Tue Jun 08 17:27:06 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-1.063815	103.594573	0.000000
-1.282808	97.564191	0.005005
-1.805698	64.610078	0.010010
-3.200331	11.297500	0.015014
-7.265850	-12.597075	0.020019
-12.624274	-14.597192	0.025024
-18.298149	-11.621967	0.030029
-22.868289	-13.776181	0.035034
-26.976727	-12.611102	0.040038
-30.877831	2.036074	0.045043
-34.274370	-0.183585	0.050048
-37.401478	0.197883	0.055053
-41.408957	-7.768197	0.060058
-45.265879	-7.850885	0.065062
-49.259644	-2.691641	0.070067
-52.926526	-5.764472	0.075072
-56.478462	-7.238699	0.080077
-60.827376	-2.180773	0.085082
-64.304330	-6.544893	0.090086
-68.149641	5.376744	0.095091
-71.712752	-7.186123	0.100096
-75.125723	-8.261035	0.105101
-79.202929	-4.339873	0.110106
-82.467723	-6.699708	0.115110
-86.735132	-2.317269	0.120115
-90.529766	0.013315	0.125120
-94.166726	-6.562534	0.130125
-98.061285	-5.611687	0.135130
-101.755833	-12.568415	0.140134
-105.291398	0.459392	0.145139
-108.891384	-0.838802	0.150144
-112.817527	-3.867124	0.155149
-116.719038	-0.065263	0.160154
-120.534607	-9.026085	0.165158
-124.627745	-5.580146	0.170163
-128.106054	-9.773072	0.175168
-131.499782	-7.097550	0.180173
-135.581723	-3.255654	0.185178
-139.523982	-14.546409	0.190182
-143.461235	-12.158959	0.195187
-146.778306	-13.151584	0.200192
-150.878022	-3.430979	0.205197
-154.852078	-1.054179	0.210202
-158.312389	-6.623363	0.215206
-162.014402	-2.539516	0.220211
-165.671126	-3.271787	0.225216
-169.481830	-3.228884	0.230221
-173.607000	7.161197	0.235226
-176.936536	-4.300921	0.240230
-180.554438	0.788051	0.245235
-184.435496	-6.144513	0.250240
-188.356706	-8.263017	0.255245
-191.973872	-6.324342	0.260250
-195.788189	-5.358360	0.265254
-199.661027	1.855653	0.270259
-203.243995	0.173327	0.275264
-207.013120	0.873823	0.280269
-210.974646	-6.720659	0.285274
-214.765564	-13.532871	0.290278
-218.589337	-3.707969	0.295283
-222.093817	0.097327	0.300288
-225.734532	-4.709070	0.305293
-229.695939	2.571075	0.310298
-233.468863	-6.723775	0.315302
-237.325221	-2.394334	0.320307
-240.857525	-11.986609	0.325312
-244.122191	-7.471693	0.330317
-248.815695	-8.708131	0.335322
-252.430466	-5.738442	0.340326
-256.283385	1.064858	0.345331
-259.965238	3.403866	0.350336
-263.204448	-6.748233	0.355341
-267.069013	-2.719313	0.360346
-270.881304	-10.438008	0.365350
-275.239132	0.856469	0.370355
-278.634884	-0.651474	0.375360
-282.295526	-8.612472	0.380365
-286.117592	-4.680030	0.385370
-289.607756	-11.032217	0.390374
-293.726036	-6.051532	0.395379
-297.408670	-7.700107	0.400384
-301.370455	-0.844153	0.405389
-305.483050	1.389577	0.410394
-308.568059	-6.710395	0.415398
-312.540195	-0.404855	0.420403
-315.955803	-1.074948	0.425408
-319.611617	-6.181020	0.430413
-323.760898	-1.087629	0.435418
-327.395557	-8.578207	0.440422
-331.649138	-5.341393	0.445427
-335.131248	2.777872	0.450432
-338.670827	-8.058772	0.455437
-342.567168	-3.480431	0.460442
-346.018538	-7.392030	0.465446
-350.194129	-2.058462	0.470451
-354.032346	-3.950282	0.475456
-357.495922	-11.072313	0.480461
-361.404691	-6.827328	0.485466
-364.893725	-4.555652	0.490470
-369.050604	-7.690598	0.495475
-372.571096	-5.461280	0.500480
-376.413504	-11.424176	0.505485
-380.521380	-7.196726	0.510490
-383.821222	-6.852488	0.515494
-387.541075	3.550727	0.520499
-391.346034	-7.822935	0.525504
-395.362297	-4.113256	0.530509
-399.366398	-5.584633	0.535514
-402.258773	-6.880828	0.540518
-406.521162	-5.351521	0.545523
-410.012922	-11.604655	0.550528
-414.275637	-11.842001	0.555533
-418.049395	3.917995	0.560538
-421.317822	-10.275117	0.565542
-425.344531	-3.083870	0.570547
-429.022739	-9.027127	0.575552
-433.055567	-1.552213	0.580557
-436.620356	1.112619	0.585562
-439.796971	-6.590247	0.590566
-443.894518	1.567970	0.595571
-447.744320	-6.393187	0.600576
-451.566795	-0.674089	0.605581
-455.772245	-4.306240	0.610586
-459.356835	-7.970697	0.615590
-463.377465	-2.229435	0.620595
-466.759803	-6.058444	0.625600
-470.158014	-10.652039	0.630605
-474.343589	-1.848347	0.635610
-477.840435	-11.367157	0.640614
-482.014604	-1.670611	0.645619
-485.709034	-3.206485	0.650624
-489.150264	-15.824206	0.655629
-493.045248	-8.059101	0.660634
-496.750662	-11.429262	0.665638
-500.277842	-8.138513	0.670643
-504.537888	-3.222920	0.675648
-507.743299	-7.833775	0.680653
-512.319739	0.579546	0.685658
-515.713521	-2.945904	0.690662
-519.393492	-2.277417	0.695667
-523.122377	9.397226	0.700672
-526.894015	-1.847034	0.705677
-530.719551	7.072161	0.710682
-534.328783	-0.910457	0.715686
-538.201367	3.869615	0.720691
-541.868863	4.902270	0.725696
-545.500606	9.039490	0.730701
-549.388081	15.057962	0.735706
-553.186456	-1.077649	0.740710
-556.942437	6.485254	0.745715
-560.796209	-1.443539	0.750720
-564.351053	9.716175	0.755725
-568.428982	11.562117	0.760730
-571.875280	-1.986181	0.765734
-575.968863	7.893186	0.770739
-579.429702	6.077721	0.775744
-583.250154	0.480693	0.780749
-587.324923	9.086671	0.785754
-590.858247	0.937537	0.790758
-594.776914	4.092657	0.795763
-598.515457	-3.146187	0.800768
-602.244993	4.184861	0.805773
-606.053513	8.426668	0.810778
-609.752406	-2.650400	0.815782
-613.195670	8.262058	0.820787
-616.949525	3.142676	0.825792
-620.889990	7.053872	0.830797
-624.686908	12.229951	0.835802
-628.191977	8.100837	0.840806
-632.405661	6.713793	0.845811
-636.114633	3.493165	0.850816
-639.894689	2.470238	0.855821
-643.381537	11.105628	0.860826
-647.181606	-4.340430	0.865830
-651.122863	8.547372	0.870835
-654.766293	3.653399	0.875840
-658.467271	0.238803	0.880845
-662.759178	-1.766714	0.885850
-665.973491	9.132146	0.890854
-669.979161	12.440804	0.895859
-673.731839	5.869930	0.900864
-677.111515	5.056989	0.905869
-680.925010	5.692872	0.910874
-684.520412	-5.585421	0.915878
-688.721780	9.056131	0.920883
-692.549197	0.558904	0.925888
-696.472003	-1.089954	0.930893
-699.927348	-5.866173	0.935898
-703.295824	-8.810460	0.940902
-707.328842	3.474227	0.945907
-711.018696	3.786570	0.950912
-714.913787	-2.834026	0.955917
-719.081459	9.114601	0.960922
-722.697804	-1.081329	0.965926
-726.212071	5.456611	0.970931
-729.926109	1.262405	0.975936
-733.794189	3.182606	0.980941
-737.636543	13.142931	0.985946
-741.257237	1.215391	0.990950
-745.217735	6.423983	0.995955
-748.817886	-6.082947	1.000960
-752.469735	3.731407	1.005965
-756.412840	5.630165	1.010970
-759.999023	-2.799458	1.015974
-763.955092	0.517346	1.020979
-767.491948	2.417831	1.025984
-771.653676	5.752179	1.030989
-775.529730	12.291467	1.035994
-778.602358	-8.369844	1.040998
-782.512584	7.145426	1.046003
-786.567855	11.081996	1.051008
-790.108598	6.526939	1.056013
-794.122986	9.696687	1.061018
-797.741027	1.669245	1.066022
-801.462393	-2.715860	1.071027
-805.406589	8.332045	1.076032
-808.887369	7.576032	1.081037
-812.836109	13.341176	1.086042
-816.614692	-0.432470	1.091046
-820.272888	-2.981172	1.096051
-823.842884	1.851798	1.101056
-827.442892	4.139721	1.106061
-831.500421	5.188252	1.111066
-835.320080	0.107207	1.116070
-839.318445	2.643897	1.121075
-842.719020	-5.725541	1.126080
-846.531030	-0.648922	1.131085
-850.802830	0.980312	1.136090
-854.211768	-0.416764	1.141094
-858.138382	-1.368161	1.146099
-861.614372	-2.608468	1.151104
-865.036664	4.134427	1.156109
-868.981171	0.087268	1.161114
-872.663030	-4.377970	1.166118
-876.921709	5.797202	1.171123
-880.352462	-5.391149	1.176128
-883.984538	-3.008473	1.181133
-888.075638	0.969070	1.186138
-891.997904	-12.048431	1.191142
-895.713050	-4.495435	1.196147
-899.300177	-4.387657	1.201152
-903.175173	-0.365097	1.206157
-906.935803	-0.304496	1.211162
-910.852271	-2.312637	1.216166
-914.365775	5.259048	1.221171
-917.985129	-5.407062	1.226176
-921.442950	-3.603306	1.231181
-925.831654	7.957153	1.236186
-929.402913	0.937778	1.241190
-933.403854	2.529673	1.246195
-936.817959	-4.393918	1.251200
-940.670844	-10.563281	1.256205
-944.607054	4.215308	1.261210
-948.362637	-1.943916	1.266214
-951.879110	7.826427	1.271219
-955.493711	3.625221	1.276224
-959.206824	1.653656	1.281229
-962.943738	3.063682	1.286234
-966.798388	4.312755	1.291238
-970.983983	-1.180170	1.296243
-974.775571	0.668299	1.301248
-978.162255	0.627266	1.306253
-982.227602	-2.865789	1.311258
-985.512151	3.079921	1.316262
-989.398002	-0.780234	1.321267
-993.467259	3.342460	1.326272
-997.108519	1.428061	1.331277
-1001.272363	0.445688	1.336282
-1004.546981	-4.898099	1.341286
-1008.140235	-12.629222	1.346291
-1012.309808	-1.961248	1.351296
-1015.740556	1.292427	1.356301
-1019.926285	-4.979967	1.361306
-1023.287095	-2.384823	1.366310
-1027.190618	-5.182515	1.371315
-1030.848873	-2.505509	1.376320
-1034.349542	-9.885428	1.381325
-1038.765619	6.298283	1.386330
-1042.627727	4.975219	1.391334
-1046.276903	-0.490527	1.396339
-1049.764115	-1.659679	1.401344
-1053.090050	-2.596408	1.406349
-1057.372964	5.486801	1.411354
-1060.908785	-5.073917	1.416358
-1064.967778	2.087104	1.421363
-1068.404859	1.636802	1.426368
-1072.184160	1.946656	1.431373
-1075.945159	3.621027	1.436378
-1079.542865	-4.869867	1.441382
-1083.525617	-1.134942	1.446387
-1087.853763	0.934034	1.451392
-1091.398592	8.199412	1.456397
-1095.324361	8.774417	1.461402
-1098.357975	-3.413432	1.466406
-1102.017676	-2.833190	1.471411
-1106.122266	3.982830	1.476416
-1109.742061	2.596513	1.481421
-1114.007492	2.333876	1.486426
-1117.434262	0.542213	1.491430
-1121.328164	-1.993379	1.496435
-1125.128773	-0.010609	1.501440
-1128.366348	-6.834090	1.506445
-1132.190306	-0.408447	1.511450
-1135.881920	-3.148880	1.516454
-1140.092496	7.407445	1.521459
-1143.914288	8.419341	1.526464
-1147.522645	-2.990088	1.531469
-1151.564569	6.678011	1.536474
-1154.911663	3.382288	1.541478
-1158.603534	-2.012475	1.546483
-1162.603392	-6.039580	1.551488
-1166.149424	2.626868	1.556493
-1170.778319	3.382287	1.561498
-1173.983609	-0.731129	1.566502
-1177.614209	-1.926862	1.571507
-1181.411957	-2.302899	1.576512
-1184.760013	-3.535305	1.581517
-1189.103261	0.014537	1.586522
-1192.930867	-1.155641	1.591526
-1196.470716	-9.768453	1.596531
-1200.196448	-5.054882	1.601536
-1203.771035	-9.773876	1.606541
-1207.884560	1.077655	1.611546
-1211.332977	-2.785573	1.616550
-1215.207264	-5.581397	1.621555
-1219.132870	1.464491	1.626560
-1222.808653	-9.255571	1.631565
-1226.593941	-2.752814	1.636570
-1230.482481	-2.166710	1.641574
-1233.777313	2.381317	1.646579
-1237.833517	-1.566570	1.651584
-1241.352317	-3.714136	1.656589
-1245.180238	-9.228728	1.661594
-1249.155513	-10.094435	1.666598
-1252.919090	-11.082541	1.671603
-1256.980711	-7.374176	1.676608
-1260.354195	-11.289304	1.681613
-1263.931171	1.369050	1.686618
-1267.470600	-0.459188	1.691622
-1271.818770	-6.152408	1.696627
-1275.521417	3.062031	1.701632
-1279.042893	-3.334832	1.706637
-1283.319182	2.372113	1.711642
-1286.860262	-10.940944	1.716646
-1290.385446	-6.897217	1.721651
-1294.296120	1.238713	1.726656
-1297.646185	-4.886807	1.731661
-1301.693414	12.394218	1.736666
-1305.185651	-6.617283	1.741670
-1309.159400	-5.988843	1.746675
-1312.919336	-5.626841	1.751680
-1316.767409	-0.308784	1.756685
-1320.774836	0.924218	1.761690
-1324.204496	-4.223739	1.766694
-1328.096282	-4.728347	1.771699
-1331.763094	4.877449	1.776704
-1335.252430	-1.022425	1.781709
-1339.425807	-0.608331	1.786714
-1343.069716	-1.168133	1.791718
-1347.005477	6.538373	1.796723
-1350.881264	3.909500	1.801728
-1354.612536	-3.065024	1.806733
-1358.280956	6.068608	1.811738
-1361.973579	-0.108140	1.816742
-1365.951688	-2.529174	1.821747
-1369.586502	-1.353025	1.826752
-1372.894340	-9.377156	1.831757
-1377.078580	11.184957	1.836762
-1380.656972	1.590195	1.841766
-1384.612828	16.023588	1.846771
-1387.983957	2.066082	1.851776
-1391.903511	2.427154	1.856781
-1396.059451	-4.218612	1.861786
-1399.836767	-5.291455	1.866790
-1403.336929	1.076427	1.871795
-1406.784299	0.628171	1.876800
-1410.319948	-9.206377	1.881805
-1414.602024	-3.164000	1.886810
-1418.274093	-6.141592	1.891814
-1422.166380	-6.283687	1.896819
-1425.965543	-6.045492	1.901824
-1429.606924	-2.092604	1.906829
-1433.407660	-0.477009	1.911834
-1437.118183	2.417721	1.916838
-1441.010336	-2.004552	1.921843
-1444.634482	-0.787938	1.926848
-1448.407324	-15.179212	1.931853
-1452.272794	1.669675	1.936858
-1455.959469	-7.734709	1.941862
-1459.703214	-2.939278	1.946867
-1463.476269	2.577580	1.951872
-1467.048575	-5.403403	1.956877
-1471.177583	1.503975	1.961882
-1474.687439	-10.984985	1.966886
-1478.343705	0.671176	1.971891
-1482.724228	-5.544367	1.976896
-1486.278507	-10.668007	1.981901
-1490.029226	2.581233	1.986906
-1493.252871	-4.509969	1.991910
-1497.080225	-2.839617	1.996915
-1501.055807	-5.682851	2.006912
-1502.203421	-0.607236	2.016909
-1499.947988	-1.647232	2.026906
-1497.149347	2.054046	2.036902
-1494.602555	3.741529	2.046899
-1492.720420	1.050462	2.056896
-1490.919941	-0.272983	2.066893
-1489.120161	7.123595	2.076890
-1487.273564	6.240791	2.086886
-1485.100193	3.967225	2.096883
-1483.267419	-0.382351	2.106880
-1481.489949	-4.512964	2.116877
-1479.513981	0.588402	2.126874
-1477.760107	3.978334	2.136870
-1475.961470	-4.156224	2.146867
-1473.601408	-0.396577	2.156864
-1471.450756	-1.667933	2.166861
-1470.096812	-0.700693	2.176858
-1468.636959	-9.486049	2.186854
-1466.293334	-11.179044	2.196851
-1464.434705	-3.509994	2.206848
-1462.276246	0.106054	2.216845
-1460.483396	-0.271121	2.226842
-1458.897017	-1.916227	2.236838
-1457.074711	-6.487682	2.246835
-1454.954744	-3.857783	2.256832
-1453.227954	-3.224122	2.266829
-1451.193891	-2.633763	2.276826
-1449.308805	-3.943665	2.286822
-1447.178182	-4.905280	2.296819
-1445.438280	-4.298372	2.306816
-1443.811622	6.704616	2.316813
-1441.610207	0.982792	2.326810
-1439.984410	-5.094635	2.336806
-1438.242050	-3.960936	2.346803
-1435.989362	-4.895299	2.356800
-1434.196711	-8.029016	2.366797
-1432.456331	-1.256915	2.376794
-1430.533076	-7.279917	2.386790
-1428.695675	-7.527594	2.396787
-1426.643141	-4.245462	2.406784
-1425.054834	-5.763628	2.416781
-1422.848298	-3.595566	2.426778
-1420.923642	-0.438085	2.436774
-1419.202709	0.714321	2.446771
-1417.440087	-7.204566	2.456768
-1415.540109	2.591937	2.466765
-1413.340298	3.696861	2.476762
-1411.959448	-1.015713	2.486758
-1409.720846	-4.543776	2.496755
-1407.681292	-6.673776	2.506752
-1406.027527	1.364847	2.516749
-1404.509134	3.668916	2.526746
-1402.246583	-0.684109	2.536742
-1400.444470	-1.685701	2.546739
-1398.586813	-3.799863	2.556736
-1396.574665	-2.997437	2.566733
-1394.974513	-1.024368	2.576730
-1392.782104	-1.957049	2.586726
-1390.852113	-2.207573	2.596723
-1388.922373	-4.586652	2.606720
-1387.539759	-3.707303	2.616717
-1385.546352	-1.975280	2.626714
-1383.366593	-6.770539	2.636710
-1381.354270	-4.992362	2.646707
-1379.753048	-2.822657	2.656704
-1378.161950	-5.011562	2.666701
-1375.836142	1.276653	2.676698
-1374.188615	-1.098603	2.686694
-1372.303001	-1.217004	2.696691
-1370.133743	-1.920427	2.706688
-1368.518833	-6.325013	2.716685
-1366.525910	-1.278667	2.726682
-1365.100435	-1.741692	2.736678
-1362.958916	2.824246	2.746675
-1360.894992	-0.343393	2.756672
-1358.887798	-3.097776	2.766669
-1357.060203	0.971164	2.776666
-1355.367351	3.382818	2.786662
-1353.478011	-1.411945	2.796659
-1351.567099	2.501202	2.806656
-1349.740711	0.251341	2.816653
-1347.804344	0.978281	2.826650
-1345.834949	3.878343	2.836646
-1344.081400	-3.726352	2.846643
-1342.092180	4.839595	2.856640
-1340.397044	-1.379340	2.866637
-1338.594247	-0.787142	2.876634
-1336.574815	2.196809	2.886630
-1334.752334	2.939761	2.896627
-1332.721735	-3.286600	2.906624
-1330.704741	-6.681708	2.916621
-1329.013221	-3.743396	2.926618
-1326.915579	-3.889105	2.936614
-1325.355174	-2.385015	2.946611
-1323.619979	-8.257504	2.956608
-1321.509281	-6.441260	2.966605
-1319.640109	-2.041935	2.976602
-1317.358370	-4.720545	2.986598
-1316.196751	-4.441477	2.996595
-1314.365466	-7.463615	3.006592
-1312.108319	-5.866173	3.016589
-1310.320105	0.111305	3.026586
-1308.444229	-4.496168	3.036582
-1306.652478	-6.998529	3.046579
-1304.682270	-15.394084	3.056576
-1302.692146	-0.146854	3.066573
-1300.892158	-2.620988	3.076570
-1298.930403	-4.151873	3.086566
-1297.242967	2.611605	3.096563
-1295.180434	-4.826011	3.106560
-1293.040268	-0.631300	3.116557
-1291.409358	0.524371	3.126554
-1289.965635	1.737091	3.136550
-1287.840146	-3.237319	3.146547
-1285.795906	0.672327	3.156544
-1284.072537	-5.107616	3.166541
-1282.295648	0.354886	3.176538
-1280.162042	1.377983	3.186534
-1278.411354	0.769024	3.196531
-1276.462640	-2.555447	3.206528
-1274.516811	-5.612655	3.216525
-1272.631041	-5.808105	3.226522
-1270.738110	-3.768684	3.236518
-1268.862989	-1.131411	3.246515
-1267.221058	-3.574433	3.256512
-1265.596681	2.141122	3.266509
-1263.358909	-1.852678	3.276506
-1261.412761	-6.429914	3.286502
-1259.623273	-2.491916	3.296499
-1257.571910	-7.246490	3.306496
-1256.040835	-8.047339	3.316493
-1253.751494	-5.616758	3.326490
-1252.117700	-2.186340	3.336486
-1250.443785	-2.216557	3.346483
-1248.357204	-2.853155	3.356480
-1246.120107	-6.102254	3.366477
-1244.800568	-0.460014	3.376474
-1242.614946	-0.778876	3.386470
-1240.850373	-4.304485	3.396467
-1238.918217	-5.105049	3.406464
-1237.141271	-2.484099	3.416461
-1235.084500	-8.638636	3.426458
-1233.276828	-6.660831	3.436454
-1231.585983	-6.579336	3.446451
-1229.610055	-2.213318	3.456448
-1227.670795	-0.201989	3.466445
-1226.021317	-2.309177	3.476442
-1223.876124	2.650233	3.486438
-1221.752270	-1.408954	3.496435
-1219.933098	-5.168412	3.506432
-1218.243001	-5.972450	3.516429
-1216.653589	-5.765637	3.526426
-1214.750783	-2.739464	3.536422
-1212.556888	3.485352	3.546419
-1210.752314	0.343746	3.556416
-1209.059659	-5.146739	3.566413
-1207.104955	-2.283212	3.576410
-1204.881214	-4.185886	3.586406
-1203.292609	-2.878268	3.596403
-1201.417090	0.330839	3.606400
-1199.535393	-7.063826	3.616397
-1197.594931	-6.013445	3.626394
-1195.763141	-5.875913	3.636390
-1193.981295	-5.190341	3.646387
-1192.006455	-11.544203	3.656384
-1190.363728	-7.973019	3.666381
-1188.547653	-5.557162	3.676378
-1186.270045	-3.022563	3.686374
-1184.313369	-7.511071	3.696371
-1182.539027	0.591924	3.706368
-1180.649017	-6.648449	3.716365
-1178.872176	-4.182772	3.726362
-1177.148713	-1.708718	3.736358
-1175.097893	-1.526981	3.746355
-1173.060651	-4.303831	3.756352
-1171.163972	-7.467955	3.766349
-1169.759764	-6.884301	3.776346
-1167.802834	-4.770456	3.786342
-1165.627511	-2.258196	3.796339
-1164.115537	-5.940771	3.806336
-1161.884601	-3.208047	3.816333
-1160.315983	0.667149	3.826330
-1158.267609	-5.000992	3.836326
-1156.292302	-5.996259	3.846323
-1154.267245	-4.609042	3.856320
-1152.717628	-1.458560	3.866317
-1150.718316	2.051806	3.876314
-1148.689445	1.586412	3.886310
-1147.041788	-3.881703	3.896307
-1145.057410	-5.355542	3.906304
-1143.159010	-7.770235	3.916301
-1141.376804	2.475845	3.926298
-1139.472685	-2.487360	3.936294
-1137.685590	3.597894	3.946291
-1135.885567	-0.637240	3.956288
-1133.997571	-3.375797	3.966285
-1132.139958	1.723154	3.976282
-1130.011051	-2.456607	3.986278
-1127.845551	1.999032	3.996275
-1126.120656	-0.707563	4.006272
-1124.689130	-0.466094	4.016269
-1122.573896	1.561309	4.026266
-1120.732671	3.650387	4.036262
-1118.711821	2.837809	4.046259
-1116.861417	-2.224451	4.056256
-1115.259945	0.318003	4.066253
-1113.294185	0.872041	4.076250
-1111.578457	-3.326081	4.086246
-1109.401248	-3.816928	4.096243
-1107.599152	1.384839	4.106240
-1105.564289	-9.262199	4.116237
-1103.948367	-4.548958	4.126234
-1101.989543	-4.752528	4.136230
-1099.926560	-4.686664	4.146227
-1098.357569	-7.807138	4.156224
-1096.188814	-8.287436	4.166221
-1094.436490	0.209852	4.176218
-1092.515294	0.470006	4.186214
-1090.583782	-1.800566	4.196211
-1088.696595	-5.074081	4.206208
-1087.009356	-2.366522	4.216205
-1085.442460	-6.267569	4.226202
-1083.113014	-9.039221	4.236198
-1081.180729	-11.358531	4.246195
-1079.378808	-9.247670	4.256192
-1077.320682	-9.359991	4.266189
-1075.741343	-8.391800	4.276186
-1074.132257	-11.041340	4.286182
-1071.904272	-7.082905	4.296179
-1069.206519	-6.681010	4.306176
-1067.953330	-5.109447	4.316173
-1066.503064	-11.778676	4.326170
-1064.758089	-7.282812	4.336166
-1062.530612	-8.416579	4.346163
-1061.123700	-13.069899	4.356160
-1058.963278	-8.786455	4.366157
-1056.741512	-10.391911	4.376154
-1055.074874	-5.933969	4.386150
-1053.150441	-11.155931	4.396147
-1051.114939	-12.830181	4.406144
-1049.356464	-5.910427	4.416141
-1047.508494	-9.609947	4.426138
-1045.774628	-6.145248	4.436134
-1043.769330	-4.629698	4.446131
-1041.842563	-10.320777	4.456128
-1040.015081	-10.265432	4.466125
-1038.088199	-8.412738	4.476122
-1036.267792	-4.587047	4.486118
-1034.703961	-5.026686	4.496115
-1032.604395	-4.282565	4.506112
-1030.549888	-6.633115	4.516109
-1028.789835	-4.319411	4.526106
-1026.816403	-7.767374	4.536102
-1024.884450	-8.264285	4.546099
-1022.834392	-6.597535	4.556096
-1021.108005	-7.027533	4.566093
-1019.881837	-5.404286	4.576090
-1017.482982	-12.149814	4.586086
-1015.440841	-15.883447	4.596083
-1013.729588	-17.177147	4.606080
-1011.751719	-13.683189	4.616077
-1009.973363	-12.017211	4.626074
-1008.500969	-13.820824	4.636070
-1006.236658	-16.048508	4.646067
-1004.184764	-17.131548	4.656064
-1002.623395	-19.438126	4.666061
-1000.629037	-12.348595	4.676058
-998.569267	-9.636587	4.686054
-996.936881	-13.606153	4.696051
-995.024096	-9.401092	4.706048
-993.160958	-9.971540	4.716045
-991.115621	-8.206742	4.726042
-989.456162	-7.169278	4.736038
-987.424885	-8.266557	4.746035
-985.419564	-7.304674	4.756032
-983.998730	-4.953264	4.766029
-982.171509	-4.486039	4.776026
-979.887463	-4.180631	4.786022
-978.079393	-11.300153	4.796019
-976.058889	-10.529783	4.806016
-974.306445	-11.751893	4.816013
-972.322337	-11.254292	4.826010
-970.402542	-13.730286	4.836006
-968.748300	-4.791246	4.846003
-966.957081	-6.924254	4.856000
-965.249465	-11.831915	4.865997
-963.027722	-6.707264	4.875994
-961.028732	-6.228812	4.885990
-959.281493	-3.786806	4.895987
-957.326995	-8.222679	4.905984
-955.929066	-11.623583	4.915981
-953.859684	-6.362901	4.925978
-951.562511	-10.363585	4.935974
-949.775679	-7.799929	4.945971
-948.216751	-1.801092	4.955968
-946.048438	-6.911144	4.965965
-944.170103	-10.852568	4.975962
-942.584201	-8.008198	4.985958
-940.581008	-11.929558	4.995955
-938.526477	-16.729194	5.005952
-936.658424	-5.601409	5.015949
-935.044288	-13.848359	5.025946
-933.022575	-9.966675	5.035942
-931.141461	-7.688731	5.045939
-929.527320	-5.973184	5.055936
-927.382822	-9.079367	5.065933
-925.615463	-6.918240	5.075930
-924.112229	-5.186814	5.085926
-922.071900	-11.125774	5.095923
-919.803317	-12.929295	5.105920
-917.884828	-10.589389	5.115917
-916.073419	-7.069572	5.125914
-914.347798	-8.476360	5.135910
-912.543718	-14.530077	5.145907
-910.379447	-14.722588	5.155904
-908.611143	-11.165729	5.165901
-906.555846	-17.482700	5.175898
-905.054106	-11.630536	5.185894
-903.320357	-10.185681	5.195891
-901.264553	-11.747947	5.205888
-899.136475	-15.901374	5.215885
-897.466132	-8.260569	5.225882
-895.726335	-17.136123	5.235878
-893.469430	-13.140661	5.245875
-891.595856	-9.923962	5.255872
-889.871752	-11.199664	5.265869
-887.983635	-12.407880	5.275866
-886.349007	-12.700743	5.285862
-884.347104	-15.869769	5.295859
-882.135023	-14.239852	5.305856
-880.484864	-12.451428	5.315853
-878.565058	-11.735260	5.325850
-876.777280	-6.538041	5.335846
-875.125339	-9.920873	5.345843
-873.004046	-14.136358	5.355840
-871.207042	-20.911686	5.365837
-869.785438	-14.091316	5.375834
-866.901336	-11.186392	5.385830
-865.252637	-9.827701	5.395827
-863.662595	-19.448991	5.405824
-861.932712	-14.361975	5.415821
-859.697288	-13.821700	5.425818
-857.857864	-9.021437	5.435814
-856.132803	-3.557345	5.445811
-854.346404	-9.946705	5.455808
-852.562198	-10.748575	5.465805
-850.509222	-8.670035	5.475802
-848.942136	-8.826008	5.485798
-846.572445	-10.399050	5.495795
-844.708880	-9.086322	5.505792
-842.993169	-14.459704	5.515789
-840.990267	-12.608506	5.525786
-839.181545	-14.913223	5.535782
-837.558531	-11.242470	5.545779
-835.304086	-15.725034	5.555776
-833.563814	-12.845465	5.565773
-831.714326	-21.898700	5.575770
-830.112820	-14.573286	5.585766
-827.810667	-12.033610	5.595763
-825.982970	-19.252877	5.605760
-824.669601	-16.697612	5.615757
-822.555443	-5.934499	5.625754
-820.265552	-14.979937	5.635750
-818.406266	-14.395629	5.645747
-816.695757	-14.669479	5.655744
-814.599747	-11.048286	5.665741
-813.095406	-11.383969	5.675738
-811.156191	-14.955200	5.685734
-809.102882	-13.243454	5.695731
-807.305037	-12.589314	5.705728
-805.434759	-11.202631	5.715725
-803.606395	-13.634012	5.725722
-801.944928	-15.345914	5.735718
-799.888266	-13.754093	5.745715
-797.963036	-11.545312	5.755712
-795.971128	-16.155899	5.765709
-794.491503	-15.500094	5.775706
-792.280241	-14.966308	5.785702
-790.476042	-19.192540	5.795699
-788.301733	-14.944924	5.805696
-786.508372	-5.559768	5.815693
-784.942118	-9.289480	5.825690
-783.037548	-11.591656	5.835686
-781.160637	-6.751550	5.845683
-779.072412	-15.878549	5.855680
-777.306802	-14.420140	5.865677
-775.384413	-15.491518	5.875674
-773.595055	-10.046330	5.885670
-771.800893	-7.061766	5.895667
-769.830127	-18.118183	5.905664
-768.155541	-5.032810	5.915661
-765.879153	-9.730548	5.925658
-764.161623	-7.691614	5.935654
-762.404787	-3.237563	5.945651
-760.469599	-3.005744	5.955648
-758.614583	-6.755368	5.965645
-756.446155	-7.654761	5.975642
-754.572506	-5.400747	5.985638
-752.783817	-1.476999	5.995635
-751.299504	-8.301775	6.005632
-749.211473	-5.391350	6.015629
-747.097179	-8.386744	6.025626
-745.784682	-1.968494	6.035622
-743.592725	-0.902178	6.045619
-741.663974	-2.403440	6.055616
-739.614834	-1.698339	6.065613
-737.596146	0.794398	6.075610
-735.995531	3.500375	6.085606
-734.037323	-0.345599	6.095603
-732.377606	0.047726	6.105600
-730.743832	-5.256229	6.115597
-728.513232	1.750623	6.125594
-726.589716	0.142373	6.135590
-724.823785	2.276564	6.145587
-722.910931	4.430201	6.155584
-721.043252	4.802858	6.165581
-719.019930	-4.175452	6.175578
-717.608245	1.764970	6.185574
-715.381792	2.227027	6.195571
-713.471154	-3.914864	6.205568
-711.679705	0.968005	6.215565
-709.721349	0.204281	6.225562
-707.560087	-1.012004	6.235558
-705.736768	0.713972	6.245555
-704.208566	0.529550	6.255552
-702.665790	-6.704808	6.265549
-700.492095	-2.664917	6.275546
-698.349048	-1.974332	6.285542
-696.570258	-2.261433	6.295539
-694.882457	-1.372179	6.305536
-692.761111	-7.621360	6.315533
-691.248829	-2.033334	6.325530
-689.209585	-2.328771	6.335526
-687.331672	1.635025	6.345523
-685.301995	-7.091426	6.355520
-683.404327	-7.116346	6.365517
-681.364382	-4.176292	6.375514
-679.781681	-1.622538	6.385510
-677.817416	0.726621	6.395507
-675.839609	-1.113824	6.405504
-674.208573	-2.392048	6.415501
-672.570573	-1.418753	6.425498
-670.306512	2.072901	6.435494
-668.468055	0.967360	6.445491
-666.434669	4.217210	6.455488
-664.866124	2.554500	6.465485
-663.004093	4.161217	6.475482
-660.981114	4.430577	6.485478
-659.229499	-1.046527	6.495475
-656.755972	3.568349	6.505472
-654.790560	0.436506	6.515469
-653.804121	2.276874	6.525466
-651.910340	-1.862720	6.535462
-649.698764	2.974167	6.545459
-647.480279	0.903916	6.555456
-645.695757	-4.054382	6.565453
-644.416424	-4.970299	6.575450
-642.291253	-3.906303	6.585446
-640.313730	-2.445074	6.595443
-638.803742	-8.637538	6.605440
-636.505342	-9.190837	6.615437
-634.906946	-6.129145	6.625434
-632.788361	-6.727862	6.635430
-630.743528	-4.505933	6.645427
-628.984412	-3.933204	6.655424
-627.182254	-5.595282	6.665421
-625.340741	-3.265741	6.675418
-623.672436	-3.385649	6.685414
-621.311321	-5.972403	6.695411
-619.812768	-6.085312	6.705408
-617.604776	-6.360271	6.715405
-615.773623	-6.709679	6.725402
-614.194506	-6.094596	6.735398
-612.352296	-6.522571	6.745395
-610.600628	-3.640117	6.755392
-608.393847	-3.175420	6.765389
-606.304835	-5.119097	6.775386
-604.744673	-7.610691	6.785382
-602.743927	-3.910595	6.795379
-601.015344	-7.128243	6.805376
-599.011099	-8.022703	6.815373
-597.466992	-11.974618	6.825370
-595.378048	1.412437	6.835366
-593.139796	1.481272	6.845363
-591.245705	0.785933	6.855360
-589.911867	5.812989	6.865357
-587.759632	2.076848	6.875354
-585.752277	-8.404040	6.885350
-584.290131	-2.738205	6.895347
-582.359971	-1.675891	6.905344
-580.151875	-4.879380	6.915341
-578.135571	-4.168963	6.925338
-576.570392	-4.275506	6.935334
-574.939260	-6.156411	6.945331
-572.877187	-4.692664	6.955328
-570.600748	-5.128339	6.965325
-568.964245	-8.983464	6.975322
-567.234597	-6.577792	6.985318
-565.120703	-5.486530	6.995315
-563.485720	-13.992261	7.005312
-561.555224	-5.724468	7.015309
-559.469779	-2.021889	7.025306
-557.910321	2.965278	7.035302
-556.221050	5.660857	7.045299
-554.076464	2.977707	7.055296
-551.939683	-2.864625	7.065293
-550.132573	-6.622548	7.075290
-548.413446	-5.564717	7.085286
-546.735149	1.754769	7.095283
-544.600780	-0.292700	7.105280
-542.614083	-3.634054	7.115277
-540.810401	-4.602759	7.125274
-539.052377	7.044079	7.135270
-537.265397	0.744436	7.145267
-535.159305	-3.359611	7.155264
-533.322435	-1.416146	7.165261
-531.274390	-2.545340	7.175258
-529.950496	-1.872998	7.185254
-528.233095	-5.562563	7.195251
-526.062870	-0.508655	7.205248
-523.722498	1.311670	7.215245
-521.941390	3.514878	7.225242
-520.432583	3.916393	7.235238
-518.120961	1.770546	7.245235
-516.517453	-1.205084	7.255232
-514.657149	-7.279378	7.265229
-512.670574	1.289460	7.275226
-510.949679	-7.745568	7.285222
-509.165871	-5.591035	7.295219
-506.794495	-1.784144	7.305216
-505.385184	-4.242710	7.315213
-503.317912	-8.406873	7.325210
-501.699721	-1.437094	7.335206
-499.755065	-3.953519	7.345203
-497.310792	-3.261952	7.355200
-495.918227	-8.371106	7.365197
-493.618719	-9.242668	7.375194
-491.873205	-11.792504	7.385190
-490.320029	-4.012049	7.395187
-488.659789	2.120969	7.405184
-486.270585	-4.974787	7.415181
-484.436731	-6.930358	7.425178
-482.715971	-6.371540	7.435174
-480.913779	-12.107823	7.445171
-478.924694	-5.457372	7.455168
-477.213961	-4.334443	7.465165
-475.282549	-8.427069	7.475162
-473.276356	-2.648229	7.485158
-470.937435	-0.398029	7.495155
-469.880338	-7.383008	7.505152
-467.719226	-7.534446	7.515149
-465.808673	-8.645159	7.525146
-464.005230	-5.768759	7.535142
-462.299590	-7.894793	7.545139
-460.108366	-6.502156	7.555136
-458.386565	-7.784413	7.565133
-456.658811	-7.184893	7.575130
-454.402950	-2.851885	7.585126
-452.879178	-3.097509	7.595123
-450.262622	-3.299015	7.605120
-449.213941	-7.574145	7.615117
-447.202446	-4.880845	7.625114
-445.086075	-8.140858	7.635110
-443.260556	-6.388272	7.645107
-441.568200	-8.864551	7.655104
-439.603115	-3.856422	7.665101
-437.192614	-0.901565	7.675098
-435.795401	-7.825533	7.685094
-433.974551	-5.564291	7.695091
-432.284480	-6.996810	7.705088
-430.200855	-7.069727	7.715085
-428.220485	-10.302843	7.725082
-426.349602	-5.660324	7.735078
-424.602783	-8.495309	7.745075
-422.461496	-6.526163	7.755072
-420.970833	-11.202372	7.765069
-419.270357	-8.685718	7.775066
-417.115366	-9.780643	7.785062
-415.083788	-5.260932	7.795059
-413.172364	-6.791095	7.805056
-411.350858	-10.915033	7.815053
-409.279152	-6.615619	7.825050
-407.791956	-4.902200	7.835046
-405.727635	-4.387668	7.845043
-403.982109	0.818998	7.855040
-401.724116	-6.292545	7.865037
-400.247866	-2.613427	7.875034
-398.449383	-2.360763	7.885030
-396.259771	1.767461	7.895027
-394.652968	-3.168956	7.905024
-392.944449	-3.478265	7.915021
-390.814447	-5.244708	7.925018
-388.687048	-9.266584	7.935014
-386.856167	-6.075524	7.945011
-385.089841	-2.647721	7.955008
-383.235936	-6.761004	7.965005
-381.543185	-7.006740	7.975002
-379.035502	-7.952291	7.984998
-377.634863	-3.980778	7.994995
-375.797094	-7.844281	8.004992
-374.100278	-9.336427	8.014989
-372.090321	-4.239134	8.024986
-369.936024	-13.296297	8.034982
-368.067308	-6.633045	8.044979
-366.450226	-6.898993	8.054976
-364.628123	-11.806726	8.064973
-362.576647	-10.555267	8.074970
-360.628738	-6.297431	8.084966
-358.884074	0.278820	8.094963
-356.983579	-1.015873	8.104960
-355.047718	-0.489951	8.114957
-353.314231	-3.777121	8.124954
-351.594826	-1.705139	8.134950
-349.698787	-4.446339	8.144947
-347.094549	-5.656235	8.154944
-345.824966	-9.813128	8.164941
-343.974638	-8.816848	8.174938
-342.120055	-8.956352	8.184934
-340.213247	-3.526759	8.194931
-338.265080	-2.951167	8.204928
-336.516517	-5.933440	8.214925
-334.299102	-7.825115	8.224922
-332.505737	-6.122296	8.234918
-330.451349	-5.495364	8.244915
-328.939308	-8.365133	8.254912
-327.205158	-6.330845	8.264909
-325.377630	-11.298381	8.274906
-323.012432	-7.348840	8.284902
-321.445844	-7.610063	8.294899
-319.514863	-4.999718	8.304896
-317.373556	-7.772701	8.314893
-315.225140	-7.989074	8.324890
-313.767774	2.234116	8.334886
-312.439329	0.031743	8.344883
-310.489861	-3.443430	8.354880
-308.203681	-7.678654	8.364877
-306.096650	-2.325675	8.374874
-304.018495	-1.366480	8.384870
-302.573415	-3.758007	8.394867
-300.631129	-3.704260	8.404864
-299.107602	0.917674	8.414861
-296.868073	-9.566580	8.424858
-294.937122	-7.609509	8.434854
-292.940474	-0.455962	8.444851
-291.664236	-5.279132	8.454848
-289.571259	-4.417719	8.464845
-287.603779	-1.005405	8.474842
-285.390910	-3.048831	8.484838
-284.035862	-2.634695	8.494835
-282.215276	-4.067413	8.504832
-279.982857	-2.963934	8.514829
-278.282954	0.001052	8.524826
-276.143689	-4.015303	8.534822
-274.247371	-1.582767	8.544819
-272.562476	-2.691054	8.554816
-270.528276	-4.001926	8.564813
-268.973097	-8.340579	8.574810
-266.727717	-4.675954	8.584807
-265.078304	-0.907527	8.594803
-263.326083	-12.136949	8.604800
-261.261458	-7.820437	8.614797
-259.178458	-9.848688	8.624794
-257.834009	-8.273167	8.634791
-256.117636	-3.985843	8.644787
-253.551728	-2.276378	8.654784
-251.639446	-8.118414	8.664781
-250.203335	-5.696648	8.674778
-247.959653	-9.811918	8.684775
-246.431908	-15.830658	8.694771
-244.753996	-10.905577	8.704768
-242.490689	-8.777052	8.714765
-240.488365	-9.771409	8.724762
-238.876741	-14.341844	8.734759
-237.019135	-10.920149	8.744755
-234.962924	-13.710511	8.754752
-232.891437	-5.656826	8.764749
-231.231911	-8.866846	8.774746
-229.279541	-16.132196	8.784743
-227.340743	-21.057917	8.794739
-225.501019	-13.734359	8.804736
-223.766442	-14.594655	8.814733
-222.123276	-15.945147	8.824730
-219.863918	-11.702721	8.834727
-218.149488	-8.056482	8.844723
-216.115119	-10.404007	8.854720
-214.465868	-13.814609	8.864717
-212.759080	-9.560008	8.874714
-210.514406	-10.270655	8.884711
-208.797971	-14.964973	8.894707
-207.021031	-17.286523	8.904704
-205.046172	-10.474221	8.914701
-203.014044	-9.669913	8.924698
-201.437826	-10.035502	8.934695
-199.464054	-11.251007	8.944691
-197.509223	-13.687243	8.954688
-195.704953	-17.353254	8.964685
-193.696734	-15.075038	8.974682
-191.701545	-18.809359	8.984679
-189.927060	-22.267909	8.994675
-188.321916	-23.346678	9.004672
-186.337195	-18.654807	9.014669
-184.197681	-22.265671	9.024666
-182.708759	-23.386950	9.034663
-180.556446	-19.888910	9.044659
-178.619693	-16.233360	9.054656
-176.687802	-17.835307	9.064653
-175.162317	-16.581686	9.074650
-173.247130	-24.055632	9.084647
-171.177570	-14.669714	9.094643
-169.552098	-18.244188	9.104640
-167.301122	-14.827086	9.114637
-165.329044	-18.004923	9.124634
-163.651514	-15.778665	9.134631
-161.873780	-12.825006	9.144627
-160.142559	-12.587981	9.154624
-158.361011	-17.119554	9.164621
-155.885405	-12.552162	9.174618
-154.486087	-15.970469	9.184615
-152.486329	-14.238550	9.194611
-150.652675	-19.247386	9.204608
-148.472963	-19.477347	9.214605
-146.979969	-20.528570	9.224602
-145.183046	-22.672515	9.234599
-142.881494	-23.133227	9.244595
-141.287400	-16.255201	9.254592
-139.469494	-21.737565	9.264589
-137.406414	-23.705435	9.274586
-135.489528	-20.135382	9.284583
-133.710629	-13.375200	9.294579
-132.107106	-13.763232	9.304576
-129.847940	-13.033395	9.314573
-127.761899	-13.238588	9.324570
-126.212858	-10.959453	9.334567
-124.319459	-9.752308	9.344563
-122.405851	-10.128697	9.354560
-120.602727	-7.815275	9.364557
-118.830363	-15.117695	9.374554
-116.965675	-9.389894	9.384551
-114.754798	-13.721984	9.394547
-112.992009	-16.361592	9.404544
-111.359542	-11.589513	9.414541
-109.317689	-12.776344	9.424538
-107.481047	-16.163319	9.434535
-105.746119	-12.697211	9.444531
-103.513672	-7.661650	9.454528
-101.751341	-9.912680	9.464525
-99.968443	-14.449998	9.474522
-98.183037	-12.020102	9.484519
-96.289491	-13.132488	9.494515
-94.238800	-4.999674	9.504512
-92.460055	-10.498628	9.514509
-90.909470	-11.837941	9.524506
-88.866842	-8.861698	9.534503
-86.736429	-5.175680	9.544499
-84.777540	-6.041586	9.554496
-83.241581	-13.326380	9.564493
-81.195800	-10.821770	9.574490
-79.274314	-17.435594	9.584487
-77.394983	-9.999399	9.594483
-75.813251	-2.380562	9.604480
-73.561555	-8.766455	9.614477
-71.685113	-11.925881	9.624474
-69.689814	-8.707544	9.634471
-67.973688	-4.709000	9.644467
-66.363549	-7.136666	9.654464
-64.537857	-10.552181	9.664461
-62.469576	-8.616183	9.674458
-60.325409	-7.958280	9.684455
-58.419381	-11.639716	9.694451
-56.867147	-11.324929	9.704448
-54.984838	-11.395164	9.714445
-52.925224	-11.544018	9.724442
-51.100335	-11.441577	9.734439
-49.379045	-10.014788	9.744435
-47.570639	-11.495519	9.754432
-45.341927	-13.602016	9.764429
-43.408869	-17.423639	9.774426
-41.980591	-11.546672	9.784423
-40.029089	-11.832301	9.794419
-37.832625	-12.388368	9.804416
-36.330045	-13.839973	9.814413
-34.376738	-14.517963	9.824410
-32.566609	-13.079922	9.834407
-30.720375	-17.573536	9.844403
-28.629339	-10.215116	9.854400
-26.782480	-11.423015	9.864397
-24.643605	-15.863259	9.874394
-22.747839	-15.584442	9.884391
-21.376654	-12.417551	9.894387
-18.881371	-14.302578	9.904384
-17.197886	-12.512810	9.914381
-15.577255	-16.649983	9.924378
-13.568693	-17.306612	9.934375
-11.480786	-11.144359	9.944371
-9.987160	-14.075688	9.954368
-8.633151	-18.565520	9.964365
-6.460303	-20.578634	9.974362
-4.949091	2.830522	9.984359
-3.759927	44.983552	9.994355
-2.406686	95.774120	10.004352
-0.954440	166.084391	10.014349
0.000000	226.017061	10.019354
0.816330	277.453959	10.024359
1.586592	312.370081	10.029363
2.036636	341.561707	10.034368
2.622299	373.968417	10.039373
2.922471	388.712241	10.044378
2.953493	411.325201	10.049383
3.394792	423.821397	10.054387
3.370896	440.271165	10.059392
3.679961	454.836297	10.064397
3.880372	458.807568	10.069402
3.758831	472.165279	10.074407
3.927408	461.745697	10.079411
3.980830	475.884961	10.084416
4.119568	490.975498	10.089421
4.277317	495.999715	10.094426
4.203864	503.126794	10.099431
4.243504	503.552212	10.104435
4.857586	504.284913	10.109440
4.646370	509.682255	10.114445
4.471695	521.058923	10.119450
4.230805	526.090713	10.124455
4.471268	520.151119	10.129459
4.998394	518.735644	10.134464
4.419933	526.703245	10.139469
4.621071	517.562079	10.144474
4.470416	522.976672	10.149479
4.831498	538.176363	10.154483
5.295702	560.984074	10.159488
5.011687	557.356693	10.164493
5.205730	533.979811	10.169498
5.191031	530.727825	10.174503
5.092218	537.036268	10.179507
4.967441	544.564917	10.184512
4.579517	554.706371	10.189517
5.400229	562.541058	10.194522
5.331574	574.891136	10.199527
5.283325	568.494594	10.204531
5.748295	571.564375	10.209536
5.863675	571.593926	10.214541
5.994532	562.268211	10.219546
5.570077	561.606004	10.224551
5.720164	553.736295	10.229555
5.683463	556.591309	10.234560
5.407702	552.469109	10.239565
5.766670	552.295057	10.244570
5.715134	557.926344	10.249575
5.924236	554.819923	10.254579
5.727521	562.750507	10.259584
5.475644	559.119590	10.264589
5.932602	573.687895	10.269594
6.026327	586.667753	10.274599
6.456665	589.996494	10.279603
6.214089	577.878171	10.284608
5.793574	577.491595	10.289613
6.363829	573.841682	10.294618
6.119641	573.935253	10.299623
5.807702	575.616578	10.304627
6.305511	584.029651	10.309632
6.438636	599.137439	10.314637
6.383208	597.051732	10.319642
6.328217	609.359627	10.324647
6.230241	594.859589	10.329651
6.576629	598.370879	10.334656
6.246251	611.811095	10.339661
6.571363	612.804527	10.344666
6.121818	608.189885	10.349671
6.244229	603.172845	10.354675
6.285814	614.266587	10.359680
6.636493	615.923907	10.364685
6.781587	618.983018	10.369690
6.714516	635.338554	10.374695
7.067424	641.948920	10.379699
7.042841	637.814814	10.384704
6.810651	637.347000	10.389709
6.994997	635.873449	10.394714
6.964768	652.467417	10.399719
6.808348	658.125013	10.404723
7.265981	664.147446	10.409728
7.022160	653.272274	10.414733
7.585562	643.674589	10.419738
7.179847	650.331349	10.424743
7.327365	655.004091	10.429747
7.444063	647.273083	10.434752
7.116484	653.747504	10.439757
7.080824	650.859868	10.444762
7.007925	657.146154	10.449767
7.239775	660.739069	10.454771
7.341127	659.440005	10.459776
7.378470	666.871444	10.464781
7.720215	680.306211	10.469786
7.725831	682.951496	10.474791
8.170708	675.951687	10.479795
7.874913	663.897288	10.484800
7.957790	658.237682	10.489805
8.256112	646.648259	10.494810
8.194433	649.388759	10.499815
8.342799	651.497603	10.504819
8.183799	654.015192	10.509824
8.061182	652.661375	10.514829
8.005453	650.550450	10.519834
8.216167	662.784804	10.524839
7.916626	656.404865	10.529843
8.316749	658.591725	10.534848
8.210264	665.311657	10.539853
8.287862	663.805882	10.544858
8.202580	665.307830	10.549863
8.394812	661.018124	10.554867
8.232329	664.167086	10.559872
8.103866	668.147038	10.564877
8.555242	683.816905	10.569882
8.341505	691.746131	10.574887
8.828782	696.106031	10.579891
8.755957	695.391817	10.584896
8.916161	706.314500	10.589901
8.920610	697.754047	10.594906
8.750346	700.039895	10.599911
9.047227	700.246743	10.604915
8.677115	693.475872	10.609920
8.673879	700.564160	10.614925
9.228340	693.791074	10.619930
8.828751	698.686317	10.624935
8.835686	703.659488	10.629939
9.157569	705.066760	10.634944
8.801434	707.390400	10.639949
8.986472	709.035868	10.644954
8.705002	715.638196	10.649959
8.890182	700.410971	10.654963
9.299174	720.076872	10.659968
9.544537	734.113199	10.664973
9.803852	724.289319	10.669978
9.519382	722.140237	10.674983
9.385171	717.849646	10.679987
9.516971	722.636023	10.684992
9.352253	732.214331	10.689997
9.978604	741.613985	10.695002
9.783627	735.211743	10.700007
9.997401	729.998211	10.705011
9.894696	722.659251	10.710016
9.691152	725.233435	10.715021
9.787918	715.669532	10.720026
9.797972	724.405123	10.725031
10.229949	735.997662	10.730035
9.529867	731.361205	10.735040
9.776171	745.574614	10.740045
10.079123	742.511668	10.745050
9.870704	751.350654	10.750055
10.026794	737.914532	10.755059
10.078645	747.550057	10.760064
9.881921	750.201627	10.765069
10.042808	743.592711	10.770074
9.742492	750.076313	10.775079
10.121061	759.460436	10.780083
10.174798	764.316656	10.785088
10.623014	773.089251	10.790093
10.538211	769.699633	10.795098
11.028185	781.036345	10.800103
10.730427	774.831707	10.805107
10.586802	775.993544	10.810112
10.232736	779.662869	10.815117
10.724143	770.407445	10.820122
10.493073	785.372993	10.825127
10.375838	764.491335	10.830131
10.678852	769.665205	10.835136
