976589
24.743345	962.231165	14.981607
24.482611	969.781912	14.986624
24.412271	963.415970	14.991642
24.789824	966.577453	14.996659
24.527273	973.845030	15.001677
24.886798	972.839626	15.006695
24.563400	962.667194	15.011712
24.628169	963.023049	15.016730
24.501295	972.634852	15.021747
24.535581	986.735494	15.026765
25.081892	996.456711	15.031783
25.225404	1001.040318	15.036800
24.928924	978.209986	15.041818
24.473004	961.711401	15.046835
24.688783	984.329555	15.051853
25.102312	995.150779	15.056871
25.165105	992.267764	15.061888
24.799254	982.812098	15.066906
24.642841	977.889749	15.071923
25.003285	990.674936	15.076941
25.191222	989.157179	15.081959
24.994444	998.567582	15.086976
24.838798	1000.314082	15.091994
25.058209	994.257530	15.097011
24.869168	999.458036	15.102029
25.033066	988.335441	15.107047
25.210149	992.714850	15.112064
25.297673	989.597658	15.117082
25.346103	988.980261	15.122099
24.957902	1002.039887	15.127117
25.444645	991.428120	15.132135
25.226289	993.738954	15.137152
25.682716	994.861578	15.142170
25.703087	996.164484	15.147187
25.139073	982.189315	15.152205
25.348557	969.918678	15.157223
25.150690	964.519155	15.162240
25.081595	975.442800	15.167258
25.423268	984.067519	15.172275
25.172611	994.089168	15.177293
25.206003	991.964004	15.182311
24.968992	1000.806068	15.187328
25.242702	1003.731408	15.192346
25.398998	994.220465	15.197363
25.483445	1004.074816	15.202381
25.228128	996.065651	15.207399
25.631619	997.486347	15.212416
25.279408	993.411009	15.217434
25.416581	998.810328	15.222451
25.490710	1011.354048	15.227469
25.657769	1022.931382	15.232487
25.903786	1028.024233	15.237504
25.799425	1028.137020	15.242522
26.042631	1010.320789	15.247539
25.739252	1003.853043	15.252557
25.651962	994.881143	15.257575
25.776133	1002.560416	15.262592
25.660107	1002.927584	15.267610
25.757395	1013.462859	15.272627
25.942093	1015.414807	15.277645
26.182829	1016.045241	15.282663
25.964024	1007.049029	15.287680
25.858149	1011.213158	15.292698
26.038123	1000.026770	15.297715
25.459316	1002.230103	15.302733
25.944664	1017.386983	15.307751
25.790190	1014.000231	15.312768
25.955126	1009.776375	15.317786
26.189703	1012.226894	15.322803
26.355952	1018.959916	15.327821
26.387675	1018.405229	15.332839
25.992658	1017.177590	15.337856
26.028131	1023.247158	15.342874
26.340826	1012.493551	15.347891
26.246511	1021.037519	15.352909
26.484200	1018.453277	15.357927
26.409380	1019.193329	15.362944
26.403706	1013.451759	15.367962
26.472138	1017.208418	15.372979
26.008454	1020.297594	15.377997
26.382491	1016.326095	15.383015
26.477784	1019.976567	15.388032
26.141011	1021.116282	15.393050
26.518640	1021.451572	15.398067
26.289565	1023.381937	15.403085
26.395023	1017.223251	15.408103
26.467004	1021.036393	15.413120
26.367008	1018.530129	15.418138
26.589849	1021.661452	15.423155
26.517976	1015.699324	15.428173
26.646545	1015.756819	15.433191
26.717122	1017.383033	15.438208
26.464898	1021.303340	15.443226
27.112216	1025.185176	15.448243
26.891128	1020.923951	15.453261
26.697314	1020.408326	15.458279
26.758546	1016.854659	15.463296
26.639990	1030.643332	15.468314
26.763581	1015.709233	15.473331
26.508870	1032.029310	15.478349
26.640605	1023.934083	15.483367
26.933873	1028.874334	15.488384
26.765325	1027.632276	15.493402
27.026710	1015.676351	15.498419
26.736623	1015.595374	15.503437
26.815591	1012.818251	15.508455
27.370063	1020.573768	15.513472
27.088527	1022.239879	15.518490
27.410340	1019.409701	15.523507
27.143186	1031.728073	15.528525
26.702065	1029.874038	15.533543
26.900441	1022.610755	15.538560
26.634265	1029.612818	15.543578
26.873045	1022.019749	15.548595
26.998690	1024.751172	15.553613
26.673957	1022.988215	15.558631
26.518360	1020.981282	15.563648
26.821714	1038.287654	15.568666
27.033788	1041.273178	15.573683
26.796206	1054.333798	15.578701
27.041418	1043.387787	15.583719
27.687564	1036.901334	15.588736
27.511746	1044.117456	15.593754
27.885042	1044.470813	15.598771
27.877441	1042.447953	15.603789
27.348160	1037.365089	15.608807
27.671580	1038.173881	15.613824
27.458068	1040.813838	15.618842
27.446623	1039.340891	15.623859
27.174685	1037.332249	15.628877
27.460959	1039.766035	15.633895
27.486790	1035.992038	15.638912
27.474575	1050.231428	15.643930
27.554652	1036.183971	15.648947
27.048982	1041.993544	15.653965
27.489341	1044.615102	15.658983
27.366217	1044.548415	15.664000
27.083279	1047.060109	15.669018
27.459041	1051.346805	15.674035
27.500063	1062.273285	15.679053
27.740052	1072.348274	15.684071
27.978204	1067.308245	15.689088
27.831850	1073.190880	15.694106
28.134299	1069.496229	15.699123
28.142441	1068.553427	15.704141
28.041294	1055.003203	15.709159
28.018523	1038.568864	15.714176
27.802083	1035.734504	15.719194
28.072096	1036.277629	15.724211
27.912050	1039.412787	15.729229
27.556727	1044.841046	15.734247
27.932647	1053.685146	15.739264
27.775530	1066.285095	15.744282
28.148365	1068.776885	15.749299
28.050043	1063.093704	15.754317
27.998877	1068.745040	15.759335
28.247312	1062.987840	15.764352
28.267677	1073.730454	15.769370
28.257504	1069.851196	15.774387
28.231159	1066.663347	15.779405
28.047077	1069.298263	15.784423
28.680215	1064.307451	15.789440
28.398046	1073.642375	15.794458
28.552215	1072.151661	15.799475
28.230988	1070.825926	15.804493
28.191391	1070.296459	15.809511
28.416919	1073.196999	15.814528
28.228643	1075.633801	15.819546
28.109703	1067.148820	15.824563
28.247693	1066.998778	15.829581
28.314268	1071.012088	15.834599
28.570450	1065.183868	15.839616
28.098632	1065.886074	15.844634
28.280932	1078.508161	15.849651
28.461121	1095.606167	15.854669
28.405879	1092.730772	15.859687
28.883948	1086.485337	15.864704
28.937870	1097.525388	15.869722
28.799918	1092.434471	15.874739
28.956403	1089.194403	15.879757
28.772693	1098.296301	15.884775
28.861085	1091.788516	15.889792
28.708703	1096.735112	15.894810
28.741315	1095.473128	15.899827
28.870546	1097.088113	15.904845
28.806947	1099.043663	15.909863
28.871416	1094.742120	15.914880
28.722779	1105.520426	15.919898
28.974161	1094.181559	15.924915
29.152937	1087.052326	15.929933
28.788188	1099.247315	15.934951
29.088559	1084.480101	15.939968
29.132806	1094.196902	15.944986
28.961632	1091.817012	15.950003
29.241903	1090.885430	15.955021
28.894865	1092.545848	15.960039
29.300509	1096.152184	15.965056
29.162068	1100.271917	15.970074
29.374275	1099.544146	15.975091
29.629395	1095.967455	15.980109
29.253800	1101.260615	15.985127
29.332514	1092.315713	15.990144
29.120523	1096.482310	15.995162
29.055629	1094.647627	16.000179
29.128679	1092.686923	16.005197
29.271189	1093.519255	16.010215
29.226084	1094.464075	16.015232
29.284432	1101.193583	16.020250
29.278786	1095.251569	16.025267
29.584031	1109.219637	16.030285
29.640191	1125.019939	16.035303
29.700599	1105.775768	16.040320
29.594497	1104.366293	16.045338
29.350125	1119.398759	16.050355
29.712329	1108.595650	16.055373
29.695947	1121.156552	16.060391
30.067375	1109.803786	16.065408
29.915939	1095.575479	16.070426
29.706040	1095.931575	16.075443
29.890644	1088.764331	16.080461
29.708847	1101.998905	16.085479
29.722161	1091.140262	16.090496
29.823421	1101.096131	16.095514
29.818476	1119.820520	16.100531
30.432228	1121.519378	16.105549
29.692049	1110.097334	16.110567
29.841259	1100.779683	16.115584
30.209022	1119.114159	16.120602
29.783268	1118.416233	16.125619
30.297419	1120.476683	16.130637
29.926217	1116.234869	16.135655
30.409278	1118.413257	16.140672
30.170171	1111.562763	16.145690
29.836351	1111.891677	16.150707
30.053649	1114.479044	16.155725
30.191999	1124.814427	16.160743
30.719133	1115.034301	16.165760
30.493018	1112.790215	16.170778
30.436724	1115.504025	16.175795
30.398750	1101.327919	16.180813
30.309357	1111.039294	16.185831
30.143600	1108.601775	16.190848
30.315335	1105.909132	16.195866
30.468055	1111.410951	16.200883
30.440708	1110.219881	16.205901
30.099375	1115.059891	16.210919
30.355368	1108.723773	16.215936
30.497808	1118.294215	16.220954
30.217626	1118.540306	16.225971
31.001232	1112.202709	16.230989
30.581318	1124.549313	16.236007
30.787347	1122.158294	16.241024
30.853892	1116.630306	16.246042
30.438420	1111.859032	16.251059
30.387416	1112.470586	16.256077
30.436387	1120.625052	16.261095
30.371951	1123.048897	16.266112
30.332946	1127.854401	16.271130
30.568091	1145.274562	16.276147
31.006497	1143.837086	16.281165
30.702715	1151.232690	16.286183
30.590654	1153.897401	16.291200
31.023719	1142.811625	16.296218
30.562966	1148.792684	16.301235
30.815758	1147.946526	16.306253
30.944220	1156.801613	16.311271
30.902529	1146.658326	16.316288
31.133258	1149.676110	16.321306
30.931108	1149.316647	16.326323
31.109427	1145.919662	16.331341
31.229258	1147.076383	16.336359
31.151695	1149.411531	16.341376
31.105438	1146.026275	16.346394
30.620035	1147.804131	16.351411
31.522332	1165.563117	16.356429
31.099764	1169.463056	16.361447
31.216174	1177.081929	16.366464
31.361351	1167.165667	16.371482
31.188312	1178.635272	16.376499
31.776076	1173.368324	16.381517
31.882038	1169.648278	16.386535
31.888126	1163.825102	16.391552
31.996263	1147.859977	16.396570
31.927492	1143.267459	16.401587
31.801545	1141.398353	16.406605
31.895576	1132.582309	16.411623
31.962830	1137.008545	16.416640
32.199987	1138.758192	16.421658
31.992203	1134.946659	16.426675
31.991503	1131.418940	16.431693
32.010603	1130.332905	16.436711
31.942311	1128.050733	16.441728
31.629586	1103.285445	16.446746
31.402781	1115.828085	16.451763
31.673927	1123.773187	16.456781
31.737336	1130.509321	16.461799
31.983580	1138.628005	16.466816
31.833037	1141.263482	16.471834
31.750295	1138.660138	16.476851
32.046758	1142.287960	16.481869
31.952596	1141.645001	16.486887
31.607939	1143.045546	16.491904
31.743571	1135.764619	16.496922
31.911745	1145.342085	16.501939
31.662669	1135.374137	16.506957
31.830244	1150.813602	16.511975
31.722694	1168.377592	16.516992
31.979811	1182.077577	16.522010
31.639324	1175.082612	16.527027
31.982712	1179.370957	16.532045
32.086498	1181.985279	16.537063
32.075058	1178.267248	16.542080
32.149166	1182.058016	16.547098
32.298437	1198.860625	16.552115
32.643417	1207.932578	16.557133
32.517468	1207.504138	16.562151
32.580456	1204.809650	16.567168
32.889062	1195.475638	16.572186
32.560087	1187.975894	16.577203
32.693051	1176.746648	16.582221
32.257573	1178.308055	16.587239
32.477678	1191.191885	16.592256
32.849689	1192.390026	16.597274
33.293847	1200.305504	16.602291
32.827150	1181.081528	16.607309
32.918965	1170.989358	16.612327
32.553401	1170.341744	16.617344
32.996404	1167.860477	16.622362
32.529196	1173.065816	16.627379
32.559322	1162.466074	16.632397
32.771204	1182.535761	16.637415
32.801009	1193.359524	16.642432
33.224265	1189.473646	16.647450
33.128929	1200.676380	16.652467
32.745998	1203.808442	16.657485
32.783716	1199.286241	16.662503
32.885449	1202.293865	16.667520
33.056477	1195.084015	16.672538
32.773496	1201.163366	16.677555
33.115505	1196.197622	16.682573
33.251712	1197.476354	16.687591
32.868231	1194.408376	16.692608
33.314823	1195.279925	16.697626
33.249622	1199.340272	16.702643
33.398217	1197.991459	16.707661
33.180216	1186.165237	16.712679
33.314992	1205.114613	16.717696
33.452298	1189.386198	16.722714
33.169060	1199.369860	16.727731
33.647835	1217.326333	16.732749
33.475268	1225.999587	16.737767
33.274709	1224.025537	16.742784
33.448967	1219.432277	16.747802
33.827363	1228.540643	16.752819
33.865749	1215.973923	16.757837
33.736986	1223.644305	16.762855
33.678035	1223.668985	16.767872
33.647287	1222.676932	16.772890
33.970931	1227.798275	16.777907
33.802982	1212.053663	16.782925
34.263628	1212.411736	16.787943
33.758150	1203.358252	16.792960
34.032711	1190.951864	16.797978
34.169181	1188.317621	16.802995
33.891887	1192.489533	16.808013
33.760921	1176.807519	16.813031
33.502889	1189.672528	16.818048
33.790481	1198.916141	16.823066
33.414825	1214.835060	16.828083
33.468493	1222.426915	16.833101
33.984244	1224.795400	16.838119
33.460814	1223.443684	16.843136
33.467743	1232.329889	16.848154
33.756070	1241.737981	16.853171
33.826230	1250.231826	16.858189
34.044855	1244.743866	16.863207
34.119509	1260.813206	16.868224
34.294344	1244.001040	16.873242
34.136965	1255.871989	16.878259
34.300174	1252.039737	16.883277
34.464956	1246.783863	16.888295
34.462963	1251.127507	16.893312
34.499337	1256.793038	16.898330
34.600648	1258.685292	16.903347
34.653646	1255.144401	16.908365
35.020630	1252.299350	16.913383
35.203482	1252.110117	16.918400
35.097069	1245.093887	16.923418
35.274099	1248.610310	16.928435
35.430837	1248.351926	16.933453
35.487247	1236.126618	16.938471
35.067934	1229.166798	16.943488
34.916414	1214.099348	16.948506
34.879531	1214.729352	16.953523
34.853633	1214.538505	16.958541
34.936777	1208.795416	16.963559
34.279775	1217.395803	16.968576
34.663847	1206.877485	16.973594
34.949721	1222.562904	16.978611
34.560800	1233.484866	16.983629
35.061929	1233.241064	16.988647
34.800231	1249.260570	16.993664
34.941722	1243.654328	16.998682
34.874254	1247.473323	17.003699
34.891786	1239.814530	17.008717
35.200311	1238.440656	17.013735
35.022934	1243.852254	17.018752
34.922890	1246.044407	17.023770
34.971253	1248.888734	17.028787
35.085112	1279.076247	17.033805
35.080615	1269.793117	17.038823
34.988949	1283.585277	17.043840
35.147442	1279.227796	17.048858
35.240203	1275.374937	17.053875
35.383224	1283.114114	17.058893
35.400288	1275.525075	17.063911
35.054562	1287.485038	17.068928
35.392973	1279.506620	17.073946
35.601945	1295.840395	17.078963
35.527380	1293.950254	17.083981
35.884683	1292.989311	17.088999
35.532589	1300.532651	17.094016
35.625970	1287.589088	17.099034
35.936702	1302.053679	17.104051
35.562119	1301.956081	17.109069
35.683060	1295.362701	17.114087
35.845967	1301.898369	17.119104
35.522400	1296.106464	17.124122
35.495763	1292.879639	17.129139
35.724800	1297.669951	17.134157
35.932309	1291.447987	17.139175
36.038534	1318.338947	17.144192
36.193718	1320.434984	17.149210
36.599480	1320.692617	17.154227
36.022346	1304.005374	17.159245
36.394620	1291.231729	17.164263
36.246798	1296.131538	17.169280
36.147593	1293.376252	17.174298
36.143770	1294.899099	17.179315
36.081722	1310.643864	17.184333
36.527348	1310.113881	17.189351
36.548716	1318.859064	17.194368
36.430253	1316.354736	17.199386
36.537501	1316.603701	17.204403
36.580707	1314.157096	17.209421
36.588420	1306.670836	17.214439
36.491612	1319.782745	17.219456
36.290691	1323.785284	17.224474
36.428819	1324.713664	17.229491
36.097951	1325.506292	17.234509
36.508463	1323.999560	17.239527
36.595905	1323.252615	17.244544
36.862090	1314.753442	17.249562
37.021877	1326.019228	17.254579
36.709253	1326.178748	17.259597
37.043806	1313.502505	17.264615
36.855115	1315.434643	17.269632
36.612169	1321.099264	17.274650
37.254395	1315.332335	17.279667
36.913776	1325.782257	17.284685
36.846003	1323.510204	17.289703
36.516494	1326.876461	17.294720
36.694370	1320.005175	17.299738
36.905678	1330.403389	17.304755
37.225488	1345.499988	17.309773
37.359126	1345.081374	17.314791
37.539876	1352.236504	17.319808
37.116841	1348.829968	17.324826
37.609235	1345.050714	17.329843
37.302685	1343.516119	17.334861
37.712232	1340.440112	17.339879
37.517938	1323.371039	17.344896
37.077740	1313.686162	17.349914
37.682164	1326.359710	17.354931
37.199675	1329.765977	17.359949
37.352868	1331.205209	17.364967
37.315231	1343.845926	17.369984
37.893076	1344.370147	17.375002
37.812843	1337.161180	17.380019
37.296831	1345.809911	17.385037
37.695512	1342.734192	17.390055
37.628479	1337.901926	17.395072
37.658822	1344.874946	17.400090
37.808162	1340.166621	17.405107
37.831582	1343.404649	17.410125
38.112679	1340.123084	17.415143
38.056693	1337.891533	17.420160
37.891430	1339.007376	17.425178
38.218243	1337.903613	17.430195
38.210255	1347.974048	17.435213
38.286097	1343.226744	17.440231
37.764777	1349.686417	17.445248
38.120026	1341.457814	17.450266
38.002744	1336.362485	17.455283
37.688693	1346.352310	17.460301
37.763508	1341.402801	17.465319
38.017894	1334.961740	17.470336
38.098737	1330.308473	17.475354
38.305590	1337.071683	17.480371
38.562636	1360.644029	17.485389
38.314969	1358.272880	17.490407
38.667134	1368.303236	17.495424
38.214631	1362.073919	17.500442
38.512953	1359.226447	17.505459
38.359715	1371.211351	17.510477
38.583995	1373.944824	17.515495
38.788635	1370.156626	17.520512
38.533486	1370.492137	17.525530
38.623908	1365.071002	17.530547
38.506462	1372.211119	17.535565
38.680248	1366.424082	17.540583
38.610895	1367.663655	17.545600
38.884350	1370.369403	17.550618
38.571091	1367.170048	17.555635
38.472609	1370.509304	17.560653
38.686505	1365.323717	17.565671
38.462376	1373.000285	17.570688
38.618836	1393.304570	17.575706
39.380351	1384.695236	17.580723
39.056661	1392.343602	17.585741
39.091142	1391.450208	17.590759
39.245530	1400.031671	17.595776
39.189934	1398.486331	17.600794
39.412204	1396.595685	17.605811
39.057193	1395.441477	17.610829
39.484137	1390.466230	17.615847
39.663383	1389.514547	17.620864
39.408056	1396.191259	17.625882
39.453075	1392.116219	17.630899
39.282751	1393.387280	17.635917
39.613479	1399.620174	17.640935
40.006378	1394.285765	17.645952
39.888234	1387.458509	17.650970
39.927915	1368.936535	17.655987
39.642779	1370.910808	17.661005
39.754922	1370.939623	17.666023
39.807962	1362.702579	17.671040
39.216867	1368.591097	17.676058
39.592923	1353.612603	17.681075
39.635037	1364.488316	17.686093
39.409645	1382.548387	17.691111
39.941086	1389.781216	17.696128
40.126346	1393.142703	17.701146
40.008688	1388.615587	17.706163
40.038047	1395.960882	17.711181
40.081802	1393.162955	17.716199
40.340011	1392.921427	17.721216
40.087752	1398.462857	17.726234
39.917437	1397.002941	17.731251
39.932838	1397.847633	17.736269
39.925208	1391.552661	17.741287
39.654188	1399.629445	17.746304
39.559395	1395.621293	17.751322
39.866150	1395.822667	17.756339
40.033006	1410.128544	17.761357
39.981021	1414.618613	17.766375
40.143453	1422.521084	17.771392
40.228913	1434.369433	17.776410
40.486216	1420.636556	17.781427
40.556509	1417.746665	17.786445
40.642827	1418.385085	17.791463
40.678857	1414.825805	17.796480
40.547741	1421.578091	17.801498
40.722967	1417.607899	17.806515
40.414369	1416.290992	17.811533
40.434705	1421.646311	17.816551
41.127790	1434.419325	17.821568
40.867038	1444.037440	17.826586
41.466633	1423.933034	17.831603
41.056506	1422.691019	17.836621
40.961796	1408.804704	17.841639
41.011285	1400.356812	17.846656
40.687679	1415.704751	17.851674
41.056285	1405.147610	17.856691
41.171706	1420.347835	17.861709
40.706699	1418.349012	17.866727
41.442224	1426.757226	17.871744
41.274122	1433.609175	17.876762
41.143112	1442.277392	17.881779
41.602451	1438.094294	17.886797
41.601700	1427.769378	17.891815
41.516429	1402.778771	17.896832
41.515069	1409.199326	17.901850
41.354830	1397.264605	17.906867
41.288051	1402.433258	17.911885
41.459955	1402.699882	17.916903
41.576263	1409.844038	17.921920
41.043935	1429.930997	17.926938
41.841051	1429.251764	17.931955
41.876462	1418.958059	17.936973
41.779334	1423.918909	17.941991
41.991618	1418.942657	17.947008
42.068718	1423.321218	17.952026
41.830264	1405.705240	17.957043
41.593216	1402.582190	17.962061
42.008186	1418.795334	17.967079
42.465129	1423.679301	17.972096
42.306559	1415.926980	17.977114
42.122013	1401.181578	17.982131
42.126941	1393.122075	17.987149
41.652940	1395.636656	17.992167
42.283085	1403.248278	17.997184
41.827424	1403.866222	18.002202
42.154205	1413.048907	18.007219
42.133172	1423.865403	18.012237
42.350025	1434.503705	18.017255
42.025681	1419.481042	18.022272
42.118714	1428.167539	18.027290
42.039791	1425.524117	18.032307
42.138219	1429.073745	18.037325
42.063209	1432.328273	18.042343
42.590009	1418.954351	18.047360
42.163655	1434.623104	18.052378
42.657535	1442.839663	18.057395
42.295626	1455.642376	18.062413
42.361778	1466.060450	18.067431
42.786315	1450.519558	18.072448
42.835510	1460.897224	18.077466
42.648775	1458.577036	18.082483
42.771454	1457.349193	18.087501
42.928854	1461.212372	18.092519
43.065465	1449.903163	18.097536
42.902515	1460.134110	18.102554
43.355840	1449.885281	18.107571
43.353692	1458.460148	18.112589
42.721017	1455.726209	18.117607
43.095363	1445.748430	18.122624
43.098256	1454.675615	18.127642
43.191923	1455.689587	18.132659
42.962007	1441.917377	18.137677
42.847074	1444.925578	18.142695
43.446876	1456.482984	18.147712
43.314790	1468.698612	18.152730
43.289938	1467.399989	18.157747
43.793605	1467.825504	18.162765
43.562806	1464.340310	18.167783
43.996138	1445.707442	18.172800
43.517350	1447.155815	18.177818
43.380154	1444.416465	18.182835
43.321773	1440.535929	18.187853
43.491198	1464.540427	18.192871
43.738926	1464.842089	18.197888
43.997639	1473.595097	18.202906
44.182850	1472.881388	18.207923
44.047960	1461.693529	18.212941
43.533249	1457.633721	18.217959
44.042386	1451.050106	18.222976
43.650277	1457.981421	18.227994
43.923949	1462.608997	18.233011
44.034205	1460.865908	18.238029
43.914241	1468.458908	18.243047
44.114701	1466.058554	18.248064
43.984619	1476.834328	18.253082
43.843799	1470.316465	18.258099
43.949616	1467.466542	18.263117
43.900402	1471.114334	18.268135
44.154869	1466.002082	18.273152
44.137402	1482.283921	18.278170
44.291528	1499.899098	18.283187
44.324113	1499.002085	18.288205
44.605042	1508.938435	18.293223
44.611272	1499.544656	18.298240
44.665162	1508.563139	18.303258
44.699239	1501.091165	18.308275
45.044863	1498.835621	18.313293
44.784556	1505.374242	18.318311
45.094530	1502.950382	18.323328
44.872611	1503.429426	18.328346
45.023085	1501.966080	18.333363
45.126716	1494.758198	18.338381
44.813988	1481.945130	18.343399
44.946294	1491.066313	18.348416
44.919111	1498.894234	18.353434
44.954503	1503.014193	18.358451
45.061508	1494.370149	18.363469
45.102966	1500.168376	18.368487
44.937091	1500.444090	18.373504
44.713631	1504.057584	18.378522
44.715849	1501.860523	18.383539
45.037436	1499.103535	18.388557
45.026820	1504.845725	18.393575
45.486070	1515.995338	18.398592
45.523164	1530.963799	18.403610
45.387341	1535.892731	18.408627
45.688359	1530.417715	18.413645
45.581170	1536.873791	18.418663
45.839955	1532.895544	18.423680
45.742350	1527.067173	18.428698
45.773397	1519.711077	18.433715
45.257830	1513.104280	18.438733
45.250425	1525.009569	18.443751
45.632124	1526.914420	18.448768
45.584542	1534.321402	18.453786
45.398755	1544.627194	18.458803
45.219410	1529.348044	18.463821
45.246127	1542.298002	18.468839
45.778566	1549.325202	18.473856
45.819550	1559.996499	18.478874
45.763820	1564.086028	18.483891
46.014892	1567.158681	18.488909
46.027824	1564.392389	18.493927
46.539177	1557.340189	18.498944
46.436038	1562.454492	18.503962
46.119580	1567.276594	18.508979
46.321353	1562.092234	18.513997
46.158906	1574.114309	18.519015
45.947463	1565.432293	18.524032
46.345385	1572.168753	18.529050
46.487515	1594.218467	18.534067
46.601905	1578.541233	18.539085
46.997567	1581.992292	18.544103
47.323473	1575.893633	18.549120
47.036288	1563.053283	18.554138
46.844221	1550.584866	18.559155
47.254685	1541.998623	18.564173
47.217723	1536.350423	18.569191
46.810526	1543.435165	18.574208
47.233319	1543.499312	18.579226
46.925396	1551.851821	18.584243
47.640637	1547.079881	18.589261
47.076255	1545.537889	18.594279
47.405401	1552.752718	18.599296
47.112956	1547.400705	18.604314
46.707533	1558.031201	18.609331
47.237421	1544.156983	18.614349
47.303570	1551.544474	18.619367
47.196695	1544.258474	18.624384
47.179010	1544.087477	18.629402
47.309401	1549.399558	18.634419
47.372745	1536.264068	18.639437
47.388402	1552.384772	18.644455
47.486204	1556.408997	18.649472
47.858919	1559.945884	18.654490
47.528954	1570.684724	18.659507
47.843835	1556.678442	18.664525
47.362125	1565.415123	18.669543
47.146213	1566.219158	18.674560
47.433271	1578.863065	18.679578
47.364151	1577.825593	18.684595
47.848902	1576.081677	18.689613
47.517940	1578.900145	18.694631
47.818698	1598.440507	18.699648
48.299441	1596.377556	18.704666
48.390307	1606.595007	18.709683
48.170737	1590.881700	18.714701
48.317700	1581.635809	18.719719
48.019753	1578.545607	18.724736
48.224264	1584.560032	18.729754
48.289458	1602.826076	18.734771
48.576783	1595.089354	18.739789
48.041898	1597.920343	18.744807
48.434652	1602.903965	18.749824
48.337542	1597.762961	18.754842
48.095413	1609.836918	18.759859
48.295299	1602.240001	18.764877
48.252787	1611.235697	18.769895
48.258418	1605.626237	18.774912
48.567835	1601.978700	18.779930
48.445485	1620.694681	18.784947
48.634702	1626.866880	18.789965
48.615711	1633.468129	18.794983
48.815955	1640.515707	18.800000
48.812018	1640.132486	18.805018
48.723587	1641.021767	18.810035
48.850880	1636.164754	18.815053
49.091758	1643.181742	18.820071
48.667988	1639.087000	18.825088
48.845709	1633.268085	18.830106
48.781068	1650.377570	18.835123
48.875388	1653.444434	18.840141
49.229458	1662.858442	18.845159
49.278805	1662.300711	18.850176
49.579804	1652.070386	18.855194
49.507674	1656.391124	18.860211
49.657174	1654.811777	18.865229
49.718413	1657.492536	18.870247
49.564746	1664.518115	18.875264
49.887401	1662.873643	18.880282
49.485149	1662.136221	18.885299
49.739055	1659.644382	18.890317
49.790584	1668.088493	18.895335
49.584191	1665.972849	18.900352
49.610224	1661.738377	18.905370
49.697444	1662.295935	18.910387
49.694305	1662.461852	18.915405
49.738218	1656.711150	18.920423
49.933719	1674.781688	18.925440
50.354051	1678.107660	18.930458
50.232934	1692.076509	18.935475
50.134758	1682.155575	18.940493
50.115341	1677.734774	18.945511
50.261953	1683.887919	18.950528
50.732207	1688.297193	18.955546
50.181559	1692.464127	18.960563
50.600135	1674.794654	18.965581
50.610064	1672.263531	18.970599
50.558573	1681.595885	18.975616
50.476015	1679.179841	18.980634
50.294082	1682.359829	18.985651
50.378451	1682.122115	18.990669
50.629387	1686.051607	18.995687
50.638014	1677.340460	19.000704
51.344619	1678.964404	19.005722
51.069303	1678.977749	19.010739
51.353519	1670.525299	19.015757
51.396840	1677.338744	19.020775
51.285260	1679.094694	19.025792
51.336330	1666.656161	19.030810
51.100035	1669.405258	19.035827
50.970115	1668.579802	19.040845
51.362181	1668.702768	19.045863
51.197177	1676.120105	19.050880
51.533688	1674.585868	19.055898
51.335127	1670.829320	19.060915
51.070974	1678.545579	19.065933
51.253134	1673.037342	19.070951
51.288163	1677.709836	19.075968
51.063248	1665.932471	19.080986
51.208626	1679.391392	19.086003
51.130051	1671.099971	19.091021
51.332291	1671.768927	19.096039
51.256548	1702.023234	19.101056
51.612197	1694.029052	19.106074
51.573052	1700.637722	19.111091
51.407905	1701.878782	19.116109
51.522113	1698.949417	19.121127
51.412321	1700.872799	19.126144
51.795496	1717.346067	19.131162
52.154149	1738.528844	19.136179
52.140073	1741.039830	19.141197
51.918014	1731.008593	19.146215
51.854094	1741.749186	19.151232
52.356332	1736.225819	19.156250
52.339404	1734.906915	19.161267
52.350375	1733.195386	19.166285
52.948255	1728.056066	19.171303
52.789212	1722.922488	19.176320
53.124631	1718.252235	19.181338
53.023237	1721.036094	19.186355
52.873757	1720.274626	19.191373
52.998554	1704.181259	19.196391
52.683203	1700.593957	19.201408
52.703222	1693.006178	19.206426
52.476487	1701.406271	19.211443
52.743597	1720.153249	19.216461
52.847826	1715.722263	19.221479
52.576374	1727.460747	19.226496
52.720018	1717.974765	19.231514
53.188305	1725.853302	19.236531
52.685451	1723.766821	19.241549
53.189808	1722.229002	19.246567
52.838461	1726.987835	19.251584
53.068705	1723.912178	19.256602
52.875074	1735.221527	19.261619
52.562080	1751.720475	19.266637
52.944888	1745.417090	19.271655
53.075061	1762.255868	19.276672
53.140037	1762.953480	19.281690
52.932777	1765.661785	19.286707
53.388284	1785.553849	19.291725
53.858222	1777.987329	19.296743
53.362174	1788.761092	19.301760
53.416923	1786.732565	19.306778
53.810751	1774.125719	19.311795
53.739975	1777.671361	19.316813
54.180073	1781.751540	19.321831
54.112573	1780.173947	19.326848
54.086551	1769.775568	19.331866
54.069991	1780.526181	19.336883
54.045089	1780.419812	19.341901
54.227359	1773.310932	19.346919
54.136885	1774.254908	19.351936
54.075970	1761.900074	19.356954
54.290871	1770.563898	19.361971
53.700818	1775.916493	19.366989
54.571636	1776.983884	19.372007
54.537315	1794.026510	19.377024
54.395841	1794.559101	19.382042
54.646858	1799.812393	19.387059
54.624605	1803.524546	19.392077
54.683453	1801.679196	19.397095
54.755697	1797.280052	19.402112
54.933961	1792.564665	19.407130
55.053856	1793.490688	19.412147
54.697507	1793.195838	19.417165
54.967949	1788.837135	19.422183
55.310483	1790.336086	19.427200
55.295400	1793.414253	19.432218
54.854587	1795.937773	19.437235
55.151845	1799.542384	19.442253
55.322084	1794.998866	19.447271
55.255023	1794.514244	19.452288
55.275201	1795.316007	19.457306
55.531026	1789.290313	19.462323
55.540497	1800.240439	19.467341
55.379275	1793.609782	19.472359
55.318655	1792.795670	19.477376
55.485025	1792.675801	19.482394
55.098259	1779.643658	19.487411
54.868699	1787.524926	19.492429
55.512531	1804.204416	19.497447
55.211978	1816.392498	19.502464
54.823295	1815.856704	19.507482
55.235820	1817.602745	19.512499
55.669587	1841.990115	19.517517
55.721396	1842.658882	19.522535
55.953950	1849.995148	19.527552
55.947949	1849.542187	19.532570
56.298592	1847.870061	19.537587
56.038859	1855.270648	19.542605
56.537970	1846.671404	19.547623
56.262533	1856.765970	19.552640
56.333228	1850.239248	19.557658
56.624678	1849.860109	19.562675
56.518140	1860.115508	19.567693
56.327644	1846.687802	19.572711
56.444061	1853.044247	19.577728
56.253355	1850.485674	19.582746
56.278016	1849.770337	19.587763
56.231146	1854.495119	19.592781
56.918477	1864.736872	19.597799
56.755583	1877.102606	19.602816
56.988766	1874.215811	19.607834
56.894245	1871.058386	19.612851
57.326419	1875.489205	19.617869
57.399813	1880.539090	19.622887
57.492684	1867.106490	19.627904
57.051699	1852.458569	19.632922
57.511837	1838.337357	19.637939
57.267422	1842.506165	19.642957
57.254791	1840.430514	19.647975
57.299082	1842.901192	19.652992
57.180094	1842.447915	19.658010
57.446551	1852.925224	19.663027
57.494790	1872.112323	19.668045
57.717297	1874.053962	19.673063
57.639551	1872.812804	19.678080
57.624070	1867.862073	19.683098
57.442819	1866.959569	19.688115
57.721431	1863.976392	19.693133
57.943921	1857.793374	19.698151
57.566361	1855.739731	19.703168
57.700662	1854.661458	19.708186
57.963348	1850.393843	19.713203
57.917332	1860.219916	19.718221
58.265718	1870.442608	19.723239
58.536188	1867.649828	19.728256
58.246524	1857.256823	19.733274
58.208568	1851.033410	19.738291
58.348829	1864.103161	19.743309
58.447099	1876.538308	19.748327
58.574178	1884.165543	19.753344
58.375564	1889.109289	19.758362
58.734909	1877.454852	19.763379
58.783754	1877.181882	19.768397
58.932138	1874.907733	19.773415
58.903387	1874.557110	19.778432
58.966724	1870.068910	19.783450
58.860343	1878.166144	19.788467
58.579906	1873.452987	19.793485
58.790085	1871.378507	19.798503
59.339314	1874.929700	19.803520
58.349939	1875.800600	19.808538
58.867823	1869.298395	19.813555
58.531953	1874.567282	19.818573
58.912866	1874.670900	19.823591
58.983990	1879.004152	19.828608
59.193530	1891.326127	19.833626
59.159864	1895.226110	19.838643
59.212964	1895.219374	19.843661
59.606786	1895.907864	19.848679
59.483609	1897.644564	19.853696
60.060931	1902.111538	19.858714
60.081428	1895.717041	19.863731
59.497973	1896.796338	19.868749
59.964977	1899.135489	19.873767
59.761841	1901.977379	19.878784
59.720406	1908.058115	19.883802
59.846932	1895.264293	19.888819
59.873805	1908.621666	19.893837
60.059929	1894.244194	19.898855
60.070292	1893.613207	19.903872
60.273374	1899.577599	19.908890
60.094280	1888.368662	19.913907
60.495382	1906.642047	19.918925
60.504278	1903.918912	19.923943
60.256744	1900.660138	19.928960
60.248979	1918.544126	19.933978
60.257016	1922.717318	19.938995
60.426744	1931.263370	19.944013
60.104633	1936.620481	19.949031
60.537413	1925.119977	19.954048
60.300615	1933.566413	19.959066
60.447169	1932.467528	19.964083
60.854726	1946.078607	19.969101
61.216219	1942.046818	19.974119
61.328178	1942.375706	19.979136
60.851013	1946.884484	19.984154
61.319531	1949.014301	19.989171
61.153062	1950.005967	19.994189
61.311400	1948.157324	19.999207
61.834218	1944.742055	20.004224
61.489256	1956.264935	20.009242
61.281485	1945.985800	20.014259
61.371295	1949.661057	20.019277
61.303941	1948.498044	20.024295
61.561570	1945.666107	20.029312
61.674219	1946.228373	20.034330
61.652136	1941.528783	20.039347
61.726950	1942.670839	20.044365
61.641885	1951.238141	20.049383
61.506189	1936.932735	20.054400
61.404354	1940.697940	20.059418
61.581572	1949.086792	20.064435
61.666920	1965.759041	20.069453
62.248810	1976.423332	20.074471
62.176894	1972.580422	20.079488
61.967177	1981.232506	20.084506
62.332037	1981.054194	20.089523
62.264601	1977.776734	20.094541
62.444021	1980.592426	20.099559
62.739736	1977.123554	20.104576
62.464819	1975.706715	20.109594
62.402379	1976.048178	20.114611
62.402494	1978.157110	20.119629
62.450900	1976.951017	20.124647
62.387271	1980.693143	20.129664
62.756152	1998.720551	20.134682
63.106212	2000.348960	20.139699
62.922669	1998.914878	20.144717
62.778598	2008.967332	20.149735
63.048063	2007.706406	20.154752
62.683146	2005.182793	20.159770
63.059572	2001.389406	20.164787
62.917138	2009.760642	20.169805
62.915536	2011.274515	20.174823
62.899300	2017.697083	20.179840
62.895418	2035.452962	20.184858
63.618055	2015.579498	20.189875
63.960752	2017.816735	20.194893
64.073745	2015.302931	20.199911
64.528594	2022.809857	20.204928
63.918728	2009.854357	20.209946
64.040179	2004.115434	20.214963
64.059950	1993.067630	20.219981
64.328424	1989.636502	20.224999
63.785206	1989.672150	20.230016
63.942916	1986.860487	20.235034
63.939458	1986.711065	20.240051
64.336907	1997.425104	20.245069
63.950218	1993.677500	20.250087
64.077749	1994.712083	20.255104
64.207409	2013.939341	20.260122
64.067990	2011.347929	20.265139
64.172599	2023.614367	20.270157
64.180696	2025.299043	20.275175
64.278723	2022.760635	20.280192
64.201720	2026.783844	20.285210
64.370520	2039.780336	20.290227
64.746635	2042.217781	20.295245
64.520613	2047.915986	20.300263
64.805543	2045.927895	20.305280
64.752881	2045.998749	20.310298
64.577100	2047.826385	20.315315
64.889748	2046.841950	20.320333
64.892433	2068.235831	20.325351
64.827354	2062.661956	20.330368
64.694298	2073.926907	20.335386
65.113735	2082.020330	20.340403
65.445932	2077.153253	20.345421
65.273839	2082.822537	20.350439
65.152085	2078.879075	20.355456
64.989054	2088.403653	20.360474
65.231326	2100.536297	20.365491
65.633339	2101.783316	20.370509
65.613138	2103.823296	20.375527
65.887793	2097.743855	20.380544
65.602460	2101.070412	20.385562
65.960373	2098.643363	20.390579
66.026257	2095.415079	20.395597
65.657563	2096.365035	20.400615
65.813891	2105.081220	20.405632
66.093545	2114.926825	20.410650
66.613733	2112.481403	20.415667
66.540243	2118.853190	20.420685
66.699826	2124.077774	20.425703
66.848619	2102.971288	20.430720
66.350176	2101.332092	20.435738
66.564405	2090.259150	20.440755
66.787252	2094.742066	20.445773
66.819707	2113.070626	20.450791
67.498790	2101.186379	20.455808
67.106812	2094.730608	20.460826
66.848062	2089.108026	20.465843
67.156980	2082.271429	20.470861
66.790907	2089.636806	20.475879
67.112563	2082.362531	20.480896
66.804361	2085.008656	20.485914
67.140625	2110.110506	20.490931
67.104653	2112.707602	20.495949
66.577524	2124.798133	20.500967
66.917079	2116.938799	20.505984
66.726638	2115.239709	20.511002
67.069034	2135.205952	20.516019
67.285771	2150.546628	20.521037
67.095923	2153.541819	20.526055
67.658431	2150.281931	20.531072
67.706072	2152.636319	20.536090
67.558433	2166.809379	20.541107
68.248525	2172.617930	20.546125
67.966323	2176.470027	20.551143
68.527103	2179.190055	20.556160
68.293734	2171.554133	20.561178
68.080979	2164.337578	20.566195
67.981856	2168.622921	20.571213
68.104989	2180.961908	20.576231
68.008244	2176.209291	20.581248
67.731292	2177.861739	20.586266
67.702052	2178.091200	20.591283
68.497878	2192.662458	20.596301
68.591542	2209.048853	20.601319
68.761806	2203.208562	20.606336
69.078106	2205.014460	20.611354
68.982123	2202.783341	20.616371
69.680883	2195.626279	20.621389
69.602083	2193.896227	20.626407
69.431292	2172.810574	20.631424
69.617046	2166.680984	20.636442
69.280229	2168.395671	20.641459
69.769136	2158.530105	20.646477
69.707662	2163.639035	20.651495
69.203687	2165.413880	20.656512
69.403379	2163.742401	20.661530
69.481724	2159.699249	20.666547
69.483820	2159.446890	20.671565
69.470727	2164.623127	20.676583
69.869766	2152.167865	20.681600
69.709374	2154.650058	20.686618
69.396298	2154.123338	20.691635
70.010798	2151.386898	20.696653
69.638660	2152.907610	20.701671
69.341876	2161.425091	20.706688
69.878385	2178.546675	20.711706
69.343659	2187.429421	20.716723
69.878803	2186.476922	20.721741
70.174695	2209.294962	20.726759
69.977069	2209.524153	20.731776
70.433681	2216.142943	20.736794
70.301227	2227.926483	20.741811
70.413062	2223.816934	20.746829
70.469967	2225.083754	20.751847
70.462256	2217.470549	20.756864
70.786957	2216.143041	20.761882
70.509918	2215.362860	20.766899
70.788688	2214.250345	20.771917
70.612359	2237.840040	20.776935
70.703485	2243.846596	20.781952
71.051025	2242.285215	20.786970
71.015707	2241.810100	20.791987
71.284951	2242.345136	20.797005
71.361963	2240.802572	20.802023
71.408930	2244.338370	20.807040
71.369914	2234.760933	20.812058
71.367625	2229.162059	20.817075
71.613141	2228.881353	20.822093
71.487998	2235.662103	20.827111
71.998302	2251.095090	20.832128
72.038157	2248.302011	20.837146
71.880826	2254.296041	20.842163
72.295783	2249.381646	20.847181
71.985370	2234.583007	20.852199
71.696036	2244.275812	20.857216
72.232437	2254.538189	20.862234
72.336532	2268.231108	20.867251
72.400129	2258.720329	20.872269
72.798112	2271.535181	20.877287
72.554085	2265.491836	20.882304
72.806005	2261.585068	20.887322
72.617886	2270.264320	20.892339
72.779196	2269.045148	20.897357
73.158827	2269.542360	20.902375
72.758483	2252.402854	20.907392
72.965311	2244.560699	20.912410
72.661342	2242.695991	20.917427
72.913377	2249.165589	20.922445
72.381808	2270.196152	20.927463
71.907865	2263.702386	20.932480
72.625906	2265.877279	20.937498
72.324538	2289.006524	20.942515
72.496556	2292.343702	20.947533
73.022948	2302.268403	20.952551
73.292419	2314.932856	20.957568
73.819690	2314.417988	20.962586
73.405835	2325.099271	20.967603
73.559486	2320.779347	20.972621
73.714200	2322.201874	20.977639
73.923957	2315.519994	20.982656
73.983635	2311.787925	20.987674
73.754222	2318.928373	20.992691
74.206116	2308.412264	20.997709
74.711687	2323.355506	21.002727
74.863079	2315.425166	21.007744
74.676572	2309.509760	21.012762
73.874822	2302.201963	21.017779
74.148154	2301.185665	21.022797
74.123776	2305.874832	21.027815
74.307213	2311.576567	21.032832
74.414602	2312.448852	21.037850
74.516958	2320.625506	21.042867
74.536710	2314.722775	21.047885
74.629669	2318.434198	21.052903
74.571999	2332.483306	21.057920
74.879186	2337.242429	21.062938
75.057665	2351.575528	21.067955
74.758171	2350.757450	21.072973
75.338839	2338.724517	21.077991
75.559383	2349.432509	21.083008
75.409228	2340.711989	21.088026
75.185406	2348.170439	21.093043
75.228302	2338.693874	21.098061
75.244914	2338.987929	21.103079
75.481438	2344.506531	21.108096
75.266037	2355.031744	21.113114
75.092207	2370.833360	21.118131
75.491773	2369.747377	21.123149
75.540750	2372.639450	21.128167
75.680074	2380.116773	21.133184
76.012657	2376.614324	21.138202
76.098751	2389.289800	21.143219
76.262992	2395.624092	21.148237
76.116099	2393.630057	21.153255
76.223197	2395.743541	21.158272
76.947836	2390.505101	21.163290
76.886538	2393.584615	21.168307
76.853195	2388.677733	21.173325
76.543657	2398.116573	21.178343
76.476851	2386.682089	21.183360
76.857076	2388.209291	21.188378
76.619317	2390.085787	21.193395
76.950717	2393.653183	21.198413
76.697379	2395.314205	21.203431
76.592648	2395.459745	21.208448
76.455944	2396.410896	21.213466
76.712546	2413.235001	21.218483
77.118747	2414.093076	21.223501
77.086836	2416.288673	21.228519
77.241851	2428.928739	21.233536
77.383363	2424.940842	21.238554
77.260755	2425.954943	21.243571
77.313014	2434.585200	21.248589
77.423598	2436.694155	21.253607
77.214262	2450.175571	21.258624
77.347679	2442.786921	21.263642
77.506623	2447.397449	21.268659
77.964175	2460.296748	21.273677
78.263144	2465.846427	21.278695
78.245345	2476.393759	21.283712
78.610451	2466.784698	21.288730
78.655478	2467.988209	21.293747
78.782540	2468.630320	21.298765
78.619262	2443.818773	21.303783
78.612675	2440.096460	21.308800
78.743103	2436.758598	21.313818
78.757893	2440.611820	21.318835
78.756212	2451.677718	21.323853
78.961911	2456.907896	21.328871
78.938078	2473.401340	21.333888
78.932987	2473.966091	21.338906
78.827965	2463.200418	21.343923
78.723023	2469.260364	21.348941
78.810392	2471.533173	21.353959
78.791574	2471.635633	21.358976
79.081486	2483.875388	21.363994
79.071691	2497.164341	21.369011
78.836096	2493.199339	21.374029
79.131185	2497.276219	21.379047
79.294758	2519.493670	21.384064
79.797177	2533.641456	21.389082
79.492083	2530.425493	21.394099
79.678660	2530.899109	21.399117
80.054565	2523.635019	21.404135
79.830689	2532.606422	21.409152
80.126799	2527.784770	21.414170
80.113619	2527.976831	21.419187
80.102185	2540.231279	21.424205
80.660298	2545.294752	21.429223
80.445314	2550.063921	21.434240
80.507957	2535.927148	21.439258
80.569696	2553.215592	21.444275
80.646847	2550.349125	21.449293
80.758456	2542.595600	21.454311
80.590897	2548.567082	21.459328
80.829964	2547.685800	21.464346
80.905516	2550.919078	21.469363
80.958023	2545.426464	21.474381
80.883227	2548.972181	21.479399
80.859506	2571.210002	21.484416
81.019412	2576.125968	21.489434
80.859634	2574.943707	21.494451
80.871046	2574.484196	21.499469
80.946008	2579.891186	21.504487
80.944596	2600.621026	21.509504
81.308340	2597.719592	21.514522
81.531043	2607.405952	21.519539
81.471728	2611.634188	21.524557
81.882640	2625.833973	21.529575
81.938750	2637.424833	21.534592
82.412137	2632.903525	21.539610
82.192269	2635.796848	21.544627
82.295626	2631.435058	21.549645
82.113177	2622.235580	21.554663
82.209982	2622.845084	21.559680
82.597301	2623.715860	21.564698
82.689682	2625.592487	21.569715
82.518803	2627.318150	21.574733
82.775603	2621.954294	21.579751
82.639575	2627.629009	21.584768
82.849427	2618.581214	21.589786
82.784916	2629.403633	21.594803
82.674163	2649.058388	21.599821
83.021952	2650.035173	21.604839
83.021570	2652.577428	21.609856
83.207538	2651.101987	21.614874
83.376406	2655.072179	21.619891
83.544856	2652.961831	21.624909
83.453204	2648.312152	21.629927
83.126465	2662.852645	21.634944
83.878127	2678.905425	21.639962
83.840692	2683.553628	21.644979
83.581478	2680.512478	21.649997
83.988795	2680.185126	21.655015
84.088292	2686.628292	21.660032
84.009033	2683.343653	21.665050
84.024373	2683.008685	21.670067
83.942668	2687.747171	21.675085
84.701694	2667.867044	21.680103
84.330593	2684.873083	21.685120
84.749215	2682.606436	21.690138
84.629682	2682.950614	21.695155
84.408400	2696.934379	21.700173
84.924822	2708.912603	21.705191
84.644062	2713.415882	21.710208
84.914251	2706.795143	21.715226
85.106616	2704.104207	21.720243
84.886932	2704.315922	21.725261
85.066755	2702.880119	21.730279
85.187640	2708.893565	21.735296
85.410826	2698.990527	21.740314
85.748566	2686.743027	21.745331
86.025190	2685.723779	21.750349
85.773939	2685.960594	21.755367
85.643710	2684.922892	21.760384
86.045476	2683.260031	21.765402
85.968510	2683.055869	21.770419
86.021562	2681.696143	21.775437
86.182025	2671.066734	21.780455
85.909824	2678.106786	21.785472
85.861062	2678.014346	21.790490
86.310739	2674.263371	21.795507
86.328943	2676.463012	21.800525
86.326978	2678.366846	21.805543
86.419484	2680.856167	21.810560
86.442715	2680.715157	21.815578
86.459266	2696.450596	21.820595
86.379102	2706.685881	21.825613
86.837965	2712.360233	21.830631
86.800055	2712.291133	21.835648
86.876779	2712.154340	21.840666
87.448239	2711.257804	21.845683
87.118538	2708.852468	21.850701
87.497814	2699.065215	21.855719
87.379188	2709.861528	21.860736
87.491040	2697.269211	21.865754
87.387790	2693.722494	21.870771
87.131724	2701.251217	21.875789
87.773305	2703.143955	21.880807
87.507793	2720.669036	21.885824
87.324955	2730.914851	21.890842
87.492310	2723.595856	21.895859
87.641437	2736.379726	21.900877
87.774292	2729.215489	21.905895
87.469479	2742.337076	21.910912
87.844108	2757.018092	21.915930
88.077928	2753.550606	21.920947
88.111593	2760.301994	21.925965
88.367073	2768.941697	21.930983
88.514680	2790.425912	21.936000
88.523073	2794.541784	21.941018
88.408128	2795.442762	21.946035
88.461059	2798.743761	21.951053
88.615038	2784.034310	21.956071
89.002245	2804.760799	21.961088
89.260478	2816.746355	21.966106
89.513955	2807.958739	21.971123
89.299387	2826.949496	21.976141
89.732862	2815.306074	21.981159
90.095689	2810.305152	21.986176
89.863146	2809.844929	21.991194
90.345766	2794.086814	21.996211
89.546294	2784.014099	22.001229
89.739616	2774.124009	22.006247
89.905946	2785.467694	22.011264
90.051901	2797.625269	22.016282
90.103877	2795.019814	22.021299
89.941233	2805.520532	22.026317
89.941490	2797.983647	22.031335
90.208068	2807.557865	22.036352
89.936700	2812.046961	22.041370
90.529933	2801.677192	22.046387
90.505119	2798.551731	22.051405
90.808632	2802.366569	22.056423
90.731458	2808.228147	22.061440
90.414015	2807.225683	22.066458
90.692126	2820.270238	22.071475
90.895051	2829.406479	22.076493
90.922611	2833.259183	22.081511
91.331876	2827.447780	22.086528
90.957175	2829.583281	22.091546
91.350716	2830.168698	22.096563
91.301849	2833.910071	22.101581
91.133705	2832.599279	22.106599
91.384628	2847.670161	22.111616
91.483396	2863.218411	22.116634
91.458473	2855.462150	22.121651
90.928792	2866.191218	22.126669
91.419755	2882.400735	22.131687
91.662919	2887.806560	22.136704
91.479185	2890.451167	22.141722
91.782048	2902.288165	22.146739
91.982411	2916.107694	22.151757
92.483839	2912.788823	22.156775
92.878280	2913.455994	22.161792
92.845898	2910.604302	22.166810
93.049447	2900.732856	22.171827
93.011168	2904.259791	22.176845
93.159523	2900.635240	22.181863
93.577586	2898.447415	22.186880
93.242213	2898.863253	22.191898
93.682899	2892.136814	22.196915
93.472396	2895.686973	22.201933
93.606692	2888.902805	22.206951
93.866560	2887.710006	22.211968
93.481116	2894.122987	22.216986
93.488632	2889.655486	22.222003
93.591220	2887.108281	22.227021
93.552773	2886.570678	22.232039
93.659950	2886.023073	22.237056
93.931785	2880.127317	22.242074
93.882365	2880.069640	22.247091
94.405718	2894.540213	22.252109
94.143164	2907.568062	22.257127
94.129017	2914.019778	22.262144
93.969248	2927.354495	22.267162
94.274102	2924.829312	22.272179
94.440700	2914.669646	22.277197
94.426805	2917.382798	22.282215
94.677120	2935.620628	22.287232
94.651860	2943.721829	22.292250
95.111429	2944.203787	22.297267
94.917926	2953.010347	22.302285
94.903726	2956.025192	22.307303
95.051298	2953.110351	22.312320
94.599132	2958.930740	22.317338
95.149140	2956.041413	22.322355
95.138172	2969.827127	22.327373
95.484359	2986.059210	22.332391
95.931371	2975.351332	22.337408
95.851055	2979.257218	22.342426
95.822268	2972.077267	22.347443
95.957702	2969.807939	22.352461
95.502734	2971.876101	22.357479
96.041156	2981.429812	22.362496
96.020741	2997.537316	22.367514
96.243190	2998.845124	22.372531
96.120032	3006.748137	22.377549
96.249959	3004.668762	22.382567
96.799816	3004.415415	22.387584
96.495641	3008.873175	22.392602
96.615194	3014.038765	22.397619
96.667646	3027.341121	22.402637
96.640838	3026.596752	22.407655
96.888279	3026.651207	22.412672
96.779553	3038.427347	22.417690
96.782097	3049.166891	22.422707
97.215367	3054.490566	22.427725
97.325174	3070.267096	22.432743
97.430941	3063.864199	22.437760
97.405004	3064.517603	22.442778
97.378028	3060.189065	22.447795
97.661603	3079.523160	22.452813
97.766958	3081.740208	22.457831
97.983090	3084.308420	22.462848
98.164706	3095.526849	22.467866
98.209714	3081.578474	22.472883
98.077438	3084.428509	22.477901
98.018654	3094.718661	22.482919
98.486306	3103.591522	22.487936
98.435736	3118.704114	22.492954
98.946088	3106.848832	22.497971
98.833085	3122.224939	22.502989
98.950974	3118.403156	22.508007
99.062942	3109.961747	22.513024
99.244069	3121.284237	22.518042
99.459746	3107.916943	22.523059
99.440899	3113.335474	22.528077
99.403511	3118.707570	22.533095
99.522993	3113.750634	22.538112
99.709849	3108.397817	22.543130
99.536399	3112.715848	22.548147
99.897793	3138.056034	22.553165
99.849591	3148.301091	22.558183
99.948085	3141.729295	22.563200
99.493235	3151.596730	22.568218
99.339186	3143.467105	22.573235
100.062660	3155.011668	22.578253
100.098953	3169.617975	22.583271
100.483915	3171.722521	22.588288
100.272553	3178.001812	22.593306
100.814223	3168.427426	22.598323
100.906506	3173.185846	22.603341
100.613217	3181.285077	22.608359
101.089717	3176.922172	22.613376
100.774350	3181.058996	22.618394
100.562889	3176.934531	22.623411
100.971944	3184.425852	22.628429
100.894729	3202.654775	22.633447
101.289917	3196.623557	22.638464
101.139568	3198.234714	22.643482
101.549599	3218.159242	22.648499
102.160263	3224.768594	22.653517
101.821828	3228.999168	22.658535
102.080887	3224.572719	22.663552
101.789605	3235.543116	22.668570
101.942266	3232.600574	22.673587
101.947407	3223.577289	22.678605
101.883734	3227.683576	22.683623
101.918542	3228.870784	22.688640
102.243838	3239.523623	22.693658
102.122166	3244.369149	22.698675
102.316808	3250.726929	22.703693
101.976202	3253.129927	22.708711
103.021679	3259.667115	22.713728
102.820756	3274.905654	22.718746
102.886274	3277.209891	22.723763
103.304191	3274.959823	22.728781
103.366888	3268.108223	22.733799
103.451612	3280.164833	22.738816
103.698593	3274.377152	22.743834
103.548076	3283.912119	22.748851
103.827296	3299.307790	22.753869
103.677626	3303.722606	22.758887
104.025549	3293.048828	22.763904
103.905539	3304.808200	22.768922
103.942754	3303.627552	22.773939
104.326282	3292.890177	22.778957
103.924367	3297.521501	22.783975
104.461794	3305.746156	22.788992
104.753260	3326.733898	22.794010
104.538249	3328.139570	22.799027
104.757944	3323.085843	22.804045
104.738522	3337.847560	22.809063
105.014756	3324.514593	22.814080
105.240327	3330.703288	22.819098
105.222050	3330.620580	22.824115
105.283073	3329.183037	22.829133
105.416810	3329.335744	22.834151
105.763333	3325.105343	22.839168
105.558198	3325.776876	22.844186
105.723382	3323.211783	22.849203
105.747475	3318.571202	22.854221
105.125338	3329.896087	22.859239
105.466236	3337.544868	22.864256
105.561531	3346.377744	22.869274
105.715537	3344.758867	22.874291
106.236957	3358.538710	22.879309
106.063780	3378.580751	22.884327
105.893035	3381.508316	22.889344
106.015489	3386.445134	22.894362
106.195554	3391.392555	22.899379
106.270464	3400.414824	22.904397
106.512962	3414.855270	22.909415
106.640856	3412.190231	22.914432
106.916492	3418.315247	22.919450
107.020848	3442.520982	22.924467
107.153393	3447.039459	22.929485
106.860413	3450.976406	22.934503
107.226687	3444.165620	22.939520
107.467287	3445.015133	22.944538
107.327968	3455.168110	22.949555
108.023404	3459.041935	22.954573
107.990017	3474.017244	22.959591
108.462713	3460.099963	22.964608
108.678735	3457.420596	22.969626
108.775490	3452.372153	22.974643
109.092957	3452.521717	22.979661
109.041926	3439.707856	22.984679
108.761926	3426.370926	22.989696
108.816991	3425.808610	22.994714
108.980888	3419.601950	22.999731
109.564529	3410.595157	23.004749
108.891091	3427.356119	23.009767
109.463979	3411.776448	23.014784
109.196854	3426.898895	23.019802
109.170339	3435.779481	23.024819
109.238567	3440.535806	23.029837
109.125927	3454.393717	23.034855
109.103481	3456.790244	23.039872
109.606225	3452.192793	23.044890
109.485337	3471.992077	23.049907
109.418722	3480.551928	23.054925
109.099246	3486.413554	23.059943
109.488602	3492.764830	23.064960
