Tue Jun 08 17:24:02 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
-0.085644	105.885251	0.000000
-0.440738	93.056405	0.005005
-1.422250	73.610647	0.010010
-3.004334	20.898942	0.015014
-7.262088	-3.185685	0.020019
-12.269815	-5.341025	0.025024
-17.661890	-3.409143	0.030029
-22.364222	3.016280	0.035034
-26.339450	-2.563763	0.040038
-30.325418	5.708049	0.045043
-33.290373	-1.296057	0.050048
-37.253153	-9.660143	0.055053
-40.764125	-1.860932	0.060058
-44.392192	-10.613961	0.065062
-48.637004	2.811777	0.070067
-52.040766	1.920819	0.075072
-55.852256	-3.323350	0.080077
-59.807738	-0.340341	0.085082
-63.183960	-1.796107	0.090086
-67.449093	-3.631119	0.095091
-70.975304	-1.750721	0.100096
-74.984959	3.788659	0.105101
-78.613297	-2.498935	0.110106
-82.038402	-4.573104	0.115110
-86.024124	4.796399	0.120115
-90.026783	-8.217201	0.125120
-93.657447	-4.095471	0.130125
-97.449171	0.370440	0.135130
-100.698607	-5.573977	0.140134
-104.914195	2.653195	0.145139
-108.482175	-14.412025	0.150144
-112.385758	-2.274673	0.155149
-116.114177	-4.423899	0.160154
-119.844914	-16.702170	0.165158
-123.915561	-9.696605	0.170163
-127.228495	-7.340800	0.175168
-130.628201	-2.575800	0.180173
-134.369420	-4.415335	0.185178
-138.254522	-15.707577	0.190182
-142.985574	-12.147054	0.195187
-146.327245	-17.222644	0.200192
-150.337401	-5.380391	0.205197
-154.345558	-2.665356	0.210202
-157.889068	-9.315165	0.215206
-162.019556	-4.045895	0.220211
-165.531268	-11.428601	0.225216
-168.639680	-2.668936	0.230221
-172.679435	-4.393692	0.235226
-176.331001	-11.874764	0.240230
-180.353818	-14.186192	0.245235
-183.884209	-18.296293	0.250240
-187.784385	-6.483531	0.255245
-191.386458	-10.868683	0.260250
-195.021126	-22.227101	0.265254
-199.256936	-6.408883	0.270259
-202.783842	-8.008424	0.275264
-206.410108	-12.852408	0.280269
-210.207907	-2.443800	0.285274
-213.969741	-9.926846	0.290278
-217.809456	-5.499187	0.295283
-221.593396	-16.345701	0.300288
-225.331995	-15.462900	0.305293
-229.002778	-2.517555	0.310298
-232.422591	-12.373033	0.315302
-236.506023	-6.897444	0.320307
-240.474159	-6.260637	0.325312
-243.833788	-7.149149	0.330317
-247.975452	-9.314220	0.335322
-251.455804	-15.151414	0.340326
-255.579944	4.393499	0.345331
-259.113384	-4.415832	0.350336
-263.060833	-8.097914	0.355341
-266.573593	-10.583584	0.360346
-270.329112	-19.672151	0.365350
-274.519905	-8.469040	0.370355
-277.893668	-13.472711	0.375360
-281.537203	-15.635563	0.380365
-286.127181	-11.143501	0.385370
-289.394749	-15.999994	0.390374
-293.179227	-14.025395	0.395379
-296.385450	-9.611998	0.400384
-300.098680	-15.422231	0.405389
-304.132003	-15.142451	0.410394
-307.891974	-17.987102	0.415398
-312.060985	-10.091807	0.420403
-315.458239	-18.663536	0.425408
-319.293327	-16.507353	0.430413
-323.302961	-14.661860	0.435418
-326.660481	-10.036187	0.440422
-330.653789	-6.605967	0.445427
-334.331592	-13.964772	0.450432
-338.051872	-7.996823	0.455437
-341.861078	-12.634848	0.460442
-345.870901	-17.848281	0.465446
-349.528101	-15.003821	0.470451
-352.953353	-19.498895	0.475456
-357.207357	-10.140401	0.480461
-361.037168	-16.792626	0.485466
-364.358696	-17.942168	0.490470
-368.655966	-11.004097	0.495475
-371.946507	-14.767188	0.500480
-375.780909	-13.317998	0.505485
-379.804560	-12.346305	0.510490
-383.159394	-16.492671	0.515494
-386.954465	-10.008996	0.520499
-390.502126	-14.863937	0.525504
-394.531288	-15.559325	0.530509
-398.631331	-8.428892	0.535514
-402.012127	-11.025505	0.540518
-406.060489	-5.225021	0.545523
-409.773618	-13.146473	0.550528
-413.398528	-14.956777	0.555533
-417.141215	-14.597684	0.560538
-420.310187	-13.869675	0.565542
-424.803231	-8.851382	0.570547
-428.225563	-15.783039	0.575552
-432.512588	-14.567972	0.580557
-436.451069	-11.513358	0.585562
-439.919534	-22.317864	0.590566
-443.771290	-9.498426	0.595571
-447.414866	-12.596987	0.600576
-450.712675	-16.766107	0.605581
-454.679364	-17.296118	0.610586
-458.076416	-18.483944	0.615590
-462.348437	-16.492663	0.620595
-465.963281	-22.902213	0.625600
-469.729563	-13.462707	0.630605
-473.850110	-6.370925	0.635610
-477.363965	-20.392382	0.640614
-481.422787	-17.417734	0.645619
-484.974319	-20.749932	0.650624
-488.817929	-21.275372	0.655629
-492.630559	-17.182510	0.660634
-495.932588	-23.203630	0.665638
-499.978509	-16.741168	0.670643
-503.666536	-18.682662	0.675648
-507.691579	-15.146985	0.680653
-511.224590	-14.723926	0.685658
-514.457667	-20.227953	0.690662
-518.821775	-10.044830	0.695667
-522.506733	-10.902177	0.700672
-525.996986	-16.989657	0.705677
-529.400337	-18.595527	0.710682
-533.406909	-18.165798	0.715686
-537.669133	-8.329720	0.720691
-541.691085	-15.593367	0.725696
-545.572157	-12.004206	0.730701
-549.131314	-11.314940	0.735706
-552.676807	-18.122734	0.740710
-556.662523	-17.162917	0.745715
-560.305766	-11.003557	0.750720
-563.780650	-11.412212	0.755725
-567.519479	-8.656986	0.760730
-571.183570	-21.956308	0.765734
-575.235397	-9.876072	0.770739
-578.706135	-9.394176	0.775744
-582.626869	-15.930731	0.780749
-586.607560	-13.208588	0.785754
-590.301348	-12.804059	0.790758
-594.401608	-13.473644	0.795763
-597.841508	-10.915729	0.800768
-600.985701	-9.712274	0.805773
-605.382301	-6.596270	0.810778
-609.021950	-8.435063	0.815782
-612.731802	-1.457052	0.820787
-616.708216	-12.116616	0.825792
-620.190820	-9.593590	0.830797
-623.914048	0.150077	0.835802
-627.455994	-6.128172	0.840806
-631.648872	-1.692858	0.845811
-635.299146	-4.122658	0.850816
-639.092643	-8.995197	0.855821
-643.266532	0.300463	0.860826
-646.748386	-9.924899	0.865830
-650.388919	-0.447622	0.870835
-653.787300	-4.490386	0.875840
-657.965267	-4.097837	0.880845
-661.545536	-2.276387	0.885850
-665.245022	-6.056696	0.890854
-669.629572	-5.247791	0.895859
-672.967276	-10.654404	0.900864
-676.691970	-3.616960	0.905869
-680.737465	-9.404565	0.910874
-684.261650	-11.419413	0.915878
-688.247059	-0.132000	0.920883
-691.794270	-13.599679	0.925888
-695.305119	-9.945647	0.930893
-699.313990	-6.097204	0.935898
-702.666116	-13.637475	0.940902
-707.074454	-10.393052	0.945907
-710.729156	-12.234306	0.950912
-714.240699	-19.367101	0.955917
-718.145460	-14.675653	0.960922
-721.863716	-11.085472	0.965926
-725.843566	-11.648896	0.970931
-729.642572	-12.400447	0.975936
-733.133971	-11.815812	0.980941
-736.537374	-8.251631	0.985946
-740.512579	-18.194086	0.990950
-744.338184	-5.886901	0.995955
-748.221298	-8.689505	1.000960
-752.012504	-7.093077	1.005965
-755.764919	-1.950539	1.010970
-759.030666	-14.594156	1.015974
-763.097032	-7.102903	1.020979
-767.239660	-10.196450	1.025984
-770.944549	-18.826291	1.030989
-774.967480	-4.957698	1.035994
-778.253033	-7.427474	1.040998
-781.809221	-7.897784	1.046003
-785.644248	-8.898874	1.051008
-789.484184	-4.242567	1.056013
-793.270718	-1.608035	1.061018
-797.083497	-4.353198	1.066022
-801.071818	-8.174593	1.071027
-804.879507	-11.028376	1.076032
-808.640181	-5.600191	1.081037
-812.274906	3.599125	1.086042
-815.682819	-14.164261	1.091046
-819.592070	-0.029374	1.096051
-823.680503	-11.380365	1.101056
-827.282597	-14.783325	1.106061
-831.167734	0.522475	1.111066
-834.634505	-6.529096	1.116070
-838.495217	-7.569936	1.121075
-841.988521	-12.437370	1.126080
-845.767702	-12.122171	1.131085
-849.994086	-4.721787	1.136090
-853.179163	-16.941040	1.141094
-857.458545	0.605708	1.146099
-861.120083	-8.509879	1.151104
-864.952370	-11.531084	1.156109
-868.635956	-8.344203	1.161114
-872.096152	-13.015598	1.166118
-875.953974	-2.137935	1.171123
-879.812926	-1.204716	1.176128
-883.677948	-13.563787	1.181133
-887.507886	-3.420321	1.186138
-891.300288	-15.282281	1.191142
-895.036611	-1.089003	1.196147
-898.763203	-3.107609	1.201152
-902.358638	-8.714508	1.206157
-906.023452	4.247652	1.211162
-909.440084	-11.400886	1.216166
-913.163471	-6.312939	1.221171
-917.590506	-11.543005	1.226176
-921.295805	-11.920502	1.231181
-925.168162	-0.865450	1.236186
-928.618360	-9.339936	1.241190
-932.460207	-6.342133	1.246195
-936.180564	-6.018797	1.251200
-940.315514	-2.738187	1.256205
-944.387784	-3.164368	1.261210
-947.787191	-13.127705	1.266214
-951.501962	-8.959688	1.271219
-955.083775	-10.535370	1.276224
-958.434714	-12.057929	1.281229
-962.452260	-3.307481	1.286234
-966.244342	-18.145901	1.291238
-970.441674	-12.849842	1.296243
-973.935328	-7.875885	1.301248
-977.670751	-11.019790	1.306253
-981.331384	-6.967614	1.311258
-984.784680	-15.977131	1.316262
-989.023991	-11.013689	1.321267
-992.307611	-18.270624	1.326272
-996.286004	-22.058400	1.331277
-1000.516101	-7.361891	1.336282
-1004.059440	-7.984211	1.341286
-1007.603650	-12.903151	1.346291
-1010.927671	-23.980991	1.351296
-1015.111139	-16.956881	1.356301
-1019.293257	-4.495523	1.361306
-1023.049195	-10.661684	1.366310
-1026.984355	-8.145898	1.371315
-1030.554903	-13.165288	1.376320
-1033.855205	-14.588724	1.381325
-1037.745001	-8.780580	1.386330
-1041.668049	-12.623998	1.391334
-1045.395411	-5.600805	1.396339
-1049.342625	-8.208979	1.401344
-1052.892162	-7.719491	1.406349
-1057.070783	-9.293265	1.411354
-1060.290402	-18.830295	1.416358
-1063.991931	-9.564859	1.421363
-1068.031263	-7.845823	1.426368
-1071.265880	-7.704053	1.431373
-1075.400928	-6.155667	1.436378
-1079.268928	-3.239686	1.441382
-1083.196311	-11.428429	1.446387
-1086.923194	-1.481697	1.451392
-1090.449070	-8.560782	1.456397
-1094.410666	-9.699321	1.461402
-1097.715179	-5.348620	1.466406
-1101.825337	-0.723012	1.471411
-1105.736685	-10.112419	1.476416
-1109.024252	-10.088623	1.481421
-1113.290506	-2.106462	1.486426
-1116.662567	-7.487070	1.491430
-1120.200232	-10.055378	1.496435
-1124.220594	-11.757699	1.501440
-1128.016679	-15.195368	1.506445
-1132.063405	-5.299857	1.511450
-1135.347082	-11.643708	1.516454
-1139.329029	-12.762132	1.521459
-1142.766377	-10.681040	1.526464
-1146.927299	-10.792615	1.531469
-1150.974146	-7.961510	1.536474
-1154.475398	-10.177648	1.541478
-1158.210175	-15.410280	1.546483
-1161.718864	-13.121543	1.551488
-1165.436667	-18.371292	1.556493
-1169.617981	-0.074615	1.561498
-1173.252940	-7.465262	1.566502
-1176.928435	-2.620172	1.571507
-1180.716607	-9.836091	1.576512
-1184.855582	-7.705129	1.581517
-1188.884247	-0.469826	1.586522
-1192.184065	-11.484568	1.591526
-1195.883535	1.066151	1.596531
-1199.440872	-6.637778	1.601536
-1203.030291	-12.686322	1.606541
-1206.831476	-5.312059	1.611546
-1210.443904	-15.053850	1.616550
-1214.681990	-5.050018	1.621555
-1218.669935	-2.426711	1.626560
-1222.130091	-17.012811	1.631565
-1226.053302	-10.749987	1.636570
-1229.509853	-15.614710	1.641574
-1233.142828	-11.590366	1.646579
-1237.379171	-1.746666	1.651584
-1240.814463	-10.792199	1.656589
-1244.877848	-1.331062	1.661594
-1248.289129	-10.587538	1.666598
-1252.602064	-10.330693	1.671603
-1256.532123	-7.212072	1.676608
-1259.921037	-8.656818	1.681613
-1263.167794	-9.820869	1.686618
-1266.708532	-12.792304	1.691622
-1270.588892	-12.926683	1.696627
-1274.869076	-18.481945	1.701632
-1278.591131	-11.163844	1.706637
-1282.841491	-10.724310	1.711642
-1286.210511	-8.738912	1.716646
-1290.205229	-12.281644	1.721651
-1293.748861	-15.064678	1.726656
-1297.147124	-18.972719	1.731661
-1301.150215	-15.462204	1.736666
-1304.707673	-22.046228	1.741670
-1308.878780	-7.475636	1.746675
-1312.410988	-5.338250	1.751680
-1316.177894	-11.086227	1.756685
-1320.009168	-5.306443	1.761690
-1323.548615	-5.819433	1.766694
-1327.257087	-15.174381	1.771699
-1330.981070	-11.070383	1.776704
-1334.199705	-12.019357	1.781709
-1338.823707	-7.019110	1.786714
-1342.462999	-13.253943	1.791718
-1346.426376	-13.889476	1.796723
-1350.222692	-10.425483	1.801728
-1353.608205	-11.526948	1.806733
-1357.594600	-10.874542	1.811738
-1361.754309	-6.759220	1.816742
-1365.581026	-10.071020	1.821747
-1369.136184	-6.564757	1.826752
-1372.608526	-16.898827	1.831757
-1376.402891	-8.475683	1.836762
-1379.505367	-15.673409	1.841766
-1383.743302	-11.639359	1.846771
-1387.381466	-9.161633	1.851776
-1391.245406	-2.814116	1.856781
-1395.504977	-5.562889	1.861786
-1398.804194	-11.139303	1.866790
-1402.785007	-7.733959	1.871795
-1406.045717	-3.769472	1.876800
-1409.719776	-2.371787	1.881805
-1414.083430	-4.869786	1.886810
-1417.788823	-15.755442	1.891814
-1421.561696	-8.122204	1.896819
-1424.990570	-8.289001	1.901824
-1428.772985	-18.342006	1.906829
-1432.879800	0.182062	1.911834
-1436.281295	-12.203560	1.916838
-1440.549306	-14.662305	1.921843
-1444.152444	-5.523596	1.926848
-1447.790507	-17.342028	1.931853
-1451.680123	-8.019900	1.936858
-1455.825034	-15.050718	1.941862
-1459.503571	-12.143661	1.946867
-1463.360326	-12.175345	1.951872
-1466.403493	-10.812580	1.956877
-1469.990849	-10.425578	1.961882
-1473.944116	-20.387610	1.966886
-1477.756896	-11.908726	1.971891
-1481.445688	-10.808029	1.976896
-1485.347250	-14.865870	1.981901
-1489.894025	-18.118969	1.986906
-1493.015947	-20.813237	1.991910
-1496.453868	-15.772669	1.996915
-1500.782404	-10.248299	2.006912
-1501.599290	-9.454211	2.016909
-1498.972781	-16.490366	2.026906
-1496.155786	-13.259693	2.036902
-1494.003162	-16.144564	2.046899
-1492.310645	-16.461357	2.056896
-1490.207385	-18.863889	2.066893
-1488.136611	-21.915304	2.076890
-1486.628574	-16.024070	2.086886
-1484.748458	-21.019962	2.096883
-1482.527497	-20.713395	2.106880
-1480.776031	-23.372836	2.116877
-1479.159578	-11.555879	2.126874
-1477.049071	-10.054979	2.136870
-1474.853686	-12.803726	2.146867
-1473.406102	-12.100685	2.156864
-1471.095072	-6.225272	2.166861
-1469.642596	-11.292736	2.176858
-1467.705164	-11.263499	2.186854
-1465.569799	-13.178708	2.196851
-1463.433380	-18.238385	2.206848
-1461.937637	-8.633612	2.216845
-1460.143388	-11.231236	2.226842
-1458.453792	-13.261933	2.236838
-1456.502468	-10.549233	2.246835
-1454.000293	-8.701427	2.256832
-1452.217706	-11.303367	2.266829
-1450.531104	-10.898660	2.276826
-1448.389425	-11.861700	2.286822
-1446.845281	-16.552460	2.296819
-1445.024807	-10.614892	2.306816
-1443.179949	-9.157260	2.316813
-1441.420356	-9.493460	2.326810
-1439.293886	-2.177002	2.336806
-1437.024358	-5.823344	2.346803
-1435.935934	-8.987766	2.356800
-1433.682953	-12.615453	2.366797
-1431.438456	-14.469561	2.376794
-1429.782612	-10.703045	2.386790
-1427.377558	-11.183714	2.396787
-1426.178888	-10.827967	2.406784
-1424.747682	-9.455376	2.416781
-1422.632037	-5.760334	2.426778
-1420.399969	-10.178795	2.436774
-1418.562900	-13.668632	2.446771
-1416.831574	-16.569224	2.456768
-1414.558712	-15.885811	2.466765
-1413.006670	-9.473312	2.476762
-1411.276173	-11.664754	2.486758
-1408.914223	-13.213373	2.496755
-1407.195486	-10.878826	2.506752
-1405.660936	-9.026806	2.516749
-1403.709962	-17.223788	2.526746
-1401.413945	-7.769105	2.536742
-1399.893622	-14.813976	2.546739
-1397.920599	-15.917564	2.556736
-1395.905257	-15.897330	2.566733
-1394.195237	-6.825321	2.576730
-1392.180811	-6.301825	2.586726
-1390.288525	-12.491726	2.596723
-1388.801633	-11.352376	2.606720
-1386.591508	-13.629359	2.616717
-1384.861795	-17.387663	2.626714
-1383.136841	-7.544393	2.636710
-1380.758139	-9.360666	2.646707
-1378.997073	-11.856916	2.656704
-1377.266113	-5.928833	2.666701
-1375.415390	-9.325754	2.676698
-1373.437504	-14.803560	2.686694
-1371.460392	-12.071930	2.696691
-1369.789107	-10.728701	2.706688
-1367.487388	-6.957304	2.716685
-1366.333358	-13.059115	2.726682
-1364.362283	-1.366632	2.736678
-1362.350360	-11.761560	2.746675
-1360.082882	-10.671706	2.756672
-1358.483790	-6.989470	2.766669
-1356.760337	-6.218766	2.776666
-1354.809591	-11.591125	2.786662
-1352.687517	-10.527669	2.796659
-1350.768004	-8.275799	2.806656
-1349.199956	-10.553134	2.816653
-1347.247218	-9.580337	2.826650
-1345.273503	-11.718285	2.836646
-1343.126548	-7.754697	2.846643
-1341.716082	-8.212684	2.856640
-1339.861886	-5.122019	2.866637
-1337.972604	-2.975608	2.876634
-1335.976724	-6.707291	2.886630
-1333.842295	-3.942985	2.896627
-1332.339882	-3.897851	2.906624
-1330.065098	-3.380314	2.916621
-1328.500042	-2.413636	2.926618
-1326.539323	-1.700667	2.936614
-1324.788639	-9.535196	2.946611
-1322.621116	-3.864263	2.956608
-1320.744220	-2.060736	2.966605
-1318.984534	-6.256131	2.976602
-1317.320687	-10.328751	2.986598
-1315.306538	-2.849862	2.996595
-1313.404687	-7.540764	3.006592
-1311.630868	-10.751742	3.016589
-1309.716446	-5.781511	3.026586
-1307.730879	-4.502908	3.036582
-1305.976373	-14.003897	3.046579
-1303.562788	-10.312144	3.056576
-1302.383317	-8.444941	3.066573
-1300.131793	-12.153329	3.076570
-1298.296635	-13.555289	3.086566
-1296.240852	-10.874677	3.096563
-1294.729397	-15.728925	3.106560
-1292.785713	-10.552275	3.116557
-1290.945736	-6.080256	3.126554
-1289.236407	-11.154632	3.136550
-1287.123860	-10.592213	3.146547
-1285.222188	-15.150675	3.156544
-1283.240708	-16.776155	3.166541
-1281.640430	-8.970465	3.176538
-1279.751554	-9.323269	3.186534
-1277.570459	-2.298673	3.196531
-1275.832940	-9.446025	3.206528
-1274.083282	-9.491945	3.216525
-1272.216233	-10.065081	3.226522
-1270.036834	-7.957796	3.236518
-1268.249001	-7.494916	3.246515
-1266.672061	-4.852587	3.256512
-1264.447616	-11.353213	3.266509
-1262.602074	-10.691175	3.276506
-1260.748629	-7.326068	3.286502
-1259.225985	-10.490726	3.296499
-1257.216777	-3.031111	3.306496
-1255.194285	-3.881896	3.316493
-1253.243722	-4.909632	3.326490
-1251.274836	-3.739190	3.336486
-1249.459899	-2.960835	3.346483
-1247.825599	-14.998965	3.356480
-1245.958214	-7.031251	3.366477
-1243.631188	-5.200659	3.376474
-1241.925539	-7.771123	3.386470
-1240.524188	-5.509251	3.396467
-1237.955067	-3.581515	3.406464
-1236.364267	-3.345225	3.416461
-1235.002931	-2.153034	3.426458
-1232.662514	-3.182109	3.436454
-1230.400292	-6.997032	3.446451
-1228.956657	-8.790168	3.456448
-1227.272575	-10.291829	3.466445
-1225.107523	-6.554182	3.476442
-1223.289142	-13.738718	3.486438
-1221.555535	-13.130158	3.496435
-1219.572711	-11.482309	3.506432
-1217.824655	-9.780704	3.516429
-1215.945839	-11.606284	3.526426
-1213.863414	-7.595578	3.536422
-1212.230233	-10.077309	3.546419
-1210.341100	-10.877901	3.556416
-1208.168142	-6.357108	3.566413
-1206.277324	-4.544853	3.576410
-1204.546621	-12.321370	3.586406
-1202.673858	-8.248173	3.596403
-1200.803416	-10.815700	3.606400
-1198.801804	-12.731127	3.616397
-1196.912420	-11.447413	3.626394
-1195.065518	-11.052346	3.636390
-1193.480964	-6.773147	3.646387
-1191.405945	-16.586818	3.656384
-1189.475582	-10.698424	3.666381
-1187.862669	-9.811840	3.676378
-1185.901288	-3.720887	3.686374
-1183.736676	-9.950758	3.696371
-1181.927901	-12.079278	3.706368
-1179.980144	-13.583913	3.716365
-1178.290216	-5.345400	3.726362
-1176.314795	1.307115	3.736358
-1174.465145	-0.517786	3.746355
-1172.367868	-11.838659	3.756352
-1170.728017	-13.606979	3.766349
-1169.370008	-13.871732	3.776346
-1167.232325	-13.372060	3.786342
-1165.156691	-14.060011	3.796339
-1163.319911	-10.846129	3.806336
-1161.470555	-7.543505	3.816333
-1159.457263	-6.678239	3.826330
-1157.390201	-8.562204	3.836326
-1155.946702	-11.087223	3.846323
-1153.834249	-7.136180	3.856320
-1152.090362	-8.247734	3.866317
-1149.899051	-11.568282	3.876314
-1147.964179	-15.275572	3.886310
-1146.450971	-15.297040	3.896307
-1144.562960	-13.887390	3.906304
-1142.275711	-7.267066	3.916301
-1140.730729	-7.246167	3.926298
-1139.142045	-6.515464	3.936294
-1137.029371	-9.898778	3.946291
-1135.056798	-6.778942	3.956288
-1133.080320	-5.717245	3.966285
-1131.503079	-10.157889	3.976282
-1129.303242	-5.908040	3.986278
-1127.839476	-9.453409	3.996275
-1125.686345	-10.830459	4.006272
-1123.867730	-9.693040	4.016269
-1121.931808	-16.118762	4.026266
-1120.276460	-13.840787	4.036262
-1117.841737	-6.157359	4.046259
-1116.082880	-21.086072	4.056256
-1114.757796	-15.070785	4.066253
-1112.674494	-10.437719	4.076250
-1111.046375	-12.328889	4.086246
-1108.745082	-17.994119	4.096243
-1106.870536	-17.829030	4.106240
-1104.976887	-18.216169	4.116237
-1103.359661	-19.738315	4.126234
-1101.143322	-16.657554	4.136230
-1099.441742	-10.817962	4.146227
-1097.626154	-11.344640	4.156224
-1095.876854	-13.380314	4.166221
-1093.901847	-14.793949	4.176218
-1091.784713	-11.625405	4.186214
-1089.872933	-15.957488	4.196211
-1088.263279	-14.067260	4.206208
-1086.246927	-15.202648	4.216205
-1084.468816	-10.355918	4.226202
-1082.382643	-13.315732	4.236198
-1080.641129	-11.275434	4.246195
-1078.528695	-12.520587	4.256192
-1076.827247	-13.455277	4.266189
-1075.077813	-14.084804	4.276186
-1073.172660	-14.454934	4.286182
-1071.431351	-20.563853	4.296179
-1069.642934	-15.789234	4.306176
-1067.433590	-11.301881	4.316173
-1065.671454	-7.758176	4.326170
-1063.692747	-12.953026	4.336166
-1062.068886	-12.757522	4.346163
-1060.230659	-16.043881	4.356160
-1058.037561	-17.030967	4.366157
-1056.238839	-15.537179	4.376154
-1054.538333	-18.839410	4.386150
-1052.296064	-16.756241	4.396147
-1050.458367	-13.655494	4.406144
-1048.892658	-15.362428	4.416141
-1047.237272	-16.171030	4.426138
-1045.167510	-15.228458	4.436134
-1042.884712	-13.472758	4.446131
-1041.277629	-16.554620	4.456128
-1039.117950	-13.385449	4.466125
-1037.611031	-12.880957	4.476122
-1036.073463	-18.627254	4.486118
-1033.816956	-11.274793	4.496115
-1031.721465	-16.542638	4.506112
-1029.928723	-15.436699	4.516109
-1028.274454	-13.626036	4.526106
-1026.031106	-18.055727	4.536102
-1024.459973	-14.876794	4.546099
-1022.400360	-13.427388	4.556096
-1020.740463	-12.059929	4.566093
-1018.585076	-19.194755	4.576090
-1016.997013	-17.968699	4.586086
-1015.106300	-6.602097	4.596083
-1012.839171	-12.677180	4.606080
-1011.278981	-13.771366	4.616077
-1009.725799	-10.920532	4.626074
-1007.802269	-8.657331	4.636070
-1005.547781	-13.602306	4.646067
-1003.674063	-7.852688	4.656064
-1001.812406	-1.333495	4.666061
-999.774824	-9.757824	4.676058
-998.092457	-7.335441	4.686054
-996.582950	-9.866605	4.696051
-994.278160	-9.482481	4.706048
-992.143541	-7.268950	4.716045
-990.614511	-11.238083	4.726042
-988.915007	-6.257666	4.736038
-986.889351	-9.128006	4.746035
-984.979816	-14.912854	4.756032
-983.110254	-10.804224	4.766029
-981.388020	-16.230865	4.776026
-979.421998	-11.199374	4.786022
-977.305560	-14.633058	4.796019
-975.592283	-19.472850	4.806016
-973.481571	-11.923010	4.816013
-971.818386	-15.429847	4.826010
-970.086990	-8.409677	4.836006
-968.141489	-8.758232	4.846003
-966.073409	-11.736229	4.856000
-964.241872	-8.053817	4.865997
-962.335430	-7.480749	4.875994
-960.688769	-18.313159	4.885990
-958.729713	-13.518380	4.895987
-956.937137	-12.553472	4.905984
-954.900791	-8.381375	4.915981
-953.271559	-14.701819	4.925978
-951.419397	-6.330591	4.935974
-949.303613	-8.868204	4.945971
-947.304526	-7.427735	4.955968
-945.410983	-9.662797	4.965965
-943.689629	-3.273622	4.975962
-941.981877	-5.913893	4.985958
-939.808675	-5.635197	4.995955
-938.178591	-5.046687	5.005952
-936.128243	-4.195974	5.015949
-934.139545	-7.507326	5.025946
-932.530657	-14.911500	5.035942
-930.637005	-9.081483	5.045939
-928.564415	-7.976511	5.055936
-927.024892	-11.004054	5.065933
-925.173224	-14.516358	5.075930
-922.765053	-12.632328	5.085926
-921.057682	-8.944390	5.095923
-919.119699	-21.911935	5.105920
-917.314108	-14.177289	5.115917
-915.877683	-11.733994	5.125914
-913.662131	-13.850032	5.135910
-911.796361	-10.748506	5.145907
-909.958421	-12.026685	5.155904
-907.836342	-9.902647	5.165901
-906.320098	-9.590201	5.175898
-904.495446	-8.191301	5.185894
-902.273338	-19.052525	5.195891
-900.258551	-15.654478	5.205888
-898.472035	-9.972834	5.215885
-897.003046	-13.549065	5.225882
-894.969236	-13.031423	5.235878
-892.931436	-7.036430	5.245875
-890.894419	-10.983259	5.255872
-889.317216	-9.310280	5.265869
-887.762005	-10.349819	5.275866
-885.734660	-8.480623	5.285862
-883.323219	-12.277517	5.295859
-881.716044	-14.746762	5.305856
-879.976175	-16.580360	5.315853
-878.161178	-11.599960	5.325850
-876.231553	-13.063014	5.335846
-874.196642	-7.445732	5.345843
-872.325394	-8.143118	5.355840
-870.334433	-8.619182	5.365837
-868.537604	-13.287136	5.375834
-866.705269	-16.197747	5.385830
-864.898802	-10.838052	5.395827
-863.237368	-7.808531	5.405824
-861.089670	-6.894263	5.415821
-859.131459	-10.201535	5.425818
-857.335015	-5.487868	5.435814
-855.463121	-3.682477	5.445811
-853.397046	-8.836119	5.455808
-851.891535	-10.656749	5.465805
-850.303929	-5.355120	5.475802
-847.880384	-4.052671	5.485798
-845.945873	-12.386133	5.495795
-844.117401	-14.492605	5.505792
-842.100912	-11.006292	5.515789
-840.617561	-14.204382	5.525786
-838.729884	-8.580384	5.535782
-837.159484	-8.615907	5.545779
-834.955575	-7.460315	5.555776
-832.737825	-13.824829	5.565773
-830.992101	-10.986027	5.575770
-829.192206	-5.932662	5.585766
-827.612579	-4.810606	5.595763
-825.486606	-7.308809	5.605760
-823.642909	-6.926862	5.615757
-821.801615	-6.702587	5.625754
-819.743042	-10.389479	5.635750
-817.749767	-8.629409	5.645747
-816.127737	-16.366596	5.655744
-814.101264	-11.213396	5.665741
-812.294920	-7.672027	5.675738
-810.474022	-10.511491	5.685734
-808.745273	-10.009819	5.695731
-806.779462	-3.788216	5.705728
-804.706556	-6.244499	5.715725
-802.910801	-8.532275	5.725722
-801.227969	-7.297109	5.735718
-799.372932	-7.087829	5.745715
-797.371935	-15.062370	5.755712
-795.311027	-14.487680	5.765709
-793.694924	-13.233548	5.775706
-791.731632	-9.949122	5.785702
-789.741741	-14.366421	5.795699
-787.696805	-9.882309	5.805696
-785.890222	-9.462359	5.815693
-784.413494	-11.125474	5.825690
-782.104115	-9.715260	5.835686
-780.511236	-6.922922	5.845683
-778.389174	-15.995584	5.855680
-776.763522	-7.250248	5.865677
-774.990957	-8.748350	5.875674
-773.121970	-8.480591	5.885670
-771.387068	-6.177394	5.895667
-769.009218	-10.212311	5.905664
-767.450041	-6.296520	5.915661
-765.318863	-1.470318	5.925658
-763.470057	-0.155334	5.935654
-761.561845	-7.394653	5.945651
-759.566890	-8.721060	5.955648
-757.863145	-11.685439	5.965645
-755.935838	-5.925924	5.975642
-754.120766	-7.628920	5.985638
-752.335818	-9.323188	5.995635
-750.573566	-12.046251	6.005632
-748.163389	-11.282498	6.015629
-746.718414	-14.788166	6.025626
-745.256235	-12.405350	6.035622
-742.839340	-11.803993	6.045619
-740.867441	-6.921198	6.055616
-739.541896	-10.769568	6.065613
-737.183984	-5.624993	6.075610
-735.587858	-8.699339	6.085606
-733.432661	-5.794816	6.095603
-731.712123	-14.636908	6.105600
-729.755154	-11.205929	6.115597
-727.856657	-9.848870	6.125594
-725.692652	-4.807753	6.135590
-724.150965	-10.508427	6.145587
-722.320789	-3.592431	6.155584
-720.393094	-2.270415	6.165581
-718.908810	-2.369368	6.175578
-716.661781	-2.852159	6.185574
-714.868348	-11.046357	6.195571
-712.922777	-10.168860	6.205568
-710.815826	-9.422208	6.215565
-708.740392	-7.197187	6.225562
-707.373435	-4.092954	6.235558
-705.531041	-3.909129	6.245555
-703.511934	-6.000837	6.255552
-701.575940	-2.869766	6.265549
-699.632637	-0.556458	6.275546
-698.045046	-6.767716	6.285542
-696.053749	-10.348158	6.295539
-693.990062	-4.102586	6.305536
-692.407629	-5.611500	6.315533
-690.573513	-2.218698	6.325530
-688.273044	-8.662557	6.335526
-686.660608	-2.198448	6.345523
-684.873861	-12.875799	6.355520
-682.705663	-8.871232	6.365517
-680.808962	-3.664072	6.375514
-679.335024	-9.918262	6.385510
-677.078367	-8.530165	6.395507
-675.131211	-4.914885	6.405504
-673.634157	-7.140680	6.415501
-671.620835	-8.829449	6.425498
-669.589305	-11.232330	6.435494
-667.671127	-11.503738	6.445491
-666.231735	-10.289185	6.455488
-664.309787	-13.657734	6.465485
-662.250144	-7.081845	6.475482
-660.156217	-5.764616	6.485478
-658.386378	-6.370999	6.495475
-656.613555	-10.513471	6.505472
-654.932451	-10.816120	6.515469
-652.976931	-5.104867	6.525466
-650.821768	-11.398885	6.535462
-648.982199	-11.105473	6.545459
-646.989253	-11.828785	6.555456
-645.151338	-14.717740	6.565453
-643.346287	-16.670327	6.575450
-641.696271	-10.569529	6.585446
-640.104658	-8.623859	6.595443
-638.109299	-11.884851	6.605440
-635.789415	-11.504310	6.615437
-633.786557	-10.071452	6.625434
-632.159540	-9.884231	6.635430
-630.609433	-11.062711	6.645427
-628.409681	-11.300611	6.655424
-626.525937	-13.331906	6.665421
-624.504825	-11.586401	6.675418
-622.731146	-8.174899	6.685414
-620.751329	-6.429419	6.695411
-619.432233	-8.976399	6.705408
-617.425027	-13.836472	6.715405
-615.125117	-7.686329	6.725402
-613.584754	-6.327837	6.735398
-611.922603	-3.467484	6.745395
-609.125402	-9.191098	6.755392
-607.533415	-10.538794	6.765389
-606.262098	-8.293908	6.775386
-604.453214	-6.473245	6.785382
-602.080508	-14.785775	6.795379
-600.166433	-7.350974	6.805376
-598.496673	-6.869131	6.815373
-596.596588	-9.818928	6.825370
-594.360894	-10.140441	6.835366
-592.695000	-12.023285	6.845363
-590.954089	-18.545764	6.855360
-589.311475	-17.069647	6.865357
-587.121462	-18.993021	6.875354
-585.567173	-14.051533	6.885350
-583.369774	-15.903454	6.895347
-581.583534	-19.358157	6.905344
-579.406863	-18.494960	6.915341
-577.944612	-17.523009	6.925338
-576.032582	-8.172245	6.935334
-573.750587	-15.895742	6.945331
-572.294752	-15.997272	6.955328
-570.172029	-10.256574	6.965325
-568.402338	-14.637975	6.975322
-566.532382	-16.179976	6.985318
-564.844277	-15.173659	6.995315
-562.705040	-15.768692	7.005312
-560.736525	-21.722770	7.015309
-559.241702	-16.786878	7.025306
-557.420433	-12.502582	7.035302
-555.266039	-17.376818	7.045299
-553.257732	-14.752499	7.055296
-551.336086	-15.707776	7.065293
-549.791720	-10.255929	7.075290
-547.780503	-15.778645	7.085286
-545.805252	-15.689478	7.095283
-543.883796	-19.744379	7.105280
-542.241125	-25.331903	7.115277
-540.229864	-20.553382	7.125274
-538.376443	-20.548435	7.135270
-536.716225	-20.666447	7.145267
-534.602087	-22.021107	7.155264
-532.319412	-19.695210	7.165261
-530.933643	-18.611711	7.175258
-529.220058	-16.661239	7.185254
-526.877198	-19.717408	7.195251
-525.345508	-19.981725	7.205248
-523.501115	-18.521627	7.215245
-521.504422	-16.911789	7.225242
-519.469676	-14.724353	7.235238
-517.636779	-18.771954	7.245235
-515.946949	-18.677276	7.255232
-513.849792	-19.812041	7.265229
-512.228736	-22.905211	7.275226
-510.377846	-21.797568	7.285222
-508.571198	-21.743086	7.295219
-506.150484	-19.201754	7.305216
-504.749934	-22.919467	7.315213
-502.812465	-22.387088	7.325210
-501.131878	-18.296394	7.335206
-498.689941	-20.885411	7.345203
-497.065167	-19.799434	7.355200
-495.362155	-27.212512	7.365197
-493.344799	-21.865510	7.375194
-491.312710	-22.812441	7.385190
-489.543653	-21.142191	7.395187
-487.700727	-16.866324	7.405184
-485.873113	-18.144929	7.415181
-483.895703	-12.872084	7.425178
-482.135014	-23.033492	7.435174
-480.076034	-20.701201	7.445171
-478.170808	-23.343168	7.455168
-476.534602	-18.167102	7.465165
-474.928571	-17.784938	7.475162
-472.471697	-17.163811	7.485158
-470.552614	-24.676001	7.495155
-468.977330	-26.881953	7.505152
-466.917569	-23.571240	7.515149
-465.306902	-15.361078	7.525146
-463.741521	-18.162498	7.535142
-461.373336	-21.428886	7.545139
-459.498687	-20.286565	7.555136
-457.561912	-21.433310	7.565133
-455.788960	-15.852678	7.575130
-453.861353	-13.921503	7.585126
-451.941374	-17.354049	7.595123
-450.184391	-15.320881	7.605120
-448.684513	-12.397449	7.615117
-446.296187	-13.548938	7.625114
-444.683787	-9.904968	7.635110
-442.657865	-9.260873	7.645107
-440.617954	-16.976769	7.655104
-439.010356	-13.013827	7.665101
-436.841286	-15.122845	7.675098
-435.460271	-15.887311	7.685094
-433.427185	-4.174095	7.695091
-431.182411	-16.255892	7.705088
-429.355518	-19.996139	7.715085
-427.877930	-15.975319	7.725082
-425.773683	-10.198174	7.735078
-424.058097	-7.100299	7.745075
-422.348879	-15.126216	7.755072
-420.173956	-10.741281	7.765069
-417.523348	-20.238037	7.775066
-416.377753	-15.716039	7.785062
-414.684748	-16.018662	7.795059
-412.709661	-23.560595	7.805056
-411.035669	-20.278526	7.815053
-408.927810	-15.817661	7.825050
-406.991180	-11.068950	7.835046
-405.234358	-16.723837	7.845043
-403.288423	-17.048900	7.855040
-401.337005	-16.369082	7.865037
-399.492926	-14.302222	7.875034
-397.409152	-19.689909	7.885030
-396.142673	-15.394153	7.895027
-394.038215	-15.738502	7.905024
-391.657713	-16.989399	7.915021
-389.997642	-13.099858	7.925018
-388.571094	-9.950014	7.935014
-386.342106	-12.577533	7.945011
-384.338935	-14.809040	7.955008
-382.990615	-8.912471	7.965005
-380.651658	-7.787321	7.975002
-378.675311	-13.119424	7.984998
-376.963942	-8.990877	7.994995
-375.179614	-14.566293	8.004992
-373.082050	-12.072600	8.014989
-371.366430	-18.140126	8.024986
-369.629609	-11.815785	8.034982
-367.793059	-10.300524	8.044979
-365.824798	-20.117312	8.054976
-363.975954	-14.122429	8.064973
-362.120267	-14.624462	8.074970
-360.108601	-9.288267	8.084966
-358.107679	-16.924725	8.094963
-356.552411	-13.948318	8.104960
-354.256060	-15.255109	8.114957
-352.555919	-17.908483	8.124954
-350.693020	-15.543677	8.134950
-348.714404	-12.903099	8.144947
-346.979669	-14.751030	8.154944
-345.061060	-22.117657	8.164941
-343.322381	-12.278191	8.174938
-341.552704	-12.885607	8.184934
-339.405970	-4.073734	8.194931
-337.831310	-12.131482	8.204928
-335.687198	-13.680500	8.214925
-333.872003	-9.665782	8.224922
-332.032752	-11.175942	8.234918
-329.954101	-16.194384	8.244915
-328.394068	-14.604406	8.254912
-326.083977	-11.022759	8.264909
-324.469202	-11.803971	8.274906
-322.914251	-17.324215	8.284902
-320.691365	-11.644036	8.294899
-318.484121	-16.475067	8.304896
-316.665806	-12.105579	8.314893
-315.041799	-11.532390	8.324890
-313.512649	-13.368757	8.334886
-311.544439	-16.076003	8.344883
-309.317199	-18.527710	8.354880
-307.717832	-11.251799	8.364877
-305.588068	-14.820261	8.374874
-303.552628	-9.429624	8.384870
-302.279735	-13.949014	8.394867
-300.307431	-12.096970	8.404864
-298.376468	-20.896773	8.414861
-296.114935	-8.284820	8.424858
-294.402103	-10.396140	8.434854
-292.054375	-12.386740	8.444851
-290.837440	-15.406570	8.454848
-289.103744	-11.584155	8.464845
-286.939112	-12.552147	8.474842
-285.043280	-6.321040	8.484838
-283.390118	-14.721451	8.494835
-281.373990	-13.291495	8.504832
-279.127663	-11.882447	8.514829
-277.276212	-8.084966	8.524826
-275.648820	-10.469737	8.534822
-273.793313	-11.000158	8.544819
-272.081023	-12.110298	8.554816
-269.961109	-14.971991	8.564813
-268.279284	-15.018123	8.574810
-266.687220	-14.185710	8.584807
-264.400793	-14.474262	8.594803
-262.483322	-18.069131	8.604800
-260.459837	-9.637615	8.614797
-258.898657	-18.587398	8.624794
-256.805391	-7.727791	8.634791
-254.691629	-11.549191	8.644787
-253.029770	-15.707266	8.654784
-251.304123	-12.718939	8.664781
-249.726819	-11.861855	8.674778
-247.310184	-12.912969	8.684775
-245.890418	-7.921789	8.694771
-243.518610	-14.478067	8.704768
-242.210349	-10.570016	8.714765
-240.020013	-11.306848	8.724762
-237.999041	-9.873355	8.734759
-236.635212	-10.979046	8.744755
-234.278904	-13.395944	8.754752
-232.344061	-15.253651	8.764749
-230.395223	-21.786381	8.774746
-228.778040	-21.800070	8.784743
-226.958392	-21.200726	8.794739
-224.994870	-16.735562	8.804736
-223.233741	-21.108654	8.814733
-221.294175	-20.483635	8.824730
-219.284014	-18.830517	8.834727
-217.548745	-16.448901	8.844723
-215.529733	-10.360614	8.854720
-213.835546	-8.303139	8.864717
-211.849175	-12.119271	8.874714
-210.024615	-18.050110	8.884711
-208.065606	-14.620022	8.894707
-206.399951	-15.513070	8.904704
-204.239887	-19.344363	8.914701
-202.562691	-15.883725	8.924698
-200.891344	-14.907984	8.934695
-198.907121	-9.795436	8.944691
-197.095670	-10.071261	8.954688
-194.843991	-13.487084	8.964685
-193.094609	-7.443046	8.974682
-191.099418	-11.922273	8.984679
-189.327879	-8.791608	8.994675
-187.488154	-13.785615	9.004672
-185.439219	-10.523490	9.014669
-184.026410	-7.347109	9.024666
-181.824306	-2.997137	9.034663
-180.078435	-6.969619	9.044659
-177.693308	-7.653275	9.054656
-176.445242	-1.335129	9.064653
-174.409886	-4.374356	9.074650
-172.617639	-9.926955	9.084647
-170.711579	-5.409223	9.094643
-168.834988	-6.197341	9.104640
-166.783405	-7.410290	9.114637
-164.645656	-9.679802	9.124634
-163.321167	-8.134734	9.134631
-161.172739	-3.127788	9.144627
-159.299262	-8.331901	9.154624
-157.541208	-7.022829	9.164621
-155.837194	-10.012337	9.174618
-153.571354	-10.188223	9.184615
-151.642064	-8.659924	9.194611
-149.956868	-8.525186	9.204608
-148.264802	-10.282336	9.214605
-146.309267	-9.009102	9.224602
-144.597977	-5.387108	9.234599
-142.381181	-4.902077	9.244595
-140.364007	-13.111146	9.254592
-138.774302	-12.828026	9.264589
-136.712589	-12.499382	9.274586
-135.144786	-9.266173	9.284583
-133.214262	-5.447803	9.294579
-131.193622	-3.521368	9.304576
-129.269390	-4.844463	9.314573
-127.399214	-2.917123	9.324570
-125.551301	1.361618	9.334567
-123.792542	1.965914	9.344563
-122.017003	0.252159	9.354560
-120.036028	-9.001576	9.364557
-117.798507	-6.741616	9.374554
-116.198784	-6.575214	9.384551
-114.352315	-7.779049	9.394547
-112.619143	-3.172359	9.404544
-110.459567	-10.244300	9.414541
-108.749462	-5.887776	9.424538
-106.925683	-5.126657	9.434535
-104.603048	-2.866267	9.444531
-103.224798	-6.901361	9.454528
-101.138104	-8.513146	9.464525
-99.195557	-8.225308	9.474522
-97.716217	-9.726222	9.484519
-95.704828	-7.255554	9.494515
-93.370376	-9.044195	9.504512
-92.020619	-8.081243	9.514509
-89.927938	-3.170617	9.524506
-88.212362	-7.273432	9.534503
-86.301116	-1.976788	9.544499
-84.088623	-2.486934	9.554496
-82.461670	-3.027092	9.564493
-80.578909	-4.489286	9.574490
-78.511307	-4.008675	9.584487
-76.756205	-2.582475	9.594483
-74.753876	-0.599520	9.604480
-73.532505	-11.048144	9.614477
-71.043375	-2.588869	9.624474
-69.039281	-3.820902	9.634471
-67.242354	-5.503129	9.644467
-65.810891	-8.592892	9.654464
-63.882195	-8.356808	9.664461
-61.956423	-12.794044	9.674458
-60.050243	-13.165892	9.684455
-57.917611	-6.953937	9.694451
-56.220367	-12.457008	9.704448
-54.165486	-7.490086	9.714445
-52.223013	-12.377567	9.724442
-50.433198	-10.394127	9.734439
-48.925049	-3.923717	9.744435
-46.868174	-1.684518	9.754432
-44.659417	-9.554508	9.764429
-43.126539	-8.570772	9.774426
-41.024808	-4.283348	9.784423
-39.425709	-7.379715	9.794419
-37.544810	-11.239347	9.804416
-35.604490	-4.564013	9.814413
-33.536573	-8.392082	9.824410
-31.717232	-7.075288	9.834407
-29.772023	-1.294767	9.844403
-27.910356	-6.321334	9.854400
-26.431532	-8.677385	9.864397
-24.205664	-7.440174	9.874394
-22.360117	-3.826526	9.884391
-20.340422	-1.059253	9.894387
-18.937909	-3.633420	9.904384
-16.804259	-6.850287	9.914381
-14.367853	-3.055762	9.924378
-13.020373	-2.835797	9.934375
-11.284225	-3.112074	9.944371
-9.402740	-10.120879	9.954368
-7.424157	-0.319607	9.964365
-5.832675	14.690209	9.974362
-4.656533	36.462283	9.984359
-2.949782	74.760352	9.994355
-1.023207	113.759095	10.004352
0.000000	143.213902	10.009357
0.410071	175.688667	10.014362
1.227683	199.814057	10.019367
1.591735	216.647894	10.024371
2.150404	230.924561	10.029376
2.542857	238.206144	10.034381
2.165734	251.057702	10.039386
2.528866	252.311066	10.044391
2.579119	253.510713	10.049395
2.560994	256.443052	10.054400
3.014007	265.510624	10.059405
2.771420	274.895618	10.064410
2.960348	288.302620	10.069415
3.404703	288.545397	10.074419
3.041415	292.925938	10.079424
3.497920	291.419214	10.084429
3.103168	289.493999	10.089434
3.278682	281.740882	10.094439
3.349612	270.993215	10.099443
2.989267	277.962597	10.104448
3.285813	292.170980	10.109453
3.403708	300.122139	10.114458
3.919412	303.263338	10.119463
3.824743	295.312604	10.124467
3.282646	288.228027	10.129472
3.485531	282.250791	10.134477
3.423602	306.063359	10.139482
3.597746	305.992878	10.144487
3.818242	312.736769	10.149491
3.411993	317.978856	10.154496
3.966742	314.819174	10.159501
3.673486	318.001979	10.164506
3.781109	321.976933	10.169511
4.220376	325.927786	10.174515
4.155642	328.522751	10.179520
4.133167	330.196301	10.184525
4.064867	323.138623	10.189530
3.998460	327.306831	10.194535
4.211941	321.454074	10.199539
4.151565	327.216308	10.204544
4.503522	318.658876	10.209549
4.201882	327.817589	10.214554
4.241130	325.670726	10.219559
4.161776	331.996716	10.224563
4.167575	337.121583	10.229568
4.309994	333.384466	10.234573
4.181806	329.770324	10.239578
4.260137	342.247036	10.244583
4.396330	339.453970	10.249587
4.219268	343.898512	10.254592
4.503807	350.033044	10.259597
4.955421	356.742459	10.264602
5.136581	358.698451	10.269607
4.964742	361.475200	10.274611
4.877895	351.764224	10.279616
4.704188	345.838903	10.284621
4.617702	355.122578	10.289626
5.243597	362.700890	10.294631
5.473142	357.018647	10.299635
5.199564	361.617895	10.304640
5.066996	347.980585	10.309645
4.948871	353.944959	10.314650
4.900248	353.111392	10.319655
5.511001	359.767470	10.324659
4.931960	359.157080	10.329664
5.343005	375.278851	10.334669
5.233465	389.379721	10.339674
5.229142	388.857885	10.344679
5.749303	385.895954	10.349683
5.153243	390.726549	10.354688
5.341161	389.651115	10.359693
5.365869	393.037565	10.364698
5.170114	391.686087	10.369703
5.364782	390.472922	10.374707
5.085986	394.810190	10.379712
5.884956	396.118306	10.384717
5.604879	404.476425	10.389722
6.126742	417.997764	10.394727
6.015861	412.504918	10.399731
6.111950	423.545812	10.404736
5.955447	414.297906	10.409741
5.400129	403.367008	10.414746
5.325390	409.268309	10.419751
5.875341	414.828432	10.424755
5.727534	423.157567	10.429760
5.805262	424.376989	10.434765
5.977621	425.732549	10.439770
5.983362	443.600268	10.444775
6.307403	445.951363	10.449779
6.167179	455.603903	10.454784
6.834358	453.339489	10.459789
6.526028	451.644953	10.464794
6.829756	455.461584	10.469799
6.912120	456.222336	10.474803
6.618044	460.161599	10.479808
7.002443	443.141212	10.484813
6.258773	447.529386	10.489818
6.529362	447.576969	10.494823
6.868927	459.083754	10.499827
6.765679	467.653553	10.504832
6.749068	469.572420	10.509837
7.089016	465.923373	10.514842
7.083622	467.505591	10.519847
7.176425	468.629277	10.524851
6.655496	481.353318	10.529856
7.042037	471.019934	10.534861
7.022509	475.436319	10.539866
6.992682	473.033262	10.544871
7.593143	471.268163	10.549875
7.372755	470.234706	10.554880
7.373357	459.369498	10.559885
7.448318	466.383138	10.564890
7.288978	472.161604	10.569895
7.659680	468.048615	10.574899
7.576101	475.489296	10.579904
7.596884	465.920841	10.584909
7.621944	475.340193	10.589914
7.477413	476.943110	10.594919
8.190032	477.116212	10.599923
7.506595	474.648386	10.604928
7.544385	469.265419	10.609933
7.579489	479.805643	10.614938
7.618648	474.430334	10.619943
7.249151	477.313622	10.624947
7.468032	482.186088	10.629952
7.885361	479.666888	10.634957
7.511907	481.656808	10.639962
7.781798	499.261808	10.644967
7.843244	506.090289	10.649971
7.621103	517.162918	10.654976
7.739455	515.455609	10.659981
7.665957	508.903590	10.664986
8.047253	516.449709	10.669991
8.138719	511.430934	10.674995
8.180814	537.809488	10.680000
8.610739	537.510814	10.685005
8.460163	546.829669	10.690010
8.228297	551.971672	10.695015
8.683867	541.170500	10.700019
8.489651	552.537962	10.705024
8.458724	543.151216	10.710029
8.488453	550.462771	10.715034
8.457889	554.302009	10.720039
8.943135	546.110799	10.725043
8.707834	548.448081	10.730048
9.039876	547.334110	10.735053
8.601562	542.354845	10.740058
8.678680	557.794347	10.745063
9.077582	558.530435	10.750067
8.613808	559.770874	10.755072
8.780463	557.760813	10.760077
8.992494	557.638837	10.765082
8.716389	552.122562	10.770087
8.944152	564.524490	10.775091
9.220222	575.493580	10.780096
9.209217	579.010927	10.785101
9.668476	581.845292	10.790106
9.317703	589.188160	10.795111
9.456094	582.589122	10.800115
9.437136	585.342461	10.805120
9.707395	584.293948	10.810125
9.522366	597.918884	10.815130
9.818638	589.012836	10.820135
9.819123	589.697241	10.825139
9.442277	592.975352	10.830144
9.955792	585.365442	10.835149
9.661005	584.125266	10.840154
9.800403	592.179859	10.845159
9.941456	591.320073	10.850163
9.950189	591.360055	10.855168
9.939069	589.445601	10.860173
9.807426	604.193068	10.865178
9.526498	603.100116	10.870183
9.998901	593.387835	10.875187
9.655212	597.845624	10.880192
9.909543	591.778926	10.885197
9.727583	587.939476	10.890202
9.770354	602.240995	10.895207
10.358396	613.060704	10.900211
10.125382	620.740623	10.905216
10.270897	626.093859	10.910221
10.494313	625.863749	10.915226
10.361500	627.167048	10.920231
10.387064	627.654923	10.925235
10.097520	634.969946	10.930240
10.827202	636.057076	10.935245
11.169591	636.409710	10.940250
10.707368	634.971665	10.945255
10.933364	628.429823	10.950259
10.985116	634.890163	10.955264
11.091893	631.022906	10.960269
10.993392	636.081677	10.965274
10.283784	625.355888	10.970279
10.975783	628.597582	10.975283
10.579621	633.586997	10.980288
10.616335	629.674517	10.985293
10.748785	639.447782	10.990298
11.011086	637.165923	10.995303
10.997311	642.316746	11.000307
10.689304	645.087287	11.005312
11.127298	650.032366	11.010317
10.901505	656.380438	11.015322
11.518197	667.047249	11.020327
11.749561	665.189103	11.025331
11.162973	674.216878	11.030336
11.121405	675.025337	11.035341
11.138767	675.126602	11.040346
11.146472	671.598025	11.045351
11.412591	671.062178	11.050355
11.077890	678.715351	11.055360
11.735135	667.182819	11.060365
11.666587	682.279533	11.065370
11.643014	685.937214	11.070375
11.695204	697.341479	11.075379
11.841628	711.411778	11.080384
12.235771	706.076575	11.085389
12.303745	708.463327	11.090394
11.993374	700.554896	11.095399
11.891053	692.017915	11.100403
11.961298	701.694913	11.105408
11.893997	699.684685	11.110413
12.237613	708.273917	11.115418
12.121086	716.295087	11.120423
12.235060	708.251922	11.125427
12.277517	724.631855	11.130432
12.452445	716.180349	11.135437
11.883852	720.043983	11.140442
12.405427	723.940564	11.145447
12.532133	718.231220	11.150451
12.222796	721.570412	11.155456
12.620796	719.522639	11.160461
12.162485	726.406781	11.165466
12.314111	721.223679	11.170471
12.398376	717.828014	11.175475
12.315862	722.048825	11.180480
12.735292	740.230814	11.185485
12.984239	744.732293	11.190490
12.854933	744.563053	11.195495
13.263359	748.665354	11.200499
12.891420	749.143626	11.205504
13.259679	750.351549	11.210509
13.228825	747.740208	11.215514
12.801660	742.671337	11.220519
12.845373	729.596747	11.225523
12.833477	752.243675	11.230528
13.140344	751.002168	11.235533
12.837277	752.367036	11.240538
13.057399	748.963861	11.245543
13.412950	749.725549	11.250547
13.013738	749.235488	11.255552
13.206928	747.714266	11.260557
13.366882	756.504354	11.265562
13.232165	772.222358	11.270567
13.590268	780.650464	11.275571
13.418737	788.394133	11.280576
13.781641	783.142022	11.285581
13.449552	785.388962	11.290586
13.511504	788.570167	11.295591
13.772438	785.483665	11.300595
13.356442	791.841115	11.305600
13.577845	785.697884	11.310605
13.533699	783.362364	11.315610
13.642849	786.955076	11.320615
13.992852	799.167682	11.325619
14.005169	813.640799	11.330624
14.456984	814.479143	11.335629
14.226046	810.995004	11.340634
14.350242	819.343238	11.345639
14.217856	800.612277	11.350643
13.868709	795.866323	11.355648
14.236162	813.196795	11.360653
14.696416	815.825774	11.365658
14.337652	815.077331	11.370663
14.691108	813.089288	11.375667
14.540004	820.477369	11.380672
14.776031	821.010874	11.385677
14.520422	808.293456	11.390682
14.473584	816.123915	11.395687
14.576673	811.440152	11.400691
14.456707	824.028616	11.405696
14.791039	815.135651	11.410701
14.711373	824.171333	11.415706
14.555941	829.305058	11.420711
14.801390	826.455279	11.425715
14.573858	835.910657	11.430720
14.631277	821.453261	11.435725
14.683195	832.631096	11.440730
14.336649	834.354343	11.445735
15.095667	843.721889	11.450739
15.090190	855.521416	11.455744
15.462761	858.213198	11.460749
15.585906	852.617309	11.465754
15.174285	861.470325	11.470759
15.508130	856.842508	11.475763
15.235619	858.358856	11.480768
15.704196	857.031193	11.485773
15.562973	859.858438	11.490778
15.463807	852.463579	11.495783
15.711724	839.148624	11.500787
15.433890	851.132606	11.505792
15.479440	857.061213	11.510797
15.886643	855.658022	11.515802
15.369066	855.092332	11.520807
15.749290	864.612468	11.525811
15.527702	865.540223	11.530816
15.618651	850.418637	11.535821
15.914053	860.786990	11.540826
15.805496	861.534708	11.545831
16.006296	859.700726	11.550835
15.862309	855.021023	11.555840
15.716266	857.622122	11.560845
16.210063	865.179913	11.565850
15.782940	869.326429	11.570855
15.925763	864.190183	11.575859
15.888141	879.201654	11.580864
15.997741	880.672619	11.585869
16.453994	883.123876	11.590874
16.250251	887.608673	11.595879
16.733385	887.295740	11.600883
16.341303	889.767715	11.605888
16.576189	897.960829	11.610893
16.645744	886.740872	11.615898
16.428907	897.929307	11.620903
16.640767	892.474113	11.625907
16.622085	898.332039	11.630912
16.495651	884.996362	11.635917
16.475880	891.382231	11.640922
16.382680	899.135813	11.645927
16.491908	889.317068	11.650931
16.522372	903.367555	11.655936
16.763022	910.195882	11.660941
16.567136	924.881245	11.665946
16.832105	914.245128	11.670951
16.983872	922.791189	11.675955
16.756404	924.616791	11.680960
17.432237	924.680947	11.685965
17.360038	928.966755	11.690970
17.382867	928.955769	11.695975
17.426906	919.714231	11.700979
17.263251	922.406781	11.705984
17.506016	921.706774	11.710989
17.235650	927.817863	11.715994
17.269744	919.867627	11.720999
17.591056	922.861892	11.726003
17.426042	921.846146	11.731008
17.844919	919.102010	11.736013
17.427482	922.822934	11.741018
17.391428	930.171999	11.746023
17.655497	925.867177	11.751027
17.613456	931.394386	11.756032
17.495399	941.408159	11.761037
18.019594	953.856677	11.766042
18.093213	952.819751	11.771047
18.351168	948.168604	11.776051
17.813800	948.265115	11.781056
18.349828	941.663670	11.786061
17.940987	939.567497	11.791066
17.586097	934.219724	11.796071
18.192702	940.504138	11.801075
18.453084	947.073310	11.806080
18.681543	942.263012	11.811085
18.395117	947.874365	11.816090
18.369577	940.093422	11.821095
18.538522	930.143623	11.826099
18.095247	932.001886	11.831104
18.597676	941.389012	11.836109
18.524002	942.463514	11.841114
18.311264	944.394356	11.846119
18.583551	947.022823	11.851123
18.609444	955.504036	11.856128
18.404196	946.888248	11.861133
18.859810	949.035679	11.866138
18.761004	948.461341	11.871143
18.652886	940.691398	11.876147
18.563206	957.847386	11.881152
18.680458	953.334835	11.886157
18.648946	946.111489	11.891162
18.499915	959.483858	11.896167
18.466655	967.244565	11.901171
18.861276	976.425988	11.906176
19.103465	981.728824	11.911181
19.408787	975.475210	11.916186
19.395222	981.909394	11.921191
19.499495	978.479453	11.926195
19.147328	989.506025	11.931200
19.208327	984.683374	11.936205
19.688033	981.248273	11.941210
19.055979	984.314827	11.946215
19.277554	979.682934	11.951219
19.306188	990.420402	11.956224
19.129891	990.158163	11.961229
19.665703	992.380271	11.966234
19.125117	981.967489	11.971239
19.863593	983.565507	11.976243
19.528144	1000.337760	11.981248
19.759736	997.990458	11.986253
19.985652	1007.447140	11.991258
19.815021	1007.890113	11.996263
20.095562	994.972458	12.001267
20.020886	1008.617909	12.006272
20.274424	1004.576976	12.011277
19.999711	1007.496608	12.016282
19.672197	998.948333	12.021287
20.121820	1004.732715	12.026291
20.041829	1009.130407	12.031296
20.341818	1003.430722	12.036301
20.043861	985.020428	12.041306
19.868627	993.238515	12.046311
20.174638	978.574141	12.051315
20.174045	981.372954	12.056320
20.106750	986.075961	12.061325
20.045005	983.813297	12.066330
19.701863	977.479419	12.071335
20.387802	975.064087	12.076339
20.180021	985.339588	12.081344
20.538401	986.962513	12.086349
20.367149	985.462307	12.091354
20.271736	993.362368	12.096359
20.156000	988.483571	12.101363
20.078980	996.869557	12.106368
20.205847	995.409025	12.111373
20.199900	985.815624	12.116378
19.671470	978.767463	12.121383
20.219593	979.318910	12.126387
19.933653	982.269278	12.131392
19.848785	968.104958	12.136397
20.044781	976.439781	12.141402
20.190221	980.800393	12.146407
20.248385	968.419439	12.151411
19.829226	967.371870	12.156416
19.941750	962.654864	12.161421
19.727953	962.022479	12.166426
19.702216	982.893043	12.171431
20.256301	981.140975	12.176435
20.189838	990.991197	12.181440
19.746166	979.028250	12.186445
20.142211	976.444334	12.191450
19.996060	984.330195	12.196455
19.955094	981.980285	12.201459
19.934049	989.333909	12.206464
20.196763	996.700464	12.211469
20.334559	995.341874	12.216474
20.054355	986.877073	12.221479
20.159939	974.573641	12.226483
19.872794	969.897528	12.231488
20.137323	980.119675	12.236493
20.244987	964.185511	12.241498
20.109607	965.520856	12.246503
19.844318	960.729683	12.251507
19.899914	976.269210	12.256512
19.982129	975.985543	12.261517
20.154292	968.208188	12.266522
19.588778	981.627117	12.271527
20.230110	972.308795	12.276531
19.636025	975.832257	12.281536
19.694511	972.093985	12.286541
19.990611	977.893628	12.291546
19.812621	985.161660	12.296551
20.349559	991.128435	12.301555
20.043050	986.155243	12.306560
19.885162	973.057778	12.311565
20.083921	979.288978	12.316570
20.020051	974.478266	12.321575
20.262051	968.537089	12.326579
19.986426	972.197395	12.331584
20.157061	964.654382	12.336589
20.147458	970.210385	12.341594
19.947379	968.496045	12.346599
19.991023	969.305698	12.351603
20.324031	966.278645	12.356608
20.023416	967.915084	12.361613
20.110031	969.455131	12.366618
19.905858	979.871324	12.371623
19.933534	971.714531	12.376627
19.541221	973.724718	12.381632
19.601321	975.390100	12.386637
19.842769	974.768869	12.391642
19.817035	975.612128	12.396647
20.418290	976.398018	12.401651
20.001488	978.987534	12.406656
20.025782	974.194074	12.411661
20.155839	976.550091	12.416666
19.617893	986.324439	12.421671
19.727309	968.053923	12.426675
19.876110	987.825625	12.431680
20.102999	1002.856600	12.436685
20.308944	1000.442642	12.441690
19.886514	990.094069	12.446695
20.098913	978.382187	12.451699
19.885273	979.433716	12.456704
20.668366	978.633170	12.461709
20.591615	981.164382	12.466714
20.219385	977.091801	12.471719
20.296505	981.804783	12.476723
20.029379	979.796018	12.481728
20.129960	979.718411	12.486733
19.902066	977.537525	12.491738
19.810388	983.784182	12.496743
20.224981	984.814444	12.501747
19.972062	988.032704	12.506752
19.941033	984.723065	12.511757
20.222962	974.990707	12.516762
19.770184	990.119256	12.521767
20.059686	981.567435	12.526771
19.931053	982.453206	12.531776
20.038679	980.831764	12.536781
20.160680	979.375226	12.541786
19.834266	988.384625	12.546791
20.377859	985.869356	12.551795
19.980242	987.583218	12.556800
19.798784	979.762672	12.561805
19.894469	988.704831	12.566810
20.083654	985.412698	12.571815
20.287684	975.648697	12.576819
20.179558	987.753685	12.581824
19.811758	969.761173	12.586829
19.998466	977.752196	12.591834
19.846011	981.893884	12.596839
20.099724	974.704121	12.601843
20.226527	986.957513	12.606848
20.121657	975.226610	12.611853
20.239913	973.677952	12.616858
20.198573	964.206685	12.621863
20.144947	953.646087	12.626867
19.879234	958.306528	12.631872
20.200067	962.194169	12.636877
20.132404	954.000047	12.641882
20.236513	963.954822	12.646887
19.933366	958.695274	12.651891
19.607569	962.123786	12.656896
19.952289	956.888946	12.661901
19.813283	958.113203	12.666906
19.853896	968.000710	12.671911
19.970501	958.381971	12.676915
19.717927	963.158187	12.681920
19.834962	962.659735	12.686925
19.696458	966.486791	12.691930
19.894619	984.196217	12.696935
20.123765	992.283392	12.701939
19.824493	999.574594	12.706944
20.186286	990.259191	12.711949
20.128528	994.129252	12.716954
20.106063	997.868921	12.721959
20.212029	990.752641	12.726963
20.014520	977.134993	12.731968
19.480189	972.460997	12.736973
19.955586	981.002522	12.741978
20.121948	1002.200175	12.746983
20.184052	988.494979	12.751987
20.043208	981.290362	12.756992
19.656778	986.881770	12.761997
20.199730	987.899893	12.767002
20.305147	995.551969	12.772007
20.147590	976.506955	12.777011
19.678803	980.490118	12.782016
19.880058	970.924752	12.787021
20.330973	974.431278	12.792026
20.071113	982.397818	12.797031
20.355862	973.359318	12.802035
20.152171	971.189678	12.807040
19.729608	968.411777	12.812045
20.017336	963.028023	12.817050
19.658859	971.599227	12.822055
20.193324	963.691072	12.827059
20.340605	973.109900	12.832064
19.953650	969.243134	12.837069
19.986841	964.905650	12.842074
19.849700	972.114963	12.847079
19.850814	969.122710	12.852083
20.105835	973.086769	12.857088
20.054787	969.992933	12.862093
20.138457	971.670458	12.867098
19.950520	970.621928	12.872103
19.966456	967.437267	12.877107
19.640112	976.822040	12.882112
19.526160	970.361632	12.887117
19.844759	981.477270	12.892122
19.710622	995.188168	12.897127
20.546780	995.361415	12.902131
20.510854	992.263009	12.907136
20.277767	983.532368	12.912141
20.056840	966.310069	12.917146
19.998847	973.100024	12.922151
20.296513	968.356404	12.927155
19.832322	979.153099	12.932160
19.957116	976.348059	12.937165
20.302545	971.483750	12.942170
20.189209	981.389372	12.947175
20.343366	978.628639	12.952179
20.490541	982.122903	12.957184
20.204022	978.740624	12.962189
20.351445	964.718058	12.967194
19.634593	957.858527	12.972199
19.865780	955.004066	12.977203
20.022489	979.613460	12.982208
19.634537	979.181065	12.987213
20.070666	972.571078	12.992218
19.519544	986.129252	12.997223
19.630936	979.281257	13.002227
19.493582	977.843529	13.007232
19.823899	980.335342	13.012237
20.104885	992.854802	13.017242
20.102212	985.508862	13.022247
20.253340	981.570756	13.027251
20.419244	978.313011	13.032256
20.321773	979.558569	13.037261
20.657082	978.975324	13.042266
20.020312	983.895181	13.047271
20.005848	963.177627	13.052275
19.750588	963.053664	13.057280
19.903522	971.917314	13.062285
20.170063	982.456486	13.067290
19.876838	980.424563	13.072295
20.130256	976.726289	13.077299
19.833131	985.729480	13.082304
19.785789	986.472629	13.087309
20.056775	990.755664	13.092314
19.621302	985.433927	13.097319
19.990555	984.837757	13.102323
20.219408	990.165382	13.107328
19.654780	981.736323	13.112333
20.188087	985.353857	13.117338
20.116858	989.450831	13.122343
20.202525	977.849889	13.127347
20.035303	984.981865	13.132352
19.979844	994.018231	13.137357
20.340691	981.650895	13.142362
19.789259	991.192691	13.147367
19.775743	982.013089	13.152371
20.617082	992.918319	13.157376
20.431321	977.358923	13.162381
20.364061	967.111706	13.167386
20.065405	966.260186	13.172391
20.127907	956.758882	13.177395
19.643795	957.210997	13.182400
19.265090	957.185963	13.187405
19.699939	954.756449	13.192410
20.042658	972.738312	13.197415
20.084609	987.165851	13.202419
20.058248	986.075012	13.207424
20.289530	987.241309	13.212429
20.065051	975.721572	13.217434
19.778595	971.604680	13.222439
19.849906	960.608579	13.227443
19.907183	963.348913	13.232448
19.940264	976.157969	13.237453
20.277913	972.668279	13.242458
20.018969	976.683356	13.247463
19.793640	963.728909	13.252467
19.871677	968.494625	13.257472
19.934589	989.927892	13.262477
20.004021	992.994173	13.267482
20.009101	997.928722	13.272487
20.173843	990.984338	13.277491
19.880542	985.703355	13.282496
19.896168	999.329763	13.287501
20.283713	996.809669	13.292506
19.922432	986.561930	13.297511
20.067437	977.804755	13.302515
20.099189	970.520419	13.307520
19.880970	971.461418	13.312525
19.970341	962.898921	13.317530
19.720453	968.733358	13.322535
19.901613	978.561642	13.327539
19.779898	991.711856	13.332544
19.832520	1001.184431	13.337549
20.280537	995.466474	13.342554
20.121539	1012.884275	13.347559
20.721678	999.664319	13.352563
20.075740	984.354343	13.357568
19.868592	977.172938	13.362573
19.980563	971.850500	13.367578
19.967536	978.110117	13.372583
20.081831	975.514904	13.377587
19.903177	975.618595	13.382592
19.588442	972.699838	13.387597
20.044676	975.674928	13.392602
19.911444	978.243455	13.397607
20.173721	977.621416	13.402611
19.946908	985.976238	13.407616
19.888548	977.462352	13.412621
20.040110	977.833899	13.417626
20.070671	983.247231	13.422631
19.788153	971.720474	13.427635
20.099093	980.986510	13.432640
20.192324	984.355418	13.437645
20.514784	973.443747	13.442650
20.104247	968.942737	13.447655
20.194820	976.339586	13.452659
19.751830	967.668233	13.457664
19.928655	965.963876	13.462669
20.478434	973.939620	13.467674
19.823946	983.922632	13.472679
20.410652	968.947246	13.477683
20.005947	974.512967	13.482688
19.954453	978.983527	13.487693
19.894787	966.521330	13.492698
19.808221	978.478931	13.497703
19.857659	978.518252	13.502707
19.835544	973.717749	13.507712
19.600438	980.222285	13.512717
19.739449	976.701126	13.517722
19.431649	981.376289	13.522727
20.019266	990.969103	13.527731
20.184379	1000.283048	13.532736
19.989287	1000.142847	13.537741
20.728182	1002.714216	13.542746
19.856588	992.430022	13.547751
19.898745	986.521129	13.552755
20.040505	979.636348	13.557760
19.809569	979.661766	13.562765
20.649709	970.919226	13.567770
19.891746	978.773009	13.572775
20.302346	981.529346	13.577779
20.226178	982.696252	13.582784