10.380957	779.847025	10.840141
10.634601	781.177980	10.845146
10.696517	797.348941	10.850151
11.420211	809.510850	10.855155
11.715067	796.134963	10.860160
11.436109	777.941501	10.865165
11.457879	771.649316	10.870170
11.520355	772.716605	10.875175
11.571235	769.408721	10.880179
11.492999	772.885885	10.885184
11.497663	778.256568	10.890189
11.748096	771.161373	10.895194
11.710574	772.215414	10.900199
11.748092	777.942431	10.905203
11.618139	776.488415	10.910208
11.562130	783.608289	10.915213
11.402874	780.101962	10.920218
11.404698	782.087136	10.925223
11.611236	778.071257	10.930227
11.870659	775.774834	10.935232
11.652035	789.501167	10.940237
12.115249	785.325226	10.945242
11.698359	787.273247	10.950247
11.668473	780.282164	10.955251
11.565399	773.980988	10.960256
11.460793	778.010166	10.965261
11.718435	774.407097	10.970266
11.793286	797.409411	10.975271
11.673062	803.157562	10.980275
12.176703	817.497833	10.985280
12.082031	809.037997	10.990285
12.403551	806.198036	10.995290
12.254980	811.649082	11.000295
12.268304	810.305889	11.005299
12.690289	806.133854	11.010304
12.143266	809.035361	11.015309
12.786062	808.430544	11.020314
12.648792	820.624030	11.025319
12.432994	813.248761	11.030323
12.871837	804.997447	11.035328
12.429810	812.833642	11.040333
12.515095	812.979274	11.045338
12.377988	812.591466	11.050343
12.775143	817.369479	11.055347
12.680969	811.037947	11.060352
12.401415	823.377409	11.065357
13.005472	826.369316	11.070362
13.086704	837.942334	11.075367
13.128562	843.340214	11.080371
13.380398	846.615934	11.085376
13.277755	836.136817	11.090381
13.399278	818.538186	11.095386
13.139579	822.415943	11.100391
13.401350	809.519000	11.105395
13.589071	805.825283	11.110400
13.198163	810.527232	11.115405
13.529433	815.503249	11.120410
13.324426	808.113500	11.125415
13.198946	821.184032	11.130419
13.245306	809.989789	11.135424
13.416132	834.456733	11.140429
13.923496	832.752125	11.145434
13.897489	838.943602	11.150439
13.361278	826.740037	11.155443
13.632696	834.143658	11.160448
13.538509	856.663470	11.165453
13.720442	844.119263	11.170458
14.082276	851.482916	11.175463
13.861434	848.703572	11.180467
14.281187	846.797670	11.185472
13.869785	855.637965	11.190477
13.947782	851.771210	11.195482
13.792036	862.164366	11.200487
13.760081	850.458133	11.205491
14.154468	853.827439	11.210496
14.013523	857.652475	11.215501
14.277724	847.482684	11.220506
14.248474	854.422347	11.225511
14.082974	848.039872	11.230515
13.999514	849.499290	11.235520
13.904046	857.299770	11.240525
14.524759	862.294069	11.245530
14.515717	878.821488	11.250535
14.464821	880.596243	11.255539
14.626301	881.905510	11.260544
14.731789	880.753349	11.265549
15.025895	874.289298	11.270554
15.132019	881.624967	11.275559
15.100270	854.549384	11.280563
15.052495	855.280324	11.285568
14.417521	851.434367	11.290573
14.339751	837.384974	11.295578
14.579340	852.012917	11.300583
15.046241	876.542451	11.305587
15.327047	876.294959	11.310592
15.218234	879.966072	11.315597
15.454780	877.902502	11.320602
15.338989	883.659396	11.325607
15.366242	874.185077	11.330611
15.563853	866.402982	11.335616
15.328202	864.753925	11.340621
15.511759	851.034710	11.345626
15.149650	857.424741	11.350631
15.296351	853.896728	11.355635
15.443630	866.792244	11.360640
15.465170	876.706991	11.365645
15.505960	872.831215	11.370650
15.529912	896.391476	11.375655
15.290302	889.688536	11.380659
15.233714	885.671560	11.385664
15.233761	883.140913	11.390669
15.143638	881.721505	11.395674
15.203902	887.263479	11.400679
15.186431	905.668538	11.405683
15.875899	903.884147	11.410688
15.911708	910.119133	11.415693
15.871804	909.815708	11.420698
15.822053	906.490706	11.425703
16.247548	917.677129	11.430707
16.291427	913.286870	11.435712
16.130492	917.121664	11.440717
16.325303	903.012056	11.445722
15.926833	907.468227	11.450727
16.187188	909.697641	11.455731
16.857578	904.628391	11.460736
16.202468	908.857778	11.465741
16.257291	917.999089	11.470746
16.185421	908.943977	11.475751
16.118991	920.479217	11.480755
16.588277	929.228552	11.485760
16.783244	944.194230	11.490765
16.815322	940.864665	11.495770
16.842614	944.307985	11.500775
16.407600	940.700877	11.505779
16.920212	938.106021	11.510784
17.049846	937.534713	11.515789
17.119048	936.102193	11.520794
17.107425	941.482040	11.525799
16.945127	933.285966	11.530803
16.995789	911.410988	11.535808
16.893259	928.628299	11.540813
17.311665	928.773658	11.545818
17.145581	934.003145	11.550823
16.979047	937.352197	11.555827
17.003276	944.953778	11.560832
17.046467	942.406645	11.565837
16.741112	945.453844	11.570842
16.946876	945.663688	11.575847
16.979038	952.459444	11.580851
17.019948	940.072365	11.585856
17.566042	958.991908	11.590861
18.245529	949.438871	11.595866
18.233389	941.506388	11.600871
17.939820	925.091958	11.605875
18.320298	928.727347	11.610880
17.737839	934.675589	11.615885
18.329555	924.038281	11.620890
18.311085	930.983629	11.625895
17.918525	916.066434	11.630899
17.757988	900.556055	11.635904
17.645585	910.307081	11.640909
18.214764	918.918495	11.645914
17.974822	923.445779	11.650919
18.060875	932.683190	11.655923
18.139697	936.058067	11.660928
18.126347	932.521558	11.665933
18.432815	929.441000	11.670938
18.025387	922.314849	11.675943
17.826116	937.620482	11.680947
18.082107	926.763236	11.685952
18.386262	932.792749	11.690957
18.426270	930.744712	11.695962
18.511800	938.050782	11.700967
18.284838	932.681436	11.705971
18.523483	929.366193	11.710976
18.158208	944.228588	11.715981
18.632882	938.575519	11.720986
18.025444	945.848039	11.725991
17.979797	947.036510	11.730995
18.289054	958.951835	11.736000
18.175862	968.455139	11.741005
18.777512	968.076845	11.746010
18.308384	969.058059	11.751015
18.792799	982.284680	11.756019
19.205528	988.957175	11.761024
19.371474	988.952006	11.766029
19.980955	963.900624	11.771034
19.852953	957.238124	11.776039
19.673638	950.154559	11.781043
19.723695	953.222926	11.786048
19.464708	951.844307	11.791053
19.596217	929.211367	11.796058
19.319265	929.423055	11.801063
19.200473	931.232351	11.806067
19.314647	925.093996	11.811072
19.521297	930.853649	11.816077
19.868310	935.863322	11.821082
19.925382	933.749991	11.826087
19.427616	929.101283	11.831091
19.695346	924.808824	11.836096
19.717599	931.401008	11.841101
19.864363	924.259967	11.846106
19.673516	927.760421	11.851111
19.533598	930.823857	11.856115
19.889079	926.686877	11.861120
19.649378	932.607139	11.866125
20.101217	944.738795	11.871130
20.157649	958.011934	11.876135
20.149260	948.560259	11.881139
19.693996	935.257998	11.886144
19.644798	951.597381	11.891149
20.077847	950.711551	11.896154
19.783737	960.579420	11.901159
19.982283	962.440889	11.906163
19.861113	956.318004	11.911168
19.837984	965.195604	11.916173
20.079570	971.203886	11.921178
20.293882	988.262334	11.926183
20.108608	990.045536	11.931187
20.415177	993.543613	11.936192
20.138976	994.217014	11.941197
20.243256	1000.188060	11.946202
20.179549	1003.108970	11.951207
20.563326	1003.996844	11.956211
21.124195	1012.721446	11.961216
20.754819	1004.955576	11.966221
20.746553	994.997800	11.971226
20.734949	1006.436467	11.976231
20.861724	1011.001558	11.981235
21.181213	1009.663091	11.986240
20.893127	1018.250229	11.991245
21.127622	1011.137527	11.996250
20.809821	1021.016996	12.001255
20.836625	1013.827009	12.006259
21.382529	1012.549195	12.011264
21.048661	1024.186418	12.016269
21.362679	1011.595350	12.021274
21.098639	1020.591260	12.026279
21.700834	1021.806029	12.031283
21.439252	1014.742855	12.036288
21.355979	1016.714229	12.041293
21.255424	1015.878833	12.046298
21.310056	1021.306558	12.051303
21.326972	1014.201160	12.056307
21.166482	1016.395378	12.061312
21.120287	1015.209215	12.066317
21.346354	1019.265048	12.071322
21.580264	1019.606251	12.076327
21.089143	1015.454140	12.081331
21.541813	1011.114949	12.086336
21.373748	1001.878908	12.091341
21.405939	994.055639	12.096346
20.937808	1003.285874	12.101351
20.829651	1000.994022	12.106355
21.332021	1005.286292	12.111360
21.346764	1022.457548	12.116365
21.135324	1008.942497	12.121370
21.119492	1012.850725	12.126375
21.265731	1020.121161	12.131379
21.601151	1018.194174	12.136384
21.120640	1010.780907	12.141389
21.175435	1001.706393	12.146394
21.146583	1009.642764	12.151399
21.204383	1021.804541	12.156403
21.528234	1010.975075	12.161408
21.221656	1017.626045	12.166413
21.409176	1002.876939	12.171418
21.230395	1003.309822	12.176423
21.196207	1002.833705	12.181427
21.133799	1000.583351	12.186432
21.174938	1009.796930	12.191437
21.214738	996.050919	12.196442
21.231699	1014.185730	12.201447
20.716453	1016.153010	12.206451
21.432052	1028.792140	12.211456
21.394996	1034.904274	12.216461
21.461181	1028.114107	12.221466
21.311741	1021.413807	12.226471
21.491952	1009.250288	12.231475
21.288151	1003.541421	12.236480
21.084119	1008.596255	12.241485
21.483145	1004.643236	12.246490
21.027741	1008.526172	12.251495
21.334894	1012.103496	12.256499
21.389218	1009.189312	12.261504
21.236934	1013.365671	12.266509
21.091424	1011.284696	12.271514
21.461153	1007.830119	12.276519
21.376111	1008.158114	12.281523
21.264712	1008.213524	12.286528
21.152155	1013.709385	12.291533
21.074737	1009.213187	12.296538
21.336944	1007.365463	12.301543
21.381756	1011.334740	12.306547
21.471363	1004.617541	12.311552
21.238666	1015.620439	12.316557
21.483636	1003.368847	12.321562
21.492758	1015.280808	12.326567
21.574433	1014.495483	12.331571
22.036098	1012.548824	12.336576
21.607665	1017.692268	12.341581
21.518092	1000.857124	12.346586
21.384733	991.255929	12.351591
21.404246	985.982462	12.356595
21.505375	985.195777	12.361600
21.237729	985.237713	12.366605
21.248781	975.002691	12.371610
21.417039	986.395900	12.376615
21.256551	983.300657	12.381619
21.470051	977.563277	12.386624
20.943772	990.960037	12.391629
21.352311	977.558977	12.396634
21.227462	975.888936	12.401639
21.190669	988.489272	12.406643
21.273729	978.076508	12.411648
20.755676	985.578457	12.416653
21.447494	977.064206	12.421658
21.247385	993.794243	12.426663
21.095508	985.501619	12.431667
21.393828	985.001254	12.436672
21.247754	990.181145	12.441677
21.156867	992.958293	12.446682
21.015296	982.985881	12.451687
20.726128	984.403213	12.456691
21.092575	989.283650	12.461696
21.125007	1009.127771	12.466701
20.999040	1012.996066	12.471706
21.312674	1025.654770	12.476711
20.978987	1029.649868	12.481715
21.140387	1026.284296	12.486720
21.089163	1023.907285	12.491725
21.238866	1023.047138	12.496730
20.925992	1038.917479	12.501735
21.080138	1032.765913	12.506739
21.518694	1025.305191	12.511744
21.209071	1032.403136	12.516749
20.798279	1026.999749	12.521754
21.196509	1028.097121	12.526759
21.051266	1028.654517	12.531763
21.371906	1019.324806	12.536768
21.066233	1023.484047	12.541773
21.312342	1024.723554	12.546778
21.498792	1030.016970	12.551783
21.165974	1031.413369	12.556787
21.417592	1020.462466	12.561792
21.438960	1029.836552	12.566797
21.862020	1025.671775	12.571802
21.505232	1026.382678	12.576807
21.297298	1024.853983	12.581811
21.497070	1020.214729	12.586816
21.427137	1017.672373	12.591821
21.411020	1005.193178	12.596826
21.542866	1000.153472	12.601831
21.571619	1001.063138	12.606835
21.747662	996.495854	12.611840
21.387140	1008.150662	12.616845
21.392179	997.895735	12.621850
21.491629	997.570784	12.626855
21.539272	999.331814	12.631859
21.587280	993.653987	12.636864
21.317049	989.923877	12.641869
21.063602	976.781976	12.646874
21.659014	978.502376	12.651879
21.295529	986.477558	12.656883
21.201612	970.138190	12.661888
20.989786	963.934531	12.666893
21.050856	969.860474	12.671898
21.174769	977.000113	12.676903
21.183021	993.273637	12.681907
21.611274	995.657040	12.686912
21.068750	999.227280	12.691917
21.397422	988.301478	12.696922
21.314060	977.111988	12.701927
21.105590	968.707497	12.706931
21.082671	972.461404	12.711936
21.257267	994.913621	12.716941
21.640151	986.426282	12.721946
21.308454	977.313443	12.726951
20.971200	976.622053	12.731955
21.105442	964.587634	12.736960
21.141087	996.060479	12.741965
21.581231	992.280808	12.746970
21.318999	989.405903	12.751975
21.420894	980.568850	12.756979
21.625367	968.807386	12.761984
21.616429	973.964153	12.766989
21.062703	976.085657	12.771994
21.179356	974.361972	12.776999
21.435317	973.970713	12.782003
21.456262	973.095145	12.787008
21.281322	976.678145	12.792013
21.401271	973.005088	12.797018
21.213537	975.950810	12.802023
21.161647	977.467589	12.807027
21.553218	973.597566	12.812032
21.441766	976.456394	12.817037
21.343061	971.535568	12.822042
21.415041	973.426634	12.827047
21.365404	980.498531	12.832051
21.435337	970.913020	12.837056
21.182483	981.061195	12.842061
21.291938	979.832953	12.847066
21.444914	975.614629	12.852071
21.010576	973.370023	12.857075
21.394137	970.902683	12.862080
21.615108	972.268074	12.867085
21.608642	958.140031	12.872090
21.517113	950.997203	12.877095
21.438138	953.824801	12.882099
21.595533	941.309985	12.887104
21.451841	945.763931	12.892109
21.075607	945.505145	12.897114
20.851948	943.296263	12.902119
20.872338	953.032047	12.907123
20.886614	952.008809	12.912128
20.591930	943.202274	12.917133
21.164468	967.244106	12.922138
21.176738	973.423548	12.927143
21.207851	980.048181	12.932147
21.340923	975.873533	12.937152
21.267585	981.374501	12.942157
21.450681	987.744527	12.947162
21.302248	978.397766	12.952167
21.078344	978.480755	12.957171
21.123950	975.961228	12.962176
21.193077	981.533296	12.967181
21.726692	982.217848	12.972186
21.642717	967.953086	12.977191
20.959894	962.403733	12.982195
20.780098	952.522367	12.987200
20.891950	974.090844	12.992205
21.271624	979.757296	12.997210
20.982838	984.919812	13.002215
21.232193	987.807569	13.007219
21.188831	982.169095	13.012224
21.299479	985.380633	13.017229
21.146652	988.297083	13.022234
21.161779	989.029086	13.027239
21.136739	995.194802	13.032243
21.443262	992.199091	13.037248
21.451239	992.549821	13.042253
21.247661	997.556022	13.047258
21.043402	984.693444	13.052263
21.445650	997.644036	13.057267
21.607826	987.656252	13.062272
21.492869	994.865671	13.067277
21.400874	984.584364	13.072282
21.558593	973.820119	13.077287
20.956185	969.452234	13.082291
21.259404	957.365165	13.087296
21.257249	956.888688	13.092301
20.964650	957.417268	13.097306
20.936735	973.385527	13.102311
21.112666	988.369512	13.107315
21.333159	988.855514	13.112320
21.027261	999.602137	13.117325
21.405109	988.973428	13.122330
21.019532	991.016762	13.127335
21.344905	988.452029	13.132339
21.405545	990.065173	13.137344
21.137746	999.628951	13.142349
21.025050	998.127744	13.147354
21.074380	997.332966	13.152359
21.201612	997.842460	13.157363
21.496981	993.165112	13.162368
21.038352	992.001507	13.167373
21.544040	989.506515	13.172378
21.351055	995.442870	13.177383
21.208227	993.783409	13.182387
21.241741	988.920040	13.187392
21.334248	993.826921	13.192397
21.018539	990.926448	13.197402
21.209195	995.452555	13.202407
21.034475	998.704734	13.207411
21.381796	987.234157	13.212416
21.241385	990.240848	13.217421
21.312632	991.479148	13.222426
21.361729	990.236385	13.227431
21.191871	999.255609	13.232435
21.689023	989.191838	13.237440
21.091656	1000.891985	13.242445
21.241278	998.231068	13.247450
21.328540	1000.353200	13.252455
21.250575	994.123420	13.257459
21.388377	994.155049	13.262464
21.476719	1001.529351	13.267469
21.057742	988.182533	13.272474
21.274378	989.868010	13.277479
21.235454	989.839151	13.282483
21.639563	983.311194	13.287488
21.448667	979.354327	13.292493
21.171064	968.213937	13.297498
21.438347	961.559450	13.302503
21.036432	964.650050	13.307507
21.463739	957.732471	13.312512
21.532745	967.813216	13.317517
21.257679	966.604325	13.322522
21.161856	964.043917	13.327527
21.287244	966.545953	13.332531
21.150683	964.521081	13.337536
20.947201	966.979636	13.342541
20.755352	969.273961	13.347546
21.068530	973.012873	13.352551
21.318397	989.861938	13.357555
21.557815	980.257230	13.362560
21.286753	979.387124	13.367565
21.067930	974.495576	13.372570
21.134021	974.095818	13.377575
20.968190	985.022494	13.382579
21.282294	992.324135	13.387584
21.209282	1004.698985	13.392589
21.674490	1001.708038	13.397594
21.372495	984.113940	13.402599
21.078005	972.608943	13.407603
21.147683	965.972940	13.412608
21.013300	984.676031	13.417613
21.083770	999.265610	13.422618
21.276224	1002.349836	13.427623
21.359332	997.150329	13.432627
21.754952	999.799853	13.437632
21.487634	989.894786	13.442637
21.328609	976.732355	13.447642
21.667209	971.588524	13.452647
21.199295	971.358877	13.457651
21.300806	969.191344	13.462656
21.055576	967.788259	13.467661
21.220315	967.051852	13.472666
21.152920	967.872608	13.477671
20.932709	977.258872	13.482675
20.949697	971.003741	13.487680
21.286049	977.915905	13.492685
20.943033	973.618807	13.497690
21.279418	983.684508	13.502695
21.121445	997.441283	13.507699
21.637316	1001.784132	13.512704
21.351764	998.841777	13.517709
21.347730	989.039595	13.522714
21.274426	984.076515	13.527719
21.077767	989.172710	13.532723
21.280797	976.552938	13.537728
21.322396	982.026305	13.542733
21.330413	979.754011	13.547738
21.050069	980.133254	13.552743
21.230192	987.485102	13.557747
21.210803	981.564230	13.562752
21.267282	990.922403	13.567757
21.161791	984.430900	13.572762
21.052951	988.938487	13.577767
21.081801	1001.234685	13.582771
21.558965	1006.236670	13.587776
21.472424	999.704806	13.592781
21.207890	984.139938	13.597786
21.147817	978.672094	13.602791
21.063726	990.052914	13.607795
21.105703	981.018109	13.612800
21.215090	999.434291	13.617805
21.497651	1002.310041	13.622810
21.195359	996.378853	13.627815
21.173031	986.582178	13.632819
21.477624	986.990209	13.637824
21.246906	992.111981	13.642829
21.292056	989.480821	13.647834
21.175836	986.591145	13.652839
21.198045	993.731256	13.657843
21.499352	989.026839	13.662848
21.701042	989.650671	13.667853
21.250514	979.897023	13.672858
21.248288	986.897242	13.677863
21.234870	988.429531	13.682867
21.514104	980.006545	13.687872
21.725373	992.227249	13.692877
21.630051	993.232794	13.697882
21.993551	988.327057	13.702887
21.699446	986.168536	13.707891
21.590526	965.649128	13.712896
21.443992	964.158068	13.717901
21.209377	957.562400	13.722906
21.191301	957.663387	13.727911
20.918595	965.692862	13.732915
21.013069	953.844479	13.737920
20.718466	961.092974	13.742925
20.864730	968.486934	13.747930
21.465382	977.644430	13.752935
21.139744	996.034144	13.757939
21.578914	983.637561	13.762944
21.198279	981.396378	13.767949
20.916779	965.907858	13.772954
21.387676	978.323640	13.777959
21.133707	993.684890	13.782963
21.592658	985.436351	13.787968
21.308721	976.523349	13.792973
21.055893	965.647527	13.797978
21.396597	967.726201	13.802983
21.236692	970.796624	13.807987
21.266595	956.187481	13.812992
21.097031	958.833639	13.817997
21.100995	973.434597	13.823002
21.337019	992.678924	13.828007
21.287254	996.901648	13.833011
21.531848	981.695541	13.838016
21.129367	975.231278	13.843021
20.961611	964.727317	13.848026
21.359033	970.732959	13.853031
21.213484	985.369825	13.858035
21.497275	981.895647	13.863040
21.094341	970.511876	13.868045
21.096062	970.891705	13.873050
21.469662	985.920348	13.878055
21.228386	984.131321	13.883059
21.559488	971.285910	13.888064
21.308923	972.679649	13.893069
21.284607	972.943152	13.898074
21.075274	964.725916	13.903079
21.047697	968.487726	13.908083
21.079147	966.753388	13.913088
21.167823	974.261040	13.918093
21.001630	984.935541	13.923098
21.542035	994.714033	13.928103
21.147448	1001.597584	13.933107
21.421845	992.335424	13.938112
21.217819	974.313619	13.943117
20.849701	984.824980	13.948122
21.119752	987.270637	13.953127
20.916090	996.570391	13.958131
21.214298	998.323197	13.963136
21.337404	1005.884171	13.968141
21.409502	1005.513383	13.973146
21.866142	999.005624	13.978151
21.101044	982.598953	13.983155
21.613091	976.075782	13.988160
21.228415	981.078686	13.993165
20.923988	976.460762	13.998170
21.442311	977.086751	14.003175
21.108805	979.366681	14.008179
21.006007	965.108702	14.013184
21.203453	992.025793	14.018189
21.205339	993.146139	14.023207
21.657786	993.478823	14.028224
21.119377	996.416608	14.033242
21.177383	989.796738	14.038259
21.155522	999.855131	14.043277
21.429620	1006.144804	14.048295
21.331856	1003.387345	14.053312
21.335961	1012.929447	14.058330
21.245476	1005.853105	14.063347
20.862036	1005.823953	14.068365
21.417483	1008.911618	14.073383
21.682643	995.351796	14.078400
21.714314	1013.774452	14.083418
21.672448	1002.855641	14.088435
21.892493	1006.044122	14.093453
21.655534	1002.486060	14.098471
21.351828	990.453407	14.103488
21.333518	994.651720	14.108506
21.400300	995.506860	14.113523
21.690379	1006.342936	14.118541
21.436132	1003.574115	14.123559
21.636798	1006.246196	14.128576
21.343808	1011.370806	14.133594
21.489966	996.132839	14.138611
21.516348	1006.911364	14.143629
21.670293	1007.035760	14.148647
21.626304	1003.328069	14.153664
21.256875	1015.781272	14.158682
21.244305	1007.129253	14.163699
21.213971	1008.296736	14.168717
21.619633	1033.659342	14.173735
21.879296	1046.483090	14.178752
21.721246	1048.788304	14.183770
21.749015	1039.891538	14.188787
21.872803	1043.208350	14.193805
21.897968	1041.771245	14.198823
21.935768	1037.966051	14.203840
21.684212	1048.535154	14.208858
21.768549	1040.846889	14.213875
21.782352	1051.191742	14.218893
21.656238	1042.178040	14.223911
21.874836	1034.776624	14.228928
21.643404	1044.094150	14.233946
21.702012	1046.629559	14.238963
21.851631	1044.999843	14.243981
22.004080	1058.097908	14.248999
22.503011	1069.488814	14.254016
22.615187	1049.179071	14.259034
22.424440	1043.026270	14.264051
22.160646	1046.411898	14.269069
22.296511	1048.367485	14.274087
22.443325	1037.887987	14.279104
22.538840	1047.295925	14.284122
22.711950	1036.119743	14.289139
22.464092	1035.651959	14.294157
22.525242	1036.891954	14.299175
22.367382	1021.812788	14.304192
22.216952	1016.406683	14.309210
22.430753	1010.842848	14.314227
22.066973	1015.374828	14.319245
21.979929	1027.050043	14.324263
22.803081	1024.609916	14.329280
22.399815	1037.200050	14.334298
22.458076	1024.762370	14.339315
22.299060	1022.939099	14.344333
22.271388	1025.983823	14.349351
22.344647	1026.612247	14.354368
22.674256	1041.627310	14.359386
22.753649	1028.487921	14.364403
22.563055	1017.788708	14.369421
21.949574	1014.475922	14.374439
22.416309	1021.762567	14.379456
22.123240	1035.473653	14.384474
22.404587	1037.652737	14.389491
22.370488	1035.255644	14.394509
22.374757	1045.027676	14.399527
22.300771	1044.110365	14.404544
22.203160	1040.161446	14.409562
22.399370	1038.242226	14.414579
22.370356	1050.191388	14.419597
22.305528	1067.831381	14.424615
22.687187	1064.378279	14.429632
22.517581	1074.764438	14.434650
22.622392	1065.134314	14.439667
22.966659	1069.924861	14.444685
22.460979	1070.241101	14.449703
22.784123	1064.694723	14.454720
22.715821	1072.898387	14.459738
22.766667	1068.340892	14.464755
22.586825	1078.419730	14.469773
22.737954	1073.385161	14.474791
23.086127	1065.706377	14.479808
22.856898	1068.168297	14.484826
22.973083	1075.496960	14.489843
23.120046	1067.030564	14.494861
23.166625	1069.737344	14.499879
23.117975	1066.059179	14.504896
23.052137	1077.561098	14.509914
22.987279	1071.599710	14.514931
23.110625	1062.485740	14.519949
22.690898	1076.208734	14.524967
23.187976	1071.557799	14.529984
22.983895	1080.013898	14.535002
23.320718	1090.811307	14.540019
23.455833	1081.761849	14.545037
22.918981	1079.456461	14.550055
23.473793	1075.367323	14.555072
23.302826	1067.682658	14.560090
23.395658	1068.054559	14.565107
23.440296	1067.949648	14.570125
23.459399	1073.620813	14.575143
23.470547	1063.543328	14.580160
23.221004	1062.271047	14.585178
22.856258	1071.459467	14.590195
23.277430	1066.937304	14.595213
23.665702	1073.599583	14.600231
23.395171	1060.987522	14.605248
23.202984	1075.709376	14.610266
23.464225	1075.440152	14.615283
23.411158	1068.390046	14.620301
23.348791	1085.656381	14.625319
23.788765	1081.887741	14.630336
23.497629	1078.605113	14.635354
23.489983	1073.516266	14.640371
23.584654	1071.582165	14.645389
23.430340	1075.095890	14.650407
23.639966	1078.415710	14.655424
23.790814	1087.549991	14.660442
23.923904	1081.249518	14.665459
23.807128	1067.990569	14.670477
23.519753	1070.673893	14.675495
24.075102	1062.737524	14.680512
23.844112	1065.469451	14.685530
23.845130	1063.070270	14.690547
23.958885	1060.021791	14.695565
23.572754	1065.818737	14.700583
23.956007	1061.872411	14.705600
23.977251	1063.181066	14.710618
23.704042	1064.212623	14.715635
23.908948	1065.257093	14.720653
23.602342	1074.549728	14.725671
23.982686	1065.743688	14.730688
23.983235	1071.885392	14.735706
23.427548	1065.200620	14.740723
24.092304	1062.617947	14.745741
23.913847	1065.802713	14.750759
24.053495	1069.857812	14.755776
23.815113	1075.480205	14.760794
24.273877	1092.136291	14.765811
24.580961	1085.841813	14.770829
24.160934	1081.959582	14.775847
23.719907	1065.638274	14.780864
24.146682	1076.596641	14.785882
24.058895	1077.095582	14.790899
23.970856	1076.058227	14.795917
24.342779	1093.273340	14.800935
24.243053	1095.563442	14.805952
24.087033	1099.263306	14.810970
24.257789	1101.082986	14.815987
24.563152	1107.144093	14.821005
24.177258	1106.667688	14.826023
24.248082	1100.282206	14.831040
24.429839	1098.854471	14.836058
24.434796	1101.194348	14.841075
24.319635	1100.666406	14.846093
23.824934	1102.876582	14.851111
24.497681	1096.816278	14.856128
24.626919	1099.228948	14.861146
24.625071	1097.338166	14.866163
24.957671	1092.810315	14.871181
24.360809	1086.353082	14.876199
24.441268	1087.737420	14.881216
24.646171	1095.019383	14.886234
24.288818	1094.759362	14.891251
24.614368	1095.478795	14.896269
24.508794	1099.119612	14.901287
24.489388	1097.629116	14.906304
24.325121	1095.450410	14.911322
24.624891	1098.480348	14.916339
24.577430	1091.882848	14.921357
24.417947	1102.588181	14.926375
24.525276	1092.340238	14.931392
24.908331	1090.453154	14.936410
24.422730	1089.099681	14.941427
24.742959	1084.939336	14.946445
24.747498	1088.550640	14.951463
24.738353	1085.253129	14.956480
24.676205	1090.842948	14.961498
24.660555	1091.329520	14.966515
25.287865	1098.196515	14.971533
24.862330	1095.786599	14.976551
24.961647	1086.332614	14.981568
25.191680	1082.383812	14.986586
24.708202	1090.593704	14.991603
24.989764	1088.618108	14.996621
24.817175	1096.810923	15.001639
25.427915	1105.616738	15.006656
25.980063	1088.319940	15.011674
25.594479	1085.133038	15.016691
25.725366	1074.183376	15.021709
25.624691	1079.188413	15.026727
25.007114	1078.230432	15.031744
25.223292	1076.419997	15.036762
25.020241	1072.287165	15.041779
25.365724	1070.608509	15.046797
25.582363	1084.877570	15.051815
25.376542	1062.413107	15.056832
25.544880	1061.666468	15.061850
24.711236	1054.786031	15.066867
25.477726	1060.244396	15.071885
25.115878	1072.862893	15.076903
24.973104	1075.027687	15.081920
25.331888	1082.753768	15.086938
24.970012	1086.788948	15.091955
25.284874	1075.902236	15.096973
25.250026	1083.107574	15.101991
25.396912	1077.796152	15.107008
25.417257	1077.910383	15.112026
25.340591	1083.287712	15.117043
25.744742	1078.680662	15.122061
25.786060	1082.647892	15.127079
25.510495	1084.847660	15.132096
25.211842	1077.932183	15.137114
25.359242	1082.385988	15.142131
25.577554	1090.444843	15.147149
25.500648	1104.014587	15.152167
25.494786	1099.577051	15.157184
25.583666	1101.944274	15.162202
25.785329	1110.304443	15.167219
25.384494	1103.382064	15.172237
25.728226	1099.724417	15.177255
25.853363	1108.351662	15.182272
25.998650	1109.776465	15.187290
25.456333	1109.667064	15.192307
25.892288	1103.848554	15.197325
25.835389	1105.958467	15.202343
26.105092	1112.206807	15.207360
26.257493	1104.611967	15.212378
26.017745	1110.542111	15.217395
26.303493	1104.146551	15.222413
26.222264	1107.328043	15.227431
25.544412	1112.051706	15.232448
25.780130	1104.442187	15.237466
25.650010	1106.128006	15.242483
25.672156	1105.111131	15.247501
25.656783	1117.001702	15.252519
25.756354	1125.380171	15.257536
26.002768	1133.361783	15.262554
26.462532	1139.723622	15.267571
26.469619	1137.556872	15.272589
26.663662	1127.264902	15.277607
26.647501	1127.408229	15.282624
26.557143	1108.631679	15.287642
26.584777	1105.211707	15.292659
26.474831	1103.332765	15.297677
26.476078	1106.817856	15.302695
26.552821	1107.443325	15.307712
26.542251	1100.073689	15.312730
26.403271	1098.084756	15.317747
26.662386	1093.854565	15.322765
26.607203	1096.719360	15.327783
26.507494	1102.657382	15.332800
26.724940	1094.934063	15.337818
26.679406	1101.393940	15.342835
26.843116	1094.399575	15.347853
26.841028	1096.067772	15.352871
26.794833	1109.281441	15.357888
27.000480	1099.943480	15.362906
26.585216	1095.066257	15.367923
26.456198	1087.570467	15.372941
26.847371	1087.452207	15.377959
26.745109	1094.541147	15.382976
26.622403	1095.696519	15.387994
26.414208	1091.686619	15.393011
26.626101	1094.932033	15.398029
26.783825	1096.529126	15.403047
26.795524	1109.104867	15.408064
27.198414	1100.181547	15.413082
26.737967	1106.562160	15.418099
26.710791	1105.658474	15.423117
26.954151	1104.528862	15.428135
26.431385	1101.156405	15.433152
26.785594	1096.326006	15.438170
26.762552	1106.735879	15.443187
26.785544	1094.851084	15.448205
26.918032	1099.053099	15.453223
26.986673	1096.454903	15.458240
27.296889	1103.158533	15.463258
27.191528	1111.426844	15.468275
27.253215	1097.636050	15.473293
26.795589	1097.505435	15.478311
26.722070	1107.858604	15.483328
26.979741	1112.847491	15.488346
26.883712	1135.898062	15.493363
27.318287	1136.808664	15.498381
26.836785	1140.895866	15.503399
26.740078	1141.006936	15.508416
27.121275	1138.108667	15.513434
26.555876	1139.093073	15.518451
26.902548	1149.678188	15.523469
27.199630	1151.037990	15.528487
27.162959	1164.041393	15.533504
27.421798	1167.101987	15.538522
27.366934	1167.405899	15.543539
27.681929	1161.596296	15.548557
27.995898	1159.900591	15.553575
27.542664	1169.888162	15.558592
28.023959	1159.292175	15.563610
27.647160	1170.269872	15.568627
28.047268	1170.837144	15.573645
28.261363	1159.725900	15.578663
27.754478	1143.150819	15.583680
27.556348	1135.072320	15.588698
27.302025	1140.554938	15.593715
27.269571	1135.825076	15.598733
27.469268	1145.567208	15.603751
27.342513	1156.212236	15.608768
27.964878	1158.123797	15.613786
27.772955	1164.448550	15.618803
27.539570	1168.245166	15.623821
27.782454	1166.081295	15.628839
27.854680	1175.147999	15.633856
28.020345	1161.518470	15.638874
27.556568	1170.064817	15.643891
27.525605	1162.276173	15.648909
28.098489	1158.469372	15.653927
27.913205	1165.441465	15.658944
27.681680	1163.702268	15.663962
27.662712	1179.441850	15.668979
28.138436	1196.142388	15.673997
27.895493	1193.488140	15.679015
27.808098	1203.135424	15.684032
28.230034	1182.614905	15.689050
28.048627	1195.376199	15.694067
28.351956	1190.148161	15.699085
28.534769	1196.395290	15.704103
27.815760	1195.555881	15.709120
28.484493	1194.802975	15.714138
28.659442	1192.193623	15.719155
28.610232	1197.513129	15.724173
28.911373	1199.276604	15.729191
28.877978	1188.621193	15.734208
28.710089	1171.952130	15.739226
28.327050	1162.662304	15.744243
28.388658	1160.335403	15.749261
28.560952	1154.877067	15.754279
28.566153	1159.084386	15.759296
28.906707	1158.812587	15.764314
28.820542	1157.168163	15.769331
28.746182	1163.044377	15.774349
28.911650	1154.667288	15.779367
28.985345	1161.350861	15.784384
28.915459	1150.859619	15.789402
29.105038	1158.999427	15.794419
28.837800	1158.162097	15.799437
28.910885	1155.702904	15.804455
28.745530	1153.887791	15.809472
28.952611	1146.214653	15.814490
28.876577	1139.766532	15.819507
28.524280	1132.151510	15.824525
28.401052	1138.569995	15.829543
28.298186	1152.483629	15.834560
28.410201	1161.184026	15.839578
28.501978	1163.158210	15.844595
28.315338	1164.033974	15.849613
28.750012	1167.516819	15.854631
28.718261	1193.676790	15.859648
28.962551	1196.894622	15.864666
29.012961	1197.953778	15.869683
28.985535	1201.901720	15.874701
29.147851	1199.739845	15.879719
28.773151	1200.022999	15.884736
28.987356	1205.044174	15.889754
28.652891	1200.609007	15.894771
28.866919	1194.713938	15.899789
29.227284	1207.726870	15.904807
28.792202	1225.519507	15.909824
29.082821	1214.466370	15.914842
29.282896	1219.165928	15.919859
29.594274	1228.589726	15.924877
29.799105	1223.687646	15.929895
29.283451	1225.345083	15.934912
29.627269	1217.254338	15.939930
29.632584	1222.885398	15.944947
29.311717	1222.293106	15.949965
29.894303	1215.619422	15.954983
29.305498	1219.139165	15.960000
29.439289	1224.085543	15.965018
29.784444	1206.939074	15.970035
29.626929	1224.720738	15.975053
29.958595	1218.107793	15.980071
29.983925	1199.803860	15.985088
30.280799	1191.419182	15.990106
30.241603	1194.667113	15.995123
29.730483	1186.095354	16.000141
30.009733	1176.451790	16.005159
29.941948	1193.775084	16.010176
30.235876	1180.586972	16.015194
30.036991	1186.111286	16.020211
30.067949	1196.511567	16.025229
30.062363	1183.507888	16.030247
29.745504	1180.674566	16.035264
30.010034	1182.628978	16.040282
30.058320	1199.049626	16.045299
29.734918	1196.384367	16.050317
29.903820	1191.753441	16.055335
29.731810	1192.990902	16.060352
29.683387	1194.878095	16.065370
30.042211	1182.747448	16.070387
29.406313	1189.072735	16.075405
29.468703	1185.561346	16.080423
29.498311	1202.000162	16.085440
29.674884	1211.791186	16.090458
29.560557	1219.422454	16.095475
29.971563	1228.091704	16.100493
30.435829	1218.700669	16.105511
30.264641	1223.963926	16.110528
30.143172	1224.519832	16.115546
30.318077	1226.772710	16.120563
30.621755	1238.918541	16.125581
30.279477	1230.817852	16.130599
30.064036	1239.218106	16.135616
30.160245	1247.740930	16.140634
30.801910	1239.438462	16.145651
30.490680	1242.296392	16.150669
30.651523	1242.208960	16.155687
30.674890	1247.971198	16.160704
30.731360	1253.749811	16.165722
30.773255	1242.784972	16.170739
30.753836	1244.828236	16.175757
30.988652	1244.668274	16.180775
31.091094	1244.067582	16.185792
30.591512	1226.959617	16.190810
30.542700	1220.329615	16.195827
30.806117	1244.902318	16.200845
30.975833	1239.040423	16.205863
30.568456	1246.325851	16.210880
30.877571	1243.843500	16.215898
31.174589	1240.515512	16.220915
30.723069	1244.220008	16.225933
30.709480	1245.098786	16.230951
30.827015	1244.638038	16.235968
30.658147	1249.101229	16.240986
30.969720	1243.693005	16.246003
30.844266	1245.333153	16.251021
31.038234	1238.996586	16.256039
31.066816	1244.687056	16.261056
30.876773	1242.087121	16.266074
30.912790	1245.461154	16.271091
30.959359	1246.268195	16.276109
31.291685	1245.048510	16.281127
31.233125	1252.228856	16.286144
31.039682	1257.337265	16.291162
31.244937	1269.850813	16.296179
31.138263	1281.863078	16.301197
31.555943	1279.308166	16.306215
31.610022	1279.442995	16.311232
31.566815	1271.828851	16.316250
32.052349	1263.615350	16.321267
31.594428	1251.288828	16.326285
31.384329	1237.371660	16.331303
31.354357	1242.140985	16.336320
31.295806	1248.029483	16.341338
31.658795	1254.200070	16.346355
31.721056	1272.296499	16.351373
31.754763	1263.990372	16.356391
31.754778	1270.782303	16.361408
31.601534	1265.952235	16.366426
32.005779	1265.219474	16.371443
31.518954	1265.688009	16.376461
31.757931	1261.304126	16.381479
31.695306	1269.528969	16.386496
31.620011	1271.546775	16.391514
31.471901	1271.561925	16.396531
31.502351	1274.101806	16.401549
31.704826	1274.691944	16.406567
31.938491	1275.160188	16.411584
31.656299	1278.277735	16.416602
32.051612	1266.631363	16.421619
31.861714	1275.473359	16.426637
31.758542	1272.272645	16.431655
31.836813	1284.166974	16.436672
32.245371	1302.307224	16.441690
32.092967	1295.085053	16.446707
31.945721	1308.009888	16.451725
32.173320	1306.805399	16.456743
32.897081	1305.151240	16.461760
32.599185	1305.696842	16.466778
32.754071	1292.266704	16.471795
32.183093	1278.507838	16.476813
32.428193	1272.036496	16.481831
32.493928	1268.572944	16.486848
32.335814	1272.079095	16.491866
32.507591	1265.493544	16.496883
32.002849	1280.004589	16.501901
32.986444	1294.514425	16.506919
33.063271	1278.397438	16.511936
32.502127	1267.952153	16.516954
32.295013	1262.772235	16.521971
32.319217	1266.149874	16.526989
32.762185	1270.981441	16.532007
32.357240	1277.612865	16.537024
32.602550	1292.075250	16.542042
33.210749	1293.907754	16.547059
32.598602	1295.067129	16.552077
32.955655	1288.344674	16.557095
33.058058	1281.253247	16.562112
32.564803	1272.287004	16.567130
32.815533	1278.218951	16.572147
32.452870	1300.678022	16.577165
32.893916	1292.763104	16.582183
33.280932	1297.846814	16.587200
33.034826	1305.885793	16.592218
33.507534	1297.138992	16.597235
33.165266	1300.838549	16.602253
32.945523	1296.417547	16.607271
33.321573	1293.987891	16.612288
32.813386	1298.056478	16.617306
33.190526	1293.815841	16.622323
33.041212	1296.291656	16.627341
33.247068	1291.122034	16.632359
33.477462	1296.390091	16.637376
33.155763	1294.330089	16.642394
33.145499	1291.129979	16.647411
33.134469	1292.765082	16.652429
33.145865	1292.538692	16.657447
33.341321	1296.414188	16.662464
33.438311	1294.329649	16.667482
33.623036	1293.852655	16.672499
33.360694	1296.930579	16.677517
33.566146	1293.811604	16.682535
33.410760	1296.058912	16.687552
32.903709	1296.008427	16.692570
33.307216	1293.842199	16.697587
33.253605	1310.461160	16.702605
33.333249	1325.869781	16.707623
33.673089	1317.747379	16.712640
33.577248	1320.693602	16.717658
33.810932	1313.627294	16.722675
33.845660	1320.871999	16.727693
33.673149	1321.582735	16.732711
34.224840	1313.166903	16.737728
33.590055	1313.787197	16.742746
33.725055	1309.078183	16.747763
34.125365	1314.315539	16.752781
34.049161	1317.709223	16.757799
34.210115	1318.735260	16.762816
34.211025	1320.975855	16.767834
34.076668	1316.287428	16.772851
33.741357	1318.391163	16.777869
33.699059	1314.512225	16.782887
34.160724	1307.959639	16.787904
33.754363	1322.482597	16.792922
33.975207	1334.232037	16.797939
34.480801	1342.452811	16.802957
34.244679	1346.546424	16.807975
34.425401	1349.739356	16.812992
34.314324	1350.524214	16.818010
34.544910	1349.431818	16.823027
34.174533	1348.099908	16.828045
34.418689	1340.347476	16.833063
34.400853	1341.589620	16.838080
34.421955	1345.193026	16.843098
34.574756	1344.192320	16.848115
34.443182	1348.230209	16.853133
34.370540	1356.452484	16.858151
34.797347	1349.028216	16.863168
34.747108	1350.470816	16.868186
35.027592	1347.757115	16.873203
34.752081	1349.691924	16.878221
34.650907	1343.621687	16.883239
34.659437	1344.061991	16.888256
34.585221	1350.674146	16.893274
34.631851	1342.763043	16.898291
34.989962	1347.386327	16.903309
34.616463	1347.588954	16.908327
35.097204	1343.773890	16.913344
34.791737	1339.805016	16.918362
34.637836	1343.156903	16.923379
34.804071	1345.610517	16.928397
34.702946	1337.868463	16.933415
35.006957	1345.686359	16.938432
34.651867	1372.642688	16.943450
34.964583	1370.147494	16.948467
34.975561	1372.472205	16.953485
35.073923	1373.103821	16.958503
35.497943	1370.863980	16.963520
35.031991	1372.128620	16.968538
35.317978	1366.352265	16.973555
35.144965	1368.140356	16.978573
35.476232	1362.466879	16.983591
35.602075	1362.525225	16.988608
35.540585	1369.509257	16.993626
35.261831	1363.094620	16.998643
35.343096	1365.342706	17.003661
35.479458	1367.360458	17.008679
35.789286	1364.770082	17.013696
35.703267	1371.687842	17.018714
35.677879	1365.197083	17.023731
35.805191	1371.819187	17.028749
35.732769	1369.321123	17.033767
35.703456	1363.824832	17.038784
35.158117	1372.720344	17.043802
35.517575	1373.708020	17.048819
35.626153	1388.581770	17.053837
35.513796	1389.865322	17.058855
36.263689	1387.149094	17.063872
36.416316	1387.533588	17.068890
36.345567	1382.820848	17.073907
36.196300	1377.550257	17.078925
36.102747	1362.487297	17.083943
36.083879	1359.540247	17.088960
35.676273	1360.762596	17.093978
35.944926	1360.318460	17.098995
36.427594	1376.919174	17.104013
35.872864	1376.711887	17.109031
36.184820	1380.166211	17.114048
36.021921	1392.834720	17.119066
36.401783	1393.109775	17.124083
36.474974	1392.570791	17.129101
36.399647	1393.994466	17.134119
36.600364	1386.710134	17.139136
36.230234	1387.235443	17.144154
36.336744	1388.624791	17.149171
36.489587	1383.727638	17.154189
36.063057	1398.762048	17.159207
36.389632	1391.410855	17.164224
36.738449	1399.895965	17.169242
36.648964	1390.014281	17.174259
36.922790	1390.042136	17.179277
36.299068	1399.291291	17.184295
36.676771	1397.246414	17.189312
36.557470	1396.747126	17.194330
36.153551	1393.819232	17.199347
36.354686	1394.689159	17.204365
36.247288	1397.407434	17.209383
36.213204	1403.932408	17.214400
36.273529	1414.420328	17.219418
36.685000	1407.389251	17.224435
36.837576	1408.810470	17.229453
36.831261	1419.440147	17.234471
37.061778	1428.843281	17.239488
37.363232	1442.780775	17.244506
37.082870	1427.771042	17.249523
37.193411	1429.926314	17.254541
37.322522	1430.787330	17.259559
37.196717	1417.932032	17.264576
37.172933	1418.597586	17.269594
37.536402	1428.693350	17.274611
37.198020	1423.456743	17.279629
37.206896	1430.884689	17.284647
37.313197	1435.786630	17.289664
37.711409	1443.577006	17.294682
37.645613	1435.512673	17.299699
37.675472	1417.538449	17.304717
37.376371	1414.623292	17.309735
37.239962	1410.643131	17.314752
37.481058	1429.424900	17.319770
37.566909	1438.628018	17.324787
37.377332	1436.748514	17.329805
37.653130	1446.574253	17.334823
37.726482	1435.407408	17.339840
37.638225	1445.075858	17.344858
37.632124	1441.639153	17.349875
37.868504	1438.965679	17.354893
37.549817	1453.581217	17.359911
37.568000	1451.540881	17.364928
37.608422	1455.272509	17.369946
37.551630	1451.462170	17.374963
37.815074	1443.255549	17.379981
38.117932	1468.648304	17.384999
38.415626	1458.883676	17.390016
38.654764	1444.042758	17.395034
38.343966	1434.718727	17.400051
38.585710	1425.516524	17.405069
38.454576	1442.784019	17.410087
38.573377	1420.120062	17.415104
38.746639	1431.268618	17.420122
38.525770	1430.299294	17.425139
38.891047	1429.511785	17.430157
38.491287	1409.088933	17.435175
38.456419	1397.146499	17.440192
38.513717	1394.325373	17.445210
38.219950	1402.180427	17.450227
38.553075	1388.107382	17.455245
38.143038	1400.674949	17.460263
38.615836	1410.668484	17.465280
38.333684	1429.847476	17.470298
38.442700	1431.755741	17.475315
38.734619	1433.298362	17.480333
38.556788	1439.186120	17.485351
38.468979	1434.913341	17.490368
38.564691	1436.526220	17.495386
38.359171	1431.955481	17.500403
38.196090	1432.433874	17.505421
38.485309	1450.210467	17.510439
38.660431	1460.935849	17.515456
38.895873	1466.716537	17.520474
38.709015	1471.739625	17.525491
38.763118	1453.625363	17.530509
38.703069	1467.692977	17.535527
39.234051	1460.159447	17.540544
38.900977	1467.168037	17.545562
39.122646	1468.089178	17.550579
38.935272	1469.581288	17.555597
38.996925	1485.887730	17.560615
39.117790	1488.379070	17.565632
39.059571	1493.601392	17.570650
39.203903	1497.929845	17.575667
39.475163	1485.873039	17.580685
39.360419	1500.198510	17.585703