109.670468	3510.018769	23.069978
109.371356	3516.844857	23.074995
109.904429	3527.694610	23.080013
109.893727	3542.996882	23.085031
110.141884	3538.799040	23.090048
110.644512	3566.200445	23.095066
110.842189	3570.374642	23.100083
111.168693	3553.320177	23.105101
111.222979	3559.056323	23.110119
111.599736	3556.684109	23.115136
111.892659	3549.738574	23.120154
111.873840	3555.593576	23.125171
112.260106	3550.965659	23.130189
111.888976	3552.577684	23.135207
112.161352	3547.665284	23.140224
112.215572	3553.021822	23.145242
112.248136	3548.978288	23.150259
112.558992	3549.881132	23.155277
112.325477	3552.446172	23.160295
112.304847	3546.973624	23.165312
112.664638	3543.448144	23.170330
112.170675	3552.404994	23.175347
112.815862	3551.057093	23.180365
112.642768	3548.259336	23.185383
112.312875	3556.144509	23.190400
112.569749	3554.413466	23.195418
112.371112	3574.327018	23.200435
112.767566	3579.369717	23.205453
112.683571	3592.355704	23.210471
112.362679	3598.434989	23.215488
113.190496	3607.707921	23.220506
112.867500	3622.091135	23.225523
113.265838	3633.873727	23.230541
113.599584	3638.152993	23.235559
114.476512	3621.634166	23.240576
114.559378	3620.525215	23.245594
114.672048	3617.751702	23.250611
115.215960	3612.524951	23.255629
114.805465	3616.687646	23.260647
115.017395	3617.181367	23.265664
114.961199	3610.590215	23.270682
115.134002	3623.837002	23.275699
115.324292	3616.986217	23.280717
115.227978	3611.058005	23.285735
115.301421	3609.036278	23.290752
115.970254	3609.615490	23.295770
115.240347	3587.657413	23.300787
115.261847	3593.022725	23.305805
115.277411	3605.943612	23.310823
115.637677	3609.701666	23.315840
115.750098	3605.227004	23.320858
115.723790	3615.071665	23.325875
115.789580	3608.977048	23.330893
116.370046	3623.202229	23.335911
115.773719	3635.497943	23.340928
116.051177	3634.886468	23.345946
115.853477	3641.862194	23.350963
115.754644	3643.589790	23.355981
115.705621	3657.949696	23.360999
115.922955	3680.319454	23.366016
116.071625	3689.678936	23.371034
116.013799	3703.785212	23.376051
116.737246	3720.917397	23.381069
116.680143	3738.406302	23.386087
116.726599	3738.418820	23.391104
116.929563	3741.468257	23.396122
117.033303	3760.062964	23.401139
117.005498	3764.180569	23.406157
117.279288	3773.767531	23.411175
117.512356	3794.206714	23.416192
118.106173	3782.456336	23.421210
118.212038	3790.795400	23.426227
118.150212	3786.978275	23.431245
118.370384	3790.340599	23.436263
118.459034	3793.582915	23.441280
118.373990	3786.247629	23.446298
118.812414	3814.386640	23.451315
119.143639	3803.153824	23.456333
119.104975	3808.053813	23.461351
118.621159	3805.447895	23.466368
119.115918	3806.596463	23.471386
119.140905	3818.671603	23.476403
119.234893	3815.265665	23.481421
119.160122	3823.225373	23.486439
119.189022	3845.682802	23.491456
119.549473	3845.975434	23.496474
119.251628	3856.770963	23.501491
119.672256	3864.866293	23.506509
120.208196	3878.138464	23.511527
119.930716	3883.021922	23.516544
120.256277	3883.092132	23.521562
120.310038	3884.031983	23.526579
120.010518	3884.410978	23.531597
120.685173	3907.058655	23.536615
120.225248	3916.697453	23.541632
120.950277	3909.393359	23.546650
120.927276	3915.824950	23.551667
120.967524	3929.084479	23.556685
121.451445	3932.112567	23.561703
121.588694	3937.997663	23.566720
121.990625	3929.176888	23.571738
122.226931	3930.649374	23.576755
122.113638	3925.815575	23.581773
122.439060	3928.023371	23.586791
122.334067	3927.563299	23.591808
122.420986	3914.883711	23.596826
122.369269	3927.086286	23.601843
122.361341	3922.514813	23.606861
122.520852	3918.176123	23.611879
122.367921	3915.194482	23.616896
122.442011	3911.876995	23.621914
122.659455	3937.451864	23.626931
122.527923	3951.937233	23.631949
123.020404	3951.117975	23.636967
122.722878	3960.941612	23.641984
122.980187	3962.093882	23.647002
123.412794	3992.668703	23.652019
123.343697	3992.508855	23.657037
123.614011	3982.592210	23.662055
123.285245	3991.616286	23.667072
123.349049	4005.804370	23.672090
123.803257	4020.283113	23.677107
124.090794	4018.971287	23.682125
124.748295	4019.342168	23.687143
123.551459	4021.834568	23.692160
123.881759	4030.087240	23.697178
124.524259	4050.787362	23.702195
124.398601	4044.217388	23.707213
124.817396	4047.753647	23.712231
124.635711	4048.999296	23.717248
124.885573	4068.634954	23.722266
124.948893	4075.562185	23.727283
124.943949	4081.498489	23.732301
125.176016	4089.240331	23.737319
125.277971	4094.714889	23.742336
125.702359	4086.262719	23.747354
125.686719	4099.931292	23.752371
125.758967	4096.529021	23.757389
125.775753	4096.087447	23.762407
125.960979	4118.512951	23.767424
126.668804	4121.481427	23.772442
126.820587	4116.704518	23.777459
126.848142	4113.379215	23.782477
127.302908	4115.672768	23.787495
127.227110	4114.949347	23.792512
127.052537	4113.250465	23.797530
127.151043	4120.915192	23.802547
127.358595	4112.554526	23.807565
127.382431	4102.390218	23.812583
126.942952	4116.362235	23.817600
127.632014	4126.337403	23.822618
127.789112	4129.340433	23.827635
127.773774	4127.998608	23.832653
128.091289	4129.250048	23.837671
128.154767	4136.259191	23.842688
127.966467	4131.211354	23.847706
128.195097	4143.366036	23.852723
128.050583	4158.006617	23.857741
128.601775	4161.483975	23.862759
128.448480	4169.120219	23.867776
128.844334	4169.691908	23.872794
128.851351	4179.732838	23.877811
128.723994	4191.725688	23.882829
129.094264	4193.321730	23.887847
128.882456	4200.864054	23.892864
129.097030	4206.332733	23.897882
129.174813	4224.609513	23.902899
129.395637	4232.443929	23.907917
130.080517	4215.349370	23.912935
129.941026	4231.332838	23.917952
130.070902	4237.204345	23.922970
130.427300	4240.155903	23.927987
130.388063	4251.197210	23.933005
130.655076	4248.857887	23.938023
130.217486	4250.360866	23.943040
130.570236	4245.726681	23.948058
130.867691	4249.075068	23.953075
130.662869	4278.650747	23.958093
131.289756	4279.549080	23.963111
131.440164	4283.577985	23.968128
131.920846	4271.410300	23.973146
131.680302	4274.832018	23.978163
131.602278	4272.200562	23.983181
131.645630	4266.529342	23.988199
131.815142	4281.272153	23.993216
131.896123	4277.594253	23.998234
132.132158	4283.175848	24.003251
131.837288	4302.863438	24.008269
132.273769	4296.901915	24.013287
132.034018	4310.635081	24.018304
132.351672	4305.609932	24.023322
132.026837	4324.005468	24.028339
132.101390	4335.184851	24.033357
132.499726	4349.438764	24.038375
132.909907	4367.497263	24.043392
132.971732	4362.141043	24.048410
133.262324	4377.494076	24.053427
133.023705	4397.025641	24.058445
133.490324	4395.457035	24.063463
133.583376	4403.715919	24.068480
133.561364	4404.171009	24.073498
134.018125	4424.098508	24.078515
133.638982	4427.864584	24.083533
134.154011	4433.228277	24.088551
134.175573	4439.783975	24.093568
134.500435	4457.906824	24.098586
134.894916	4461.860066	24.103603
134.744684	4469.804680	24.108621
134.891063	4457.873743	24.113639
134.969544	4485.332919	24.118656
134.947238	4489.749858	24.123674
135.599615	4488.033618	24.128691
135.460519	4494.936660	24.133709
135.698403	4486.530429	24.138727
135.684494	4496.296325	24.143744
135.987828	4512.338847	24.148762
136.090702	4514.833772	24.153779
135.868383	4529.971642	24.158797
136.261136	4513.359255	24.163815
136.209994	4520.528416	24.168832
136.131952	4541.910353	24.173850
136.668206	4534.316984	24.178867
136.482708	4537.482792	24.183885
136.529912	4557.000210	24.188903
136.422787	4572.870566	24.193920
136.762585	4581.643316	24.198938
137.437751	4602.340928	24.203955
136.891708	4608.380429	24.208973
137.661631	4600.009742	24.213991
137.756548	4616.800125	24.219008
137.625410	4639.149065	24.224026
137.768382	4637.342129	24.229043
138.087011	4639.811901	24.234061
138.336959	4637.439217	24.239079
138.364358	4636.911532	24.244096
138.412456	4649.957655	24.249114
138.591019	4650.997455	24.254131
138.929174	4673.781111	24.259149
138.991043	4665.963398	24.264167
139.107747	4665.257361	24.269184
139.087909	4672.811106	24.274202
139.433746	4681.716776	24.279219
139.624602	4685.882201	24.284237
139.761386	4690.894162	24.289255
139.733367	4696.770853	24.294272
139.710600	4695.330223	24.299290
140.178342	4701.364524	24.304307
139.772045	4720.343948	24.309325
140.274991	4722.935727	24.314343
140.560548	4718.589389	24.319360
140.435382	4728.848663	24.324378
140.918250	4740.115077	24.329395
141.163968	4745.597509	24.334413
141.395387	4742.039427	24.339431
141.598622	4741.205132	24.344448
141.535643	4745.037592	24.349466
141.808653	4732.358531	24.354483
141.756881	4748.316455	24.359501
141.864326	4746.770007	24.364519
141.793588	4732.612388	24.369536
141.663259	4739.657385	24.374554
141.836022	4753.968450	24.379571
142.240365	4765.394058	24.384589
142.153867	4765.360845	24.389607
142.619387	4787.885751	24.394624
142.318735	4796.317088	24.399642
142.725294	4789.354686	24.404659
142.680936	4796.477124	24.409677
143.100133	4810.668805	24.414695
143.578776	4824.029577	24.419712
143.492501	4819.178270	24.424730
144.076757	4814.534955	24.429747
143.725998	4822.118720	24.434765
143.895561	4812.174723	24.439783
144.128886	4818.369764	24.444800
144.541810	4839.511983	24.449818
144.646808	4840.395849	24.454835
144.639280	4841.132023	24.459853
144.567861	4840.479494	24.464871
145.014315	4839.126183	24.469888
144.515854	4841.963690	24.474906
145.003708	4834.178414	24.479923
144.900207	4858.784270	24.484941
144.847480	4868.192367	24.489959
145.223811	4876.172154	24.494976
144.985932	4881.444528	24.499994
145.483080	4891.883931	24.505011
145.359012	4910.070079	24.510029
145.611454	4908.092330	24.515047
146.068373	4914.718522	24.520064
146.254096	4927.790904	24.525082
146.504579	4931.823299	24.530099
146.354395	4940.959863	24.535117
146.119351	4933.136994	24.540135
146.667263	4946.311135	24.545152
146.775607	4967.395466	24.550170
147.074468	4965.619269	24.555187
147.237242	4971.404281	24.560205
146.802597	4969.819202	24.565223
147.134745	4993.093483	24.570240
147.089073	4999.167865	24.575258
147.584378	5017.046318	24.580275
147.794300	5024.643549	24.585293
148.351033	5015.025309	24.590311
148.329198	5010.730011	24.595328
148.641162	5022.529241	24.600346
148.696736	5012.580241	24.605363
148.431389	5020.759895	24.610381
148.471325	5040.739936	24.615399
149.584246	5036.046101	24.620416
149.227211	5044.806238	24.625434
149.614816	5039.397881	24.630451
149.488354	5045.052916	24.635469
149.606848	5062.596672	24.640487
150.045955	5074.315070	24.645504
149.877910	5089.878170	24.650522
150.152820	5075.300243	24.655539
149.972438	5070.850946	24.660557
149.918502	5087.205775	24.665575
150.266742	5102.101451	24.670592
150.411477	5107.235056	24.675610
150.541279	5107.166338	24.680627
150.483409	5127.082912	24.685645
150.780419	5131.798952	24.690663
150.651861	5139.188819	24.695680
150.679788	5169.689572	24.700698
151.062935	5171.521387	24.705715
151.236520	5188.441458	24.710733
151.417383	5210.805455	24.715751
152.117700	5205.960969	24.720768
151.873935	5215.337430	24.725786
152.103531	5234.716505	24.730803
152.101522	5234.447471	24.735821
152.204037	5233.182233	24.740839
152.643354	5254.830105	24.745856
152.877739	5260.076782	24.750874
152.775872	5267.647236	24.755891
153.327086	5270.894055	24.760909
154.028641	5268.982629	24.765927
154.264349	5250.636738	24.770944
154.072675	5247.296005	24.775962
154.514074	5243.404865	24.780979
154.380466	5242.450274	24.785997
154.266549	5238.848885	24.791015
154.540007	5238.955609	24.796032
154.162645	5245.551670	24.801050
154.655144	5252.840638	24.806067
154.800432	5260.020569	24.811085
155.031396	5268.697360	24.816103
155.193137	5265.822991	24.821120
155.536742	5261.047515	24.826138
155.343426	5253.157471	24.831155
155.484445	5260.409812	24.836173
155.252327	5263.167863	24.841191
155.528746	5270.306415	24.846208
155.318862	5290.397336	24.851226
155.632036	5298.463781	24.856243
156.005647	5307.244530	24.861261
155.897315	5330.204917	24.866279
156.385286	5325.809539	24.871296
156.599342	5331.478768	24.876314
157.206726	5341.601832	24.881331
157.239368	5346.247468	24.886349
156.814088	5355.065946	24.891367
157.546897	5339.248247	24.896384
157.611307	5350.939713	24.901402
157.331302	5346.442039	24.906419
157.517204	5359.743173	24.911437
157.583070	5369.709391	24.916455
157.880750	5378.707992	24.921472
157.900703	5388.025169	24.926490
158.372795	5401.460020	24.931507
158.561136	5407.229782	24.936525
158.542447	5406.323222	24.941543
158.743985	5402.173844	24.946560
158.552623	5421.704866	24.951578
158.940066	5427.289269	24.956595
159.320993	5425.155527	24.961613
159.229985	5444.257417	24.966631
159.563149	5454.035296	24.971648
159.475509	5456.037645	24.976666
159.699929	5461.523190	24.981683
159.588034	5467.648487	24.986701
159.762495	5493.330910	24.991719
159.756701	5504.073549	24.996736
160.125923	5519.197599	25.001754
160.228910	5533.218858	25.006771
160.458249	5546.927026	25.011789
160.554916	5559.329122	25.016807
160.896984	5572.574520	25.021824
161.079616	5582.839868	25.026842
160.907876	5584.631371	25.031859
161.426268	5603.581725	25.036877
161.659934	5616.654334	25.041895
161.863975	5614.955762	25.046912
162.319540	5621.780196	25.051930
162.164246	5631.759283	25.056947
162.626917	5650.850790	25.061965
162.363131	5649.756225	25.066983
162.784365	5645.581727	25.072000
162.902505	5653.760556	25.077018
163.168156	5650.842313	25.082035
163.397271	5667.295727	25.087053
163.197518	5672.662649	25.092071
163.414090	5668.614601	25.097088
163.406122	5677.853238	25.102106
163.445042	5687.225628	25.107123
163.868042	5699.092187	25.112141
163.738756	5710.450055	25.117159
163.952342	5721.483702	25.122176
164.309201	5735.201681	25.127194
164.073611	5740.963890	25.132211
164.488558	5756.077966	25.137229
164.373251	5770.407034	25.142247
164.883077	5767.323245	25.147264
164.881523	5797.233968	25.152282
164.972432	5805.248188	25.157299
165.245102	5820.971187	25.162317
165.663368	5835.219875	25.167335
165.546158	5844.912934	25.172352
165.952472	5844.482521	25.177370
166.208474	5856.671637	25.182387
166.694263	5862.345677	25.187405
166.653199	5863.510643	25.192423
166.746964	5873.916657	25.197440
166.785910	5892.046837	25.202458
167.063061	5902.904296	25.207475
167.464715	5902.022539	25.212493
167.359562	5906.721893	25.217511
167.647762	5913.315989	25.222528
168.178150	5915.241596	25.227546
167.948901	5923.384014	25.232563
168.351923	5922.191666	25.237581
168.181071	5928.065727	25.242599
168.175088	5946.773182	25.247616
168.592621	5954.147009	25.252634
168.555901	5953.206486	25.257651
169.124363	5958.549731	25.262669
169.144471	5984.270433	25.267687
169.295768	5987.643461	25.272704
169.300825	5985.945090	25.277722
169.321031	6004.640246	25.282739
169.462480	6007.740844	25.287757
169.603816	6019.969434	25.292775
169.565306	6023.180443	25.297792
170.173776	6045.325800	25.302810
170.065236	6054.674058	25.307827
170.432068	6061.937682	25.312845
170.289139	6076.205591	25.317863
171.211507	6062.616998	25.322880
171.809776	6067.916574	25.327898
171.866281	6067.282237	25.332915
172.487287	6051.251419	25.337933
172.429191	6045.270055	25.342951
172.284501	6037.090072	25.347968
172.730639	6036.807220	25.352986
172.128856	6044.277050	25.358003
172.835651	6037.262643	25.363021
172.543639	6039.081114	25.368039
172.717344	6034.260489	25.373056
173.021738	6043.843587	25.378074
172.989296	6067.611246	25.383091
173.052901	6061.499523	25.388109
173.296298	6066.410934	25.393127
173.529282	6070.626220	25.398144
173.518819	6076.767446	25.403162
173.688948	6095.121136	25.408179
174.362061	6081.565802	25.413197
174.342576	6092.419889	25.418215
174.359980	6089.129785	25.423232
175.002100	6103.983116	25.428250
174.498466	6120.444451	25.433267
174.882800	6125.037116	25.438285
174.854596	6127.027784	25.443303
174.952051	6130.091836	25.448320
175.420380	6141.304243	25.453338
175.216597	6157.394402	25.458355
175.648270	6161.763917	25.463373
175.621046	6171.227490	25.468391
175.807495	6186.451252	25.473408
175.928857	6193.761742	25.478426
175.881858	6204.873479	25.483443
176.088614	6213.803068	25.488461
176.304616	6233.836349	25.493479
176.335542	6250.847386	25.498496
176.685337	6265.390203	25.503514
176.699124	6284.535788	25.508531
177.322262	6287.055242	25.513549
177.189875	6309.496539	25.518567
177.414585	6310.898771	25.523584
177.896312	6321.176344	25.528602
178.038281	6354.052135	25.533619
178.202436	6351.552117	25.538637
178.360706	6349.972385	25.543655
178.263094	6368.668470	25.548672
178.558044	6372.421059	25.553690
178.902325	6384.289023	25.558707
179.211457	6400.947680	25.563725
179.089542	6404.640185	25.568743
179.623544	6407.542020	25.573760
179.718996	6426.121578	25.578778
179.947985	6442.481288	25.583795
179.560442	6435.464458	25.588813
180.002460	6460.328238	25.593831
180.469779	6470.533543	25.598848
180.086411	6470.785957	25.603866
180.396204	6487.565902	25.608883
180.744640	6495.063685	25.613901
180.805000	6504.910246	25.618919
181.235090	6512.339687	25.623936
181.381052	6519.334954	25.628954
181.769233	6536.359103	25.633971
181.818669	6529.804559	25.638989
181.881895	6536.588725	25.644007
181.992943	6557.614043	25.649024
182.752371	6557.454722	25.654042
182.614738	6555.845344	25.659059
182.925167	6556.151344	25.664077
183.439866	6561.766328	25.669095
183.523072	6579.707735	25.674112
183.716903	6572.722738	25.679130
183.693748	6579.219238	25.684148
183.925345	6575.958488	25.689165
183.855676	6582.546463	25.694183
183.911544	6587.362569	25.699200
184.161481	6587.348877	25.704218
184.072886	6612.374748	25.709236
184.370793	6615.022479	25.714253
184.774523	6629.612313	25.719271
184.843401	6636.952484	25.724288
184.941911	6636.347162	25.729306
185.096888	6645.684466	25.734324
186.145144	6645.112487	25.739341
185.942188	6646.333619	25.744359
186.314069	6651.919551	25.749376
186.550399	6641.653389	25.754394
186.597418	6644.522161	25.759412
186.702938	6650.253007	25.764429
187.030015	6645.661924	25.769447
187.059130	6651.824158	25.774464
187.635306	6673.886915	25.779482
187.160867	6676.770244	25.784500
187.342269	6674.705992	25.789517
187.664128	6673.864659	25.794535
187.438766	6692.234840	25.799552
187.969269	6693.920267	25.804570
188.281243	6699.418805	25.809588
188.508167	6694.291094	25.814605
189.133595	6699.804435	25.819623
188.716297	6701.208045	25.824640
189.264213	6715.547948	25.829658
189.233667	6726.041212	25.834676
189.285385	6730.430328	25.839693
189.606331	6730.657330	25.844711
189.948420	6737.723057	25.849728
189.838303	6751.043013	25.854746
189.788716	6769.111379	25.859764
189.961089	6775.452342	25.864781
190.079356	6779.470851	25.869799
190.237878	6794.161951	25.874816
190.124653	6800.352580	25.879834
189.855301	6817.543308	25.884852
190.247611	6827.541920	25.889869
190.656070	6853.065899	25.894887
190.292333	6869.610364	25.899904
190.719474	6884.745482	25.904922
190.813961	6910.877162	25.909940
191.131452	6924.341383	25.914957
191.160591	6940.065483	25.919975
191.477242	6966.801979	25.924992
191.965612	6980.195205	25.930010
192.188562	6990.693241	25.935028
192.580144	7012.680974	25.940045
192.789093	7013.681065	25.945063
193.556794	7004.260231	25.950080
194.357362	7004.555485	25.955098
194.427486	7001.534235	25.960116
194.641422	6990.821880	25.965133
195.000093	6982.376306	25.970151
194.914840	6990.014048	25.975168
194.636779	6983.435894	25.980186
195.033462	7008.902271	25.985204
195.168535	7020.894800	25.990221
195.226710	7016.943678	25.995239
195.049293	7033.363418	26.000256
195.321322	7025.177666	26.005274
195.511587	7042.013346	26.010292
196.113535	7046.988068	26.015309
196.115663	7058.047862	26.020327
195.769578	7065.586979	26.025344
196.299145	7085.846447	26.030362
196.286261	7095.655511	26.035380
195.986313	7108.157520	26.040397
196.349329	7116.811110	26.045415
196.093847	7152.485485	26.050432
196.553898	7159.532755	26.055450
197.438857	7183.161358	26.060468
197.596063	7188.339191	26.065485
197.409911	7203.914541	26.070503
197.570829	7216.906403	26.075520
198.203959	7225.360136	26.080538
198.371362	7248.523373	26.085556
198.826124	7246.636706	26.090573
199.243502	7266.518598	26.095591
199.563897	7263.930212	26.100608
199.811211	7270.004864	26.105626
200.452174	7260.683597	26.110644
200.552493	7264.071150	26.115661
200.597258	7264.281694	26.120679
200.744334	7263.215844	26.125696
200.971145	7269.322370	26.130714
200.563775	7262.836376	26.135732
200.351623	7277.006144	26.140749
200.865498	7281.388666	26.145767
200.746607	7286.875398	26.150784
200.660879	7303.547540	26.155802
201.030165	7317.112715	26.160820
201.398904	7325.429847	26.165837
201.583469	7344.193716	26.170855
200.991726	7360.613125	26.175872
202.007558	7363.722450	26.180890
202.519104	7376.600771	26.185908
203.099702	7384.207281	26.190925
203.542529	7375.465053	26.195943
203.402100	7379.346082	26.200960
203.632103	7383.982114	26.205978
204.061361	7396.761117	26.210996
203.958278	7405.168621	26.216013
204.713531	7395.966334	26.221031
204.128055	7399.993767	26.226048
203.954101	7405.394657	26.231066
204.557201	7411.870014	26.236084
203.969851	7427.058228	26.241101
204.322677	7435.977644	26.246119
204.992856	7460.327269	26.251136
204.744416	7470.116280	26.256154
204.728304	7493.933676	26.261172
205.000316	7508.835223	26.266189
205.460731	7521.447489	26.271207
205.662500	7543.108474	26.276224
205.594176	7555.163841	26.281242
206.138521	7570.838848	26.286260
205.903598	7603.181518	26.291277
206.614531	7602.268721	26.296295
206.906069	7629.665282	26.301312
207.019304	7634.285953	26.306330
207.389827	7658.477692	26.311348
207.244945	7665.581614	26.316365
207.360655	7676.052004	26.321383
207.937697	7698.669848	26.326400
207.970916	7699.099808	26.331418
208.350161	7724.798774	26.336436
208.160448	7747.511093	26.341453
208.885191	7759.286505	26.346471
209.099750	7767.334085	26.351488
209.076266	7768.884558	26.356506
209.491971	7787.981954	26.361524
209.837274	7801.119151	26.366541
209.978821	7804.443031	26.371559
210.202785	7821.760613	26.376576
209.956243	7826.584025	26.381594
210.556630	7839.761824	26.386612
210.495260	7854.238705	26.391629
210.628132	7873.426437	26.396647
211.109588	7889.700237	26.401664
211.020027	7893.932694	26.406682
211.471042	7913.294403	26.411700
211.465686	7932.813931	26.416717
212.112912	7942.388252	26.421735
212.413901	7947.321100	26.426752
212.389829	7953.920728	26.431770
213.128133	7970.295540	26.436788
212.865620	7985.711417	26.441805
213.586040	7982.628935	26.446823
213.506403	7983.502875	26.451840
213.791647	7990.056589	26.456858
214.188768	7982.612295	26.461876
214.036318	7994.932934	26.466893
214.431420	7999.347834	26.471911
214.243291	8010.051719	26.476928
214.324562	8015.113636	26.481946
214.617695	8030.514669	26.486964
214.697999	8040.881073	26.491981
215.178806	8055.595292	26.496999
215.304948	8071.387381	26.502016
215.609928	8077.960594	26.507034
215.652611	8083.732661	26.512052
215.899467	8105.736464	26.517069
215.747554	8110.523257	26.522087
216.026399	8130.778183	26.527104
216.202095	8143.485439	26.532122
216.772451	8150.203057	26.537140
216.721741	8171.403965	26.542157
216.873631	8183.543379	26.547175
217.121536	8197.881684	26.552192
217.464995	8220.716777	26.557210
217.516735	8231.805114	26.562228
217.704840	8262.834206	26.567245
218.157298	8272.195524	26.572263
218.095464	8279.051497	26.577280
218.266871	8302.262050	26.582298
218.705089	8313.843550	26.587316
218.780756	8332.197878	26.592333
219.315128	8346.410006	26.597351
219.838564	8355.596127	26.602368
219.696490	8359.068791	26.607386
219.912523	8387.784225	26.612404
220.070572	8387.237962	26.617421
221.290695	8387.867072	26.622439
221.845675	8381.908164	26.627456
222.053622	8385.759655	26.632474
222.948739	8379.164181	26.637492
222.430628	8372.067243	26.642509
222.593369	8369.375717	26.647527
222.967001	8371.310389	26.652544
223.349026	8370.770641	26.657562
223.274498	8347.737986	26.662580
223.440291	8346.662555	26.667597
223.577256	8340.625626	26.672615
223.617008	8344.280621	26.677632
223.578498	8366.674824	26.682650
223.905535	8367.371932	26.687668
223.461463	8375.451568	26.692685
223.827380	8386.199391	26.697703
223.991490	8403.193823	26.702720
223.888449	8414.722426	26.707738
223.887264	8423.762164	26.712756
223.825447	8452.509583	26.717773
224.309680	8468.154809	26.722791
224.787523	8471.082417	26.727808
224.752751	8500.932187	26.732826
225.357603	8517.506910	26.737844
225.356637	8538.535906	26.742861
225.649052	8551.695391	26.747879
226.087817	8581.836788	26.752896
225.844663	8581.810718	26.757914
226.437697	8592.456723	26.762932
226.368038	8615.645234	26.767949
227.060159	8640.326937	26.772967
226.949504	8644.506482	26.777984
227.191068	8667.996249	26.783002
227.474593	8677.508877	26.788020
227.507314	8699.660495	26.793037
227.832153	8720.499950	26.798055
228.132484	8739.112461	26.803072
228.274939	8752.924149	26.808090
228.726214	8773.723092	26.813108
229.009142	8782.224292	26.818125
229.015354	8810.779484	26.823143
229.223182	8814.985631	26.828160
229.341387	8842.981221	26.833178
229.849832	8855.726546	26.838196
229.814594	8876.681496	26.843213
230.268196	8896.681319	26.848231
230.645453	8908.670777	26.853248
230.769562	8916.041129	26.858266
231.264121	8932.551674	26.863284
231.656470	8950.800427	26.868301
231.982560	8958.396169	26.873319
233.497862	8943.142020	26.878336
234.062597	8944.542146	26.883354
234.505615	8913.391753	26.888372
234.735323	8899.817104	26.893389
234.229489	8894.866296	26.898407
234.304895	8880.186759	26.903424
234.280787	8861.235243	26.908442
234.477835	8853.943812	26.913460
234.302486	8866.212315	26.918477
234.368131	8883.283220	26.923495
234.574488	8894.049280	26.928512
234.549915	8904.604393	26.933530
234.646817	8912.078676	26.938548
234.633912	8931.517196	26.943565
234.621878	8954.916916	26.948583
234.935615	8968.437863	26.953600
235.136871	8996.532936	26.958618
235.070344	9017.211380	26.963636
235.251502	9037.196625	26.968653
235.676690	9066.346981	26.973671
235.971804	9082.965926	26.978688
235.572315	9115.614009	26.983706
236.290793	9131.782264	26.988724
236.369085	9152.574721	26.993741
236.364615	9186.434727	26.998759
236.876432	9206.903980	27.003776
236.716645	9233.673130	27.008794
237.453477	9265.403479	27.013812
237.826110	9280.104275	27.018829
237.755461	9298.705385	27.023847
238.278462	9311.517910	27.028864
238.303649	9346.208310	27.033882
238.633421	9362.326818	27.038900
239.121027	9381.405907	27.043917
239.428626	9413.041515	27.048935
239.945586	9420.292762	27.053952
240.188600	9442.094201	27.058970
240.453869	9450.340358	27.063988
240.914459	9459.635584	27.069005
241.005784	9470.606109	27.074023
241.153310	9471.472706	27.079040
241.594406	9504.707066	27.084058
242.098459	9511.361777	27.089076
242.110792	9520.084659	27.094093
242.044822	9535.114563	27.099111
242.132155	9539.333675	27.104128
242.399937	9564.257350	27.109146
242.692384	9585.415476	27.114164
243.009654	9608.808545	27.119181
243.300492	9619.765459	27.124199
243.836653	9631.227123	27.129216
243.758578	9650.034760	27.134234
244.285782	9657.147266	27.139252
244.600066	9672.268122	27.144269
244.648347	9684.290910	27.149287
245.115849	9689.692914	27.154304
245.685896	9703.908011	27.159322
246.155409	9697.146235	27.164340
246.818401	9698.718684	27.169357
246.755583	9703.850740	27.174375
247.168380	9694.374164	27.179392
247.180874	9702.693717	27.184410
247.225440	9711.865002	27.189428
247.377587	9721.258946	27.194445
247.114784	9728.714898	27.199463
247.554842	9723.541821	27.204480
247.567552	9755.537499	27.209498
247.658558	9754.675709	27.214516
247.938844	9776.190722	27.219533
248.061845	9782.699705	27.224551
248.873031	9796.102991	27.229568
248.869488	9813.038612	27.234586
248.795730	9830.744242	27.239604
249.222023	9838.912572	27.244621
248.930628	9849.518763	27.249639
249.473639	9869.190887	27.254656
249.655156	9896.339125	27.259674
249.819879	9907.484886	27.264692
249.951591	9933.122652	27.269709
250.277790	9963.011736	27.274727
250.972428	9964.829342	27.279744
251.456233	9979.962401	27.284762
251.570848	9987.339598	27.289780
252.471880	9996.662070	27.294797
252.517188	10000.871172	27.299815
252.873937	9994.561950	27.304832
253.094535	10006.509743	27.309850
253.076511	10000.258453	27.314868
253.671261	10009.731131	27.319885
253.506737	10028.454749	27.324903
253.660853	10021.271005	27.329920
253.521823	10035.292771	27.334938
253.729574	10058.705263	27.339956
254.240768	10062.598156	27.344973
254.148507	10090.091474	27.349991
254.802811	10101.994940	27.355008
254.813413	10118.783480	27.360026
254.763709	10138.288060	27.365044
255.604907	10156.196507	27.370061
255.228480	10171.600106	27.375079
255.510912	10187.324142	27.380096
255.837778	10204.857507	27.385114
255.909564	10221.279528	27.390132
256.495503	10250.519504	27.395149
256.527877	10280.730580	27.400167
257.168574	10303.182022	27.405184
257.185947	10312.752267	27.410202
257.420824	10332.039687	27.415220
257.798016	10345.982693	27.420237
257.320213	10373.028848	27.425255
258.294800	10392.736370	27.430272
258.350330	10412.188573	27.435290
258.857385	10423.652640	27.440308
259.435843	10444.080525	27.445325
259.885514	10455.116364	27.450343
260.173015	10473.414752	27.455360
260.384637	10482.493228	27.460378
260.481963	10489.028959	27.465396
260.646311	10508.602876	27.470413
260.803601	10528.627147	27.475431
260.825381	10548.324828	27.480448
261.251021	10558.329515	27.485466
261.310536	10582.307116	27.490484
261.854196	10597.857555	27.495501
261.905883	10612.411288	27.500519
262.327357	10636.733503	27.505536
262.807887	10650.317095	27.510554
262.849691	10663.681210	27.515572
263.641696	10680.490833	27.520589
263.373459	10695.022257	27.525607
263.501319	10711.310669	27.530624
263.825159	10731.052926	27.535642
264.124057	10758.018595	27.540660
264.406643	10762.169890	27.545677
264.579243	10789.410976	27.550695
264.976050	10791.583877	27.555712
265.641290	10796.265279	27.560730
265.558002	10822.798583	27.565748
266.099423	10822.078585	27.570765
266.023747	10836.758358	27.575783
266.130319	10852.976493	27.580800
266.493616	10860.155450	27.585818
266.644489	10884.470837	27.590836
267.040344	10900.737143	27.595853
267.070449	10921.585828	27.600871
267.629340	10927.692774	27.605888
268.137617	10945.030376	27.610906
268.024411	10952.716540	27.615924
268.553492	10973.426187	27.620941
269.261796	10980.577582	27.625959
269.645468	10977.062174	27.630976
269.819693	10992.247668	27.635994
269.773873	11006.660875	27.641012
270.140854	11011.472258	27.646029
270.039329	11026.903612	27.651047
270.298007	11042.167656	27.656064
270.627040	11058.543279	27.661082
270.886044	11075.714151	27.666100
271.201523	11083.339507	27.671117
271.248336	11100.162251	27.676135
271.526536	11121.699894	27.681152
272.036734	11127.342487	27.686170
272.624494	11138.547388	27.691188
273.261448	11161.804382	27.696205
272.848409	11161.720741	27.701223
273.279777	11176.055462	27.706240
273.342021	11187.903617	27.711258
273.790322	11209.555631	27.716276
274.186028	11219.832191	27.721293
274.138920	11237.476473	27.726311
274.268328	11256.715304	27.731328
274.628452	11262.646847	27.736346
274.392687	11295.012783	27.741364
274.856838	11310.098451	27.746381
274.759086	11333.735344	27.751399
274.760893	11359.050918	27.756416
275.627702	11389.046960	27.761434
275.227792	11411.794918	27.766452
275.865903	11432.513254	27.771469
276.152178	11469.517900	27.776487
276.420945	11505.200253	27.781504
276.480434	11526.667177	27.786522
276.658422	11559.210143	27.791540
277.255639	11588.280393	27.796557
277.594622	11619.851885	27.801575
277.878433	11640.427913	27.806592
278.081621	11667.602185	27.811610
278.506484	11694.536784	27.816628
279.517129	11706.534806	27.821645
279.856471	11721.724198	27.826663
280.692948	11708.407266	27.831680
281.188444	11713.961179	27.836698
281.389021	11725.251760	27.841716
281.801028	11718.379241	27.846733
281.814831	11722.800642	27.851751
282.005039	11724.192727	27.856768
282.002182	11712.081858	27.861786
282.170081	11734.312157	27.866804
282.546955	11751.703088	27.871821
282.959029	11760.579294	27.876839
283.080068	11774.261693	27.881856
283.274690	11771.210340	27.886874
283.122140	11796.877700	27.891892
283.029074	11806.526062	27.896909
283.600060	11834.881025	27.901927
283.575213	11859.128697	27.906944
283.965485	11866.949633	27.911962
283.889999	11900.219127	27.916980
284.106446	11918.039610	27.921997
284.293078	11949.663069	27.927015
284.720862	11979.719689	27.932032
285.333346	11997.867956	27.937050
285.969059	12025.159387	27.942068
285.795671	12036.941377	27.947085
286.333233	12066.334754	27.952103
286.533238	12094.987003	27.957120
287.022606	12095.766787	27.962138
287.105551	12128.759005	27.967156
287.582016	12148.771538	27.972173
288.004381	12164.002274	27.977191
288.384443	12193.550533	27.982208
288.907471	12205.924067	27.987226
288.944903	12228.804657	27.992244
289.124052	12247.126763	27.997261
289.025891	12263.048848	28.002279
289.289634	12276.765523	28.007296
290.115773	12302.711949	28.012314
290.096648	12330.294218	28.017332
290.722570	12339.636843	28.022349
291.164897	12358.728776	28.027367
291.415354	12379.456448	28.032384
291.778063	12379.285541	28.037402
292.000406	12395.873072	28.042420
292.131860	12401.469130	28.047437
292.510196	12431.407397	28.052455
292.500057	12439.612446	28.057472
293.089766	12454.375056	28.062490
293.099617	12466.546752	28.067508
293.500110	12493.489999	28.072525
293.946416	12506.403312	28.077543
293.620289	12536.705223	28.082560
294.577956	12557.721684	28.087578
294.947883	12561.032621	28.092596
295.125505	12563.270127	28.097613
295.301298	12586.526244	28.102631
295.580188	12605.961690	28.107648
295.670944	12627.927463	28.112666
295.639307	12648.215245	28.117684
295.966613	12664.403652	28.122701
296.317370	12680.277570	28.127719
296.455476	12710.375725	28.132736
296.879296	12729.999249	28.137754
296.854998	12754.695754	28.142772
296.960025	12784.971508	28.147789
297.648216	12812.537379	28.152807
297.842507	12841.866476	28.157824
298.649328	12859.210115	28.162842
298.675179	12888.117403	28.167860
299.186801	12908.857723	28.172877
299.364758	12931.403141	28.177895
299.590519	12955.153989	28.182912
300.236801	12975.961151	28.187930
299.787031	12997.334458	28.192948
300.168399	13025.906815	28.197965
300.192215	13049.574204	28.202983
300.436396	13076.631886	28.208000
301.217727	13106.524381	28.213018
301.219090	13136.039952	28.218036
301.766062	13165.660652	28.223053
302.850970	13188.451312	28.228071
303.036310	13209.903599	28.233088
303.232413	13222.409592	28.238106
303.721778	13240.717467	28.243124
303.950181	13257.752451	28.248141
304.534325	13274.286743	28.253159
304.706990	13297.817072	28.258176
304.833305	13311.856056	28.263194
305.086980	13335.424568	28.268212
305.235387	13351.688447	28.273229
305.917896	13358.460748	28.278247
305.386483	13398.661289	28.283264
305.697035	13423.777401	28.288282
306.087500	13451.393799	28.293300
306.346422	13481.742180	28.298317
306.898347	13495.720984	28.303335
307.495445	13517.616925	28.308352
308.341139	13532.803177	28.313370
308.696127	13547.108943	28.318388
308.678555	13563.852258	28.323405
309.191460	13568.768638	28.328423
309.301106	13599.585720	28.333440
309.630612	13603.198541	28.338458
310.009080	13617.311204	28.343476
310.144819	13623.480666	28.348493
310.699560	13644.417852	28.353511
311.231644	13662.225539	28.358528
311.511039	13665.889518	28.363546
311.529271	13683.774264	28.368564
311.416422	13692.478272	28.373581
311.618096	13705.204341	28.378599
311.824949	13730.094388	28.383616
311.891890	13748.137930	28.388634
311.790442	13770.462861	28.393652
312.120540	13809.044602	28.398669
312.470952	13837.659928	28.403687
312.518973	13878.607158	28.408704
313.239895	13904.385019	28.413722
313.143992	13942.319767	28.418740
313.520126	13976.149684	28.423757
314.209306	13995.439223	28.428775
314.295912	14032.994561	28.433792
314.690586	14059.389706	28.438810
315.305365	14070.067126	28.443828
315.680225	14101.993470	28.448845
316.130462	14118.007774	28.453863
316.437138	14151.909852	28.458880
317.096180	14166.770886	28.463898
317.528573	14181.011922	28.468916
318.266826	14198.813228	28.473933
318.885915	14190.813459	28.478951
319.244702	14209.803652	28.483968
319.591878	14222.855104	28.488986
319.576772	14228.658169	28.494004
319.887605	14235.939031	28.499021
320.369503	14259.231742	28.504039
320.385494	14273.150171	28.509056
320.485727	14288.464890	28.514074
320.728252	14304.150869	28.519092
320.798713	14326.631506	28.524109
321.346710	14340.551809	28.529127
321.420802	14369.858518	28.534144
321.566991	14379.580868	28.539162
321.831418	14407.551481	28.544180
321.973111	14449.700924	28.549197
322.601181	14472.942089	28.554215
322.625817	14504.500500	28.559232
323.030611	14532.083154	28.564250
323.477914	14554.813188	28.569268
323.634292	14585.122854	28.574285
324.369492	14602.628787	28.579303
324.231037	14624.820927	28.584320
324.672360	14647.333014	28.589338
325.153635	14676.393940	28.594356
325.571673	14705.051197	28.599373
326.071459	14726.881886	28.604391
325.956548	14754.544525	28.609408
326.201065	14782.755625	28.614426
326.606489	14800.271000	28.619444
326.451048	14840.352279	28.624461
326.868518	14872.277539	28.629479
327.203146	14907.566653	28.634496
327.720412	14926.614053	28.639514
328.970558	14946.498978	28.644532
329.399412	14977.196142	28.649549
329.791750	14967.800446	28.654567
329.891554	14986.016250	28.659584
330.590036	15005.723098	28.664602
331.128251	15005.373926	28.669620
330.718712	15018.984449	28.674637
331.151993	15036.255704	28.679655
330.884604	15053.506771	28.684672
331.054057	15081.787992	28.689690
331.324540	15113.574975	28.694708
331.229310	15136.550117	28.699725
331.564254	15156.005765	28.704743
332.257011	15191.601385	28.709760
332.234994	15232.210875	28.714778
333.083828	15259.321411	28.719796
332.979438	15291.530805	28.724813
333.358901	15322.951146	28.729831
333.803226	15354.079844	28.734848
334.126127	15391.949286	28.739866
334.634128	15420.105280	28.744884
334.548075	15460.395272	28.749901
335.168748	15485.789249	28.754919
335.564024	15524.478895	28.759936
336.280307	15536.624785	28.764954
337.255854	15553.981772	28.769972
338.043948	15564.926816	28.774989
339.394728	15556.859324	28.780007
340.266627	15560.125833	28.785024
340.434869	15549.749900	28.790042
340.340304	15529.442363	28.795060
340.417021	15527.889137	28.800077
340.467560	15530.456219	28.805095
340.854210	15536.922308	28.810112
340.801867	15549.028118	28.815130
341.041693	15559.723481	28.820148
341.150864	15570.001443	28.825165
340.653909	15598.341008	28.830183
341.548830	15617.491575	28.835200
341.015502	15642.178747	28.840218
341.190269	15659.543826	28.845236
341.859348	15695.532372	28.850253
342.018679	15733.725407	28.855271
342.282893	15765.913533	28.860288
342.301271	15798.156465	28.865306
342.860095	15831.323592	28.870324
342.976255	15876.967963	28.875341
343.222919	15904.687200	28.880359
343.455379	15948.324026	28.885376
344.042949	15982.456001	28.890394
344.949214	16010.224737	28.895412
345.471295	16052.484886	28.900429
346.489947	16062.254173	28.905447
346.546067	16077.182431	28.910464
346.762192	16106.669643	28.915482
347.329315	16117.838942	28.920500
347.378516	16147.255521	28.925517
347.754162	16167.696935	28.930535
347.977118	16184.433203	28.935552
348.370191	16212.417918	28.940570
348.634160	16228.020072	28.945588
348.469485	16262.533769	28.950605
349.848038	16260.547703	28.955623
350.260276	16275.353627	28.960640
350.192646	16299.889442	28.965658
351.000985	16315.480357	28.970676
351.554062	16336.425976	28.975693
351.167049	16348.816726	28.980711
351.483947	16368.294231	28.985728
351.292222	16389.347068	28.990746
352.188690	16424.174236	28.995764
352.226487	16447.494118	29.000781
352.261958	16481.702822	29.005799
352.859814	16514.068527	29.010816
352.672185	16553.090625	29.015834
353.186400	16576.083113	29.020852
353.115122	16609.827984	29.025869
353.636015	16654.408810	29.030887
354.118199	16693.431522	29.035904
354.669709	16729.097214	29.040922
355.266409	16765.790968	29.045940
355.559863	16790.699146	29.050957
356.020607	16816.899765	29.055975
356.784837	16843.641164	29.060992
356.844981	16878.100261	29.066010
357.121677	16910.789777	29.071028
357.600158	16931.419447	29.076045
357.546826	16971.918730	29.081063
358.109787	16996.658063	29.086080
358.316644	17038.929018	29.091098
359.060076	17078.625159	29.096116
359.241773	17105.056926	29.101133
359.905280	17137.592311	29.106151
360.266850	17158.108296	29.111168
360.429879	17198.094945	29.116186
360.388675	17212.210084	29.121204
361.298613	17260.173654	29.126221
361.472300	17291.218357	29.131239
361.921784	17322.496471	29.136256
362.286007	17349.088100	29.141274
362.803923	17373.403747	29.146292
363.279494	17392.223073	29.151309
363.573351	17410.619526	29.156327
364.514133	17437.336351	29.161344
364.399925	17475.911320	29.166362
364.916674	17492.718366	29.171380
365.269202	17518.464099	29.176397
364.650573	17554.743564	29.181415
365.366238	17584.991220	29.186432
365.416988	17615.113249	29.191450
365.848499	17644.014475	29.196468
365.752271	17681.126959	29.201485
366.277785	17725.495441	29.206503
366.682931	17751.270351	29.211520
366.667667	17797.662972	29.216538
367.438198	17824.862065	29.221556
367.854998	17868.855418	29.226573
367.705591	17905.510850	29.231591
368.363129	17945.222192	29.236608
368.891937	17991.337648	29.241626
369.402228	18029.001233	29.246644
369.430507	18059.864171	29.251661
369.817991	18100.080946	29.256679
370.582189	18137.699685	29.261696
370.933187	18185.801113	29.266714
370.748846	18219.333685	29.271732
371.601121	18256.746829	29.276749
371.911085	18286.472481	29.281767
372.952865	18322.141109	29.286784
373.027243	18353.461782	29.291802
373.980336	18380.986807	29.296820
374.264090	18404.150590	29.301837
374.475232	18435.640325	29.306855
375.141217	18461.154053	29.311872
375.191983	18493.659919	29.316890
375.441624	18514.863658	29.321908
376.155366	18546.816132	29.326925
376.379201	18567.245509	29.331943
377.256874	18579.995052	29.336960
377.661423	18605.594795	29.341978
377.855726	18624.009641	29.346996
378.276138	18651.200709	29.352013
378.502134	18677.009321	29.357031
378.808231	18686.189646	29.362048
379.173588	18728.257958	29.367066
379.609590	18753.292829	29.372084
379.927220	18786.962812	29.377101
380.144047	18824.104574	29.382119
380.512886	18851.131372	29.387136
380.692944	18875.440882	29.392154
381.005071	18901.596131	29.397172
381.450446	18939.343832	29.402189
382.122474	18973.841114	29.407207
382.283920	19009.376696	29.412224
382.497899	19042.189902	29.417242
383.080050	19078.022471	29.422260
383.357098	19110.251093	29.427277
383.804898	19145.294842	29.432295
384.244485	19172.924937	29.437312
384.583917	19209.769042	29.442330
384.840690	19245.334508	29.447348
385.241729	19264.430442	29.452365
385.374507	19299.205275	29.457383
386.118027	19329.506491	29.462400
386.597961	19361.839573	29.467418
386.880619	19385.736484	29.472436
387.412392	19410.478421	29.477453
387.666402	19435.982243	29.482471
387.913723	19464.894517	29.487488
388.245103	19491.048958	29.492506
388.943539	19515.366733	29.497524
389.506115	19549.023065	29.502541
389.397796	19571.927688	29.507559
390.244755	19583.108122	29.512576
390.891242	19602.386270	29.517594
391.223641	19623.802695	29.522612
391.776831	19643.502097	29.527629
392.171408	19666.008474	29.532647
393.144925	19672.845471	29.537664
393.521897	19684.232654	29.542682
394.092603	19707.355362	29.547700
394.305523	19704.961666	29.552717
394.555550	19717.456993	29.557735
395.147980	19735.538359	29.562752
395.625996	19749.514611	29.567770
395.567058	19767.587805	29.572788
395.816292	19774.080675	29.577805
395.959493	19804.449359	29.582823
396.133160	19819.890586	29.587840
396.254101	19850.031386	29.592858
396.323345	19891.073273	29.597876
396.904260	19919.883432	29.602893
396.889546	19967.209055	29.607911
397.031672	20002.412611	29.612928
397.644519	20050.435067	29.617946
397.764489	20090.379200	29.622964
398.396525	20130.475343	29.627981
398.578183	20188.109971	29.632999
399.189272	20225.671319	29.638016
399.472728	20267.774846	29.643034
400.233386	20312.890357	29.648052
400.591643	20334.717946	29.653069
400.813575	20378.746515	29.658087
401.847352	20394.463450	29.663104
402.442447	20422.161972	29.668122
403.440273	20451.362017	29.673140
403.983309	20451.431373	29.678157
404.037838	20483.700746	29.683175
404.615699	20503.887312	29.688192
405.104615	20527.338945	29.693210
405.533416	20552.177467	29.698228
405.770459	20564.511658	29.703245
405.779014	20610.058019	29.708263
406.214438	20628.069486	29.713280
406.334158	20655.108750	29.718298
406.857902	20697.556911	29.723316
407.257944	20721.768304	29.728333
407.401610	20754.814483	29.733351
407.712922	20778.599651	29.738368
408.188132	20813.541244	29.743386
408.557622	20845.287434	29.748404
408.632909	20870.936001	29.753421
408.685380	20911.292573	29.758439
408.975241	20946.598917	29.763456
409.857840	20987.545069	29.768474
409.665887	21029.191094	29.773492
409.994857	21074.442530	29.778509
410.317917	21129.930516	29.783527
410.972261	21165.614799	29.788544
411.252487	21217.609767	29.793562
411.231594	21270.134289	29.798580
411.946242	21316.168634	29.803597
411.963390	21377.690958	29.808615
412.591069	21420.629293	29.813632
413.314513	21463.598632	29.818650
413.606880	21529.240494	29.823668
414.513218	21565.653537	29.828685
414.866662	21608.918454	29.833703
415.251701	21660.538853	29.838720
415.565588	21699.829075	29.843738
415.971834	21746.390508	29.848756
416.847254	21784.335777	29.853773
417.462234	21828.923626	29.858791
418.269208	21865.344878	29.863808
419.066336	21879.205129	29.868826
419.661776	21909.200456	29.873844
420.342286	21933.009124	29.878861
420.624925	21961.030205	29.883879
420.904761	21975.039105	29.888896
421.361930	22003.575969	29.893914
420.888282	22032.777013	29.898932
421.745464	22047.775130	29.903949
421.778218	22089.501926	29.908967
422.200962	22125.667880	29.913984
422.568671	22167.050460	29.919002
422.851271	22204.107924	29.924020
424.002697	22237.052089	29.929037
424.387465	22278.384707	29.934055
424.226118	22309.358834	29.939072
424.801943	22350.520112	29.944090
425.000880	22384.589742	29.949108
425.432867	22420.382569	29.954125
425.865888	22466.463551	29.959143
426.146870	22495.889310	29.964160
426.986578	22547.177425	29.969178
426.829322	22588.449129	29.974196
427.603296	22626.401042	29.979213
428.074752	22663.758308	29.984231
428.593215	22704.384623	29.989248
428.665751	22729.733667	29.994266
429.237443	22778.302327	29.999284
429.722418	22803.192856	30.004301
430.409064	22846.604089	30.009319
430.882689	22882.128961	30.014336
431.644928	22908.413532	30.019354
431.536070	22951.002516	30.024372
431.997398	22981.293958	30.029389
432.351473	23008.124891	30.034407
432.713487	23041.350976	30.039424
433.359183	23073.295265	30.044442
433.325656	23115.808667	30.049460
433.935890	23149.900805	30.054477
434.076667	23179.834342	30.059495
434.077957	23224.865331	30.064512
434.487128	23268.350413	30.069530
435.280517	23315.068983	30.074548
435.653335	23361.093296	30.079565
435.914166	23410.183827	30.084583
436.458874	23453.538911	30.089600
436.952829	23501.063142	30.094618
437.020087	23550.114697	30.099636
437.731219	23594.122918	30.104653
438.442318	23645.553064	30.109671
438.971470	23686.378587	30.114688
439.808712	23713.146751	30.119706
439.819595	23762.388361	30.124724
440.491622	23806.867497	30.129741
441.121717	23845.193730	30.134759
441.100959	23881.978761	30.139776
441.591338	23924.047952	30.144794
442.142809	23979.455560	30.149812
442.414558	24005.933111	30.154829
443.576120	24038.468963	30.159847
444.194271	24085.137646	30.164864
445.068070	24109.588085	30.169882
445.396543	24145.134134	30.174900
445.659033	24161.456730	30.179917
446.094504	24194.779703	30.184935
446.413584	24216.041734	30.189952
447.043644	24239.717164	30.194970
447.221595	24275.667792	30.199988
447.814250	24311.642060	30.205005
448.624085	24339.390581	30.210023
449.264852	24368.644340	30.215040
449.863641	24385.083008	30.220058
449.947494	24438.641777	30.225076
450.180192	24460.221729	30.230093
450.458577	24480.670934	30.235111
450.834816	24516.439830	30.240128
451.320999	24552.896537	30.245146
451.180581	24595.384586	30.250164
451.484017	24629.311427	30.255181
451.990373	24675.420461	30.260199
452.064412	24726.228031	30.265216
452.813908	24773.412316	30.270234
453.186083	24818.711965	30.275252
453.228716	24870.802874	30.280269
453.340516	24913.425130	30.285287
453.956017	24976.023356	30.290304
454.218441	25024.512555	30.295322
454.712672	25078.911461	30.300340
455.520448	25124.332842	30.305357
456.151720	25163.368403	30.310375
456.711546	25205.394118	30.315392
457.191253	25244.960550	30.320410
457.475356	25294.418370	30.325428
457.792408	25336.413450	30.330445
458.605935	25383.878643	30.335463
458.902970	25427.205420	30.340480
459.643891	25465.159801	30.345498
460.367330	25506.533615	30.350516
461.183232	25547.856985	30.355533
461.619981	25570.015335	30.360551
462.086605	25612.121099	30.365568
462.786861	25647.780029	30.370586
462.814528	25682.816118	30.375604
463.330020	25709.850724	30.380621
463.346476	25749.374661	30.385639
463.764928	25802.148445	30.390656
464.591195	25840.931299	30.395674
464.257593	25889.616531	30.400692
464.585160	25941.658672	30.405709
464.774683	25995.680485	30.410727
465.298940	26049.503149	30.415744
465.848690	26107.643465	30.420762
466.393173	26160.630183	30.425780
466.627797	26219.386397	30.430797
467.058866	26269.080489	30.435815
468.169030	26335.693613	30.440832
468.517521	26381.042409	30.445850
468.997902	26430.857855	30.450868
469.338647	26483.139112	30.455885
470.549901	26524.958601	30.460903
470.693957	26585.069165	30.465920
471.673720	26623.682348	30.470938
472.189631	26665.028234	30.475956
472.804051	26701.975398	30.480973
473.373453	26735.990125	30.485991
473.692362	26777.303785	30.491008
474.077959	26817.407305	30.496026
474.583323	26863.206844	30.501044
474.833575	26906.318177	30.506061
475.315223	26944.790282	30.511079
475.550630	26996.292966	30.516096
475.912169	27034.877340	30.521114
476.644892	27084.089857	30.526132
476.855025	27132.868360	30.531149
477.585389	27173.001954	30.536167
477.846495	27228.838811	30.541184
478.915994	27267.762995	30.546202
479.320398	27303.425539	30.551220
480.067701	27351.563662	30.556237
480.421979	27380.653912	30.561255
480.835958	27428.896687	30.566272
480.687616	27470.380386	30.571290
481.503747	27516.320835	30.576308
481.682342	27554.243627	30.581325
482.258546	27584.570767	30.586343
482.629387	27631.679417	30.591360
483.149132	27658.937166	30.596378
483.598669	27701.069834	30.601396
484.079264	27750.311655	30.606413
484.711938	27787.715455	30.611431
485.142570	27826.128833	30.616448
485.762178	27869.232882	30.621466
486.273436	27912.570140	30.626484
486.739424	27951.905295	30.631501
487.513820	27984.205730	30.636519
487.911333	28039.157332	30.641536
488.448482	28063.948687	30.646554
489.246215	28101.766573	30.651572
489.376093	28148.454117	30.656589
489.693825	28188.556633	30.661607
489.868013	28239.101715	30.666624
490.464517	28278.298503	30.671642
490.840086	28322.439316	30.676660
490.895259	28380.877017	30.681677
491.414636	28428.123261	30.686695
491.188683	28489.751929	30.691712
491.930670	28546.990308	30.696730
492.310879	28607.344988	30.701748
492.963801	28667.164105	30.706765
494.057770	28720.124370	30.711783
495.949435	28738.377524	30.716800
497.202455	28757.279654	30.721818
498.047135	28783.006883	30.726836
498.610474	28809.675256	30.731853
499.237730	28810.018965	30.736871
499.465038	28834.586850	30.741888
499.706178	28844.929067	30.746906
500.259409	28872.015745	30.751924
500.238487	28893.023082	30.756941
500.731232	28926.017163	30.761959
501.141109	28956.517160	30.766976
501.750872	28991.072042	30.771994
502.001426	29009.272239	30.777012
502.350583	29058.855768	30.782029
503.274119	29090.473258	30.787047
502.882376	29123.452039	30.792064
503.294651	29170.362095	30.797082
503.492889	29210.455864	30.802100
503.433624	29258.626994	30.807117
503.949086	29314.111374	30.812135