20.008810	985.071181	13.587789
19.891644	978.194479	13.592794
20.062068	985.548431	13.597799
20.324075	976.845407	13.602803
19.735085	979.056684	13.607808
20.050743	984.215872	13.612813
20.170152	975.475719	13.617818
19.867596	979.732747	13.622823
20.022581	979.562129	13.627827
20.008383	982.309195	13.632832
20.006694	985.965562	13.637837
20.080741	979.956862	13.642842
20.078873	986.929436	13.647847
19.822795	981.797599	13.652851
20.197878	981.820164	13.657856
20.177375	981.465293	13.662861
20.255027	981.527407	13.667866
19.941451	990.466711	13.672871
19.989447	980.998275	13.677875
20.117596	984.643827	13.682880
19.701619	982.940845	13.687885
20.032285	984.904047	13.692890
19.977888	985.604195	13.697895
20.213782	986.029967	13.702899
20.074970	977.349481	13.707904
20.205056	986.069819	13.712909
20.022578	984.920880	13.717914
19.772900	981.786493	13.722919
19.962686	983.350299	13.727923
20.012330	982.278008	13.732928
19.838454	981.870486	13.737933
20.330968	984.020675	13.742938
19.961642	989.806914	13.747943
19.988750	978.186407	13.752947
20.351704	980.727492	13.757952
19.710006	980.622023	13.762957
20.085548	970.498224	13.767962
19.958604	976.834214	13.772967
20.398940	976.185593	13.777971
19.972079	967.424632	13.782976
19.671457	963.786223	13.787981
20.094832	961.123018	13.792986
19.783162	969.257513	13.797991
20.324601	973.048516	13.802995
20.020502	958.819557	13.808000
19.577594	961.077232	13.813005
20.091723	972.126970	13.818010
19.930339	982.107145	13.823015
20.007786	985.683628	13.828019
20.254506	983.963733	13.833024
19.976726	982.879291	13.838029
19.777923	960.650324	13.843034
19.853780	980.892417	13.848039
19.821428	976.383405	13.853043
20.398753	984.112063	13.858048
20.206104	979.148956	13.863053
20.319942	956.421919	13.868058
19.508689	967.968898	13.873063
19.739467	962.049385	13.878067
20.166451	976.984843	13.883072
20.120935	981.048196	13.888077
19.861880	975.941740	13.893082
20.205154	981.068560	13.898087
20.106419	967.411880	13.903091
20.268629	967.827785	13.908096
19.696725	968.340742	13.913101
19.775297	959.799835	13.918106
19.979727	968.491628	13.923111
19.996162	972.881461	13.928115
20.213415	968.391628	13.933120
20.215204	973.989100	13.938125
19.797553	962.326046	13.943130
19.339337	967.436336	13.948135
19.959126	978.902962	13.953139
20.188762	984.325188	13.958144
20.216588	991.641224	13.963149
20.479146	975.536017	13.968154
20.095020	972.828104	13.973159
19.754075	968.452136	13.978163
19.751777	968.386248	13.983168
19.802233	966.563031	13.988173
19.741912	973.835752	13.993178
19.947426	992.258792	13.998183
20.162335	989.559484	14.003187
19.972326	982.518822	14.008192
19.879353	989.053334	14.013210
19.998133	988.496350	14.018227
19.873141	997.623588	14.023245
20.023503	989.320080	14.028263
19.957129	990.003195	14.033280
20.023698	1001.604858	14.038298
20.425665	994.918171	14.043315
20.237527	999.538983	14.048333
20.216723	1001.798258	14.053351
20.281983	996.051255	14.058368
19.936385	998.776091	14.063386
20.200605	991.323201	14.068403
20.417221	1003.270032	14.073421
20.536547	996.933794	14.078439
19.894468	982.309788	14.083456
20.098504	992.066485	14.088474
20.248339	991.272663	14.093491
20.455601	994.544485	14.098509
20.353811	1002.070782	14.103527
20.554411	990.829707	14.108544
20.399186	986.485963	14.113562
20.300888	987.442681	14.118579
20.224418	992.715653	14.123597
20.525372	994.477996	14.128615
20.503005	995.750461	14.133632
20.661611	993.651891	14.138650
20.723609	987.892850	14.143667
20.444951	971.480042	14.148685
20.417608	971.024889	14.153703
20.808583	968.531338	14.158720
20.075495	977.556513	14.163738
20.666081	979.241241	14.168755
20.771994	989.711660	14.173773
20.697260	973.979290	14.178791
20.480964	961.504899	14.183808
20.061895	977.283403	14.188826
20.540452	985.731915	14.193843
20.251530	991.742543	14.198861
20.765663	995.501553	14.203879
20.715464	994.044340	14.208896
20.488924	993.415451	14.213914
20.780764	994.287954	14.218931
20.650103	989.634464	14.223949
20.350005	997.717238	14.228967
20.236127	989.685824	14.233984
20.060926	998.032244	14.239002
20.683624	1014.016842	14.244019
20.620111	1023.944637	14.249037
20.605654	1024.736578	14.254055
21.067924	1020.155839	14.259072
20.716089	1029.452708	14.264090
20.747881	1029.516981	14.269107
20.458334	1030.879355	14.274125
20.602977	1034.917490	14.279143
20.915443	1029.304087	14.284160
20.963191	1036.189755	14.289178
21.054479	1027.914860	14.294195
20.751576	1035.613461	14.299213
20.791370	1048.797426	14.304231
21.261847	1051.436291	14.309248
21.017767	1051.817176	14.314266
21.440648	1061.860434	14.319283
21.172489	1044.876413	14.324301
20.963787	1036.393875	14.329319
20.993206	1037.815349	14.334336
21.094653	1062.084078	14.339354
21.342341	1062.904702	14.344371
21.545514	1060.550038	14.349389
21.198414	1047.970042	14.354407
21.100331	1037.097492	14.359424
20.904388	1060.891578	14.364442
21.315539	1054.833260	14.369459
21.425572	1063.855669	14.374477
21.348431	1063.434643	14.379495
21.236968	1058.932183	14.384512
21.412241	1058.584424	14.389530
21.312952	1062.161596	14.394547
21.554311	1059.630687	14.399565
21.430034	1060.162304	14.404583
21.836734	1055.257987	14.409600
21.616496	1052.907805	14.414618
21.553975	1040.719607	14.419635
21.222197	1041.356097	14.424653
21.125366	1061.342355	14.429671
21.285914	1060.614809	14.434688
21.253517	1059.988459	14.439706
21.056864	1063.287814	14.444723
21.533313	1062.631311	14.449741
21.688709	1061.402640	14.454759
21.819556	1064.774200	14.459776
21.590575	1055.218667	14.464794
22.107820	1064.654365	14.469811
22.373617	1068.878839	14.474829
22.152680	1062.472559	14.479847
22.261152	1054.847509	14.484864
21.875024	1046.433578	14.489882
22.023716	1039.065045	14.494899
21.873417	1025.658352	14.499917
21.403215	1031.184685	14.504935
21.695901	1026.143614	14.509952
21.899462	1028.474276	14.514970
21.725290	1025.192509	14.519987
21.909616	1042.605942	14.525005
21.781276	1050.572280	14.530023
21.885357	1055.192615	14.535040
22.039079	1064.490232	14.540058
21.545008	1065.757351	14.545075
22.257883	1063.037715	14.550093
21.875081	1063.167167	14.555111
22.079748	1063.182113	14.560128
21.496700	1070.477942	14.565146
21.828664	1060.091921	14.570163
21.803809	1056.345536	14.575181
21.934586	1067.971282	14.580199
22.252508	1056.652166	14.585216
22.211747	1065.820518	14.590234
21.897365	1067.260781	14.595251
21.677547	1057.244192	14.600269
22.107193	1060.074719	14.605287
21.986541	1052.877567	14.610304
21.972924	1065.818717	14.615322
22.557897	1081.610231	14.620339
22.115878	1082.940874	14.625357
22.427914	1090.606119	14.630375
22.520079	1084.041021	14.635392
22.345673	1070.247053	14.640410
22.343472	1072.602370	14.645427
22.364460	1064.110358	14.650445
22.147008	1078.308214	14.655463
22.611071	1087.955422	14.660480
22.557313	1083.901758	14.665498
22.454861	1075.491145	14.670515
22.210091	1069.724825	14.675533
22.516950	1089.548984	14.680551
22.930151	1087.739059	14.685568
22.841103	1083.627268	14.690586
22.005450	1073.876899	14.695603
22.834098	1067.514692	14.700621
22.632543	1068.171379	14.705639
22.433601	1065.031263	14.710656
22.283380	1074.034122	14.715674
22.454014	1089.025357	14.720691
22.628791	1082.878806	14.725709
22.704902	1090.891219	14.730727
22.858050	1084.921223	14.735744
22.866365	1087.640516	14.740762
22.951443	1089.096550	14.745779
23.098748	1083.672481	14.750797
22.563522	1096.159740	14.755815
23.284721	1084.829732	14.760832
23.161305	1080.860458	14.765850
22.735068	1064.826819	14.770867
22.869078	1064.685362	14.775885
22.580832	1074.778110	14.780903
22.829427	1083.336975	14.785920
23.045753	1097.646316	14.790938
23.015115	1091.317641	14.795955
23.270387	1089.439118	14.800973
23.219463	1080.931078	14.805991
22.917565	1067.127867	14.811008
22.737269	1072.165498	14.816026
22.908485	1080.524620	14.821043
23.114672	1090.542053	14.826061
23.036274	1091.544189	14.831079
23.079001	1089.420196	14.836096
23.126059	1091.281205	14.841114
23.142550	1099.666865	14.846131
23.365246	1101.929686	14.851149
23.221274	1101.621701	14.856167
23.361521	1094.428226	14.861184
23.469749	1099.156927	14.866202
23.143841	1101.439394	14.871219
23.490622	1101.363039	14.876237
23.277269	1105.355478	14.881255
23.349544	1094.092627	14.886272
23.353212	1097.142271	14.891290
23.009259	1097.206396	14.896307
23.556970	1085.894321	14.901325
23.324905	1097.785071	14.906343
23.245743	1090.678040	14.911360
23.451813	1088.570533	14.916378
23.468525	1099.178770	14.921395
23.574107	1091.458915	14.926413
23.482258	1099.739913	14.931431
23.395096	1091.171540	14.936448
23.486894	1098.265842	14.941466
23.300668	1094.390411	14.946483
23.817055	1091.074095	14.951501
23.440831	1097.848610	14.956519
23.917102	1096.034171	14.961536
23.838868	1091.833508	14.966554
24.167447	1096.967770	14.971571
24.173025	1093.609497	14.976589
23.883608	1101.477091	14.981607
23.682680	1091.277306	14.986624
23.644808	1096.068067	14.991642
23.566867	1097.975707	14.996659
24.043032	1095.204519	15.001677
23.617915	1093.608806	15.006695
23.613988	1090.909301	15.011712
23.688662	1091.513116	15.016730
23.733450	1087.064966	15.021747
23.513373	1084.786411	15.026765
23.277987	1095.796558	15.031783
23.563923	1099.709296	15.036800
23.674046	1098.371053	15.041818
23.841775	1122.399753	15.046835
24.111651	1113.418155	15.051853
23.844754	1114.328586	15.056871
23.770700	1114.341710	15.061888
24.065477	1120.358617	15.066906
24.041892	1121.717921	15.071923
24.292034	1111.478189	15.076941
24.175171	1124.422128	15.081959
24.279991	1114.503003	15.086976
23.888684	1116.965595	15.091994
23.524216	1116.952916	15.097011
24.094242	1113.376198	15.102029
23.899426	1127.309961	15.107047
24.304977	1135.178898	15.112064
24.258837	1142.430739	15.117082
24.175237	1153.871633	15.122099
24.583006	1149.433283	15.127117
24.579944	1148.619208	15.132135
25.021670	1146.580353	15.137152
24.699288	1126.100529	15.142170
24.470223	1127.370645	15.147187
24.763470	1116.214391	15.152205
24.543947	1118.367586	15.157223
24.658758	1115.679218	15.162240
24.785361	1112.382874	15.167258
24.467570	1114.347390	15.172275
24.802690	1111.170819	15.177293
24.294199	1104.553174	15.182311
24.553746	1113.299169	15.187328
24.715787	1115.428285	15.192346
24.646381	1125.334712	15.197363
24.384885	1115.345706	15.202381
24.470070	1122.553366	15.207399
24.271937	1115.945106	15.212416
24.437097	1119.580108	15.217434
24.566917	1140.649744	15.222451
24.957995	1143.126634	15.227469
25.030541	1153.346170	15.232487
24.927186	1150.777098	15.237504
24.888570	1136.561725	15.242522
24.592863	1143.254732	15.247539
24.708123	1141.484074	15.252557
25.029595	1149.720219	15.257575
24.622698	1139.050951	15.262592
24.926481	1140.532095	15.267610
25.045687	1143.650135	15.272627
25.054738	1133.429282	15.277645
25.204745	1143.886733	15.282663
24.753846	1142.842330	15.287680
24.680776	1141.204364	15.292698
24.757048	1139.067525	15.297715
25.277458	1141.166306	15.302733
24.843445	1155.442311	15.307751
25.020741	1157.147916	15.312768
25.416939	1173.440039	15.317786
25.403376	1173.995988	15.322803
25.481797	1162.211124	15.327821
25.367356	1152.151207	15.332839
25.168433	1148.976423	15.337856
25.501890	1149.760297	15.342874
25.127935	1155.488299	15.347891
25.312200	1157.659677	15.352909
25.716016	1169.602101	15.357927
25.226309	1163.760801	15.362944
25.478170	1169.134244	15.367962
24.882289	1173.166300	15.372979
25.485583	1169.843336	15.377997
25.183268	1182.550987	15.383015
25.365455	1184.836908	15.388032
25.648018	1168.299319	15.393050
25.581770	1181.409445	15.398067
26.115983	1176.660801	15.403085
25.699404	1174.584048	15.408103
25.453172	1171.185461	15.413120
25.666598	1169.760204	15.418138
25.448880	1179.723593	15.423155
25.595869	1168.548280	15.428173
25.878601	1174.603891	15.433191
25.753752	1179.354861	15.438208
25.986315	1166.671445	15.443226
25.789725	1172.584021	15.448243
25.620399	1170.103428	15.453261
25.467010	1169.201338	15.458279
25.895390	1169.970907	15.463296
26.010839	1166.637879	15.468314
25.969752	1172.145021	15.473331
26.076765	1161.619534	15.478349
25.914928	1162.652517	15.483367
25.675970	1162.932124	15.488384
26.059823	1161.020916	15.493402
26.348445	1166.622720	15.498419
26.090021	1163.478608	15.503437
25.784896	1169.577129	15.508455
26.233370	1167.226852	15.513472
26.562595	1154.930449	15.518490
26.416144	1166.046274	15.523507
26.192751	1158.878500	15.528525
26.494024	1161.612149	15.533543
26.262465	1164.421406	15.538560
26.319897	1163.666649	15.543578
26.497115	1162.136961	15.548595
26.417456	1164.089396	15.553613
26.309291	1161.136075	15.558631
26.398857	1163.145330	15.563648
26.526729	1159.045542	15.568666
26.249816	1166.179468	15.573683
26.211384	1170.380929	15.578701
26.603972	1165.781778	15.583719
26.307488	1164.219913	15.588736
26.216305	1161.421962	15.593754
25.813854	1166.382348	15.598771
25.983478	1167.890435	15.603789
26.290987	1184.661201	15.608807
26.471124	1190.055217	15.613824
26.866801	1190.363819	15.618842
26.538334	1187.885310	15.623859
26.889589	1186.313969	15.628877
27.024344	1186.326334	15.633895
26.617195	1189.134596	15.638912
26.948729	1191.397668	15.643930
26.989277	1189.860305	15.648947
27.071750	1184.401250	15.653965
26.953142	1179.534201	15.658983
26.438877	1167.274919	15.664000
26.929734	1171.175771	15.669018
26.979147	1189.922452	15.674035
27.022761	1187.575046	15.679053
26.973104	1175.387293	15.684071
26.393766	1169.526710	15.689088
26.971226	1178.509991	15.694106
27.087980	1183.905029	15.699123
27.127757	1188.170650	15.704141
27.190229	1185.053412	15.709159
26.952303	1195.110441	15.714176
27.296192	1187.763494	15.719194
27.229232	1185.175183	15.724211
27.040308	1194.648958	15.729229
27.286028	1190.156879	15.734247
27.420733	1195.998881	15.739264
27.591943	1180.564715	15.744282
26.982676	1167.477163	15.749299
26.925024	1171.398037	15.754317
27.259743	1182.738093	15.759335
27.250106	1192.045289	15.764352
27.177019	1196.823220	15.769370
27.095702	1195.853647	15.774387
27.294677	1187.885429	15.779405
27.605073	1189.421748	15.784423
26.903516	1194.409409	15.789440
27.469742	1191.334155	15.794458
27.542727	1190.823995	15.799475
27.527383	1185.608896	15.804493
27.486065	1187.789820	15.809511
27.216307	1197.503460	15.814528
27.817972	1191.707332	15.819546
27.386048	1196.096748	15.824563
27.809476	1186.799780	15.829581
27.844110	1191.666728	15.834599
27.650772	1192.968129	15.839616
27.866731	1189.787168	15.844634
27.964623	1195.320888	15.849651
27.722993	1193.892935	15.854669
27.640811	1201.744340	15.859687
27.376823	1202.073518	15.864704
27.861619	1206.533340	15.869722
27.677508	1217.184358	15.874739
27.876362	1223.302011	15.879757
28.112449	1222.699313	15.884775
28.018282	1227.618280	15.889792
27.773233	1217.468106	15.894810
27.890497	1224.169482	15.899827
28.203498	1217.925551	15.904845
28.172682	1213.941154	15.909863
27.883953	1230.985078	15.914880
28.052764	1221.263988	15.919898
28.230884	1215.813722	15.924915
28.133524	1213.586161	15.929933
28.815301	1214.404421	15.934951
28.358212	1220.967243	15.939968
28.161131	1217.231843	15.944986
28.238031	1215.264193	15.950003
28.015980	1217.405629	15.955021
28.392125	1219.831938	15.960039
28.188903	1225.401940	15.965056
27.996669	1215.921905	15.970074
28.073777	1223.705062	15.975091
27.946745	1217.220408	15.980109
28.635109	1209.494676	15.985127
28.504395	1214.339584	15.990144
28.355060	1217.997819	15.995162
28.382835	1218.236418	16.000179
28.406239	1218.866746	16.005197
28.611645	1220.011979	16.010215
28.247844	1232.395538	16.015232
28.477335	1242.429155	16.020250
28.681899	1240.375040	16.025267
28.620529	1245.454152	16.030285
29.010418	1245.433011	16.035303
28.919747	1256.718092	16.040320
28.736106	1252.434269	16.045338
28.580282	1248.505551	16.050355
28.554230	1248.330114	16.055373
28.748325	1250.793941	16.060391
28.912910	1251.790650	16.065408
29.038160	1242.558947	16.070426
29.120177	1240.828232	16.075443
29.071121	1251.218695	16.080461
29.017949	1240.361139	16.085479
28.849831	1247.390614	16.090496
28.776652	1240.640787	16.095514
28.939500	1250.661424	16.100531
28.808116	1245.816231	16.105549
29.187515	1248.906612	16.110567
29.055741	1250.722311	16.115584
28.911808	1246.354902	16.120602
29.027888	1252.295403	16.125619
28.866759	1250.492586	16.130637
29.159573	1247.832736	16.135655
29.352704	1258.949465	16.140672
29.286526	1260.128272	16.145690
29.800643	1270.024909	16.150707
29.340189	1256.914916	16.155725
29.546598	1246.474308	16.160743
29.460226	1251.564796	16.165760
29.679920	1245.604985	16.170778
29.623102	1239.313025	16.175795
29.054281	1245.467418	16.180813
29.434696	1241.426681	16.185831
29.375058	1249.154549	16.190848
29.421653	1257.310704	16.195866
29.780991	1264.432445	16.200883
29.299260	1274.292723	16.205901
29.887260	1257.094349	16.210919
29.862014	1270.397537	16.215936
30.163147	1266.480633	16.220954
29.739156	1248.616333	16.225971
29.716848	1241.328998	16.230989
29.592109	1237.439839	16.236007
29.481565	1244.639378	16.241024
29.840400	1258.916166	16.246042
29.812794	1269.562436	16.251059
30.275148	1273.841463	16.256077
29.910398	1264.008659	16.261095
29.872118	1275.647008	16.266112
30.017859	1269.564422	16.271130
30.381331	1260.678120	16.276147
29.849015	1256.578497	16.281165
30.130206	1255.233354	16.286183
29.962424	1264.787807	16.291200
30.239875	1272.785086	16.296218
30.166327	1265.475420	16.301235
30.240053	1268.317399	16.306253
30.520166	1265.570739	16.311271
30.000101	1260.485463	16.316288
30.373981	1267.148766	16.321306
30.485172	1259.406211	16.326323
30.183158	1257.262555	16.331341
29.986488	1254.660642	16.336359
30.078617	1269.406827	16.341376
29.965024	1261.092914	16.346394
30.160738	1266.700053	16.351411
30.059893	1269.269968	16.356429
30.140001	1260.685422	16.361447
30.410297	1276.007419	16.366464
30.009679	1274.340945	16.371482
30.485758	1289.463091	16.376499
30.558084	1304.173724	16.381517
30.714861	1302.304189	16.386535
30.473781	1300.994252	16.391552
30.130192	1302.882497	16.396570
30.459029	1302.210346	16.401587
30.559421	1306.516005	16.406605
30.934415	1296.152375	16.411623
30.926984	1299.560687	16.416640
30.793445	1312.199739	16.421658
30.576729	1303.216413	16.426675
30.649970	1307.272767	16.431693
30.777444	1302.822979	16.436711
30.860233	1309.511010	16.441728
30.647698	1304.259989	16.446746
31.102597	1313.604945	16.451763
30.915538	1335.427665	16.456781
31.109060	1322.464963	16.461799
30.921618	1333.843470	16.466816
31.175488	1329.313730	16.471834
31.316659	1329.198212	16.476851
31.189272	1333.473241	16.481869
31.229778	1327.207083	16.486887
31.506309	1334.363922	16.491904
31.174594	1329.762913	16.496922
31.536295	1327.878320	16.501939
31.192704	1330.403242	16.506957
31.498061	1325.044127	16.511975
31.498964	1331.164656	16.516992
31.590855	1326.299269	16.522010
31.738771	1302.702074	16.527027
31.323452	1301.253491	16.532045
31.202969	1296.506423	16.537063
31.208073	1296.422109	16.542080
31.589010	1323.395152	16.547098
32.032310	1325.871387	16.552115
31.680542	1323.367714	16.557133
31.546600	1308.173161	16.562151
31.531126	1306.988730	16.567168
31.368072	1318.804818	16.572186
31.392568	1315.704696	16.577203
31.612316	1327.403184	16.582221
31.846203	1325.029435	16.587239
31.697262	1328.085603	16.592256
31.529006	1331.484485	16.597274
31.740596	1318.951406	16.602291
31.510399	1332.469725	16.607309
31.972439	1324.926850	16.612327
31.848405	1317.091120	16.617344
31.361454	1319.031115	16.622362
32.255213	1332.809919	16.627379
31.997935	1346.932556	16.632397
32.102894	1341.123496	16.637415
32.314822	1350.289639	16.642432
32.184744	1339.466461	16.647450
32.396047	1330.724331	16.652467
31.980605	1333.455292	16.657485
31.985396	1328.411906	16.662503
31.940677	1341.336568	16.667520
31.684161	1361.974664	16.672538
32.398310	1345.724736	16.677555
32.073769	1355.816799	16.682573
32.112387	1363.437711	16.687591
32.542145	1360.706327	16.692608
32.566116	1359.200927	16.697626
32.384970	1352.407353	16.702643
32.416511	1351.097130	16.707661
32.420695	1347.292543	16.712679
32.241531	1352.358024	16.717696
32.126113	1359.110378	16.722714
32.763313	1367.571667	16.727731
32.891623	1383.588257	16.732749
32.546206	1374.176519	16.737767
32.768480	1367.188168	16.742784
32.465157	1384.121364	16.747802
33.027134	1381.119645	16.752819
32.948705	1394.786029	16.757837
32.983694	1379.143898	16.762855
32.777870	1364.679400	16.767872
32.619178	1377.874838	16.772890
33.302737	1381.452125	16.777907
33.173926	1374.301504	16.782925
32.489838	1357.740456	16.787943
33.136405	1371.984552	16.792960
33.266479	1376.220962	16.797978
33.186030	1362.267699	16.802995
33.188973	1362.581432	16.808013
32.831647	1350.599063	16.813031
32.960668	1357.069719	16.818048
32.817758	1376.713460	16.823066
33.423650	1378.923221	16.828083
33.307143	1379.336182	16.833101
33.352176	1378.195314	16.838119
33.333045	1383.031773	16.843136
33.129295	1377.568570	16.848154
33.242827	1378.586247	16.853171
33.669865	1385.413339	16.858189
33.054324	1374.926939	16.863207
33.526885	1381.331223	16.868224
33.153140	1386.395428	16.873242
33.481350	1376.456342	16.878259
33.246691	1378.354662	16.883277
32.806218	1376.982045	16.888295
33.109931	1380.670132	16.893312
33.279946	1399.013278	16.898330
33.594825	1406.076953	16.903347
33.321544	1406.731775	16.908365
33.561873	1415.853320	16.913383
33.851497	1406.374419	16.918400
34.004131	1416.378408	16.923418
34.157708	1414.088107	16.928435
33.877709	1415.652439	16.933453
33.861779	1411.003563	16.938471
33.647502	1405.830372	16.943488
33.359582	1412.845419	16.948506
33.873297	1408.667994	16.953523
33.832587	1412.803762	16.958541
33.857354	1427.508491	16.963559
34.044768	1432.594620	16.968576
34.257735	1438.592210	16.973594
34.165250	1430.091893	16.978611
34.509048	1433.769969	16.983629
34.360616	1437.649382	16.988647
34.719624	1433.303575	16.993664
34.430885	1422.380365	16.998682
34.524916	1409.321646	17.003699
34.181130	1406.542154	17.008717
34.231161	1411.092721	17.013735
34.716730	1407.380010	17.018752
34.482185	1412.458944	17.023770
34.198351	1401.456947	17.028787
34.326267	1410.561538	17.033805
34.365133	1425.637113	17.038823
34.167445	1419.297572	17.043840
34.283463	1431.248986	17.048858
34.709259	1429.095887	17.053875
34.659867	1429.126832	17.058893
34.566035	1436.888218	17.063911
34.629795	1428.468210	17.068928
34.751309	1429.216384	17.073946
34.783281	1427.573371	17.078963
35.068369	1427.366636	17.083981
34.794893	1429.751193	17.088999
34.934960	1433.709106	17.094016
34.903892	1439.054373	17.099034
34.889390	1433.361439	17.104051
34.853682	1433.112846	17.109069
34.778026	1432.508466	17.114087
34.370174	1427.245611	17.119104
34.716131	1445.869701	17.124122
35.190322	1461.476246	17.129139
35.005585	1460.438553	17.134157
34.915090	1463.783576	17.139175
35.730130	1462.952065	17.144192
35.232288	1471.630855	17.149210
35.475985	1467.185505	17.154227
35.692798	1464.163021	17.159245
35.100496	1466.393565	17.164263
35.523455	1454.481291	17.169280
35.459762	1463.556161	17.174298
35.471856	1458.952077	17.179315
35.634930	1455.537586	17.184333
35.576600	1464.317018	17.189351
35.580685	1457.307763	17.194368
35.442974	1460.601426	17.199386
36.349797	1437.041251	17.204403
37.003222	1420.144900	17.209421
36.281237	1404.411640	17.214439
36.677921	1394.281651	17.219456
36.435945	1387.764658	17.224474
36.071046	1373.185286	17.229491
36.088964	1358.478869	17.234509
35.933085	1360.376279	17.239527
36.130119	1354.884924	17.244544
36.271490	1360.864442	17.249562
36.360153	1356.899291	17.254579
36.316198	1359.398043	17.259597
36.238115	1363.749675	17.264615
36.192218	1361.360892	17.269632
36.120003	1361.294559	17.274650
36.120147	1359.936958	17.279667
36.559884	1366.389782	17.284685
35.959974	1348.504342	17.289703
36.435638	1340.790604	17.294720
36.332748	1345.655587	17.299738
36.418023	1338.993522	17.304755
36.862738	1330.235390	17.309773
36.222433	1328.170986	17.314791
36.047473	1323.504910	17.319808
36.245700	1335.221663	17.324826
36.254542	1353.123842	17.329843
36.812177	1361.833438	17.334861
36.317257	1361.765557	17.339879
36.466172	1359.990285	17.344896
36.152558	1362.784115	17.349914
36.395617	1358.985817	17.354931
36.868817	1362.518451	17.359949
36.532762	1363.837640	17.364967
36.609013	1361.899613	17.369984
36.536712	1364.202026	17.375002
36.285467	1365.337367	17.380019
36.588911	1364.488448	17.385037
36.525443	1366.670437	17.390055
36.794450	1378.368788	17.395072
36.850894	1396.374676	17.400090
36.502822	1395.127567	17.405107
37.145362	1393.604699	17.410125
37.017343	1394.996107	17.415143
36.861562	1391.311464	17.420160
37.074324	1394.909233	17.425178
36.849571	1392.497955	17.430195
37.204567	1389.284454	17.435213
36.896131	1395.256058	17.440231
36.956725	1391.155146	17.445248
37.107215	1398.659248	17.450266
36.590997	1410.884809	17.455283
37.416587	1422.045595	17.460301
37.366383	1433.693194	17.465319
37.022050	1430.614943	17.470336
37.092008	1426.227742	17.475354
37.116400	1429.038048	17.480371
37.282603	1430.471543	17.485389
37.007149	1432.493017	17.490407
37.508007	1448.612353	17.495424
37.487829	1457.910490	17.500442
37.621278	1459.914622	17.505459
38.099325	1453.391093	17.510477
37.793211	1457.120362	17.515495
38.548835	1458.286250	17.520512
38.230107	1449.806993	17.525530
37.951786	1441.148354	17.530547
38.127935	1428.472430	17.535565
38.326772	1433.036077	17.540583
38.200723	1425.049441	17.545600
37.740630	1427.817997	17.550618
38.023934	1427.924592	17.555635
38.165717	1424.172779	17.560653
37.960554	1431.388627	17.565671
37.564431	1431.673528	17.570688
38.283986	1431.717532	17.575706
37.534665	1439.497594	17.580723
38.118019	1448.236691	17.585741
38.053446	1453.529827	17.590759
38.198545	1453.384893	17.595776
38.171225	1452.410377	17.600794
38.041547	1455.515241	17.605811
38.499482	1459.491504	17.610829
38.399571	1460.959603	17.615847
38.199767	1460.215468	17.620864
38.507973	1460.304799	17.625882
38.433050	1466.098978	17.630899
38.452297	1452.735689	17.635917
38.076677	1475.166189	17.640935
38.117367	1481.886711	17.645952
38.469271	1486.718255	17.650970
38.435676	1497.808666	17.655987
38.654289	1482.796828	17.661005
38.595316	1498.461355	17.666023
38.419949	1491.051311	17.671040
39.018628	1495.911027	17.676058
39.493684	1499.838298	17.681075
39.368116	1489.363885	17.686093
39.181028	1499.871890	17.691111
38.955145	1484.787819	17.696128
38.814501	1487.726835	17.701146
38.786338	1495.540384	17.706163
39.224165	1489.717115	17.711181
38.931485	1496.899962	17.716199
39.364097	1499.778100	17.721216
39.417612	1500.011110	17.726234
38.997568	1502.816517	17.731251
39.404954	1503.806658	17.736269
39.454803	1515.825393	17.741287
39.117313	1512.758945	17.746304
39.194511	1516.739077	17.751322
38.882295	1515.649607	17.756339
39.265933	1507.875968	17.761357
38.729256	1509.542984	17.766375
39.236158	1516.673011	17.771392
39.614744	1531.256932	17.776410
39.786356	1538.882690	17.781427
39.722330	1538.391679	17.786445
39.426785	1535.372372	17.791463
39.634305	1541.004754	17.796480
39.809626	1544.926728	17.801498
39.191686	1549.867480	17.806515
39.417932	1533.519102	17.811533
39.495882	1539.874955	17.816551
39.707542	1557.132292	17.821568
40.279273	1568.313084	17.826586
40.729340	1570.956722	17.831603
40.297239	1549.997853	17.836621
40.101925	1549.957744	17.841639
40.078818	1540.522930	17.846656
40.500213	1534.991864	17.851674
40.132114	1534.195075	17.856691
39.963400	1526.930739	17.861709
40.368272	1542.917794	17.866727
40.435462	1550.716596	17.871744
40.218359	1564.833722	17.876762
40.485384	1563.883939	17.881779
40.683457	1558.583694	17.886797
40.701463	1562.601549	17.891815
40.428237	1560.918319	17.896832
40.901620	1556.199286	17.901850
40.389693	1554.714874	17.906867
40.562390	1554.945169	17.911885
40.656492	1553.926992	17.916903
40.633060	1564.799937	17.921920
40.639013	1562.630210	17.926938
40.516078	1569.418593	17.931955
40.837985	1560.740845	17.936973
40.617201	1564.133820	17.941991
40.688746	1568.050361	17.947008
41.043031	1568.004221	17.952026
40.593695	1568.364002	17.957043
40.649142	1572.382133	17.962061
40.937352	1566.660482	17.967079
40.854602	1574.244819	17.972096
41.305821	1587.130329	17.977114
40.979093	1596.037358	17.982131
41.172113	1599.831887	17.987149
41.110632	1593.248819	17.992167
41.449208	1603.740397	17.997184
41.373084	1590.739050	18.002202
41.299268	1602.364441	18.007219
41.466781	1590.473812	18.012237
41.365570	1600.781707	18.017255
41.196028	1596.046896	18.022272
41.641692	1591.302287	18.027290
41.597702	1593.212829	18.032307
41.290062	1591.894591	18.037325
41.643091	1591.036371	18.042343
40.992969	1591.673912	18.047360
41.622955	1593.058224	18.052378
41.635297	1609.013818	18.057395
41.588867	1613.982602	18.062413
42.059741	1616.106481	18.067431
41.977656	1616.130038	18.072448
42.216651	1613.390369	18.077466
42.265779	1617.075306	18.082483
42.289582	1608.155302	18.087501
42.444875	1600.399505	18.092519
41.874776	1596.920509	18.097536
42.104832	1579.597306	18.102554
41.982197	1584.491341	18.107571
42.510093	1600.415627	18.112589
42.314497	1604.794166	18.117607
42.174778	1616.716333	18.122624
42.253462	1611.574350	18.127642
42.051517	1614.866458	18.132659
42.538109	1614.590918	18.137677
42.514594	1607.052016	18.142695
42.335120	1613.848536	18.147712
42.802402	1608.793882	18.152730
42.438273	1616.996232	18.157747
42.607680	1618.698123	18.162765
42.382407	1609.872010	18.167783
42.301033	1617.927445	18.172800
42.755805	1611.212939	18.177818
42.516438	1612.555733	18.182835
42.386595	1611.112117	18.187853
42.475256	1610.510663	18.192871
42.600415	1634.509653	18.197888
42.908785	1635.641202	18.202906
42.891989	1646.526847	18.207923
42.817428	1654.325985	18.212941
43.312084	1652.223263	18.217959
42.592217	1650.179148	18.222976
42.918750	1643.766568	18.227994
42.955267	1648.662080	18.233011
42.777811	1644.571203	18.238029
42.966633	1650.095402	18.243047
42.786580	1661.763858	18.248064
43.544702	1669.406459	18.253082
43.345456	1682.349234	18.258099
43.728763	1685.480377	18.263117
43.897993	1678.502952	18.268135
43.667225	1673.365968	18.273152
43.975004	1665.329635	18.278170
43.722708	1662.768295	18.283187
43.671556	1655.554223	18.288205
43.558858	1637.559717	18.293223
43.536841	1650.921738	18.298240
43.748109	1652.320752	18.303258
43.948776	1652.045015	18.308275
44.062583	1664.961271	18.313293
43.981506	1648.594196	18.318311
43.685055	1639.745620	18.323328
43.837682	1656.964758	18.328346
43.772827	1669.554128	18.333363
43.899289	1671.925276	18.338381
43.945481	1665.197718	18.343399
43.974014	1679.633110	18.348416
44.393078	1680.526761	18.353434
43.952035	1671.663189	18.358451
43.963162	1684.985693	18.363469
43.990551	1679.102002	18.368487
43.774483	1675.183505	18.373504
44.133845	1686.150764	18.378522
44.297196	1696.392100	18.383539
44.419906	1695.019362	18.388557
44.727212	1696.490508	18.393575
45.141842	1704.583009	18.398592
44.999967	1688.606676	18.403610
44.926149	1680.737740	18.408627
44.853563	1667.325439	18.413645
44.777556	1665.009889	18.418663
44.479984	1664.887694	18.423680
44.677703	1653.898635	18.428698
44.292097	1666.190200	18.433715
44.870496	1685.189339	18.438733
44.882400	1692.540158	18.443751
44.800566	1703.688203	18.448768
44.922759	1698.465496	18.453786
45.070456	1692.474154	18.458803
44.795689	1698.388913	18.463821
44.931121	1692.922570	18.468839
44.940807	1693.726549	18.473856
45.217493	1688.058016	18.478874
44.753582	1698.499428	18.483891
44.870861	1690.974146	18.488909
45.367023	1704.975408	18.493927
45.056042	1710.786131	18.498944
45.530639	1714.155596	18.503962
45.758019	1718.794364	18.508979
45.495633	1715.055865	18.513997
45.796229	1712.155206	18.519015
45.632420	1723.816592	18.524032
45.561893	1707.605540	18.529050
45.613779	1712.386612	18.534067
45.496696	1719.730815	18.539085
46.036242	1715.943417	18.544103
45.701406	1720.182456	18.549120
45.623945	1716.713469	18.554138
45.844441	1714.043497	18.559155
45.808983	1720.923652	18.564173
46.295577	1720.820572	18.569191
45.935106	1720.273675	18.574208
46.274631	1717.038349	18.579226
46.165015	1723.455573	18.584243
46.084605	1715.345202	18.589261
46.283741	1714.038109	18.594279
45.876340	1720.034283	18.599296
45.860875	1724.107530	18.604314
46.490887	1737.945700	18.609331
46.097790	1745.920378	18.614349
46.438355	1749.579398	18.619367
46.264873	1750.967213	18.624384
46.433182	1743.470168	18.629402
46.784861	1739.880743	18.634419
46.305526	1750.991844	18.639437
46.354820	1748.994210	18.644455
46.111145	1755.737618	18.649472
46.392247	1764.796465	18.654490
46.475181	1774.472435	18.659507
46.288855	1775.824261	18.664525
46.747873	1775.317591	18.669543
46.545452	1775.646460	18.674560
46.520926	1773.793385	18.679578
47.026509	1783.754816	18.684595
47.115657	1795.203573	18.689613
47.788141	1791.679622	18.694631
47.134667	1787.292321	18.699648
46.950723	1776.404445	18.704666
47.203876	1780.828945	18.709683
47.586515	1788.660013	18.714701
47.470967	1779.295242	18.719719
47.484448	1774.827852	18.724736
47.602264	1773.844183	18.729754
47.442775	1775.921811	18.734771
47.410154	1769.393964	18.739789
47.750348	1764.189770	18.744807
47.521986	1769.143333	18.749824
47.035872	1768.950694	18.754842
47.851700	1780.436682	18.759859
47.755286	1793.857648	18.764877
48.306036	1801.871738	18.769895
47.729253	1804.973789	18.774912
47.946503	1803.070596	18.779930
48.062838	1804.169720	18.784947
47.789293	1805.029352	18.789965
48.327608	1800.560959	18.794983
48.038502	1808.856464	18.800000
47.975397	1803.131961	18.805018
48.304629	1803.671684	18.810035
48.327905	1813.450439	18.815053
48.411856	1808.323632	18.820071
48.307567	1809.544452	18.825088
48.311745	1810.064306	18.830106
48.074394	1800.829080	18.835123
48.106997	1802.387497	18.840141
48.474130	1807.188969	18.845159
47.972782	1803.864299	18.850176
47.892180	1804.993251	18.855194
48.159555	1800.974510	18.860211
48.208135	1819.876046	18.865229
48.417562	1818.480949	18.870247
48.234181	1824.475767	18.875264
48.371756	1830.470291	18.880282
48.665464	1825.707567	18.885299
48.756280	1846.615532	18.890317
48.958122	1846.166340	18.895335
48.985805	1859.334561	18.900352
48.829098	1859.431943	18.905370
48.946726	1851.702561	18.910387
48.968414	1857.493708	18.915405
49.011821	1848.116999	18.920423
49.293580	1854.109256	18.925440
48.935730	1849.419252	18.930458
49.411370	1848.828618	18.935475
49.043888	1848.505781	18.940493
49.174431	1846.936386	18.945511
49.347215	1849.444126	18.950528
49.525179	1870.953008	18.955546
49.745980	1869.106292	18.960563
49.700217	1885.206005	18.965581
49.876430	1879.962950	18.970599
50.005623	1859.344495	18.975616
49.637415	1860.600329	18.980634
49.969856	1843.497895	18.985651
49.876429	1846.638751	18.990669
49.949048	1857.563156	18.995687
49.793666	1840.311655	19.000704
50.066527	1844.444569	19.005722
50.179809	1840.264419	19.010739
49.821473	1842.222979	19.015757
50.015878	1852.882769	19.020775
50.393446	1847.472903	19.025792
50.296976	1849.949237	19.030810
50.787229	1837.931424	19.035827
50.199897	1835.588541	19.040845
50.451976	1831.258990	19.045863
50.043115	1834.338950	19.050880
50.565233	1841.798450	19.055898
50.485214	1849.072964	19.060915
50.445276	1851.872326	19.065933
50.721704	1859.234176	19.070951
50.798573	1857.168801	19.075968
50.322570	1864.653358	19.080986
50.835618	1858.048457	19.086003
50.572296	1863.388407	19.091021
50.679343	1862.901524	19.096039
50.523037	1856.477927	19.101056
50.551292	1864.624550	19.106074
50.582117	1865.042188	19.111091
50.676435	1871.058319	19.116109
50.773150	1884.308438	19.121127
51.024504	1889.548737	19.126144
50.835550	1901.587843	19.131162
51.450489	1895.621054	19.136179
51.169257	1894.536087	19.141197
51.120051	1893.637746	19.146215
51.008301	1891.938213	19.151232
51.084419	1902.516335	19.156250
51.350594	1900.004271	19.161267
51.384896	1912.093702	19.166285
51.361022	1919.640156	19.171303
52.327275	1923.141937	19.176320
52.003784	1921.359790	19.181338
52.256981	1902.715555	19.186355
51.539904	1903.737467	19.191373
51.644135	1893.135578	19.196391
51.899969	1893.827671	19.201408
52.095548	1902.233852	19.206426
52.433777	1896.986246	19.211443
52.231524	1904.081717	19.216461
52.102579	1891.357714	19.221479
51.785339	1889.373686	19.226496
51.829422	1898.629961	19.231514
52.288315	1900.252720	19.236531
52.163795	1907.830599	19.241549
52.129494	1916.312819	19.246567
52.451759	1913.836811	19.251584
52.628417	1918.631599	19.256602
52.350934	1914.259730	19.261619
52.303817	1921.063616	19.266637
52.317193	1918.514565	19.271655
52.419533	1911.417779	19.276672
52.130595	1926.480345	19.281690
52.536350	1917.843544	19.286707
52.211011	1929.087837	19.291725
52.000810	1934.482097	19.296743
52.777133	1943.375818	19.301760
52.507261	1948.567687	19.306778
52.543801	1943.842718	19.311795
52.684747	1953.044224	19.316813
52.851600	1964.704223	19.321831
53.205410	1960.940344	19.326848
52.987412	1970.315621	19.331866
53.013954	1973.388684	19.336883
53.328399	1971.896817	19.341901
53.557080	1967.708267	19.346919
53.778457	1966.595005	19.351936
53.258865	1957.488401	19.356954
53.689995	1955.634753	19.361971
54.006327	1959.117245	19.366989
54.187030	1948.516383	19.372007
54.199411	1930.533957	19.377024
53.907239	1930.515964	19.382042
54.092224	1925.092627	19.387059
53.907673	1931.414108	19.392077
54.111697	1931.981997	19.397095
54.144624	1914.993443	19.402112
53.945979	1928.126106	19.407130
54.129148	1925.454230	19.412147
54.303699	1922.735401	19.417165
54.027190	1921.197987	19.422183
53.929272	1921.551468	19.427200
53.987615	1932.375603	19.432218
54.257215	1932.510935	19.437235
53.753022	1928.198012	19.442253
53.952643	1933.519646	19.447271
54.301507	1934.057584	19.452288
54.320874	1953.754159	19.457306
54.142852	1956.414987	19.462323
54.146406	1955.163851	19.467341
54.124569	1963.298638	19.472359
54.092484	1956.915128	19.477376
54.850459	1975.883048	19.482394
54.840030	1983.034261	19.487411
54.675247	1998.076397	19.492429
54.736681	1999.264487	19.497447
55.069765	1993.668864	19.502464
55.001299	1993.663311	19.507482
55.150629	1990.164829	19.512499
55.036114	1992.970702	19.517517
55.139936	1988.744490	19.522535
55.395425	1985.332941	19.527552
54.886163	1993.808434	19.532570
55.110128	1983.183593	19.537587
54.953699	1986.048232	19.542605
54.906581	1988.058584	19.547623
55.494872	1986.850913	19.552640
55.478389	2001.256914	19.557658
55.519352	2007.250351	19.562675
55.727740	2015.913094	19.567693
55.763298	2007.403109	19.572711
55.914238	2003.703534	19.577728
55.776224	2011.268813	19.582746
55.873323	2008.280139	19.587763
55.551190	2005.388936	19.592781
55.200070	2016.532972	19.597799
55.400224	2003.629996	19.602816
55.239168	2012.386791	19.607834
55.514482	2026.082459	19.612851
55.641252	2038.866863	19.617869
55.791487	2035.117000	19.622887
56.196317	2033.008761	19.627904
56.052505	2049.197903	19.632922
56.181748	2056.477587	19.637939
56.779446	2054.609151	19.642957
56.457214	2058.577577	19.647975
56.669158	2061.054224	19.652992
56.828695	2057.435457	19.658010
56.658988	2058.681687	19.663027
57.197400	2053.150460	19.668045
56.816028	2045.719558	19.673063
56.564341	2033.895345	19.678080
56.773818	2038.673125	19.683098
56.841651	2052.540628	19.688115
56.864578	2054.058991	19.693133
56.842168	2052.513044	19.698151
56.920381	2056.885321	19.703168
56.938271	2063.159546	19.708186
57.206242	2064.171266	19.713203
57.425956	2055.357596	19.718221
57.804852	2061.543939	19.723239
57.908202	2055.479736	19.728256
57.474555	2057.251600	19.733274
57.379354	2047.571718	19.738291
57.725035	2049.425745	19.743309
57.607038	2048.395075	19.748327
57.558079	2044.243474	19.753344
57.543054	2046.690125	19.758362
57.527267	2052.848843	19.763379
57.759737	2061.146408	19.768397
57.697219	2056.763631	19.773415
57.779506	2052.566295	19.778432
57.578059	2055.874946	19.783450
57.664449	2060.962459	19.788467
58.238693	2068.427701	19.793485
58.110018	2086.770103	19.798503
58.188700	2078.766932	19.803520
58.202511	2079.873809	19.808538
58.267008	2090.965148	19.813555
58.269640	2080.083659	19.818573
58.334151	2084.601621	19.823591
58.646609	2081.341724	19.828608
58.553534	2078.666783	19.833626
58.470978	2084.986195	19.838643
58.270538	2079.256391	19.843661
58.180456	2090.106083	19.848679
58.241065	2090.946240	19.853696
58.025394	2099.025341	19.858714
58.558385	2103.471651	19.863731
59.362082	2102.738532	19.868749
59.062611	2109.450706	19.873767
59.216135	2120.859133	19.878784
59.297781	2113.318102	19.883802
59.340632	2113.417103	19.888819
59.308714	2110.774985	19.893837
59.468073	2110.146036	19.898855
59.669567	2109.284634	19.903872
59.195205	2112.967300	19.908890
58.933506	2113.750103	19.913907
59.455731	2114.057510	19.918925
59.286335	2117.863507	19.923943
59.246651	2112.125424	19.928960
59.254746	2115.500933	19.933978
59.490301	2121.844178	19.938995
60.022558	2123.413827	19.944013
59.719311	2150.228792	19.949031
59.834910	2148.140988	19.954048
59.547583	2147.000346	19.959066
59.207146	2139.707283	19.964083
59.527256	2134.924977	19.969101
59.494840	2149.976852	19.974119
59.841255	2158.558128	19.979136
59.839426	2166.102102	19.984154
59.725921	2173.124989	19.989171
60.252892	2164.167228	19.994189
60.015995	2168.921169	19.999207
60.457899	2173.465018	20.004224
60.715326	2188.223894	20.009242
60.811508	2202.132345	20.014259
60.872022	2192.729266	20.019277
60.499564	2194.634375	20.024295
60.700160	2191.938992	20.029312
60.902193	2193.458949	20.034330
61.062986	2198.172279	20.039347
61.343772	2190.645894	20.044365
61.109493	2193.988160	20.049383
61.545101	2185.861133	20.054400
61.096960	2168.345637	20.059418
60.959539	2162.540028	20.064435
61.222115	2166.142036	20.069453
60.947437	2176.997054	20.074471
61.102689	2180.356011	20.079488
61.393016	2180.908720	20.084506
61.372482	2189.624589	20.089523
61.809100	2183.003126	20.094541
61.738124	2191.911924	20.099559
61.359389	2175.676050	20.104576
61.435424	2187.187589	20.109594
61.575135	2188.682005	20.114611
61.896577	2175.494275	20.119629
61.346677	2176.152451	20.124647
61.792100	2177.446399	20.129664
61.982554	2187.242007	20.134682
61.812701	2203.564926	20.139699
62.013528	2202.120870	20.144717
61.656967	2218.611268	20.149735
61.642763	2213.580698	20.154752
61.787888	2209.270168	20.159770
61.923202	2217.908145	20.164787
62.320868	2233.069069	20.169805
62.260287	2248.922051	20.174823
62.551109	2245.211825	20.179840
62.700500	2238.274173	20.184858
62.330752	2243.258818	20.189875
62.491670	2230.683692	20.194893
62.767240	2244.968574	20.199911
63.158438	2240.365416	20.204928
62.889164	2239.831213	20.209946
62.980708	2241.748916	20.214963
63.081611	2230.605555	20.219981
62.832308	2232.257236	20.224999
62.725260	2235.247726	20.230016
62.938093	2241.983951	20.235034
62.775177	2256.585002	20.240051
62.909745	2261.238270	20.245069
63.275696	2263.404251	20.250087
63.433789	2268.055850	20.255104
63.676555	2268.916764	20.260122
62.997421	2272.788928	20.265139
63.525230	2270.887168	20.270157
63.830582	2289.435358	20.275175
63.683437	2301.076596	20.280192
64.436258	2291.160215	20.285210
63.828093	2287.229246	20.290227
64.122236	2274.654081	20.295245
63.863472	2278.970791	20.300263
63.642762	2292.595806	20.305280
63.931459	2295.783854	20.310298
64.038516	2296.414453	20.315315
64.245764	2289.399919	20.320333
64.012011	2294.017117	20.325351
63.865525	2297.467994	20.330368
64.226889	2298.914181	20.335386
64.117095	2311.498777	20.340403
64.614133	2315.789083	20.345421
64.459645	2318.097851	20.350439
64.724024	2319.296847	20.355456
64.308355	2311.862246	20.360474
64.515821	2320.980113	20.365491
64.894814	2316.335711	20.370509
64.574522	2323.095647	20.375527
64.448448	2322.787322	20.380544
65.283953	2334.316815	20.385562
65.352154	2340.439195	20.390579
65.392280	2344.669241	20.395597
65.219185	2330.097432	20.400615
65.675059	2333.153660	20.405632
65.420914	2311.608050	20.410650
65.224944	2314.115297	20.415667
65.064082	2328.158495	20.420685
65.360015	2336.849328	20.425703
65.348142	2334.518745	20.430720
65.725189	2333.625659	20.435738
65.489669	2350.667975	20.440755
65.467839	2343.286328	20.445773
65.832072	2340.710919	20.450791
65.526674	2339.445781	20.455808
65.817496	2351.406519	20.460826
65.826802	2364.774016	20.465843
65.856586	2366.134516	20.470861
65.880370	2359.324661	20.475879
66.065974	2369.923705	20.480896
66.169603	2362.963131	20.485914
66.298350	2369.569709	20.490931
66.365929	2360.333062	20.495949
66.332693	2380.942879	20.500967
66.084050	2394.851556	20.505984
66.822884	2391.759874	20.511002
66.633485	2399.812573	20.516019
66.527738	2397.152351	20.521037
66.873677	2391.931611	20.526055
66.702018	2403.631467	20.531072
67.016466	2388.749208	20.536090
66.904657	2404.703271	20.541107
66.753993	2394.661364	20.546125
67.081668	2403.688579	20.551143
67.099763	2412.850779	20.556160
67.724537	2414.128175	20.561178
67.654452	2428.396096	20.566195
67.572962	2418.390353	20.571213
66.962616	2401.923043	20.576231
67.129846	2421.344814	20.581248
67.448740	2413.790526	20.586266
67.748508	2417.636651	20.591283
67.668369	2426.040771	20.596301
67.993674	2421.241738	20.601319
67.827845	2430.019665	20.606336
67.926598	2418.622167	20.611354
68.078017	2424.761815	20.616371
68.097284	2416.325673	20.621389
68.357689	2410.128091	20.626407
67.984142	2415.257559	20.631424
68.223291	2414.735411	20.636442
68.282161	2415.978312	20.641459
68.131299	2420.459267	20.646477
68.448462	2430.075010	20.651495
68.024557	2453.646077	20.656512
68.605235	2448.379560	20.661530
68.745856	2462.890174	20.666547
68.896983	2450.613451	20.671565
68.936196	2445.519308	20.676583
68.744531	2464.354525	20.681600
68.680560	2459.289094	20.686618
68.990811	2451.089707	20.691635
69.110156	2451.806409	20.696653
68.866821	2453.510641	20.701671
68.858076	2452.196208	20.706688
68.536163	2455.326744	20.711706
68.632465	2478.169184	20.716723
68.721246	2479.325059	20.721741
68.822039	2481.778303	20.726759
69.045079	2499.272959	20.731776
69.335751	2509.232720	20.736794
69.938626	2511.097442	20.741811
70.260652	2497.368308	20.746829
70.374047	2501.186554	20.751847
70.125157	2506.030855	20.756864
70.491502	2494.358253	20.761882
70.284114	2482.510748	20.766899
70.037120	2471.218166	20.771917
70.135608	2459.903375	20.776935
70.094549	2488.529391	20.781952
70.478209	2486.261705	20.786970
70.192017	2491.844015	20.791987
70.367322	2496.318687	20.797005
70.419557	2487.798101	20.802023
70.223658	2492.586849	20.807040
70.636663	2489.172207	20.812058
70.723477	2500.022174	20.817075
70.366238	2492.740488	20.822093
70.584068	2493.997094	20.827111
70.497711	2507.506331	20.832128
70.673556	2512.920444	20.837146
70.547650	2521.941226	20.842163
70.494094	2524.429603	20.847181
70.887304	2521.120728	20.852199
70.358093	2536.896050	20.857216
70.972473	2544.670051	20.862234
71.020703	2556.282707	20.867251
70.901047	2555.192828	20.872269
71.538354	2560.516816	20.877287
71.360883	2578.459032	20.882304
71.743922	2577.457012	20.887322
71.891729	2582.201824	20.892339
71.838894	2583.437113	20.897357
72.010221	2583.553468	20.902375
71.713085	2580.461379	20.907392
72.166422	2577.157935	20.912410
72.389390	2578.945255	20.917427
72.516375	2577.198809	20.922445
72.589479	2568.705316	20.927463
72.436883	2568.615743	20.932480
72.142078	2559.752184	20.937498
72.266525	2563.610291	20.942515
72.638555	2569.702722	20.947533
72.769708	2571.391590	20.952551
72.330279	2579.788874	20.957568
72.641371	2564.411664	20.962586
72.363374	2568.920758	20.967603
72.359586	2572.721311	20.972621
73.010157	2567.067118	20.977639
72.742086	2571.718631	20.982656
72.751668	2565.649832	20.987674
73.172848	2589.017151	20.992691
72.561920	2598.494424	20.997709
73.250722	2602.363677	21.002727
73.193603	2603.696570	21.007744
73.572908	2602.125011	21.012762
73.681626	2600.727425	21.017779
73.364868	2608.979262	21.022797
73.792637	2611.497750	21.027815
73.730892	2602.736755	21.032832
73.922075	2603.298604	21.037850
73.878985	2604.951982	21.042867
73.498231	2609.314109	21.047885
73.884641	2604.330499	21.052903
73.305835	2611.964944	21.057920
73.812173	2620.586786	21.062938
73.933994	2633.380005	21.067955
73.752044	2636.047920	21.072973
74.178952	2621.169787	21.077991
74.386544	2639.225615	21.083008
74.571536	2661.315977	21.088026
74.563348	2663.950956	21.093043
74.843117	2662.155469	21.098061
75.210371	2658.390304	21.103079
74.718850	2655.240171	21.108096
75.092556	2650.808428	21.113114
75.154696	2644.703024	21.118131
74.875531	2646.500049	21.123149
75.382204	2653.662537	21.128167
75.174991	2656.565537	21.133184
75.062458	2656.506109	21.138202
74.974898	2658.727847	21.143219
74.819530	2666.511022	21.148237
74.807417	2660.388416	21.153255
74.851037	2669.237673	21.158272
75.241398	2680.968961	21.163290
75.467756	2684.499334	21.168307
75.502518	2693.183951	21.173325
75.460281	2689.867792	21.178343
75.308253	2690.671195	21.183360
75.909314	2709.541694	21.188378
76.035665	2720.269266	21.193395
75.889344	2715.141478	21.198413
76.323973	2718.463679	21.203431
76.256381	2713.924866	21.208448
76.446827	2712.730621	21.213466
76.308317	2710.633543	21.218483
76.491827	2710.836803	21.223501
76.927602	2695.642063	21.228519
76.776689	2709.299574	21.233536
76.858987	2707.177241	21.238554
76.855618	2707.784262	21.243571
76.845771	2712.134018	21.248589
77.031329	2709.076492	21.253607
76.340548	2696.311519	21.258624
76.500006	2703.068120	21.263642
76.782390	2706.745613	21.268659
76.692370	2708.536206	21.273677
77.335136	2719.528061	21.278695
77.352037	2727.465229	21.283712
77.487690	2724.259535	21.288730
77.595643	2724.823844	21.293747
77.109498	2732.537754	21.298765
77.533920	2731.030902	21.303783
77.713802	2730.500005	21.308800
77.538185	2728.041503	21.313818
77.513472	2727.742568	21.318835
77.222003	2756.327736	21.323853
77.792197	2754.526550	21.328871
77.440029	2763.034190	21.333888
77.812521	2764.447014	21.338906
78.147916	2767.246769	21.343923
77.748773	2782.673204	21.348941
78.237820	2779.632938	21.353959
78.053152	2779.059795	21.358976
78.312552	2789.592919	21.363994
78.467519	2787.973961	21.369011
78.507799	2804.762358	21.374029
78.922785	2814.519865	21.379047
79.004410	2814.536619	21.384064
79.221238	2811.735967	21.389082
79.271612	2813.389882	21.394099
78.950619	2812.859798	21.399117
79.539121	2805.385110	21.404135
79.635074	2813.423751	21.409152
79.458737	2809.176834	21.414170
79.992919	2800.252132	21.419187
79.731145	2792.470383	21.424205
80.085859	2771.118237	21.429223
79.805981	2754.961680	21.434240
79.978737	2752.924639	21.439258
79.991143	2752.327160	21.444275
79.628740	2756.197115	21.449293
79.916818	2751.732771	21.454311
80.341955	2760.821453	21.459328
80.130230	2765.596457	21.464346
80.454552	2747.936850	21.469363
79.990186	2761.960802	21.474381
80.085593	2772.585033	21.479399
80.366899	2782.539487	21.484416
80.530913	2790.711357	21.489434
80.650735	2780.008541	21.494451
80.251509	2795.712221	21.499469
80.490384	2789.077942	21.504487
80.592020	2789.307054	21.509504
80.725506	2793.384969	21.514522
80.545395	2783.024965	21.519539
80.908652	2793.166201	21.524557
81.949973	2793.794158	21.529575
81.558240	2784.394229	21.534592
81.499214	2786.055084	21.539610
81.783558	2777.183466	21.544627
81.367513	2784.961774	21.549645
81.044615	2775.323236	21.554663
81.394037	2778.136339	21.559680
81.228655	2803.960885	21.564698
81.479080	2809.878160	21.569715
81.610487	2814.389589	21.574733
81.472632	2820.245065	21.579751
81.685309	2813.346713	21.584768
81.663083	2821.907289	21.589786
81.751033	2828.326531	21.594803
81.789286	2842.914114	21.599821
81.791836	2837.429991	21.604839
82.217289	2853.238847	21.609856
81.948371	2864.427272	21.614874
82.298983	2876.948350	21.619891
82.189075	2872.745943	21.624909
82.491631	2876.562566	21.629927
82.809952	2877.273527	21.634944
82.609996	2878.437193	21.639962
82.933506	2882.953510	21.644979
83.069035	2901.681964	21.649997
83.341778	2898.403903	21.655015
83.406552	2893.747051	21.660032
83.212725	2904.005917	21.665050
83.505046	2897.437249	21.670067
83.404134	2900.863117	21.675085
83.572287	2905.644704	21.680103
83.288830	2900.816798	21.685120
83.336864	2905.219689	21.690138
83.548149	2892.283363	21.695155
83.346465	2907.092490	21.700173
83.786053	2912.519804	21.705191
84.020345	2919.072293	21.710208
83.751953	2928.819447	21.715226
83.971837	2924.113942	21.720243
83.978753	2922.244709	21.725261
83.780541	2925.080847	21.730279
84.450807	2944.956501	21.735296
84.224953	2953.228372	21.740314
84.334213	2955.016330	21.745331
84.742447	2958.402175	21.750349
84.748027	2959.836969	21.755367
84.962741	2945.862011	21.760384
84.525331	2952.752550	21.765402
85.088100	2950.569076	21.770419
84.878736	2952.397483	21.775437
84.898687	2953.157239	21.780455
85.068045	2962.190657	21.785472
85.541379	2971.479901	21.790490
85.434599	2974.362589	21.795507
85.467838	2981.202379	21.800525
85.659121	2978.915627	21.805543
85.964517	2968.847142	21.810560
85.537156	2982.086837	21.815578
85.867670	2979.676196	21.820595
85.540819	2980.170148	21.825613
85.817708	2976.850407	21.830631
85.834460	2966.951118	21.835648
85.816079	2975.278788	21.840666
86.065101	2991.325158	21.845683
86.103102	3003.418734	21.850701
86.236357	3003.857433	21.855719
86.224210	3003.219263	21.860736
86.296745	3011.099783	21.865754
86.758431	2990.250365	21.870771
86.950150	2995.297285	21.875789
87.149013	2988.720187	21.880807
87.276006	2981.383606	21.885824
87.115626	2986.994924	21.890842
86.991733	2980.958299	21.895859
87.453613	2980.596414	21.900877
86.982498	2980.202319	21.905895
87.728770	2990.274868	21.910912
87.817453	3001.023266	21.915930
87.517757	2992.817124	21.920947
87.764581	2992.535424	21.925965
87.440374	3001.966143	21.930983
87.892774	3007.337740	21.936000
87.605501	3014.515228	21.941018
88.104302	3001.372796	21.946035
88.383248	3001.336820	21.951053
87.793714	3003.891959	21.956071
88.216571	2999.201250	21.961088
88.382780	3005.817427	21.966106
88.405466	3007.867527	21.971123
88.686051	2998.315978	21.976141
88.255695	3000.738294	21.981159
88.285371	3000.989197	21.986176
88.327434	3015.399085	21.991194
88.460004	3024.391592	21.996211
88.517896	3029.845009	22.001229
88.901938	3028.340328	22.006247
89.427467	3018.186031	22.011264
88.552927	3025.615417	22.016282
88.793575	3036.613433	22.021299
89.564491	3048.520750	22.026317
89.394084	3058.130688	22.031335
89.436474	3053.503616	22.036352
89.399236	3062.269299	22.041370
89.394012	3058.174905	22.046387
89.349693	3060.086075	22.051405
89.245892	3065.324655	22.056423
89.499691	3064.870069	22.061440
89.401914	3083.839568	22.066458
89.598842	3081.478590	22.071475
89.941410	3085.752280	22.076493
89.917992	3093.079883	22.081511
90.302699	3094.889152	22.086528
90.512868	3116.423757	22.091546
90.542702	3104.288605	22.096563
90.855743	3104.709084	22.101581
90.542197	3111.883244	22.106599
90.917753	3110.456405	22.111616
90.766906	3105.453700	22.116634
91.011851	3101.793670	22.121651
91.112737	3099.810647	22.126669
90.903226	3105.686389	22.131687
91.109067	3105.327444	22.136704
91.260040	3128.799386	22.141722
91.162873	3128.621550	22.146739
91.571642	3134.898496	22.151757
91.236855	3131.254367	22.156775
91.535037	3129.894346	22.161792
91.579619	3134.735779	22.166810
91.589814	3132.054766	22.171827
92.209738	3148.329897	22.176845
92.091221	3156.362166	22.181863
92.172193	3150.025731	22.186880
92.246297	3159.689108	22.191898
92.409037	3151.427229	22.196915
92.718381	3140.670412	22.201933
92.382604	3146.835589	22.206951
92.561749	3139.773518	22.211968
92.464827	3138.103989	22.216986
92.498675	3149.778617	22.222003
92.787136	3143.167980	22.227021
93.106809	3161.840760	22.232039
93.249097	3159.630113	22.237056
93.195417	3171.248095	22.242074
93.209106	3175.741219	22.247091
93.329289	3170.897583	22.252109
93.156350	3172.670153	22.257127
93.478429	3167.397333	22.262144
93.578700	3168.266190	22.267162
93.304179	3169.055177	22.272179
93.583785	3161.318253	22.277197
93.441427	3175.738642	22.282215
93.970627	3185.138934	22.287232
93.976473	3199.278764	22.292250
94.175788	3185.796102	22.297267
94.276461	3186.696393	22.302285
94.272643	3197.095352	22.307303
94.324371	3183.277288	22.312320
94.458259	3189.000468	22.317338
94.358352	3188.015055	22.322355
94.489200	3184.598236	22.327373
94.871493	3211.979513	22.332391
95.445237	3213.520117	22.337408
95.399317	3199.951899	22.342426
95.140388	3191.659118	22.347443
95.123071	3181.908084	22.352461
95.229389	3189.923090	22.357479
95.195403	3200.791889	22.362496
94.947524	3212.362862	22.367514
95.052201	3218.706940	22.372531
95.276024	3210.612549	22.377549
95.025352	3219.861463	22.382567
95.615343	3237.389330	22.387584
95.884588	3250.790199	22.392602
95.641629	3244.035930	22.397619
95.759811	3237.909663	22.402637
95.407948	3259.328175	22.407655
96.164454	3262.583500	22.412672
96.433780	3266.591783	22.417690
96.655889	3280.919068	22.422707
96.752777	3276.526735	22.427725
96.377382	3283.402059	22.432743
96.845290	3271.068813	22.437760
96.973657	3278.446875	22.442778
97.008629	3273.552448	22.447795
97.129507	3263.183842	22.452813
97.266099	3270.888908	22.457831
96.646334	3270.766797	22.462848
97.189967	3281.812276	22.467866
97.576887	3295.320596	22.472883
97.531313	3286.341439	22.477901
97.813074	3290.535039	22.482919
98.032263	3286.589555	22.487936
98.410457	3278.632479	22.492954
98.142995	3276.867736	22.497971
98.581339	3272.408201	22.502989
98.604795	3274.733067	22.508007
98.485105	3275.104090	22.513024
98.766485	3263.093443	22.518042
99.108492	3258.493702	22.523059
99.079357	3238.354222	22.528077
98.702587	3240.752423	22.533095
98.671932	3231.068226	22.538112
98.956349	3228.044057	22.543130
99.125514	3235.313508	22.548147
98.860501	3228.876480	22.553165
98.744003	3236.720215	22.558183
98.906931	3249.601399	22.563200
99.120880	3247.204401	22.568218
98.984108	3258.589395	22.573235
99.236660	3253.971913	22.578253
98.984314	3265.747672	22.583271
99.262585	3271.556390	22.588288
99.883732	3284.262962	22.593306
99.448907	3287.817829	22.598323
99.667591	3281.603433	22.603341
99.911063	3302.893164	22.608359
99.741897	3292.225368	22.613376
99.892550	3292.056235	22.618394
100.121307	3308.465539	22.623411
100.067861	3319.566153	22.628429
99.993055	3324.184752	22.633447
100.174737	3324.638785	22.638464
100.359796	3323.174493	22.643482
100.286382	3340.871340	22.648499
100.745023	3346.750761	22.653517
100.460795	3345.444891	22.658535
100.495222	3337.220664	22.663552
100.993464	3362.388927	22.668570
101.414208	3372.619131	22.673587
101.328764	3380.405633	22.678605
101.367793	3379.757888	22.683623
101.331363	3379.141980	22.688640
101.914359	3362.541524	22.693658
101.664948	3374.501154	22.698675
102.009014	3359.278183	22.703693
101.995623	3376.348107	22.708711
102.335289	3382.978811	22.713728
102.750436	3381.712128	22.718746
102.694624	3371.138257	22.723763
103.098072	3352.588622	22.728781
102.369007	3348.590681	22.733799
102.563834	3344.479242	22.738816
102.696268	3358.169859	22.743834
102.766105	3380.381788	22.748851
102.863200	3378.078048	22.753869
103.317441	3378.486144	22.758887
103.507817	3376.804351	22.763904
103.384723	3381.688783	22.768922
103.270630	3384.284546	22.773939
103.388338	3375.687673	22.778957
103.415619	3378.133185	22.783975
103.592413	3379.924578	22.788992
103.696154	3373.148619	22.794010
103.183778	3373.497182	22.799027
103.476111	3391.899272	22.804045
103.920882	3398.984511	22.809063
103.948227	3401.652114	22.814080
104.199689	3397.257662	22.819098
104.133679	3396.380623	22.824115
104.436502	3405.286668	22.829133
104.438254	3417.638016	22.834151
104.656472	3427.645439	22.839168
105.306431	3413.831723	22.844186
104.948420	3433.346370	22.849203
105.408640	3426.141474	22.854221
105.693969	3418.394782	22.859239
104.857311	3399.634762	22.864256
105.515951	3400.644968	22.869274
105.451403	3409.381661	22.874291
105.910173	3407.892489	22.879309
105.716296	3397.567517	22.884327
105.506108	3387.177616	22.889344
106.292705	3394.464940	22.894362
105.623021	3394.793216	22.899379
105.865230	3390.674430	22.904397
106.068642	3402.335929	22.909415
106.505577	3405.637409	22.914432
106.739658	3397.848319	22.919450
106.611298	3411.188327	22.924467
106.719229	3405.898587	22.929485
106.602287	3407.212662	22.934503
106.283570	3398.840236	22.939520
107.062770	3399.435984	22.944538
106.455510	3406.530680	22.949555
106.536814	3402.738756	22.954573
107.054216	3414.250349	22.959591
107.258887	3424.805886	22.964608
107.177912	3428.375728	22.969626
107.122717	3430.133654	22.974643
107.021485	3427.307876	22.979661
107.404889	3429.709670	22.984679
107.264527	3454.359074	22.989696
107.593754	3460.837235	22.994714
107.294984	3464.761819	22.999731
107.534538	3458.113756	23.004749
107.679086	3482.391450	23.009767
107.826879	3485.767719	23.014784
108.075996	3486.533106	23.019802
108.009725	3500.596573	23.024819
108.223656	3509.752618	23.029837
108.248896	3521.845630	23.034855