39.716319	1497.321445	17.590720
39.650905	1494.109486	17.595738
39.673936	1502.302442	17.600755
39.624502	1496.289815	17.605773
39.422859	1498.306869	17.610791
39.172705	1493.290963	17.615808
39.737319	1490.409220	17.620826
39.460075	1498.474897	17.625843
39.656103	1492.866690	17.630861
39.644699	1496.985599	17.635879
39.435763	1500.624937	17.640896
39.462520	1498.058267	17.645914
39.727022	1509.185330	17.650931
40.155252	1511.131404	17.655949
40.047668	1502.942297	17.660967
40.201484	1513.194940	17.665984
40.053998	1510.334880	17.671002
40.114708	1512.571156	17.676019
40.219044	1509.748638	17.681037
39.958161	1506.445768	17.686055
40.144484	1512.347111	17.691072
40.375866	1511.817619	17.696090
40.158512	1510.313773	17.701107
40.613729	1501.891939	17.706125
40.355336	1508.558181	17.711143
40.511638	1510.730818	17.716160
40.604500	1508.673339	17.721178
40.144308	1513.814178	17.726195
40.630092	1505.738713	17.731213
40.490322	1508.443658	17.736231
40.179763	1512.815457	17.741248
40.763427	1507.121097	17.746266
40.688503	1507.771404	17.751283
40.787240	1510.875267	17.756301
40.596574	1517.671648	17.761319
40.957833	1513.710477	17.766336
40.848337	1517.526097	17.771354
40.581376	1510.806589	17.776371
40.667398	1506.490993	17.781389
40.189603	1512.574317	17.786407
40.013484	1509.155328	17.791424
40.371538	1519.954516	17.796442
40.479471	1535.171859	17.801459
40.763224	1543.180356	17.806477
40.700974	1547.796236	17.811495
40.716064	1542.294239	17.816512
41.321067	1551.410777	17.821530
41.107482	1545.792063	17.826547
41.020686	1547.492156	17.831565
41.315852	1567.291308	17.836583
41.431151	1567.512897	17.841600
42.091381	1549.363902	17.846618
41.895584	1536.766202	17.851635
42.006769	1530.119267	17.856653
42.037636	1531.712956	17.861671
42.020965	1524.316998	17.866688
42.367385	1508.806769	17.871706
41.936402	1503.719883	17.876723
42.142786	1488.338025	17.881741
42.149040	1486.156014	17.886759
41.979196	1487.766786	17.891776
42.032104	1482.169340	17.896794
41.908180	1488.350661	17.901811
41.894328	1481.316875	17.906829
41.791973	1473.993117	17.911847
41.735054	1476.604316	17.916864
41.856230	1471.757845	17.921882
41.709161	1481.206850	17.926899
42.157276	1479.236907	17.931917
42.270148	1485.694589	17.936935
42.114085	1490.553332	17.941952
42.231487	1491.105697	17.946970
42.094430	1493.375090	17.951987
42.219260	1483.471563	17.957005
42.075477	1484.266366	17.962023
42.029794	1489.188870	17.967040
42.500199	1484.767609	17.972058
41.689945	1492.176560	17.977075
42.017449	1492.862211	17.982093
42.020862	1493.545155	17.987111
41.611499	1493.893316	17.992128
41.717761	1497.900703	17.997146
42.039124	1513.803949	18.002163
42.215461	1518.540349	18.007181
42.016312	1524.923184	18.012199
42.216273	1529.820122	18.017216
42.575576	1532.182784	18.022234
42.559363	1557.490217	18.027251
43.010820	1551.739366	18.032269
42.594586	1550.828335	18.037287
42.563052	1551.250315	18.042304
42.955274	1559.506787	18.047322
42.866076	1553.658847	18.052339
42.655407	1552.248349	18.057357
42.691135	1559.578829	18.062375
42.468312	1556.608830	18.067392
42.999331	1554.948714	18.072410
42.719690	1568.875309	18.077427
42.891993	1576.369015	18.082445
43.354284	1575.616447	18.087463
43.056097	1581.048857	18.092480
43.259126	1579.061861	18.097498
43.316923	1585.713693	18.102515
43.304719	1581.935840	18.107533
43.567646	1581.875005	18.112551
43.388158	1583.715024	18.117568
43.380741	1573.484076	18.122586
43.267409	1585.824523	18.127603
43.152337	1583.385711	18.132621
43.230001	1581.029221	18.137639
43.401469	1583.556393	18.142656
43.820591	1586.212384	18.147674
43.719349	1597.494747	18.152691
43.885393	1601.689177	18.157709
44.183683	1595.830304	18.162727
43.722419	1590.435161	18.167744
44.091601	1576.556181	18.172762
43.921832	1575.973404	18.177779
43.794995	1580.651948	18.182797
43.691787	1578.293395	18.187815
44.180758	1589.214689	18.192832
44.018888	1591.044600	18.197850
43.774056	1594.253059	18.202867
43.821873	1601.645273	18.207885
44.030916	1608.923617	18.212903
43.948820	1609.092034	18.217920
43.854334	1594.636557	18.222938
43.889910	1609.869529	18.227955
43.799021	1605.464539	18.232973
44.664690	1618.982192	18.237991
44.370687	1628.297798	18.243008
44.782371	1624.489783	18.248026
44.416765	1622.128568	18.253043
44.566749	1626.368676	18.258061
44.748077	1623.066744	18.263079
44.198728	1632.883270	18.268096
44.598302	1634.159001	18.273114
44.381788	1642.560835	18.278131
44.488610	1636.134707	18.283149
44.923069	1637.767884	18.288167
44.869432	1639.400485	18.293184
45.087462	1639.136693	18.298202
44.744619	1638.717855	18.303219
44.912196	1635.318660	18.308237
45.062973	1636.281497	18.313255
44.925370	1639.373537	18.318272
45.091995	1627.190058	18.323290
45.235738	1639.130133	18.328307
44.818816	1633.819901	18.333325
45.194348	1628.860474	18.338343
44.974907	1637.060422	18.343360
45.475958	1628.405440	18.348378
45.334311	1640.500757	18.353395
45.431925	1647.868312	18.358413
45.587869	1636.208763	18.363431
45.209109	1646.264190	18.368448
45.652449	1656.816934	18.373466
45.453457	1661.357856	18.378483
46.150612	1666.864554	18.383501
45.912877	1647.970086	18.388519
45.548220	1639.692291	18.393536
45.629565	1630.481244	18.398554
45.494134	1645.943593	18.403571
45.773113	1661.676283	18.408589
46.057530	1654.629868	18.413607
45.788547	1669.179205	18.418624
46.033791	1664.437008	18.423642
45.791224	1664.369129	18.428659
46.029392	1659.323388	18.433677
46.174660	1664.319913	18.438695
45.585730	1661.869407	18.443712
45.920631	1660.308267	18.448730
46.420281	1661.289646	18.453747
46.020282	1659.578490	18.458765
46.170728	1663.121599	18.463783
45.487189	1664.195588	18.468800
45.686904	1662.440672	18.473818
45.946178	1684.379834	18.478835
46.147141	1687.285869	18.483853
46.359186	1692.736362	18.488871
46.450427	1696.817250	18.493888
46.856245	1698.388408	18.498906
46.777113	1688.313004	18.503923
46.645615	1692.379712	18.508941
46.705549	1694.037339	18.513959
46.575344	1699.502021	18.518976
46.854595	1691.176799	18.523994
46.683135	1688.836230	18.529011
46.807729	1689.842146	18.534029
46.701658	1688.143198	18.539047
46.831373	1698.968271	18.544064
47.013413	1692.993845	18.549082
46.977240	1693.572941	18.554099
46.611803	1707.247015	18.559117
47.173436	1703.006926	18.564135
46.918716	1716.077311	18.569152
47.096599	1718.958959	18.574170
47.632839	1717.400700	18.579187
47.218070	1718.727071	18.584205
47.301040	1708.812861	18.589223
47.235011	1715.478104	18.594240
47.261663	1712.751162	18.599258
46.996912	1712.575261	18.604275
46.886106	1717.570820	18.609293
46.925413	1716.763980	18.614311
47.649331	1725.675173	18.619328
48.302833	1727.504297	18.624346
48.597415	1727.914075	18.629363
48.500006	1704.619373	18.634381
48.570703	1700.677654	18.639399
48.338598	1700.254003	18.644416
48.364367	1689.117579	18.649434
48.076549	1668.598413	18.654451
47.946222	1668.653432	18.659469
48.089931	1656.359673	18.664487
47.514028	1664.205349	18.669504
47.789507	1675.338524	18.674522
47.955546	1685.300570	18.679539
47.740144	1688.494551	18.684557
47.809271	1681.976431	18.689575
48.101284	1695.546043	18.694592
48.260612	1695.701024	18.699610
48.044285	1695.342392	18.704627
48.151331	1713.669478	18.709645
48.131756	1722.496304	18.714663
48.135574	1731.676648	18.719680
48.602983	1729.103296	18.724698
48.458839	1724.524704	18.729715
47.907633	1732.980426	18.734733
48.415914	1730.961944	18.739751
48.439118	1733.461011	18.744768
48.679877	1747.184748	18.749786
48.894148	1752.624250	18.754803
48.765944	1764.962269	18.759821
49.120118	1761.374343	18.764839
48.984710	1763.213913	18.769856
48.891993	1763.812156	18.774874
49.470211	1758.424584	18.779891
48.973397	1760.209173	18.784909
49.558796	1756.726898	18.789927
49.182414	1743.670563	18.794944
49.325896	1738.752855	18.799962
49.394754	1745.586345	18.804979
49.093051	1744.985232	18.809997
49.299479	1746.007440	18.815015
49.110461	1752.849315	18.820032
49.035598	1757.396546	18.825050
49.489158	1761.108601	18.830067
49.551997	1766.037392	18.835085
49.479955	1755.284271	18.840103
49.582461	1762.593553	18.845120
49.421326	1750.038169	18.850138
49.534927	1748.207840	18.855155
49.565350	1758.146327	18.860173
49.754618	1754.328771	18.865191
49.597744	1756.411025	18.870208
49.673384	1770.228454	18.875226
50.037948	1789.414736	18.880243
50.072940	1789.872960	18.885261
50.269095	1786.008148	18.890279
50.264390	1792.760559	18.895296
50.335224	1790.209909	18.900314
50.227529	1780.900853	18.905331
49.551214	1790.500239	18.910349
49.964893	1783.529648	18.915367
50.000010	1790.989885	18.920384
49.986309	1794.113869	18.925402
50.364494	1785.790534	18.930419
50.485819	1795.748504	18.935437
50.728749	1787.332203	18.940455
50.516803	1781.609566	18.945472
51.017058	1787.767070	18.950490
51.046614	1779.523199	18.955507
50.682841	1781.075112	18.960525
51.015062	1762.654903	18.965543
50.897781	1774.101580	18.970560
50.782502	1771.648992	18.975578
51.013476	1764.727453	18.980595
51.162953	1777.096623	18.985613
51.334893	1761.184118	18.990631
51.142214	1773.568242	18.995648
50.893463	1773.591197	19.000666
51.102500	1766.670267	19.005683
50.867740	1771.063004	19.010701
51.266876	1771.748988	19.015719
51.369231	1766.504030	19.020736
51.128881	1772.334907	19.025754
51.436796	1771.726136	19.030771
51.536824	1768.569230	19.035789
51.169638	1772.255056	19.040807
51.116370	1780.836088	19.045824
51.210077	1798.442244	19.050842
51.393987	1785.966666	19.055859
51.196821	1796.359996	19.060877
51.486885	1798.350273	19.065895
51.277695	1799.156699	19.070912
50.873196	1807.440438	19.075930
51.208713	1820.303402	19.080947
51.358934	1831.384926	19.085965
51.582531	1830.050360	19.090983
51.568707	1837.675328	19.096000
52.047504	1851.420165	19.101018
52.128838	1855.972931	19.106035
51.841228	1863.415296	19.111053
52.085768	1848.566770	19.116071
52.843759	1854.625775	19.121088
52.422952	1856.132349	19.126106
52.474606	1859.631804	19.131123
52.412274	1854.299683	19.136141
52.567775	1854.986098	19.141159
52.627934	1848.795865	19.146176
52.730909	1857.154063	19.151194
53.118656	1844.899428	19.156211
52.792252	1845.437728	19.161229
52.363381	1828.639850	19.166247
52.895529	1825.156453	19.171264
53.057074	1840.018009	19.176282
52.938134	1835.438607	19.181299
52.469308	1832.036262	19.186317
52.977078	1841.679549	19.191335
52.776977	1844.852039	19.196352
52.493176	1846.520184	19.201370
52.680152	1849.536930	19.206387
52.799889	1841.448058	19.211405
53.243891	1844.316786	19.216423
52.995136	1840.824733	19.221440
53.119843	1852.852104	19.226458
53.691884	1859.563543	19.231475
53.458064	1867.960195	19.236493
53.762445	1855.933258	19.241511
53.899288	1845.259237	19.246528
53.566138	1845.627805	19.251546
53.652127	1836.737140	19.256563
53.580139	1839.802221	19.261581
53.432138	1838.024213	19.266599
53.644543	1839.269053	19.271616
53.312811	1843.563067	19.276634
53.783444	1857.539653	19.281651
53.551824	1868.676039	19.286669
53.762100	1869.631052	19.291687
53.855907	1879.576468	19.296704
53.812698	1871.478112	19.301722
54.187569	1867.388913	19.306739
54.207184	1879.802086	19.311757
53.740168	1875.089411	19.316775
54.322918	1869.732918	19.321792
53.968379	1879.975703	19.326810
53.831899	1872.087457	19.331827
54.395635	1875.243969	19.336845
54.493692	1889.459681	19.341863
54.433532	1892.660950	19.346880
54.230991	1897.450612	19.351898
54.705770	1888.689348	19.356915
54.621784	1896.987877	19.361933
54.599092	1890.402331	19.366951
54.688470	1882.769489	19.371968
54.655251	1884.143857	19.376986
54.541533	1884.595292	19.382003
54.783002	1889.107620	19.387021
54.928755	1892.101910	19.392039
54.780064	1890.729185	19.397056
54.705223	1887.248254	19.402074
54.893995	1888.506206	19.407091
55.015479	1909.894827	19.412109
55.154507	1916.845906	19.417127
55.567509	1919.391180	19.422144
55.314034	1924.163988	19.427162
55.328987	1917.432194	19.432179
55.376956	1921.562692	19.437197
55.449219	1922.442538	19.442215
55.399169	1922.150286	19.447232
55.384221	1926.524673	19.452250
55.920135	1907.441731	19.457267
56.194458	1914.275506	19.462285
55.879677	1905.662990	19.467303
56.019239	1911.327589	19.472320
55.912149	1913.081601	19.477338
56.086939	1909.317284	19.482355
55.967417	1906.735070	19.487373
55.866155	1908.287663	19.492391
56.027151	1904.168580	19.497408
55.856215	1907.732983	19.502426
56.299150	1906.797083	19.507443
55.995080	1900.334587	19.512461
56.075143	1905.697139	19.517479
55.934913	1900.931579	19.522496
55.967820	1917.015418	19.527514
56.204280	1910.903216	19.532531
55.968410	1912.652139	19.537549
55.972974	1927.573373	19.542567
56.460171	1925.575414	19.547584
56.109482	1940.845402	19.552602
56.476351	1933.547688	19.557619
56.001743	1939.050630	19.562637
56.094803	1945.016165	19.567655
56.561099	1959.185738	19.572672
56.312240	1969.428181	19.577690
56.738531	1971.817228	19.582707
56.693398	1979.416920	19.587725
56.716781	1969.021357	19.592743
57.095967	1975.983657	19.597760
57.007832	1990.247133	19.602778
57.423917	1991.323976	19.607795
57.838375	1995.187301	19.612813
57.658734	1982.852648	19.617831
57.708258	1965.610348	19.622848
57.741991	1967.659557	19.627866
57.864532	1963.158023	19.632883
57.558244	1965.324590	19.637901
57.619515	1961.606892	19.642919
57.823385	1953.736247	19.647936
57.507516	1962.749065	19.652954
57.348570	1958.852166	19.657971
57.346334	1965.698730	19.662989
57.100306	1963.500055	19.668007
57.852924	1973.258947	19.673024
57.972537	1993.810095	19.678042
57.856546	1986.355739	19.683059
57.504127	1994.654273	19.688077
57.433212	1999.765934	19.693095
57.885070	1992.348488	19.698112
57.682177	2019.398354	19.703130
58.082930	2030.123638	19.708147
58.515329	2026.621861	19.713165
58.445041	2030.783688	19.718183
58.650233	2024.907937	19.723200
58.752755	2030.604129	19.728218
58.659105	2024.775282	19.733235
58.775051	2015.085965	19.738253
58.725230	2011.409746	19.743271
58.903189	2012.116731	19.748288
58.845372	2014.642334	19.753306
58.799703	2008.031146	19.758323
58.873478	2007.421954	19.763341
58.633429	2012.780756	19.768359
59.010875	2005.606409	19.773376
59.200618	2005.240755	19.778394
59.122529	2005.399826	19.783411
59.012444	2007.533154	19.788429
58.908166	2011.575983	19.793447
59.138659	2008.916417	19.798464
58.922105	2017.510216	19.803482
59.329219	2036.022094	19.808499
59.498943	2036.901381	19.813517
59.381776	2041.294901	19.818535
59.762332	2038.840737	19.823552
59.695991	2047.089069	19.828570
59.618055	2042.701816	19.833587
60.149771	2044.701882	19.838605
59.970102	2041.835035	19.843623
59.700168	2021.675381	19.848640
59.656226	2032.422964	19.853658
59.285359	2033.189000	19.858675
59.482020	2033.846711	19.863693
59.269941	2047.806247	19.868711
59.584775	2048.242488	19.873728
59.608249	2071.430269	19.878746
60.028801	2075.496929	19.883763
60.129722	2081.061506	19.888781
59.973105	2077.946571	19.893799
60.353247	2074.362787	19.898816
60.255391	2078.263173	19.903834
60.344863	2075.126523	19.908851
60.487793	2079.688088	19.913869
60.569521	2086.688443	19.918887
60.808944	2094.313825	19.923904
60.915526	2084.590632	19.928922
61.068875	2096.060446	19.933939
61.290988	2089.801795	19.938957
61.045999	2077.389281	19.943975
61.251329	2058.524668	19.948992
61.077830	2053.338722	19.954010
61.238485	2054.538113	19.959027
61.566576	2049.757185	19.964045
61.312873	2050.068823	19.969063
61.170427	2046.735687	19.974080
61.013463	2049.099135	19.979098
61.136219	2054.984021	19.984115
61.364825	2064.616246	19.989133
61.149500	2073.901694	19.994151
61.211371	2070.714257	19.999168
61.612881	2080.785418	20.004186
61.327322	2082.697624	20.009203
61.397597	2081.000293	20.014221
61.323528	2082.098965	20.019239
61.460703	2085.314479	20.024256
61.756253	2104.587402	20.029274
61.907817	2109.654261	20.034291
62.256631	2106.079778	20.039309
62.154945	2110.185976	20.044327
62.442904	2110.119275	20.049344
62.217097	2112.590612	20.054362
62.102157	2114.725575	20.059379
62.599261	2106.691964	20.064397
62.256857	2116.263042	20.069415
62.506662	2111.199018	20.074432
62.702107	2115.942563	20.079450
62.228418	2118.749355	20.084467
62.781338	2105.094351	20.089485
62.326439	2113.151425	20.094503
62.468939	2100.628359	20.099520
62.556260	2101.233154	20.104538
62.285087	2105.318009	20.109555
62.710494	2115.142541	20.114573
62.324183	2130.829115	20.119591
62.685436	2134.296814	20.124608
62.984627	2138.468956	20.129626
62.823747	2143.086959	20.134643
62.907915	2139.359387	20.139661
62.525621	2154.711390	20.144679
63.171665	2162.334030	20.149696
63.284831	2168.526552	20.154714
62.897941	2177.897390	20.159731
63.195609	2171.911621	20.164749
63.172757	2184.744187	20.169767
63.485163	2174.967144	20.174784
63.371360	2180.651260	20.179802
63.373088	2192.520422	20.184819
63.682238	2200.782029	20.189837
63.902864	2210.685832	20.194855
64.324287	2202.900616	20.199872
64.121730	2200.024670	20.204890
64.075219	2205.235772	20.209907
64.079733	2196.740031	20.214925
64.257818	2197.585213	20.219943
64.471664	2195.229302	20.224960
64.473386	2198.955537	20.229978
64.244259	2200.539136	20.234995
64.451493	2193.178107	20.240013
64.339124	2207.237242	20.245031
64.402548	2199.460642	20.250048
64.801035	2189.351462	20.255066
64.286354	2198.163820	20.260083
64.780249	2190.527627	20.265101
64.132150	2199.160467	20.270119
64.299978	2191.095066	20.275136
64.431973	2212.869363	20.280154
64.789318	2219.069655	20.285171
64.917927	2222.642625	20.290189
65.010175	2228.408772	20.295207
65.239055	2222.771835	20.300224
65.537347	2210.413339	20.305242
65.850297	2215.001315	20.310259
65.884899	2205.188405	20.315277
65.656019	2206.555395	20.320295
65.782799	2205.068081	20.325312
66.138549	2192.753298	20.330330
66.057534	2182.000240	20.335347
65.966895	2170.963758	20.340365
65.368008	2173.588845	20.345383
65.445547	2170.477453	20.350400
65.603685	2167.505810	20.355418
65.656181	2186.676783	20.360435
65.920384	2191.288073	20.365453
65.836182	2197.349066	20.370471
66.146566	2199.912768	20.375488
66.097070	2203.091797	20.380506
65.841207	2211.460517	20.385523
65.878500	2199.807504	20.390541
65.673873	2202.463441	20.395559
65.847784	2209.155877	20.400576
66.103601	2209.693201	20.405594
66.427477	2231.609457	20.410611
66.493406	2227.070696	20.415629
66.514348	2227.727040	20.420647
66.882119	2236.996092	20.425664
67.269888	2231.946965	20.430682
66.861338	2229.373299	20.435699
67.155989	2222.375278	20.440717
66.923925	2229.202689	20.445735
67.132850	2225.676576	20.450752
66.996321	2237.343459	20.455770
67.150960	2233.922728	20.460787
66.794516	2234.225601	20.465805
66.788978	2233.131104	20.470823
67.289815	2227.453840	20.475840
67.188761	2226.763967	20.480858
67.017186	2232.717887	20.485875
67.455089	2243.924819	20.490893
67.252329	2257.174175	20.495911
66.988706	2261.474343	20.500928
67.349110	2257.614331	20.505946
67.461078	2259.235535	20.510963
67.438471	2263.225838	20.515981
67.458218	2268.887876	20.520999
67.635233	2281.109002	20.526016
67.595434	2282.220713	20.531034
67.461208	2292.635869	20.536051
67.697118	2290.736075	20.541069
67.517437	2308.811395	20.546087
68.010393	2313.159058	20.551104
68.286638	2302.248588	20.556122
68.086351	2305.356625	20.561139
68.438053	2299.662378	20.566157
68.247919	2315.514745	20.571175
68.392232	2324.863899	20.576192
69.004860	2327.692389	20.581210
68.845702	2340.241317	20.586227
68.810430	2331.937393	20.591245
69.191378	2336.750792	20.596263
69.301224	2331.839060	20.601280
69.392797	2327.284061	20.606298
69.308043	2318.196378	20.611315
69.178172	2300.754509	20.616333
69.039312	2302.207665	20.621351
69.037376	2309.878470	20.626368
69.356434	2311.934327	20.631386
69.267936	2333.452061	20.636403
69.755822	2324.873379	20.641421
69.896470	2321.237671	20.646439
69.556253	2317.404049	20.651456
70.059513	2321.173480	20.656474
69.954170	2322.824072	20.661491
69.948238	2311.777693	20.666509
69.824791	2306.496453	20.671527
69.479527	2314.944345	20.676544
69.663022	2310.637412	20.681562
69.729717	2320.762981	20.686579
69.886757	2321.378671	20.691597
69.980512	2320.710520	20.696615
69.742807	2322.814581	20.701632
70.199297	2321.692054	20.706650
70.585203	2350.004354	20.711667
70.409686	2351.217303	20.716685
70.449399	2354.118821	20.721703
70.434047	2357.025056	20.726720
70.626844	2356.525780	20.731738
70.693903	2359.868351	20.736755
70.708120	2353.133346	20.741773
70.974122	2356.789895	20.746791
70.472975	2357.053001	20.751808
70.813384	2360.805472	20.756826
70.925867	2357.652614	20.761843
70.700476	2358.517365	20.766861
70.908988	2372.724817	20.771879
70.647280	2389.618827	20.776896
71.130613	2383.789366	20.781914
70.927653	2391.741173	20.786931
71.167246	2389.702131	20.791949
70.926664	2397.761194	20.796967
71.163205	2413.292437	20.801984
71.523450	2404.252053	20.807002
71.195811	2409.483857	20.812019
71.479052	2413.553279	20.817037
71.726787	2421.234098	20.822055
71.921099	2423.237329	20.827072
72.528662	2422.570863	20.832090
72.568937	2421.425184	20.837107
72.622248	2407.561039	20.842125
72.439746	2394.581565	20.847143
72.321452	2400.031059	20.852160
72.624330	2391.449408	20.857178
72.218964	2398.734232	20.862195
72.357335	2387.045638	20.867213
72.500883	2396.121694	20.872231
72.398651	2414.313012	20.877248
72.744613	2418.766235	20.882266
72.767573	2426.434404	20.887283
72.976573	2418.011377	20.892301
72.823687	2419.293691	20.897319
72.859276	2427.166816	20.902336
73.018472	2421.483479	20.907354
73.119217	2426.528440	20.912371
72.770832	2421.476308	20.917389
72.922676	2417.822909	20.922407
72.980821	2427.638939	20.927424
73.333187	2434.698579	20.932442
73.088500	2449.131855	20.937459
73.439184	2450.908247	20.942477
73.709722	2448.337822	20.947495
73.296139	2451.927410	20.952512
73.457776	2446.061726	20.957530
73.306134	2448.016381	20.962547
73.671852	2452.267768	20.967565
73.959584	2452.095577	20.972583
73.604576	2474.175028	20.977600
74.362875	2470.964190	20.982618
73.768243	2481.001636	20.987635
73.904599	2477.002001	20.992653
74.494980	2472.493747	20.997671
74.484120	2477.064077	21.002688
74.492982	2469.333712	21.007706
74.447383	2482.587814	21.012723
74.654243	2470.057357	21.017741
74.443764	2470.216291	21.022759
74.185274	2480.787543	21.027776
74.242747	2495.299787	21.032794
74.616990	2501.501234	21.037811
74.777349	2503.168507	21.042829
74.884403	2507.446930	21.047847
74.676184	2516.328203	21.052864
74.613481	2511.224700	21.057882
74.911405	2528.856125	21.062899
74.899613	2530.204038	21.067917
75.452637	2529.079910	21.072935
75.410749	2537.669642	21.077952
75.797684	2535.033571	21.082970
75.350085	2531.976701	21.087987
75.463110	2524.172536	21.093005
75.822571	2528.321062	21.098023
75.532462	2536.931298	21.103040
75.830753	2529.236337	21.108058
76.033363	2551.437656	21.113075
76.234535	2555.040001	21.118093
76.264050	2546.863462	21.123111
76.282464	2559.023792	21.128128
76.272298	2550.235838	21.133146
76.242567	2550.314170	21.138163
76.328115	2548.661422	21.143181
76.322487	2549.459367	21.148199
76.217699	2557.295983	21.153216
76.636338	2555.212836	21.158234
76.264486	2558.534619	21.163251
76.097268	2551.480181	21.168269
77.069553	2564.657497	21.173287
77.130251	2580.037920	21.178304
77.174596	2574.005651	21.183322
77.276252	2580.231811	21.188339
76.916882	2578.864036	21.193357
77.196285	2577.093784	21.198375
77.143681	2576.827158	21.203392
77.159668	2575.561989	21.208410
77.509130	2575.207530	21.213427
77.353850	2578.993061	21.218445
77.372450	2566.897235	21.223463
77.404990	2588.980495	21.228480
77.256170	2569.391598	21.233498
77.589878	2582.358669	21.238515
77.304485	2597.244017	21.243533
77.767562	2604.712387	21.248551
78.020919	2607.726169	21.253568
77.816120	2607.904607	21.258586
77.562375	2613.356133	21.263603
77.613496	2611.283222	21.268621
77.891670	2618.249348	21.273639
78.156871	2638.000262	21.278656
78.489645	2634.485115	21.283674
78.617381	2632.044673	21.288691
78.479879	2638.459916	21.293709
78.543781	2639.876765	21.298727
78.516018	2642.407161	21.303744
78.533600	2632.013334	21.308762
78.326333	2654.468566	21.313779
78.501243	2665.262541	21.318797
78.669300	2663.422376	21.323815
78.708440	2669.433266	21.328832
78.873265	2673.609688	21.333850
79.198820	2681.993170	21.338867
79.229806	2697.801712	21.343885
79.406862	2690.799232	21.348903
79.463756	2691.326575	21.353920
79.744933	2694.388370	21.358938
79.624826	2698.899527	21.363955
79.667355	2697.537655	21.368973
80.035654	2689.269095	21.373991
79.619699	2694.190878	21.379008
79.980843	2687.811287	21.384026
79.812340	2688.452090	21.389043
79.997088	2699.205812	21.394061
79.972614	2705.704085	21.399079
80.320618	2717.476476	21.404096
80.332598	2718.128865	21.409114
80.364644	2722.580078	21.414131
80.098119	2727.251803	21.419149
80.286407	2720.495460	21.424167
80.378372	2715.994622	21.429184
80.217867	2724.016496	21.434202
80.701455	2736.222432	21.439219
80.684207	2742.320197	21.444237
81.246026	2739.407608	21.449255
80.915749	2744.932153	21.454272
81.217855	2734.346934	21.459290
81.531758	2733.859173	21.464307
81.309333	2729.568953	21.469325
81.681021	2732.793224	21.474343
81.586167	2735.801363	21.479360
81.814795	2734.576117	21.484378
81.743500	2729.540958	21.489395
81.872460	2728.605290	21.494413
81.854219	2721.982798	21.499431
81.883925	2729.661772	21.504448
81.860406	2737.427842	21.509466
81.872474	2736.189320	21.514483
81.637218	2735.834299	21.519501
81.824648	2726.065741	21.524519
81.940259	2728.733804	21.529536
81.715478	2736.962803	21.534554
81.978831	2747.535335	21.539571
82.053932	2764.911473	21.544589
82.204279	2759.383104	21.549607
82.198666	2767.991156	21.554624
82.397398	2779.457628	21.559642
82.608352	2784.713775	21.564659
82.648181	2786.804967	21.569677
83.106709	2787.602890	21.574695
83.113875	2795.548801	21.579712
82.740780	2792.579912	21.584730
83.253978	2791.260984	21.589747
83.012153	2790.148679	21.594765
83.174641	2781.729494	21.599783
83.280401	2792.611805	21.604800
83.599958	2809.297142	21.609818
84.127584	2818.406827	21.614835
83.846331	2811.021363	21.619853
83.708269	2788.709366	21.624871
83.995533	2787.033824	21.629888
83.916654	2778.943477	21.634906
84.166839	2791.891177	21.639923
83.965533	2797.633044	21.644941
84.163967	2810.034410	21.649959
84.332344	2802.764026	21.654976
84.604933	2805.903708	21.659994
84.764666	2799.423144	21.665011
84.415746	2798.181140	21.670029
84.759517	2791.767471	21.675047
85.062591	2792.032099	21.680064
84.524899	2790.862623	21.685082
84.752564	2796.856204	21.690099
84.956431	2795.113054	21.695117
85.225160	2800.106498	21.700135
85.127100	2799.977606	21.705152
85.249231	2798.685559	21.710170
85.339466	2801.765148	21.715187
84.960201	2799.346235	21.720205
84.826219	2796.264683	21.725223
84.928560	2796.026618	21.730240
84.911155	2800.603676	21.735258
85.369523	2808.046176	21.740275
85.277980	2827.452902	21.745293
85.600780	2820.049717	21.750311
85.739324	2837.844273	21.755328
85.723114	2823.826294	21.760346
85.920489	2820.893480	21.765363
85.695269	2832.336593	21.770381
85.701036	2839.206186	21.775399
85.447535	2855.780331	21.780416
85.684882	2861.650994	21.785434
85.888447	2863.243957	21.790451
86.228429	2882.234972	21.795469
86.438840	2882.247721	21.800487
86.253346	2886.565377	21.805504
86.095146	2893.803327	21.810522
86.499084	2892.613381	21.815539
86.623007	2912.581812	21.820557
87.241824	2901.659452	21.825575
87.215526	2915.234294	21.830592
87.146642	2914.213614	21.835610
87.353289	2911.299669	21.840627
86.943714	2914.998930	21.845645
87.314878	2912.962468	21.850663
87.214315	2912.629240	21.855680
87.116768	2918.115521	21.860698
87.623971	2928.616443	21.865715
87.646700	2936.639301	21.870733
87.770228	2938.346800	21.875751
88.041688	2928.020298	21.880768
88.082998	2939.536716	21.885786
88.070851	2931.990863	21.890803
87.964565	2939.368781	21.895821
88.148072	2935.234151	21.900839
88.433799	2933.820326	21.905856
88.230658	2936.102042	21.910874
88.180446	2935.401056	21.915891
88.214776	2956.694608	21.920909
88.340625	2961.120357	21.925927
88.502298	2959.537997	21.930944
88.261778	2972.580999	21.935962
88.573744	2975.687188	21.940979
88.644506	2999.323048	21.945997
88.766019	2998.010613	21.951015
88.620590	3000.761279	21.956032
88.892561	3002.769385	21.961050
88.817013	3011.046185	21.966067
89.067310	3024.954880	21.971085
89.201162	3034.837855	21.976103
89.707759	3033.160125	21.981120
89.481665	3024.501857	21.986138
89.625860	3038.214538	21.991155
89.776390	3048.882222	21.996173
90.092859	3044.212067	22.001191
90.546002	3048.564402	22.006208
90.363012	3050.678866	22.011226
90.496568	3044.228679	22.016243
90.601683	3047.145103	22.021261
90.454207	3047.879185	22.026279
90.669165	3039.092528	22.031296
90.896758	3045.046838	22.036314
90.962644	3042.186929	22.041331
90.682993	3035.552417	22.046349
91.469325	3034.738724	22.051367
90.966768	3024.578722	22.056384
90.698068	3025.008324	22.061402
91.081196	3031.868434	22.066419
90.948956	3037.968701	22.071437
90.893304	3031.443849	22.076455
91.500436	3038.249021	22.081472
91.174781	3046.489962	22.086490
91.244329	3043.196267	22.091507
91.354364	3038.498499	22.096525
91.868091	3060.872443	22.101543
92.058485	3059.256010	22.106560
91.462995	3063.466803	22.111578
92.011674	3069.328272	22.116595
91.701903	3071.244745	22.121613
91.872209	3079.603866	22.126631
92.157724	3074.686201	22.131648
91.780497	3084.979727	22.136666
91.788251	3085.802969	22.141683
92.146138	3099.582239	22.146701
92.137020	3102.311916	22.151719
92.481782	3099.055296	22.156736
92.017932	3116.398210	22.161754
92.259373	3121.355482	22.166771
93.010439	3130.188411	22.171789
92.793027	3130.747834	22.176807
93.073469	3129.201012	22.181824
92.963693	3129.235577	22.186842
92.850497	3141.164537	22.191859
93.029618	3151.195762	22.196877
93.336410	3152.244964	22.201895
93.310658	3153.323612	22.206912
93.097938	3160.518264	22.211930
93.444165	3178.063383	22.216947
93.842427	3181.824251	22.221965
93.724258	3183.864614	22.226983
94.210987	3178.902183	22.232000
94.199769	3177.780241	22.237018
94.335663	3176.903214	22.242035
94.546178	3174.535918	22.247053
94.234782	3168.836120	22.252071
94.776450	3159.438938	22.257088
94.776924	3168.735287	22.262106
94.776028	3161.723728	22.267123
94.815886	3168.729382	22.272141
94.436888	3174.665663	22.277159
94.769749	3183.534092	22.282176
94.996118	3190.714123	22.287194
95.136708	3196.948817	22.292211
95.257010	3198.437167	22.297229
95.081033	3193.915974	22.302247
95.574700	3190.755880	22.307264
95.211894	3195.333200	22.312282
95.682072	3189.560045	22.317299
95.644715	3191.917333	22.322317
95.514992	3194.518852	22.327335
95.769924	3202.539052	22.332352
95.964759	3221.534099	22.337370
95.862913	3228.091531	22.342387
95.670725	3227.990586	22.347405
95.858543	3229.644568	22.352423
96.408360	3214.781797	22.357440
96.146806	3221.794257	22.362458
96.278621	3229.497711	22.367475
96.602707	3239.838070	22.372493
96.565774	3248.584854	22.377511
96.735937	3244.221673	22.382528
96.259914	3256.974505	22.387546
96.750001	3251.412133	22.392563
96.799547	3259.565233	22.397581
97.018532	3273.779582	22.402599
97.351157	3270.705362	22.407616
96.995385	3285.399443	22.412634
97.415238	3283.314421	22.417651
97.458085	3281.476750	22.422669
97.474510	3276.834339	22.427687
97.470823	3279.486721	22.432704
97.796730	3289.310153	22.437722
97.937298	3293.504288	22.442739
98.192987	3301.342480	22.447757
98.368407	3313.153572	22.452775
98.319238	3297.119906	22.457792
98.283809	3302.310570	22.462810
98.150328	3297.494596	22.467827
98.220317	3300.410001	22.472845
98.285592	3313.824574	22.477863
98.627689	3302.796590	22.482880
98.468407	3313.734151	22.487898
98.724979	3319.277998	22.492915
98.955491	3328.019929	22.497933
98.775712	3331.330206	22.502951
99.001823	3322.924241	22.507968
99.137034	3327.083863	22.512986
99.191002	3326.140541	22.518003
99.687048	3341.933007	22.523021
99.173718	3356.530516	22.528039
99.895243	3359.179080	22.533056
99.657816	3368.789622	22.538074
99.684525	3361.993763	22.543091
99.828877	3368.288524	22.548109
99.617052	3368.841483	22.553127
99.689941	3364.485494	22.558144
100.058363	3383.429712	22.563162
100.265623	3385.364693	22.568179
100.496334	3395.567584	22.573197
100.018856	3398.360280	22.578215
100.439913	3399.736445	22.583232
100.471692	3398.685087	22.588250
100.467665	3393.861066	22.593267
100.872694	3404.976810	22.598285
100.426918	3424.154384	22.603303
100.710726	3418.007494	22.608320
100.815528	3426.522157	22.613338
100.670328	3424.433180	22.618355
100.803319	3438.992417	22.623373
100.569949	3451.086341	22.628391
101.033021	3447.150950	22.633408
101.260805	3462.909983	22.638426
101.559220	3466.923526	22.643443
101.940893	3472.509774	22.648461
101.812999	3474.889714	22.653479
102.112400	3474.533584	22.658496
102.218473	3472.172336	22.663514
102.645229	3466.200179	22.668531
102.853357	3460.271019	22.673549
102.428414	3468.017272	22.678567
102.478390	3459.377591	22.683584
102.743504	3462.697469	22.688602
102.452415	3463.931102	22.693619
102.719500	3471.138147	22.698637
102.715164	3485.803667	22.703655
103.079711	3487.770764	22.708672
103.084052	3496.002619	22.713690
102.876077	3498.227748	22.718707
103.318524	3498.377139	22.723725
103.155226	3508.521639	22.728743
103.346152	3508.675558	22.733760
103.373691	3525.399120	22.738778
103.677458	3531.058601	22.743795
103.901140	3531.937783	22.748813
103.976937	3530.533120	22.753831
103.915499	3527.651635	22.758848
104.040006	3532.688941	22.763866
103.864688	3536.426154	22.768883
103.839980	3546.152338	22.773901
104.100687	3564.144935	22.778919
103.804750	3565.367592	22.783936
104.222963	3576.502462	22.788954
104.465244	3575.577247	22.793971
104.990263	3571.313809	22.798989
104.714357	3581.989593	22.804007
105.085062	3575.750561	22.809024
105.214815	3576.677353	22.814042
105.188087	3574.916946	22.819059
105.174819	3590.806430	22.824077
105.521344	3598.507122	22.829095
105.754109	3593.458937	22.834112
105.905142	3594.115877	22.839130
105.766074	3599.514214	22.844147
105.952860	3601.630727	22.849165
106.292192	3606.643041	22.854183
106.584654	3599.228156	22.859200
106.526786	3595.572634	22.864218
106.261495	3609.023653	22.869235
106.830568	3594.927488	22.874253
106.725127	3604.046142	22.879271
107.047850	3599.697664	22.884288
106.797571	3599.993380	22.889306
106.130449	3601.719937	22.894323
106.778331	3594.182689	22.899341
106.432273	3601.163336	22.904359
106.604941	3599.573515	22.909376
106.539579	3616.862837	22.914394
106.117459	3628.150473	22.919411
106.490638	3645.024405	22.924429
106.798526	3666.988726	22.929447
106.929806	3673.917500	22.934464
107.245710	3689.493108	22.939482
107.516559	3692.927041	22.944499
107.897538	3682.481248	22.949517
107.933681	3698.957790	22.954535
108.045899	3693.207230	22.959552
108.721443	3696.202403	22.964570
108.545358	3703.971477	22.969587
108.607264	3703.314243	22.974605
108.662692	3708.956506	22.979623
109.271745	3716.145207	22.984640
108.719721	3700.925076	22.989658
108.893422	3715.997402	22.994675
109.330848	3708.751361	22.999693
109.096126	3717.921385	23.004711
109.261022	3713.883467	23.009728
109.311820	3712.472047	23.014746
109.008012	3713.139235	23.019763
109.423084	3707.151665	23.024781
109.084944	3714.597259	23.029799
109.364189	3724.336815	23.034816
109.645367	3740.261819	23.039834
109.752382	3747.190846	23.044851
109.665785	3743.261407	23.049869
109.499057	3758.432303	23.054887
109.664669	3768.337859	23.059904
109.900405	3765.830686	23.064922
109.887478	3777.846900	23.069939
110.303247	3803.258345	23.074957
110.379375	3802.315922	23.079975
110.733308	3801.525134	23.084992
110.820180	3810.200599	23.090010
110.873832	3823.011146	23.095027
111.181397	3827.893511	23.100045
111.413959	3831.797936	23.105063
111.590107	3837.092695	23.110080
111.861430	3823.193080	23.115098
111.573824	3823.283335	23.120115
111.645340	3823.894059	23.125133
111.721981	3830.646395	23.130151
111.989754	3824.684821	23.135168
112.023990	3824.709662	23.140186
111.548415	3832.563221	23.145203
111.915682	3824.521866	23.150221
112.340861	3849.432435	23.155239
112.369635	3850.858566	23.160256
112.117112	3859.658401	23.165274
112.226857	3853.980665	23.170291
112.444538	3856.774767	23.175309
112.376697	3858.156029	23.180327
112.568548	3865.076866	23.185344
112.552590	3877.529219	23.190362
112.731764	3882.555690	23.195379
113.200139	3878.469642	23.200397
113.619412	3899.385009	23.205415
113.637378	3907.595839	23.210432
113.848316	3907.181621	23.215450
113.606277	3908.084747	23.220467
113.858231	3901.156316	23.225485
113.791880	3910.989890	23.230503
114.044409	3896.795718	23.235520
114.376949	3901.413916	23.240538
113.930354	3903.076705	23.245555
114.565026	3896.575704	23.250573
114.693742	3916.829701	23.255591
114.818850	3928.004044	23.260608
114.853470	3932.403177	23.265626
114.815500	3934.563779	23.270643
115.094761	3927.030501	23.275661
114.711832	3929.582610	23.280679
115.042279	3929.540130	23.285696
114.883438	3925.240255	23.290714
114.913671	3935.328222	23.295731
115.086355	3942.200396	23.300749
115.276850	3950.381672	23.305767
115.267730	3948.635531	23.310784
115.481706	3963.444430	23.315802
115.679300	3973.658888	23.320819
116.020540	3970.535015	23.325837
116.284719	3975.624129	23.330855
116.425086	3969.754440	23.335872
116.596458	3968.066354	23.340890
116.366769	3977.269532	23.345907
116.472992	3998.513574	23.350925
116.637024	4001.711490	23.355943
116.840524	4005.058588	23.360960
116.969950	4003.458026	23.365978
116.737920	4009.012633	23.370995
117.276441	3995.379741	23.376013
117.133685	4005.873098	23.381031
117.157008	4030.907192	23.386048
117.608327	4024.863670	23.391066
117.534718	4035.141202	23.396083
117.365377	4025.484200	23.401101
117.928490	4021.115663	23.406119
118.296398	4023.474483	23.411136
118.436485	4016.272977	23.416154
118.344074	4017.628536	23.421171
118.614155	4009.943996	23.426189
118.755296	4009.140060	23.431207
118.455542	4015.468686	23.436224
119.130223	4019.673052	23.441242
118.836186	4025.492693	23.446259
118.965839	4025.947751	23.451277
119.065834	4033.131719	23.456295
118.764156	4037.419198	23.461312
118.899415	4037.214065	23.466330
118.973496	4040.976375	23.471347
119.320630	4039.005327	23.476365
119.296272	4050.594461	23.481383
119.355295	4065.823038	23.486400
119.936961	4072.999272	23.491418
119.379751	4073.736694	23.496435
119.537226	4084.314891	23.501453
120.167574	4092.871349	23.506471
120.325738	4098.889159	23.511488
120.236667	4094.542620	23.516506
120.393017	4106.027567	23.521523
120.397269	4100.328448	23.526541
120.698290	4120.427937	23.531559
120.891283	4137.943689	23.536576
120.896142	4130.525092	23.541594
120.646922	4137.017589	23.546611
120.694609	4137.927767	23.551629
120.914649	4153.791210	23.556647
121.013139	4172.369156	23.561664
120.857870	4168.564012	23.566682
121.245337	4183.344163	23.571699
121.330213	4198.888997	23.576717
121.620065	4208.256854	23.581735
121.646987	4219.846771	23.586752
121.796885	4220.806379	23.591770
122.318679	4226.305079	23.596787
122.679437	4213.933525	23.601805
123.051833	4211.427271	23.606823
122.963530	4217.266058	23.611840
123.277365	4209.484132	23.616858
122.966862	4207.147721	23.621875
123.262221	4216.008988	23.626893
123.266323	4206.380425	23.631911
123.107034	4211.060190	23.636928
123.691961	4213.955222	23.641946
123.247361	4232.541280	23.646963
123.243608	4243.287420	23.651981
123.659877	4239.375614	23.656999
123.772086	4247.562589	23.662016
123.837889	4234.933623	23.667034
124.059784	4266.697343	23.672051
124.131690	4272.640218	23.677069
123.980086	4273.029295	23.682087
124.270696	4271.183690	23.687104
124.489469	4265.153953	23.692122
124.265761	4279.986200	23.697139
124.117870	4293.935140	23.702157
124.800695	4297.986964	23.707175
124.641130	4313.155587	23.712192
125.043119	4302.907418	23.717210
125.056155	4320.989021	23.722227
125.012139	4333.106289	23.727245
125.237665	4331.393917	23.732263
124.974889	4338.273181	23.737280
125.433487	4350.809954	23.742298
125.834501	4363.144736	23.747315
126.081149	4369.719297	23.752333
126.243810	4366.694486	23.757351
126.311926	4375.983099	23.762368
126.517350	4370.836965	23.767386
126.445765	4373.884745	23.772403
126.356809	4392.540767	23.777421
126.610000	4389.843049	23.782439
126.313184	4403.370243	23.787456
126.641759	4392.768355	23.792474
126.724511	4414.734509	23.797491
126.755668	4422.147053	23.802509
127.109806	4421.417638	23.807527
127.007511	4444.937257	23.812544
127.430028	4454.754308	23.817562
127.558723	4455.712840	23.822579
127.934743	4449.970341	23.827597
127.814763	4450.242157	23.832615
128.135489	4466.406856	23.837632
128.786319	4465.400526	23.842650
129.120056	4467.131230	23.847667
129.172880	4466.336112	23.852685
129.184076	4439.724076	23.857703
129.108914	4440.835699	23.862720
129.046778	4434.041221	23.867738
128.985726	4444.631130	23.872755
129.145363	4456.264630	23.877773
128.890299	4462.960683	23.882791
128.714388	4472.034419	23.887808
129.065046	4467.791187	23.892826
129.062498	4487.902228	23.897843
129.224727	4494.489738	23.902861
129.760969	4504.992257	23.907879
130.056399	4527.354518	23.912896
129.874162	4526.186973	23.917914
129.830088	4528.638553	23.922931
130.153909	4536.282164	23.927949
130.392775	4549.060761	23.932967
130.312516	4561.252153	23.937984
130.470277	4562.140334	23.943002
130.429768	4574.857365	23.948019
130.669690	4587.955593	23.953037
130.479236	4600.835398	23.958055
130.656375	4607.058086	23.963072
131.141531	4619.988277	23.968090
131.308278	4622.291097	23.973107
131.730929	4615.294499	23.978125
132.123213	4609.384538	23.983143
131.823519	4617.505269	23.988160
131.813148	4612.857608	23.993178
132.174331	4623.373676	23.998195
131.982531	4641.647501	24.003213
132.443710	4639.111784	24.008231
132.203107	4643.236151	24.013248
132.717239	4638.330011	24.018266
133.156749	4631.695981	24.023283
132.948959	4639.502452	24.028301
133.315777	4647.399455	24.033319
133.400354	4660.051002	24.038336
133.747695	4661.008296	24.043354
133.666866	4660.950471	24.048371
133.572908	4664.477089	24.053389
133.895437	4659.060317	24.058407
133.906734	4665.069652	24.063424
134.212831	4655.613523	24.068442
134.130861	4660.321909	24.073459
133.835830	4673.363840	24.078477
134.615347	4678.222274	24.083495
134.230210	4695.884226	24.088512
134.520042	4697.642962	24.093530
134.733172	4695.545157	24.098547
134.251592	4696.891875	24.103565
134.702857	4707.787954	24.108583
134.965117	4731.176976	24.113600
135.224735	4731.390811	24.118618
134.915268	4741.200415	24.123635
135.004877	4751.185781	24.128653
135.645568	4747.834778	24.133671
135.421406	4754.220837	24.138688
135.948285	4767.589805	24.143706
136.179179	4762.721944	24.148723
136.154999	4771.482349	24.153741
136.368499	4771.704878	24.158759
136.519786	4772.498089	24.163776
136.509548	4777.559681	24.168794
136.815297	4802.853761	24.173811
136.877878	4801.029072	24.178829
137.241876	4801.061183	24.183847
137.012814	4811.191009	24.188864
136.895291	4814.286130	24.193882
137.399144	4818.900437	24.198899
137.109793	4832.441681	24.203917
137.502439	4831.917526	24.208935
137.288454	4843.985557	24.213952