504.557915	29373.817395	30.817152
504.998902	29426.273252	30.822170
505.204712	29481.823837	30.827188
505.865284	29548.564090	30.832205
506.285135	29606.283914	30.837223
506.480465	29671.305846	30.842240
507.365745	29732.555971	30.847258
507.958356	29775.666164	30.852276
508.269283	29838.479128	30.857293
508.898543	29886.808502	30.862311
509.359935	29939.139326	30.867328
509.800276	29983.938975	30.872346
510.289920	30026.966453	30.877364
510.896799	30087.741725	30.882381
511.373436	30126.439376	30.887399
512.113472	30182.768347	30.892416
512.268380	30243.974999	30.897434
513.362360	30288.622401	30.902452
513.816902	30340.772573	30.907469
514.324866	30392.443590	30.912487
514.949478	30438.235165	30.917504
515.460257	30488.691145	30.922522
516.040305	30537.096991	30.927540
516.452673	30594.818163	30.932557
516.870264	30640.620489	30.937575
517.564235	30684.879891	30.942592
517.669102	30745.702414	30.947610
518.326507	30793.679183	30.952628
518.605038	30857.204975	30.957645
518.976053	30910.914167	30.962663
519.887727	30972.750981	30.967680
520.411925	31024.619853	30.972698
521.000455	31075.509106	30.977716
521.359213	31136.819591	30.982733
522.378047	31186.180728	30.987751
522.602502	31248.142563	30.992768
522.986088	31299.970063	30.997786
524.293959	31343.469560	31.002804
524.609808	31382.768659	31.007821
525.368994	31433.257337	31.012839
525.691406	31489.144492	31.017856
526.608104	31527.157609	31.022874
527.428423	31565.420837	31.027892
527.652998	31611.182999	31.032909
528.074364	31650.190069	31.037927
528.895052	31686.462293	31.042944
529.265881	31733.117998	31.047962
529.741901	31764.580280	31.052980
530.114138	31820.005521	31.057997
530.655166	31857.244307	31.063015
531.295182	31905.441639	31.068032
531.443358	31951.315589	31.073050
532.116794	31996.809334	31.078068
532.440953	32047.825555	31.083085
533.526423	32078.000579	31.088103
533.776720	32125.198652	31.093120
534.121731	32172.759307	31.098138
534.782738	32216.504317	31.103156
535.270055	32279.683828	31.108173
535.656750	32319.395719	31.113191
536.212567	32372.326580	31.118208
536.728492	32424.068398	31.123226
537.406887	32473.062251	31.128244
537.620189	32520.700046	31.133261
538.023459	32561.596209	31.138279
538.590742	32603.098679	31.143296
538.305751	32658.800073	31.148314
538.928366	32718.019502	31.153332
539.103043	32788.916699	31.158349
539.737266	32842.656031	31.163367
540.203882	32918.149113	31.168384
540.963141	32978.980722	31.173402
541.947578	33038.726206	31.178420
541.972528	33104.847066	31.183437
542.728600	33162.505023	31.188455
543.440344	33224.330244	31.193472
543.924210	33292.942072	31.198490
544.116132	33344.773619	31.203508
544.447748	33416.192375	31.208525
545.134404	33486.225083	31.213543
545.619971	33553.710939	31.218560
546.360266	33624.318847	31.223578
546.970257	33683.477345	31.228596
547.297978	33764.735361	31.233613
548.340748	33824.249387	31.238631
549.226892	33881.016304	31.243648
549.711590	33946.070487	31.248666
550.541137	33987.124091	31.253684
551.514211	34043.977621	31.258701
552.169038	34092.064676	31.263719
553.032374	34141.258629	31.268736
553.592572	34193.016891	31.273754
554.474333	34228.011905	31.278772
554.644692	34273.259919	31.283789
555.105493	34322.283472	31.288807
555.633980	34362.300662	31.293824
556.453557	34416.502135	31.298842
557.116779	34452.219905	31.303860
557.652494	34489.231512	31.308877
558.000165	34531.801803	31.313895
558.401274	34574.208387	31.318912
558.734344	34625.918434	31.323930
559.166010	34679.104598	31.328948
559.596726	34733.089593	31.333965
560.097269	34788.694529	31.338983
561.005217	34833.366236	31.344000
561.240632	34904.226622	31.349018
562.000926	34954.504087	31.354036
562.513385	35008.419086	31.359053
562.942307	35065.618408	31.364071
563.667294	35115.053343	31.369088
564.179611	35175.846303	31.374106
564.431630	35219.791786	31.379124
564.692301	35282.215813	31.384141
564.466983	35353.178985	31.389159
565.445313	35412.377880	31.394176
566.032818	35491.048858	31.399194
566.683057	35556.680166	31.404212
567.006409	35615.206021	31.409229
567.415047	35680.150058	31.414247
568.072258	35744.205839	31.419264
568.565369	35806.623404	31.424282
569.424437	35866.106191	31.429300
569.645668	35937.074038	31.434317
570.398161	35994.984691	31.439335
571.070135	36057.533449	31.444352
571.630164	36137.543930	31.449370
572.506247	36199.411140	31.454388
573.169493	36261.810587	31.459405
573.942871	36319.848109	31.464423
574.667769	36380.637083	31.469440
575.264692	36430.902437	31.474458
575.892506	36474.290999	31.479476
577.097768	36529.998320	31.484493
577.271318	36578.228089	31.489511
578.261775	36620.453252	31.494528
578.372144	36678.791746	31.499546
579.096722	36730.636405	31.504564
579.703137	36782.258403	31.509581
579.673474	36839.273564	31.514599
580.596187	36894.932559	31.519616
580.890888	36962.520616	31.524634
581.442492	37023.442432	31.529652
582.583759	37081.810763	31.534669
582.597017	37140.337821	31.539687
583.489915	37184.594909	31.544704
583.975644	37252.179716	31.549722
584.570152	37310.566696	31.554740
585.524279	37362.686325	31.559757
585.603863	37426.228278	31.564775
586.531815	37483.302340	31.569792
586.582464	37555.890333	31.574810
587.105187	37604.239753	31.579828
588.187525	37677.153377	31.584845
588.987350	37739.888019	31.589863
589.778021	37786.512655	31.594880
590.047044	37845.490585	31.599898
590.511982	37904.040550	31.604916
590.823549	37965.827370	31.609933
591.332637	38035.017834	31.614951
591.603386	38094.832804	31.619968
592.028056	38167.737942	31.624986
592.715952	38240.860282	31.630004
593.462510	38320.756800	31.635021
593.378645	38384.772018	31.640039
594.223577	38454.490527	31.645056
594.450490	38530.300522	31.650074
595.098531	38609.223927	31.655092
596.022939	38691.235075	31.660109
596.294003	38777.926508	31.665127
597.120622	38847.112973	31.670144
597.812114	38929.414478	31.675162
598.404129	38993.344421	31.680180
599.464946	39062.901969	31.685197
599.704052	39129.951898	31.690215
600.667497	39192.546653	31.695232
601.037616	39265.077169	31.700250
601.302934	39334.832013	31.705268
602.030312	39395.504271	31.710285
602.868915	39470.793448	31.715303
603.999674	39522.784761	31.720320
605.266214	39575.611664	31.725338
605.834439	39641.148524	31.730356
606.694521	39677.991946	31.735373
607.306012	39732.828894	31.740391
607.918573	39780.275194	31.745408
607.927002	39834.022400	31.750426
608.676974	39893.944202	31.755444
609.052263	39962.760709	31.760461
609.337538	40021.064033	31.765479
609.784177	40077.919204	31.770496
610.321110	40150.642446	31.775514
611.065896	40217.394992	31.780532
611.584726	40284.435902	31.785549
611.481898	40364.265773	31.790567
612.216879	40433.934813	31.795584
612.631371	40520.988685	31.800602
612.907779	40603.883359	31.805620
613.200120	40686.936689	31.810637
614.098659	40777.994239	31.815655
614.852318	40860.599915	31.820672
615.846864	40954.795946	31.825690
616.733457	41025.407341	31.830708
617.729582	41095.577165	31.835725
618.062840	41177.593247	31.840743
618.530473	41254.803375	31.845760
619.463363	41324.492358	31.850778
619.753591	41396.252394	31.855796
620.827130	41473.615365	31.860813
621.279291	41548.297183	31.865831
622.551143	41613.890943	31.870848
623.525821	41678.121348	31.875866
623.979984	41738.715454	31.880884
625.363790	41794.859612	31.885901
625.145232	41866.307629	31.890919
625.801154	41924.907033	31.895936
626.397504	41986.358496	31.900954
626.545468	42062.461640	31.905972
627.482667	42129.383828	31.910989
627.615266	42204.950260	31.916007
628.473182	42273.559993	31.921024
628.966744	42352.431031	31.926042
629.164256	42426.604262	31.931060
630.474852	42483.792372	31.936077
630.679133	42568.722591	31.941095
631.665847	42636.203299	31.946112
632.335421	42699.501176	31.951130
632.929276	42768.622115	31.956148
633.192490	42838.207278	31.961165
634.459234	42912.565523	31.966183
634.819350	42974.717467	31.971200
635.489642	43032.938961	31.976218
635.673927	43094.685677	31.981236
636.829570	43155.277854	31.986253
636.888145	43228.975989	31.991271
637.807971	43303.786760	31.996288
638.532678	43365.713336	32.001306
639.106131	43444.208978	32.006324
639.507745	43511.512035	32.011341
639.601740	43593.219683	32.016359
640.298389	43668.799561	32.021376
640.884202	43753.278198	32.026394
641.164473	43840.351524	32.031412
642.018047	43914.610835	32.036429
642.682576	44010.160784	32.041447
643.578796	44090.154269	32.046464
644.091856	44176.532446	32.051482
644.424780	44266.687018	32.056500
645.490240	44348.124131	32.061517
646.196690	44428.142082	32.066535
646.919291	44514.814316	32.071552
647.507058	44603.190021	32.076570
648.454970	44685.829760	32.081588
649.772374	44740.481483	32.086605
650.303573	44824.993204	32.091623
650.697684	44890.878242	32.096640
651.349776	44965.949878	32.101658
651.994383	45047.553674	32.106676
652.951173	45115.259954	32.111693
653.056559	45200.098925	32.116711
653.894150	45275.812648	32.121728
654.234278	45354.526705	32.126746
654.908519	45441.779888	32.131764
655.975730	45518.986866	32.136781
656.212389	45606.735782	32.141799
656.697716	45687.153771	32.146816
657.345767	45764.537766	32.151834
658.267797	45847.180671	32.156852
659.028697	45916.496071	32.161869
660.377619	46006.781693	32.166887
661.419611	46064.983566	32.171904
662.250267	46120.793243	32.176922
663.016317	46189.954009	32.181940
664.190817	46236.230788	32.186957
664.980712	46287.645519	32.191975
665.536012	46340.774390	32.196992
666.039970	46384.428297	32.202010
666.726697	46447.145181	32.207028
667.300409	46498.938596	32.212045
667.472579	46563.386255	32.217063
668.114398	46617.552745	32.222080
668.968717	46680.475389	32.227098
669.170187	46746.254558	32.232116
670.037743	46797.230999	32.237133
670.313152	46857.508913	32.242151
670.550105	46929.769620	32.247168
671.188325	46991.252252	32.252186
671.808217	47064.948032	32.257204
672.458451	47131.096956	32.262221
673.195179	47210.107590	32.267239
674.297414	47258.818470	32.272256
675.653876	47301.052476	32.277274
676.476817	47365.053406	32.282292
677.502667	47418.910025	32.287309
678.140363	47454.436071	32.292327
678.906440	47510.516690	32.297344
679.518327	47564.378308	32.302362
680.105053	47616.898932	32.307380
680.937067	47662.372451	32.312397
681.405905	47721.126037	32.317415
681.668599	47776.955721	32.322432
682.460457	47822.878671	32.327450
682.763460	47893.366150	32.332468
683.577497	47947.165785	32.337485
683.974153	48013.898115	32.342503
684.352885	48084.847082	32.347520
684.945289	48141.467797	32.352538
685.868666	48221.268645	32.357556
686.608500	48286.682910	32.362573
687.366196	48364.668196	32.367591
687.321233	48428.186487	32.372608
688.271796	48500.833039	32.377626
688.610634	48579.617397	32.382644
689.043513	48668.101564	32.387661
689.876777	48740.472211	32.392679
690.374694	48836.715990	32.397696
691.268304	48916.581662	32.402714
692.003542	49008.332074	32.407732
692.784124	49091.313231	32.412749
693.394889	49180.893723	32.417767
694.020560	49270.276241	32.422784
694.764866	49352.639324	32.427802
694.727555	49454.303303	32.432820
695.351027	49542.613511	32.437837
696.033496	49641.741951	32.442855
696.587491	49749.004427	32.447872
697.268800	49854.792678	32.452890
697.665011	49962.689832	32.457908
698.389142	50060.246537	32.462925
699.281380	50159.430123	32.467943
700.249331	50256.307972	32.472960
701.823644	50338.413011	32.477978
703.209753	50430.267115	32.482996
704.283303	50510.955074	32.488013
705.684120	50563.467425	32.493031
706.152838	50638.965333	32.498048
706.745183	50687.295222	32.503066
707.454485	50751.942790	32.508084
708.092484	50812.142467	32.513101
708.429015	50872.027543	32.518119
709.180757	50944.432994	32.523136
709.853302	50994.424114	32.528154
710.803696	51060.231782	32.533172
711.409892	51128.922705	32.538189
711.818052	51175.769073	32.543207
712.117049	51241.265639	32.548224
712.954416	51307.927461	32.553242
713.631598	51386.380905	32.558260
713.954243	51454.887779	32.563277
714.626405	51548.335202	32.568295
714.992540	51630.867451	32.573312
715.877129	51716.350204	32.578330
715.990562	51820.060328	32.583348
716.485806	51896.417791	32.588365
717.051175	51994.586279	32.593383
717.707511	52103.448929	32.598400
718.636897	52204.367683	32.603418
719.168124	52314.320701	32.608436
719.408772	52426.124808	32.613453
720.374545	52531.063726	32.618471
720.795475	52639.881206	32.623488
722.000995	52757.505355	32.628506
722.271507	52864.669156	32.633524
723.194681	52970.710789	32.638541
724.131852	53081.470482	32.643559
724.907635	53197.648115	32.648576
725.705511	53290.387224	32.653594
726.742009	53398.079827	32.658612
727.272411	53492.717038	32.663629
728.375811	53598.560561	32.668647
729.016997	53705.418986	32.673664
730.195865	53797.640263	32.678682
730.814784	53898.045843	32.683700
731.340628	53996.723899	32.688717
732.854495	54092.478212	32.693735
733.493214	54194.196203	32.698752
734.048137	54287.828311	32.703770
735.270605	54376.398836	32.708788
736.144561	54456.340971	32.713805
737.337145	54526.497713	32.718823
738.276839	54609.891973	32.723840
739.255986	54669.950199	32.728858
739.976893	54738.343348	32.733876
740.892708	54810.513706	32.738893
741.839238	54863.759896	32.743911
743.440511	54918.473836	32.748928
744.370768	54954.667973	32.753946
745.259812	55012.145537	32.758964
746.340646	55067.543029	32.763981
746.908621	55103.590964	32.768999
747.008295	55156.774470	32.774016
747.611366	55204.254179	32.779034
748.099881	55254.047475	32.784052
748.686089	55305.252292	32.789069
749.354714	55358.067151	32.794087
749.636811	55423.365586	32.799104
749.955769	55478.237526	32.804122
750.362530	55547.502439	32.809140
750.707908	55618.124108	32.814157
751.602764	55699.912872	32.819175
751.541474	55791.136186	32.824192
752.003564	55887.085605	32.829210
752.623806	55980.404808	32.834228
752.788116	56086.782606	32.839245
753.443648	56189.879186	32.844263
753.818428	56300.310739	32.849280
754.604410	56413.143392	32.854298
755.219108	56531.011099	32.859316
755.909229	56655.470544	32.864333
757.048061	56780.808161	32.869351
757.172348	56904.095818	32.874368
758.308621	57028.108280	32.879386
758.702954	57152.596178	32.884404
759.571966	57279.152260	32.889421
760.731977	57402.379301	32.894439
761.660715	57523.693872	32.899456
762.856590	57632.734415	32.904474
763.330106	57755.329128	32.909492
764.278881	57861.158463	32.914509
765.568794	57977.433756	32.919527
765.854423	58096.422393	32.924544
766.662705	58214.247790	32.929562
767.759965	58319.061828	32.934580
768.481574	58439.646305	32.939597
769.724566	58544.556627	32.944615
770.360603	58662.053873	32.949632
771.426371	58761.888942	32.954650
772.823864	58853.147951	32.959668
774.103976	58935.579058	32.964685
775.249545	59012.143004	32.969703
776.002908	59108.588711	32.974720
776.794649	59189.271595	32.979738
777.519645	59263.209723	32.984756
778.394130	59355.470707	32.989773
779.453303	59424.201031	32.994791
779.955258	59513.663376	32.999808
780.525704	59591.181273	33.004826
781.803569	59664.748054	33.009844
782.047868	59750.008175	33.014861
782.650208	59820.391898	33.019879
783.346702	59915.321575	33.024896
783.982060	60004.396620	33.029914
784.683096	60090.528018	33.034932
784.999352	60182.679768	33.039949
785.742798	60289.568191	33.044967
786.474763	60388.330656	33.049984
787.233765	60486.349434	33.055002
787.748634	60583.335959	33.060020
788.254827	60694.034324	33.065037
789.041567	60788.731351	33.070055
789.863253	60901.285694	33.075072
790.376270	61000.531064	33.080090
791.115915	61105.913676	33.085108
791.029458	61213.113390	33.090125
791.904189	61346.299147	33.095143
792.662797	61457.558874	33.100160
793.389416	61575.069934	33.105178
794.202523	61706.922175	33.110196
794.692817	61837.408280	33.115213
795.992671	61955.942169	33.120231
796.170336	62088.740082	33.125248
796.918126	62220.278072	33.130266
797.873307	62355.409826	33.135284
798.428983	62489.125361	33.140301
799.145166	62618.800158	33.145319
800.066512	62759.218726	33.150336
801.025529	62896.034849	33.155354
802.208192	63018.729150	33.160372
803.386047	63146.393765	33.165389
804.626216	63259.376001	33.170407
805.272295	63377.783441	33.175424
806.079859	63505.368280	33.180442
807.528247	63628.760298	33.185460
808.404686	63730.523095	33.190477
809.538610	63848.312295	33.195495
810.640081	63953.628418	33.200512
811.421448	64047.329743	33.205530
812.709031	64149.422437	33.210548
813.530152	64251.146668	33.215565
814.836467	64340.138068	33.220583
815.456553	64436.979159	33.225600
816.033277	64532.886145	33.230618
816.975856	64630.450500	33.235636
817.666155	64717.424808	33.240653
818.523304	64809.883760	33.245671
819.073939	64905.917037	33.250688
820.101104	65007.261925	33.255706
820.852211	65105.133131	33.260724
821.366170	65217.327280	33.265741
822.140886	65317.414524	33.270759
823.114102	65428.993749	33.275776
823.965573	65529.618893	33.280794
824.907752	65623.527307	33.285812
825.482409	65727.197590	33.290829
826.066769	65821.952145	33.295847
826.506016	65936.413683	33.300864
827.301435	66055.834869	33.305882
827.978854	66160.709911	33.310900
828.347149	66279.990552	33.315917
829.796003	66394.237385	33.320935
830.808499	66510.608094	33.325952
831.085869	66631.569128	33.330970
832.225139	66737.335280	33.335988
832.926214	66846.066484	33.341005
833.602144	66959.177880	33.346023
834.477496	67060.564934	33.351040
835.043693	67167.556832	33.356058
835.998600	67275.203494	33.361076
836.953292	67395.471161	33.366093
838.202313	67501.626981	33.371111
839.504051	67594.730116	33.376128
840.418939	67701.867308	33.381146
841.325519	67798.794847	33.386164
842.077320	67900.592761	33.391181
843.026373	68008.180895	33.396199
843.591171	68106.983083	33.401216
844.291632	68217.447582	33.406234
845.161425	68322.369876	33.411252
845.720792	68432.062932	33.416269
846.327020	68551.941522	33.421287
847.091187	68655.758008	33.426304
847.570934	68775.925086	33.431322
848.605295	68894.518194	33.436340
848.784983	69027.428940	33.441357
849.058593	69162.657746	33.446375
849.978661	69294.798351	33.451392
851.015063	69424.618103	33.456410
852.269866	69563.861183	33.461428
853.097081	69697.872947	33.466445
853.946070	69831.262102	33.471463
855.700676	69953.512859	33.476480
856.458073	70082.998617	33.481498
858.054470	70184.409743	33.486516
859.268576	70290.800343	33.491533
860.693556	70388.808012	33.496551
862.108613	70493.679116	33.501568
862.650765	70596.145413	33.506586
863.505134	70690.464221	33.511604
864.232276	70797.826049	33.516621
864.636222	70897.370520	33.521639
865.570027	70997.836526	33.526656
866.002475	71120.054711	33.531674
866.693101	71222.289841	33.536692
867.192917	71346.603646	33.541709
867.656098	71469.969501	33.546727
868.698875	71583.965675	33.551744
868.967776	71722.702148	33.556762
869.702239	71851.620551	33.561780
870.435468	71992.372509	33.566797
871.068649	72137.986880	33.571815
871.973120	72286.332119	33.576832
872.750967	72415.638521	33.581850
874.219014	72539.736365	33.586868
875.800162	72664.283548	33.591885
876.747144	72786.169948	33.596903
878.006477	72903.045148	33.601920
878.710361	73019.731496	33.606938
879.803484	73129.122859	33.611956
880.624610	73237.169946	33.616973
881.348582	73346.088022	33.621991
882.384502	73455.516104	33.627008
883.112493	73567.192122	33.632026
884.222886	73671.106069	33.637044
885.312266	73778.515348	33.642061
886.644912	73875.978934	33.647079
887.673755	73971.040969	33.652096
888.401198	74071.860002	33.657114
889.589095	74169.722839	33.662132
889.891672	74267.623884	33.667149
890.658672	74384.749383	33.672167
891.405832	74482.221041	33.677184
891.812612	74598.953970	33.682202
892.276537	74713.925704	33.687220
893.356080	74834.959495	33.692237
893.875389	74966.829836	33.697255
895.183791	75096.478537	33.702272
895.253217	75236.321241	33.707290
896.248981	75362.071824	33.712308
896.661787	75503.913078	33.717325
897.473029	75643.220149	33.722343
898.215376	75791.894993	33.727360
898.759689	75947.277967	33.732378
900.011626	76093.704281	33.737396
901.716837	76223.936769	33.742413
902.443291	76374.876382	33.747431
903.731564	76500.191099	33.752448
904.649766	76651.327452	33.757466
905.788818	76783.462932	33.762484
906.462559	76918.468472	33.767501
907.065544	77060.432500	33.772519
908.458495	77200.073448	33.777536
908.756626	77344.779895	33.782554
909.699038	77487.959960	33.787572
910.252070	77626.102691	33.792589
911.202920	77771.294715	33.797607
912.369155	77926.584861	33.802624
913.283079	78078.421044	33.807642
914.246799	78233.463313	33.812660
915.244881	78376.778646	33.817677
915.431932	78541.837274	33.822695
916.706513	78691.117001	33.827712
917.339222	78849.085891	33.832730
918.376137	79001.558783	33.837748
919.458124	79152.190371	33.842765
920.006705	79325.815427	33.847783
921.180344	79481.241469	33.852800
922.089073	79651.315196	33.857818
923.074270	79799.772387	33.862836
924.193615	79955.552583	33.867853
925.011968	80122.557984	33.872871
926.072715	80270.094274	33.877888
927.569628	80419.347242	33.882906
928.526315	80543.330278	33.887924
929.699973	80680.910764	33.892941
930.446156	80806.791309	33.897959
931.749236	80934.975002	33.902976
932.456877	81081.185098	33.907994
933.626406	81201.566942	33.913012
934.631764	81332.929277	33.918029
934.850729	81467.603121	33.923047
935.593375	81608.242919	33.928064
936.559708	81752.394685	33.933082
936.953204	81894.639793	33.938100
937.867664	82045.774612	33.943117
938.744522	82201.023125	33.948135
939.797945	82346.346838	33.953152
940.613707	82510.421553	33.958170
941.444547	82663.548791	33.963188
942.716611	82825.168560	33.968205
943.134086	82992.054576	33.973223
943.702381	83151.101706	33.978240
944.753499	83327.530791	33.983258
945.672215	83491.936470	33.988276
946.918816	83663.949719	33.993293
947.580853	83844.258474	33.998311
949.189610	84002.108162	34.003328
950.061081	84168.273093	34.008346
950.747192	84338.887643	34.013364
951.970677	84494.281892	34.018381
952.573249	84675.575358	34.023399
953.413269	84844.990266	34.028416
954.836161	85015.160835	34.033434
955.563403	85195.487778	34.038452
956.479299	85362.261013	34.043469
957.172018	85539.464172	34.048487
958.735429	85706.388399	34.053504
959.409392	85890.931576	34.058522
960.819981	86056.485941	34.063540
961.636225	86221.820505	34.068557
963.196809	86375.979725	34.073575
964.365117	86538.187030	34.078592
965.695170	86714.536771	34.083610
966.214083	86870.478636	34.088628
967.371629	87017.325878	34.093645
967.598679	87190.792442	34.098663
968.883972	87350.143786	34.103680
969.932068	87514.428741	34.108698
971.130962	87677.746049	34.113716
972.115297	87836.563619	34.118733
972.758203	88004.655188	34.123751
973.291708	88172.481879	34.128768
974.626634	88338.476408	34.133786
975.432469	88510.499063	34.138804
976.601864	88680.486103	34.143821
977.431543	88854.412103	34.148839
978.516570	89001.328220	34.153856
979.738144	89177.239998	34.158874
980.296412	89336.279665	34.163892
981.838764	89483.272297	34.168909
982.566092	89635.272432	34.173927
983.736175	89791.001488	34.178944
985.046639	89941.878376	34.183962
985.924889	90093.197307	34.188980
986.674759	90235.665609	34.193997
987.454343	90397.535140	34.199015
988.404161	90551.914358	34.204032
989.523085	90706.341549	34.209050
990.366808	90866.937349	34.214068
991.192943	91018.543118	34.219085
991.816493	91204.363589	34.224103
992.602497	91371.295719	34.229120
993.375137	91551.371421	34.234138
993.792543	91732.275156	34.239156
994.880465	91914.970628	34.244173
995.794796	92108.242454	34.249191
996.740551	92298.117675	34.254208
997.857750	92492.870590	34.259226
998.953829	92674.386632	34.264244
1000.053878	92866.898344	34.269261
1000.910688	93064.707057	34.274279
1002.104195	93255.053608	34.279296
1003.063864	93444.726369	34.284314
1004.157222	93641.435734	34.289332
1005.279544	93829.197216	34.294349
1006.112102	94026.986104	34.299367
1007.343778	94215.428095	34.304384
1008.594632	94404.849422	34.309402
1009.338464	94601.499620	34.314420
1010.384869	94789.483907	34.319437
1011.397266	94990.060320	34.324455
1011.924775	95181.675114	34.329472
1013.292334	95373.020916	34.334490
1014.555996	95576.312772	34.339508
1015.462996	95765.651339	34.344525
1016.306975	95964.434824	34.349543
1017.501763	96160.747800	34.354560
1018.308750	96364.915560	34.359578
1019.075991	96569.705866	34.364596
1020.350162	96771.941983	34.369613
1021.137281	96982.524976	34.374631
1022.091247	97197.272257	34.379648
1023.305204	97398.618352	34.384666
1023.744023	97617.287665	34.389684
1025.186237	97821.295063	34.394701
1025.968390	98031.887592	34.399719
1027.427818	98244.252596	34.404736
1028.477281	98457.949492	34.409754
1029.440985	98677.272431	34.414772
1030.953998	98871.044626	34.419789
1032.115377	99068.519077	34.424807
1032.957348	99270.298171	34.429824
1034.002979	99464.338485	34.434842
1035.493955	99645.222940	34.439860
1036.761700	99822.360574	34.444877
1038.146147	99996.788479	34.449895
1038.847461	100170.150503	34.454912
1040.051869	100351.443551	34.459930
1040.607471	100534.153313	34.464948
1041.964814	100706.127566	34.469965
1043.093191	100895.326916	34.474983
1044.089968	101078.921083	34.480000
1045.741488	101246.485838	34.485018
1046.709538	101426.718763	34.490036
1047.908446	101593.527422	34.495053
1048.901025	101764.475678	34.500071
1050.020102	101933.757035	34.505088
1051.265449	102106.665204	34.510106
1052.050057	102293.660297	34.515124
1053.129252	102462.419990	34.520141
1053.872228	102635.886254	34.525159
1054.917346	102823.131794	34.530176
1056.406876	102996.307964	34.535194
1057.059730	103177.138809	34.540212
1058.045665	103361.181423	34.545229
1059.290819	103529.298950	34.550247
1060.091336	103710.589432	34.555264
1061.250456	103884.537247	34.560282
1061.993086	104076.643583	34.565300
1063.119521	104257.058749	34.570317
1064.059569	104453.440243	34.575335
1064.994439	104652.129209	34.580352
1066.259796	104849.306515	34.585370
1066.996116	105043.295424	34.590388
1068.836045	105223.404979	34.595405
1069.766683	105413.918192	34.600423
1070.924614	105595.451618	34.605440
1072.280952	105785.121952	34.610458
1073.480954	105969.842571	34.615476
1074.546965	106153.548765	34.620493
1075.568971	106337.960399	34.625511
1076.269405	106526.126964	34.630528
1077.740884	106704.092905	34.635546
1078.729163	106897.140061	34.640564
1079.529972	107093.957380	34.645581
1080.436117	107288.554063	34.650599
1081.597493	107481.601078	34.655616
1082.740291	107662.922996	34.660634
1083.965844	107856.747041	34.665652
1084.947307	108053.553046	34.670669
1086.158275	108241.276740	34.675687
1086.841638	108430.700815	34.680704
1088.306927	108622.424472	34.685722
1089.072369	108821.160440	34.690740
1090.152448	109019.831309	34.695757
1091.040547	109218.511150	34.700775
1091.711010	109428.162017	34.705792
1093.115027	109623.044774	34.710810
1093.617944	109828.331606	34.715828
1095.097900	110016.110056	34.720845
1096.429570	110211.883456	34.725863
1096.868450	110398.487255	34.730880
1098.511999	110589.611347	34.735898
1100.069233	110788.010552	34.740916
1100.901563	110974.208808	34.745933
1101.919054	111164.215197	34.750951
1102.649013	111362.861492	34.755968
1104.271384	111547.965494	34.760986
1105.258258	111753.513077	34.766004
1106.361473	111950.287990	34.771021
1107.818327	112141.087287	34.776039
1109.343770	112331.014639	34.781056
1110.441804	112511.919949	34.786074
1111.533368	112692.143388	34.791092
1112.897944	112874.234316	34.796109
1114.306985	113058.586641	34.801127
1115.923719	113244.133559	34.806144
1117.800185	113394.504350	34.811162
1118.897084	113554.739733	34.816180
1120.444514	113716.064506	34.821197
1121.185323	113876.818788	34.826215
1121.773598	114045.480779	34.831232
1123.079458	114210.295936	34.836250
1123.483064	114379.777063	34.841268
1124.535351	114561.539530	34.846285
1125.509724	114752.451724	34.851303
1126.244170	114949.754097	34.856320
1127.223336	115136.398139	34.861338
1127.815903	115333.588070	34.866356
1128.632800	115541.282863	34.871373
1129.527784	115753.704615	34.876391
1130.425788	115968.357470	34.881408
1131.388818	116182.772715	34.886426
1132.910142	116392.735161	34.891444
1133.606859	116619.490060	34.896461
1134.911953	116844.026493	34.901479
1135.506682	117077.150674	34.906496
1136.588681	117298.675048	34.911514
1138.107888	117534.330939	34.916532
1138.706944	117760.579255	34.921549
1140.230573	117991.258164	34.926567
1141.289259	118235.551917	34.931584
1142.453395	118474.279380	34.936602
1143.111169	118713.336243	34.941620
1144.307592	118952.682989	34.946637
1145.574342	119190.714407	34.951655
1146.502426	119445.989316	34.956672
1147.733966	119690.557007	34.961690
1148.485243	119949.668240	34.966708
1149.952280	120205.186901	34.971725
1151.172685	120447.646413	34.976743
1152.218405	120696.626279	34.981760
1153.618869	120943.355074	34.986778
1154.923302	121177.556070	34.991796
1155.791267	121411.643526	34.996813
1157.295064	121639.718240	35.001831
1158.016512	121884.872825	35.006848
1159.105495	122121.842830	35.011866
1160.395487	122361.226269	35.016884
1160.945514	122598.761205	35.021901
1162.726990	122834.439597	35.026919
1164.127154	123072.707189	35.031936
1165.678734	123307.541449	35.036954
1167.112382	123541.320423	35.041972
1168.720651	123765.819209	35.046989
1170.124013	123966.438558	35.052007
1171.536522	124195.840901	35.057024
1173.789756	124398.434189	35.062042
1174.969445	124606.535869	35.067060
1175.880187	124818.221192	35.072077
1177.038605	125021.221487	35.077095
1178.107647	125234.834461	35.082112
1179.068670	125447.453423	35.087130
1179.904622	125666.546765	35.092148
1181.194808	125886.299040	35.097165
1182.474581	126091.592426	35.102183
1184.045208	126299.866730	35.107200
1185.617533	126511.386993	35.112218
1187.005663	126722.065629	35.117236
1187.839692	126923.080501	35.122253
1189.258069	127135.962265	35.127271
1190.348086	127346.658117	35.132288
1191.638195	127546.990485	35.137306
1192.905541	127750.243442	35.142324
1193.786958	127950.648346	35.147341
1195.302612	128156.992339	35.152359
1196.770244	128365.424760	35.157376
1198.154974	128554.250235	35.162394
1199.432107	128750.967123	35.167412
1200.606172	128953.736744	35.172429
1201.802695	129147.059990	35.177447
1202.914226	129341.476449	35.182464
1204.741220	129524.185359	35.187482
1206.287884	129718.314125	35.192500
1207.644087	129911.703405	35.197517
1208.622546	130097.235613	35.202535
1209.318715	130285.238473	35.207552
1210.285658	130472.080520	35.212570
1211.942619	130669.973853	35.217588
1212.833839	130859.404516	35.222605
1214.756517	131043.246628	35.227623
1216.374981	131210.471491	35.232640
1217.885607	131385.093785	35.237658
1218.958657	131573.305852	35.242676
1220.069964	131752.600318	35.247693
1221.549827	131923.947360	35.252711
1221.732134	132107.320121	35.257728
1222.716868	132292.965273	35.262746
1224.175073	132473.281910	35.267764
1224.893325	132647.983239	35.272781
1226.420547	132826.160163	35.277799
1227.279408	133001.549258	35.282816
1227.896406	133171.630641	35.287834
1228.840414	133367.088829	35.292852
1229.770189	133560.255894	35.297869
1231.004728	133757.061239	35.302887
1231.867067	133968.676161	35.307904
1233.084378	134176.035174	35.312922
1234.375751	134389.658572	35.317940
1234.990234	134607.849334	35.322957
1235.871111	134823.992723	35.327975
1237.403030	135054.745878	35.332992
1238.224032	135286.712691	35.338010
1239.781161	135519.353858	35.343028
1240.367968	135763.497621	35.348045
1241.845358	135988.941436	35.353063
1242.837968	136241.907128	35.358080
1244.471252	136481.147681	35.363098
1245.701896	136712.940091	35.368116
1247.119833	136952.474425	35.373133
1248.338577	137204.242106	35.378151
1249.065390	137453.078147	35.383168
1250.211848	137696.468035	35.388186
1252.226259	137943.261381	35.393204
1253.468364	138189.072896	35.398221
1254.672191	138424.723501	35.403239
1255.731147	138677.277493	35.408256
1257.188754	138934.114339	35.413274
1258.512906	139181.313701	35.418292
1259.912356	139431.507146	35.423309
1261.520784	139684.468969	35.428327
1262.388225	139934.617628	35.433344
1263.567890	140180.403277	35.438362
1265.541336	140427.081905	35.443380
1266.310557	140685.127385	35.448397
1267.934966	140929.561425	35.453415
1269.183377	141180.757008	35.458432
1270.369338	141437.024763	35.463450
1272.262723	141678.298457	35.468468
1273.461748	141910.118430	35.473485
1274.822741	142145.932129	35.478503
1276.328807	142394.226289	35.483520
1277.144190	142633.750783	35.488538
1279.139483	142857.971326	35.493556
1280.839434	143094.291271	35.498573
1282.287201	143313.662607	35.503591
1283.655328	143535.192121	35.508608
1284.695028	143771.857823	35.513626
1286.101530	143990.999407	35.518644
1287.171864	144219.242068	35.523661
1288.201936	144451.944440	35.528679
1289.722098	144695.572460	35.533696
1290.587114	144916.232728	35.538714
1291.952166	145142.820121	35.543732
1292.703272	145371.479772	35.548749
1293.962802	145597.606123	35.553767
1295.281445	145814.287997	35.558784
1296.358923	146048.780677	35.563802
1297.677772	146262.877925	35.568820
1299.030775	146499.456997	35.573837
1300.242791	146725.205258	35.578855
1302.106679	146944.311645	35.583872
1303.442497	147182.508753	35.588890
1304.761722	147399.161789	35.593908
1306.199234	147626.449632	35.598925
1307.710057	147844.011010	35.603943
1309.165505	148080.037246	35.608960
1310.345201	148305.546966	35.613978
1311.712282	148521.729040	35.618996
1312.352670	148759.928409	35.624013
1313.558716	148997.385599	35.629031
1314.882024	149238.261474	35.634048
1316.106148	149475.680523	35.639066
1317.897634	149713.168833	35.644084
1318.759683	149960.647717	35.649101
1319.827940	150192.314076	35.654119
1321.276476	150437.222294	35.659136
1322.275283	150700.677128	35.664154
1323.613696	150960.283064	35.669172
1324.683800	151215.129333	35.674189
1325.529739	151475.114771	35.679207
1326.967480	151743.220191	35.684224
1328.044862	152020.179538	35.689242
1329.680293	152276.699182	35.694260
1331.112064	152556.328883	35.699277
1332.446449	152826.311426	35.704295
1333.956517	153085.217215	35.709312
1335.022984	153370.953269	35.714330
1336.359502	153642.209556	35.719348
1337.525535	153922.807797	35.724365
1338.651561	154208.463606	35.729383
1340.123980	154490.865473	35.734400
1340.947439	154778.936642	35.739418
1342.546461	155067.118167	35.744436
1343.644553	155355.603162	35.749453
1344.985578	155639.304192	35.754471
1346.640645	155942.958980	35.759488
1347.733347	156250.251672	35.764506
1349.014794	156535.364643	35.769524
1350.833046	156818.535568	35.774541
1352.678812	157110.939283	35.779559
1354.225735	157386.447402	35.784576
1356.290708	157655.183005	35.789594
1358.708411	157902.470695	35.794612
1361.228735	158143.031156	35.799629
1362.776557	158383.746786	35.804647
1364.504814	158599.351462	35.809664
1366.100077	158833.388421	35.814682
1367.354901	159029.576913	35.819700
1368.503045	159238.649024	35.824717
1370.018684	159439.463555	35.829735
1371.757166	159641.230493	35.834752
1373.177741	159827.346304	35.839770
1374.766688	160021.059045	35.844788
1376.204382	160215.597855	35.849805
1377.387853	160395.032588	35.854823
1378.927889	160585.698689	35.859840
1379.745464	160785.319653	35.864858
1380.525222	160976.244508	35.869876
1381.656820	161189.934645	35.874893
1382.704803	161412.521396	35.879911
1383.770599	161624.144224	35.884928
1384.889946	161851.681875	35.889946
1386.019226	162086.095751	35.894964
1387.375209	162313.963292	35.899981
1388.367164	162560.355106	35.904999
1390.117605	162795.072534	35.910016
1391.264499	163029.590021	35.915034
1392.558355	163281.808787	35.920052
1393.848604	163537.696491	35.925069
1394.773097	163786.948938	35.930087
1396.505734	164031.090698	35.935104
1398.029847	164286.765117	35.940122
1399.664727	164534.149234	35.945140
1400.930520	164784.402056	35.950157
1402.419691	165045.428690	35.955175
1404.221163	165278.450415	35.960192
1405.507061	165533.512998	35.965210
1406.763673	165790.904090	35.970228
1408.393426	166038.081747	35.975245
1409.805353	166294.725887	35.980263
1411.327748	166535.745168	35.985280
1412.514465	166793.293539	35.990298
1413.708935	167043.723465	35.995316
1415.580981	167296.246722	36.000333
1416.766746	167559.078293	36.005351
1417.805425	167809.564472	36.010368
1419.386074	168068.994103	36.015386
1420.403781	168345.906098	36.020404
1421.825159	168614.959297	36.025421
1422.144550	168892.070217	36.030439
1423.365142	169183.609003	36.035456
1424.905223	169491.401289	36.040474
1425.998774	169781.290505	36.045492
1427.449499	170093.340455	36.050509
1427.965211	170400.083099	36.055527
1429.407741	170701.250445	36.060544
1430.940999	171023.330286	36.065562
1432.071095	171340.405200	36.070580
1433.297703	171653.506314	36.075597
1434.851722	171988.457133	36.080615
1436.708619	172297.342877	36.085632
1437.521727	172628.110168	36.090650
1438.776978	172941.163985	36.095668
1440.382098	173262.954646	36.100685
1441.384645	173580.484898	36.105703
1443.242254	173892.489915	36.110720
1444.612847	174215.443770	36.115738
1446.007962	174537.189886	36.120756
1447.770638	174860.499657	36.125773
1449.357523	175186.697148	36.130791
1451.163857	175481.397369	36.135808
1452.566009	175807.732054	36.140826
1453.808036	176126.075225	36.145844
1455.656792	176445.001912	36.150861
1456.705990	176773.167361	36.155879
1457.987209	177103.719338	36.160896
1459.489243	177441.114631	36.165914
1461.034649	177771.194174	36.170932
1462.620105	178104.759273	36.175949
1464.068539	178444.569085	36.180967
1466.064055	178772.547244	36.185984
1467.588412	179110.749191	36.191002
1468.837802	179435.229208	36.196020
1470.876731	179761.289577	36.201037
1472.071236	180103.197055	36.206055
1473.723796	180424.631406	36.211072
1474.908662	180755.870284	36.216090
1476.316211	181082.770270	36.221108
1478.376130	181407.656680	36.226125
1479.898016	181732.954438	36.231143
1481.904480	182045.516361	36.236160
1483.929629	182367.495088	36.241178
1485.395419	182683.313743	36.246196
1487.325852	182995.259443	36.251213
1488.583161	183308.451793	36.256231
1490.152753	183613.709932	36.261248
1491.758653	183918.074995	36.266266
1492.839151	184223.305923	36.271284
1495.018491	184546.210223	36.276301
1495.868822	184868.544105	36.281319
1497.242764	185177.868081	36.286336
1498.961395	185499.841160	36.291354
1500.093461	185814.782519	36.296372
1502.163379	186129.412785	36.301389
1503.280676	186462.093528	36.306407
1504.920091	186771.329873	36.311424
1506.525606	187090.233843	36.316442
1507.651790	187395.880042	36.321460
1509.519130	187774.595786	36.326477
1510.715509	188119.979318	36.331495
1512.218724	188435.264807	36.336512
1513.429475	188759.031105	36.341530
1515.286819	189080.682773	36.346548
1516.652636	189404.134035	36.351565
1517.739410	189741.840063	36.356583
1519.253527	190067.491041	36.361600
1520.989152	190398.463038	36.366618
1521.652563	190713.827928	36.371636
1522.956287	191032.398221	36.376653
1524.678798	191366.335560	36.381671
1525.829468	191688.972403	36.386688
1527.246787	192021.111989	36.391706
1528.433882	192357.456734	36.396724
1530.168676	192684.454719	36.401741
1531.623455	193027.599935	36.406759
1533.280809	193371.270921	36.411776
1534.708599	193713.827741	36.416794
1536.799421	194063.852130	36.421812
1538.139170	194399.864064	36.426829
1539.605842	194749.668852	36.431847
1540.930959	195091.844215	36.436864
1542.358888	195447.816747	36.441882
1544.045543	195809.256902	36.446900
1545.323364	196155.013353	36.451917
1546.505696	196531.232851	36.456935
1548.057742	196895.126798	36.461952
1549.828044	197254.211604	36.466970
1550.972981	197628.399482	36.471988
1553.081244	198004.494035	36.477005
1554.242965	198381.158876	36.482023
1555.822430	198760.458591	36.487040
1557.000503	199147.104101	36.492058
1558.214958	199536.107047	36.497076
1560.112219	199918.164512	36.502093
1561.407803	200320.552739	36.507111
1562.720322	200720.527928	36.512128
1564.271840	201117.963148	36.517146
1565.774255	201516.386581	36.522164
1567.767967	201915.629578	36.527181
1569.871612	202327.045029	36.532199
1571.695424	202710.970674	36.537216
1573.401797	203091.667901	36.542234
1575.689891	203485.764615	36.547252
1577.762087	203853.655061	36.552269
1579.372715	204233.853761	36.557287
1580.741219	204615.048054	36.562304
1582.856294	204989.628064	36.567322
1584.733084	205345.763065	36.572340
1586.822949	205703.894814	36.577357
1588.513662	206057.004723	36.582375
1590.121992	206411.869858	36.587392
1592.062482	206755.607297	36.592410
1593.759288	207117.850448	36.597428
1595.349845	207458.349289	36.602445
1597.243355	207804.841887	36.607463
1598.579172	208150.961525	36.612480
1600.266108	208490.724310	36.617498
1601.797320	208830.896046	36.622516
1603.795892	209164.309978	36.627533
1605.511800	209502.014751	36.632551
1607.328766	209833.786197	36.637568
1608.836782	210161.294373	36.642586
1610.380319	210484.785038	36.647604
1612.296046	210782.257831	36.652621
1614.476133	211080.397497	36.657639
1615.830799	211373.193678	36.662656
1616.944011	211675.403581	36.667674
1618.206722	211981.779415	36.672692
1619.855984	212279.607518	36.677709
1621.697296	212587.867354	36.682727
1623.253769	212893.941998	36.687744
1625.177864	213200.081736	36.692762
1625.957357	213509.364414	36.697780
1627.940040	213820.626422	36.702797
1629.832345	214126.774606	36.707815
1631.707973	214444.914313	36.712832
1633.414832	214752.162921	36.717850
1634.158907	215076.492175	36.722868
1635.498785	215397.825200	36.727885
1636.928467	215719.880447	36.732903
1638.665063	216059.510482	36.737920
1640.017527	216397.988279	36.742938
1641.264631	216749.463734	36.747956
1643.237277	217095.609606	36.752973
1644.556054	217444.001982	36.757991
1645.672573	217801.141817	36.763008
1647.147564	218151.821091	36.768026
1648.391693	218521.742421	36.773044
1649.927807	218891.742069	36.778061
1651.622146	219271.951649	36.783079
1652.886538	219655.741170	36.788096
1654.790888	220043.791168	36.793114
1656.323012	220437.011428	36.798132
1657.609101	220812.444918	36.803149
1659.376197	221206.313430	36.808167
1660.831658	221606.738850	36.813184
1663.034418	222007.342586	36.818202
1664.496539	222413.713105	36.823220
1666.065907	222817.247304	36.828237
1667.670291	223225.780609	36.833255
1669.019716	223629.380543	36.838272
1671.625529	224033.833638	36.843290
1673.251156	224439.090744	36.848308
1675.524379	224838.624942	36.853325
1677.252535	225234.850026	36.858343
1678.062505	225641.977698	36.863360
1680.177698	226035.217972	36.868378
1681.595884	226435.792360	36.873396
1683.910955	226827.730749	36.878413
1685.951107	227226.880242	36.883431
1687.265790	227620.516076	36.888448
1689.240349	228010.153822	36.893466
1691.178808	228416.512482	36.898484
1693.225823	228806.952824	36.903501
1694.820569	229196.658759	36.908519
1696.262515	229592.538882	36.913536
1697.890665	229978.100791	36.918554
1699.259793	230356.417889	36.923572
1700.512528	230733.358763	36.928589
1702.461893	231118.258931	36.933607
1703.913818	231499.384146	36.938624
1705.305282	231872.849414	36.943642
1707.229492	232263.268691	36.948660
1708.746186	232658.381656	36.953677
1710.484217	233051.806580	36.958695
1712.160499	233452.685612	36.963712
1713.927076	233842.398819	36.968730
1715.463068	234247.215497	36.973748
1717.147245	234639.129067	36.978765
1719.023590	235040.714060	36.983783
1720.704656	235462.756366	36.988800
1722.340561	235853.791660	36.993818
1723.847584	236262.275492	36.998836
1725.731017	236672.550108	37.003853
1727.953640	237066.916672	37.008871
1729.542691	237479.173813	37.013888
1731.412667	237885.973047	37.018906
1733.167621	238303.105998	37.023924
1734.535087	238719.594761	37.028941
1736.548614	239131.833199	37.033959
1737.991318	239562.916914	37.038976
1739.851230	239976.656448	37.043994
1741.704421	240396.011759	37.049012
1743.491131	240821.907571	37.054029
1744.937044	241244.687082	37.059047
1746.495243	241669.429458	37.064064
1749.056568	242085.872077	37.069082
1750.669842	242516.702950	37.074100
1752.459180	242936.123978	37.079117
1754.579084	243354.879385	37.084135
1755.991617	243783.434803	37.089152
1758.171799	244207.032963	37.094170
1759.927510	244627.884583	37.099188
1761.325226	245055.961556	37.104205
1763.458075	245491.559540	37.109223
1765.326084	245914.451126	37.114240
1767.089940	246329.638530	37.119258
1769.087603	246745.853298	37.124276
1771.078749	247171.417882	37.129293
1773.268834	247577.769632	37.134311
1774.713398	248004.927305	37.139328
1776.666155	248417.544129	37.144346
1778.167852	248825.869144	37.149364
1780.014711	249252.832069	37.154381
1782.121069	249660.419214	37.159399
1783.787895	250081.926508	37.164416
1785.328433	250496.774684	37.169434
1786.909934	250918.881402	37.174452
1788.292778	251339.625186	37.179469
1790.099451	251768.476510	37.184487
1791.274077	252217.301436	37.189504
1793.223321	252634.214728	37.194522
1794.696812	253060.837379	37.199540
1796.117756	253488.510712	37.204557
1797.511557	253912.022711	37.209575
1799.048688	254348.262717	37.214592
1800.890180	254785.797140	37.219610
1802.160652	255236.638997	37.224628
1803.900385	255689.001058	37.229645
1805.723886	256143.635130	37.234663
1807.172125	256605.090679	37.239680
1808.771884	257069.873538	37.244698
1810.864997	257537.594967	37.249716
1812.273013	258020.014985	37.254733
1814.323933	258488.658034	37.259751
1815.816494	258976.321878	37.264768
1817.870294	259458.935967	37.269786
1819.623230	259944.751360	37.274804
1821.150926	260436.142985	37.279821
1823.030213	260910.809782	37.284839
1824.954632	261421.668102	37.289856
1827.219985	261928.581125	37.294874
1829.345602	262424.543583	37.299892
1830.624736	262923.597252	37.304909
1832.542482	263417.663917	37.309927
1834.226938	263921.321633	37.314944
1836.466547	264415.764257	37.319962
1838.561705	264922.704002	37.324980
1840.629449	265433.255144	37.329997
1842.470139	265923.903258	37.335015
1844.344994	266437.636236	37.340032
1846.386152	266930.509777	37.345050
1848.363300	267425.476695	37.350068
1850.340970	267925.269417	37.355085
1852.361657	268420.608610	37.360103
1854.450336	268928.433622	37.365120
1856.074999	269422.264135	37.370138
1857.885651	269924.800594	37.375156
1859.711099	270424.590224	37.380173
1861.685064	270911.982556	37.385191
1864.182953	271425.830098	37.390208
1866.328872	271904.325825	37.395226
1868.638037	272394.833537	37.400244
1870.448661	272885.298589	37.405261
1872.268236	273355.693305	37.410279
1874.728798	273846.858170	37.415296
1876.133769	274331.369375	37.420314
1878.156593	274814.579986	37.425332
1879.687050	275300.541004	37.430349
1881.683768	275776.107953	37.435367
1883.416294	276264.267635	37.440384
1885.697218	276743.517897	37.445402
1888.082611	277209.921205	37.450420
1889.744102	277693.415671	37.455437
1891.547261	278167.486048	37.460455
1893.271910	278658.232199	37.465472
1894.920631	279134.663515	37.470490
1896.563173	279594.786829	37.475508
1898.202398	280071.522116	37.480525
1900.319189	280529.631367	37.485543
1902.128100	280993.177146	37.490560
1903.915698	281450.095554	37.495578
1906.484850	281908.733313	37.500596
1907.627739	282363.930552	37.505613
1909.526773	282835.507869	37.510631
1911.647992	283299.527064	37.515648
1913.760253	283765.527663	37.520666
1916.351237	284234.188238	37.525684
1917.787087	284712.189182	37.530701
1919.515671	285172.739020	37.535719
1921.198027	285651.228117	37.540736
1923.184236	286131.568663	37.545754
1924.727169	286621.229119	37.550772
1926.303792	287110.958260	37.555789
1927.938678	287605.400097	37.560807
1930.004049	288107.005501	37.565824
1931.440690	288608.691106	37.570842
1933.275249	289120.974666	37.575860
1934.664931	289648.191140	37.580877
1936.429479	290165.892561	37.585895
1938.392019	290707.814561	37.590912
1940.320122	291243.669527	37.595930
1942.379539	291772.768770	37.600948
1944.156082	292321.522228	37.605965
1946.279339	292864.092570	37.610983
1948.701858	293401.249929	37.616000
1950.531075	293946.964003	37.621018
1953.184010	294483.492521	37.626036
1955.052009	295015.326879	37.631053
1957.335098	295539.366443	37.636071
1959.713240	296081.064423	37.641088
1961.376803	296618.132312	37.646106
1963.093941	297138.984216	37.651124
1964.779409	297690.875201	37.656141
1967.098392	298240.089601	37.661159
1969.167433	298785.127662	37.666176
1970.443526	299333.345985	37.671194
1972.310817	299876.964720	37.676212
1974.325200	300442.193650	37.681229
1975.938881	300999.893953	37.686247
1977.852302	301566.403160	37.691264
1979.480949	302139.662301	37.696282
1981.811708	302721.788118	37.701300
1983.427721	303289.683352	37.706317
1985.653421	303864.835567	37.711335
1988.022278	304438.562692	37.716352
1989.805871	305019.928663	37.721370
1992.020117	305599.490073	37.726388
1993.739663	306178.268615	37.731405
1995.929754	306728.697514	37.736423
1998.067838	307308.564701	37.741440
1999.641842	307873.210961	37.746458
2002.194890	308425.318479	37.751476
2004.467427	308969.673929	37.756493
2006.845095	309505.221094	37.761511
2009.229284	310046.477169	37.766528
2011.097523	310571.920888	37.771546
2013.183902	311094.124014	37.776564
2015.092525	311630.929971	37.781581
2017.453821	312155.237141	37.786599
2019.690793	312698.606943	37.791616
2021.404496	313234.368018	37.796634
2023.058413	313770.643206	37.801652
2024.911024	314307.921505	37.806669
2027.034549	314851.319830	37.811687
2029.327781	315401.083839	37.816704
2031.174020	315954.373298	37.821722
2033.440851	316502.177871	37.826740
2035.046942	317057.353124	37.831757
2037.112625	317611.861217	37.836775
2039.331539	318169.563237	37.841792
2040.662963	318736.629368	37.846810
2042.459028	319292.159800	37.851828
2044.558127	319858.094697	37.856845
2046.702349	320436.280579	37.861863
2049.265348	321014.719702	37.866880
2050.786783	321592.722304	37.871898
2052.879170	322170.799690	37.876916
2054.830841	322769.105943	37.881933
2056.531857	323349.854409	37.886951
2058.795901	323941.266093	37.891968
2060.542900	324546.267334	37.896986
2062.907862	325139.884255	37.902004
2064.437668	325745.418299	37.907021
2066.503224	326355.246675	37.912039
2068.544722	326962.254765	37.917056
2070.605472	327576.387136	37.922074
2073.022339	328184.181390	37.927092
2075.020883	328812.731159	37.932109
2077.188881	329431.191808	37.937127
2079.349505	330047.285958	37.942144
2080.969736	330686.998706	37.947162
2083.033409	331304.923256	37.952180
2085.113436	331928.702107	37.957197
2087.003783	332568.372050	37.962215
2089.567349	333201.293776	37.967232
2091.677499	333830.401661	37.972250
2093.495490	334458.790491	37.977268
2095.532599	335108.355444	37.982285
2097.205199	335761.934490	37.987303
2099.428412	336402.643223	37.992320
2101.374368	337055.803706	37.997338
2103.485623	337705.373926	38.002356
2105.814505	338355.431588	38.007373
2107.780770	339013.411265	38.012391
2110.250380	339670.966174	38.017408
2112.503058	340306.365967	38.022426
2114.852765	340930.446278	38.027444
2117.468875	341541.681051	38.032461
2119.178956	342156.387822	38.037479
2122.019892	342762.162526	38.042496
2123.863822	343371.475484	38.047514
2126.042502	343973.972358	38.052532
2128.180476	344579.437791	38.057549
2130.914986	345177.737994	38.062567
2133.459565	345777.204939	38.067584
2135.312318	346373.711563	38.072602
2138.127752	346959.361664	38.077620
2139.970491	347557.377094	38.082637
2141.880740	348149.790025	38.087655
2144.683878	348741.154222	38.092672
2146.845011	349338.355392	38.097690
2149.094776	349936.497599	38.102708
2150.412314	350527.178266	38.107725
2152.562636	351131.994917	38.112743
2154.516219	351738.029363	38.117760
2156.299070	352363.826010	38.122778
2158.448861	352977.523265	38.127796
2160.059129	353607.949232	38.132813
2162.145857	354254.954761	38.137831
2164.199364	354881.429001	38.142848
2166.766431	355527.241584	38.147866
2168.541314	356157.270971	38.152884
2170.783950	356807.888927	38.157901
2172.606174	357459.862321	38.162919
2174.709228	358124.691148	38.167936
2176.416696	358789.348274	38.172954
2178.556675	359457.751312	38.177972
2180.649689	360130.489376	38.182989
2183.093037	360809.422323	38.188007
2185.434732	361479.862230	38.193024
2187.479856	362168.809648	38.198042
2190.105695	362835.220019	38.203060