107.894519	3529.130152	23.039872
108.411679	3527.586854	23.044890
108.573006	3540.191321	23.049907
108.776241	3548.449799	23.054925
109.235098	3557.074790	23.059943
109.158671	3569.738942	23.064960
109.375531	3568.384164	23.069978
109.607236	3573.474822	23.074995
109.557211	3578.428697	23.080013
109.570587	3577.642787	23.085031
109.496893	3586.645776	23.090048
110.469637	3595.682808	23.095066
110.030809	3596.470054	23.100083
110.403459	3593.114867	23.105101
110.480623	3597.836657	23.110119
111.169438	3601.439962	23.115136
111.983064	3567.015210	23.120154
111.733217	3541.565462	23.125171
111.939524	3533.664504	23.130189
112.225853	3512.747587	23.135207
111.755421	3499.225109	23.140224
112.097615	3493.741599	23.145242
111.814042	3478.785205	23.150259
111.811026	3463.669679	23.155277
111.634348	3459.568344	23.160295
111.598476	3464.659947	23.165312
111.666361	3453.864767	23.170330
111.682854	3459.548316	23.175347
111.573858	3457.772136	23.180365
111.938538	3461.701905	23.185383
111.645710	3467.003740	23.190400
112.361771	3478.091470	23.195418
112.037006	3485.739484	23.200435
112.048395	3495.639857	23.205453
112.082680	3488.752892	23.210471
111.790013	3502.923694	23.215488
112.425679	3510.326734	23.220506
112.154090	3524.853081	23.225523
112.469224	3521.202187	23.230541
112.585270	3540.233239	23.235559
112.443331	3558.473700	23.240576
112.732724	3556.096801	23.245594
112.962526	3569.512582	23.250611
112.918977	3581.277983	23.255629
113.238827	3587.751504	23.260647
113.132867	3593.043397	23.265664
113.534337	3614.936537	23.270682
113.954905	3618.925285	23.275699
113.896993	3616.801665	23.280717
113.948350	3624.336434	23.285735
113.939264	3631.527153	23.290752
114.152943	3640.118614	23.295770
113.918855	3649.617753	23.300787
114.205319	3658.078607	23.305805
114.463907	3647.065518	23.310823
114.577064	3659.604305	23.315840
115.043264	3670.715318	23.320858
115.469793	3678.147990	23.325875
115.467480	3681.472064	23.330893
115.448296	3672.627566	23.335911
115.821995	3661.625448	23.340928
116.078245	3649.684186	23.345946
116.295823	3654.609536	23.350963
116.381117	3642.220306	23.355981
116.926163	3642.427760	23.360999
116.185772	3623.687195	23.366016
116.191646	3624.358036	23.371034
116.132317	3617.987184	23.376051
116.571544	3613.377763	23.381069
116.930621	3611.585116	23.386087
116.501780	3615.280794	23.391104
117.023054	3626.088563	23.396122
116.437282	3608.566689	23.401139
116.380582	3629.865794	23.406157
116.616311	3635.747312	23.411175
116.418917	3638.885083	23.416192
116.892934	3630.006462	23.421210
116.584669	3648.612630	23.426227
116.882040	3672.688786	23.431245
117.000298	3677.021573	23.436263
117.200810	3696.135207	23.441280
117.549649	3700.425320	23.446298
117.630703	3702.295384	23.451315
117.452882	3701.354799	23.456333
117.885818	3710.599431	23.461351
118.072009	3726.953463	23.466368
118.316432	3733.254890	23.471386
118.282650	3730.221383	23.476403
117.848388	3732.213660	23.481421
118.225829	3737.133683	23.486439
118.147306	3749.450221	23.491456
118.546694	3754.691764	23.496474
119.166151	3766.709087	23.501491
119.043678	3780.227969	23.506509
119.634015	3794.001924	23.511527
119.556418	3795.162792	23.516544
119.714342	3786.561164	23.521562
119.983869	3787.924793	23.526579
120.113976	3778.144965	23.531597
120.540706	3760.670659	23.536615
120.778776	3763.334488	23.541632
120.905464	3759.694581	23.546650
120.866585	3737.684014	23.551667
120.721452	3722.863536	23.556685
120.795430	3722.347614	23.561703
120.716928	3726.637749	23.566720
120.728480	3722.542669	23.571738
121.018516	3720.172724	23.576755
120.884142	3733.176158	23.581773
121.151052	3738.506565	23.586791
120.916138	3758.677055	23.591808
121.063563	3765.505487	23.596826
120.984894	3758.216405	23.601843
121.060642	3764.452250	23.606861
121.278085	3773.109298	23.611879
120.996244	3779.805764	23.616896
121.139443	3786.801113	23.621914
121.797288	3798.064448	23.626931
121.637027	3811.120427	23.631949
122.034811	3818.964496	23.636967
122.262965	3834.257637	23.641984
121.997776	3836.345383	23.647002
122.335927	3835.578605	23.652019
122.300024	3839.595259	23.657037
122.657617	3846.145115	23.662055
122.950278	3872.097663	23.667072
122.991494	3865.424362	23.672090
123.134971	3867.365655	23.677107
122.993711	3873.054345	23.682125
123.086891	3863.750206	23.687143
123.375774	3882.318073	23.692160
123.309048	3888.748514	23.697178
123.526840	3889.208189	23.702195
123.675786	3890.857134	23.707213
124.135135	3902.155361	23.712231
124.833662	3918.944730	23.717248
124.515000	3903.560764	23.722266
124.890158	3890.698704	23.727283
124.435675	3902.200061	23.732301
124.809214	3901.063340	23.737319
124.683499	3916.131325	23.742336
124.695446	3912.876503	23.747354
125.099262	3919.906781	23.752371
124.562797	3924.359753	23.757389
125.079248	3920.450577	23.762407
125.544545	3938.889029	23.767424
125.388733	3944.079321	23.772442
125.612656	3949.002100	23.777459
125.206709	3949.953059	23.782477
125.565285	3950.226354	23.787495
125.468986	3964.690761	23.792512
125.885642	3977.050179	23.797530
126.263994	3977.259439	23.802547
126.272734	3989.576169	23.807565
126.693614	3984.027021	23.812583
126.573420	3988.970213	23.817600
126.758325	3995.455223	23.822618
127.365871	3985.913976	23.827635
126.970955	3992.368430	23.832653
127.619604	3991.060098	23.837671
127.525291	3987.644689	23.842688
127.495400	3986.387311	23.847706
127.714598	3986.161528	23.852723
127.802760	3990.540517	23.857741
127.949889	3976.082404	23.862759
127.821748	3982.992039	23.867776
127.909445	4000.544654	23.872794
128.251065	4007.172139	23.877811
128.161907	4005.538991	23.882829
128.788617	4008.059051	23.887847
129.139943	4000.141664	23.892864
128.853917	4000.848386	23.897882
128.904816	3994.536458	23.902899
128.894618	3999.093771	23.907917
129.233523	3990.810705	23.912935
129.360698	3996.195872	23.917952
129.633998	4000.499019	23.922970
129.868152	3991.047770	23.927987
129.489389	4004.037402	23.933005
129.434810	4007.728080	23.938023
129.921307	4017.407924	23.943040
129.863082	4026.942511	23.948058
130.203060	4025.031014	23.953075
130.002052	4020.991199	23.958093
130.175643	4014.407770	23.963111
130.462422	4017.635098	23.968128
130.502506	4023.232895	23.973146
130.693818	4034.727601	23.978163
130.540992	4048.017997	23.983181
130.266771	4046.183436	23.988199
130.110042	4047.641429	23.993216
130.530268	4059.565539	23.998234
130.956321	4069.855939	24.003251
131.039683	4073.355222	24.008269
131.246038	4091.798077	24.013287
131.593217	4099.444609	24.018304
131.148095	4108.246931	24.023322
131.956709	4104.099384	24.028339
132.043110	4128.096625	24.033357
132.527956	4117.746187	24.038375
132.839257	4121.558470	24.043392
132.629035	4120.921919	24.048410
132.790626	4123.250796	24.053427
132.889439	4126.843531	24.058445
132.929698	4120.983893	24.063463
133.109940	4112.321554	24.068480
132.638991	4115.482686	24.073498
133.611219	4121.343668	24.078515
133.778961	4142.014276	24.083533
133.511245	4139.591028	24.088551
134.013150	4141.770991	24.093568
133.803688	4142.218069	24.098586
134.102194	4137.122248	24.103603
134.110312	4143.666769	24.108621
134.203572	4148.799464	24.113639
134.020603	4136.606271	24.118656
133.965085	4151.311957	24.123674
134.335078	4155.100009	24.128691
134.333303	4165.441761	24.133709
134.647089	4177.807160	24.138727
134.867131	4193.744737	24.143744
134.545869	4193.623419	24.148762
135.417161	4199.901057	24.153779
135.237030	4202.752436	24.158797
135.470612	4214.325090	24.163815
135.483854	4224.938399	24.168832
135.564536	4227.704902	24.173850
135.876083	4219.641427	24.178867
136.137742	4233.765110	24.183885
135.967111	4246.044268	24.188903
136.655080	4237.974538	24.193920
136.562330	4236.501080	24.198938
137.102751	4241.096391	24.203955
137.194603	4230.777020	24.208973
137.563150	4240.763917	24.213991
137.722396	4231.142640	24.219008
137.508102	4237.625300	24.224026
137.602503	4230.160620	24.229043
137.934284	4225.342609	24.234061
137.831567	4230.174189	24.239079
138.011511	4224.689890	24.244096
137.622151	4230.043181	24.249114
138.255305	4231.486286	24.254131
138.394617	4234.801950	24.259149
138.400567	4224.005834	24.264167
138.070762	4219.869116	24.269184
137.684455	4226.673467	24.274202
138.075736	4230.677635	24.279219
137.799730	4243.522251	24.284237
138.246345	4252.586071	24.289255
138.602222	4273.299423	24.294272
138.469327	4277.647077	24.299290
139.023124	4289.646130	24.304307
139.504099	4296.701946	24.309325
139.751900	4297.772412	24.314343
140.040977	4291.948030	24.319360
140.177098	4295.302060	24.324378
140.454974	4285.183900	24.329395
140.912815	4286.044294	24.334413
140.769944	4282.159057	24.339431
140.976144	4278.629058	24.344448
141.156138	4281.387996	24.349466
141.214355	4268.309810	24.354483
141.214237	4278.860073	24.359501
140.837473	4278.869561	24.364519
141.086497	4271.854079	24.369536
140.910297	4270.819452	24.374554
141.071211	4272.267118	24.379571
141.264215	4295.446902	24.384589
141.371515	4306.495450	24.389607
141.797553	4302.619798	24.394624
141.671386	4313.079062	24.399642
141.883407	4319.598152	24.404659
141.869277	4331.233049	24.409677
141.938099	4334.385177	24.414695
142.617235	4340.053900	24.419712
142.448534	4361.233783	24.424730
142.666979	4357.381890	24.429747
143.454792	4364.366233	24.434765
143.767741	4366.351785	24.439783
143.833003	4359.070043	24.444800
143.521633	4360.564025	24.449818
143.764137	4346.804389	24.454835
143.989539	4352.241363	24.459853
144.043409	4352.145523	24.464871
143.929637	4345.260725	24.469888
144.188015	4345.826088	24.474906
144.411446	4347.215786	24.479923
144.739143	4356.280362	24.484941
144.981841	4361.735640	24.489959
145.254453	4349.530342	24.494976
145.122770	4344.678329	24.499994
144.964606	4327.183160	24.505011
145.150815	4339.880095	24.510029
145.053594	4345.971757	24.515047
145.536361	4346.340341	24.520064
145.523529	4362.403863	24.525082
145.633788	4359.379410	24.530099
145.717139	4354.910336	24.535117
145.621298	4354.275432	24.540135
145.856437	4364.470371	24.545152
145.706636	4381.632505	24.550170
146.111242	4385.462726	24.555187
146.047808	4380.657287	24.560205
146.091305	4401.556682	24.565223
146.816554	4408.537592	24.570240
146.396227	4416.169353	24.575258
146.353122	4423.574987	24.580275
146.731585	4445.910365	24.585293
146.497806	4441.764214	24.590311
147.138208	4458.498756	24.595328
146.904427	4471.943584	24.600346
147.570744	4474.840512	24.605363
148.116080	4496.826789	24.610381
148.089492	4502.390502	24.615399
148.493313	4502.141729	24.620416
148.347930	4506.051299	24.625434
148.456416	4505.236436	24.630451
148.598689	4503.916422	24.635469
148.952659	4516.359476	24.640487
148.860200	4519.871672	24.645504
148.696245	4524.576003	24.650522
148.665179	4523.174645	24.655539
149.071512	4538.470220	24.660557
149.079549	4544.179238	24.665575
149.666332	4529.438103	24.670592
150.115653	4559.236159	24.675610
150.149981	4564.927288	24.680627
150.414680	4563.445294	24.685645
150.176057	4569.828292	24.690663
150.473503	4566.059686	24.695680
150.411145	4563.618494	24.700698
150.698539	4569.485993	24.705715
150.838928	4590.212288	24.710733
150.971860	4600.171281	24.715751
151.738788	4582.572378	24.720768
151.367679	4587.889579	24.725786
151.599484	4583.800625	24.730803
152.164917	4571.359865	24.735821
151.880033	4580.671358	24.740839
152.090299	4580.914958	24.745856
152.406040	4593.247269	24.750874
152.674402	4595.972999	24.755891
152.865829	4594.699685	24.760909
152.678312	4609.035394	24.765927
152.843516	4602.080606	24.770944
152.973385	4603.250075	24.775962
152.724750	4604.011058	24.780979
152.985393	4601.483772	24.785997
152.638432	4606.668453	24.791015
153.124807	4618.712399	24.796032
153.220164	4632.517600	24.801050
153.109042	4624.805991	24.806067
153.702822	4649.534618	24.811085
153.487313	4665.504806	24.816103
153.848888	4662.922400	24.821120
154.022761	4678.654145	24.826138
154.018307	4693.856461	24.831155
154.020369	4701.742821	24.836173
154.058775	4704.295327	24.841191
154.522650	4709.181939	24.846208
154.965402	4718.249841	24.851226
155.108371	4742.588821	24.856243
155.704153	4750.542770	24.861261
156.099389	4749.737812	24.866279
156.224798	4741.998200	24.871296
156.487461	4732.100543	24.876314
156.730699	4740.281903	24.881331
156.870125	4728.896244	24.886349
156.526740	4732.967410	24.891367
156.738752	4720.821050	24.896384
157.237610	4725.961593	24.901402
157.332923	4721.607725	24.906419
157.455010	4723.540978	24.911437
157.122309	4724.696023	24.916455
157.608147	4717.104149	24.921472
157.349341	4714.076734	24.926490
157.115263	4718.356000	24.931507
157.274377	4722.553686	24.936525
157.402356	4737.627010	24.941543
157.661042	4738.395549	24.946560
158.062808	4753.926834	24.951578
157.945851	4769.123304	24.956595
158.678926	4772.320755	24.961613
158.308436	4780.675083	24.966631
158.534799	4793.801856	24.971648
159.079161	4793.170608	24.976666
159.227885	4800.321416	24.981683
159.639426	4801.687573	24.986701
159.203671	4792.829580	24.991719
159.739804	4814.106632	24.996736
160.020291	4821.826387	25.001754
160.300243	4817.725182	25.006771
160.315492	4814.588543	25.011789
160.306420	4821.595491	25.016807
160.422006	4814.831063	25.021824
160.846208	4820.046660	25.026842
160.834700	4839.379975	25.031859
161.110577	4835.857600	25.036877
160.932373	4845.023360	25.041895
161.236417	4838.803177	25.046912
161.659903	4838.229668	25.051930
161.077548	4844.877277	25.056947
161.680666	4843.987845	25.061965
161.865334	4880.315035	25.066983
161.589119	4874.389647	25.072000
162.120453	4869.366315	25.077018
161.733483	4868.938040	25.082035
162.465660	4885.673847	25.087053
162.407174	4896.389695	25.092071
162.310734	4897.126176	25.097088
162.732294	4895.796848	25.102106
162.770881	4918.388073	25.107123
163.113581	4922.685092	25.112141
163.080454	4928.719519	25.117159
163.104180	4925.531782	25.122176
163.481467	4932.756891	25.127194
163.745167	4948.171047	25.132211
164.025657	4951.579234	25.137229
164.063095	4974.471621	25.142247
164.394477	4963.299425	25.147264
164.918299	4963.913828	25.152282
164.673615	4972.093884	25.157299
165.168876	4965.290299	25.162317
165.260736	4977.369069	25.167335
165.282633	4981.590346	25.172352
166.060626	4976.586136	25.177370
166.079307	4983.762471	25.182387
166.134345	4974.871437	25.187405
165.981895	4978.111249	25.192423
166.641037	4979.038786	25.197440
166.826804	4973.731242	25.202458
166.778450	4982.206101	25.207475
166.550068	4971.119617	25.212493
166.736600	4970.410289	25.217511
166.635036	4971.391038	25.222528
167.189571	4981.452860	25.227546
167.371467	4989.528292	25.232563
167.451698	4993.640328	25.237581
167.375680	4987.258393	25.242599
167.708621	4997.722110	25.247616
167.702820	5001.532257	25.252634
167.424844	5018.889549	25.257651
167.720033	5028.022311	25.262669
168.225243	5049.015123	25.267687
168.100097	5058.538961	25.272704
168.264625	5060.786346	25.277722
168.340098	5082.664949	25.282739
168.839334	5085.047151	25.287757
168.801374	5085.927998	25.292775
169.147612	5109.352090	25.297792
169.452335	5109.000574	25.302810
169.422504	5115.477174	25.307827
169.818906	5125.106200	25.312845
169.893697	5142.740275	25.317863
170.234374	5153.482390	25.322880
170.641543	5146.481160	25.327898
170.074286	5143.961020	25.332915
170.640599	5144.829653	25.337933
170.541232	5160.710327	25.342951
171.006488	5166.450678	25.347968
171.450820	5159.916460	25.352986
171.245127	5158.741110	25.358003
172.103863	5158.900339	25.363021
171.670030	5161.154216	25.368039
171.867987	5182.163642	25.373056
172.493416	5178.552128	25.378074
172.564822	5186.604068	25.383091
172.435629	5187.062616	25.388109
172.678270	5187.548794	25.393127
172.414383	5183.866817	25.398144
172.614189	5177.608447	25.403162
172.834817	5201.851329	25.408179
173.077807	5202.609192	25.413197
173.673811	5207.764750	25.418215
173.312968	5210.089614	25.423232
173.815833	5227.306979	25.428250
174.560207	5218.604045	25.433267
175.090342	5214.819030	25.438285
175.335328	5215.915251	25.443303
175.276605	5193.238902	25.448320
175.527634	5179.102154	25.453338
175.407481	5180.253088	25.458355
175.473512	5171.023726	25.463373
175.638756	5173.156006	25.468391
175.510469	5167.599769	25.473408
175.682578	5170.686312	25.478426
175.960880	5186.876414	25.483443
176.411114	5201.005661	25.488461
176.369679	5197.553355	25.493479
175.955532	5200.511977	25.498496
176.151016	5206.404924	25.503514
176.393612	5203.608104	25.508531
176.157671	5221.386903	25.513549
176.688155	5228.114862	25.518567
176.641892	5234.855834	25.523584
177.125785	5244.210004	25.528602
176.911792	5252.721277	25.533619
177.099084	5258.553421	25.538637
177.089895	5273.254570	25.543655
177.347870	5295.136840	25.548672
178.031151	5306.734820	25.553690
177.728309	5319.522678	25.558707
177.641248	5328.267440	25.563725
178.045989	5342.242349	25.568743
178.595594	5356.631963	25.573760
179.152005	5363.750949	25.578778
179.306408	5376.718042	25.583795
179.512593	5366.563438	25.588813
179.793460	5360.963777	25.593831
180.213213	5356.200452	25.598848
180.594985	5350.610278	25.603866
180.306293	5350.108426	25.608883
180.325933	5352.795797	25.613901
180.721156	5344.099086	25.618919
180.746491	5352.550483	25.623936
180.727715	5368.022135	25.628954
180.988910	5377.357847	25.633971
181.082842	5376.075980	25.638989
180.897364	5380.398290	25.644007
181.053891	5399.905917	25.649024
181.655850	5395.120800	25.654042
181.490049	5405.293772	25.659059
181.849100	5401.508110	25.664077
182.244057	5416.249600	25.669095
182.196715	5428.143053	25.674112
182.502951	5433.371201	25.679130
182.561051	5437.601361	25.684148
182.590462	5443.876533	25.689165
183.164002	5457.368906	25.694183
182.868649	5464.393705	25.699200
183.010921	5468.878043	25.704218
183.351154	5491.528652	25.709236
183.507319	5485.678573	25.714253
183.820701	5498.956430	25.719271
183.953041	5514.971029	25.724288
184.214550	5510.723937	25.729306
184.392016	5523.298868	25.734324
184.486479	5537.048299	25.739341
184.649429	5547.469054	25.744359
184.906716	5555.218353	25.749376
185.492046	5561.094229	25.754394
185.965537	5566.894756	25.759412
185.685291	5574.213971	25.764429
186.131584	5576.602176	25.769447
185.935801	5567.261503	25.774464
186.445520	5575.110111	25.779482
186.480407	5594.521463	25.784500
186.504205	5594.748210	25.789517
186.924846	5595.221218	25.794535
187.079601	5597.430184	25.799552
187.274671	5599.012329	25.804570
187.656584	5608.425945	25.809588
187.760874	5617.684720	25.814605
187.949186	5612.874349	25.819623
187.926545	5617.727281	25.824640
188.211863	5612.762435	25.829658
187.942569	5635.470473	25.834676
188.331781	5644.543364	25.839693
188.454313	5645.674786	25.844711
188.267415	5657.896382	25.849728
188.711007	5668.705491	25.854746
189.020104	5666.577758	25.859764
188.989999	5688.817941	25.864781
189.651531	5686.418690	25.869799
189.537763	5699.632878	25.874816
189.671685	5707.179694	25.879834
189.790833	5720.477642	25.884852
190.363361	5719.387825	25.889869
190.872996	5710.750074	25.894887
190.515796	5715.498120	25.899904
190.740922	5719.688696	25.904922
190.916018	5741.304581	25.909940
191.292236	5746.245144	25.914957
191.672456	5734.407100	25.919975
191.708532	5741.461854	25.924992
192.072636	5735.810772	25.930010
192.780704	5742.250935	25.935028
192.837118	5730.967011	25.940045
193.362158	5725.710551	25.945063
193.558147	5719.193471	25.950080
194.003664	5712.870717	25.955098
193.982101	5698.657356	25.960116
193.416607	5697.186028	25.965133
193.955761	5687.019829	25.970151
193.696703	5694.845893	25.975168
194.210337	5697.918108	25.980186
194.174304	5698.910511	25.985204
194.219778	5699.404510	25.990221
194.417968	5692.591679	25.995239
194.319196	5709.951301	26.000256
194.582152	5715.850989	26.005274
194.755420	5716.411305	26.010292
194.691552	5741.663193	26.015309
195.238069	5744.819578	26.020327
195.533315	5740.023921	26.025344
195.703763	5744.698857	26.030362
195.677832	5762.214616	26.035380
195.458605	5775.583217	26.040397
195.895757	5778.583486	26.045415
195.752391	5800.969273	26.050432
196.135206	5810.165451	26.055450
196.611079	5820.718643	26.060468
196.898682	5831.345863	26.065485
196.846201	5843.183005	26.070503
196.961979	5859.677350	26.075520
197.440896	5871.378523	26.080538
197.404763	5872.202386	26.085556
197.943455	5886.428150	26.090573
198.240391	5885.637631	26.095591
198.447670	5903.288438	26.100608
198.758690	5917.788781	26.105626
198.924416	5919.544557	26.110644
198.902233	5920.184859	26.115661
199.294959	5925.732333	26.120679
199.321131	5939.478852	26.125696
199.593650	5945.296641	26.130714
199.888307	5942.044141	26.135732
200.072975	5949.492575	26.140749
200.877422	5950.391335	26.145767
201.076799	5954.109037	26.150784
201.297134	5959.501750	26.155802
201.108765	5952.658184	26.160820
201.128664	5960.713832	26.165837
201.287025	5949.321692	26.170855
201.277153	5951.140656	26.175872
201.243284	5951.732549	26.180890
201.564840	5959.712856	26.185908
201.424257	5985.553307	26.190925
201.925478	5988.272451	26.195943
201.613077	5993.568234	26.200960
201.645829	6012.861519	26.205978
202.193205	6024.027244	26.210996
202.055270	6038.816550	26.216013
202.376054	6047.330314	26.221031
203.260857	6045.498490	26.226048
203.983941	6041.895257	26.231066
204.494847	6032.990870	26.236084
204.911136	6031.328370	26.241101
204.935888	6022.115831	26.246119
205.216853	6024.427682	26.251136
205.373397	6029.389449	26.256154
205.487610	6027.469160	26.261172
205.173742	6026.979476	26.266189
205.426738	6020.003508	26.271207
205.969050	6020.786514	26.276224
205.848769	6028.817388	26.281242
206.229014	6033.303631	26.286260
205.850829	6059.242434	26.291277
206.164743	6052.903508	26.296295
206.189678	6056.529042	26.301312
206.338011	6076.491840	26.306330
206.514742	6072.303245	26.311348
206.653829	6077.164042	26.316365
207.430127	6091.488688	26.321383
207.675450	6093.103230	26.326400
207.884649	6107.224193	26.331418
207.892482	6098.534402	26.336436
208.053385	6114.650264	26.341453
208.132840	6114.370430	26.346471
208.466520	6125.755609	26.351488
208.404917	6138.612262	26.356506
208.410803	6153.506206	26.361524
208.859230	6162.668500	26.366541
209.210482	6179.262239	26.371559
209.534605	6195.054022	26.376576
209.763296	6199.799456	26.381594
210.176339	6199.715297	26.386612
209.976617	6218.695784	26.391629
210.393737	6216.912603	26.396647
210.529361	6220.787025	26.401664
210.362565	6232.587335	26.406682
210.477871	6249.011271	26.411700
211.076441	6258.314880	26.416717
212.338695	6257.797635	26.421735
212.579543	6260.125063	26.426752
212.471282	6248.017473	26.431770
212.432355	6228.115333	26.436788
212.134810	6230.549223	26.441805
212.582277	6248.698045	26.446823
212.690925	6255.536567	26.451840
212.926547	6250.587133	26.456858
212.941232	6248.310499	26.461876
212.905107	6267.513497	26.466893
213.295156	6278.444059	26.471911
213.391722	6285.034958	26.476928
213.746743	6298.812855	26.481946
214.055132	6307.103596	26.486964
213.824935	6317.223594	26.491981
214.036592	6333.230936	26.496999
214.186290	6340.579994	26.502016
214.073171	6359.667113	26.507034
214.620635	6373.479832	26.512052
215.160712	6392.088730	26.517069
215.017555	6412.376831	26.522087
215.442123	6412.604213	26.527104
215.631038	6436.839451	26.532122
215.716200	6433.516421	26.537140
216.510811	6458.707365	26.542157
216.404794	6469.270934	26.547175
217.060765	6464.898472	26.552192
216.622659	6479.054312	26.557210
217.088178	6483.147956	26.562228
217.619288	6494.720910	26.567245
217.788490	6505.795042	26.572263
218.182381	6518.282462	26.577280
218.003392	6525.351584	26.582298
217.850781	6527.485755	26.587316
218.210103	6538.280760	26.592333
218.588277	6551.067875	26.597351
219.100799	6565.055327	26.602368
218.774600	6585.451434	26.607386
219.181044	6590.918806	26.612404
219.245861	6607.866946	26.617421
219.786814	6609.655374	26.622439
219.941892	6635.734508	26.627456
220.028521	6642.829836	26.632474
220.593276	6641.992588	26.637492
220.952411	6655.318714	26.642509
221.714703	6658.970027	26.647527
221.760919	6658.511551	26.652544
221.715859	6656.854811	26.657562
221.980421	6653.667985	26.662580
221.994222	6661.049938	26.667597
222.059174	6675.875952	26.672615
222.536475	6684.056011	26.677632
222.389953	6697.915499	26.682650
222.830285	6695.562689	26.687668
222.900949	6707.492799	26.692685
223.039381	6706.488363	26.697703
223.395298	6719.259736	26.702720
223.955836	6728.828523	26.707738
224.266118	6737.158551	26.712756
223.893297	6746.753421	26.717773
223.943948	6748.054005	26.722791
224.651884	6757.135925	26.727808
224.534425	6769.990844	26.732826
224.797083	6766.016575	26.737844
225.212497	6776.951012	26.742861
225.444540	6794.248804	26.747879
225.701664	6786.022429	26.752896
225.692870	6786.847166	26.757914
226.374074	6801.407752	26.762932
226.295187	6799.811150	26.767949
226.561202	6802.592027	26.772967
226.814440	6811.774763	26.777984
226.668716	6830.497790	26.783002
227.311753	6835.705699	26.788020
227.630565	6841.200784	26.793037
227.499477	6847.665510	26.798055
227.799777	6862.812146	26.803072
228.019231	6870.712734	26.808090
227.918270	6880.963759	26.813108
228.285890	6896.336789	26.818125
228.602337	6901.577856	26.823143
228.674758	6919.969763	26.828160
228.583434	6934.655013	26.833178
228.798774	6946.551837	26.838196
229.410330	6960.914965	26.843213
229.049860	6983.774464	26.848231
229.604447	6993.427933	26.853248
229.780363	7020.905546	26.858266
230.049571	7023.336937	26.863284
230.485109	7048.115347	26.868301
230.810841	7063.452392	26.873319
231.027106	7069.790707	26.878336
231.196594	7084.933981	26.883354
231.698043	7100.879816	26.888372
232.059606	7110.725572	26.893389
232.123651	7118.452042	26.898407
232.300688	7123.118379	26.903424
233.179258	7126.007799	26.908442
233.588284	7120.736115	26.913460
233.712523	7118.212127	26.918477
234.074973	7122.559148	26.923495
234.493617	7117.917604	26.928512
234.489209	7124.094463	26.933530
234.290771	7111.971740	26.938548
234.362975	7126.696095	26.943565
234.463283	7144.432788	26.948583
235.073274	7147.120891	26.953600
234.805840	7160.665128	26.958618
235.016425	7172.098941	26.963636
235.332683	7189.323644	26.968653
235.143770	7201.483741	26.973671
235.709336	7210.371327	26.978688
235.518747	7235.949013	26.983706
235.788390	7243.333860	26.988724
236.185494	7260.615681	26.993741
236.107303	7274.274889	26.998759
236.661426	7285.467922	27.003776
237.087704	7304.625202	27.008794
237.654205	7302.026954	27.013812
237.840073	7311.400351	27.018829
237.964599	7326.524776	27.023847
238.644489	7333.714089	27.028864
238.380455	7331.699350	27.033882
238.736149	7327.259178	27.038900
238.831312	7343.197697	27.043917
238.978115	7348.727956	27.048935
239.451986	7363.457732	27.053952
239.452764	7376.976659	27.058970
239.647145	7385.452151	27.063988
240.102582	7398.678101	27.069005
240.421428	7415.678088	27.074023
240.628219	7425.671098	27.079040
240.858013	7430.570330	27.084058
241.234732	7433.960991	27.089076
241.561676	7439.972462	27.094093
241.700465	7460.048915	27.099111
242.080065	7465.956048	27.104128
241.835575	7465.038472	27.109146
242.021374	7483.962253	27.114164
242.345790	7489.969449	27.119181
242.158221	7515.119296	27.124199
242.542267	7526.451154	27.129216
242.626490	7547.128695	27.134234
243.176826	7569.371265	27.139252
243.580529	7585.481657	27.144269
243.428501	7603.978208	27.149287
244.052606	7612.207636	27.154304
244.294379	7622.482316	27.159322
244.597163	7637.432315	27.164340
245.211775	7659.892452	27.169357
245.331120	7660.154846	27.174375
245.543921	7667.772578	27.179392
245.425623	7674.838103	27.184410
245.677263	7685.045745	27.189428
246.033727	7697.221451	27.194445
246.433971	7706.424409	27.199463
246.671649	7722.427897	27.204480
246.994266	7739.973523	27.209498
246.958397	7737.179884	27.214516
247.749691	7759.944691	27.219533
247.964173	7773.339088	27.224551
248.169222	7770.466335	27.229568
247.577552	7784.223443	27.234586
248.329431	7789.114440	27.239604
248.663564	7792.735424	27.244621
248.921308	7812.902222	27.249639
249.702573	7815.995162	27.254656
250.071573	7813.671755	27.259674
250.183444	7813.743997	27.264692
250.523122	7806.730342	27.269709
250.183770	7811.126945	27.274727
250.709568	7821.787934	27.279744
250.646201	7834.097154	27.284762
250.533601	7837.325193	27.289780
251.130166	7843.002268	27.294797
250.983353	7867.186928	27.299815
251.216373	7865.460340	27.304832
251.431458	7890.906509	27.309850
251.465547	7894.915338	27.314868
251.741369	7918.575435	27.319885
251.751274	7937.945860	27.324903
252.104058	7960.038489	27.329920
252.583023	7982.947746	27.334938
253.007463	7992.311374	27.339956
253.078499	8020.019022	27.344973
253.382022	8041.552985	27.349991
253.822616	8058.925904	27.355008
253.871655	8063.962668	27.360026
254.354372	8093.514257	27.365044
254.806542	8096.870858	27.370061
254.608623	8114.484846	27.375079
254.928326	8120.468666	27.380096
256.451529	8118.993596	27.385114
257.023838	8129.293879	27.390132
256.986314	8129.645407	27.395149
257.469297	8121.687674	27.400167
257.671080	8119.300712	27.405184
257.800310	8130.841330	27.410202
257.600055	8125.747811	27.415220
257.850975	8114.513952	27.420237
258.220036	8117.564164	27.425255
258.277742	8106.910958	27.430272
258.348618	8130.065269	27.435290
258.405991	8135.597738	27.440308
259.037715	8134.926204	27.445325
259.113345	8155.038776	27.450343
259.465919	8159.391716	27.455360
259.812831	8161.285281	27.460378
259.986723	8177.960346	27.465396
260.241936	8189.347847	27.470413
260.244536	8200.108222	27.475431
260.383780	8205.119328	27.480448
261.228726	8212.930702	27.485466
260.672001	8229.035408	27.490484
261.153838	8237.549529	27.495501
261.498822	8255.809590	27.500519
261.625173	8268.516773	27.505536
261.885092	8277.258029	27.510554
261.963472	8296.086159	27.515572
262.594446	8313.852935	27.520589
262.654154	8327.689508	27.525607
262.558656	8344.355773	27.530624
262.969225	8362.294311	27.535642
262.863801	8389.677533	27.540660
263.458958	8392.595293	27.545677
263.723186	8416.733171	27.550695
263.609718	8425.902484	27.555712
263.856454	8439.581831	27.560730
264.504337	8456.221636	27.565748
265.371323	8459.793985	27.570765
265.511285	8479.564259	27.575783
265.714297	8488.771538	27.580800
266.287996	8493.813049	27.585818
266.399666	8499.808247	27.590836
267.244946	8501.718850	27.595853
267.313004	8514.108481	27.600871
267.433628	8512.778463	27.605888
267.705741	8521.938465	27.610906
267.715103	8520.693695	27.615924
267.801567	8525.996779	27.620941
268.079237	8548.019583	27.625959
268.449279	8560.177863	27.630976
268.643442	8566.316513	27.635994
268.705126	8587.884784	27.641012
268.782975	8591.840591	27.646029
269.049092	8612.009322	27.651047
269.011316	8629.060693	27.656064
269.969950	8649.981334	27.661082
270.022309	8669.037317	27.666100
270.610627	8670.833631	27.671117
270.966383	8688.963921	27.676135
270.856354	8694.516608	27.681152
271.512823	8697.068601	27.686170
271.148366	8718.478462	27.691188
271.658046	8721.655954	27.696205
272.160712	8745.063307	27.701223
271.960069	8757.014657	27.706240
272.488958	8771.896235	27.711258
272.735931	8789.717541	27.716276
273.371848	8806.296734	27.721293
272.942085	8825.838128	27.726311
273.449896	8841.296936	27.731328
274.388598	8843.011155	27.736346
274.299027	8860.288306	27.741364
274.648456	8874.255320	27.746381
275.143265	8887.658538	27.751399
275.439858	8901.993892	27.756416
275.607811	8897.290030	27.761434
275.883431	8913.478863	27.766452
276.114406	8922.422395	27.771469
276.209845	8932.536277	27.776487
276.330879	8946.756797	27.781504
277.109155	8953.610119	27.786522
277.066925	8965.726707	27.791540
276.963401	8979.339704	27.796557
277.439911	8991.354794	27.801575
277.669975	9012.083280	27.806592
278.383266	9022.195315	27.811610
279.085160	9011.813997	27.816628
279.791104	9023.145320	27.821645
280.104789	9019.435931	27.826663
279.865407	9003.015521	27.831680
280.414062	9012.309612	27.836698
280.386927	9017.395972	27.841716
280.597473	9021.776644	27.846733
280.403310	9022.454425	27.851751
280.708769	9020.969779	27.856768
281.332501	9032.693370	27.861786
281.091298	9043.673364	27.866804
281.597156	9048.365843	27.871821
281.681373	9064.286672	27.876839
281.545223	9073.080492	27.881856
282.077587	9093.464186	27.886874
282.064057	9112.181389	27.891892
282.304382	9133.696135	27.896909
283.252674	9139.036065	27.901927
283.501172	9162.092083	27.906944
283.920731	9162.647345	27.911962
283.939525	9177.038437	27.916980
284.043257	9196.197328	27.921997
284.310198	9203.314883	27.927015
284.455270	9229.611097	27.932032
285.077776	9231.532404	27.937050
285.242668	9251.323777	27.942068
285.519450	9261.936231	27.947085
285.774268	9277.022828	27.952103
285.718538	9295.667114	27.957120
286.256480	9323.623155	27.962138
286.464148	9345.017721	27.967156
286.845976	9359.064694	27.972173
286.928642	9369.497764	27.977191
286.910251	9400.221761	27.982208
287.795403	9411.809431	27.987226
287.787094	9435.579550	27.992244
288.644953	9451.719554	27.997261
288.976616	9476.967827	28.002279
288.838052	9486.049072	28.007296
289.562035	9493.315329	28.012314
289.772928	9515.272114	28.017332
289.911068	9518.313329	28.022349
290.602720	9534.563844	28.027367
290.199989	9553.572023	28.032384
290.867184	9565.431951	28.037402
291.103594	9585.855964	28.042420
291.183033	9603.582399	28.047437
291.394672	9615.769417	28.052455
291.432831	9639.709934	28.057472
292.238310	9651.703802	28.062490
292.618359	9668.784717	28.067508
292.979272	9683.015196	28.072525
293.547277	9700.985762	28.077543
293.625687	9706.030612	28.082560
294.047127	9723.298312	28.087578
294.411437	9730.145712	28.092596
294.634012	9738.731860	28.097613
294.969832	9738.496272	28.102631
294.805382	9750.303480	28.107648
295.453747	9757.912159	28.112666
295.434094	9763.662453	28.117684
295.783618	9787.315030	28.122701
296.217437	9790.957994	28.127719
296.082151	9812.827968	28.132736
296.410380	9818.176710	28.137754
296.771258	9837.112645	28.142772
296.861192	9862.308403	28.147789
297.406477	9874.873351	28.152807
297.475733	9894.429775	28.157824
297.710575	9914.205243	28.162842
297.900411	9935.433459	28.167860
298.157949	9956.029233	28.172877
298.548800	9972.449932	28.177895
298.742965	9992.402654	28.182912
299.470601	10009.243138	28.187930
300.020512	10020.891861	28.192948
300.404679	10037.684089	28.197965
301.123538	10040.945760	28.202983
300.905837	10047.644071	28.208000
301.408660	10063.267220	28.213018
301.754700	10076.053996	28.218036
302.145392	10093.209177	28.223053
302.314596	10099.132077	28.228071
302.697170	10095.779382	28.233088
303.858760	10091.966974	28.238106
304.130381	10098.442766	28.243124
303.886519	10103.160052	28.248141
304.479492	10105.122777	28.253159
304.555028	10106.687260	28.258176
304.857663	10101.703108	28.263194
304.980088	10106.166941	28.268212
304.827767	10130.471753	28.273229
305.339815	10129.095003	28.278247
305.411553	10156.580856	28.283264
305.586837	10156.658003	28.288282
305.483828	10183.551401	28.293300
305.728375	10201.281709	28.298317
306.008029	10213.835720	28.303335
306.317757	10250.445972	28.308352
306.325328	10268.722812	28.313370
306.569420	10295.788553	28.318388
306.984678	10327.434336	28.323405
308.172142	10343.042843	28.328423
308.383182	10355.849828	28.333440
309.280124	10368.952136	28.338458
309.345703	10376.804399	28.343476
309.131065	10388.608065	28.348493
309.920520	10404.842699	28.353511
309.763784	10418.224918	28.358528
310.261332	10434.197594	28.363546
310.067363	10457.578704	28.368564
310.646198	10478.274508	28.373581
311.020972	10489.327974	28.378599
311.230352	10513.300317	28.383616
311.602759	10521.219827	28.388634
311.919854	10549.726422	28.393652
311.798300	10563.898542	28.398669
312.157747	10579.612951	28.403687
312.308817	10601.343506	28.408704
312.860419	10614.016684	28.413722
313.087954	10636.733282	28.418740
313.344455	10667.901085	28.423757
313.823181	10673.835757	28.428775
314.041743	10703.747856	28.433792
314.357016	10732.940591	28.438810
314.598173	10747.665298	28.443828
314.856849	10770.740774	28.448845
315.242019	10792.306967	28.453863
315.626758	10819.330564	28.458880
315.811735	10840.749905	28.463898
316.574918	10860.825220	28.468916
316.493609	10889.083939	28.473933
317.227392	10899.768854	28.478951
317.367209	10931.674194	28.483968
317.495462	10943.487257	28.488986
318.129851	10971.284635	28.494004
318.632903	10990.482791	28.499021
319.239645	10994.550257	28.504039
319.519173	11009.092123	28.509056
320.213595	11017.169434	28.514074
320.745287	11024.834961	28.519092
320.471898	11058.407764	28.524109
321.268686	11049.367337	28.529127
321.200542	11056.395007	28.534144
321.183370	11077.430114	28.539162
321.495146	11093.695307	28.544180
322.068991	11109.687091	28.549197
322.215924	11116.252428	28.554215
322.343251	11138.597650	28.559232
322.552943	11160.038391	28.564250
322.646507	11184.561083	28.569268
323.217240	11205.114220	28.574285
323.789400	11223.029035	28.579303
324.026053	11236.435906	28.584320
324.341399	11272.270564	28.589338
324.773390	11284.075942	28.594356
325.007738	11306.100472	28.599373
325.465503	11324.796183	28.604391
325.530848	11345.497578	28.609408
326.440644	11348.547144	28.614426
327.007328	11368.852184	28.619444
327.213166	11380.935937	28.624461
327.597623	11374.974477	28.629479
327.978790	11388.886222	28.634496
328.345531	11401.285969	28.639514
328.600391	11394.319197	28.644532
328.315693	11405.952796	28.649549
328.735088	11413.648787	28.654567
328.567230	11424.488584	28.659584
329.097524	11445.836931	28.664602
329.424175	11456.714920	28.669620
329.618493	11485.776870	28.674637
329.884239	11496.094829	28.679655
330.535719	11516.957593	28.684672
330.346603	11541.277117	28.689690
330.891809	11558.768263	28.694708
331.026538	11591.679654	28.699725
331.535911	11602.319973	28.704743
331.430888	11630.642351	28.709760
331.827964	11660.642234	28.714778
332.579719	11672.851700	28.719796
332.663276	11691.575720	28.724813
333.653905	11707.473024	28.729831
334.391804	11724.521570	28.734848
334.141785	11741.863954	28.739866
334.768271	11759.642397	28.744884
334.999868	11778.973114	28.749901
335.160414	11796.944925	28.754919
335.475140	11811.982640	28.759936
335.412248	11838.578758	28.764954
336.103560	11853.389643	28.769972
336.325113	11878.337447	28.774989
336.799050	11902.512348	28.780007
337.446993	11918.049378	28.785024
337.565335	11935.940320	28.790042
338.148748	11960.250992	28.795060
338.011102	11979.408830	28.800077
338.402890	11993.431168	28.805095
338.719339	12018.994900	28.810112
338.941168	12041.928773	28.815130
339.714861	12064.010036	28.820148
339.983640	12085.764949	28.825165
340.224848	12107.835091	28.830183
340.422881	12122.803260	28.835200
340.312932	12136.333315	28.840218
340.681275	12158.993231	28.845236
340.826400	12198.898432	28.850253
341.372291	12222.448403	28.855271
341.669614	12251.867580	28.860288
342.098368	12278.890784	28.865306
342.812746	12297.535753	28.870324
343.035428	12322.868594	28.875341
343.508591	12337.999418	28.880359
343.701404	12361.844933	28.885376
343.973088	12392.176554	28.890394
344.549958	12407.864925	28.895412
344.881273	12429.973644	28.900429
345.740298	12446.872954	28.905447
346.060512	12460.829160	28.910464
346.587980	12484.945317	28.915482
346.927284	12483.107839	28.920500
347.412626	12494.050736	28.925517
347.324979	12496.995669	28.930535
347.892863	12517.032433	28.935552
347.842842	12530.045053	28.940570
349.294010	12510.425115	28.945588
349.713837	12520.266566	28.950605
350.162087	12513.140094	28.955623
350.541432	12510.039638	28.960640
350.706857	12515.360441	28.965658
351.144591	12507.361065	28.970676
351.142835	12513.200672	28.975693
351.587792	12517.313594	28.980711
351.873748	12514.673590	28.985728
351.813779	12528.189098	28.990746
352.127472	12539.237095	28.995764
352.020606	12556.248473	29.000781
352.270005	12566.095520	29.005799
352.524886	12587.327080	29.010816
352.554991	12610.051896	29.015834
352.877380	12630.978796	29.020852
352.941195	12663.143258	29.025869
353.152022	12692.210829	29.030887
353.654021	12716.366367	29.035904
354.077714	12741.499919	29.040922
354.783940	12764.889230	29.045940
354.819423	12798.836628	29.050957
355.134630	12826.811662	29.055975
355.954686	12854.003591	29.060992
356.002218	12887.788347	29.066010
356.377891	12913.163653	29.071028
356.849414	12939.164041	29.076045
356.786010	12968.127794	29.081063
357.150563	12998.827614	29.086080
357.431388	13030.553698	29.091098
358.244319	13057.673111	29.096116
358.789688	13089.305112	29.101133
359.035736	13112.089755	29.106151
359.802185	13137.601755	29.111168
359.917801	13169.414738	29.116186
360.225160	13183.358002	29.121204
360.432071	13209.728849	29.126221
360.793680	13245.544142	29.131239
361.603597	13266.367810	29.136256
361.442477	13294.809850	29.141274
361.747816	13317.581465	29.146292
362.041622	13348.703857	29.151309
362.623810	13375.803450	29.156327
363.059181	13392.885104	29.161344
363.190975	13434.931260	29.166362
363.771625	13447.555968	29.171380
364.142725	13487.732922	29.176397
364.403690	13506.340347	29.181415
365.234126	13533.886261	29.186432
365.497151	13547.935155	29.191450
366.332551	13548.115129	29.196468
367.664249	13567.893035	29.201485
367.980246	13562.205743	29.206503
368.355738	13563.883073	29.211520
368.623542	13565.413364	29.216538
368.733990	13557.833665	29.221556
368.878312	13557.370794	29.226573
368.652747	13563.846492	29.231591
368.989642	13578.374513	29.236608
369.317176	13600.521712	29.241626
369.280173	13617.017843	29.246644
369.495415	13639.430220	29.251661
369.450479	13663.463379	29.256679
370.313569	13689.123598	29.261696
369.969839	13720.608142	29.266714
370.619847	13751.785313	29.271732
370.992745	13785.900737	29.276749
370.692120	13820.120626	29.281767
371.655824	13854.257881	29.286784
371.688182	13890.387923	29.291802
372.502841	13919.959434	29.296820
373.017142	13961.269925	29.301837
373.598646	13993.146512	29.306855
374.087545	14022.515542	29.311872
374.333339	14054.366243	29.316890
374.581145	14063.316029	29.321908
375.038359	14105.470474	29.326925
375.282155	14133.786245	29.331943
375.968249	14158.675243	29.336960
376.360087	14190.371929	29.341978
376.413984	14210.041751	29.346996
377.053524	14241.428128	29.352013
377.055643	14272.941144	29.357031
377.931807	14296.145896	29.362048
377.943902	14331.917845	29.367066
378.548918	14356.858866	29.372084
379.426281	14373.615174	29.377101
379.791590	14403.890329	29.382119
380.111068	14412.017838	29.387136
380.222264	14447.509822	29.392154
380.690304	14462.238398	29.397172
381.421023	14487.438646	29.402189
381.386110	14520.619838	29.407207
382.036127	14532.319274	29.412224
382.232817	14561.089928	29.417242
382.404453	14578.024136	29.422260
382.942475	14608.582164	29.427277
383.099954	14641.522561	29.432295
383.657357	14674.583637	29.437312
383.639221	14701.881297	29.442330
383.778998	14723.214154	29.447348
384.682996	14751.056875	29.452365
385.258342	14777.275665	29.457383
385.854299	14795.808222	29.462400
385.994388	14819.234436	29.467418
386.291192	14846.041733	29.472436
386.583256	14864.500345	29.477453
386.775753	14883.620739	29.482471
387.092142	14915.024372	29.487488
387.514590	14946.179751	29.492506
387.768231	14978.982965	29.497524
388.408711	15005.810437	29.502541
388.322107	15038.848624	29.507559
388.834638	15067.066345	29.512576
389.305632	15099.293456	29.517594
389.587092	15136.710772	29.522612
390.182582	15161.577405	29.527629
390.266954	15197.371938	29.532647
390.644644	15227.019107	29.537664
390.862256	15269.903279	29.542682
391.299452	15297.144377	29.547700
391.907805	15324.630468	29.552717
392.598521	15368.081683	29.557735
393.236015	15395.298075	29.562752
393.672562	15432.979526	29.567770
393.937030	15447.953522	29.572788
394.352613	15467.759895	29.577805
394.882467	15493.620332	29.582823
395.338000	15519.034832	29.587840
395.611176	15542.757681	29.592858
396.300202	15575.503225	29.597876
396.542433	15591.348152	29.602893
396.526352	15616.170523	29.607911
396.932809	15647.252720	29.612928
397.783153	15683.156637	29.617946
398.707694	15702.089469	29.622964
399.581795	15715.622482	29.627981
399.413412	15726.996421	29.632999
399.989328	15752.430058	29.638016
399.978177	15769.303803	29.643034
400.678682	15790.289721	29.648052
401.016459	15804.061321	29.653069
401.739341	15811.327477	29.658087
402.150911	15815.784305	29.663104
402.848437	15828.006183	29.668122
403.400600	15831.314971	29.673140
403.710564	15842.236566	29.678157
403.886268	15861.849642	29.683175
404.759978	15869.610179	29.688192
404.900569	15878.850461	29.693210
404.519221	15900.132266	29.698228
405.260497	15905.333414	29.703245
405.139180	15937.148186	29.708263
405.821390	15950.173581	29.713280
405.819767	15976.472657	29.718298
405.992833	15994.962381	29.723316
406.333820	16029.188790	29.728333
406.500256	16060.126881	29.733351
406.835279	16090.741352	29.738368
407.821944	16120.837497	29.743386
408.238251	16144.885062	29.748404
408.805858	16178.150749	29.753421
408.649268	16197.906292	29.758439
409.057596	16219.953301	29.763456
409.425850	16247.149449	29.768474
409.646528	16289.594334	29.773492
410.208860	16315.324375	29.778509
410.052976	16343.617831	29.783527
410.790344	16369.351065	29.788544
411.058172	16411.947400	29.793562
411.307669	16452.529157	29.798580
411.803851	16475.519917	29.803597
412.322443	16510.200843	29.808615
413.093902	16546.594656	29.813632
413.560123	16575.111369	29.818650
414.113566	16613.369782	29.823668
414.603941	16626.754910	29.828685
414.849480	16670.300014	29.833703
415.029219	16689.903914	29.838720
415.287343	16725.913155	29.843738
415.637838	16766.905588	29.848756
416.483557	16800.355021	29.853773
416.622915	16839.184652	29.858791
416.936062	16869.343976	29.863808
417.662889	16901.967426	29.868826
418.186801	16926.533680	29.873844
418.783260	16959.539019	29.878861
419.405416	16974.114153	29.883879
419.727746	17013.270693	29.888896
420.213894	17045.737033	29.893914
420.781094	17070.554625	29.898932
421.445717	17094.628798	29.903949
421.711875	17125.047298	29.908967
421.674472	17134.129601	29.913984
422.256909	17159.091327	29.919002
422.517094	17183.346867	29.924020
422.782126	17209.067755	29.929037
423.673752	17246.049457	29.934055
424.154916	17278.878124	29.939072
424.578259	17308.185386	29.944090
424.339795	17335.695380	29.949108
425.223594	17360.042950	29.954125
425.924529	17400.399880	29.959143
426.438826	17417.312943	29.964160
426.833526	17429.483853	29.969178
426.782821	17468.328597	29.974196
427.512872	17489.245389	29.979213
427.906006	17515.006280	29.984231
428.248328	17537.673309	29.989248
428.312091	17562.445477	29.994266
428.374173	17601.618039	29.999284
429.321642	17626.109587	30.004301
430.469779	17647.200872	30.009319
431.108967	17660.540836	30.014336
431.744403	17675.245164	30.019354
432.192328	17697.448151	30.024372
432.929291	17697.676617	30.029389
432.864273	17728.094634	30.034407
433.865880	17728.898910	30.039424
434.076478	17734.615677	30.044442
433.622020	17739.237201	30.049460
433.894766	17760.346212	30.054477
434.083011	17777.506279	30.059495
434.498863	17808.272436	30.064512
434.695350	17830.884449	30.069530
434.755332	17871.000781	30.074548
435.077271	17905.352544	30.079565
434.929249	17948.612115	30.084583
435.525698	18002.707706	30.089600
436.269832	18041.266217	30.094618
436.575501	18086.179476	30.099636
437.195656	18117.500831	30.104653
437.396015	18162.282564	30.109671
437.930621	18205.499916	30.114688
438.594750	18251.892521	30.119706
438.763565	18291.932873	30.124724
438.739910	18334.800046	30.129741
439.423251	18391.491279	30.134759
439.959156	18434.352683	30.139776
440.817782	18467.817438	30.144794
441.209632	18521.200867	30.149812
441.982854	18550.485031	30.154829
442.580979	18593.752409	30.159847
443.089254	18625.475429	30.164864
443.729013	18658.207097	30.169882
444.248435	18697.392132	30.174900
444.628956	18722.622561	30.179917
445.229475	18758.754080	30.184935
445.452714	18787.787621	30.189952
446.008484	18813.396506	30.194970
446.151758	18852.903355	30.199988
446.631369	18881.620365	30.205005
447.512094	18911.768089	30.210023
448.006223	18943.161459	30.215040
448.756108	18960.759401	30.220058
449.086249	18993.940523	30.225076
449.297122	19019.293491	30.230093
449.760561	19051.862211	30.235111
450.031373	19075.782835	30.240128
450.598095	19106.446683	30.245146
450.740264	19146.514130	30.250164
451.098847	19176.173164	30.255181
451.771231	19203.572693	30.260199
451.889336	19234.610067	30.265216
452.342732	19273.115591	30.270234
452.668277	19327.047435	30.275252
453.541077	19345.704756	30.280269
454.524287	19371.848275	30.285287
455.505345	19378.193547	30.290304
456.431697	19401.756335	30.295322
456.775485	19420.370373	30.300340
456.913726	19418.341148	30.305357
457.270140	19439.133627	30.310375
457.845073	19438.811248	30.315392
458.856136	19430.961038	30.320410
458.819080	19438.064180	30.325428
459.383936	19452.376955	30.330445
459.568973	19462.589161	30.335463
459.798928	19477.793426	30.340480
460.221316	19485.459579	30.345498
460.454811	19518.530583	30.350516
460.845861	19532.830638	30.355533
461.197521	19555.230750	30.360551
461.135156	19581.777661	30.365568
461.580288	19622.912219	30.370586
461.869952	19653.222476	30.375604
462.079339	19690.785314	30.380621
462.380101	19736.321893	30.385639
462.636694	19780.696223	30.390656
463.139083	19816.786913	30.395674
463.845260	19876.520771	30.400692
463.862417	19917.306814	30.405709
464.247097	19964.660235	30.410727
464.479238	20023.821490	30.415744
465.010030	20069.431496	30.420762
465.499524	20126.030912	30.425780
466.360098	20177.571701	30.430797
466.869089	20224.341637	30.435815
467.259910	20279.865766	30.440832
468.703774	20305.857693	30.445850
469.131140	20349.753288	30.450868
469.881258	20381.080240	30.455885
470.453870	20407.729348	30.460903
470.693873	20444.900720	30.465920
471.092396	20470.826048	30.470938
471.623920	20508.310269	30.475956
472.805142	20533.704218	30.480973
472.911928	20567.178992	30.485991
472.735830	20605.035396	30.491008
473.321812	20634.672214	30.496026
473.256666	20674.239530	30.501044
473.781412	20707.266099	30.506061
474.829253	20750.695316	30.511079
474.770766	20799.397933	30.516096
475.309975	20846.244826	30.521114
476.093260	20883.275180	30.526132
476.746372	20915.356129	30.531149
476.741247	20950.175383	30.536167
477.051300	20999.141827	30.541184
477.413071	21045.688536	30.546202
477.603653	21092.870221	30.551220
478.449012	21136.961138	30.556237
479.813753	21164.587392	30.561255
480.803991	21193.375366	30.566272
481.763400	21215.772877	30.571290
481.837189	21237.890109	30.576308
482.520311	21254.336584	30.581325
483.026001	21270.457105	30.586343
482.869624	21293.000184	30.591360
483.386165	21304.858150	30.596378
483.969425	21341.401833	30.601396
484.138043	21363.876701	30.606413
484.844959	21387.065148	30.611431
485.055226	21422.540714	30.616448
485.090552	21447.340794	30.621466
485.483432	21473.858381	30.626484
486.660095	21494.454487	30.631501
487.459778	21520.500330	30.636519
487.362993	21546.475907	30.641536
487.816539	21570.166900	30.646554
488.255639	21612.863724	30.651572
488.933706	21646.141807	30.656589
489.414644	21672.236194	30.661607
490.226715	21697.638382	30.666624
490.887209	21721.344587	30.671642
491.258998	21751.318097	30.676660
491.738948	21780.844203	30.681677
492.555569	21800.491569	30.686695
492.790243	21834.733808	30.691712
493.049767	21856.801094	30.696730
493.276521	21897.276850	30.701748
493.226404	21937.298679	30.706765
493.900168	21969.116309	30.711783
494.322402	22019.446288	30.716800
494.973564	22063.565002	30.721818
494.977115	22103.988032	30.726836
495.347230	22152.056518	30.731853
495.800699	22191.279864	30.736871
495.973090	22246.992920	30.741888
496.589691	22292.534265	30.746906
496.881883	22352.119102	30.751924
497.404206	22416.811985	30.756941
498.049155	22460.749859	30.761959
498.290911	22522.731491	30.766976
499.011266	22571.636874	30.771994
499.634931	22631.648446	30.777012
500.129155	22679.643529	30.782029
501.081323	22724.879358	30.787047
501.576008	22787.244399	30.792064
501.961432	22822.396377	30.797082
502.495824	22877.642582	30.802100
502.807026	22923.824591	30.807117
503.523544	22964.953845	30.812135
504.069780	23020.050239	30.817152
504.657212	23067.371234	30.822170
505.264419	23117.581277	30.827188
505.721999	23160.073781	30.832205
506.377734	23205.345904	30.837223
506.669466	23250.115930	30.842240
507.324038	23289.465038	30.847258
508.117013	23328.711668	30.852276
508.846994	23366.303795	30.857293
509.330197	23391.621348	30.862311
509.647732	23421.338978	30.867328
510.164417	23448.010316	30.872346
511.709657	23459.579971	30.877364
512.535231	23482.315667	30.882381
513.113556	23489.960076	30.887399
513.142344	23520.673604	30.892416
513.217250	23535.996380	30.897434
514.100794	23553.918435	30.902452
514.738777	23581.430288	30.907469
515.538143	23591.657992	30.912487
515.546970	23620.406908	30.917504
515.907851	23640.553997	30.922522
516.337416	23668.650531	30.927540
516.826975	23701.998040	30.932557
517.762031	23733.884581	30.937575
517.938393	23765.033773	30.942592
517.365735	23788.637149	30.947610
518.408917	23825.605705	30.952628
518.438284	23861.533677	30.957645
518.801628	23896.227966	30.962663
518.854689	23954.749047	30.967680
519.417634	24006.240436	30.972698
519.972740	24060.319821	30.977716
520.011533	24121.228538	30.982733
520.954595	24176.109238	30.987751
521.486028	24232.249815	30.992768
521.790702	24295.753738	30.997786
522.407291	24346.271731	31.002804
523.151631	24411.722665	31.007821
524.340683	24464.272089	31.012839
524.754802	24514.042989	31.017856
524.931082	24561.835996	31.022874
524.917512	24614.746506	31.027892
525.418709	24679.700719	31.032909
526.275500	24732.487692	31.037927
526.577292	24786.912425	31.042944
527.224986	24854.113360	31.047962
527.693091	24907.197738	31.052980
528.380014	24967.052051	31.057997
528.670787	25022.151305	31.063015
529.494118	25075.661118	31.068032
530.195924	25121.312074	31.073050
531.098661	25175.038865	31.078068
531.045628	25238.541294	31.083085
531.880051	25281.674754	31.088103
532.714051	25341.962564	31.093120
533.355312	25389.940006	31.098138
534.672015	25423.562357	31.103156
535.117738	25468.122480	31.108173
535.984768	25503.872477	31.113191
536.495510	25535.506989	31.118208
536.673151	25561.706576	31.123226
537.372436	25592.151170	31.128244
537.617476	25627.619987	31.133261
538.145724	25647.163460	31.138279
539.066565	25684.425107	31.143296
539.109183	25720.159080	31.148314
539.506458	25755.444346	31.153332
539.856867	25795.065802	31.158349
540.115674	25836.286649	31.163367
540.575916	25882.271223	31.168384
541.248873	25921.538014	31.173402
541.827579	25960.171194	31.178420
541.948175	26010.946225	31.183437
542.745726	26052.330799	31.188455
543.169611	26116.549686	31.193472
543.329933	26168.842063	31.198490
543.991024	26217.291594	31.203508
543.979858	26278.102874	31.208525
544.367041	26331.741770	31.213543
544.719159	26402.128788	31.218560
545.485791	26466.179822	31.223578
545.939165	26535.256600	31.228596
546.547317	26615.528510	31.233613
547.182339	26678.975084	31.238631
548.007241	26733.934614	31.243648
548.663812	26800.321324	31.248666
549.287120	26854.441905	31.253684
550.296951	26907.632017	31.258701
550.824254	26966.015735	31.263719
551.399963	27035.127162	31.268736
551.565558	27088.339438	31.273754
552.457391	27124.631153	31.278772
553.097857	27190.763410	31.283789
553.658700	27234.727841	31.288807
554.421463	27286.033830	31.293824
555.138173	27338.038776	31.298842
555.708286	27378.146738	31.303860
556.403071	27430.360781	31.308877
556.911963	27484.051771	31.313895
557.566117	27513.844937	31.318912
558.398073	27564.928512	31.323930
559.105461	27609.685897	31.328948
559.192419	27656.713976	31.333965
559.676453	27695.506039	31.338983
560.373782	27744.612982	31.344000
560.425550	27810.577125	31.349018
561.332114	27848.344337	31.354036
561.601606	27908.535838	31.359053
561.712023	27962.419611	31.364071
562.461157	28019.926459	31.369088
563.135371	28082.355505	31.374106
563.271180	28130.868796	31.379124
564.132631	28191.489883	31.384141
565.027669	28244.908810	31.389159
565.563829	28297.881429	31.394176
565.607521	28363.022409	31.399194
566.281214	28402.777380	31.404212
567.319902	28463.782352	31.409229
567.851793	28511.935410	31.414247
568.397878	28556.057129	31.419264
569.290892	28597.109563	31.424282
570.320128	28631.667653	31.429300
570.705482	28664.935267	31.434317
571.363261	28695.490203	31.439335
572.051740	28729.390661	31.444352
572.142871	28785.977882	31.449370
572.413533	28812.847909	31.454388
572.739833	28866.508154	31.459405
572.921828	28915.511051	31.464423
573.144911	28980.166080	31.469440
573.553194	29041.303154	31.474458
574.186052	29107.712129	31.479476
574.651668	29181.053568	31.484493
575.735283	29245.565286	31.489511
576.727574	29291.836818	31.494528
576.812795	29364.278698	31.499546
577.869252	29402.711415	31.504564
579.003345	29447.122715	31.509581
579.524244	29507.099912	31.514599
580.166213	29565.993245	31.519616
580.678476	29613.572109	31.524634
581.376060	29653.534062	31.529652
581.855891	29716.191524	31.534669
582.087850	29766.939406	31.539687
582.682801	29821.821800	31.544704
583.086467	29876.125005	31.549722
583.418770	29923.369519	31.554740
583.737660	29994.546522	31.559757
584.395251	30054.965990	31.564775
585.323914	30116.364713	31.569792
585.704599	30188.503758	31.574810
586.492698	30244.297825	31.579828
586.690076	30313.947636	31.584845
587.286485	30382.838320	31.589863
588.238106	30432.243663	31.594880
589.103328	30504.509234	31.599898
589.939246	30555.771205	31.604916
590.301494	30608.408212	31.609933
591.019865	30669.204326	31.614951
591.889788	30722.505690	31.619968
592.343435	30773.903207	31.624986
593.291070	30819.773027	31.630004
594.095563	30874.591224	31.635021
594.544743	30922.345341	31.640039
595.101393	30965.830701	31.645056
595.598899	31021.172119	31.650074
596.354641	31065.380936	31.655092
596.654201	31114.423415	31.660109
597.125631	31172.486688	31.665127
597.714753	31223.139673	31.670144
597.754559	31274.552740	31.675162
598.157164	31318.339889	31.680180
599.345535	31374.838891	31.685197
599.997432	31429.233696	31.690215
601.007124	31476.861713	31.695232
600.939389	31526.239635	31.700250
601.666338	31563.288237	31.705268
602.162505	31618.445559	31.710285
602.531105	31665.991427	31.715303
603.739879	31714.232876	31.720320
603.967191	31777.606713	31.725338
604.118992	31824.237139	31.730356
604.876358	31878.233409	31.735373
605.183307	31941.518446	31.740391
605.998964	32005.085767	31.745408
606.323842	32071.514420	31.750426
607.113977	32134.878299	31.755444
607.752918	32193.159185	31.760461
608.140276	32247.901602	31.765479
609.475650	32308.818505	31.770496
610.141731	32375.697905	31.775514
611.224815	32422.776242	31.780532
611.975758	32460.819822	31.785549
612.344742	32506.698456	31.790567
614.051078	32541.470079	31.795584
614.602330	32586.661288	31.800602
615.162656	32618.909108	31.805620
615.976719	32649.371508	31.810637
616.656945	32687.484492	31.815655
617.427313	32724.594341	31.820672
617.469749	32754.557957	31.825690
617.859978	32792.638797	31.830708
618.550010	32836.430917	31.835725
618.700403	32891.231679	31.840743
619.305693	32933.302837	31.845760
619.922734	32994.212602	31.850778
620.024208	33048.974888	31.855796
620.615164	33104.432984	31.860813
620.608637	33167.937010	31.865831
621.624097	33235.160560	31.870848
621.829950	33303.911673	31.875866
622.223282	33378.598802	31.880884
622.862200	33454.323499	31.885901
623.287609	33527.396216	31.890919
624.001042	33597.743617	31.895936
624.775067	33665.366765	31.900954
625.641581	33726.113185	31.905972
626.083728	33791.717021	31.910989
626.758892	33873.162268	31.916007
627.559121	33940.390613	31.921024
627.981338	34019.601202	31.926042
628.859417	34073.678086	31.931060
629.791224	34154.755563	31.936077
630.091723	34231.740813	31.941095
630.828191	34279.341043	31.946112
631.798900	34338.136991	31.951130
632.612928	34398.768427	31.956148
634.144147	34433.545335	31.961165
634.346786	34476.083599	31.966183
635.122624	34510.005358	31.971200
636.043404	34571.524896	31.976218
636.363940	34615.444618	31.981236
637.024672	34654.758139	31.986253
637.348852	34702.139753	31.991271
637.579924	34744.904178	31.996288
638.260055	34813.848062	32.001306
638.573737	34860.862616	32.006324
639.330367	34920.871244	32.011341
639.228787	34988.639891	32.016359
639.946529	35052.408358	32.021376
639.997426	35128.019879	32.026394
641.127978	35203.547748	32.031412
641.819260	35280.959729	32.036429
642.258303	35351.256811	32.041447
643.033797	35423.204078	32.046464
644.108693	35494.967772	32.051482
644.908718	35564.881894	32.056500
645.380406	35629.272149	32.061517
645.965986	35699.996831	32.066535
647.067421	35753.232452	32.071552
647.794220	35817.282971	32.076570
648.689880	35884.577943	32.081588