137.554770	4851.642330	24.218970
137.941179	4860.570267	24.223987
137.983245	4868.246588	24.229005
138.633118	4882.978474	24.234023
138.617868	4892.917318	24.239040
138.629683	4889.668582	24.244058
138.847629	4892.591999	24.249075
138.800522	4893.559429	24.254093
138.688675	4884.855345	24.259111
138.676861	4892.625193	24.264128
138.920296	4914.009986	24.269146
139.115631	4912.980111	24.274163
138.765004	4925.826201	24.279181
139.346842	4933.163484	24.284199
139.586751	4943.264195	24.289216
139.559571	4946.975554	24.294234
139.635083	4951.781479	24.299251
139.520798	4966.916184	24.304269
139.957308	4969.491811	24.309287
140.266823	4985.569958	24.314304
140.880534	4982.997801	24.319322
141.375217	4983.136686	24.324339
141.344995	4990.337110	24.329357
141.382409	4984.917121	24.334375
141.346757	4985.316267	24.339392
141.793433	4987.204104	24.344410
141.907538	4989.819251	24.349427
141.689499	4984.038986	24.354445
141.863146	4983.417680	24.359463
141.541595	4990.093058	24.364480
141.810372	4994.831208	24.369498
142.079929	5014.537886	24.374515
142.081662	5017.292025	24.379533
142.197756	5023.128362	24.384551
142.147381	5032.884277	24.389568
142.549937	5050.940108	24.394586
142.420532	5053.004689	24.399603
142.601421	5068.433884	24.404621
142.914696	5077.544617	24.409639
143.686836	5069.022071	24.414656
143.754867	5062.621681	24.419674
143.993691	5055.507537	24.424691
144.003897	5059.973394	24.429709
144.353098	5061.503025	24.434727
144.183891	5059.755849	24.439744
144.261449	5066.102911	24.444762
144.567945	5079.094040	24.449779
144.581952	5087.714170	24.454797
144.624778	5091.363152	24.459815
144.862389	5093.123796	24.464832
144.769836	5096.432086	24.469850
144.837617	5086.413207	24.474867
144.768051	5111.813079	24.479885
144.978334	5127.639002	24.484903
145.363140	5126.870432	24.489920
145.310364	5137.223872	24.494938
145.514993	5142.271589	24.499955
145.530842	5160.731746	24.504973
146.005275	5157.676182	24.509991
145.584234	5156.948873	24.515008
145.831449	5187.811373	24.520026
146.583614	5183.832307	24.525043
146.147023	5199.147724	24.530061
146.499715	5201.950429	24.535079
146.541952	5200.416681	24.540096
146.335462	5222.057821	24.545114
146.520881	5226.312524	24.550131
146.291283	5244.910951	24.555149
146.551789	5250.840766	24.560167
147.285636	5263.266491	24.565184
147.284079	5279.480182	24.570202
147.800764	5272.694029	24.575219
148.098632	5285.976669	24.580237
148.409002	5280.637389	24.585255
148.365069	5290.862598	24.590272
148.530777	5303.559038	24.595290
148.978620	5300.031464	24.600307
148.903352	5297.933397	24.605325
149.142032	5300.641452	24.610343
149.558290	5304.358008	24.615360
148.954231	5303.498229	24.620378
149.500443	5284.121574	24.625395
149.522707	5293.823450	24.630413
149.408074	5299.562386	24.635431
149.851399	5309.118049	24.640448
150.131991	5321.239500	24.645466
150.618364	5316.262298	24.650483
150.577478	5314.834947	24.655501
151.000754	5306.324821	24.660519
150.953111	5315.135233	24.665536
150.816050	5317.597360	24.670554
150.869074	5311.393999	24.675571
150.646675	5319.716082	24.680589
150.398612	5330.306345	24.685607
150.753394	5346.425936	24.690624
150.674669	5358.358531	24.695642
150.911665	5367.619563	24.700659
151.156509	5385.617744	24.705677
151.344612	5392.209858	24.710695
152.313777	5406.618901	24.715712
151.916496	5417.678265	24.720730
152.319400	5407.900264	24.725747
152.277133	5422.475620	24.730765
152.104081	5435.496474	24.735783
152.582578	5438.302862	24.740800
152.603863	5437.977046	24.745818
152.856292	5449.922257	24.750835
153.185503	5462.100858	24.755853
153.835231	5458.273192	24.760871
154.011993	5459.348000	24.765888
153.942216	5453.722525	24.770906
154.139214	5451.319405	24.775923
154.176580	5458.288692	24.780941
154.302590	5447.195447	24.785959
154.463882	5460.036916	24.790976
154.789325	5452.024757	24.795994
154.971235	5449.138225	24.801011
154.670525	5457.298940	24.806029
154.829212	5452.021839	24.811047
154.519110	5456.025210	24.816064
154.739920	5475.747908	24.821082
154.876667	5475.730761	24.826099
155.065780	5481.598072	24.831117
155.317144	5505.558025	24.836135
155.644211	5508.358090	24.841152
155.236213	5512.138014	24.846170
155.560729	5522.642064	24.851187
155.394316	5543.348091	24.856205
155.797814	5550.430307	24.861223
155.947497	5568.551346	24.866240
156.098504	5577.630321	24.871258
156.456132	5578.742661	24.876275
156.397878	5602.348602	24.881293
156.354280	5614.941752	24.886311
156.866492	5621.211374	24.891328
157.081974	5648.373347	24.896346
157.337049	5641.609830	24.901363
157.262213	5655.160684	24.906381
157.376336	5660.962147	24.911399
157.436486	5666.351451	24.916416
157.530742	5697.456991	24.921434
158.436599	5697.667186	24.926451
158.635640	5709.606779	24.931469
158.238219	5716.857089	24.936487
158.308184	5726.724344	24.941504
158.749299	5733.268501	24.946522
158.871897	5738.863740	24.951539
158.888862	5759.155003	24.956557
158.865383	5766.209687	24.961575
159.354819	5770.540815	24.966592
159.631035	5791.875486	24.971610
160.510370	5780.318887	24.976627
161.317537	5766.817243	24.981645
161.206548	5754.550573	24.986663
162.169804	5747.935791	24.991680
161.644220	5737.003669	24.996698
162.192442	5721.037645	25.001715
161.865911	5715.213482	25.006733
161.781154	5693.902793	25.011751
162.114811	5673.464847	25.016768
161.620662	5686.063610	25.021786
161.910892	5677.535135	25.026803
162.076777	5676.073093	25.031821
161.793687	5679.106179	25.036839
161.890265	5689.908566	25.041856
162.024489	5707.633842	25.046874
162.101403	5709.372480	25.051891
162.233676	5708.627484	25.056909
162.202782	5720.838872	25.061927
162.938047	5734.739292	25.066944
162.765649	5741.795863	25.071962
162.540506	5743.698926	25.076979
162.814591	5753.719466	25.081997
162.726874	5774.631282	25.087015
162.768566	5773.129080	25.092032
163.016895	5796.268425	25.097050
163.625562	5800.662619	25.102067
163.471479	5820.584708	25.107085
163.620383	5835.100888	25.112103
164.170277	5837.719453	25.117120
164.121243	5849.750515	25.122138
164.297880	5875.817544	25.127155
164.473438	5886.248121	25.132173
164.456092	5888.166779	25.137191
164.666308	5899.335802	25.142208
164.787176	5914.915533	25.147226
165.094707	5913.762387	25.152243
165.218864	5929.156458	25.157261
165.232692	5939.810146	25.162279
165.343025	5946.244890	25.167296
165.553415	5969.945535	25.172314
165.743476	5973.915283	25.177331
166.481195	5999.472785	25.182349
166.669358	6009.838265	25.187367
166.608863	6010.930153	25.192384
166.735913	6007.230558	25.197402
166.640523	6018.496952	25.202419
166.993905	6037.748628	25.207437
166.947770	6034.353626	25.212455
167.466722	6054.286665	25.217472
167.583411	6061.808195	25.222490
167.774108	6069.936182	25.227507
167.885338	6082.691423	25.232525
167.845527	6097.218924	25.237543
168.330011	6101.736894	25.242560
168.231583	6124.480860	25.247578
168.568119	6125.606310	25.252595
169.027835	6122.558604	25.257613
168.633999	6128.339398	25.262631
169.227772	6147.976152	25.267648
169.171640	6161.165031	25.272666
169.713350	6159.580229	25.277683
170.043929	6158.701967	25.282701
170.076307	6178.512191	25.287719
170.816505	6167.718833	25.292736
170.610755	6177.322485	25.297754
170.695664	6168.712365	25.302771
170.740861	6166.861355	25.307789
170.493591	6172.689510	25.312807
170.888964	6164.951738	25.317824
170.707636	6191.124758	25.322842
171.054267	6197.751474	25.327859
171.197870	6201.598482	25.332877
171.198668	6218.403513	25.337895
171.435263	6218.082521	25.342912
171.836146	6232.864655	25.347930
172.200144	6221.817512	25.352947
172.491912	6228.097598	25.357965
172.679944	6240.750787	25.362983
172.882375	6245.181662	25.368000
173.012669	6254.003051	25.373018
173.098160	6262.264967	25.378035
173.481052	6256.016507	25.383053
173.286285	6256.810038	25.388071
173.552663	6242.553114	25.393088
173.704804	6250.259284	25.398106
173.699140	6243.912015	25.403123
174.094496	6266.117023	25.408141
173.778028	6284.028905	25.413159
174.115677	6283.804808	25.418176
174.227397	6293.745606	25.423194
173.577626	6306.040686	25.428211
174.341949	6312.770724	25.433229
174.155817	6334.862822	25.438247
174.221116	6344.134166	25.443264
174.665033	6370.004942	25.448282
174.703438	6382.123820	25.453299
175.217331	6394.726786	25.458317
175.152640	6413.206140	25.463335
175.782833	6428.710093	25.468352
175.808525	6437.863031	25.473370
175.882347	6453.411179	25.478387
176.113206	6462.911798	25.483405
175.939497	6480.890804	25.488423
176.505685	6497.104513	25.493440
176.952687	6508.714678	25.498458
176.930951	6502.090416	25.503475
177.625026	6510.051991	25.508493
177.418784	6528.864535	25.513511
177.572456	6530.578289	25.518528
178.030597	6533.472655	25.523546
178.069735	6548.799186	25.528563
178.438531	6561.847021	25.533581
178.540548	6556.427239	25.538599
178.793056	6557.120480	25.543616
179.118177	6562.140118	25.548634
178.822110	6559.202984	25.553651
179.139723	6576.877309	25.558669
178.905426	6590.539003	25.563687
179.322110	6598.519815	25.568704
179.421285	6609.561065	25.573722
179.382827	6620.436070	25.578739
179.936789	6625.765469	25.583757
180.026537	6644.053978	25.588775
180.069483	6638.739611	25.593792
180.046690	6654.826000	25.598810
180.906262	6668.894205	25.603827
181.811738	6660.916719	25.608845
181.768892	6656.049522	25.613863
181.686544	6661.937810	25.618880
181.363239	6660.282253	25.623898
181.784834	6664.189640	25.628915
181.957207	6663.162018	25.633933
181.951863	6660.807585	25.638951
182.178064	6662.824017	25.643968
182.237041	6687.756140	25.648986
182.248081	6682.486614	25.654003
182.780322	6684.757019	25.659021
182.209607	6697.327159	25.664039
182.511953	6718.312774	25.669056
182.744042	6714.928227	25.674074
182.182685	6749.461450	25.679092
182.788520	6756.333070	25.684109
182.909179	6783.605400	25.689127
183.591769	6789.174336	25.694144
184.364349	6802.335121	25.699162
183.983577	6820.892761	25.704180
184.881663	6816.299845	25.709197
184.544719	6817.867710	25.714215
185.034325	6833.411126	25.719232
185.542860	6840.586203	25.724250
185.632330	6850.505953	25.729268
185.735481	6847.691754	25.734285
185.709838	6851.623074	25.739303
185.659002	6844.627115	25.744320
185.712155	6851.677019	25.749338
185.617536	6876.954017	25.754356
185.653718	6882.369898	25.759373
185.546157	6904.386293	25.764391
185.760504	6920.213303	25.769408
186.445177	6934.956896	25.774426
186.358052	6955.915844	25.779444
186.953773	6970.298959	25.784461
186.830884	6988.988255	25.789479
187.255515	6991.994798	25.794496
187.657053	7000.566076	25.799514
187.907545	7011.051504	25.804532
188.059075	7013.625910	25.809549
188.150350	7026.729576	25.814567
188.437469	7029.380787	25.819584
188.568395	7049.899148	25.824602
188.543704	7061.183303	25.829620
189.114189	7060.556918	25.834637
189.225567	7082.065733	25.839655
189.869629	7084.474582	25.844672
190.011336	7090.739769	25.849690
190.053966	7097.103082	25.854708
190.155781	7089.760229	25.859725
190.300287	7101.061099	25.864743
190.441745	7111.063480	25.869760
190.580643	7114.548357	25.874778
190.556129	7123.644910	25.879796
190.949741	7139.439045	25.884813
190.839493	7152.725459	25.889831
190.750633	7157.437337	25.894848
191.108055	7161.852928	25.899866
191.192636	7187.980419	25.904884
191.152751	7187.739891	25.909901
191.481987	7209.271403	25.914919
191.616166	7216.388718	25.919936
192.139457	7242.500965	25.924954
192.354855	7253.069770	25.929972
192.362442	7257.831317	25.934989
192.328023	7279.697041	25.940007
192.653689	7289.528521	25.945024
193.106982	7296.632134	25.950042
192.816855	7308.967949	25.955060
193.886956	7316.831600	25.960077
194.122251	7334.364109	25.965095
194.227901	7342.167007	25.970112
194.625236	7337.618822	25.975130
194.893090	7345.164675	25.980148
195.130352	7337.005991	25.985165
194.759610	7343.370149	25.990183
195.050893	7361.480769	25.995200
195.739697	7358.350240	26.000218
195.687819	7365.243488	26.005236
195.885620	7358.337817	26.010253
195.703403	7371.746250	26.015271
196.119118	7387.816502	26.020288
196.517851	7393.632045	26.025306
196.781908	7391.420391	26.030324
196.327468	7390.884606	26.035341
196.487573	7407.668304	26.040359
196.883454	7410.129201	26.045376
197.366270	7428.817592	26.050394
197.301842	7452.006648	26.055412
197.588604	7447.064591	26.060429
198.010708	7447.544462	26.065447
197.857366	7470.939429	26.070464
198.504052	7467.662482	26.075482
198.701031	7460.568629	26.080500
199.094578	7463.534113	26.085517
199.339889	7463.501509	26.090535
199.260194	7474.954516	26.095552
199.576605	7489.232363	26.100570
199.428971	7498.858352	26.105588
199.693662	7490.896560	26.110605
199.996836	7497.081448	26.115623
199.714413	7510.682848	26.120640
199.978574	7526.077305	26.125658
199.616497	7539.289827	26.130676
199.934164	7550.706284	26.135693
200.579803	7564.382616	26.140711
200.222478	7587.826900	26.145728
200.893991	7590.773120	26.150746
200.571908	7617.599673	26.155764
201.051195	7632.534315	26.160781
201.407428	7641.342163	26.165799
201.955586	7651.097914	26.170816
201.911915	7646.193531	26.175834
202.180190	7660.317497	26.180852
202.536150	7674.341364	26.185869
202.705170	7677.626618	26.190887
202.617494	7681.015746	26.195904
202.773615	7687.530789	26.200922
202.678393	7710.509642	26.205940
203.189920	7715.951463	26.210957
203.432126	7735.508640	26.215975
203.776470	7744.424147	26.220992
204.165541	7751.631146	26.226010
204.291144	7772.238789	26.231028
204.738708	7767.276161	26.236045
204.681834	7778.696324	26.241063
204.936067	7790.271144	26.246080
205.250766	7797.082045	26.251098
205.087755	7810.326052	26.256116
204.934627	7813.554688	26.261133
205.494417	7831.455165	26.266151
205.395103	7841.918382	26.271168
205.701314	7864.151924	26.276186
205.924642	7887.844530	26.281204
206.346290	7893.205707	26.286221
206.716669	7903.630994	26.291239
206.602595	7911.023575	26.296256
206.702145	7924.402287	26.301274
206.891766	7946.066652	26.306292
207.263400	7961.788951	26.311309
207.957748	7965.848436	26.316327
207.672801	7985.974477	26.321344
208.344583	7988.876612	26.326362
208.401837	8004.601635	26.331380
208.687165	7994.823317	26.336397
208.834579	8002.862810	26.341415
209.136858	8022.265083	26.346432
209.278532	8018.208795	26.351450
209.241846	8030.389061	26.356468
209.721650	8047.458961	26.361485
210.125897	8056.165847	26.366503
210.011610	8065.317711	26.371520
210.036276	8066.436892	26.376538
210.134830	8087.246529	26.381556
209.997817	8090.204602	26.386573
210.348143	8110.871059	26.391591
210.248858	8131.044237	26.396608
210.873763	8141.645849	26.401626
210.803245	8166.058088	26.406644
210.960272	8186.248061	26.411661
211.350616	8208.987618	26.416679
211.666908	8235.638019	26.421696
212.319803	8238.549741	26.426714
212.211617	8251.573577	26.431732
212.337567	8260.946716	26.436749
213.327951	8272.854997	26.441767
213.187393	8278.620711	26.446784
213.849594	8271.440455	26.451802
213.743971	8278.339368	26.456820
213.880625	8279.656018	26.461837
214.320117	8299.119402	26.466855
214.045399	8314.288709	26.471872
214.609311	8312.714088	26.476890
214.481479	8320.310108	26.481908
214.394978	8336.626542	26.486925
214.946273	8346.811545	26.491943
214.918339	8360.286528	26.496960
215.113303	8368.430713	26.501978
214.999575	8381.691163	26.506996
215.004025	8407.843039	26.512013
215.781972	8414.692184	26.517031
216.096412	8442.402873	26.522048
216.766501	8443.442960	26.527066
216.808295	8447.885440	26.532084
216.660399	8461.726140	26.537101
217.134489	8472.928152	26.542119
217.075133	8486.663883	26.547136
217.724881	8492.616428	26.552154
217.527776	8507.113197	26.557172
217.821006	8531.933186	26.562189
218.216174	8547.708750	26.567207
218.432128	8554.287159	26.572224
218.345013	8567.852031	26.577242
218.468298	8588.149135	26.582260
218.675880	8593.818258	26.587277
218.905733	8598.695730	26.592295
218.879025	8621.349791	26.597312
219.010334	8639.887922	26.602330
219.354633	8653.559331	26.607348
219.567350	8669.525432	26.612365
220.061061	8679.005161	26.617383
219.820268	8697.945913	26.622400
220.522017	8714.545167	26.627418
220.899077	8736.332096	26.632436
221.166810	8750.524082	26.637453
221.654082	8751.691645	26.642471
221.981796	8753.228483	26.647488
222.616250	8754.069862	26.652506
222.875399	8763.515791	26.657524
223.233561	8770.912117	26.662541
223.441599	8769.820740	26.667559
222.944483	8772.568857	26.672576
223.508591	8773.300967	26.677594
223.355577	8782.570174	26.682612
223.304940	8788.211934	26.687629
223.657569	8802.233420	26.692647
223.771036	8817.576951	26.697664
224.008495	8832.695979	26.702682
224.188188	8837.600243	26.707700
224.208153	8858.963235	26.712717
224.712986	8866.488882	26.717735
224.623464	8883.535933	26.722752
224.727988	8896.753880	26.727770
224.834478	8911.313998	26.732788
225.224740	8929.908132	26.737805
225.821054	8930.806482	26.742823
225.645050	8943.232703	26.747840
226.381869	8952.163547	26.752858
226.612145	8958.174777	26.757876
226.876048	8970.826574	26.762893
227.240565	8984.283654	26.767911
227.139992	8999.356784	26.772928
227.110567	9003.250673	26.777946
227.499325	9013.093671	26.782964
227.743668	9020.990215	26.787981
228.369271	9025.835436	26.792999
228.582662	9048.156645	26.798016
228.721879	9056.485639	26.803034
229.148401	9054.228581	26.808052
229.014368	9047.368829	26.813069
229.432352	9075.806597	26.818087
229.282789	9078.399070	26.823104
229.604660	9082.253246	26.828122
229.755899	9101.323448	26.833140
229.718238	9120.575746	26.838157
230.005834	9140.208789	26.843175
230.623135	9148.206917	26.848192
230.570496	9159.116796	26.853210
230.958435	9174.533374	26.858228
231.267608	9179.234340	26.863245
231.732866	9195.083616	26.868263
231.984634	9198.138337	26.873280
232.255746	9188.681609	26.878298
232.382444	9205.906237	26.883316
232.480775	9222.755994	26.888333
233.055936	9217.028889	26.893351
232.770033	9238.862380	26.898368
233.198472	9242.513968	26.903386
233.597249	9247.437531	26.908404
233.741719	9249.733817	26.913421
234.370490	9264.530907	26.918439
234.528430	9284.972643	26.923456
234.330342	9272.774147	26.928474
235.129420	9274.138848	26.933492
234.853925	9296.035238	26.938509
234.956564	9294.522262	26.943527
235.364251	9311.549144	26.948544
235.416945	9324.758993	26.953562
235.713600	9327.802893	26.958580
236.080548	9344.326252	26.963597
236.140909	9352.479826	26.968615
235.964287	9373.024717	26.973632
236.071336	9383.069078	26.978650
236.183041	9406.216571	26.983668
236.514717	9434.269526	26.988685
237.342637	9437.223959	26.993703
237.522633	9467.926599	26.998720
237.718351	9477.687941	27.003738
238.221516	9479.965323	27.008756
238.108777	9492.024999	27.013773
238.335176	9502.494916	27.018791
238.428670	9513.562773	27.023808
238.824061	9522.675371	27.028826
239.157980	9541.577689	27.033844
239.240429	9551.303340	27.038861
239.533555	9552.824125	27.043879
239.753472	9572.798631	27.048896
239.808859	9575.371810	27.053914
240.947793	9582.426681	27.058932
240.492625	9593.052877	27.063949
240.988160	9589.143545	27.068967
240.744974	9601.268208	27.073984
241.081955	9620.978463	27.079002
241.402159	9638.271233	27.084020
241.023286	9655.362390	27.089037
241.651514	9669.904672	27.094055
241.558454	9686.699476	27.099072
241.613580	9715.266750	27.104090
241.834742	9734.960754	27.109108
242.242747	9759.369014	27.114125
242.739017	9784.912506	27.119143
242.589410	9806.912493	27.124160
242.778382	9823.706369	27.129178
243.510296	9843.543023	27.134196
243.501905	9867.718693	27.139213
244.062431	9887.102585	27.144231
244.349706	9915.899882	27.149248
244.622063	9932.263567	27.154266
245.229749	9947.072780	27.159284
244.981480	9970.730309	27.164301
245.056250	9982.814938	27.169319
245.407218	10008.222956	27.174336
245.471788	10015.285684	27.179354
246.558696	10016.591665	27.184372
246.950878	10036.675887	27.189389
247.271125	10051.841748	27.194407
247.403938	10054.378095	27.199424
247.584895	10056.285320	27.204442
247.976353	10067.871352	27.209460
248.061432	10079.216805	27.214477
248.782685	10065.486019	27.219495
248.811620	10084.304153	27.224512
248.787130	10097.835146	27.229530
249.193163	10096.780658	27.234548
249.276066	10109.185454	27.239565
249.462261	10112.437536	27.244583
249.656870	10125.822267	27.249600
249.509153	10139.509937	27.254618
250.074215	10154.772604	27.259636
249.828005	10174.659136	27.264653
250.495214	10189.705774	27.269671
250.516862	10203.726908	27.274688
250.694369	10211.986901	27.279706
251.274467	10226.232226	27.284724
251.008096	10245.944232	27.289741
251.278770	10253.996027	27.294759
251.620465	10276.196087	27.299776
251.949393	10308.620816	27.304794
252.132371	10314.193123	27.309812
252.584776	10328.647950	27.314829
253.191213	10339.953073	27.319847
253.471187	10343.999110	27.324864
253.336140	10363.925126	27.329882
254.070037	10363.548767	27.334900
254.832228	10357.905823	27.339917
255.258621	10350.024437	27.344935
255.415388	10342.677781	27.349952
255.354318	10349.711763	27.354970
255.734720	10357.916569	27.359988
255.915487	10376.765748	27.365005
256.043049	10377.829633	27.370023
256.266111	10377.394280	27.375040
256.145224	10385.782725	27.380058
256.697432	10395.752988	27.385076
256.752170	10410.518732	27.390093
256.836405	10416.750944	27.395111
257.220922	10415.366046	27.400128
257.197060	10429.384145	27.405146
257.676598	10438.427685	27.410164
257.811494	10464.541616	27.415181
258.064264	10472.057647	27.420199
258.070230	10492.241728	27.425216
258.168124	10510.419769	27.430234
258.253454	10517.553223	27.435252
258.422224	10534.584527	27.440269
258.670932	10559.776136	27.445287
258.891643	10571.227906	27.450304
259.461813	10595.598602	27.455322
259.944610	10610.434560	27.460340
260.130271	10630.034882	27.465357
260.692156	10639.285042	27.470375
260.925804	10648.739600	27.475392
261.087969	10672.901417	27.480410
261.459203	10680.936189	27.485428
261.692198	10703.863034	27.490445
262.161510	10710.659706	27.495463
262.424450	10717.816385	27.500480
262.294236	10737.609656	27.505498
262.406190	10750.649769	27.510516
262.567117	10763.408872	27.515533
262.678135	10788.107547	27.520551
263.435605	10805.837203	27.525568
263.592222	10830.090030	27.530586
263.802734	10843.404864	27.535604
263.606143	10870.644717	27.540621
263.680845	10889.407085	27.545639
264.063756	10910.959562	27.550656
264.186028	10937.328559	27.555674
264.671228	10954.304489	27.560692
264.831482	10986.488429	27.565709
264.814861	11006.335046	27.570727
265.549245	11021.137713	27.575744
265.358493	11054.888517	27.580762
265.850850	11065.186211	27.585780
266.095114	11094.889666	27.590797
266.869140	11124.680452	27.595815
267.234605	11136.035317	27.600832
267.579524	11152.602123	27.605850
267.749311	11173.706095	27.610868
267.797251	11186.617273	27.615885
267.685570	11207.446469	27.620903
268.174344	11218.543868	27.625920
268.989607	11233.871834	27.630938
269.332811	11245.361394	27.635956
270.122270	11256.271753	27.640973
270.528383	11256.454287	27.645991
270.938947	11256.134912	27.651008
271.064251	11263.038060	27.656026
271.548704	11273.335667	27.661044
271.733914	11279.238869	27.666061
271.799933	11273.721246	27.671079
272.445882	11273.109377	27.676096
272.265002	11277.652263	27.681114
272.397232	11268.782320	27.686132
271.988724	11277.548315	27.691149
272.498663	11299.479821	27.696167
272.285963	11310.629753	27.701184
272.967098	11340.556628	27.706202
273.110980	11353.557082	27.711220
272.997424	11379.141424	27.716237
273.066312	11403.679628	27.721255
273.270388	11420.844491	27.726272
273.473731	11454.801211	27.731290
273.637969	11476.803241	27.736308
274.292370	11507.081714	27.741325
274.473509	11545.719857	27.746343
274.450506	11561.954577	27.751360
274.883170	11598.250410	27.756378
275.492620	11615.037108	27.761396
275.731446	11645.000956	27.766413
276.106575	11655.025990	27.771431
276.493723	11680.444608	27.776448
276.756929	11696.193861	27.781466
277.418427	11713.178191	27.786484
277.325107	11727.781389	27.791501
277.908771	11745.404755	27.796519
278.556160	11748.089568	27.801536
278.939007	11766.431351	27.806554
279.233192	11775.414428	27.811572
279.265459	11782.954678	27.816589
279.394000	11799.844483	27.821607
280.166691	11797.828741	27.826624
279.956133	11806.679286	27.831642
280.704613	11818.307818	27.836660
280.766918	11831.543273	27.841677
280.820835	11828.205547	27.846695
280.915285	11832.100944	27.851712
281.107111	11849.599315	27.856730
281.183458	11855.160485	27.861748
281.574715	11884.773994	27.866765
281.617939	11897.636111	27.871783
281.718673	11918.896299	27.876800
281.523525	11954.321840	27.881818
282.044339	11973.584231	27.886836
282.348886	11995.999464	27.891853
282.361473	12042.479904	27.896871
282.680226	12067.215830	27.901888
282.687112	12100.411681	27.906906
282.980650	12127.987262	27.911924
283.376636	12167.564026	27.916941
283.463780	12184.932552	27.921959
284.423414	12213.186847	27.926976
284.399726	12253.180898	27.931994
285.206237	12272.449835	27.937012
285.485345	12296.132236	27.942029
286.262782	12319.773388	27.947047
286.462305	12329.300967	27.952064
286.711088	12349.006011	27.957082
287.255490	12367.758917	27.962100
287.487549	12380.158790	27.967117
287.418612	12394.455802	27.972135
287.991466	12410.910747	27.977152
287.694163	12437.399785	27.982170
288.204009	12453.626013	27.987188
288.723166	12473.669420	27.992205
288.975752	12492.418902	27.997223
289.873617	12500.369042	28.002240
290.001538	12521.251828	28.007258
290.473732	12530.685508	28.012276
290.653439	12547.039337	28.017293
290.675531	12554.477667	28.022311
291.207058	12564.911447	28.027328
291.335622	12583.702779	28.032346
291.606137	12605.057689	28.037364
291.712362	12616.888287	28.042381
291.984789	12633.746411	28.047399
293.222679	12634.155203	28.052416
293.254672	12639.074905	28.057434
293.579342	12641.596112	28.062452
293.879514	12662.191081	28.067469
293.746512	12670.972060	28.072487
294.188088	12659.758323	28.077504
294.735921	12679.111481	28.082522
294.710580	12683.041798	28.087540
295.369570	12695.932968	28.092557
295.236718	12690.081731	28.097575
295.698360	12702.882222	28.102592
295.960662	12724.691029	28.107610
295.956348	12723.167702	28.112628
295.735324	12732.483903	28.117645
295.837750	12755.516390	28.122663
296.272314	12771.738503	28.127680
296.150869	12800.614106	28.132698
296.623532	12824.725890	28.137716
296.849997	12850.742834	28.142733
297.134010	12871.186380	28.147751
297.909430	12893.165942	28.152768
297.919038	12910.557984	28.157786
298.422004	12928.294181	28.162804
299.044254	12943.420435	28.167821
299.277583	12970.085742	28.172839
299.614097	12976.283575	28.177856
299.802352	12995.545856	28.182874
299.783881	13017.874429	28.187892
300.373593	13027.895053	28.192909
300.592634	13047.085923	28.197927
301.140305	13053.112049	28.202944
301.258130	13073.302208	28.207962
301.663136	13088.399635	28.212980
302.174913	13110.246577	28.217997
302.256781	13123.943098	28.223015
302.711797	13139.610433	28.228032
303.054745	13145.033358	28.233050
303.084212	13175.068988	28.238068
303.466264	13189.580976	28.243085
303.227730	13209.889121	28.248103
303.764534	13228.713670	28.253120
303.864309	13256.411048	28.258138
304.461385	13277.542220	28.263156
304.712009	13296.420624	28.268173
304.725264	13331.175084	28.273191
305.293993	13352.210338	28.278208
305.364000	13372.996958	28.283226
305.425344	13410.269881	28.288244
306.174060	13428.117386	28.293261
306.368147	13462.240620	28.298279
306.526001	13480.364403	28.303296
306.643510	13515.604172	28.308314
307.297933	13549.251500	28.313332
307.562977	13568.693582	28.318349
307.927440	13600.910707	28.323367
308.237394	13613.287130	28.328384
308.805596	13643.461398	28.333402
308.751109	13672.185198	28.338420
309.291631	13680.761436	28.343437
309.555668	13716.941133	28.348455
309.632676	13737.526839	28.353472
309.626184	13761.069590	28.358490
309.538003	13796.351517	28.363508
309.931659	13825.154817	28.368525
310.211591	13859.978168	28.373543
310.645386	13887.666644	28.378560
311.084436	13918.758823	28.383578
311.465117	13954.263356	28.388596
311.687692	13969.563090	28.393613
312.210632	14002.232999	28.398631
312.323522	14019.510785	28.403648
312.983243	14055.249849	28.408666
313.531419	14075.778866	28.413684
313.708390	14100.959852	28.418701
313.874459	14129.373963	28.423719
314.076054	14154.379004	28.428736
314.703624	14167.777957	28.433754
314.868024	14201.124432	28.438772
315.527161	14218.876241	28.443789
315.499157	14244.444072	28.448807
316.011568	14265.237955	28.453824
316.779178	14272.295515	28.458842
317.345468	14292.448135	28.463860
317.516944	14297.952848	28.468877
317.517195	14322.803506	28.473895
317.831591	14334.240282	28.478912
318.423105	14356.834957	28.483930
318.664319	14366.474791	28.488948
319.070641	14388.447115	28.493965
318.946425	14409.496882	28.498983
319.450180	14416.530373	28.504000
319.700908	14440.409878	28.509018
319.905566	14468.468035	28.514036
320.486350	14486.202038	28.519053
320.957639	14508.023102	28.524071
321.424614	14523.256242	28.529088
321.813756	14539.576158	28.534106
321.828742	14557.629461	28.539124
322.009476	14572.481390	28.544141
322.365079	14596.563822	28.549159
322.374102	14615.808277	28.554176
322.771236	14637.629612	28.559194
323.096978	14664.384280	28.564212
323.634879	14679.083668	28.569229
324.160383	14699.604740	28.574247
324.506163	14711.848173	28.579264
324.604405	14734.206351	28.584282
324.909998	14754.519284	28.589300
325.029553	14768.916879	28.594317
325.729562	14797.311559	28.599335
325.802080	14813.028708	28.604352
326.258427	14832.701156	28.609370
326.214410	14857.560204	28.614388
326.804396	14870.029867	28.619405
326.894255	14901.090745	28.624423
326.936180	14920.265288	28.629440
327.409790	14947.240970	28.634458
327.645000	14980.564272	28.639476
328.038731	15007.080856	28.644493
328.234115	15034.961867	28.649511
328.405423	15060.104301	28.654528
328.972508	15085.357063	28.659546
328.988144	15108.027823	28.664564
329.590917	15128.991736	28.669581
329.903847	15160.932276	28.674599
330.699499	15185.304271	28.679616
330.849331	15196.092040	28.684634
330.896092	15223.467624	28.689652
331.407162	15241.723537	28.694669
331.616865	15266.162974	28.699687
332.046158	15298.838890	28.704704
332.508305	15316.794313	28.709722
332.307765	15347.505413	28.714740
332.755614	15365.034580	28.719757
333.051975	15402.080978	28.724775
333.488750	15429.669069	28.729792
334.302701	15446.832922	28.734810
334.835451	15463.151208	28.739828
335.508011	15467.728672	28.744845
336.122414	15501.360046	28.749863
336.422909	15505.900402	28.754880
336.695870	15507.018526	28.759898
336.690066	15535.284805	28.764916
337.370624	15531.756966	28.769933
337.823968	15548.505098	28.774951
337.762203	15558.632626	28.779968
338.431451	15568.406304	28.784986
338.462601	15592.386582	28.790004
338.759436	15597.676354	28.795021
338.954329	15617.356714	28.800039
339.498373	15622.987178	28.805056
339.933119	15636.708851	28.810074
339.870082	15657.086071	28.815092
340.016450	15678.415799	28.820109
340.560653	15695.818459	28.825127
340.376648	15730.438365	28.830144
340.612037	15748.152528	28.835162
340.654696	15770.223697	28.840180
340.954243	15798.143312	28.845197
341.206079	15848.887479	28.850215
341.894956	15880.968326	28.855232
342.162871	15901.109417	28.860250
342.396062	15938.327053	28.865268
342.783327	15962.049784	28.870285
343.400847	15991.480571	28.875303
343.717897	16017.540577	28.880320
344.294612	16051.494804	28.885338
344.304895	16086.602359	28.890356
344.719367	16105.448010	28.895373
345.226629	16129.859792	28.900391
345.923892	16154.541714	28.905408
346.879574	16173.807017	28.910426
347.229262	16172.356697	28.915444
347.752656	16188.827061	28.920461
348.175660	16200.200801	28.925479
348.150954	16212.603427	28.930496
348.528427	16206.359233	28.935514
348.343895	16223.516887	28.940532
348.719945	16235.597045	28.945549
348.794814	16254.333970	28.950567
349.414366	16282.640949	28.955584
349.386481	16299.060873	28.960602
349.574471	16320.415820	28.965620
349.843078	16350.253852	28.970637
350.230863	16373.535686	28.975655
350.606956	16402.847785	28.980672
351.496818	16428.228566	28.985690
351.196942	16463.740038	28.990708
351.734828	16488.046206	28.995725
351.804748	16508.839927	29.000743
351.917746	16535.123311	29.005760
352.448120	16567.454927	29.010778
352.776334	16603.521154	29.015796
353.346694	16621.538268	29.020813
353.978950	16641.189022	29.025831
354.387116	16664.184010	29.030848
355.004364	16691.371228	29.035866
354.771410	16716.888130	29.040884
355.523361	16736.416015	29.045901
355.778134	16758.575103	29.050919
356.008802	16785.879174	29.055936
356.366718	16798.725856	29.060954
356.612973	16833.152922	29.065972
356.904989	16871.407754	29.070989
356.982543	16896.488633	29.076007
357.324449	16934.878518	29.081024
357.723336	16969.542978	29.086042
357.819990	17002.186240	29.091060
358.114675	17029.356773	29.096077
358.445815	17073.495089	29.101095
358.797806	17110.217305	29.106112
359.499989	17143.543734	29.111130
359.642184	17186.754648	29.116148
360.468170	17214.375164	29.121165
360.958680	17245.031227	29.126183
361.083298	17281.095974	29.131200
361.636013	17308.760327	29.136218
361.805227	17346.260074	29.141236
362.100932	17367.252644	29.146253
363.103133	17382.458174	29.151271
363.305449	17412.550673	29.156288
364.020546	17428.740323	29.161306
364.315474	17464.686417	29.166324
364.675729	17498.193545	29.171341
364.900910	17514.459359	29.176359
365.076749	17535.680784	29.181376
365.631062	17561.105037	29.186394
365.691427	17591.423981	29.191412
366.001110	17623.910553	29.196429
366.707675	17648.241532	29.201447
366.800072	17671.654628	29.206464
367.614880	17680.083475	29.211482
367.426275	17705.143388	29.216500
367.718451	17737.262692	29.221517
367.759448	17761.865556	29.226535
368.224711	17794.784572	29.231552
368.339727	17821.552055	29.236570
368.223425	17857.779149	29.241588
369.181006	17892.294593	29.246605
369.400878	17923.978904	29.251623
369.956902	17961.722742	29.256640
370.985623	17983.090233	29.261658
371.245025	18022.128956	29.266676
372.287044	18035.046962	29.271693
372.937565	18050.671259	29.276711
372.599734	18065.501665	29.281728
372.968689	18081.372894	29.286746
373.237876	18115.197990	29.291764
373.261197	18128.319030	29.296781
373.856011	18160.786156	29.301799
373.937169	18189.868150	29.306816
374.381008	18212.045636	29.311834
374.588368	18252.930542	29.316852
374.506049	18287.137850	29.321869
374.802638	18327.641875	29.326887
375.297902	18366.691428	29.331904
375.609791	18411.875550	29.336922
375.665024	18452.378670	29.341940
375.801455	18497.304571	29.346957
376.440795	18543.820352	29.351975
376.497445	18596.107246	29.356992
377.263776	18626.021699	29.362010
378.348765	18673.803177	29.367028
378.547352	18711.338777	29.372045
379.035993	18748.433746	29.377063
379.514274	18776.568930	29.382080
379.911205	18800.672430	29.387098
380.243500	18841.051746	29.392116
380.962305	18872.710675	29.397133
381.570922	18892.155286	29.402151
381.619664	18928.726912	29.407168
382.264472	18955.626138	29.412186
382.628818	18978.193504	29.417204
383.427160	19000.159918	29.422221
383.870053	19021.088341	29.427239
384.223939	19040.936259	29.432256
384.870516	19069.492442	29.437274
384.916105	19085.705416	29.442292
385.265528	19112.319684	29.447309
385.770650	19137.603399	29.452327
385.715075	19163.467283	29.457344
386.270010	19183.411778	29.462362
386.227260	19206.336173	29.467380
386.820884	19238.599041	29.472397
387.005379	19259.553123	29.477415
387.397586	19282.675847	29.482432
387.828443	19307.926822	29.487450
388.318995	19334.643390	29.492468
388.598919	19352.401040	29.497485
389.334106	19370.022350	29.502503
389.607741	19399.712008	29.507520
389.569059	19421.756199	29.512538
389.434180	19454.727708	29.517556
389.607917	19473.572690	29.522573
390.256982	19521.931104	29.527591
390.565681	19563.188115	29.532608
390.904054	19587.668576	29.537626
391.454889	19623.619576	29.542644
391.920152	19669.774121	29.547661
392.135971	19697.561642	29.552679
392.776809	19737.584343	29.557696
393.369481	19768.282692	29.562714
394.160373	19802.896858	29.567732
393.997322	19846.042349	29.572749
394.251110	19879.236620	29.577767
394.530267	19917.227811	29.582784
395.545103	19940.328302	29.587802
396.170892	19969.706332	29.592820
396.770481	19992.345115	29.597837
397.810340	20003.494327	29.602855
397.852396	20025.227459	29.607872
398.367790	20041.252041	29.612890
399.169044	20052.036948	29.617908
399.614710	20066.105704	29.622925
400.035555	20073.267768	29.627943
400.282145	20098.644534	29.632960
400.706690	20102.764395	29.637978
400.929010	20114.635612	29.642996
401.013617	20133.711045	29.648013
401.470111	20151.718365	29.653031
401.795637	20178.562312	29.658048
402.310676	20201.550142	29.663066
402.288237	20216.755685	29.668084
402.572243	20248.542172	29.673101
402.659562	20277.762309	29.678119
402.907290	20311.991262	29.683136
403.357408	20338.547634	29.688154
403.774954	20379.705991	29.693172
403.792271	20417.467238	29.698189
404.544458	20443.863210	29.703207
404.828581	20485.087261	29.708224
405.131805	20516.908801	29.713242
405.482357	20558.211523	29.718260
405.728625	20593.540330	29.723277
406.164970	20626.882962	29.728295
406.620462	20668.210542	29.733312
407.359756	20698.147503	29.738330
407.603823	20733.932681	29.743348
407.699098	20774.322543	29.748365
408.703404	20802.932313	29.753383
409.153709	20827.947278	29.758400
409.953772	20849.903201	29.763418
411.060731	20864.084784	29.768436
411.082375	20881.680160	29.773453
411.654100	20900.338687	29.778471
411.844527	20922.919536	29.783488
412.243468	20928.243966	29.788506
412.749166	20943.172007	29.793524
412.236122	20986.823466	29.798541
412.830634	21003.790974	29.803559
413.017458	21044.004950	29.808576
413.130611	21072.689051	29.813594
413.546687	21109.708605	29.818612
413.592981	21145.046021	29.823629
414.307421	21184.982266	29.828647
414.420041	21234.173898	29.833664
414.846477	21281.766556	29.838682
415.108227	21317.521547	29.843700
415.219511	21365.053332	29.848717
416.031316	21403.856972	29.853735
416.169843	21463.923776	29.858752
416.617544	21507.170657	29.863770
417.162512	21551.343965	29.868788
417.643560	21597.560972	29.873805
418.247331	21642.810929	29.878823
418.817215	21688.639232	29.883840
419.131127	21743.384843	29.888858
419.624557	21777.256101	29.893876
419.782062	21823.308396	29.898893
420.436284	21863.879439	29.903911
420.769272	21912.950109	29.908928
420.981619	21964.476388	29.913946
421.920667	22003.038817	29.918964
422.718436	22040.736147	29.923981
423.397602	22070.758374	29.928999
423.561658	22105.129850	29.934016
424.162148	22130.560965	29.939034
425.211622	22154.950079	29.944052
425.258229	22191.902834	29.949069
425.670386	22218.252606	29.954087
426.439942	22251.959217	29.959104
426.384407	22276.787028	29.964122
426.570363	22296.880430	29.969140
427.127757	22336.694900	29.974157
427.745306	22366.087955	29.979175
427.547390	22412.529178	29.984192
428.026311	22444.718456	29.989210
428.392592	22485.493289	29.994228
428.392008	22529.885624	29.999245
428.863817	22570.771889	30.004263
429.921128	22608.798169	30.009280
430.340537	22652.207344	30.014298
430.705458	22687.523309	30.019316
431.297847	22727.029906	30.024333
432.023468	22750.466087	30.029351
432.001615	22797.934779	30.034368
432.487620	22823.414932	30.039386
433.332207	22834.943285	30.044404
433.703389	22863.505746	30.049421
434.337681	22886.468888	30.054439
434.686644	22909.298022	30.059456
434.801526	22939.071529	30.064474
435.440180	22963.440737	30.069492
435.615826	22990.522968	30.074509
436.203726	23010.109913	30.079527
436.122579	23047.313498	30.084544
436.712701	23088.202803	30.089562
436.884937	23128.943029	30.094580
436.988881	23171.928158	30.099597
437.307986	23220.304744	30.104615
437.589875	23260.682694	30.109632
438.044505	23310.982401	30.114650
438.604473	23352.722809	30.119668
439.004394	23410.318231	30.124685
439.699639	23454.363463	30.129703
439.767467	23495.532490	30.134720
439.899633	23546.534747	30.139738
440.633564	23591.715510	30.144756
441.171568	23648.969497	30.149773
441.699709	23699.387065	30.154791
442.360357	23744.132891	30.159808
442.445673	23790.201260	30.164826
443.140632	23842.871158	30.169844
443.526196	23892.764889	30.174861
444.084114	23930.274072	30.179879
444.773709	23987.878564	30.184896
444.952859	24030.010762	30.189914
445.774037	24060.766012	30.194932
446.954489	24092.264091	30.199949
447.822896	24118.589069	30.204967
448.743028	24126.619883	30.209984
449.218359	24149.447936	30.215002
450.221637	24147.001772	30.220020
450.931267	24170.445794	30.225037
451.312667	24172.055355	30.230055
451.846206	24175.578729	30.235072
451.899345	24176.862873	30.240090
452.486154	24184.736343	30.245108
452.287296	24203.573119	30.250125
452.635429	24225.637654	30.255143
453.281241	24240.708600	30.260160
453.127119	24265.127190	30.265178
453.392921	24290.836516	30.270196
453.283316	24327.577749	30.275213
453.947781	24360.685122	30.280231
454.105618	24399.084009	30.285248
454.204156	24436.344966	30.290266
455.121501	24466.270648	30.295284
455.638416	24516.626293	30.300301
455.306192	24547.706238	30.305319
456.004726	24587.353489	30.310336
456.005388	24631.628008	30.315354
456.626724	24668.585382	30.320372
457.069608	24705.368380	30.325389
457.609716	24737.734426	30.330407
458.096114	24777.793839	30.335424
458.368171	24824.315589	30.340442
458.953880	24866.730300	30.345460
459.644628	24915.956431	30.350477
460.139859	24963.146902	30.355495
460.535144	25000.459165	30.360512
460.755243	25052.021754	30.365530
461.222272	25080.114077	30.370548
461.714818	25131.860492	30.375565
462.346460	25173.100934	30.380583
463.519913	25201.766385	30.385600
463.551946	25240.482062	30.390618
464.271065	25273.985595	30.395636
464.947261	25293.711433	30.400653
465.825182	25313.295473	30.405671
466.427200	25349.301803	30.410688
466.526816	25379.978017	30.415706
467.220342	25399.732551	30.420724
467.651912	25435.601080	30.425741
467.984910	25457.417421	30.430759
468.621772	25486.941845	30.435776
468.578653	25530.588949	30.440794
469.069298	25560.580188	30.445812
469.480370	25595.632381	30.450829
469.332767	25638.029533	30.455847
470.012617	25674.518467	30.460864
470.262095	25731.734164	30.465882
470.521276	25775.049324	30.470900
470.780266	25827.465597	30.475917
471.018748	25876.831897	30.480935
471.662585	25926.245596	30.485952
471.722075	25984.400050	30.490970
472.241392	26028.636576	30.495988
472.991225	26096.086500	30.501005
473.121436	26157.311489	30.506023
474.118536	26207.217516	30.511040
475.158296	26255.939688	30.516058
475.792548	26290.103280	30.521076
476.356247	26335.683181	30.526093
477.273974	26365.539535	30.531111
478.121099	26403.206427	30.536128
478.197896	26428.415015	30.541146
478.446622	26451.865404	30.546164
479.293859	26493.696674	30.551181
479.565571	26539.197799	30.556199
480.232054	26561.400043	30.561216
480.382314	26602.672742	30.566234
481.365432	26619.199085	30.571252
482.063570	26649.203971	30.576269
482.228108	26680.060635	30.581287
482.794287	26700.128713	30.586304