2192.356913	363519.693965	38.208077
2194.364802	364202.066378	38.213095
2196.896862	364874.570655	38.218112
2198.781553	365566.705707	38.223130
2200.753874	366252.268574	38.228148
2203.394721	366938.592290	38.233165
2205.315034	367624.189403	38.238183
2207.673854	368308.785621	38.243200
2210.321593	368993.776148	38.248218
2213.137814	369681.565643	38.253236
2216.123485	370342.681844	38.258253
2218.616535	371008.815770	38.263271
2221.219947	371671.063327	38.268288
2223.306257	372334.401372	38.273306
2225.233739	372986.899501	38.278324
2227.526764	373645.688504	38.283341
2229.407184	374318.077925	38.288359
2231.573912	374984.166849	38.293376
2233.837985	375648.273580	38.298394
2235.557854	376302.139463	38.303412
2237.417533	376942.960105	38.308429
2239.440738	377599.766762	38.313447
2241.284978	378257.909779	38.318464
2242.587636	378923.004131	38.323482
2244.342158	379603.602036	38.328500
2246.318860	380292.642130	38.333517
2248.072105	381006.680842	38.338535
2250.500366	381709.508617	38.343552
2252.230682	382422.252555	38.348570
2254.140561	383141.770188	38.353588
2256.380848	383870.697235	38.358605
2258.123213	384598.197012	38.363623
2260.181184	385352.194817	38.368640
2262.020911	386113.386322	38.373658
2264.174685	386880.285620	38.378676
2267.191519	387633.735210	38.383693
2269.530258	388410.198175	38.388711
2272.326601	389173.863727	38.393728
2274.788604	389939.493883	38.398746
2277.037795	390709.906515	38.403764
2279.798348	391473.267168	38.408781
2282.320589	392227.068430	38.413799
2285.010347	392986.702251	38.418816
2287.438986	393753.331178	38.423834
2289.613132	394517.221288	38.428852
2292.348055	395278.968271	38.433869
2295.057911	396032.919511	38.438887
2297.850575	396773.456444	38.443904
2300.716622	397512.111997	38.448922
2303.105057	398253.389717	38.453940
2305.798808	398981.824632	38.458957
2308.414247	399717.501468	38.463975
2310.620721	400445.247406	38.468992
2312.911151	401173.872432	38.474010
2315.398002	401900.874068	38.479028
2318.003552	402629.610106	38.484045
2319.918805	403364.829811	38.489063
2322.009105	404087.534959	38.494080
2324.305719	404827.185629	38.499098
2326.220184	405576.711359	38.504116
2328.486740	406316.960232	38.509133
2330.470981	407068.155636	38.514151
2333.058195	407809.398198	38.519168
2334.933204	408563.635762	38.524186
2337.069753	409324.747959	38.529204
2339.592402	410085.721718	38.534221
2341.182466	410853.494609	38.539239
2343.408621	411634.281879	38.544256
2345.343535	412420.211870	38.549274
2347.335189	413213.909173	38.554292
2349.507163	414005.145374	38.559309
2351.924121	414823.692186	38.564327
2354.179887	415622.309996	38.569344
2356.202208	416423.576409	38.574362
2358.259212	417213.517562	38.579380
2360.492798	417997.605057	38.584397
2362.899650	418792.222847	38.589415
2364.774275	419588.906712	38.594432
2367.262656	420402.778916	38.599450
2369.202768	421208.312211	38.604468
2371.343250	422025.785730	38.609485
2373.115690	422858.333374	38.614503
2375.455470	423688.629066	38.619520
2377.485651	424526.341422	38.624538
2379.986969	425379.841785	38.629556
2382.505541	426225.917282	38.634573
2385.180524	427082.010610	38.639591
2387.702356	427944.376659	38.644608
2390.219314	428795.069068	38.649626
2392.645644	429657.490108	38.654644
2395.261817	430523.390230	38.659661
2398.249887	431386.916881	38.664679
2400.489081	432241.074474	38.669696
2403.173554	433116.584086	38.674714
2405.491433	433987.213743	38.679732
2408.195965	434842.055428	38.684749
2410.347843	435711.534201	38.689767
2412.951419	436581.003563	38.694784
2415.475103	437449.491544	38.699802
2417.693406	438332.520518	38.704820
2420.085750	439200.355691	38.709837
2422.477492	440079.389537	38.714855
2425.047613	440948.997831	38.719872
2427.906810	441827.325458	38.724890
2430.395326	442711.752054	38.729908
2432.830921	443593.723480	38.734925
2435.679308	444470.681511	38.739943
2438.267662	445349.874019	38.744960
2441.075734	446213.969891	38.749978
2443.766179	447085.587390	38.754996
2446.539541	447942.436612	38.760013
2449.056678	448817.451852	38.765031
2451.149642	449686.586025	38.770048
2453.814526	450541.122737	38.775066
2455.999153	451422.508707	38.780084
2458.918750	452281.380590	38.785101
2461.346145	453158.100102	38.790119
2463.659348	454029.795968	38.795136
2466.072698	454895.976970	38.800154
2468.289185	455778.081043	38.805172
2470.584025	456641.781124	38.810189
2473.022841	457534.792167	38.815207
2475.443633	458406.837798	38.820224
2478.195744	459271.105138	38.825242
2480.433758	460168.127690	38.830260
2483.444290	461045.618527	38.835277
2485.801797	461928.185848	38.840295
2488.570085	462804.123513	38.845312
2491.278379	463670.783562	38.850330
2493.526499	464522.827987	38.855348
2496.068577	465351.387115	38.860365
2498.810380	466197.360965	38.865383
2501.201436	467028.552153	38.870400
2503.591772	467855.058844	38.875418
2506.088219	468704.046333	38.880436
2508.362629	469540.503965	38.885453
2510.836975	470390.177719	38.890471
2512.764450	471240.967600	38.895488
2515.294584	472099.547171	38.900506
2517.460919	472976.031762	38.905524
2519.910155	473855.255497	38.910541
2522.277973	474729.552054	38.915559
2524.386761	475616.983502	38.920576
2527.135087	476503.303295	38.925594
2529.477708	477396.669448	38.930612
2532.159995	478291.196356	38.935629
2534.343500	479197.126473	38.940647
2536.329439	480119.102474	38.945664
2538.916715	481033.001262	38.950682
2541.188186	481964.881908	38.955700
2543.531476	482902.103854	38.960717
2546.261759	483849.812085	38.965735
2548.217355	484795.178922	38.970752
2550.693188	485762.415112	38.975770
2552.572272	486741.208647	38.980788
2554.875744	487718.966402	38.985805
2557.685344	488707.888202	38.990823
2560.272703	489701.535562	38.995840
2563.475086	490684.069802	39.000858
2566.183219	491677.027501	39.005876
2568.623295	492667.652311	39.010893
2571.050206	493658.171353	39.015911
2573.481214	494672.748426	39.020928
2576.274935	495676.608118	39.025946
2578.932116	496692.639404	39.030964
2581.378619	497707.837969	39.035981
2584.410087	498724.791531	39.040999
2586.654030	499753.064987	39.046016
2589.145119	500769.127987	39.051034
2591.700784	501793.438426	39.056052
2594.093572	502830.017175	39.061069
2596.747951	503859.476317	39.066087
2599.487184	504909.982463	39.071104
2602.210411	505930.928311	39.076122
2604.312722	506979.795227	39.081140
2607.080311	508027.370822	39.086157
2609.218115	509083.806836	39.091175
2611.865008	510139.228793	39.096192
2614.917891	511196.930312	39.101210
2617.763119	512252.580406	39.106228
2620.303288	513312.797590	39.111245
2624.105106	514356.148395	39.116263
2627.112650	515395.130788	39.121280
2629.968160	516416.283599	39.126298
2633.055754	517420.249788	39.131316
2635.381458	518403.474280	39.136333
2637.959360	519385.786550	39.141351
2640.653208	520368.217240	39.146368
2643.353778	521359.548901	39.151386
2645.754845	522341.750664	39.156404
2648.351180	523334.783673	39.161421
2650.975499	524326.587991	39.166439
2653.107956	525314.684303	39.171456
2656.031229	526311.844778	39.176474
2658.591125	527317.207208	39.181492
2661.169908	528323.756699	39.186509
2664.159664	529320.350537	39.191527
2666.572527	530334.342017	39.196544
2669.663760	531328.264964	39.201562
2672.385760	532334.514377	39.206580
2674.982525	533352.089515	39.211597
2677.971779	534358.857171	39.216615
2680.519913	535377.354561	39.221632
2683.403648	536384.350576	39.226650
2686.018402	537404.252212	39.231668
2688.723434	538416.921312	39.236685
2691.540326	539439.862126	39.241703
2693.988776	540469.129981	39.246720
2697.071728	541483.727991	39.251738
2699.931780	542513.681091	39.256756
2702.456179	543544.772308	39.261773
2705.246169	544568.801997	39.266791
2707.976961	545604.633264	39.271808
2710.704053	546625.202750	39.276826
2713.516237	547670.468473	39.281844
2716.089375	548710.014499	39.286861
2718.748049	549739.463233	39.291879
2721.210091	550793.145823	39.296896
2723.730878	551846.937529	39.301914
2726.303013	552902.950084	39.306932
2729.026969	553966.894372	39.311949
2732.008158	555025.635068	39.316967
2734.547547	556095.773020	39.321984
2737.518217	557162.033350	39.327002
2740.634397	558229.087308	39.332020
2742.941943	559301.065820	39.337037
2746.172609	560367.274066	39.342055
2749.299806	561439.239354	39.347072
2752.129328	562512.021251	39.352090
2754.606766	563567.600694	39.357108
2757.352814	564629.224461	39.362125
2760.656971	565692.372704	39.367143
2763.480169	566755.615684	39.372160
2766.041889	567823.282994	39.377178
2769.079940	568881.192254	39.382196
2771.636852	569948.029950	39.387213
2774.909541	571010.640619	39.392231
2777.788047	572073.128915	39.397248
2780.381696	573123.583405	39.402266
2783.270566	574153.327749	39.407284
2786.121834	575161.470356	39.412301
2789.207607	576164.524817	39.417319
2791.778536	577174.659214	39.422336
2794.292171	578178.049862	39.427354
2797.104131	579194.097425	39.432372
2798.884507	580233.808043	39.437389
2801.460297	581263.867106	39.442407
2803.935184	582313.261510	39.447424
2806.700855	583358.153812	39.452442
2809.262017	584426.553706	39.457460
2811.473899	585502.388057	39.462477
2814.109867	586577.903541	39.467495
2816.351787	587678.600237	39.472512
2818.493352	588781.518130	39.477530
2821.268508	589896.101934	39.482548
2823.810963	591027.456413	39.487565
2826.570877	592156.210682	39.492583
2829.368594	593294.769480	39.497600
2832.606199	594447.869600	39.502618
2835.339025	595608.204876	39.507636
2838.162931	596751.932509	39.512653
2841.563888	597915.429428	39.517671
2844.255872	599081.684483	39.522688
2846.828951	600250.946092	39.527706
2850.254326	601426.250881	39.532724
2852.526229	602616.548733	39.537741
2855.322311	603797.824057	39.542759
2858.001963	604988.104814	39.547776
2860.242542	606191.946420	39.552794
2863.650045	607405.617343	39.557812
2866.429508	608614.411757	39.562829
2869.659443	609822.848760	39.567847
2872.595753	611043.359563	39.572864
2875.528951	612265.437417	39.577882
2878.672575	613482.043803	39.582900
2881.570070	614698.908197	39.587917
2884.846961	615906.723860	39.592935
2888.184530	617120.644904	39.597952
2891.340148	618331.912856	39.602970
2894.807582	619548.740369	39.607988
2897.444979	620736.038479	39.613005
2900.770457	621945.024771	39.618023
2903.919544	623144.212632	39.623040
2907.060327	624333.326360	39.628058
2910.026765	625536.523901	39.633076
2912.692829	626735.541288	39.638093
2916.126916	627925.352731	39.643111
2918.830599	629127.439079	39.648128
2921.669091	630317.332426	39.653146
2924.757211	631501.656635	39.658164
2927.721320	632712.274572	39.663181
2930.842579	633904.856711	39.668199
2933.627885	635098.956450	39.673216
2936.240519	636283.716490	39.678234
2939.372986	637439.462468	39.683252
2941.878914	638600.274404	39.688269
2944.431572	639751.868192	39.693287
2946.936956	640913.016725	39.698304
2949.442764	642081.414024	39.703322
2952.304269	643253.455921	39.708340
2954.917743	644440.163299	39.713357
2958.058028	645623.500293	39.718375
2960.793169	646821.323156	39.723392
2963.444032	648033.023153	39.728410
2966.683442	649234.757483	39.733428
2969.091768	650452.534244	39.738445
2971.674296	651679.847635	39.743463
2974.678507	652918.644029	39.748480
2977.012977	654163.625627	39.753498
2980.067483	655419.184110	39.758516
2982.554236	656689.767693	39.763533
2985.770160	657963.646327	39.768551
2988.637768	659249.465752	39.773568
2991.279083	660541.674267	39.778586
2994.367116	661836.818968	39.783604
2997.231939	663135.957988	39.788621
3000.634424	664438.959120	39.793639
3004.303721	665753.229722	39.798656
3007.212388	667055.957511	39.803674
3010.829379	668362.513704	39.808692
3012.870523	669685.470438	39.813709
3016.166170	670992.761605	39.818727
3019.809733	672319.350356	39.823744
3022.413169	673642.647654	39.828762
3025.697651	674973.096307	39.833780
3028.547854	676307.553332	39.838797
3031.900131	677636.465119	39.843815
3034.944918	678974.578156	39.848832
3037.802179	680309.746587	39.853850
3041.115266	681642.407466	39.858868
3044.090989	682995.639701	39.863885
3047.612246	684326.730103	39.868903
3050.839426	685667.505038	39.873920
3053.903341	687013.171894	39.878938
3056.859944	688351.558658	39.883956
3059.734274	689700.081418	39.888973
3062.680520	691050.472302	39.893991
3065.780665	692401.624333	39.899008
3068.895572	693761.793896	39.904026
3072.436363	695099.513428	39.909044
3075.523617	696468.941326	39.914061
3078.253112	697822.302371	39.919079
3081.507984	699183.246137	39.924096
3084.609146	700544.003844	39.929114
3087.524709	701900.764570	39.934132
3090.339423	703271.351828	39.939149
3093.276854	704637.539327	39.944167
3096.270435	706011.920625	39.949184
3099.265746	707392.915555	39.954202
3101.947949	708730.167499	39.959220
3104.894284	710079.392753	39.964237
3108.226271	711416.111330	39.969255
3111.367678	712755.373315	39.974272
3114.288289	714095.054131	39.979290
3118.070248	715442.983155	39.984308
3121.060492	716778.067734	39.989325
3124.143885	718116.780841	39.994343
3127.345592	719467.918155	39.999360
3129.862995	720828.742168	40.004378
3132.930892	722184.106907	40.009396
3136.401732	723543.232992	40.014413
3139.637602	724911.514566	40.019431
3143.021004	726271.438820	40.024448
3146.116171	727642.350693	40.029466
3149.759451	728998.168898	40.034484
3152.983359	730366.524208	40.039501
3156.255469	731742.786893	40.044519
3159.612697	733113.714787	40.049536
3162.017011	734499.971869	40.054554
3165.034668	735883.465786	40.059572
3168.114405	737292.614518	40.064589
3170.725251	738692.762530	40.069607
3173.944267	740101.635241	40.074624
3176.895283	741528.549679	40.079642
3180.125333	742951.262361	40.084660
3183.013967	744382.649103	40.089677
3185.975108	745832.047984	40.094695
3189.311544	747263.421223	40.099712
3192.701054	748721.423903	40.104730
3196.065231	750164.820747	40.109748
3199.272525	751631.911259	40.114765
3202.583222	753096.635791	40.119783
3205.809828	754559.174405	40.124800
3208.488110	756032.503551	40.129818
3212.091982	757497.711725	40.134836
3215.192252	758984.176393	40.139853
3218.273036	760466.711439	40.144871
3221.664412	761966.461048	40.149888
3224.489045	763466.696146	40.154906
3227.817336	764955.039334	40.159924
3230.821707	766464.523740	40.164941
3234.050657	767970.959972	40.169959
3237.017845	769477.036038	40.174976
3240.084559	771003.273370	40.179994
3243.267885	772517.926320	40.185012
3246.370541	774051.578569	40.190029
3249.370012	775599.213101	40.195047
3252.762346	777146.451366	40.200064
3255.731746	778689.358465	40.205082
3259.346634	780236.830436	40.210100
3262.604571	781796.392240	40.215117
3265.417635	783351.228150	40.220135
3268.673635	784913.005197	40.225152
3271.932118	786471.155103	40.230170
3275.296360	788003.557550	40.235188
3278.852981	789525.403305	40.240205
3282.157559	791042.505667	40.245223
3285.575926	792555.293892	40.250240
3288.420735	794072.995099	40.255258
3291.451997	795586.173239	40.260276
3294.934933	797111.769448	40.265293
3298.095192	798648.927799	40.270311
3301.062646	800184.798813	40.275328
3304.039997	801741.016595	40.280346
3307.280334	803291.604208	40.285364
3310.443726	804857.792489	40.290381
3313.586020	806443.030415	40.295399
3316.959080	808012.123381	40.300416
3320.199163	809605.060303	40.305434
3323.801356	811196.533815	40.310452
3326.987089	812791.852943	40.315469
3329.864449	814399.783296	40.320487
3333.780431	815999.730164	40.325504
3336.859412	817610.073807	40.330522
3340.251669	819222.851732	40.335540
3343.656256	820850.696161	40.340557
3347.086186	822472.916548	40.345575
3350.951382	824092.565679	40.350592
3354.030359	825734.270874	40.355610
3357.218712	827367.650506	40.360628
3360.731561	828997.300485	40.365645
3364.107623	830643.804555	40.370663
3367.696422	832288.878622	40.375680
3371.145548	833933.312524	40.380698
3374.914452	835572.744250	40.385716
3378.192679	837229.402638	40.390733
3381.424726	838883.400512	40.395751
3385.097994	840535.724942	40.400768
3388.568615	842193.388738	40.405786
3392.033864	843848.576197	40.410804
3395.483748	845502.066788	40.415821
3398.760533	847154.275782	40.420839
3402.524446	848802.564622	40.425856
3405.615978	850469.757017	40.430874
3408.888051	852134.431449	40.435892
3412.680013	853805.652805	40.440909
3416.238243	855469.862702	40.445927
3419.530098	857136.673266	40.450944
3422.860132	858812.040772	40.455962
3426.454540	860481.958297	40.460980
3430.082092	862152.089135	40.465997
3432.980273	863822.174035	40.471015
3436.624851	865507.941565	40.476032
3439.780855	867198.645346	40.481050
3443.297056	868882.711482	40.486068
3446.672220	870579.198002	40.491085
3449.653131	872276.719140	40.496103
3453.263107	873963.780944	40.501120
3456.590078	875645.156188	40.506125
3459.787304	877288.827770	40.511130
3462.698804	878873.566485	40.516135
3465.562453	880407.514708	40.521140
3468.476760	881861.545453	40.526144
3471.568417	883261.061865	40.531149
3474.763886	884584.916849	40.536154
3477.533050	885834.606730	40.541159
3480.466363	887017.044444	40.546164
3483.328154	888125.926456	40.551168
3486.065614	889156.467937	40.556173
3488.339115	890116.118010	40.561178
3490.810861	891006.926089	40.566183
3492.757033	891839.294935	40.571188
3495.223952	892587.263224	40.576192
3497.304728	893285.522241	40.581197
3498.892383	893918.356613	40.586202
3501.038949	894490.826437	40.591207
3502.253189	895004.557105	40.596212
3504.195505	895474.352429	40.601216
3506.038988	895883.072404	40.606221
3507.682218	896234.418275	40.611226
3509.261419	896533.496887	40.616231
3510.399325	896800.857620	40.621236
3512.167985	897009.375008	40.626240
3513.047356	897183.557017	40.631245
3514.094228	897314.824071	40.636250
3515.527295	897407.777559	40.641255
3516.263417	897473.227684	40.646260
3517.756504	897493.929868	40.651264
3518.853480	897491.038492	40.656269
3519.809884	897446.063747	40.661274
3520.416329	897365.511118	40.666279
3520.699414	897268.014497	40.671284
3521.686179	897139.393298	40.676288
3522.276296	897003.689638	40.681293
3522.843766	896831.573256	40.686298
3523.777504	896635.627840	40.691303
3523.975404	896432.749868	40.696308
3524.822217	896197.586730	40.701312
3525.390720	895957.438008	40.706317
3525.747492	895683.792708	40.711322
3526.339389	895396.085336	40.716327
3526.502097	895115.876103	40.721332
3527.180555	894794.597326	40.726336
3527.405245	894470.575605	40.731341
3528.247655	894137.636307	40.736346
3528.157214	893782.223153	40.741351
3528.557246	893425.350997	40.746356
3528.836983	893050.016501	40.751360
3529.096009	892664.801630	40.756365
3529.377775	892284.100062	40.761370
3529.860357	891877.140793	40.766375
3530.025442	891470.206680	40.771380
3530.144644	891049.618699	40.776384
3530.072825	890627.678649	40.781389
3530.547951	890198.941774	40.786394
3530.909340	889757.523505	40.791399
3530.883283	889311.108157	40.796404
3530.797642	888856.736932	40.801408
3531.258146	888405.622047	40.806413
3531.160233	887959.694154	40.811418
3531.523243	887494.207100	40.816423
3531.601239	887027.666738	40.821428
3531.937597	886550.497452	40.826432
3532.230280	886073.683188	40.831437
3532.144984	885584.409699	40.836442
3532.241633	885094.192604	40.841447
3532.232953	884598.531418	40.846452
3532.414630	884099.987984	40.851456
3532.444783	883597.555046	40.856461
3532.628180	883103.282042	40.861466
3532.648249	882595.826240	40.866471
3532.611470	882093.952298	40.871476
3532.655662	881573.523865	40.876480
3532.656369	881059.061224	40.881485
3532.754329	880544.923989	40.886490
3533.154749	880033.886518	40.891495
3532.794037	879505.786647	40.896500
3533.174461	878973.637004	40.901504
3533.231583	878451.958991	40.906509
3532.835223	877931.377865	40.911514
3533.532663	877398.934108	40.916519
3533.288360	876866.699733	40.921524
3533.471779	876324.263217	40.926528
3533.284337	875791.340155	40.931533
3533.206075	875253.114937	40.936538
3533.666653	874704.955786	40.941543
3532.957348	874162.472553	40.946548
3533.152677	873620.657835	40.951552
3533.260296	873079.778293	40.956557
3533.426536	872540.779198	40.961562
3533.608346	871988.342026	40.966567
3533.385435	871448.922087	40.971572
3533.486846	870896.494027	40.976576
3533.587443	870351.194976	40.981581
3533.240616	869792.919155	40.986586
3533.815892	869245.497059	40.991591
3533.532955	868697.491839	40.996596
3533.207031	868139.640031	41.001600
3533.189333	867593.817870	41.006605
3533.255203	867036.961230	41.011610
3533.372519	866473.538849	41.016615
3533.832581	865923.210872	41.021620
3533.904634	865361.245438	41.026624
3533.685751	864805.589917	41.031629
3533.098637	864237.804858	41.036634
3533.771631	863669.362628	41.041639
3533.584072	863114.711474	41.046644
3533.383358	862541.357679	41.051648
3533.634060	861982.447229	41.056653
3533.625756	861415.852640	41.061658
3533.719965	860841.607281	41.066663
3533.829664	860276.635407	41.071668
3533.813366	859710.368877	41.076672
3533.751899	859139.196801	41.081677
3533.311455	858552.869539	41.086682
3534.062283	857981.741952	41.091687
3533.532623	857400.277791	41.096692
3533.549957	856823.332786	41.101696
3534.073753	856246.830454	41.106701
3533.711074	855681.513482	41.111706
3533.719056	855095.167038	41.116711
3533.702150	854521.318485	41.121716
3533.839780	853936.298554	41.126720
3533.827022	853353.875847	41.131725
3533.499239	852781.864191	41.136730
3533.942428	852193.901932	41.141735
3533.395952	851616.661606	41.146740
3533.614730	851024.927904	41.151744
3533.826483	850448.422532	41.156749
3533.448003	849871.380151	41.161754
3534.091815	849288.851807	41.166759
3533.767590	848711.789757	41.171764
3533.676051	848111.554281	41.176768
3534.056119	847533.775860	41.181773
3533.694859	846949.641863	41.186778
3533.988489	846364.659521	41.191783
3533.696003	845775.533375	41.196788
3533.989615	845177.482966	41.201792
3533.932574	844595.707774	41.206797
3533.812520	843991.865950	41.211802
3533.716178	843397.610391	41.216807
3533.480866	842815.505810	41.221812
3533.644525	842222.167001	41.226816
3534.064248	841632.433092	41.231821
3533.771747	841039.743338	41.236826
3534.030489	840426.428061	41.241831
3533.783119	839850.487321	41.246836
3533.664607	839253.163659	41.251840
3534.026323	838656.043129	41.256845
3533.927336	838056.311516	41.261850
3533.797780	837443.310552	41.266855
3533.661537	836855.178067	41.271860
3533.781524	836258.605514	41.276864
3533.937024	835657.336226	41.281869
3533.672352	835059.497621	41.286874
3533.744208	834455.641177	41.291879
3533.597658	833859.231864	41.296884
3533.630498	833261.125847	41.301888
3533.740836	832672.957241	41.306893
3533.327478	832058.463651	41.311898
3533.679530	831464.529496	41.316903
3533.657954	830866.698416	41.321908
3533.635744	830259.680946	41.326912
3533.538405	829656.819032	41.331917
3533.377849	829050.541876	41.336922
3533.403372	828446.178802	41.341927
3533.230186	827858.059664	41.346932
3533.628609	827260.654346	41.351936
3533.748891	826654.154302	41.356941
3533.517801	826056.208483	41.361946
3533.755982	825434.769869	41.366951
3533.496231	824837.694600	41.371956
3533.496298	824228.692727	41.376960
3533.521560	823627.352846	41.381965
3533.106618	823025.446334	41.386970
3533.446799	822415.778006	41.391975
3533.325990	821813.465757	41.396980
3533.138658	821210.131778	41.401984
3533.309782	820609.762168	41.406989
3533.353555	820002.317155	41.411994
3533.102961	819393.350295	41.416999
3532.930889	818795.711215	41.422004
3533.159525	818204.456104	41.427008
3533.172250	817595.278935	41.432013
3533.323446	817000.554011	41.437018
3533.307274	816385.399421	41.442023
3533.213030	815773.626934	41.447028
3533.041686	815165.726809	41.452032
3533.020047	814552.312697	41.457037
3532.527397	813955.565981	41.462042
3533.133144	813358.970170	41.467047
3532.802522	812758.662247	41.472052
3532.744073	812152.574311	41.477056
3533.134753	811550.860109	41.482061
3532.740839	810943.985932	41.487066
3532.825400	810336.632536	41.492071
3533.178349	809740.689293	41.497076
3532.800373	809131.934941	41.502080
3533.039736	808527.380522	41.507085
3533.147392	807913.191635	41.512090
3532.906503	807300.035582	41.517095
3532.892072	806696.341172	41.522100
3533.066449	806082.220233	41.527104
3532.924870	805470.499422	41.532109
3532.712688	804867.215640	41.537114
3532.878513	804254.598022	41.542119
3532.906655	803646.312250	41.547124
3532.813468	803036.571241	41.552128
3532.585166	802425.965439	41.557133
3532.540458	801818.069133	41.562138
3532.673454	801199.544461	41.567143
3532.618465	800601.007554	41.572148
3532.679543	799994.550570	41.577152
3532.417910	799382.404860	41.582157
3532.353631	798787.146005	41.587162
3532.523574	798166.331477	41.592167
3532.640987	797556.363545	41.597172
3532.530255	796952.269668	41.602176
3532.785002	796335.546084	41.607181
3532.554806	795730.777444	41.612186
3532.643546	795113.188521	41.617191
3532.618450	794510.291422	41.622196
3532.590105	793898.898523	41.627200
3532.877530	793281.113564	41.632205
3532.470859	792670.070604	41.637210
3532.493942	792053.106295	41.642215
3532.524546	791449.297539	41.647220
3532.434347	790829.494792	41.652224
3532.535422	790215.155397	41.657229
3532.287740	789612.022388	41.662234
3532.688545	788987.110397	41.667239
3532.554095	788379.038077	41.672244
3532.077313	787762.618556	41.677248
3532.578611	787143.226474	41.682253
3532.293449	786536.004490	41.687258
3532.458849	785925.360609	41.692263
3532.209851	785305.248238	41.697268
3532.212601	784690.298874	41.702272
3532.454846	784078.451192	41.707277
3532.541882	783473.608486	41.712282
3532.581405	782858.593454	41.717287
3532.230813	782245.116637	41.722292
3532.255001	781619.621843	41.727296
3532.608623	780997.459212	41.732301
3532.241584	780387.957977	41.737306
3532.712765	779772.949267	41.742311
3532.471076	779153.237730	41.747316
3532.105947	778529.065989	41.752320
3532.270639	777916.559134	41.757325
3531.946342	777302.213990	41.762330
3532.296504	776672.199405	41.767335
3532.185273	776061.059309	41.772340
3531.772430	775441.108620	41.777344
3532.102821	774824.030266	41.782349
3532.018525	774216.274980	41.787354
3531.762259	773587.573884	41.792359
3531.695479	772980.451313	41.797364
3531.962435	772372.088842	41.802368
3531.737068	771759.426233	41.807373
3531.818503	771151.634437	41.812378
3531.869876	770527.198644	41.817383
3531.683041	769919.006022	41.822388
3531.563691	769303.165189	41.827392
3531.776483	768687.511878	41.832397
3532.119597	768079.964080	41.837402
3532.283317	767466.976772	41.842407
3531.911251	766840.921916	41.847412
3532.114084	766214.173991	41.852416
3532.136388	765592.874989	41.857421
3531.914050	764971.713773	41.862426
3532.227175	764345.775566	41.867431
3531.728880	763721.796807	41.872436
3531.567341	763111.957371	41.877440
3531.684506	762490.630491	41.882445
3531.475420	761879.515453	41.887450
3531.720264	761259.494882	41.892455
3531.575968	760636.629036	41.897460
3531.696795	760028.414395	41.902464
3531.579428	759407.957920	41.907469
3531.309047	758799.711016	41.912474
3531.706979	758173.589319	41.917479
3531.529446	757563.451072	41.922484
3531.668585	756942.551268	41.927488
3531.598022	756319.267768	41.932493
3531.627023	755704.207407	41.937498
3531.341123	755088.065283	41.942503
3531.530356	754461.969518	41.947508
3531.288004	753845.966475	41.952512
3531.463190	753230.681796	41.957517
3531.204487	752626.036830	41.962522
3531.414197	752002.303713	41.967527
3531.368728	751382.908985	41.972532
3531.100957	750763.206021	41.977536
3531.436801	750152.931478	41.982541
3531.579420	749543.135569	41.987546
3531.534474	748915.096379	41.992551
3531.154169	748303.563092	41.997556
3530.623487	747679.310362	42.002560
3531.017633	747057.616359	42.007565
3530.874967	746452.616075	42.012570
3530.832787	745836.433050	42.017575
3530.951987	745229.069282	42.022580
3530.709812	744628.540367	42.027584
3530.509921	744009.768839	42.032589
3530.613626	743400.683928	42.037594
3531.107949	742785.948274	42.042599
3531.202468	742184.235154	42.047604
3531.117321	741571.629255	42.052608
3531.401983	740940.716195	42.057613
3530.890472	740336.542386	42.062618
3531.311869	739709.562452	42.067623
3531.166242	739088.119464	42.072628
3530.901140	738478.815759	42.077632
3531.325418	737852.380731	42.082637
3530.776222	737237.242651	42.087642
3531.047071	736623.005396	42.092647
3531.045706	736009.806265	42.097652
3531.121565	735383.681674	42.102656
3531.013727	734761.943536	42.107661
3530.553895	734145.611453	42.112666
3530.483768	733525.651420	42.117671
3530.451888	732912.219988	42.122676
3530.404909	732302.357816	42.127680
3530.492734	731680.693931	42.132685
3530.154341	731075.441958	42.137690
3530.439843	730461.918172	42.142695
3530.355083	729856.283960	42.147700
3530.040356	729241.036984	42.152704
3530.308365	728631.437985	42.157709
3530.064015	728037.531039	42.162714
3530.214616	727420.580828	42.167719
3530.042017	726817.458990	42.172724
3530.040927	726218.919773	42.177728
3530.339046	725604.283801	42.182733
3530.256957	725001.160952	42.187738
3530.522796	724395.506402	42.192743
3530.227494	723779.645611	42.197748
3530.139675	723171.136597	42.202752
3530.461119	722555.524788	42.207757
3530.128347	721949.643500	42.212762
3529.911821	721338.146361	42.217767
3530.106615	720725.591894	42.222772
3529.984699	720119.986539	42.227776
3530.238222	719514.669447	42.232781
3530.040398	718909.533998	42.237786
3529.844968	718299.792243	42.242791
3529.922931	717694.075002	42.247796
3529.923961	717080.888028	42.252800
3529.786687	716471.399318	42.257805
3529.594553	715873.035431	42.262810
3529.553901	715268.352926	42.267815
3529.675402	714659.184135	42.272820
3529.457167	714055.535893	42.277824
3529.656236	713455.494110	42.282829
3529.309293	712851.483788	42.287834
3529.737214	712257.817547	42.292839
3529.584033	711658.700494	42.297844
3529.151150	711057.603640	42.302848
3529.801733	710440.744523	42.307853
3529.468704	709847.734033	42.312858
3529.394058	709234.683376	42.317863
3529.707339	708635.372466	42.322868
3529.437876	708040.636645	42.327872
3529.547878	707423.700791	42.332877
3529.211844	706827.402387	42.337882
3529.361446	706213.301989	42.342887
3529.211367	705617.682141	42.347892
3529.049299	705028.777187	42.352896
3529.290559	704419.797156	42.357901
3529.156425	703830.457773	42.362906
3529.261914	703233.784917	42.367911
3529.431395	702632.439993	42.372916
3529.062501	702036.858405	42.377920
3529.108857	701431.277944	42.382925
3529.106166	700841.762200	42.387930
3528.812710	700243.808740	42.392935
3528.963140	699646.135967	42.397940
3528.385566	699055.205926	42.402944
3528.580303	698459.780077	42.407949
3528.628276	697869.756469	42.412954
3528.723642	697278.939404	42.417959
3528.667629	696690.047093	42.422964
3528.815293	696097.550833	42.427968
3528.807384	695502.207336	42.432973
3528.749886	694906.732628	42.437978
3528.563958	694307.212003	42.442983
3528.512730	693717.622909	42.447988
3528.461786	693133.166473	42.452992
3528.428352	692545.087659	42.457997
3528.345509	691962.499147	42.463002
3528.512484	691376.745892	42.468007
3528.526768	690776.256000	42.473012
3528.433812	690184.449728	42.478016
3528.775951	689599.345760	42.483021
3528.593933	689008.969359	42.488026
3528.775888	688420.482180	42.493031
3528.685352	687826.977134	42.498036
3528.886207	687234.726746	42.503040
3528.617038	686625.547128	42.508045
3528.981242	686033.189834	42.513050
3528.675162	685430.853865	42.518055
3528.724841	684834.340455	42.523060
3528.675323	684240.542578	42.528064
3528.822217	683643.336804	42.533069
3528.392710	683045.094859	42.538074
3528.271684	682454.279155	42.543079
3528.291134	681870.521550	42.548084
3527.891299	681280.673242	42.553088
3528.084148	680694.669621	42.558093
3528.062326	680111.603480	42.563098
3527.729112	679509.826433	42.568103
3528.061002	678925.528788	42.573108
3527.843741	678350.951321	42.578112
3527.793819	677771.527167	42.583117
3527.962756	677191.979423	42.588122
3527.911419	676595.393956	42.593127
3527.809207	676014.373845	42.598132
3527.596502	675436.176344	42.603136
3527.901343	674850.977783	42.608141
3527.772521	674279.520779	42.613146
3527.715401	673690.722962	42.618151
3527.391858	673109.658681	42.623156
3527.531516	672547.319929	42.628160
3527.668444	671958.030800	42.633165
3527.288232	671388.882224	42.638170
3527.283338	670812.256859	42.643175
3527.400751	670233.232004	42.648180
3526.875532	669663.255775	42.653184
3527.267236	669090.096821	42.658189
3527.558572	668526.344611	42.663194
3527.286505	667947.146134	42.668199
3527.376387	667380.717049	42.673204
3527.221690	666794.496031	42.678208
3527.568211	666222.717259	42.683213
3527.095351	665647.702056	42.688218
3527.308979	665079.967455	42.693223
3527.481164	664501.730144	42.698228
3527.200540	663932.564999	42.703232
3527.446933	663350.852987	42.708237
3527.420903	662784.669431	42.713242
3527.283809	662209.090680	42.718247
3527.380852	661628.547225	42.723252
3527.094463	661056.018810	42.728256
3527.476076	660479.499546	42.733261
3527.260360	659906.890888	42.738266
3527.027610	659329.010420	42.743271
3527.048068	658751.950729	42.748276
3526.882103	658182.825584	42.753280
3527.050868	657611.413419	42.758285
3526.797365	657033.899111	42.763290
3526.869682	656456.145181	42.768295
3526.727089	655896.768070	42.773300
3526.581216	655341.054562	42.778304
3526.845838	654766.413618	42.783309
3526.359751	654199.058369	42.788314
3526.553189	653632.802881	42.793319
3526.575446	653066.444147	42.798324
3526.512804	652520.745571	42.803329
3526.872036	651949.670033	42.808333
3526.446796	651387.637037	42.813338
3526.464495	650815.755112	42.818343
3526.613299	650254.309169	42.823348
3526.266289	649697.762411	42.828353
3526.412809	649132.906098	42.833357
3526.276892	648568.016017	42.838362
3526.163192	648010.035996	42.843367
3526.585652	647443.937639	42.848372
3526.385891	646886.459338	42.853377
3526.485698	646324.001009	42.858381
3526.419312	645765.338123	42.863386
3526.349795	645196.697925	42.868391
3526.537164	644637.029384	42.873396
3526.451337	644077.726369	42.878401
3526.556544	643506.761557	42.883405
3526.359601	642954.514310	42.888410
3525.808862	642388.647959	42.893415
3525.914341	641837.888227	42.898420
3526.019817	641281.898323	42.903425
3526.174747	640720.668996	42.908429
3526.084050	640172.353003	42.913434
3526.147295	639613.278845	42.918439
3526.041222	639053.252780	42.923444
3525.701690	638503.739531	42.928449
3525.789758	637938.467715	42.933453
3525.652554	637391.261362	42.938458
3525.702372	636830.287147	42.943463
3526.178996	636283.217325	42.948468
3525.650281	635728.835652	42.953473
3525.429060	635184.278315	42.958477
3525.414213	634633.602812	42.963482
3525.433924	634078.989204	42.968487
3525.541680	633536.240734	42.973492
3525.596462	632989.019142	42.978497
3526.045859	632442.302023	42.983501
3525.950965	631894.147755	42.988506
3525.604316	631333.194567	42.993511
3525.896405	630782.713780	42.998516
3525.880177	630233.808524	43.003521
3525.412239	629677.342697	43.008525
3525.437233	629128.472852	43.013530
3525.245655	628578.610123	43.018535
3525.309676	628034.082389	43.023540
3524.923776	627498.265510	43.028545
3525.222199	626948.985471	43.033549
3525.282520	626413.338027	43.038554
3525.083243	625871.548394	43.043559
3525.388694	625330.596538	43.048564
3525.187296	624783.844125	43.053569
3525.018623	624246.073442	43.058573
3525.070407	623702.427929	43.063578
3525.057108	623158.916216	43.068583
3524.982394	622609.326250	43.073588
3524.614482	622079.646027	43.078593
3525.136351	621535.009030	43.083597
3524.734743	620996.514216	43.088602
3524.397347	620464.444827	43.093607
3524.485305	619930.773491	43.098612
3524.382778	619396.507100	43.103617
3524.486309	618869.996388	43.108621
3524.274294	618340.006175	43.113626
3524.473454	617817.787992	43.118631
3524.649556	617283.069535	43.123636
3524.373481	616761.483346	43.128641
3524.713515	616224.078870	43.133645
3524.625789	615698.801092	43.138650
3524.181758	615170.300744	43.143655
3524.326979	614640.170491	43.148660
3524.178809	614115.529163	43.153665
3524.157157	613586.329191	43.158669
3523.861355	613070.436847	43.163674
3523.792065	612548.314680	43.168679
3523.949306	612027.783888	43.173684
3523.809693	611522.573140	43.178689
3524.335509	610998.772145	43.183693
3523.891064	610479.424901	43.188698
3523.982664	609947.775344	43.193703
3523.918602	609430.169877	43.198708
3523.842431	608913.244690	43.203713
3524.139910	608397.134687	43.208717
3524.051890	607877.555567	43.213722
3523.524348	607366.354376	43.218727
3524.077767	606843.909223	43.223732
3523.542664	606338.933236	43.228737
3523.729820	605819.864359	43.233741
3523.982552	605307.433245	43.238746
3523.698346	604790.354298	43.243751
3523.996402	604267.482489	43.248756
3523.569294	603750.029313	43.253761
3523.752126	603238.821383	43.258765
3523.574659	602737.989668	43.263770
3523.674358	602220.577827	43.268775
3523.379790	601704.815872	43.273780
3523.085765	601195.103509	43.278785
3523.359767	600693.302171	43.283789
3523.622866	600179.233483	43.288794
3523.250576	599673.281680	43.293799
3523.648595	599166.774557	43.298804
3523.359393	598663.173763	43.303809
3523.688327	598147.497259	43.308813
3523.329890	597643.462271	43.313818
3523.207745	597145.189046	43.318823
3523.783828	596625.034640	43.323828
3523.192051	596123.534195	43.328833
3523.245949	595599.958558	43.333837
3523.030139	595094.432991	43.338842
3523.081092	594592.003751	43.343847
3523.677560	594093.628090	43.348852
3523.186047	593586.125878	43.353857
3523.139841	593083.045908	43.358861
3522.963775	592579.464328	43.363866
3522.668822	592082.310802	43.368871
3523.309554	591581.309727	43.373876
3523.189840	591078.056305	43.378881
3523.073474	590569.405756	43.383885
3523.361105	590070.510925	43.388890
3522.835709	589569.221979	43.393895
3522.745132	589073.514957	43.398900
3522.180141	588574.652718	43.403905
3522.363722	588079.661470	43.408909
3522.368337	587591.513974	43.413914
3522.220240	587103.473146	43.418919
3522.436731	586607.360166	43.423924
3522.291803	586122.042735	43.428929
3522.539387	585632.467467	43.433933
3522.333661	585145.060536	43.438938
3522.255693	584658.064443	43.443943
3522.464206	584174.367368	43.448948
3522.166187	583684.504711	43.453953
3522.174630	583198.088559	43.458957
3521.972026	582706.611881	43.463962
3521.795179	582235.319507	43.468967
3522.061511	581755.286453	43.473972
3522.234316	581282.188290	43.478977
3522.153217	580795.691491	43.483981
3521.859672	580319.669431	43.488986
3521.780593	579832.078175	43.493991
3521.998088	579348.841725	43.498996
3521.669389	578875.384320	43.504001
3521.719090	578392.541240	43.509005
3521.870526	577924.345906	43.514010
3521.712226	577448.843430	43.519015
3521.958735	576969.733158	43.524020
3521.397579	576505.025609	43.529025
3521.583722	576027.750117	43.534029
3521.647769	575552.941718	43.539034
3521.391856	575076.509968	43.544039
3521.449037	574609.161366	43.549044
3521.596067	574138.812063	43.554049
3521.944856	573660.764287	43.559053
3521.494771	573193.298489	43.564058
3521.224092	572729.759027	43.569063
3521.514669	572251.265037	43.574068
3521.361772	571793.104492	43.579073
3521.417011	571324.124515	43.584077
3521.357610	570853.838476	43.589082
3521.490701	570384.005268	43.594087
3521.769927	569915.186407	43.599092
3521.567097	569454.836254	43.604097
3521.489608	568979.904523	43.609101
3521.590972	568517.908493	43.614106
3521.067184	568048.956644	43.619111
3521.151732	567575.807049	43.624116
3520.773777	567111.275177	43.629121
3520.925096	566657.004636	43.634125
3520.905409	566198.519111	43.639130
3520.910546	565740.365343	43.644135
3521.219048	565278.217101	43.649140
3520.898333	564821.495751	43.654145
3521.140092	564353.184303	43.659149
3520.858429	563904.025450	43.664154
3520.649061	563440.188210	43.669159
3520.625468	562977.813077	43.674164
3520.662301	562535.097559	43.679169
3520.525590	562085.146136	43.684173
3520.645741	561623.151483	43.689178
3520.607885	561180.755179	43.694183
3520.769227	560723.404598	43.699188
3520.591869	560275.512725	43.704193
3520.615596	559828.779843	43.709197
3520.578516	559379.322660	43.714202
3520.177351	558927.091975	43.719207
3519.985606	558476.472034	43.724212
3519.965990	558039.154323	43.729217
3520.034040	557603.771515	43.734221
3520.158186	557166.148560	43.739226
3520.034919	556724.624462	43.744231
3520.224975	556275.778515	43.749236
3519.901449	555842.973793	43.754241
3520.080604	555408.356396	43.759245
3519.784294	554963.428217	43.764250
3519.499292	554537.022884	43.769255
3519.755671	554098.571248	43.774260
3519.748253	553672.544423	43.779265
3519.410479	553232.553677	43.784269
3519.571099	552806.722622	43.789274
3519.654522	552377.162612	43.794279
3519.791838	551939.215140	43.799284
3519.394903	551512.329843	43.804289
3519.517144	551089.373805	43.809293
3519.493798	550663.607366	43.814298
3519.548847	550239.426832	43.819303
3519.404357	549808.161154	43.824308
3519.264482	549387.565509	43.829313
3519.397188	548957.586326	43.834317
3519.381388	548538.052101	43.839322
3518.987685	548113.478797	43.844327
3519.451261	547691.114981	43.849332
3519.329373	547280.885223	43.854337
3519.482725	546843.829658	43.859341
3519.559598	546429.759967	43.864346
3519.236936	546007.125775	43.869351
3519.138651	545582.070937	43.874356
3519.412828	545167.677617	43.879361
3519.412899	544737.185714	43.884365
3519.332623	544314.609646	43.889370
3519.188595	543896.720530	43.894375
3519.502390	543474.959174	43.899380
3519.313314	543052.716263	43.904385
3519.182640	542628.988321	43.909389
3519.174633	542217.933607	43.914394
3519.110218	541797.497172	43.919399
3519.240053	541372.526884	43.924404
3519.481742	540961.241383	43.929409
3519.524145	540533.991333	43.934413
3519.117644	540114.117634	43.939418
3518.812098	539699.257563	43.944423
3519.009434	539274.061085	43.949428
3519.040129	538870.114139	43.954433
3518.886269	538451.761867	43.959437
3519.014202	538033.601340	43.964442
3518.697194	537628.266077	43.969447
3518.603111	537210.270560	43.974452
3518.270977	536813.792578	43.979457
3518.392220	536403.807691	43.984461
3518.232335	535995.574235	43.989466
3517.940117	535608.287764	43.994471
3518.518198	535198.190346	43.999476
3518.251329	534805.530205	44.004481
3518.156759	534404.959338	44.009485
3518.494135	534003.395409	44.014490
3518.352699	533612.346289	44.019495
3518.397383	533210.759824	44.024500
3518.442433	532812.542835	44.029505
3518.580891	532411.473224	44.034509
3518.869825	532002.848170	44.039514
3518.419126	531606.146074	44.044519
3518.351491	531194.531451	44.049524
3518.127228	530803.067496	44.054529
3518.270634	530404.313574	44.059533
3518.657996	529996.675265	44.064538
3518.179877	529597.046570	44.069543
3518.338528	529192.856853	44.074548
3517.987417	528808.477563	44.079553
3518.098160	528410.482548	44.084557
3518.075951	528017.698364	44.089562
3517.976181	527617.497001	44.094567
3517.881667	527216.526739	44.099572
3517.799195	526833.614916	44.104577
3517.459532	526444.982397	44.109581
3517.476514	526061.175489	44.114586
3517.510954	525678.062446	44.119591
3517.381533	525294.664617	44.124596
3517.502098	524907.629800	44.129601
3517.367054	524527.848156	44.134605
3517.638710	524156.519850	44.139610
3517.157575	523778.494857	44.144615
3517.435447	523388.919942	44.149620
3517.394570	523015.597138	44.154625
3517.152221	522635.533431	44.159629
3517.124533	522259.563997	44.164634
3516.773592	521888.033477	44.169639
3517.093338	521514.157458	44.174644
3516.899003	521149.651569	44.179649
3516.882277	520776.370256	44.184653
3516.734246	520407.445202	44.189658
3516.556976	520039.980724	44.194663
3516.984019	519674.575809	44.199668
3516.951807	519308.735509	44.204673
3516.766514	518942.963080	44.209677
3517.008139	518577.563563	44.214682
3516.661096	518208.316246	44.219687
3516.759983	517845.954099	44.224692
3516.692646	517487.551552	44.229697
3517.013944	517124.730342	44.234701
3516.637279	516764.393828	44.239706
3516.659997	516398.070625	44.244711
3516.741454	516019.605177	44.249716
3516.795029	515675.536546	44.254721
3516.499623	515308.837725	44.259725
3516.609047	514954.387553	44.264730
3516.545700	514599.099960	44.269735
3516.744836	514226.784542	44.274740
3516.466672	513879.752050	44.279745
3516.383621	513522.270823	44.284749
3516.648097	513156.587715	44.289754
3516.379640	512812.510767	44.294759
3516.246972	512443.544151	44.299764
3516.227558	512104.108075	44.304769
3516.475833	511750.218335	44.309773
3516.162165	511388.635008	44.314778
3515.905038	511035.573439	44.319783
3516.049367	510686.124257	44.324788
3516.130461	510334.050424	44.329793
3516.156133	509998.907167	44.334797
3515.943288	509643.179165	44.339802
3516.118376	509298.798177	44.344807
3516.063581	508945.604916	44.349812
3516.274544	508601.809160	44.354817
3515.568368	508258.718514	44.359821
3515.740528	507917.138367	44.364826
3515.676954	507575.287918	44.369831
3515.811931	507238.703270	44.374836
3515.609370	506901.411025	44.379841
3515.752658	506559.756313	44.384845
3515.921136	506213.945256	44.389850
3515.694603	505885.178064	44.394855
3515.704677	505540.643274	44.399860
3515.575980	505199.359978	44.404865
3515.427027	504864.240076	44.409869
3515.797586	504531.097140	44.414874
3515.862495	504201.588767	44.419879
3515.709706	503855.276569	44.424884
3515.507666	503532.574366	44.429889
3515.301223	503185.802080	44.434893
3515.552087	502857.094161	44.439898
3515.417182	502532.742885	44.444903
3515.400278	502201.944080	44.449908
3515.390010	501879.732593	44.454913
3515.332604	501542.607432	44.459917
3515.584949	501214.270753	44.464922
3515.288996	500887.032384	44.469927
3515.447829	500554.855744	44.474932
3515.193509	500228.962408	44.479937
3515.145686	499893.672723	44.484941
3515.223938	499570.440156	44.489946
3515.147597	499249.907759	44.494951
3514.999941	498910.873197	44.499956
3514.829612	498590.495807	44.504961
3514.976023	498277.795469	44.509965
3515.013760	497961.011511	44.514970
3515.083550	497643.406897	44.519975
3515.020639	497312.012316	44.524980
3514.867165	496992.916242	44.529985
3514.828389	496680.875066	44.534989
3515.137943	496354.152014	44.539994
3514.937569	496041.367881	44.544999
3514.773420	495722.097709	44.550004
3514.857059	495412.288081	44.555009
3515.095069	495088.992052	44.560013
3515.120839	494773.009764	44.565018
3514.871283	494461.823297	44.570023
3514.952971	494126.193488	44.575028
3514.886709	493812.636966	44.580033
3514.626313	493499.563058	44.585037
3514.801471	493170.777948	44.590042
3514.604122	492869.114095	44.595047
3514.852109	492555.227788	44.600052
3514.579574	492242.891655	44.605057
3514.710211	491938.069420	44.610061
3514.753131	491611.148645	44.615066
3514.441276	491311.955777	44.620071
3514.504865	490992.304842	44.625076
3514.469898	490686.274401	44.630081
3514.296069	490386.586503	44.635085
3514.618271	490072.743250	44.640090
3514.468762	489767.272581	44.645095
3514.363411	489452.124949	44.650100
3514.286518	489160.241727	44.655105
3514.150228	488848.478436	44.660109
3514.738339	488539.520632	44.665114
3514.530052	488235.146158	44.670119
3514.362079	487931.822099	44.675124
3514.402920	487628.001681	44.680129
3514.482641	487318.248758	44.685133
3514.711077	487010.438507	44.690138
3514.263837	486709.063822	44.695143
3514.081602	486402.173269	44.700148
3513.945146	486108.326053	44.705153
3513.821342	485802.832022	44.710157
3514.067253	485501.571271	44.715162
3513.731612	485212.601495	44.720167
3513.949506	484919.129389	44.725172
3514.103651	484619.893640	44.730177
3513.944800	484330.879237	44.735181
3513.937385	484039.354237	44.740186
3513.770660	483748.863910	44.745191
3513.746672	483447.462381	44.750196
3513.790745	483154.446232	44.755201
3513.748507	482871.866881	44.760205
3514.072893	482568.771272	44.765210
3513.883412	482288.890508	44.770215
3513.622115	481990.946844	44.775220
3513.567463	481698.075478	44.780225
3513.166550	481414.167578	44.785229
3513.632492	481127.778611	44.790234
3513.208161	480843.055735	44.795239
3513.164359	480563.831848	44.800244
3513.181387	480282.365819	44.805249
3513.045286	480001.073412	44.810253
3513.085868	479726.428929	44.815258
3513.125855	479459.880466	44.820263
3513.333525	479176.339623	44.825268
3513.260977	478898.816190	44.830273
3513.392737	478624.341929	44.835277
3513.120933	478348.869223	44.840282
3512.923100	478072.822789	44.845287
3513.157638	477791.736584	44.850292
3513.144134	477524.814441	44.855297
3513.166813	477253.426625	44.860301
3513.616875	476966.569534	44.865306
3513.111520	476694.099029	44.870311
3512.991554	476415.178781	44.875316
3513.348149	476147.312576	44.880321
3513.441466	475869.613493	44.885325
3513.748190	475582.809882	44.890330
3513.478712	475310.683670	44.895335
3513.177427	475026.912171	44.900340
3513.191959	474760.350149	44.905345
3512.913114	474479.857923	44.910349
3512.887882	474210.762806	44.915354
3512.796401	473946.891096	44.920359
3512.972817	473673.753136	44.925364
3512.811074	473403.201014	44.930369
3512.867401	473123.998409	44.935373
3512.868870	472864.805278	44.940378
3512.255293	472605.257760	44.945383
3512.564142	472332.887844	44.950388
3512.759524	472069.598954	44.955393
3512.439700	471815.561366	44.960397
3512.809066	471552.539386	44.965402
3512.457159	471286.294106	44.970407
3512.346725	471024.005073	44.975412
3512.737820	470763.044936	44.980417
3512.204006	470508.215822	44.985421
3512.302194	470248.970037	44.990426
3512.153559	469992.244761	44.995431
3512.266766	469731.824334	45.000436
3511.991537	469479.875027	45.005441
3512.013270	469230.201729	45.010445
3512.392948	468985.884029	45.015450
3512.162781	468738.577372	45.020455
3512.213292	468481.595030	45.025460
3512.132729	468228.329504	45.030465
3512.357995	467976.984015	45.035469
3512.266532	467726.499819	45.040474
3511.460863	467487.937641	45.045479
3511.962953	467238.966778	45.050484
3512.060299	466988.845963	45.055489
3511.831811	466748.808226	45.060493
3512.348848	466496.481615	45.065498
3512.006922	466252.404187	45.070503
3511.658783	466006.298243	45.075508
3511.967949	465760.583553	45.080513
3511.732664	465524.635396	45.085517
3511.825024	465278.799608	45.090522
3511.701482	465045.207729	45.095527
3511.893531	464787.949154	45.100532
3511.921938	464557.922692	45.105537
3511.877943	464324.460549	45.110541
3511.862521	464070.267881	45.115546
3511.558077	463836.439014	45.120551
3511.811199	463586.044922	45.125556
3511.471595	463352.520265	45.130561
3511.048261	463117.030998	45.135565
3511.285712	462888.418557	45.140570
3511.293549	462658.170517	45.145575
3511.370751	462424.512947	45.150580
3511.567262	462189.920128	45.155585
3511.020124	461974.605716	45.160589
3511.413529	461735.311980	45.165594
3511.331453	461509.525071	45.170599
3511.142602	461271.896012	45.175604
3511.089111	461044.325295	45.180609
3510.830798	460824.641634	45.185613
3511.033737	460609.082891	45.190618
3510.726490	460391.936586	45.195623
3511.424509	460168.484320	45.200628
3511.448897	459932.779184	45.205633
3511.076830	459717.714359	45.210637
3511.136537	459484.734511	45.215642
3510.888489	459270.099783	45.220647
3511.216404	459037.170267	45.225652
3510.736015	458815.880553	45.230657
3510.823986	458596.315866	45.235661
3511.164331	458378.884993	45.240666
3511.125304	458165.368389	45.245671
3510.992891	457942.286403	45.250676
3511.248638	457721.264365	45.255681
3510.939624	457496.991185	45.260685
3511.005534	457275.540506	45.265690
3510.686020	457057.042250	45.270695
3510.661833	456845.891298	45.275700
3510.844830	456626.542295	45.280705
3510.945344	456408.573536	45.285709
3511.032356	456191.770540	45.290714
3510.608310	455983.213216	45.295719
3510.878965	455768.047027	45.300724
3510.958915	455550.173924	45.305729
3510.620034	455333.231718	45.310733
3510.742581	455113.268395	45.315738
3510.696864	454907.930278	45.320743
3510.656711	454702.335689	45.325748
3510.765840	454493.874818	45.330753
3510.593884	454276.436639	45.335757
3510.612861	454059.723935	45.340762
3510.735981	453849.682642	45.345767
3510.430212	453643.717219	45.350772
3510.410143	453424.368400	45.355777
3510.219911	453221.217882	45.360781
3510.584057	453021.012405	45.365786
3510.501805	452817.738076	45.370791
3510.592239	452605.560436	45.375796
3510.366728	452413.358334	45.380801
3509.892321	452209.840793	45.385805
3510.569917	452001.612463	45.390810