649.125077	35934.831836	32.086605
649.738198	36009.798337	32.091623
650.459422	36080.791649	32.096640
650.529847	36149.838748	32.101658
651.149708	36219.331728	32.106676
651.806251	36276.552761	32.111693
652.403277	36352.587150	32.116711
653.202794	36413.631836	32.121728
653.898480	36498.084000	32.126746
654.151407	36576.416213	32.131764
655.012321	36652.305633	32.136781
655.112609	36737.697381	32.141799
656.243974	36820.498136	32.146816
656.518991	36898.487039	32.151834
657.579528	36983.324014	32.156852
658.118622	37063.285421	32.161869
658.620636	37140.892401	32.166887
659.157455	37218.853600	32.171904
659.578634	37304.666506	32.176922
659.859063	37389.863130	32.181940
661.120468	37479.778581	32.186957
661.978006	37569.984629	32.191975
662.727965	37648.050031	32.196992
663.040254	37727.967962	32.202010
663.722949	37814.849606	32.207028
664.671164	37891.991892	32.212045
665.109942	37976.264443	32.217063
666.227686	38048.936824	32.222080
667.082519	38131.655142	32.227098
667.514917	38193.125370	32.232116
668.605332	38256.705449	32.237133
669.012359	38334.649425	32.242151
669.769884	38391.357838	32.247168
670.416432	38461.997518	32.252186
671.289729	38529.366032	32.257204
671.875698	38597.645833	32.262221
672.597276	38668.661743	32.267239
673.324892	38729.890620	32.272256
673.505548	38798.600482	32.277274
674.148555	38875.189902	32.282292
675.022893	38930.105793	32.287309
675.767128	38999.054484	32.292327
676.660153	39072.025114	32.297344
677.823618	39138.904179	32.302362
678.593465	39199.142417	32.307380
679.580617	39257.364216	32.312397
679.982868	39315.402274	32.317415
680.928485	39370.720829	32.322432
681.689917	39430.819201	32.327450
681.964647	39494.079213	32.332468
683.355565	39537.369616	32.337485
683.952288	39598.087108	32.342503
683.827921	39654.641097	32.347520
684.744827	39721.495058	32.352538
685.018233	39794.549432	32.357556
685.654604	39854.395942	32.362573
685.993960	39931.878376	32.367591
686.545093	40007.787356	32.372608
687.213517	40084.607895	32.377626
687.771634	40172.159709	32.382644
688.663526	40245.106746	32.387661
689.464656	40318.341132	32.392679
689.886993	40388.976068	32.397696
690.532706	40460.204436	32.402714
691.486784	40541.139060	32.407732
692.610841	40618.480458	32.412749
693.341950	40700.704218	32.417767
694.302853	40768.195324	32.422784
695.054495	40832.315885	32.427802
695.801922	40898.094934	32.432820
697.389639	40943.454477	32.437837
697.941262	41004.165349	32.442855
698.966532	41056.548523	32.447872
699.468746	41110.473791	32.452890
699.934524	41164.421243	32.457908
700.777955	41205.094085	32.462925
701.584956	41257.654138	32.467943
702.377449	41307.337367	32.472960
703.149003	41356.585451	32.477978
703.398418	41421.523413	32.482996
704.085087	41475.942254	32.488013
704.624366	41533.654347	32.493031
704.704997	41593.952121	32.498048
705.180803	41666.660274	32.503066
705.718127	41728.222123	32.508084
706.336205	41793.050860	32.513101
706.946397	41860.845964	32.518119
707.941030	41930.697232	32.523136
708.996610	41993.885647	32.528154
708.984689	42075.216588	32.533172
709.919415	42133.658461	32.538189
710.573140	42209.637767	32.543207
711.078306	42285.939631	32.548224
711.259093	42355.009919	32.553242
711.820746	42434.049712	32.558260
712.140565	42520.769264	32.563277
712.479739	42619.478157	32.568295
713.385914	42712.706838	32.573312
713.901062	42809.517322	32.578330
714.450210	42918.750670	32.583348
715.370381	43012.130002	32.588365
716.017435	43095.284909	32.593383
717.389615	43194.198769	32.598400
718.729279	43284.798359	32.603418
719.300802	43370.907177	32.608436
720.655602	43436.913178	32.613453
721.989050	43521.247025	32.618471
723.047024	43587.367555	32.623488
723.749828	43642.898264	32.628506
724.512919	43699.189289	32.633524
725.439790	43756.753402	32.638541
726.680630	43817.080594	32.643559
727.308037	43869.985034	32.648576
728.075557	43926.329660	32.653594
728.428598	43986.995784	32.658612
729.730904	44037.262041	32.663629
730.173786	44089.052439	32.668647
731.094364	44138.228613	32.673664
731.374161	44189.620923	32.678682
732.019361	44252.738816	32.683700
732.589911	44312.797165	32.688717
733.001214	44381.879594	32.693735
733.610967	44444.000012	32.698752
734.022856	44516.692226	32.703770
734.465729	44608.790717	32.708788
734.944909	44694.580334	32.713805
735.715876	44776.565635	32.718823
736.302633	44857.177583	32.723840
737.087360	44951.300228	32.728858
737.416326	45039.971885	32.733876
738.181098	45127.031386	32.738893
738.799213	45227.941929	32.743911
739.359196	45316.966890	32.748928
739.971231	45412.975128	32.753946
740.619335	45508.014481	32.758964
741.789406	45603.454389	32.763981
742.646023	45702.466518	32.768999
743.278593	45791.051766	32.774016
744.266664	45883.625166	32.779034
744.947468	45968.460670	32.784052
745.605100	46045.806372	32.789069
746.530363	46133.512493	32.794087
747.039990	46207.650304	32.799104
747.993650	46296.473441	32.804122
748.648802	46383.854322	32.809140
749.100585	46463.081330	32.814157
749.837042	46563.441773	32.819175
750.371907	46663.306697	32.824192
751.021529	46745.602328	32.829210
751.300013	46849.109333	32.834228
752.409747	46948.469857	32.839245
753.374369	47044.725924	32.844263
753.875104	47144.807644	32.849280
754.976520	47235.697443	32.854298
755.594072	47352.410724	32.859316
756.320809	47451.498361	32.864333
757.339364	47535.401774	32.869351
758.042568	47633.568988	32.874368
759.102798	47734.748637	32.879386
759.652668	47837.604907	32.884404
760.199589	47935.626718	32.889421
761.255348	48043.842515	32.894439
761.745815	48146.846421	32.899456
762.580574	48246.244959	32.904474
763.138167	48352.346378	32.909492
763.899684	48456.970020	32.914509
764.913368	48562.372244	32.919527
765.522191	48666.536765	32.924544
766.452109	48759.888872	32.929562
767.340109	48865.724888	32.934580
768.178050	48964.924427	32.939597
769.360075	49059.416099	32.944615
770.090482	49161.869456	32.949632
771.048489	49264.063265	32.954650
771.698173	49370.391381	32.959668
772.415258	49458.862160	32.964685
773.226772	49552.162556	32.969703
773.797514	49646.989222	32.974720
774.778757	49742.017683	32.979738
775.549672	49840.032870	32.984756
777.173601	49919.013264	32.989773
778.045852	50005.469956	32.994791
779.003812	50080.041768	32.999808
780.323027	50164.129353	33.004826
781.268655	50241.035062	33.009844
781.947560	50300.025901	33.014861
782.257880	50371.765777	33.019879
783.132158	50450.699847	33.024896
783.914993	50525.019066	33.029914
784.249127	50612.606719	33.034932
784.662244	50695.209206	33.039949
785.141667	50780.233008	33.044967
785.744081	50885.004370	33.049984
786.164324	50977.841601	33.055002
786.693824	51073.996365	33.060020
787.778861	51159.391915	33.065037
788.974895	51241.628843	33.070055
789.293851	51328.716867	33.075072
790.453093	51413.424800	33.080090
791.288747	51513.951832	33.085108
791.691111	51604.368994	33.090125
792.566769	51685.064208	33.095143
793.053627	51790.643634	33.100160
793.859608	51877.082043	33.105178
794.559747	51991.705096	33.110196
794.759807	52095.553574	33.115213
795.768923	52202.884337	33.120231
796.363891	52323.415880	33.125248
796.956064	52431.413216	33.130266
797.785588	52541.682983	33.135284
798.595000	52659.879993	33.140301
799.019756	52768.811371	33.145319
799.612437	52903.101925	33.150336
801.047784	53013.674936	33.155354
802.041373	53138.414440	33.160372
802.769855	53253.014686	33.165389
803.961434	53359.429571	33.170407
805.158231	53476.332989	33.175424
806.126643	53574.648916	33.180442
806.806018	53684.862312	33.185460
807.149925	53796.334331	33.190477
808.350604	53899.445882	33.195495
809.333001	54004.775328	33.200512
810.242632	54108.474911	33.205530
811.255834	54221.408053	33.210548
812.034325	54330.375880	33.215565
813.212810	54416.123376	33.220583
813.919276	54527.960759	33.225600
814.535307	54632.263105	33.230618
815.366708	54730.684045	33.235636
816.222485	54825.651111	33.240653
817.821122	54908.017598	33.245671
819.029892	55002.526947	33.250688
820.260586	55084.780252	33.255706
821.026517	55178.734376	33.260724
821.777276	55244.868307	33.265741
823.130925	55306.861245	33.270759
823.523760	55397.802868	33.275776
824.392368	55475.001250	33.280794
824.730079	55555.469444	33.285812
825.171818	55642.157266	33.290829
825.895001	55734.370881	33.295847
826.742975	55831.934979	33.300864
827.579751	55928.250236	33.305882
828.217989	56004.529573	33.310900
829.207107	56093.602790	33.315917
830.506304	56181.599543	33.320935
831.904923	56259.455863	33.325952
832.772789	56329.257567	33.330970
833.923580	56401.241844	33.335988
834.637261	56463.278464	33.341005
835.649740	56511.556996	33.346023
836.745836	56564.889613	33.351040
837.363928	56607.927493	33.356058
838.687220	56669.948814	33.361076
838.849807	56721.179319	33.366093
839.962695	56774.389544	33.371111
840.508205	56839.110374	33.376128
841.133701	56909.966752	33.381146
841.758456	56979.382616	33.386164
842.629069	57055.297516	33.391181
842.517345	57136.885449	33.396199
842.703869	57235.909434	33.401216
843.490298	57328.675666	33.406234
843.888403	57426.166551	33.411252
843.865426	57538.670189	33.416269
844.735687	57659.534374	33.421287
845.286599	57788.752064	33.426304
845.795764	57919.248045	33.431322
846.314528	58055.835728	33.436340
846.804152	58187.202621	33.441357
847.926630	58314.202216	33.446375
848.917638	58459.528283	33.451392
849.911836	58599.229864	33.456410
850.667257	58728.999962	33.461428
851.340928	58887.662262	33.466445
852.493139	59016.791086	33.471463
853.165801	59168.724596	33.476480
854.104496	59313.642248	33.481498
854.844625	59460.111847	33.486516
855.506289	59604.320551	33.491533
857.001250	59739.266992	33.496551
858.257472	59872.409601	33.501568
859.231003	60001.044317	33.506586
860.609213	60132.366343	33.511604
861.680288	60258.476662	33.516621
862.751750	60375.580624	33.521639
863.669191	60509.594450	33.526656
864.691368	60615.640525	33.531674
865.621434	60736.645425	33.536692
866.254227	60854.415086	33.541709
867.374676	60966.798640	33.546727
868.137044	61090.514414	33.551744
868.808351	61206.313669	33.556762
869.778512	61326.265879	33.561780
870.578304	61458.978613	33.566797
871.091402	61581.166071	33.571815
871.958954	61709.987646	33.576832
872.256796	61842.200940	33.581850
873.713117	61973.224230	33.586868
873.630358	62101.484056	33.591885
874.777504	62238.541903	33.596903
875.490516	62373.582640	33.601920
876.832787	62503.288687	33.606938
877.961659	62632.659129	33.611956
878.320658	62766.422906	33.616973
879.458100	62888.043340	33.621991
880.946584	63008.902671	33.627008
881.803236	63119.636271	33.632026
883.252289	63226.153629	33.637044
884.163967	63334.236510	33.642061
885.286022	63438.282297	33.647079
885.750934	63552.612787	33.652096
886.610689	63658.525249	33.657114
887.730024	63756.839266	33.662132
888.548027	63878.248351	33.667149
889.311906	63979.924282	33.672167
889.973671	64086.233165	33.677184
890.414005	64201.367964	33.682202
891.773424	64325.443268	33.687220
892.249994	64463.901302	33.692237
893.029368	64580.193935	33.697255
893.692459	64709.334589	33.702272
894.788775	64840.355370	33.707290
895.691435	64966.384032	33.712308
896.312451	65101.470790	33.717325
897.106944	65232.071537	33.722343
898.549922	65363.345992	33.727360
899.393959	65486.517499	33.732378
900.587278	65608.839615	33.737396
901.354420	65744.373316	33.742413
902.431513	65865.009780	33.747431
903.192079	65996.708523	33.752448
903.743160	66133.963494	33.757466
904.729591	66261.325907	33.762484
905.258400	66406.394778	33.767501
906.144907	66545.106058	33.772519
906.984194	66696.180800	33.777536
908.122337	66832.239602	33.782554
909.241852	66977.179592	33.787572
909.622818	67107.666721	33.792589
911.187885	67229.302246	33.797607
912.967588	67357.218238	33.802624
913.826400	67486.879757	33.807642
914.621262	67606.139153	33.812660
916.068538	67731.066671	33.817677
917.101178	67836.565807	33.822695
918.284543	67955.943990	33.827712
919.392304	68073.103745	33.832730
920.668536	68183.204006	33.837748
921.582909	68272.841936	33.842765
922.921793	68369.887828	33.847783
923.969660	68467.483532	33.852800
924.794654	68566.951579	33.857818
925.913056	68646.369443	33.862836
926.672879	68754.474414	33.867853
927.610742	68843.756607	33.872871
928.479115	68936.484635	33.877888
929.083860	69036.915784	33.882906
930.157792	69113.876889	33.887924
930.896368	69210.188384	33.892941
931.876477	69296.866308	33.897959
933.307400	69369.454616	33.902976
933.721701	69469.294377	33.907994
934.740632	69549.390257	33.913012
935.087633	69649.432082	33.918029
935.908992	69739.876182	33.923047
936.696974	69829.649754	33.928064
937.020328	69942.312531	33.933082
937.827222	70050.030202	33.938100
938.575456	70172.087911	33.943117
939.119366	70294.307774	33.948135
939.879054	70415.087500	33.953152
940.404197	70559.002547	33.958170
941.269270	70694.032260	33.963188
941.851535	70832.058170	33.968205
942.485170	70983.027536	33.973223
943.327419	71133.861040	33.978240
943.969770	71292.520997	33.983258
944.442489	71443.913202	33.988276
945.557162	71613.783041	33.993293
946.911948	71786.977530	33.998311
947.245977	71951.627131	34.003328
948.196671	72128.903072	34.008346
948.965495	72283.551641	34.013364
950.472335	72453.272302	34.018381
951.815668	72615.047224	34.023399
954.073298	72753.955731	34.028416
954.745540	72902.104718	34.033434
956.401626	73046.702603	34.038452
957.139884	73203.943294	34.043469
957.660040	73336.151745	34.048487
959.184043	73477.827824	34.053504
959.823669	73630.522061	34.058522
961.356968	73759.751393	34.063540
962.217115	73899.216370	34.068557
962.848018	74043.376534	34.073575
964.218469	74191.060423	34.078592
964.963017	74332.483328	34.083610
966.492429	74450.806953	34.088628
967.366920	74588.547115	34.093645
968.420300	74733.158066	34.098663
969.591898	74856.737955	34.103680
970.297517	75001.587308	34.108698
970.931385	75132.471398	34.113716
971.873687	75275.852530	34.118733
972.919808	75426.528727	34.123751
973.668476	75565.593151	34.128768
974.388374	75720.052757	34.133786
975.358264	75874.495921	34.138804
976.091586	76014.856135	34.143821
976.733373	76177.327530	34.148839
978.016066	76319.246506	34.153856
979.006636	76472.361912	34.158874
980.047207	76612.439213	34.163892
981.375439	76749.760786	34.168909
982.118903	76894.767738	34.173927
983.952855	77017.430156	34.178944
984.442517	77145.934322	34.183962
985.949577	77262.132284	34.188980
986.520461	77397.753053	34.193997
987.339692	77538.443345	34.199015
988.246416	77675.703585	34.204032
988.699697	77823.113086	34.209050
989.903871	77955.023012	34.214068
991.066475	78102.281237	34.219085
991.584995	78250.295965	34.224103
992.663101	78393.939441	34.229120
993.339483	78562.849353	34.234138
994.686793	78706.271578	34.239156
995.481361	78852.218605	34.244173
996.453288	79019.531395	34.249191
997.776013	79161.353849	34.254208
998.895809	79317.996454	34.259226
1000.240732	79476.600705	34.264244
1001.211846	79621.086353	34.269261
1001.987394	79776.456193	34.274279
1002.928179	79922.714011	34.279296
1003.659225	80067.737055	34.284314
1005.724069	80205.421599	34.289332
1007.145055	80341.686200	34.294349
1007.915157	80483.858238	34.299367
1009.331459	80618.651189	34.304384
1010.267201	80759.961456	34.309402
1011.180095	80890.976609	34.314420
1012.598825	81019.122118	34.319437
1013.499299	81162.465460	34.324455
1014.455051	81299.694837	34.329472
1015.114269	81452.172948	34.334490
1016.229418	81579.443510	34.339508
1017.058046	81728.085637	34.344525
1017.658449	81876.710857	34.349543
1018.922518	82016.662921	34.354560
1019.154823	82173.268186	34.359578
1020.326063	82321.482158	34.364596
1021.299940	82483.074833	34.369613
1022.151445	82647.530499	34.374631
1023.226917	82794.207399	34.379648
1024.676337	82963.744926	34.384666
1025.850882	83115.936936	34.389684
1027.019200	83262.468016	34.394701
1028.238751	83410.674334	34.399719
1029.498025	83550.668099	34.404736
1030.314989	83704.677884	34.409754
1030.928989	83859.913012	34.414772
1031.908471	84009.581604	34.419789
1032.281932	84183.912375	34.424807
1033.285557	84341.380899	34.429824
1034.075860	84511.466473	34.434842
1035.147521	84667.343607	34.439860
1035.891080	84838.743067	34.444877
1036.272536	85011.749771	34.449895
1037.527804	85162.618739	34.454912
1038.383316	85336.660358	34.459930
1039.269168	85515.659192	34.464948
1040.203498	85688.209159	34.469965
1040.859343	85882.190602	34.474983
1041.710448	86057.997485	34.480000
1042.366032	86252.184498	34.485018
1044.025383	86441.600607	34.490036
1045.414825	86623.141455	34.495053
1046.492022	86809.540346	34.500071
1047.930762	86984.987676	34.505088
1049.418143	87157.251109	34.510106
1050.840456	87335.444032	34.515124
1052.311391	87494.726733	34.520141
1054.239018	87637.667959	34.525159
1055.767811	87787.671407	34.530176
1056.901089	87937.762505	34.535194
1057.821726	88087.739065	34.540212
1059.047263	88224.798127	34.545229
1059.949456	88388.873721	34.550247
1060.593539	88534.698149	34.555264
1061.668476	88686.943043	34.560282
1062.911750	88841.830852	34.565300
1064.207895	88985.198352	34.570317
1065.270374	89122.834735	34.575335
1066.590192	89266.820090	34.580352
1067.810694	89421.620587	34.585370
1068.847222	89562.599304	34.590388
1069.954510	89702.895844	34.595405
1070.976276	89847.771131	34.600423
1072.626805	89975.647124	34.605440
1073.357284	90116.630834	34.610458
1074.227672	90256.471135	34.615476
1075.202772	90414.775748	34.620493
1075.605639	90563.438576	34.625511
1076.528025	90718.456623	34.630528
1077.529191	90884.241104	34.635546
1078.392577	91049.923713	34.640564
1079.279651	91205.248381	34.645581
1079.759009	91384.961821	34.650599
1080.834487	91554.883956	34.655616
1081.934098	91729.898466	34.660634
1082.679279	91912.836333	34.665652
1083.776790	92092.904850	34.670669
1084.794752	92275.083450	34.675687
1085.971780	92446.893290	34.680704
1087.117937	92638.958749	34.685722
1087.975977	92831.119344	34.690740
1089.027618	93019.279415	34.695757
1090.353004	93212.185843	34.700775
1091.791872	93387.299622	34.705792
1092.937726	93567.389605	34.710810
1093.657144	93738.153685	34.715828
1095.275096	93914.468566	34.720845
1095.946795	94085.869891	34.725863
1097.354093	94248.955106	34.730880
1098.520474	94422.331376	34.735898
1099.425506	94599.659415	34.740916
1100.749087	94768.985085	34.745933
1101.185257	94946.389531	34.750951
1101.984966	95112.838257	34.755968
1102.740566	95309.821360	34.760986
1103.620754	95503.948583	34.766004
1104.797716	95696.627428	34.771021
1106.174488	95886.912202	34.776039
1106.852288	96081.072200	34.781056
1107.935270	96293.840056	34.786074
1108.746560	96504.636693	34.791092
1110.363748	96701.571788	34.796109
1111.436047	96911.428142	34.801127
1112.685614	97107.296101	34.806144
1113.720378	97306.139941	34.811162
1114.743758	97511.869152	34.816180
1116.182470	97713.306060	34.821197
1117.775078	97913.306362	34.826215
1119.869399	98082.781873	34.831232
1121.913170	98253.337148	34.836250
1122.969454	98427.633484	34.841268
1124.603916	98603.326210	34.846285
1125.562347	98773.678241	34.851303
1126.148832	98936.972238	34.856320
1127.041121	99110.889756	34.861338
1128.225220	99300.555593	34.866356
1129.226837	99470.170392	34.871373
1129.989377	99646.969274	34.876391
1131.303851	99824.909539	34.881408
1132.257441	100022.325754	34.886426
1133.183818	100211.966437	34.891444
1134.620312	100397.285212	34.896461
1135.371878	100587.256165	34.901479
1136.599695	100784.333639	34.906496
1137.620644	100972.918934	34.911514
1138.494974	101174.555547	34.916532
1139.803656	101362.752476	34.921549
1140.711613	101564.411674	34.926567
1141.934074	101762.472602	34.931584
1142.746693	101971.192564	34.936602
1143.820497	102174.867027	34.941620
1145.295971	102375.194193	34.946637
1145.967650	102594.885385	34.951655
1147.057677	102794.002610	34.956672
1148.526724	103010.470565	34.961690
1148.958338	103218.708409	34.966708
1150.427260	103435.838450	34.971725
1151.087931	103665.089863	34.976743
1152.145507	103882.547296	34.981760
1153.447514	104095.721776	34.986778
1154.647016	104306.813055	34.991796
1155.768904	104507.546226	34.996813
1157.086828	104717.404596	35.001831
1158.527001	104918.529667	35.006848
1160.337817	105115.805718	35.011866
1161.140627	105324.870446	35.016884
1162.371544	105508.126179	35.021901
1163.641721	105712.592153	35.026919
1165.332236	105895.759183	35.031936
1167.004030	106078.804006	35.036954
1168.214823	106266.438225	35.041972
1169.862322	106438.355925	35.046989
1170.996886	106621.141751	35.052007
1171.896336	106808.136383	35.057024
1172.973471	106990.959875	35.062042
1173.696452	107181.255305	35.067060
1174.826159	107361.792276	35.072077
1175.680954	107563.772014	35.077095
1176.601658	107767.920701	35.082112
1178.296150	107973.635844	35.087130
1179.155123	108181.243665	35.092148
1180.214866	108384.144439	35.097165
1181.291376	108586.511815	35.102183
1182.572125	108790.226483	35.107200
1183.470686	108992.234628	35.112218
1185.043808	109196.928340	35.117236
1186.435969	109402.097931	35.122253
1187.922353	109600.969638	35.127271
1189.461436	109790.852147	35.132288
1191.372690	109971.639908	35.137306
1192.681513	110169.393317	35.142324
1193.840833	110356.165018	35.147341
1194.558735	110551.121288	35.152359
1195.513168	110751.675886	35.157376
1196.723907	110941.673176	35.162394
1197.269912	111153.182853	35.167412
1198.435147	111350.981927	35.172429
1199.671362	111547.351346	35.177447
1200.532424	111771.721277	35.182464
1201.759583	111977.191535	35.187482
1202.296053	112211.629061	35.192500
1203.920465	112424.192625	35.197517
1205.542174	112647.957913	35.202535
1206.792394	112855.622437	35.207552
1208.099043	113065.103235	35.212570
1208.938456	113282.647408	35.217588
1210.536290	113499.581967	35.222605
1211.673909	113722.184346	35.227623
1212.734501	113931.599652	35.232640
1214.382231	114152.090894	35.237658
1215.509584	114370.861111	35.242676
1216.537464	114579.311189	35.247693
1217.868329	114798.480631	35.252711
1218.821923	115018.425880	35.257728
1220.147771	115228.831597	35.262746
1221.135447	115445.340597	35.267764
1222.116133	115647.103812	35.272781
1222.719372	115861.134959	35.277799
1223.291000	116085.727896	35.282816
1224.857863	116307.415285	35.287834
1225.863165	116538.348984	35.292852
1227.312786	116764.545488	35.297869
1227.953236	117005.378154	35.302887
1229.038540	117239.940382	35.307904
1230.996439	117471.972892	35.312922
1232.518000	117694.705022	35.317940
1234.426166	117914.521555	35.322957
1236.000519	118131.190945	35.327975
1236.987624	118355.210743	35.332992
1238.579706	118574.110612	35.338010
1239.353304	118800.413282	35.343028
1240.663915	119038.068664	35.348045
1241.498036	119267.025697	35.353063
1243.108430	119494.711109	35.358080
1243.953862	119730.576197	35.363098
1244.968917	119973.776846	35.368116
1246.080920	120212.806276	35.373133
1247.240609	120451.246519	35.378151
1248.508336	120693.003123	35.383168
1250.276778	120926.679365	35.388186
1251.190650	121172.251603	35.393204
1252.328569	121415.430301	35.398221
1253.874544	121652.546685	35.403239
1254.951070	121906.461406	35.408256
1255.887868	122149.680471	35.413274
1257.704214	122408.782940	35.418292
1258.365725	122661.190863	35.423309
1259.855893	122913.623792	35.428327
1261.164064	123179.524257	35.433344
1262.638058	123430.367344	35.438362
1263.478648	123673.209529	35.443380
1264.822934	123934.484368	35.448397
1266.020283	124193.505224	35.453415
1267.245206	124460.343642	35.458432
1268.841709	124712.760573	35.463450
1270.351929	124981.316429	35.468468
1271.747402	125233.290406	35.473485
1272.812501	125480.519243	35.478503
1273.539780	125748.924276	35.483520
1275.560820	125999.238390	35.488538
1276.962306	126264.997470	35.493556
1278.024281	126525.632769	35.498573
1279.488739	126776.149809	35.503591
1280.720171	127033.363349	35.508608
1281.900378	127294.289026	35.513626
1283.186131	127547.251176	35.518644
1284.825503	127795.109885	35.523661
1286.588336	128036.041080	35.528679
1287.640477	128292.395624	35.533696
1289.751541	128528.454109	35.538714
1291.082854	128763.760503	35.543732
1292.367291	128979.352470	35.548749
1293.962158	129187.210925	35.553767
1294.797496	129416.877365	35.558784
1296.184222	129616.876863	35.563802
1297.374163	129835.381030	35.568820
1298.592454	130049.508396	35.573837
1299.714920	130275.835926	35.578855
1300.397606	130515.614373	35.583872
1301.986335	130746.771334	35.588890
1302.737167	130990.763061	35.593908
1304.071351	131242.136266	35.598925
1305.479282	131489.771701	35.603943
1306.479441	131742.739906	35.608960
1307.663468	131987.362231	35.613978
1309.017123	132246.447733	35.618996
1310.025657	132497.696224	35.624013
1311.601915	132754.313551	35.629031
1312.320387	133013.361719	35.634048
1313.905091	133262.134018	35.639066
1315.396209	133529.079097	35.644084
1316.424441	133805.436648	35.649101
1317.981576	134065.934293	35.654119
1319.108850	134333.607414	35.659136
1320.679042	134586.335114	35.664154
1321.771662	134859.913857	35.669172
1322.781437	135131.734020	35.674189
1324.392571	135409.691381	35.679207
1325.621924	135696.350671	35.684224
1326.956918	135957.737915	35.689242
1328.682985	136233.780588	35.694260
1329.660612	136520.528019	35.699277
1330.998421	136796.730504	35.704295
1332.463597	137076.159347	35.709312
1333.922642	137355.084360	35.714330
1335.445366	137632.935676	35.719348
1336.756554	137905.931120	35.724365
1338.702087	138174.128658	35.729383
1339.328208	138462.131814	35.734400
1340.915765	138726.248629	35.739418
1342.509702	139010.438890	35.744436
1343.546320	139292.254253	35.749453
1345.373432	139568.154408	35.754471
1346.239802	139857.218568	35.759488
1347.437343	140136.071392	35.764506
1348.481358	140420.633616	35.769524
1349.968651	140703.296265	35.774541
1351.535338	140980.063728	35.779559
1352.736642	141267.940948	35.784576
1354.144534	141555.873927	35.789594
1355.649295	141836.982936	35.794612
1356.791876	142136.163440	35.799629
1358.321436	142426.682318	35.804647
1359.391151	142717.168143	35.809664
1360.426937	143004.973664	35.814682
1361.880772	143285.062948	35.819700
1362.649115	143572.639810	35.824717
1364.165414	143848.969021	35.829735
1365.448804	144139.518565	35.834752
1366.838491	144417.192716	35.839770
1368.256950	144716.892855	35.844788
1369.307635	145012.942533	35.849805
1370.999431	145305.346523	35.854823
1372.434828	145602.983842	35.859840
1374.403439	145881.660760	35.864858
1375.604531	146172.544991	35.869876
1377.153088	146467.608069	35.874893
1378.574337	146743.874030	35.879911
1379.947199	147045.490752	35.884928
1381.206671	147330.603390	35.889946
1382.936364	147624.021255	35.894964
1383.999258	147907.180708	35.899981
1385.215751	148201.769022	35.904999
1386.579617	148502.384402	35.910016
1388.411659	148784.264645	35.915034
1390.232488	149063.916607	35.920052
1391.698833	149352.078637	35.925069
1393.692276	149633.519032	35.930087
1395.332351	149914.121440	35.935104
1396.431054	150190.100142	35.940122
1398.256075	150467.706924	35.945140
1399.496805	150745.111304	35.950157
1401.368807	151023.043855	35.955175
1402.400425	151296.568578	35.960192
1403.686925	151566.626823	35.965210
1405.527097	151849.022999	35.970228
1406.677686	152112.575795	35.975245
1408.136338	152384.500273	35.980263
1409.470222	152671.720458	35.985280
1410.398819	152950.437153	35.990298
1411.866008	153240.581580	35.995316
1412.980245	153528.073956	36.000333
1414.567893	153822.045619	36.005351
1415.773595	154112.900844	36.010368
1417.394835	154406.756930	36.015386
1418.976644	154701.370375	36.020404
1419.994943	155004.378766	36.025421
1421.464574	155292.723757	36.030439
1423.185238	155581.941226	36.035456
1424.421033	155874.262976	36.040474
1426.179100	156165.837791	36.045492
1427.318943	156459.080889	36.050509
1429.004695	156749.149961	36.055527
1430.726382	157035.218812	36.060544
1432.258693	157317.427404	36.065562
1433.931684	157597.063913	36.070580
1435.331915	157879.019876	36.075597
1437.315495	158142.152665	36.080615
1438.947837	158411.753965	36.085632
1440.156835	158682.216046	36.090650
1441.735700	158929.450608	36.095668
1442.841022	159195.417295	36.100685
1444.548371	159449.788318	36.105703
1445.692025	159711.717298	36.110720
1446.682098	159979.992348	36.115738
1447.967659	160240.936124	36.120756
1449.053091	160516.303060	36.125773
1450.472746	160797.032063	36.130791
1451.612866	161077.442829	36.135808
1452.669155	161359.379596	36.140826
1454.295236	161636.589754	36.145844
1455.758358	161932.543852	36.150861
1457.510300	162218.693704	36.155879
1458.623698	162513.468253	36.160896
1459.766113	162809.863896	36.165914
1461.538794	163104.694584	36.170932
1462.375484	163407.300293	36.175949
1464.438226	163708.340642	36.180967
1465.816227	164013.446290	36.185984
1466.924389	164327.076042	36.191002
1467.861504	164636.334414	36.196020
1469.109435	164963.407178	36.201037
1470.114743	165283.786224	36.206055
1471.617802	165623.077369	36.211072
1473.076792	165960.196158	36.216090
1475.189807	166286.661084	36.221108
1476.199153	166634.216011	36.226125
1477.550836	166968.454932	36.231143
1479.185118	167309.220942	36.236160
1480.350585	167659.764335	36.241178
1481.804621	168012.710077	36.246196
1483.342157	168368.702402	36.251213
1484.696167	168711.430222	36.256231
1485.990438	169070.984597	36.261248
1487.138425	169443.167718	36.266266
1489.205118	169803.839159	36.271284
1490.027344	170172.276870	36.276301
1491.994968	170541.701622	36.281319
1493.558149	170916.921736	36.286336
1494.803299	171294.267752	36.291354
1496.493808	171650.982161	36.296372
1498.563475	172010.857715	36.301389
1500.792009	172355.442055	36.306407
1502.585752	172706.702389	36.311424
1504.220251	173064.223665	36.316442
1505.959883	173401.449652	36.321460
1507.706118	173748.854938	36.326477
1509.118632	174084.656771	36.331495
1510.958454	174428.205469	36.336512
1512.251990	174771.012419	36.341530
1513.960042	175106.415254	36.346548
1515.234491	175442.110297	36.351565
1517.273996	175772.752394	36.356583
1518.323792	176105.660128	36.361600
1520.132793	176437.881703	36.366618
1522.091355	176742.691249	36.371636
1523.520956	177054.192842	36.376653
1524.746756	177373.358989	36.381671
1526.308611	177685.336767	36.386688
1527.468257	178004.200848	36.391706
1528.900024	178315.405097	36.396724
1530.064155	178651.330502	36.401741
1531.406039	178974.243519	36.406759
1532.655925	179315.755778	36.411776
1533.848348	179650.908513	36.416794
1535.672526	179990.181850	36.421812
1536.492679	180339.567420	36.426829
1537.843107	180691.796529	36.431847
1539.341454	181060.350840	36.436864
1540.334696	181419.347586	36.441882
1542.028787	181782.783522	36.446900
1543.343824	182160.540946	36.451917
1544.929407	182537.988128	36.456935
1546.842782	182921.487210	36.461952
1547.520996	183310.112595	36.466970
1549.144957	183685.441280	36.471988
1551.154858	184079.886173	36.477005
1552.657101	184472.148575	36.482023
1554.731393	184858.527543	36.487040
1556.347577	185241.128661	36.492058
1558.894397	185609.851158	36.497076
1560.944530	185979.587671	36.502093
1562.398414	186343.030856	36.507111
1564.437185	186706.833220	36.512128
1566.160965	187078.701713	36.517146
1567.868562	187423.511425	36.522164
1569.155726	187789.365946	36.527181
1570.892189	188143.797147	36.532199
1572.243950	188514.113476	36.537216
1573.765998	188928.363861	36.542234
1575.703426	189275.277649	36.547252
1577.172862	189646.075900	36.552269
1578.515899	190001.842143	36.557287
1579.996996	190377.479522	36.562304
1581.437740	190744.239714	36.567322
1583.357932	191109.561686	36.572340
1584.911902	191467.407649	36.577357
1586.649641	191841.448503	36.582375
1588.010412	192191.574978	36.587392
1589.822977	192557.228490	36.592410
1592.354962	192903.045242	36.597428
1594.283399	193256.495480	36.602445
1596.138998	193606.138806	36.607463
1597.733449	193941.774815	36.612480
1599.069090	194287.956057	36.617498
1601.006462	194617.316053	36.622516
1602.449147	194951.497832	36.627533
1604.139991	195299.197891	36.632551
1605.893854	195633.875787	36.637568
1607.067548	195961.836951	36.642586
1608.588608	196287.543885	36.647604
1609.879915	196615.716637	36.652621
1611.135687	196936.609523	36.657639
1612.724201	197272.098295	36.662656
1614.245216	197613.453194	36.667674
1615.975166	197942.725303	36.672692
1617.979209	198265.984818	36.677709
1619.041049	198602.128794	36.682727
1620.730539	198925.838767	36.687744
1621.876152	199283.631746	36.692762
1623.324216	199639.229060	36.697780
1624.715261	199986.902523	36.702797
1626.151105	200345.654190	36.707815
1627.900476	200714.892274	36.712832
1629.283923	201086.327902	36.717850
1630.569611	201454.163533	36.722868
1632.149616	201823.969449	36.727885
1632.793010	202212.449665	36.732903
1634.397593	202607.255629	36.737920
1636.037288	203011.732857	36.742938
1637.297949	203409.763435	36.747956
1638.969002	203825.070313	36.752973
1640.092463	204243.330018	36.757991
1641.686769	204666.907802	36.763008
1642.996506	205093.647442	36.768026
1644.789114	205524.966760	36.773044
1646.396475	205961.119801	36.778061
1647.478706	206400.602962	36.783079
1649.574230	206846.035440	36.788096
1651.188892	207291.946250	36.793114
1653.153715	207727.577768	36.798132
1655.322751	208161.398913	36.803149
1657.317301	208599.315514	36.808167
1659.391497	209029.678096	36.813184
1660.850087	209467.233730	36.818202
1662.404666	209901.346643	36.823220
1664.359366	210329.958403	36.828237
1666.050500	210758.668141	36.833255
1667.801449	211194.252238	36.838272
1669.988676	211632.963815	36.843290
1672.193385	212064.360189	36.848308
1673.709226	212487.520805	36.853325
1674.948227	212918.146723	36.858343
1677.102008	213332.008245	36.863360
1679.080420	213757.965391	36.868378
1681.471639	214162.748430	36.873396
1683.788404	214562.821948	36.878413
1685.294314	214975.480767	36.883431
1687.012018	215371.418674	36.888448
1688.917693	215762.932156	36.893466
1690.884465	216156.697155	36.898484
1692.517739	216558.114813	36.903501
1694.477598	216942.816902	36.908519
1696.219563	217319.150847	36.913536
1697.852464	217705.410226	36.918554
1699.268442	218076.164219	36.923572
1701.268654	218443.365342	36.928589
1702.108174	218811.121892	36.933607
1703.976173	219177.179808	36.938624
1705.260826	219555.809626	36.943642
1706.709937	219926.437327	36.948660
1708.617506	220307.045868	36.953677
1709.761943	220689.716600	36.958695
1711.810767	221077.593141	36.963712
1713.029786	221476.280689	36.968730
1714.629960	221870.535696	36.973748
1716.142578	222269.226526	36.978765
1717.207328	222675.716800	36.983783
1719.162748	223078.474716	36.988800
1720.513314	223501.454073	36.993818
1722.178410	223930.172244	36.998836
1723.807380	224354.249880	37.003853
1725.307197	224781.449843	37.008871
1727.555215	225206.796022	37.013888
1728.972048	225650.497746	37.018906
1730.709645	226082.207954	37.023924
1733.037424	226506.300083	37.028941
1734.677437	226936.683516	37.033959
1736.380949	227370.257904	37.038976
1738.457150	227813.777725	37.043994
1740.393901	228241.955380	37.049012
1742.159544	228676.107365	37.054029
1743.619149	229111.100428	37.059047
1745.251929	229548.275022	37.064064
1747.089904	229993.213888	37.069082
1748.248291	230445.026994	37.074100
1750.048867	230885.580452	37.079117
1751.359487	231345.015850	37.084135
1753.541204	231811.212683	37.089152
1754.932140	232268.655653	37.094170
1756.943402	232737.678407	37.099188
1758.835123	233201.210780	37.104205
1760.265685	233675.720552	37.109223
1762.313078	234135.088309	37.114240
1763.623255	234608.300264	37.119258
1765.125724	235081.886962	37.124276
1767.138885	235557.140208	37.129293
1768.620383	236048.514164	37.134311
1770.710973	236522.715039	37.139328
1772.272884	237016.008165	37.144346
1773.797498	237491.476599	37.149364
1775.673294	237984.819914	37.154381
1777.721668	238472.114508	37.159399
1779.961667	238958.666121	37.164416
1782.149340	239436.540135	37.169434
1784.283525	239908.378513	37.174452
1786.792171	240367.401756	37.179469
1788.614642	240834.570392	37.184487
1790.867412	241281.598318	37.189504
1792.654146	241718.850551	37.194522
1794.293343	242153.410652	37.199540
1796.131069	242576.455496	37.204557
1797.705625	243014.939970	37.209575
1799.886385	243430.535203	37.214592
1801.518199	243861.390312	37.219610
1802.801028	244295.150810	37.224628
1805.201387	244726.688491	37.229645
1806.518550	245150.638760	37.234663
1807.968950	245587.877826	37.239680
1809.702128	246036.830560	37.244698
1810.712188	246494.976350	37.249716
1812.747574	246943.446581	37.254733
1814.527845	247405.780133	37.259751
1816.153666	247865.041431	37.264768
1817.850834	248335.519104	37.269786
1818.852688	248815.083435	37.274804
1820.725627	249286.954502	37.279821
1822.421372	249790.127448	37.284839
1824.084087	250282.560972	37.289856
1825.551436	250783.741561	37.294874
1827.422789	251289.171935	37.299892
1828.902885	251788.623632	37.304909
1830.500217	252320.800232	37.309927
1832.426189	252845.350779	37.314944
1834.452668	253374.279144	37.319962
1835.501102	253896.643197	37.324980
1837.377699	254428.264955	37.329997
1839.074065	254971.857206	37.335015
1841.318361	255507.912718	37.340032
1843.523976	256048.750735	37.345050
1845.401001	256591.524845	37.350068
1847.015106	257131.956037	37.355085
1849.037115	257694.646843	37.360103
1851.156916	258233.213210	37.365120
1852.875643	258779.951694	37.370138
1854.881675	259332.407406	37.375156
1857.085435	259869.358567	37.380173
1859.177033	260407.141594	37.385191
1861.464777	260945.881532	37.390208
1863.681589	261479.857514	37.395226
1865.227120	262014.252825	37.400244
1867.121824	262554.938815	37.405261
1868.597679	263103.189941	37.410279
1870.294903	263653.282559	37.415296
1872.344454	264190.689091	37.420314
1873.843038	264746.123861	37.425332
1876.191899	265296.535214	37.430349
1877.915928	265850.278983	37.435367
1879.784822	266393.582093	37.440384
1881.900991	266939.992166	37.445402
1883.643890	267508.565815	37.450420
1885.647045	268047.169588	37.455437
1886.806336	268608.449153	37.460455
1888.542373	269172.169424	37.465472
1890.642070	269736.232967	37.470490
1892.283514	270284.090790	37.475508
1893.750615	270821.003519	37.480525
1895.518976	271381.462684	37.485543
1897.234390	271931.438552	37.490560
1898.898068	272485.816764	37.495578
1900.053401	273063.473110	37.500596
1902.362616	273627.696152	37.505613
1904.407634	274206.493156	37.510631
1906.609658	274786.404971	37.515648
1908.171822	275361.115697	37.520666
1909.660382	275947.090618	37.525684
1911.323711	276530.366822	37.530701
1913.065540	277125.008007	37.535719
1915.502536	277720.138170	37.540736
1917.688367	278311.931038	37.545754
1919.801397	278916.536952	37.550772
1922.565291	279491.512907	37.555789
1924.771022	280076.438272	37.560807
1926.751678	280661.298572	37.565824
1929.490447	281239.956284	37.570842
1931.221694	281813.653255	37.575860
1933.688609	282381.634125	37.580877
1935.828065	282954.495179	37.585895
1937.562790	283517.796379	37.590912
1939.505462	284093.811173	37.595930
1942.000864	284663.226609	37.600948
1943.940489	285228.111960	37.605965
1946.016811	285782.582867	37.610983
1947.571278	286340.823911	37.616000
1949.905179	286896.414750	37.621018
1951.940080	287466.253198	37.626036
1954.369452	288018.597225	37.631053
1956.805989	288567.584881	37.636071
1958.670045	289111.486511	37.641088
1960.786239	289659.559045	37.646106
1962.101530	290225.495138	37.651124
1964.429471	290765.424017	37.656141
1966.191351	291335.520271	37.661159
1968.024299	291891.022382	37.666176
1970.241415	292445.338567	37.671194
1971.692331	293012.406466	37.676212
1972.834473	293573.276166	37.681229
1974.381470	294153.351518	37.686247
1976.191333	294740.287279	37.691264
1978.129589	295333.064947	37.696282
1979.903913	295941.588956	37.701300
1982.006221	296525.518578	37.706317
1985.032260	297100.270557	37.711335
1987.402594	297673.658327	37.716352
1989.955111	298233.677772	37.721370
1992.099745	298812.405699	37.726388
1994.505861	299376.227888	37.731405
1995.847885	299935.834989	37.736423
1997.713472	300503.146193	37.741440
2000.165958	301073.350430	37.746458
2002.007884	301628.976125	37.751476
2003.662400	302162.382892	37.756493
2005.426867	302703.158111	37.761511
2006.513324	303257.429933	37.766528
2008.608526	303813.532049	37.771546
2010.716042	304382.885281	37.776564
2012.356557	304943.172044	37.781581
2014.170077	305515.412334	37.786599
2015.836510	306098.035283	37.791616
2017.567999	306676.249588	37.796634
2019.595871	307271.957247	37.801652
2021.681853	307866.355425	37.806669
2023.820656	308454.442212	37.811687
2025.884193	309040.328150	37.816704
2028.762815	309628.051069	37.821722
2031.078791	310219.268568	37.826740
2033.174861	310807.624165	37.831757
2035.371073	311397.151563	37.836775
2037.438324	311980.424114	37.841792
2039.507979	312562.041069	37.846810
2041.934463	313135.720449	37.851828
2044.326130	313698.482195	37.856845
2047.062489	314262.907291	37.861863
2049.093047	314848.575327	37.866880
2051.254630	315415.247879	37.871898
2053.215463	316001.426027	37.876916
2055.073348	316569.080580	37.881933
2057.065797	317145.619939	37.886951
2059.112523	317725.623749	37.891968
2060.986243	318306.134554	37.896986
2062.555852	318895.858499	37.902004
2064.317216	319494.608928	37.907021
2066.213043	320097.875789	37.912039
2067.816751	320709.159564	37.917056
2070.052449	321317.282579	37.922074
2071.436791	321932.426014	37.927092
2073.721668	322564.979103	37.932109
2076.129149	323192.223760	37.937127
2077.904211	323816.853508	37.942144
2079.583405	324444.235242	37.947162
2081.185493	325091.401411	37.952180
2083.050123	325743.847233	37.957197
2084.929437	326403.696673	37.962215
2086.574352	327070.865066	37.967232
2088.108249	327746.574979	37.972250
2090.020479	328424.141680	37.977268
2091.918308	329117.747307	37.982285
2094.100285	329814.519907	37.987303
2095.545591	330517.324784	37.992320
2097.986263	331210.583104	37.997338
2100.320472	331928.804925	38.002356
2102.625529	332626.206284	38.007373
2105.146705	333328.435551	38.012391
2107.387266	334026.591230	38.017408
2109.884422	334710.326285	38.022426
2112.097193	335380.799831	38.027444
2115.237618	336033.489832	38.032461
2118.074410	336671.348836	38.037479
2120.490841	337303.712860	38.042496
2123.238279	337920.452784	38.047514
2125.832572	338543.379242	38.052532
2128.171654	339156.544071	38.057549
2131.114701	339750.003300	38.062567
2133.332488	340347.843455	38.067584
2135.678649	340942.862403	38.072602
2137.122861	341531.530766	38.077620
2139.506224	342132.112469	38.082637
2141.452462	342736.466868	38.087655
2143.582224	343335.046329	38.092672
2145.655534	343928.729576	38.097690
2147.513438	344533.685116	38.102708
2149.723685	345137.202067	38.107725
2151.780901	345736.473685	38.112743
2153.916369	346354.656240	38.117760
2155.904978	346959.557494	38.122778
2158.152511	347568.136873	38.127796
2160.362886	348188.717765	38.132813
2162.356485	348811.940893	38.137831
2163.669566	349444.026489	38.142848
2165.885670	350078.892224	38.147866
2167.568611	350712.215842	38.152884
2169.626457	351365.182762	38.157901
2172.073755	352006.705204	38.162919
2174.104722	352673.790665	38.167936
2176.094849	353323.313698	38.172954
2178.572919	353989.946730	38.177972
2180.325927	354651.897557	38.182989
2182.092772	355321.092160	38.188007
2184.199859	356002.117483	38.193024
2186.366399	356674.063488	38.198042
2189.113173	357351.734703	38.203060
2191.471122	358038.011176	38.208077
2193.737308	358707.952797	38.213095
2195.507246	359402.856415	38.218112
2197.921833	360083.963226	38.223130
2199.428477	360781.678331	38.228148
2201.524887	361479.787548	38.233165
2203.688781	362186.777078	38.238183
2205.569456	362885.912596	38.243200
2207.771853	363600.733699	38.248218
2209.884938	364311.675482	38.253236
2211.860559	365037.441580	38.258253
2214.157967	365758.902494	38.263271
2216.393432	366498.978507	38.268288
2218.745859	367227.072739	38.273306
2220.777441	367966.393280	38.278324
2222.887980	368701.272018	38.283341
2225.300896	369436.515390	38.288359
2227.330514	370183.019848	38.293376
2229.858352	370907.180559	38.298394
2231.962453	371618.515040	38.303412
2233.894602	372332.933397	38.308429
2236.226653	373041.359748	38.313447
2238.393841	373767.882049	38.318464
2240.407638	374471.946377	38.323482
2243.163015	375184.720063	38.328500
2245.423444	375905.703823	38.333517
2248.130901	376630.982949	38.338535
2249.989025	377347.465786	38.343552
2252.454838	378070.042077	38.348570
2255.135538	378783.919370	38.353588
2257.271295	379496.175667	38.358605
2259.984100	380208.039087	38.363623
2262.171992	380936.990209	38.368640
2264.751753	381655.716256	38.373658
2266.511798	382363.233300	38.378676
2268.585198	383088.124543	38.383693
2270.771339	383813.791482	38.388711
2273.019740	384555.175144	38.393728
2275.488792	385274.295650	38.398746
2278.663355	386000.022614	38.403764
2280.576826	386731.652315	38.408781
2282.926550	387451.149061	38.413799
2285.375753	388198.673975	38.418816
2287.480787	388920.155729	38.423834
2289.659090	389650.074339	38.428852
2292.139776	390396.906734	38.433869
2294.748142	391131.000122	38.438887
2296.900259	391872.909677	38.443904
2299.064039	392601.416386	38.448922
2301.195457	393346.283836	38.453940
2303.402971	394109.088861	38.458957
2305.881920	394862.830760	38.463975
2307.711869	395620.364398	38.468992
2309.683573	396379.628167	38.474010
2312.411838	397141.758469	38.479028
2314.292459	397918.584773	38.484045
2316.490747	398680.156856	38.489063
2318.690098	399459.294315	38.494080
2320.920098	400240.178946	38.499098
2323.301710	401019.723857	38.504116
2325.286061	401830.201727	38.509133
2327.880277	402605.840259	38.514151
2330.343588	403401.317840	38.519168
2333.003858	404196.130844	38.524186
2335.324654	404977.728846	38.529204
2337.667968	405764.975525	38.534221
2340.208683	406546.845712	38.539239
2343.169135	407333.941431	38.544256
2345.277528	408112.369665	38.549274
2347.991598	408904.071927	38.554292
2349.988315	409698.507673	38.559309
2352.621013	410476.372008	38.564327
2354.800837	411269.336175	38.569344
2356.771204	412040.327422	38.574362
2359.396601	412811.791806	38.579380
2361.273181	413578.473265	38.584397
2363.766531	414329.223237	38.589415
2365.552661	415111.323395	38.594432
2367.593663	415881.554974	38.599450
2370.294179	416643.268441	38.604468
2372.359369	417433.859656	38.609485
2374.683094	418210.302885	38.614503
2377.143411	418992.522643	38.619520
2379.209285	419787.597473	38.624538
2381.557166	420581.282063	38.629556
2383.517422	421398.705829	38.634573
2385.969573	422200.523810	38.639591
2388.081320	423021.310924	38.644608
2390.016959	423847.011859	38.649626
2392.324066	424685.430763	38.654644
2394.844188	425521.505829	38.659661
2397.095894	426354.509408	38.664679
2399.786839	427195.508929	38.669696
2402.368001	428045.508460	38.674714
2404.472153	428895.407116	38.679732
2406.745479	429764.329869	38.684749
2409.069416	430625.214083	38.689767
2411.446046	431508.632267	38.694784
2413.868561	432372.370635	38.699802
2416.352230	433240.317633	38.704820
2418.627496	434115.707145	38.709837
2421.771266	434989.902474	38.714855
2423.905380	435869.651624	38.719872
2426.032185	436759.235658	38.724890
2428.513027	437646.092665	38.729908
2430.954385	438546.633990	38.734925
2433.389269	439430.138941	38.739943
2436.080679	440336.434364	38.744960
2438.613654	441238.975630	38.749978
2441.083485	442136.077187	38.754996
2443.521867	443047.008927	38.760013
2446.385293	443932.029943	38.765031
2449.620455	444823.780272	38.770048
2452.240545	445713.929480	38.775066
2455.240872	446594.366151	38.780084
2457.952650	447483.616598	38.785101
2460.446833	448345.352768	38.790119
2462.924355	449222.836139	38.795136
2465.144399	450095.421250	38.800154
2467.564570	450962.625763	38.805172
2470.395005	451854.300600	38.810189
2473.063939	452721.035168	38.815207
2475.135943	453598.251681	38.820224
2477.559310	454473.550405	38.825242
2480.035058	455357.145160	38.830260
2482.165018	456241.620126	38.835277
2484.458872	457131.033500	38.840295
2486.727877	458014.850965	38.845312
2488.912284	458899.250587	38.850330
2491.460464	459768.333538	38.855348
2493.558352	460630.328327	38.860365
2495.990017	461501.377190	38.865383
2498.491450	462379.047285	38.870400
2500.522408	463258.274765	38.875418
2503.853390	464124.605975	38.880436
2506.627986	464997.765514	38.885453
2508.947677	465858.279513	38.890471
2511.805238	466725.788138	38.895488
2514.110748	467605.984212	38.900506
2516.991326	468472.045604	38.905524
2519.939973	469342.956861	38.910541
2522.326054	470205.133429	38.915559
2525.048309	471076.407810	38.920576
2527.629866	471948.070027	38.925594
2530.697220	472822.336483	38.930612
2533.071690	473692.992956	38.935629
2535.761547	474562.089934	38.940647
2538.675867	475427.218615	38.945664
2540.910777	476290.655098	38.950682
2544.137322	477154.437033	38.955700
2546.801753	478020.041744	38.960717
2549.451178	478876.821132	38.965735
2552.167258	479727.943584	38.970752
2554.349990	480589.165333	38.975770
2557.352571	481447.428734	38.980788
2559.652180	482320.110001	38.985805
2561.982163	483188.704511	38.990823
2564.624374	484046.652096	38.995840
2567.055154	484930.794126	39.000858
2569.430287	485809.247722	39.005876
2571.500303	486697.098152	39.010893
2574.211980	487584.793892	39.015911
2576.883895	488480.072372	39.020928
2579.050980	489385.938891	39.025946
2581.018053	490279.226136	39.030964
2583.393404	491202.221085	39.035981
2585.494318	492134.346628	39.040999
2587.628995	493065.204574	39.046016
2589.452408	494028.507307	39.051034
2591.791062	494983.494019	39.056052
2594.094017	495958.713342	39.061069
2596.456206	496936.287370	39.066087
2598.534795	497931.810530	39.071104
2600.920568	498941.798919	39.076122
2603.208156	499945.437983	39.081140
2605.639959	500972.997983	39.086157
2607.902309	502005.111950	39.091175
2610.595054	503041.020677	39.096192
2612.970584	504097.087514	39.101210
2615.989705	505136.235907	39.106228
2618.578015	506183.558783	39.111245
2622.095653	507231.915055	39.116263
2625.056756	508274.702186	39.121280
2627.718487	509291.915506	39.126298
2630.907980	510307.562180	39.131316
2633.561075	511302.973902	39.136333
2636.176359	512293.087774	39.141351
2638.708470	513299.380635	39.146368
2641.061172	514303.018994	39.151386
2643.808234	515291.962939	39.156404
2646.416841	516290.894171	39.161421
2649.172286	517297.998369	39.166439
2651.923621	518299.243759	39.171456
2654.347757	519317.305050	39.176474
2657.014192	520326.542634	39.181492
2659.169304	521355.494765	39.186509
2661.434041	522387.783069	39.191527
2664.270333	523419.046878	39.196544
2666.499162	524465.451164	39.201562
2669.151199	525520.773783	39.206580
2671.982946	526579.163038	39.211597
2674.723230	527626.818696	39.216615
2677.484672	528686.680380	39.221632
2680.124258	529759.272983	39.226650
2683.100903	530823.272912	39.231668
2686.068946	531898.622311	39.236685
2688.165722	532963.975158	39.241703
2691.395628	534047.173176	39.246720
2693.566775	535134.798365	39.251738
2696.564149	536213.998176	39.256756
2699.227381	537306.607481	39.261773
2701.660228	538404.505199	39.266791
2704.394817	539497.185442	39.271808
2707.249399	540602.587756	39.276826
2710.093576	541704.685889	39.281844
2712.657324	542821.280324	39.286861
2715.232096	543930.189683	39.291879
2718.419449	545035.687564	39.296896
2721.063587	546151.447547	39.301914
2724.089240	547256.694716	39.306932
2727.175611	548368.177083	39.311949
2729.689456	549489.117702	39.316967
2732.680734	550600.132908	39.321984
2735.594566	551717.956221	39.327002
2738.453643	552826.398744	39.332020
2741.294931	553940.934199	39.337037
2743.298363	555064.565025	39.342055
2745.992323	556181.853437	39.347072
2749.030412	557311.247960	39.352090
2751.758668	558431.355610	39.357108
2754.740745	559558.407566	39.362125
2757.646808	560676.435291	39.367143
2760.493506	561802.614368	39.372160
2763.138401	562924.612698	39.377178
2766.161154	564059.505464	39.382196
2768.718512	565195.533058	39.387213
2770.827433	566332.641699	39.392231
2773.812889	567461.116234	39.397248
2776.816588	568600.732268	39.402266
2779.468348	569703.766183	39.407284
2782.143184	570797.114319	39.412301
2784.957538	571890.595029	39.417319
2788.311967	572978.318624	39.422336
2791.227716	574062.209584	39.427354
2794.292578	575150.897925	39.432372
2797.589945	576225.153928	39.437389
2799.878427	577309.271040	39.442407
2802.667546	578393.307982	39.447424
2805.146799	579483.371152	39.452442
2807.484950	580587.704369	39.457460
2810.430304	581697.951879	39.462477
2812.509437	582812.909342	39.467495
2815.638455	583932.448305	39.472512
2818.247527	585061.597671	39.477530
2820.840807	586193.952386	39.482548
2823.236585	587337.260843	39.487565
2825.533851	588492.705389	39.492583
2828.654829	589651.254819	39.497600
2830.821392	590831.600603	39.502618
2833.863541	592008.021800	39.507636
2836.694888	593200.592955	39.512653
2838.754966	594389.367963	39.517671
2841.639031	595594.259738	39.522688
2843.997848	596823.155645	39.527706
2846.713641	598044.850077	39.532724
2849.518297	599286.779008	39.537741
2851.753252	600532.876982	39.542759
2854.831659	601786.204632	39.547776
2857.791847	603037.963654	39.552794
2860.384359	604316.523948	39.557812
2863.167820	605600.812693	39.562829
2866.219637	606889.012792	39.567847
2868.975803	608166.409443	39.572864
2871.803319	609458.405996	39.577882
2874.604385	610764.563325	39.582900
2877.781812	612060.300354	39.587917
2880.916291	613371.795795	39.592935
2883.995527	614672.794584	39.597952
2887.048489	615979.243572	39.602970
2890.136950	617277.232435	39.607988
2893.370467	618580.640406	39.613005
2896.251494	619879.604283	39.618023
2899.340238	621184.023767	39.623040
2902.625150	622494.497807	39.628058
2905.486551	623799.788528	39.633076
2908.394687	625105.611521	39.638093
2911.036914	626414.966271	39.643111
2913.608623	627729.765193	39.648128
2916.503925	629040.700290	39.653146
2919.275438	630361.679086	39.658164
2922.487226	631673.480425	39.663181
2925.465917	632987.553139	39.668199
2928.817325	634291.713999	39.673216
2932.361544	635594.729989	39.678234
2935.331844	636874.377722	39.683252
2938.338142	638141.237927	39.688269
2941.317416	639404.255001	39.693287
2944.109920	640653.630851	39.698304
2947.335335	641908.016412	39.703322
2949.905389	643162.758035	39.708340
2952.799247	644412.452414	39.713357
2955.501191	645685.556213	39.718375
2958.476788	646950.227150	39.723392
2961.378707	648225.766140	39.728410
2963.795087	649501.972666	39.733428
2966.993278	650782.117462	39.738445
2969.244938	652087.767823	39.743463
2972.245647	653379.667395	39.748480
2975.554998	654682.103543	39.753498
2978.160924	655987.574661	39.758516
2981.025747	657305.724391	39.763533
2983.984358	658633.537970	39.768551
2987.252531	659957.184162	39.773568
2989.993998	661286.164637	39.778586
2992.882622	662624.989930	39.783604
2996.160440	663953.261331	39.788621
2999.068977	665299.571834	39.793639
3001.748233	666644.786099	39.798656
3004.984320	668014.187074	39.803674
3007.950737	669366.874667	39.808692
3011.487513	670726.232411	39.813709
3014.509106	672089.309751	39.818727
3017.906782	673449.091901	39.823744
3021.158877	674804.972768	39.828762
3024.137583	676173.822527	39.833780
3027.671799	677531.890448	39.838797
3030.318526	678901.982852	39.843815
3033.819320	680269.936876	39.848832
3036.979031	681630.344331	39.853850
3040.002810	682996.283142	39.858868
3043.302237	684346.775935	39.863885
3045.967799	685718.821118	39.868903
3049.441191	687074.586123	39.873920
3052.541223	688444.305626	39.878938
3055.292758	689809.161252	39.883956
3058.599811	691170.538160	39.888973
3061.809542	692551.864188	39.893991
3064.492396	693920.169203	39.899008
3067.980952	695297.051455	39.904026
3070.602788	696662.610894	39.909044
3073.573924	698050.653977	39.914061
3076.328311	699440.595763	39.919079
3079.692944	700822.083794	39.924096
3082.697661	702206.485895	39.929114
3085.290676	703618.828892	39.934132
3088.443279	705006.374001	39.939149
3091.316489	706413.851559	39.944167
3094.446548	707822.440617	39.949184
3098.110446	709208.524542	39.954202
3100.762193	710579.308116	39.959220
3104.000300	711932.693662	39.964237
3106.967216	713296.152909	39.969255
3110.311835	714651.261598	39.974272
3113.724869	716001.538875	39.979290
3116.439343	717369.673154	39.984308
3119.462472	718732.139513	39.989325
3122.376548	720096.428516	39.994343
3125.116935	721483.264919	39.999360
3128.357259	722870.425595	40.004378
3130.758835	724265.897590	40.009396
3133.519517	725663.986285	40.014413
3136.623136	727091.174001	40.019431
3139.441048	728514.504984	40.024448
3142.966300	729937.070468	40.029466
3145.907196	731374.003292	40.034484
3149.239689	732814.908401	40.039501
3152.051442	734261.715540	40.044519
3155.017140	735709.962296	40.049536
3158.079410	737184.032836	40.054554
3160.740534	738657.059869	40.059572
3164.148065	740139.994697	40.064589
3167.109293	741645.659356	40.069607
3169.680433	743144.889775	40.074624
3172.891960	744656.689398	40.079642
3175.491174	746195.705051	40.084660
3178.522901	747722.417264	40.089677
3181.850535	749261.686720	40.094695
3185.377653	750812.339004	40.099712
3188.582315	752355.396016	40.104730
3192.053103	753898.491145	40.109748
3195.565212	755451.802654	40.114765
3199.069601	757011.098685	40.119783
3202.504843	758558.965061	40.124800
3206.101353	760116.523553	40.129818
3208.843025	761680.743219	40.134836
3212.059659	763245.736237	40.139853
3215.109054	764819.477295	40.144871
3218.260487	766394.540087	40.149888
3221.252231	767981.238822	40.154906
3224.359790	769556.866024	40.159924
3227.941182	771135.072388	40.164941
3231.141557	772730.391558	40.169959
3234.358881	774321.677487	40.174976
3237.736275	775910.821693	40.179994
3240.629073	777514.229767	40.185012
3243.633114	779119.374088	40.190029
3246.881363	780725.297271	40.195047
3249.752149	782352.312043	40.200064
3252.755112	783969.568555	40.205082
3255.844552	785606.545289	40.210100
3259.134594	787244.875753	40.215117
3262.364942	788877.937339	40.220135
3265.083179	790532.265882	40.225152
3269.257001	792142.020391	40.230170
3272.358477	793753.939042	40.235188
3275.992471	795343.656984	40.240205
3279.239800	796935.721243	40.245223
3282.475751	798528.205210	40.250240
3285.985169	800099.090887	40.255258
3288.882655	801685.864848	40.260276
3292.655671	803275.056966	40.265293
3295.484540	804890.394004	40.270311
3298.246101	806504.773466	40.275328
3301.586124	808106.697966	40.280346
3304.235205	809740.411765	40.285364
3307.644895	811375.651831	40.290381
3310.951734	813013.588390	40.295399
3313.839245	814662.766884	40.300416
3317.190187	816314.387620	40.305434
3320.242281	817982.874780	40.310452
3323.529875	819664.220127	40.315469
3326.873379	821338.300082	40.320487
3330.107609	823031.964463	40.325504
3334.053056	824717.416990	40.330522
3336.887100	826421.436105	40.335540
3339.922054	828110.504979	40.340557
3343.635099	829826.928654	40.345575
3346.561548	831540.401535	40.350592
3350.427719	833255.449161	40.355610
3353.944540	834963.673940	40.360628
3357.392503	836697.437017	40.365645
3360.983754	838420.440414	40.370663
3363.772785	840161.738716	40.375680
3367.322461	841892.899323	40.380698
3370.623197	843648.706459	40.385716
3373.824057	845394.808062	40.390733
3376.618932	847146.029712	40.395751
3379.981213	848919.292946	40.400768
3383.334273	850687.099967	40.405786
3386.669077	852474.886987	40.410804
3389.971712	854254.786476	40.415821
3393.528892	856045.962720	40.420839
3397.209235	857839.309714	40.425856
3400.776427	859627.398249	40.430874
3404.561615	861414.632991	40.435892
3407.928826	863200.927369	40.440909
3411.671856	864987.113378	40.445927
3414.977172	866783.302426	40.450944
3418.803001	868569.376789	40.455962
3422.334545	870365.806755	40.460980
3425.830173	872148.929048	40.465997
3429.703352	873928.742295	40.471015
3432.827294	875711.338088	40.476032
3436.874516	877485.986525	40.481050
3440.485832	879262.588260	40.486068
3443.995075	881033.740383	40.491085
3447.799154	882809.132378	40.496103
3450.781023	884576.301143	40.501120
3454.494157	886316.985948	40.506125
3457.809915	888013.538028	40.511130
3461.335234	889648.336276	40.516135
3465.036321	891204.518021	40.521140
3467.931053	892705.124962	40.526144
3471.367559	894123.395458	40.531149
3473.969488	895474.116570	40.536154
3476.645667	896743.851336	40.541159
3479.693323	897940.521415	40.546164
3482.522917	899073.252331	40.551168
3485.446326	900107.470839	40.556173
3487.753456	901073.850866	40.561178
3490.531023	901956.029837	40.566183
3492.777657	902776.216907	40.571188
3494.607850	903537.024422	40.576192
3497.255479	904221.481883	40.581197
3499.344305	904845.862824	40.586202
3501.570777	905401.196096	40.591207
3503.851369	905889.638091	40.596212
3505.311114	906316.562681	40.601216
3506.963930	906690.295735	40.606221
3508.279310	907014.505786	40.611226
3509.950128	907287.347942	40.616231