483.434726	26722.237829	30.591322
483.620944	26753.412692	30.596340
484.406394	26779.714938	30.601357
484.517160	26806.653368	30.606375
484.762535	26828.947042	30.611392
485.087942	26866.164872	30.616410
485.631613	26896.638321	30.621428
485.689975	26937.930715	30.626445
486.015165	26984.291403	30.631463
486.329434	27012.113325	30.636480
486.600402	27066.130755	30.641498
487.152109	27112.314157	30.646516
487.291286	27167.345095	30.651533
487.669521	27225.146202	30.656551
488.051316	27271.627301	30.661568
488.179769	27338.743678	30.666586
488.953024	27393.250233	30.671604
489.562354	27455.161152	30.676621
489.899248	27508.155933	30.681639
491.170456	27567.493023	30.686656
491.881038	27621.648217	30.691674
492.506342	27656.648919	30.696692
492.778867	27701.755411	30.701709
493.191308	27744.762101	30.706727
493.693181	27795.347510	30.711744
494.112348	27849.957176	30.716762
494.673676	27899.870160	30.721780
495.155309	27944.118001	30.726797
495.496669	28000.779578	30.731815
495.899380	28044.438594	30.736832
496.501306	28099.024030	30.741850
497.416735	28141.185151	30.746868
498.243158	28191.791812	30.751885
498.504138	28233.576269	30.756903
499.714418	28273.809951	30.761920
499.646045	28317.742825	30.766938
500.577739	28360.283445	30.771956
501.181094	28394.623670	30.776973
501.219983	28438.513226	30.781991
501.932770	28475.936278	30.787008
502.070065	28526.150866	30.792026
502.229583	28568.653930	30.797044
503.224934	28613.149871	30.802061
503.575903	28651.916261	30.807079
504.660100	28692.081011	30.812096
504.782038	28744.737746	30.817114
505.240567	28773.244490	30.822132
505.906046	28810.266196	30.827149
506.125896	28862.632011	30.832167
506.624390	28896.928083	30.837184
507.115256	28945.347956	30.842202
507.745958	28993.251797	30.847220
507.752433	29032.737482	30.852237
508.442629	29074.308407	30.857255
508.757303	29115.044551	30.862272
509.289080	29165.745522	30.867290
509.926738	29205.205475	30.872308
510.614490	29244.404516	30.877325
511.314963	29285.163293	30.882343
511.831595	29320.365782	30.887360
511.891421	29363.465248	30.892378
512.865094	29403.240386	30.897396
514.380415	29421.482997	30.902413
514.916670	29438.025489	30.907431
515.735123	29457.416151	30.912448
515.715516	29489.309516	30.917466
516.179349	29510.146151	30.922484
516.326043	29533.804306	30.927501
516.631103	29572.145163	30.932519
517.235567	29608.901342	30.937536
517.657088	29651.387365	30.942554
517.914135	29687.483835	30.947572
518.510073	29728.832656	30.952589
518.828896	29767.158956	30.957607
519.043862	29811.570777	30.962624
519.094590	29867.019724	30.967642
519.608238	29914.472828	30.972660
520.360920	29966.728531	30.977677
520.551595	30031.282378	30.982695
521.288886	30082.985721	30.987712
521.182955	30138.626438	30.992730
521.791533	30202.348861	30.997748
522.945525	30263.226567	31.002765
523.048565	30324.350821	31.007783
523.576647	30387.614394	31.012800
524.000006	30462.116792	31.017818
524.302963	30525.302679	31.022836
524.676941	30589.533693	31.027853
524.875368	30657.575248	31.032871
525.817783	30731.368214	31.037888
526.718369	30794.348526	31.042906
527.297141	30848.776040	31.047924
528.271366	30906.285145	31.052941
528.972013	30967.571120	31.057959
529.539979	31015.308169	31.062976
530.101350	31065.987424	31.067994
530.752760	31115.988734	31.073012
531.224375	31162.761318	31.078029
531.501778	31228.948691	31.083047
532.673372	31269.353627	31.088064
533.666296	31313.323504	31.093082
533.749915	31355.969329	31.098100
534.235629	31385.722079	31.103117
534.643441	31446.324629	31.108135
535.257431	31487.983706	31.113152
535.610070	31535.866338	31.118170
536.175149	31585.609222	31.123188
536.990948	31624.889420	31.128205
537.028020	31685.818224	31.133223
537.668108	31717.918114	31.138240
538.258895	31764.138556	31.143258
539.082685	31795.654873	31.148276
539.669727	31833.453703	31.153293
539.944629	31886.147196	31.158311
540.307878	31921.816614	31.163328
540.867943	31965.559326	31.168346
541.538711	32004.887302	31.173364
542.269135	32049.033359	31.178381
542.432779	32097.694625	31.183399
542.643556	32142.254987	31.188416
543.194148	32200.361553	31.193434
543.734496	32249.791798	31.198452
545.060666	32279.064373	31.203469
545.495684	32323.813979	31.208487
546.719655	32362.745007	31.213504
546.923285	32396.666034	31.218522
547.422885	32435.730803	31.223540
548.107323	32480.513804	31.228557
548.421879	32524.596593	31.233575
548.848360	32571.396383	31.238592
549.117669	32606.944410	31.243610
549.585572	32652.531800	31.248628
550.299610	32707.456207	31.253645
550.376479	32762.429994	31.258663
550.832541	32804.166540	31.263680
551.229489	32862.705528	31.268698
551.858401	32926.730858	31.273716
552.163754	32977.396288	31.278733
553.192764	33035.152188	31.283751
553.748346	33090.723469	31.288768
554.264672	33153.364531	31.293786
554.622920	33205.318612	31.298804
555.113557	33259.923216	31.303821
555.427088	33324.976022	31.308839
556.512199	33366.123239	31.313856
557.686954	33422.365817	31.318874
557.970046	33467.990101	31.323892
559.127232	33515.926379	31.328909
559.514302	33565.260276	31.333927
560.540025	33600.737476	31.338944
561.535873	33627.872311	31.343962
561.970125	33661.989757	31.348980
562.818395	33693.221192	31.353997
562.648568	33728.395373	31.359015
563.396297	33766.423234	31.364032
563.550705	33806.913524	31.369050
563.922556	33853.918533	31.374068
564.586518	33896.411000	31.379085
564.797213	33943.147187	31.384103
565.040687	33995.520875	31.389120
565.557218	34059.029810	31.394138
565.470516	34117.406420	31.399156
566.215884	34182.915397	31.404173
566.366538	34253.623582	31.409191
566.900173	34314.627711	31.414208
567.389256	34373.891197	31.419226
567.828014	34444.165719	31.424244
568.253241	34503.765652	31.429261
568.650344	34578.008771	31.434279
569.732907	34641.343868	31.439296
570.290519	34699.138537	31.444314
570.929942	34763.304309	31.449332
571.890359	34818.009888	31.454349
572.331001	34880.960287	31.459367
573.079050	34938.931403	31.464384
573.923180	34991.593274	31.469402
574.506593	35050.473538	31.474420
575.059271	35099.499192	31.479437
575.460333	35153.424190	31.484455
576.132947	35211.655291	31.489472
576.707226	35272.125434	31.494490
576.998062	35337.328249	31.499508
578.037298	35390.652233	31.504525
578.413578	35446.387740	31.509543
578.962760	35515.078820	31.514560
579.473332	35571.978474	31.519578
579.863448	35635.852325	31.524596
580.613623	35688.251406	31.529613
581.013862	35748.894991	31.534631
581.616555	35824.613563	31.539648
582.419162	35887.514906	31.544666
582.638000	35959.146026	31.549684
583.342763	36015.764443	31.554701
583.785349	36091.612562	31.559719
584.222775	36160.290506	31.564736
585.139887	36222.456882	31.569754
585.048196	36303.053147	31.574772
585.766364	36362.943575	31.579789
586.208616	36447.243047	31.584807
586.631494	36525.391096	31.589824
587.287219	36589.165963	31.594842
588.159322	36679.235521	31.599860
588.954536	36744.653668	31.604877
589.903526	36819.884600	31.609895
590.563979	36878.359857	31.614912
591.570795	36941.580227	31.619930
592.123311	37010.983441	31.624948
592.897955	37067.116510	31.629965
593.689671	37122.719677	31.634983
594.368908	37175.605521	31.640000
595.132857	37223.991478	31.645018
595.548085	37275.530783	31.650036
595.988955	37330.465517	31.655053
596.565731	37393.514913	31.660071
596.701564	37444.089284	31.665088
597.563030	37502.819354	31.670106
597.822062	37560.241800	31.675124
598.570079	37630.387247	31.680141
598.879277	37694.692527	31.685159
599.422840	37750.845187	31.690176
599.833202	37809.934473	31.695194
600.270657	37885.775126	31.700212
600.809045	37945.688912	31.705229
601.207494	38007.363072	31.710247
601.754619	38079.053570	31.715264
603.076113	38138.650727	31.720282
603.621212	38203.561349	31.725300
604.847044	38252.521183	31.730317
605.198900	38318.750127	31.735335
606.238802	38360.999211	31.740352
607.203790	38410.944883	31.745370
607.565736	38462.935446	31.750388
608.175099	38498.563016	31.755405
608.981210	38557.242808	31.760423
609.571378	38598.871833	31.765440
609.947785	38648.442308	31.770458
610.310227	38704.502638	31.775476
610.770268	38760.518006	31.780493
611.966142	38811.015541	31.785511
612.797323	38855.950139	31.790528
613.540787	38901.114544	31.795546
613.698978	38950.227585	31.800564
614.430316	38997.976644	31.805581
614.698459	39051.500251	31.810599
615.239882	39116.190579	31.815616
615.529921	39154.178679	31.820634
615.748909	39229.670835	31.825652
616.229445	39294.261724	31.830669
616.597425	39368.169383	31.835687
617.073948	39442.292357	31.840704
617.804993	39521.776791	31.845722
618.014917	39614.215647	31.850740
618.625543	39682.864458	31.855757
619.332001	39767.064429	31.860775
619.426238	39850.312061	31.865792
620.328906	39936.275545	31.870810
621.053505	40029.158679	31.875828
621.328916	40118.109725	31.880845
622.072780	40211.154636	31.885863
622.902642	40297.615306	31.890880
623.336466	40379.781064	31.895898
623.828829	40469.864764	31.900916
624.692347	40555.695751	31.905933
625.522085	40640.361608	31.910951
625.787587	40734.157256	31.915968
626.612437	40809.962471	31.920986
627.343294	40900.465190	31.926004
628.866725	40968.150960	31.931021
629.966893	41035.978950	31.936039
630.532151	41100.397429	31.941056
631.597499	41155.735393	31.946074
631.673296	41228.693337	31.951092
632.166912	41295.031760	31.956109
632.932341	41370.716831	31.961127
633.872743	41423.039668	31.966144
634.865818	41467.965495	31.971162
635.675156	41522.764306	31.976180
635.951832	41567.427913	31.981197
636.323647	41615.314763	31.986215
637.396783	41670.536102	31.991232
638.256081	41704.500981	31.996250
638.482417	41759.855028	32.001268
639.452727	41809.808958	32.006285
639.785335	41862.268729	32.011303
640.169321	41925.726534	32.016320
640.911023	41976.720970	32.021338
641.172398	42035.119883	32.026356
641.706417	42104.835852	32.031373
642.407412	42164.918542	32.036391
642.985472	42229.171375	32.041408
643.745152	42289.430700	32.046426
644.036868	42360.322658	32.051444
644.329173	42437.378191	32.056461
645.212164	42501.813371	32.061479
645.331382	42584.854199	32.066496
645.742789	42662.354404	32.071514
646.271748	42745.695175	32.076532
647.037485	42836.333900	32.081549
647.954400	42913.543297	32.086567
648.389064	42997.914918	32.091584
649.436975	43075.923510	32.096602
649.964436	43166.765685	32.101620
650.466894	43249.465918	32.106637
651.086960	43333.516778	32.111655
651.250491	43429.291638	32.116672
652.196971	43502.399754	32.121690
653.272669	43593.996317	32.126708
653.974895	43681.160753	32.131725
654.908096	43754.044766	32.136743
655.482611	43835.127949	32.141760
656.826151	43898.396441	32.146778
657.310495	43980.430383	32.151796
658.148023	44054.036121	32.156813
658.614261	44120.607095	32.161831
659.499351	44195.376767	32.166848
660.314105	44252.345693	32.171866
660.713563	44318.423557	32.176884
661.419643	44388.573222	32.181901
662.150521	44452.750615	32.186919
662.837817	44532.203817	32.191936
663.602703	44598.194790	32.196954
663.732601	44674.946229	32.201972
664.221659	44750.351195	32.206989
665.043851	44823.994133	32.212007
666.062870	44903.281534	32.217024
666.591351	44962.995326	32.222042
667.685612	45038.484074	32.227060
668.206179	45104.502873	32.232077
668.842023	45157.538812	32.237095
669.505876	45231.576777	32.242112
670.495723	45287.179848	32.247130
671.386961	45351.771767	32.252148
671.372424	45409.590467	32.257165
671.651467	45471.057054	32.262183
672.089203	45547.914018	32.267200
673.045229	45622.064508	32.272218
672.968893	45691.955114	32.277236
673.663290	45762.727670	32.282253
674.355827	45841.215926	32.287271
674.878530	45931.380545	32.292288
675.854360	46005.946000	32.297306
676.054273	46086.670310	32.302324
676.529772	46180.836021	32.307341
677.265570	46264.453689	32.312359
678.034905	46375.620727	32.317376
678.271028	46468.612978	32.322394
679.214562	46547.793829	32.327412
680.148744	46638.184999	32.332429
681.230004	46728.702992	32.337447
681.697571	46820.798273	32.342464
682.368322	46904.840449	32.347482
682.851009	47006.433979	32.352500
682.955936	47087.286153	32.357517
684.445770	47182.612646	32.362535
684.583608	47289.796886	32.367552
685.071105	47387.001580	32.372570
685.703282	47492.216753	32.377588
686.199320	47594.051132	32.382605
686.902696	47699.113112	32.387623
687.296971	47812.374067	32.392640
688.566514	47909.242130	32.397658
688.885873	48028.142281	32.402676
689.420031	48147.950737	32.407693
690.721683	48234.695327	32.412711
692.794564	48314.665952	32.417728
694.065996	48389.486926	32.422746
695.254946	48446.363198	32.427764
696.411352	48519.675679	32.432781
697.300932	48566.148986	32.437799
697.821326	48634.908914	32.442816
698.548267	48684.455172	32.447834
698.984464	48749.085954	32.452852
699.367735	48817.307802	32.457869
700.558216	48881.146518	32.462887
700.744306	48949.983785	32.467904
701.014432	49020.234574	32.472922
701.707028	49096.414558	32.477940
702.413301	49169.522342	32.482957
702.774252	49244.704749	32.487975
703.521688	49321.627972	32.492992
704.208783	49406.079388	32.498010
704.876576	49485.126870	32.503028
705.237787	49563.614414	32.508045
705.970888	49635.885471	32.513063
706.478417	49717.766256	32.518080
706.879312	49793.645171	32.523098
707.815279	49873.804379	32.528116
708.358909	49964.606538	32.533133
709.147186	50041.298184	32.538151
709.659731	50129.472049	32.543168
710.102194	50208.643198	32.548186
711.135795	50298.446936	32.553204
711.748777	50381.733897	32.558221
712.640983	50472.169146	32.563239
713.204731	50555.458964	32.568256
713.706650	50647.642376	32.573274
714.052468	50743.548819	32.578292
714.861590	50840.361933	32.583309
715.637313	50935.001618	32.588327
716.041885	51040.003351	32.593344
716.524962	51144.625764	32.598362
717.346855	51242.645385	32.603380
717.858043	51345.033845	32.608397
719.012543	51442.662642	32.613415
720.318247	51532.861376	32.618432
721.791987	51611.949994	32.623450
722.348609	51686.836610	32.628468
723.244883	51769.916680	32.633485
724.261431	51857.771907	32.638503
725.106244	51936.609442	32.643520
726.298407	52006.213894	32.648538
726.854308	52082.056174	32.653556
727.405644	52166.422727	32.658573
728.364548	52235.600406	32.663591
728.740706	52327.149840	32.668608
729.355122	52401.713367	32.673626
729.638914	52488.325874	32.678644
730.318987	52573.967363	32.683661
730.706225	52649.297344	32.688679
731.321105	52749.565032	32.693696
731.918956	52851.169324	32.698714
732.761348	52933.979208	32.703732
733.167487	53040.210794	32.708749
733.956454	53139.073216	32.713767
734.472693	53247.214187	32.718784
735.254687	53337.637271	32.723802
736.666808	53426.297366	32.728820
737.581337	53520.995210	32.733837
738.658829	53610.282124	32.738855
739.073843	53702.210382	32.743872
739.955730	53794.318157	32.748890
740.887009	53882.361288	32.753908
741.279802	53976.676776	32.758925
742.270518	54056.110694	32.763943
743.515994	54140.771162	32.768960
744.135775	54218.689573	32.773978
744.727808	54294.123419	32.778996
745.576800	54384.609306	32.784013
746.260832	54454.732791	32.789031
746.968818	54544.087199	32.794048
747.638668	54631.053660	32.799066
748.365320	54689.006701	32.804084
749.267158	54777.122027	32.809101
749.663321	54845.906021	32.814119
750.299292	54927.735902	32.819136
750.618097	55012.072245	32.824154
751.128597	55099.952714	32.829172
751.324759	55200.013813	32.834189
752.538699	55290.599274	32.839207
753.376406	55392.712595	32.844224
753.964726	55479.443947	32.849242
754.727472	55576.313459	32.854260
755.504405	55685.794286	32.859277
756.527808	55775.858486	32.864295
757.619101	55862.246248	32.869312
758.118465	55953.153011	32.874330
759.150329	56049.599550	32.879348
759.793455	56153.386799	32.884365
760.722335	56235.374071	32.889383
761.452958	56329.851332	32.894400
762.055448	56428.060539	32.899418
762.855596	56521.521989	32.904436
763.451780	56626.564669	32.909453
764.347044	56710.651417	32.914471
764.854192	56814.433769	32.919488
765.776946	56917.785243	32.924506
765.861626	57023.416861	32.929524
766.417863	57133.556382	32.934541
767.321274	57234.934717	32.939559
767.799125	57360.654488	32.944576
768.577637	57476.432988	32.949594
769.392292	57576.854985	32.954612
770.108159	57696.241479	32.959629
771.382746	57809.510066	32.964647
772.533035	57916.847159	32.969664
773.231044	58014.523156	32.974682
774.708118	58107.920234	32.979700
775.220618	58217.611779	32.984717
776.240673	58310.215902	32.989735
777.298322	58404.773248	32.994752
778.529318	58499.914397	32.999770
779.316032	58579.432751	33.004788
780.207960	58662.131420	33.009805
781.262447	58728.856635	33.014823
782.613981	58810.661874	33.019840
783.058553	58885.442957	33.024858
783.969009	58959.120626	33.029876
784.209448	59041.850266	33.034893
785.127957	59113.687899	33.039911
785.780240	59196.145371	33.044928
786.076496	59290.293697	33.049946
786.737504	59375.828436	33.054964
787.367289	59471.437371	33.059981
787.981158	59562.675701	33.064999
788.653862	59650.326949	33.070016
789.169912	59736.817143	33.075034
790.396285	59821.125529	33.080052
791.026302	59905.169816	33.085069
791.619152	59979.803093	33.090087
792.558184	60068.605110	33.095104
793.271352	60167.850027	33.100122
794.422124	60246.446585	33.105140
795.525525	60337.117822	33.110157
796.114452	60419.888150	33.115175
796.792914	60504.084612	33.120192
797.292631	60589.841671	33.125210
798.074892	60677.453261	33.130228
798.455745	60791.062154	33.135245
798.965943	60884.062356	33.140263
799.974168	60985.435070	33.145280
800.400389	61095.883731	33.150298
801.650937	61199.156526	33.155316
802.473687	61312.458725	33.160333
802.819940	61414.781310	33.165351
803.627830	61519.869821	33.170368
804.358222	61636.198454	33.175386
805.017535	61748.260491	33.180404
805.723175	61863.817141	33.185421
806.724871	61978.520931	33.190439
807.564646	62094.966153	33.195456
808.019381	62222.767823	33.200474
809.108078	62330.966685	33.205492
809.951618	62458.102682	33.210509
810.926408	62579.180028	33.215527
811.664118	62686.321971	33.220544
811.987920	62821.893522	33.225562
813.102426	62932.208793	33.230580
813.900759	63062.618133	33.235597
814.558458	63182.488990	33.240615
815.287093	63307.260294	33.245632
815.889203	63440.569306	33.250650
816.916028	63555.909662	33.255668
817.640812	63681.316031	33.260685
818.829122	63805.493196	33.265703
819.556356	63926.077093	33.270720
820.932235	64047.189094	33.275738
821.837912	64158.703517	33.280756
822.764484	64277.579997	33.285773
823.597813	64394.216181	33.290791
824.877491	64500.674018	33.295808
825.790095	64620.433591	33.300826
826.659532	64716.259597	33.305844
827.422583	64828.712387	33.310861
828.284178	64932.259996	33.315879
829.407898	65032.886639	33.320896
830.057582	65139.398719	33.325914
831.629218	65235.941352	33.330932
832.439368	65336.553610	33.335949
833.047025	65433.148455	33.340967
833.384322	65517.689168	33.345984
833.883030	65609.738783	33.351002
834.747541	65701.858915	33.356020
835.392458	65802.463761	33.361037
836.022529	65901.642764	33.366055
837.187610	65991.063586	33.371072
837.964876	66092.494351	33.376090
839.310021	66191.937912	33.381108
839.843990	66279.963296	33.386125
840.844543	66377.468831	33.391143
841.932211	66477.141185	33.396160
842.206846	66577.579199	33.401178
843.451609	66682.656739	33.406196
844.448231	66779.488274	33.411213
845.087554	66869.925968	33.416231
846.642042	66948.036056	33.421248
847.018867	67049.325011	33.426266
848.428729	67139.220899	33.431284
849.453031	67221.216470	33.436301
849.923469	67313.790471	33.441319
851.113914	67400.822867	33.446336
851.496041	67495.379192	33.451354
852.338516	67589.484038	33.456372
852.791354	67687.702717	33.461389
853.425212	67792.574225	33.466407
854.195803	67894.609093	33.471424
854.785473	68005.824867	33.476442
855.574239	68114.212323	33.481460
856.511608	68230.687416	33.486477
857.005877	68346.922876	33.491495
857.908662	68455.836322	33.496512
858.495653	68587.030473	33.501530
859.433555	68702.806164	33.506548
859.990486	68820.702793	33.511565
861.000585	68960.786846	33.516583
862.117704	69071.690170	33.521600
862.992836	69189.066393	33.526618
864.216094	69310.677234	33.531636
865.541810	69426.889955	33.536653
867.033403	69512.835991	33.541671
868.022547	69609.744857	33.546688
868.636456	69716.355497	33.551706
869.356363	69822.151739	33.556724
870.388157	69928.413618	33.561741
870.861476	70037.762747	33.566759
871.554778	70151.286315	33.571776
872.342613	70269.246172	33.576794
872.704366	70370.831616	33.581812
873.776931	70497.578205	33.586829
874.198658	70623.444164	33.591847
875.199265	70745.373140	33.596864
875.919337	70870.158647	33.601882
876.456312	71005.941895	33.606900
876.893653	71136.108412	33.611917
877.796789	71274.619488	33.616935
878.903254	71398.557674	33.621952
879.644217	71519.903056	33.626970
880.840784	71646.021668	33.631988
882.005441	71759.713225	33.637005
882.711459	71877.417556	33.642023
883.886211	71999.203568	33.647040
884.436111	72128.458689	33.652058
885.172536	72242.188153	33.657076
885.979627	72363.925327	33.662093
887.003740	72488.098827	33.667111
888.300672	72608.627735	33.672128
889.312378	72738.933105	33.677146
890.127363	72859.906426	33.682164
890.989351	72970.380044	33.687181
891.692905	73099.190829	33.692199
892.470366	73221.627207	33.697216
893.297989	73357.286721	33.702234
894.230501	73485.409120	33.707252
895.263796	73616.392727	33.712269
896.162294	73745.635605	33.717287
897.532928	73872.502500	33.722304
898.034667	74006.868326	33.727322
898.631029	74138.809006	33.732340
899.699104	74266.691353	33.737357
900.410034	74405.109625	33.742375
901.552498	74538.837655	33.747392
902.166762	74684.636449	33.752410
903.359940	74823.461764	33.757428
904.180178	74960.043174	33.762445
904.754709	75102.372735	33.767463
905.572802	75242.055539	33.772480
906.905858	75388.159628	33.777498
907.219344	75521.573805	33.782516
908.470350	75665.524218	33.787533
908.925302	75815.582968	33.792551
910.118578	75950.968011	33.797568
911.243099	76081.153546	33.802586
912.456928	76232.248995	33.807604
913.601098	76361.041204	33.812621
914.777533	76498.545147	33.817639
916.244784	76616.776865	33.822656
917.125663	76738.209150	33.827674
918.443505	76850.167437	33.832692
919.966701	76967.297098	33.837709
920.812350	77093.064060	33.842727
921.556880	77198.398098	33.847744
921.712035	77316.826582	33.852762
922.680493	77437.014129	33.857780
923.953854	77544.953992	33.862797
925.050399	77666.031737	33.867815
925.978597	77769.420269	33.872832
926.547763	77901.457396	33.877850
927.264694	78028.731878	33.882868
928.258159	78150.361250	33.887885
928.573582	78276.339479	33.892903
929.315500	78390.750991	33.897920
929.862146	78528.735763	33.902938
930.402953	78656.132495	33.907956
930.972136	78781.424808	33.912973
931.720874	78932.510464	33.917991
932.593880	79072.435389	33.923008
933.703896	79207.095107	33.928026
934.282981	79366.563341	33.933044
935.100315	79512.383952	33.938061
935.879260	79678.140140	33.943079
936.885573	79826.821549	33.948096
937.871729	79976.089411	33.953114
938.735113	80138.601658	33.958132
939.707908	80299.217337	33.963149
940.952624	80462.982502	33.968167
942.039124	80600.109175	33.973184
943.193371	80759.596171	33.978202
944.017002	80924.467988	33.983220
945.076896	81055.591556	33.988237
945.883594	81225.972710	33.993255
947.376236	81366.507817	33.998272
949.252457	81492.552816	34.003290
950.672166	81621.612370	34.008308
951.868949	81755.550936	34.013325
952.687921	81890.200332	34.018343
953.744627	82020.216383	34.023360
954.187724	82153.362578	34.028378
954.930314	82282.453201	34.033396
956.042827	82418.156312	34.038413
956.525564	82568.375022	34.043431
957.176563	82717.199211	34.048448
958.265816	82858.204751	34.053466
958.746760	83006.572715	34.058484
959.725417	83151.275124	34.063501
960.505537	83318.506225	34.068519
962.064600	83468.280672	34.073536
962.876130	83622.727206	34.078554
963.730864	83777.920334	34.083572
964.560030	83924.298285	34.088589
965.387710	84080.649665	34.093607
966.195574	84246.383015	34.098624
967.026231	84409.202907	34.103642
967.722191	84568.674325	34.108660
969.142548	84735.052907	34.113677
969.746211	84905.109762	34.118695
970.952888	85070.685713	34.123712
971.770835	85240.031210	34.128730
972.623157	85415.510134	34.133748
973.951336	85562.458278	34.138765
975.263938	85735.918072	34.143783
976.755975	85890.978037	34.148800
978.129915	86037.864348	34.153818
978.957320	86179.883899	34.158836
980.503368	86319.851143	34.163853
980.843104	86473.985833	34.168871
982.187908	86611.761728	34.173888
983.085147	86742.457767	34.178906
983.706571	86873.562470	34.183924
984.829876	87020.997721	34.188941
985.558909	87163.432350	34.193959
986.305578	87304.542165	34.198976
987.028342	87455.162281	34.203994
988.063222	87607.925893	34.209012
988.758312	87754.287210	34.214029
989.685782	87919.310636	34.219047
990.539763	88069.374214	34.224064
991.582987	88233.038306	34.229082
991.815781	88401.841987	34.234100
993.151159	88562.604038	34.239117
993.670279	88735.683579	34.244135
994.584655	88919.550678	34.249152
995.590930	89084.397725	34.254170
996.218823	89271.196213	34.259188
997.364729	89455.565707	34.264205
998.355088	89645.602428	34.269223
999.433259	89834.669908	34.274240
1000.965659	90017.167370	34.279258
1002.130454	90176.709870	34.284276
1003.681734	90348.763427	34.289293
1005.000219	90519.528918	34.294311
1005.545689	90679.231401	34.299328
1006.767521	90861.579515	34.304346
1007.507059	91030.738795	34.309364
1008.965159	91201.010444	34.314381
1009.867628	91372.125307	34.319399
1010.647538	91538.724067	34.324416
1012.005771	91702.920959	34.329434
1013.579985	91877.867659	34.334452
1014.920990	92037.708627	34.339469
1016.317366	92188.571948	34.344487
1017.232407	92332.549563	34.349504
1018.265185	92487.331796	34.354522
1019.329345	92643.318626	34.359540
1020.413228	92794.346777	34.364557
1021.324964	92950.804741	34.369575
1022.435516	93096.006655	34.374592
1023.570340	93244.990595	34.379610
1024.250155	93399.484505	34.384628
1025.394290	93550.899420	34.389645
1026.078704	93718.731972	34.394663
1027.104840	93875.391409	34.399680
1027.947463	94032.988472	34.404698
1028.809437	94202.465053	34.409716
1030.381059	94353.950925	34.414733
1031.378881	94509.872231	34.419751
1032.264473	94669.111839	34.424768
1033.907569	94816.644479	34.429786
1035.005994	94965.891844	34.434804
1035.800930	95115.514920	34.439821
1036.730266	95268.236810	34.444839
1037.425947	95412.288825	34.449856
1038.718039	95548.940396	34.454874
1039.535692	95690.377588	34.459892
1040.747225	95828.183982	34.464909
1041.189424	95992.496458	34.469927
1042.221649	96141.091093	34.474944
1043.208946	96298.892884	34.479962
1044.011174	96455.822046	34.484980
1044.829559	96606.925049	34.489997
1045.336263	96774.441299	34.495015
1046.630966	96954.903403	34.500032
1047.535344	97134.129448	34.505050
1048.116548	97307.587569	34.510068
1049.508125	97480.730843	34.515085
1050.185359	97669.629088	34.520103
1050.927393	97853.914896	34.525120
1052.253194	98028.972505	34.530138
1052.887676	98227.562587	34.535156
1054.080268	98411.515690	34.540173
1055.264292	98609.748728	34.545191
1056.262095	98808.357081	34.550208
1057.622461	98993.254335	34.555226
1058.359062	99193.309636	34.560244
1060.291653	99371.659862	34.565261
1061.191328	99564.814101	34.570279
1062.442832	99746.506312	34.575296
1063.758883	99914.423738	34.580314
1065.362844	100097.843599	34.585332
1066.832738	100264.027399	34.590349
1068.327648	100426.174642	34.595367
1069.508407	100586.356841	34.600384
1070.779541	100738.128519	34.605402
1071.675664	100907.017077	34.610420
1072.955010	101057.187244	34.615437
1074.284144	101208.432520	34.620455
1075.247493	101367.789283	34.625472
1076.809699	101519.224409	34.630490
1077.411365	101675.573940	34.635508
1078.332356	101839.404952	34.640525
1079.263965	101993.749598	34.645543
1080.242655	102155.799707	34.650560
1081.188257	102315.652865	34.655578
1081.684381	102483.929894	34.660596
1082.677654	102656.631485	34.665613
1083.795372	102834.594090	34.670631
1084.013468	103024.553526	34.675648
1085.081461	103206.035305	34.680666
1086.126008	103401.947765	34.685684
1087.501287	103594.043520	34.690701
1088.344088	103777.226904	34.695719
1089.976889	103965.380389	34.700736
1091.054328	104142.586116	34.705754
1092.362015	104330.506554	34.710772
1093.450799	104504.698381	34.715789
1095.052298	104663.174217	34.720807
1096.170878	104827.990521	34.725824
1097.535500	104980.327956	34.730842
1098.553231	105150.065160	34.735860
1099.304166	105302.534838	34.740877
1100.111183	105464.457261	34.745895
1101.258431	105636.632572	34.750912
1102.579596	105791.641939	34.755930
1103.039316	105963.493750	34.760948
1103.975124	106142.991579	34.765965
1105.003166	106322.664808	34.770983
1105.744957	106505.022870	34.776000
1106.606558	106685.132337	34.781018
1107.713176	106879.261016	34.786036
1108.739429	107071.213503	34.791053
1109.575758	107271.749970	34.796071
1110.237174	107474.243236	34.801088
1111.441011	107674.783090	34.806106
1112.479214	107886.867178	34.811124
1113.378629	108091.325689	34.816141
1114.882743	108310.300260	34.821159
1115.468483	108526.292310	34.826176
1116.903233	108737.010363	34.831194
1118.031317	108958.283982	34.836212
1119.065435	109170.277381	34.841229
1120.625060	109383.398549	34.846247
1121.917480	109604.053845	34.851264
1123.488723	109806.129893	34.856282
1124.503740	110019.779939	34.861300
1125.654061	110222.931884	34.866317
1127.436353	110419.782332	34.871335
1128.192914	110623.410015	34.876352
1130.152282	110804.131391	34.881370
1131.395819	111003.434555	34.886388
1132.719159	111186.953047	34.891405
1134.530967	111358.265170	34.896423
1135.294116	111548.228970	34.901440
1136.899615	111721.010217	34.906458
1138.261435	111892.542020	34.911476
1139.520561	112080.511510	34.916493
1140.997212	112235.327984	34.921511
1141.951104	112408.668455	34.926528
1142.897568	112582.454690	34.931546
1144.357816	112756.141365	34.936564
1145.130696	112932.848090	34.941581
1146.058509	113106.209989	34.946599
1146.388905	113293.028958	34.951616
1147.347873	113473.330699	34.956634
1148.241352	113677.704631	34.961652
1148.822173	113878.370623	34.966669
1150.235046	114069.393140	34.971687
1150.823637	114281.907024	34.976704
1152.063366	114485.593982	34.981722
1153.239541	114694.982192	34.986740
1154.418077	114902.496330	34.991757
1155.342418	115115.516427	34.996775
1156.542608	115323.346668	35.001792
1158.101876	115519.460022	35.006810
1158.857401	115714.774694	35.011828
1160.137692	115922.139409	35.016845
1160.930458	116115.220371	35.021863
1161.913598	116325.084326	35.026880
1163.181791	116535.255790	35.031898
1163.874960	116756.437043	35.036916
1164.784158	116967.560081	35.041933
1166.204136	117176.202334	35.046951
1167.140905	117405.342404	35.051968
1168.506089	117627.276885	35.056986
1169.471590	117845.746111	35.062004
1170.370164	118082.957162	35.067021
1172.002969	118308.804565	35.072039
1172.569151	118548.864083	35.077056
1173.798501	118773.947795	35.082074
1174.816542	119018.229583	35.087092
1175.993973	119263.221095	35.092109
1177.840350	119497.430048	35.097127
1178.816293	119749.911394	35.102144
1180.571504	119970.478863	35.107162
1181.740283	120194.481259	35.112180
1182.855578	120422.283630	35.117197
1184.572732	120652.937463	35.122215
1185.881470	120878.403758	35.127232
1187.513186	121088.038619	35.132250
1188.757879	121314.380927	35.137268
1189.933504	121528.773315	35.142285
1191.522174	121727.888638	35.147303
1192.421307	121951.253332	35.152320
1193.877810	122159.582303	35.157338
1195.080777	122380.540907	35.162356
1195.956883	122605.219754	35.167373
1197.589830	122830.632512	35.172391
1198.121100	123055.272340	35.177408
1199.574034	123274.547079	35.182426
1200.609777	123495.466392	35.187444
1201.531918	123718.434604	35.192461
1202.790584	123950.079328	35.197479
1203.513520	124181.804847	35.202496
1205.018068	124406.211952	35.207514
1206.253086	124642.694889	35.212532
1207.739825	124862.304762	35.217549
1209.050352	125090.121505	35.222567
1210.519133	125318.394477	35.227584
1211.974813	125548.357130	35.232602
1213.158428	125766.517028	35.237620
1214.846143	125985.796287	35.242637
1215.971194	126200.673763	35.247655
1217.226362	126420.625868	35.252672
1218.558399	126619.740917	35.257690
1220.189107	126828.984403	35.262708
1221.426854	127036.319195	35.267725
1222.901196	127216.780821	35.272743
1223.857406	127414.139995	35.277760
1224.910075	127611.027573	35.282778
1225.922270	127811.573923	35.287796
1226.655302	128010.546835	35.292813
1227.879351	128208.220058	35.297831
1229.106233	128412.219344	35.302848
1229.965001	128623.356204	35.307866
1231.124671	128822.894992	35.312884
1232.106165	129031.820587	35.317901
1233.276726	129247.877302	35.322919
1234.732744	129465.090873	35.327936
1236.390228	129667.908984	35.332954
1238.169578	129878.845871	35.337972
1239.115726	130086.453383	35.342989
1240.301946	130303.211767	35.348007
1241.425461	130515.925768	35.353024
1242.678728	130724.562356	35.358042
1243.842916	130944.929071	35.363060
1244.519551	131163.301714	35.368077
1246.002960	131381.410949	35.373095
1246.860400	131608.033817	35.378112
1248.443806	131838.844284	35.383130
1249.491358	132064.055958	35.388148
1250.392019	132306.130064	35.393165
1251.794266	132531.487086	35.398183
1252.435351	132785.031689	35.403200
1253.676264	133022.488876	35.408218
1254.925452	133262.596040	35.413236
1256.248733	133519.414522	35.418253
1257.357889	133762.021502	35.423271
1258.786014	134015.618345	35.428288
1260.295956	134261.875087	35.433306
1261.916566	134498.111491	35.438324
1263.779529	134732.165433	35.443341
1265.256756	134951.681387	35.448359
1266.824773	135185.383289	35.453376
1268.181351	135414.089575	35.458394
1270.252822	135626.813889	35.463412
1270.894362	135859.360497	35.468429
1272.326680	136072.894387	35.473447
1273.268818	136299.496868	35.478464
1274.387095	136529.709625	35.483482
1276.120318	136755.812055	35.488500
1276.853701	136990.011704	35.493517
1278.273200	137214.522589	35.498535
1279.223078	137443.324926	35.503552
1280.481641	137678.453771	35.508570
1281.559521	137910.090226	35.513588
1282.648508	138155.217572	35.518605
1284.338339	138386.194588	35.523623
1285.285813	138629.003777	35.528640
1286.424071	138868.510584	35.533658
1287.555451	139113.168342	35.538676
1288.857290	139367.093217	35.543693
1290.139932	139607.797728	35.548711
1291.348641	139850.532738	35.553728
1292.448238	140080.201913	35.558746
1293.708523	140309.325194	35.563764
1294.931818	140559.873845	35.568781
1296.122656	140784.675363	35.573799
1297.400836	141021.712995	35.578816
1298.840293	141274.448885	35.583834
1299.987999	141518.169649	35.588852
1300.936970	141774.683240	35.593869
1302.537100	142021.918771	35.598887
1303.362055	142270.556838	35.603904
1304.818409	142528.003526	35.608922
1305.975679	142781.369134	35.613940
1307.160087	143041.744760	35.618957
1308.752398	143299.300557	35.623975
1309.612208	143562.855203	35.628992
1310.986841	143831.700729	35.634010
1312.517834	144105.708381	35.639028
1313.510548	144375.371564	35.644045
1314.612867	144642.177212	35.649063
1315.843351	144917.345785	35.654080
1317.315165	145202.012183	35.659098
1318.703736	145474.646821	35.664116
1320.383978	145758.838002	35.669133
1321.391408	146022.156950	35.674151
1322.961084	146305.458148	35.679168
1324.222795	146577.399784	35.684186
1325.935376	146849.748196	35.689204
1326.792902	147145.403974	35.694221
1328.233009	147422.914453	35.699239
1329.635768	147714.955557	35.704256
1330.847413	148017.114814	35.709274
1331.892576	148297.350188	35.714292
1333.423506	148573.661436	35.719309
1335.232287	148863.320932	35.724327
1337.120434	149140.095218	35.729344
1338.966330	149416.003589	35.734362
1340.112830	149672.310411	35.739380
1341.648047	149961.949038	35.744397
1343.027566	150219.982722	35.749415
1344.651960	150498.384861	35.754432
1345.232338	150766.515993	35.759450
1347.057797	151036.921991	35.764468
1348.426604	151302.829015	35.769485
1350.769828	151558.220620	35.774503
1352.311936	151819.433681	35.779520
1353.440328	152068.909985	35.784538
1355.023258	152308.238485	35.789556
1355.791305	152569.424176	35.794573
1357.247459	152833.373286	35.799591
1358.510822	153087.729340	35.804608
1359.290825	153359.269123	35.809626
1360.792676	153617.710404	35.814644
1361.839796	153890.945982	35.819661
1363.025994	154156.434333	35.824679
1364.656250	154407.399877	35.829696
1365.993451	154653.571343	35.834714
1367.823668	154911.470123	35.839732
1368.278980	155155.727897	35.844749
1370.225783	155405.465783	35.849767
1371.313587	155668.481962	35.854784
1372.453396	155938.100259	35.859802
1373.865476	156197.499675	35.864820
1374.925133	156460.538516	35.869837
1375.914784	156729.743775	35.874855
1377.546051	157007.886210	35.879872
1378.784488	157281.251641	35.884890
1380.325741	157546.625443	35.889908
1381.135109	157838.577346	35.894925
1382.501662	158128.697905	35.899943
1383.780640	158421.905641	35.904960
1384.658306	158712.684867	35.909978
1386.472304	158997.875944	35.914996
1387.943439	159292.376358	35.920013
1389.607360	159585.234613	35.925031
1390.783159	159893.314069	35.930048
1391.841853	160183.501629	35.935066
1393.447066	160470.489284	35.940084
1395.442897	160776.988506	35.945101
1397.131141	161058.104409	35.950119
1398.777812	161347.806004	35.955136
1400.672071	161639.180008	35.960154
1402.602278	161900.492871	35.965172
1403.814371	162179.160122	35.970189
1405.357819	162461.616863	35.975207
1407.509386	162701.403609	35.980224
1409.175859	162960.408099	35.985242
1410.763346	163221.939878	35.990260
1411.839886	163493.393940	35.995277
1413.522455	163754.608128	36.000295
1414.522356	164007.693361	36.005312
1415.399540	164282.295048	36.010330
1416.652843	164550.109229	36.015348
1417.596949	164831.212021	36.020365
1419.012586	165118.415218	36.025383
1419.980017	165409.922294	36.030400
1420.617453	165712.983731	36.035418
1422.329893	166009.138169	36.040436
1423.321057	166319.629560	36.045453
1424.687936	166622.991029	36.050471
1425.910117	166940.020040	36.055488
1427.439223	167252.379886	36.060506
1428.842376	167554.561285	36.065524
1430.632017	167873.098521	36.070541
1432.059022	168181.104376	36.075559
1434.241090	168477.905143	36.080576
1436.375245	168780.109090	36.085594
1438.283419	169057.152036	36.090612
1439.950100	169338.527093	36.095629
1441.720214	169618.122265	36.100647
1442.845958	169886.433881	36.105664
1444.111380	170145.497536	36.110682
1445.506736	170394.972111	36.115700
1446.848473	170661.626861	36.120717
1447.797956	170929.923824	36.125735
1449.101087	171211.753013	36.130752
1450.147883	171496.470368	36.135770
1451.333685	171774.414346	36.140788
1451.771002	172081.650699	36.145805
1452.882669	172380.664348	36.150823
1454.016781	172687.848765	36.155840
1455.379122	173013.321442	36.160858
1456.679135	173338.261258	36.165876
1458.179321	173662.724797	36.170893
1459.532085	173985.946617	36.175911
1461.581206	174300.231113	36.180928
1463.519118	174632.900693	36.185946
1465.052381	174941.947276	36.190964
1466.460593	175270.891725	36.195981
1467.248897	175606.252036	36.200999
1468.833899	175933.495317	36.206016
1470.533185	176268.171094	36.211034
1472.205676	176584.945798	36.216052
1473.675123	176917.406085	36.221069
1475.597502	177250.704832	36.226087
1477.254435	177574.113447	36.231104
1478.499981	177907.037301	36.236122
1480.113230	178232.653227	36.241140
1481.535280	178569.853729	36.246157
1482.750095	178899.971561	36.251175
1484.043318	179224.506152	36.256192
1485.475127	179579.544117	36.261210
1487.260557	179912.997590	36.266228
1488.303691	180267.662448	36.271245
1489.952757	180620.728245	36.276263
1491.480479	180961.936789	36.281280
1492.738894	181311.989666	36.286298
1494.094313	181660.010047	36.291316
1495.744155	182007.106462	36.296333
1497.426748	182355.811493	36.301351
1499.350131	182701.469277	36.306368
1500.821098	183051.725419	36.311386
1502.595851	183386.027161	36.316404
1504.638992	183740.086561	36.321421
1505.962768	184069.481107	36.326439
1507.743956	184401.020668	36.331456
1509.039919	184746.925453	36.336474
1510.453132	185087.062075	36.341492
1512.077980	185437.751059	36.346509
1513.292134	185776.961137	36.351527
1514.615375	186139.536627	36.356544
1516.121298	186493.260847	36.361562
1517.534724	186837.939529	36.366580
1518.542543	187191.055058	36.371597
1520.226953	187526.856346	36.376615
1521.858692	187928.869004	36.381632
1522.898466	188281.465131	36.386650
1524.275212	188625.475049	36.391668
1526.051128	188962.728654	36.396685
1527.731057	189293.323252	36.401703
1528.989145	189636.762615	36.406720
1530.706811	189973.841410	36.411738
1532.013839	190318.228340	36.416756
1533.884058	190673.425676	36.421773
1534.992189	191016.276389	36.426791
1536.849556	191359.521279	36.431808
1538.162590	191710.579784	36.436826
1539.715826	192060.850138	36.441844
1541.374623	192419.673617	36.446861
1543.077285	192786.362672	36.451879
1544.144582	193134.881304	36.456896
1545.807459	193506.672119	36.461914
1547.331375	193861.019904	36.466932
1549.172970	194224.291003	36.471949
1550.358615	194592.322960	36.476967
1551.896524	194956.386434	36.481984
1553.149992	195330.466746	36.487002
1554.562612	195702.985737	36.492020
1556.273070	196076.611165	36.497037
1557.760769	196467.098928	36.502055
1559.600807	196833.622032	36.507072
1561.558551	197202.501139	36.512090
1563.270224	197573.163713	36.517108
1565.228264	197937.438009	36.522125
1566.903957	198319.258031	36.527143
1568.671557	198668.904521	36.532160
1570.077733	199037.354523	36.537178
1571.883572	199407.667924	36.542196
1573.610629	199775.127312	36.547213
1575.025657	200144.838493	36.552231
1576.731317	200504.293702	36.557248
1578.100485	200880.110901	36.562266
1579.478901	201246.050326	36.567284
1581.045453	201629.138262	36.572301
1582.247478	202013.788794	36.577319
1584.039981	202391.801311	36.582336
1585.039375	202776.160312	36.587354
1586.107055	203161.106348	36.592372
1587.870069	203557.020010	36.597389
1589.116250	203963.981899	36.602407
1590.529874	204355.947115	36.607424
1592.147470	204770.607754	36.612442
1593.516830	205174.723368	36.617460
1595.083714	205582.959341	36.622477
1597.026303	205993.164733	36.627495
1599.279517	206393.186332	36.632512
1600.884436	206798.374531	36.637530
1602.323455	207197.942609	36.642548
1604.476023	207592.171716	36.647565
1606.134539	207998.474059	36.652583
1608.026728	208369.565015	36.657600
1609.563603	208743.664341	36.662618
1611.702086	209104.303998	36.667636
1613.053249	209469.219478	36.672653
1614.418447	209839.670509	36.677671
1616.372255	210188.587778	36.682688
1618.133027	210553.666291	36.687706
1619.751356	210916.561175	36.692724
1621.345806	211274.001315	36.697741
1622.823428	211648.275607	36.702759
1624.268602	212013.617257	36.707776
1626.075134	212398.809863	36.712794
1628.025422	212758.582286	36.717812
1629.839247	213123.560502	36.722829
1630.987897	213495.689033	36.727847
1632.740670	213868.883949	36.732864