3510.250160	451800.497973	45.395815
3510.463427	451593.155989	45.400820
3510.195382	451386.603902	45.405825
3510.144104	451192.636949	45.410829
3510.224817	450984.398927	45.415834
3509.887106	450796.104891	45.420839
3509.986275	450598.811178	45.425844
3510.155394	450393.949128	45.430849
3509.909113	450198.890782	45.435853
3510.474410	450003.539935	45.440858
3509.865896	449819.795848	45.445863
3509.849600	449617.949325	45.450868
3510.147869	449428.621711	45.455873
3509.912393	449235.175064	45.460877
3509.849835	449033.127997	45.465882
3510.221820	448846.216379	45.470887
3510.018535	448653.367345	45.475892
3510.018156	448466.313113	45.480897
3509.852334	448262.805805	45.485901
3510.218014	448060.270635	45.490906
3509.935307	447878.228699	45.495911
3509.739073	447681.566511	45.500916
3509.826384	447492.105402	45.505921
3509.902546	447310.707230	45.510925
3509.911344	447113.345545	45.515930
3509.719259	446924.129909	45.520935
3509.478759	446736.340745	45.525940
3509.787827	446551.245179	45.530945
3509.515937	446366.551469	45.535949
3509.743304	446186.233538	45.540954
3509.589847	446004.863442	45.545959
3509.724066	445812.336647	45.550964
3509.651030	445624.204824	45.555969
3509.304213	445445.145080	45.560973
3509.612918	445257.654844	45.565978
3509.357546	445083.901422	45.570983
3509.337510	444901.129914	45.575988
3509.328709	444731.743718	45.580993
3509.167288	444548.384772	45.585997
3509.637613	444363.192054	45.591002
3509.276444	444196.397611	45.596007
3509.303997	444012.798976	45.601012
3509.630301	443838.530451	45.606017
3509.126600	443659.482636	45.611021
3509.407260	443477.864946	45.616026
3509.144108	443302.171209	45.621031
3509.153588	443124.705056	45.626036
3509.237127	442958.940954	45.631041
3509.228119	442780.714358	45.636045
3509.426608	442602.298712	45.641050
3509.243559	442436.018222	45.646055
3509.148375	442258.562871	45.651060
3509.020114	442085.778082	45.656065
3509.337877	441914.640304	45.661069
3509.272106	441741.334903	45.666074
3508.977518	441569.791762	45.671079
3509.192314	441391.515603	45.676084
3509.243366	441236.395764	45.681089
3508.902936	441069.573794	45.686093
3509.163018	440891.995974	45.691098
3509.076212	440723.099104	45.696103
3508.734517	440548.715452	45.701108
3508.941617	440382.099123	45.706113
3508.969716	440226.773178	45.711117
3508.995441	440056.736020	45.716122
3509.083543	439894.194401	45.721127
3509.202239	439723.225727	45.726132
3509.456907	439553.196330	45.731137
3509.124428	439385.447164	45.736141
3509.160928	439212.814575	45.741146
3509.294313	439039.859731	45.746151
3508.631003	438872.163168	45.751156
3508.766797	438707.981386	45.756161
3508.565924	438545.174842	45.761165
3508.530967	438377.823826	45.766170
3508.721747	438228.087105	45.771175
3508.520415	438067.610736	45.776180
3508.694431	437908.946165	45.781185
3508.623367	437754.127157	45.786189
3508.613846	437586.816597	45.791194
3508.423290	437438.458719	45.796199
3508.764626	437279.659652	45.801204
3509.016644	437119.200535	45.806209
3508.822005	436968.202143	45.811213
3509.003247	436794.663674	45.816218
3508.818953	436640.414375	45.821223
3508.792791	436475.432123	45.826228
3509.174041	436310.429833	45.831233
3508.575623	436151.986201	45.836237
3508.863281	435989.838697	45.841242
3509.130924	435832.513325	45.846247
3508.760100	435677.426783	45.851252
3508.935139	435504.133124	45.856257
3508.344136	435347.864246	45.861261
3508.406048	435188.387850	45.866266
3508.210954	435043.312883	45.871271
3508.251707	434888.759514	45.876276
3508.204156	434738.532903	45.881281
3508.224114	434594.889755	45.886285
3508.318672	434443.165517	45.891290
3507.995402	434287.959882	45.896295
3508.116892	434141.201458	45.901300
3508.142032	433994.610761	45.906305
3508.080668	433862.697746	45.911309
3507.999787	433709.679348	45.916314
3507.893951	433572.241558	45.921319
3507.947826	433426.251199	45.926324
3508.386718	433282.122336	45.931329
3508.021308	433141.072911	45.936333
3508.316927	432996.611529	45.941338
3508.168515	432841.619935	45.946343
3507.907106	432706.791376	45.951348
3508.249752	432559.731352	45.956353
3507.857043	432426.699570	45.961357
3508.054566	432277.531313	45.966362
3507.927881	432143.894299	45.971367
3507.925166	431998.970162	45.976372
3508.205667	431854.199736	45.981377
3507.993894	431714.130226	45.986381
3508.350657	431566.604766	45.991386
3508.292936	431426.557957	45.996391
3507.850525	431286.119276	46.001396
3508.128821	431146.977572	46.006401
3508.163934	431006.201932	46.011405
3508.048388	430861.898904	46.016410
3508.097204	430731.420809	46.021415
3508.071386	430583.903686	46.026420
3508.163369	430443.926888	46.031425
3507.731883	430292.823370	46.036429
3508.093732	430164.724548	46.041434
3508.035540	430032.586127	46.046439
3508.022377	429895.973389	46.051444
3508.112143	429749.547727	46.056449
3507.915106	429614.943954	46.061453
3507.960713	429466.443343	46.066458
3508.029556	429332.756793	46.071463
3507.645110	429194.731615	46.076468
3507.913872	429060.552628	46.081473
3507.632947	428930.780548	46.086477
3507.656419	428792.277348	46.091482
3507.654863	428656.061418	46.096487
3507.825317	428525.347257	46.101492
3507.844184	428391.207126	46.106497
3507.994139	428268.666100	46.111501
3508.326970	428125.030942	46.116506
3508.224296	427981.824543	46.121511
3507.867667	427840.233985	46.126516
3507.828933	427703.460625	46.131521
3507.918047	427578.947033	46.136525
3507.848192	427438.979981	46.141530
3507.755285	427309.420658	46.146535
3507.583555	427180.939932	46.151540
3507.761607	427040.674430	46.156545
3507.322878	426916.247492	46.161549
3507.441087	426779.035970	46.166554
3507.641852	426649.473664	46.171559
3507.313426	426520.407060	46.176564
3507.319661	426398.540748	46.181569
3507.111450	426275.644546	46.186573
3507.339043	426154.145242	46.191578
3507.529551	426027.372931	46.196583
3507.226963	425891.852385	46.201588
3507.454733	425776.949578	46.206593
3507.435841	425657.520141	46.211597
3507.490310	425525.997178	46.216602
3507.554322	425408.785701	46.221607
3507.245988	425285.241655	46.226612
3507.369599	425153.248019	46.231617
3507.039175	425045.847810	46.236621
3506.953999	424916.020402	46.241626
3507.095886	424806.355828	46.246631
3507.085262	424695.650841	46.251636
3507.208818	424567.664028	46.256641
3507.024885	424452.774436	46.261645
3507.251454	424328.575788	46.266650
3507.601415	424203.441739	46.271655
3507.194855	424087.167120	46.276660
3507.423639	423961.900230	46.281665
3507.500121	423850.313558	46.286669
3507.210783	423721.529825	46.291674
3507.054149	423602.875163	46.296679
3507.249066	423486.748773	46.301684
3507.352242	423364.139886	46.306689
3506.907616	423260.101575	46.311693
3506.858378	423136.959177	46.316698
3506.991893	423015.460140	46.321703
3506.553294	422917.003294	46.326708
3507.154627	422800.042782	46.331713
3507.061391	422692.236293	46.336717
3507.019987	422569.648096	46.341722
3506.785852	422462.169236	46.346727
3507.072845	422354.956273	46.351732
3507.245076	422232.989852	46.356737
3506.825021	422131.937664	46.361741
3507.244220	422015.664450	46.366746
3507.270812	421900.879159	46.371751
3507.225155	421784.734989	46.376756
3507.153434	421655.446302	46.381761
3507.001343	421547.238695	46.386765
3506.894505	421433.235497	46.391770
3507.118922	421328.313232	46.396775
3506.827116	421208.832380	46.401780
3506.982353	421097.575066	46.406785
3507.167257	420996.617982	46.411789
3507.192345	420875.939140	46.416794
3507.325889	420758.972635	46.421799
3507.217531	420649.560573	46.426804
3507.135987	420531.233591	46.431809
3506.954037	420406.805563	46.436813
3507.099087	420292.347937	46.441818
3506.968580	420184.130668	46.446823
3507.116383	420070.077699	46.451828
3507.137439	419960.412034	46.456833
3506.760470	419853.910805	46.461837
3506.898652	419739.071027	46.466842
3507.080477	419639.835122	46.471847
3507.114325	419528.769187	46.476852
3507.037691	419408.887517	46.481857
3506.940417	419309.164858	46.486861
3506.932032	419180.030126	46.491866
3506.748750	419070.700058	46.496871
3506.416925	418963.146497	46.501876
3507.375160	418858.240805	46.506881
3506.144813	418766.147520	46.511885
3506.190721	418656.751122	46.516890
3506.359171	418554.568397	46.521895
3506.234407	418463.478373	46.526900
3506.396776	418362.336742	46.531905
3506.293236	418275.050372	46.536909
3506.350550	418168.315478	46.541914
3506.890159	418066.727445	46.546919
3506.819192	417962.780734	46.551924
3506.824343	417852.042286	46.556929
3506.379714	417757.830951	46.561933
3506.315558	417661.218682	46.566938
3506.445397	417543.653836	46.571943
3506.307037	417450.607644	46.576948
3506.443481	417365.206579	46.581953
3506.344864	417263.597348	46.586957
3506.228821	417161.584481	46.591962
3506.731476	417074.139666	46.596967
3506.297981	416978.425643	46.601972
3506.332839	416871.714482	46.606977
3506.383950	416775.358410	46.611981
3506.351484	416673.557797	46.616986
3506.306739	416587.093354	46.621991
3506.091813	416488.115854	46.626996
3506.453965	416393.863229	46.632001
3506.254399	416312.806628	46.637005
3506.256584	416204.600319	46.642010
3506.215807	416110.161556	46.647015
3506.219866	416026.251128	46.652020
3506.313552	415927.828081	46.657025
3506.177923	415842.087510	46.662029
3506.056420	415751.291820	46.667034
3506.089758	415649.171201	46.672039
3506.143034	415557.380190	46.677044
3506.066235	415463.579913	46.682049
3505.827532	415387.554136	46.687053
3506.100690	415294.429776	46.692058
3505.814231	415213.282956	46.697063
3505.765557	415123.945195	46.702068
3506.172710	415024.601895	46.707073
3505.897040	414951.627906	46.712077
3505.992180	414859.827243	46.717082
3506.186966	414768.085409	46.722087
3505.902166	414689.983449	46.727092
3506.011013	414606.837563	46.732097
3506.078984	414525.145632	46.737101
3506.276982	414434.747742	46.742106
3506.050194	414343.939648	46.747111
3505.585017	414254.720760	46.752116
3505.984319	414168.578561	46.757121
3505.830356	414090.350877	46.762125
3505.859645	414004.499826	46.767130
3505.873767	413915.477221	46.772135
3505.780732	413843.662271	46.777140
3506.247463	413749.178933	46.782145
3506.367306	413668.008639	46.787149
3506.207483	413568.908881	46.792154
3506.475793	413479.206591	46.797159
3505.975597	413394.662704	46.802164
3506.043822	413312.586019	46.807169
3506.116353	413229.543461	46.812173
3506.140998	413143.537995	46.817178
3506.136310	413055.226607	46.822183
3506.014524	412965.843066	46.827188
3506.383558	412883.713662	46.832193
3506.162924	412796.987173	46.837197
3506.214254	412712.067575	46.842202
3506.023094	412618.606566	46.847207
3505.705222	412539.945126	46.852212
3506.344568	412448.068367	46.857217
3506.146695	412360.854083	46.862221
3506.053723	412287.638233	46.867226
3506.157166	412183.257387	46.872231
3506.268067	412101.575874	46.877236
3506.250463	412006.356336	46.882241
3506.174061	411927.321711	46.887245
3505.919457	411842.375340	46.892250
3506.136212	411750.035033	46.897255
3506.050611	411674.149942	46.902260
3506.308046	411582.614676	46.907265
3506.061293	411500.484493	46.912269
3505.972299	411415.356099	46.917274
3506.075462	411324.150992	46.922279
3505.769929	411250.333698	46.927284
3505.849730	411154.967465	46.932289
3505.888770	411074.285367	46.937293
3505.779479	410991.469884	46.942298
3506.141206	410918.121778	46.947303
3505.511243	410842.555775	46.952308
3505.511106	410752.255107	46.957313
3505.626647	410687.734697	46.962317
3505.607779	410616.660015	46.967322
3505.383634	410534.929258	46.972327
3505.464200	410460.307390	46.977332
3505.842396	410383.907679	46.982337
3505.433304	410313.025781	46.987341
3505.860479	410234.661909	46.992346
3505.524990	410155.564616	46.997351
3505.575455	410084.705215	47.002356
3505.863869	410010.630662	47.007361
3505.504141	409942.761306	47.012365
3505.680582	409857.887294	47.017370
3505.894567	409789.030764	47.022375
3505.653274	409715.629916	47.027380
3506.195522	409623.099604	47.032385
3505.807564	409549.291624	47.037389
3505.765299	409464.631463	47.042394
3505.946685	409385.342033	47.047399
3505.663808	409325.584454	47.052404
3505.937966	409238.456989	47.057409
3505.808520	409169.835263	47.062413
3505.274599	409092.927296	47.067418
3505.435541	409017.805129	47.072423
3505.432877	408951.929314	47.077428
3505.507103	408867.298153	47.082433
3505.246649	408805.605500	47.087437
3505.228597	408721.853091	47.092442
3505.173876	408659.007551	47.097447
3505.246996	408594.032167	47.102452
3505.326549	408522.579527	47.107457
3505.381558	408460.527459	47.112461
3505.506748	408387.923841	47.117466
3505.381577	408315.769116	47.122471
3505.278484	408251.026157	47.127476
3505.490869	408173.150027	47.132481
3505.333534	408110.498494	47.137485
3505.060822	408035.015872	47.142490
3505.452062	407974.479851	47.147495
3505.057723	407923.423798	47.152500
3505.027487	407847.670675	47.157505
3505.141780	407791.905320	47.162509
3505.268039	407726.182251	47.167514
3505.110654	407645.955031	47.172519
3505.103945	407597.321066	47.177524
3505.192640	407536.861116	47.182529
3505.158128	407473.145847	47.187533
3505.039116	407401.139994	47.192538
3505.471537	407333.128740	47.197543
3505.256394	407277.647145	47.202548
3505.312598	407215.744379	47.207553
3505.225100	407152.545346	47.212557
3505.538605	407077.391693	47.217562
3505.457501	407011.041953	47.222567
3505.021134	406950.111597	47.227572
3505.249171	406877.613329	47.232577
3505.226666	406815.646893	47.237581
3505.126089	406760.170069	47.242586
3505.129655	406691.392302	47.247591
3505.105173	406627.190765	47.252596
3504.994244	406570.724804	47.257601
3505.012641	406513.474704	47.262605
3504.890718	406460.591504	47.267610
3505.085922	406395.996335	47.272615
3504.816151	406338.617284	47.277620
3505.055139	406279.601950	47.282625
3505.062060	406220.778504	47.287629
3505.015452	406164.275315	47.292634
3504.857062	406103.879750	47.297639
3504.838157	406042.342703	47.302644
3505.125295	405986.213930	47.307649
3504.965914	405940.396884	47.312653
3505.162298	405873.031833	47.317658
3505.238145	405810.462140	47.322663
3504.835884	405753.434657	47.327668
3505.124498	405692.453878	47.332673
3505.178805	405629.176281	47.337677
3505.080928	405562.089296	47.342682
3504.957518	405503.286552	47.347687
3504.935941	405444.491693	47.352692
3505.043392	405386.995424	47.357697
3504.897408	405335.917476	47.362701
3504.783713	405289.202567	47.367706
3504.859500	405218.224418	47.372711
3504.866676	405176.339919	47.377716
3505.275141	405111.603694	47.382721
3504.990692	405060.447276	47.387725
3504.791185	405015.930894	47.392730
3505.388048	404947.860195	47.397735
3505.082397	404892.541577	47.402740
3504.648892	404826.627671	47.407745
3504.872721	404778.482682	47.412749
3504.604535	404718.051997	47.417754
3505.084339	404660.947818	47.422759
3504.820320	404610.549062	47.427764
3504.628732	404558.283661	47.432769
3504.682633	404501.505872	47.437773
3504.781746	404450.105022	47.442778
3504.878492	404397.713883	47.447783
3504.652766	404352.388102	47.452788
3504.978646	404291.169240	47.457793
3504.658474	404250.990226	47.462797
3504.577665	404186.157562	47.467802
3505.137398	404138.055696	47.472807
3504.530958	404089.314663	47.477812
3504.910184	404028.340111	47.482817
3504.634578	403983.403243	47.487821
3504.318308	403933.062967	47.492826
3504.516640	403892.820295	47.497831
3504.459811	403841.343335	47.502836
3504.594831	403794.380209	47.507841
3505.031495	403750.007154	47.512845
3504.485151	403692.593573	47.517850
3504.538623	403643.002453	47.522855
3504.351644	403602.063130	47.527860
3504.306950	403565.544575	47.532865
3504.545036	403517.699757	47.537869
3504.435057	403481.700254	47.542874
3504.538489	403422.447908	47.547879
3504.546203	403392.498993	47.552884
3504.591173	403338.463626	47.557889
3504.746895	403303.612366	47.562893
3504.423891	403245.169083	47.567898
3504.711302	403200.719029	47.572903
3504.499821	403157.674945	47.577908
3504.692491	403107.703483	47.582913
3504.463078	403055.543297	47.587917
3504.427286	403013.383433	47.592922
3504.545502	402969.977948	47.597927
3504.644445	402924.391175	47.602932
3504.729263	402876.342809	47.607937
3504.558849	402835.475728	47.612941
3503.852606	402789.873812	47.617946
3504.349106	402742.770976	47.622951
3504.393730	402703.645086	47.627956
3504.573775	402670.185960	47.632961
3504.469031	402610.891223	47.637965
3504.369633	402576.514439	47.642970
3504.781638	402526.021849	47.647975
3504.556960	402495.781426	47.652980
3504.555828	402438.373756	47.657985
3504.598940	402401.864078	47.662989
3504.169035	402350.117829	47.667994
3504.464690	402308.865571	47.672999
3504.633962	402280.615197	47.678004
3504.675383	402221.497888	47.683009
3504.338720	402180.810645	47.688013
3504.390112	402129.794668	47.693018
3504.313721	402100.112741	47.698023
3504.301141	402049.590179	47.703028
3504.654628	402010.283566	47.708033
3504.454124	401969.242537	47.713037
3504.033585	401929.458325	47.718042
3504.650028	401886.956766	47.723047
3504.532634	401848.136765	47.728052
3504.264023	401802.737929	47.733057
3504.347664	401777.067302	47.738061
3503.852758	401728.353876	47.743066
3504.422099	401687.587420	47.748071
3504.167880	401659.611949	47.753076
3504.340687	401609.006132	47.758081
3504.659411	401575.623625	47.763085
3504.700054	401533.702498	47.768090
3504.810959	401486.663388	47.773095
3504.727629	401442.324643	47.778100
3504.309478	401397.941387	47.783105
3504.428363	401348.944677	47.788109
3504.649437	401305.950889	47.793114
3504.269232	401248.859532	47.798119
3504.222193	401226.030427	47.803124
3504.141386	401194.214455	47.808129
3504.455775	401153.668578	47.813133
3504.232108	401111.766549	47.818138
3504.411020	401071.523119	47.823143
3504.221354	401033.349405	47.828148
3504.123897	400989.495014	47.833153
3504.412687	400959.622508	47.838157
3504.499306	400913.094647	47.843162
3504.574110	400883.487228	47.848167
3504.068425	400840.972468	47.853172
3504.363656	400796.110806	47.858177
3504.766415	400760.604516	47.863181
3504.180884	400722.040715	47.868186
3504.398062	400683.314394	47.873191
3504.509877	400641.760835	47.878196
3504.787217	400604.065671	47.883201
3504.591962	400555.400657	47.888205
3504.493507	400519.268350	47.893210
3504.607177	400475.885179	47.898215
3504.701487	400433.394372	47.903220
3504.361570	400393.390986	47.908225
3504.226938	400351.269394	47.913229
3504.149501	400329.384687	47.918234
3504.199657	400267.492777	47.923239
3503.965411	400246.523910	47.928244
3504.190862	400214.222675	47.933249
3504.400475	400172.575515	47.938253
3504.098575	400139.043243	47.943258
3504.226211	400097.054316	47.948263
3504.241387	400063.645641	47.953268
3504.071703	400028.541024	47.958273
3504.289625	399995.224669	47.963277
3503.806718	399957.429821	47.968282
3504.178721	399919.158694	47.973287
3503.948430	399895.140409	47.978292
3503.989607	399870.389841	47.983297
3503.814757	399831.017980	47.988301
3503.760917	399800.186592	47.993306
3503.826424	399770.935253	47.998311
3503.572490	399762.798481	48.003316
3503.656987	399733.213606	48.008321
3503.545562	399710.851545	48.013325
3504.011762	399684.478585	48.018330
3503.595342	399637.805882	48.023335
3504.090716	399617.245456	48.028340
3503.503255	399592.398752	48.033345
3504.060861	399571.040132	48.038349
3503.786111	399538.544090	48.043354
3503.965623	399498.044277	48.048359
3504.030969	399477.862030	48.053364
3503.783615	399456.488346	48.058369
3504.238978	399429.862957	48.063373
3503.957903	399392.566386	48.068378
3503.756445	399363.436426	48.073383
3504.077020	399340.974904	48.078388
3503.973310	399311.497941	48.083393
3504.103620	399281.803157	48.088397
3503.976602	399248.087542	48.093402
3504.054317	399219.951355	48.098407
3503.872800	399192.316689	48.103412
3503.802428	399149.267771	48.108417
3504.130024	399129.243736	48.113421
3503.687032	399109.757741	48.118426
3504.088360	399079.355945	48.123431
3503.896321	399044.126906	48.128436
3503.784324	399005.632338	48.133441
3503.939131	398985.891754	48.138445
3503.856286	398971.221899	48.143450
3503.839684	398939.214596	48.148455
3503.291488	398910.778501	48.153460
3503.471558	398878.585118	48.158465
3503.892670	398853.184477	48.163469
3503.690400	398838.687376	48.168474
3503.685722	398815.747475	48.173479
3503.726788	398807.509247	48.178484
3503.900937	398779.711830	48.183489
3503.668583	398736.918594	48.188493
3503.704405	398713.743050	48.193498
3503.899128	398689.422529	48.198503
3503.685783	398675.689389	48.203508
3503.480919	398661.853174	48.208513
3503.945666	398636.698943	48.213517
3503.553468	398629.169773	48.218522
3504.087900	398593.231812	48.223527
3503.934387	398562.720967	48.228532
3504.140849	398537.941019	48.233537
3503.751643	398517.378414	48.238541
3503.686148	398484.591387	48.243546
3503.689149	398447.727775	48.248551
3503.639456	398427.284971	48.253556
3503.275356	398407.912051	48.258561
3503.808622	398384.854545	48.263565
3503.770025	398370.481690	48.268570
3503.949713	398353.251556	48.273575
3503.502568	398334.502497	48.278580
3503.804576	398303.557918	48.283585
3503.826419	398276.065479	48.288589
3503.736709	398255.451547	48.293594
3504.018908	398235.561666	48.298599
3504.011649	398221.107170	48.303604
3504.057742	398186.293711	48.308609
3504.242912	398153.565127	48.313613
3503.628595	398129.204437	48.318618
3503.954310	398107.452428	48.323623
3503.839950	398082.345784	48.328628
3503.717322	398050.152346	48.333633
3503.943590	398022.167456	48.338637
3503.987678	398011.311695	48.343642
3503.732454	397990.420965	48.348647
3503.700313	397944.365831	48.353652
3503.600926	397916.512662	48.358657
3503.950184	397898.643562	48.363661
3503.593834	397886.814492	48.368666
3503.870203	397879.679081	48.373671
3503.692077	397859.003743	48.378676
3503.660265	397833.044393	48.383681
3503.720069	397785.626794	48.388685
3503.469863	397771.518426	48.393690
3503.758096	397752.618012	48.398695
3503.404640	397740.000803	48.403700
3503.664545	397722.832812	48.408705
3503.708058	397711.214858	48.413709
3503.498131	397695.244938	48.418714
3503.865162	397680.192733	48.423719
3504.070613	397652.693753	48.428724
3503.747484	397612.759815	48.433729
3503.948343	397589.275716	48.438733
3503.708470	397581.085107	48.443738
3503.910481	397554.221773	48.448743
3504.034631	397522.417511	48.453748
3503.993492	397496.205388	48.458753
3503.897186	397476.760707	48.463757
3503.378105	397455.863830	48.468762
3503.530064	397437.494604	48.473767
3503.459383	397428.258813	48.478772
3503.457355	397416.013360	48.483777
3503.659083	397386.634700	48.488781
3503.208251	397363.668195	48.493786
3503.543748	397328.728065	48.498791
3503.703236	397316.277147	48.503796
3503.294244	397296.275984	48.508801
3503.607073	397287.508196	48.513805
3503.787315	397271.725483	48.518810
3503.834559	397262.952224	48.523815
3503.455114	397247.544535	48.528820
3503.446066	397225.340895	48.533825
3503.806337	397218.241809	48.538829
3503.451125	397197.824892	48.543834
3503.578680	397158.245278	48.548839
3503.550674	397134.037695	48.553844
3503.370026	397127.970989	48.558849
3504.153782	397105.885950	48.563853
3503.400283	397102.813396	48.568858
3503.308905	397081.131833	48.573863
3503.720195	397069.628668	48.578868
3503.460157	397049.169989	48.583873
3503.544226	397038.865980	48.588877
3503.299008	397030.930193	48.593882
3503.656739	397016.565209	48.598887
3503.536867	396979.542852	48.603892
3503.446287	396955.345804	48.608897
3503.511102	396935.314300	48.613901
3503.371518	396919.331939	48.618906
3503.468885	396901.301981	48.623911
3503.405058	396892.141068	48.628916
3503.087769	396877.357736	48.633921
3503.867382	396858.931783	48.638925
3503.489189	396854.702628	48.643930
3503.482682	396827.340682	48.648935
3503.531879	396814.628907	48.653940
3503.284299	396809.945528	48.658945
3503.201822	396795.045838	48.663949
3503.453907	396785.475254	48.668954
3503.694466	396767.217508	48.673959
3503.681109	396758.733919	48.678964
3503.398052	396745.367455	48.683969
3503.824299	396723.622647	48.688973
3503.581026	396700.645580	48.693978
3503.487563	396668.394807	48.698983
3503.751648	396649.142101	48.703988
3503.558096	396646.609057	48.708993
3503.619540	396626.781172	48.713997
3503.578432	396615.888621	48.719002
3503.559101	396599.783922	48.724007
3503.517260	396591.635438	48.729012
3503.353874	396583.279044	48.734017
3503.694311	396573.540862	48.739021
3503.131119	396537.432068	48.744026
3503.367631	396530.862087	48.749031
3503.424290	396526.457003	48.754036
3503.538231	396504.562102	48.759041
3504.387983	396479.568918	48.764045
3503.853778	396461.646528	48.769050
3503.749466	396438.315234	48.774055
3503.778575	396428.579349	48.779060
3503.347745	396400.806721	48.784065
3504.036327	396361.435110	48.789069
3503.397780	396349.602779	48.794074
3503.752719	396343.063348	48.799079
3504.079224	396324.689021	48.804084
3503.762369	396316.765269	48.809089
3503.740404	396300.076489	48.814093
3503.240192	396270.206783	48.819098
3503.453249	396241.968355	48.824103
3503.496186	396224.684082	48.829108
3503.124087	396215.473965	48.834113
3503.421167	396198.857685	48.839117
3503.180396	396188.761286	48.844122
3503.176660	396164.066010	48.849127
3503.265924	396168.446242	48.854132
3503.146528	396166.662714	48.859137
3503.439417	396175.683124	48.864141
3503.253722	396177.264683	48.869146
3503.522835	396155.622504	48.874151
3503.162733	396141.964029	48.879156
3503.157955	396138.788931	48.884161
3503.660703	396128.946664	48.889165
3503.399277	396115.169699	48.894170
3503.274654	396088.614854	48.899175
3503.556786	396071.111796	48.904180
3503.329748	396050.341887	48.909185
3503.486742	396031.208688	48.914189
3503.396197	396031.147932	48.919194
3503.567321	396016.102910	48.924199
3503.405305	395999.132982	48.929204
3503.219124	395991.644163	48.934209
3503.950607	395979.781006	48.939213
3503.312380	395977.273017	48.944218
3503.286498	395950.828224	48.949223
3503.470074	395945.029376	48.954228
3503.491179	395938.267375	48.959233
3503.605918	395918.760205	48.964237
3503.403166	395919.379204	48.969242
3503.538815	395910.031475	48.974247
3503.640797	395896.776727	48.979252
3503.318797	395891.419901	48.984257
3503.509370	395876.981269	48.989261
3503.583769	395858.446435	48.994266
3503.282388	395828.059580	48.999271
3503.573676	395801.585902	49.004276
3503.461700	395789.866691	49.009281
3503.554518	395774.479208	49.014285
3503.097161	395769.247103	49.019290
3503.460670	395761.816811	49.024295
3503.395028	395756.060479	49.029300
3503.380253	395738.938219	49.034305
3503.213176	395726.694829	49.039309
3503.405925	395728.897801	49.044314
3503.461628	395704.039540	49.049319
3503.276825	395694.136674	49.054324
3503.510535	395689.523379	49.059329
3503.449701	395674.848089	49.064333
3503.364153	395669.831965	49.069338
3503.076253	395658.574672	49.074343
3503.393006	395646.147002	49.079348
3503.221526	395644.169072	49.084353
3503.513210	395627.883691	49.089357
3503.318045	395623.546879	49.094362
3503.587130	395613.388629	49.099367
3503.320464	395603.626750	49.104372
3503.076246	395602.677550	49.109377
3503.464270	395575.755218	49.114381
3503.355918	395572.928046	49.119386
3503.411005	395565.347104	49.124391
3503.690900	395554.500976	49.129396
3503.488069	395542.492285	49.134401
3503.551672	395529.853712	49.139405
3503.343263	395535.123328	49.144410
3503.401491	395517.226236	49.149415
3503.257034	395510.263735	49.154420
3503.249799	395497.408573	49.159425
3503.671859	395485.928355	49.164429
3503.438924	395482.919183	49.169434
3503.533325	395459.248279	49.174439
3503.624364	395432.173262	49.179444
3503.211004	395405.717915	49.184449
3503.531279	395392.857600	49.189453
3503.473487	395377.495626	49.194458
3503.331158	395374.826684	49.199463
3503.404041	395364.473178	49.204468
3503.248038	395358.986278	49.209473
3503.459085	395343.273484	49.214477
3503.329421	395333.183225	49.219482
3503.418952	395325.062771	49.224487
3503.422002	395317.871772	49.229492
3503.407201	395321.710923	49.234497
3503.715428	395303.567748	49.239501
3504.186737	395294.289549	49.244506
3504.038915	395284.253189	49.249511
3503.577710	395251.834968	49.254516
3504.003487	395240.608101	49.259521
3503.895743	395214.303661	49.264525
3503.868346	395220.228445	49.269530
3503.930057	395205.227098	49.274535
3503.823252	395170.309088	49.279540
3503.800509	395148.588959	49.284545
3504.041538	395136.809209	49.289549
3503.798083	395128.491477	49.294554
3503.803649	395107.681180	49.299559
3503.579004	395079.363920	49.304564
3503.856831	395065.113255	49.309569
3503.700867	395044.203453	49.314573
3503.294489	395033.321866	49.319578
3503.509241	395024.417698	49.324583
3503.256670	395007.030714	49.329588
3503.334636	394998.454794	49.334593
3503.499526	394994.488350	49.339597
3503.286164	394981.439484	49.344602
3503.198194	394976.169570	49.349607
3503.438928	394971.046795	49.354612
3503.171888	394967.738493	49.359617
3502.969542	394948.132370	49.364621
3502.980344	394948.155939	49.369626
3503.049964	394934.245663	49.374631
3503.019445	394928.229087	49.379636
3503.070340	394929.287555	49.384641
3503.158923	394928.815083	49.389645
3502.876677	394950.180928	49.394650
3503.064019	394927.560878	49.399655
3503.143560	394921.500099	49.404660
3502.946341	394926.488420	49.409665
3503.173481	394911.560309	49.414669
3503.186075	394902.004595	49.419674
3503.197043	394892.296706	49.424679
3503.248751	394883.623602	49.429684
3503.461221	394870.984736	49.434689
3503.249213	394870.919308	49.439693
3503.014799	394863.616294	49.444698
3503.358832	394852.022110	49.449703
3503.121394	394849.953755	49.454708
3502.734492	394855.330195	49.459713
3503.424482	394854.678806	49.464717
3503.197868	394874.129571	49.469722
3503.383991	394864.798300	49.474727
3503.155240	394859.374544	49.479732
3503.227481	394852.933871	49.484737
3503.407950	394837.785016	49.489741
3503.640307	394836.856048	49.494746
3503.774840	394825.602528	49.499751
3503.662577	394795.360168	49.504756
3502.921425	394776.531962	49.509761
3503.053891	394771.351414	49.514765
3503.181625	394776.284274	49.519770
3503.191995	394781.211765	49.524775
3503.555506	394770.833833	49.529780
3502.978996	394763.081037	49.534785
3503.341510	394760.097158	49.539789
3502.829043	394765.799958	49.544794
3503.060661	394753.894619	49.549799
3503.481225	394735.198333	49.554804
3503.316326	394729.789060	49.559809
3503.570992	394718.921523	49.564813
3503.552934	394715.926398	49.569818
3503.239639	394712.092384	49.574823
3503.310671	394695.717121	49.579828
3503.369326	394702.669069	49.584833
3503.141732	394681.110616	49.589837
3503.225397	394681.223378	49.594842
3503.151958	394667.667716	49.599847
3503.338402	394657.523248	49.604852
3503.189951	394656.938794	49.609857
3503.387324	394633.503728	49.614861
3503.756128	394637.988910	49.619866
3503.229931	394624.612172	49.624871
3503.438632	394624.220819	49.629876
3503.403669	394603.035956	49.634881
3503.642250	394597.252858	49.639885
3503.522128	394602.126435	49.644890
3503.560163	394592.921998	49.649895
3503.646081	394581.778321	49.654900
3503.454549	394551.015662	49.659905
3503.873423	394529.651617	49.664909
3503.542162	394514.793244	49.669914
3503.554141	394510.090582	49.674919
3503.465873	394500.043785	49.679924
3503.464785	394493.564737	49.684929
3503.666218	394483.265197	49.689933
3503.290052	394479.238617	49.694938
3503.758180	394471.180326	49.699943
3503.643021	394459.054584	49.704948
3502.711826	394457.180887	49.709953
3503.395432	394448.221897	49.714957
3503.314293	394441.756506	49.719962
3503.068443	394434.455338	49.724967
3503.281895	394423.594731	49.729972
3502.907439	394419.593260	49.734977
3503.164049	394403.491053	49.739981
3502.851761	394403.036204	49.744986
3502.856956	394392.922594	49.749991
3503.286755	394380.500497	49.754996
3502.907500	394376.906381	49.760001
3502.967788	394395.114256	49.765005
3502.909326	394404.957474	49.770010
3502.838294	394406.062189	49.775015
3502.738199	394394.975612	49.780020
3502.761991	394398.198481	49.785025
3502.915056	394397.765808	49.790029
3502.961333	394404.186353	49.795034
3502.692536	394398.311991	49.800039
3502.982053	394390.207949	49.805044
3502.990054	394387.284568	49.810049
3503.018409	394385.882243	49.815053
3503.242585	394379.695021	49.820058
3503.116171	394380.046927	49.825063
3502.999836	394394.219540	49.830068
3502.971907	394400.297033	49.835073
3503.112549	394391.227466	49.840077
3503.032863	394390.732901	49.845082
3502.868904	394383.900506	49.850087
3502.950919	394370.496025	49.855092
3502.748992	394377.060594	49.860097
3503.132448	394381.899037	49.865101
3502.926828	394394.384500	49.870106
3502.766662	394393.573361	49.875111
3502.797184	394383.658694	49.880116
3502.834335	394382.331094	49.885121
3502.979226	394378.266347	49.890125
3502.933066	394382.873241	49.895130
3503.055937	394399.749165	49.900135
3503.165274	394398.231378	49.905140
3502.774932	394399.339798	49.910145
3502.997430	394393.406954	49.915149
3503.293467	394385.886202	49.920154
3503.005520	394372.087534	49.925159
3503.245918	394374.663606	49.930164
3502.764966	394378.709520	49.935169
3503.124690	394380.604586	49.940173
3503.092694	394394.152984	49.945178
3503.113222	394389.245572	49.950183
3503.176887	394379.782604	49.955188
3503.011176	394381.487891	49.960193
3502.780138	394375.607076	49.965197
3502.899099	394364.737173	49.970202
3502.916542	394364.505520	49.975207
3503.294621	394369.319474	49.980212
3502.893123	394385.370224	49.985217
3503.155758	394383.673806	49.990221
3503.226363	394378.732433	49.995226
3502.894785	394373.834323	50.000231
3503.019610	394367.155885	50.005236
3503.169820	394366.799926	50.010241
3503.266017	394361.981224	50.015245
3503.180831	394360.013881	50.020250
3503.218181	394346.617016	50.025255
3503.177386	394343.422464	50.030260
3502.469844	394344.610458	50.035265
3502.934100	394353.856259	50.040269
3502.804567	394366.125471	50.045274
3502.899331	394362.170917	50.050279
3503.328622	394356.075711	50.055284
3502.825295	394350.546292	50.060289
3503.005508	394353.437550	50.065293
3502.839198	394350.493110	50.070298
3503.049280	394376.120228	50.075303
3503.251055	394376.416095	50.080308
3503.280316	394380.832249	50.085313
3503.553085	394375.551449	50.090317
3503.023249	394365.402142	50.095322
3502.893565	394355.997590	50.100327
3503.349812	394347.306071	50.105332
3503.173565	394350.918827	50.110337
3503.261425	394334.870806	50.115341
3503.203490	394333.127488	50.120346
3502.861672	394325.766453	50.125351
3503.038092	394315.445717	50.130356
3503.029549	394323.857537	50.135361
3502.928662	394333.911294	50.140365
3503.200766	394340.750654	50.145370
3503.295588	394342.919635	50.150375
3502.909703	394335.642354	50.155380
3503.294332	394331.511255	50.160385
3503.192708	394327.971363	50.165389
3503.250859	394326.208223	50.170394
3503.127026	394318.073106	50.175399
3503.482447	394308.509480	50.180404
3503.128269	394314.973014	50.185409
3502.748861	394302.130061	50.190413
3502.828764	394299.118167	50.195418
3502.852328	394306.609788	50.200423
3502.935890	394324.203917	50.205428
3502.709894	394328.663665	50.210433
3502.932307	394320.571062	50.215437
3503.043713	394319.840595	50.220442
3502.832527	394313.956378	50.225447
3503.030824	394317.886318	50.230452
3503.166946	394336.259143	50.235457
3503.113811	394334.108462	50.240461
3503.304952	394336.133953	50.245466
3503.471226	394333.666310	50.250471
3503.282225	394321.299031	50.255476
3503.658306	394324.563390	50.260481
3503.629475	394316.971047	50.265485
3503.232607	394313.583203	50.270490
3503.295659	394306.356302	50.275495
3503.430483	394293.679629	50.280500
3503.376651	394296.509220	50.285505
3503.508422	394291.074617	50.290509
3503.928639	394265.060313	50.295514
3503.323239	394244.201275	50.300519
3503.774357	394230.860751	50.305524
3503.682184	394228.691320	50.310529
3503.330172	394216.834603	50.315533
3503.404300	394220.938212	50.320538
3503.559392	394217.761017	50.325543
3503.350535	394198.866958	50.330548
3502.998457	394206.397337	50.335553
3503.121160	394194.434144	50.340557
3503.119299	394189.454294	50.345562
3502.821719	394186.328981	50.350567
3502.894405	394173.002231	50.355572
3502.709685	394185.204714	50.360577
3502.860627	394194.199156	50.365581
3502.936027	394203.892539	50.370586
3503.074447	394201.785368	50.375591
3503.126290	394192.908766	50.380596
3502.700495	394186.934124	50.385601
3502.865970	394184.695287	50.390605
3502.934964	394199.192074	50.395610
3503.144619	394212.064068	50.400615
3503.024618	394206.621623	50.405620
3502.564050	394217.702379	50.410625
3503.066057	394204.073654	50.415629
3502.817969	394203.760294	50.420634
3502.647552	394221.423262	50.425639
3502.964276	394220.149553	50.430644
3503.229836	394230.039138	50.435649
3503.138954	394233.434059	50.440653
3503.029601	394226.566895	50.445658
3503.119302	394222.765640	50.450663
3503.281548	394214.632464	50.455668
3502.838012	394215.597520	50.460673
3503.177629	394211.347046	50.465677
3503.072734	394212.762458	50.470682
3502.728564	394238.713016	50.475687
3503.269477	394229.879961	50.480692
3503.120162	394236.816712	50.485697
3503.002794	394227.384607	50.490701
3503.070627	394227.296802	50.495706
3503.001741	394220.244863	50.500711
3502.932851	394206.662804	50.505716
3503.185659	394222.144555	50.510721
3503.070212	394208.494218	50.515725
3503.192646	394206.745504	50.520730
3503.018738	394196.027182	50.525735
3503.311473	394173.896739	50.530740
3503.070434	394154.728647	50.535745
3503.225979	394109.677178	50.540749
3503.155615	394044.718023	50.545754
3502.651637	393986.566210	50.550759
3503.154599	393898.920034	50.555764
3502.824945	393821.808200	50.560769
3503.196121	393724.630091	50.565773
3502.875112	393609.249580	50.570778
3502.779664	393494.363708	50.575783
3503.075056	393353.467299	50.580788
3502.918408	393212.647410	50.585793
3502.774185	393053.656576	50.590797
3502.987917	392898.212012	50.595802
3502.910092	392716.745463	50.600807
3503.246624	392523.975633	50.605812
3502.988083	392325.715832	50.610817
3502.992027	392097.501367	50.615821
3502.728674	391880.384601	50.620826
3502.565134	391640.175847	50.625831
3502.819504	391383.605092	50.630836
3502.467808	391125.458475	50.635841
3502.541939	390851.049578	50.640845
3502.625933	390571.503264	50.645850
3502.527567	390275.696194	50.650855
3502.628777	389969.737950	50.655860
3502.763483	389661.407519	50.660865
3502.702882	389318.189666	50.665869
3502.650334	388967.672935	50.670874
3502.696409	388612.865856	50.675879
3502.564842	388236.940540	50.680884
3502.585273	387845.151544	50.685889
3502.801478	387445.699757	50.690893
3502.682570	387029.348231	50.695898
3502.391052	386599.296312	50.700903
3502.262608	386152.614154	50.705908
3502.261546	385702.193136	50.710913
3502.503346	385236.830149	50.715917
3502.510088	384747.456090	50.720922
3502.252610	384259.949646	50.725927
3502.193821	383740.095952	50.730932
3502.145959	383210.878084	50.735937
3502.092658	382665.715010	50.740941
3501.974950	382113.538089	50.745946
3501.973654	381532.074138	50.750951
3501.981284	380942.972317	50.755956
3501.695038	380347.071999	50.760961
3501.879633	379719.634930	50.765965
3501.919825	379078.584784	50.770970
3501.732615	378428.409246	50.775975
3502.144929	377750.128704	50.780980
3501.662772	377057.521602	50.785985
3501.366609	376344.606104	50.790989
3501.677376	375630.275395	50.795994
3501.663536	374891.323467	50.800999
3501.948337	374121.870920	50.806004
3501.646542	373341.339605	50.811009
3501.101493	372530.931157	50.816013
3501.210577	371720.468587	50.821018
3501.056110	370891.597604	50.826023
3500.805222	370039.508058	50.831028
3500.966430	369170.341617	50.836033
3500.864862	368279.635189	50.841037
3500.821917	367368.095378	50.846042
3500.548707	366446.883270	50.851047
3500.622435	365495.198831	50.856052
3500.466952	364535.187688	50.861057
3500.250069	363546.296784	50.866061
3500.535311	362542.492387	50.871066
3499.722432	361526.742814	50.876071
3499.937946	360474.318036	50.881076
3499.641988	359419.281662	50.886081
3499.724670	358343.905612	50.891085
3499.821450	357244.231827	50.896090
3499.596274	356123.800929	50.901095
3499.870364	354994.732404	50.906100
3499.844057	353827.933458	50.911105
3499.523285	352651.027445	50.916109
3499.842405	351448.183289	50.921114
3499.309210	350231.662092	50.926119
3498.998618	348978.891057	50.931124
3498.302242	347730.195633	50.936129
3498.313287	346468.928385	50.941133
3498.306532	345178.419784	50.946138
3497.859058	343869.986517	50.951143
3497.963972	342537.758328	50.956148
3497.754773	341200.050062	50.961153
3497.656635	339837.551673	50.966157
3497.354346	338463.115486	50.971162
3496.953241	337052.776639	50.976167
3497.212466	335634.498488	50.981172
3496.564739	334205.342094	50.986177
3496.760374	332755.311915	50.991181
3496.362715	331291.753081	50.996186
3496.242421	329814.185713	51.001191
3496.290479	328302.470034	51.006196
3495.937414	326797.196759	51.011201
3495.811620	325254.785465	51.016205
3495.542949	323705.002274	51.021210
3495.258230	322145.560400	51.026215
3495.266388	320559.046716	51.031220
3494.930493	318945.467100	51.036225
3494.688364	317330.355171	51.041229
3494.828741	315700.399321	51.046234
3494.049036	314053.428945	51.051239
3493.783570	312385.482066	51.056244
3493.173736	310716.461185	51.061249
3493.114539	309032.084471	51.066253
3493.324631	307323.998290	51.071258
3492.482130	305603.325221	51.076263
3492.379459	303871.134531	51.081268
3492.634101	302128.255964	51.086273
3492.031058	300354.935315	51.091277
3492.054538	298579.997074	51.096282
3491.524888	296788.315175	51.101287
3491.239296	294971.936670	51.106292
3491.044134	293148.610900	51.111297
3490.441107	291325.044835	51.116301
3490.335373	289485.195351	51.121306
3490.216720	287612.979983	51.126311
3490.047405	285735.195073	51.131316
3489.839046	283853.520771	51.136321
3489.024851	281954.965739	51.141325
3489.189352	280034.778347	51.146330
3488.493347	278110.438227	51.151335
3488.259642	276159.412028	51.156340
3487.820542	274218.029156	51.161345
3487.436540	272254.285584	51.166349
3487.346514	270277.412032	51.171354
3486.688354	268287.684665	51.176359
3486.479389	266297.308830	51.181364
3486.130347	264281.657654	51.186369
3485.631891	262263.706608	51.191373
3485.551412	260229.327841	51.196378
3484.875893	258187.941231	51.201383
3484.841084	256128.182736	51.206388
3484.361992	254065.953613	51.211393
3483.415027	251995.198625	51.216397
3483.578062	249911.473775	51.221402
3482.936644	247816.916535	51.226407
3482.699490	245713.283889	51.231412
3482.227340	243603.743532	51.236417
3481.609135	241476.058286	51.241421
3481.321222	239347.798372	51.246426
3480.729424	237206.621080	51.251431
3480.167149	235062.557080	51.256436
3479.734708	232910.625783	51.261441
3479.139922	230746.295898	51.266445
3479.045073	228571.621877	51.271450
3478.994086	226395.189994	51.276455
3478.344278	224201.273406	51.281460
3477.744896	222004.814216	51.286465
3477.395939	219791.877653	51.291469
3477.207293	217578.779332	51.296474
3476.344537	215347.000085	51.301479
3476.196176	213113.417434	51.306484
3475.587067	210867.490060	51.311489
3475.170372	208625.023270	51.316493
3474.341208	206360.777048	51.321498
3473.649722	204096.366415	51.326503
3473.292982	201826.516041	51.331508
3472.603208	199554.678326	51.336513
3471.926799	197285.163103	51.341517
3471.756551	194998.058291	51.346522
3470.838615	192716.976367	51.351527
3470.481012	190421.141639	51.356532
3469.837771	188128.940697	51.361537
3468.937806	185825.646787	51.366541
3468.831388	183512.510147	51.371546
3467.927327	181207.329454	51.376551
3467.507879	178881.562503	51.381556
3466.756415	176574.201380	51.386561
3466.151843	174251.052952	51.391565
3466.165890	171920.451807	51.396570
3465.447658	169593.866649	51.401575
3464.661451	167253.719653	51.406580
3463.854097	164912.996223	51.411585
3463.010119	162573.266860	51.416589
3463.043489	160222.002227	51.421594
3462.081386	157884.316511	51.426599
3461.309636	155524.091790	51.431604
3460.777000	153169.979366	51.436609
3460.042506	150816.410464	51.441613
3459.112220	148454.854786	51.446618
3458.307815	146097.570388	51.451623
3457.557377	143736.930681	51.456628
3456.928140	141321.680125	51.461633
3455.937737	138967.790789	51.466637
3455.214030	136603.998740	51.471642
3454.442769	134265.927875	51.476647
3453.804380	131907.802116	51.481652
3453.015662	129558.056589	51.486657
3452.290138	127209.908248	51.491661
3451.816261	124858.626139	51.496666
3450.728597	122511.350381	51.501671
3449.812220	120161.240896	51.506676
3449.010809	117827.342011	51.511681
3448.196297	115490.150211	51.516685
3447.299083	113151.624784	51.521690
3446.518464	110826.506531	51.526695
3445.591992	108489.300430	51.531700
3444.720513	106169.376364	51.536705
3443.443402	103859.764439	51.541709
3442.558173	101545.422968	51.546714
3442.075344	99243.042808	51.551719
3441.181616	96937.415170	51.556724
3440.100770	94629.679931	51.561729
3439.237972	92341.919284	51.566733
3438.183062	90056.687300	51.571738
3437.053467	87783.134563	51.576743
3436.367412	85500.305957	51.581748
3435.402329	83245.929341	51.586753
3434.061402	80982.921883	51.591757
3433.451457	78738.327992	51.596762
3431.714863	76502.347208	51.601767
3430.951927	74273.866547	51.606772
3430.293450	72057.549433	51.611777
3429.032532	69855.075314	51.616781
3428.164604	67650.652837	51.621786
3426.921088	65473.814943	51.626791
3425.643927	63288.276094	51.631796
3424.335451	61122.166072	51.636801
3422.701857	58975.430208	51.641805
3422.008631	56838.167503	51.646810
3420.247658	54726.571292	51.651815
3419.154633	52623.635113	51.656820
3417.888510	50534.632720	51.661825
3416.785433	48456.160647	51.666829
3415.403081	46404.653649	51.671834
3413.600869	44371.853552	51.676839
3412.354687	42353.705661	51.681844
3410.867304	40354.135568	51.686849
3409.424539	38383.626726	51.691853
3408.137957	36425.215755	51.696858
3406.367830	34492.619580	51.701863
3404.668988	32590.783629	51.706868
3403.012819	30711.817956	51.711873
3400.692095	28875.488265	51.716877
3398.451662	27055.966117	51.721882
3394.407451	25330.545417	51.726887
3389.745462	23675.643175	51.731892
3384.477061	22105.765037	51.736897
3378.362427	20615.644848	51.741901
3372.394530	19222.350300	51.746906
3366.506049	17952.484743	51.751911
3361.859895	16766.686563	51.756916
3356.748876	15683.191620	51.761921
3352.058974	14703.118627	51.766925
3347.921257	13810.839531	51.771930
3343.706448	13046.300023	51.776935
3339.399545	12353.612041	51.781940
3335.490296	11747.549729	51.786945
3332.014454	11208.473754	51.791949
3329.322995	10753.234248	51.796954
3326.414571	10378.560520	51.801959
3323.977961	10052.053676	51.806964
3322.465852	9781.273743	51.811969
3320.440031	9559.513869	51.816973
3319.050299	9365.612886	51.821978
3317.613867	9241.835881	51.826983
3316.600215	9118.768025	51.831988
3316.049876	9026.312617	51.836993
3315.433181	8961.338422	51.841997
3314.998519	8900.417132	51.847002
3314.213115	8855.894051	51.852007
3313.992300	8833.999720	51.857012
3313.751771	8810.987147	51.862017
3313.373149	8792.371007	51.867021
3313.044842	8784.283369	51.872026
3312.624057	8784.541667	51.877031
3312.492034	8787.613185	51.882036
3312.415474	8775.800098	51.887041
3312.133661	8777.832436	51.892045
3312.291939	8774.211424	51.897050
3312.164901	8772.013552	51.902055
3311.725703	8753.531027	51.907060
3311.811400	8748.003000	51.912065
3311.671451	8753.300180	51.917069
3311.669877	8719.525030	51.922074
3311.405741	8709.129489	51.927079
3311.047920	8678.247799	51.932084
3311.494633	8647.923828	51.937089
3310.855519	8612.700166	51.942093
3310.571664	8557.488918	51.947098
3310.393283	8520.232604	51.952103
3310.245658	8474.536877	51.957108
3309.564176	8418.709999	51.962113
3309.387641	8367.894849	51.967117
3308.560253	8310.045940	51.972122
3308.259824	8267.885471	51.977127
3308.069787	8196.434118	51.982132
3307.426687	8135.629511	51.987137
3306.639995	8080.388891	51.992141
3306.292468	8019.574513	51.997146
3305.554800	7956.271070	52.002151
3305.770862	7906.838091	52.007156
3305.406284	7835.005064	52.012161
3304.587831	7769.518820	52.017165
3303.936890	7684.084646	52.022170
3303.392764	7625.005848	52.027175
3302.775862	7545.409754	52.032180
3302.678887	7460.816495	52.037185
3301.805353	7398.571539	52.042189
3301.385725	7320.794979	52.047194
3300.847925	7253.774091	52.052199
3299.914887	7170.810022	52.057204
3299.330794	7083.268310	52.062209
3298.694350	7008.187985	52.067213
3298.088997	6932.970015	52.072218
3297.694473	6863.811205	52.077223
3297.188070	6790.005735	52.082228
3296.582416	6710.033544	52.087233
3296.121880	6630.334710	52.092237
3295.602890	6553.429429	52.097242
3294.683036	6468.142427	52.102247
3294.385694	6394.599226	52.107252
3293.805865	6304.867052	52.112257
3293.134497	6223.702541	52.117261
3293.021829	6136.808089	52.122266
3292.014541	6048.998399	52.127271
3291.408383	5967.534998	52.132276
3290.923695	5875.532666	52.137281
3289.999923	5802.091299	52.142285
3289.241594	5709.211883	52.147290
3288.697866	5631.989883	52.152295
3288.243254	5543.349369	52.157300
3287.879658	5454.433980	52.162305
3287.172520	5371.409053	52.167309
3286.533515	5273.537351	52.172314
3285.495745	5191.530133	52.177319
3284.718212	5102.992242	52.182324
3284.327689	5018.687862	52.187329
3283.292743	4942.530761	52.192333
3282.896343	4852.786459	52.197338
3282.351294	4784.119584	52.202343
3281.596431	4689.301299	52.207348
3281.247342	4600.278427	52.212353
3280.494274	4524.272595	52.217357
3280.159531	4432.757569	52.222362
3279.442553	4354.254180	52.227367
3278.456583	4262.309671	52.232372
3277.900877	4170.026077	52.237377
3276.966126	4087.560008	52.242381
3276.615033	3998.328429	52.247386
3275.786004	3923.633476	52.252391
3274.820885	3838.607536	52.257396
3274.386001	3752.745265	52.262401
3273.672619	3684.483029	52.267405
3273.074360	3600.607785	52.272410
3272.336213	3524.548129	52.277415
3271.323889	3434.114007	52.282420
3271.593720	3355.664129	52.287425
3270.717255	3277.549434	52.292429
3270.048023	3194.917893	52.297434
3269.040813	3120.560378	52.302439
3268.757638	3039.321314	52.307444
3268.427956	2936.588274	52.312449
3266.734222	2867.419239	52.317453
3266.436339	2787.928192	52.322458
3265.630398	2718.106760	52.327463
3265.138294	2639.739268	52.332468
3264.313896	2556.153756	52.337473
3263.614095	2490.202297	52.342477
3262.982798	2408.830920	52.347482
3262.249450	2347.413191	52.352487
3262.025891	2273.036339	52.357492
3261.189470	2193.016532	52.362497
3260.565953	2113.891649	52.367501
3259.841251	2039.063035	52.372506
3259.447575	1966.474234	52.377511
3258.428163	1897.979871	52.382516
3258.007621	1826.973027	52.387521
3257.310881	1757.726986	52.392525
3256.898970	1669.407963	52.397530
3256.061815	1604.884313	52.402535
3255.122481	1517.801458	52.407540
3254.673337	1438.299240	52.412545
3253.684195	1375.826043	52.417549
3253.630091	1299.052732	52.422554
3252.324177	1230.383637	52.427559
3251.985329	1167.350946	52.432564
3251.347895	1097.624374	52.437569
3250.495644	1034.493207	52.442573
3249.929427	955.993205	52.447578
3248.947428	888.934140	52.452583
3248.105701	821.611394	52.457588
3247.763238	758.201220	52.462593
3246.256881	702.129059	52.467597
3246.074677	642.405323	52.472602
3245.132067	585.797925	52.477607
3244.336442	527.556274	52.482612
3243.703464	486.334568	52.487617
3242.867229	426.052731	52.492621
3242.555577	372.381731	52.497626
3241.749412	329.800165	52.502631
3240.607055	279.172691	52.507636
3239.641985	229.902179	52.512641
3238.835079	204.112551	52.517645
3237.784622	170.117095	52.522650
3237.256629	146.248430	52.527655
3235.328329	130.355306	52.532660
3234.029615	124.655861	52.537665
3232.702213	129.180439	52.542669
3231.895013	141.048886	52.547674
3232.181993	134.355003	52.552679
3231.626301	143.023052	52.557684
3231.150014	138.645570	52.562689
3230.474080	146.273921	52.567693
3229.780444	145.191267	52.572698
3228.857293	138.447546	52.577703
3228.175877	142.332043	52.582708
3228.463728	135.940374	52.587713
3227.528299	144.223701	52.592717
3226.772841	139.018405	52.597722
3225.950740	134.702372	52.602727
3225.372808	147.100065	52.607732
3224.764825	136.240745	52.612737
3224.193750	139.556929	52.617741
3223.405421	135.598277	52.622746
3223.084881	130.329736	52.627751