3511.766953	907513.492883	40.621236
3512.832344	907698.594315	40.626240
3514.083914	907831.121450	40.631245
3515.279495	907931.940897	40.636250
3516.333161	907980.633416	40.641255
3517.254987	908001.875685	40.646260
3518.399812	907994.643506	40.651264
3519.260042	907942.250643	40.656269
3520.102043	907874.918951	40.661274
3521.076831	907752.423993	40.666279
3521.675565	907621.507239	40.671284
3522.354242	907469.654195	40.676288
3523.169930	907282.103163	40.681293
3523.843639	907089.653095	40.686298
3523.981984	906863.639278	40.691303
3524.710578	906618.810333	40.696308
3525.204127	906366.682567	40.701312
3525.440392	906082.669751	40.706317
3526.052000	905798.674751	40.711322
3526.510453	905489.713959	40.716327
3527.068328	905159.115631	40.721332
3526.945634	904828.324456	40.726336
3527.757924	904481.245931	40.731341
3528.076656	904130.564467	40.736346
3528.435656	903753.904156	40.741351
3528.776469	903376.642633	40.746356
3529.095853	902978.808693	40.751360
3529.308544	902570.736808	40.756365
3529.502354	902159.839941	40.761370
3529.926974	901748.583948	40.766375
3530.024050	901313.998168	40.771380
3530.124474	900882.852708	40.776384
3530.237346	900431.208550	40.781389
3530.411885	899989.267337	40.786394
3530.611114	899536.764146	40.791399
3530.443238	899081.583793	40.796404
3530.488851	898624.785222	40.801408
3530.717941	898157.489267	40.806413
3530.936348	897698.847891	40.811418
3530.863061	897226.407978	40.816423
3531.383904	896742.043246	40.821428
3531.217525	896269.539125	40.826432
3531.093770	895773.706358	40.831437
3531.307137	895283.086342	40.836442
3531.417030	894790.122553	40.841447
3531.501727	894292.771813	40.846452
3531.369763	893796.284212	40.851456
3531.728165	893301.022564	40.856461
3531.657190	892794.965592	40.861466
3531.780189	892293.277078	40.866471
3532.171549	891779.511084	40.871476
3531.662738	891259.761490	40.876480
3532.394042	890745.941086	40.881485
3531.981584	890224.920561	40.886490
3531.980072	889701.364697	40.891495
3532.091753	889180.159569	40.896500
3531.802307	888660.039504	40.901504
3531.944788	888130.802195	40.906509
3532.063975	887617.869801	40.911514
3532.126337	887090.194978	40.916519
3532.424500	886557.206405	40.921524
3532.063386	886026.506790	40.926528
3532.215852	885493.928634	40.931533
3532.121332	884962.988913	40.936538
3532.479067	884415.370882	40.941543
3532.399429	883878.908434	40.946548
3532.159784	883347.845264	40.951552
3532.316828	882804.078583	40.956557
3532.484963	882264.132407	40.961562
3532.517209	881732.003481	40.966567
3532.306229	881168.971832	40.971572
3532.175742	880629.021711	40.976576
3532.373040	880077.631880	40.981581
3532.644209	879544.293665	40.986586
3532.461702	878985.599667	40.991591
3532.594812	878429.317743	40.996596
3532.475325	877877.289963	41.001600
3532.677339	877321.375619	41.006605
3532.449604	876766.063523	41.011610
3532.493110	876214.917710	41.016615
3532.573160	875654.892225	41.021620
3532.240955	875101.379630	41.026624
3532.444400	874542.972524	41.031629
3532.186430	873991.573201	41.036634
3532.320794	873440.928248	41.041639
3532.809645	872875.041345	41.046644
3533.011221	872321.759101	41.051648
3532.668215	871750.571943	41.056653
3532.862178	871185.253138	41.061658
3532.717236	870613.534727	41.066663
3532.838100	870050.934277	41.071668
3532.758715	869487.926687	41.076672
3532.898511	868913.667417	41.081677
3532.856962	868346.372346	41.086682
3532.822316	867778.439809	41.091687
3532.976095	867198.383168	41.096692
3532.600760	866630.691133	41.101696
3532.698375	866046.357702	41.106701
3532.672892	865484.517662	41.111706
3532.520614	864910.507016	41.116711
3532.657481	864341.345735	41.121716
3532.570283	863764.980843	41.126720
3532.839535	863189.374334	41.131725
3532.633234	862609.810788	41.136730
3532.713917	862026.256113	41.141735
3532.858315	861441.759738	41.146740
3532.400146	860868.971808	41.151744
3532.449436	860288.462176	41.156749
3532.142666	859714.470340	41.161754
3532.167597	859144.353326	41.166759
3532.357959	858570.752000	41.171764
3532.008498	857991.063434	41.176768
3532.280752	857421.715372	41.181773
3531.874969	856845.525463	41.186778
3532.189710	856272.367728	41.191783
3532.309860	855700.064965	41.196788
3532.056273	855124.076157	41.201792
3531.813552	854544.723799	41.206797
3532.442006	853982.388904	41.211802
3532.109388	853408.295910	41.216807
3532.694923	852819.979927	41.221812
3532.584599	852248.562988	41.226816
3532.623464	851657.017921	41.231821
3532.537182	851071.764615	41.236826
3532.311504	850487.550589	41.241831
3532.000942	849903.295972	41.246836
3531.772786	849325.787873	41.251840
3531.839249	848747.104663	41.256845
3532.023746	848171.268980	41.261850
3531.830087	847591.256710	41.266855
3531.901673	847016.599703	41.271860
3531.726799	846436.282031	41.276864
3531.788542	845858.208152	41.281869
3531.902087	845287.086903	41.286874
3531.478420	844698.758789	41.291879
3531.717282	844120.104529	41.296884
3531.516014	843552.289686	41.301888
3531.689607	842974.320701	41.306893
3531.697488	842393.402726	41.311898
3531.778501	841820.509776	41.316903
3531.706950	841237.841701	41.321908
3531.553754	840663.323859	41.326912
3531.585988	840081.847760	41.331917
3531.823546	839500.917085	41.336922
3531.701162	838926.528953	41.341927
3531.742949	838328.944742	41.346932
3532.086604	837758.467953	41.351936
3532.087904	837167.560906	41.356941
3531.766789	836583.629852	41.361946
3531.749307	835996.959055	41.366951
3531.832534	835403.044963	41.371956
3531.696366	834825.654675	41.376960
3531.825236	834236.894403	41.381965
3531.524721	833652.204078	41.386970
3531.406741	833070.504240	41.391975
3531.714236	832475.597281	41.396980
3531.616929	831893.348102	41.401984
3531.633528	831305.461174	41.406989
3531.738337	830727.954387	41.411994
3531.590431	830138.573287	41.416999
3531.686478	829541.283208	41.422004
3531.603796	828953.248036	41.427008
3531.591208	828361.142344	41.432013
3531.949040	827780.642995	41.437018
3531.528565	827192.457078	41.442023
3531.679047	826597.475929	41.447028
3531.445977	826012.424815	41.452032
3531.777623	825408.753458	41.457037
3531.840746	824823.056496	41.462042
3531.988798	824227.175472	41.467047
3532.523288	823626.481825	41.472052
3531.846155	823027.504257	41.477056
3531.820801	822419.071954	41.482061
3532.016907	821825.017798	41.487066
3531.958982	821224.694531	41.492071
3531.992570	820618.286025	41.497076
3531.833767	820028.091471	41.502080
3531.821964	819419.428707	41.507085
3531.416085	818814.396915	41.512090
3531.914835	818221.042851	41.517095
3531.715202	817617.431977	41.522100
3531.557449	817027.948283	41.527104
3531.628898	816424.084843	41.532109
3531.515798	815823.574785	41.537114
3531.539374	815228.419790	41.542119
3531.174164	814623.978361	41.547124
3531.493914	814029.498029	41.552128
3531.054400	813429.954253	41.557133
3531.268949	812838.078592	41.562138
3531.119989	812249.689154	41.567143
3531.551129	811650.425226	41.572148
3531.214548	811055.646438	41.577152
3531.016204	810459.273234	41.582157
3531.148251	809865.729704	41.587162
3531.057325	809275.503023	41.592167
3531.180018	808671.912250	41.597172
3531.147668	808080.003581	41.602176
3531.088859	807476.141240	41.607181
3531.169773	806885.774917	41.612186
3531.057611	806285.833991	41.617191
3531.072144	805692.287947	41.622196
3530.438482	805094.977655	41.627200
3530.866839	804492.727876	41.632205
3531.088548	803905.069322	41.637210
3530.805119	803319.799833	41.642215
3530.884936	802717.355138	41.647220
3530.598237	802130.170378	41.652224
3530.841541	801534.998417	41.657229
3531.072306	800943.112107	41.662234
3531.037949	800338.222158	41.667239
3531.121603	799733.896656	41.672244
3530.681387	799139.075780	41.677248
3530.895130	798534.034359	41.682253
3531.013967	797934.010043	41.687258
3530.921178	797339.760186	41.692263
3530.832149	796741.778176	41.697268
3530.800636	796145.354457	41.702272
3530.659306	795540.210631	41.707277
3530.810497	794934.375227	41.712282
3530.426221	794347.773384	41.717287
3530.514125	793746.509326	41.722292
3530.446047	793155.089259	41.727296
3530.530670	792564.035088	41.732301
3530.942343	791968.406404	41.737306
3530.891338	791367.158244	41.742311
3531.095969	790764.145036	41.747316
3530.786881	790170.009588	41.752320
3530.985283	789567.926542	41.757325
3530.846188	788959.413818	41.762330
3530.691883	788358.565207	41.767335
3531.053453	787743.278468	41.772340
3530.989370	787145.161445	41.777344
3530.720323	786543.392177	41.782349
3530.761845	785931.246526	41.787354
3530.578832	785328.081762	41.792359
3530.813735	784717.174999	41.797364
3530.504787	784115.649661	41.802368
3530.441766	783516.588333	41.807373
3530.917739	782918.122365	41.812378
3530.484147	782322.171233	41.817383
3530.790225	781698.995742	41.822388
3530.764421	781101.152290	41.827392
3530.549825	780494.142479	41.832397
3530.710327	779893.855079	41.837402
3530.443704	779286.801599	41.842407
3530.688721	778678.576516	41.847412
3530.241107	778073.124717	41.852416
3530.318498	777470.140663	41.857421
3530.290281	776868.108715	41.862426
3530.228110	776263.522591	41.867431
3530.203702	775652.776391	41.872436
3529.843867	775058.674066	41.877440
3529.963348	774461.635447	41.882445
3529.908139	773856.651367	41.887450
3529.697398	773264.445249	41.892455
3529.782613	772675.144337	41.897460
3529.817710	772079.304309	41.902464
3529.595816	771480.110860	41.907469
3529.603680	770901.318326	41.912474
3529.452964	770309.158861	41.917479
3529.485078	769704.753266	41.922484
3529.455647	769118.979838	41.927488
3529.279925	768536.239547	41.932493
3529.801014	767945.992836	41.937498
3529.546004	767356.077958	41.942503
3529.667193	766761.370321	41.947508
3529.438486	766174.806626	41.952512
3529.765222	765575.977029	41.957517
3529.431291	764984.556530	41.962522
3529.318271	764387.333091	41.967527
3529.737644	763793.126159	41.972532
3529.238951	763198.042657	41.977536
3529.142602	762610.584414	41.982541
3528.983141	762019.589798	41.987546
3529.057405	761442.316978	41.992551
3528.888736	760845.313716	41.997556
3529.065114	760266.157702	42.002560
3529.282921	759670.376361	42.007565
3529.156343	759079.638494	42.012570
3529.046700	758495.314352	42.017575
3529.283927	757904.471903	42.022580
3528.695276	757328.230921	42.027584
3528.717672	756743.156995	42.032589
3528.780152	756153.639054	42.037594
3528.638591	755576.448605	42.042599
3528.812787	754991.115308	42.047604
3528.390760	754401.001510	42.052608
3528.229703	753825.212051	42.057613
3528.704077	753245.518767	42.062618
3528.595040	752678.619210	42.067623
3528.439423	752090.009736	42.072628
3528.220033	751508.032272	42.077632
3528.336650	750936.965864	42.082637
3528.374882	750360.635473	42.087642
3528.329288	749770.595099	42.092647
3528.057589	749191.958345	42.097652
3528.257633	748627.029199	42.102656
3528.372767	748049.377100	42.107661
3528.262647	747470.386467	42.112666
3528.077176	746899.863861	42.117671
3528.220078	746324.647939	42.122676
3528.038631	745736.250711	42.127680
3528.042735	745169.423366	42.132685
3527.936178	744599.114092	42.137690
3528.133662	744021.050068	42.142695
3528.198893	743440.148362	42.147700
3527.829546	742875.640611	42.152704
3527.555275	742296.343458	42.157709
3527.898207	741725.995500	42.162714
3527.618178	741165.898276	42.167719
3527.769616	740585.611352	42.172724
3527.793454	740023.254767	42.177728
3527.577206	739456.843747	42.182733
3527.635904	738879.958729	42.187738
3527.644199	738316.939429	42.192743
3527.835906	737743.708200	42.197748
3527.674903	737181.626597	42.202752
3527.774110	736607.834534	42.207757
3528.176477	736030.881784	42.212762
3527.690624	735464.578346	42.217767
3527.902995	734881.637252	42.222772
3527.694446	734303.575343	42.227776
3528.181676	733733.519017	42.232781
3527.895333	733162.069383	42.237786
3527.640208	732584.881407	42.242791
3527.905266	732008.503726	42.247796
3527.707324	731441.866932	42.252800
3527.585563	730865.176464	42.257805
3527.040722	730286.833593	42.262810
3527.292398	729731.387883	42.267815
3527.192176	729161.009246	42.272820
3527.280826	728588.824923	42.277824
3527.162529	728019.656718	42.282829
3527.195356	727456.465514	42.287834
3526.943198	726901.308397	42.292839
3527.151757	726334.294602	42.297844
3526.821598	725776.250621	42.302848
3526.905564	725213.787541	42.307853
3527.079269	724644.284360	42.312858
3526.854818	724090.021552	42.317863
3527.121678	723529.244997	42.322868
3527.002171	722968.793480	42.327872
3527.015427	722403.523313	42.332877
3526.850413	721849.198419	42.337882
3526.830027	721287.128673	42.342887
3526.945531	720722.370247	42.347892
3526.574794	720160.382851	42.352896
3526.606357	719603.048069	42.357901
3526.565012	719044.597518	42.362906
3526.368521	718488.565525	42.367911
3526.476247	717930.361761	42.372916
3526.331598	717377.916186	42.377920
3526.233556	716823.243933	42.382925
3526.611325	716279.960149	42.387930
3526.280989	715726.147494	42.392935
3526.346493	715164.839687	42.397940
3526.324103	714622.508783	42.402944
3526.228280	714067.752857	42.407949
3526.260419	713510.209746	42.412954
3526.341009	712965.968345	42.417959
3525.991641	712414.173375	42.422964
3526.212264	711867.505084	42.427968
3526.371691	711308.851946	42.432973
3526.535878	710753.784103	42.437978
3526.022299	710209.317799	42.442983
3526.191538	709650.851537	42.447988
3525.882312	709104.343713	42.452992
3525.729560	708557.327304	42.457997
3526.252676	708005.195840	42.463002
3525.955517	707467.566880	42.468007
3525.998968	706926.271011	42.473012
3525.519976	706376.539076	42.478016
3525.319788	705837.599442	42.483021
3525.490002	705292.057084	42.488026
3525.592289	704759.454140	42.493031
3525.773421	704212.748843	42.498036
3525.730884	703674.789107	42.503040
3525.474966	703134.894980	42.508045
3525.802081	702589.502468	42.513050
3525.849611	702059.375098	42.518055
3525.717003	701494.616883	42.523060
3525.416484	700955.886252	42.528064
3525.365813	700421.750362	42.533069
3525.888270	699888.278912	42.538074
3525.274188	699343.340085	42.543079
3525.676094	698794.565755	42.548084
3525.392283	698266.848154	42.553088
3525.234454	697722.972877	42.558093
3525.407769	697175.030668	42.563098
3525.257308	696646.496764	42.568103
3525.745509	696102.758713	42.573108
3525.285555	695572.323923	42.578112
3525.580274	695028.900593	42.583117
3525.571953	694482.959644	42.588122
3525.437800	693941.829864	42.593127
3525.416214	693401.592609	42.598132
3525.355666	692864.114052	42.603136
3525.272585	692331.331607	42.608141
3525.150845	691787.432186	42.613146
3525.147094	691251.587171	42.618151
3525.008233	690704.838997	42.623156
3525.157535	690184.125392	42.628160
3524.639761	689634.988488	42.633165
3525.061579	689102.175510	42.638170
3524.243998	688575.413646	42.643175
3524.615468	688033.490110	42.648180
3524.819074	687518.185213	42.653184
3524.588169	686990.832111	42.658189
3524.717943	686465.028878	42.663194
3524.505795	685938.705877	42.668199
3524.880936	685409.215736	42.673204
3524.398457	684882.528934	42.678208
3524.359016	684352.350844	42.683213
3524.740758	683822.020059	42.688218
3524.210120	683309.089512	42.693223
3524.516649	682788.021017	42.698228
3524.415413	682260.519502	42.703232
3524.381345	681730.386714	42.708237
3524.391995	681213.312005	42.713242
3524.055444	680690.639984	42.718247
3524.345729	680165.390781	42.723252
3524.288754	679649.683537	42.728256
3524.374827	679130.884609	42.733261
3524.565601	678603.620506	42.738266
3524.041297	678077.843054	42.743271
3524.084603	677563.645542	42.748276
3524.099865	677041.552735	42.753280
3524.021170	676526.371723	42.758285
3523.972867	676007.021381	42.763290
3523.758463	675502.469050	42.768295
3524.251994	674979.430895	42.773300
3524.496932	674464.329196	42.778304
3524.034749	673941.944001	42.783309
3524.174740	673417.034447	42.788314
3524.514895	672902.926612	42.793319
3524.209021	672382.221665	42.798324
3524.399211	671860.755029	42.803329
3523.959245	671336.126716	42.808333
3524.195941	670815.192173	42.813338
3524.248927	670299.096066	42.818343
3524.124434	669766.947666	42.823348
3524.135702	669254.191736	42.828353
3523.819290	668728.200184	42.833357
3524.166973	668216.427445	42.838362
3523.782986	667702.856915	42.843367
3523.772872	667185.204970	42.848372
3523.905151	666666.752347	42.853377
3523.821906	666152.597650	42.858381
3523.891559	665627.615017	42.863386
3523.508641	665115.051583	42.868391
3523.367423	664602.369448	42.873396
3522.876685	664100.395459	42.878401
3523.188106	663605.941291	42.883405
3523.286366	663079.167292	42.888410
3523.042458	662587.948573	42.893415
3522.770355	662080.891779	42.898420
3522.939855	661580.968488	42.903425
3522.430564	661088.470941	42.908429
3522.929180	660585.196075	42.913434
3522.901592	660091.417554	42.918439
3522.850355	659598.466340	42.923444
3522.615056	659109.264975	42.928449
3522.683114	658608.955642	42.933453
3522.618918	658112.087501	42.938458
3522.280974	657624.326380	42.943463
3522.581976	657137.480126	42.948468
3522.564496	656647.368795	42.953473
3522.399977	656151.366349	42.958477
3522.489775	655646.257724	42.963482
3522.302998	655178.420946	42.968487
3522.559770	654689.562813	42.973492
3522.692077	654203.797782	42.978497
3522.398911	653714.285838	42.983501
3522.536216	653215.386501	42.988506
3522.242823	652729.821144	42.993511
3522.330770	652242.568419	42.998516
3522.361337	651757.199602	43.003521
3522.470934	651267.897094	43.008525
3522.528161	650779.428610	43.013530
3522.064399	650294.871824	43.018535
3522.081027	649805.762847	43.023540
3522.098204	649323.674567	43.028545
3521.995972	648842.582652	43.033549
3522.198016	648362.714752	43.038554
3521.935439	647884.452205	43.043559
3521.821086	647390.649823	43.048564
3521.887267	646913.484086	43.053569
3521.750341	646437.529783	43.058573
3521.385540	645969.238786	43.063578
3521.402387	645496.162455	43.068583
3521.884519	645019.485511	43.073588
3521.774652	644551.934788	43.078593
3521.436630	644066.954995	43.083597
3521.872204	643595.067724	43.088602
3521.274352	643125.934588	43.093607
3521.559583	642661.678610	43.098612
3521.547545	642191.152289	43.103617
3521.209642	641718.759764	43.108621
3521.527419	641253.933894	43.113626
3521.193022	640790.298287	43.118631
3521.646878	640317.205529	43.123636
3521.165181	639841.550026	43.128641
3521.301973	639374.519023	43.133645
3521.288770	638906.091911	43.138650
3520.998318	638442.942544	43.143655
3521.066968	637983.312375	43.148660
3520.975938	637522.238291	43.153665
3521.403659	637059.954464	43.158669
3521.415153	636589.766807	43.163674
3520.975968	636130.841053	43.168679
3521.004131	635663.860248	43.173684
3520.687094	635205.673072	43.178689
3520.509641	634746.991485	43.183693
3520.802267	634296.065226	43.188698
3520.680710	633840.036047	43.193703
3520.663042	633383.618848	43.198708
3520.541620	632934.255550	43.203713
3520.696524	632483.624612	43.208717
3520.978590	632025.145007	43.213722
3520.481450	631574.886499	43.218727
3520.556314	631113.699621	43.223732
3520.485591	630661.126731	43.228737
3520.316107	630208.701364	43.233741
3520.346960	629755.972027	43.238746
3520.187134	629326.534197	43.243751
3520.578482	628872.904387	43.248756
3520.629928	628427.573898	43.253761
3520.383854	627978.670583	43.258765
3520.599847	627520.206178	43.263770
3520.322049	627072.922174	43.268775
3520.374789	626616.148991	43.273780
3520.468615	626174.321881	43.278785
3520.080273	625736.865452	43.283789
3520.154463	625291.098946	43.288794
3520.248651	624841.203654	43.293799
3520.180727	624385.056541	43.298804
3520.335644	623939.971124	43.303809
3519.903155	623497.121301	43.308813
3520.205453	623052.474742	43.313818
3520.039173	622606.988102	43.318823
3519.976035	622162.567473	43.323828
3520.177337	621723.093027	43.328833
3519.987734	621285.470959	43.333837
3519.924951	620847.709289	43.338842
3519.686087	620407.204286	43.343847
3519.993824	619964.784247	43.348852
3519.830628	619532.297620	43.353857
3519.720154	619092.218294	43.358861
3519.575409	618650.423213	43.363866
3519.391122	618223.400275	43.368871
3519.687189	617785.904781	43.373876
3519.674428	617359.369965	43.378881
3519.210060	616921.668946	43.383885
3519.261906	616486.217950	43.388890
3518.964731	616068.001377	43.393895
3519.284823	615643.498109	43.398900
3519.104579	615225.730700	43.403905
3519.104551	614789.719934	43.408909
3519.369108	614366.931342	43.413914
3518.954175	613950.509102	43.418919
3519.059718	613523.654583	43.423924
3519.246397	613114.517984	43.428929
3518.941031	612684.843451	43.433933
3518.925965	612265.080573	43.438938
3518.778525	611852.244004	43.443943
3518.778012	611432.346848	43.448948
3519.099516	611022.056989	43.453953
3518.965995	610602.853265	43.458957
3518.965139	610178.897059	43.463962
3519.082401	609771.905914	43.468967
3519.080787	609348.118895	43.473972
3519.096806	608932.287482	43.478977
3519.006493	608515.656271	43.483981
3519.089795	608091.757055	43.488986
3518.358874	607678.865739	43.493991
3518.441435	607255.436700	43.498996
3518.655079	606848.623969	43.504001
3518.593595	606429.201621	43.509005
3518.605237	606012.811459	43.514010
3518.360880	605613.708135	43.519015
3518.443723	605205.554125	43.524020
3518.457401	604804.070300	43.529025
3518.376611	604395.915073	43.534029
3518.382698	603992.196108	43.539034
3517.985213	603589.936718	43.544039
3518.236781	603185.846154	43.549044
3518.204596	602788.765071	43.554049
3518.170382	602384.945837	43.559053
3518.310105	601968.787067	43.564058
3518.230171	601573.077099	43.569063
3518.434048	601163.402508	43.574068
3518.508599	600766.835300	43.579073
3518.404304	600365.516595	43.584077
3518.629590	599950.223647	43.589082
3518.121159	599552.208234	43.594087
3518.034923	599136.286575	43.599092
3518.079514	598740.959856	43.604097
3517.762600	598354.014836	43.609101
3518.114560	597945.656382	43.614106
3517.951366	597547.563170	43.619111
3518.183851	597148.183772	43.624116
3518.012087	596747.704859	43.629121
3518.011841	596350.647391	43.634125
3517.968812	595956.596418	43.639130
3517.746203	595563.818130	43.644135
3518.184162	595161.875044	43.649140
3517.971072	594770.374053	43.654145
3517.438546	594373.892604	43.659149
3517.789279	593973.279499	43.664154
3517.584959	593586.809743	43.669159
3517.634141	593186.823953	43.674164
3517.654435	592800.189532	43.679169
3517.336901	592414.855777	43.684173
3517.549450	592022.788696	43.689178
3517.211220	591647.228047	43.694183
3517.585505	591254.756246	43.699188
3517.273507	590871.832577	43.704193
3517.352117	590491.040200	43.709197
3517.653283	590092.262940	43.714202
3517.300722	589722.722417	43.719207
3516.965700	589330.207566	43.724212
3517.497433	588952.001494	43.729217
3517.332420	588579.579909	43.734221
3517.275533	588180.699268	43.739226
3517.193338	587806.430601	43.744231
3517.118132	587421.898355	43.749236
3517.336332	587042.529674	43.754241
3517.186087	586665.724482	43.759245
3517.715658	586279.343796	43.764250
3517.443001	585898.314166	43.769255
3517.604135	585513.831230	43.774260
3517.598828	585130.671157	43.779265
3517.348227	584740.102373	43.784269
3517.279980	584353.862557	43.789274
3517.053713	583968.290805	43.794279
3517.263484	583590.574112	43.799284
3517.416849	583210.995446	43.804289
3517.423869	582833.691942	43.809293
3517.196592	582451.289282	43.814298
3517.262880	582072.494246	43.819303
3517.100846	581682.163797	43.824308
3516.987849	581302.571100	43.829313
3516.772770	580933.089394	43.834317
3516.743280	580539.482183	43.839322
3516.547656	580187.621864	43.844327
3516.693104	579807.285050	43.849332
3516.249706	579441.970604	43.854337
3516.119564	579081.167566	43.859341
3516.222080	578715.185214	43.864346
3516.347689	578354.116073	43.869351
3516.118695	577991.990586	43.874356
3516.075911	577622.128486	43.879361
3515.779550	577275.733932	43.884365
3515.922391	576914.720379	43.889370
3515.760371	576565.919325	43.894375
3515.644855	576214.032555	43.899380
3515.910821	575864.987857	43.904385
3515.399231	575517.977425	43.909389
3515.643256	575164.239161	43.914394
3515.674981	574820.486565	43.919399
3515.765165	574471.885563	43.924404
3515.455135	574126.914685	43.929409
3515.373576	573774.601140	43.934413
3515.860381	573435.662615	43.939418
3515.472142	573095.053274	43.944423
3515.478199	572739.174177	43.949428
3515.897668	572404.143379	43.954433
3515.613302	572065.098307	43.959437
3515.666374	571707.974550	43.964442
3515.494227	571372.564518	43.969447
3515.993959	571023.848220	43.974452
3515.241387	570678.958930	43.979457
3515.229872	570338.915213	43.984461
3515.441328	569992.987236	43.989466
3515.131735	569669.279976	43.994471
3515.195462	569328.391193	43.999476
3515.403649	568981.530427	44.004481
3515.425277	568640.982680	44.009485
3515.357204	568320.571631	44.014490
3515.107010	567977.183972	44.019495
3514.900166	567628.293828	44.024500
3514.943054	567303.610694	44.029505
3514.667036	566987.580450	44.034509
3515.487843	566643.269491	44.039514
3514.764969	566311.947385	44.044519
3514.763428	565983.614363	44.049524
3514.964909	565661.631047	44.054529
3515.074487	565333.363135	44.059533
3515.103170	564997.499458	44.064538
3514.606645	564668.260974	44.069543
3514.784770	564339.150618	44.074548
3514.918447	564013.613834	44.079553
3514.300136	563698.517834	44.084557
3514.547803	563370.982012	44.089562
3514.355399	563051.568545	44.094567
3514.465534	562728.017380	44.099572
3514.504168	562412.073112	44.104577
3514.201174	562091.144456	44.109581
3514.333939	561772.550379	44.114586
3514.446562	561463.871490	44.119591
3514.055909	561143.639430	44.124596
3513.948097	560826.221491	44.129601
3513.869642	560519.265007	44.134605
3514.104579	560213.959988	44.139610
3514.116551	559903.096095	44.144615
3514.085586	559595.807741	44.149620
3513.995941	559291.090647	44.154625
3513.871014	558989.142454	44.159629
3514.115343	558678.109213	44.164634
3513.903118	558375.003492	44.169639
3513.866104	558060.528561	44.174644
3514.173694	557753.391281	44.179649
3513.781418	557452.309822	44.184653
3514.111152	557143.341351	44.189658
3513.890161	556849.268665	44.194663
3514.151371	556545.687626	44.199668
3514.011851	556233.806173	44.204673
3513.984527	555930.814459	44.209677
3514.117126	555612.474480	44.214682
3514.195136	555309.803287	44.219687
3514.051511	555006.105142	44.224692
3513.877824	554696.611675	44.229697
3513.834336	554392.277940	44.234701
3513.829651	554077.552173	44.239706
3513.771352	553783.887918	44.244711
3513.734795	553488.349343	44.249716
3513.815245	553186.889317	44.254721
3513.566792	552886.032928	44.259725
3513.450683	552586.759589	44.264730
3513.097404	552298.555005	44.269735
3513.349564	551997.240580	44.274740
3513.817454	551696.739229	44.279745
3513.622955	551413.880373	44.284749
3513.462110	551108.484591	44.289754
3513.442746	550812.733270	44.294759
3513.601720	550516.239529	44.299764
3513.368921	550229.280540	44.304769
3513.278350	549937.755524	44.309773
3513.458285	549632.721919	44.314778
3513.513354	549346.501517	44.319783
3513.515567	549052.724169	44.324788
3513.491187	548770.134017	44.329793
3513.090470	548476.312257	44.334797
3513.189285	548181.693250	44.339802
3513.078992	547898.142087	44.344807
3513.235658	547608.742893	44.349812
3513.389157	547319.892603	44.354817
3513.242382	547034.716822	44.359821
3513.494768	546744.829414	44.364826
3513.272714	546449.774336	44.369831
3513.105513	546163.827850	44.374836
3513.469644	545871.735344	44.379841
3513.287795	545594.248671	44.384845
3513.237931	545296.971797	44.389850
3513.103847	545017.751334	44.394855
3513.126890	544728.717789	44.399860
3513.466421	544445.119594	44.404865
3512.863236	544162.785749	44.409869
3512.811496	543869.007800	44.414874
3512.851096	543600.670019	44.419879
3513.072129	543312.178225	44.424884
3513.013417	543036.484927	44.429889
3512.654945	542757.156498	44.434893
3513.054645	542471.339635	44.439898
3512.652161	542194.276532	44.444903
3512.543898	541910.602350	44.449908
3512.732647	541640.285240	44.454913
3512.750674	541372.261314	44.459917
3512.835644	541088.487076	44.464922
3512.815911	540815.869957	44.469927
3512.783418	540540.677764	44.474932
3512.631422	540260.154831	44.479937
3512.490292	539998.486286	44.484941
3512.551386	539715.243194	44.489946
3512.649239	539445.958544	44.494951
3512.238674	539173.628562	44.499956
3512.640590	538900.145882	44.504961
3512.359797	538644.074559	44.509965
3512.438285	538356.060154	44.514970
3512.136251	538098.166810	44.519975
3512.115305	537839.817265	44.524980
3512.225444	537565.652517	44.529985
3512.029434	537308.332035	44.534989
3512.244708	537047.203887	44.539994
3512.396314	536784.114509	44.544999
3512.197158	536518.154358	44.550004
3512.434790	536257.159275	44.555009
3512.293745	535986.538280	44.560013
3512.010648	535722.847778	44.565018
3512.067529	535468.881431	44.570023
3511.975641	535198.993897	44.575028
3512.186610	534945.042420	44.580033
3512.164757	534678.261079	44.585037
3512.206423	534416.610093	44.590042
3512.050120	534159.629861	44.595047
3511.915197	533898.050059	44.600052
3512.192723	533637.757382	44.605057
3511.994229	533386.169274	44.610061
3512.231077	533120.475428	44.615066
3511.908104	532865.216151	44.620071
3511.944563	532603.280907	44.625076
3512.027246	532351.424970	44.630081
3511.512744	532089.120373	44.635085
3511.905815	531838.514517	44.640090
3511.746894	531594.659610	44.645095
3511.533805	531332.491745	44.650100
3511.666023	531076.214963	44.655105
3511.230198	530834.009447	44.660109
3511.195248	530583.808343	44.665114
3511.236379	530348.477610	44.670119
3510.958933	530095.533887	44.675124
3511.165190	529851.335158	44.680129
3511.194795	529613.521630	44.685133
3511.379035	529372.599176	44.690138
3511.486290	529130.928852	44.695143
3511.234239	528888.558826	44.700148
3511.368118	528645.462768	44.705153
3510.952440	528414.923418	44.710157
3511.481885	528160.748654	44.715162
3511.502460	527922.555999	44.720167
3511.465174	527685.378894	44.725172
3511.460042	527437.087650	44.730177
3511.406032	527197.129353	44.735181
3511.381115	526956.253590	44.740186
3511.115179	526713.345421	44.745191
3511.186403	526470.678584	44.750196
3511.671549	526226.069321	44.755201
3511.364269	525987.598631	44.760205
3511.519445	525745.915251	44.765210
3511.205641	525502.288695	44.770215
3511.241438	525271.118483	44.775220
3511.464851	525025.776926	44.780225
3511.424952	524784.060772	44.785229
3511.413591	524530.168608	44.790234
3510.905104	524298.672378	44.795239
3511.248163	524069.551573	44.800244
3511.206403	523825.750242	44.805249
3511.000180	523595.049837	44.810253
3511.026873	523346.937420	44.815258
3510.725720	523116.195373	44.820263
3510.557764	522889.971319	44.825268
3510.764554	522663.275937	44.830273
3510.577620	522439.320523	44.835277
3510.873600	522201.090446	44.840282
3510.477923	521990.948941	44.845287
3510.637426	521768.540258	44.850292
3510.727205	521530.789277	44.855297
3510.687154	521312.195192	44.860301
3510.732391	521081.766861	44.865306
3510.405452	520849.227124	44.870311
3510.385087	520629.256359	44.875316
3510.609873	520411.260560	44.880321
3510.467891	520200.293388	44.885325
3510.862277	519963.374849	44.890330
3510.432546	519744.016690	44.895335
3510.459182	519515.941405	44.900340
3510.595269	519298.601360	44.905345
3510.396826	519077.375977	44.910349
3510.329917	518847.488507	44.915354
3510.473751	518628.874977	44.920359
3510.354917	518410.303172	44.925364
3510.596839	518193.484926	44.930369
3510.728904	517976.025763	44.935373
3510.492522	517754.737233	44.940378
3510.743459	517533.412819	44.945383
3510.501072	517312.068428	44.950388
3511.022422	517089.428692	44.955393
3510.712329	516869.958417	44.960397
3510.645362	516645.392237	44.965402
3510.740881	516416.602433	44.970407
3510.580655	516195.025914	44.975412
3510.662029	515973.607024	44.980417
3510.550713	515759.997263	44.985421
3510.741351	515533.249283	44.990426
3510.281527	515311.761782	44.995431
3510.006716	515086.905355	45.000436
3510.444712	514874.149431	45.005441
3509.937070	514662.663475	45.010445
3510.284250	514445.926186	45.015450
3510.093196	514230.843914	45.020455
3510.124543	514023.753571	45.025460
3510.281652	513805.625232	45.030465
3509.860327	513597.747648	45.035469
3509.772819	513375.209072	45.040474
3509.763618	513172.661456	45.045479
3509.432141	512968.599979	45.050484
3510.171015	512763.292058	45.055489
3509.586767	512566.847292	45.060493
3509.588961	512359.133564	45.065498
3509.726782	512162.055175	45.070503
3509.899161	511957.086067	45.075508
3509.718824	511742.119330	45.080513
3509.625665	511544.819998	45.085517
3509.934398	511341.537583	45.090522
3509.575672	511145.087064	45.095527
3509.266242	510948.170899	45.100532
3509.423339	510743.794986	45.105537
3508.911698	510553.427019	45.110541
3509.095200	510363.645529	45.115546
3509.251050	510178.161839	45.120551
3509.011438	509982.383991	45.125556
3509.244187	509792.536715	45.130561
3509.385035	509600.681442	45.135565
3509.430380	509401.158679	45.140570
3509.251692	509209.201625	45.145575
3509.164109	509026.020179	45.150580
3509.375798	508835.710229	45.155585
3509.395242	508644.369522	45.160589
3509.582639	508450.976278	45.165594
3509.287916	508263.171830	45.170599
3509.698924	508065.793644	45.175604
3509.486493	507869.378662	45.180609
3509.509419	507687.477034	45.185613
3509.375858	507483.715331	45.190618
3509.102189	507292.459014	45.195623
3509.092014	507094.989137	45.200628
3509.163822	506912.918735	45.205633
3508.825447	506726.518929	45.210637
3508.772423	506546.234739	45.215642
3508.948820	506361.006426	45.220647
3508.924113	506178.034352	45.225652
3509.169156	505983.944385	45.230657
3508.921137	505807.779508	45.235661
3509.062307	505613.146790	45.240666
3508.967981	505434.626386	45.245671
3508.894834	505258.021258	45.250676
3508.883628	505071.596984	45.255681
3509.123929	504893.518963	45.260685
3509.036760	504695.982271	45.265690
3509.159688	504523.430265	45.270695
3508.861949	504350.341624	45.275700
3509.247295	504164.698586	45.280705
3508.712381	503983.457014	45.285709
3509.184594	503791.425187	45.290714
3508.727425	503621.540878	45.295719
3508.584842	503436.687424	45.300724
3508.824400	503255.811052	45.305729
3508.914397	503079.204905	45.310733
3508.566667	502906.008309	45.315738
3508.657553	502737.537896	45.320743
3508.604223	502559.029427	45.325748
3508.705815	502381.857623	45.330753
3508.522817	502202.002327	45.335757
3508.620476	502030.136040	45.340762
3508.701739	501856.956197	45.345767
3508.413450	501684.596027	45.350772
3508.515596	501512.470744	45.355777
3508.565239	501333.577410	45.360781
3508.397753	501169.129320	45.365786
3508.347296	500988.884155	45.370791
3508.036704	500821.221027	45.375796
3508.441607	500656.619520	45.380801
3508.393643	500501.043496	45.385805
3508.351646	500329.233827	45.390810
3508.614617	500167.483276	45.395815
3508.092228	499995.398200	45.400820
3508.442290	499824.628777	45.405825
3508.479180	499659.827336	45.410829
3508.410901	499495.143344	45.415834
3507.947154	499328.047432	45.420839
3508.136102	499171.862201	45.425844
3508.643816	499005.810800	45.430849
3508.260274	498843.399170	45.435853
3508.286053	498677.123354	45.440858
3508.230554	498515.309906	45.445863
3507.807124	498352.849718	45.450868
3508.039269	498188.758880	45.455873
3507.732129	498027.641074	45.460877
3507.955673	497864.812799	45.465882
3507.960568	497705.004037	45.470887
3507.608005	497550.261490	45.475892
3508.079035	497394.011405	45.480897
3507.894301	497242.625764	45.485901
3507.604606	497089.081979	45.490906
3508.086209	496934.140723	45.495911
3507.980383	496778.286830	45.500916
3507.947009	496626.111138	45.505921
3507.930153	496464.928694	45.510925
3508.143231	496311.089627	45.515930
3507.876709	496155.459686	45.520935
3507.771948	496004.858436	45.525940
3507.833052	495844.567120	45.530945
3507.530628	495702.139962	45.535949
3507.601264	495546.042182	45.540954
3507.775397	495388.761959	45.545959
3507.036073	495245.242206	45.550964
3507.460108	495100.359249	45.555969
3507.479688	494956.555719	45.560973
3507.526025	494800.657510	45.565978
3507.418486	494663.094664	45.570983
3507.578644	494524.372188	45.575988
3507.522393	494371.876531	45.580993
3507.734239	494226.769404	45.585997
3507.762742	494082.198172	45.591002
3507.758483	493926.452297	45.596007
3507.384878	493777.445168	45.601012
3507.723475	493627.961034	45.606017
3507.739608	493493.959085	45.611021
3507.891807	493336.562361	45.616026
3507.858911	493191.184655	45.621031
3507.756796	493034.941452	45.626036
3507.533031	492887.772631	45.631041
3507.372335	492735.937741	45.636045
3507.286106	492589.956959	45.641050
3507.507002	492442.253078	45.646055
3507.296127	492311.518225	45.651060
3507.350776	492170.163943	45.656065
3507.093349	492032.150087	45.661069
3507.222879	491883.596957	45.666074
3507.388050	491753.299524	45.671079
3506.977289	491613.841356	45.676084
3507.332209	491470.355808	45.681089
3507.195860	491344.406984	45.686093
3507.369758	491203.176131	45.691098
3507.524829	491066.601816	45.696103
3507.148491	490925.664997	45.701108
3507.246887	490776.551073	45.706113
3507.320526	490646.311454	45.711117
3507.464544	490492.482085	45.716122
3507.551407	490355.610204	45.721127
3507.181211	490229.237785	45.726132
3507.379896	490084.451885	45.731137
3507.207699	489957.891883	45.736141
3507.058780	489809.469554	45.741146
3506.875152	489681.593983	45.746151
3506.880172	489542.199807	45.751156
3507.071140	489406.162764	45.756161
3506.982721	489282.467542	45.761165
3506.919192	489140.349569	45.766170
3507.272962	489009.391995	45.771175
3506.811354	488878.977441	45.776180
3507.287324	488743.341918	45.781185
3506.921825	488624.243218	45.786189
3507.229494	488485.649053	45.791194
3507.291855	488351.244883	45.796199
3506.969898	488220.447333	45.801204
3507.038177	488080.018588	45.806209
3507.296444	487958.734181	45.811213
3507.076338	487814.203222	45.816218
3506.992903	487682.956090	45.821223
3507.106557	487554.862276	45.826228
3507.219471	487420.695302	45.831233
3507.506872	487295.808504	45.836237
3507.466120	487152.202895	45.841242
3507.258854	487015.354878	45.846247
3507.209198	486881.970585	45.851252
3507.379850	486740.096650	45.856257
3507.199292	486612.805236	45.861261
3507.343588	486473.919352	45.866266
3507.514019	486334.015785	45.871271
3506.677927	486209.970946	45.876276
3507.178151	486064.391608	45.881281
3506.891140	485940.807787	45.886285
3507.011922	485804.855837	45.891290
3506.965123	485676.623855	45.896295
3506.615929	485553.098531	45.901300
3507.085371	485417.539530	45.906305
3506.672148	485294.580020	45.911309
3506.749770	485167.132825	45.916314
3506.691025	485046.540308	45.921319
3506.509117	484931.433883	45.926324
3506.809040	484811.436450	45.931329
3506.748168	484687.855830	45.936333
3506.905667	484558.062503	45.941338
3506.826056	484425.929968	45.946343
3506.838074	484303.397056	45.951348
3507.028512	484169.141407	45.956353
3506.763588	484050.348723	45.961357
3506.405263	483921.043698	45.966362
3506.741856	483806.296934	45.971367
3506.542779	483693.665435	45.976372
3506.626591	483560.435654	45.981377
3506.532023	483453.909080	45.986381
3506.820694	483322.515264	45.991386
3506.829192	483201.392549	45.996391
3506.406069	483075.129324	46.001396
3507.047051	482955.921561	46.006401
3506.563726	482836.196344	46.011405
3506.628426	482713.289150	46.016410
3506.615983	482594.797936	46.021415
3506.215901	482481.686913	46.026420
3506.649000	482361.953886	46.031425
3506.505964	482243.533255	46.036429
3506.283237	482127.504493	46.041434
3506.417555	482014.198026	46.046439
3506.124159	481898.989741	46.051444
3506.495292	481775.062012	46.056449
3506.284917	481667.127200	46.061453
3507.042371	481551.585394	46.066458
3506.777720	481426.498319	46.071463
3506.385448	481309.075838	46.076468
3506.600595	481188.056046	46.081473
3506.255300	481071.383298	46.086477
3506.273385	480954.698368	46.091482
3506.421562	480842.951393	46.096487
3506.219224	480723.822137	46.101492
3506.490481	480607.041101	46.106497
3506.122327	480499.176827	46.111501
3506.095145	480382.749028	46.116506
3505.965749	480275.703238	46.121511
3506.279887	480170.454154	46.126516
3506.120906	480056.577930	46.131521
3505.993005	479949.884318	46.136525
3506.028916	479842.807733	46.141530
3505.939810	479732.258749	46.146535
3505.900147	479631.471289	46.151540
3506.252548	479511.074923	46.156545
3506.111723	479406.962207	46.161549
3505.948427	479301.587078	46.166554
3506.304592	479198.046440	46.171559
3506.004528	479092.946581	46.176564
3506.270219	478978.383536	46.181569
3505.857284	478886.717879	46.186573
3506.038322	478770.952926	46.191578
3505.870220	478672.207158	46.196583
3505.802063	478559.014790	46.201588
3505.946661	478451.708911	46.206593
3505.865659	478353.402193	46.211597
3505.823323	478246.532051	46.216602
3505.656059	478146.517559	46.221607
3505.704549	478053.401919	46.226612
3505.913571	477950.486850	46.231617
3505.768109	477856.998285	46.236621
3505.823533	477738.666078	46.241626
3506.185467	477645.342944	46.246631
3505.575104	477548.438662	46.251636
3505.881182	477439.377798	46.256641
3505.779180	477346.081718	46.261645
3505.581592	477245.915568	46.266650
3505.856690	477149.465560	46.271655
3505.451597	477058.346305	46.276660
3505.655452	476953.451841	46.281665
3505.481906	476856.418669	46.286669
3505.584922	476761.768149	46.291674
3505.557315	476666.582476	46.296679
3505.392834	476569.546236	46.301684
3505.670398	476471.320061	46.306689
3505.740235	476383.458190	46.311693
3505.463882	476298.996877	46.316698
3505.377092	476194.097060	46.321703
3505.467340	476108.002598	46.326708
3505.535985	476015.733937	46.331713
3505.318970	475929.640468	46.336717
3505.344186	475834.846546	46.341722
3505.770179	475738.616536	46.346727
3505.360987	475645.212344	46.351732
3505.486203	475549.944155	46.356737
3505.574884	475458.378188	46.361741
3505.626286	475369.349978	46.366746
3505.995402	475274.950188	46.371751
3505.553941	475174.206726	46.376756
3505.901881	475082.138888	46.381761
3505.618440	474998.938759	46.386765
3505.653449	474904.999229	46.391770
3505.629773	474808.436042	46.396775
3505.551419	474718.869827	46.401780
3505.955451	474612.104845	46.406785
3505.625788	474527.340676	46.411789
3505.335888	474422.870574	46.416794
3505.711699	474334.997338	46.421799
3505.556168	474246.961209	46.426804
3505.831452	474144.013512	46.431809
3505.648318	474055.626706	46.436813
3505.640109	473960.474390	46.441818
3505.815572	473866.556251	46.446823
3505.703014	473779.776593	46.451828
3506.231167	473680.125471	46.456833
3505.723905	473584.600667	46.461837
3505.404907	473484.333515	46.466842
3505.731736	473385.019039	46.471847
3505.413695	473297.360652	46.476852
3505.758412	473206.904620	46.481857
3505.605697	473117.545945	46.486861
3505.686780	473022.778730	46.491866
3505.553218	472923.033969	46.496871
3505.770027	472830.876071	46.501876
3505.350317	472735.433246	46.506881
3505.251385	472646.316350	46.511885
3505.238169	472569.541665	46.516890
3505.085562	472478.711219	46.521895
3504.848816	472401.923368	46.526900
3505.141099	472318.005186	46.531905
3505.163207	472241.324413	46.536909
3504.950176	472151.161083	46.541914
3504.915983	472069.880463	46.546919
3504.986303	471995.672100	46.551924
3505.051051	471923.692832	46.556929
3504.665881	471834.114476	46.561933
3504.685234	471754.089507	46.566938
3504.998588	471676.495698	46.571943
3505.036099	471611.458515	46.576948
3505.131992	471520.732932	46.581953
3504.790910	471449.682145	46.586957
3505.032970	471353.916689	46.591962
3505.163671	471292.509133	46.596967
3504.786589	471217.158532	46.601972
3505.122636	471125.123830	46.606977
3504.972902	471057.077792	46.611981
3505.058803	470970.048608	46.616986
3505.103011	470896.498796	46.621991
3504.990343	470818.062505	46.626996
3505.422574	470731.986072	46.632001
3505.207224	470656.453662	46.637005
3505.005710	470575.650995	46.642010
3505.366991	470483.304951	46.647015
3505.320333	470402.930954	46.652020
3505.093583	470326.690064	46.657025
3505.020416	470249.865483	46.662029
3505.013653	470164.621183	46.667034
3505.097639	470086.705434	46.672039
3504.934678	470015.162959	46.677044
3505.299288	469935.425871	46.682049
3505.298331	469861.981044	46.687053
3505.374972	469771.655548	46.692058
3505.597642	469691.536453	46.697063
3505.208676	469617.194534	46.702068
3505.501802	469524.804797	46.707073
3505.604339	469434.473271	46.712077
3505.325299	469345.270186	46.717082
3505.311490	469258.604720	46.722087
3504.603930	469188.367792	46.727092
3505.154352	469098.768653	46.732097
3504.736755	469027.924428	46.737101
3504.819747	468950.206794	46.742106
3505.344538	468868.057121	46.747111
3504.559504	468795.552515	46.752116
3504.860730	468724.888352	46.757121
3504.973857	468656.434212	46.762125
3504.873376	468564.765530	46.767130
3504.967027	468500.974444	46.772135
3504.794458	468433.530738	46.777140
3505.007240	468356.295075	46.782145
3504.987234	468278.693598	46.787149
3504.484807	468210.190990	46.792154
3504.791960	468132.178462	46.797159
3504.535837	468070.370603	46.802164
3504.529806	468000.364098	46.807169
3504.522591	467928.229946	46.812173
3504.535182	467855.180309	46.817178
3504.550033	467778.381362	46.822183
3504.095522	467725.876561	46.827188
3504.203676	467652.860492	46.832193
3504.582390	467592.614395	46.837197
3504.264357	467536.995641	46.842202
3504.277283	467470.631337	46.847207
3504.526271	467403.922546	46.852212
3504.695545	467341.279818	46.857217
3504.568082	467280.359290	46.862221
3504.539462	467206.655651	46.867226
3504.706533	467150.294378	46.872231
3504.438623	467092.943368	46.877236
3504.534091	467014.303860	46.882241
3504.651729	466951.111421	46.887245
3504.545178	466880.408750	46.892250
3504.621929	466810.839700	46.897255
3504.405480	466746.133172	46.902260
3504.545843	466679.237769	46.907265
3504.694533	466624.245919	46.912269
3504.786961	466556.750350	46.917274
3504.963573	466483.971447	46.922279
3504.845258	466416.055421	46.927284
3504.903228	466337.672853	46.932289
3504.561263	466271.567645	46.937293
3504.181033	466209.825636	46.942298
3504.259900	466142.280268	46.947303
3504.416241	466087.792196	46.952308
3504.484565	466020.856145	46.957313
3504.299434	465964.602197	46.962317
3504.638611	465900.507225	46.967322
3504.790413	465837.203972	46.972327
3504.477399	465771.041441	46.977332
3504.497163	465698.894308	46.982337
3504.340776	465637.010917	46.987341
3504.418724	465571.186250	46.992346
3504.557946	465507.326768	46.997351
3504.392302	465448.028185	47.002356
3504.221571	465386.957059	47.007361
3504.544289	465331.779819	47.012365
3504.382562	465262.296564	47.017370
3504.657843	465196.284936	47.022375
3504.375854	465144.250264	47.027380
3504.747199	465070.318167	47.032385
3504.561539	465010.616345	47.037389
3504.115330	464939.001923	47.042394
3504.567784	464884.713225	47.047399
3504.557337	464823.359629	47.052404
3504.690093	464761.778725	47.057409
3504.400012	464690.947373	47.062413
3504.441820	464633.130838	47.067418
3504.955369	464569.964337	47.072423
3504.277390	464514.752976	47.077428
3504.488845	464442.467100	47.082433
3504.762543	464377.871611	47.087437
3504.807137	464313.872357	47.092442
3504.378177	464259.276414	47.097447
3503.976041	464198.038387	47.102452
3504.117280	464122.621971	47.107457
3504.025703	464080.887997	47.112461
3504.295375	464025.006763	47.117466
3504.584431	463963.295308	47.122471
3504.278409	463904.522649	47.127476
3504.344210	463835.198107	47.132481
3504.303763	463782.358525	47.137485
3504.500045	463720.966152	47.142490
3504.637644	463660.546302	47.147495
3504.521917	463608.327121	47.152500
3504.628492	463530.836932	47.157505
3504.094305	463467.643083	47.162509
3503.988887	463418.765767	47.167514
3503.948559	463358.882052	47.172519
3503.765262	463322.735701	47.177524
3503.981752	463263.415871	47.182529
3504.005822	463218.417475	47.187533
3504.134524	463161.341775	47.192538
3504.104498	463106.117118	47.197543
3504.068159	463051.957448	47.202548
3503.983092	462992.840296	47.207553
3503.592453	462954.397851	47.212557
3503.606336	462898.354390	47.217562
3504.184961	462847.078689	47.222567
3503.796063	462798.805601	47.227572
3504.164043	462758.409103	47.232577
3504.282531	462702.752586	47.237581
3503.931735	462649.709580	47.242586
3504.032277	462591.167573	47.247591
3503.901850	462544.876564	47.252596
3504.146186	462487.171103	47.257601
3503.991963	462439.667799	47.262605
3503.650991	462393.969767	47.267610
3504.104082	462335.113444	47.272615
3504.128488	462289.606140	47.277620
3504.086014	462234.279809	47.282625
3504.117414	462187.656294	47.287629
3504.173646	462124.002587	47.292634
3504.287316	462076.300646	47.297639
3504.284890	462025.679411	47.302644
3504.367345	461972.965978	47.307649
3504.183830	461924.402305	47.312653
3504.083622	461873.189302	47.317658
3504.190517	461809.272563	47.322663
3504.304875	461766.738396	47.327668
3504.083317	461704.549611	47.332673
3503.693569	461660.834459	47.337677
3503.938661	461601.656745	47.342682
3504.051010	461559.223820	47.347687
3504.102319	461518.068070	47.352692
3504.006703	461461.532470	47.357697
3503.955290	461405.039834	47.362701
3503.730509	461350.350234	47.367706
3504.067539	461298.655687	47.372711
3503.862259	461257.897926	47.377716
3503.701083	461213.737358	47.382721
3503.861040	461160.957846	47.387725
3504.058128	461118.610855	47.392730
3504.105781	461068.282659	47.397735
3504.065213	461020.857874	47.402740
3504.137745	460964.545515	47.407745
3503.969435	460923.020623	47.412749
3503.760199	460873.546598	47.417754
3503.919056	460815.242734	47.422759
3504.082577	460766.870333	47.427764
3504.317860	460714.380822	47.432769
3504.168352	460670.521102	47.437773
3504.142773	460609.866358	47.442778
3503.987568	460546.851780	47.447783
3503.234327	460532.791081	47.452788
3503.673084	460485.840609	47.457793
3503.742315	460432.567882	47.462797
3503.775329	460398.862372	47.467802
3504.015084	460351.692179	47.472807
3503.722639	460298.835585	47.477812
3503.962056	460252.830782	47.482817
3503.917162	460204.441917	47.487821
3503.583362	460163.247751	47.492826
3503.770658	460110.562127	47.497831
3504.003076	460080.065376	47.502836
3504.445723	460022.318854	47.507841
3504.222994	459972.692851	47.512845
3503.781409	459919.911390	47.517850
3504.087556	459880.026345	47.522855
3503.920861	459828.211263	47.527860
3503.598772	459778.753774	47.532865
3503.947015	459731.969012	47.537869
3503.449749	459687.710393	47.542874
3504.024539	459649.755475	47.547879
3503.471373	459614.679046	47.552884
3503.514886	459556.239143	47.557889
3503.848038	459519.896278	47.562893
3503.473409	459474.856063	47.567898
3503.914637	459438.545275	47.572903
3504.136978	459398.470860	47.577908
3503.821784	459337.912362	47.582913
3503.958598	459296.331966	47.587917
3503.651231	459250.722285	47.592922
3503.819157	459211.366299	47.597927
3503.767473	459176.862306	47.602932
3503.495028	459121.819939	47.607937
3503.606617	459095.903499	47.612941
3503.696992	459053.418288	47.617946
3503.700980	459005.829043	47.622951
3503.346975	458966.156250	47.627956
3503.737461	458932.843342	47.632961
3503.459971	458900.810083	47.637965
3503.206692	458853.669846	47.642970
3503.590406	458813.617383	47.647975
3503.228323	458795.991694	47.652980
3503.209070	458735.887643	47.657985
3503.060187	458707.430452	47.662989
3503.289758	458688.436622	47.667994
3503.637392	458643.879376	47.672999
3503.279691	458613.075696	47.678004
3503.656131	458583.717733	47.683009
3503.633696	458539.223443	47.688013
3503.454991	458506.260419	47.693018
3503.662501	458464.463496	47.698023
3503.642386	458430.510320	47.703028
3503.880551	458386.072556	47.708033
3503.913389	458338.578161	47.713037
3503.565003	458307.062872	47.718042
3503.949212	458258.089197	47.723047
3503.882730	458218.872647	47.728052
3504.073515	458159.592600	47.733057
3503.490378	458127.103466	47.738061
3503.456055	458080.025384	47.743066
3503.616971	458038.539624	47.748071
3503.481250	458007.139600	47.753076
3503.579971	457982.085521	47.758081
3503.368431	457936.760576	47.763085
3503.412319	457896.713625	47.768090
3503.333319	457864.695497	47.773095
3503.335814	457830.484029	47.778100
3503.365483	457792.365256	47.783105
3503.264425	457766.635456	47.788109
3503.351812	457744.370597	47.793114
3503.560915	457689.698217	47.798119
3503.159043	457663.056662	47.803124
3503.240235	457634.812080	47.808129
3503.615254	457600.739348	47.813133
3504.111294	457570.295127	47.818138
3503.947804	457512.644859	47.823143
3503.856664	457485.291120	47.828148
3503.819910	457433.396959	47.833153
3503.801164	457391.484384	47.838157
3503.854969	457359.949618	47.843162
3504.209592	457315.590971	47.848167
3503.860036	457276.370231	47.853172
3503.828073	457228.985646	47.858177
3503.763801	457179.883185	47.863181
3503.777530	457143.033022	47.868186
3503.678134	457100.728134	47.873191
3503.775355	457067.158099	47.878196
3503.936820	457019.283828	47.883201
3503.771094	456986.924316	47.888205
3503.432615	456946.940763	47.893210
3503.642201	456901.997748	47.898215
3503.529639	456866.891950	47.903220
3503.393221	456829.357254	47.908225
3503.576605	456792.730912	47.913229
3503.321417	456756.331446	47.918234
3503.684361	456723.881243	47.923239
3503.499084	456681.590139	47.928244
3503.328330	456636.255300	47.933249
3503.610301	456614.361458	47.938253
3503.249233	456574.279651	47.943258
3503.751030	456540.994465	47.948263
3503.193105	456509.866940	47.953268
3503.522976	456472.606769	47.958273
3503.801860	456444.276079	47.963277
3503.669259	456406.841320	47.968282
3503.545489	456372.699624	47.973287
3503.360268	456329.343351	47.978292
3503.910197	456293.413822	47.983297
3503.308502	456252.764220	47.988301
3503.457815	456224.607408	47.993306
3503.505048	456186.685351	47.998311
3503.411525	456161.307026	48.003316
3503.399327	456121.570251	48.008321
3503.662712	456092.532093	48.013325
3503.495887	456054.646338	48.018330
3503.581044	456014.183103	48.023335
3503.404297	455988.717397	48.028340
3503.423796	455947.048733	48.033345
3503.259606	455916.613382	48.038349
3503.266629	455893.194383	48.043354
3503.377831	455858.707571	48.048359
3503.129330	455826.563087	48.053364
3503.368235	455799.961721	48.058369
3502.900140	455763.495445	48.063373
3502.741817	455738.229031	48.068378
3502.828011	455696.193645	48.073383
3502.940836	455691.612451	48.078388
3502.876453	455667.850564	48.083393
3503.194921	455653.096537	48.088397
3502.980974	455628.092926	48.093402
3503.285802	455580.393530	48.098407
3503.152251	455566.629019	48.103412
3503.249404	455543.295604	48.108417
3503.268194	455497.469652	48.113421
3503.043697	455471.453870	48.118426
3503.620833	455444.642220	48.123431
3503.167957	455427.941482	48.128436
3502.998275	455378.041621	48.133441
3503.440898	455353.990040	48.138445
3503.251095	455340.133601	48.143450
3502.999574	455301.449872	48.148455
3503.325617	455266.063651	48.153460
3502.874912	455243.786539	48.158465
3503.005558	455224.299448	48.163469
3503.198916	455200.999904	48.168474
3503.009746	455164.282165	48.173479
3503.078494	455148.353857	48.178484
3503.229334	455129.978405	48.183489
3503.602386	455081.556533	48.188493
3502.995376	455058.444176	48.193498
3503.067410	455020.211566	48.198503
3502.886797	455014.007548	48.203508
3502.951328	454994.987739	48.208513
3502.877107	454957.692408	48.213517
3503.398675	454933.018568	48.218522
3503.420197	454901.688251	48.223527
3502.854037	454885.006408	48.228532
3503.167460	454847.492615	48.233537
3503.612856	454819.891591	48.238541
3503.200809	454804.095799	48.243546
3503.496701	454773.529488	48.248551
3503.503087	454738.653150	48.253556
3503.336036	454709.939970	48.258561
3503.499191	454675.847812	48.263565
3503.173775	454640.267596	48.268570
3503.398301	454614.528886	48.273575
3503.449609	454591.354283	48.278580
3503.591576	454555.694115	48.283585
3503.582245	454533.188786	48.288589
3503.166012	454498.891114	48.293594
3503.391940	454462.202617	48.298599
3503.349183	454451.767490	48.303604
3503.110507	454404.411604	48.308609
3502.844889	454383.166471	48.313613
3503.080012	454352.812674	48.318618
3503.296520	454333.664916	48.323623
3502.927227	454306.050229	48.328628
3502.941311	454262.452750	48.333633
3503.072359	454245.296490	48.338637
3502.991121	454236.287203	48.343642
3503.118395	454223.541782	48.348647
3502.681028	454196.749645	48.353652
3502.964751	454160.101430	48.358657
3503.010910	454137.535499	48.363661
3502.871311	454122.148889	48.368666
3503.311001	454106.460585	48.373671
3503.000776	454092.978707	48.378676
3503.000482	454053.185171	48.383681
3503.390014	454018.039413	48.388685
3503.505990	454007.374185	48.393690
3503.211552	453980.760131	48.398695
3502.762623	453946.315034	48.403700
3502.924889	453929.913573	48.408705
3502.890451	453909.490253	48.413709
3502.462201	453891.770189	48.418714
3502.823872	453880.201163	48.423719
3503.256959	453864.057565	48.428724
3503.535268	453831.363743	48.433729
3503.318086	453803.418246	48.438733
3503.299788	453785.019773	48.443738
3502.972219	453739.299708	48.448743
3502.955574	453722.320309	48.453748
3502.827652	453686.299163	48.458753
3503.066754	453676.068981	48.463757
3503.252376	453665.797232	48.468762
3503.650127	453623.755077	48.473767
3503.540549	453596.551329	48.478772
3503.521406	453568.318228	48.483777
3503.729820	453532.340770	48.488781
3503.417129	453504.613949	48.493786
3503.494542	453460.192847	48.498791
3503.150370	453440.937215	48.503796
3503.342937	453419.815624	48.508801
3503.369823	453384.933480	48.513805
3503.060665	453358.067659	48.518810
3502.852514	453339.650509	48.523815
3503.007873	453326.849043	48.528820
3502.941357	453311.550733	48.533825
3502.934933	453269.931727	48.538829
3503.047911	453242.233258	48.543834
3503.148500	453222.191755	48.548839
3503.152235	453215.195293	48.553844
3503.333790	453176.433594	48.558849
3503.167783	453138.947843	48.563853
3502.925759	453129.357185	48.568858
3503.371998	453108.648214	48.573863
3503.278447	453076.777110	48.578868
3503.160080	453041.969882	48.583873
3503.303950	453026.635437	48.588877
3503.361030	453007.462971	48.593882
3503.467878	452980.880490	48.598887
3503.290565	452962.812603	48.603892
3502.784425	452940.846613	48.608897
3503.012975	452891.683815	48.613901
3502.724927	452875.003535	48.618906
3503.043266	452849.652160	48.623911
3503.046502	452839.816706	48.628916
3503.139327	452822.057439	48.633921
3503.114831	452792.455406	48.638925
3502.824402	452764.673088	48.643930
3502.972913	452744.268067	48.648935
3502.841704	452737.091702	48.653940
3502.673925	452714.712825	48.658945
3503.071734	452699.385474	48.663949
3502.723988	452694.375294	48.668954
3503.555913	452660.064207	48.673959
3503.176545	452623.526476	48.678964
3503.308567	452610.779246	48.683969
3503.422236	452587.591733	48.688973
3503.062705	452550.746309	48.693978
3503.092437	452530.513448	48.698983
3502.945646	452510.006528	48.703988
3502.999913	452489.211777	48.708993
3503.507229	452450.494484	48.713997
3503.017177	452430.958634	48.719002
3503.391801	452405.647801	48.724007
3503.377916	452378.274013	48.729012
3503.208768	452354.374078	48.734017
3503.178407	452338.561905	48.739021
3502.830713	452314.185442	48.744026
3503.285145	452278.772152	48.749031
3503.025690	452254.076371	48.754036
3503.113480	452240.677404	48.759041
3503.119980	452216.088257	48.764045
3502.997224	452198.720143	48.769050
3503.180777	452158.891553	48.774055
3503.114390	452147.648135	48.779060
3503.079498	452131.836577	48.784065
3502.971403	452113.502640	48.789069
3502.903107	452080.307554	48.794074
3503.068963	452053.561712	48.799079
3502.998659	452042.369603	48.804084
3502.808057	452039.208238	48.809089
3503.144772	452007.262015	48.814093
3502.717439	451989.134570	48.819098
3502.851391	451953.521957	48.824103
3502.727797	451943.961221	48.829108
3502.925636	451924.003248	48.834113
3502.795947	451911.908648	48.839117
3503.090242	451897.815128	48.844122
3503.173863	451878.637082	48.849127
3502.954461	451853.731191	48.854132
3502.668391	451827.518504	48.859137
3503.340916	451809.811480	48.864141
3503.067999	451800.935249	48.869146
3503.027764	451772.297706	48.874151
3502.829805	451754.130889	48.879156
3502.786909	451723.313709	48.884161
3502.951698	451707.011447	48.889165
3502.653937	451697.531034	48.894170
3503.043471	451680.683394	48.899175
3502.854617	451676.507707	48.904180
3502.678647	451662.291530	48.909185
3503.080882	451635.352692	48.914189
3502.780612	451610.713809	48.919194
3503.126890	451584.544938	48.924199
3503.123579	451566.648913	48.929204
3503.054555	451555.152130	48.934209
3503.385582	451525.284783	48.939213
3503.192854	451506.711266	48.944218
3503.156011	451476.855963	48.949223
3502.901102	451468.483504	48.954228
3502.783779	451443.863883	48.959233
3502.670783	451407.785510	48.964237
3502.729644	451394.086742	48.969242
3503.053552	451370.101482	48.974247
3503.192303	451374.944942	48.979252
3503.360319	451351.138376	48.984257
3503.415598	451330.443687	48.989261
3502.707051	451310.487790	48.994266