1634.085083	214254.747407	36.737882
1635.130679	214643.025528	36.742900
1637.402240	215012.555048	36.747917
1639.194561	215391.336603	36.752935
1640.911115	215765.713326	36.757952
1642.530609	216149.505355	36.762970
1645.000884	216511.590227	36.767988
1646.925979	216876.436490	36.773005
1648.264329	217236.761944	36.778023
1650.439636	217607.612802	36.783040
1651.823448	217973.977867	36.788058
1653.333058	218340.373481	36.793076
1655.066464	218712.548373	36.798093
1656.363090	219084.977078	36.803111
1658.338921	219463.183396	36.808128
1659.656441	219846.481854	36.813146
1660.973860	220230.518231	36.818164
1662.229310	220611.442433	36.823181
1664.020816	221007.464947	36.828199
1665.618452	221386.936245	36.833216
1666.927034	221783.120257	36.838234
1668.379252	222200.413420	36.843252
1669.623130	222604.866111	36.848269
1671.267899	223031.196897	36.853287
1672.543689	223446.568817	36.858304
1673.862313	223878.317718	36.863322
1675.813510	224302.492309	36.868340
1677.426104	224729.875866	36.873357
1679.085529	225167.793887	36.878375
1680.514732	225603.212761	36.883392
1682.258389	226044.776949	36.888410
1683.739726	226481.713816	36.893428
1685.767567	226923.003676	36.898445
1687.093526	227370.511168	36.903463
1689.034081	227806.611681	36.908480
1690.376192	228267.505395	36.913498
1692.028578	228715.240709	36.918516
1694.262069	229157.442201	36.923533
1695.402982	229609.890703	36.928551
1697.373654	230031.285597	36.933568
1699.586222	230462.622885	36.938586
1701.138155	230890.823052	36.943604
1703.521682	231294.928778	36.948621
1705.232159	231710.251022	36.953639
1706.640326	232115.135298	36.958656
1708.427599	232544.747456	36.963674
1710.000548	232972.492268	36.968692
1711.929042	233388.848241	36.973709
1713.438050	233819.908280	36.978727
1715.202407	234244.905489	36.983744
1716.548995	234668.832090	36.988762
1718.199800	235102.893719	36.993780
1719.834518	235531.497709	36.998797
1721.896989	235977.607565	37.003815
1723.406918	236413.575988	37.008832
1725.047404	236846.932020	37.013850
1726.749627	237289.372332	37.018868
1728.797172	237724.108473	37.023885
1730.771589	238168.866446	37.028903
1732.820983	238604.518510	37.033920
1734.732557	239045.046823	37.038938
1736.437347	239481.597793	37.043956
1738.823182	239907.948334	37.048973
1740.873067	240327.854091	37.053991
1742.717193	240741.495961	37.059008
1744.687357	241170.790254	37.064026
1746.464212	241593.513671	37.069044
1748.193576	241993.612220	37.074061
1749.612883	242432.909750	37.079079
1751.347527	242850.739611	37.084096
1753.456983	243283.188674	37.089114
1754.992155	243699.199455	37.094132
1757.086100	244110.745932	37.099149
1758.977429	244532.793525	37.104167
1761.390088	244949.011440	37.109184
1762.878198	245364.524325	37.114202
1764.251389	245786.408059	37.119220
1766.457111	246201.418090	37.124237
1767.726503	246616.969788	37.129255
1769.412238	247046.346085	37.134272
1771.320827	247464.050150	37.139290
1773.212451	247887.066734	37.144308
1775.190702	248296.351274	37.149325
1777.183103	248714.677212	37.154343
1779.028786	249128.532257	37.159360
1780.313069	249542.534466	37.164378
1782.033806	249963.600575	37.169396
1784.197314	250385.327924	37.174413
1785.752078	250808.912501	37.179431
1787.420887	251220.741592	37.184448
1789.743108	251636.777667	37.189466
1791.393997	252059.355795	37.194484
1793.428103	252476.610121	37.199501
1795.445831	252886.500515	37.204519
1796.904488	253267.654107	37.209536
1799.044938	253665.381081	37.214554
1800.777027	254059.901020	37.219572
1802.577491	254437.668662	37.224589
1803.713427	254823.120214	37.229607
1805.107839	255223.007444	37.234624
1806.915788	255628.361891	37.239642
1808.192031	256037.668625	37.244660
1809.629670	256450.224794	37.249677
1810.867657	256880.546566	37.254695
1812.001350	257308.676094	37.259712
1813.994377	257747.429556	37.264730
1815.745879	258194.632746	37.269748
1818.067870	258634.320545	37.274765
1819.586254	259090.022713	37.279783
1821.473190	259540.022212	37.284800
1823.205386	259994.569807	37.289818
1824.394527	260460.971797	37.294836
1826.489786	260931.105273	37.299853
1827.668622	261406.221880	37.304871
1829.223173	261896.947688	37.309888
1830.871812	262374.701514	37.314906
1832.254602	262875.820537	37.319924
1834.368426	263374.629472	37.324941
1836.108346	263876.448715	37.329959
1837.850060	264383.500235	37.334976
1839.745125	264902.743887	37.339994
1841.312511	265422.220872	37.345012
1842.917880	265940.801684	37.350029
1844.490824	266482.935937	37.355047
1846.012339	267029.676208	37.360064
1847.944443	267563.821892	37.365082
1849.407324	268121.671692	37.370100
1851.343154	268675.451492	37.375117
1852.881726	269232.905535	37.380135
1854.591928	269808.720809	37.385152
1856.624664	270365.402479	37.390170
1857.581655	270956.865437	37.395188
1859.232688	271544.067850	37.400205
1860.968921	272138.417938	37.405223
1863.342638	272735.807553	37.410240
1865.363675	273316.236521	37.415258
1867.415841	273914.745229	37.420276
1869.416593	274518.570291	37.425293
1871.052352	275108.383404	37.430311
1873.624024	275708.678342	37.435328
1876.185033	276285.933802	37.440346
1878.188151	276872.072167	37.445364
1880.102822	277461.780231	37.450381
1881.961987	278049.260667	37.455399
1884.050183	278627.580912	37.460416
1886.392747	279215.330669	37.465434
1887.840168	279807.626103	37.470452
1889.682489	280382.655218	37.475469
1891.649247	280947.271969	37.480487
1893.293891	281510.316244	37.485504
1895.081526	282073.537349	37.490522
1896.888916	282636.600702	37.495540
1899.629323	283180.832702	37.500557
1902.457755	283715.649379	37.505575
1905.243837	284235.357902	37.510592
1907.581909	284761.770836	37.515610
1909.757010	285279.802119	37.520628
1912.302516	285766.550854	37.525645
1914.598966	286263.830911	37.530663
1916.238729	286766.733386	37.535680
1917.939535	287250.395526	37.540698
1919.462805	287769.849791	37.545716
1921.534789	288267.491058	37.550733
1923.405547	288785.586444	37.555751
1925.119069	289286.891875	37.560768
1927.571667	289786.240109	37.565786
1929.377632	290303.705315	37.570804
1931.501453	290802.394453	37.575821
1933.183350	291315.482415	37.580839
1934.790699	291819.995908	37.585856
1937.255873	292318.645662	37.590874
1939.152808	292825.289577	37.595892
1941.076803	293330.174062	37.600909
1942.902041	293842.311849	37.605927
1944.858669	294358.615585	37.610944
1946.887307	294871.094747	37.615962
1948.128068	295406.056943	37.620980
1949.633913	295926.011417	37.625997
1951.338806	296460.863458	37.631015
1952.812832	297004.514570	37.636032
1954.716594	297556.597612	37.641050
1956.417111	298105.537632	37.646068
1957.982380	298669.710981	37.651085
1959.973992	299238.430509	37.656103
1961.329500	299809.185667	37.661120
1963.405135	300379.128503	37.666138
1964.776864	300979.283852	37.671156
1967.062590	301558.148711	37.676173
1969.057218	302146.354906	37.681191
1970.659696	302749.862300	37.686208
1972.683096	303353.572964	37.691226
1974.655354	303972.246621	37.696244
1976.222146	304586.032958	37.701261
1978.111999	305212.660750	37.706279
1979.467384	305843.895726	37.711296
1981.856603	306456.892886	37.716314
1984.107271	307089.235012	37.721332
1985.879518	307704.715476	37.726349
1988.315906	308338.666722	37.731367
1990.869561	308966.167966	37.736384
1993.425395	309566.669417	37.741402
1995.413393	310179.833508	37.746420
1997.626177	310784.371020	37.751437
1999.291814	311388.463995	37.756455
2001.315781	311983.247490	37.761472
2003.860636	312559.679176	37.766490
2005.718403	313142.699120	37.771508
2007.362162	313718.564715	37.776525
2009.625733	314294.319684	37.781543
2011.896938	314876.112136	37.786560
2014.072484	315450.146024	37.791578
2016.455153	316027.237609	37.796596
2018.438630	316603.376942	37.801613
2020.583610	317180.372503	37.806631
2022.452991	317756.013725	37.811648
2024.209614	318329.561789	37.816666
2026.068754	318921.445190	37.821684
2028.047281	319502.308552	37.826701
2030.278543	320089.928221	37.831719
2032.409418	320682.917093	37.836736
2034.682186	321268.411452	37.841754
2036.085074	321871.162027	37.846772
2037.973279	322470.294632	37.851789
2040.024208	323073.151279	37.856807
2041.472957	323684.635795	37.861824
2043.202904	324307.161091	37.866842
2045.239096	324941.611092	37.871860
2046.914311	325568.524940	37.876877
2049.174455	326204.903487	37.881895
2051.384680	326830.671520	37.886912
2053.654708	327469.091041	37.891930
2055.432390	328100.910812	37.896948
2057.228237	328754.908813	37.901965
2059.244344	329405.967505	37.906983
2060.882929	330062.211279	37.912000
2063.475880	330713.359191	37.917018
2065.465585	331372.776830	37.922036
2067.202451	332028.751927	37.927053
2069.642009	332691.173706	37.932071
2072.273325	333350.939873	37.937088
2075.156486	333991.768618	37.942106
2077.421854	334636.807491	37.947124
2080.006139	335259.649005	37.952141
2083.062915	335882.300717	37.957159
2085.275822	336508.160601	37.962176
2088.392835	337105.403744	37.967194
2090.531180	337728.672301	37.972212
2092.459551	338336.003456	37.977229
2094.647422	338928.992677	37.982247
2096.547964	339532.785868	37.987264
2098.622919	340133.851386	37.992282
2100.173719	340749.187274	37.997300
2101.381310	341362.061338	38.002317
2103.858642	341977.070886	38.007335
2105.404412	342599.642864	38.012352
2107.561490	343225.046225	38.017370
2109.501689	343864.031087	38.022388
2111.074603	344489.923571	38.027405
2113.191219	345120.942713	38.032423
2115.054766	345750.778325	38.037440
2117.283686	346359.326601	38.042458
2118.721307	346976.249857	38.047476
2120.400546	347591.727612	38.052493
2122.276340	348236.829245	38.057511
2123.821974	348884.718688	38.062528
2125.892310	349530.174292	38.067546
2127.695319	350188.734793	38.072564
2129.611782	350870.459308	38.077581
2131.289159	351540.287601	38.082599
2133.567947	352227.130655	38.087616
2135.878860	352899.671349	38.092634
2138.199680	353572.960896	38.097652
2140.974872	354255.474105	38.102669
2143.691232	354919.895113	38.107687
2146.152420	355598.735503	38.112704
2148.256560	356267.958878	38.117722
2150.340885	356952.042683	38.122740
2152.595018	357624.770232	38.127757
2155.138907	358298.984669	38.132775
2157.245244	358972.704433	38.137792
2159.795612	359643.546154	38.142810
2162.128923	360318.117617	38.147828
2164.105212	360987.182653	38.152845
2166.418065	361656.280163	38.157863
2168.252022	362340.846723	38.162880
2170.723435	363015.880584	38.167898
2173.147172	363695.223203	38.172916
2175.025402	364385.707060	38.177933
2177.481350	365062.178582	38.182951
2179.699269	365747.404620	38.187968
2181.868894	366426.690754	38.192986
2184.218730	367110.321846	38.198004
2186.090451	367800.388594	38.203021
2188.460323	368474.174714	38.208039
2190.185959	369173.092692	38.213056
2192.361928	369876.384143	38.218074
2194.540973	370566.650156	38.223092
2196.204013	371264.523708	38.228109
2198.798222	371969.630032	38.233127
2200.602698	372686.295294	38.238144
2202.957095	373391.693122	38.243162
2204.693134	374116.608447	38.248180
2206.220891	374850.293368	38.253197
2208.801047	375576.504629	38.258215
2210.973015	376308.678863	38.263232
2212.762002	377044.224749	38.268250
2215.012936	377791.745894	38.273268
2217.008191	378547.306961	38.278285
2218.830354	379306.886857	38.283303
2221.019881	380068.262904	38.288320
2222.905919	380830.586059	38.293338
2224.965700	381607.440743	38.298356
2226.803323	382395.115730	38.303373
2229.446862	383161.134023	38.308391
2231.327791	383925.565818	38.313408
2233.690324	384681.834981	38.318426
2236.148529	385436.219124	38.323444
2237.572499	386205.820609	38.328461
2240.327362	386956.061475	38.333479
2243.114390	387706.887210	38.338496
2246.279231	388444.296499	38.343514
2249.236520	389184.816184	38.348532
2251.637036	389930.989753	38.353549
2254.526014	390648.520401	38.358567
2256.564278	391378.244607	38.363584
2259.199840	392102.323593	38.368602
2261.613681	392828.577398	38.373620
2263.573218	393554.485692	38.378637
2265.673414	394283.570935	38.383655
2267.729879	395023.568803	38.388672
2269.899310	395753.796990	38.393690
2272.103268	396489.272261	38.398708
2274.364531	397236.959213	38.403725
2276.715270	397969.660275	38.408743
2279.254405	398729.146031	38.413760
2281.525403	399476.038249	38.418778
2283.925507	400217.567577	38.423796
2286.730311	400946.212367	38.428813
2289.172302	401682.577690	38.433831
2291.164965	402429.084663	38.438848
2293.877266	403165.744757	38.443866
2296.196201	403904.707416	38.448884
2298.082930	404653.756878	38.453901
2300.568173	405390.523067	38.458919
2302.733668	406133.860150	38.463936
2305.299200	406891.041685	38.468954
2307.572366	407632.089973	38.473972
2309.830876	408381.631783	38.478989
2311.613643	409148.028329	38.484007
2313.494157	409905.875179	38.489024
2315.395986	410684.618835	38.494042
2317.691902	411454.179126	38.499060
2319.784700	412261.110258	38.504077
2321.808349	413043.232995	38.509095
2324.098873	413840.583683	38.514112
2326.255946	414650.114174	38.519130
2328.107173	415472.283182	38.524148
2329.699591	416295.280358	38.529165
2332.087666	417107.099327	38.534183
2334.362687	417940.055698	38.539200
2336.673712	418781.562315	38.544218
2339.068330	419615.430174	38.549236
2341.074910	420482.885094	38.554253
2343.362455	421324.664256	38.559271
2345.852322	422185.064745	38.564288
2348.210546	423038.520650	38.569306
2351.315411	423882.148256	38.574324
2353.344570	424731.904815	38.579341
2356.096458	425570.318929	38.584359
2358.259355	426405.412428	38.589376
2360.229745	427234.333353	38.594394
2362.984170	428053.725987	38.599412
2365.172751	428881.691429	38.604429
2367.782138	429706.063035	38.609447
2370.367219	430538.002523	38.614464
2372.940899	431354.223164	38.619482
2375.981361	432168.563782	38.624500
2378.168094	432985.400414	38.629517
2381.121888	433782.743448	38.634535
2383.212256	434596.097614	38.639552
2385.968854	435410.320998	38.644570
2388.954522	436219.769638	38.649588
2391.247397	437031.584828	38.654605
2393.610630	437834.452679	38.659623
2396.161017	438634.932093	38.664640
2398.749192	439440.486696	38.669658
2401.433965	440241.290012	38.674676
2403.535250	441043.631233	38.679693
2405.821181	441860.684702	38.684711
2408.383762	442670.931744	38.689728
2410.286966	443491.783856	38.694746
2412.689016	444301.542189	38.699764
2415.009094	445132.934623	38.704781
2416.936612	445966.233549	38.709799
2419.280010	446797.759729	38.714816
2421.656334	447638.807278	38.719834
2424.467779	448474.588182	38.724852
2426.690722	449323.434395	38.729869
2429.040922	450160.491555	38.734887
2431.581518	451016.092848	38.739904
2433.978135	451870.520481	38.744922
2436.677072	452714.191563	38.749940
2438.916163	453578.790040	38.754957
2441.486787	454432.323325	38.759975
2443.731394	455281.882400	38.764992
2446.766024	456143.961179	38.770010
2449.161978	457004.848526	38.775028
2451.498147	457873.191378	38.780045
2453.743964	458727.509221	38.785063
2456.206377	459605.158130	38.790080
2458.105486	460482.965726	38.795098
2460.477578	461362.169973	38.800116
2462.697371	462250.812638	38.805133
2465.109450	463138.169268	38.810151
2467.611318	464033.253223	38.815168
2469.507425	464933.402648	38.820186
2472.177788	465830.244862	38.825204
2474.727540	466744.145633	38.830221
2477.513062	467651.090701	38.835239
2479.886922	468563.368422	38.840256
2482.173439	469477.638345	38.845274
2484.999239	470388.033413	38.850292
2486.989905	471307.216629	38.855309
2489.224333	472217.068670	38.860327
2492.057752	473121.672157	38.865344
2494.269552	474015.983027	38.870362
2497.100895	474900.699635	38.875380
2499.118643	475802.836860	38.880397
2501.503288	476685.119860	38.885415
2504.400007	477574.848190	38.890432
2506.909090	478476.719311	38.895450
2509.945993	479355.883221	38.900468
2512.313914	480253.751310	38.905485
2515.075382	481139.793222	38.910503
2517.574512	482025.583782	38.915520
2520.292819	482922.349695	38.920538
2522.864214	483813.996597	38.925556
2525.277053	484717.993879	38.930573
2528.214869	485605.297886	38.935591
2530.969957	486510.760066	38.940608
2533.066329	487416.792764	38.945626
2535.628162	488317.146985	38.950644
2537.890177	489225.782729	38.955661
2539.644061	490137.182804	38.960679
2542.261430	491057.773389	38.965696
2544.635756	492001.214967	38.970714
2547.413563	492938.833764	38.975732
2549.517218	493888.625429	38.980749
2552.118373	494820.620493	38.985767
2555.319393	495776.929733	38.990784
2557.230058	496728.360426	38.995802
2559.646687	497687.822543	39.000820
2561.917726	498652.752434	39.005837
2564.432745	499622.325769	39.010855
2566.943344	500602.081367	39.015872
2569.353284	501585.275720	39.020890
2571.815008	502570.419473	39.025908
2574.454012	503566.516825	39.030925
2576.984821	504554.100642	39.035943
2579.886529	505555.174232	39.040960
2582.162699	506575.551760	39.045978
2584.632465	507586.555352	39.050996
2586.892407	508602.118255	39.056013
2589.640553	509606.040215	39.061031
2592.536921	510622.625493	39.066048
2594.960710	511647.441416	39.071066
2598.577327	512659.538645	39.076084
2601.254498	513681.608257	39.081101
2604.162510	514689.058973	39.086119
2607.189354	515689.772938	39.091136
2609.141821	516700.733030	39.096154
2612.341876	517706.073285	39.101172
2614.756556	518714.756470	39.106189
2617.488414	519734.199774	39.111207
2619.829760	520746.186709	39.116224
2622.500323	521754.927115	39.121242
2625.310230	522766.447137	39.126260
2628.977659	523766.119320	39.131277
2632.085289	524744.670370	39.136295
2635.125966	525693.258339	39.141312
2637.949011	526636.083005	39.146330
2640.581841	527567.954732	39.151348
2642.699171	528504.990935	39.156365
2645.335534	529438.153543	39.161383
2647.963472	530371.660935	39.166400
2650.175587	531312.881032	39.171418
2652.414101	532270.997613	39.176436
2654.771694	533233.711141	39.181453
2657.340553	534199.545280	39.186471
2659.631356	535164.053823	39.191488
2661.703698	536150.272378	39.196506
2664.093512	537143.362438	39.201524
2666.434731	538139.510889	39.206541
2668.777466	539161.849759	39.211559
2671.441758	540174.351131	39.216576
2673.300553	541217.449651	39.221594
2675.805825	542254.877892	39.226612
2677.489676	543317.918223	39.231629
2680.155942	544393.985825	39.236647
2683.250070	545478.344716	39.241664
2685.254465	546566.525502	39.246682
2687.626620	547661.797315	39.251700
2690.320484	548770.450063	39.256717
2692.950379	549887.921299	39.261735
2695.472496	551015.120728	39.266752
2698.055013	552154.680608	39.271770
2700.338147	553296.858970	39.276788
2703.261184	554451.645110	39.281805
2705.388990	555621.893405	39.286823
2708.364908	556792.095026	39.291840
2711.242930	557964.370456	39.296858
2714.011733	559131.336255	39.301876
2717.274298	560312.329194	39.306893
2720.069393	561481.090955	39.311911
2722.910876	562661.541987	39.316928
2725.561549	563850.957328	39.321946
2728.329576	565027.389322	39.326964
2731.258293	566217.794643	39.331981
2734.067698	567412.477618	39.336999
2737.466996	568592.290658	39.342016
2740.337639	569786.038333	39.347034
2743.495298	570962.259686	39.352052
2746.152961	572145.181581	39.357069
2748.709079	573325.902213	39.362087
2752.233520	574495.107328	39.367104
2754.923212	575680.650584	39.372122
2757.871920	576842.208596	39.377140
2760.781093	578022.825500	39.382157
2763.010948	579204.197913	39.387175
2766.282631	580367.124587	39.392192
2769.382114	581537.090925	39.397210
2772.869113	582698.555599	39.402228
2776.298174	583837.759237	39.407245
2779.198482	584969.075502	39.412263
2782.366432	586070.715548	39.417280
2784.981544	587166.134020	39.422298
2788.139627	588251.085557	39.427316
2791.048625	589322.350391	39.432333
2793.661018	590400.384211	39.437351
2796.531818	591474.618335	39.442368
2799.047544	592553.174130	39.447386
2801.666161	593638.125903	39.452404
2804.194435	594719.937365	39.457421
2806.728462	595812.616504	39.462439
2809.256989	596915.009980	39.467456
2811.640025	598025.636307	39.472474
2814.461098	599133.577738	39.477492
2817.056447	600248.761005	39.482509
2819.195092	601389.195046	39.487527
2822.164950	602516.459112	39.492544
2824.749694	603655.439716	39.497562
2827.669947	604816.769753	39.502580
2830.675618	605966.807107	39.507597
2832.939633	607125.110014	39.512615
2836.038616	608295.558727	39.517632
2838.518989	609475.745943	39.522650
2840.843759	610659.936792	39.527668
2843.823074	611830.886090	39.532685
2846.692651	613024.484890	39.537703
2849.676061	614230.086374	39.542720
2852.777038	615427.086109	39.547738
2855.607804	616628.750827	39.552756
2858.835091	617837.513981	39.557773
2861.638617	619045.215826	39.562791
2864.310231	620254.505110	39.567808
2867.044093	621476.890883	39.572826
2870.208810	622709.357278	39.577844
2872.716992	623934.350501	39.582861
2875.203809	625178.139597	39.587879
2878.281891	626410.144746	39.592896
2880.887152	627661.015804	39.597914
2883.517449	628917.627267	39.602932
2886.178918	630184.668882	39.607949
2888.781364	631455.362076	39.612967
2891.710454	632730.188153	39.617984
2894.312676	634015.395756	39.623002
2897.277456	635309.864579	39.628020
2900.412917	636598.254365	39.633037
2903.143146	637909.702793	39.638055
2905.841722	639205.125453	39.643072
2908.633471	640512.688775	39.648090
2911.836478	641817.919620	39.653108
2914.954235	643130.776761	39.658125
2917.720201	644438.039150	39.663143
2921.096488	645745.576368	39.668160
2924.383008	647056.847018	39.673178
2927.006094	648369.454921	39.678196
2930.411680	649675.925908	39.683213
2933.593891	650987.495384	39.688231
2935.989192	652264.549079	39.693248
2938.373056	653535.910097	39.698266
2940.625364	654812.757755	39.703284
2944.085834	656093.914230	39.708301
2946.230207	657387.725849	39.713319
2949.256050	658678.825139	39.718336
2952.036872	659980.746621	39.723354
2955.182524	661275.362321	39.728372
2958.121744	662570.486307	39.733389
2960.821950	663889.760404	39.738407
2963.821575	665197.705985	39.743424
2966.934355	666523.063759	39.748442
2969.920341	667853.530864	39.753460
2973.000056	669173.897771	39.758477
2975.724979	670526.861130	39.763495
2978.351317	671859.410402	39.768512
2981.546270	673213.795327	39.773530
2983.943471	674572.494039	39.778548
2987.110360	675922.761882	39.783565
2989.584496	677314.791325	39.788583
2992.418116	678698.947865	39.793600
2994.961881	680097.302035	39.798618
2997.769920	681509.354566	39.803636
3000.916779	682918.200861	39.808653
3003.910151	684345.872294	39.813671
3006.734329	685768.631437	39.818688
3009.493960	687203.686049	39.823706
3012.178961	688650.683696	39.828724
3015.450467	690110.844558	39.833741
3018.082853	691574.299100	39.838759
3021.181344	693043.584307	39.843776
3024.899973	694512.916779	39.848794
3027.846413	695977.475278	39.853812
3031.067866	697448.039645	39.858829
3034.345623	698932.723421	39.863847
3037.425821	700392.605066	39.868864
3040.779998	701881.580993	39.873882
3043.401925	703373.498018	39.878900
3046.630577	704860.496171	39.883917
3049.280003	706350.357466	39.888935
3052.268702	707848.865046	39.893952
3055.209917	709361.476146	39.898970
3058.104686	710872.291612	39.903988
3061.091013	712377.674711	39.909005
3064.027073	713895.515684	39.914023
3067.788110	715405.817285	39.919040
3071.050788	716918.157790	39.924058
3074.201181	718437.612807	39.929076
3078.062677	719935.553940	39.934093
3081.479774	721442.644416	39.939111
3084.734723	722937.623954	39.944128
3087.900927	724434.323877	39.949146
3091.438267	725929.007084	39.954164
3094.696143	727408.890171	39.959181
3098.083257	728879.393315	39.964199
3101.350271	730309.548355	39.969216
3104.844078	731732.350510	39.974234
3107.669626	733149.930383	39.979252
3110.801910	734554.324403	39.984269
3114.142573	735970.478180	39.989287
3117.677895	737370.014559	39.994304
3120.848403	738767.048005	39.999322
3123.831594	740173.732189	40.004340
3126.741129	741579.093319	40.009357
3129.351656	742991.305570	40.014375
3132.790988	744396.860979	40.019392
3136.126317	745821.355321	40.024410
3139.136610	747230.564578	40.029428
3142.385888	748648.543379	40.034445
3144.528712	750078.914914	40.039463
3147.802093	751503.607239	40.044480
3150.979469	752957.254143	40.049498
3154.140674	754398.713011	40.054516
3157.397617	755838.603537	40.059533
3159.948923	757306.740245	40.064551
3162.987362	758766.439650	40.069568
3166.070077	760241.937283	40.074586
3168.590229	761732.490278	40.079604
3171.649650	763220.048883	40.084621
3174.489032	764730.900945	40.089639
3177.245469	766258.371494	40.094656
3180.490082	767792.866087	40.099674
3183.279959	769333.115166	40.104692
3186.158881	770880.642342	40.109709
3188.928473	772451.193103	40.114727
3191.817328	774014.855781	40.119744
3195.190277	775605.496405	40.124762
3197.990098	777200.010289	40.129780
3201.627705	778786.571205	40.134797
3205.384926	780380.122736	40.139815
3208.837394	781981.565260	40.144832
3212.573875	783569.066307	40.149850
3215.617516	785172.905359	40.154868
3219.287935	786764.658640	40.159885
3222.411754	788366.587030	40.164903
3225.750216	789966.793001	40.169920
3229.059964	791549.691287	40.174938
3231.643974	793157.236078	40.179956
3235.505327	794758.073060	40.184973
3239.286352	796366.045962	40.189991
3242.241719	797967.131726	40.195008
3245.517712	799566.667186	40.200026
3249.276115	801176.462658	40.205044
3252.511175	802769.195479	40.210061
3256.019991	804374.713202	40.215079
3258.939066	805964.604506	40.220096
3262.171011	807558.225168	40.225114
3265.232746	809174.465193	40.230132
3268.488442	810784.863322	40.235149
3271.992157	812382.526926	40.240167
3274.922437	813945.632050	40.245184
3278.163313	815518.570069	40.250202
3281.093130	817074.792130	40.255220
3284.404406	818627.413131	40.260237
3287.887938	820204.518826	40.265255
3290.875011	821777.089568	40.270272
3293.985582	823339.414382	40.275290
3297.080340	824920.282928	40.280308
3300.193585	826506.857618	40.285325
3302.962848	828099.779452	40.290343
3305.843549	829697.795611	40.295360
3309.254018	831309.595029	40.300378
3312.265133	832942.481224	40.305396
3315.599825	834570.224666	40.310413
3318.239242	836211.735927	40.315431
3321.528157	837873.875901	40.320448
3324.877996	839527.351778	40.325466
3328.071751	841203.810211	40.330484
3331.001096	842884.049209	40.335501
3334.438711	844569.681641	40.340519
3337.515695	846254.825456	40.345536
3341.685705	847953.899306	40.350554
3345.186511	849655.828568	40.355572
3348.875984	851342.501775	40.360589
3352.514419	853038.817945	40.365607
3355.796481	854741.520394	40.370624
3359.520390	856456.771206	40.375642
3362.809104	858160.463037	40.380660
3366.456488	859861.484815	40.385677
3369.756473	861570.909961	40.390695
3373.044201	863272.296791	40.395712
3376.587570	864990.112612	40.400730
3379.923059	866711.443840	40.405748
3383.142958	868434.139957	40.410765
3386.381088	870159.046156	40.415783
3389.630895	871890.223578	40.420800
3392.836638	873616.840652	40.425818
3395.877453	875370.928155	40.430836
3399.360187	877110.207107	40.435853
3402.806521	878867.918996	40.440871
3405.952175	880622.835269	40.445888
3409.243570	882381.930976	40.450906
3412.591235	884159.698867	40.455924
3416.072896	885924.542528	40.460941
3419.494422	887709.506559	40.465959
3423.014465	889483.095180	40.470976
3426.967749	891254.517560	40.475994
3430.137997	893032.272112	40.481012
3433.874312	894814.867714	40.486029
3437.614251	896588.230791	40.491047
3440.795520	898365.081205	40.496064
3444.791006	900142.001846	40.501082
3447.946954	901918.021379	40.506100
3451.521452	903681.569481	40.511117
3455.143826	905441.607009	40.516122
3458.252200	907151.454671	40.521127
3461.767567	908798.249801	40.526132
3464.664050	910374.128446	40.531136
3468.085129	911886.179368	40.536141
3471.971996	913328.300643	40.541146
3474.733102	914676.941204	40.546151
3477.892047	915953.181825	40.551156
3480.684345	917167.692512	40.556160
3484.015654	918276.293677	40.561165
3486.873799	919320.201824	40.566170
3489.692791	920283.414397	40.571175
3492.046858	921168.739478	40.576180
3494.262143	921987.120392	40.581184
3496.798894	922726.396012	40.586189
3499.018311	923408.335395	40.591194
3500.773666	924026.065366	40.596199
3502.760385	924569.590947	40.601204
3504.408880	925086.405462	40.606208
3506.505560	925511.525864	40.611213
3508.035888	925886.268552	40.616218
3509.346334	926206.549987	40.621223
3511.272394	926491.834994	40.626228
3512.330549	926741.613909	40.631232
3513.469732	926918.074788	40.636237
3514.944398	927063.926720	40.641242
3516.458649	927169.137024	40.646247
3517.545019	927232.155005	40.651252
3518.258881	927262.385891	40.656256
3519.173252	927239.945527	40.661261
3520.167633	927204.332063	40.666266
3521.142086	927146.533152	40.671271
3522.065286	927037.064069	40.676276
3522.803403	926920.227806	40.681280
3523.672035	926756.584799	40.686285
3524.305530	926584.138943	40.691290
3524.715774	926388.477101	40.696295
3525.321279	926164.145221	40.701300
3525.465749	925933.733705	40.706304
3526.366170	925680.027675	40.711309
3526.855337	925407.354779	40.716314
3527.054830	925117.805362	40.721319
3527.636709	924809.436126	40.726324
3527.909457	924495.335732	40.731328
3528.463774	924159.640562	40.736333
3528.649693	923828.120158	40.741338
3528.923284	923466.574607	40.746343
3529.387806	923104.203062	40.751348
3529.335132	922744.875478	40.756352
3529.980818	922351.947680	40.761357
3530.204489	921957.332523	40.766362
3530.285773	921558.097260	40.771367
3530.826598	921144.618052	40.776372
3530.696893	920731.413896	40.781376
3530.540697	920295.484680	40.786381
3531.054868	919873.929776	40.791386
3531.081980	919438.573326	40.796391
3531.620193	918991.069439	40.801396
3531.382465	918546.066194	40.806400
3531.453419	918087.503290	40.811405
3532.197095	917629.267852	40.816410
3531.865355	917166.269365	40.821415
3531.928042	916696.330872	40.826420
3532.225290	916225.926672	40.831424
3532.301806	915737.326588	40.836429
3532.625093	915262.502974	40.841434
3532.230964	914784.679609	40.846439
3532.912280	914286.025965	40.851444
3533.009991	913794.455774	40.856448
3533.022044	913290.240427	40.861453
3532.815463	912784.956471	40.866458
3532.863927	912278.619114	40.871463
3533.052774	911772.403642	40.876468
3533.065613	911268.965262	40.881472
3533.242296	910749.748269	40.886477
3533.547458	910244.431822	40.891482
3533.527269	909722.935269	40.896487
3533.689434	909191.335312	40.901492
3533.921074	908680.201774	40.906496
3533.572418	908134.804388	40.911501
3533.755518	907609.795890	40.916506
3533.691790	907085.840175	40.921511
3533.718271	906543.403248	40.926516
3533.520716	906008.087213	40.931520
3533.662801	905466.971628	40.936525
3533.761356	904936.805798	40.941530
3533.945076	904399.726382	40.946535
3533.740574	903848.094907	40.951540
3533.800355	903318.070801	40.956544
3533.589931	902771.157488	40.961549
3533.958559	902223.705737	40.966554
3533.550603	901675.850381	40.971559
3533.775593	901130.921733	40.976564
3533.651036	900592.080666	40.981568
3533.554063	900045.170881	40.986573
3534.072992	899496.557969	40.991578
3533.675231	898950.944494	40.996583
3533.757266	898384.918377	41.001588
3533.795485	897843.371720	41.006592
3533.928778	897295.285947	41.011597
3534.263693	896738.999014	41.016602
3533.909895	896175.240142	41.021607
3533.705158	895614.491056	41.026612
3533.760778	895062.627419	41.031616
3533.912047	894503.350022	41.036621
3534.511335	893946.260284	41.041626
3534.071821	893390.259687	41.046631
3534.381893	892808.752869	41.051636
3534.175265	892249.894647	41.056640
3534.433108	891675.820964	41.061645
3534.530130	891100.846788	41.066650
3534.356033	890531.662681	41.071655
3534.300187	889958.146710	41.076660
3533.998000	889376.781456	41.081664
3533.498633	888809.996176	41.086669
3533.965018	888236.218675	41.091674
3533.387723	887678.814841	41.096679
3533.853096	887110.826453	41.101684
3533.749665	886546.556072	41.106688
3533.908560	885982.282416	41.111693
3533.923976	885409.170986	41.116698
3533.922285	884835.134481	41.121703
3534.130938	884258.004263	41.126708
3534.107924	883692.376419	41.131712
3533.677740	883117.371392	41.136717
3534.084856	882538.777415	41.141722
3533.691668	881966.653766	41.146727
3533.970111	881381.672049	41.151732
3534.248714	880804.961311	41.156736
3533.800189	880220.761965	41.161741
3533.999566	879642.303023	41.166746
3533.711549	879069.295658	41.171751
3533.923411	878496.146810	41.176756
3533.780893	877914.183934	41.181760
3533.825286	877335.814152	41.186765
3533.932292	876761.447525	41.191770
3534.026975	876182.180138	41.196775
3534.269193	875593.814734	41.201780
3534.019780	875012.746001	41.206784
3533.969772	874415.683974	41.211789
3533.615200	873837.135400	41.216794
3533.653491	873256.232519	41.221799
3533.707995	872668.771374	41.226804
3533.491490	872097.109487	41.231808
3533.820617	871495.905013	41.236813
3533.911670	870910.688771	41.241818
3533.914954	870324.556632	41.246823
3533.982947	869734.668207	41.251828
3533.727789	869147.590988	41.256832
3534.209287	868557.127293	41.261837
3533.990985	867964.297982	41.266842
3533.797241	867367.328410	41.271847
3534.340799	866766.969547	41.276852
3534.198163	866185.213378	41.281856
3534.158255	865583.670529	41.286861
3533.858162	864986.773490	41.291866
3533.727929	864385.903164	41.296871
3534.150914	863791.775137	41.301876
3534.332830	863204.429948	41.306880
3534.357117	862595.000290	41.311885
3534.308344	861991.837411	41.316890
3534.123189	861393.982322	41.321895
3534.438170	860780.822104	41.326900
3534.310076	860185.559312	41.331904
3533.864610	859580.766407	41.336909
3534.167596	858977.924291	41.341914
3533.768245	858380.197999	41.346919
3533.576056	857782.863903	41.351924
3533.450279	857180.500682	41.356928
3533.641982	856579.968937	41.361933
3533.831015	855977.919813	41.366938
3533.380848	855383.215956	41.371943
3533.536706	854781.346828	41.376948
3533.587915	854187.122475	41.381952
3533.312538	853586.863927	41.386957
3533.420194	852994.850000	41.391962
3533.480466	852400.646330	41.396967
3533.621854	851796.152267	41.401972
3533.314807	851199.365235	41.406976
3533.655722	850599.294959	41.411981
3533.700071	850001.066957	41.416986
3533.542620	849395.318619	41.421991
3533.785224	848791.000903	41.426996
3533.352634	848193.264445	41.432000
3533.400023	847584.870195	41.437005
3533.426395	846974.277304	41.442010
3533.235517	846387.430340	41.447015
3533.113441	845777.525099	41.452020
3533.120587	845178.060889	41.457024
3533.050392	844594.630125	41.462029
3532.917951	843992.250607	41.467034
3532.775105	843392.543928	41.472039
3533.138341	842796.299976	41.477044
3532.775334	842202.170563	41.482048
3532.862876	841616.097068	41.487053
3533.330113	841010.892783	41.492058
3532.997378	840410.837358	41.497063
3533.037486	839811.197703	41.502068
3533.073959	839220.669077	41.507072
3533.006863	838608.987453	41.512077
3533.166059	838009.937470	41.517082
3532.997129	837414.740326	41.522087
3533.289240	836808.091904	41.527092
3533.104579	836207.272518	41.532096
3532.845541	835596.065970	41.537101
3533.216144	834991.280657	41.542106
3532.980421	834392.543909	41.547111
3532.766783	833784.572480	41.552116
3532.807865	833193.289757	41.557120
3532.723729	832596.311794	41.562125
3532.786979	831982.899692	41.567130
3532.652824	831385.769172	41.572135
3532.829381	830789.555653	41.577140
3532.593864	830188.230250	41.582144
3532.818098	829583.938006	41.587149
3532.654957	828986.541830	41.592154
3532.601017	828391.611822	41.597159
3532.561361	827779.625604	41.602164
3532.470882	827190.307032	41.607168
3532.648017	826582.421317	41.612173
3532.885228	825979.745714	41.617178
3532.363242	825383.350063	41.622183
3532.779085	824764.356952	41.627188
3532.707504	824172.270011	41.632192
3532.981506	823572.445270	41.637197
3532.871385	822953.321867	41.642202
3532.734953	822352.135734	41.647207
3532.761128	821733.705218	41.652212
3532.619565	821140.623335	41.657216
3532.665866	820525.743297	41.662221
3532.844357	819918.755250	41.667226
3532.782253	819312.975299	41.672231
3532.735872	818698.430133	41.677236
3532.471689	818092.132707	41.682240
3532.374392	817485.017485	41.687245
3532.560735	816880.538389	41.692250
3532.545507	816268.551864	41.697255
3532.466020	815652.458163	41.702260
3532.279413	815048.757328	41.707264
3532.579036	814446.778890	41.712269
3532.561020	813834.765354	41.717274
3532.339649	813233.990505	41.722279
3532.326954	812625.047667	41.727284
3532.269276	812007.341455	41.732288
3532.385078	811404.680449	41.737293
3532.167342	810801.679581	41.742298
3531.954455	810188.387428	41.747303
3532.224593	809577.406196	41.752308
3531.752124	808987.560957	41.757312
3531.779098	808379.403180	41.762317
3532.311182	807781.001726	41.767322
3532.019803	807172.741011	41.772327
3531.931495	806565.126197	41.777332
3531.992984	805962.283391	41.782336
3532.214371	805356.762200	41.787341
3532.206994	804746.324509	41.792346
3531.875912	804141.279904	41.797351
3531.946976	803538.662445	41.802356
3531.589959	802937.241733	41.807360
3531.633417	802331.286710	41.812365
3531.951454	801730.870819	41.817370
3531.534230	801133.617720	41.822375
3531.741813	800524.140326	41.827380
3531.560058	799936.699882	41.832384
3531.566146	799331.075558	41.837389
3531.696549	798728.565844	41.842394
3531.453549	798129.845377	41.847399
3531.537248	797521.841429	41.852404
3531.561240	796927.387702	41.857408
3531.549423	796327.294338	41.862413
3531.845704	795716.642130	41.867418
3531.710339	795111.949476	41.872423
3531.501598	794497.006061	41.877428
3531.398798	793911.054463	41.882432
3531.522766	793301.938565	41.887437
3531.536685	792703.443821	41.892442
3531.324782	792102.137388	41.897447
3531.808839	791491.722304	41.902452
3531.614788	790886.281541	41.907456
3531.360421	790283.205844	41.912461
3531.563352	789682.751402	41.917466
3531.303664	789083.160006	41.922471
3531.282770	788471.635980	41.927476
3531.370505	787873.897123	41.932480
3531.236150	787269.659122	41.937485
3531.295438	786668.875026	41.942490
3531.065697	786066.467512	41.947495
3531.449194	785460.807598	41.952500
3531.312949	784868.604930	41.957504
3531.241130	784247.189141	41.962509
3531.279358	783642.318608	41.967514
3531.376708	783044.418135	41.972519
3531.258760	782428.752554	41.977524
3531.130390	781824.297754	41.982528
3530.943564	781229.540181	41.987533
3530.946346	780628.306750	41.992538
3530.627245	780035.637232	41.997543
3530.774845	779418.881393	42.002548
3530.508985	778836.533547	42.007552
3530.677471	778238.860907	42.012557
3530.774863	777641.889143	42.017562
3530.849092	777047.283488	42.022567
3530.817778	776442.410369	42.027572
3531.033184	775846.304228	42.032576
3531.332026	775246.837042	42.037581
3531.026761	774642.057877	42.042586
3530.775008	774042.930264	42.047591
3530.759200	773426.677743	42.052596
3530.983007	772838.792873	42.057600
3530.819278	772233.937967	42.062605
3530.743987	771635.814239	42.067610
3530.683264	771039.510864	42.072615
3530.715109	770432.553377	42.077620
3530.828820	769838.684208	42.082624
3530.773791	769232.775697	42.087629
3531.098360	768630.004326	42.092634
3530.652828	768029.631054	42.097639
3531.088919	767413.339633	42.102644
3530.525184	766813.380727	42.107648
3530.175916	766201.015769	42.112653
3530.295240	765612.720668	42.117658
3530.223333	765016.032148	42.122663
3530.240180	764418.393394	42.127668
3530.640339	763832.325338	42.132672
3530.880031	763233.469161	42.137677
3530.693402	762627.340363	42.142682
3530.716339	762025.712725	42.147687
3530.768306	761410.864709	42.152692
3530.531566	760810.959453	42.157696
3530.665990	760206.010686	42.162701
3530.800430	759605.946086	42.167706
3530.373726	759003.265692	42.172711
3530.358614	758398.098879	42.177716
3530.287463	757794.718786	42.182720
3529.884698	757195.047985	42.187725
3529.949246	756594.855238	42.192730
3529.925089	756006.671802	42.197735
3529.694793	755402.585944	42.202740
3529.996748	754810.849015	42.207744
3529.760582	754214.024401	42.212749
3530.033803	753622.299014	42.217754
3529.639496	753036.664955	42.222759
3529.786768	752433.859758	42.227764
3529.783820	751854.783440	42.232768
3529.613204	751264.680096	42.237773
3529.733747	750665.394936	42.242778
3529.133845	750075.816987	42.247783
3529.451812	749487.963590	42.252788
3529.468081	748907.921599	42.257792
3529.359597	748321.534211	42.262797
3529.587814	747733.859265	42.267802
3529.489676	747151.432717	42.272807
3529.565639	746553.269407	42.277812
3529.416420	745976.248184	42.282816
3528.878658	745380.570277	42.287821
3529.471833	744794.933680	42.292826
3528.905489	744223.587004	42.297831
3529.107180	743631.603552	42.302836
3529.047676	743056.427339	42.307840
3528.828298	742466.602853	42.312845
3528.985766	741892.540235	42.317850
3528.535623	741313.347786	42.322855
3528.902243	740728.682355	42.327860
3528.849125	740166.743555	42.332864
3528.711048	739589.547082	42.337869
3528.825898	739009.050473	42.342874
3528.704055	738432.459251	42.347879
3528.382294	737853.139594	42.352884
3528.854233	737280.370035	42.357888
3528.944661	736711.681154	42.362893
3528.553381	736126.112849	42.367898
3528.467534	735557.816990	42.372903
3529.016898	734976.704367	42.377908
3528.383854	734399.462933	42.382912
3528.363290	733820.937008	42.387917
3528.570536	733253.268744	42.392922
3528.514908	732682.387846	42.397927
3528.749310	732105.971715	42.402932
3528.410464	731534.562688	42.407936
3528.225022	730963.384011	42.412941
3528.363972	730373.542461	42.417946
3528.425296	729818.530209	42.422951
3528.661315	729243.592921	42.427956
3528.500467	728670.168285	42.432960
3528.134450	728088.566337	42.437965
3528.459012	727518.543410	42.442970
3528.224137	726954.866777	42.447975
3528.300208	726376.534318	42.452980
3528.029870	725805.403328	42.457984
3528.275498	725234.887488	42.462989
3528.222298	724668.198012	42.467994
3527.644465	724102.252616	42.472999
3528.015555	723526.195413	42.478004
3528.027810	722965.373181	42.483008
3527.889277	722392.842157	42.488013
3527.900883	721825.152565	42.493018
3527.995827	721261.424657	42.498023
3527.672898	720694.408381	42.503028
3527.646740	720138.456781	42.508032
3527.673517	719571.997975	42.513037
3527.720080	719005.992927	42.518042
3527.379835	718450.824737	42.523047
3527.518517	717890.529385	42.528052
3527.659684	717332.030794	42.533056
3527.885647	716767.429840	42.538061
3527.666817	716206.636087	42.543066
3527.537878	715650.997487	42.548071
3527.613391	715087.598470	42.553076
3527.537448	714524.633941	42.558080
3527.587908	713957.641229	42.563085
3528.003697	713397.295470	42.568090
3527.630881	712829.654060	42.573095
3527.880044	712266.879970	42.578100
3527.628304	711703.608039	42.583104
3527.403285	711134.537242	42.588109
3527.628819	710579.099026	42.593114
3527.187232	710019.469806	42.598119
3527.507232	709444.583936	42.603124
3527.234542	708897.360613	42.608128
3527.068111	708334.744048	42.613133
3527.295678	707771.973461	42.618138
3527.086477	707228.355748	42.623143
3527.348598	706658.058382	42.628148
3527.207383	706111.229935	42.633152
3527.172398	705552.976355	42.638157
3527.296138	704990.140038	42.643162
3527.344657	704439.845350	42.648167
3527.109538	703877.593545	42.653172
3526.935760	703320.559937	42.658176
3527.110195	702762.387758	42.663181