3221.848303	137.864394	52.632756
3221.557997	135.040767	52.637761
3220.953270	137.522717	52.642765
3220.511086	138.239699	52.647770
3219.575277	136.722377	52.652775
3218.777501	138.303380	52.657780
3217.796546	135.436300	52.662785
3217.156575	143.411788	52.667789
3216.925027	139.919320	52.672794
3216.450392	139.938045	52.677799
3215.776871	145.941282	52.682804
3215.373785	139.271344	52.687809
3214.509954	137.292524	52.692813
3213.851650	136.223178	52.697818
3213.767171	138.756773	52.702823
3212.487547	142.488475	52.707828
3211.562567	134.075766	52.712833
3211.336473	133.086130	52.717837
3210.587558	141.857844	52.722842
3210.199935	141.765785	52.727847
3209.417046	139.754981	52.732852
3208.816935	129.105899	52.737857
3207.993549	143.475743	52.742861
3207.054047	139.819230	52.747866
3206.667838	136.944094	52.752871
3206.330029	132.452962	52.757876
3205.372937	137.205986	52.762881
3204.713714	138.878976	52.767885
3204.318411	139.031382	52.772890
3203.855856	143.286245	52.777895
3203.357965	145.991519	52.782900
3202.363438	146.526557	52.787905
3201.294256	148.370243	52.792909
3200.531569	138.948512	52.797914
3200.014474	135.230098	52.802919
3199.066819	142.680665	52.807924
3199.316837	129.332058	52.812929
3198.587892	138.882711	52.817933
3197.739399	132.680839	52.822938
3197.555488	140.819195	52.827943
3196.365192	138.122486	52.832948
3195.400005	127.831036	52.837953
3195.378788	139.160209	52.842957
3194.982241	133.077700	52.847962
3194.593519	133.066749	52.852967
3193.167769	140.315186	52.857972
3192.135683	135.900432	52.862977
3191.427553	124.382857	52.867981
3191.607355	133.310104	52.872986
3190.962697	128.956265	52.877991
3189.662738	131.449233	52.882996
3189.345085	127.756748	52.888001
3188.815993	134.437923	52.893005
3188.338200	127.283005	52.898010
3187.914341	135.221568	52.903015
3186.727225	134.312832	52.908020
3185.414676	122.024595	52.913025
3184.974244	135.851779	52.918029
3184.433253	131.895088	52.923034
3184.060491	128.922134	52.928039
3183.397968	125.271597	52.933044
3183.042061	131.638978	52.938049
3182.624709	134.624960	52.943053
3181.498213	126.337084	52.948058
3180.372915	125.369631	52.953063
3179.917125	125.976837	52.958068
3179.680648	118.936219	52.963073
3179.167536	135.341946	52.968077
3178.059976	122.511463	52.973082
3177.571316	125.994351	52.978087
3176.323711	130.455570	52.983092
3176.495288	123.465628	52.988097
3175.788057	126.642841	52.993101
3175.216347	126.895649	52.998106
3174.392510	131.400913	53.003111
3173.218223	134.644108	53.008116
3172.492112	121.138998	53.013121
3172.491260	132.580340	53.018125
3171.893765	137.041410	53.023130
3171.103863	125.350314	53.028135
3170.296993	136.116226	53.033140
3169.865487	128.646699	53.038145
3168.641025	126.796606	53.043149
3168.398566	126.884218	53.048154
3168.433708	123.551057	53.053159
3167.140416	127.247205	53.058164
3166.608996	125.810405	53.063169
3165.680279	125.013839	53.068173
3164.651296	122.307737	53.073178
3164.013233	129.605146	53.078183
3163.681014	127.511827	53.083188
3163.262578	126.986099	53.088193
3162.654266	125.063500	53.093197
3161.694228	127.100907	53.098202
3160.949917	128.526733	53.103207
3159.947232	139.134659	53.108212
3160.109640	121.572307	53.113217
3159.841805	128.510416	53.118221
3159.248144	126.568342	53.123226
3158.081239	131.146826	53.128231
3157.055364	134.545847	53.133236
3156.364879	132.985833	53.138241
3155.702581	135.326838	53.143245
3154.946206	134.207545	53.148250
3154.533083	125.009130	53.153255
3153.625418	131.834719	53.158260
3153.469742	131.147653	53.163265
3152.846803	128.294418	53.168269
3151.957227	124.670441	53.173274
3151.321590	117.273692	53.178279
3150.464310	131.536028	53.183284
3150.164790	125.232876	53.188289
3149.032810	132.540465	53.193293
3148.938274	125.583357	53.198298
3148.674188	123.768130	53.203303
3146.949820	129.996692	53.208308
3146.973231	117.220094	53.213313
3146.577339	127.239221	53.218317
3145.924992	129.054722	53.223322
3144.685567	121.094830	53.228327
3143.897653	127.903905	53.233332
3143.554860	117.114964	53.238337
3142.735912	130.379194	53.243341
3141.918902	124.907336	53.248346
3141.688077	118.822577	53.253351
3140.786820	127.922281	53.258356
3139.815358	125.267933	53.263361
3139.185479	126.966309	53.268365
3139.256545	116.448493	53.273370
3138.667821	126.183204	53.278375
3137.203094	128.405919	53.283380
3136.901064	117.789615	53.288385
3136.477028	122.738929	53.293389
3135.547051	120.642745	53.298394
3135.010994	126.686438	53.303399
3134.424145	131.480813	53.308404
3133.731013	129.978095	53.313409
3132.676788	127.641040	53.318413
3132.099357	118.991351	53.323418
3131.638066	116.207211	53.328423
3130.887919	123.061147	53.333428
3130.552299	113.821475	53.338433
3129.832450	124.632511	53.343437
3129.013407	125.905717	53.348442
3128.110031	116.795021	53.353447
3127.173559	125.578249	53.358452
3127.390688	116.796359	53.363457
3127.005280	119.134265	53.368461
3125.656018	115.823304	53.373466
3124.621284	116.931657	53.378471
3124.394198	126.230378	53.383476
3124.094270	114.414536	53.388481
3123.307349	115.930933	53.393485
3122.466023	115.815743	53.398490
3122.257730	112.773251	53.403495
3121.169401	118.700911	53.408500
3120.692553	113.621721	53.413505
3119.927280	126.022981	53.418509
3118.994547	124.635807	53.423514
3118.090653	114.915349	53.428519
3117.138370	119.376247	53.433524
3116.895077	118.704942	53.438529
3116.085439	118.842096	53.443533
3115.654792	120.840767	53.448538
3115.924917	122.003275	53.453543
3114.621066	129.669040	53.458548
3113.727227	118.103484	53.463553
3113.087453	123.677803	53.468557
3112.411129	123.702577	53.473562
3112.484644	114.510237	53.478567
3111.331868	122.859906	53.483572
3110.571979	118.686425	53.488577
3109.590666	119.289875	53.493581
3109.498888	114.701065	53.498586
3109.325581	119.927269	53.503591
3107.781467	126.440428	53.508596
3106.942807	112.446954	53.513601
3106.709325	111.591215	53.518605
3106.052405	115.810205	53.523610
3105.400662	111.861006	53.528615
3104.603763	124.373850	53.533620
3104.386068	121.921503	53.538625
3103.099154	121.145097	53.543629
3102.454964	122.547112	53.548634
3102.624478	110.932904	53.553639
3101.402935	120.439031	53.558644
3100.471465	116.131057	53.563649
3100.070449	116.945220	53.568653
3099.606325	126.874952	53.573658
3098.924343	108.987961	53.578663
3097.729281	110.988165	53.583668
3097.634929	117.476241	53.588673
3096.966010	110.108876	53.593677
3095.968022	109.198635	53.598682
3095.202436	110.814018	53.603687
3095.424253	112.473056	53.608692
3094.793810	112.794722	53.613697
3093.656938	105.673100	53.618701
3092.862631	114.817682	53.623706
3092.198908	113.774146	53.628711
3091.172920	114.111686	53.633716
3090.536718	111.614010	53.638721
3089.692878	114.540233	53.643725
3088.966288	113.469940	53.648730
3089.112511	105.851989	53.653735
3088.551688	110.024559	53.658740
3087.893415	113.451169	53.663745
3086.656801	117.421848	53.668749
3085.926870	116.869614	53.673754
3085.682183	113.481247	53.678759
3085.127875	114.965008	53.683764
3084.596601	108.102668	53.688769
3083.636350	109.729603	53.693773
3082.688198	118.769819	53.698778
3082.141858	105.260084	53.703783
3081.821587	119.642226	53.708788
3081.112407	114.064726	53.713793
3080.450920	113.276593	53.718797
3079.822284	113.864787	53.723802
3079.226480	114.066459	53.728807
3078.621652	122.242772	53.733812
3078.005273	115.833908	53.738817
3077.624237	112.996194	53.743821
3075.975963	115.790665	53.748826
3075.413229	118.841750	53.753831
3075.209882	122.716408	53.758836
3074.617320	115.421260	53.763841
3073.696461	119.007209	53.768845
3072.576326	120.916065	53.773850
3072.452153	113.640752	53.778855
3072.137183	117.244752	53.783860
3071.404684	119.199082	53.788865
3070.238618	113.513733	53.793869
3069.277741	112.448738	53.798874
3069.300012	111.488119	53.803879
3068.425690	115.780968	53.808884
3067.799198	122.462993	53.813889
3067.104242	105.347162	53.818893
3066.009504	115.415820	53.823898
3065.808572	106.523008	53.828903
3065.098288	112.314632	53.833908
3064.678294	108.765173	53.838913
3064.173361	108.333178	53.843917
3063.084789	119.997062	53.848922
3062.802591	105.567482	53.853927
3061.752401	118.861739	53.858932
3061.040321	101.663185	53.863937
3060.590490	107.175441	53.868941
3059.649999	111.940637	53.873946
3059.567374	107.690523	53.878951
3059.039660	113.129250	53.883956
3058.515215	117.037457	53.888961
3057.389374	112.085352	53.893965
3056.211121	117.498660	53.898970
3056.002117	106.356495	53.903975
3055.308552	120.422298	53.908980
3054.314447	113.296025	53.913985
3054.069358	115.625352	53.918989
3052.982009	127.636788	53.923994
3052.549507	117.669619	53.928999
3052.040171	114.998300	53.934004
3051.414757	112.308527	53.939009
3050.645975	107.950662	53.944013
3049.882016	109.320646	53.949018
3049.764403	101.411473	53.954023
3048.713347	110.911759	53.959028
3048.392790	107.728592	53.964033
3047.835366	111.973609	53.969037
3046.993241	113.228269	53.974042
3046.189677	106.222993	53.979047
3044.817200	118.401560	53.984052
3044.698415	110.969808	53.989057
3044.435658	108.492800	53.994061
3042.920650	115.805447	53.999066
3042.730768	101.607990	54.004071
3042.416481	111.902098	54.009076
3041.273890	106.737735	54.014081
3040.608012	106.941911	54.019085
3040.112037	110.129613	54.024090
3039.469939	98.574760	54.029095
3038.895540	106.266273	54.034100
3037.883390	107.227495	54.039105
3037.450095	101.932463	54.044109
3037.096555	107.875492	54.049114
3036.405190	103.560059	54.054119
3035.991144	109.331064	54.059124
3035.086571	115.058786	54.064129
3034.047707	104.248289	54.069133
3033.076456	114.283217	54.074138
3033.130799	109.834046	54.079143
3031.927379	111.744113	54.084148
3031.640249	108.114326	54.089153
3030.464439	96.866588	54.094157
3030.046920	109.383672	54.099162
3030.348042	106.394271	54.104167
3029.371836	98.232743	54.109172
3028.443889	102.781854	54.114177
3027.613263	108.233261	54.119181
3027.018674	115.138380	54.124186
3027.039519	114.377736	54.129191
3025.164834	110.738963	54.134196
3024.580543	105.307894	54.139201
3024.299978	110.311637	54.144205
3023.441933	106.527174	54.149210
3022.755319	108.765765	54.154215
3022.179012	109.323708	54.159220
3021.842957	104.121401	54.164225
3021.106736	99.783637	54.169229
3020.669022	106.288930	54.174234
3020.415634	104.645959	54.179239
3019.943230	108.673165	54.184244
3018.518022	108.039223	54.189249
3017.561595	100.287991	54.194253
3016.579066	108.967379	54.199258
3016.054885	109.063269	54.204263
3015.488977	112.133056	54.209268
3014.980770	109.850356	54.214273
3014.234829	105.133736	54.219277
3013.646621	109.432565	54.224282
3013.900561	104.944160	54.229287
3013.100197	115.930391	54.234292
3012.042963	114.404646	54.239297
3011.315663	103.770254	54.244301
3009.783464	109.994818	54.249306
3009.534273	104.944638	54.254311
3008.753437	109.981366	54.259316
3008.683466	108.736912	54.264321
3007.885883	98.932802	54.269325
3006.592709	106.639376	54.274330
3006.002262	106.549227	54.279335
3005.727942	108.479349	54.284340
3005.981952	106.474947	54.289345
3004.945175	104.459406	54.294349
3003.977201	108.115384	54.299354
3003.676953	101.301607	54.304359
3002.808509	107.873397	54.309364
3001.245234	107.713436	54.314369
3001.009438	96.387185	54.319373
3000.353706	106.010177	54.324378
3000.066989	98.893308	54.329383
2999.250564	104.338738	54.334388
2998.569654	103.109867	54.339393
2998.132710	101.684574	54.344397
2997.054249	102.320037	54.349402
2997.038944	99.340893	54.354407
2996.604176	105.044387	54.359412
2995.468602	104.792395	54.364417
2994.366698	98.800063	54.369421
2993.318469	112.927251	54.374426
2993.169766	102.027814	54.379431
2992.594549	105.462736	54.384436
2991.599520	109.335307	54.389441
2991.504725	98.820993	54.394445
2990.616026	102.947360	54.399450
2990.387688	99.879096	54.404455
2990.010799	107.459098	54.409460
2989.217078	101.525022	54.414465
2988.460461	105.317775	54.419469
2987.084488	106.464330	54.424474
2986.505817	99.039335	54.429479
2985.833139	103.476937	54.434484
2985.349240	98.182272	54.439489
2984.712835	95.531888	54.444493
2984.312407	103.788525	54.449498
2983.824911	93.528420	54.454503
2983.313058	103.244059	54.459508
2982.002974	102.950446	54.464513
2980.904341	103.186737	54.469517
2980.284602	113.892240	54.474522
2979.972591	106.559830	54.479527
2979.084202	102.317547	54.484532
2978.808957	97.403269	54.489537
2978.423047	105.985444	54.494541
2977.761255	109.111091	54.499546
2977.439675	109.606958	54.504551
2976.660799	109.747558	54.509556
2975.580499	110.416891	54.514561
2974.850381	110.606790	54.519565
2974.006468	118.785669	54.524570
2973.418205	108.533698	54.529575
2973.039987	112.965195	54.534580
2972.393634	111.448587	54.539585
2972.179400	96.322175	54.544589
2971.080032	112.408050	54.549594
2970.391210	111.591839	54.554599
2968.956397	114.982607	54.559604
2968.416588	107.040193	54.564609
2968.429310	103.762978	54.569613
2967.139608	116.205689	54.574618
2967.163551	111.719085	54.579623
2966.825581	111.678556	54.584628
2966.095641	110.181759	54.589633
2965.371071	107.391709	54.594637
2963.737584	111.663905	54.599642
2963.324018	101.796945	54.604647
2962.280652	109.291896	54.609652
2962.230632	112.030773	54.614657
2961.604156	102.101514	54.619661
2960.742616	112.166643	54.624666
2960.436564	109.201263	54.629671
2959.914100	108.386230	54.634676
2958.948315	112.152364	54.639681
2958.878024	112.071225	54.644685
2958.105374	116.726833	54.649690
2956.972622	107.163948	54.654695
2955.950578	111.868488	54.659700
2955.052317	97.190539	54.664705
2955.339870	101.728916	54.669709
2954.626864	107.848237	54.674714
2954.019283	98.304165	54.679719
2953.236245	108.310089	54.684724
2952.711736	108.994578	54.689729
2951.837565	105.535771	54.694733
2950.662828	109.503003	54.699738
2949.740970	102.779668	54.704743
2950.275872	108.890208	54.709748
2949.218339	111.746783	54.714753
2949.079453	109.631103	54.719757
2947.962171	106.170421	54.724762
2947.588642	104.711008	54.729767
2946.280579	109.691788	54.734772
2945.032497	103.403138	54.739777
2945.106146	93.922652	54.744781
2944.267885	103.008825	54.749786
2943.593835	111.043020	54.754791
2943.066538	104.107790	54.759796
2942.352827	108.595434	54.764801
2942.080240	99.896462	54.769805
2941.784887	105.181012	54.774810
2941.033117	105.159489	54.779815
2940.212010	106.023344	54.784820
2938.652689	112.018880	54.789825
2938.640196	108.529663	54.794829
2937.749054	104.347462	54.799834
2937.470585	107.010907	54.804839
2936.931631	108.322323	54.809844
2936.606027	110.132529	54.814849
2935.421427	97.440047	54.819853
2934.250847	113.813217	54.824858
2933.971763	99.673261	54.829863
2933.226585	98.826030	54.834868
2932.857359	100.492905	54.839873
2932.256924	100.244606	54.844877
2931.311763	100.312579	54.849882
2930.373791	105.446425	54.854887
2929.866361	102.644142	54.859892
2928.810101	103.738048	54.864897
2928.404163	92.841534	54.869901
2927.646141	102.045833	54.874906
2927.009444	100.610079	54.879911
2926.710592	99.999989	54.884916
2926.471025	106.896541	54.889921
2925.640521	103.860134	54.894925
2925.031561	110.865601	54.899930
2924.618676	99.765408	54.904935
2923.295411	97.085572	54.909940
2922.642641	94.958243	54.914945
2922.053366	93.309918	54.919949
2921.347980	112.642981	54.924954
2920.714365	101.848922	54.929959
2920.229188	97.757215	54.934964
2919.814379	113.351116	54.939969
2918.781825	100.254506	54.944973
2917.870344	109.286092	54.949978
2917.355863	103.707326	54.954983
2916.746559	100.530886	54.959988
2916.006689	100.689696	54.964993
2915.439477	94.451673	54.969997
2915.029962	105.456367	54.975002
2914.716632	93.607343	54.980007
2913.328652	95.497656	54.985012
2912.231806	100.768387	54.990017
2912.041152	102.588689	54.995021
2911.267538	101.659480	55.000026
2911.049009	97.702991	55.005031
2910.571351	98.042775	55.010036
2909.917636	101.480458	55.015041
2909.539197	93.086155	55.020045
2908.241539	99.120657	55.025050
2907.253677	94.568557	55.030055
2907.026178	102.746299	55.035060
2906.232171	103.613028	55.040065
2906.252204	93.812507	55.045069
2904.496391	106.776174	55.050074
2903.832016	102.147870	55.055079
2903.586737	101.303632	55.060084
2902.446506	105.176555	55.065089
2902.523812	101.850806	55.070093
2901.634074	107.343903	55.075098
2901.320050	99.509364	55.080103
2900.887832	101.341343	55.085108
2899.536234	101.634696	55.090113
2899.105699	95.389502	55.095117
2898.072608	104.917119	55.100122
2897.425015	99.793725	55.105127
2897.194693	99.897037	55.110132
2896.565802	105.986987	55.115137
2896.055770	98.960399	55.120141
2894.999186	106.842077	55.125146
2894.020197	106.685317	55.130151
2893.465862	100.072868	55.135156
2892.825189	110.687211	55.140161
2892.672871	103.597516	55.145165
2891.999696	106.015791	55.150170
2891.555575	95.481456	55.155175
2890.507282	96.532561	55.160180
2889.209957	103.555405	55.165185
2889.150612	101.573369	55.170189
2888.415755	107.964053	55.175194
2887.896232	100.217528	55.180199
2887.449758	108.396773	55.185204
2886.579926	107.916631	55.190209
2885.831735	98.563177	55.195213
2884.660438	101.981555	55.200218
2883.289625	98.849605	55.205223
2883.585009	100.800391	55.210228
2883.526532	99.132014	55.215233
2882.950459	97.023950	55.220237
2882.243417	103.616321	55.225242
2881.645968	97.776617	55.230247
2880.637751	103.275753	55.235252
2879.649690	96.632433	55.240257
2879.311809	93.267908	55.245261
2878.601814	96.053650	55.250266
2878.152629	105.281354	55.255271
2877.422470	93.877379	55.260276
2876.186859	93.116733	55.265281
2875.941688	95.251869	55.270285
2875.101033	102.225880	55.275290
2874.686256	94.804081	55.280295
2874.195722	97.051016	55.285300
2873.358043	100.828028	55.290305
2872.318984	93.729624	55.295309
2871.912278	94.266095	55.300314
2870.824595	88.769512	55.305319
2870.604349	90.412902	55.310324
2870.171690	95.292240	55.315329
2869.944137	93.201193	55.320333
2868.535426	98.018794	55.325338
2868.006152	88.854115	55.330343
2867.310590	89.196801	55.335348
2866.102186	90.754470	55.340353
2865.938803	88.258521	55.345357
2865.277797	101.503232	55.350362
2865.105617	91.183344	55.355367
2864.168202	93.021534	55.360372
2863.221407	94.760277	55.365377
2862.546059	89.559927	55.370381
2861.819282	91.017523	55.375386
2861.146629	93.293214	55.380391
2861.089091	89.237377	55.385396
2860.010296	94.607657	55.390401
2859.471187	89.479944	55.395405
2858.776232	97.409157	55.400410
2857.860300	91.637309	55.405415
2857.132345	93.930742	55.410420
2856.364249	98.149008	55.415425
2855.873366	95.948627	55.420429
2855.485026	101.087623	55.425434
2855.186409	95.893150	55.430439
2854.746082	94.219378	55.435444
2852.990705	101.685630	55.440449
2852.723705	88.617290	55.445453
2851.800996	98.036834	55.450458
2851.018912	96.146346	55.455463
2850.956255	89.437642	55.460468
2850.451012	95.999866	55.465473
2850.248053	85.152759	55.470477
2848.857627	93.392272	55.475482
2848.637255	100.632896	55.480487
2848.071494	98.186768	55.485492
2846.627532	112.071336	55.490497
2845.881613	93.975507	55.495501
2844.829446	100.778437	55.500506
2844.213574	93.415089	55.505511
2844.675386	94.152067	55.510516
2843.653674	101.676482	55.515521
2843.135093	99.354129	55.520525
2842.734912	96.766022	55.525530
2842.058944	93.913610	55.530535
2841.133376	96.352920	55.535540
2839.456114	95.139619	55.540545
2839.028980	97.284145	55.545549
2838.605589	96.360221	55.550554
2837.696670	104.021673	55.555559
2837.535073	94.462589	55.560564
2837.159172	97.729643	55.565569
2836.697419	86.770060	55.570573
2835.946138	100.284007	55.575578
2834.895809	101.940978	55.580583
2834.499471	100.552181	55.585588
2833.806212	98.562833	55.590593
2833.240791	91.762429	55.595597
2832.305366	94.883141	55.600602
2831.274273	95.893422	55.605607
2830.946093	98.455629	55.610612
2830.021750	97.978892	55.615617
2829.688525	97.939534	55.620621
2829.172960	94.844190	55.625626
2828.870135	97.226016	55.630631
2828.124162	100.626974	55.635636
2826.458000	107.002754	55.640641
2826.697346	94.168789	55.645645
2825.823674	95.685835	55.650650
2824.771783	91.982700	55.655655
2824.951641	99.000188	55.660660
2823.718651	99.975900	55.665665
2822.727371	88.397497	55.670669
2822.051172	95.922859	55.675674
2821.329906	99.995760	55.680679
2821.033632	100.765591	55.685684
2820.312241	111.539779	55.690689
2820.089549	100.219210	55.695693
2820.067217	97.661656	55.700698
2818.687612	99.425826	55.705703
2818.003913	99.791358	55.710708
2817.003571	104.264842	55.715713
2816.523444	96.817906	55.720717
2815.340224	98.269046	55.725722
2814.746017	102.143001	55.730727
2814.181329	92.363085	55.735732
2813.909649	97.204650	55.740737
2812.937341	93.557387	55.745741
2812.437099	95.292447	55.750746
2812.478073	94.257189	55.755751
2811.940008	90.185984	55.760756
2810.615441	101.692051	55.765761
2810.270495	98.313739	55.770765
2809.650792	103.915425	55.775770
2808.369492	103.407727	55.780775
2807.600399	98.361955	55.785780
2806.929424	97.563242	55.790785
2806.600942	92.511638	55.795789
2806.007500	94.941161	55.800794
2805.125976	98.246475	55.805799
2805.010059	92.391590	55.810804
2804.150499	98.373733	55.815809
2803.078492	91.655968	55.820813
2802.625934	98.933116	55.825818
2801.840702	94.138782	55.830823
2801.719270	90.299520	55.835828
2800.886594	93.470963	55.840833
2799.694766	94.768845	55.845837
2799.163027	97.594389	55.850842
2798.202000	82.821445	55.855847
2797.878022	90.812776	55.860852
2797.401261	93.463533	55.865857
2797.217876	88.666994	55.870861
2796.282651	104.919409	55.875866
2795.031644	103.538140	55.880871
2794.380565	93.967198	55.885876
2793.553871	95.277672	55.890881
2793.167938	95.167591	55.895885
2792.669828	95.862975	55.900890
2792.373481	99.574316	55.905895
2792.227398	89.501419	55.910900
2791.017571	105.301835	55.915905
2790.098760	89.411308	55.920909
2789.464534	96.456617	55.925914
2788.887882	98.085136	55.930919
2788.258721	88.029677	55.935924
2787.108764	100.333641	55.940929
2786.591973	92.436280	55.945933
2785.836920	98.290434	55.950938
2785.243725	94.424044	55.955943
2785.086556	90.584180	55.960948
2784.496818	95.633259	55.965953
2783.653580	89.871109	55.970957
2782.928722	91.954420	55.975962
2782.208400	100.832157	55.980967
2781.396267	95.935058	55.985972
2780.640179	102.900938	55.990977
2780.266526	93.655993	55.995981
2779.252871	104.928931	56.000986
2778.120380	92.152209	56.005991
2777.794255	92.384791	56.010996
2777.335070	93.525484	56.016001
2776.995318	100.584016	56.021005
2776.583603	96.810946	56.026010
2775.700377	97.204270	56.031015
2775.461991	96.893714	56.036020
2774.318897	93.871685	56.041025
2773.193737	96.701949	56.046029
2772.544842	92.390357	56.051034
2772.032062	96.852352	56.056039
2772.058868	90.436645	56.061044
2771.331867	97.459129	56.066049
2770.096560	91.559919	56.071053
2769.510367	91.629721	56.076058
2768.812978	96.410234	56.081063
2769.094932	89.660401	56.086068
2767.790899	97.326230	56.091073
2766.666498	92.720922	56.096077
2766.243544	91.048926	56.101082
2765.348644	93.262352	56.106087
2765.515430	93.817649	56.111092
2764.352550	99.070476	56.116097
2763.857140	93.998068	56.121101
2762.376804	100.017239	56.126106
2761.467042	99.406183	56.131111
2761.939968	95.532044	56.136116
2761.168437	100.150763	56.141121
2760.337633	90.337793	56.146125
2760.015380	95.645882	56.151130
2759.522669	95.281693	56.156135
2758.725770	89.401499	56.161140
2757.446901	99.212704	56.166145
2756.974996	94.817575	56.171149
2756.650178	93.937204	56.176154
2755.810832	100.348515	56.181159
2754.673148	91.580732	56.186164
2753.600719	102.502148	56.191169
2753.413070	97.074383	56.196173
2752.963369	97.105462	56.201178
2752.343473	100.670794	56.206183
2752.510426	93.150770	56.211188
2751.882072	104.818104	56.216193
2750.624780	100.543397	56.221197
2750.246602	92.225257	56.226202
2749.283818	93.329268	56.231207
2748.605646	92.355745	56.236212
2747.263846	108.341350	56.241217
2746.717053	96.139902	56.246221
2746.483839	103.658238	56.251226
2745.827780	92.935953	56.256231
2745.824455	93.303621	56.261236
2744.929319	90.813149	56.266241
2744.071605	90.332538	56.271245
2743.084169	88.669792	56.276250
2742.429880	91.382474	56.281255
2742.187748	95.345461	56.286260
2741.439150	101.922442	56.291265
2740.491980	91.631616	56.296269
2739.910888	91.586868	56.301274
2739.307391	96.549488	56.306279
2738.764626	81.368373	56.311284
2738.047350	95.144125	56.316289
2736.600786	87.689503	56.321293
2736.071510	92.896401	56.326298
2735.560218	90.858597	56.331303
2735.092862	84.692354	56.336308
2734.243854	95.802545	56.341313
2734.072042	87.220987	56.346317
2733.472499	89.796026	56.351322
2733.146875	99.790081	56.356327
2732.591365	96.954200	56.361332
2731.369124	100.247499	56.366337
2731.015757	94.882798	56.371341
2730.933713	98.912367	56.376346
2729.224263	105.299120	56.381351
2728.581353	93.930399	56.386356
2728.111584	103.316350	56.391361
2727.488988	94.832364	56.396365
2726.392492	97.241301	56.401370
2725.377626	99.552210	56.406375
2725.179851	84.631856	56.411380
2724.139782	94.570792	56.416385
2724.000222	99.572532	56.421389
2723.601387	94.829007	56.426394
2722.907162	96.363947	56.431399
2722.633600	93.677238	56.436404
2721.485381	99.702412	56.441409
2720.750787	88.596072	56.446413
2720.212937	90.275199	56.451418
2719.419748	95.926670	56.456423
2719.311720	92.994569	56.461428
2717.970276	98.988430	56.466433
2716.783266	90.988146	56.471437
2716.542616	94.543129	56.476442
2716.046848	96.700576	56.481447
2715.700111	92.876935	56.486452
2714.655046	95.990352	56.491457
2714.227182	90.711017	56.496461
2713.601148	85.877255	56.501466
2712.537643	90.772059	56.506471
2712.399746	89.201734	56.511476
2711.705923	98.154677	56.516481
2711.442221	102.502262	56.521485
2710.393211	96.182814	56.526490
2709.106142	91.256388	56.531495
2709.007679	83.432406	56.536500
2708.201646	91.868883	56.541505
2707.642950	98.845235	56.546509
2706.511923	91.475235	56.551514
2705.588161	101.741261	56.556519
2704.967083	91.554176	56.561524
2704.598612	94.353398	56.566529
2704.658856	91.237408	56.571533
2704.098824	91.313403	56.576538
2703.440902	91.436523	56.581543
2702.364542	88.578363	56.586548
2701.442870	109.037813	56.591553
2700.652735	100.424576	56.596557
2700.399922	87.483311	56.601562
2699.982380	96.687836	56.606567
2698.804888	96.057028	56.611572
2697.492700	96.953937	56.616577
2697.218459	94.214058	56.621581
2697.297055	93.365391	56.626586
2696.482383	94.154365	56.631591
2696.206193	89.979205	56.636596
2695.544403	86.899795	56.641601
2694.523678	89.876030	56.646605
2693.934354	90.320969	56.651610
2692.762218	91.872472	56.656615
2692.346150	84.399613	56.661620
2691.680372	91.607811	56.666625
2690.517698	89.897663	56.671629
2689.973486	88.011540	56.676634
2689.002342	89.553555	56.681639
2688.919360	86.250871	56.686644
2688.431192	91.305485	56.691649
2687.938127	94.190739	56.696653
2688.067197	88.065839	56.701658
2687.050535	95.838475	56.706663
2686.263177	86.193753	56.711668
2685.292445	88.115423	56.716673
2684.100337	87.981314	56.721677
2683.449127	86.002563	56.726682
2682.492605	93.886494	56.731687
2682.243027	88.598794	56.736692
2681.906551	89.476552	56.741697
2681.144204	95.939441	56.746701
2680.928196	84.007124	56.751706
2679.973721	86.857962	56.756711
2679.002692	87.651166	56.761716
2678.326572	81.175233	56.766721
2677.983435	86.303736	56.771725
2677.712702	80.079421	56.776730
2676.373511	89.430823	56.781735
2675.461997	79.403922	56.786740
2674.913411	92.985840	56.791745
2674.473616	86.085838	56.796749
2673.882817	80.566345	56.801754
2673.296745	89.995061	56.806759
2673.096433	80.139082	56.811764
2671.669358	83.065177	56.816769
2671.257316	83.215349	56.821773
2670.903723	84.861799	56.826778
2670.096261	86.923321	56.831783
2669.462751	79.978674	56.836788
2668.194262	81.773222	56.841793
2667.736931	86.185479	56.846797
2667.281433	82.945683	56.851802
2666.840777	93.954495	56.856807
2666.084542	90.595188	56.861812
2664.889318	93.409816	56.866817
2664.094601	88.063727	56.871821
2663.664057	85.550696	56.876826
2663.113909	88.058483	56.881831
2663.118073	86.671503	56.886836
2662.535960	89.336723	56.891841
2661.620439	91.982359	56.896845
2660.824200	86.036550	56.901850
2660.000706	91.970696	56.906855
2659.674703	83.704050	56.911860
2658.123194	86.441030	56.916865
2657.483558	86.726420	56.921869
2657.017793	79.249038	56.926874
2656.292703	92.798760	56.931879
2656.023232	83.570374	56.936884
2655.662006	90.647570	56.941889
2655.345067	88.000649	56.946893
2655.050734	84.260031	56.951898
2653.117470	81.961242	56.956903
2652.793653	77.063991	56.961908
2652.161416	83.069254	56.966913
2651.274415	90.198825	56.971917
2650.171168	76.342325	56.976922
2649.443573	82.024030	56.981927
2649.445680	83.265084	56.986932
2648.995809	86.354923	56.991937
2648.235547	83.514977	56.996941
2647.752806	78.550948	57.001946
2646.939809	85.566817	57.006951
2645.987303	82.273434	57.011956
2645.318915	87.338329	57.016961
2644.849156	84.169261	57.021965
2644.491099	74.123156	57.026970
2643.602705	84.717065	57.031975
2642.845965	84.048293	57.036980
2641.879084	89.075401	57.041985
2641.097939	94.188783	57.046989
2641.702202	79.410816	57.051994
2640.782830	92.100880	57.056999
2639.724577	87.038654	57.062004
2638.691166	90.502184	57.067009
2638.132298	90.239706	57.072013
2637.853437	80.974247	57.077018
2636.559838	80.333302	57.082023
2635.571805	79.426972	57.087028
2635.084691	87.636835	57.092033
2634.428293	92.305748	57.097037
2634.283751	86.262752	57.102042
2633.557520	85.252856	57.107047
2633.545815	84.668301	57.112052
2633.252709	85.782983	57.117057
2631.798310	88.295745	57.122061
2631.275365	83.365825	57.127066
2630.325517	91.925571	57.132071
2629.179970	81.236077	57.137076
2628.620714	84.203303	57.142081
2627.563768	86.360765	57.147085
2627.446720	81.084365	57.152090
2627.193834	90.180608	57.157095
2627.263944	81.995855	57.162100
2626.314087	86.047846	57.167105
2624.861734	88.628548	57.172109
2624.488774	80.581113	57.177114
2623.468468	91.287574	57.182119
2623.087216	83.620096	57.187124
2621.870401	80.382951	57.192129
2620.963679	89.811613	57.197133
2620.828286	81.622913	57.202138
2620.318874	90.846294	57.207143
2620.181626	85.143885	57.212148
2619.761866	82.202318	57.217153
2618.460303	85.847474	57.222157
2618.234975	80.345644	57.227162
2616.959560	86.964526	57.232167
2616.843380	81.031946	57.237172
2615.270547	80.033358	57.242177
2614.237761	87.297585	57.247181
2614.492108	77.354816	57.252186
2613.688853	85.420173	57.257191
2613.327826	80.288504	57.262196
2612.806875	92.561921	57.267201
2612.072180	81.912327	57.272205
2611.123260	78.970037	57.277210
2610.351361	90.411641	57.282215
2609.705206	82.449197	57.287220
2609.262583	88.672306	57.292225
2608.878676	90.432097	57.297229
2607.879179	81.434300	57.302234
2606.757528	89.176731	57.307239
2606.533726	84.795264	57.312244
2605.803311	92.559235	57.317249
2605.593922	88.440953	57.322253
2604.806567	79.296765	57.327258
2603.758753	89.751752	57.332263
2603.010320	78.681761	57.337268
2602.731940	82.254638	57.342273
2602.143178	80.318117	57.347277
2601.051237	85.832776	57.352282
2599.864252	90.256877	57.357287
2599.363156	85.500062	57.362292
2599.288035	80.907659	57.367297
2598.625784	83.741709	57.372301
2598.387811	74.846626	57.377306
2597.749874	83.741853	57.382311
2596.727937	82.507390	57.387316
2595.898845	89.372074	57.392321
2595.002850	87.768328	57.397325
2594.823537	74.495987	57.402330
2594.079619	86.860407	57.407335
2592.983122	80.986073	57.412340
2592.593630	82.645374	57.417345
2591.790013	79.697591	57.422349
2591.434677	84.691210	57.427354
2590.627735	83.538807	57.432359
2590.288505	84.606113	57.437364
2589.450448	83.972171	57.442369
2588.236556	89.950956	57.447373
2588.124062	83.984985	57.452378
2587.484453	89.290088	57.457383
2587.337612	86.297922	57.462388
2586.459612	82.347229	57.467393
2585.509286	84.488839	57.472397
2584.999544	81.028597	57.477402
2583.829528	81.824650	57.482407
2582.779108	83.563780	57.487412
2582.467663	84.959089	57.492417
2581.461649	90.105785	57.497421
2581.212428	86.750606	57.502426
2580.946650	90.122389	57.507431
2580.675231	81.731165	57.512436
2580.104684	88.855983	57.517441
2578.719363	84.469403	57.522445
2578.427403	81.697040	57.527450
2577.261868	82.100761	57.532455
2576.931571	82.178546	57.537460
2576.039812	82.251264	57.542465
2575.055001	82.942239	57.547469
2574.820006	72.342627	57.552474
2574.318942	87.944504	57.557479
2573.958793	83.057418	57.562484
2572.856771	83.127399	57.567489
2571.711645	88.563921	57.572493
2571.386350	85.464109	57.577498
2570.830654	86.050543	57.582503
2570.301768	87.122247	57.587508
2569.932174	84.695119	57.592513
2568.685911	91.978874	57.597517
2567.811084	87.736335	57.602522
2567.394205	85.965033	57.607527
2567.122030	90.770759	57.612532
2566.917167	87.658648	57.617537
2565.381515	88.774967	57.622541
2565.078084	80.508029	57.627546
2564.028367	80.198029	57.632551
2563.996654	82.479041	57.637556
2562.799785	75.741641	57.642561
2561.701417	83.530225	57.647565
2561.392648	77.836226	57.652570
2560.787894	76.439269	57.657575
2560.364539	80.766775	57.662580
2560.169411	86.469957	57.667585
2559.308981	91.827813	57.672589
2558.476223	75.732805	57.677594
2557.487593	82.832782	57.682599
2557.081824	85.543650	57.687604
2556.923665	91.123280	57.692609
2555.311228	87.836157	57.697613
2554.883656	88.659628	57.702618
2553.688955	94.967892	57.707623
2553.375439	92.586834	57.712628
2553.499337	91.241752	57.717633
2552.891455	91.536330	57.722637
2551.970914	89.572852	57.727642
2550.942421	84.342540	57.732647
2550.554247	84.620083	57.737652
2550.120126	83.036857	57.742657
2548.701978	87.125101	57.747661
2548.102126	75.925518	57.752666
2547.639558	88.373283	57.757671
2547.206492	86.339102	57.762676
2546.622649	82.730090	57.767681
2545.654988	93.888595	57.772685
2544.925711	76.230159	57.777690
2543.798095	82.352877	57.782695
2543.193311	77.511960	57.787700
2542.879723	87.610911	57.792705
2542.321693	87.634475	57.797709
2541.959576	78.996666	57.802714
2541.675911	80.798530	57.807719
2540.931148	82.890795	57.812724
2540.095128	78.520448	57.817729
2538.901271	88.886332	57.822733
2539.290344	82.429631	57.827738
2537.828848	86.366214	57.832743
2536.827307	85.572340	57.837748
2536.320502	90.526333	57.842753
2535.577996	83.059176	57.847757
2535.586744	79.433724	57.852762
2534.282980	88.405679	57.857767
2533.290117	81.638935	57.862772
2532.847338	80.724669	57.867777
2532.185772	94.559179	57.872781
2531.781078	79.638323	57.877786
2531.633897	87.947171	57.882791
2531.411642	87.364271	57.887796
2530.308787	78.505348	57.892801
2529.228410	83.029255	57.897805
2528.878726	80.767670	57.902810
2528.155374	81.844598	57.907815
2526.828829	78.791232	57.912820
2526.279994	80.383438	57.917825
2525.758846	82.260244	57.922829
2525.407466	71.370285	57.927834
2524.910454	78.587920	57.932839
2524.189068	75.082951	57.937844
2523.384335	71.983403	57.942849
2522.415570	83.041041	57.947853
2522.153161	77.043078	57.952858
2521.569836	82.510661	57.957863
2520.671136	78.705622	57.962868
2519.881845	74.483997	57.967873
2519.069414	78.040021	57.972877
2518.887395	73.365641	57.977882
2517.954558	77.283686	57.982887
2517.599265	78.030857	57.987892
2517.034320	82.794663	57.992897
2516.321307	82.727888	57.997901
2515.893367	72.383106	58.002906
2514.610024	82.287065	58.007911
2513.694444	78.607672	58.012916
2513.175323	77.951189	58.017921
2512.637794	74.652018	58.022925
2511.913485	83.767270	58.027930
2511.539227	86.953526	58.032935
2510.873370	83.360514	58.037940
2509.890583	77.913196	58.042945
2509.142845	86.811410	58.047949
2508.721296	74.602832	58.052954
2508.119047	79.082103	58.057959
2507.776258	81.536687	58.062964
2507.159084	77.288007	58.067969
2505.743987	79.991440	58.072973
2505.400310	81.362264	58.077978
2505.142081	81.411548	58.082983
2504.217214	87.972491	58.087988
2503.358850	75.309269	58.092993
2502.343211	89.812971	58.097997
2501.961921	74.122756	58.103002
2501.379527	86.066811	58.108007
2500.810752	77.214875	58.113012
2500.299459	77.743594	58.118017
2500.023004	83.979740	58.123021
2499.053445	71.404214	58.128026
2497.973557	83.897121	58.133031
2497.637349	79.818294	58.138036
2497.122072	82.985635	58.143041
2495.901681	89.291587	58.148045
2495.454827	84.775374	58.153050
2494.808415	80.550245	58.158055
2494.318702	80.560951	58.163060
2493.974999	81.676788	58.168065
2492.806276	86.383168	58.173069
2492.038552	87.659917	58.178074
2491.611504	85.791286	58.183079
2490.693303	84.948831	58.188084
2490.786516	82.776918	58.193089
2489.694143	87.621820	58.198093
2488.986822	93.536909	58.203098
2487.982258	84.715267	58.208103
2487.981789	84.660091	58.213108
2487.569938	82.188882	58.218113
2486.296685	87.320095	58.223117
2485.331365	73.950452	58.228122
2484.716061	81.592510	58.233127
2484.229489	87.114604	58.238132
2484.348133	78.073700	58.243137
2483.316361	81.769068	58.248141
2482.362066	69.254885	58.253146
2481.851426	76.987595	58.258151
2481.057215	80.624980	58.263156
2480.258245	81.245910	58.268161
2478.820588	80.755943	58.273165
2478.504955	77.059246	58.278170
2478.511518	78.203223	58.283175
2478.119231	82.009516	58.288180
2477.402331	77.332247	58.293185
2476.511104	89.960267	58.298189
2475.821296	74.934627	58.303194
2474.817614	81.769563	58.308199
2474.273556	84.954852	58.313204
2473.671180	75.984723	58.318209
2473.367197	83.390404	58.323213
2472.715339	76.000132	58.328218
2471.575479	83.285047	58.333223
2470.974046	79.395248	58.338228
2470.167034	70.018414	58.343233
2469.732420	81.797861	58.348237
2469.997367	73.699810	58.353242
2468.475699	70.872052	58.358247
2467.454371	78.845229	58.363252
2467.163218	69.911498	58.368257
2466.835800	85.235789	58.373261
2466.254873	73.680502	58.378266
2465.082828	74.744154	58.383271
2464.068208	79.887201	58.388276
2463.734548	72.525026	58.393281
2463.219738	80.641728	58.398285
2462.830982	69.890799	58.403290
2461.862521	74.935166	58.408295
2460.682697	71.263070	58.413300
2461.045608	77.740808	58.418305
2459.939991	84.882902	58.423309
2459.606399	65.576775	58.428314
2458.582592	78.188377	58.433319
2457.424454	83.256098	58.438324
2457.184728	84.756384	58.443329
2456.559469	77.415643	58.448333
2456.297227	76.499333	58.453338
2455.290336	75.846911	58.458343
2454.363093	78.088801	58.463348
2453.683540	69.729092	58.468353
2453.109929	77.513621	58.473357
2452.604585	73.603055	58.478362
2452.334651	65.678561	58.483367
2451.496132	71.522526	58.488372
2450.975948	73.379830	58.493377
2449.860050	82.873077	58.498381
2449.745686	75.807740	58.503386
2448.973182	76.306126	58.508391
2447.586579	77.074897	58.513396
2447.257072	67.199207	58.518401
2446.848760	81.093030	58.523405
2446.376998	76.659240	58.528410
2445.239533	73.083324	58.533415
2444.167712	76.890540	58.538420
2443.871147	66.956325	58.543425
2442.993998	78.619595	58.548429
2442.659051	70.667533	58.553434
2442.346752	74.348047	58.558439
2442.160735	78.438799	58.563444
2441.353287	74.778433	58.568449
2440.472302	75.222739	58.573453
2439.508747	73.166774	58.578458
2438.276989	68.186372	58.583463
2437.425573	74.993696	58.588468
2437.340588	65.477241	58.593473
2436.646730	74.500443	58.598477
2436.503657	81.397443	58.603482
2435.859597	75.532241	58.608487
2434.417520	84.353389	58.613492
2433.910747	78.948644	58.618497
2433.244404	76.985938	58.623501
2433.203620	76.481749	58.628506
2432.901570	76.183278	58.633511
2431.420400	80.465472	58.638516
2430.516057	72.210910	58.643521
2429.375311	77.481705	58.648525
2429.349825	77.665272	58.653530
2428.796403	70.393571	58.658535
2428.542722	82.051689	58.663540
2428.027568	80.115631	58.668545
2426.682479	87.697345	58.673549
2426.240770	72.058927	58.678554
2425.912683	77.459189	58.683559
2424.887388	83.503642	58.688564
2424.019243	71.588936	58.693569
2423.295055	77.774529	58.698573
2422.618337	79.735966	58.703578
2422.231060	74.175009	58.708583
2421.605829	74.594536	58.713588
2421.767912	69.651338	58.718593
2420.121063	79.955737	58.723597
2419.595159	71.128464	58.728602
2419.110413	72.181975	58.733607
2418.426323	75.108586	58.738612
2417.726915	72.514058	58.743617
2416.541969	78.474495	58.748621
2416.174625	79.093869	58.753626
2415.473612	78.617700	58.758631
2415.251618	84.499149	58.763636
2414.885853	70.231652	58.768641
2413.382261	78.987531	58.773645
2412.865962	77.548628	58.778650
2412.422417	74.157220	58.783655
2411.684109	79.724329	58.788660
2411.955181	73.916998	58.793665
2410.443783	79.437086	58.798669
2409.999512	75.693709	58.803674
2409.208217	72.112295	58.808679
2408.230881	76.402292	58.813684
2407.499450	76.932344	58.818689
2406.984490	76.411340	58.823693
2406.877377	73.659096	58.828698
2406.123579	79.027939	58.833703
2404.893239	79.365806	58.838708
2404.095444	73.816229	58.843713
2403.605858	68.465000	58.848717
2403.199087	79.188138	58.853722
2402.602216	72.118863	58.858727
2401.632405	79.018669	58.863732
2400.979736	75.175535	58.868737
2399.973685	82.941247	58.873741
2399.716589	81.001331	58.878746
2399.441329	80.286190	58.883751
2398.664064	79.375445	58.888756
2397.679371	69.733362	58.893761
2396.719201	73.911481	58.898765
2396.426657	72.608790	58.903770
2396.082484	74.050753	58.908775
2395.514007	78.697145	58.913780
2394.904903	65.202686	58.918785
2393.689872	75.242602	58.923789
2392.829466	74.217789	58.928794
2392.828654	76.142604	58.933799
2391.808853	88.412096	58.938804
2391.315506	77.120524	58.943809
2390.215365	80.790491	58.948813
2389.552585	74.147342	58.953818
2389.420921	82.638255	58.958823
2388.438244	78.129994	58.963828
2388.552153	74.554460	58.968833
2387.277633	77.889124	58.973837
2386.489992	85.469867	58.978842
2385.992767	69.363339	58.983847
2385.158138	74.781134	58.988852
2385.097687	74.551484	58.993857
2383.876460	74.594517	58.998861
2383.228551	78.400705	59.003866
2382.722178	72.110143	59.008871
2382.056741	74.886732	59.013876
2381.465291	67.657857	59.018881
2380.281007	72.790450	59.023885
2379.844064	79.149556	59.028890
2379.582965	66.271757	59.033895
2378.802421	78.080742	59.038900
2377.895059	65.850665	59.043905
2376.828374	72.994395	59.048909
2376.483086	67.739283	59.053914
2376.158492	66.189451	59.058919
2375.262231	73.353382	59.063924
2375.528666	72.221157	59.068929
2374.220949	74.859287	59.073933
2373.127337	72.355458	59.078938
2372.787509	70.036941	59.083943
2372.195982	75.790131	59.088948
2371.796953	66.767497	59.093953
2370.918527	62.033006	59.098957
2370.231534	66.858339	59.103962
2369.620810	68.113388	59.108967
2368.182862	85.385653	59.113972
2367.720524	68.590688	59.118977
2366.988101	71.828715	59.123981
2366.338114	76.111295	59.128986
2366.420394	69.478514	59.133991
2365.683079	75.918583	59.138996
2365.386164	65.566825	59.144001
2364.529701	75.476356	59.149005
2363.355852	73.718066	59.154010
2362.988143	68.067329	59.159015
2361.835505	72.486775	59.164020
2360.940934	71.997133	59.169025
2360.154428	72.178989	59.174029
2360.420505	70.421979	59.179034
2360.067778	68.207508	59.184039
2359.492852	77.268797	59.189044
2358.721386	69.276919	59.194049
2357.243386	68.484816	59.199053
2356.691504	70.231103	59.204058
2356.395396	71.823923	59.209063
2355.642371	68.367814	59.214068
2354.549299	59.364786	59.219073
2353.961948	66.503131	59.224077
2353.515980	62.445855	59.229082
2353.624086	65.523186	59.234087
2352.560778	66.129729	59.239092
2351.374097	63.478405	59.244097
2350.781102	69.446179	59.249101
2350.087118	69.231309	59.254106
2349.983217	65.880515	59.259111
2348.993307	75.234991	59.264116
2348.247279	68.687399	59.269121
2347.538577	59.141430	59.274125
2346.738555	63.658471	59.279130
2346.532292	68.218059	59.284135
2345.527076	71.741541	59.289140
2344.873879	70.611045	59.294145
2343.843667	72.425309	59.299149
2343.281967	67.847446	59.304154
2342.950414	65.080692	59.309159
2342.228059	74.467573	59.314164
2341.928886	64.023052	59.319169
2341.400844	69.309875	59.324173
2340.649304	68.399478	59.329178
2339.849536	63.324712	59.334183
2338.956456	69.007890	59.339188
2338.646236	72.712523	59.344193
2337.262174	71.485956	59.349197
2336.602809	71.631470	59.354202
2336.547561	67.759612	59.359207
2335.676933	67.194830	59.364212
2335.625870	63.149369	59.369217
2334.219959	75.101995	59.374221
2333.054888	62.761269	59.379226
2333.269529	63.263763	59.384231
2332.620174	63.677557	59.389236
2332.418366	64.754533	59.394241
2331.544274	63.463660	59.399245
2330.414583	68.288119	59.404250
2329.564458	62.827244	59.409255
2329.441249	70.412786	59.414260
2328.464197	65.798584	59.419265
2327.446992	67.185905	59.424269
2326.709899	65.240050	59.429274
2326.274570	62.196185	59.434279
2325.803020	69.250785	59.439284
2325.380972	56.798407	59.444289
2324.715966	67.335567	59.449293
2323.814787	68.197409	59.454298
2323.216873	66.655240	59.459303
2322.568838	69.502276	59.464308
2322.211433	61.987087	59.469313
2321.313524	67.971476	59.474317
2320.049205	62.852998	59.479322
2319.559179	65.311842	59.484327
2318.910200	66.524492	59.489332
2318.667057	60.320377	59.494337
2318.002049	65.055510	59.499341
2317.716295	59.974168	59.504346
2316.763591	65.289398	59.509351
2315.844257	75.379808	59.514356
2315.295852	68.469231	59.519361
2314.797351	73.726927	59.524365
2313.670047	71.514653	59.529370
2313.141629	62.885985	59.534375
2312.644807	69.177961	59.539380
2312.249549	59.823524	59.544385
2311.585320	69.902675	59.549389
2310.088967	71.833364	59.554394
2309.654447	65.836440	59.559399
2309.198657	68.544423	59.564404
2308.580634	65.577982	59.569409
2308.170054	68.418755	59.574413
2307.964551	62.153337	59.579418
2306.732712	60.037886	59.584423
2306.189396	67.358959	59.589428
2305.922195	67.941478	59.594433
2304.732748	71.703699	59.599437
2303.774470	69.826063	59.604442
2303.308896	72.937942	59.609447
2302.763607	72.231483	59.614452
2302.132566	64.036009	59.619457
2301.460859	71.219176	59.624461
2300.676540	75.433945	59.629466
2300.528901	67.010155	59.634471
2299.745476	72.309468	59.639476
2298.589705	65.179478	59.644481
2297.818057	65.950097	59.649485
2297.262486	73.220376	59.654490
2296.886178	69.272767	59.659495
2295.874342	72.513978	59.664500
2295.659440	62.501881	59.669505
2294.755418	69.661619	59.674509
2293.992789	74.150169	59.679514
2293.655828	60.401580	59.684519
2293.223581	71.299190	59.689524
2291.914913	63.248408	59.694529
2291.286685	72.584063	59.699533
2290.219471	64.221213	59.704538
2290.349314	66.268940	59.709543
2289.424582	65.909990	59.714548
2289.382675	67.154617	59.719553
2287.840126	71.530228	59.724557
2287.117769	63.873775	59.729562
2286.841570	62.716712	59.734567
2285.928889	63.106465	59.739572
2285.712525	57.111320	59.744577
2285.429269	57.404491	59.749581
2284.108097	65.623157	59.754586
2283.639147	67.595654	59.759591
2282.895939	71.439065	59.764596
2282.784198	69.317597	59.769601
2281.475297	71.625960	59.774605
2280.789209	72.805488	59.779610
2280.156350	56.606146	59.784615
2279.508871	72.456830	59.789620
2279.295354	58.266756	59.794625
2278.432704	64.016180	59.799629
2277.356210	66.903330	59.804634
2277.151311	60.586500	59.809639
2276.450247	66.798932	59.814644
2276.008446	65.300728	59.819649
2275.169188	71.318908	59.824653
2274.147324	72.731508	59.829658
2273.674373	53.875973	59.834663
2273.284855	64.337602	59.839668
2272.362177	64.397894	59.844673
2271.539166	66.910526	59.849677
2271.025003	73.522827	59.854682
2270.383404	64.289070	59.859687
2269.600475	72.106236	59.864692
2268.722954	68.821821	59.869697
2267.865322	64.606803	59.874701
2267.306544	62.755591	59.879706
2267.330614	58.936094	59.884711
2266.639566	67.058849	59.889716
2266.188158	62.307408	59.894721
2265.141035	63.135797	59.899725
2264.170435	59.788752	59.904730
2263.860521	63.537540	59.909735
2263.156410	61.138046	59.914740
2262.504117	67.174777	59.919745
2261.527106	62.857021	59.924750
2260.962333	64.114880	59.929754
2260.766621	60.936497	59.934759
2260.003823	72.049706	59.939764
2259.024834	69.450910	59.944769
2258.176250	59.054967	59.949774
2257.617689	74.273494	59.954778
2256.996370	69.416508	59.959783
2256.461441	68.946695	59.964788
2256.236729	64.460818	59.969793
2255.438903	60.549380	59.974798
2254.409440	65.525257	59.979802
2253.920096	53.417946	59.984807
2253.610937	68.699208	59.989812
2252.304907	54.144152	59.994817
2251.700783	59.270703	59.999822
2250.933795	62.189005	60.004826
2251.232684	64.013223	60.009831
2250.071627	67.446136	60.014836
2249.274562	67.610867	60.019841
2248.431225	64.658888	60.024846
2247.940490	63.116558	60.029850
2247.783087	53.491337	60.034855
2246.046022	64.068545	60.039860
2245.237934	62.874948	60.044865
2244.866904	59.601815	60.049870
2244.402474	65.577606	60.054874
2244.052811	58.964626	60.059879
2243.380032	68.809590	60.064884
2243.280032	58.990609	60.069889
2242.201458	62.814402	60.074894
2241.197875	63.314835	60.079898
2240.891529	65.119796	60.084903
2239.770684	73.487760	60.089908
2238.936948	59.620461	60.094913
2238.267166	61.141008	60.099918
2237.746767	66.144695	60.104922
2237.558514	56.810134	60.109927
2236.912088	60.495290	60.114932
2236.390127	68.683076	60.119937
2235.197813	59.037080	60.124942
2234.006051	63.810196	60.129946
2234.170293	62.740047	60.134951
2233.770143	72.156299	60.139956
2233.018481	67.046092	60.144961
2232.039509	62.442110	60.149966
2230.954539	56.916423	60.154970
2231.174827	63.771791	60.159975
2230.317788	70.430491	60.164980
2229.345276	64.573345	60.169985
2228.463083	63.783988	60.174990
2227.983957	72.218257	60.179994
2227.256333	60.804961	60.184999
2227.073094	65.865064	60.190004
2226.043182	68.672813	60.195009
2225.187787	62.980764	60.200014
2224.373572	73.314113	60.205018
2224.217507	57.558624	60.210023
2223.537801	65.111831	60.215028
2223.213952	54.312358	60.220033
2222.278143	63.365886	60.225038
2221.511750	66.533554	60.230042
2220.906521	60.181774	60.235047
2220.710772	62.068476	60.240052
2219.271533	59.789576	60.245057
2218.634246	51.343361	60.250062
2217.777921	64.869312	60.255066
2217.545961	62.515784	60.260071
2216.849283	71.412768	60.265076
2216.297380	68.695155	60.270081
2215.152817	61.325256	60.275086
2214.682983	71.381033	60.280090
2214.436217	60.816656	60.285095
2214.071633	68.625436	60.290100
2213.274334	61.021288	60.295105
2212.086514	64.327342	60.300110
2211.390844	66.457033	60.305114
2211.168417	62.076556	60.310119
2210.823129	67.090560	60.315124
2209.889866	65.565494	60.320129
2209.095126	69.840472	60.325134
2208.466843	63.048178	60.330138
2207.509847	64.824287	60.335143
2206.301384	71.732951	60.340148
2205.725620	63.945659	60.345153
2205.786629	66.010286	60.350158
2205.228817	75.376137	60.355162
2204.828948	62.809859	60.360167
2203.658464	66.845949	60.365172
2202.536366	70.471937	60.370177
2202.156920	67.752069	60.375182
2201.273689	74.888525	60.380186
2200.920161	62.253141	60.385191
2200.388905	72.834535	60.390196
2199.546790	63.900735	60.395201
2199.156949	60.644244	60.400206
2198.791912	65.210063	60.405210
2198.609525	62.694907	60.410215
2197.079892	62.070357	60.415220
2196.333701	57.970107	60.420225
2196.043600	60.564499	60.425230
2194.860806	63.876800	60.430234
2193.638598	64.571336	60.435239
2193.501327	67.728122	60.440244
2192.939804	61.448212	60.445249
2192.665131	57.456790	60.450254
2191.548008	64.263388	60.455258
2191.257662	58.889567	60.460263
2190.731722	72.644801	60.465268
2189.656033	62.170876	60.470273
2189.031448	66.491357	60.475278
2188.177012	75.005207	60.480282
2188.190743	72.648739	60.485287
2187.431146	71.320942	60.490292
2186.224210	65.001021	60.495297
2185.502794	74.259856	60.500302
2184.757531	69.471446	60.505306
2184.487047	71.393825	60.510311
2183.802851	79.640150	60.515316
2183.528246	72.404490	60.520321
2182.864363	73.306294	60.525326
2181.799628	69.732610	60.530330
2181.615304	68.232616	60.535335
2180.458241	75.902598	60.540340
2179.171708	68.567645	60.545345
2179.045457	74.580337	60.550350
2178.397518	75.913215	60.555354
2178.475783	70.465298	60.560359
2177.465445	66.791920	60.565364
2176.231417	74.945969	60.570369
2175.591455	71.988825	60.575374
2174.899539	70.982995	60.580378
2174.848625	70.265813	60.585383
2174.051606	73.026636	60.590388
2173.639527	67.064181	60.595393
2173.079293	66.782645	60.600398
2172.252412	75.646245	60.605402
2171.555727	64.375295	60.610407
2170.184410	68.291797	60.615412
2169.553245	65.087238	60.620417