3503.312712	451290.459574	48.999271
3503.021469	451278.949882	49.004276
3503.378276	451254.806774	49.009281
3503.364472	451218.812534	49.014285
3503.078086	451205.172592	49.019290
3502.841699	451181.485582	49.024295
3502.656729	451152.466299	49.029300
3502.875010	451127.687601	49.034305
3502.966274	451113.273318	49.039309
3502.553732	451092.354073	49.044314
3502.950143	451083.718147	49.049319
3502.723991	451073.616822	49.054324
3503.146684	451057.523514	49.059329
3503.336143	451030.975125	49.064333
3503.112429	451011.950156	49.069338
3503.455185	450989.482240	49.074343
3503.185826	450979.793848	49.079348
3502.871404	450941.619654	49.084353
3503.078102	450925.563125	49.089357
3503.169789	450903.644989	49.094362
3503.510072	450884.270100	49.099367
3503.155479	450859.233997	49.104372
3502.979075	450823.773841	49.109377
3502.878043	450807.161359	49.114381
3502.883955	450799.808806	49.119386
3502.710401	450787.163333	49.124391
3502.612845	450772.476852	49.129396
3502.751755	450753.541831	49.134401
3502.842903	450723.612892	49.139405
3502.178514	450709.327357	49.144410
3502.675929	450687.238314	49.149415
3502.606598	450680.456275	49.154420
3502.692411	450670.707094	49.159425
3502.731470	450660.205377	49.164429
3502.526173	450655.119675	49.169434
3502.656241	450641.408253	49.174439
3503.020638	450619.493955	49.179444
3502.774714	450613.198355	49.184449
3502.947448	450601.203456	49.189453
3502.645770	450601.255000	49.194458
3502.661535	450573.417459	49.199463
3502.619015	450540.722521	49.204468
3502.560948	450528.969794	49.209473
3502.790252	450506.774236	49.214477
3503.106554	450499.216475	49.219482
3503.382246	450484.212553	49.224487
3503.060491	450476.763730	49.229492
3502.822322	450460.681401	49.234497
3503.093656	450431.684603	49.239501
3502.588416	450422.746047	49.244506
3502.874683	450404.140458	49.249511
3502.861491	450396.638920	49.254516
3502.695487	450384.651034	49.259521
3502.952493	450375.075290	49.264525
3502.459504	450365.881109	49.269530
3502.694081	450347.791312	49.274535
3502.519717	450347.161997	49.279540
3502.428439	450338.000616	49.284545
3502.864527	450321.549543	49.289549
3502.522940	450288.905276	49.294554
3502.690605	450262.359630	49.299559
3502.975406	450254.148034	49.304564
3502.859056	450240.478425	49.309569
3502.868045	450222.579144	49.314573
3502.667694	450220.788117	49.319578
3503.086970	450201.044193	49.324583
3502.614885	450193.519533	49.329588
3502.484627	450185.885802	49.334593
3503.014984	450168.150962	49.339597
3502.545201	450143.082964	49.344602
3502.691798	450117.402667	49.349607
3502.765067	450100.506350	49.354612
3502.903698	450093.435100	49.359617
3503.327162	450082.056221	49.364621
3502.734227	450074.247938	49.369626
3503.337728	450054.218909	49.374631
3503.294176	450025.376719	49.379636
3503.001562	450003.523256	49.384641
3502.986122	449991.255923	49.389645
3503.091546	449986.117001	49.394650
3502.909139	449949.946550	49.399655
3502.459649	449929.438064	49.404660
3502.515839	449915.535970	49.409665
3502.543558	449905.542838	49.414669
3502.620876	449904.414210	49.419674
3502.673772	449885.695900	49.424679
3502.619749	449872.066110	49.429684
3502.065601	449865.315884	49.434689
3502.682817	449859.481110	49.439693
3502.507057	449856.063362	49.444698
3502.745507	449837.009109	49.449703
3502.866746	449832.425181	49.454708
3502.584948	449821.318692	49.459713
3502.563666	449805.807260	49.464717
3502.830618	449804.696949	49.469722
3502.809509	449781.732134	49.474727
3503.126708	449777.064031	49.479732
3502.702188	449755.334238	49.484737
3502.912576	449725.839838	49.489741
3502.788602	449707.050162	49.494746
3502.998822	449699.713040	49.499751
3502.583810	449697.248775	49.504756
3502.613070	449687.863714	49.509761
3502.704008	449675.578032	49.514765
3502.913495	449681.119655	49.519770
3502.587369	449641.069058	49.524775
3502.898951	449628.238640	49.529780
3502.519530	449609.441790	49.534785
3503.048063	449591.199741	49.539789
3502.638804	449580.672625	49.544794
3502.415006	449571.584239	49.549799
3502.712220	449573.003926	49.554804
3502.800854	449557.017211	49.559809
3502.676629	449544.818894	49.564813
3502.677995	449537.162451	49.569818
3502.977360	449527.477681	49.574823
3502.817926	449515.995210	49.579828
3502.671169	449496.093755	49.584833
3502.355462	449475.561980	49.589837
3502.400043	449456.692595	49.594842
3502.509865	449442.273992	49.599847
3502.716686	449427.990928	49.604852
3502.636975	449416.342678	49.609857
3502.451834	449404.256089	49.614861
3502.477493	449407.192569	49.619866
3502.423084	449397.416033	49.624871
3502.552618	449390.396804	49.629876
3502.352139	449381.608577	49.634881
3502.758037	449367.747816	49.639885
3502.460737	449371.956342	49.644890
3502.725461	449359.184465	49.649895
3502.526305	449357.545271	49.654900
3502.615250	449348.606204	49.659905
3503.031861	449339.763297	49.664909
3502.635791	449330.501405	49.669914
3502.642521	449319.294679	49.674919
3503.141961	449312.770008	49.679924
3502.997748	449307.318617	49.684929
3503.253562	449278.627099	49.689933
3502.778577	449270.595557	49.694938
3502.926435	449254.446386	49.699943
3502.929924	449240.958478	49.704948
3502.639652	449231.577068	49.709953
3502.922034	449225.393659	49.714957
3503.083323	449208.836525	49.719962
3502.928260	449168.502293	49.724967
3502.939569	449154.607359	49.729972
3502.559214	449148.993429	49.734977
3502.758978	449147.691739	49.739981
3502.825749	449132.469002	49.744986
3502.899659	449119.830970	49.749991
3502.738511	449109.311957	49.754996
3502.434540	449082.439711	49.760001
3502.807843	449049.316510	49.765005
3502.509653	449046.375876	49.770010
3502.572042	449037.136982	49.775015
3502.836365	449027.914309	49.780020
3502.572200	449022.128392	49.785025
3502.305502	449005.796290	49.790029
3502.566149	449007.374375	49.795034
3502.442882	448986.859967	49.800039
3502.400581	448984.889731	49.805044
3502.491685	448981.831912	49.810049
3502.720407	448966.074351	49.815053
3502.277125	448973.755821	49.820058
3502.285718	448943.382090	49.825063
3502.802504	448936.397996	49.830068
3502.301484	448933.491979	49.835073
3502.672684	448927.090497	49.840077
3502.763367	448922.055243	49.845082
3502.765140	448903.649017	49.850087
3502.638455	448901.388951	49.855092
3502.662782	448902.094702	49.860097
3503.142978	448890.401263	49.865101
3502.776893	448891.934255	49.870106
3502.721821	448878.912460	49.875111
3503.056478	448843.868737	49.880116
3502.705782	448826.333911	49.885121
3502.840978	448815.966972	49.890125
3502.580794	448813.628280	49.895130
3502.465307	448794.075757	49.900135
3502.472972	448787.989833	49.905140
3502.490809	448782.510635	49.910145
3502.660549	448768.182750	49.915149
3502.362931	448760.779897	49.920154
3502.445335	448761.425031	49.925159
3502.652452	448753.885288	49.930164
3502.555856	448749.186203	49.935169
3502.810594	448732.257799	49.940173
3502.749947	448728.008921	49.945178
3502.941300	448716.567528	49.950183
3503.178970	448713.078999	49.955188
3502.839836	448690.775760	49.960193
3503.010433	448662.402187	49.965197
3502.700254	448654.088738	49.970202
3502.938166	448639.444891	49.975207
3503.043712	448633.139386	49.980212
3503.018051	448614.129122	49.985217
3503.071649	448585.521894	49.990221
3502.811857	448575.070162	49.995226
3503.250270	448545.940820	50.000231
3503.165499	448546.208858	50.005236
3502.539557	448522.382526	50.010241
3502.924907	448492.907229	50.015245
3502.785315	448483.398344	50.020250
3502.810559	448477.157210	50.025255
3502.917406	448469.533074	50.030260
3502.507717	448471.428484	50.035265
3502.569658	448453.062297	50.040269
3502.444292	448455.669753	50.045274
3502.726354	448434.933479	50.050279
3502.608125	448431.302849	50.055284
3502.431577	448423.524260	50.060289
3502.904329	448416.243277	50.065293
3502.520021	448408.449451	50.070298
3502.325571	448402.296514	50.075303
3502.617694	448390.178554	50.080308
3502.468857	448393.043558	50.085313
3502.713451	448382.657727	50.090317
3502.400086	448377.539214	50.095322
3502.307948	448361.835989	50.100327
3502.526494	448358.553494	50.105332
3502.312941	448355.192659	50.110337
3502.411655	448344.527478	50.115341
3502.524044	448343.544899	50.120346
3502.702415	448326.274264	50.125351
3502.554902	448326.806550	50.130356
3502.405534	448320.341652	50.135361
3502.703918	448319.986498	50.140365
3502.606488	448312.954957	50.145370
3502.700393	448289.309687	50.150375
3502.768825	448283.010414	50.155380
3502.422066	448259.186820	50.160385
3502.564786	448244.609660	50.165389
3502.815812	448229.709757	50.170394
3502.942013	448225.124633	50.175399
3503.390182	448218.152021	50.180404
3503.166130	448213.373165	50.185409
3503.139812	448186.858021	50.190413
3502.722539	448163.959083	50.195418
3502.566349	448148.215928	50.200423
3502.877057	448140.303330	50.205428
3502.528988	448131.539780	50.210433
3502.772417	448118.669376	50.215437
3502.348651	448118.031868	50.220442
3502.348581	448108.955354	50.225447
3502.316995	448093.038762	50.230452
3502.410333	448097.383667	50.235457
3502.745775	448085.663793	50.240461
3502.478862	448094.177487	50.245466
3502.424254	448075.222387	50.250471
3502.804952	448074.041860	50.255476
3502.488295	448067.047669	50.260481
3502.609989	448057.848928	50.265485
3502.614083	448052.270473	50.270490
3502.687037	448038.465691	50.275495
3502.641362	448037.357965	50.280500
3502.621197	448036.499419	50.285505
3502.585532	448029.051579	50.290509
3502.311782	448025.041775	50.295514
3502.396672	448017.015567	50.300519
3502.711228	448003.270924	50.305524
3502.471820	448002.145568	50.310529
3502.370384	447993.339848	50.315533
3502.400550	447991.407853	50.320538
3502.411105	447981.923811	50.325543
3502.572437	447978.701734	50.330548
3502.332653	447979.452613	50.335553
3502.252675	447968.209266	50.340557
3502.673056	447961.494852	50.345562
3502.669592	447947.753766	50.350567
3502.506254	447937.285248	50.355572
3502.659767	447940.352224	50.360577
3502.772449	447934.349537	50.365581
3502.578813	447925.001750	50.370586
3502.565494	447910.501711	50.375591
3502.278001	447909.333853	50.380596
3502.426013	447901.448946	50.385601
3502.509658	447896.617479	50.390605
3502.488621	447891.195396	50.395610
3502.542644	447882.210963	50.400615
3502.664593	447878.184274	50.405620
3502.461939	447882.174103	50.410625
3502.779710	447872.384017	50.415629
3502.494243	447864.877358	50.420634
3502.553095	447856.094920	50.425639
3503.001819	447838.473479	50.430644
3502.586945	447810.959347	50.435649
3503.018782	447788.523510	50.440653
3502.708831	447781.173124	50.445658
3502.856733	447775.417918	50.450663
3502.769568	447767.218162	50.455668
3502.846163	447764.568307	50.460673
3502.526260	447753.010857	50.465677
3502.284035	447747.981460	50.470682
3502.226091	447744.543249	50.475687
3502.610984	447740.928008	50.480692
3502.444348	447738.725345	50.485697
3502.660062	447715.869962	50.490701
3502.522690	447713.459468	50.495706
3502.503827	447714.223342	50.500711
3502.672494	447705.117843	50.505716
3502.362483	447703.091782	50.510721
3502.386123	447698.625473	50.515725
3502.521006	447687.750954	50.520730
3502.598908	447655.335212	50.525735
3502.467241	447629.243021	50.530740
3502.297830	447596.920126	50.535745
3502.442314	447547.961947	50.540749
3502.240743	447486.892698	50.545754
3502.179352	447427.219179	50.550759
3502.473510	447343.043117	50.555764
3502.579521	447253.980064	50.560769
3502.643653	447138.149258	50.565773
3502.452343	447021.651501	50.570778
3502.215164	446888.680204	50.575783
3502.397652	446749.449762	50.580788
3502.062939	446608.329006	50.585793
3502.435234	446437.471366	50.590797
3502.328442	446266.795584	50.595802
3502.310601	446086.873689	50.600807
3502.440815	445876.801869	50.605812
3502.099576	445673.654723	50.610817
3502.270489	445442.779412	50.615821
3502.153882	445219.963510	50.620826
3502.020677	444961.495837	50.625831
3502.333592	444700.159547	50.630836
3502.236924	444447.460984	50.635841
3502.153294	444163.566656	50.640845
3502.139736	443863.072135	50.645850
3502.064824	443561.721710	50.650855
3502.246715	443233.797432	50.655860
3501.730293	442902.183480	50.660865
3502.204471	442560.606331	50.665869
3501.984608	442211.483465	50.670874
3502.054745	441835.828701	50.675879
3502.423722	441440.841811	50.680884
3501.853952	441042.964671	50.685889
3502.041638	440627.806056	50.690893
3501.940954	440193.565287	50.695898
3502.059815	439750.299864	50.700903
3502.239128	439284.086310	50.705908
3501.889638	438819.525837	50.710913
3501.971079	438326.067496	50.715917
3501.711483	437826.315079	50.720922
3501.820796	437297.165272	50.725927
3501.348562	436767.544205	50.730932
3501.327655	436234.992455	50.735937
3501.461695	435665.110792	50.740941
3501.322458	435097.087977	50.745946
3501.222803	434508.647313	50.750951
3501.424481	433895.125244	50.755956
3501.256688	433280.482746	50.760961
3501.145231	432630.497277	50.765965
3501.155231	431985.750104	50.770970
3501.110319	431308.161949	50.775975
3501.262788	430612.302098	50.780980
3500.697465	429913.549854	50.785985
3501.103936	429186.190703	50.790989
3501.090855	428444.365662	50.795994
3500.724976	427680.093774	50.800999
3501.034813	426895.836615	50.806004
3500.488423	426089.316080	50.811009
3500.809249	425272.722355	50.816013
3500.574730	424445.739106	50.821018
3500.290063	423588.837260	50.826023
3500.569653	422716.072023	50.831028
3500.235029	421831.907418	50.836033
3500.410351	420924.930779	50.841037
3500.251495	420006.859366	50.846042
3499.681929	419050.821736	50.851047
3499.912309	418082.983804	50.856052
3499.747445	417117.156327	50.861057
3499.704061	416109.456078	50.866061
3499.775677	415100.096732	50.871066
3499.512975	414052.414723	50.876071
3499.580547	412989.703384	50.881076
3499.242490	411925.138735	50.886081
3498.947423	410818.979035	50.891085
3498.962835	409717.316324	50.896090
3498.845386	408592.418596	50.901095
3498.725152	407437.099066	50.906100
3498.783535	406282.436011	50.911105
3498.686745	405088.991018	50.916109
3498.597105	403884.392760	50.921114
3498.236860	402658.374613	50.926119
3498.713623	401408.128585	50.931124
3498.141027	400154.805160	50.936129
3498.469504	398870.710236	50.941133
3498.084615	397571.918462	50.946138
3497.974909	396247.740974	50.951143
3498.196957	394917.373984	50.956148
3497.956278	393549.470436	50.961153
3497.692567	392162.221015	50.966157
3497.110355	390774.834754	50.971162
3496.513371	389367.031593	50.976167
3496.702019	387943.171054	50.981172
3496.155701	386507.323619	50.986177
3496.095269	385054.959052	50.991181
3496.159619	383593.940770	50.996186
3495.642213	382105.502712	51.001191
3495.590020	380594.597980	51.006196
3495.432879	379085.192304	51.011201
3495.362530	377545.603020	51.016205
3495.030035	375999.606721	51.021210
3495.024738	374435.331123	51.026215
3494.821876	372840.659826	51.031220
3494.449593	371255.963129	51.036225
3494.399420	369627.683807	51.041229
3494.249244	367997.339037	51.046234
3493.754668	366345.033792	51.051239
3493.578210	364679.045555	51.056244
3493.582028	363019.005882	51.061249
3493.575236	361319.168252	51.066253
3493.137544	359607.858719	51.071258
3492.707607	357879.914879	51.076263
3492.460855	356137.824177	51.081268
3492.036031	354384.522316	51.086273
3492.034592	352623.696959	51.091277
3491.608067	350848.497285	51.096282
3490.864928	349046.209061	51.101287
3490.926669	347241.979609	51.106292
3490.857026	345435.537493	51.111297
3490.583484	343605.395667	51.116301
3490.366309	341748.683933	51.121306
3489.949235	339877.251686	51.126311
3489.989375	337999.613311	51.131316
3489.729828	336108.468053	51.136321
3489.357091	334204.547692	51.141325
3489.065776	332292.298533	51.146330
3488.712547	330358.205854	51.151335
3488.719734	328410.647076	51.156340
3488.086928	326451.244266	51.161345
3487.545478	324475.978736	51.166349
3487.519710	322500.636551	51.171354
3487.350615	320505.909667	51.176359
3487.429838	318497.637144	51.181364
3486.473951	316476.013421	51.186369
3486.463143	314449.967759	51.191373
3485.981386	312404.646785	51.196378
3485.734310	310339.319424	51.201383
3485.511331	308266.904805	51.206388
3484.599044	306197.990623	51.211393
3484.556767	304104.382197	51.216397
3484.009185	302003.399611	51.221402
3483.547635	299884.809624	51.226407
3483.314160	297764.045053	51.231412
3483.147673	295647.654230	51.236417
3482.570398	293491.465074	51.241421
3481.824784	291345.015411	51.246426
3481.809739	289190.023738	51.251431
3481.497890	287008.434363	51.256436
3481.029313	284835.978363	51.261441
3481.056907	282636.690992	51.266445
3480.242167	280436.676101	51.271450
3479.432165	278225.273859	51.276455
3479.628340	275994.726308	51.281460
3478.886516	273771.878931	51.286465
3478.442592	271532.176683	51.291469
3478.152857	269280.689002	51.296474
3477.283509	267023.146644	51.301479
3477.529099	264756.690654	51.306484
3476.947283	262479.719865	51.311489
3476.523063	260198.537731	51.316493
3475.486161	257901.665172	51.321498
3475.191172	255611.260283	51.326503
3475.117764	253301.997648	51.331508
3474.559278	250981.666910	51.336513
3473.807287	248660.255801	51.341517
3473.337332	246323.118563	51.346522
3472.889423	243988.537828	51.351527
3472.479667	241646.479709	51.356532
3471.793977	239310.982691	51.361537
3471.490369	236939.458377	51.366541
3470.848392	234577.645054	51.371546
3470.003257	232216.991277	51.376551
3469.411015	229844.893073	51.381556
3469.014600	227468.112330	51.386561
3468.533660	225075.393921	51.391565
3467.678311	222690.524585	51.396570
3467.509882	220299.575324	51.401575
3466.824020	217902.602741	51.406580
3466.314506	215496.156478	51.411585
3465.723240	213082.321671	51.416589
3465.360891	210670.470077	51.421594
3464.669082	208250.974245	51.426599
3464.196691	205822.051445	51.431604
3463.293448	203398.698101	51.436609
3462.596235	200957.462887	51.441613
3462.231679	198532.137357	51.446618
3461.737117	196087.633770	51.451623
3460.749001	193644.129999	51.456628
3459.946914	191199.324337	51.461633
3459.248557	188755.449065	51.466637
3459.011372	186306.783344	51.471642
3458.167210	183845.191053	51.476647
3457.637981	181398.897561	51.481652
3456.604104	178948.588267	51.486657
3456.068943	176489.807955	51.491661
3455.384340	174028.919418	51.496666
3454.649424	171584.548728	51.501671
3453.793158	169111.189009	51.506676
3452.935698	166656.991742	51.511681
3452.213496	164199.036679	51.516685
3451.917546	161740.471150	51.521690
3451.148472	159290.267054	51.526695
3449.977690	156818.601893	51.531700
3449.031084	154371.707529	51.536705
3448.869665	151912.200774	51.541709
3448.093449	149466.458669	51.546714
3447.089736	147010.231307	51.551719
3446.554809	144485.643150	51.556724
3445.767929	142035.292122	51.561729
3444.591475	139580.408793	51.566733
3443.898990	137124.573191	51.571738
3442.959698	134692.103019	51.576743
3442.191883	132246.345789	51.581748
3441.177324	129821.910151	51.586753
3440.510846	127386.910206	51.591757
3439.681802	124954.400466	51.596762
3438.485556	122535.092057	51.601767
3437.973007	120108.236299	51.606772
3436.814129	117692.804244	51.611777
3435.679571	115285.303086	51.616781
3434.720011	112883.320631	51.621786
3433.652824	110496.585296	51.626791
3433.088859	108096.913013	51.631796
3431.770236	105728.259670	51.636801
3430.615900	103352.294681	51.641805
3429.635044	100988.701221	51.646810
3428.656213	98630.900664	51.651815
3427.879815	96285.328134	51.656820
3426.540472	93954.551264	51.661825
3425.671052	91626.633849	51.666829
3424.479318	89301.447047	51.671834
3423.422701	87006.590532	51.676839
3422.772590	84691.837234	51.681844
3421.223620	82423.073446	51.686849
3420.325492	80140.845681	51.691853
3419.142338	77873.093113	51.696858
3417.937380	75621.786050	51.701863
3416.868262	73369.343909	51.706868
3415.329550	71151.594350	51.711873
3413.869876	68940.782532	51.716877
3412.566967	66746.733885	51.721882
3411.036020	64566.367866	51.726887
3410.707016	62400.262557	51.731892
3409.061829	60261.254040	51.736897
3407.646205	58122.358400	51.741901
3406.162827	56009.168029	51.746906
3404.510067	53916.423921	51.751911
3403.161746	51849.666026	51.756916
3401.569827	49791.152684	51.761921
3400.176232	47770.918541	51.766925
3398.613146	45760.862774	51.771930
3396.936935	43776.414589	51.776935
3395.810783	41821.981456	51.781940
3393.848491	39886.420119	51.786945
3392.325148	37969.749373	51.791949
3390.689506	36092.125793	51.796954
3388.659159	34235.424627	51.801959
3387.199422	32402.016896	51.806964
3385.272230	30598.626205	51.811969
3383.407004	28832.904660	51.816973
3380.978297	27102.441055	51.821978
3377.480344	25437.256969	51.826983
3371.638195	23895.307537	51.831988
3363.599180	22476.523215	51.836993
3355.212115	21175.984988	51.841997
3348.401163	19983.724797	51.847002
3341.584960	18925.111534	51.852007
3335.862044	17968.476330	51.857012
3330.766181	17127.955101	51.862017
3326.112070	16400.140466	51.867021
3322.124843	15765.764369	51.872026
3318.353989	15223.437655	51.877031
3315.691492	14752.587255	51.882036
3312.928975	14379.864751	51.887041
3310.345162	14063.875762	51.892045
3308.991645	13788.399409	51.897050
3306.780838	13569.031622	51.902055
3305.575195	13394.034955	51.907060
3304.538974	13269.222115	51.912065
3303.889692	13156.890851	51.917069
3303.337281	13073.235207	51.922074
3302.195999	13013.381682	51.927079
3302.037478	12961.996147	51.932084
3301.631181	12938.721680	51.937089
3301.253456	12914.227215	51.942093
3301.001416	12897.248718	51.947098
3301.001755	12905.184303	51.952103
3300.757450	12896.704219	51.957108
3300.760473	12898.944415	51.962113
3300.075268	12895.521923	51.967117
3299.955578	12893.244838	51.972122
3299.674262	12898.777693	51.977127
3300.081655	12893.259712	51.982132
3299.738014	12903.543720	51.987137
3299.672459	12896.205587	51.992141
3299.480599	12883.269958	51.997146
3299.186838	12865.265192	52.002151
3299.336277	12852.086405	52.007156
3298.773272	12839.617154	52.012161
3298.953327	12817.551069	52.017165
3298.547173	12792.440639	52.022170
3298.368216	12754.738680	52.027175
3298.032752	12714.486316	52.032180
3297.791010	12681.584689	52.037185
3297.404660	12639.841640	52.042189
3297.255708	12594.834658	52.047194
3296.684441	12557.064277	52.052199
3296.430889	12503.906111	52.057204
3296.356942	12456.130947	52.062209
3295.781083	12398.908790	52.067213
3295.511147	12345.467933	52.072218
3294.922942	12283.477919	52.077223
3294.568131	12201.132886	52.082228
3294.017861	12149.823128	52.087233
3293.368303	12076.124803	52.092237
3293.238530	11995.867577	52.097242
3292.554453	11932.082914	52.102247
3292.309251	11845.086579	52.107252
3291.271358	11777.387510	52.112257
3291.054385	11695.231615	52.117261
3290.696330	11624.337519	52.122266
3290.259390	11552.640324	52.127271
3290.230444	11471.903904	52.132276
3289.217562	11397.305297	52.137281
3288.375590	11307.019870	52.142285
3288.108714	11219.613432	52.147290
3287.382953	11130.648972	52.152295
3286.602743	11043.318529	52.157300
3285.568140	10960.250562	52.162305
3285.168299	10878.665616	52.167309
3284.575018	10805.508488	52.172314
3283.829029	10714.933442	52.177319
3283.677845	10632.567826	52.182324
3282.928186	10552.124957	52.187329
3282.798345	10464.487433	52.192333
3282.250734	10372.687547	52.197338
3281.465194	10284.990789	52.202343
3280.937184	10193.171186	52.207348
3280.015788	10097.423738	52.212353
3279.590850	10005.628661	52.217357
3279.235278	9914.381530	52.222362
3278.161958	9818.958692	52.227367
3277.623687	9721.182648	52.232372
3276.983729	9637.922880	52.237377
3276.402127	9552.983672	52.242381
3275.932650	9465.430080	52.247386
3275.100406	9370.613267	52.252391
3274.786964	9270.976822	52.257396
3273.974529	9183.652378	52.262401
3273.301264	9091.536789	52.267405
3272.609206	8987.143634	52.272410
3271.798737	8909.245370	52.277415
3271.578649	8810.008131	52.282420
3270.754302	8711.410266	52.287425
3270.123909	8619.568075	52.292429
3269.633628	8520.524104	52.297434
3268.638471	8436.531835	52.302439
3268.047188	8328.482837	52.307444
3267.562217	8248.465866	52.312449
3266.930996	8149.744441	52.317453
3266.449413	8060.686357	52.322458
3265.678894	7968.600094	52.327463
3265.399584	7869.773661	52.332468
3264.425534	7780.899191	52.337473
3263.793138	7682.999092	52.342477
3263.091048	7583.432321	52.347482
3262.047730	7489.003015	52.352487
3261.710700	7379.829347	52.357492
3261.105842	7285.865775	52.362497
3260.423202	7196.297893	52.367501
3259.814728	7109.775960	52.372506
3258.606585	7023.848982	52.377511
3258.275426	6925.353118	52.382516
3257.602799	6837.257704	52.387521
3257.399012	6751.501004	52.392525
3256.458578	6649.582940	52.397530
3255.641724	6563.868003	52.402535
3254.842619	6462.678851	52.407540
3254.326292	6380.673658	52.412545
3253.660539	6290.991056	52.417549
3253.138086	6194.146633	52.422554
3252.303362	6117.928459	52.427559
3251.827014	6023.612305	52.432564
3251.076166	5938.987978	52.437569
3250.330087	5853.663574	52.442573
3250.010451	5757.297317	52.447578
3249.392008	5666.702722	52.452583
3248.924957	5576.895408	52.457588
3247.947394	5491.204194	52.462593
3247.307429	5390.522170	52.467597
3246.700970	5289.284626	52.472602
3245.694474	5210.284797	52.477607
3245.169539	5121.804008	52.482612
3244.363417	5031.648619	52.487617
3243.401850	4943.601147	52.492621
3242.910295	4851.175570	52.497626
3242.276596	4773.629639	52.502631
3241.694686	4686.731691	52.507636
3241.167207	4606.364259	52.512641
3240.162041	4519.528476	52.517645
3239.687394	4430.838408	52.522650
3238.917421	4358.648066	52.527655
3238.551300	4260.378320	52.532660
3237.740654	4183.317973	52.537665
3236.848171	4101.815957	52.542669
3236.427783	4024.489928	52.547674
3235.809515	3943.486737	52.552679
3235.296179	3849.868066	52.557684
3234.453513	3772.772544	52.562689
3233.339732	3690.505806	52.567693
3232.840544	3601.541083	52.572698
3231.983936	3532.549144	52.577703
3231.470570	3456.922883	52.582708
3230.770742	3383.797978	52.587713
3230.099414	3315.088813	52.592717
3229.531471	3231.868158	52.597722
3228.929105	3158.753700	52.602727
3228.643109	3075.375945	52.607732
3227.623127	3004.579970	52.612737
3226.807689	2925.077225	52.617741
3226.442944	2842.042626	52.622746
3225.426794	2769.370980	52.627751
3225.160866	2690.802791	52.632756
3224.405635	2626.361292	52.637761
3223.520022	2532.600038	52.642765
3222.880905	2460.764731	52.647770
3221.761767	2400.089429	52.652775
3221.305197	2313.100181	52.657780
3220.615937	2262.816881	52.662785
3219.878379	2190.859870	52.667789
3219.374633	2125.485253	52.672794
3218.286040	2059.307576	52.677799
3217.860563	1990.415322	52.682804
3217.042252	1931.306645	52.687809
3216.343947	1862.808172	52.692813
3215.681762	1801.192566	52.697818
3214.660681	1739.017150	52.702823
3214.248238	1693.416131	52.707828
3213.545416	1626.888559	52.712833
3213.051063	1568.498065	52.717837
3212.646687	1503.183670	52.722842
3211.643996	1454.241854	52.727847
3210.982170	1385.914109	52.732852
3210.078649	1334.381497	52.737857
3209.586210	1277.343017	52.742861
3209.226486	1205.664275	52.747866
3208.283615	1158.029675	52.752871
3207.730266	1095.178458	52.757876
3207.364460	1039.891251	52.762881
3206.367998	988.074068	52.767885
3206.094498	923.308563	52.772890
3204.901423	868.886474	52.777895
3204.266682	807.472589	52.782900
3203.274897	761.632593	52.787905
3202.766911	703.408706	52.792909
3202.119227	640.431745	52.797914
3201.075998	607.368108	52.802919
3200.600360	554.571665	52.807924
3199.877748	507.027737	52.812929
3198.917104	459.995542	52.817933
3198.477008	421.801498	52.822938
3197.642813	379.396349	52.827943
3196.977639	334.147991	52.832948
3196.417613	290.592569	52.837953
3195.850570	254.412047	52.842957
3195.125702	207.383754	52.847962
3193.906665	179.042433	52.852967
3193.099779	149.393670	52.857972
3191.635592	131.071881	52.862977
3190.019649	124.012761	52.867981
3189.257773	126.898556	52.872986
3188.000195	134.196052	52.877991
3187.927317	134.756814	52.882996
3187.415322	138.402402	52.888001
3187.021456	139.709174	52.893005
3186.307985	136.080789	52.898010
3185.231203	135.735458	52.903015
3184.543892	136.152911	52.908020
3184.372910	136.747802	52.913025
3184.086596	138.055146	52.918029
3183.001070	134.681769	52.923034
3182.305498	142.087326	52.928039
3181.755079	138.141353	52.933044
3181.092542	131.674854	52.938049
3180.372129	138.760977	52.943053
3180.063146	132.547488	52.948058
3178.952286	145.105335	52.953063
3178.548741	139.429041	52.958068
3177.954250	137.096748	52.963073
3177.376387	139.717823	52.968077
3176.795102	127.484280	52.973082
3176.578538	132.790145	52.978087
3175.446752	125.430027	52.983092
3174.663022	130.879369	52.988097
3174.145775	140.414806	52.993101
3173.697194	128.363060	52.998106
3172.739576	135.930619	53.003111
3171.747041	133.350945	53.008116
3171.321438	133.419746	53.013121
3170.268018	138.535439	53.018125
3170.340760	134.202349	53.023130
3169.408892	136.833776	53.028135
3169.206839	132.873286	53.033140
3168.624535	143.075878	53.038145
3167.617880	135.527013	53.043149
3166.911287	132.011533	53.048154
3166.645320	131.042556	53.053159
3165.604438	125.835546	53.058164
3165.089760	138.031798	53.063169
3164.772968	135.050891	53.068173
3164.078073	128.492427	53.073178
3162.749832	129.365958	53.078183
3162.405148	126.452974	53.083188
3162.011267	132.907003	53.088193
3161.113481	132.999242	53.093197
3160.709629	129.799926	53.098202
3160.190575	135.612989	53.103207
3159.681941	132.644728	53.108212
3158.702501	128.245098	53.113217
3157.346842	132.592184	53.118221
3157.206552	125.495293	53.123226
3156.176222	130.606251	53.128231
3156.293965	129.445404	53.133236
3155.983195	129.091963	53.138241
3155.019353	136.117047	53.143245
3154.135811	127.873749	53.148250
3152.912816	137.849493	53.153255
3152.640405	130.707280	53.158260
3152.233948	123.660208	53.163265
3150.867523	138.357326	53.168269
3150.902733	129.947582	53.173274
3150.306417	135.067677	53.178279
3149.580381	131.127241	53.183284
3148.887322	132.620919	53.188289
3147.958255	125.945762	53.193293
3147.947002	126.675202	53.198298
3147.206954	126.220242	53.203303
3146.668038	125.196456	53.208308
3145.525268	130.828720	53.213313
3144.498634	127.497790	53.218317
3144.638552	121.565237	53.223322
3143.731224	129.717479	53.228327
3142.670582	124.491746	53.233332
3142.324254	120.863404	53.238337
3141.299061	129.712348	53.243341
3141.311792	127.988798	53.248346
3140.466157	133.434905	53.253351
3139.531919	130.745016	53.258356
3138.896699	131.488304	53.263361
3137.657498	132.928061	53.268365
3137.928504	125.004601	53.273370
3136.790788	126.150314	53.278375
3136.429778	119.532840	53.283380
3135.928211	122.077723	53.288385
3135.606901	119.660475	53.293389
3135.355187	121.759258	53.298394
3133.739396	128.362847	53.303399
3133.383491	124.769694	53.308404
3132.248038	123.504024	53.313409
3131.152756	123.286598	53.318413
3130.768661	122.175179	53.323418
3130.409906	122.420452	53.328423
3129.773252	125.707611	53.333428
3129.403151	117.894482	53.338433
3128.704279	127.813434	53.343437
3127.928843	124.395380	53.348442
3126.914915	134.042515	53.353447
3126.883943	125.229619	53.358452
3126.360180	119.900714	53.363457
3125.398595	127.307508	53.368461
3124.882371	124.408837	53.373466
3123.919769	125.547527	53.378471
3123.110744	117.012044	53.383476
3122.358631	124.715011	53.388481
3122.314338	125.497464	53.393485
3122.204842	115.928270	53.398490
3120.836257	118.408139	53.403495
3119.879914	120.193113	53.408500
3119.744867	127.348162	53.413505
3118.495758	127.039392	53.418509
3118.065154	122.314293	53.423514
3116.708897	128.312239	53.428519
3116.466764	121.145126	53.433524
3116.482539	122.463223	53.438529
3115.608914	132.522560	53.443533
3115.125323	118.010951	53.448538
3114.546845	128.683394	53.453543
3113.575953	134.476556	53.458548
3113.131082	121.412506	53.463553
3111.955838	131.907843	53.468557
3111.471657	115.697034	53.473562
3110.577026	121.618078	53.478567
3109.786263	118.074756	53.483572
3109.151478	123.027741	53.488577
3108.906394	130.933022	53.493581
3108.616288	114.695371	53.498586
3107.699905	122.970735	53.503591
3107.126962	124.636915	53.508596
3106.172600	123.194260	53.513601
3105.320419	127.218888	53.518605
3104.947320	116.363320	53.523610
3104.300156	122.178532	53.528615
3104.196406	120.860534	53.533620
3102.844547	126.201693	53.538625
3102.746287	126.339697	53.543629
3102.044201	120.908241	53.548634
3101.022790	128.899587	53.553639
3100.615742	119.001902	53.558644
3100.058325	120.955160	53.563649
3098.749110	126.391662	53.568653
3098.404804	121.120123	53.573658
3097.794113	123.989963	53.578663
3097.080440	125.390854	53.583668
3096.650421	123.598090	53.588673
3095.906219	130.705250	53.593677
3095.043353	111.569090	53.598682
3094.198805	122.668692	53.603687
3093.453556	123.232236	53.608692
3092.826835	122.398322	53.613697
3092.537076	120.330941	53.618701
3092.703916	124.532764	53.623706
3091.063443	124.757833	53.628711
3090.094062	114.916762	53.633716
3090.179626	123.850648	53.638721
3089.382770	120.216003	53.643725
3089.046002	113.483083	53.648730
3087.636568	126.735341	53.653735
3087.470381	126.380885	53.658740
3086.909974	124.613952	53.663745
3085.642088	120.982424	53.668749
3085.075694	121.943688	53.673754
3084.837168	119.141650	53.678759
3084.485204	121.112697	53.683764
3083.718325	119.975504	53.688769
3082.277923	119.130231	53.693773
3082.350804	113.400186	53.698778
3081.457913	124.702256	53.703783
3080.839879	123.793045	53.708788
3079.545619	120.767590	53.713793
3078.982420	122.777099	53.718797
3079.027024	116.893204	53.723802
3077.949615	124.243608	53.728807
3077.482373	120.769350	53.733812
3077.009825	120.938940	53.738817
3075.776358	122.419570	53.743821
3075.601860	111.708888	53.748826
3074.601146	111.837280	53.753831
3073.795214	118.139477	53.758836
3073.428548	114.567512	53.763841
3072.394497	121.902612	53.768845
3072.147842	120.692716	53.773850
3071.156909	118.404495	53.778855
3070.425285	117.672981	53.783860
3070.648763	111.922730	53.788865
3069.812149	119.464088	53.793869
3068.692198	114.317193	53.798874
3068.010052	122.177150	53.803879
3067.589083	114.258648	53.808884
3066.669913	111.735540	53.813889
3066.446246	122.770500	53.818893
3065.717511	111.987551	53.823898
3064.802285	121.903601	53.828903
3064.099044	112.890990	53.833908
3063.911674	106.879767	53.838913
3062.889304	113.201972	53.843917
3062.057335	115.383719	53.848922
3061.564204	123.182170	53.853927
3061.264345	117.108060	53.858932
3060.216120	103.023739	53.863937
3059.258358	117.660884	53.868941
3059.180498	112.162645	53.873946
3058.767685	109.503283	53.878951
3057.652022	111.797056	53.883956
3057.176574	114.316164	53.888961
3056.031922	119.996520	53.893965
3055.216869	114.992525	53.898970
3055.046671	112.777616	53.903975
3054.720588	118.931904	53.908980
3054.040208	114.417648	53.913985
3052.841711	117.845812	53.918989
3052.113167	115.806833	53.923994
3051.513980	115.465576	53.928999
3051.336733	111.560071	53.934004
3050.442531	112.682348	53.939009
3049.412102	118.780939	53.944013
3049.184645	116.698574	53.949018
3048.205378	110.588985	53.954023
3048.219516	123.009459	53.959028
3047.278002	116.047121	53.964033
3046.029306	123.296141	53.969037
3045.479878	112.725710	53.974042
3045.224455	116.709949	53.979047
3044.927893	111.541574	53.984052
3044.410995	118.287795	53.989057
3043.169402	120.176389	53.994061
3042.859294	118.275116	53.999066
3041.825661	115.936567	54.004071
3041.179549	120.306505	54.009076
3041.023572	111.868661	54.014081
3040.024893	118.623391	54.019085
3039.569779	116.124412	54.024090
3038.116092	113.263181	54.029095
3037.730229	119.336895	54.034100
3037.604034	113.976782	54.039105
3036.285285	119.504130	54.044109
3035.944890	118.731427	54.049114
3034.957376	112.678511	54.054119
3035.045528	118.468339	54.059124
3033.452426	110.167514	54.064129
3033.071471	118.101922	54.069133
3032.782465	110.466792	54.074138
3032.145468	110.840534	54.079143
3030.792368	108.712494	54.084148
3030.827761	104.393693	54.089153
3029.752666	108.147343	54.094157
3029.455073	103.924125	54.099162
3028.859963	109.072431	54.104167
3027.520171	109.284034	54.109172
3027.304530	114.247503	54.114177
3026.808690	113.418865	54.119181
3026.267060	106.096108	54.124186
3025.489517	114.294461	54.129191
3024.935572	110.983050	54.134196
3024.283793	104.484360	54.139201
3023.603311	109.238712	54.144205
3023.150694	106.271953	54.149210
3022.738756	108.425351	54.154215
3021.236260	116.532061	54.159220
3020.399454	102.047294	54.164225
3019.399543	113.430800	54.169229
3019.570553	102.265577	54.174234
3019.521520	108.635407	54.179239
3017.993390	112.798043	54.184244
3017.259657	109.698535	54.189249
3016.540119	116.356227	54.194253
3016.043102	109.373997	54.199258
3015.165754	108.158194	54.204263
3015.063605	113.602783	54.209268
3014.321958	110.626203	54.214273
3013.495103	110.741476	54.219277
3013.127828	108.425249	54.224282
3012.601567	106.363553	54.229287
3011.792979	106.002426	54.234292
3011.090459	109.047431	54.239297
3010.251035	102.015165	54.244301
3009.837139	101.965927	54.249306
3008.597179	104.151871	54.254311
3007.823751	108.663560	54.259316
3008.301899	101.491806	54.264321
3006.632818	109.166335	54.269325
3005.694189	102.042867	54.274330
3005.544124	108.948236	54.279335
3005.222754	106.130363	54.284340
3004.600355	106.661478	54.289345
3003.331677	107.313290	54.294349
3002.868539	105.867240	54.299354
3002.256139	103.469353	54.304359
3001.417866	104.029856	54.309364
3001.097650	100.287732	54.314369
3000.526188	113.527450	54.319373
3000.457796	105.117279	54.324378
2999.400835	101.180136	54.329383
2998.078462	109.978812	54.334388
2997.360619	95.615042	54.339393
2997.062096	105.900559	54.344397
2996.605292	103.020174	54.349402
2995.681915	115.023352	54.354407
2994.682622	113.775891	54.359412
2994.149078	109.638388	54.364417
2993.579025	106.120530	54.369421
2992.915493	102.122080	54.374426
2992.407345	112.095668	54.379431
2991.656517	108.345023	54.384436
2991.591748	96.079337	54.389441
2990.639524	102.011805	54.394445
2990.316018	105.234802	54.399450
2989.698595	107.087401	54.404455
2988.595251	110.191428	54.409460
2987.726143	102.047163	54.414465
2986.499700	115.218416	54.419469
2985.929684	108.423135	54.424474
2986.207329	109.016365	54.429479
2985.326247	111.217960	54.434484
2985.136339	110.470466	54.439489
2983.958824	107.646924	54.444493
2983.468008	111.742438	54.449498
2982.666719	109.130126	54.454503
2981.968974	105.097261	54.459508
2981.232963	99.304931	54.464513
2980.152006	110.882677	54.469517
2979.786670	104.095842	54.474522
2978.954679	108.468335	54.479527
2978.271156	113.183738	54.484532
2978.219729	107.406260	54.489537
2977.294566	113.293058	54.494541
2976.414038	101.693335	54.499546
2976.194547	102.969133	54.504551
2975.611170	107.674132	54.509556
2975.127408	104.856776	54.514561
2974.263169	103.263355	54.519565
2973.210276	95.655358	54.524570
2972.519818	96.258893	54.529575
2971.383903	106.536326	54.534580
2971.406124	98.070809	54.539585
2970.402420	110.691248	54.544589
2969.923841	104.274283	54.549594
2969.460193	109.091056	54.554599
2968.586213	112.365492	54.559604
2968.052469	105.221394	54.564609
2967.647467	112.015595	54.569613
2967.328152	102.759382	54.574618
2967.027456	109.894564	54.579623
2965.100091	113.089278	54.584628
2964.845112	108.743522	54.589633
2963.872234	110.356085	54.594637
2963.212064	105.160254	54.599642
2962.661740	115.997607	54.604647
2961.927371	109.129760	54.609652
2961.807303	108.885055	54.614657
2960.892168	106.041945	54.619661
2960.679292	105.134565	54.624666
2959.099855	112.365902	54.629671
2958.143070	126.422641	54.634676
2958.315267	113.217658	54.639681
2957.652703	112.002265	54.644685
2956.771672	115.134226	54.649690
2955.819274	112.307352	54.654695
2955.290514	115.404772	54.659700
2955.021880	101.656990	54.664705
2954.453483	106.545346	54.669709
2953.800955	110.326661	54.674714
2953.367589	109.196046	54.679719
2952.375737	104.812404	54.684724
2951.182496	103.002058	54.689729
2950.396197	111.730053	54.694733
2950.062569	106.626049	54.699738
2949.291318	105.908429	54.704743
2948.524248	106.183621	54.709748
2948.807001	105.467458	54.714753
2947.759294	116.900980	54.719757
2947.616249	110.470097	54.724762
2946.809072	111.791853	54.729767
2945.691848	108.295666	54.734772
2944.888527	112.250380	54.739777
2943.986942	114.548640	54.744781
2943.461269	103.414455	54.749786
2942.758937	108.170967	54.754791
2942.269366	116.881809	54.759796
2941.971153	101.107821	54.764801
2941.245729	107.331924	54.769805
2940.912901	102.342257	54.774810
2939.469407	104.019457	54.779815
2938.371619	108.894864	54.784820
2938.343568	101.404625	54.789825
2937.416717	105.250188	54.794829
2936.929521	101.920279	54.799834
2936.221418	102.435258	54.804839
2935.835454	107.986762	54.809844
2935.822933	98.612210	54.814849
2934.898533	103.967971	54.819853
2934.117299	101.703942	54.824858
2933.111874	99.642038	54.829863
2932.089383	108.962222	54.834868
2931.601550	100.108227	54.839873
2930.612025	104.082918	54.844877
2930.230109	102.052221	54.849882
2929.672580	106.368341	54.854887
2929.413964	102.558856	54.859892
2928.877044	101.365021	54.864897
2928.448427	111.024628	54.869901
2927.141119	106.015970	54.874906
2926.377593	98.937597	54.879911
2926.074146	106.589943	54.884916
2925.428329	94.323304	54.889921
2924.552884	108.250867	54.894925
2924.094124	109.892416	54.899930
2922.949151	97.535819	54.904935
2921.898784	112.393648	54.909940
2921.901529	102.023749	54.914945
2920.995878	111.780667	54.919949
2920.428593	103.740755	54.924954
2920.022776	106.710194	54.929959
2918.983464	110.211436	54.934964
2918.785456	98.399965	54.939969
2918.006281	105.644149	54.944973
2917.786333	101.852530	54.949978
2917.146288	97.807449	54.954983
2915.535067	102.951384	54.959988
2915.123662	101.546238	54.964993
2914.460754	113.441353	54.969997
2913.902409	99.859140	54.975002
2913.340556	107.215787	54.980007
2912.620430	108.014658	54.985012
2912.545800	94.460703	54.990017
2911.581542	100.652202	54.995021
2910.243495	108.542145	55.000026
2909.555540	108.130024	55.005031
2908.887229	99.925017	55.010036
2908.283309	97.001497	55.015041
2907.996919	112.698609	55.020045
2907.527405	98.473208	55.025050
2907.062411	105.064111	55.030055
2906.360834	109.198409	55.035060
2906.038553	98.406835	55.040065
2904.558719	109.646578	55.045069
2903.844739	99.553900	55.050074
2903.295823	108.018702	55.055079
2902.425224	110.031415	55.060084
2902.413163	100.940594	55.065089
2901.614168	105.606657	55.070093
2901.318128	99.814940	55.075098
2900.273934	97.195604	55.080103
2898.948950	99.728852	55.085108
2898.735109	89.809651	55.090113
2898.023256	97.354160	55.095117
2897.363947	95.095748	55.100122
2896.893176	91.274764	55.105127
2896.505870	97.510554	55.110132
2895.801162	92.777469	55.115137
2894.553879	98.360514	55.120141
2893.934942	98.081859	55.125146
2893.847722	101.662359	55.130151
2892.994478	104.941942	55.135156
2892.648693	100.672897	55.140161
2891.753535	102.381922	55.145165
2891.001793	99.624584	55.150170
2890.211869	98.099791	55.155175
2889.155351	107.735258	55.160180
2888.313928	98.340531	55.165185
2887.721189	100.865087	55.170189
2887.522833	98.742236	55.175194
2887.088899	100.647168	55.180199
2886.351610	106.606467	55.185204
2886.458519	98.839755	55.190209
2885.191398	107.722947	55.195213
2883.765913	107.302665	55.200218
2883.510510	101.971755	55.205223
2882.788411	100.067882	55.210228
2882.451024	95.955294	55.215233
2881.921053	106.717320	55.220237
2881.262210	102.208101	55.225242
2880.304968	103.534591	55.230247
2878.950922	102.145680	55.235252
2878.469048	90.159714	55.240257
2878.129573	104.026858	55.245261
2877.949515	99.413711	55.250266
2877.394193	98.493809	55.255271
2876.181558	99.751449	55.260276
2876.031652	93.708979	55.265281
2875.344636	106.536604	55.270285
2873.962221	98.723638	55.275290
2873.145009	94.883707	55.280295
2872.676920	105.473714	55.285300
2872.984128	92.267789	55.290305
2871.952391	103.053989	55.295309
2871.359202	99.826279	55.300314
2870.868350	98.056172	55.305319
2869.401211	99.408623	55.310324
2868.600808	94.695054	55.315329
2867.826074	100.716803	55.320333
2868.078423	92.203680	55.325338
2867.214712	93.453004	55.330343
2866.360103	98.163308	55.335348
2866.384607	96.311047	55.340353
2865.482848	102.835677	55.345357
2864.653653	95.080534	55.350362
2863.554541	98.038990	55.355367
2862.647098	105.060763	55.360372
2862.497266	89.973925	55.365377
2861.646470	100.977483	55.370381
2861.377469	96.446247	55.375386
2861.255862	95.861554	55.380391
2860.056008	94.986677	55.385396
2858.824002	88.665343	55.390401
2857.823278	89.340074	55.395405
2857.305990	96.603051	55.400410
2857.122543	88.369667	55.405415
2856.107438	99.621167	55.410420
2856.316035	95.233303	55.415425
2855.421021	98.602919	55.420429
2854.899758	93.514814	55.425434
2854.604621	91.507188	55.430439
2853.238021	98.835977	55.435444
2852.559054	90.802145	55.440449
2851.797042	94.072454	55.445453
2851.098849	90.775461	55.450458
2850.949395	93.350570	55.455463
2850.245910	87.827834	55.460468
2848.892094	87.869379	55.465473
2847.769862	100.127976	55.470477
2847.977295	90.657427	55.475482
2847.337562	86.484416	55.480487
2846.248546	101.623571	55.485492
2846.062127	89.124104	55.490497
2845.564633	93.120894	55.495501
2845.105751	99.944824	55.500506
2844.992357	96.365521	55.505511
2843.463457	95.614776	55.510516
2842.822720	91.196022	55.515521
2841.924540	101.734008	55.520525
2841.225929	94.405751	55.525530
2840.803686	92.904177	55.530535
2839.696818	103.913213	55.535540
2839.253725	87.322467	55.540545
2838.657264	100.264080	55.545549
2837.782848	99.549502	55.550554
2837.780104	85.785524	55.555559
2836.823518	95.386542	55.560564
2836.655166	93.102255	55.565569
2835.129710	98.455358	55.570573
2834.456165	90.760857	55.575578
2833.762098	94.806244	55.580583
2833.173031	95.106685	55.585588
2833.288469	85.598179	55.590593
2832.553751	100.819278	55.595597
2831.779861	90.973303	55.600602
2830.879882	97.155402	55.605607
2829.825328	95.349802	55.610612
2829.137218	90.070356	55.615617
2828.841641	94.155397	55.620621
2828.354873	97.745762	55.625626
2828.237690	85.121577	55.630631
2826.662128	94.272609	55.635636
2825.707398	88.129284	55.640641
2824.896681	87.930386	55.645645
2824.335371	99.241300	55.650650
2824.613254	97.499282	55.655655
2823.335179	101.626327	55.660660
2823.311861	95.614330	55.665665
2823.060863	100.320552	55.670669
2821.622608	95.699429	55.675674
2821.009312	89.989183	55.680679
2820.191450	101.458415	55.685684
2819.765066	88.407877	55.690689
2819.323767	97.958328	55.695693
2818.142009	101.284197	55.700698
2817.600174	96.939328	55.705703
2816.877294	92.685402	55.710708
2816.168318	87.861091	55.715713
2815.590841	95.241325	55.720717
2814.955564	96.513981	55.725722
2814.629102	88.712402	55.730727
2813.577388	92.657868	55.735732
2812.390149	97.835147	55.740737
2811.828649	90.294391	55.745741
2811.519548	93.117043	55.750746
2810.932292	98.744395	55.755751
2810.540077	98.035432	55.760756
2810.359456	85.587876	55.765761
2809.496676	93.782244	55.770765
2808.455787	87.223398	55.775770
2807.582410	85.464995	55.780775
2806.795192	93.036992	55.785780
2806.652814	93.399244	55.790785
2805.808757	96.995414	55.795789
2805.331186	94.706349	55.800794
2804.034399	94.196199	55.805799
2803.289573	94.644445	55.810804
2802.990846	89.900804	55.815809
2802.078502	89.483628	55.820813
2801.436076	87.018667	55.825818
2801.453392	90.353539	55.830823
2800.655142	102.481376	55.835828
2800.547814	86.661783	55.840833
2799.343062	92.960708	55.845837
2798.648231	93.148575	55.850842
2798.260024	89.006395	55.855847
2797.004919	89.164499	55.860852
2796.059083	86.192464	55.865857
2795.289206	93.581504	55.870861
2794.680669	90.055255	55.875866
2794.387254	85.414521	55.880871
2793.808007	96.711919	55.885876
2793.415413	88.822570	55.890881
2792.790694	94.536453	55.895885
2792.349178	98.652755	55.900890
2791.951437	87.182152	55.905895
2790.396572	90.459691	55.910900
2789.624915	92.286564	55.915905
2789.515967	95.843933	55.920909
2788.830582	95.921637	55.925914
2787.768423	99.965601	55.930919
2786.834309	93.611923	55.935924
2785.933866	92.353924	55.940929
2785.937243	93.388351	55.945933
2784.964225	98.833354	55.950938
2784.753012	99.276055	55.955943
2784.224320	97.762681	55.960948
2784.146261	94.203789	55.965953
2783.118147	96.790529	55.970957
2781.861536	94.336994	55.975962
2781.887189	89.753038	55.980967
2780.336935	95.760503	55.985972
2779.402948	92.520401	55.990977
2778.522713	92.080373	55.995981
2778.546101	93.530183	56.000986
2778.342357	96.326145	56.005991
2777.311544	93.616525	56.010996
2777.308373	89.449194	56.016001
2776.657474	89.539163	56.021005
2775.013423	99.829644	56.026010
2774.806064	90.220396	56.031015
2773.702438	94.440786	56.036020
2773.300304	92.612896	56.041025
2773.019784	93.688740	56.046029
2772.435401	96.763702	56.051034
2771.446197	85.694188	56.056039
2769.904289	89.587657	56.061044
2769.813065	83.057159	56.066049
2769.232400	90.431226	56.071053
2768.413105	97.405964	56.076058
2768.417236	88.680675	56.081063
2767.736148	97.969355	56.086068
2767.306428	88.849286	56.091073
2766.207940	87.138445	56.096077
2765.053994	98.567622	56.101082
2764.762880	95.223958	56.106087
2764.238983	90.268945	56.111092
2763.721408	86.307562	56.116097
2762.862051	88.811776	56.121101
2761.708217	84.330346	56.126106
2761.260524	84.251377	56.131111
2760.416605	96.228335	56.136116
2760.299271	92.191831	56.141121
2759.636608	84.826267	56.146125
2759.154857	86.439781	56.151130
2758.648044	86.678804	56.156135
2757.444303	91.835622	56.161140
2757.050346	87.426017	56.166145
2756.208668	90.018787	56.171149
2755.724334	100.924975	56.176154
2755.100791	85.690189	56.181159
2753.639401	102.736756	56.186164
2753.231754	89.650267	56.191169
2752.444648	87.302407	56.196173
2751.774891	93.651998	56.201178
2751.846288	86.255703	56.206183
2750.928747	91.799775	56.211188
2750.837463	89.112727	56.216193
2750.225994	93.653987	56.221197
2749.049997	92.299018	56.226202
2748.339455	91.198430	56.231207
2747.976241	92.753001	56.236212
2747.060236	97.134742	56.241217
2745.891356	92.179056	56.246221
2744.967583	94.036672	56.251226
2744.448976	93.992720	56.256231
2744.327703	96.427228	56.261236
2743.620376	90.968717	56.266241
2743.291166	94.506893	56.271245
2742.957433	95.955771	56.276250
2742.669186	92.870559	56.281255
2740.947052	96.548927	56.286260
2740.288166	92.177896	56.291265
2739.872044	93.926637	56.296269
2738.929636	97.075822	56.301274
2738.261165	85.776239	56.306279
2736.980528	98.052838	56.311284
2736.759445	91.254412	56.316289
2736.408747	92.899210	56.321293
2735.851384	99.260382	56.326298
2735.597620	91.255735	56.331303
2735.099063	92.247274	56.336308
2734.265944	85.267288	56.341313
2733.360612	84.629852	56.346317
2732.492560	89.619562	56.351322
2731.998950	78.738899	56.356327
2730.380658	91.864237	56.361332
2729.959476	86.679706	56.366337
2729.605635	89.041863	56.371341
2728.865260	90.493539	56.376346
2728.668265	89.806081	56.381351
2727.924172	98.034247	56.386356
2727.693855	82.808440	56.391361
2726.613462	93.848083	56.396365
2725.892028	99.783760	56.401370
2725.604843	92.039819	56.406375
2724.665452	95.922679	56.411380
2724.020085	102.366787	56.416385
2723.098008	94.496110	56.421389
2722.211725	93.851473	56.426394
2721.903183	88.725450	56.431399
2721.164845	94.287842	56.436404
2720.816236	84.031321	56.441409
2720.191593	88.193134	56.446413
2718.998535	91.015701	56.451418
2718.605187	85.964569	56.456423
2717.684148	89.078919	56.461428
2717.504276	84.574307	56.466433
2717.136857	84.945029	56.471437
2715.551871	92.823519	56.476442
2714.956339	91.592359	56.481447
2714.091754	92.265160	56.486452
2713.887775	98.768816	56.491457
2713.075323	93.613667	56.496461
2712.502181	91.631465	56.501466
2712.176167	80.815313	56.506471
2711.811767	96.134941	56.511476
2710.715196	85.653781	56.516481
2710.006986	81.882091	56.521485
2708.968720	90.526841	56.526490
2708.700275	79.623484	56.531495
2707.939740	93.210086	56.536500
2708.029801	92.297515	56.541505
2707.016609	86.537621	56.546509
2706.082154	92.669572	56.551514
2705.428444	85.023813	56.556519
2704.790565	79.566864	56.561524
2704.035326	80.437284	56.566529
2702.915509	86.063697	56.571533
2702.122678	94.486897	56.576538
2701.718001	77.393067	56.581543
2701.660711	98.984878	56.586548
2700.826282	83.316039	56.591553
2701.080457	83.908527	56.596557
2699.508265	92.592835	56.601562
2698.458486	82.191312	56.606567
2697.732925	91.286281	56.611572
2697.710193	87.013749	56.616577
2696.913541	82.728248	56.621581
2696.553655	87.025195	56.626586
2695.641319	75.648896	56.631591
2694.399337	92.522167	56.636596
2693.913018	82.446292	56.641601
2693.617556	87.641674	56.646605
2692.951338	88.770424	56.651610
2692.362427	84.115081	56.656615
2690.950332	89.759484	56.661620
2690.533529	83.760683	56.666625
2689.754738	90.166806	56.671629
2689.075610	85.196894	56.676634
2689.065942	83.238772	56.681639
2688.279586	89.900391	56.686644
2688.201824	85.139124	56.691649
2687.277576	85.856468	56.696653
2686.269981	89.334949	56.701658
2685.710021	90.419091	56.706663
2684.951134	95.790793	56.711668
2684.633737	97.831732	56.716673
2683.432313	85.867363	56.721677
2682.066337	96.174271	56.726682
2682.460374	77.745137	56.731687
2681.685187	86.217422	56.736692
2681.435885	87.490033	56.741697
2680.772564	76.491159	56.746701
2679.334709	85.699198	56.751706
2678.800097	87.415698	56.756711
2678.347890	91.051475	56.761716
2677.733785	83.190932	56.766721
2677.116328	85.449340	56.771725
2676.202426	88.937465	56.776730
2675.717054	74.084477	56.781735
2674.621112	85.064803	56.786740
2673.938614	78.453417	56.791745
2673.768128	84.169392	56.796749
2673.028820	79.288322	56.801754
2672.909192	72.958081	56.806759
2671.787357	85.326343	56.811764
2671.126552	78.854929	56.816769
2670.718827	83.382678	56.821773
2670.013948	92.013470	56.826778
2668.735626	81.144590	56.831783
2667.832507	86.068854	56.836788
2667.165409	81.678321	56.841793
2666.735861	78.328728	56.846797
2666.125175	91.671430	56.851802
2666.108263	84.113400	56.856807
2665.398086	83.406697	56.861812
2665.142217	83.284289	56.866817
2664.130969	84.507546	56.871821
2663.093331	85.093491	56.876826
2662.738648	88.102353	56.881831
2661.961455	100.218300	56.886836
2660.771310	87.954781	56.891841
2660.440476	78.562052	56.896845
2659.586171	83.855329	56.901850
2659.389023	83.506574	56.906855
2658.732710	83.783397	56.911860
2658.191426	81.392349	56.916865
2656.726427	81.925037	56.921869
2656.051606	91.243037	56.926874
2655.761889	81.644732	56.931879
2655.326680	82.360587	56.936884
2654.886598	80.709717	56.941889
2654.283283	77.251676	56.946893
2652.862890	88.737454	56.951898
2652.381907	80.324442	56.956903
2651.822314	89.288017	56.961908
2651.195152	84.112262	56.966913
2650.940797	87.900134	56.971917
2650.010730	87.465487	56.976922
2649.243953	83.226202	56.981927
2648.511884	91.569545	56.986932
2647.797694	87.290876	56.991937
2647.541967	84.876673	56.996941
2647.118026	79.596314	57.001946
2645.999822	83.761977	57.006951
2644.737669	78.048212	57.011956
2644.641739	82.478454	57.016961
2644.074303	84.022151	57.021965
2643.633127	86.505026	57.026970
2643.060380	85.861673	57.031975
2641.750941	85.197414	57.036980
2641.384515	86.719382	57.041985
2640.953749	83.026194	57.046989
2639.886832	91.761504	57.051994
2638.966738	92.384596	57.056999
2638.187802	90.222063	57.062004
2637.536537	87.183522	57.067009
2637.147604	87.070046	57.072013
2636.500166	96.275609	57.077018
2636.362496	84.819000	57.082023
2635.727846	86.840358	57.087028
2635.445670	89.424734	57.092033
2634.352963	80.408159	57.097037
2633.375675	85.017878	57.102042
2633.177317	80.531829	57.107047
2631.866292	88.057984	57.112052
2631.008899	84.569959	57.117057
2630.349265	77.512582	57.122061
2629.467882	96.245735	57.127066
2629.517331	82.067093	57.132071
2629.002116	83.686731	57.137076
2628.761055	89.149121	57.142081
2627.775197	90.699217	57.147085
2626.679543	88.652010	57.152090
2626.227524	80.975738	57.157095
2625.248337	87.549539	57.162100
2625.209246	79.969254	57.167105
2624.244365	80.960782	57.172109
2623.062981	82.423912	57.177114
2622.458069	82.999443	57.182119
2621.963578	98.093810	57.187124
2621.391210	92.098714	57.192129
2621.261654	89.650313	57.197133
2620.532929	88.861526	57.202138
2620.049622	87.342780	57.207143
2618.949196	92.267624	57.212148
2618.386741	88.163541	57.217153
2617.586561	85.007175	57.222157
2616.239288	86.683790	57.227162
2615.800957	87.552941	57.232167
2615.192515	83.111732	57.237172
2615.229240	86.582221	57.242177
2614.696191	90.259451	57.247181
2614.052191	95.182058	57.252186
2613.723797	81.728384	57.257191
2612.738390	85.798327	57.262196
2611.952451	88.558423	57.267201
2610.663453	90.222710	57.272205
2609.692877	95.404822	57.277210
2609.205599	84.669936	57.282215
2608.979706	95.458912	57.287220
2608.443993	80.614145	57.292225
2607.882467	91.396548	57.297229
2606.910810	92.388054	57.302234
2605.980055	92.178525	57.307239
2605.123683	89.429648	57.312244
2604.526330	90.496505	57.317249
2604.252012	75.069445	57.322253
2603.865472	82.803867	57.327258
2603.459472	78.595678	57.332263
2602.864952	86.751696	57.337268
2601.905844	89.237458	57.342273
2601.444281	88.799306	57.347277
2600.959822	86.336973	57.352282
2600.157307	82.440112	57.357287
2599.266455	92.493706	57.362292
2598.077968	86.265268	57.367297
2598.125903	86.231056	57.372301
2596.412006	91.391033	57.377306
2595.979508	84.626005	57.382311
2595.396218	87.823550	57.387316
2594.595648	86.214969	57.392321
2594.006092	85.265030	57.397325
2593.585250	84.242436	57.402330
2593.147268	88.721679	57.407335
2592.705128	89.428461	57.412340
2592.362418	87.812660	57.417345
2591.612730	80.285567	57.422349
2590.476522	88.819574	57.427354
2589.823593	87.083916	57.432359
2589.141227	83.978070	57.437364
2588.752303	86.271626	57.442369
2587.791105	75.461852	57.447373
2586.340219	84.008600	57.452378
2586.369423	77.096755	57.457383
2585.804672	90.751327	57.462388
2585.510679	93.642058	57.467393
2585.227997	81.994335	57.472397
2583.943945	91.219913	57.477402
2583.185519	83.985226	57.482407
2582.617475	88.508018	57.487412
2582.339171	88.753780	57.492417
2581.113807	79.915026	57.497421
2579.855861	86.827002	57.502426
2579.540359	83.169378	57.507431
2578.751446	81.543018	57.512436
2578.236192	77.739944	57.517441
2578.291527	79.320468	57.522445
2577.591986	75.007337	57.527450
2577.502070	72.811498	57.532455
2576.158014	81.895360	57.537460
2575.261671	77.530218	57.542465
2574.906834	80.202013	57.547469
2573.982788	78.344554	57.552474
2573.197619	73.841201	57.557479
2572.461718	73.640208	57.562484
2571.806125	81.068926	57.567489
2571.757658	78.128655	57.572493
2570.652076	83.157801	57.577498
2569.943196	74.194838	57.582503
2569.086336	76.813513	57.587508
2568.421219	79.521379	57.592513
2568.147906	76.297452	57.597517
2567.554547	79.934073	57.602522
2566.944578	74.626321	57.607527
2565.660008	73.122593	57.612532
2564.966743	79.350684	57.617537
2564.396151	76.120738	57.622541
2564.243131	73.545700	57.627546
2563.923744	72.079068	57.632551
2563.330813	77.360036	57.637556
2562.307262	76.912966	57.642561
2561.444468	73.954021	57.647565
2560.803530	78.565060	57.652570
2560.370263	73.086580	57.657575
2559.085756	76.914775	57.662580
2558.348642	84.480585	57.667585
2558.046832	74.102024	57.672589
2557.337817	81.331855	57.677594
2557.025217	75.447099	57.682599
2556.436856	80.982674	57.687604
2555.567336	78.183953	57.692609
2555.225373	75.535824	57.697613
2554.171466	82.976192	57.702618
2554.134999	78.266295	57.707623
2552.867087	77.640746	57.712628
2551.767058	79.942981	57.717633
2551.235874	72.936686	57.722637
2550.639474	80.283839	57.727642
2550.557203	76.269383	57.732647
2550.139083	75.650525	57.737652
2548.969515	71.590645	57.742657
2548.447328	70.292891	57.747661
2547.441388	82.913311	57.752666
2546.882419	79.854269	57.757671
2546.058577	75.316481	57.762676
2545.234355	72.009904	57.767681
2544.623720	71.556191	57.772685
2544.025973	78.050180	57.777690
2543.821563	72.641916	57.782695
2543.458953	70.935972	57.787700
2542.236674	81.673440	57.792705
2541.559358	76.206684	57.797709
2540.869407	87.126693	57.802714
2540.437199	79.462838	57.807719
2539.630612	79.519058	57.812724
2538.997143	70.648603	57.817729
2537.884451	74.878072	57.822733
2536.781944	75.216191	57.827738
2536.455020	73.057319	57.832743
2536.324628	83.981528	57.837748
2535.824485	81.979765	57.842753
2535.716026	73.478223	57.847757
2534.798744	85.531270	57.852762
2534.101370	71.354017	57.857767
2533.237519	74.736498	57.862772
2532.496958	79.715875	57.867777
2531.648118	73.356766	57.872781
2530.686423	78.024223	57.877786
2530.039995	67.721165	57.882791
2529.204522	79.290895	57.887796
2528.983372	73.936018	57.892801
2528.867543	67.835661	57.897805
2528.198388	89.540314	57.902810
2527.339114	79.692440	57.907815
2526.418738	83.340368	57.912820
2525.635839	81.375105	57.917825
2525.644474	71.674900	57.922829
2524.004347	78.416570	57.927834