3527.231757	702211.690156	42.668186
3526.711864	701663.749899	42.673191
3526.756698	701104.648414	42.678196
3526.824224	700559.916798	42.683200
3526.739237	700004.145516	42.688205
3526.971078	699451.266381	42.693210
3526.712486	698903.654234	42.698215
3526.911929	698348.822270	42.703220
3526.908660	697797.170804	42.708224
3526.631223	697248.016773	42.713229
3526.771486	696698.110805	42.718234
3526.319211	696158.661735	42.723239
3526.797800	695595.753182	42.728244
3526.981772	695045.388404	42.733248
3526.885249	694489.766522	42.738253
3526.736915	693935.759496	42.743258
3526.502172	693392.275132	42.748263
3526.689493	692835.854407	42.753268
3526.407089	692288.680037	42.758272
3526.490100	691738.823165	42.763277
3526.542859	691186.052452	42.768282
3526.317296	690639.463294	42.773287
3526.257888	690091.419333	42.778292
3526.124129	689556.239885	42.783296
3525.907714	689025.570108	42.788301
3526.494352	688477.914034	42.793306
3526.139084	687931.878127	42.798311
3526.307958	687389.999133	42.803316
3525.996753	686854.091575	42.808321
3525.988572	686304.015849	42.813325
3525.944174	685770.536516	42.818330
3526.058556	685236.301721	42.823335
3525.973665	684686.638334	42.828340
3525.714567	684161.762067	42.833345
3525.632444	683620.994069	42.838349
3526.047749	683083.295283	42.843354
3525.922398	682549.789537	42.848359
3525.934272	682009.905489	42.853364
3525.779533	681481.670010	42.858369
3525.691101	680942.287681	42.863373
3525.716579	680404.696732	42.868378
3525.499638	679878.122288	42.873383
3525.830073	679336.183273	42.878388
3525.682215	678807.344098	42.883393
3525.471750	678280.776579	42.888397
3525.584185	677741.321254	42.893402
3525.381425	677215.189691	42.898407
3525.625892	676684.418075	42.903412
3525.652193	676159.980900	42.908417
3525.347377	675618.031497	42.913421
3525.452950	675087.341554	42.918426
3525.351071	674562.786116	42.923431
3525.393831	674035.335781	42.928436
3525.299342	673501.549549	42.933441
3525.076729	672977.373970	42.938445
3525.191819	672453.858973	42.943450
3524.960129	671932.317896	42.948455
3525.289356	671399.734985	42.953460
3525.142789	670878.120711	42.958465
3524.832225	670351.769237	42.963469
3525.134554	669824.934661	42.968474
3524.770137	669305.264652	42.973479
3524.968628	668785.270448	42.978484
3524.751214	668263.373846	42.983489
3524.674830	667751.896810	42.988493
3524.921933	667240.037693	42.993498
3524.612655	666718.620227	42.998503
3524.632105	666203.602005	43.003508
3524.597012	665697.942563	43.008513
3524.551889	665175.746963	43.013517
3525.019436	664656.378458	43.018522
3524.488374	664150.073107	43.023527
3524.491292	663626.736959	43.028532
3524.550262	663112.692644	43.033537
3524.311651	662601.665322	43.038541
3524.329196	662098.700497	43.043546
3524.450204	661582.917057	43.048551
3524.423656	661072.171452	43.053556
3524.159716	660571.720008	43.058561
3524.338025	660056.793373	43.063565
3524.299578	659550.011901	43.068570
3523.980948	659049.990140	43.073575
3524.141652	658537.531335	43.078580
3524.214060	658035.194179	43.083585
3524.045652	657521.190461	43.088589
3524.139841	657015.951416	43.093594
3523.945813	656518.524021	43.098599
3524.247619	656007.206048	43.103604
3524.050608	655507.430917	43.108609
3523.836957	655001.790740	43.113613
3523.965958	654491.571618	43.118618
3523.810283	654002.449235	43.123623
3523.849081	653503.280835	43.128628
3524.181556	652998.493097	43.133633
3524.267615	652493.471847	43.138637
3524.078664	651996.213974	43.143642
3523.903875	651490.586586	43.148647
3523.922129	650974.459780	43.153652
3523.639680	650479.839271	43.158657
3523.600760	649976.409500	43.163661
3523.949931	649478.383878	43.168666
3523.639284	648987.890808	43.173671
3523.664787	648482.375873	43.178676
3523.685286	647989.678537	43.183681
3523.535156	647491.189219	43.188685
3523.276794	646999.340245	43.193690
3523.151066	646497.249057	43.198695
3523.437455	646011.255941	43.203700
3523.514118	645523.425786	43.208705
3523.210398	645028.339132	43.213709
3523.795276	644522.879018	43.218714
3523.459861	644045.395071	43.223719
3523.434890	643550.938197	43.228724
3523.373099	643060.912979	43.233729
3522.999734	642568.967373	43.238733
3523.112650	642080.514859	43.243738
3522.846028	641609.704317	43.248743
3523.118268	641106.877317	43.253748
3523.069451	640621.732687	43.258753
3523.053146	640134.108999	43.263757
3523.644518	639646.608354	43.268762
3523.307244	639166.395008	43.273767
3523.277649	638666.850405	43.278772
3522.706194	638177.377715	43.283777
3523.111405	637694.867954	43.288781
3523.145179	637213.149338	43.293786
3522.528749	636732.619772	43.298791
3523.232255	636240.736264	43.303796
3522.745512	635764.892171	43.308801
3522.739989	635284.491130	43.313805
3522.718760	634810.224791	43.318810
3522.504812	634322.759849	43.323815
3522.770553	633843.846984	43.328820
3522.726324	633371.720646	43.333825
3522.771900	632891.100126	43.338829
3522.568463	632408.648260	43.343834
3522.867827	631937.999866	43.348839
3522.714586	631461.601663	43.353844
3523.038564	630978.192969	43.358849
3522.636551	630497.639006	43.363853
3522.936191	629999.422999	43.368858
3522.171314	629516.833768	43.373863
3522.467235	629034.391749	43.378868
3522.699159	628561.250651	43.383873
3522.320587	628088.042393	43.388877
3522.071672	627612.687916	43.393882
3522.011182	627146.893662	43.398887
3522.395439	626670.938213	43.403892
3522.325218	626207.457864	43.408897
3521.779229	625741.284250	43.413901
3521.631628	625268.461693	43.418906
3521.501037	624813.043974	43.423911
3521.863192	624348.006636	43.428916
3521.442615	623889.393650	43.433921
3521.751699	623424.625775	43.438925
3522.413685	622972.400465	43.443930
3521.940091	622510.381451	43.448935
3521.926511	622045.809369	43.453940
3521.884231	621576.312585	43.458945
3522.125995	621120.975178	43.463949
3522.257885	620652.210046	43.468954
3522.112126	620182.820643	43.473959
3521.778973	619719.656047	43.478964
3521.553092	619262.416231	43.483969
3521.188398	618799.618602	43.488973
3521.743478	618334.038385	43.493978
3521.209852	617882.205207	43.498983
3521.146588	617436.988628	43.503988
3521.243328	616981.251756	43.508993
3521.200756	616532.486465	43.513997
3521.418184	616078.044623	43.519002
3521.278290	615626.602320	43.524007
3521.517301	615179.036790	43.529012
3521.159033	614739.224748	43.534017
3521.069628	614285.212270	43.539021
3521.477241	613835.357545	43.544026
3521.232901	613392.364037	43.549031
3521.030827	612936.360024	43.554036
3521.267559	612491.593765	43.559041
3520.924573	612048.262441	43.564045
3521.241647	611597.229078	43.569050
3521.021773	611156.097552	43.574055
3521.044005	610701.066552	43.579060
3520.838774	610261.301186	43.584065
3520.628702	609827.236548	43.589069
3521.000654	609382.021967	43.594074
3520.548320	608942.146539	43.599079
3520.880080	608501.568232	43.604084
3520.925776	608072.808847	43.609089
3520.798357	607616.223266	43.614093
3520.818868	607180.812878	43.619098
3520.616969	606747.129234	43.624103
3520.641886	606302.102622	43.629108
3520.459244	605869.335118	43.634113
3520.223267	605442.480304	43.639117
3520.605889	605003.010777	43.644122
3520.607365	604573.222821	43.649127
3520.607398	604129.269049	43.654132
3520.559941	603701.011916	43.659137
3520.351041	603265.188994	43.664141
3520.437799	602830.152023	43.669146
3520.138958	602402.390827	43.674151
3520.450410	601971.648812	43.679156
3520.307856	601537.354563	43.684161
3519.962443	601115.073860	43.689165
3519.969477	600680.470659	43.694170
3520.070763	600263.653650	43.699175
3520.282495	599834.856177	43.704180
3520.181926	599418.394392	43.709185
3520.045038	598985.006675	43.714189
3520.198513	598557.476837	43.719194
3519.814398	598144.129963	43.724199
3520.108150	597712.076894	43.729204
3519.939854	597291.282661	43.734209
3520.021294	596873.141784	43.739213
3519.808895	596452.123850	43.744218
3519.955552	596032.636165	43.749223
3520.134144	595605.646089	43.754228
3520.085325	595187.316293	43.759233
3519.942699	594764.267109	43.764237
3519.824251	594344.814281	43.769242
3519.594276	593933.752373	43.774247
3519.991994	593504.438498	43.779252
3519.744560	593085.816468	43.784257
3519.656731	592668.709307	43.789261
3519.882332	592252.588653	43.794266
3519.882690	591837.596835	43.799271
3519.826127	591419.887647	43.804276
3519.550706	591009.334212	43.809281
3519.531900	590581.843720	43.814285
3519.693165	590180.128859	43.819290
3519.356796	589769.693616	43.824295
3519.692971	589343.353895	43.829300
3519.657281	588929.020042	43.834305
3519.411013	588514.858472	43.839309
3519.463413	588106.711260	43.844314
3519.405803	587697.463453	43.849319
3519.296491	587288.059731	43.854324
3519.400150	586879.761430	43.859329
3519.277542	586474.804532	43.864333
3518.930443	586070.173838	43.869338
3519.016182	585665.154097	43.874343
3519.283316	585253.154229	43.879348
3519.176116	584860.503753	43.884353
3519.001580	584456.392532	43.889357
3519.462549	584040.146548	43.894362
3519.206509	583632.955728	43.899367
3519.353328	583224.023674	43.904372
3519.221582	582833.573637	43.909377
3519.235998	582418.554699	43.914381
3519.367736	582013.505517	43.919386
3518.982399	581607.626251	43.924391
3518.809981	581203.255638	43.929396
3519.115332	580803.666846	43.934401
3518.528085	580409.044057	43.939405
3519.031361	580001.954233	43.944410
3518.731899	579609.217458	43.949415
3518.730921	579210.986657	43.954420
3518.853803	578821.974096	43.959425
3518.607804	578420.843092	43.964429
3518.807867	578023.142999	43.969434
3518.717306	577638.001667	43.974439
3518.544085	577235.512226	43.979444
3518.559982	576838.861597	43.984449
3518.090204	576453.345825	43.989453
3518.318740	576064.178182	43.994458
3518.177295	575686.478911	43.999463
3518.304818	575294.035130	44.004468
3517.709970	574914.880916	44.009473
3517.899384	574534.625550	44.014477
3518.166354	574151.327193	44.019482
3517.604230	573779.829299	44.024487
3517.937421	573397.251117	44.029492
3517.755649	573027.678229	44.034497
3517.634660	572643.192613	44.039501
3517.557967	572269.756004	44.044506
3517.441296	571907.182540	44.049511
3517.770041	571531.994544	44.054516
3517.929634	571162.258297	44.059521
3517.524166	570791.500746	44.064525
3517.948049	570421.949313	44.069530
3517.789586	570049.115132	44.074535
3517.881508	569667.773331	44.079540
3517.707783	569304.984073	44.084545
3517.602182	568926.622774	44.089549
3517.835454	568557.754185	44.094554
3517.645029	568195.087126	44.099559
3517.772359	567809.808476	44.104564
3518.071839	567449.200711	44.109569
3517.349889	567072.651222	44.114573
3517.849527	566704.086309	44.119578
3517.547584	566348.835180	44.124583
3517.047721	565974.279216	44.129588
3517.392353	565603.796456	44.134593
3517.559431	565241.689517	44.139597
3517.358429	564880.994427	44.144602
3517.084624	564512.549150	44.149607
3517.265654	564151.869155	44.154612
3517.179545	563798.272871	44.159617
3517.340297	563435.612977	44.164621
3517.280692	563068.348667	44.169626
3516.949647	562715.016410	44.174631
3516.887612	562358.305554	44.179636
3516.891155	562002.631098	44.184641
3516.907438	561652.835977	44.189645
3517.108845	561291.368192	44.194650
3516.469546	560945.946127	44.199655
3516.489388	560591.741115	44.204660
3516.780904	560244.177714	44.209665
3516.745082	559890.920068	44.214669
3516.951247	559540.230343	44.219674
3516.388627	559200.943541	44.224679
3516.526661	558846.218017	44.229684
3516.609137	558498.493079	44.234689
3516.144242	558156.997045	44.239693
3516.636827	557815.782009	44.244698
3516.389767	557470.604630	44.249703
3516.530297	557128.777209	44.254708
3516.428054	556790.155790	44.259713
3516.274910	556447.555026	44.264717
3516.649069	556103.293824	44.269722
3516.439556	555771.868179	44.274727
3516.530062	555417.864994	44.279732
3516.511204	555079.135423	44.284737
3515.913633	554743.770677	44.289741
3516.413298	554401.308138	44.294746
3515.968482	554069.628520	44.299751
3516.150746	553728.664032	44.304756
3516.151009	553394.322217	44.309761
3515.970144	553055.468365	44.314765
3515.927692	552725.349538	44.319770
3515.862236	552406.866030	44.324775
3515.751904	552072.006375	44.329780
3516.090337	551742.302336	44.334785
3516.220196	551424.820499	44.339789
3516.361740	551085.055849	44.344794
3515.799177	550753.566646	44.349799
3516.117084	550415.720454	44.354804
3516.137768	550088.701350	44.359809
3516.377879	549750.347940	44.364813
3516.401059	549413.333520	44.369818
3515.881425	549088.096174	44.374823
3516.259197	548752.416069	44.379828
3515.990293	548417.140541	44.384833
3515.645257	548088.976667	44.389837
3515.806175	547769.892170	44.394842
3515.874326	547441.591838	44.399847
3515.660346	547113.029381	44.404852
3515.511636	546790.547308	44.409857
3515.554926	546465.252380	44.414861
3515.790621	546132.607394	44.419866
3515.486099	545822.530244	44.424871
3515.280939	545500.884626	44.429876
3514.886179	545183.649912	44.434881
3515.422235	544856.014717	44.439885
3515.290837	544540.333582	44.444890
3515.146559	544236.646819	44.449895
3515.363732	543923.564264	44.454900
3515.182962	543612.710651	44.459905
3515.137478	543306.818658	44.464909
3515.087935	542986.802494	44.469914
3515.066036	542671.665312	44.474919
3514.988848	542357.891912	44.479924
3515.126776	542059.908302	44.484929
3515.018309	541751.017885	44.489933
3515.123123	541441.075693	44.494938
3515.121935	541136.742332	44.499943
3515.154660	540819.940435	44.504948
3515.527025	540507.813917	44.509953
3515.147717	540195.304499	44.514957
3515.223965	539883.517298	44.519962
3514.933420	539566.994578	44.524967
3515.157598	539265.860538	44.529972
3514.934238	538971.151485	44.534977
3514.760653	538651.057742	44.539981
3514.993436	538345.060646	44.544986
3514.792678	538046.192530	44.549991
3514.573157	537740.764031	44.554996
3514.762890	537440.807697	44.560001
3514.243940	537152.517460	44.565005
3514.380314	536845.445258	44.570010
3514.249017	536563.634636	44.575015
3514.358849	536257.210097	44.580020
3514.145000	535971.315762	44.585025
3513.810022	535692.045086	44.590029
3513.950730	535395.736880	44.595034
3514.108989	535118.943728	44.600039
3514.201167	534826.516710	44.605044
3514.308639	534542.960695	44.610049
3513.929914	534255.748581	44.615053
3514.219612	533964.884830	44.620058
3513.926457	533684.054378	44.625063
3513.778836	533392.648300	44.630068
3513.767703	533115.492390	44.635073
3513.444254	532837.728541	44.640077
3514.120185	532549.596017	44.645082
3513.678118	532278.249988	44.650087
3513.758626	531995.657801	44.655092
3514.035009	531719.082102	44.660097
3514.125856	531442.078660	44.665101
3513.969518	531158.652784	44.670106
3513.724766	530886.237815	44.675111
3513.930461	530596.431103	44.680116
3513.680265	530327.034575	44.685121
3513.719023	530045.572446	44.690125
3513.831681	529773.782265	44.695130
3513.882157	529504.975364	44.700135
3514.063188	529219.839279	44.705140
3513.828720	528933.809642	44.710145
3513.405747	528663.301667	44.715149
3513.519729	528385.580294	44.720154
3513.477679	528117.016178	44.725159
3513.907472	527846.044749	44.730164
3513.727881	527574.314300	44.735169
3513.232202	527306.065262	44.740173
3513.494139	527032.735161	44.745178
3513.197527	526768.278714	44.750183
3513.202501	526498.768553	44.755188
3513.471034	526227.542635	44.760193
3513.345604	525964.001759	44.765197
3513.527179	525699.949453	44.770202
3513.271432	525433.089575	44.775207
3513.570036	525165.675909	44.780212
3513.290347	524902.395006	44.785217
3513.217324	524641.850911	44.790221
3513.266297	524369.114074	44.795226
3513.003200	524114.702176	44.800231
3512.856004	523848.502283	44.805236
3512.774062	523588.395773	44.810241
3512.710083	523329.846894	44.815245
3512.892531	523074.280974	44.820250
3512.673596	522826.858002	44.825255
3512.804508	522561.092733	44.830260
3512.888086	522309.822632	44.835265
3512.423649	522067.175530	44.840269
3512.711032	521807.278151	44.845274
3512.604975	521560.168594	44.850279
3512.784511	521315.228118	44.855284
3512.528316	521064.752787	44.860289
3512.603140	520815.630769	44.865293
3512.406160	520556.855109	44.870298
3512.363214	520333.146660	44.875303
3512.618037	520075.497675	44.880308
3512.693388	519825.248299	44.885313
3512.476710	519587.165403	44.890317
3512.647354	519334.770576	44.895322
3512.489896	519098.841612	44.900327
3512.756782	518842.533360	44.905332
3512.240714	518596.708288	44.910337
3512.264052	518358.565259	44.915341
3512.546180	518110.878863	44.920346
3512.266048	517874.446888	44.925351
3512.305709	517625.632357	44.930356
3512.263597	517386.929819	44.935361
3512.077588	517151.430341	44.940365
3512.308778	516915.199373	44.945370
3511.886351	516671.044878	44.950375
3512.338092	516433.506058	44.955380
3512.421865	516202.542740	44.960385
3512.199700	515964.606632	44.965389
3512.293878	515730.957201	44.970394
3512.209606	515484.200427	44.975399
3512.604141	515248.976949	44.980404
3512.392118	515009.407882	44.985409
3512.047274	514772.939443	44.990413
3512.348140	514534.134295	44.995418
3511.883478	514294.142658	45.000423
3512.204849	514056.640213	45.005428
3511.979859	513833.777740	45.010433
3512.159688	513595.585135	45.015437
3512.211316	513364.281969	45.020442
3511.906465	513140.463291	45.025447
3512.138871	512899.118601	45.030452
3511.948602	512667.139081	45.035457
3511.830415	512431.556445	45.040461
3511.538595	512206.307453	45.045466
3511.909943	511984.630532	45.050471
3511.984300	511752.895482	45.055476
3511.820097	511519.024990	45.060481
3511.379120	511293.838922	45.065485
3511.937355	511063.324889	45.070490
3511.573390	510851.914258	45.075495
3511.889925	510621.081316	45.080500
3511.831435	510393.795810	45.085505
3511.777546	510171.963885	45.090509
3511.424002	509943.458947	45.095514
3511.475352	509722.714518	45.100519
3511.454585	509497.127896	45.105524
3511.464364	509289.018476	45.110529
3511.383424	509073.189640	45.115533
3511.700263	508845.817868	45.120538
3511.368057	508636.646469	45.125543
3511.412860	508421.899181	45.130548
3511.769054	508198.655671	45.135553
3511.516112	507973.036555	45.140557
3511.503023	507755.763159	45.145562
3511.223659	507534.539456	45.150567
3511.351985	507323.048369	45.155572
3511.455841	507106.453789	45.160577
3511.128895	506888.009165	45.165581
3511.876223	506668.518885	45.170586
3511.528042	506462.303918	45.175591
3511.207921	506250.521448	45.180596
3511.619449	506027.794266	45.185601
3511.544894	505813.082948	45.190605
3511.647712	505587.925573	45.195610
3511.410098	505374.398863	45.200615
3511.414882	505156.531235	45.205620
3511.205587	504940.314829	45.210625
3511.203928	504729.266815	45.215629
3511.219106	504507.749018	45.220634
3510.742996	504308.352820	45.225639
3510.984452	504092.199787	45.230644
3511.341898	503893.212247	45.235649
3511.002824	503692.824575	45.240653
3511.040539	503471.491008	45.245658
3510.734800	503272.912442	45.250663
3510.753300	503059.766524	45.255668
3510.802111	502868.048660	45.260673
3510.762924	502665.473768	45.265677
3510.877295	502454.528096	45.270682
3510.959956	502264.162428	45.275687
3510.761321	502051.090981	45.280692
3510.819376	501852.888065	45.285697
3511.113308	501653.024547	45.290701
3511.080156	501450.787515	45.295706
3510.563958	501254.596736	45.300711
3510.716351	501040.643243	45.305716
3510.693314	500843.352106	45.310721
3510.722680	500643.824866	45.315725
3510.758671	500449.299920	45.320730
3510.585087	500250.914984	45.325735
3510.613048	500046.324285	45.330740
3510.399702	499854.565426	45.335745
3510.315011	499659.798954	45.340749
3510.467601	499459.932966	45.345754
3510.230161	499285.718397	45.350759
3510.430604	499088.873819	45.355764
3510.476292	498902.217658	45.360769
3510.201141	498708.635606	45.365773
3510.344350	498506.635819	45.370778
3510.375300	498329.230042	45.375783
3510.274734	498134.650656	45.380788
3510.559523	497946.021233	45.385793
3510.515664	497752.489706	45.390797
3510.380093	497566.810386	45.395802
3510.207999	497381.539823	45.400807
3510.551760	497174.179436	45.405812
3510.600609	496985.023126	45.410817
3510.361677	496815.688698	45.415821
3510.381170	496624.257444	45.420826
3510.338084	496435.768112	45.425831
3510.457684	496248.614458	45.430836
3510.663868	496049.608821	45.435841
3510.493517	495858.757600	45.440845
3510.609899	495658.498216	45.445850
3509.979511	495485.272071	45.450855
3510.300740	495292.105008	45.455860
3510.008503	495108.397826	45.460865
3509.764376	494925.034495	45.465869
3509.806417	494740.962753	45.470874
3509.852604	494567.611659	45.475879
3509.776690	494376.879283	45.480884
3509.672024	494209.114340	45.485889
3509.585256	494036.792169	45.490893
3510.309505	493858.107940	45.495898
3509.850693	493683.215330	45.500903
3510.164146	493499.539015	45.505908
3510.252024	493317.619141	45.510913
3509.659930	493142.946066	45.515917
3510.032032	492956.066942	45.520922
3509.640955	492791.017984	45.525927
3509.750822	492612.071457	45.530932
3509.832382	492434.493769	45.535937
3509.221426	492258.651315	45.540941
3509.772678	492082.810968	45.545946
3509.594254	491924.142151	45.550951
3509.270577	491756.693964	45.555956
3509.664126	491581.128340	45.560961
3509.300522	491414.998987	45.565965
3509.052901	491242.170111	45.570970
3509.078914	491088.922558	45.575975
3509.264365	490912.829111	45.580980
3509.293016	490760.488847	45.585985
3509.302172	490605.975036	45.590989
3509.417768	490430.445107	45.595994
3509.278114	490272.867471	45.600999
3509.293359	490107.166732	45.606004
3509.422562	489938.156231	45.611009
3509.059098	489773.781841	45.616013
3509.320459	489609.198008	45.621018
3509.073250	489457.652279	45.626023
3509.044673	489296.555569	45.631028
3509.075696	489143.239265	45.636033
3509.220328	488978.315176	45.641037
3509.320657	488812.840495	45.646042
3509.017136	488663.574378	45.651047
3509.296166	488499.027579	45.656052
3509.356954	488342.460726	45.661057
3509.209733	488183.600346	45.666061
3509.270880	488024.854741	45.671066
3509.081258	487871.716683	45.676071
3509.114852	487704.370583	45.681076
3509.269098	487549.399905	45.686081
3508.941632	487395.876381	45.691085
3509.178944	487233.399468	45.696090
3509.067491	487090.311288	45.701095
3508.650394	486935.280900	45.706100
3509.539465	486786.048086	45.711105
3508.831805	486629.242825	45.716109
3508.922887	486471.894933	45.721114
3508.792711	486321.212807	45.726119
3508.740699	486159.989877	45.731124
3508.824430	486010.837366	45.736129
3508.553891	485859.011276	45.741133
3508.884953	485704.550760	45.746138
3508.608850	485566.387216	45.751143
3508.401297	485422.441491	45.756148
3508.530918	485268.163366	45.761153
3508.434435	485124.955382	45.766157
3508.394183	484976.321367	45.771162
3508.242632	484842.989438	45.776167
3508.727793	484697.957924	45.781172
3508.819415	484553.194859	45.786177
3508.678743	484422.995797	45.791181
3508.661345	484268.177309	45.796186
3508.467714	484123.408819	45.801191
3508.581533	483970.842886	45.806196
3508.384028	483831.943765	45.811201
3508.319006	483694.033210	45.816205
3508.502630	483553.396582	45.821210
3508.205057	483412.132401	45.826215
3508.391622	483283.387526	45.831220
3508.596617	483145.679683	45.836225
3508.266857	483008.720083	45.841229
3508.508621	482855.515336	45.846234
3508.483661	482725.233444	45.851239
3508.439200	482574.150422	45.856244
3508.487459	482445.068785	45.861249
3508.275925	482300.946531	45.866253
3508.455423	482160.350226	45.871258
3508.352092	482023.597486	45.876263
3508.315098	481894.222714	45.881268
3508.322883	481762.713357	45.886273
3508.262104	481620.989598	45.891277
3508.343619	481483.694976	45.896282
3508.125597	481348.424638	45.901287
3508.181255	481214.017723	45.906292
3508.366119	481081.308856	45.911297
3508.174170	480948.055889	45.916301
3508.209731	480816.636096	45.921306
3507.912805	480691.397393	45.926311
3508.521331	480555.271243	45.931316
3508.065550	480417.351494	45.936321
3508.090809	480292.713104	45.941325
3508.165142	480155.510809	45.946330
3508.018168	480026.040111	45.951335
3507.929356	479905.215320	45.956340
3508.006033	479771.654660	45.961345
3507.793845	479644.875473	45.966349
3508.086633	479519.629190	45.971354
3507.711074	479396.166806	45.976359
3507.737807	479273.546161	45.981364
3507.872290	479139.363449	45.986369
3508.058952	479019.295728	45.991373
3508.555509	478881.505406	45.996378
3507.959859	478761.316417	46.001383
3508.172265	478626.762214	46.006388
3508.127104	478501.262831	46.011393
3507.714561	478375.319023	46.016397
3507.818655	478252.526383	46.021402
3507.777411	478139.073523	46.026407
3507.732708	478011.899918	46.031412
3507.895816	477888.942861	46.036417
3507.446927	477766.089470	46.041421
3508.017701	477644.326915	46.046426
3507.608471	477509.769337	46.051431
3507.632768	477392.148891	46.056436
3507.618941	477269.521659	46.061441
3507.318778	477153.119604	46.066445
3507.644962	477041.673096	46.071450
3507.488222	476928.637489	46.076455
3507.384621	476818.781987	46.081460
3507.523744	476696.529863	46.086465
3507.304287	476592.211812	46.091469
3507.789242	476474.608082	46.096474
3507.450192	476361.549471	46.101479
3507.365336	476232.446241	46.106484
3507.573711	476118.381240	46.111489
3507.533656	476016.206583	46.116493
3507.642190	475889.954131	46.121498
3507.715310	475776.821545	46.126503
3507.716329	475654.586066	46.131508
3507.629704	475539.605759	46.136513
3507.221035	475435.262810	46.141517
3507.371515	475313.455279	46.146522
3507.600334	475201.761052	46.151527
3507.614366	475091.520680	46.156532
3507.564259	474962.402612	46.161537
3507.474961	474855.723140	46.166541
3507.692076	474737.242563	46.171546
3507.553986	474632.241208	46.176551
3507.601075	474517.029146	46.181556
3508.070578	474393.084868	46.186561
3507.768342	474283.096237	46.191565
3508.184576	474163.362632	46.196570
3508.100334	474047.714314	46.201575
3508.095214	473911.896682	46.206580
3508.007781	473786.372295	46.211585
3507.767546	473669.077090	46.216589
3508.119916	473543.779819	46.221594
3508.009037	473424.030168	46.226599
3507.724561	473308.056939	46.231604
3507.833272	473185.786774	46.236609
3507.716091	473065.124318	46.241613
3507.565512	472948.315693	46.246618
3507.807965	472840.808344	46.251623
3507.798278	472717.795669	46.256628
3507.784808	472601.822416	46.261633
3507.671448	472495.639946	46.266637
3507.743927	472373.016129	46.271642
3507.285293	472261.674835	46.276647
3507.450439	472148.048604	46.281652
3507.631272	472034.520298	46.286657
3507.438386	471928.854650	46.291661
3507.536355	471811.743253	46.296666
3507.347536	471695.338503	46.301671
3507.588346	471588.685241	46.306676
3507.378638	471477.448724	46.311681
3507.182141	471367.120953	46.316685
3507.377021	471249.634968	46.321690
3507.238678	471148.615242	46.326695
3507.401662	471040.554003	46.331700
3507.488819	470929.364852	46.336705
3507.045885	470827.585026	46.341709
3507.274692	470721.789936	46.346714
3507.058837	470612.676636	46.351719
3506.791845	470506.509145	46.356724
3506.965413	470407.255592	46.361729
3506.862999	470309.011003	46.366733
3506.885330	470206.793829	46.371738
3506.710572	470120.412931	46.376743
3506.741043	470016.977712	46.381748
3507.269602	469917.964886	46.386753
3507.123940	469817.901666	46.391757
3507.413673	469707.734425	46.396762
3506.877367	469611.434431	46.401767
3507.096339	469504.519853	46.406772
3507.171760	469412.419890	46.411777
3506.753875	469315.844908	46.416781
3507.200497	469203.672471	46.421786
3506.671463	469114.662834	46.426791
3507.172883	469012.306760	46.431796
3507.090300	468912.785190	46.436801
3507.085705	468808.538897	46.441805
3506.918843	468710.195714	46.446810
3506.907091	468613.851748	46.451815
3507.105302	468510.278366	46.456820
3507.159504	468405.867862	46.461825
3507.042019	468312.478459	46.466829
3507.283933	468209.706479	46.471834
3507.123058	468109.484891	46.476839
3507.126905	468014.350989	46.481844
3507.000853	467904.193641	46.486849
3506.849373	467814.910832	46.491853
3506.503301	467704.992532	46.496858
3506.309720	467627.519259	46.501863
3506.646381	467528.628091	46.506868
3506.687701	467435.561891	46.511873
3506.770841	467348.111202	46.516877
3506.853634	467242.878925	46.521882
3506.775924	467163.762907	46.526887
3506.438872	467060.121086	46.531892
3506.521180	466973.276740	46.536897
3506.282699	466886.030837	46.541901
3506.460164	466800.486617	46.546906
3506.425902	466712.749117	46.551911
3506.432305	466632.704664	46.556916
3506.630278	466538.644818	46.561921
3506.072842	466453.123212	46.566925
3506.220441	466361.502826	46.571930
3506.274721	466290.973074	46.576935
3506.231800	466202.626789	46.581940
3506.306111	466115.475966	46.586945
3506.091804	466031.160442	46.591949
3506.609152	465945.199754	46.596954
3506.264139	465869.315774	46.601959
3506.464561	465783.965769	46.606964
3506.616415	465688.187117	46.611969
3506.532974	465614.486641	46.616973
3506.285225	465529.516014	46.621978
3506.402486	465444.634680	46.626983
3506.340537	465351.120062	46.631988
3506.272007	465276.402474	46.636993
3506.299305	465187.583580	46.641997
3506.751490	465100.971632	46.647002
3506.194187	465020.155444	46.652007
3506.400502	464935.358002	46.657012
3506.646807	464849.793383	46.662017
3505.908216	464768.399117	46.667021
3506.467207	464690.278876	46.672026
3506.377654	464600.666595	46.677031
3506.200917	464519.580677	46.682036
3506.028342	464446.245637	46.687041
3505.911311	464365.250212	46.692045
3506.081198	464282.685461	46.697050
3506.050646	464222.346641	46.702055
3505.804427	464144.868363	46.707060
3506.291069	464069.139329	46.712065
3506.125493	463990.430654	46.717069
3506.313023	463911.864040	46.722074
3506.211835	463839.882550	46.727079
3506.444856	463759.078171	46.732084
3506.706622	463682.778018	46.737089
3506.498328	463592.624020	46.742093
3506.669545	463499.871374	46.747098
3506.138451	463417.270641	46.752103
3506.280287	463328.170353	46.757108
3506.375375	463250.731583	46.762113
3506.106159	463178.675005	46.767117
3506.189969	463089.228850	46.772122
3506.241703	463017.978264	46.777127
3506.052622	462940.232096	46.782132
3506.208910	462866.176250	46.787137
3506.049297	462790.856631	46.792141
3506.139283	462721.473243	46.797146
3506.140398	462649.115204	46.802151
3506.014129	462564.465582	46.807156
3506.448866	462489.246005	46.812161
3506.074965	462407.120878	46.817165
3506.004648	462333.152383	46.822170
3505.949362	462264.197556	46.827175
3506.200693	462180.495241	46.832180
3505.839383	462113.619020	46.837185
3505.789327	462037.720409	46.842189
3505.958329	461964.013696	46.847194
3506.109826	461899.177436	46.852199
3505.774584	461824.188131	46.857204
3506.112878	461743.408142	46.862209
3505.935883	461672.850481	46.867213
3506.051523	461602.191927	46.872218
3505.977858	461547.679684	46.877223
3506.335952	461470.898418	46.882228
3506.211932	461388.726371	46.887233
3506.528490	461319.958117	46.892237
3506.742196	461232.457629	46.897242
3506.005354	461150.389226	46.902247
3506.019639	461077.364388	46.907252
3506.177097	460995.649393	46.912257
3505.845482	460926.280990	46.917261
3506.168109	460852.239842	46.922266
3506.195356	460779.515744	46.927271
3505.568575	460699.048294	46.932276
3505.849819	460628.864742	46.937281
3505.724735	460570.861935	46.942285
3506.000754	460493.229393	46.947290
3505.953134	460425.736447	46.952295
3506.015691	460355.741298	46.957300
3506.248423	460287.794600	46.962305
3506.183739	460217.060534	46.967309
3506.303585	460139.047856	46.972314
3505.935713	460068.060964	46.977319
3506.258923	459990.519754	46.982324
3506.414210	459912.094712	46.987329
3505.890817	459843.008651	46.992333
3505.950507	459778.991968	46.997338
3506.071090	459699.862520	47.002343
3505.610324	459631.018420	47.007348
3506.008624	459567.196633	47.012353
3505.846615	459498.453099	47.017357
3505.729191	459429.498999	47.022362
3505.668507	459355.973835	47.027367
3505.776269	459291.693982	47.032372
3505.795341	459228.087900	47.037377
3505.665578	459167.041017	47.042381
3505.706599	459099.275035	47.047386
3505.612487	459028.997890	47.052391
3505.952841	458975.168086	47.057396
3505.952728	458904.671733	47.062401
3505.648202	458843.298936	47.067405
3505.693154	458766.307283	47.072410
3505.645456	458705.143614	47.077415
3505.832559	458647.487343	47.082420
3506.069793	458575.986364	47.087425
3505.632888	458509.567018	47.092429
3505.799220	458443.500585	47.097434
3505.761321	458374.681309	47.102439
3505.661442	458319.353774	47.107444
3506.041311	458260.244381	47.112449
3505.781754	458188.928210	47.117453
3505.927732	458123.624432	47.122458
3505.844542	458060.336193	47.127463
3505.881758	457990.489120	47.132468
3506.089823	457920.359218	47.137473
3505.590880	457853.137361	47.142477
3505.601098	457784.966725	47.147482
3505.729909	457720.830284	47.152487
3505.666926	457659.615352	47.157492
3505.728456	457597.061195	47.162497
3505.457598	457532.080086	47.167501
3505.703950	457463.107782	47.172506
3505.568781	457411.889182	47.177511
3505.741007	457345.716764	47.182516
3506.298181	457280.137299	47.187521
3506.447728	457212.042302	47.192525
3506.593360	457133.861449	47.197530
3506.427180	457067.188364	47.202535
3506.193474	456994.951211	47.207540
3506.074907	456917.270796	47.212545
3506.025221	456852.908643	47.217549
3506.512690	456769.700820	47.222554
3506.436947	456704.937158	47.227559
3506.208616	456630.112795	47.232564
3506.619858	456542.101864	47.237569
3506.120475	456473.912434	47.242573
3506.399593	456402.041776	47.247578
3506.284323	456345.190841	47.252583
3506.173995	456263.198119	47.257588
3505.981780	456195.766297	47.262593
3506.046826	456121.346144	47.267597
3505.911861	456050.203877	47.272602
3505.805108	455993.198437	47.277607
3505.468009	455915.804928	47.282612
3505.724911	455855.036784	47.287617
3505.755492	455788.376574	47.292621
3505.877188	455720.636130	47.297626
3505.767043	455664.846869	47.302631
3505.618474	455599.281088	47.307636
3505.810824	455535.633752	47.312641
3505.773275	455474.458547	47.317645
3505.591677	455408.593655	47.322650
3505.545216	455350.460952	47.327655
3505.639813	455281.608506	47.332660
3505.752429	455223.701727	47.337665
3505.354396	455172.927860	47.342669
3505.450645	455112.032858	47.347674
3505.880518	455054.629018	47.352679
3505.442734	454997.069023	47.357684
3505.739422	454936.494105	47.362689
3505.589870	454881.571161	47.367693
3505.785084	454813.257548	47.372698
3505.743978	454763.030004	47.377703
3505.583707	454688.389625	47.382708
3505.735578	454624.290135	47.387713
3505.290641	454566.780838	47.392717
3505.716552	454508.514386	47.397722
3505.791177	454440.828416	47.402727
3505.607044	454381.094324	47.407732
3505.687873	454326.890927	47.412737
3505.700476	454264.588306	47.417741
3505.862086	454198.153982	47.422746
3505.879486	454139.043771	47.427751
3505.739789	454078.997054	47.432756
3506.264343	454008.241970	47.437761
3506.176093	453946.411836	47.442765
3506.136871	453878.946218	47.447770
3505.918924	453807.354053	47.452775
3505.777975	453742.338629	47.457780
3505.881353	453686.659581	47.462785
3505.374864	453618.461795	47.467789
3505.626023	453554.950329	47.472794
3505.860156	453500.566490	47.477799
3505.716566	453442.495638	47.482804
3505.788002	453378.659456	47.487809
3505.666147	453312.828303	47.492813
3505.916395	453246.122291	47.497818
3505.825121	453188.548734	47.502823
3505.607789	453123.544393	47.507828
3505.776128	453059.335810	47.512833
3505.573799	453007.559945	47.517837
3505.628443	452943.015546	47.522842
3505.555465	452884.525500	47.527847
3505.611998	452826.925694	47.532852
3505.670710	452765.371086	47.537857
3505.602179	452716.816173	47.542861
3505.864298	452649.447155	47.547866
3505.918035	452593.469450	47.552871
3505.778572	452533.722355	47.557876
3505.829250	452466.033967	47.562881
3505.554075	452413.812780	47.567885
3505.873421	452347.345545	47.572890
3505.758841	452290.432518	47.577895
3505.506473	452222.288106	47.582900
3505.880427	452159.055557	47.587905
3505.460594	452107.973635	47.592909
3505.754786	452049.215739	47.597914
3505.700970	451989.807330	47.602919
3505.839927	451932.850029	47.607924
3505.970882	451863.827820	47.612929
3505.868134	451817.101763	47.617933
3505.935355	451744.287680	47.622938
3505.869012	451680.976757	47.627943
3505.913096	451614.452774	47.632948
3505.929069	451556.197273	47.637953
3505.868138	451489.589424	47.642957
3506.313943	451420.461281	47.647962
3505.990568	451359.221226	47.652967
3505.921379	451284.857147	47.657972
3506.027201	451226.129085	47.662977
3506.002258	451165.141698	47.667981
3506.219984	451090.829335	47.672986
3505.908509	451036.075877	47.677991
3505.829554	450978.798266	47.682996
3505.621282	450909.222405	47.688001
3505.315615	450851.881755	47.693005
3505.544748	450789.379570	47.698010
3505.496629	450729.510277	47.703015
3505.455536	450672.073255	47.708020
3505.563800	450619.122964	47.713025
3505.297537	450565.171764	47.718029
3505.209576	450506.829668	47.723034
3505.228644	450453.691382	47.728039
3505.137835	450400.318214	47.733044
3505.390530	450357.685712	47.738049
3505.153799	450293.639135	47.743053
3505.474490	450252.262354	47.748058
3505.191991	450205.259156	47.753063
3505.263153	450150.336631	47.758068
3505.326035	450095.212568	47.763073
3505.136943	450046.266375	47.768077
3505.451080	449995.206042	47.773082
3505.304653	449938.494823	47.778087
3505.542154	449888.157152	47.783092
3505.515206	449842.630587	47.788097
3505.289784	449786.946504	47.793101
3505.327653	449735.070757	47.798106
3505.151511	449682.521577	47.803111
3505.147567	449630.906228	47.808116
3505.308609	449579.059767	47.813121
3505.221216	449535.875219	47.818125
3505.492904	449480.156143	47.823130
3505.412319	449421.099907	47.828135
3505.196451	449376.111625	47.833140
3505.429054	449316.849507	47.838145
3505.218218	449265.217881	47.843149
3505.511060	449211.117017	47.848154
3505.698210	449168.746812	47.853159
3505.310315	449106.547777	47.858164
3505.469452	449053.990479	47.863169
3505.133868	449008.311983	47.868173
3505.380254	448947.778848	47.873178
3505.523827	448897.556250	47.878183
3505.626969	448847.137615	47.883188
3505.761015	448784.544275	47.888193
3505.486317	448741.085843	47.893197
3505.659661	448679.753120	47.898202
3505.700353	448621.637339	47.903207
3505.545256	448557.470107	47.908212
3505.925042	448508.930255	47.913217
3505.683921	448456.439809	47.918221
3505.512414	448391.311455	47.923226
3505.520832	448343.848761	47.928231
3505.352323	448286.274841	47.933236
3505.409940	448232.262336	47.938241
3505.386678	448189.976797	47.943245
3505.719359	448126.181328	47.948250
3505.357991	448076.093699	47.953255
3505.374612	448022.087656	47.958260
3505.538686	447962.377066	47.963265
3505.509209	447921.663982	47.968269
3505.354398	447863.275250	47.973274
3505.623693	447814.448423	47.978279
3505.580523	447761.466080	47.983284
3505.390487	447707.088856	47.988289
3505.267720	447656.046745	47.993293
3505.674201	447603.342187	47.998298
3505.542569	447552.656299	48.003303
3505.616752	447489.562260	48.008308
3505.663169	447438.135777	48.013313
3505.123902	447383.006012	48.018317
3505.619258	447325.417541	48.023322
3505.376158	447289.658486	48.028327
3505.456276	447233.915484	48.033332
3505.586448	447169.999589	48.038337
3505.355635	447130.333549	48.043341
3505.258723	447071.172106	48.048346
3505.394359	447018.918020	48.053351
3505.438658	446975.604327	48.058356
3505.357345	446916.997599	48.063361
3505.211521	446860.683678	48.068365
3505.460966	446808.916745	48.073370
3505.768320	446757.342639	48.078375
3505.607526	446703.769215	48.083380
3505.614346	446648.595010	48.088385
3505.622404	446603.968274	48.093389
3505.727317	446542.691762	48.098394
3505.649027	446487.024562	48.103399
3505.058477	446434.740904	48.108404
3505.402583	446367.033447	48.113409
3505.310546	446324.350244	48.118413
3505.154497	446271.434171	48.123418
3505.193545	446232.481050	48.128423
3505.078780	446181.738302	48.133428
3505.186356	446134.405871	48.138433
3505.017356	446094.575210	48.143437
3505.085851	446040.098866	48.148442
3505.191299	445993.375030	48.153447
3505.031111	445963.076498	48.158452
3504.937532	445910.960259	48.163457
3505.246489	445878.857283	48.168461
3505.439100	445821.671432	48.173466
3505.102709	445770.356998	48.178471
3505.505743	445719.930442	48.183476
3505.633293	445668.485834	48.188481
3505.293679	445635.783255	48.193485
3505.585152	445586.693972	48.198490
3505.688036	445523.589212	48.203495
3505.202422	445477.066599	48.208500
3505.424416	445419.164669	48.213505
3505.165005	445371.183224	48.218509
3505.557558	445318.982538	48.223514
3505.354386	445276.011936	48.228519
3505.310740	445213.945562	48.233524
3505.654947	445164.389882	48.238529
3505.070504	445116.260508	48.243533
3505.275255	445063.888413	48.248538
3505.714851	445008.078221	48.253543
3505.186174	444963.387566	48.258548
3504.891772	444913.179630	48.263553
3505.394026	444859.843375	48.268557
3505.461724	444814.746291	48.273562
3505.301918	444772.426570	48.278567
3505.307924	444721.101876	48.283572
3505.414014	444672.752170	48.288577
3504.968192	444634.588950	48.293581
3505.041738	444588.476086	48.298586
3505.019195	444534.315755	48.303591
3505.015259	444500.996258	48.308596
3505.031993	444436.685840	48.313601
3504.876435	444409.832998	48.318605
3505.430190	444347.763550	48.323610
3505.659584	444317.548321	48.328615
3505.299302	444271.052409	48.333620
3505.669874	444211.296077	48.338625
3505.419948	444168.229811	48.343629
3505.347020	444113.265563	48.348634
3505.649781	444061.127878	48.353639
3505.606399	444011.737162	48.358644
3505.465117	443963.580255	48.363649
3505.169261	443900.538820	48.368653
3505.309853	443850.254131	48.373658
3504.867328	443804.481297	48.378663
3505.166988	443772.731790	48.383668
3505.236345	443710.083896	48.388673
3504.934328	443674.683884	48.393677
3504.931794	443625.183874	48.398682
3504.773559	443593.563008	48.403687
3505.118245	443541.315476	48.408692
3504.965421	443494.630315	48.413697
3505.035406	443456.529090	48.418701
3505.173066	443408.069726	48.423706
3505.285910	443363.215494	48.428711
3504.837031	443335.244878	48.433716
3505.137343	443281.584182	48.438721
3504.799188	443262.368869	48.443725
3505.369796	443213.987302	48.448730
3505.109267	443168.029890	48.453735
3505.012994	443120.979236	48.458740
3505.240612	443078.742201	48.463745
3504.870893	443031.839482	48.468749
3505.214469	442991.408365	48.473754
3504.665297	442941.492940	48.478759
3504.877329	442908.489149	48.483764
3505.196350	442851.324558	48.488769
3505.203250	442824.797045	48.493773
3505.298613	442774.720464	48.498778
3505.381693	442733.775431	48.503783
3505.365965	442693.151511	48.508788
3505.481153	442635.919719	48.513793
3505.043293	442593.541771	48.518797
3505.506330	442533.917191	48.523802
3504.967253	442492.570733	48.528807
3505.052107	442445.994895	48.533812
3505.182202	442400.172041	48.538817
3505.181006	442352.241240	48.543821
3505.425857	442312.332927	48.548826
3505.260729	442269.907780	48.553831
3505.220352	442220.867521	48.558836
3505.731015	442171.783783	48.563841
3505.412703	442130.348221	48.568845
3505.544178	442078.184304	48.573850
3505.662522	442029.573006	48.578855
3505.322778	441977.134257	48.583860