2169.170311	63.376485	60.625422
2168.588060	62.185723	60.630426
2168.046578	61.644412	60.635431
2167.752979	70.820210	60.640436
2166.404132	63.835776	60.645441
2165.646975	61.131564	60.650446
2165.220687	68.943791	60.655450
2164.768256	63.920574	60.660455
2164.406496	73.025139	60.665460
2163.356673	72.953253	60.670465
2162.552104	65.339306	60.675470
2161.832623	74.313216	60.680474
2161.561733	64.902797	60.685479
2161.193434	75.978935	60.690484
2160.346163	60.773496	60.695489
2159.363793	68.452283	60.700494
2158.650531	75.965449	60.705498
2158.237128	68.331574	60.710503
2157.120848	71.003321	60.715508
2156.436519	68.331258	60.720513
2156.016758	72.607634	60.725518
2155.248660	73.169647	60.730522
2154.754532	66.675722	60.735527
2154.568734	70.690644	60.740532
2153.458322	71.313965	60.745537
2152.792995	68.160250	60.750542
2151.483446	70.043636	60.755546
2151.541028	58.956709	60.760551
2151.293711	64.836555	60.765556
2150.216313	58.994211	60.770561
2149.821452	66.172269	60.775566
2148.855498	63.974674	60.780570
2148.333860	66.684848	60.785575
2147.372838	72.344537	60.790580
2146.399121	70.821664	60.795585
2146.197921	62.198642	60.800590
2145.501757	68.358537	60.805594
2144.943390	60.592361	60.810599
2144.676945	70.502039	60.815604
2143.796492	71.806005	60.820609
2143.472147	68.129385	60.825614
2142.276880	74.380565	60.830618
2141.220190	73.955396	60.835623
2140.526116	72.033000	60.840628
2139.897441	71.122934	60.845633
2139.783600	67.043221	60.850638
2139.269141	79.988499	60.855642
2138.543071	71.196699	60.860647
2137.432438	62.570540	60.865652
2136.619374	74.803887	60.870657
2136.391402	64.206702	60.875662
2135.854412	73.452942	60.880666
2135.267518	73.291228	60.885671
2134.158419	75.580451	60.890676
2133.247483	70.298957	60.895681
2133.264547	62.726461	60.900686
2132.373822	77.565626	60.905690
2131.321561	71.244527	60.910695
2130.477290	74.715647	60.915700
2129.810344	76.648206	60.920705
2129.859593	67.641308	60.925710
2129.113113	78.564635	60.930714
2128.774577	76.652087	60.935719
2127.765058	70.518277	60.940724
2127.076083	73.912707	60.945729
2126.565409	71.042402	60.950734
2125.739254	73.030610	60.955738
2124.870390	68.901222	60.960743
2123.871901	72.832913	60.965748
2123.288015	85.837831	60.970753
2123.085440	65.395088	60.975758
2122.600852	74.317378	60.980762
2122.424986	76.784476	60.985767
2121.090191	76.635027	60.990772
2120.213420	68.229388	60.995777
2119.762106	65.566424	61.000782
2119.319924	75.004468	61.005786
2118.803386	71.648868	61.010791
2117.970416	73.155894	61.015796
2117.170947	70.264723	61.020801
2117.078310	65.927973	61.025806
2115.641987	79.706684	61.030810
2114.811496	76.262681	61.035815
2114.123426	77.868472	61.040820
2113.819260	66.711579	61.045825
2113.883235	70.882721	61.050830
2112.282355	71.051931	61.055834
2111.519935	72.192430	61.060839
2111.109039	72.102061	61.065844
2110.242647	62.384176	61.070849
2110.116321	61.688578	61.075854
2109.480529	70.500549	61.080858
2108.828573	69.526181	61.085863
2107.790197	66.110238	61.090868
2107.075354	68.450449	61.095873
2107.003813	65.788449	61.100878
2105.670720	79.268858	61.105882
2104.918026	65.228266	61.110887
2104.384570	75.005593	61.115892
2103.645871	75.910334	61.120897
2103.845735	74.180035	61.125902
2102.699615	72.306936	61.130906
2101.951880	70.462405	61.135911
2101.236300	71.844359	61.140916
2101.049024	72.748731	61.145921
2100.812052	63.538170	61.150926
2099.208347	70.911146	61.155930
2098.637733	67.565983	61.160935
2098.305549	71.347006	61.165940
2096.694545	73.199467	61.170945
2096.156371	64.796317	61.175950
2095.457338	64.559449	61.180954
2095.297006	61.031224	61.185959
2094.811838	63.159659	61.190964
2094.229538	72.112476	61.195969
2093.813191	67.453345	61.200974
2092.823447	67.537375	61.205978
2092.396882	65.885405	61.210983
2092.225813	62.503879	61.215988
2090.447411	70.113176	61.220993
2090.039516	52.012331	61.225998
2088.837860	72.664843	61.231002
2088.527130	63.413218	61.236007
2088.345273	64.714148	61.241012
2087.023286	69.829684	61.246017
2086.447817	62.471823	61.251022
2085.937075	71.458188	61.256026
2085.663739	71.512444	61.261031
2084.974174	67.037409	61.266036
2084.298336	70.207762	61.271041
2083.584014	64.761604	61.276046
2082.480486	78.918775	61.281050
2081.856526	60.543048	61.286055
2081.592054	72.780849	61.291060
2080.879363	71.360575	61.296065
2080.436580	70.096233	61.301070
2079.341089	73.561777	61.306074
2078.581073	69.155238	61.311079
2078.242411	61.169135	61.316084
2077.442988	70.049750	61.321089
2076.512583	63.163110	61.326094
2075.649359	74.329026	61.331098
2075.104362	66.065198	61.336103
2074.600995	69.838001	61.341108
2074.501882	70.646771	61.346113
2074.372220	70.911313	61.351118
2072.778247	67.359495	61.356122
2071.877077	62.313970	61.361127
2071.377737	68.830189	61.366132
2070.949396	71.563094	61.371137
2070.758219	65.214727	61.376142
2069.462356	71.688773	61.381146
2068.899137	66.918193	61.386151
2068.174593	69.514269	61.391156
2067.721843	73.915101	61.396161
2067.520089	70.149628	61.401166
2065.819132	70.389652	61.406170
2065.428612	61.206940	61.411175
2065.233835	67.371472	61.416180
2064.249987	69.362188	61.421185
2063.276952	68.346039	61.426190
2062.565968	70.764144	61.431194
2062.002574	69.693323	61.436199
2061.562004	69.516458	61.441204
2061.227995	64.006834	61.446209
2061.136319	61.821552	61.451214
2059.590029	70.694526	61.456218
2058.995916	69.270157	61.461223
2058.519828	67.666133	61.466228
2057.755534	71.569222	61.471233
2056.841629	67.781092	61.476238
2055.833911	74.570973	61.481242
2055.105650	77.688719	61.486247
2055.227504	68.100615	61.491252
2054.297113	75.455537	61.496257
2054.337896	61.021885	61.501262
2053.306825	72.267034	61.506266
2052.451830	75.903412	61.511271
2052.149790	76.746103	61.516276
2051.222417	81.089968	61.521281
2050.367308	69.844959	61.526286
2049.298593	72.945153	61.531290
2048.346175	70.700263	61.536295
2048.590527	66.935063	61.541300
2048.009191	72.372720	61.546305
2047.885462	65.456656	61.551310
2046.484519	69.679424	61.556314
2046.226565	70.007356	61.561319
2045.265801	66.822089	61.566324
2043.789539	69.187550	61.571329
2043.292231	64.067031	61.576334
2042.374273	58.829787	61.581338
2042.358698	70.402139	61.586343
2042.194840	64.751312	61.591348
2041.580000	67.920313	61.596353
2041.141014	70.681881	61.601358
2040.223361	72.774564	61.606362
2039.248444	77.471155	61.611367
2038.670049	63.589842	61.616372
2037.345946	70.734223	61.621377
2036.754794	71.169279	61.626382
2036.027444	71.074231	61.631386
2035.580080	75.936364	61.636391
2035.641697	71.973086	61.641396
2034.951203	75.419888	61.646401
2034.558310	66.367448	61.651406
2033.334835	67.142758	61.656410
2032.539846	66.431279	61.661415
2032.378592	66.326240	61.666420
2030.817585	64.314923	61.671425
2030.354247	60.592225	61.676430
2029.431477	73.839037	61.681434
2029.236786	68.426369	61.686439
2028.777648	67.175093	61.691444
2028.371607	68.909882	61.696449
2027.729263	69.429876	61.701454
2026.723467	72.245769	61.706458
2026.011243	69.217722	61.711463
2025.602628	59.956012	61.716468
2024.188009	67.653092	61.721473
2023.701417	66.788209	61.726478
2022.864467	68.397371	61.731482
2022.493376	70.333411	61.736487
2022.062354	67.736457	61.741492
2021.432583	73.700670	61.746497
2021.438362	61.749887	61.751502
2020.120627	67.692439	61.756506
2019.515855	67.864178	61.761511
2018.682697	53.468321	61.766516
2017.634657	67.226799	61.771521
2017.191865	64.256084	61.776526
2016.236080	68.006808	61.781530
2016.010668	67.123301	61.786535
2015.964856	63.440102	61.791540
2015.238874	61.311219	61.796545
2014.158087	60.566527	61.801550
2013.171512	72.517724	61.806554
2012.777867	68.967441	61.811559
2012.427856	60.781192	61.816564
2010.864545	71.017691	61.821569
2010.446700	62.264778	61.826574
2010.053510	68.401671	61.831578
2009.358072	66.520185	61.836583
2009.107184	70.554924	61.841588
2008.327640	63.443161	61.846593
2007.592301	64.927185	61.851598
2006.769320	60.625377	61.856602
2006.447370	73.682971	61.861607
2005.998231	59.228135	61.866612
2004.547003	67.622244	61.871617
2003.802827	54.898604	61.876622
2002.968002	65.084302	61.881626
2003.025734	63.995264	61.886631
2002.807574	57.493239	61.891636
2001.641116	67.600278	61.896641
2000.880378	59.254955	61.901646
2000.080604	59.358610	61.906650
1999.664615	64.353525	61.911655
1999.462313	66.632521	61.916660
1998.233465	68.847518	61.921665
1997.903294	66.197396	61.926670
1996.970675	67.149927	61.931674
1996.290261	66.227414	61.936679
1995.391256	60.157235	61.941684
1994.307495	62.389649	61.946689
1993.882215	70.060787	61.951694
1992.911866	70.950302	61.956698
1992.682107	72.322189	61.961703
1992.411519	59.265705	61.966708
1992.618556	65.198480	61.971713
1991.415411	59.718333	61.976718
1990.596738	63.492181	61.981722
1989.734456	67.664660	61.986727
1989.258868	58.036270	61.991732
1987.972996	67.062070	61.996737
1987.851964	65.354294	62.001742
1987.273114	74.109161	62.006746
1986.213334	69.635500	62.011751
1985.558701	58.216889	62.016756
1984.676044	64.870517	62.021761
1984.113080	67.549089	62.026766
1983.721751	63.415805	62.031770
1983.593015	62.532341	62.036775
1982.964634	61.806185	62.041780
1981.958669	70.421358	62.046785
1981.174961	60.718969	62.051790
1980.181429	72.376896	62.056794
1979.113111	64.947446	62.061799
1978.679892	55.463780	62.066804
1978.080552	75.465391	62.071809
1977.583854	69.200083	62.076814
1977.236241	60.396480	62.081818
1976.940424	66.651315	62.086823
1976.298747	68.449309	62.091828
1975.116058	68.088753	62.096833
1974.537955	66.862569	62.101838
1974.100596	64.235522	62.106842
1972.470602	66.822685	62.111847
1972.195582	69.352927	62.116852
1971.532494	75.031143	62.121857
1970.905763	60.448410	62.126862
1970.577764	73.044028	62.131866
1970.243184	73.100082	62.136871
1969.702112	68.911496	62.141876
1968.258755	74.869628	62.146881
1967.900887	69.240547	62.151886
1967.664662	64.988762	62.156890
1966.713487	66.102361	62.161895
1965.849621	59.640535	62.166900
1964.869772	72.470812	62.171905
1964.628263	67.647190	62.176910
1964.184482	68.387425	62.181914
1962.889100	63.657639	62.186919
1962.299279	63.805117	62.191924
1961.398424	65.400352	62.196929
1961.455198	64.690805	62.201934
1960.928542	64.447757	62.206938
1960.347504	73.403123	62.211943
1959.509975	69.430639	62.216948
1958.285236	68.648217	62.221953
1958.245139	72.522561	62.226958
1957.488099	73.658213	62.231962
1956.381019	72.927898	62.236967
1955.939451	70.264863	62.241972
1955.320887	73.588451	62.246977
1955.300680	67.732275	62.251982
1953.989187	68.234119	62.256986
1952.772195	62.084140	62.261991
1952.616257	56.294606	62.266996
1951.736160	66.750937	62.272001
1951.165747	69.365657	62.277006
1950.868847	66.228683	62.282010
1949.871032	63.320554	62.287015
1949.919651	64.517326	62.292020
1948.653191	61.781465	62.297025
1948.170507	59.015339	62.302030
1947.201610	63.809588	62.307034
1946.086313	70.276448	62.312039
1945.996415	61.516392	62.317044
1945.272243	68.472506	62.322049
1944.989911	62.951688	62.327054
1944.542560	71.277102	62.332058
1943.486886	66.454212	62.337063
1942.958358	58.192728	62.342068
1942.047054	66.852496	62.347073
1941.467067	66.045044	62.352078
1940.465231	69.465774	62.357082
1939.649048	66.077383	62.362087
1939.693649	64.208254	62.367092
1938.973312	60.936885	62.372097
1938.211357	49.072459	62.377102
1937.702789	58.603553	62.382106
1936.904189	69.561450	62.387111
1936.431657	58.178802	62.392116
1935.743877	67.938709	62.397121
1934.974139	55.419189	62.402126
1934.040385	65.606421	62.407130
1932.977457	62.956925	62.412135
1933.014976	67.121529	62.417140
1932.400529	70.393100	62.422145
1931.741694	59.799397	62.427150
1930.416973	58.893961	62.432154
1929.990686	64.097473	62.437159
1929.809093	57.538677	62.442164
1928.847775	66.132400	62.447169
1928.516445	60.403660	62.452174
1927.209349	65.456680	62.457178
1926.252795	66.608704	62.462183
1925.965888	60.696319	62.467188
1925.501846	66.771914	62.472193
1925.246731	66.448471	62.477198
1925.054132	58.194652	62.482202
1923.735588	62.007049	62.487207
1923.156747	58.415042	62.492212
1922.555704	67.332776	62.497217
1921.397122	60.021808	62.502222
1920.580546	58.568412	62.507226
1920.122904	72.940344	62.512231
1919.894220	59.054107	62.517236
1919.456596	66.978792	62.522241
1918.694014	69.219827	62.527246
1917.797755	62.791578	62.532250
1916.996083	67.843002	62.537255
1916.178378	65.944159	62.542260
1914.837158	63.407009	62.547265
1914.793365	58.321817	62.552270
1913.931837	61.311196	62.557274
1913.146460	59.346037	62.562279
1912.722702	44.018509	62.567284
1912.130213	61.804148	62.572289
1912.258042	66.668141	62.577294
1912.119111	59.935081	62.582298
1910.661553	65.572374	62.587303
1909.974019	54.135334	62.592308
1909.094166	62.659465	62.597313
1908.304629	62.900718	62.602318
1907.473914	55.756685	62.607322
1906.332833	70.154746	62.612327
1906.061448	52.023493	62.617332
1905.437782	57.497603	62.622337
1905.595765	55.279881	62.627342
1905.093093	53.501220	62.632346
1904.149913	65.564200	62.637351
1903.475564	52.967191	62.642356
1902.342269	60.299597	62.647361
1901.116184	54.026855	62.652366
1900.742071	61.551083	62.657370
1900.027682	58.965123	62.662375
1899.526904	62.675914	62.667380
1899.164372	61.725085	62.672385
1899.024857	58.725002	62.677390
1898.778364	60.448686	62.682394
1898.000645	64.624470	62.687399
1897.099882	63.226926	62.692404
1895.605780	61.838128	62.697409
1894.882320	62.340831	62.702414
1894.592591	61.911210	62.707418
1893.850476	66.239187	62.712423
1893.445085	67.023779	62.717428
1891.772753	64.638409	62.722433
1891.163288	63.560885	62.727438
1890.658904	58.444364	62.732442
1890.869470	65.494768	62.737447
1890.044305	65.843957	62.742452
1889.532151	64.734392	62.747457
1889.048609	67.382805	62.752462
1888.144004	58.840289	62.757466
1887.141445	64.434877	62.762471
1887.029231	58.206834	62.767476
1885.977997	70.216464	62.772481
1885.039639	64.514606	62.777486
1884.648779	63.222455	62.782490
1884.389111	63.569239	62.787495
1883.745214	60.790834	62.792500
1882.442721	62.900037	62.797505
1881.888352	63.216715	62.802510
1881.432403	63.183017	62.807514
1880.610776	68.269832	62.812519
1880.597660	67.224491	62.817524
1878.733171	62.916158	62.822529
1878.012947	67.112107	62.827534
1877.859630	64.975666	62.832538
1877.518344	64.434477	62.837543
1877.460026	55.470484	62.842548
1876.139697	70.182622	62.847553
1875.676498	60.839490	62.852558
1874.929473	59.121976	62.857562
1873.650849	65.384691	62.862567
1873.106799	60.951904	62.867572
1872.417825	71.654612	62.872577
1871.998179	64.000144	62.877582
1871.765210	69.728722	62.882586
1871.201320	76.667685	62.887591
1870.890592	64.567393	62.892596
1869.098460	66.510114	62.897601
1868.483319	70.016272	62.902606
1868.369589	61.571342	62.907610
1867.241652	67.499607	62.912615
1866.288863	59.202172	62.917620
1865.304676	59.635410	62.922625
1865.375123	61.879587	62.927630
1864.766265	58.879673	62.932634
1864.439973	67.626066	62.937639
1864.311362	54.376382	62.942644
1863.241740	69.428112	62.947649
1862.581477	67.520895	62.952654
1861.959625	59.700111	62.957658
1860.458603	63.716628	62.962663
1859.545421	58.100073	62.967668
1859.360654	71.832050	62.972673
1858.961011	62.401077	62.977678
1858.559916	55.820634	62.982682
1857.947225	66.349637	62.987687
1857.101866	52.111834	62.992692
1856.160425	64.007945	62.997697
1855.289953	63.311381	63.002702
1855.150176	60.677646	63.007706
1854.300045	61.782660	63.012711
1853.620196	58.845812	63.017716
1852.580766	64.338559	63.022721
1852.604705	65.177592	63.027726
1852.022476	57.258458	63.032730
1850.793173	67.043910	63.037735
1849.761540	62.202326	63.042740
1849.119284	73.950948	63.047745
1848.714377	63.628807	63.052750
1848.448138	52.156022	63.057754
1847.987942	68.391856	63.062759
1847.155019	57.959401	63.067764
1845.907295	63.331080	63.072769
1845.733298	64.243844	63.077774
1845.499065	60.123173	63.082778
1844.669557	71.642918	63.087783
1843.529064	62.660393	63.092788
1843.191110	60.483704	63.097793
1842.682234	64.554290	63.102798
1841.292338	62.197588	63.107802
1840.140027	65.083573	63.112807
1839.711725	56.411427	63.117812
1839.863502	63.595430	63.122817
1839.230960	61.325068	63.127822
1839.055631	54.392200	63.132826
1838.184832	58.762327	63.137831
1836.781907	58.151336	63.142836
1836.433311	59.089629	63.147841
1836.161018	60.782204	63.152846
1835.271536	61.353976	63.157850
1834.015162	60.369769	63.162855
1833.835224	60.751465	63.167860
1833.324428	58.787893	63.172865
1832.664968	59.789239	63.177870
1831.653809	61.625593	63.182874
1830.853925	65.817413	63.187879
1830.171759	60.208312	63.192884
1829.848625	61.830641	63.197889
1829.625422	66.841524	63.202894
1829.211790	70.853977	63.207898
1827.614985	65.274653	63.212903
1827.279842	63.494573	63.217908
1826.399471	70.150195	63.222913
1825.723391	62.384483	63.227918
1824.817707	60.879246	63.232922
1823.700278	66.898084	63.237927
1823.830239	59.376559	63.242932
1823.121240	61.044381	63.247937
1822.874463	58.818149	63.252942
1822.633498	48.837432	63.257946
1821.330949	56.854041	63.262951
1820.470856	59.125584	63.267956
1819.886395	63.641716	63.272961
1819.538630	61.265006	63.277966
1818.509615	59.920996	63.282970
1817.600235	66.413035	63.287975
1817.274561	60.265332	63.292980
1816.801142	61.938637	63.297985
1816.246232	56.329083	63.302990
1815.334116	53.066470	63.307994
1814.565243	70.415333	63.312999
1814.288157	61.374304	63.318004
1813.583536	57.677523	63.323009
1812.714100	55.306780	63.328014
1812.482382	57.794091	63.333018
1811.668547	64.963307	63.338023
1810.550203	65.367800	63.343028
1808.910360	59.539674	63.348033
1808.386120	57.175002	63.353038
1808.852214	52.339278	63.358042
1808.195181	70.908823	63.363047
1807.666346	59.327422	63.368052
1807.055589	62.888489	63.373057
1805.913647	66.402681	63.378062
1805.081817	62.043614	63.383066
1804.284043	67.255428	63.388071
1803.910756	57.555890	63.393076
1803.305482	66.904989	63.398081
1803.378631	65.747000	63.403086
1802.571391	57.077722	63.408090
1801.260355	59.594177	63.413095
1800.928363	60.231222	63.418100
1800.142009	58.564659	63.423105
1799.158357	61.302984	63.428110
1798.367755	60.622764	63.433114
1797.814744	66.377677	63.438119
1797.706829	64.034533	63.443124
1797.430336	61.051575	63.448129
1796.461608	70.042879	63.453134
1795.828522	58.542868	63.458138
1794.641058	64.186867	63.463143
1794.172677	61.830795	63.468148
1793.209236	65.464837	63.473153
1791.899388	58.353467	63.478158
1791.715310	60.863811	63.483162
1790.539174	67.705823	63.488167
1790.813827	60.891355	63.493172
1790.006330	62.725237	63.498177
1790.083008	60.986406	63.503182
1790.041651	65.121473	63.508186
1788.575778	70.673378	63.513191
1787.976473	65.188258	63.518196
1786.835838	58.646334	63.523201
1785.810851	66.196271	63.528206
1785.379125	61.001810	63.533210
1784.840723	63.731060	63.538215
1784.910034	59.559248	63.543220
1783.661551	67.518067	63.548225
1782.634156	70.653471	63.553230
1782.561836	65.156341	63.558234
1781.745439	68.636943	63.563239
1781.072858	62.246637	63.568244
1779.992288	61.473144	63.573249
1778.885551	74.145938	63.578254
1778.611964	66.883318	63.583258
1777.988211	72.683889	63.588263
1777.762350	65.511785	63.593268
1777.669918	64.119242	63.598273
1776.536925	74.084800	63.603278
1776.123245	62.936051	63.608282
1775.174892	65.813993	63.613287
1774.366926	62.837896	63.618292
1773.391728	68.949245	63.623297
1772.773923	56.825336	63.628302
1772.364356	49.934135	63.633306
1772.114831	62.854183	63.638311
1770.932640	57.418275	63.643316
1770.043713	57.619320	63.648321
1769.300764	62.944908	63.653326
1769.199624	59.099486	63.658330
1768.409522	65.862031	63.663335
1768.588827	65.828199	63.668340
1766.790851	60.190955	63.673345
1765.996436	60.397933	63.678350
1765.860122	59.090660	63.683354
1765.391121	56.612335	63.688359
1764.636738	64.890019	63.693364
1763.395042	57.067554	63.698369
1763.021812	58.206242	63.703374
1762.826596	54.297184	63.708378
1761.900810	64.458985	63.713383
1760.748758	58.633071	63.718388
1759.752868	58.064163	63.723393
1759.325862	56.001399	63.728398
1759.356613	49.778118	63.733402
1758.730989	59.520679	63.738407
1758.517012	56.744126	63.743412
1757.538251	58.510609	63.748417
1756.450584	64.087015	63.753422
1756.453674	63.374416	63.758426
1754.780230	76.054576	63.763431
1754.109771	61.421755	63.768436
1753.704475	58.596230	63.773441
1753.221710	64.157158	63.778446
1752.937794	66.900103	63.783450
1751.795279	68.952359	63.788455
1751.097358	59.869273	63.793460
1750.218131	57.123260	63.798465
1749.832369	62.690089	63.803470
1749.595646	54.921456	63.808474
1748.815404	61.024709	63.813479
1748.126160	50.419288	63.818484
1747.631759	53.006805	63.823489
1746.695079	55.603291	63.828494
1746.190901	56.874907	63.833498
1745.198494	62.147658	63.838503
1744.378374	58.533016	63.843508
1744.290164	62.496500	63.848513
1742.904699	74.472940	63.853518
1742.456287	59.648980	63.858522
1741.208415	60.600628	63.863527
1740.818231	62.501660	63.868532
1740.208352	64.819214	63.873537
1739.954731	64.919849	63.878542
1739.502893	64.114966	63.883546
1739.037730	72.420139	63.888551
1738.357473	64.105314	63.893556
1737.249777	65.703214	63.898561
1736.851162	68.743667	63.903566
1736.792350	63.877756	63.908570
1734.758223	64.007137	63.913575
1734.846834	66.394642	63.918580
1733.910007	58.150958	63.923585
1733.453404	62.201553	63.928590
1733.148508	52.335993	63.933594
1732.144016	62.961242	63.938599
1731.679983	58.381371	63.943604
1731.007959	58.337686	63.948609
1729.737270	66.882130	63.953614
1729.530157	58.205706	63.958618
1728.425480	64.324608	63.963623
1727.629719	58.813908	63.968628
1727.647470	66.496866	63.973633
1727.120266	69.939043	63.978638
1726.689904	59.044203	63.983642
1725.242963	69.093875	63.988647
1724.418141	59.474374	63.993652
1724.114602	64.842013	63.998657
1723.524472	66.190704	64.003662
1722.812138	53.875757	64.008666
1721.628129	68.854700	64.013671
1720.873628	56.956686	64.018676
1720.740133	52.317102	64.023681
1720.435437	58.961855	64.028686
1720.255851	52.182486	64.033690
1718.878892	67.390620	64.038695
1718.610528	61.487718	64.043700
1717.879275	55.304827	64.048705
1716.529534	60.918186	64.053710
1715.819080	57.360177	64.058714
1714.937491	60.266175	64.063719
1714.450402	67.313177	64.068724
1714.162342	58.187994	64.073729
1713.704555	58.970906	64.078734
1713.953775	51.623977	64.083738
1712.573923	63.037766	64.088743
1712.262297	63.380423	64.093748
1710.938767	58.818944	64.098753
1709.337483	58.245482	64.103758
1709.118459	53.418832	64.108762
1708.409454	56.643048	64.113767
1708.140228	50.735167	64.118772
1707.856762	57.509307	64.123777
1707.516398	66.069031	64.128782
1706.893912	54.740513	64.133786
1705.943984	65.873118	64.138791
1705.263108	62.117425	64.143796
1704.502890	57.850727	64.148801
1702.920187	58.116420	64.153806
1702.607490	55.861609	64.158810
1702.375501	62.969165	64.163815
1701.682040	58.045282	64.168820
1701.399848	58.414481	64.173825
1700.729480	63.265044	64.178830
1699.995874	59.216020	64.183834
1699.111125	63.546712	64.188839
1698.273319	54.571257	64.193844
1697.077157	46.799051	64.198849
1696.347579	57.652378	64.203854
1696.722310	57.646285	64.208858
1695.670755	58.651190	64.213863
1695.226248	58.343588	64.218868
1694.932441	54.615215	64.223873
1693.780949	69.755168	64.228878
1692.977476	58.769449	64.233882
1692.018033	60.208573	64.238887
1691.859114	60.203405	64.243892
1691.658785	62.618639	64.248897
1690.298974	65.221226	64.253902
1689.673564	51.214646	64.258906
1688.859337	55.902726	64.263911
1688.378219	60.272899	64.268916
1688.415872	56.835162	64.273921
1687.129027	50.110667	64.278926
1686.665092	56.914503	64.283930
1685.402678	51.233808	64.288935
1685.383599	57.871132	64.293940
1684.879584	49.726292	64.298945
1683.255586	57.185323	64.303950
1682.876221	48.779954	64.308954
1682.510995	55.862149	64.313959
1681.778863	56.441361	64.318964
1681.665627	58.060937	64.323969
1680.627910	60.299344	64.328974
1680.007407	55.564684	64.333978
1679.610917	61.593988	64.338983
1678.861823	62.381752	64.343988
1677.952370	57.155769	64.348993
1677.586888	62.014555	64.353998
1677.184321	57.369702	64.359002
1675.695606	59.982112	64.364007
1674.942536	51.415306	64.369012
1674.542219	49.596263	64.374017
1673.663871	59.447593	64.379022
1673.934891	51.170133	64.384026
1672.216168	58.989177	64.389031
1671.149040	53.884911	64.394036
1670.969964	57.362252	64.399041
1670.398644	65.029562	64.404046
1669.973531	50.183090	64.409050
1669.594079	52.945540	64.414055
1668.915187	58.755941	64.419060
1668.236454	51.030195	64.424065
1667.275887	50.889453	64.429070
1666.861237	58.360616	64.434074
1666.363944	57.087092	64.439079
1665.156545	54.362517	64.444084
1664.825912	57.147402	64.449089
1663.950521	61.010727	64.454094
1663.494451	43.008251	64.459098
1662.316799	55.673437	64.464103
1661.692037	52.996788	64.469108
1661.109340	58.662051	64.474113
1660.616394	62.466248	64.479118
1660.805086	52.054416	64.484122
1659.860056	64.367185	64.489127
1658.824988	52.064064	64.494132
1658.125766	57.289418	64.499137
1657.530089	62.225488	64.504142
1657.114260	57.368969	64.509146
1656.095953	59.954176	64.514151
1655.204453	53.202694	64.519156
1654.794992	44.243165	64.524161
1653.995389	56.996417	64.529166
1653.639516	50.598918	64.534170
1652.286894	54.290892	64.539175
1651.928735	48.492970	64.544180
1651.724951	54.186940	64.549185
1651.053524	60.345787	64.554190
1650.610451	43.556037	64.559194
1649.165880	59.719119	64.564199
1648.486822	55.504462	64.569204
1648.253013	53.424439	64.574209
1647.627922	63.686363	64.579214
1647.124391	56.743760	64.584218
1645.675823	55.601051	64.589223
1645.165448	59.439808	64.594228
1644.591610	56.611558	64.599233
1644.115176	59.795194	64.604238
1644.268583	59.532905	64.609242
1643.319336	57.625044	64.614247
1641.870454	59.063066	64.619252
1641.402639	51.543985	64.624257
1640.868803	64.433335	64.629262
1640.740697	58.306714	64.634266
1639.488093	61.921579	64.639271
1639.098527	61.349197	64.644276
1637.902231	54.883156	64.649281
1637.658042	61.275986	64.654286
1637.588120	62.298044	64.659290
1636.298749	61.473079	64.664295
1635.496094	60.984018	64.669300
1635.295054	53.575200	64.674305
1634.198939	57.711551	64.679310
1633.557147	53.902213	64.684314
1632.938118	55.500189	64.689319
1632.065256	52.686404	64.694324
1632.294495	51.566833	64.699329
1630.873648	59.279653	64.704334
1630.385102	54.921482	64.709338
1629.843149	53.522189	64.714343
1629.195414	60.114728	64.719348
1628.655501	49.932578	64.724353
1627.434925	56.673667	64.729358
1626.713858	56.659309	64.734362
1626.014408	55.298021	64.739367
1625.851030	55.344141	64.744372
1625.551096	58.399683	64.749377
1624.269486	58.590191	64.754382
1623.620818	52.643836	64.759386
1622.823486	60.056150	64.764391
1622.366855	62.741026	64.769396
1622.340576	52.530187	64.774401
1620.761832	60.506467	64.779406
1620.186204	58.888342	64.784410
1619.413606	60.368922	64.789415
1619.197616	65.535665	64.794420
1618.969139	52.805198	64.799425
1618.031827	61.058536	64.804430
1616.895419	60.161613	64.809434
1616.428174	54.137635	64.814439
1615.455672	57.452345	64.819444
1615.480659	56.697713	64.824449
1614.310042	63.808399	64.829454
1613.434030	54.869108	64.834458
1612.719872	55.663534	64.839463
1612.440776	59.022997	64.844468
1612.335361	57.059549	64.849473
1611.270642	65.193779	64.854478
1611.020639	51.957414	64.859482
1610.326540	57.490171	64.864487
1609.766555	55.335316	64.869492
1608.806261	53.459746	64.874497
1607.308592	59.557894	64.879502
1607.170248	53.542367	64.884506
1606.748865	55.211518	64.889511
1606.362900	61.006927	64.894516
1605.546140	63.254112	64.899521
1604.492556	62.577481	64.904526
1604.376337	54.037489	64.909530
1603.061936	57.340055	64.914535
1601.865862	58.286029	64.919540
1601.961030	54.802927	64.924545
1600.988446	59.366546	64.929550
1600.715458	60.934911	64.934554
1600.243615	54.786202	64.939559
1599.168374	52.661896	64.944564
1598.331672	60.603953	64.949569
1597.310119	64.515588	64.954574
1597.152013	57.096662	64.959578
1597.043579	58.064129	64.964583
1596.742090	60.151296	64.969588
1596.241699	56.178429	64.974593
1594.955703	55.321321	64.979598
1594.119010	55.802786	64.984602
1592.944147	49.912541	64.989607
1592.297917	60.318996	64.994612
1592.129951	53.662383	64.999617
1591.568584	52.796526	65.004622
1591.153063	45.192721	65.009626
1589.895111	50.427647	65.014631
1588.952787	54.413350	65.019636
1588.473250	51.646336	65.024641
1587.631409	52.375383	65.029646
1587.616879	51.121088	65.034650
1587.246998	55.394468	65.039655
1585.927631	57.030989	65.044660
1585.586740	50.962499	65.049665
1584.953474	60.998068	65.054670
1584.348765	57.588558	65.059674
1583.475088	50.742864	65.064679
1582.355859	48.502939	65.069684
1581.625672	48.792897	65.074689
1580.802430	48.744322	65.079694
1580.407405	48.346556	65.084698
1580.411516	56.142746	65.089703
1579.964854	58.872889	65.094708
1579.704064	47.660527	65.099713
1578.871006	59.547179	65.104718
1577.967704	54.515949	65.109722
1576.528275	47.798656	65.114727
1576.100989	57.911073	65.119732
1575.680547	50.544153	65.124737
1574.410692	60.195266	65.129742
1573.119694	51.064914	65.134746
1573.330730	52.688203	65.139751
1572.968792	51.920449	65.144756
1572.449741	44.076219	65.149761
1571.601693	52.481642	65.154766
1571.463956	47.144145	65.159770
1569.979289	56.057185	65.164775
1569.167507	47.490586	65.169780
1568.621680	49.767983	65.174785
1568.162394	63.263885	65.179790
1568.151030	45.377951	65.184794
1567.441177	52.720824	65.189799
1566.420441	65.791390	65.194804
1566.242083	42.677165	65.199809
1564.854821	61.112319	65.204814
1563.760189	47.005692	65.209818
1562.864885	50.550739	65.214823
1562.416921	53.114533	65.219828
1562.232787	55.868429	65.224833
1561.634267	55.072088	65.229838
1561.008363	53.672567	65.234842
1560.971077	54.214982	65.239847
1560.246713	62.738974	65.244852
1559.759970	50.177056	65.249857
1558.535513	52.070090	65.254862
1557.693885	53.570781	65.259866
1556.907716	49.991024	65.264871
1556.382713	55.697731	65.269876
1555.795719	48.354582	65.274881
1554.871011	54.716246	65.279886
1554.299109	55.883815	65.284890
1553.534277	53.569034	65.289895
1552.885692	58.539426	65.294900
1552.642417	43.188997	65.299905
1552.020541	56.901394	65.304910
1550.933356	50.636172	65.309914
1550.220921	52.981162	65.314919
1549.615906	55.256849	65.319924
1549.389672	42.414708	65.324929
1548.710582	49.450356	65.329934
1547.665222	58.356899	65.334938
1546.782263	56.020890	65.339943
1546.138104	55.692999	65.344948
1546.442602	49.052636	65.349953
1545.258578	53.140891	65.354958
1544.159958	43.698169	65.359962
1543.443660	45.290696	65.364967
1542.964897	54.274340	65.369972
1542.623542	50.445572	65.374977
1542.248471	57.123681	65.379982
1541.342337	56.290387	65.384986
1540.471266	45.784820	65.389991
1539.608773	50.120008	65.394996
1539.499874	53.802432	65.400001
1538.529123	53.134928	65.405006
1538.099260	53.710584	65.410010
1537.492268	48.075258	65.415015
1536.777435	58.110970	65.420020
1535.707058	54.892079	65.425025
1534.512601	46.190070	65.430030
1533.765496	48.588756	65.435034
1533.440379	41.450258	65.440039
1532.889075	52.670161	65.445044
1532.843118	46.143855	65.450049
1532.222384	58.142978	65.455054
1532.116007	50.617713	65.460058
1530.777903	50.538847	65.465063
1530.169982	60.606393	65.470068
1529.875917	51.447535	65.475073
1528.403305	51.931270	65.480078
1527.804168	44.843616	65.485082
1527.586354	53.175127	65.490087
1527.264865	57.562984	65.495092
1526.229038	51.783562	65.500097
1525.012626	52.870790	65.505102
1524.478022	48.176324	65.510106
1524.463012	53.131041	65.515111
1523.408110	54.161024	65.520116
1522.525298	52.283658	65.525121
1521.647841	58.939990	65.530126
1521.046707	49.397919	65.535130
1520.881249	55.946999	65.540135
1520.514899	52.548018	65.545140
1519.294661	45.896649	65.550145
1518.583326	47.326101	65.555150
1518.203146	48.307315	65.560154
1517.950022	49.002717	65.565159
1516.731205	54.463449	65.570164
1516.253100	43.872478	65.575169
1515.548154	50.502440	65.580174
1514.249539	47.360512	65.585178
1513.829031	50.386957	65.590183
1512.539825	57.140206	65.595188
1512.828047	45.896260	65.600193
1511.951727	58.593175	65.605198
1511.581738	55.745845	65.610202
1511.027721	47.263823	65.615207
1510.664349	46.187650	65.620212
1509.547361	40.757243	65.625217
1508.954504	61.648162	65.630222
1508.051694	45.788147	65.635226
1507.875671	45.622498	65.640231
1506.719939	52.108965	65.645236
1505.747743	54.518943	65.650241
1505.245022	54.067382	65.655246
1504.942558	45.843084	65.660250
1504.598229	48.807941	65.665255
1503.002427	50.118388	65.670260
1502.705139	52.999803	65.675265
1501.982804	47.543691	65.680270
1501.211545	51.419210	65.685274
1501.249353	49.833080	65.690279
1500.639292	50.990607	65.695284
1500.178990	51.939353	65.700289
1499.101515	55.596900	65.705294
1498.318810	54.961559	65.710298
1497.524258	56.713137	65.715303
1496.421254	56.950868	65.720308
1495.984536	45.464699	65.725313
1495.252600	56.595526	65.730318
1494.961733	53.240468	65.735322
1495.020537	41.891719	65.740327
1493.436714	52.559689	65.745332
1492.801375	38.323569	65.750337
1491.857073	52.899134	65.755342
1491.667477	46.890024	65.760346
1491.525222	50.651573	65.765351
1490.364473	53.948786	65.770356
1489.664924	53.741693	65.775361
1488.711928	44.866142	65.780366
1488.540872	52.670198	65.785370
1488.129811	53.647227	65.790375
1486.916072	53.831284	65.795380
1486.588773	50.791923	65.800385
1485.427567	54.324862	65.805390
1485.149580	60.412434	65.810394
1484.234700	57.465349	65.815399
1482.985090	58.609977	65.820404
1482.500457	49.180995	65.825409
1482.037456	51.338439	65.830414
1481.647578	47.561403	65.835418
1481.527793	48.444765	65.840423
1481.194349	58.123111	65.845428
1480.173673	53.707623	65.850433
1479.021415	56.181976	65.855438
1478.723951	55.974352	65.860442
1477.714319	56.632270	65.865447
1476.829571	47.096518	65.870452
1476.538871	49.083557	65.875457
1476.106480	61.824489	65.880462
1475.410794	46.234941	65.885466
1474.354535	41.246103	65.890471
1473.372247	52.138341	65.895476
1472.871993	50.828637	65.900481
1472.685130	55.266081	65.905486
1472.335016	48.794205	65.910490
1471.448387	45.014960	65.915495
1470.380782	56.907811	65.920500
1469.943627	49.651527	65.925505
1469.217368	53.245809	65.930510
1468.162169	56.496935	65.935514
1467.735406	51.249175	65.940519
1466.961242	59.257508	65.945524
1466.627549	50.878303	65.950529
1466.584689	53.051465	65.955534
1465.330727	57.014344	65.960538
1464.511036	59.658742	65.965543
1463.486336	65.255992	65.970548
1463.165320	57.019476	65.975553
1462.847479	61.105540	65.980558
1461.901015	58.301623	65.985562
1461.046897	58.528340	65.990567
1460.128573	62.474825	65.995572
1460.206654	53.712523	66.000577
1459.619887	65.087313	66.005582
1458.609517	61.480028	66.010586
1458.132368	55.082787	66.015591
1457.258347	58.096073	66.020596
1456.958519	61.200152	66.025601
1455.907639	58.418055	66.030606
1455.017904	60.210798	66.035610
1454.534420	47.003773	66.040615
1453.693954	62.491926	66.045620
1453.654376	52.671392	66.050625
1453.075644	53.355821	66.055630
1451.929630	55.833057	66.060634
1451.075523	57.091569	66.065639
1450.659114	60.301650	66.070644
1450.187484	49.875363	66.075649
1449.810269	50.896730	66.080654
1448.303471	51.878553	66.085658
1447.564123	46.240636	66.090663
1447.437123	55.796411	66.095668
1447.314660	51.605730	66.100673
1446.131781	55.373691	66.105678
1445.077346	56.677939	66.110682
1444.478312	53.177878	66.115687
1444.134273	53.663460	66.120692
1443.980875	49.592148	66.125697
1443.230595	50.349753	66.130702
1442.116341	51.471222	66.135706
1441.434733	48.945252	66.140711
1440.859769	54.991289	66.145716
1440.291606	50.151007	66.150721
1439.124789	56.327557	66.155726
1438.570365	51.359798	66.160730
1438.201474	54.612269	66.165735
1437.524464	57.568944	66.170740
1436.706010	51.197364	66.175745
1435.877837	52.482227	66.180750
1434.756810	54.576655	66.185754
1434.832279	47.929313	66.190759
1434.242037	53.042482	66.195764
1434.414866	57.072981	66.200769
1433.018081	58.550297	66.205774
1431.982590	60.425226	66.210778
1431.650547	53.881974	66.215783
1431.251179	60.297018	66.220788
1430.237282	51.571239	66.225793
1429.615323	49.381624	66.230798
1428.971033	55.353084	66.235802
1428.247288	49.961962	66.240807
1427.751489	47.892062	66.245812
1427.013385	46.288354	66.250817
1425.850344	44.761328	66.255822
1425.671892	45.903404	66.260826
1425.463725	47.628830	66.265831
1423.992240	53.076381	66.270836
1423.236985	45.700878	66.275841
1422.870864	52.625336	66.280846
1422.205816	47.736118	66.285850
1421.873749	55.355373	66.290855
1421.294958	49.509198	66.295860
1420.144622	49.376511	66.300865
1419.753024	51.110836	66.305870
1419.272671	56.261641	66.310874
1418.562179	45.350483	66.315879
1417.335872	50.779753	66.320884
1416.516099	47.895743	66.325889
1415.980650	56.456479	66.330894
1415.755434	53.713452	66.335898
1415.530237	37.639602	66.340903
1414.358553	53.386931	66.345908
1413.645057	45.622985	66.350913
1413.217951	43.380679	66.355918
1412.495269	44.273690	66.360922
1412.021644	46.375722	66.365927
1410.987464	47.572698	66.370932
1410.302658	47.666236	66.375937
1409.716816	54.621594	66.380942
1408.951066	59.811384	66.385946
1408.700677	48.002036	66.390951
1407.532912	54.630705	66.395956
1406.924657	45.927473	66.400961
1406.787391	53.802711	66.405966
1406.035403	53.699339	66.410970
1405.403079	48.295336	66.415975
1404.210489	56.961844	66.420980
1404.042962	54.533797	66.425985
1403.392066	49.210733	66.430990
1402.287715	54.104023	66.435994
1401.375488	53.968082	66.440999
1400.682739	49.506353	66.446004
1400.437360	51.982193	66.451009
1400.015590	50.879316	66.456014
1399.366374	52.437090	66.461018
1398.730910	44.640450	66.466023
1397.637085	50.919372	66.471028
1397.060430	52.942336	66.476033
1396.615825	56.160403	66.481038
1396.196974	52.596352	66.486042
1395.094831	56.716802	66.491047
1393.971965	54.910156	66.496052
1393.691160	54.227603	66.501057
1393.749145	56.207064	66.506062
1393.134141	55.791311	66.511066
1392.224014	53.829835	66.516071
1390.961019	59.450120	66.521076
1390.565392	49.844086	66.526081
1390.148761	56.216691	66.531086
1389.036898	59.756597	66.536090
1388.611472	50.150533	66.541095
1387.812024	67.165940	66.546100
1387.108961	48.348092	66.551105
1386.673620	50.679220	66.556110
1386.017102	56.793691	66.561114
1385.012857	46.109263	66.566119
1384.740744	57.211117	66.571124
1384.191606	51.930634	66.576129
1383.445620	50.536298	66.581134
1382.180205	51.575897	66.586138
1381.641799	52.007126	66.591143
1380.845204	52.454525	66.596148
1380.905994	42.761687	66.601153
1380.477406	54.645024	66.606158
1379.625139	47.912160	66.611162
1378.608541	46.837687	66.616167
1378.148834	54.046178	66.621172
1377.669056	48.419893	66.626177
1377.404523	55.135919	66.631182
1376.180370	53.674625	66.636186
1375.420997	47.595303	66.641191
1375.016276	56.542985	66.646196
1373.727465	40.135309	66.651201
1372.804573	46.449708	66.656206
1372.242483	57.483967	66.661210
1372.123462	47.956900	66.666215
1371.246026	55.480043	66.671220
1371.233081	52.679764	66.676225
1370.585194	57.498082	66.681230
1369.024127	58.146208	66.686234
1369.137345	48.347293	66.691239
1368.044525	45.701471	66.696244
1367.633834	49.796323	66.701249
1367.113631	60.321332	66.706254
1365.962814	54.843069	66.711258
1365.494081	48.572689	66.716263
1365.360388	52.279879	66.721268
1364.167557	51.463328	66.726273
1363.411949	43.382539	66.731278
1362.488205	47.813097	66.736282
1362.368447	41.506271	66.741287
1361.654669	44.699365	66.746292
1360.315466	45.488322	66.751297
1359.486832	44.985202	66.756302
1358.805864	59.118218	66.761306
1358.296581	46.930848	66.766311
1358.308655	55.509170	66.771316
1357.659022	46.778296	66.776321
1357.557062	47.006534	66.781326
1356.598733	51.188816	66.786330
1356.132896	55.378763	66.791335
1355.216139	45.231975	66.796340
1354.103404	47.260264	66.801345
1353.424340	43.293942	66.806350
1352.489513	53.859924	66.811354
1352.225470	54.908501	66.816359
1351.575451	55.976574	66.821364
1351.148768	52.938844	66.826369
1350.709708	40.589467	66.831374
1349.723922	48.604423	66.836378
1349.540114	42.839458	66.841383
1348.564333	49.183835	66.846388
1347.179908	44.605661	66.851393
1346.569281	53.638322	66.856398
1345.935616	61.968386	66.861402
1345.947334	48.536491	66.866407
1345.502651	50.546736	66.871412
1344.455673	47.884389	66.876417
1343.393643	49.503757	66.881422
1342.622311	52.364091	66.886426
1342.458440	50.601312	66.891431
1341.602269	50.511441	66.896436
1341.474332	49.114730	66.901441
1340.559860	43.275115	66.906446
1339.962696	51.231048	66.911450
1339.352260	40.338706	66.916455
1338.164555	51.793066	66.921460
1337.320857	47.201670	66.926465
1337.072011	53.050576	66.931470
1336.392589	57.086833	66.936474
1336.140258	43.663436	66.941479
1335.289598	55.161940	66.946484
1333.908773	50.214091	66.951489
1333.630009	49.629872	66.956494
1333.034370	50.235896	66.961498
1333.024182	43.585463	66.966503
1332.241235	50.037746	66.971508
1330.876061	47.115281	66.976513
1330.537565	49.378915	66.981518
1329.797551	49.365869	66.986522
1329.351176	54.231401	66.991527
1328.073871	54.648603	66.996532
1327.898862	53.248898	67.001537
1327.284366	45.008967	67.006542
1326.401072	48.698430	67.011546
1326.319817	44.191245	67.016551
1325.323465	44.739161	67.021556
1324.988577	54.283147	67.026561
1324.167015	35.812842	67.031566
1322.969177	47.718914	67.036570
1322.285241	39.811780	67.041575
1321.281349	45.359693	67.046580
1321.033158	49.785133	67.051585
1320.871917	41.031451	67.056590
1320.035757	53.019291	67.061594
1319.670523	49.991176	67.066599
1318.338304	52.191250	67.071604
1317.619027	45.646415	67.076609
1317.125441	52.106794	67.081614
1317.040818	57.430244	67.086618
1316.354413	50.956355	67.091623
1315.576907	51.188138	67.096628
1314.936299	44.710360	67.101633
1314.329732	43.203358	67.106638
1313.081987	53.983954	67.111642
1312.545604	46.146687	67.116647
1312.148385	49.642816	67.121652
1311.321604	47.340262	67.126657
1310.505587	43.418708	67.131662
1309.500237	52.787349	67.136666
1309.184394	53.568888	67.141671
1308.651434	56.901554	67.146676
1308.079559	62.191186	67.151681
1308.104518	53.045246	67.156686
1306.662113	55.193136	67.161690
1305.921649	48.685480	67.166695
1305.538955	51.840455	67.171700
1305.191291	55.116534	67.176705
1304.062419	53.350014	67.181710
1302.902458	61.722020	67.186714
1302.699523	52.442997	67.191719
1302.040357	54.604826	67.196724
1301.471309	54.834871	67.201729
1300.436773	50.969276	67.206734
1299.632290	53.853053	67.211738
1299.308652	51.765933	67.216743
1299.308745	47.716906	67.221748
1298.573528	51.903236	67.226753
1297.679724	44.418461	67.231758
1296.508661	54.425312	67.236762
1296.568951	51.229622	67.241767
1295.727845	50.849431	67.246772
1294.161422	50.997993	67.251777
1293.381809	46.013155	67.256782
1292.855563	53.906821	67.261786
1292.842483	47.507531	67.266791
1292.312640	48.792656	67.271796
1292.065463	49.015757	67.276801
1291.443144	41.921461	67.281806
1289.882569	59.163466	67.286810
1288.928728	43.950131	67.291815
1288.630069	52.434410	67.296820
1288.521367	48.513345	67.301825
1288.309395	53.454797	67.306830
1286.497982	56.990143	67.311834
1286.265721	46.345685	67.316839
1285.892499	55.724135	67.321844
1284.933244	41.403398	67.326849
1284.132177	46.031244	67.331854
1283.265121	45.199993	67.336858
1283.163067	41.659089	67.341863
1282.293151	55.050011	67.346868
1281.870723	52.730737	67.351873
1280.968234	42.489165	67.356878
1280.252612	51.527960	67.361882
1279.694305	53.053212	67.366887
1279.170637	61.859423	67.371892
1277.831322	52.043928	67.376897
1277.089524	44.649182	67.381902
1276.636126	48.973969	67.386906
1276.484996	46.058410	67.391911
1276.058917	48.885698	67.396916
1275.134645	53.642396	67.401921
1274.748429	44.100694	67.406926
1273.673808	55.818718	67.411930
1273.619267	51.049605	67.416935
1272.711795	51.890985	67.421940
1271.299058	51.622079	67.426945
1270.627725	54.479513	67.431950
1269.939142	54.435566	67.436954
1269.789041	45.209083	67.441959
1269.591942	43.219508	67.446964
1268.615363	49.609424	67.451969
1268.079329	41.442518	67.456974
1266.969239	49.079704	67.461978
1266.610901	46.453028	67.466983
1265.668711	55.136290	67.471988
1264.621048	47.689703	67.476993
1264.245850	41.917252	67.481998
1263.692725	54.562394	67.487002
1263.485102	39.969706	67.492007
1262.338059	52.029321	67.497012
1261.278730	47.585772	67.502017
1261.239210	49.790331	67.507022
1260.540324	55.124996	67.512026
1260.245907	48.942021	67.517031
1259.460467	56.152203	67.522036
1258.254359	55.474523	67.527041
1257.794009	46.604298	67.532046
1257.106200	50.584368	67.537050
1256.641903	45.157943	67.542055
1255.282984	48.094408	67.547060
1254.535253	45.977270	67.552065
1254.472728	53.273284	67.557070
1253.743577	53.441933	67.562074
1253.638114	46.823999	67.567079
1253.324143	46.427777	67.572084
1252.096954	48.772509	67.577089
1251.520864	48.191831	67.582094
1250.524344	52.878010	67.587098
1249.996492	46.471725	67.592103
1248.709379	48.815665	67.597108
1248.223468	51.749509	67.602113
1248.311450	52.190350	67.607118
1247.351794	58.783418	67.612122
1246.818640	46.952644	67.617127
1245.763015	53.913043	67.622132
1245.103088	50.339365	67.627137
1244.778028	45.432631	67.632142
1244.103264	59.606028	67.637146
1242.963708	38.906747	67.642151
1242.050678	44.568188	67.647156
1241.396043	48.967295	67.652161
1241.119564	47.837191	67.657166
1240.569598	55.236392	67.662170
1240.666817	40.344426	67.667175
1239.817275	46.197883	67.672180
1238.895610	50.367983	67.677185
1238.439449	43.513265	67.682190
1237.240157	46.270440	67.687194
1236.213897	52.033370	67.692199
1235.861673	46.991952	67.697204
1235.036912	48.804787	67.702209
1234.770564	48.390546	67.707214
1234.763126	51.740214	67.712218
1234.074997	42.744395	67.717223
1233.234084	51.681490	67.722228
1232.047279	48.354325	67.727233
1230.552387	52.718481	67.732238
1230.218136	50.203337	67.737242
1229.877506	44.145511	67.742247
1229.193947	46.280339	67.747252
1228.573917	44.109765	67.752257
1228.448925	38.572760	67.757262
1227.868831	50.442554	67.762266
1227.286136	45.648610	67.767271
1226.485233	47.042909	67.772276
1225.773354	46.817834	67.777281
1224.412623	50.144993	67.782286
1223.481817	56.264593	67.787290
1223.403506	46.442827	67.792295
1223.034655	52.999085	67.797300
1222.488724	51.261461	67.802305
1221.832225	52.723007	67.807310
1220.761329	53.420673	67.812314
1219.870523	38.782730	67.817319
1219.451365	44.632370	67.822324
1219.210883	50.750223	67.827329
1218.367949	45.130484	67.832334
1217.002979	52.482910	67.837338
1216.831388	51.168280	67.842343
1216.327837	38.474730	67.847348
1215.814394	57.910507	67.852353
1215.387141	43.012814	67.857358
1213.782908	44.555701	67.862362
1213.399502	44.161107	67.867367
1213.045646	42.021146	67.872372
1212.402318	50.717187	67.877377
1211.855445	47.954644	67.882382
1210.319747	44.758663	67.887386
1210.119717	44.161367	67.892391
1209.968147	41.351673	67.897396
1209.126346	52.911029	67.902401
1208.357423	49.682055	67.907406
1207.025642	51.700905	67.912410
1206.727364	48.477796	67.917415
1206.524655	50.211765	67.922420
1206.013194	63.135950	67.927425
1205.027624	45.376619	67.932430
1204.148616	47.699643	67.937434
1203.469771	50.861512	67.942439
1203.391198	49.918174	67.947444
1202.825178	57.135003	67.952449
1201.925208	45.348097	67.957454
1200.567215	49.695532	67.962458
1200.063035	43.186525	67.967463
1199.857715	50.258704	67.972468
1199.008767	51.789516	67.977473
1198.049964	44.660089	67.982478
1197.264640	51.493298	67.987482
1196.606226	45.793027	67.992487
1196.287047	52.449723	67.997492
1195.846335	52.733593	68.002497
1195.612489	47.995975	68.007502
1195.024560	50.866766	68.012506
1194.172744	49.519790	68.017511
1193.755945	50.149286	68.022516
1192.321002	56.511512	68.027521
1191.820764	45.918082	68.032526
1191.065274	37.909550	68.037530
1190.305312	39.866421	68.042535
1189.044881	43.364694	68.047540
1188.714785	45.980168	68.052545
1188.702696	36.722572	68.057550
1187.448851	51.870194	68.062554
1187.108547	47.741301	68.067559
1186.664084	48.661310	68.072564
1186.103242	47.465428	68.077569
1185.266454	44.338468	68.082574
1183.951626	48.019733	68.087578
1183.640549	44.612117	68.092583
1183.364740	44.453697	68.097588
1182.844099	46.508534	68.102593
1182.415958	47.308517	68.107598
1181.053474	46.624869	68.112602
1180.531320	43.080112	68.117607
1180.153843	50.863444	68.122612
1178.793394	51.839234	68.127617
1178.236562	42.548594	68.132622
1177.865820	52.592502	68.137626
1177.135412	49.444567	68.142631
1176.773260	43.895671	68.147636
1176.218021	47.722398	68.152641
1175.527850	49.011697	68.157646
1174.665385	46.803695	68.162650
1174.163976	48.663803	68.167655
1173.279021	45.548645	68.172660
1172.294949	47.924397	68.177665
1172.117628	39.469922	68.182670
1171.693797	58.449847	68.187674
1170.976436	49.641404	68.192679
1170.104351	41.562843	68.197684
1168.793886	48.476492	68.202689
1168.731238	47.655555	68.207694
1167.682269	48.256718	68.212698
1167.703684	53.145183	68.217703
1166.869768	53.051927	68.222708
1165.683902	52.465142	68.227713
1165.326099	52.979544	68.232718
1165.174880	48.767755	68.237722
1164.107559	42.617266	68.242727
1163.047024	41.836927	68.247732
1162.179688	45.606964	68.252737
1162.368305	49.318173	68.257742
1161.610338	48.997188	68.262746
1160.910461	46.210721	68.267751
1159.900910	43.795813	68.272756
1159.082601	49.334080	68.277761
1158.956851	46.935604	68.282766
1157.942773	46.517951	68.287770
1157.937911	44.697958	68.292775
1156.887267	47.044850	68.297780
1155.870852	50.386489	68.302785
1155.629779	48.132490	68.307790
1154.837147	52.689831	68.312794
1153.699854	49.331711	68.317799
1153.096469	50.832721	68.322804
1152.337288	48.136932	68.327809
1152.198728	48.142109	68.332814
1151.529104	45.608214	68.337818
1151.246193	48.867289	68.342823
1150.947271	55.586040	68.347828
1149.370000	55.310605	68.352833
1148.801841	42.400379	68.357838
1148.615190	48.238631	68.362842
1147.325473	49.949124	68.367847
1146.285563	43.622639	68.372852
1145.984152	49.771447	68.377857
1145.998357	43.772872	68.382862
1145.008290	49.208713	68.387866
1144.088904	44.663081	68.392871
1143.290035	46.775033	68.397876
1142.541258	56.593554	68.402881
1142.509699	44.920463	68.407886
1142.089617	45.544605	68.412890
1140.902556	43.747433	68.417895
1140.127349	49.490680	68.422900
1139.419747	53.051013	68.427905
1139.223545	49.594522	68.432910
1138.529488	47.471371	68.437914
1137.642308	50.005794	68.442919
1136.948183	62.546403	68.447924
1136.318250	54.535719	68.452929
1135.627508	41.199272	68.457934
1134.358884	50.954437	68.462938
1133.695821	50.589182	68.467943
1133.383329	54.695255	68.472948
1133.004623	58.320848	68.477953
1132.867326	51.516936	68.482958
1132.101642	57.513543	68.487962
1130.844626	56.971711	68.492967
1130.554814	45.525595	68.497972
1129.761292	59.213690	68.502977
1129.401107	52.521360	68.507982
1128.318526	57.317421	68.512986
1127.724976	58.633601	68.517991
1126.837207	53.313648	68.522996
1125.959623	49.817914	68.528001
1125.803444	53.495005	68.533006
1125.406661	64.339917	68.538010
1123.921125	43.620587	68.543015
1123.439116	51.363793	68.548020
1123.044757	54.593797	68.553025
1123.050784	50.787301	68.558030
1122.491401	58.882821	68.563034
1121.369159	54.671516	68.568039
1120.284489	50.291155	68.573044
1119.897188	51.745302	68.578049
1119.435925	51.526670	68.583054
1118.200221	51.433538	68.588058
1118.105088	59.877440	68.593063
1117.221738	51.399389	68.598068
1116.202477	53.264097	68.603073
1115.913518	48.318040	68.608078
1115.426231	44.462600	68.613082
1114.771362	50.004069	68.618087
1114.086848	47.347604	68.623092
1112.713802	45.589785	68.628097
1112.199174	42.629115	68.633102
1112.012774	44.395818	68.638106
1111.223326	43.447894	68.643111
1110.582006	42.750910	68.648116
1109.428829	55.256832	68.653121
1108.961331	47.236107	68.658126
1108.343260	54.125550	68.663130
1107.668433	45.815474	68.668135
1107.697243	48.797764	68.673140
1106.744066	51.205341	68.678145
1105.798222	48.475604	68.683150
1105.063314	53.433178	68.688154
1104.392204	50.834811	68.693159
1104.066482	44.594853	68.698164