2523.507511	74.539699	57.932839
2522.662941	80.284467	57.937844
2522.035699	81.714850	57.942849
2521.828118	73.838525	57.947853
2521.589464	83.486152	57.952858
2521.548908	72.801626	57.957863
2519.979245	79.691113	57.962868
2518.688295	76.961291	57.967873
2518.543949	73.478880	57.972877
2518.239371	87.691315	57.977882
2517.276776	74.822525	57.982887
2516.282324	76.613705	57.987892
2515.389927	82.281390	57.992897
2515.263610	71.624553	57.997901
2514.910554	76.798594	58.002906
2514.207993	78.385929	58.007911
2512.675543	79.811209	58.012916
2512.182407	76.054887	58.017921
2511.929524	73.989540	58.022925
2511.701541	75.120357	58.027930
2511.115698	74.611885	58.032935
2509.933918	71.876032	58.037940
2508.996426	76.087000	58.042945
2508.694788	75.797167	58.047949
2508.089357	86.957322	58.052954
2507.213668	81.170419	58.057959
2505.930380	82.550339	58.062964
2505.247632	77.226619	58.067969
2505.088588	73.944479	58.072973
2504.288417	77.657513	58.077978
2504.094971	73.401550	58.082983
2503.876790	80.317343	58.087988
2503.211884	83.046495	58.092993
2502.321509	80.058723	58.097997
2501.414621	78.389390	58.103002
2500.838801	73.622899	58.108007
2500.271261	81.156955	58.113012
2498.973778	80.568447	58.118017
2498.602972	66.565895	58.123021
2498.242610	78.633456	58.128026
2497.815247	73.517910	58.133031
2497.162568	80.161420	58.138036
2495.690687	83.876011	58.143041
2495.510819	74.161458	58.148045
2494.735124	79.008297	58.153050
2494.264299	80.164055	58.158055
2492.929560	78.442350	58.163060
2491.663406	75.275678	58.168065
2492.327716	76.096052	58.173069
2491.273241	78.421297	58.178074
2490.941314	76.165393	58.183079
2490.508055	77.086183	58.188084
2489.481701	83.744636	58.193089
2488.648631	70.179130	58.198093
2487.804568	81.233637	58.203098
2487.305434	72.211940	58.208103
2486.967558	77.356545	58.213108
2486.571017	85.494505	58.218113
2485.980683	73.235875	58.223117
2484.622965	87.257320	58.228122
2484.406591	75.068959	58.233127
2483.808958	79.235640	58.238132
2482.735558	87.899048	58.243137
2481.541389	73.674117	58.248141
2480.871134	79.266326	58.253146
2480.342061	80.724534	58.258151
2480.296778	79.166440	58.263156
2479.860502	84.045643	58.268161
2479.661916	71.540833	58.273165
2478.269914	85.943917	58.278170
2477.545392	79.441987	58.283175
2477.155013	80.546888	58.288180
2476.209996	88.930592	58.293185
2475.966027	85.120225	58.298189
2474.453505	80.029953	58.303194
2473.982960	87.006263	58.308199
2473.371957	86.153556	58.313204
2472.905849	82.514586	58.318209
2472.739341	73.211424	58.323213
2471.940589	82.770472	58.328218
2470.794125	70.238653	58.333223
2470.547258	82.683508	58.338228
2470.058589	78.817483	58.343233
2469.072895	75.826675	58.348237
2467.533471	82.517984	58.353242
2467.061792	69.157531	58.358247
2466.719504	77.468573	58.363252
2466.088211	79.468452	58.368257
2466.251583	76.736301	58.373261
2465.302662	81.050674	58.378266
2464.213822	78.033292	58.383271
2463.375718	85.413880	58.388276
2462.772092	85.285809	58.393281
2462.453396	80.430362	58.398285
2461.901113	77.681626	58.403290
2461.459949	72.657652	58.408295
2460.538944	82.116028	58.413300
2459.380797	79.598375	58.418305
2459.157246	74.756662	58.423309
2458.421196	76.902736	58.428314
2458.102544	77.997348	58.433319
2457.031701	80.243295	58.438324
2456.292496	76.303665	58.443329
2455.990284	67.594085	58.448333
2455.538334	76.010715	58.453338
2454.387410	77.204205	58.458343
2453.694233	75.135986	58.463348
2453.141387	79.122517	58.468353
2452.837813	74.756708	58.473357
2451.559807	79.072086	58.478362
2450.888778	74.791996	58.483367
2450.381332	73.804353	58.488372
2449.268506	76.899424	58.493377
2448.965712	73.958039	58.498381
2448.651311	81.785515	58.503386
2448.405983	83.984659	58.508391
2447.147920	76.634123	58.513396
2445.936988	74.182734	58.518401
2445.856128	76.054556	58.523405
2445.334447	78.797907	58.528410
2444.934316	75.620936	58.533415
2444.381266	82.390305	58.538420
2443.505339	78.217088	58.543425
2442.982860	73.411487	58.548429
2441.991035	80.731913	58.553434
2441.061087	80.505301	58.558439
2440.324472	75.982225	58.563444
2439.414973	75.952242	58.568449
2439.428615	74.898400	58.573453
2438.772102	87.486320	58.578458
2438.187541	79.854451	58.583463
2437.216601	76.507059	58.588468
2436.471975	79.925219	58.593473
2436.056239	80.128172	58.598477
2435.573113	80.984468	58.603482
2434.541456	81.835475	58.608487
2433.658521	74.550669	58.613492
2432.894506	76.848760	58.618497
2432.577479	71.325950	58.623501
2431.795235	79.660112	58.628506
2431.632491	76.884250	58.633511
2430.894655	79.136814	58.638516
2429.559588	82.473565	58.643521
2429.493422	70.208615	58.648525
2428.691962	78.297387	58.653530
2428.366049	79.593761	58.658535
2427.984580	82.119331	58.663540
2426.639875	78.989000	58.668545
2425.891641	74.461992	58.673549
2425.198670	74.833527	58.678554
2424.771117	75.610851	58.683559
2423.988414	69.594131	58.688564
2423.090660	74.934329	58.693569
2422.507971	60.643169	58.698573
2421.832165	74.956160	58.703578
2421.574782	72.098589	58.708583
2420.965245	73.171888	58.713588
2420.178118	76.964802	58.718593
2419.240475	75.085224	58.723597
2418.515606	77.564907	58.728602
2417.876490	76.561097	58.733607
2417.969068	75.204821	58.738612
2417.166270	79.712102	58.743617
2416.601859	69.081241	58.748621
2415.386033	77.745713	58.753626
2414.947198	71.140875	58.758631
2414.385378	62.924494	58.763636
2412.892373	72.335016	58.768641
2412.429929	66.777471	58.773645
2411.730108	63.967921	58.778650
2411.463717	72.668599	58.783655
2411.147595	70.048828	58.788660
2410.456185	76.089511	58.793665
2410.247158	64.422923	58.798669
2409.033324	76.949026	58.803674
2408.342543	77.016253	58.808679
2407.572912	71.581886	58.813684
2406.306277	78.275509	58.818689
2405.832911	68.677075	58.823693
2405.318999	70.849907	58.828698
2404.585365	66.725790	58.833703
2404.319841	67.474621	58.838708
2403.877906	62.358820	58.843713
2403.644655	65.821380	58.848717
2402.780988	73.218574	58.853722
2401.919842	73.717548	58.858727
2401.568838	68.790269	58.863732
2399.689181	75.210565	58.868737
2399.430249	67.442510	58.873741
2398.397148	75.643912	58.878746
2398.089037	62.217225	58.883751
2397.693232	69.188643	58.888756
2397.155470	77.181013	58.893761
2396.369491	68.509950	58.898765
2395.357338	74.534030	58.903770
2394.665658	68.573199	58.908775
2394.479481	69.864627	58.913780
2394.059510	68.345736	58.918785
2393.874742	68.316180	58.923789
2392.642713	78.054704	58.928794
2391.574417	69.527042	58.933799
2390.940092	66.268943	58.938804
2390.403233	74.707195	58.943809
2389.247202	65.729948	58.948813
2389.088659	76.442643	58.953818
2388.612832	64.309722	58.958823
2388.380877	69.894487	58.963828
2387.723044	65.918459	58.968833
2386.468935	59.997750	58.973837
2385.575534	64.200796	58.978842
2385.062955	71.575853	58.983847
2384.088721	63.081454	58.988852
2382.930695	67.246068	58.993857
2382.993128	58.470602	58.998861
2381.823516	70.301139	59.003866
2381.579276	71.467896	59.008871
2381.207352	63.566801	59.013876
2380.830398	67.994953	59.018881
2380.068729	73.059657	59.023885
2379.289421	70.940653	59.028890
2378.314388	65.160113	59.033895
2377.767512	66.758341	59.038900
2377.174195	68.782126	59.043905
2377.045064	60.262434	59.048909
2375.765350	73.770032	59.053914
2374.987655	67.934039	59.058919
2374.497131	63.355479	59.063924
2373.700720	66.575267	59.068929
2373.456876	59.042656	59.073933
2372.777402	68.137241	59.078938
2371.511752	64.759735	59.083943
2371.247734	71.084168	59.088948
2370.182625	68.133802	59.093953
2369.908743	62.307189	59.098957
2369.519182	62.501723	59.103962
2368.886975	67.018124	59.108967
2368.086178	63.287591	59.113972
2367.291817	66.036519	59.118977
2366.906309	67.888198	59.123981
2365.661147	68.740989	59.128986
2364.630542	62.399976	59.133991
2364.265034	63.976665	59.138996
2363.844126	69.008365	59.144001
2363.779856	68.027054	59.149005
2363.371108	72.323280	59.154010
2362.617790	64.678054	59.159015
2361.966912	63.605214	59.164020
2360.245220	66.715596	59.169025
2359.268340	61.124056	59.174029
2359.131988	69.568424	59.179034
2359.130471	65.673196	59.184039
2358.194458	63.724671	59.189044
2357.327020	68.218535	59.194049
2356.857082	62.211507	59.199053
2355.435314	69.833209	59.204058
2355.150115	72.261400	59.209063
2354.656122	63.930803	59.214068
2353.707762	69.202689	59.219073
2353.911059	59.218180	59.224077
2353.285313	70.249563	59.229082
2352.129604	69.724872	59.234087
2351.542074	62.938244	59.239092
2350.664363	70.386787	59.244097
2350.390666	61.564987	59.249101
2349.132021	62.726392	59.254106
2347.913496	66.067307	59.259111
2347.926361	69.262001	59.264116
2347.082250	69.310850	59.269121
2346.978792	62.487632	59.274125
2346.251600	72.470612	59.279130
2346.054584	65.918381	59.284135
2345.773343	72.267468	59.289140
2344.769775	72.178984	59.294145
2343.185404	66.380282	59.299149
2341.771285	64.999417	59.304154
2341.284268	66.918979	59.309159
2341.693072	69.226920	59.314164
2340.764482	73.683088	59.319169
2340.167292	66.984162	59.324173
2339.570868	69.510964	59.329178
2339.041991	67.854784	59.334183
2338.655371	66.934121	59.339188
2337.187564	66.477406	59.344193
2336.955793	67.494405	59.349197
2336.598203	65.266193	59.354202
2335.509806	71.446206	59.359207
2334.668893	64.786983	59.364212
2334.405027	72.091881	59.369217
2333.578822	62.946942	59.374221
2333.303378	67.356158	59.379226
2332.464233	64.196247	59.384231
2332.064426	64.618318	59.389236
2330.999909	78.461744	59.394241
2331.322880	68.664391	59.399245
2329.536169	67.522893	59.404250
2328.522764	63.161246	59.409255
2328.349153	69.684158	59.414260
2327.995837	67.168646	59.419265
2326.718301	54.994422	59.424269
2325.931660	69.993438	59.429274
2324.830737	63.933265	59.434279
2324.586412	63.554303	59.439284
2324.157891	72.627690	59.444289
2323.722920	57.405805	59.449293
2323.293267	70.305825	59.454298
2322.843859	64.795010	59.459303
2322.006476	66.335554	59.464308
2321.005304	74.323485	59.469313
2320.660684	68.225165	59.474317
2319.955256	72.634885	59.479322
2319.192515	69.633615	59.484327
2318.385318	65.370520	59.489332
2318.084550	75.734910	59.494337
2317.191009	72.196684	59.499341
2315.984479	57.021478	59.504346
2315.583806	63.675579	59.509351
2315.082531	68.643262	59.514356
2314.520991	70.021774	59.519361
2314.045014	60.834715	59.524365
2312.896353	63.617393	59.529370
2311.502563	60.326156	59.534375
2311.551846	63.171212	59.539380
2311.234144	71.307522	59.544385
2310.632709	58.688882	59.549389
2310.199429	69.828664	59.554394
2309.012077	72.220869	59.559399
2308.305131	64.235369	59.564404
2307.460236	75.957102	59.569409
2307.309986	69.823178	59.574413
2307.125701	70.972185	59.579418
2306.283177	63.374199	59.584423
2305.297607	64.392605	59.589428
2304.319423	74.181673	59.594433
2304.263395	60.092975	59.599437
2302.790416	58.787316	59.604442
2301.661901	67.646464	59.609447
2301.628442	66.569890	59.614452
2300.964387	76.043147	59.619457
2300.370733	60.444599	59.624461
2299.889507	71.755995	59.629466
2299.445866	71.864654	59.634471
2299.180658	64.569380	59.639476
2297.818248	72.441460	59.644481
2297.129476	68.613232	59.649485
2296.880611	68.516090	59.654490
2295.953587	68.657675	59.659495
2295.500731	65.547763	59.664500
2294.548675	70.699108	59.669505
2293.804569	70.272590	59.674509
2293.253560	72.010080	59.679514
2293.002660	74.679504	59.684519
2292.294298	72.660089	59.689524
2291.472355	70.636018	59.694529
2290.639994	67.696394	59.699533
2289.974724	66.254195	59.704538
2288.775305	70.088811	59.709543
2288.467620	66.348964	59.714548
2287.707355	69.842834	59.719553
2287.285218	67.905916	59.724557
2286.608417	67.246846	59.729562
2286.253883	75.940489	59.734567
2286.092252	66.314822	59.739572
2284.466478	75.652154	59.744577
2283.869761	67.531365	59.749581
2283.399186	74.282290	59.754586
2282.886761	72.266078	59.759591
2282.451033	66.283999	59.764596
2281.445327	66.856263	59.769601
2281.162815	71.543784	59.774605
2280.401262	65.193096	59.779610
2279.163930	74.254010	59.784615
2278.153631	64.457301	59.789620
2277.691318	74.200783	59.794625
2277.616818	64.677452	59.799629
2277.269717	69.594693	59.804634
2276.612859	65.614175	59.809639
2275.372109	62.537558	59.814644
2274.599521	61.912632	59.819649
2274.067152	61.361096	59.824653
2273.521959	67.023108	59.829658
2273.094063	68.508633	59.834663
2272.480330	63.518935	59.839668
2271.062552	67.745750	59.844673
2270.307175	60.045243	59.849677
2269.815358	67.243071	59.854682
2269.344098	69.000870	59.859687
2269.239869	66.819333	59.864692
2268.199442	69.178526	59.869697
2267.306970	67.618873	59.874701
2266.950806	64.400854	59.879706
2266.330538	80.451783	59.884711
2266.134994	61.822373	59.889716
2264.961634	69.947512	59.894721
2264.413118	66.897776	59.899725
2263.900816	69.071133	59.904730
2262.548703	71.291793	59.909735
2261.958062	70.206295	59.914740
2260.869127	69.654811	59.919745
2260.473040	62.153775	59.924750
2260.334077	64.844317	59.929754
2259.772738	73.703977	59.934759
2259.826013	61.072462	59.939764
2258.466988	66.511292	59.944769
2257.736685	71.658271	59.949774
2257.273035	65.012705	59.954778
2256.477927	72.996191	59.959783
2255.387364	69.930603	59.964788
2254.464879	67.799001	59.969793
2254.157556	65.783244	59.974798
2253.428289	66.466917	59.979802
2253.130102	68.450111	59.984807
2252.891749	66.053494	59.989812
2251.619520	71.255650	59.994817
2250.923682	68.657015	59.999822
2250.464909	68.999969	60.004826
2250.129854	70.984336	60.009831
2249.545844	67.290169	60.014836
2248.438054	75.629487	60.019841
2247.454226	74.946745	60.024846
2247.051885	66.829432	60.029850
2246.166617	69.019599	60.034855
2245.364583	58.701778	60.039860
2244.392012	66.204049	60.044865
2244.236310	58.517440	60.049870
2243.961842	63.342131	60.054874
2243.424113	67.392794	60.059879
2242.955746	60.570809	60.064884
2241.918440	74.553260	60.069889
2241.111937	64.546848	60.074894
2240.713843	69.635436	60.079898
2240.031947	61.865134	60.084903
2239.189325	66.462526	60.089908
2237.974719	71.980081	60.094913
2237.911739	68.703636	60.099918
2237.117589	70.410476	60.104922
2236.745142	73.382914	60.109927
2236.137523	63.766818	60.114932
2235.054423	64.083915	60.119937
2234.374469	69.294124	60.124942
2234.103542	60.261480	60.129946
2233.416191	68.575471	60.134951
2232.396879	66.643189	60.139956
2231.062489	63.590886	60.144961
2230.888181	65.139226	60.149966
2230.267296	66.896170	60.154970
2229.910747	60.555572	60.159975
2230.057913	60.754245	60.164980
2228.687455	63.326194	60.169985
2228.140308	64.603966	60.174990
2227.518019	67.771493	60.179994
2226.643333	68.577930	60.184999
2225.862082	74.242422	60.190004
2224.563788	71.862475	60.195009
2224.061389	65.515635	60.200014
2223.871419	70.293115	60.205018
2223.451665	67.556484	60.210023
2223.387765	60.004960	60.215028
2222.124530	68.741505	60.220033
2221.294334	64.196583	60.225038
2220.620764	64.265626	60.230042
2220.135369	65.573494	60.235047
2220.035425	62.615597	60.240052
2218.881244	72.592264	60.245057
2218.128329	65.287646	60.250062
2217.239675	73.702775	60.255066
2215.852243	73.919165	60.260071
2215.654894	66.216389	60.265076
2214.896160	60.370874	60.270081
2214.101849	60.927129	60.275086
2214.193173	54.106930	60.280090
2213.710743	67.403977	60.285095
2213.590994	58.382982	60.290100
2212.261663	62.377585	60.295105
2211.264071	66.052175	60.300110
2210.815518	63.216265	60.305114
2209.975054	69.925845	60.310119
2209.609674	58.703650	60.315124
2208.711790	68.761611	60.320129
2208.122768	62.071576	60.325134
2207.425747	65.480035	60.330138
2206.918969	68.025463	60.335143
2206.210967	63.596220	60.340148
2205.056517	69.405455	60.345153
2204.318459	58.157001	60.350158
2204.372359	63.771028	60.355162
2203.600738	69.980169	60.360167
2203.442493	57.037483	60.365172
2201.857191	71.700209	60.370177
2201.450243	70.790928	60.375182
2200.894097	64.746168	60.380186
2200.248087	67.023709	60.385191
2199.469745	68.770085	60.390196
2198.471506	68.743873	60.395201
2197.939006	61.338016	60.400206
2197.674196	64.923996	60.405210
2196.922488	66.294384	60.410215
2196.554356	55.714878	60.415220
2195.386886	64.397942	60.420225
2194.942762	61.958761	60.425230
2194.130294	53.919104	60.430234
2193.733580	66.305471	60.435239
2193.403743	49.024144	60.440244
2191.754125	65.933175	60.445249
2191.380915	65.413242	60.450254
2191.091438	53.942030	60.455258
2190.676815	62.023067	60.460263
2189.769994	65.975810	60.465268
2188.537776	65.583446	60.470273
2188.193382	63.157998	60.475278
2187.513856	67.890522	60.480282
2187.213088	72.075921	60.485287
2186.722163	57.169945	60.490292
2185.289027	68.691106	60.495297
2184.689679	62.275595	60.500302
2184.234831	60.156000	60.505306
2183.767380	66.028921	60.510311
2183.604747	55.628212	60.515316
2182.455037	67.107610	60.520321
2181.808907	68.931242	60.525326
2181.111032	63.889637	60.530330
2179.884341	74.256458	60.535335
2179.127581	62.314126	60.540340
2178.713295	63.034331	60.545345
2178.132407	62.155984	60.550350
2177.882516	65.226669	60.555354
2177.643726	70.850098	60.560359
2177.156630	66.633728	60.565364
2176.092793	65.425888	60.570369
2175.451510	62.939115	60.575374
2174.020812	63.437247	60.580378
2173.098928	71.530836	60.585383
2172.945547	70.711607	60.590388
2171.631959	68.222583	60.595393
2171.279689	73.966865	60.600398
2171.181220	61.356182	60.605402
2170.475676	67.669677	60.610407
2170.366945	59.991226	60.615412
2169.673317	74.111078	60.620417
2168.356278	65.862069	60.625422
2167.968832	59.911224	60.630426
2167.373372	61.466463	60.635431
2166.618031	57.906215	60.640436
2165.840196	63.793142	60.645441
2164.875518	67.001469	60.650446
2164.870696	63.825604	60.655450
2163.729890	66.523285	60.660455
2163.270777	66.079228	60.665460
2162.267267	65.332766	60.670465
2161.957510	66.988349	60.675470
2161.971226	60.202344	60.680474
2160.160842	70.509525	60.685479
2159.488251	67.560757	60.690484
2158.653134	61.406224	60.695489
2158.451844	71.354919	60.700494
2158.089051	59.122198	60.705498
2157.678210	65.795012	60.710503
2156.968855	55.671358	60.715508
2156.343038	62.995125	60.720513
2155.965822	64.274628	60.725518
2154.758361	60.012920	60.730522
2153.353865	67.810906	60.735527
2153.162642	62.272933	60.740532
2152.219655	69.588188	60.745537
2151.792949	64.172985	60.750542
2151.742606	63.594677	60.755546
2150.487283	75.242535	60.760551
2149.727276	66.293154	60.765556
2149.291261	72.072284	60.770561
2148.971690	64.479627	60.775566
2148.733562	63.076100	60.780570
2147.188944	65.570885	60.785575
2146.487680	61.642588	60.790580
2145.789955	68.403942	60.795585
2145.108547	71.921838	60.800590
2144.664244	64.504457	60.805594
2143.600095	64.694388	60.810599
2142.888631	54.524521	60.815604
2142.380682	58.780877	60.820609
2141.759026	54.443850	60.825614
2141.472383	57.840544	60.830618
2140.859254	69.923675	60.835623
2140.737560	57.925238	60.840628
2139.958535	61.157077	60.845633
2138.973295	59.737652	60.850638
2138.823571	61.767296	60.855642
2136.915624	66.260336	60.860647
2136.651908	66.210740	60.865652
2135.695900	69.877835	60.870657
2135.652863	61.558964	60.875662
2134.724493	65.498032	60.880666
2133.796619	66.664883	60.885671
2133.043573	60.559474	60.890676
2132.114884	73.834168	60.895681
2132.340093	59.638979	60.900686
2131.852825	64.774002	60.905690
2131.006255	68.378566	60.910695
2130.738373	60.147098	60.915700
2129.100764	62.355040	60.920705
2128.870408	65.420805	60.925710
2128.523653	64.387555	60.930714
2127.704545	65.705140	60.935719
2126.879820	62.980944	60.940724
2125.978761	71.062291	60.945729
2125.411630	62.471493	60.950734
2124.962231	59.523636	60.955738
2124.435730	65.625334	60.960743
2123.243436	66.239803	60.965748
2122.565067	67.058466	60.970753
2122.337329	65.682373	60.975758
2121.607796	59.187697	60.980762
2121.198638	67.805808	60.985767
2120.445685	57.178848	60.990772
2119.665066	62.869289	60.995777
2118.978179	61.704354	61.000782
2118.750995	61.035903	61.005786
2117.609041	68.728599	61.010791
2116.932951	67.664050	61.015796
2115.592022	65.298530	61.020801
2115.596171	66.197425	61.025806
2115.566473	55.176380	61.030810
2114.216565	64.566815	61.035815
2113.658310	61.379430	61.040820
2112.823071	50.125918	61.045825
2112.480887	60.118436	61.050830
2112.107057	59.639666	61.055834
2110.641786	68.762479	61.060839
2110.211198	66.454802	61.065844
2109.631213	61.692641	61.070849
2109.258481	68.875629	61.075854
2108.857173	57.697888	61.080858
2107.612811	61.837446	61.085863
2106.821291	59.817285	61.090868
2106.108225	55.930881	61.095873
2105.773667	62.407891	61.100878
2105.664561	65.079906	61.105882
2104.240189	64.083346	61.110887
2103.583739	62.826763	61.115892
2103.189690	58.007934	61.120897
2102.486094	58.752365	61.125902
2102.009870	52.536463	61.130906
2100.615183	67.695523	61.135911
2099.930743	61.144193	61.140916
2099.727486	64.038751	61.145921
2099.327635	60.245217	61.150926
2099.099892	52.518451	61.155930
2097.738236	65.382870	61.160935
2097.328260	54.414240	61.165940
2096.394162	63.264233	61.170945
2095.897993	63.795167	61.175950
2095.429554	59.662853	61.180954
2093.935544	65.453211	61.185959
2093.495710	59.631331	61.190964
2092.778887	61.028132	61.195969
2092.221625	65.424369	61.200974
2091.886115	61.147744	61.205978
2091.417320	60.243919	61.210983
2091.164613	56.247595	61.215988
2089.879086	63.305270	61.220993
2088.927055	63.573136	61.225998
2088.931833	64.327850	61.231002
2087.867462	64.519014	61.236007
2087.168041	60.806325	61.241012
2086.213279	66.933908	61.246017
2085.585964	59.704152	61.251022
2085.868694	61.975606	61.256026
2084.934360	62.275576	61.261031
2084.383202	64.749659	61.266036
2083.344491	61.828396	61.271041
2082.411102	53.828790	61.276046
2081.640619	52.256991	61.281050
2080.798192	65.559160	61.286055
2080.346153	56.322660	61.291060
2079.996686	51.836856	61.296065
2079.119275	59.664692	61.301070
2079.195507	58.768300	61.306074
2078.211658	57.422068	61.311079
2077.490014	59.324939	61.316084
2076.941260	59.162264	61.321089
2076.068036	58.480374	61.326094
2075.586045	56.891204	61.331098
2073.974880	54.346138	61.336103
2073.686215	53.912407	61.341108
2073.353158	60.469287	61.346113
2072.855975	58.821534	61.351118
2072.332031	54.949366	61.356122
2071.257345	65.484002	61.361127
2070.725387	63.067358	61.366132
2069.909348	61.410593	61.371137
2069.380744	67.286082	61.376142
2069.328165	61.541646	61.381146
2068.150961	67.927929	61.386151
2067.338147	64.561467	61.391156
2066.992831	63.381929	61.396161
2066.119962	65.148043	61.401166
2065.716717	56.479888	61.406170
2064.565074	64.349898	61.411175
2064.433437	66.685911	61.416180
2063.830273	58.373255	61.421185
2062.680240	61.229631	61.426190
2061.856106	59.173610	61.431194
2061.278650	59.958441	61.436199
2060.977068	53.042437	61.441204
2060.292874	53.223839	61.446209
2059.115355	64.383147	61.451214
2058.483897	52.309296	61.456218
2057.615968	63.904708	61.461223
2057.219585	57.665682	61.466228
2056.840640	54.085676	61.471233
2056.168603	62.277055	61.476238
2056.226551	61.203402	61.481242
2055.370391	68.347900	61.486247
2054.412855	59.884288	61.491252
2053.718698	61.264980	61.496257
2052.732099	61.047338	61.501262
2051.898448	56.791190	61.506266
2050.936694	69.326304	61.511271
2050.752807	63.038298	61.516276
2050.464279	64.314083	61.521281
2049.645773	55.351845	61.526286
2049.378587	56.046107	61.531290
2048.091153	62.532953	61.536295
2047.353699	59.485961	61.541300
2047.245235	54.917491	61.546305
2046.801915	55.515965	61.551310
2046.242636	53.938834	61.556314
2045.374482	57.777220	61.561319
2043.996860	60.588058	61.566324
2042.939571	54.076440	61.571329
2042.796481	62.044323	61.576334
2042.115733	53.216017	61.581338
2041.134047	59.819505	61.586343
2040.689092	49.714602	61.591348
2040.296391	59.982590	61.596353
2039.869378	58.494936	61.601358
2039.575814	48.797937	61.606362
2038.443040	63.551029	61.611367
2037.847963	64.578078	61.616372
2037.469158	67.973567	61.621377
2036.282439	66.154037	61.626382
2035.527874	50.711777	61.631386
2034.879327	59.468326	61.636391
2034.066045	62.454993	61.641396
2033.846010	67.630754	61.646401
2033.490863	64.270090	61.651406
2032.520573	60.236257	61.656410
2031.547852	60.784767	61.661415
2031.050096	53.773249	61.666420
2030.451891	54.551764	61.671425
2030.033556	63.357354	61.676430
2029.109028	64.120639	61.681434
2027.803327	64.074027	61.686439
2027.505903	56.446815	61.691444
2027.248928	63.341589	61.696449
2026.632451	67.770063	61.701454
2026.403480	61.958306	61.706458
2025.011049	72.594669	61.711463
2024.366154	58.377809	61.716468
2023.976112	60.536189	61.721473
2023.281998	63.560103	61.726478
2022.453726	56.776824	61.731482
2021.465521	60.617592	61.736487
2020.916673	62.786558	61.741492
2020.535885	65.756482	61.746497
2020.207370	60.468971	61.751502
2019.828606	59.158190	61.756506
2018.862471	68.291162	61.761511
2017.887963	60.235447	61.766516
2017.558744	56.749961	61.771521
2016.083580	68.930809	61.776526
2015.605881	62.448338	61.781530
2014.536870	69.809241	61.786535
2014.392864	59.921269	61.791540
2014.010168	64.748288	61.796545
2013.831930	65.425759	61.801550
2013.462454	62.047812	61.806554
2011.752721	68.255601	61.811559
2011.628791	60.345302	61.816564
2010.384054	67.559428	61.821569
2009.445017	60.245251	61.826574
2008.922466	58.337381	61.831578
2008.181370	62.498630	61.836583
2008.141521	57.011750	61.841588
2007.942242	58.400160	61.846593
2006.674452	67.862616	61.851598
2005.652731	60.093654	61.856602
2004.879961	67.482433	61.861607
2004.712094	58.613768	61.866612
2004.271221	65.293298	61.871617
2003.662103	63.785089	61.876622
2002.388581	58.250300	61.881626
2001.680136	64.238261	61.886631
2001.193092	59.581399	61.891636
2000.927815	60.887945	61.896641
2000.302887	65.132347	61.901646
1999.667795	63.966857	61.906650
1998.775370	58.585950	61.911655
1998.437468	60.534104	61.916660
1997.948489	58.579047	61.921665
1996.986923	58.933426	61.926670
1995.951405	55.710071	61.931674
1994.927743	64.249748	61.936679
1994.605826	63.205550	61.941684
1994.282444	54.502433	61.946689
1993.177740	60.577123	61.951694
1992.389335	57.886212	61.956698
1991.903084	56.112260	61.961703
1991.414863	60.888649	61.966708
1991.248827	56.309899	61.971713
1990.156890	57.075380	61.976718
1989.297787	52.044816	61.981722
1988.379636	58.997032	61.986727
1987.823422	57.977519	61.991732
1987.496934	65.496396	61.996737
1987.156397	61.347348	62.001742
1986.829695	53.888567	62.006746
1985.603123	63.139112	62.011751
1984.997831	62.728760	62.016756
1984.516814	59.449631	62.021761
1983.444123	68.199796	62.026766
1982.835388	56.984145	62.031770
1981.537480	58.005116	62.036775
1981.261422	65.646809	62.041780
1981.002383	54.953159	62.046785
1980.539171	71.677036	62.051790
1980.003137	65.217574	62.056794
1978.634317	75.818724	62.061799
1978.318500	67.111940	62.066804
1978.005688	71.990953	62.071809
1976.915134	77.498385	62.076814
1975.923336	70.221262	62.081818
1975.322637	80.550104	62.086823
1974.820042	72.757865	62.091828
1974.757772	66.357092	62.096833
1973.774139	77.654954	62.101838
1972.950867	63.466643	62.106842
1972.343603	73.312280	62.111847
1971.739063	68.911957	62.116852
1971.313423	65.013116	62.121857
1969.706368	71.679781	62.126862
1969.427230	58.996225	62.131866
1968.839652	67.612093	62.136871
1968.381092	63.889798	62.141876
1968.220664	61.128570	62.146881
1967.213724	60.346814	62.151886
1966.997438	57.288049	62.156890
1965.734586	57.742129	62.161895
1965.024462	61.058117	62.166900
1964.105538	72.596739	62.171905
1963.479010	65.524364	62.176910
1963.478389	58.989500	62.181914
1962.791042	69.828137	62.186919
1962.012641	71.359036	62.191924
1960.792011	61.972993	62.196929
1960.368790	73.312349	62.201934
1959.931002	66.403864	62.206938
1959.262762	64.828409	62.211943
1958.167278	63.640239	62.216948
1957.715283	65.879481	62.221953
1957.112654	63.674670	62.226958
1956.889635	59.661831	62.231962
1955.725717	70.294637	62.236967
1954.387347	66.517990	62.241972
1954.109524	65.074688	62.246977
1953.380284	70.056515	62.251982
1953.100877	62.999758	62.256986
1952.917006	66.875436	62.261991
1952.475666	65.943640	62.266996
1951.771778	61.180990	62.272001
1949.954478	65.254386	62.277006
1950.086373	59.197755	62.282010
1949.424496	70.135058	62.287015
1948.285284	64.693750	62.292020
1947.418799	71.300834	62.297025
1946.608342	72.359606	62.302030
1946.531282	70.815647	62.307034
1946.284193	62.653275	62.312039
1945.775891	65.003199	62.317044
1944.508019	63.888731	62.322049
1943.501555	64.925773	62.327054
1943.349125	69.264212	62.332058
1942.691626	72.550282	62.337063
1942.352560	67.995212	62.342068
1941.176102	77.929539	62.347073
1940.212749	72.688663	62.352078
1939.998891	68.752017	62.357082
1939.246670	70.911968	62.362087
1939.115006	63.786520	62.367092
1937.986925	70.152578	62.372097
1936.924404	73.769636	62.377102
1936.933510	62.212650	62.382106
1936.408225	73.091063	62.387111
1935.301495	75.138772	62.392116
1934.452973	64.333607	62.397121
1933.788729	75.782877	62.402126
1933.873623	69.605210	62.407130
1932.784629	61.722650	62.412135
1932.057208	70.307576	62.417140
1931.629849	66.317853	62.422145
1930.662283	70.125107	62.427150
1929.986256	67.472215	62.432154
1928.933433	65.529941	62.437159
1928.217359	70.542279	62.442164
1927.792498	65.937549	62.447169
1927.462251	70.970723	62.452174
1926.950730	70.343028	62.457178
1926.222206	72.132231	62.462183
1925.288889	73.952522	62.467188
1924.433447	71.353217	62.472193
1923.742272	69.102375	62.477198
1923.289196	65.009689	62.482202
1922.709045	70.521781	62.487207
1922.410071	67.927539	62.492212
1921.794383	69.492184	62.497217
1920.457649	75.827234	62.502222
1920.079029	66.184662	62.507226
1919.631213	66.197360	62.512231
1919.137449	68.159946	62.517236
1918.090020	56.922652	62.522241
1917.527069	65.294711	62.527246
1916.827255	56.097867	62.532250
1916.192420	61.852196	62.537255
1915.940197	61.287903	62.542260
1914.892398	66.503038	62.547265
1914.077272	63.515933	62.552270
1914.304727	56.063408	62.557274
1912.504669	58.923255	62.562279
1911.812796	64.675897	62.567284
1911.840052	61.071808	62.572289
1910.810708	66.444832	62.577294
1910.534294	61.994308	62.582298
1909.314407	60.490339	62.587303
1908.348571	56.912466	62.592308
1908.015871	57.376373	62.597313
1907.643611	65.979878	62.602318
1907.176604	59.177846	62.607322
1906.789042	61.102922	62.612327
1905.659051	60.538406	62.617332
1905.045975	65.755747	62.622337
1904.437381	62.890806	62.627342
1903.731797	65.263036	62.632346
1902.631029	58.246150	62.637351
1901.774168	66.127723	62.642356
1901.564835	62.120047	62.647361
1901.126489	72.535183	62.652366
1900.932882	61.049195	62.657370
1899.570781	64.360681	62.662375
1899.036283	60.460737	62.667380
1898.361253	64.644641	62.672385
1897.652883	65.607800	62.677390
1897.115523	61.843341	62.682394
1895.926589	65.450847	62.687399
1895.358144	67.273849	62.692404
1895.160896	54.192239	62.697409
1894.403000	70.322336	62.702414
1894.226467	59.604320	62.707418
1893.119260	65.423676	62.712423
1892.069268	64.036693	62.717428
1891.831802	61.962832	62.722433
1891.247304	64.737489	62.727438
1890.813521	65.928399	62.732442
1889.570279	61.320399	62.737447
1888.915211	67.198189	62.742452
1888.602915	69.575767	62.747457
1888.001664	67.562563	62.752462
1887.305511	52.015622	62.757466
1886.129480	64.332013	62.762471
1885.707341	65.216601	62.767476
1885.596884	48.517138	62.772481
1884.106089	66.275315	62.777486
1883.478127	54.337482	62.782490
1882.635749	63.634413	62.787495
1882.279002	65.317387	62.792500
1881.804993	66.388080	62.797505
1881.480471	67.723712	62.802510
1881.092412	57.937904	62.807514
1880.348981	59.600983	62.812519
1879.870154	58.834679	62.817524
1878.366856	59.755424	62.822529
1877.237978	69.497673	62.827534
1876.641310	63.832913	62.832538
1875.895701	68.336777	62.837543
1875.555276	64.974400	62.842548
1875.499660	61.896047	62.847553
1875.099352	64.781294	62.852558
1874.451781	50.392052	62.857562
1873.147322	63.524198	62.862567
1872.303611	61.073681	62.867572
1871.779084	64.113595	62.872577
1871.343143	65.568549	62.877582
1870.678208	62.213535	62.882586
1869.923631	65.612925	62.887591
1869.118457	62.005994	62.892596
1869.002105	58.705938	62.897601
1868.256997	63.790349	62.902606
1867.081127	61.799669	62.907610
1866.373925	71.610695	62.912615
1865.714370	61.992515	62.917620
1865.648106	56.360564	62.922625
1864.856652	70.107947	62.927630
1863.948497	56.517991	62.932634
1863.538010	58.679481	62.937639
1863.087982	56.745406	62.942644
1862.129715	47.968966	62.947649
1861.062621	68.307969	62.952654
1860.430259	66.311144	62.957658
1859.948280	62.952461	62.962663
1859.190653	66.831960	62.967668
1858.944265	60.293363	62.972673
1858.033854	69.263268	62.977678
1857.014575	66.467805	62.982682
1856.653509	62.146238	62.987687
1856.217972	52.441189	62.992692
1856.222038	57.097439	62.997697
1854.696782	63.659347	63.002702
1854.184911	51.158526	63.007706
1853.290480	60.630146	63.012711
1852.570845	60.147008	63.017716
1852.484508	62.117653	63.022721
1851.016491	66.311709	63.027726
1850.491341	65.935818	63.032730
1849.977008	64.871262	63.037735
1849.474265	68.255595	63.042740
1849.255916	61.975480	63.047745
1847.839229	64.169783	63.052750
1847.182709	55.474738	63.057754
1846.810755	52.547612	63.062759
1845.763731	62.594790	63.067764
1846.044278	47.962300	63.072769
1844.846133	68.201755	63.077774
1844.215159	61.758561	63.082778
1843.523295	59.706001	63.087783
1842.985668	61.597942	63.092788
1842.843784	57.442554	63.097793
1841.360900	65.182167	63.102798
1841.007508	61.577286	63.107802
1840.274253	61.736716	63.112807
1839.417564	57.732438	63.117812
1838.855402	56.039778	63.122817
1838.040915	52.991793	63.127822
1837.805373	58.382561	63.132826
1837.035246	64.101624	63.137831
1836.119013	62.796764	63.142836
1835.308388	62.492216	63.147841
1834.484560	62.536491	63.152846
1834.107126	55.976505	63.157850
1833.975091	62.070324	63.162855
1833.241720	66.572492	63.167860
1832.674044	61.207505	63.172865
1831.561569	70.218694	63.177870
1831.023188	61.978681	63.182874
1830.419465	58.045593	63.187879
1829.405748	55.750482	63.192884
1829.057268	59.907336	63.197889
1828.363495	65.321638	63.202894
1827.868857	58.496322	63.207898
1827.097409	67.654813	63.212903
1825.836666	72.893369	63.217908
1825.423130	60.828074	63.222913
1824.507201	68.613579	63.227918
1824.263877	58.272514	63.232922
1824.041033	61.235947	63.237927
1823.394630	63.794632	63.242932
1822.864778	65.241184	63.247937
1821.557823	55.916932	63.252942
1821.151755	59.654183	63.257946
1820.772316	59.490592	63.262951
1819.505338	62.955550	63.267956
1818.754465	62.713410	63.272961
1817.833437	60.273763	63.277966
1817.747637	64.934732	63.282970
1817.187641	64.790586	63.287975
1816.784870	56.548691	63.292980
1815.952312	60.439435	63.297985
1814.893144	64.389475	63.302990
1814.460216	66.819272	63.307994
1814.261928	60.625331	63.312999
1813.112612	73.239126	63.318004
1812.593232	58.256011	63.323009
1811.701535	60.931266	63.328014
1811.397219	65.448050	63.333018
1810.774642	66.758500	63.338023
1809.498265	64.867922	63.343028
1808.872375	62.146869	63.348033
1808.216721	64.038481	63.353038
1808.038494	59.978520	63.358042
1807.784273	57.566100	63.363047
1806.807773	69.769419	63.368052
1805.909961	61.568803	63.373057
1805.519627	59.354137	63.378062
1804.356494	60.180387	63.383066
1803.360800	59.306348	63.388071
1802.825591	70.169482	63.393076
1802.464944	64.401592	63.398081
1802.000982	65.277158	63.403086
1801.781186	64.189450	63.408090
1800.961430	58.287360	63.413095
1800.036503	65.853758	63.418100
1799.646465	65.959602	63.423105
1798.484321	65.263248	63.428110
1797.480213	61.046184	63.433114
1796.760843	62.994881	63.438119
1796.094059	65.191939	63.443124
1795.731753	62.847746	63.448129
1795.178610	72.684123	63.453134
1794.748355	64.822704	63.458138
1794.694942	69.486026	63.463143
1793.631020	62.663384	63.468148
1792.867716	59.290083	63.473153
1792.114528	66.155678	63.478158
1791.570725	52.797476	63.483162
1790.532822	54.342403	63.488167
1789.473392	57.008071	63.493172
1789.251215	56.758368	63.498177
1788.712300	61.123061	63.503182
1788.285667	54.024813	63.508186
1787.483891	53.568370	63.513191
1786.627186	59.824858	63.518196
1786.337490	57.740995	63.523201
1785.728672	60.049315	63.528206
1783.966844	59.594116	63.533210
1783.605074	60.314836	63.538215
1782.998942	59.051662	63.543220
1782.687114	59.530952	63.548225
1781.998694	62.475366	63.553230
1781.859343	56.291081	63.558234
1781.212517	60.844363	63.563239
1779.938165	64.806360	63.568244
1779.228638	55.865015	63.573249
1778.755280	60.471113	63.578254
1778.536166	58.066898	63.583258
1777.732484	54.778270	63.588263
1776.887793	59.884858	63.593268
1776.347693	57.039005	63.598273
1775.598265	61.463006	63.603278
1774.364843	59.437594	63.608282
1773.833493	59.480386	63.613287
1773.345923	61.658229	63.618292
1773.134774	57.588905	63.623297
1772.448050	69.864219	63.628302
1771.874053	58.667541	63.633306
1770.846040	63.632215	63.638311
1769.796124	53.993620	63.643316
1769.625237	55.085874	63.648321
1768.781671	60.241610	63.653326
1768.219496	56.222875	63.658330
1767.115390	58.509366	63.663335
1766.674431	61.343943	63.668340
1766.582673	59.052932	63.673345
1765.922939	60.273037	63.678350
1765.337284	55.853732	63.683354
1764.732720	51.535948	63.688359
1763.409603	50.903460	63.693364
1763.224450	49.234325	63.698369
1761.929713	57.862639	63.703374
1761.567328	53.070410	63.708378
1760.817344	47.831761	63.713383
1759.990628	57.116938	63.718388
1760.110877	49.544218	63.723393
1759.192337	56.553361	63.728398
1758.574203	58.189095	63.733402
1757.900504	58.654518	63.738407
1756.928121	59.351039	63.743412
1756.287668	55.430170	63.748417
1755.227668	59.010113	63.753422
1754.872935	51.337883	63.758426
1754.470729	53.526382	63.763431
1754.021126	55.794830	63.768436
1753.375762	52.738055	63.773441
1752.086285	58.352179	63.778446
1751.490496	68.300846	63.783450
1751.213212	63.507474	63.788455
1750.124492	58.404938	63.793460
1749.611003	52.679001	63.798465
1748.318493	63.008182	63.803470
1748.079973	63.374672	63.808474
1747.766341	59.236441	63.813479
1747.301817	57.289070	63.818484
1746.612210	52.604541	63.823489
1746.161228	56.587099	63.828494
1745.101183	53.045119	63.833498
1744.414426	57.924564	63.838503
1743.556439	60.841550	63.843508
1743.567729	50.341284	63.848513
1742.695378	57.155823	63.853518
1741.674442	57.989334	63.858522
1741.275262	56.323270	63.863527
1740.793478	56.009836	63.868532
1740.008730	48.824064	63.873537
1739.049247	59.955172	63.878542
1738.339232	55.591096	63.883546
1737.740697	56.383908	63.888551
1737.069185	56.601075	63.893556
1736.052015	55.817958	63.898561
1735.420913	59.670687	63.903566
1734.750514	55.183786	63.908570
1734.385714	59.589739	63.913575
1733.785230	63.798399	63.918580
1733.928244	49.808768	63.923585
1733.315256	49.677646	63.928590
1732.081845	51.496026	63.933594
1731.692642	51.805803	63.938599
1730.360868	56.154196	63.943604
1729.743908	55.953889	63.948609
1728.989610	61.489865	63.953614
1728.855713	46.902252	63.958618
1728.421411	50.904850	63.963623
1727.053463	56.730159	63.968628
1726.199656	45.147188	63.973633
1725.244288	59.813886	63.978638
1724.528352	60.094311	63.983642
1724.438872	54.949877	63.988647
1724.092852	59.837332	63.993652
1723.771740	50.841384	63.998657
1723.064945	56.847630	64.003662
1722.021409	57.682643	64.008666
1721.557232	58.055774	64.013671
1720.730533	60.865967	64.018676
1720.170387	56.378753	64.023681
1719.226720	54.858752	64.028686
1718.590838	53.022018	64.033690
1718.500749	54.222021	64.038695
1717.530671	51.777763	64.043700
1716.651232	48.818677	64.048705
1715.669732	51.970738	64.053710
1715.070830	53.348985	64.058714
1714.947625	57.224540	64.063719
1714.060327	57.214961	64.068724
1713.720349	58.759684	64.073729
1712.435261	56.925489	64.078734
1712.205746	54.956066	64.083738
1711.667873	52.740999	64.088743
1710.653422	57.954006	64.093748
1710.075875	55.298905	64.098753
1709.321374	55.279629	64.103758
1709.149151	46.634771	64.108762
1708.675155	45.197425	64.113767
1706.772741	57.738773	64.118772
1706.509560	57.550167	64.123777
1706.040034	49.269982	64.128782
1705.608440	49.978972	64.133786
1705.220150	47.615158	64.138791
1704.247586	56.520311	64.143796
1703.517387	41.585947	64.148801
1702.969051	51.743974	64.153806
1702.421986	48.216460	64.158810
1701.586466	39.984304	64.163815
1700.393402	51.205901	64.168820
1700.031647	50.574708	64.173825
1699.728900	50.966400	64.178830
1699.262893	59.411866	64.183834
1698.311883	55.717429	64.188839
1697.251271	60.643482	64.193844
1696.859146	50.615655	64.198849
1696.539799	51.993434	64.203854
1695.768549	56.898392	64.208858
1694.837132	56.934653	64.213863
1694.256670	55.779594	64.218868
1693.509068	48.072762	64.223873
1692.912996	56.386147	64.228878
1692.247859	52.809367	64.233882
1691.344891	43.641031	64.238887
1690.921811	55.269272	64.243892
1690.422427	52.554222	64.248897
1689.998599	61.357982	64.253902
1688.792243	52.288528	64.258906
1687.985763	49.383670	64.263911
1687.035173	56.135422	64.268916
1686.786592	46.399207	64.273921
1686.568158	51.618497	64.278926
1686.068703	43.974992	64.283930
1685.418420	49.901703	64.288935
1684.313257	52.472983	64.293940
1684.023928	49.671071	64.298945
1682.785415	55.754492	64.303950
1682.243953	53.083747	64.308954
1681.778294	50.193987	64.313959
1680.872319	57.463477	64.318964
1680.598078	52.341978	64.323969
1679.905735	51.776041	64.328974
1679.052716	50.243694	64.333978
1678.125815	41.422470	64.338983
1677.977860	53.125203	64.343988
1677.543695	49.420090	64.348993
1676.337857	51.774925	64.353998
1675.350759	45.098643	64.359002
1675.036994	38.762651	64.364007
1674.297452	45.757747	64.369012
1674.254213	43.058983	64.374017
1673.057479	42.282134	64.379022
1672.320987	50.125751	64.384026
1671.911899	50.237233	64.389031
1671.383682	60.932590	64.394036
1670.838293	49.227384	64.399041
1669.680987	56.120296	64.404046
1668.489935	55.751405	64.409050
1668.141988	51.996014	64.414055
1667.496714	54.510705	64.419060
1667.337073	48.687917	64.424065
1666.745742	58.513848	64.429070
1665.629206	51.162641	64.434074
1665.096989	49.110421	64.439079
1664.200890	49.904821	64.444084
1664.086237	43.337001	64.449089
1663.379418	53.318869	64.454094
1663.094833	45.926744	64.459098
1662.118681	44.313634	64.464103
1661.437410	53.345777	64.469108
1660.621853	48.935044	64.474113
1659.403113	45.098546	64.479118
1658.666811	47.400271	64.484122
1658.500623	41.728206	64.489127
1658.011939	57.892737	64.494132
1657.799506	45.744130	64.499137
1656.585596	56.483008	64.504142
1655.632081	53.036500	64.509146
1655.228245	49.490403	64.514151
1654.097495	59.093260	64.519156
1654.172633	51.186833	64.524161
1653.853093	52.403601	64.529166
1652.719347	46.512650	64.534170
1651.937294	44.702124	64.539175
1651.443524	51.825290	64.544180
1650.694532	47.537768	64.549185
1649.627889	47.464157	64.554190
1648.851401	51.871879	64.559194
1648.598267	44.465690	64.564199
1647.850547	50.473022	64.569204
1648.040548	48.246297	64.574209
1647.214801	53.544646	64.579214
1645.885819	47.021215	64.584218
1645.279767	51.771991	64.589223
1644.505758	61.947723	64.594228
1644.484284	50.206944	64.599233
1643.214814	62.737100	64.604238
1642.746344	53.061410	64.609242
1642.264495	46.201180	64.614247
1641.479702	60.812640	64.619252
1640.693875	56.507737	64.624257
1639.858205	58.786998	64.629262
1639.125963	55.214999	64.634266
1638.923959	48.919090	64.639271
1638.112902	56.430488	64.644276
1637.588444	49.368742	64.649281
1636.708825	53.762142	64.654286
1635.827625	49.970120	64.659290
1635.702514	53.821921	64.664295
1635.501205	52.418441	64.669300
1634.694174	48.961869	64.674305
1633.476621	51.020309	64.679310
1632.857148	60.571201	64.684314
1631.673254	57.069783	64.689319
1630.709498	63.273557	64.694324
1630.869119	51.163515	64.699329
1629.922592	52.039573	64.704334
1629.191529	54.055418	64.709338
1628.760623	45.263795	64.714343
1628.031821	52.185220	64.719348
1628.025917	55.367308	64.724353
1627.084100	55.876261	64.729358
1626.108805	54.546025	64.734362
1625.550176	53.690382	64.739367
1624.761172	52.766800	64.744372
1624.469002	49.925907	64.749377
1623.698247	57.118975	64.754382
1623.028974	58.852681	64.759386
1622.445851	45.705721	64.764391
1621.543057	59.097954	64.769396
1620.829571	53.562966	64.774401
1620.352709	55.800958	64.779406
1619.507357	54.502957	64.784410
1619.079051	54.292483	64.789415
1618.498822	58.518209	64.794420
1617.599845	48.740550	64.799425
1616.940844	48.397852	64.804430
1616.178849	46.609162	64.809434
1616.023322	41.976546	64.814439
1614.821676	58.141115	64.819444
1614.102408	51.790839	64.824449
1613.554883	47.944877	64.829454
1612.662021	41.140388	64.834458
1612.437730	48.858461	64.839463
1611.998848	51.564800	64.844468
1610.911063	45.396797	64.849473
1610.524135	49.028545	64.854478
1609.953092	56.669784	64.859482
1609.637113	50.100106	64.864487
1608.398569	53.081050	64.869492
1607.527608	49.070976	64.874497
1607.058185	55.423433	64.879502
1606.749505	52.710493	64.884506
1606.065679	49.436124	64.889511
1604.861467	58.110547	64.894516
1604.361998	46.665515	64.899521
1603.929978	48.598609	64.904526
1602.952771	52.189670	64.909530
1602.300927	42.981936	64.914535
1601.246598	51.156648	64.919540
1600.966076	45.491128	64.924545
1600.441524	52.005380	64.929550
1599.771823	41.181565	64.934554
1599.498902	41.215673	64.939559
1598.127545	49.278462	64.944564
1597.799406	47.669726	64.949569
1597.161237	38.859900	64.954574
1596.745730	43.131247	64.959578
1595.895840	37.438832	64.964583
1594.937129	46.621474	64.969588
1594.262285	45.095361	64.974593
1593.834413	52.819855	64.979598
1593.423810	47.451321	64.984602
1592.892535	45.438027	64.989607
1591.731083	52.257056	64.994612
1590.898861	48.999796	64.999617
1590.731160	52.097471	65.004622
1590.106907	51.551471	65.009626
1589.457262	51.665840	65.014631
1588.115346	54.542511	65.019636
1587.941678	51.091631	65.024641
1587.423717	51.068995	65.029646
1586.705849	45.001897	65.034650
1586.371991	46.150859	65.039655
1585.564133	43.585715	65.044660
1584.846450	38.319078	65.049665
1583.863084	51.050125	65.054670
1582.961748	52.214102	65.059674
1581.827187	36.844925	65.064679
1581.524561	49.567624	65.069684
1581.058625	47.522228	65.074689
1580.860121	48.425010	65.079694
1580.187005	51.509317	65.084698
1579.981379	49.466344	65.089703
1578.629268	49.209902	65.094708
1578.077256	50.504747	65.099713
1577.576057	51.123031	65.104718
1576.422769	52.605248	65.109722
1575.980082	44.704164	65.114727
1575.014506	55.010963	65.119732
1574.507318	52.718823	65.124737
1574.195791	50.564902	65.129742
1573.615082	61.386472	65.134746
1572.792018	53.565480	65.139751
1571.799120	48.336074	65.144756
1571.390035	49.143849	65.149761
1571.153926	50.322660	65.154766
1570.093183	47.074514	65.159770
1569.638139	51.878396	65.164775
1568.647054	57.016374	65.169780
1568.246156	44.945825	65.174785
1567.197085	56.433705	65.179790
1566.398688	55.295039	65.184794
1565.735248	45.696550	65.189799
1565.275931	54.507562	65.194804
1564.803038	45.616167	65.199809
1564.558493	48.580552	65.204814
1563.370568	52.920939	65.209818
1562.494085	48.652489	65.214823
1561.845893	56.750991	65.219828
1561.476198	45.332311	65.224833
1561.343043	44.924494	65.229838
1560.302581	44.621037	65.234842
1559.719432	49.871955	65.239847
1558.774259	56.942516	65.244852
1558.499559	45.907824	65.249857
1557.708053	50.804023	65.254862
1556.704278	46.324081	65.259866
1556.494422	43.500291	65.264871
1555.914236	47.109855	65.269876
1555.248556	40.901602	65.274881
1553.942565	44.877738	65.279886
1553.140450	43.560904	65.284890
1552.758310	44.422091	65.289895
1552.357158	57.165998	65.294900
1552.211108	44.881318	65.299905
1550.880343	46.156292	65.304910
1549.949834	45.880201	65.309914
1549.819865	47.887125	65.314919
1549.072189	46.128757	65.319924
1547.894896	45.295719	65.324929
1547.152732	43.437333	65.329934
1546.298888	49.090616	65.334938
1546.213729	43.289040	65.339943
1545.794808	48.645267	65.344948
1545.503288	46.444110	65.349953
1544.689702	50.890558	65.354958
1543.629780	54.624463	65.359962
1543.290353	55.727015	65.364967
1542.434665	51.457378	65.369972
1541.417829	48.657625	65.374977
1540.701033	46.529647	65.379982
1539.940430	53.084695	65.384986
1539.496494	48.239745	65.389991
1539.207264	45.208498	65.394996
1538.882840	47.420404	65.400001
1537.869055	38.492517	65.405006
1536.810089	45.967007	65.410010
1536.563968	38.693445	65.415015
1536.010821	48.057330	65.420020
1535.122021	47.907518	65.425025
1533.797667	39.109755	65.430030
1533.183166	46.877634	65.435034
1533.333172	41.985111	65.440039
1532.431180	46.474714	65.445044
1532.315729	37.147173	65.450049
1531.161361	44.308400	65.455054
1530.366429	48.998750	65.460058
1530.065652	46.281308	65.465063
1529.169817	51.865205	65.470068
1528.068693	49.060934	65.475073
1527.554866	42.666046	65.480078
1526.983929	48.310383	65.485082
1526.828020	40.818102	65.490087
1526.408697	46.242683	65.495092
1525.494241	44.527072	65.500097
1524.525544	48.632586	65.505102
1523.811269	56.637010	65.510106
1523.383044	49.351193	65.515111
1522.114675	57.545972	65.520116
1521.316616	49.647692	65.525121
1520.846721	50.500218	65.530126
1520.456476	52.212625	65.535130
1520.138548	46.347473	65.540135
1519.567409	47.386266	65.545140
1519.084444	50.381195	65.550145
1517.924697	55.821981	65.555150
1517.119736	51.887468	65.560154
1516.661540	45.511084	65.565159
1515.330685	50.460126	65.570164
1514.802414	50.192958	65.575169
1514.422866	54.172773	65.580174
1513.777915	54.222404	65.585178
1513.551300	37.895788	65.590183
1512.986460	45.735295	65.595188
1512.045573	46.187270	65.600193
1511.397332	49.982161	65.605198
1510.746670	56.640365	65.610202
1510.370140	43.036123	65.615207
1508.893487	52.368209	65.620212
1508.174045	46.284818	65.625217
1507.967059	50.828755	65.630222
1507.006072	49.811475	65.635226
1507.105986	40.990997	65.640231
1506.315621	59.067853	65.645236
1505.310452	52.864817	65.650241
1505.435957	50.556369	65.655246
1504.086137	54.238849	65.660250
1503.260214	48.639450	65.665255
1502.489306	52.949131	65.670260
1501.862191	55.010356	65.675265
1501.674153	49.853598	65.680270
1501.154003	51.961249	65.685274
1499.909896	58.595898	65.690279
1499.235106	57.130969	65.695284
1498.806243	54.491501	65.700289
1498.020572	44.978288	65.705294
1497.386004	48.704133	65.710298
1496.556144	41.897572	65.715303
1495.725248	51.615693	65.720308
1495.256506	47.490620	65.725313
1495.394215	45.749268	65.730318
1494.174597	49.842866	65.735322
1493.437428	47.477604	65.740327
1492.616421	51.836122	65.745332
1492.166133	44.916440	65.750337
1492.030025	44.749515	65.755342
1491.100195	51.363923	65.760346
1489.919170	46.388570	65.765351
1489.395405	45.654470	65.770356
1489.259588	48.582090	65.775361
1488.394380	44.905779	65.780366
1487.167996	50.236401	65.785370
1487.008723	47.883146	65.790375
1486.109777	54.137024	65.795380
1485.867799	52.521443	65.800385
1484.774110	46.778414	65.805390
1483.925550	55.956034	65.810394
1483.288040	47.163484	65.815399
1482.519115	47.364199	65.820404
1482.248639	47.155144	65.825409
1481.811955	52.146535	65.830414
1481.029422	46.072763	65.835418
1480.395096	49.854618	65.840423
1479.688624	56.528691	65.845428
1479.220901	52.163061	65.850433
1478.370459	49.088933	65.855438
1476.923744	54.437928	65.860442
1476.646131	41.265165	65.865447
1476.078692	46.408797	65.870452
1475.495017	41.544356	65.875457
1475.312706	39.330040	65.880462
1474.355095	51.837222	65.885466
1473.853441	43.557845	65.890471
1472.973705	48.559939	65.895476
1472.603361	45.960589	65.900481
1471.771905	42.640462	65.905486
1470.346053	45.063389	65.910490
1469.860120	47.804629	65.915495
1469.518226	45.380401	65.920500
1469.095398	36.548352	65.925505
1469.046821	43.205732	65.930510
1467.691301	45.429920	65.935514
1467.482951	39.874822	65.940519
1466.899337	48.898543	65.945524
1465.948381	45.623738	65.950529
1465.169188	45.101116	65.955534
1464.223426	49.514145	65.960538
1464.002692	42.986606	65.965543
1462.428571	42.238087	65.970548
1462.020824	47.008219	65.975553
1461.662754	48.040548	65.980558
1460.838449	52.137935	65.985562
1460.430210	50.503053	65.990567
1459.892171	50.358347	65.995572
1459.276893	49.196645	66.000577
1458.679941	46.261889	66.005582
1457.452768	58.657723	66.010586
1457.356202	43.823390	66.015591
1456.691184	54.081517	66.020596
1455.972919	46.282093	66.025601
1455.259954	40.187738	66.030606
1454.400683	56.765796	66.035610
1453.955438	44.055129	66.040615
1453.308066	49.364016	66.045620
1452.101763	52.779586	66.050625
1451.697930	49.695728	66.055630
1451.262998	48.942086	66.060634
1450.836087	47.098043	66.065639
1449.814185	47.574553	66.070644
1448.623048	41.055621	66.075649
1448.013758	43.373524	66.080654
1447.580990	49.718919	66.085658
1447.630230	40.232544	66.090663
1447.127117	50.534796	66.095668
1446.306718	50.367371	66.100673
1445.587652	43.773558	66.105678
1444.522983	44.714473	66.110682
1444.195289	44.633629	66.115687
1442.762710	53.848058	66.120692
1441.880931	43.117026	66.125697
1441.467679	44.265375	66.130702
1441.145682	55.690391	66.135706
1441.067091	42.455939	66.140711
1440.717453	50.328086	66.145716
1439.750313	53.838110	66.150721
1439.055362	49.932545	66.155726
1437.573697	52.063864	66.160730
1436.916261	42.303730	66.165735
1435.915042	48.701031	66.170740
1435.428431	52.026179	66.175745
1435.389052	45.525624	66.180750
1434.795641	46.732440	66.185754
1434.454855	45.377318	66.190759
1433.907482	52.652947	66.195764
1432.894456	49.646523	66.200769
1432.492775	45.804046	66.205774
1431.397684	50.267113	66.210778
1430.281959	45.830442	66.215783
1429.518913	53.079832	66.220788
1428.713502	51.600168	66.225793
1428.581335	50.340779	66.230798
1428.438759	51.749100	66.235802
1428.149755	45.110492	66.240807
1427.147483	41.580413	66.245812
1425.902019	49.035528	66.250817
1425.566108	43.123732	66.255822
1424.883209	46.060129	66.260826
1423.975354	47.697331	66.265831
1423.055303	46.890946	66.270836
1422.175006	39.028482	66.275841
1422.053866	44.656224	66.280846
1421.447632	49.347838	66.285850
1421.478911	43.499501	66.290855
1420.229432	43.962474	66.295860
1419.338799	45.312136	66.300865
1419.352576	45.901100	66.305870
1418.082166	42.735852	66.310874
1417.541882	36.251177	66.315879
1416.693064	47.587948	66.320884
1416.051984	47.486541	66.325889
1415.732990	42.353789	66.330894
1415.172328	47.538499	66.335898
1414.349222	33.616009	66.340903
1413.394415	36.737099	66.345908
1412.954867	42.151328	66.350913
1412.601348	48.500525	66.355918
1410.856278	49.097670	66.360922
1410.739678	47.070653	66.365927
1409.790581	50.629696	66.370932
1409.339371	49.343211	66.375937
1409.223492	50.679861	66.380942
1408.732269	54.097769	66.385946
1407.809386	46.831910	66.390951
1407.082316	49.432465	66.395956
1406.549758	47.721768	66.400961
1406.021398	46.883469	66.405966
1404.597629	54.620941	66.410970
1404.305052	52.607073	66.415975
1403.984560	54.334388	66.420980
1402.911597	53.899953	66.425985
1402.227929	41.929158	66.430990
1401.088170	56.802283	66.435994
1400.668949	43.838107	66.440999
1400.385267	49.744713	66.446004
1399.736705	50.200352	66.451009
1399.573410	46.460751	66.456014
1397.970034	49.780885	66.461018
1397.550656	45.087271	66.466023
1396.740465	50.350221	66.471028
1396.341032	51.490682	66.476033
1395.907985	43.680738	66.481038
1395.328338	52.211175	66.486042
1394.481154	45.325107	66.491047
1393.543301	51.794459	66.496052
1393.410329	55.965745	66.501057
1392.379060	51.292794	66.506062
1391.558822	52.019388	66.511066
1391.078020	48.994894	66.516071
1390.596866	53.326432	66.521076
1389.617133	58.146718	66.526081
1388.900709	49.724521	66.531086
1387.640044	53.709120	66.536090
1387.556445	46.902731	66.541095
1386.976215	55.396560	66.546100
1386.796092	58.072830	66.551105
1386.632099	54.994106	66.556110
1385.664658	60.087012	66.561114
1385.035273	53.105243	66.566119
1383.725948	49.643521	66.571124
1382.603293	57.831537	66.576129
1381.913915	50.582946	66.581134
1381.304135	55.260566	66.586138
1380.991376	47.602920	66.591143
1380.352925	47.279235	66.596148
1380.267120	46.785560	66.601153
1379.816590	50.672929	66.606158
1378.426700	50.503924	66.611162
1378.231231	49.739692	66.616167
1377.575283	53.939712	66.621172
1376.533030	51.536697	66.626177
1375.569870	46.601842	66.631182
1374.930809	53.496476	66.636186
1374.501766	48.131523	66.641191
1374.061728	46.616168	66.646196
1373.404512	51.608209	66.651201
1372.466451	45.976722	66.656206
1371.433877	48.783912	66.661210
1371.041350	56.814974	66.666215
1370.933963	48.605092	66.671220
1370.102658	44.243299	66.676225
1369.502205	50.008744	66.681230
1368.571644	47.630821	66.686234
1368.347484	46.834397	66.691239
1367.432310	45.463530	66.696244
1366.289867	44.189591	66.701249
1365.539538	46.613745	66.706254
1364.708893	52.082690	66.711258
1364.512312	37.672851	66.716263
1364.083862	45.781500	66.721268
1363.637689	51.753026	66.726273
1363.416354	40.914884	66.731278
1362.319487	55.864744	66.736282
1361.266176	49.578414	66.741287
1361.094029	49.013865	66.746292
1359.693231	44.666669	66.751297
1359.075396	42.281004	66.756302
1357.981723	52.369757	66.761306
1358.237377	41.349312	66.766311
1357.860051	42.770977	66.771316
1356.863628	44.928590	66.776321
1356.380554	41.572928	66.781326
1355.293822	44.375970	66.786330
1354.894535	43.716889	66.791335
1354.219915	44.538950	66.796340
1352.825727	45.507477	66.801345
1352.738771	43.842081	66.806350
1351.986388	47.950062	66.811354
1351.940291	43.265578	66.816359
1351.571852	45.525682	66.821364
1350.437629	51.173300	66.826369
1349.626024	43.854068	66.831374
1348.146107	47.008615	66.836378
1347.729242	48.696774	66.841383
1347.020726	50.764844	66.846388
1346.054074	47.826289	66.851393
1346.200263	47.947737	66.856398
1345.693650	57.785219	66.861402
1345.302485	43.277640	66.866407
1345.012765	44.341300	66.871412
1343.710563	48.566295	66.876417
1343.219499	43.146443	66.881422
1342.204684	54.792678	66.886426
1341.281107	39.481813	66.891431
1340.519659	38.272522	66.896436
1340.049326	43.675840	66.901441
1339.670585	43.123764	66.906446
1338.965847	55.067823	66.911450
1338.406316	40.701960	66.916455
1337.378352	46.731632	66.921460
1336.587600	45.244345	66.926465
1336.405080	42.639697	66.931470
1335.992636	45.738611	66.936474
1335.633581	46.921898	66.941479
1334.334250	40.866369	66.946484
1333.574942	47.976183	66.951489
1333.236489	36.125122	66.956494
1331.843229	43.918561	66.961498
1331.229072	33.803697	66.966503
1330.688469	46.811836	66.971508
1329.958908	47.885268	66.976513
1329.535153	43.782121	66.981518
1329.099067	49.018139	66.986522
1328.607534	44.229128	66.991527
1327.463160	43.666416	66.996532
1327.002782	50.699401	67.001537
1326.675028	43.049858	67.006542
1325.902905	51.893890	67.011546
1325.117797	40.639527	67.016551
1323.921880	44.318593	67.021556
1323.721908	44.778365	67.026561
1322.786228	42.260020	67.031566
1322.703323	56.969598	67.036570
1321.832067	48.138943	67.041575
1321.013819	49.687010	67.046580
1320.050071	47.903304	67.051585
1319.966571	44.575949	67.056590
1319.245910	46.750701	67.061594
1318.644070	45.612769	67.066599
1317.978880	41.686344	67.071604
1317.219274	54.634879	67.076609
1316.805694	43.384412	67.081614
1315.423561	55.886913	67.086618
1314.717451	44.132340	67.091623
1314.103617	42.611218	67.096628
1313.914960	45.468149	67.101633
1313.866631	36.354528	67.106638
1312.197167	46.136082	67.111642
1311.253521	49.766045	67.116647
1311.004540	43.884775	67.121652
1310.258507	44.641308	67.126657
1310.221964	29.793977	67.131662
1309.518464	47.918701	67.136666
1308.581291	39.987849	67.141671
1307.915879	47.103300	67.146676
1307.443464	48.629269	67.151681
1306.835016	40.961469	67.156686
1305.678175	43.581531	67.161690
1305.015078	40.006049	67.166695
1304.590463	41.887370	67.171700
1304.282588	47.442870	67.176705
1303.558102	37.336240	67.181710
1302.373711	46.958576	67.186714
1302.217016	48.821662	67.191719
1301.650304	45.046530	67.196724
1300.358071	45.020295	67.201729
1299.560391	41.889807	67.206734
1299.074889	43.289733	67.211738
1298.493257	45.051889	67.216743
1298.542995	39.609723	67.221748
1297.330280	46.193635	67.226753
1296.814743	41.561496	67.231758
1295.627447	56.518946	67.236762
1295.512257	43.604583	67.241767
1294.930551	50.577817	67.246772
1293.603038	43.637431	67.251777
1293.007833	41.285400	67.256782
1292.185955	46.512861	67.261786
1292.084163	44.237405	67.266791
1291.867345	51.074361	67.271796
1291.118419	52.783846	67.276801
1290.216703	42.094560	67.281806
1289.231584	47.709161	67.286810
1288.801521	42.775035	67.291815
1287.693388	43.744343	67.296820
1286.579502	50.253316	67.301825
1286.400257	42.096799	67.306830
1285.824475	51.290885	67.311834
1285.408765	39.867905	67.316839
1285.504907	46.916532	67.321844
1284.534444	49.883622	67.326849
1283.545310	44.787850	67.331854
1282.932242	38.797608	67.336858
1282.156366	46.104462	67.341863
1281.353784	38.765942	67.346868
1280.402667	51.636740	67.351873