1103.601919	54.999413	68.703169
1102.783956	54.431749	68.708174
1101.552392	45.377046	68.713178
1101.299079	45.335956	68.718183
1101.376754	44.640590	68.723188
1099.586145	49.773799	68.728193
1099.190600	45.327550	68.733198
1098.590866	49.509252	68.738202
1097.955519	52.281993	68.743207
1098.243669	50.077898	68.748212
1096.817484	47.773421	68.753217
1096.121663	43.049000	68.758222
1095.591402	49.903277	68.763226
1094.307582	43.088466	68.768231
1093.656711	38.375297	68.773236
1093.202107	45.658305	68.778241
1092.823137	43.965132	68.783246
1091.818696	46.471484	68.788250
1091.402863	51.553625	68.793255
1090.675987	44.470168	68.798260
1089.547940	47.378982	68.803265
1089.232439	44.552762	68.808270
1088.725068	41.174426	68.813274
1088.224740	50.538318	68.818279
1088.222475	42.128873	68.823284
1086.674537	43.407567	68.828289
1086.103522	41.533738	68.833294
1085.475980	48.302440	68.838298
1084.584541	50.992724	68.843303
1083.886207	41.403061	68.848308
1082.805877	51.780828	68.853313
1082.437486	40.217528	68.858318
1081.859167	49.792528	68.863322
1081.403861	53.025469	68.868327
1081.320869	45.278366	68.873332
1080.926599	54.717648	68.878337
1079.639695	50.718489	68.883342
1079.264850	50.595190	68.888346
1077.940172	46.750914	68.893351
1077.536120	42.130871	68.898356
1076.526913	49.447272	68.903361
1076.050834	42.590860	68.908366
1076.034733	53.050067	68.913370
1075.277170	48.312539	68.918375
1074.537333	47.586641	68.923380
1073.165026	42.706497	68.928385
1073.413099	40.846353	68.933390
1071.978537	52.941405	68.938394
1070.549127	48.303922	68.943399
1070.956470	41.315974	68.948404
1069.920287	46.488156	68.953409
1070.063230	47.332456	68.958414
1069.380239	46.371837	68.963418
1068.078609	47.806113	68.968423
1067.723316	48.637050	68.973428
1066.715149	50.955370	68.978433
1066.555800	46.657749	68.983438
1065.873775	51.023669	68.988442
1064.860391	47.159643	68.993447
1064.242593	39.356894	68.998452
1063.347538	52.076368	69.003457
1062.911370	41.812639	69.008462
1062.710858	42.152095	69.013466
1061.747673	43.522892	69.018471
1061.334047	45.043915	69.023476
1060.402631	46.840303	69.028481
1059.836352	45.168156	69.033486
1059.009672	47.391851	69.038490
1057.983096	48.465231	69.043495
1057.825327	46.862861	69.048500
1057.104779	46.229974	69.053505
1056.690727	45.713147	69.058510
1055.289843	54.804562	69.063514
1054.447534	46.614752	69.068519
1054.013528	47.412196	69.073524
1053.687477	52.607247	69.078529
1053.374696	46.237980	69.083534
1052.925130	44.266784	69.088538
1051.848807	48.086833	69.093543
1050.888131	41.794173	69.098548
1050.418117	54.336266	69.103553
1050.077022	45.108572	69.108558
1048.855534	43.813085	69.113562
1048.284473	48.916675	69.118567
1048.165947	43.223847	69.123572
1047.369459	50.786443	69.128577
1046.638539	41.276577	69.133582
1045.641068	47.265907	69.138586
1044.793596	50.271546	69.143591
1044.734894	41.885190	69.148596
1044.161658	41.159977	69.153601
1043.121907	49.673657	69.158606
1042.288579	41.378109	69.163610
1041.535970	43.167169	69.168615
1041.461090	43.019742	69.173620
1040.799789	45.495763	69.178625
1039.748126	44.451050	69.183630
1039.092268	43.888400	69.188634
1038.404493	42.335740	69.193639
1037.886239	48.533522	69.198644
1037.287392	49.743255	69.203649
1036.253893	40.062980	69.208654
1035.627569	38.598477	69.213658
1034.830334	41.173562	69.218663
1034.695357	39.631629	69.223668
1034.173968	38.308623	69.228673
1033.845081	41.127568	69.233678
1032.450962	46.721031	69.238682
1031.940094	54.281297	69.243687
1031.716994	36.931449	69.248692
1030.536904	48.348618	69.253697
1030.010331	38.784818	69.258702
1029.245546	40.730693	69.263706
1028.240855	47.251762	69.268711
1028.553207	46.681200	69.273716
1027.058423	50.252797	69.278721
1026.402444	47.605671	69.283726
1025.916278	43.746499	69.288730
1025.474033	49.960475	69.293735
1025.013566	41.367803	69.298740
1023.738346	45.809255	69.303745
1023.372118	39.895177	69.308750
1022.639496	45.680086	69.313754
1022.261131	53.768685	69.318759
1021.547038	44.739074	69.323764
1020.558753	44.794640	69.328769
1020.046836	44.648636	69.333774
1019.635474	45.138274	69.338778
1019.094547	46.455321	69.343783
1018.071787	36.975705	69.348788
1017.080688	40.880238	69.353793
1016.884157	37.762877	69.358798
1016.230071	44.225880	69.363802
1015.107710	43.290380	69.368807
1014.413342	36.601225	69.373812
1013.898560	45.092108	69.378817
1013.374567	40.554978	69.383822
1012.971021	43.123039	69.388826
1012.528517	46.311556	69.393831
1011.710784	44.571561	69.398836
1010.283416	41.792076	69.403841
1009.875851	45.343670	69.408846
1009.888125	47.977885	69.413850
1009.342839	51.392809	69.418855
1008.248107	48.938051	69.423860
1007.230885	45.862552	69.428865
1006.852201	45.499928	69.433870
1006.601710	38.927777	69.438874
1005.343558	43.401833	69.443879
1004.598879	44.122228	69.448884
1004.103210	45.125621	69.453889
1003.316024	45.653173	69.458894
1003.422525	44.880242	69.463898
1002.182595	50.497043	69.468903
1001.514257	38.800794	69.473908
1000.576361	50.600813	69.478913
999.804265	47.700826	69.483918
1000.321577	49.745290	69.488922
998.904317	47.373792	69.493927
998.216331	38.238673	69.498932
997.650595	48.444642	69.503937
997.146554	46.976966	69.508942
995.858034	41.740675	69.513946
994.815430	48.430469	69.518951
995.080729	48.460827	69.523956
994.478394	44.296703	69.528961
993.694719	47.502991	69.533966
993.443365	48.387576	69.538970
992.265550	46.142041	69.543975
991.669426	41.763707	69.548980
990.777013	49.810868	69.553985
990.748296	40.043796	69.558990
989.873944	39.177536	69.563994
988.906128	42.917042	69.568999
988.089098	43.335241	69.574004
987.349732	36.718136	69.579009
987.249047	42.759148	69.584014
986.755358	41.597974	69.589018
985.467873	40.866803	69.594023
985.077469	43.995086	69.599028
984.735442	48.652900	69.604033
983.784280	50.640568	69.609038
982.765972	35.403261	69.614042
981.670613	46.185035	69.619047
981.565748	47.972513	69.624052
980.929309	45.691897	69.629057
980.668365	42.004546	69.634062
980.570151	38.144073	69.639066
979.265560	48.175800	69.644071
978.493331	39.574953	69.649076
977.570142	49.488473	69.654081
976.901196	47.913651	69.659086
976.394201	40.498897	69.664090
975.515982	45.276955	69.669095
975.331699	36.436482	69.674100
974.531800	42.079765	69.679105
974.217354	45.209644	69.684110
973.370996	47.879988	69.689114
972.030192	45.040692	69.694119
972.027041	48.088448	69.699124
971.393744	45.447314	69.704129
970.456281	42.248039	69.709134
969.851816	43.690440	69.714138
969.261345	42.216648	69.719143
969.037184	37.187281	69.724148
968.038712	47.918914	69.729153
967.124805	46.184740	69.734158
966.912089	45.000316	69.739162
966.203732	51.252762	69.744167
964.847386	47.156590	69.749172
964.080157	48.712914	69.754177
963.449955	52.055152	69.759182
963.151867	50.887322	69.764186
962.758991	57.954119	69.769191
962.122981	41.511796	69.774196
961.136384	51.704584	69.779201
960.203125	41.734417	69.784206
960.062103	37.196838	69.789210
959.198305	39.893852	69.794215
959.194707	37.981284	69.799220
957.947244	43.593066	69.804225
957.072199	47.561415	69.809230
957.062568	40.536725	69.814234
956.281499	56.508094	69.819239
955.298589	41.834305	69.824244
953.982120	53.629298	69.829249
953.832668	42.301277	69.834254
953.432825	50.451180	69.839258
952.634413	57.371518	69.844263
952.561271	50.176132	69.849268
951.240292	50.955364	69.854273
950.079781	45.137457	69.859278
950.082616	49.343468	69.864282
949.350393	54.650316	69.869287
949.034929	51.899887	69.874292
947.773859	51.175254	69.879297
947.281942	55.345609	69.884302
946.693043	43.708789	69.889306
946.401411	51.887132	69.894311
945.635144	44.614674	69.899316
944.693634	43.000095	69.904321
943.846479	52.241421	69.909326
943.240147	58.338248	69.914330
942.925259	61.255060	69.919335
942.617322	48.405311	69.924340
941.475179	41.254463	69.929345
940.454118	45.935416	69.934350
940.527388	48.992976	69.939354
939.567696	57.734132	69.944359
939.053051	47.415184	69.949364
937.924135	48.926092	69.954369
937.267776	54.272051	69.959374
936.795919	41.701027	69.964378
935.954942	47.675807	69.969383
935.392694	44.837389	69.974388
934.483533	44.376948	69.979393
934.046508	39.918090	69.984398
933.702037	39.043586	69.989402
932.891336	50.060023	69.994407
932.740625	49.766119	69.999412
931.447997	50.406297	70.004417
930.456528	48.103602	70.009422
930.355094	44.334467	70.014426
930.081719	54.922979	70.019431
928.863721	42.364485	70.024436
927.821161	37.131881	70.029441
927.086054	43.563373	70.034446
927.215663	38.228302	70.039450
926.958519	50.079096	70.044455
925.798411	38.574058	70.049460
925.064551	44.094332	70.054465
924.300594	46.666100	70.059470
923.839677	45.352486	70.064474
922.280893	48.288527	70.069479
922.085094	45.790356	70.074484
921.570607	45.374027	70.079489
921.173934	44.882656	70.084494
920.457814	38.287636	70.089498
919.365552	43.135514	70.094503
919.080813	43.348882	70.099508
918.744219	51.518346	70.104513
917.842088	50.598438	70.109518
917.161135	44.767089	70.114522
916.143620	52.497413	70.119527
915.361039	44.778174	70.124532
914.813895	52.001645	70.129537
914.489289	46.125844	70.134542
914.288095	49.238304	70.139546
912.893996	50.038358	70.144551
912.194059	41.759470	70.149556
911.337181	48.169586	70.154561
911.405687	53.031024	70.159566
910.579403	46.988131	70.164570
909.539259	45.744907	70.169575
908.868044	51.212221	70.174580
908.262110	52.938287	70.179585
907.882486	50.008597	70.184590
907.831527	50.054039	70.189594
906.253506	56.100192	70.194599
905.839297	46.081007	70.199604
905.373485	53.703423	70.204609
904.526185	53.056743	70.209614
903.735193	49.302292	70.214618
903.045469	56.035870	70.219623
902.477693	53.356683	70.224628
902.203791	49.186451	70.229633
900.987621	49.523821	70.234638
900.122018	43.308465	70.239642
899.748683	51.970117	70.244647
899.705679	49.464330	70.249652
898.756859	57.681024	70.254657
897.606883	45.432584	70.259662
896.450664	47.645246	70.264666
896.172758	50.684796	70.269671
895.775851	44.191414	70.274676
895.293880	52.346701	70.279681
894.846943	45.258761	70.284686
894.427775	41.425238	70.289690
893.090685	55.265242	70.294695
892.674944	47.290952	70.299700
892.053516	53.738505	70.304705
891.098879	51.909879	70.309710
890.516428	45.599058	70.314714
889.626623	55.843563	70.319719
889.558182	42.131012	70.324724
889.298620	43.718023	70.329729
887.859568	52.223536	70.334734
887.182136	52.660865	70.339738
886.427758	52.234314	70.344743
886.196492	43.638726	70.349748
885.079833	39.799145	70.354753
884.054454	51.587709	70.359758
883.422099	39.778360	70.364762
882.762982	39.943356	70.369767
882.650697	43.800415	70.374772
882.123133	38.976960	70.379777
881.573565	42.378021	70.384782
881.630469	37.914307	70.389786
880.147178	53.327032	70.394791
879.854166	49.668470	70.399796
879.090701	37.214904	70.404801
877.521314	43.522067	70.409806
877.502533	35.799122	70.414810
876.638737	35.632485	70.419815
876.083514	39.979858	70.424820
875.039547	44.429889	70.429825
874.172350	44.926168	70.434830
873.963608	38.370960	70.439834
873.832398	46.038295	70.444839
873.136116	46.620162	70.449844
872.359282	41.427713	70.454849
871.563954	49.287740	70.459854
870.878046	44.146818	70.464858
870.191411	49.611249	70.469863
869.356998	41.119364	70.474868
868.707072	54.643924	70.479873
868.286920	50.059031	70.484878
867.979199	49.639266	70.489882
866.444235	45.310838	70.494887
865.774303	45.212835	70.499892
865.185242	48.480144	70.504897
864.622839	53.214783	70.509902
864.681988	46.952356	70.514906
864.137702	51.687050	70.519911
863.345252	46.790155	70.524916
861.976983	43.988359	70.529921
861.294084	47.141878	70.534926
860.987997	42.091818	70.539930
859.633698	44.550376	70.544935
859.159626	43.619133	70.549940
858.708432	43.924563	70.554945
858.156005	40.980270	70.559950
857.964925	35.703683	70.564954
857.094911	47.435242	70.569959
856.039025	44.755197	70.574964
855.305541	41.925200	70.579969
854.666654	46.366639	70.584974
854.901584	44.044948	70.589978
853.972551	54.109079	70.594983
852.954108	47.364545	70.599988
852.228171	50.424786	70.604993
851.747415	42.424538	70.609998
851.354461	38.867568	70.615002
850.041947	44.930226	70.620007
849.426020	39.481682	70.625012
849.179090	42.620921	70.630017
848.585013	48.016213	70.635022
847.681133	34.906613	70.640026
847.121566	44.763780	70.645031
846.765008	50.062736	70.650036
845.853899	48.322976	70.655041
844.790525	47.350967	70.660046
844.181066	45.087855	70.665050
843.355282	46.806981	70.670055
843.207998	41.114361	70.675060
842.640554	39.103776	70.680065
841.443460	44.146852	70.685070
840.749512	36.635074	70.690074
840.039226	44.466720	70.695079
839.901446	37.657401	70.700084
839.315777	45.811894	70.705089
838.995290	51.046254	70.710094
838.156827	30.322835	70.715098
837.199423	37.305931	70.720103
836.563623	36.522781	70.725108
835.039261	43.902974	70.730113
834.274669	40.774379	70.735118
834.412424	34.425077	70.740122
833.284977	48.226806	70.745127
833.450775	43.249072	70.750132
833.074057	45.975171	70.755137
831.587927	44.324038	70.760142
831.132816	39.966181	70.765146
830.001612	44.118942	70.770151
829.734182	43.511499	70.775156
829.281713	44.009771	70.780161
828.934515	50.630606	70.785166
827.715440	45.578648	70.790170
826.768015	48.150277	70.795175
826.422378	45.974998	70.800180
825.867942	44.132705	70.805185
825.235356	47.473784	70.810190
824.868848	41.355714	70.815194
823.619708	43.594175	70.820199
823.180018	44.790879	70.825204
822.712083	38.972010	70.830209
821.869870	46.339175	70.835214
821.217570	40.701877	70.840218
820.362849	46.268519	70.845223
819.880681	47.620913	70.850228
819.434005	39.219330	70.855233
819.102618	49.434105	70.860238
818.255801	44.810597	70.865242
817.229916	39.753183	70.870247
816.935126	42.404857	70.875252
815.909520	41.684531	70.880257
814.725773	44.961736	70.885262
814.374492	36.164494	70.890266
813.917858	40.697868	70.895271
813.304740	35.850398	70.900276
813.253387	37.980400	70.905281
811.876706	43.032532	70.910286
811.550223	49.297732	70.915290
810.884461	48.907327	70.920295
809.972628	38.402250	70.925300
808.827681	41.049554	70.930305
808.250856	48.107199	70.935310
807.905178	39.852915	70.940314
806.907165	45.843949	70.945319
806.495776	39.871720	70.950324
806.580905	38.151972	70.955329
806.049784	43.081770	70.960334
805.243014	44.741989	70.965338
804.288927	56.299679	70.970343
803.453570	43.028752	70.975348
802.611362	39.339541	70.980353
801.770986	38.995231	70.985358
801.543135	39.074921	70.990362
801.217429	49.019130	70.995367
800.201073	39.570456	71.000372
799.469447	39.582498	71.005377
798.086902	43.380048	71.010382
798.252621	33.565093	71.015386
797.605831	49.563975	71.020391
797.162762	43.988336	71.025396
796.572601	49.504533	71.030401
795.782223	44.336524	71.035406
794.860539	40.586721	71.040410
793.729300	52.058707	71.045415
792.993968	45.015448	71.050420
792.458555	44.116823	71.055425
791.860612	44.147807	71.060430
791.653367	44.001743	71.065434
791.314491	44.641211	71.070439
789.970363	39.969482	71.075444
789.232919	46.206002	71.080449
788.648443	49.825408	71.085454
788.803568	49.451886	71.090458
787.900202	43.830758	71.095463
786.700862	44.220533	71.100468
786.149559	42.727821	71.105473
785.391350	50.518342	71.110478
785.482340	39.099430	71.115482
784.538824	45.258359	71.120487
783.413695	48.778544	71.125492
783.298571	51.317344	71.130497
782.062554	53.017149	71.135502
781.348392	44.140759	71.140506
780.145739	45.111730	71.145511
779.649448	44.293638	71.150516
779.536717	39.106657	71.155521
778.903142	44.596740	71.160526
778.836657	39.820235	71.165530
778.273609	44.734584	71.170535
777.235970	55.501762	71.175540
776.570989	45.511349	71.180545
775.548951	49.954484	71.185550
775.058337	42.322235	71.190554
774.222379	51.652440	71.195559
773.315435	41.346655	71.200564
773.212548	33.801934	71.205569
772.538820	47.949477	71.210574
772.430197	34.616446	71.215578
771.238671	48.505337	71.220583
770.142678	47.266580	71.225588
769.651477	37.892555	71.230593
768.563165	54.233505	71.235598
767.986176	34.381849	71.240602
767.428630	45.250325	71.245607
767.013262	56.306417	71.250612
766.536874	49.199464	71.255617
766.029663	54.926445	71.260622
765.433879	46.751320	71.265626
764.638149	59.314069	71.270631
764.147540	46.814974	71.275636
763.471138	56.054302	71.280641
761.551189	49.454351	71.285646
761.369729	35.956176	71.290650
760.773889	45.749298	71.295655
760.302938	55.689182	71.300660
760.004736	52.712799	71.305665
759.382247	55.103655	71.310670
759.108720	47.161866	71.315674
757.554062	49.153089	71.320679
757.054113	46.891362	71.325684
756.667552	44.180761	71.330689
756.191283	57.047187	71.335694
755.039730	44.883935	71.340698
754.383021	53.619784	71.345703
754.093084	52.292687	71.350708
753.604474	52.897020	71.355713
752.467521	54.997867	71.360718
751.390649	49.899467	71.365722
751.014985	49.037031	71.370727
750.552544	46.846244	71.375732
750.163994	40.333298	71.380737
749.522146	48.136649	71.385742
748.400730	42.743925	71.390746
747.649193	45.816061	71.395751
747.219399	48.874134	71.400756
747.162237	45.595951	71.405761
745.795668	48.966065	71.410766
745.478356	41.596619	71.415770
744.794085	44.444481	71.420775
744.552004	47.050026	71.425780
743.317092	47.481035	71.430785
742.484408	49.821851	71.435790
742.089019	37.127652	71.440794
741.500801	43.913317	71.445799
740.140538	44.390667	71.450804
739.612227	39.729196	71.455809
739.058408	54.012511	71.460814
738.463067	41.604389	71.465818
738.102143	49.740519	71.470823
737.587624	52.665482	71.475828
736.766941	38.311337	71.480833
735.553029	43.845576	71.485838
735.407150	38.655593	71.490842
734.945477	41.072977	71.495847
734.699394	43.729336	71.500852
733.110796	38.106007	71.505857
732.298228	43.740433	71.510862
732.079498	40.590582	71.515866
731.843896	40.000587	71.520871
731.027134	45.643626	71.525876
730.044642	34.559002	71.530881
729.285835	46.430586	71.535886
728.965982	40.463213	71.540890
728.356612	47.995358	71.545895
727.417872	40.536196	71.550900
726.670815	40.252093	71.555905
725.710477	42.125726	71.560910
725.180245	45.105878	71.565914
725.040742	43.136469	71.570919
724.237845	32.485267	71.575924
723.428393	37.722864	71.580929
722.859796	41.414549	71.585934
722.354004	39.950758	71.590938
721.711746	48.204551	71.595943
720.809354	45.807307	71.600948
720.190403	34.519495	71.605953
719.611155	49.298186	71.610958
719.109106	38.235859	71.615962
718.271100	41.571876	71.620967
717.500603	43.403516	71.625972
716.929629	34.559458	71.630977
716.336718	45.124141	71.635982
715.598666	37.216943	71.640986
714.371026	37.712236	71.645991
713.621309	44.516885	71.650996
713.554021	39.708945	71.656001
712.728657	41.943910	71.661006
712.572057	37.345076	71.666010
712.154320	36.415251	71.671015
710.430991	40.527766	71.676020
710.241662	27.213314	71.681025
709.431450	36.995395	71.686030
708.969618	35.092257	71.691034
708.781001	33.808594	71.696039
707.555761	41.515316	71.701044
706.740720	39.492696	71.706049
706.184139	38.971504	71.711054
705.856494	34.741033	71.716058
705.236775	44.239446	71.721063
703.944407	37.563595	71.726068
703.294871	41.745173	71.731073
703.140596	46.099264	71.736078
702.467728	38.913098	71.741082
702.195917	39.924746	71.746087
701.282099	52.737445	71.751092
700.454466	38.473313	71.756097
699.376466	40.788662	71.761102
699.189667	35.962121	71.766106
698.258252	49.243596	71.771111
697.143507	40.667157	71.776116
697.163351	34.127283	71.781121
696.586580	36.579780	71.786126
696.109916	39.909553	71.791130
694.885314	41.793727	71.796135
694.036951	49.334450	71.801140
693.933410	40.200328	71.806145
693.382051	46.061969	71.811150
692.816112	38.151342	71.816154
691.881191	41.194509	71.821159
690.867364	43.498078	71.826164
690.646777	34.633865	71.831169
689.898005	46.108227	71.836174
688.894514	45.634389	71.841178
688.197263	45.398599	71.846183
687.418557	50.536600	71.851188
687.523684	45.128760	71.856193
686.591547	45.844606	71.861198
685.923901	44.350129	71.866202
684.970138	47.047598	71.871207
684.306276	43.367725	71.876212
683.962490	39.209885	71.881217
683.620264	47.967248	71.886222
682.846480	44.471987	71.891226
682.173662	39.898830	71.896231
681.291983	43.732571	71.901236
680.361773	43.667736	71.906241
679.264686	42.761933	71.911246
678.796556	33.150701	71.916250
678.088137	37.111065	71.921255
677.876216	39.184499	71.926260
677.520877	30.196542	71.931265
677.086741	41.696337	71.936270
676.324555	41.496145	71.941274
675.873544	39.730886	71.946279
674.659016	40.071583	71.951284
673.742281	32.106198	71.956289
672.786453	35.539769	71.961294
672.161891	41.050418	71.966298
671.991622	49.817400	71.971303
670.865643	44.281409	71.976308
670.920960	34.566293	71.981313
670.377091	36.664623	71.986318
669.339990	40.888918	71.991322
668.569308	37.048938	71.996327
668.035034	34.429967	72.001332
667.742067	31.634269	72.006337
666.828072	34.849502	72.011342
666.136313	34.143064	72.016346
665.684091	34.412374	72.021351
664.724713	34.203337	72.026356
663.547885	39.447830	72.031361
663.107098	45.316187	72.036366
662.883493	35.209932	72.041370
662.330361	34.335280	72.046375
661.471193	40.711865	72.051380
660.481977	37.263385	72.056385
659.763376	40.199238	72.061390
659.291309	38.400880	72.066394
659.013890	36.753506	72.071399
658.370620	40.291420	72.076404
657.975013	36.176012	72.081409
656.426290	44.096049	72.086414
655.958305	35.001082	72.091418
655.696510	30.110821	72.096423
654.758577	41.870994	72.101428
653.992385	30.278841	72.106433
653.075497	42.246187	72.111438
652.924194	45.538774	72.116442
652.450970	39.090084	72.121447
651.395062	40.289352	72.126452
650.671980	37.528661	72.131457
650.255108	42.825714	72.136462
649.715537	35.211353	72.141466
649.172242	38.950021	72.146471
648.037796	41.477145	72.151476
647.523135	32.468727	72.156481
646.291377	35.653539	72.161486
646.560616	30.459155	72.166490
645.869387	31.319251	72.171495
644.562337	28.410333	72.176500
643.981486	34.328338	72.181505
643.323029	38.689466	72.186510
642.928239	29.527890	72.191514
642.494858	34.944605	72.196519
641.714100	36.256989	72.201524
640.898368	35.096558	72.206529
640.288694	38.476356	72.211534
640.191397	33.035311	72.216538
638.792150	41.336298	72.221543
637.966832	40.328684	72.226548
637.553603	34.925976	72.231553
636.932829	38.501482	72.236558
636.405812	40.144190	72.241562
636.039914	36.510774	72.246567
634.540236	47.101738	72.251572
634.245128	31.075177	72.256577
633.351210	32.106966	72.261582
633.256327	32.659644	72.266586
632.769853	39.694314	72.271591
631.664867	49.594800	72.276596
631.266270	38.041111	72.281601
630.822187	46.451601	72.286606
629.848051	38.661839	72.291610
628.916080	35.243031	72.296615
628.261375	40.274138	72.301620
627.764910	37.948678	72.306625
626.302863	38.976362	72.311630
626.111880	39.723521	72.316634
625.385977	33.354047	72.321639
624.728169	38.444103	72.326644
624.081252	31.135098	72.331649
623.687927	45.703517	72.336654
623.028700	45.396488	72.341658
623.122938	38.346137	72.346663
622.027416	31.907760	72.351668
621.392677	28.750251	72.356673
620.869140	32.103056	72.361678
619.572289	28.649666	72.366682
618.817117	33.791137	72.371687
618.059152	31.433512	72.376692
618.032056	28.162819	72.381697
617.370397	31.331669	72.386702
616.741406	32.995007	72.391706
615.749986	36.478893	72.396711
615.012430	31.271880	72.401716
615.019357	20.660383	72.406721
613.977809	29.216645	72.411726
613.065443	29.979246	72.416730
612.153073	30.434760	72.421735
611.557792	31.929306	72.426740
611.651937	29.272542	72.431745
610.664066	31.120518	72.436750
609.735624	41.155350	72.441754
609.489181	33.766287	72.446759
608.403987	40.180024	72.451764
608.281225	40.555516	72.456769
607.149304	24.300913	72.461774
606.247407	40.923715	72.466778
606.050954	36.568152	72.471783
604.960791	36.476267	72.476788
604.874933	37.043977	72.481793
604.020626	42.582942	72.486798
603.072538	45.142091	72.491802
602.750692	27.032082	72.496807
601.852425	42.688793	72.501812
601.619846	40.271943	72.506817
600.337642	40.157700	72.511822
599.538079	39.701045	72.516826
599.447950	30.989355	72.521831
598.706399	31.536387	72.526836
598.254811	32.713438	72.531841
596.959491	35.388917	72.536846
596.176200	30.636561	72.541850
595.809835	25.827378	72.546855
595.211847	35.847035	72.551860
595.327004	39.355268	72.556865
594.455324	31.100755	72.561870
593.243083	32.516677	72.566874
592.996832	37.409124	72.571879
592.006600	36.483061	72.576884
591.815530	25.121190	72.581889
590.876145	29.221785	72.586894
589.949274	34.701738	72.591898
589.645006	28.892366	72.596903
588.219698	26.087013	72.601908
587.710283	29.006372	72.606913
586.909936	27.010863	72.611918
586.477520	32.376890	72.616922
586.577046	29.422379	72.621927
586.214999	32.244652	72.626932
585.518551	28.429471	72.631937
583.907429	31.954410	72.636942
583.014194	39.648081	72.641946
583.175092	33.069838	72.646951
581.619846	34.660578	72.651956
581.401540	28.740168	72.656961
580.838591	34.686292	72.661966
579.806607	36.206721	72.666970
579.387848	23.717877	72.671975
579.104635	37.951648	72.676980
578.348861	27.308996	72.681985
577.290094	41.704465	72.686990
577.002519	31.934037	72.691994
576.340826	36.670308	72.696999
575.488132	41.339049	72.702004
574.574038	33.046415	72.707009
573.932545	30.577268	72.712014
573.448890	35.351715	72.717018
573.374146	28.103363	72.722023
572.601578	30.967949	72.727028
571.297035	24.838941	72.732033
570.837891	41.507062	72.737038
570.360204	37.252974	72.742042
569.736321	30.625258	72.747047
568.676752	36.189526	72.752052
568.033977	30.309874	72.757057
567.247544	36.298238	72.762062
566.759934	39.779885	72.767066
566.530224	35.255955	72.772071
566.007855	35.316253	72.777076
565.269154	41.801281	72.782081
564.478534	43.062080	72.787086
563.921462	36.568566	72.792090
562.842802	33.504494	72.797095
561.695668	36.322345	72.802100
561.475257	41.585739	72.807105
560.767077	37.532584	72.812110
560.746627	40.439217	72.817114
560.297625	31.174056	72.822119
558.859144	37.836610	72.827124
558.322175	32.569978	72.832129
557.766369	29.733278	72.837134
557.251206	37.636104	72.842138
556.809169	40.653259	72.847143
555.423498	44.081558	72.852148
555.122981	30.670926	72.857153
554.731923	40.745916	72.862158
553.422239	37.221721	72.867162
552.629332	41.626815	72.872167
552.054964	33.995937	72.877172
551.734334	37.570151	72.882177
551.452108	36.954604	72.887182
550.892206	37.141723	72.892186
550.191531	40.584093	72.897191
549.115063	50.074331	72.902196
548.718287	43.762550	72.907201
547.517615	42.987020	72.912206
546.325147	43.615269	72.917210
546.305083	41.197533	72.922215
545.645788	41.751005	72.927220
545.377275	42.227651	72.932225
544.677042	42.301849	72.937230
544.052722	41.376254	72.942234
543.421539	39.202170	72.947239
542.380893	41.963493	72.952244
542.193696	31.889309	72.957249
541.245142	35.815837	72.962254
540.403122	38.387610	72.967258
540.015473	43.906620	72.972263
539.270315	40.654364	72.977268
538.264171	39.545128	72.982273
537.272713	34.351637	72.987278
536.545879	35.088383	72.992282
536.571054	36.197958	72.997287
535.771928	36.641582	73.002292
535.154439	42.527586	73.007297
535.207520	37.189064	73.012302
534.508214	35.437551	73.017306
533.302829	34.799405	73.022311
532.427371	36.591031	73.027316
532.205102	40.626788	73.032321
531.203811	42.669700	73.037326
529.764820	44.919445	73.042330
529.600361	37.531737	73.047335
529.164656	44.233652	73.052340
528.681619	44.561541	73.057345
528.487780	36.860728	73.062350
527.951025	41.292587	73.067354
527.101434	34.462382	73.072359
526.366331	35.901164	73.077364
525.369214	34.563029	73.082369
524.492706	46.359266	73.087374
524.017145	38.111101	73.092378
523.657383	32.120993	73.097383
522.475487	39.388896	73.102388
521.452705	34.872579	73.107393
520.977634	38.747979	73.112398
520.321851	37.337544	73.117402
520.437291	37.609857	73.122407
519.712127	37.528866	73.127412
519.451504	30.127642	73.132417
518.220525	39.823948	73.137422
517.271994	43.990859	73.142426
516.855436	39.402244	73.147431
515.879952	41.197988	73.152436
515.217531	37.340673	73.157441
514.480861	36.408677	73.162446
513.863221	34.601335	73.167450
514.226995	34.090613	73.172455
512.749878	32.778679	73.177460
511.900284	28.795159	73.182465
511.266471	36.082037	73.187470
510.440392	42.591120	73.192474
510.477740	33.446303	73.197479
510.003867	44.066375	73.202484
508.582690	34.847810	73.207489
508.126931	39.719713	73.212494
507.194473	40.342100	73.217498
507.503434	30.960097	73.222503
506.173436	37.859850	73.227508
505.395553	32.754106	73.232513
504.832095	39.032672	73.237518
504.178154	41.347236	73.242522
503.647050	39.739397	73.247527
502.669172	40.130765	73.252532
502.291573	44.847180	73.257537
501.259249	40.185668	73.262542
500.650740	35.537585	73.267546
500.597093	36.536725	73.272551
499.131025	39.543049	73.277556
498.722796	34.771442	73.282561
498.105608	37.343377	73.287566
497.333141	41.918649	73.292570
497.549737	39.757188	73.297575
496.592873	47.559664	73.302580
495.470667	43.703773	73.307585
494.997900	42.586041	73.312590
494.377192	36.212384	73.317594
493.955836	31.585915	73.322599
492.381147	25.108510	73.327604
491.816117	29.653365	73.332609
491.756781	35.100722	73.337614
491.637112	41.996363	73.342618
490.582627	28.596529	73.347623
489.335851	35.702273	73.352628
488.632567	32.865198	73.357633
488.429627	34.684479	73.362638
487.857598	34.913549	73.367642
487.541952	36.251646	73.372647
486.247925	42.371996	73.377652
485.482330	33.560549	73.382657
484.894401	33.155275	73.387662
484.328648	33.531288	73.392666
484.072673	33.787117	73.397671
482.967875	39.658343	73.402676
482.224613	34.138932	73.407681
481.815998	37.561261	73.412686
481.437448	41.536171	73.417690
480.395032	32.913862	73.422695
479.128833	39.839397	73.427700
478.790964	32.304186	73.432705
478.895750	31.650746	73.437710
477.889004	32.457963	73.442714
477.155656	27.852198	73.447719
475.904752	37.502189	73.452724
475.593199	29.780112	73.457729
475.225417	35.611093	73.462734
474.848143	32.694078	73.467738
474.167683	30.380827	73.472743
472.941230	30.804929	73.477748
472.457860	26.086465	73.482753
472.064547	33.343579	73.487758
470.982844	35.981695	73.492762
470.311849	35.412641	73.497767
469.696946	35.154878	73.502772
469.359637	37.560048	73.507777
468.775409	30.022452	73.512782
467.722527	37.372460	73.517786
467.173304	29.170089	73.522791
466.293638	31.408474	73.527796
465.922864	31.200057	73.532801
465.679133	24.991536	73.537806
464.757228	30.363292	73.542810
464.098046	26.226766	73.547815
463.502113	32.435111	73.552820
462.933190	31.293995	73.557825
461.863769	39.099181	73.562830
460.865306	38.585849	73.567834
460.682717	32.265407	73.572839
460.332812	42.538200	73.577844
459.146998	33.252878	73.582849
458.487650	29.400970	73.587854
457.618366	33.964810	73.592858
457.359620	29.963733	73.597863
456.975765	27.438615	73.602868
456.002939	27.795577	73.607873
454.986836	25.309727	73.612878
454.544948	33.947979	73.617882
453.946880	34.606228	73.622887
453.428317	31.892627	73.627892
452.579155	36.844181	73.632897
451.542215	29.339169	73.637902
450.955769	35.532866	73.642906
450.526630	35.468654	73.647911
450.201646	35.637237	73.652916
449.587521	32.861070	73.657921
449.228550	33.615312	73.662926
448.014939	41.505600	73.667930
447.864365	33.917378	73.672935
446.966282	36.261548	73.677940
445.721575	39.574144	73.682945
445.111663	38.950813	73.687950
444.481576	35.973314	73.692954
444.719337	32.964723	73.697959
443.653379	40.266058	73.702964
442.743248	37.448252	73.707969
442.176313	43.835571	73.712974
441.376605	39.944956	73.717978
441.003068	28.907253	73.722983
440.097132	35.813687	73.727988
439.295509	38.373815	73.732993
438.669387	30.705649	73.737998
437.679096	35.354172	73.743002
437.947455	34.151679	73.748007
436.914533	34.823267	73.753012
436.191628	31.999036	73.758017
435.683033	31.126253	73.763022
434.855857	40.956257	73.768026
434.404207	28.325062	73.773031
433.114754	48.500398	73.778036
432.423205	36.894328	73.783041
432.036966	30.678259	73.788046
431.284071	36.708254	73.793050
431.202119	28.753824	73.798055
430.556199	34.425639	73.803060
429.405331	31.434762	73.808065
428.823384	28.351918	73.813070
428.312097	31.911836	73.818074
427.899064	24.711208	73.823079
426.782912	39.325322	73.828084
425.854696	31.120015	73.833089
425.465927	35.343372	73.838094
424.735723	33.854526	73.843098
424.647800	26.923034	73.848103
423.845121	28.779175	73.853108
422.621473	29.981184	73.858113
422.218767	38.468654	73.863118
421.627834	41.650273	73.868122
421.230099	39.398309	73.873127
420.521282	45.357602	73.878132
419.565900	42.874378	73.883137
418.870213	36.656867	73.888142
418.363552	45.614102	73.893146
417.739467	37.062219	73.898151
416.812523	35.993909	73.903156
415.899640	31.454051	73.908161
415.686803	30.731496	73.913166
415.231750	41.799102	73.918170
414.853018	39.039833	73.923175
413.490563	41.896196	73.928180
413.005770	40.867766	73.933185
412.384355	39.699337	73.938190
411.701728	39.911845	73.943194
411.212872	38.783855	73.948199
410.297138	39.732191	73.953204
409.325254	38.892624	73.958209
408.931656	39.406896	73.963214
408.649755	46.512299	73.968218
407.961136	36.717472	73.973223
407.170822	40.989909	73.978228
406.050249	38.896161	73.983233
405.978969	41.123910	73.988238
405.296272	45.013190	73.993242
404.743691	39.627291	73.998247
403.753768	39.028828	74.003252
402.903578	35.302391	74.008257
402.654975	37.732228	74.013262
401.980168	46.867087	74.018266
401.189468	45.342824	74.023271
400.521146	44.499391	74.028276
399.812938	41.631202	74.033281
399.588530	39.201914	74.038286
398.133912	37.532104	74.043290
397.488951	38.401278	74.048295
396.859496	42.754301	74.053300
396.391413	48.428408	74.058305
396.044393	33.166281	74.063310
395.393832	41.406902	74.068314
394.786445	33.207802	74.073319
393.715874	34.468054	74.078324
393.127542	28.716467	74.083329
393.080980	34.443455	74.088334
392.154259	29.060894	74.093338
391.128882	34.763796	74.098343
390.361536	36.462713	74.103348
389.859522	34.168628	74.108353
389.600142	29.354556	74.113358
388.299104	37.068795	74.118362
387.703591	31.949586	74.123367
387.198121	31.851885	74.128372
386.609997	37.537877	74.133377
386.260370	36.049733	74.138382
385.432393	36.042826	74.143386
384.481228	29.547022	74.148391
383.967262	28.528727	74.153396
383.145900	38.906389	74.158401
383.207287	27.339847	74.163406
382.108335	29.805289	74.168410
381.242386	30.688654	74.173415
380.687012	36.231672	74.178420
380.118251	32.521349	74.183425
379.539211	28.974621	74.188430
378.236795	36.963423	74.193434
377.695916	22.969198	74.198439
377.328633	34.130696	74.203444
377.029855	28.031086	74.208449
376.583197	40.978061	74.213454
375.130563	41.567259	74.218458
374.854956	23.806212	74.223463
374.355568	38.309497	74.228468
373.275754	37.709474	74.233473
372.305736	31.302161	74.238478
371.593242	38.473066	74.243482
371.486722	29.740529	74.248487
371.193203	33.668502	74.253492
370.389939	40.956010	74.258497
369.535572	30.317285	74.263502
368.527901	40.857134	74.268506
368.003319	35.125807	74.273511
367.491233	37.593301	74.278516
367.059913	42.909022	74.283521
366.612795	38.610648	74.288526
365.520885	39.233154	74.293530
365.241892	41.555313	74.298535
363.995334	40.681123	74.303540
363.173093	42.417477	74.308545
363.000538	30.522366	74.313550
362.498311	44.241452	74.318554
362.033513	46.039304	74.323559
360.932254	35.185537	74.328564
360.214099	37.679664	74.333569
359.513206	32.645622	74.338574
358.654700	48.905756	74.343578
357.695552	37.710678	74.348583
357.191177	38.171313	74.353588
356.503858	35.222978	74.358593
356.372473	22.763088	74.363598
355.967164	46.659825	74.368602
355.679927	35.329466	74.373607
354.393018	24.905397	74.378612
353.615597	34.888313	74.383617
353.148929	34.098744	74.388622
352.417481	41.370788	74.393626
351.709872	31.953027	74.398631
350.793800	34.685536	74.403636
350.451228	34.814511	74.408641
349.800707	35.062575	74.413646
348.395060	39.436925	74.418650
347.430135	30.819535	74.423655
347.285618	41.637746	74.428660
346.200077	43.225818	74.433665
346.260506	31.488926	74.438670
346.032398	42.315148	74.443674
345.732692	28.714567	74.448679
345.415561	32.527383	74.453684
344.356544	32.308253	74.458689
343.143485	26.330213	74.463694
341.886718	36.829468	74.468698
341.491075	31.841793	74.473703
340.917605	42.041192	74.478708
340.549224	34.916601	74.483713
340.021463	32.523521	74.488718
338.315138	35.296739	74.493722
337.754918	40.040508	74.498727
337.105537	33.817448	74.503732
336.529717	40.054329	74.508737
336.700610	32.204984	74.513742
335.866454	33.890097	74.518746
336.007861	28.020559	74.523751
334.965350	38.993066	74.528756
333.764772	33.944410	74.533761
333.571470	26.726269	74.538766
332.079339	32.163801	74.543770
331.756562	35.260786	74.548775
331.010425	38.922933	74.553780
330.454792	43.332779	74.558785
329.986513	27.742529	74.563790
329.000377	40.022138	74.568794
328.483058	38.552477	74.573799
327.927994	34.889943	74.578804
327.019723	42.201768	74.583809
326.809866	30.065572	74.588814
325.548501	31.658125	74.593818
324.939073	33.661150	74.598823
324.467867	31.195620	74.603828
323.880996	32.411273	74.608833
323.717697	32.394663	74.613838
322.309536	29.818549	74.618842
321.835119	29.501204	74.623847
321.480353	38.080713	74.628852
320.409301	39.464609	74.633857
320.302284	27.520383	74.638862
319.265624	38.755161	74.643866
318.488117	27.437399	74.648871
318.014492	33.316125	74.653876
317.398973	38.168841	74.658881
316.798972	31.871406	74.663886
315.864806	35.652617	74.668890
315.304494	33.905344	74.673895
314.290368	41.213603	74.678900
314.173905	37.811010	74.683905
313.688309	37.933713	74.688910
312.315668	37.673217	74.693914
311.876783	32.506652	74.698919
311.724997	28.061757	74.703924
310.788689	34.489493	74.708929
309.842786	31.870864	74.713934
308.853119	44.053588	74.718938
308.543909	37.409488	74.723943
308.086185	33.841978	74.728948
307.665290	36.098464	74.733953
306.712158	29.374085	74.738958
305.721300	30.870547	74.743962
305.352633	37.291384	74.748967
305.217097	38.403632	74.753972
303.959830	38.837796	74.758977
303.314308	33.377062	74.763982
302.691188	44.849240	74.768986
301.833073	28.839920	74.773991
301.443728	29.372812	74.778996
300.742510	32.410721	74.784001
300.510747	25.271409	74.789006
299.290025	36.980208	74.794010
298.962698	38.075201	74.799015
298.389947	37.443153	74.804020
297.158820	43.276067	74.809025
296.677779	31.594883	74.814030
295.383041	39.309245	74.819034
295.397238	36.299102	74.824039
295.097046	29.507023	74.829044
294.746531	44.725670	74.834049
293.741270	38.941748	74.839054
292.620646	42.677954	74.844058
292.443647	37.948844	74.849063
291.644229	34.175048	74.854068
290.571179	39.503661	74.859073
290.008907	29.133035	74.864078
289.631025	42.024406	74.869082
289.235668	30.045529	74.874087
288.654357	29.112205	74.879092
286.939205	39.277561	74.884097
286.624714	28.340289	74.889102
285.891642	36.406382	74.894106
285.594697	29.855707	74.899111
285.594694	36.805426	74.904116
284.102096	41.161539	74.909121
283.754229	39.564161	74.914126
282.783357	43.868745	74.919130
282.527086	31.056868	74.924135
281.664732	33.334945	74.929140
280.441129	35.809931	74.934145
280.218189	39.732125	74.939150
279.696849	43.611524	74.944154
279.382303	38.232609	74.949159
278.371692	42.134292	74.954164
277.175368	46.312135	74.959169
276.972808	35.889722	74.964174
276.339975	40.718174	74.969178
275.956958	36.724598	74.974183
275.024487	32.651920	74.979188
274.205390	42.130046	74.984193
273.850426	47.142175	74.989198
273.068767	45.149835	74.994202
272.141431	45.836123	74.999207
271.073373	43.781564	75.004212
270.347633	37.947766	75.009217
270.225177	30.515000	75.014222
270.067239	47.159103	75.019226
269.450803	33.600191	75.024231
269.225761	43.777764	75.029236
267.687134	54.390086	75.034241
267.475230	37.765564	75.039246
266.721606	42.756817	75.044250
265.548672	38.250516	75.049255
264.820819	35.814378	75.054260
264.437490	38.909114	75.059265
264.289483	32.972743	75.064270
263.340029	39.806531	75.069274
262.639693	35.320668	75.074279
262.077663	40.283819	75.079284
261.068531	38.405073	75.084289
260.159604	41.617923	75.089294
259.375046	44.593154	75.094298
258.473762	42.977354	75.099303
258.464417	42.742527	75.104308
257.940992	39.451136	75.109313
257.675586	42.621971	75.114318
256.923706	42.627701	75.119322
255.916842	39.443251	75.124327
255.818023	35.840281	75.129332
254.443535	35.375657	75.134337
253.654349	30.642543	75.139342
253.077715	41.572704	75.144346
252.290155	40.962482	75.149351
252.167721	34.638461	75.154356
250.956646	40.101259	75.159361
249.979988	33.075024	75.164366
249.631416	41.792806	75.169370
249.060928	41.345101	75.174375
248.874524	36.977191	75.179380
248.385909	48.365926	75.184385
247.341071	37.017030	75.189390
246.365060	42.838199	75.194394
245.596533	32.044278	75.199399
245.591515	41.618117	75.204404
244.772180	42.358920	75.209409
244.242656	36.018234	75.214414
242.759079	44.084694	75.219418
242.177131	40.020620	75.224423
242.230312	34.086079	75.229428
241.645250	50.463546	75.234433
241.060911	33.184100	75.239438
239.808107	42.471716	75.244442
239.285666	41.304110	75.249447
238.982214	39.279544	75.254452
237.972626	45.031474	75.259457
236.788649	43.914896	75.264462
236.312642	51.650376	75.269466
235.800333	46.376410	75.274471
235.409510	38.623745	75.279476
234.951405	46.030910	75.284481
234.574003	32.223812	75.289486
232.871754	40.643525	75.294490
232.310098	45.826865	75.299495
232.030986	44.638865	75.304500
231.645345	47.334946	75.309505
231.293296	43.248834	75.314510
230.035454	45.839433	75.319514
229.539555	54.228417	75.324519
228.856978	50.470916	75.329524
228.318832	50.209502	75.334529
227.507634	38.744384	75.339534
226.612054	44.294416	75.344538
225.924642	44.191606	75.349543
225.709878	45.614656	75.354548
224.630314	45.865232	75.359553
223.705087	38.613489	75.364558
223.254350	45.329038	75.369562
222.818105	47.252261	75.374567
222.292479	48.900297	75.379572
222.121890	43.872479	75.384577
220.922784	51.405084	75.389582
220.037726	50.046625	75.394586
219.242981	53.811062	75.399591
218.963065	42.645248	75.404596
218.449356	48.711633	75.409601
217.476270	34.465887	75.414606
216.771627	45.607456	75.419610
216.280730	44.387474	75.424615
216.025127	39.858148	75.429620
214.643425	48.073328	75.434625
214.153591	37.713192	75.439630
213.107392	44.138860	75.444634
212.835905	41.870015	75.449639
212.744352	39.163774	75.454644
211.619460	54.322540	75.459649
210.841746	43.086934	75.464654
210.287725	45.791353	75.469658
209.858958	36.753302	75.474663
209.596027	36.606546	75.479668
208.502149	53.403186	75.484673
207.956876	37.891284	75.489678
207.022644	45.379275	75.494682
205.978891	40.144311	75.499687
205.347710	46.385954	75.504692
204.649438	51.315627	75.509697
204.437325	42.668699	75.514702
203.941490	45.614972	75.519706
203.462008	44.316856	75.524711
202.437251	41.446125	75.529716
201.176144	47.054082	75.534721
200.762563	41.665312	75.539726
200.469092	42.102046	75.544730
199.444459	39.069858	75.549735
198.877961	41.167374	75.554740
197.888844	42.234112	75.559745
197.396795	43.161963	75.564750
197.032164	48.140622	75.569754
196.968865	48.346861	75.574759
196.279869	45.207010	75.579764
195.354009	48.444484	75.584769
194.651532	46.335566	75.589774
193.914025	46.306081	75.594778
192.705055	42.774997	75.599783
192.162858	39.036862	75.604788
191.341129	41.539687	75.609793
191.390879	35.487717	75.614798
190.867694	48.818048	75.619802
189.753339	48.063340	75.624807
188.833144	41.005731	75.629812
188.077684	52.658881	75.634817
187.626981	46.631118	75.639822
187.107797	45.255736	75.644826
186.650987	41.429547	75.649831
186.351253	41.447776	75.654836
185.236150	41.549725	75.659841
184.915119	37.276341	75.664846
184.055219	33.839758	75.669850
182.867537	39.853920	75.674855
182.439050	39.476219	75.679860
181.812672	37.606876	75.684865
181.248076	40.116543	75.689870
180.693416	42.807653	75.694874
179.561929	43.414093	75.699879
179.220414	36.837124	75.704884
178.740578	41.470421	75.709889
178.316026	39.795809	75.714894
177.081856	40.934951	75.719898
176.171595	32.399026	75.724903
175.836701	32.317500	75.729908
174.705848	36.981871	75.734913
174.626512	34.557731	75.739918
174.411706	33.897102	75.744922
173.625955	40.224448	75.749927
172.822549	34.821987	75.754932
172.030721	43.152358	75.759937
171.699353	29.722626	75.764942
170.599442	33.085852	75.769946
169.444413	34.824812	75.774951
168.954953	37.723812	75.779956
168.282941	37.722180	75.784961
168.325591	28.789634	75.789966
167.791787	36.984593	75.794970
166.735168	41.818205	75.799975
166.013588	31.465838	75.804980
165.273927	34.241948	75.809985
164.787775	31.185748	75.814990
164.100612	32.036135	75.819994
162.959984	33.025831	75.824999
162.579865	27.104000	75.830004
162.298612	39.592767	75.835009
161.596326	30.661218	75.840014
160.713047	43.260294	75.845018
160.036568	46.226485	75.850023
159.581376	36.690109	75.855028
159.050093	47.039377	75.860033
157.971146	31.747263	75.865038
157.181438	37.928850	75.870042
156.124122	35.739066	75.875047
156.119024	29.398100	75.880052
155.523406	37.507347	75.885057
155.398905	36.507178	75.890062
154.670259	32.122107	75.895066
153.209174	41.415049	75.900071
153.267360	36.676422	75.905076
151.776146	42.732756	75.910081
151.101608	32.390485	75.915086
150.516099	36.592714	75.920090
149.924371	33.705788	75.925095
149.780992	36.781895	75.930100
149.034208	39.232407	75.935105
148.616285	35.481264	75.940110
147.556684	41.642414	75.945114
146.678358	41.070663	75.950119
146.507363	36.291593	75.955124
145.668323	38.894097	75.960129
144.563319	33.709519	75.965134
144.091291	37.558368	75.970138
143.333470	30.634378	75.975143
143.535997	30.371915	75.980148
142.644512	34.699619	75.985153
141.655713	33.524741	75.990158
141.072889	37.554021	75.995162
139.917211	36.243156	76.000167
139.732518	36.515992	76.005172
138.341669	39.622804	76.010177
137.878939	36.785209	76.015182
137.542673	31.359515	76.020186
137.169888	40.062893	76.025191
136.889344	30.855379	76.030196
135.780344	42.230861	76.035201
135.164525	33.917218	76.040206
134.687803	35.618057	76.045210
133.419693	37.027880	76.050215
132.936000	41.441591	76.055220
132.123482	35.381926	76.060225
131.894306	43.426778	76.065230
131.294540	50.249980	76.070234
130.580298	46.959741	76.075239
129.653758	32.999716	76.080244
129.049350	40.614713	76.085249
128.563852	33.674829	76.090254
127.453095	41.540830	76.095258
126.322174	36.361489	76.100263
126.272873	30.146911	76.105268
125.272265	33.058545	76.110273
124.388968	39.229339	76.115278
124.397728	44.918808	76.120282
124.059661	47.391621	76.125287
123.960862	30.728014	76.130292
122.616281	43.116455	76.135297
121.893864	37.519343	76.140302
121.694911	32.013667	76.145306
120.600795	42.303903	76.150311
119.464163	39.916555	76.155316
118.746533	43.595945	76.160321
118.287475	39.761862	76.165326
117.770920	40.648925	76.170330
117.019518	35.876996	76.175335
116.207201	37.961008	76.180340
115.651855	41.524556	76.185345
114.955492	38.815432	76.190350
114.696973	41.338155	76.195354
114.194290	42.703600	76.200359
113.524081	35.000828	76.205364
112.549653	35.547596	76.210369
111.868588	28.433625	76.215374
111.510473	36.953313	76.220378
110.459423	38.835504	76.225383
110.066864	33.024751	76.230388
109.031131	39.444298	76.235393
108.834764	36.455655	76.240398
107.659537	35.433921	76.245402
106.934268	44.511920	76.250407
106.840116	35.410209	76.255412
105.757921	33.870848	76.260417
105.727794	43.497922	76.265422
104.369749	41.554695	76.270426
103.245854	51.285211	76.275431
103.502223	31.088037	76.280436
102.669199	42.521204	76.285441
101.989103	34.960647	76.290446
101.455270	32.605349	76.295450
100.474056	42.735715	76.300455
100.217739	30.893690	76.305460
99.215221	42.537088	76.310465
98.945431	35.724034	76.315470
97.924195	38.711442	76.320474
97.038598	44.408586	76.325479
96.664769	41.520231	76.330484
95.945303	43.798315	76.335489
95.594363	39.251795	76.340494
94.499995	43.920982	76.345498
93.473029	41.847187	76.350503
93.053546	35.052692	76.355508
92.464923	37.856599	76.360513
92.453766	33.168546	76.365518
92.271345	34.884457	76.370522
90.698991	35.965158	76.375527
90.871594	34.629075	76.380532
89.004406	38.791713	76.385537
88.185188	40.632585	76.390542
87.787901	34.206499	76.395546
87.268974	39.626058	76.400551
87.073576	40.335705	76.405556
86.275174	29.403673	76.410561
85.996045	31.482721	76.415566
85.347203	35.807910	76.420570
83.984458	39.947223	76.425575
83.729370	35.417429	76.430580
82.249013	37.946349	76.435585
81.750482	32.362571	76.440590
81.590938	33.570118	76.445594
80.712194	38.145894	76.450599
80.699709	31.143083	76.455604
79.636529	36.301102	76.460609
78.588733	37.872893	76.465614
77.941423	36.073467	76.470618
77.489749	43.173234	76.475623
77.424671	29.312236	76.480628
76.329044	37.665092	76.485633
75.530194	38.064932	76.490638
75.418085	28.151227	76.495642
73.542056	36.826945	76.500647
73.025878	34.298503	76.505652
72.335496	45.385529	76.510657
72.013427	39.478226	76.515662
71.620143	40.667034	76.520666
70.996063	37.686200	76.525671
71.038146	32.304984	76.530676
69.434780	31.145492	76.535681
68.707173	35.671675	76.540686
67.829268	32.182946	76.545690
67.466444	34.352128	76.550695
67.189396	31.560073	76.555700
66.348442	36.522110	76.560705
65.374248	38.236407	76.565710
64.937334	34.080004	76.570714
64.112209	38.311480	76.575719
63.879334	33.023191	76.580724
63.140383	40.349041	76.585729
62.451685	36.122522	76.590734
61.571738	41.225055	76.595738
61.063644	45.572695	76.600743
60.943793	29.936595	76.605748
59.521157	36.008428	76.610753
58.769122	29.855129	76.615758
58.656887	32.008979	76.620762
58.042781	37.224213	76.625767
57.266605	40.413941	76.630772
56.205789	41.566022	76.635777
55.726395	33.701872	76.640782
55.330150	26.131741	76.645786
54.080683	41.677764	76.650791
53.627308	34.460823	76.655796
52.947046	38.182363	76.660801
52.467709	31.847320	76.665806
52.526990	36.778167	76.670810
51.136358	45.583031	76.675815
50.699615	31.445515	76.680820
50.107109	41.152027	76.685825
48.919822	40.099616	76.690830
48.233058	30.464031	76.695834
47.314671	36.711503	76.700839
46.863221	33.336362	76.705844
46.823605	46.936257	76.710849
46.078874	38.933663	76.715854
45.583608	34.328611	76.720858
44.012144	41.434456	76.725863
44.190155	38.723056	76.730868
43.117034	39.572532	76.735873
42.605218	39.867906	76.740878
41.515888	32.442259	76.745882
40.598165	41.583254	76.750887
40.301573	28.570721	76.755892
39.674141	42.377175	76.760897
39.390613	38.896669	76.765902
39.312216	31.620969	76.770906
37.355919	35.120393	76.775911
37.137411	29.589660	76.780916
36.339219	44.968716	76.785921
36.158122	38.037443	76.790926
35.853570	35.975586	76.795930
34.483241	37.293230	76.800935
33.958969	33.265092	76.805940
33.558153	34.620578	76.810945
32.606393	33.388062	76.815950
31.574532	24.866717	76.820954
30.566059	37.958152	76.825959
30.372071	31.661816	76.830964
29.866060	38.279087	76.835969
29.449046	40.318230	76.840974
29.492827	38.598467	76.845978
27.971695	39.842107	76.850983
27.788632	35.903485	76.855988
26.799771	33.891855	76.860993
25.191101	33.860190	76.865998
24.547953	33.426947	76.871002
23.976592	36.224349	76.876007
23.929876	41.200998	76.881012
23.578925	35.612846	76.886017
23.520046	24.731663	76.891022
23.054051	22.980892	76.896026
21.891730	27.320707	76.901031
20.618068	21.567888	76.906036
19.593078	31.904301	76.911041
18.631859	31.822811	76.916046
18.462903	27.832040	76.921050
17.518836	28.688207	76.926055
17.390363	22.000141	76.931060
16.605302	31.559280	76.936065
16.371601	30.984788	76.941070
16.125566	34.839894	76.946074
14.649089	34.768990	76.951079
14.592138	21.773798	76.956084
13.906714	29.060470	76.961089
12.932488	35.117007	76.966094
12.069433	29.263395	76.971098
11.400103	30.446250	76.976103
11.127951	22.136082	76.981108
10.060314	35.813150	76.986113
8.865024	35.287484	76.991118
8.905421	30.998729	76.996122
8.373595	38.855875	77.001127
7.909126	34.694732	77.006132
6.894573	39.262622	77.011137
5.796935	29.547505	77.016142
5.634949	27.352267	77.021147
4.923143	37.499996	77.026151
4.476931	25.715024	77.031156
3.123286	34.330799	77.036161