1279.891206	40.317386	67.356878
1279.308875	50.369130	67.361882
1279.240522	42.653871	67.366887
1278.724710	46.399269	67.371892
1277.573561	48.893633	67.376897
1276.833961	44.505502	67.381902
1276.335067	41.362944	67.386906
1275.087444	39.233918	67.391911
1274.388096	38.362937	67.396916
1273.275171	49.367186	67.401921
1273.593169	41.513947	67.406926
1272.779102	51.593128	67.411930
1272.393805	46.363590	67.416935
1272.353408	44.671280	67.421940
1270.877465	52.834136	67.426945
1270.331366	40.599047	67.431950
1269.449499	50.928640	67.436954
1268.972587	40.141769	67.441959
1268.149320	49.571240	67.446964
1267.017980	51.148444	67.451969
1266.630013	42.280462	67.456974
1265.806944	53.563891	67.461978
1265.611254	45.273618	67.466983
1266.036426	49.094753	67.471988
1264.319713	50.872036	67.476993
1263.706259	51.654428	67.481998
1263.398926	50.502398	67.487002
1262.173693	55.092375	67.492007
1261.033165	52.157159	67.497012
1260.250203	56.528532	67.502017
1259.870072	49.641874	67.507022
1259.278277	53.239633	67.512026
1259.349837	43.451837	67.517031
1258.911304	50.632655	67.522036
1257.830428	46.590308	67.527041
1256.939579	45.838952	67.532046
1256.381309	47.633427	67.537050
1255.860288	48.542094	67.542055
1255.182990	40.828463	67.547060
1253.996368	43.377849	67.552065
1253.364961	41.572390	67.557070
1253.110894	46.402265	67.562074
1252.809784	46.191757	67.567079
1251.841203	50.200585	67.572084
1250.840877	56.787619	67.577089
1250.824752	45.183343	67.582094
1249.918718	46.987622	67.587098
1248.865599	44.097049	67.592103
1248.284593	39.507703	67.597108
1247.015254	42.668064	67.602113
1246.996621	46.961473	67.607118
1246.327967	44.468478	67.612122
1246.331985	46.420097	67.617127
1245.519842	47.215192	67.622132
1244.565612	51.636413	67.627137
1244.386286	42.155242	67.632142
1243.385641	45.659190	67.637146
1242.216902	37.942073	67.642151
1241.713361	36.984287	67.647156
1241.215500	48.794640	67.652161
1240.557647	39.343689	67.657166
1239.532309	47.610579	67.662170
1238.756892	44.399320	67.667175
1238.313657	47.971251	67.672180
1237.630042	44.646385	67.677185
1237.482760	42.169520	67.682190
1236.941851	44.160751	67.687194
1235.860587	44.391295	67.692199
1235.153767	41.038431	67.697204
1234.269513	45.242023	67.702209
1233.930573	38.084256	67.707214
1233.629018	46.055133	67.712218
1232.835276	50.707813	67.717223
1232.057576	46.624225	67.722228
1231.106564	42.849376	67.727233
1230.145787	37.223396	67.732238
1229.355981	47.910631	67.737242
1229.046937	37.524482	67.742247
1228.208455	40.926066	67.747252
1227.794740	50.230557	67.752257
1227.534936	43.907488	67.757262
1227.019949	50.214465	67.762266
1226.213313	49.932226	67.767271
1225.501637	45.323414	67.772276
1224.855021	47.057231	67.777281
1224.605108	45.269352	67.782286
1223.115840	51.748266	67.787290
1222.246338	50.178959	67.792295
1222.088776	44.589138	67.797300
1221.079435	48.711916	67.802305
1220.970326	45.994054	67.807310
1219.947414	50.205599	67.812314
1218.990104	53.408463	67.817319
1218.821595	41.467538	67.822324
1217.938894	54.686611	67.827329
1218.178842	40.826898	67.832334
1216.872159	51.435269	67.837338
1215.620431	41.003684	67.842343
1215.356360	46.817330	67.847348
1214.547079	48.726622	67.852353
1214.215867	46.728858	67.857358
1213.006595	49.810263	67.862362
1212.675481	42.264333	67.867367
1212.161339	48.885361	67.872372
1211.597656	52.436471	67.877377
1210.777403	45.878189	67.882382
1209.358992	46.321980	67.887386
1209.086652	46.616524	67.892391
1208.724703	43.550786	67.897396
1208.119955	46.081081	67.902401
1208.080565	47.721989	67.907406
1207.183956	48.548919	67.912410
1206.017645	43.897561	67.917415
1206.106445	44.506044	67.922420
1204.776819	48.120400	67.927425
1203.855846	43.556505	67.932430
1203.176726	36.882096	67.937434
1202.755958	55.709562	67.942439
1202.480424	43.320801	67.947444
1201.923863	52.413709	67.952449
1201.009066	45.165072	67.957454
1200.406781	50.251137	67.962458
1199.790920	44.383749	67.967463
1199.168675	38.638635	67.972468
1197.769474	47.646874	67.977473
1197.299604	40.668231	67.982478
1196.500939	45.641082	67.987482
1196.307525	43.813533	67.992487
1195.897778	41.127805	67.997492
1194.906588	50.823257	68.002497
1194.192708	47.484239	68.007502
1193.597466	49.552273	68.012506
1193.119949	48.492936	68.017511
1192.462744	42.902221	68.022516
1191.286837	50.393621	68.027521
1191.028261	41.322719	68.032526
1190.176447	43.782822	68.037530
1189.753466	45.891228	68.042535
1189.380918	43.222024	68.047540
1188.270037	54.248434	68.052545
1187.806781	42.485867	68.057550
1187.347542	45.480700	68.062554
1186.199312	43.901494	68.067559
1185.195249	46.416481	68.072564
1184.591736	50.902392	68.077569
1184.216826	40.701597	68.082574
1183.761037	44.326598	68.087578
1183.264130	44.709326	68.092583
1183.070334	39.855152	68.097588
1181.692825	49.559515	68.102593
1181.087903	40.113725	68.107598
1180.601562	40.824628	68.112602
1179.513222	39.223724	68.117607
1178.864329	39.414591	68.122612
1178.120046	49.746684	68.127617
1177.897137	40.558762	68.132622
1177.567260	42.766484	68.137626
1176.354315	44.163477	68.142631
1175.205648	46.818086	68.147636
1174.840297	56.023909	68.152641
1174.746791	43.493466	68.157646
1174.116597	38.555335	68.162650
1172.847623	42.044844	68.167655
1172.251482	37.157723	68.172660
1171.134849	47.060565	68.177665
1170.802556	42.669425	68.182670
1170.419839	43.615600	68.187674
1170.009578	46.956505	68.192679
1169.429014	37.506549	68.197684
1168.151191	39.701718	68.202689
1168.090306	36.196037	68.207694
1167.340466	40.261759	68.212698
1166.876836	33.663747	68.217703
1165.992020	29.102358	68.222708
1164.762607	37.268805	68.227713
1164.384212	35.072293	68.232718
1163.973223	43.446754	68.237722
1163.527963	40.507386	68.242727
1162.471824	46.419149	68.247732
1161.221051	52.018863	68.252737
1160.823926	41.131120	68.257742
1160.353719	44.282167	68.262746
1160.256822	44.397865	68.267751
1159.951752	36.758281	68.272756
1158.638042	41.433683	68.277761
1158.181783	36.035534	68.282766
1157.558754	41.972213	68.287770
1156.271484	46.758742	68.292775
1155.643467	35.918827	68.297780
1155.005290	43.701824	68.302785
1154.786642	37.573024	68.307790
1154.298835	41.417050	68.312794
1153.438846	43.828035	68.317799
1152.462029	32.096971	68.322804
1151.751236	38.078281	68.327809
1151.417860	40.096349	68.332814
1150.870812	42.868994	68.337818
1150.214891	41.328656	68.342823
1149.475033	37.233871	68.347828
1148.529247	43.083716	68.352833
1148.265808	42.361921	68.357838
1147.586183	46.000777	68.362842
1146.446133	46.555206	68.367847
1145.770866	38.885461	68.372852
1145.330724	49.740187	68.377857
1144.975727	36.858231	68.382862
1144.148677	47.424746	68.387866
1143.094127	36.631025	68.392871
1142.866297	37.746067	68.397876
1142.266557	40.676543	68.402881
1141.799359	39.945033	68.407886
1140.688370	50.124006	68.412890
1139.806845	46.735944	68.417895
1139.139305	44.643807	68.422900
1138.751106	47.751211	68.427905
1138.418843	40.785329	68.432910
1137.583373	41.383919	68.437914
1136.707156	39.889987	68.442919
1136.346449	36.774706	68.447924
1135.251686	51.755791	68.452929
1134.902901	45.976494	68.457934
1133.712808	43.768580	68.462938
1132.873987	48.107294	68.467943
1132.538553	43.664988	68.472948
1132.037936	51.976250	68.477953
1132.003391	43.802475	68.482958
1131.359944	49.178210	68.487962
1130.139888	47.752230	68.492967
1129.430439	43.205026	68.497972
1128.745611	46.127575	68.502977
1128.786366	43.955212	68.507982
1127.873934	41.221360	68.512986
1127.270446	40.435430	68.517991
1126.595742	42.579441	68.522996
1125.124182	46.250879	68.528001
1124.288300	36.001141	68.533006
1124.052133	44.061471	68.538010
1123.359772	42.472115	68.543015
1123.067552	40.361109	68.548020
1122.564290	48.569013	68.553025
1121.688908	40.680918	68.558030
1120.783907	40.161737	68.563034
1120.179857	40.787806	68.568039
1119.763939	48.519329	68.573044
1119.029645	48.472603	68.578049
1118.228919	39.197717	68.583054
1117.457175	35.538640	68.588058
1116.721531	46.256471	68.593063
1116.656119	38.878998	68.598068
1115.745704	41.602159	68.603073
1114.866208	38.829515	68.608078
1114.055318	34.948995	68.613082
1113.515130	51.352808	68.618087
1113.098479	45.228705	68.623092
1112.824715	42.822055	68.628097
1112.167790	38.983063	68.633102
1111.208996	40.376418	68.638106
1110.374936	47.045913	68.643111
1109.552314	38.729599	68.648116
1108.666633	47.710711	68.653121
1108.045096	43.586199	68.658126
1107.635493	37.116306	68.663130
1107.097385	44.755071	68.668135
1106.686933	38.487418	68.673140
1105.719890	40.859901	68.678145
1104.907872	37.260220	68.683150
1104.265062	38.912875	68.688154
1103.495485	39.073104	68.693159
1103.922962	38.180114	68.698164
1102.433950	48.264353	68.703169
1101.446217	37.456441	68.708174
1101.068846	34.713867	68.713178
1100.443275	37.748238	68.718183
1100.466677	34.781915	68.723188
1099.033109	53.775685	68.728193
1098.154389	36.252339	68.733198
1098.055773	45.670624	68.738202
1097.429885	48.555454	68.743207
1096.794734	44.003033	68.748212
1095.613048	48.576506	68.753217
1094.827606	49.099040	68.758222
1094.657729	45.498345	68.763226
1094.009738	47.965401	68.768231
1093.035837	35.043784	68.773236
1092.017030	42.990639	68.778241
1091.585404	36.986733	68.783246
1091.140704	51.962687	68.788250
1090.537346	53.584907	68.793255
1090.648874	44.287231	68.798260
1089.487710	49.052181	68.803265
1088.662453	49.102347	68.808270
1088.195727	44.078610	68.813274
1086.942981	48.144805	68.818279
1086.493979	48.343296	68.823284
1085.801422	51.861222	68.828289
1085.392029	48.052079	68.833294
1085.133288	47.885245	68.838298
1083.897248	53.464688	68.843303
1083.519796	40.063983	68.848308
1082.242376	47.360028	68.853313
1081.895927	50.363975	68.858318
1081.631467	44.648795	68.863322
1080.406305	51.024493	68.868327
1079.421387	43.547514	68.873332
1078.888171	48.775698	68.878337
1078.791460	46.581483	68.883342
1078.389570	41.258898	68.888346
1077.744008	54.717617	68.893351
1076.949812	40.499371	68.898356
1075.934186	47.430079	68.903361
1075.509972	36.861190	68.908366
1074.547756	40.390556	68.913370
1073.550152	50.773925	68.918375
1073.107010	43.270093	68.923380
1072.318639	48.217513	68.928385
1072.053019	43.476694	68.933390
1071.648520	42.813794	68.938394
1071.101403	47.706087	68.943399
1069.948028	46.861569	68.948404
1069.271743	50.798268	68.953409
1068.918150	39.283780	68.958414
1068.204279	46.232287	68.963418
1067.506932	44.826942	68.968423
1066.783830	45.306044	68.973428
1065.862305	46.308967	68.978433
1065.369887	47.912587	68.983438
1064.890059	48.812639	68.988442
1064.152664	47.720058	68.993447
1063.808249	40.846264	68.998452
1062.935865	51.971574	69.003457
1062.368125	43.960159	69.008462
1061.369746	38.256192	69.013466
1060.413684	43.773878	69.018471
1059.971256	46.114952	69.023476
1059.447870	49.949289	69.028481
1059.218057	49.475544	69.033486
1058.310856	44.545396	69.038490
1057.130035	47.501572	69.043495
1056.598729	45.906752	69.048500
1055.828464	57.810724	69.053505
1055.891529	52.585746	69.058510
1055.328828	44.344929	69.063514
1054.483512	48.720289	69.068519
1053.654312	48.219717	69.073524
1053.074462	42.487500	69.078529
1052.237370	43.159799	69.083534
1051.134798	46.730966	69.088538
1050.638441	48.360523	69.093543
1050.410028	42.963237	69.098548
1049.593828	41.283790	69.103553
1049.364819	42.792175	69.108558
1048.470989	43.336039	69.113562
1047.333252	42.983430	69.118567
1047.179595	48.307269	69.123572
1046.598186	49.682589	69.128577
1045.947780	41.487976	69.133582
1045.028413	47.278447	69.138586
1044.411294	45.571618	69.143591
1043.906615	41.431844	69.148596
1042.792203	50.048730	69.153601
1041.973752	47.964689	69.158606
1041.472450	50.681355	69.163610
1041.139018	49.145410	69.168615
1040.997177	43.140830	69.173620
1039.376753	51.922918	69.178625
1038.581515	42.847233	69.183630
1038.157698	49.413722	69.188634
1037.349582	51.279027	69.193639
1036.988665	45.399194	69.198644
1036.620961	56.894773	69.203649
1036.377012	48.398066	69.208654
1035.402403	49.431795	69.213658
1034.628411	39.566198	69.218663
1033.548034	45.879611	69.223668
1032.425854	54.642693	69.228673
1031.745655	49.818932	69.233678
1031.476527	50.604752	69.238682
1030.687566	45.281354	69.243687
1030.711665	46.683242	69.248692
1030.285452	51.190510	69.253697
1029.767594	55.680712	69.258702
1028.623177	53.301985	69.263706
1027.956119	54.084505	69.268711
1027.653075	44.926509	69.273716
1026.622523	43.876636	69.278721
1025.768334	46.150864	69.283726
1025.128486	48.656400	69.288730
1024.476952	51.954950	69.293735
1023.911466	44.900739	69.298740
1022.874404	52.821919	69.303745
1022.257672	57.289977	69.308750
1021.920733	52.542823	69.313754
1021.640232	51.090178	69.318759
1021.134446	51.905474	69.323764
1019.935359	45.331195	69.328769
1019.275850	46.967379	69.333774
1018.162189	48.794621	69.338778
1016.893649	48.690196	69.343783
1016.918248	41.962415	69.348788
1016.739972	54.220905	69.353793
1015.786127	46.587444	69.358798
1015.302162	40.060039	69.363802
1014.688577	53.130010	69.368807
1014.622564	42.615440	69.373812
1013.083644	46.344229	69.378817
1012.551087	46.399938	69.383822
1012.081296	43.822007	69.388826
1011.090725	46.766138	69.393831
1010.553254	37.763157	69.398836
1009.835795	43.972583	69.403841
1009.187217	50.365600	69.408846
1008.567131	40.173669	69.413850
1007.925574	43.103818	69.418855
1008.078311	37.261944	69.423860
1007.065698	37.310658	69.428865
1005.794322	39.849742	69.433870
1005.492193	42.773867	69.438874
1004.223592	44.829740	69.443879
1003.711587	41.973659	69.448884
1002.994164	48.572667	69.453889
1002.462049	42.364150	69.458894
1002.094913	39.249984	69.463898
1001.545948	52.455722	69.468903
1001.319679	37.903809	69.473908
1000.260949	36.928633	69.478913
999.626446	48.144647	69.483918
999.083789	50.433421	69.488922
998.013914	48.888604	69.493927
997.630906	38.748834	69.498932
996.933558	46.455924	69.503937
996.434373	43.617780	69.508942
995.614646	42.095648	69.513946
994.381902	54.278152	69.518951
993.789883	53.100688	69.523956
993.371013	54.786846	69.528961
992.790898	53.456562	69.533966
991.993717	48.080109	69.538970
990.797759	50.629572	69.543975
990.483414	46.972708	69.548980
989.985185	49.961205	69.553985
989.847786	45.342903	69.558990
989.584077	42.764812	69.563994
988.161078	43.040513	69.568999
987.433197	44.154358	69.574004
986.945171	46.837571	69.579009
986.609328	37.188650	69.584014
985.401359	49.936483	69.589018
984.508571	51.033179	69.594023
983.880216	40.855300	69.599028
983.280828	42.520269	69.604033
983.172545	42.596475	69.609038
982.884504	44.042344	69.614042
981.294276	50.141518	69.619047
980.897071	44.414348	69.624052
980.234052	39.585290	69.629057
979.955985	44.529400	69.634062
978.906210	46.121904	69.639066
978.117129	46.927301	69.644071
977.426137	42.541958	69.649076
977.019718	47.567653	69.654081
976.544612	39.654466	69.659086
975.307306	36.639197	69.664090
974.617014	49.972551	69.669095
974.338850	44.930354	69.674100
973.895216	51.672335	69.679105
973.531313	43.103425	69.684110
972.572551	47.214818	69.689114
971.577673	44.933648	69.694119
971.320353	34.406460	69.699124
970.136884	48.117152	69.704129
969.536090	47.471299	69.709134
968.638711	34.787660	69.714138
968.158512	49.200106	69.719143
967.892982	43.631957	69.724148
967.423461	44.849184	69.729153
966.375224	44.706254	69.734158
965.568744	47.316118	69.739162
964.964365	49.388108	69.744167
964.611970	40.723682	69.749172
963.986659	45.606873	69.754177
962.819397	48.925071	69.759182
962.105288	44.063714	69.764186
961.426409	54.754860	69.769191
961.335307	43.877507	69.774196
960.870912	47.016913	69.779201
959.773541	43.833611	69.784206
959.220115	45.551498	69.789210
958.129758	43.994804	69.794215
957.864830	35.121992	69.799220
957.334383	49.699351	69.804225
956.228332	41.744626	69.809230
955.750397	45.853407	69.814234
954.770832	49.257481	69.819239
954.661473	40.926021	69.824244
954.074930	37.043820	69.829249
953.010196	39.548317	69.834254
952.464061	49.333351	69.839258
951.758923	56.145382	69.844263
951.881236	40.933414	69.849268
950.277837	47.836124	69.854273
949.456307	50.572509	69.859278
949.341635	40.311007	69.864282
948.720915	46.210597	69.869287
948.268390	35.681318	69.874292
947.167416	45.480456	69.879297
946.435218	41.149147	69.884302
946.210178	43.846530	69.889306
945.186097	41.993504	69.894311
944.809065	35.692918	69.899316
943.549471	44.153109	69.904321
942.886582	42.960556	69.909326
942.897815	40.409589	69.914330
941.999470	46.218575	69.919335
941.445073	42.404682	69.924340
940.316467	39.707894	69.929345
939.875504	39.872654	69.934350
939.375654	39.650810	69.939354
938.604559	41.084679	69.944359
938.532332	31.094979	69.949364
937.218531	44.623135	69.954369
936.497847	42.068052	69.959374
936.090065	34.403069	69.964378
935.490668	46.708012	69.969383
934.637449	40.559239	69.974388
933.893838	42.889538	69.979393
933.534313	39.566850	69.984398
932.933705	35.846133	69.989402
931.362081	44.373581	69.994407
931.216917	38.708249	69.999412
930.299934	51.350204	70.004417
929.999635	49.759649	70.009422
929.380078	39.988809	70.014426
928.746171	48.178433	70.019431
928.895848	41.399238	70.024436
927.759090	43.928312	70.029441
927.142297	43.103636	70.034446
926.074345	36.474564	70.039450
924.937772	42.534341	70.044455
924.705573	37.120746	70.049460
924.226095	45.302472	70.054465
923.781391	41.131524	70.059470
922.946795	36.798417	70.064474
921.132226	42.752878	70.069479
920.763908	41.280152	70.074484
920.465310	40.597944	70.079489
919.805264	42.069635	70.084494
919.690201	39.032694	70.089498
919.173020	46.640251	70.094503
918.872333	40.432770	70.099508
917.810085	52.367802	70.104513
916.956776	45.837355	70.109518
916.313156	42.083350	70.114522
915.125106	46.052452	70.119527
914.728784	41.222331	70.124532
914.183891	51.393187	70.129537
913.343967	41.112620	70.134542
913.295425	43.875691	70.139546
912.286876	47.833391	70.144551
911.268304	34.866990	70.149556
910.500560	48.954095	70.154561
910.019528	46.747951	70.159566
910.013242	35.558468	70.164570
908.993806	49.760914	70.169575
908.391710	38.357306	70.174580
907.571667	38.245170	70.179585
906.902096	46.573133	70.184590
906.586162	40.799689	70.189594
905.377097	43.218000	70.194599
904.708957	35.866809	70.199604
903.989806	46.805231	70.204609
903.383234	42.209663	70.209614
903.280301	38.116755	70.214618
902.399525	41.996917	70.219623
901.494603	33.203729	70.224628
900.696639	47.902292	70.229633
900.313894	46.135212	70.234638
900.311549	36.220777	70.239642
899.312535	38.883361	70.244647
898.524252	41.261971	70.249652
897.825517	42.071643	70.254657
897.459619	48.675974	70.259662
896.632293	49.532142	70.264666
895.648364	49.169014	70.269671
895.303528	40.530541	70.274676
894.535851	44.959330	70.279681
893.479847	42.818904	70.284686
892.986648	34.165190	70.289690
892.339001	51.695359	70.294695
892.065967	39.397807	70.299700
891.108400	40.423117	70.304705
889.916684	42.389667	70.309710
889.659597	40.627119	70.314714
888.826396	39.894378	70.319719
889.059167	35.145584	70.324724
888.114382	39.365904	70.329729
886.986858	41.092130	70.334734
886.437918	35.868572	70.339738
885.913718	41.375468	70.344743
885.263598	38.222551	70.349748
884.097348	47.381597	70.354753
883.245172	38.976856	70.359758
883.365771	44.648432	70.364762
882.237438	47.967873	70.369767
882.283949	31.639624	70.374772
881.114335	40.048887	70.379777
880.176041	41.902170	70.384782
879.527958	36.659280	70.389786
878.947895	43.777107	70.394791
878.870591	37.495058	70.399796
878.141797	44.204567	70.404801
877.340800	36.369717	70.409806
876.890167	29.608879	70.414810
875.941338	39.811809	70.419815
875.850371	35.722774	70.424820
874.264315	48.201051	70.429825
873.736774	43.531956	70.434830
873.223240	30.520120	70.439834
872.702592	45.109212	70.444839
871.862806	39.424314	70.449844
870.954913	41.001616	70.454849
870.231304	34.914341	70.459854
870.049319	43.747707	70.464858
869.500293	49.356353	70.469863
869.036937	40.496224	70.474868
867.917761	42.632318	70.479873
867.143902	45.095300	70.484878
866.477237	38.785519	70.489882
866.158153	54.954090	70.494887
865.299580	39.794489	70.499892
864.459270	46.463498	70.504897
863.668943	42.997511	70.509902
863.244536	34.136240	70.514906
862.675989	50.523577	70.519911
862.519335	36.922482	70.524916
861.262618	38.514535	70.529921
860.336187	37.680143	70.534926
860.243578	36.091125	70.539930
859.296617	43.998072	70.544935
859.231059	34.500238	70.549940
858.080541	38.264378	70.554945
857.124338	42.890848	70.559950
856.744749	35.918906	70.564954
856.488227	44.479264	70.569959
855.540229	36.040421	70.574964
854.606574	43.622607	70.579969
853.974929	40.654020	70.584974
853.433271	32.036640	70.589978
852.780683	36.906352	70.594983
851.987331	39.630818	70.599988
851.344772	47.983366	70.604993
850.973263	35.629274	70.609998
850.409388	36.464008	70.615002
849.146326	46.673006	70.620007
848.609283	35.188013	70.625012
847.966219	32.976871	70.630017
847.444754	36.038825	70.635022
847.286695	35.129666	70.640026
846.242071	37.093530	70.645031
845.118229	33.880848	70.650036
844.699400	35.386227	70.655041
844.451448	37.906361	70.660046
844.205295	35.849853	70.665050
843.024930	38.795338	70.670055
842.580279	34.931877	70.675060
841.624532	37.300890	70.680065
839.893981	41.523182	70.685070
839.986122	40.377757	70.690074
839.361552	32.079697	70.695079
838.553051	37.810544	70.700084
837.636709	41.098812	70.705089
837.272009	44.141417	70.710094
836.971414	32.856311	70.715098
836.606916	41.871322	70.720103
836.182781	31.490356	70.725108
835.322391	31.936167	70.730113
834.470721	42.591776	70.735118
833.945135	41.898719	70.740122
832.518071	40.065406	70.745127
832.096799	39.843929	70.750132
831.559791	40.132908	70.755137
830.976050	41.791660	70.760142
830.584784	32.885249	70.765146
829.356118	37.698119	70.770151
828.491445	45.326516	70.775156
828.426659	40.310153	70.780161
827.670091	48.776173	70.785166
827.241281	36.418481	70.790170
826.951452	41.757347	70.795175
826.167617	31.602592	70.800180
825.401812	33.883814	70.805185
824.112466	37.113218	70.810190
823.231459	22.218398	70.815194
822.610924	33.804621	70.820199
822.164665	29.879864	70.825204
821.860503	29.509651	70.830209
821.810745	37.048194	70.835214
820.842280	36.569149	70.840218
819.836269	33.203272	70.845223
819.536433	34.411180	70.850228
818.264704	37.403107	70.855233
816.953176	40.768148	70.860238
816.799955	28.304841	70.865242
816.041420	36.688302	70.870247
815.338534	31.883868	70.875252
815.042564	29.982337	70.880257
814.574525	35.513165	70.885262
814.462416	31.805499	70.890266
812.994174	29.520587	70.895271
812.240103	26.819282	70.900276
811.736725	28.863327	70.905281
811.040410	36.011329	70.910286
810.967757	29.488900	70.915290
809.846499	39.271789	70.920295
809.010583	28.653882	70.925300
808.546204	35.903069	70.930305
808.113908	39.518144	70.935310
807.338735	36.721379	70.940314
806.575269	43.625901	70.945319
805.809577	34.116560	70.950324
805.531756	40.380161	70.955329
804.484495	39.869224	70.960334
803.792043	38.794249	70.965338
802.691493	41.968032	70.970343
802.145087	46.735488	70.975348
802.019633	40.813384	70.980353
801.418254	35.633162	70.985358
801.059282	37.107372	70.990362
799.891667	41.197330	70.995367
799.302351	32.311429	71.000372
798.896368	38.328970	71.005377
797.911082	35.929758	71.010382
797.203804	32.497716	71.015386
796.106247	34.416581	71.020391
795.908204	25.696543	71.025396
795.863830	34.097008	71.030401
794.876981	38.034035	71.035406
794.363469	33.623459	71.040410
793.579315	41.225434	71.045415
792.998262	27.817446	71.050420
791.827630	34.706846	71.055425
790.796494	34.583919	71.060430
790.778578	31.376802	71.065434
789.987784	39.892496	71.070439
789.569184	27.891471	71.075444
788.560890	35.573283	71.080449
787.549504	34.755827	71.085454
787.366900	30.814331	71.090458
786.521624	32.287373	71.095463
786.623062	32.055700	71.100468
785.575501	35.626965	71.105473
784.582243	30.213892	71.110478
784.066523	28.229617	71.115482
783.190190	32.216395	71.120487
783.253697	30.569061	71.125492
782.201329	31.399062	71.130497
781.391632	39.493676	71.135502
780.848825	40.513876	71.140506
780.224043	41.138800	71.145511
779.713755	38.342848	71.150516
778.838591	40.349931	71.155521
778.410114	44.401304	71.160526
777.840179	41.733194	71.165530
775.970270	38.760822	71.170535
775.431770	30.466190	71.175540
774.902402	40.352157	71.180545
774.463205	43.525151	71.185550
774.189726	34.434765	71.190554
773.827492	43.990543	71.195559
773.354555	41.741584	71.200564
772.867883	43.493051	71.205569
771.718554	35.840654	71.210574
771.322535	35.944444	71.215578
769.810371	40.338152	71.220583
769.157638	33.179343	71.225588
768.743184	30.737615	71.230593
768.345196	33.511596	71.235598
768.031337	18.534252	71.240602
767.044670	43.420756	71.245607
766.239835	37.575562	71.250612
765.591396	37.765222	71.255617
764.701737	37.950020	71.260622
764.524167	37.436949	71.265626
763.231866	45.244388	71.270631
762.379564	26.246733	71.275636
762.055207	29.524388	71.280641
762.018643	38.571242	71.285646
761.702120	33.839574	71.290650
760.498295	32.777998	71.295655
759.399286	34.744485	71.300660
759.169969	33.579130	71.305665
758.408490	32.796630	71.310670
757.474991	36.883199	71.315674
756.676165	48.461688	71.320679
756.006807	38.334703	71.325684
755.756298	37.435070	71.330689
755.157529	36.983493	71.335694
754.660979	37.127399	71.340698
753.341788	40.182732	71.345703
752.606044	37.282519	71.350708
752.159526	44.553123	71.355713
751.942909	40.405886	71.360718
751.698749	35.524067	71.365722
750.248731	41.075492	71.370727
749.346897	40.519920	71.375732
749.005023	40.374450	71.380737
748.570535	39.245031	71.385742
748.348248	35.089689	71.390746
747.305306	41.411730	71.395751
746.809280	32.993779	71.400756
745.782175	31.099085	71.405761
745.034214	40.079918	71.410766
744.340498	43.684124	71.415770
743.249764	44.683724	71.420775
742.958167	40.921154	71.425780
742.832513	39.629890	71.430785
741.903795	48.821683	71.435790
740.883036	36.550020	71.440794
740.235559	36.869774	71.445799
739.824177	42.662071	71.450804
739.526330	35.672593	71.455809
738.543874	38.409337	71.460814
738.234639	33.556430	71.465818
737.228590	36.023679	71.470823
736.814524	36.163325	71.475828
735.953907	23.846084	71.480833
734.606338	33.516966	71.485838
734.017793	29.745667	71.490842
733.849122	37.990983	71.495847
733.401390	41.702648	71.500852
732.969656	34.607429	71.505857
732.184452	35.924540	71.510862
731.200243	35.830295	71.515866
730.440184	41.602590	71.520871
729.985624	33.880133	71.525876
729.628370	43.180464	71.530881
728.173181	43.488200	71.535886
728.013805	35.005477	71.540890
727.475351	37.959042	71.545895
726.457005	37.115161	71.550900
725.567215	42.860342	71.555905
724.450553	34.909090	71.560910
724.625761	33.826799	71.565914
723.831901	40.513914	71.570919
723.407744	40.227418	71.575924
723.037606	32.400900	71.580929
722.319865	43.183170	71.585934
721.774530	32.867592	71.590938
720.916472	35.280678	71.595943
720.297450	36.582347	71.600948
719.021369	28.662357	71.605953
718.048288	37.389272	71.610958
717.964775	26.635000	71.615962
717.727733	34.923604	71.620967
717.190170	36.977461	71.625972
716.349487	32.075080	71.630977
715.061434	35.260474	71.635982
714.609933	33.175211	71.640986
713.842566	34.527556	71.645991
713.633100	33.768912	71.650996
712.653129	32.232841	71.656001
711.658712	29.597201	71.661006
711.223497	25.283747	71.666010
710.914622	34.272249	71.671015
710.445733	33.621596	71.676020
708.979966	30.574495	71.681025
708.115255	36.485501	71.686030
708.156193	31.284468	71.691034
707.391746	38.624929	71.696039
707.241635	33.019674	71.701044
706.598185	30.076424	71.706049
705.784250	40.202972	71.711054
705.205056	32.701202	71.716058
704.641847	34.270402	71.721063
703.352184	32.144001	71.726068
702.754856	36.209697	71.731073
701.761168	31.747983	71.736078
701.539272	35.049533	71.741082
701.160803	36.618662	71.746087
700.099877	36.194558	71.751092
699.222765	32.577694	71.756097
698.413535	36.993885	71.761102
698.200564	32.890633	71.766106
697.639686	31.283164	71.771111
697.077113	33.050797	71.776116
696.158848	23.386850	71.781121
694.903606	38.509118	71.786126
695.034908	32.670139	71.791130
694.458457	44.220793	71.796135
694.109877	39.601985	71.801140
693.590827	32.285298	71.806145
692.345718	42.855168	71.811150
691.912685	33.539907	71.816154
690.624577	38.122608	71.821159
689.939111	32.199355	71.826164
689.429874	31.179059	71.831169
688.569572	42.212319	71.836174
688.794951	38.223039	71.841178
688.016971	29.774462	71.846183
686.859593	35.713111	71.851188
686.823872	36.507510	71.856193
685.807887	33.564140	71.861198
684.648057	25.713059	71.866202
683.669064	36.686916	71.871207
683.207372	29.582631	71.876212
683.064287	26.226051	71.881217
682.368687	38.594831	71.886222
682.241991	27.772965	71.891226
681.304341	31.197925	71.896231
680.497879	31.944769	71.901236
679.999023	36.702900	71.906241
678.967392	37.828564	71.911246
678.203833	31.955007	71.916250
677.324638	37.528255	71.921255
676.406357	29.411200	71.926260
676.614499	40.099582	71.931265
675.585766	35.095618	71.936270
675.546111	26.659498	71.941274
674.783597	36.026883	71.946279
673.885656	36.665066	71.951284
673.146550	32.685110	71.956289
672.421407	36.171554	71.961294
671.644792	32.275783	71.966298
670.791386	43.442066	71.971303
670.156684	36.125854	71.976308
669.921041	34.671868	71.981313
669.387726	35.250741	71.986318
669.178158	26.366126	71.991322
668.002432	25.562247	71.996327
667.296392	33.339519	72.001332
666.799661	37.828091	72.006337
665.721277	42.942073	72.011342
664.995839	29.397416	72.016346
664.244478	35.038758	72.021351
663.350890	28.116621	72.026356
663.470861	31.693925	72.031361
662.891766	37.517324	72.036366
661.809077	36.247926	72.041370
660.635760	35.645334	72.046375
660.560196	30.014288	72.051380
660.480101	30.444073	72.056385
659.135961	39.721249	72.061390
658.147327	25.238848	72.066394
657.443134	33.412098	72.071399
656.947601	29.454359	72.076404
656.921277	27.112720	72.081409
656.305639	35.925236	72.086414
655.978451	31.162253	72.091418
654.545914	37.208439	72.096423
653.899379	32.638712	72.101428
653.447552	40.769125	72.106433
652.611128	31.962694	72.111438
651.586901	32.961576	72.116442
651.054279	38.362958	72.121447
650.481700	35.176271	72.126452
650.229669	26.439058	72.131457
649.502114	33.883326	72.136462
648.641623	34.963888	72.141466
647.706331	37.575338	72.146471
647.379623	33.396055	72.151476
647.076683	28.733913	72.156481
646.414634	36.055256	72.161486
645.297190	25.062103	72.166490
644.568648	33.069008	72.171495
643.907343	29.872658	72.176500
643.541613	28.000459	72.181505
642.608721	38.910768	72.186510
642.036105	27.947028	72.191514
641.630181	32.482407	72.196519
640.833351	30.243566	72.201524
640.429472	34.981084	72.206529
638.893132	37.337899	72.211534
638.393523	31.436102	72.216538
638.044369	33.321509	72.221543
637.704388	35.857415	72.226548
637.316156	29.436039	72.231553
636.287953	38.442786	72.236558
635.552943	28.092231	72.241562
635.131121	37.930563	72.246567
634.321457	29.300728	72.251572
633.255890	31.208225	72.256577
632.611829	30.481809	72.261582
632.363372	25.692315	72.266586
631.752080	40.424808	72.271591
631.004057	39.692520	72.276596
629.956025	28.082380	72.281601
629.551791	39.101448	72.286606
629.173104	27.167827	72.291610
627.962504	32.184472	72.296615
627.142103	38.826802	72.301620
626.784730	35.114987	72.306625
625.982478	43.763703	72.311630
626.040318	29.804216	72.316634
625.098585	37.772655	72.321639
623.982583	37.820216	72.326644
623.448468	41.667864	72.331649
622.694117	39.004139	72.336654
622.374354	39.884305	72.341658
621.905821	38.486406	72.346663
620.802498	27.550047	72.351668
620.511122	23.600362	72.356673
619.494538	31.142700	72.361678
619.225912	34.758556	72.366682
618.348214	39.387792	72.371687
617.451938	35.043612	72.376692
616.868194	24.185596	72.381697
616.277184	30.369042	72.386702
616.093246	29.361306	72.391706
614.899101	30.958486	72.396711
614.292198	29.246815	72.401716
613.849009	31.914870	72.406721
612.755159	30.892120	72.411726
612.673835	25.501658	72.416730
611.238743	29.921672	72.421735
610.803268	38.110857	72.426740
610.428397	31.627593	72.431745
609.883189	33.460545	72.436750
609.335084	27.790472	72.441754
608.073991	29.958039	72.446759
607.475105	36.706884	72.451764
607.105502	25.546538	72.456769
606.310917	35.007837	72.461774
606.368091	32.978321	72.466778
605.060401	34.015911	72.471783
604.328103	29.318001	72.476788
604.139666	28.234858	72.481793
603.212988	37.437360	72.486798
602.525229	25.617486	72.491802
601.530913	31.479661	72.496807
600.999602	37.931944	72.501812
600.797730	34.308746	72.506817
599.423532	39.745380	72.511822
598.732364	37.454102	72.516826
598.370558	39.902174	72.521831
597.407205	37.698581	72.526836
597.430823	33.391391	72.531841
596.795126	33.287985	72.536846
596.390313	28.743166	72.541850
595.359467	34.157285	72.546855
594.060714	34.874812	72.551860
593.956174	30.360646	72.556865
593.339126	31.753960	72.561870
592.558355	28.332181	72.566874
591.709586	35.373694	72.571879
591.426277	32.452042	72.576884
591.414394	24.960066	72.581889
590.010359	34.091601	72.586894
589.117837	32.554389	72.591898
588.688629	27.794290	72.596903
587.776876	32.422258	72.601908
586.916503	23.493646	72.606913
585.735047	27.296689	72.611918
585.753188	21.882873	72.616922
585.519490	30.429039	72.621927
584.980436	27.632518	72.626932
584.794232	23.920591	72.631937
583.432268	34.071966	72.636942
583.062802	24.630188	72.641946
582.011671	23.532630	72.646951
580.740280	28.339448	72.651956
580.429750	24.263583	72.656961
579.776874	32.202662	72.661966
579.475903	25.538595	72.666970
578.973373	26.649804	72.671975
577.946090	29.308603	72.676980
577.100085	27.607117	72.681985
576.269864	35.423040	72.686990
575.792674	28.365243	72.691994
575.223226	37.115772	72.696999
575.144296	35.839403	72.702004
573.834194	36.622035	72.707009
573.355427	31.482029	72.712014
572.944567	30.475679	72.717018
572.175367	26.051716	72.722023
571.127308	30.681331	72.727028
570.697691	25.242397	72.732033
569.813937	31.376536	72.737038
569.406696	29.319627	72.742042
569.069975	32.336132	72.747047
568.520931	35.112323	72.752052
567.703401	26.812652	72.757057
566.661108	40.904164	72.762062
566.503450	31.652660	72.767066
564.845963	36.076058	72.772071
564.059537	36.753966	72.777076
563.701928	27.889994	72.782081
562.863571	36.396878	72.787086
562.755092	33.461852	72.792090
562.530565	36.191124	72.797095
561.886711	45.343596	72.802100
561.520911	31.060016	72.807105
560.342108	44.115113	72.812110
559.770006	36.153497	72.817114
559.237445	37.538655	72.822119
557.868816	31.973261	72.827124
557.329618	25.105688	72.832129
556.802424	34.438680	72.837134
556.382483	23.469723	72.842138
555.661672	30.355110	72.847143
554.453971	31.819634	72.852148
553.904853	28.269360	72.857153
553.199526	39.024638	72.862158
553.156993	26.962387	72.867162
552.818447	27.809462	72.872167
551.713436	27.800686	72.877172
550.690070	28.300523	72.882177
549.750851	31.136464	72.887182
549.705351	25.016752	72.892186
549.199903	34.694550	72.897191
548.260227	32.130485	72.902196
547.631625	29.659954	72.907201
546.873215	35.082265	72.912206
546.363199	30.645473	72.917210
545.930511	35.654757	72.922215
544.639901	32.376394	72.927220
544.054496	26.654307	72.932225
543.412146	32.022391	72.937230
543.182518	26.128823	72.942234
542.681277	28.817486	72.947239
541.532349	32.304326	72.952244
541.300147	25.334420	72.957249
540.445686	34.140494	72.962254
540.077463	36.290476	72.967258
539.270650	36.053776	72.972263
538.261757	34.494279	72.977268
537.973623	36.122146	72.982273
536.966093	40.702196	72.987278
535.978683	27.981238	72.992282
535.104789	38.636724	72.997287
534.608144	34.556437	73.002292
534.485727	25.453630	73.007297
533.883889	32.150091	73.012302
533.561527	29.097776	73.017306
532.845974	30.726253	73.022311
531.500732	37.753374	73.027316
531.215529	32.547052	73.032321
530.795030	41.154438	73.037326
529.899929	32.891749	73.042330
528.855923	38.668508	73.047335
528.380787	27.890186	73.052340
528.045171	31.279903	73.057345
527.487068	33.755693	73.062350
526.233690	36.121684	73.067354
525.727455	43.235164	73.072359
524.901575	42.909765	73.077364
525.204525	34.818743	73.082369
523.632706	36.299880	73.087374
522.967969	39.553768	73.092378
522.454878	41.808306	73.097383
521.876161	36.666882	73.102388
521.585547	33.739778	73.107393
520.388980	37.323597	73.112398
519.582415	35.239596	73.117402
519.023807	37.557983	73.122407
518.391569	39.148503	73.127412
518.248477	32.472388	73.132417
517.314602	43.377352	73.137422
516.514697	30.582035	73.142426
515.925874	39.658763	73.147431
515.276195	37.651295	73.152436
515.087425	29.667031	73.157441
513.626040	39.219703	73.162446
513.109625	42.857101	73.167450
512.655531	37.853394	73.172455
511.714062	36.532993	73.177460
511.617610	40.001724	73.182465
510.458842	31.715146	73.187470
509.553146	36.130522	73.192474
508.993565	30.171133	73.197479
508.543316	35.420651	73.202484
508.281792	35.517205	73.207489
507.917972	28.366577	73.212494
506.562480	31.933422	73.217498
506.029291	32.906216	73.222503
505.540248	38.475785	73.227508
504.954001	24.108033	73.232513
503.663528	40.835345	73.237518
503.048289	32.011580	73.242522
502.655703	31.196304	73.247527
502.286786	43.670944	73.252532
501.804446	36.530754	73.257537
500.380928	36.259612	73.262542
499.691545	36.189496	73.267546
499.307376	29.217214	73.272551
498.870467	32.764018	73.277556
498.509747	34.437875	73.282561
497.316848	40.892221	73.287566
496.655531	27.709633	73.292570
496.444554	34.611868	73.297575
495.523165	33.999699	73.302580
494.597012	25.995356	73.307585
493.590919	32.387297	73.312590
492.893952	36.619285	73.317594
492.745543	35.944922	73.322599
492.439316	38.595832	73.327604
492.226783	29.390846	73.332609
490.969047	33.278424	73.337614
490.388470	39.787311	73.342618
489.929012	26.615528	73.347623
488.723298	28.963491	73.352628
488.103032	33.138128	73.357633
487.369729	33.833391	73.362638
486.963656	30.697536	73.367642
486.529400	30.912106	73.372647
485.313776	34.016068	73.377652
485.027803	25.755589	73.382657
484.272846	32.616441	73.387662
484.127489	37.767928	73.392666
482.495432	36.471534	73.397671
481.812323	27.965705	73.402676
481.396544	24.617975	73.407681
481.011235	33.086308	73.412686
480.653141	32.925085	73.417690
479.580537	38.463609	73.422695
478.867820	38.697477	73.427700
478.604129	27.207972	73.432705
477.737688	35.832170	73.437710
476.919038	31.798387	73.442714
476.197306	38.961820	73.447719
475.371445	38.156059	73.452724
475.180489	27.769158	73.457729
474.089271	37.470761	73.462734
473.543589	30.540368	73.467738
472.462744	35.623226	73.472743
471.485249	40.230507	73.477748
471.583910	24.663487	73.482753
470.976532	28.994985	73.487758
470.443534	32.090126	73.492762
470.455028	29.907791	73.497767
469.713354	33.279466	73.502772
469.228015	27.285654	73.507777
467.970107	31.199318	73.512782
467.093952	30.692687	73.517786
466.618781	33.875414	73.522791
465.031552	32.997242	73.527796
464.596144	28.616753	73.532801
464.192947	29.232953	73.537806
463.364675	26.062483	73.542810
462.469784	25.392101	73.547815
462.095969	25.982345	73.552820
461.617679	23.150959	73.557825
461.357349	30.696742	73.562830
460.991821	32.063548	73.567834
460.198047	33.497030	73.572839
459.282821	25.601344	73.577844
458.552715	25.004955	73.582849
457.294969	24.613845	73.587854
456.426891	24.636723	73.592858
456.278437	21.988406	73.597863
455.812684	34.231750	73.602868
455.758420	21.035542	73.607873
454.944346	32.225877	73.612878
453.589932	32.527478	73.617882
453.168513	29.155851	73.622887
452.479693	27.067474	73.627892
452.413609	28.090089	73.632897
451.267070	35.752215	73.637902
450.123596	23.203684	73.642906
449.796063	20.511850	73.647911
449.008129	24.252222	73.652916
448.850443	17.296007	73.657921
447.928731	26.543847	73.662926
446.631410	28.582275	73.667930
446.184660	28.128766	73.672935
445.766972	37.596538	73.677940
445.419065	30.138472	73.682945
445.099605	32.731260	73.687950
444.169971	31.369769	73.692954
443.323209	30.825345	73.697959
442.355111	34.768294	73.702964
442.058530	27.591944	73.707969
441.057358	37.177863	73.712974
440.085310	34.117294	73.717978
439.625759	29.318207	73.722983
439.258739	31.568639	73.727988
439.261974	31.782053	73.732993
438.232979	31.041109	73.737998
437.220153	34.873310	73.743002
436.785944	33.437183	73.748007
436.295721	30.004327	73.753012
435.845332	27.717997	73.758017
434.749411	33.352491	73.763022
433.918830	25.221268	73.768026
433.413261	19.843527	73.773031
432.236152	30.336251	73.778036
431.420084	15.325847	73.783041
430.870462	24.041004	73.788046
430.826480	25.467175	73.793050
430.248330	31.005044	73.798055
429.349763	37.444486	73.803060
429.106442	25.552840	73.808065
428.276943	36.212564	73.813070
427.275664	33.395020	73.818074
426.507621	28.665380	73.823079
426.173895	35.744560	73.828084
425.750418	22.746225	73.833089
424.186888	36.614453	73.838094
423.763057	35.719675	73.843098
423.167318	29.569537	73.848103
422.873862	27.664844	73.853108
422.974728	27.824819	73.858113
421.844900	28.117940	73.863118
420.831321	35.000619	73.868122
420.250941	34.011888	73.873127
419.903182	25.925024	73.878132
418.710482	25.176614	73.883137
417.757618	30.485033	73.888142
417.676541	30.001227	73.893146
417.182213	20.024334	73.898151
416.305328	32.245374	73.903156
415.708298	35.154926	73.908161
415.011339	41.284705	73.913166
414.569671	32.771458	73.918170
412.846279	26.025934	73.923175
412.541267	26.564131	73.928180
412.182743	34.169766	73.933185
411.708197	23.625042	73.938190
411.412921	22.418121	73.943194
410.073820	25.714959	73.948199
409.422327	32.348098	73.953204
409.035027	25.927388	73.958209
408.434505	27.741418	73.963214
407.430529	22.920778	73.968218
406.499291	26.539670	73.973223
405.787277	23.588486	73.978228
405.635630	30.821581	73.983233
404.759845	28.778279	73.988238
404.917673	24.494280	73.993242
403.957278	20.135487	73.998247
402.492484	26.772222	74.003252
401.938898	23.488380	74.008257
401.562840	28.313499	74.013262
401.210708	30.280741	74.018266
400.599211	27.735858	74.023271
399.227256	33.577128	74.028276
398.751841	22.156292	74.033281
397.898213	31.223929	74.038286
397.497971	31.285845	74.043290
397.541375	21.365213	74.048295
396.825144	33.045990	74.053300
396.116629	33.360461	74.058305
395.167398	33.189638	74.063310
394.657639	34.651031	74.068314
393.398049	24.101909	74.073319
392.718021	25.903910	74.078324
392.524877	25.233665	74.083329
391.692092	32.625726	74.088334
391.502057	22.591162	74.093338
390.639746	25.283693	74.098343
389.592204	22.735389	74.103348
389.732595	27.994206	74.108353
388.261474	30.592929	74.113358
387.334123	32.329165	74.118362
386.840462	32.549978	74.123367
385.929529	33.821192	74.128372
385.415588	27.694541	74.133377
385.275235	32.769776	74.138382
385.052657	31.602894	74.143386
384.349332	27.336223	74.148391
382.943686	27.593339	74.153396
382.836783	21.959005	74.158401
381.567613	38.735565	74.163406
380.776917	23.848315	74.168410
380.200474	29.136040	74.173415
379.499991	29.903453	74.178420
379.433541	28.632056	74.183425
378.973773	33.394160	74.188430
377.951190	27.004176	74.193434
377.056985	24.188820	74.198439
376.289385	26.025172	74.203444
376.217265	27.408011	74.208449
375.690641	25.933259	74.213454
374.494318	28.401211	74.218458
373.667448	21.983215	74.223463
372.868818	33.457865	74.228468
372.759866	16.332201	74.233473
371.896968	34.178272	74.238478
370.961854	34.002666	74.243482
370.272323	30.752388	74.248487
369.393588	28.471982	74.253492
369.342549	31.625839	74.258497
368.807510	28.968785	74.263502
368.777008	25.403075	74.268506
367.510940	23.026430	74.273511
366.599763	28.351788	74.278516
366.285677	27.030470	74.283521
365.268621	33.404177	74.288526
364.297531	32.098359	74.293530
364.047308	28.237167	74.298535
363.565783	33.924261	74.303540
362.672459	24.266401	74.308545
362.231755	30.384235	74.313550
361.240652	29.411827	74.318554
360.761574	25.624988	74.323559
359.801507	28.679652	74.328564
359.612690	24.719127	74.333569
358.807047	34.074580	74.338574
357.584273	30.088375	74.343578
356.804515	27.203281	74.348583
356.316405	30.378363	74.353588
356.371115	19.363233	74.358593
356.082599	30.366399	74.363598
355.285859	29.948805	74.368602
354.408681	29.115154	74.373607
353.317887	37.540591	74.378612
352.691166	22.523807	74.383617
351.728673	33.655511	74.388622
350.939686	26.656323	74.393626
350.747882	29.804701	74.398631
350.258849	32.959812	74.403636
350.026639	29.279865	74.408641
348.923517	34.598653	74.413646
347.899213	24.663659	74.418650
347.306522	25.362868	74.423655
346.834378	29.422925	74.428660
346.640730	23.334935	74.433665
345.681073	31.180560	74.438670
344.770350	29.891240	74.443674
344.421378	26.439320	74.448679
343.419245	32.542857	74.453684
342.522740	29.306743	74.458689
341.948034	27.175935	74.463694
341.414847	33.235414	74.468698
341.382733	27.465903	74.473703
340.381946	37.172548	74.478708
339.502766	25.202803	74.483713
338.825562	27.856118	74.488718
338.138238	37.501146	74.493722
338.065145	35.889066	74.498727
336.481817	34.392939	74.503732
335.973587	22.723151	74.508737
335.417815	30.131288	74.513742
335.045025	30.059433	74.518746
334.686112	22.603669	74.523751
333.720181	23.205806	74.528756
332.782419	28.956884	74.533761
332.000779	20.585211	74.538766
331.486883	26.988730	74.543770
331.470262	19.251290	74.548775
330.945673	25.329819	74.553780
329.843367	19.161530	74.558785
329.367003	26.638551	74.563790
328.234584	28.080753	74.568794
327.365175	23.223650	74.573799
326.674072	35.453511	74.578804
326.537867	28.376788	74.583809
325.787700	27.722677	74.588814
325.203823	22.562442	74.593818
324.348089	22.201540	74.598823
323.192993	24.514026	74.603828
322.775413	15.803267	74.608833
322.278176	22.680348	74.613838
321.986046	19.023701	74.618842
321.183364	22.228622	74.623847
320.133433	27.781440	74.628852
319.523528	22.611457	74.633857
319.085286	28.692555	74.638862
319.134527	31.084005	74.643866
317.764507	22.602402	74.648871
316.577815	35.626898	74.653876
316.297261	27.923640	74.658881
315.664914	27.734045	74.663886
315.205939	37.162315	74.668890
314.865780	22.053010	74.673895
313.725285	39.885089	74.678900
312.712918	21.484621	74.683905
312.466879	27.121486	74.688910
312.181328	21.544618	74.693914
311.153305	21.583489	74.698919
310.253983	28.643165	74.703924
309.803145	25.603421	74.708929
309.238253	31.552290	74.713934
308.901053	30.750828	74.718938
308.143223	25.776715	74.723943
306.837043	40.877361	74.728948
306.586456	30.955414	74.733953
306.313722	31.323490	74.738958
305.505921	29.397233	74.743962
304.397375	19.611292	74.748967
303.786605	30.275765	74.753972
303.354071	19.745180	74.758977
302.575491	33.090887	74.763982
301.361202	34.654490	74.768986
300.844116	23.242792	74.773991
299.837353	33.529903	74.778996
299.630847	25.342274	74.784001
299.399215	27.790942	74.789006
298.685899	26.671864	74.794010
298.862164	18.216145	74.799015
296.941482	32.312176	74.804020
296.935855	26.534576	74.809025
296.130352	35.310176	74.814030
295.266488	31.921645	74.819034
294.534086	35.038347	74.824039
293.827983	34.090917	74.829044
293.447687	28.520025	74.834049
292.945156	30.387926	74.839054
292.128831	36.816840	74.844058
291.306916	27.656731	74.849063
290.318383	28.051184	74.854068
290.245949	27.236314	74.859073
289.727009	30.876921	74.864078
288.727663	28.417085	74.869082
288.618895	22.812682	74.874087
287.676048	25.723494	74.879092
286.711925	24.139805	74.884097
286.286375	29.082746	74.889102
285.472505	31.518717	74.894106
285.230967	27.184757	74.899111
283.685990	31.355285	74.904116
283.232540	30.131671	74.909121
282.559757	32.512673	74.914126
282.030045	27.964043	74.919130
281.692352	19.968632	74.924135
280.519229	24.994314	74.929140
280.121581	24.902646	74.934145
279.448574	31.332257	74.939150
278.847881	37.126618	74.944154
278.575076	29.004824	74.949159
277.316459	43.120409	74.954164
276.440067	29.015199	74.959169
275.880446	30.828944	74.964174
275.353393	29.983057	74.969178
275.530092	29.818601	74.974183
274.112124	34.027754	74.979188
272.935641	32.992804	74.984193
272.528571	34.690802	74.989198
271.948360	34.993957	74.994202
271.726399	28.458486	74.999207
271.071583	31.276909	75.004212
270.035784	36.727058	75.009217
269.590216	32.276500	75.014222
269.078475	32.162549	75.019226
268.657744	27.622477	75.024231
267.367125	34.187159	75.029236
266.551234	29.231296	75.034241
266.140177	38.275191	75.039246
265.627334	33.268567	75.044250
265.442943	35.430867	75.049255
264.905670	42.417446	75.054260
263.940253	31.595723	75.059265
263.195492	34.547584	75.064270
261.537088	33.299205	75.069274
260.554882	29.496388	75.074279
260.628956	36.905118	75.079284
260.817776	29.100888	75.084289
259.642324	33.538065	75.089294
258.802067	35.077039	75.094298
258.846569	33.072987	75.099303
257.474190	41.557362	75.104308
256.784305	27.012454	75.109313
256.195892	30.037773	75.114318
255.824096	31.604206	75.119322
255.358574	33.542342	75.124327
254.276817	40.596592	75.129332
253.620527	34.357396	75.134337
252.814063	37.511270	75.139342
252.625996	22.966794	75.144346
252.008502	20.351522	75.149351
250.767667	23.212371	75.154356
250.648109	22.925417	75.159361
249.662693	30.815729	75.164366
249.151455	30.028314	75.169370
248.539008	21.708578	75.174375
247.273529	31.309425	75.179380
246.803646	27.058817	75.184385
246.523961	24.627995	75.189390
245.541786	29.247557	75.194394
245.882901	20.355056	75.199399
244.818342	32.877074	75.204404
243.983584	28.760057	75.209409
243.332879	25.666560	75.214414
241.959997	27.559711	75.219418
241.327457	14.597261	75.224423
240.362099	30.189319	75.229428
240.194141	29.948159	75.234433
240.195251	25.997717	75.239438
239.336067	30.694482	75.244442
239.090333	20.145312	75.249447
237.879303	22.894088	75.254452
237.389809	24.818571	75.259457
236.900303	32.536255	75.264462
235.572355	34.428023	75.269466
234.680433	24.447481	75.274471
233.927676	37.459576	75.279476
234.160002	24.640170	75.284481
233.532570	25.153517	75.289486
232.885858	25.530836	75.294490
231.938087	17.112672	75.299495
230.906536	30.270833	75.304500
230.656169	23.392101	75.309505
230.102332	27.410907	75.314510
229.286584	27.474590	75.319514
228.569612	25.754608	75.324519
227.374989	28.292561	75.329524
227.032541	27.343594	75.334529
226.692503	26.753401	75.339534
226.292807	26.421709	75.344538
225.839649	20.813585	75.349543
224.729363	28.869769	75.354548
224.102196	22.456655	75.359553
223.636259	21.944882	75.364558
222.124823	29.525915	75.369562
221.501621	27.865250	75.374567
220.949067	33.672676	75.379572
220.650778	33.831992	75.384577
220.450750	21.429313	75.389582
219.876336	35.344726	75.394586
218.908850	33.490855	75.399591
218.219028	27.905140	75.404596
217.610622	33.675564	75.409601
216.209788	38.295850	75.414606
215.574828	35.558451	75.419610
214.963435	29.672731	75.424615
214.511546	38.864143	75.429620
214.247006	30.562532	75.434625
213.780009	31.858331	75.439630
213.132911	32.931202	75.444634
212.269190	27.865926	75.449639
211.605118	34.140862	75.454644
210.758600	36.055894	75.459649
209.929883	27.844284	75.464654
208.965024	30.433245	75.469658
208.637940	25.503337	75.474663
208.009550	33.059314	75.479668
207.764774	25.777809	75.484673
207.099717	26.033941	75.489678
206.048100	31.009997	75.494682
205.389241	20.441655	75.499687
204.644201	37.022206	75.504692
204.743566	32.692181	75.509697
203.213287	34.114592	75.514702
202.564590	35.266286	75.519706
202.171485	25.193143	75.524711
201.637236	26.929523	75.529716
201.250537	26.235628	75.534721
200.282599	28.911955	75.539726
198.946305	32.327175	75.544730
199.149934	24.916703	75.549735
198.543837	25.686118	75.554740
198.051431	29.785576	75.559745
196.979481	31.014561	75.564750
195.816733	35.294451	75.569754
195.654436	28.144456	75.574759
194.735779	27.876071	75.579764
194.405989	27.888429	75.584769
193.403749	32.086334	75.589774
192.293384	30.151179	75.594778
192.143222	32.038813	75.599783
191.991855	42.166677	75.604788
191.193060	29.803088	75.609793
190.120018	24.574765	75.614798
189.421383	32.034634	75.619802
189.266540	22.579032	75.624807
188.792864	30.245848	75.629812
187.677491	24.239304	75.634817
187.203827	29.169576	75.639822
186.244310	24.175594	75.644826
186.130335	26.721325	75.649831
184.628548	40.217459	75.654836
184.264968	36.780689	75.659841
183.835337	31.927963	75.664846
183.393919	35.155840	75.669850
182.591977	26.819655	75.674855
181.330381	28.053523	75.679860
180.728920	25.741020	75.684865
180.176022	31.621923	75.689870
179.859239	37.783254	75.694874
179.699157	25.857649	75.699879
178.424533	28.584185	75.704884
177.746890	25.151523	75.709889
177.394737	27.831630	75.714894
176.195575	32.007641	75.719898
175.055678	32.977900	75.724903
174.358148	36.289943	75.729908
174.893275	25.995319	75.734913
174.172729	29.229600	75.739918
173.555485	30.025401	75.744922
172.657786	24.152458	75.749927
171.891813	30.494598	75.754932
171.534294	31.061546	75.759937
170.493120	22.143126	75.764942
169.242848	35.210113	75.769946
168.520186	28.859165	75.774951
168.094264	24.698922	75.779956
167.711206	23.412337	75.784961
167.357847	24.263554	75.789966
166.781402	28.530962	75.794970
166.557330	25.241193	75.799975
165.201035	30.173965	75.804980
164.814908	25.529298	75.809985
163.919228	28.049175	75.814990
162.766152	34.841733	75.819994
162.425853	24.417330	75.824999
161.661969	33.273431	75.830004
161.001277	29.747476	75.835009
160.812262	31.387181	75.840014
160.003802	32.444697	75.845018
159.172791	22.787664	75.850023
158.239091	38.068403	75.855028
157.562569	31.935322	75.860033
157.316879	34.004322	75.865038
156.890472	31.743124	75.870042
156.026651	30.782099	75.875047
155.150443	33.684274	75.880052
154.616410	29.060226	75.885057
154.226656	24.978253	75.890062
153.388336	20.345191	75.895066
152.559528	23.750392	75.900071
152.132333	21.739578	75.905076
151.596613	22.570745	75.910081
151.283288	29.020015	75.915086
150.050037	24.842657	75.920090
149.432072	19.486601	75.925095
149.037654	30.666189	75.930100
147.948007	21.975940	75.935105
147.167500	28.061247	75.940110
146.162767	23.624072	75.945114
145.947650	24.118849	75.950119
145.075302	24.937072	75.955124
145.059013	19.938105	75.960129
144.247129	24.050888	75.965134
143.190068	25.987419	75.970138
142.667550	21.603755	75.975143
142.047337	24.022336	75.980148
141.429382	24.465390	75.985153
140.618447	24.761144	75.990158
139.414819	29.996546	75.995162
139.131573	27.773568	76.000167
138.638095	31.986890	76.005172
138.401858	30.833812	76.010177
137.983403	25.091470	76.015182
136.893654	30.287220	76.020186
136.013325	17.619102	76.025191
135.638375	33.648734	76.030196
135.096030	26.321941	76.035201
133.992600	27.268591	76.040206
132.986792	31.307654	76.045210
132.871076	25.803132	76.050215
132.131342	31.444111	76.055220
131.929131	26.035728	76.060225
131.002236	27.860348	76.065230
129.845590	31.896851	76.070234
129.646957	26.522195	76.075239
129.012250	31.416530	76.080244
128.189997	33.880802	76.085249
127.393846	33.509328	76.090254
126.220711	32.912369	76.095258
126.263585	30.439679	76.100263
125.727914	32.279331	76.105268
125.181963	29.660891	76.110273
124.294203	27.703381	76.115278
123.496632	41.690603	76.120282
122.960771	18.826825	76.125287
122.380136	29.345221	76.130292
121.757005	33.248424	76.135297
120.932477	30.236849	76.140302
119.917829	26.788555	76.145306
119.640879	28.056913	76.150311
119.381563	28.894774	76.155316
118.119380	23.859940	76.160321
117.412283	25.663458	76.165326
116.627381	27.877002	76.170330
116.294432	25.527555	76.175335
116.051448	30.317238	76.180340
115.220181	31.145790	76.185345
114.518116	32.075739	76.190350
113.385263	26.993472	76.195354
113.114256	20.076061	76.200359
112.672704	36.438802	76.205364
111.945512	29.298034	76.210369
110.924261	29.523277	76.215374
110.675102	39.031227	76.220378
110.012652	26.123271	76.225383
108.697315	29.287830	76.230388
108.028513	37.395446	76.235393
107.468733	32.255193	76.240398
106.731624	29.594927	76.245402
106.717667	26.197698	76.250407
106.081192	27.006672	76.255412
104.873504	24.491026	76.260417
104.225678	27.123148	76.265422
103.579194	30.929704	76.270426
103.218201	19.985475	76.275431
102.570554	32.130917	76.280436
101.919772	35.088001	76.285441
101.193692	28.734496	76.290446
100.498664	39.761165	76.295450
100.184624	21.470393	76.300455
99.025451	24.998946	76.305460
98.314101	41.218878	76.310465
97.475566	34.117330	76.315470
97.161605	35.107052	76.320474
96.760381	30.652864	76.325479
95.702095	31.357324	76.330484
95.034549	27.861765	76.335489
94.420989	24.143807	76.340494
93.948073	33.452103	76.345498
93.660785	22.723381	76.350503
92.403094	24.949303	76.355508
91.463625	28.997920	76.360513
91.610790	27.787798	76.365518
90.564127	28.557762	76.370522
90.244171	28.072683	76.375527
89.311664	28.322188	76.380532
88.676386	25.169234	76.385537
88.295612	33.188787	76.390542
87.091593	37.481302	76.395546
86.440106	30.215857	76.400551
85.893919	34.714913	76.405556
85.763230	34.477631	76.410561
84.805732	24.875460	76.415566
83.324421	33.827330	76.420570
82.937464	29.438588	76.425575
82.384593	26.292822	76.430580
81.866991	29.965186	76.435585
81.546842	30.758614	76.440590
80.963044	38.744296	76.445594
80.177821	28.393818	76.450599
79.160719	32.710336	76.455604
78.577913	24.143991	76.460609
78.220824	16.980440	76.465614
76.967070	33.920947	76.470618
76.453908	23.038728	76.475623
75.809023	32.430977	76.480628
75.413035	32.136160	76.485633
75.217523	30.301147	76.490638
73.977440	37.297705	76.495642
73.609801	32.832630	76.500647
72.542800	30.612984	76.505652
72.434255	28.087313	76.510657
71.565859	25.560477	76.515662
70.296277	47.167630	76.520666
70.014701	32.332128	76.525671
69.328049	28.934580	76.530676
68.898580	29.559262	76.535681
68.024371	28.657268	76.540686
66.916013	28.905349	76.545690
66.245125	23.912437	76.550695
65.806420	31.331301	76.555700
65.436835	32.886711	76.560705
65.520444	29.720240	76.565710
64.521440	36.389300	76.570714
63.900824	28.145209	76.575719
63.117959	31.803451	76.580724
62.325779	33.079231	76.585729
61.273932	30.434647	76.590734
60.015783	36.916048	76.595738
60.044352	30.617894	76.600743
59.352296	31.141554	76.605748
59.175677	28.586505	76.610753
58.638430	33.448744	76.615758
57.852963	25.223840	76.620762
56.761191	20.948840	76.625767
56.470087	30.036106	76.630772
55.375794	31.516437	76.635777
54.597291	24.139761	76.640782
53.471655	29.707182	76.645786
52.991330	30.701351	76.650791
53.055270	27.047231	76.655796
52.303405	26.749094	76.660801
52.196862	28.098363	76.665806
51.247524	30.447470	76.670810
50.415724	21.179396	76.675815
49.705607	32.785322	76.680820
49.217887	35.706955	76.685825
48.262053	30.140438	76.690830
47.322244	27.857547	76.695834
47.110298	22.932786	76.700839
46.399265	25.692586	76.705844
45.467637	24.968589	76.710849
44.665150	20.834639	76.715854
43.844411	32.986077	76.720858
43.608517	22.377624	76.725863
43.124186	38.776510	76.730868
42.871138	20.516743	76.735873
41.962176	25.049578	76.740878
41.054709	30.849579	76.745882
40.607744	30.374044	76.750887
40.355237	33.569540	76.755892
39.046426	27.807377	76.760897
38.590111	22.442572	76.765902
37.981604	31.077053	76.770906
36.871328	30.838001	76.775911
35.860954	34.798922	76.780916
35.059161	32.885503	76.785921
34.715155	23.980612	76.790926
34.148663	34.818277	76.795930
34.000805	29.096656	76.800935
33.724278	30.092989	76.805940
32.758330	33.892356	76.810945
31.873683	29.379756	76.815950
31.133705	29.152210	76.820954
30.560236	33.278208	76.825959
29.505648	31.236433	76.830964
28.555092	31.776000	76.835969
28.206157	30.678170	76.840974
27.514501	36.395386	76.845978
27.065684	32.532357	76.850983
26.708646	32.343359	76.855988
25.837210	30.926984	76.860993
25.111387	30.117181	76.865998
24.195374	35.863786	76.871002
23.868920	33.236540	76.876007
23.875833	30.428592	76.881012
22.542320	31.685489	76.886017
22.293957	27.681916	76.891022
21.276788	33.897809	76.896026
20.758252	23.882917	76.901031
19.627196	32.389113	76.906036
18.824343	29.954070	76.911041
18.566062	32.175224	76.916046
17.766330	30.945885	76.921050
17.622987	35.062474	76.926055
16.629690	40.230264	76.931060
15.583046	34.131465	76.936065
15.196017	22.553071	76.941070
14.524590	27.173465	76.946074
14.283181	22.101006	76.951079
13.026806	38.103744	76.956084
12.168962	28.052691	76.961089
11.879785	22.158739	76.966094
11.001860	38.697734	76.971098
11.095012	24.877934	76.976103
10.606744	27.674144	76.981108
9.703157	31.047586	76.986113
8.837137	25.881708	76.991118
7.464067	36.314547	76.996122
6.863537	21.335217	77.001127
6.136026	34.416007	77.006132
5.963326	28.088423	77.011137
5.627942	28.152278	77.016142
5.286658	38.598854	77.021147
4.560093	28.792515	77.026151
3.306404	31.221839	77.031156
2.378880	28.955798	77.036161