3505.533058	441925.210126	48.588865
3505.601623	441880.106791	48.593869
3505.553125	441823.103703	48.598874
3505.531030	441766.958233	48.603879
3505.236223	441719.329786	48.608884
3505.461271	441667.909744	48.613889
3505.130305	441622.113262	48.618893
3505.734585	441571.744134	48.623898
3505.202191	441534.655408	48.628903
3505.233782	441485.753378	48.633908
3505.099298	441425.010454	48.638913
3504.886321	441391.671158	48.643917
3504.851455	441342.780157	48.648922
3504.640717	441315.527125	48.653927
3505.033979	441267.475869	48.658932
3505.350450	441224.307058	48.663937
3504.786873	441181.186982	48.668941
3505.250821	441133.579875	48.673946
3505.312274	441093.041249	48.678951
3505.454725	441052.032204	48.683956
3505.270418	441005.651429	48.688961
3505.071265	440954.961558	48.693965
3505.478255	440921.414241	48.698970
3505.119776	440874.809309	48.703975
3504.877239	440826.764203	48.708980
3505.183625	440776.647015	48.713985
3504.999528	440752.178573	48.718989
3504.806967	440703.921767	48.723994
3504.735311	440674.818109	48.728999
3504.771549	440626.065545	48.734004
3504.850669	440581.312809	48.739009
3504.657997	440558.722432	48.744013
3504.754911	440507.930252	48.749018
3504.371733	440485.676679	48.754023
3504.467239	440457.609416	48.759028
3505.217498	440408.988079	48.764033
3505.065480	440376.448435	48.769037
3504.752117	440335.363708	48.774042
3504.724600	440302.143267	48.779047
3504.502667	440267.992186	48.784052
3504.993179	440221.646710	48.789057
3504.873627	440191.891159	48.794061
3504.906354	440141.920706	48.799066
3504.864690	440103.984881	48.804071
3504.584199	440070.300026	48.809076
3504.704088	440036.343851	48.814081
3504.579335	440013.487688	48.819085
3504.481609	439983.677403	48.824090
3504.760175	439936.809532	48.829095
3504.703263	439906.941448	48.834100
3504.838218	439870.750487	48.839105
3505.048982	439839.010454	48.844109
3504.939289	439797.585591	48.849114
3504.689177	439757.097706	48.854119
3505.034200	439721.986620	48.859124
3504.966164	439677.916626	48.864129
3504.665436	439645.147662	48.869133
3504.329971	439609.442412	48.874138
3504.629630	439571.802482	48.879143
3504.618444	439553.390437	48.884148
3505.035995	439512.991011	48.889153
3504.694919	439474.344321	48.894157
3504.683210	439431.228038	48.899162
3504.402576	439390.896877	48.904167
3504.572128	439356.220993	48.909172
3504.975693	439335.049385	48.914177
3504.408503	439301.006489	48.919181
3504.874153	439272.062876	48.924186
3504.647180	439239.990906	48.929191
3504.516168	439206.025571	48.934196
3504.705854	439180.071179	48.939201
3504.338800	439162.480493	48.944205
3504.598953	439114.092184	48.949210
3504.863997	439078.232813	48.954215
3504.737549	439053.042448	48.959220
3504.788202	439003.370734	48.964225
3504.674209	438971.076170	48.969229
3504.613335	438949.171842	48.974234
3504.686747	438892.799826	48.979239
3504.852293	438874.001940	48.984244
3504.884168	438845.588397	48.989249
3504.972389	438808.947124	48.994253
3504.881053	438761.937015	48.999258
3504.826430	438729.581234	49.004263
3504.631183	438702.068682	49.009268
3504.798926	438650.194834	49.014273
3504.526576	438621.173471	49.019277
3504.667228	438593.349784	49.024282
3504.930055	438559.214753	49.029287
3504.524478	438527.425897	49.034292
3504.710864	438500.913252	49.039297
3504.641075	438456.232377	49.044301
3504.627809	438421.687711	49.049306
3504.634046	438395.510080	49.054311
3504.790720	438357.791050	49.059316
3505.021621	438331.169143	49.064321
3504.647135	438287.250175	49.069325
3504.830188	438260.230513	49.074330
3504.829775	438221.574203	49.079335
3504.925564	438179.350281	49.084340
3504.783295	438151.980193	49.089345
3504.724298	438118.406743	49.094349
3504.993096	438082.088554	49.099354
3504.551730	438042.746269	49.104359
3504.653165	438008.637954	49.109364
3504.914537	437982.264081	49.114369
3504.834232	437942.403392	49.119373
3504.841407	437911.862181	49.124378
3505.009608	437867.139490	49.129383
3504.809998	437839.372962	49.134388
3504.790925	437804.473215	49.139393
3504.542955	437781.990911	49.144397
3504.512178	437747.498923	49.149402
3504.818589	437722.182410	49.154407
3504.656324	437680.001606	49.159412
3505.028414	437645.389940	49.164417
3504.414452	437606.380745	49.169421
3504.708033	437578.276023	49.174426
3505.024979	437550.725325	49.179431
3504.781226	437507.797134	49.184436
3504.812709	437475.729223	49.189441
3504.686970	437442.927132	49.194445
3504.811183	437410.589634	49.199450
3504.888902	437384.956666	49.204455
3504.572601	437339.503935	49.209460
3504.894299	437305.407671	49.214465
3504.786453	437275.240357	49.219469
3504.704249	437234.008957	49.224474
3505.084898	437203.098614	49.229479
3504.544688	437168.388324	49.234484
3504.974688	437136.251881	49.239489
3504.879892	437108.212885	49.244493
3504.758973	437062.878430	49.249498
3505.077776	437035.783379	49.254503
3504.346634	437000.750300	49.259508
3504.598424	436963.722942	49.264513
3504.749582	436935.996866	49.269517
3504.594825	436895.842628	49.274522
3504.824263	436872.415429	49.279527
3504.530100	436836.242081	49.284532
3504.911282	436799.293825	49.289537
3504.877432	436776.976885	49.294541
3504.939388	436733.386210	49.299546
3504.799909	436697.541361	49.304551
3504.305117	436656.125680	49.309556
3504.926432	436624.057307	49.314561
3504.475340	436599.782082	49.319565
3504.641102	436575.097100	49.324570
3504.515845	436536.662136	49.329575
3504.746277	436510.748424	49.334580
3504.816986	436471.874016	49.339585
3504.897477	436446.290238	49.344589
3504.420618	436414.967156	49.349594
3504.681547	436367.688931	49.354599
3504.434134	436361.034230	49.359604
3504.369918	436334.714017	49.364609
3504.464700	436294.668300	49.369613
3504.302128	436263.088405	49.374618
3504.167082	436238.505151	49.379623
3504.618602	436224.425272	49.384628
3504.706534	436195.085570	49.389633
3504.241867	436162.288746	49.394637
3504.624899	436135.283115	49.399642
3504.704386	436111.221176	49.404647
3504.457019	436070.827604	49.409652
3504.557722	436046.000946	49.414657
3504.260556	436024.184837	49.419661
3504.630078	435991.499003	49.424666
3505.013025	435964.949801	49.429671
3504.638723	435944.618109	49.434676
3504.489896	435892.538261	49.439681
3504.264123	435869.441425	49.444685
3504.354486	435850.146488	49.449690
3504.478904	435822.728023	49.454695
3504.247332	435789.129820	49.459700
3504.282558	435761.523568	49.464705
3504.384706	435744.966259	49.469709
3504.447363	435723.849456	49.474714
3504.081908	435689.462193	49.479719
3504.104265	435665.663213	49.484724
3504.608526	435640.970148	49.489729
3504.033980	435635.081394	49.494733
3504.271133	435615.000151	49.499738
3504.335650	435587.794574	49.504743
3504.104965	435553.181147	49.509748
3504.378742	435531.216336	49.514753
3503.814905	435519.237370	49.519757
3504.073220	435498.797257	49.524762
3504.107104	435487.933886	49.529767
3503.854412	435473.263476	49.534772
3504.341079	435451.363710	49.539777
3504.003116	435415.855134	49.544781
3504.113808	435382.755989	49.549786
3504.296846	435355.428422	49.554791
3504.006885	435350.810153	49.559796
3504.149674	435332.165399	49.564801
3503.970009	435323.215671	49.569805
3503.923798	435306.226743	49.574810
3504.143287	435269.760228	49.579815
3504.103854	435254.596631	49.584820
3504.403724	435226.437170	49.589825
3504.074807	435216.447407	49.594829
3504.139696	435193.909095	49.599834
3504.402233	435178.186515	49.604839
3504.039230	435150.546041	49.609844
3504.339145	435120.356956	49.614849
3504.283080	435099.665741	49.619853
3504.452878	435080.305848	49.624858
3504.405654	435069.100964	49.629863
3504.290227	435036.039922	49.634868
3504.298771	435001.790703	49.639873
3504.315115	434990.371977	49.644877
3504.420886	434975.842987	49.649882
3504.281316	434947.656739	49.654887
3504.177530	434910.686734	49.659892
3504.279062	434885.909402	49.664897
3504.390067	434873.256748	49.669901
3504.253582	434856.739538	49.674906
3504.247141	434824.928024	49.679911
3503.950853	434801.131808	49.684916
3504.272624	434785.551057	49.689921
3504.068652	434761.130181	49.694925
3504.134651	434750.311712	49.699930
3504.240451	434739.334226	49.704935
3504.296103	434718.369899	49.709940
3504.517490	434680.988830	49.714945
3504.110498	434668.678201	49.719949
3504.069109	434647.324472	49.724954
3504.265270	434632.475399	49.729959
3503.934691	434620.100958	49.734964
3504.388384	434594.552841	49.739969
3504.320796	434569.093705	49.744973
3504.078398	434556.805649	49.749978
3504.255261	434546.678491	49.754983
3504.159744	434520.716684	49.759988
3504.134734	434502.658026	49.764993
3503.895438	434473.574924	49.769997
3504.316909	434443.567141	49.775002
3504.418212	434426.653845	49.780007
3503.856682	434423.603918	49.785012
3504.261023	434405.167439	49.790017
3503.886626	434396.098378	49.795021
3504.379565	434371.558087	49.800026
3504.180826	434337.901389	49.805031
3504.126626	434316.346581	49.810036
3504.376330	434292.608822	49.815041
3504.164654	434288.687315	49.820045
3504.255504	434271.268298	49.825050
3504.264536	434238.895193	49.830055
3504.416727	434216.138049	49.835060
3504.448316	434189.139377	49.840065
3504.262963	434185.213357	49.845069
3504.248871	434167.609223	49.850074
3504.536371	434129.099696	49.855079
3504.389857	434113.395489	49.860084
3504.512015	434083.844256	49.865089
3504.692936	434061.031312	49.870093
3504.196677	434024.786497	49.875098
3504.162021	434010.230130	49.880103
3503.955122	434001.030832	49.885108
3504.317663	433975.649807	49.890113
3504.203420	433964.658782	49.895117
3504.323282	433933.027416	49.900122
3504.148040	433914.435806	49.905127
3503.822375	433893.637310	49.910132
3504.287944	433874.936250	49.915137
3504.198716	433868.862683	49.920141
3504.156445	433839.694391	49.925146
3504.387814	433812.356721	49.930151
3504.080055	433786.328838	49.935156
3504.444608	433763.129061	49.940161
3504.091862	433755.578253	49.945165
3504.162416	433740.800790	49.950170
3504.157274	433711.270812	49.955175
3503.812564	433689.257613	49.960180
3504.366268	433666.786547	49.965185
3504.038141	433658.216694	49.970189
3504.066003	433646.998290	49.975194
3504.431108	433631.460095	49.980199
3503.992727	433625.852005	49.985204
3504.109131	433592.597063	49.990209
3503.882682	433577.717985	49.995213
3503.779417	433548.458254	50.000218
3504.265977	433533.254439	50.005223
3504.403732	433521.256099	50.010228
3504.471101	433506.073101	50.015233
3504.283672	433502.350280	50.020237
3503.784034	433468.287012	50.025242
3504.184721	433436.099600	50.030247
3504.385516	433423.380071	50.035252
3504.717487	433406.071448	50.040257
3504.266433	433396.456926	50.045261
3504.551973	433358.301625	50.050266
3504.354761	433336.059936	50.055271
3503.852863	433325.033313	50.060276
3504.228821	433298.279236	50.065281
3504.249431	433295.434201	50.070285
3503.960936	433264.734240	50.075290
3504.269328	433238.042371	50.080295
3504.188165	433224.000859	50.085300
3504.115436	433203.716701	50.090305
3504.001329	433197.748687	50.095309
3503.945064	433183.246225	50.100314
3504.410797	433176.062885	50.105319
3503.933931	433150.316861	50.110324
3504.539012	433112.106590	50.115329
3504.461313	433107.197910	50.120333
3504.452686	433091.773906	50.125338
3504.454947	433065.083367	50.130343
3504.349054	433031.307409	50.135348
3504.344565	433012.229233	50.140353
3504.098145	433006.689696	50.145357
3503.734295	432991.123312	50.150362
3503.858963	432977.706148	50.155367
3503.907788	432977.545579	50.160372
3504.087192	432953.108050	50.165377
3503.935712	432915.838508	50.170381
3504.074469	432897.090972	50.175386
3503.849343	432888.706211	50.180391
3503.911496	432880.120169	50.185396
3503.757843	432856.602023	50.190401
3504.483793	432853.281301	50.195405
3504.672037	432838.330935	50.200410
3504.205628	432826.486134	50.205415
3504.085313	432792.661545	50.210420
3504.346968	432777.292665	50.215425
3504.429011	432767.333139	50.220429
3504.383073	432752.219733	50.225434
3504.244302	432721.189025	50.230439
3503.929298	432696.987871	50.235444
3504.102448	432674.834530	50.240449
3503.702366	432670.691200	50.245453
3503.779645	432658.144567	50.250458
3503.925756	432641.983443	50.255463
3503.729603	432631.868390	50.260468
3503.745576	432618.723290	50.265473
3503.595361	432611.898662	50.270477
3503.984329	432593.869298	50.275482
3503.893841	432587.744863	50.280487
3503.952589	432579.413004	50.285492
3503.791908	432562.949009	50.290497
3503.607980	432562.422237	50.295501
3503.832400	432548.226648	50.300506
3503.887965	432539.489374	50.305511
3503.591309	432539.134078	50.310516
3503.822621	432518.746658	50.315521
3503.841509	432512.299070	50.320525
3503.986926	432501.110777	50.325530
3504.005619	432488.421825	50.330535
3503.921719	432485.391563	50.335540
3504.011276	432465.028300	50.340545
3504.070888	432439.697305	50.345549
3504.049435	432412.654856	50.350554
3504.112996	432393.107859	50.355559
3503.554299	432397.211965	50.360564
3503.655036	432372.330563	50.365569
3504.084514	432371.699048	50.370573
3504.066437	432363.075768	50.375578
3504.003179	432346.747214	50.380583
3503.717684	432331.116259	50.385588
3504.176988	432321.904018	50.390593
3503.909752	432328.292565	50.395597
3503.696734	432313.004426	50.400602
3504.058586	432297.161427	50.405607
3503.697465	432277.788333	50.410612
3503.574629	432257.917845	50.415617
3503.520765	432266.908639	50.420621
3503.161395	432265.802894	50.425626
3503.546486	432260.510551	50.430631
3503.741340	432255.808868	50.435636
3503.890606	432239.443950	50.440641
3503.851038	432244.423569	50.445645
3503.754602	432228.354314	50.450650
3503.905274	432223.913887	50.455655
3503.551193	432212.506282	50.460660
3503.872025	432195.401626	50.465665
3503.763340	432198.870747	50.470669
3503.603742	432181.746628	50.475674
3504.169138	432180.127769	50.480679
3503.663687	432164.026821	50.485684
3503.991532	432145.449363	50.490689
3503.859808	432155.062421	50.495693
3503.705014	432145.041579	50.500698
3504.038196	432130.471956	50.505703
3503.899813	432126.639048	50.510708
3504.089733	432089.208386	50.515713
3503.771926	432062.063896	50.520717
3503.797517	432044.806566	50.525722
3503.885698	432038.296270	50.530727
3503.911134	432027.483442	50.535732
3503.630903	431989.168759	50.540737
3503.997936	431953.382191	50.545741
3503.879053	431899.410589	50.550746
3503.970569	431834.239157	50.555751
3503.585196	431759.761215	50.560756
3503.667552	431663.687367	50.565761
3503.666745	431578.233034	50.570765
3503.588545	431465.236934	50.575770
3503.645739	431347.142611	50.580775
3503.649059	431223.728578	50.585780
3503.779687	431067.916135	50.590785
3503.768706	430918.774616	50.595789
3503.566894	430747.589859	50.600794
3503.815380	430572.064188	50.605799
3503.532111	430376.227446	50.610804
3503.625926	430168.652613	50.615809
3503.744340	429958.128318	50.620813
3503.577864	429732.426065	50.625818
3503.707224	429482.108333	50.630823
3503.749223	429242.561872	50.635828
3503.560892	428970.216619	50.640833
3503.345777	428689.752579	50.645837
3503.469392	428397.148404	50.650842
3503.315966	428098.396095	50.655847
3503.331030	427791.795244	50.660852
3503.620794	427462.202752	50.665857
3503.500202	427112.069360	50.670861
3503.496542	426752.774868	50.675866
3503.558628	426395.849274	50.680871
3503.349892	426014.855019	50.685876
3503.778983	425614.711598	50.690881
3503.464858	425194.994024	50.695885
3503.327987	424778.335197	50.700890
3503.765952	424335.327821	50.705895
3503.433285	423881.276388	50.710900
3503.606697	423406.012845	50.715905
3503.211207	422933.730673	50.720909
3503.304925	422422.977850	50.725914
3503.235413	421903.612081	50.730919
3503.216259	421368.742874	50.735924
3503.156151	420818.460999	50.740929
3503.107731	420258.315685	50.745933
3502.886100	419686.053220	50.750938
3503.066715	419093.324203	50.755943
3502.680639	418483.897534	50.760948
3502.736184	417855.467370	50.765953
3502.691435	417213.938644	50.770957
3502.736209	416557.703939	50.775962
3502.651601	415885.377782	50.780967
3502.256037	415194.247899	50.785972
3502.661072	414479.832077	50.790977
3502.996760	413753.474468	50.795981
3502.777660	413004.490940	50.800986
3502.668226	412235.127674	50.805991
3502.494006	411437.109161	50.810996
3502.457477	410634.751255	50.816001
3502.185207	409807.496833	50.821005
3502.062529	408963.099768	50.826010
3502.428695	408110.491007	50.831015
3501.641493	407230.978553	50.836020
3501.990016	406326.988247	50.841025
3502.020921	405430.971945	50.846029
3501.588935	404496.016509	50.851034
3501.514996	403541.841359	50.856039
3501.440514	402570.842901	50.861044
3501.323895	401584.271425	50.866049
3501.199424	400574.955896	50.871053
3501.075540	399549.396200	50.876058
3501.170470	398499.525507	50.881063
3500.883038	397441.678664	50.886068
3500.863125	396362.532383	50.891073
3501.009577	395267.945745	50.896077
3500.242222	394145.371833	50.901082
3500.552037	393006.232679	50.906087
3500.197805	391857.456369	50.911092
3500.021061	390681.618286	50.916097
3499.874448	389497.063632	50.921101
3499.833658	388291.402257	50.926106
3499.795042	387053.365542	50.931111
3499.394577	385817.806817	50.936116
3499.552493	384558.491822	50.941121
3499.710301	383273.200552	50.946125
3499.093486	381972.967444	50.951130
3499.368798	380654.100322	50.956135
3499.135309	379313.633667	50.961140
3499.206174	377954.858578	50.966145
3498.935868	376577.705711	50.971149
3498.852350	375173.439054	50.976154
3498.987097	373762.009451	50.981159
3498.147384	372336.501016	50.986164
3498.512321	370877.622649	50.991169
3497.954578	369413.807279	50.996173
3497.618537	367929.779975	51.001178
3497.857354	366436.846208	51.006183
3497.721334	364913.169620	51.011188
3497.633616	363376.121813	51.016193
3497.165677	361834.473521	51.021197
3497.004281	360250.261114	51.026202
3497.405977	358662.200531	51.031207
3496.735303	357067.977041	51.036212
3496.753024	355431.677500	51.041217
3496.506834	353803.116880	51.046221
3496.407767	352134.324088	51.051226
3496.093089	350465.451948	51.056231
3495.220140	348779.132588	51.061236
3495.287752	347077.424504	51.066241
3494.852132	345374.872994	51.071245
3494.735212	343642.026749	51.076250
3494.117601	341886.529991	51.081255
3493.861067	340131.288794	51.086260
3493.865708	338366.244456	51.091265
3493.530604	336585.977640	51.096269
3492.980455	334789.118022	51.101274
3493.112391	332977.624442	51.106279
3492.817687	331171.156061	51.111284
3492.843970	329326.981113	51.116289
3492.511907	327475.858178	51.121293
3492.358158	325610.416845	51.126298
3491.983311	323715.020366	51.131303
3491.528271	321827.444011	51.136308
3491.070207	319908.857122	51.141313
3490.656760	317995.551309	51.146317
3490.286087	316069.734547	51.151322
3490.265211	314124.939715	51.156327
3490.009467	312173.028713	51.161332
3489.831915	310192.512684	51.166337
3489.139071	308217.456043	51.171341
3488.960849	306222.963101	51.176346
3489.218873	304212.765067	51.181351
3488.536101	302201.280108	51.186356
3488.453729	300159.296378	51.191361
3487.824797	298107.125385	51.196365
3487.647041	296053.535827	51.201370
3487.523166	293975.170891	51.206375
3486.705734	291895.051341	51.211380
3486.631288	289793.453450	51.216385
3486.203588	287699.825012	51.221389
3485.731797	285580.246704	51.226394
3485.860762	283442.962339	51.231399
3485.103238	281312.394984	51.236404
3485.239947	279157.530492	51.241409
3484.378544	276991.019520	51.246413
3484.047743	274815.073403	51.251418
3484.264271	272629.156698	51.256423
3483.456809	270443.727048	51.261428
3482.959568	268227.666789	51.266433
3482.469635	266006.115551	51.271437
3481.767028	263777.228851	51.276442
3481.457310	261545.642947	51.281447
3481.011874	259308.369153	51.286452
3480.814413	257052.432276	51.291457
3480.183658	254798.096735	51.296461
3479.634306	252526.940377	51.301466
3479.840537	250256.194760	51.306471
3478.914378	247972.636202	51.311476
3478.689105	245663.908420	51.316481
3478.310142	243368.897060	51.321485
3477.847305	241051.072563	51.326490
3477.140950	238724.014340	51.331495
3476.467279	236396.464656	51.336500
3476.162762	234057.036501	51.341505
3475.527069	231732.108769	51.346509
3475.311818	229372.126274	51.351514
3474.975044	227018.618693	51.356519
3474.026390	224659.118377	51.361524
3473.757740	222281.490830	51.366529
3473.187304	219899.658615	51.371533
3472.708193	217512.412311	51.376538
3472.162642	215134.092678	51.381543
3471.231787	212740.313092	51.386548
3471.066142	210340.989828	51.391553
3470.275457	207936.084051	51.396557
3469.928056	205518.937599	51.401562
3469.564468	203104.463528	51.406567
3468.738215	200694.777969	51.411572
3468.067412	198256.976160	51.416577
3467.439844	195825.221163	51.421581
3466.924947	193393.254605	51.426586
3466.161486	190942.801524	51.431591
3465.411893	188509.585454	51.436596
3465.187772	186062.977186	51.441601
3464.675422	183607.371362	51.446605
3463.886040	181153.243771	51.451610
3462.984564	178699.526261	51.456615
3461.989462	176245.672125	51.461620
3461.660108	173782.012739	51.466625
3460.926646	171326.267956	51.471629
3460.022983	168867.879070	51.476634
3459.536069	166401.750379	51.481639
3458.768972	163942.889135	51.486644
3458.220583	161476.266552	51.491649
3457.121549	159015.641419	51.496653
3456.535355	156559.690087	51.501658
3456.278844	154086.495762	51.506663
3455.324937	151633.361609	51.511668
3454.435453	149162.657452	51.516673
3453.555841	146702.182716	51.521677
3452.750197	144171.470957	51.526682
3452.155992	141715.159422	51.531687
3451.212337	139255.543228	51.536692
3450.560182	136792.110524	51.541697
3449.752167	134343.195032	51.546701
3448.822141	131890.819626	51.551706
3448.077136	129435.648008	51.556711
3446.715281	126997.798382	51.561716
3446.257575	124553.680582	51.566721
3445.449683	122122.433102	51.571725
3444.344833	119685.447332	51.576730
3443.784050	117256.597048	51.581735
3442.728176	114839.846717	51.586740
3442.042986	112416.440909	51.591745
3440.652709	109998.862835	51.596749
3439.840065	107589.778269	51.601754
3438.864638	105179.626016	51.606759
3437.942309	102796.789519	51.611764
3437.039824	100392.745891	51.616769
3436.081885	98022.829186	51.621773
3435.123005	95646.879955	51.626778
3433.972786	93276.917566	51.631783
3432.822656	90928.743462	51.636788
3431.880469	88569.756268	51.641793
3430.915718	86230.969043	51.646797
3429.609396	83908.436985	51.651802
3428.940595	81584.147839	51.656807
3427.353581	79277.087882	51.661812
3426.419612	76977.372368	51.666817
3425.343557	74699.120433	51.671821
3423.738349	72426.346523	51.676826
3422.590905	70170.865939	51.681831
3420.779376	67938.655634	51.686836
3419.835463	65706.155066	51.691841
3418.553497	63498.994719	51.696845
3417.078164	61316.295483	51.701850
3416.010730	59148.393950	51.706855
3414.202235	56988.616057	51.711860
3412.999005	54858.189614	51.716865
3411.784138	52752.297433	51.721869
3409.947815	50651.858989	51.726874
3408.504160	48581.756296	51.731879
3406.960576	46536.841674	51.736884
3405.363536	44509.680324	51.741889
3403.738865	42515.639913	51.746893
3401.940597	40540.622797	51.751898
3400.383359	38592.352680	51.756903
3398.374474	36679.482788	51.761908
3395.685870	34798.169747	51.766913
3393.769506	32962.262735	51.771917
3390.817159	31173.754120	51.776922
3387.280165	29451.322604	51.781927
3380.808726	27853.084732	51.786932
3374.209124	26349.632992	51.791937
3367.109530	24962.184118	51.796941
3359.428538	23695.418001	51.801946
3352.879302	22550.872300	51.806951
3346.769597	21532.742346	51.811956
3341.204273	20623.313592	51.816961
3336.097701	19847.217444	51.821965
3331.704967	19163.613321	51.826970
3328.191919	18571.287326	51.831975
3324.736661	18077.088110	51.836980
3322.007893	17643.952219	51.841985
3319.808802	17292.489350	51.846989
3317.716126	16991.492209	51.851994
3316.008534	16757.368576	51.856999
3314.141338	16551.158889	51.862004
3312.900159	16398.635450	51.867009
3311.961892	16272.106497	51.872013
3311.349731	16184.687034	51.877018
3310.495881	16120.392115	51.882023
3309.382412	16086.173863	51.887028
3309.297024	16060.262429	51.892033
3308.939844	16040.145617	51.897037
3308.536945	16026.687234	51.902042
3308.331908	16025.203426	51.907047
3307.800433	16045.786525	51.912052
3307.884585	16048.997876	51.917057
3307.857112	16060.238104	51.922061
3307.537645	16080.491062	51.927066
3307.344055	16090.362553	51.932071
3307.322986	16109.510397	51.937076
3306.909069	16115.359307	51.942081
3307.221628	16124.373084	51.947085
3307.013243	16138.071877	51.952090
3306.790207	16137.120593	51.957095
3306.698772	16146.135434	51.962100
3306.667557	16130.761156	51.967105
3306.492988	16121.597353	51.972109
3306.545579	16114.578964	51.977114
3306.356531	16092.133781	51.982119
3306.423092	16071.122701	51.987124
3306.135882	16019.025851	51.992129
3306.104843	15992.297621	51.997133
3305.954995	15935.243367	52.002138
3305.660934	15874.613677	52.007143
3305.474874	15826.117800	52.012148
3305.234649	15760.229088	52.017153
3304.507687	15705.908797	52.022157
3304.148199	15631.256917	52.027162
3303.922994	15581.093186	52.032167
3303.077771	15518.128254	52.037172
3302.832584	15439.544596	52.042177
3302.439959	15362.930389	52.047181
3301.515818	15285.195168	52.052186
3301.422301	15225.301652	52.057191
3300.642892	15162.096089	52.062196
3300.197433	15077.493906	52.067201
3299.748319	14986.691419	52.072205
3299.331160	14908.455718	52.077210
3298.580524	14828.083824	52.082215
3298.071335	14750.375041	52.087220
3297.596520	14667.869171	52.092225
3297.021053	14574.822737	52.097229
3295.999622	14502.367131	52.102234
3295.825727	14423.066532	52.107239
3295.440524	14330.665338	52.112244
3294.701782	14244.363362	52.117249
3294.394583	14157.041524	52.122253
3293.744764	14070.688915	52.127258
3293.043047	13966.452226	52.132263
3292.260411	13883.411824	52.137268
3292.080346	13787.380362	52.142273
3291.633844	13695.588936	52.147277
3290.769765	13609.765211	52.152282
3290.271683	13501.242674	52.157287
3289.281759	13406.867204	52.162292
3288.947685	13307.456313	52.167297
3287.950716	13228.659165	52.172301
3287.518256	13136.805237	52.177306
3287.162360	13034.921977	52.182311
3286.271470	12940.190941	52.187316
3285.726439	12843.805404	52.192321
3285.003158	12749.467155	52.197325
3284.322593	12662.149050	52.202330
3283.978266	12558.724536	52.207335
3283.294607	12470.230778	52.212340
3282.578229	12361.211052	52.217345
3282.290154	12260.275386	52.222349
3281.168533	12161.070731	52.227354
3280.844362	12057.767590	52.232359
3279.972829	11978.101760	52.237364
3279.227322	11874.111734	52.242369
3278.596931	11779.606758	52.247373
3277.722504	11685.106093	52.252378
3277.250014	11583.517188	52.257383
3276.264666	11497.322292	52.262388
3276.147672	11413.359024	52.267393
3275.292898	11313.229103	52.272397
3274.496117	11223.051822	52.277402
3274.456647	11126.292958	52.282407
3273.270608	11026.301964	52.287412
3272.851549	10929.201474	52.292417
3272.366772	10835.817814	52.297421
3271.998894	10745.294984	52.302426
3271.388048	10644.040479	52.307431
3270.376004	10541.940354	52.312436
3269.992827	10435.805732	52.317441
3269.329264	10335.208340	52.322445
3268.458717	10240.118160	52.327450
3267.981283	10131.717067	52.332455
3267.231407	10043.882862	52.337460
3266.470399	9947.489646	52.342465
3265.991406	9854.500848	52.347469
3265.068486	9747.826223	52.352474
3264.371174	9639.707689	52.357479
3263.800782	9561.645256	52.362484
3263.604900	9458.011181	52.367489
3262.437533	9356.902409	52.372493
3261.915882	9261.729911	52.377498
3261.420645	9166.311749	52.382503
3260.524871	9069.404893	52.387508
3259.932234	8968.664819	52.392513
3259.177083	8882.030539	52.397517
3258.596253	8780.362288	52.402522
3257.941088	8683.084887	52.407527
3257.223253	8589.480639	52.412532
3256.996915	8491.579798	52.417537
3256.059056	8400.116869	52.422541
3255.218248	8309.299782	52.427546
3254.469252	8205.872463	52.432551
3253.940922	8117.272332	52.437556
3253.098509	8010.645155	52.442561
3253.045046	7916.197540	52.447565
3252.514719	7827.043293	52.452570
3251.537190	7717.807024	52.457575
3250.343037	7633.281939	52.462580
3249.711665	7532.931019	52.467585
3249.658124	7444.147637	52.472589
3248.294123	7350.315024	52.477594
3248.081851	7256.552368	52.482599
3247.680795	7170.419650	52.487604
3246.402440	7071.050924	52.492609
3246.041535	6980.160923	52.497613
3245.333983	6897.786173	52.502618
3244.989852	6805.608511	52.507623
3243.974311	6709.695885	52.512628
3243.231761	6607.989188	52.517633
3242.945261	6523.690027	52.522637
3241.794072	6428.924523	52.527642
3241.567272	6341.540757	52.532647
3241.046474	6241.916649	52.537652
3240.063265	6146.601298	52.542657
3239.060519	6061.988611	52.547661
3238.548311	5969.572002	52.552666
3238.413348	5875.074477	52.557671
3236.928798	5791.906257	52.562676
3236.832040	5695.920134	52.567681
3235.654507	5599.078363	52.572685
3235.100318	5520.412015	52.577690
3234.343323	5425.003881	52.582695
3233.782163	5350.711451	52.587700
3233.370072	5267.334319	52.592705
3232.630276	5177.825455	52.597709
3231.821789	5089.064833	52.602714
3231.409302	5008.577855	52.607719
3230.391825	4922.890257	52.612724
3229.745317	4828.637144	52.617729
3229.363971	4746.936362	52.622733
3228.582301	4671.025640	52.627738
3228.045538	4577.399647	52.632743
3227.083896	4496.784805	52.637748
3226.688622	4410.119502	52.642753
3226.160190	4323.437937	52.647757
3224.947020	4239.629744	52.652762
3224.693405	4150.539506	52.657767
3223.670570	4088.024294	52.662772
3223.191702	4005.794381	52.667777
3222.569875	3922.104783	52.672781
3221.982467	3840.377533	52.677786
3221.326926	3749.755237	52.682791
3220.519191	3668.410006	52.687796
3219.923863	3589.892889	52.692801
3219.171506	3510.703381	52.697805
3218.352066	3435.046650	52.702810
3217.905881	3349.931648	52.707815
3217.016053	3282.823433	52.712820
3216.328057	3198.379089	52.717825
3215.794939	3113.957692	52.722829
3214.749500	3043.396501	52.727834
3214.163153	2972.161045	52.732839
3213.466170	2907.544246	52.737844
3212.906176	2825.070598	52.742849
3212.339729	2748.466693	52.747853
3211.463891	2685.627136	52.752858
3210.946508	2604.114602	52.757863
3210.177673	2534.632003	52.762868
3209.446899	2466.480745	52.767873
3208.775776	2397.585290	52.772877
3207.961594	2333.592518	52.777882
3207.510380	2256.465204	52.782887
3206.439853	2202.803971	52.787892
3206.004644	2131.092496	52.792897
3205.351840	2066.076032	52.797901
3204.785113	2003.947515	52.802906
3203.944724	1925.587133	52.807911
3203.095120	1871.624001	52.812916
3202.190129	1811.958193	52.817921
3202.085982	1749.375832	52.822925
3201.402023	1686.283257	52.827930
3200.906866	1619.703694	52.832935
3200.007789	1558.264160	52.837940
3199.286970	1492.040687	52.842945
3198.728620	1437.457279	52.847949
3197.809213	1377.505043	52.852954
3197.273513	1311.424005	52.857959
3196.476125	1246.835918	52.862964
3195.761823	1202.372699	52.867969
3194.955190	1135.833403	52.872973
3194.078534	1092.286430	52.877978
3193.557295	1032.667373	52.882983
3192.716451	977.236958	52.887988
3192.167269	930.630842	52.892993
3191.578681	877.246296	52.897997
3190.495073	824.644810	52.903002
3190.228041	767.050615	52.908007
3189.848145	725.659965	52.913012
3188.704583	674.942280	52.918017
3188.193557	626.270002	52.923021
3187.273158	582.565738	52.928026
3186.911424	523.770453	52.933031
3186.201726	488.684687	52.938036
3185.261973	430.812716	52.943041
3185.132561	381.925212	52.948045
3184.144504	345.596939	52.953050
3183.129873	300.656682	52.958055
3182.515027	270.483038	52.963060
3181.432382	217.641860	52.968065
3180.420239	177.264220	52.973069
3179.276265	153.327530	52.978074
3178.556054	129.162560	52.983079
3177.244642	128.051244	52.988084
3175.666149	141.706933	52.993089
3175.199012	136.738956	52.998093
3174.328991	138.516635	53.003098
3174.129336	147.841059	53.008103
3173.584518	139.840630	53.013108
3173.573870	142.393175	53.018113
3172.629238	144.639513	53.023117
3171.278493	156.418845	53.028122
3170.802317	151.149651	53.033127
3170.380315	145.429898	53.038132
3169.843605	151.718821	53.043137
3169.035424	143.092744	53.048141
3168.347359	153.212311	53.053146
3168.334411	136.276735	53.058151
3167.291015	149.058264	53.063156
3166.677776	145.203118	53.068161
3166.179599	140.047027	53.073165
3165.689488	144.016459	53.078170
3165.002661	143.967617	53.083175
3163.691440	142.213258	53.088180
3163.195074	141.982274	53.093185
3162.665143	143.241992	53.098189
3162.174074	147.371848	53.103194
3161.579231	139.129711	53.108199
3160.977185	148.320783	53.113204
3160.190023	147.168846	53.118209
3159.542533	146.200673	53.123213
3159.048898	150.971218	53.128218
3158.432186	146.062741	53.133223
3157.664212	146.321048	53.138228
3157.045910	151.485516	53.143233
3156.421781	141.205269	53.148237
3155.264499	150.190818	53.153242
3155.296974	150.295787	53.158247
3154.226866	151.191491	53.163252
3153.929897	138.065807	53.168257
3153.142380	143.359444	53.173261
3152.025223	148.925714	53.178266
3151.821250	134.035106	53.183271
3151.076937	143.609289	53.188276
3150.363263	139.024876	53.193281
3150.185957	140.101587	53.198285
3149.018978	145.261114	53.203290
3148.642327	136.717629	53.208295
3148.070347	151.568701	53.213300
3147.454690	148.371192	53.218305
3146.451905	143.447366	53.223309
3145.797080	142.094799	53.228314
3145.310609	141.111748	53.233319
3144.551630	134.497888	53.238324
3144.494812	138.420525	53.243329
3143.710100	136.263196	53.248333
3142.491114	145.176788	53.253338
3142.280965	138.518496	53.258343
3141.071911	147.710254	53.263348
3140.775656	143.470172	53.268353
3140.586199	135.600873	53.273357
3139.254539	137.364669	53.278362
3138.723835	133.538848	53.283367
3138.387471	139.737486	53.288372
3137.451547	133.603453	53.293377
3136.772834	132.976532	53.298381
3135.976986	139.591956	53.303386
3136.279441	132.848455	53.308391
3135.043220	143.996387	53.313396
3134.366931	141.827244	53.318401
3133.770317	135.417349	53.323405
3132.681610	146.261796	53.328410
3132.596406	135.041999	53.333415
3132.278133	137.466712	53.338420
3131.353196	134.114818	53.343425
3130.663703	132.422396	53.348429
3129.362451	139.690212	53.353434
3128.454509	133.253382	53.358439
3128.037231	133.545718	53.363444
3127.727788	135.796821	53.368449
3127.135004	137.298195	53.373453
3126.058317	131.614523	53.378458
3125.771479	134.481485	53.383463
3125.536370	136.672915	53.388468
3124.580972	133.910425	53.393473
3123.706236	133.068713	53.398477
3122.416925	141.697880	53.403482
3122.275513	128.174983	53.408487
3121.799507	138.954214	53.413492
3120.628285	128.966402	53.418497
3120.833146	122.475627	53.423501
3120.184599	135.358627	53.428506
3119.853357	136.449008	53.433511
3119.195805	133.171429	53.438516
3118.117941	129.824748	53.443521
3117.258500	131.262344	53.448525
3116.392894	135.042518	53.453530
3115.754111	135.434278	53.458535
3114.832157	135.824291	53.463540
3114.302354	135.457713	53.468545
3114.074354	122.662494	53.473549
3113.476154	132.431965	53.478554
3112.963550	121.159683	53.483559
3112.122666	130.512734	53.488564
3111.454723	130.476067	53.493569
3110.392735	119.264892	53.498573
3110.017566	128.949281	53.503578
3110.025825	122.730513	53.508583
3109.372555	126.860844	53.513588
3107.988226	124.369404	53.518593
3107.514431	130.220870	53.523597
3106.512085	134.549396	53.528602
3106.167910	131.163803	53.533607
3105.202743	129.499540	53.538612
3104.140748	127.797348	53.543617
3104.239269	125.223070	53.548621
3104.042640	143.260183	53.553626
3103.325283	127.084445	53.558631
3103.059622	132.444045	53.563636
3101.618172	135.290792	53.568641
3100.680916	131.112872	53.573645
3100.001937	131.080065	53.578650
3099.732250	127.073472	53.583655
3099.006023	132.667683	53.588660
3098.215166	129.343808	53.593665
3097.253839	130.227250	53.598669
3096.382279	133.224908	53.603674
3096.648928	129.010625	53.608679
3095.924365	129.658618	53.613684
3095.135699	133.293808	53.618689
3094.809752	124.960354	53.623693
3093.792507	132.740553	53.628698
3093.489904	129.106286	53.633703
3092.570256	138.537930	53.638708
3091.512453	132.704991	53.643713
3091.181527	131.271037	53.648717
3090.601529	136.042520	53.653722
3089.469979	120.788201	53.658727
3088.583121	129.426757	53.663732
3087.982150	130.644540	53.668737
3087.157221	131.617965	53.673741
3087.085378	138.621647	53.678746
3086.682762	129.372892	53.683751
3086.314834	134.178006	53.688756
3085.333962	131.539084	53.693761
3085.184201	123.379207	53.698765
3083.101709	131.755884	53.703770
3083.395574	125.855018	53.708775
3082.752841	134.183845	53.713780
3082.072824	122.787019	53.718785
3081.178037	121.665722	53.723789
3080.045512	135.006406	53.728794
3079.680433	132.745808	53.733799
3078.899207	142.469981	53.738804
3078.028350	138.010330	53.743809
3077.775439	134.363231	53.748813
3077.691835	131.016800	53.753818
3077.253702	133.266998	53.758823
3075.540948	135.599990	53.763828
3075.426723	131.911826	53.768833
3075.221328	133.143729	53.773837
3073.887582	138.407548	53.778842
3072.927583	135.340729	53.783847
3072.671682	125.647314	53.788852
3072.105896	134.209303	53.793857
3071.710427	132.416914	53.798861
3070.925594	131.368802	53.803866
3070.595192	131.962869	53.808871
3069.191129	134.052463	53.813876
3068.290996	131.348040	53.818881
3068.260614	129.446692	53.823885
3067.362643	129.173815	53.828890
3067.151493	130.994844	53.833895
3066.378720	130.754257	53.838900
3064.985705	137.321726	53.843905
3064.171523	129.321954	53.848909
3063.472319	136.997685	53.853914
3063.623377	126.280284	53.858919
3062.997518	138.939151	53.863924
3062.273991	134.947345	53.868929
3061.670231	129.110646	53.873933
3060.636949	133.274730	53.878938
3059.883673	124.702068	53.883943
3059.095256	130.457693	53.888948
3058.799293	133.454502	53.893953
3058.148049	122.718671	53.898957
3057.567938	130.900220	53.903962
3057.310446	129.510167	53.908967
3056.212917	131.068188	53.913972
3055.286010	129.940146	53.918977
3054.875580	128.883719	53.923981
3054.480172	134.542192	53.928986
3053.808440	127.187542	53.933991
3052.682902	127.898133	53.938996
3052.253472	135.446058	53.944001
3051.584213	129.405032	53.949005
3051.326026	132.173944	53.954010
3050.372906	133.345326	53.959015
3049.666069	130.187493	53.964020
3048.915813	129.967139	53.969025
3048.505416	125.950253	53.974029
3047.684473	128.460069	53.979034
3047.024512	128.708617	53.984039
3046.431118	128.406594	53.989044
3045.667665	131.266183	53.994049
3045.216728	126.970442	53.999053
3044.256181	130.481852	54.004058
3043.775623	127.432194	54.009063
3043.209410	125.204390	54.014068
3042.571676	125.340591	54.019073
3041.743010	119.400227	54.024077
3040.995436	122.161973	54.029082
3040.072899	118.102735	54.034087
3039.722400	128.219868	54.039092
3039.221909	133.569858	54.044097
3038.712902	122.679072	54.049101
3037.778498	133.685041	54.054106
3037.303500	120.119300	54.059111
3036.205163	125.348817	54.064116
3035.782315	125.094230	54.069121
3035.338652	126.745389	54.074125
3034.308195	124.557835	54.079130
3034.102303	130.515495	54.084135
3033.303463	130.563571	54.089140
3032.562006	125.246184	54.094145
3031.995453	123.906970	54.099149
3031.261137	126.989734	54.104154
3030.784481	125.892915	54.109159
3030.243953	124.531492	54.114164
3028.974123	117.751143	54.119169
3028.270525	120.712213	54.124173
3028.055792	122.978316	54.129178
3027.590595	123.417002	54.134183
3026.332230	119.480675	54.139188
3025.904657	118.603623	54.144193
3025.629356	117.070173	54.149197
3024.128541	135.171435	54.154202
3023.807336	124.554869	54.159207
3023.584845	121.323752	54.164212
3022.822274	124.445291	54.169217
3022.150453	122.274614	54.174221
3020.897691	127.974194	54.179226
3020.544446	124.718447	54.184231
3019.674055	118.804560	54.189236
3019.189143	125.048310	54.194241
3019.291784	116.004942	54.199245
3018.278320	122.224537	54.204250
3017.420852	120.026374	54.209255
3016.748110	123.838335	54.214260
3016.090564	124.980925	54.219265
3015.519775	127.038667	54.224269
3014.556282	129.859812	54.229274
3014.279829	119.838746	54.234279
3013.703867	124.206128	54.239284
3013.033715	119.066822	54.244289
3012.677103	109.863518	54.249293
3011.647065	125.128740	54.254298
3010.655426	117.062602	54.259303
3009.716695	128.312065	54.264308
3009.103172	120.094474	54.269313
3008.527287	124.204877	54.274317
3007.934937	129.822004	54.279322
3007.972781	119.802100	54.284327
3006.811868	124.201546	54.289332
3005.832639	120.974612	54.294337
3005.449335	127.325734	54.299341
3004.970678	124.633774	54.304346
3004.397707	112.625408	54.309351
3003.486168	119.024161	54.314356
3003.078454	124.272245	54.319361
3002.768112	116.947826	54.324365
3001.844285	122.114765	54.329370
3001.104451	117.936291	54.334375
3000.058020	124.757559	54.339380
2999.222291	127.022413	54.344385
2998.832655	117.428445	54.349389
2998.400036	119.565206	54.354394
2997.501475	121.806455	54.359399
2996.534022	117.574906	54.364404
2996.518743	116.901738	54.369409
2995.667591	117.486113	54.374413
2994.478809	121.407966	54.379418
2994.398946	118.147349	54.384423
2993.620835	123.007948	54.389428
2993.027235	120.656939	54.394433
2992.945601	120.568648	54.399437
2991.931662	127.060690	54.404442
2991.638509	121.393161	54.409447
2990.875519	117.033913	54.414452
2989.443643	118.821969	54.419457
2988.635255	116.680554	54.424461
2987.999224	127.364752	54.429466
2987.862745	118.892758	54.434471
2987.032860	123.451161	54.439476
2986.094896	125.568096	54.444481
2985.666721	118.734723	54.449485
2985.063990	119.673349	54.454490
2984.666929	117.791244	54.459495
2983.933742	125.291204	54.464500
2983.076725	138.752182	54.469505
2983.201808	120.746649	54.474509
2982.158102	126.186701	54.479514
2980.879627	120.279399	54.484519
2980.315351	126.296324	54.489524
2979.498488	125.822105	54.494529
2979.467496	120.796998	54.499533
2978.205083	126.065613	54.504538
2977.472212	126.610041	54.509543
2976.944899	125.958057	54.514548
2976.293573	128.132589	54.519553
2975.890127	114.301226	54.524557
2975.238215	118.344491	54.529562
2974.443858	114.892558	54.534567
2974.116328	120.168780	54.539572
2973.340616	120.051073	54.544577
2973.082676	112.019830	54.549581
2972.306992	124.560605	54.554586
2971.665089	118.990962	54.559591
2970.444612	119.718977	54.564596
2969.570159	119.157103	54.569601
2969.208490	116.109245	54.574605
2968.193108	120.578956	54.579610
2967.754849	118.341138	54.584615
2967.162871	121.462345	54.589620
2966.514911	123.793402	54.594625
2966.206494	119.337927	54.599629
2965.304112	115.546438	54.604634
2965.180409	112.482784	54.609639
2964.789074	115.983376	54.614644
2963.748085	118.105287	54.619649
2962.849007	117.951429	54.624653
2961.781310	123.445317	54.629658
2961.074288	120.400423	54.634663
2960.608009	123.857773	54.639668
2960.040641	123.904987	54.644673
2959.430692	128.085949	54.649677
2958.403131	123.903756	54.654682
2957.903747	112.587413	54.659687
2957.563268	114.738035	54.664692
2957.073976	115.967138	54.669697
2956.567246	109.276668	54.674701
2955.310532	116.711752	54.679706
2954.382503	109.700919	54.684711
2953.495106	113.560616	54.689716
2952.665655	121.259390	54.694721
2952.773940	119.239616	54.699725
2952.349389	120.696861	54.704730
2951.556940	125.072822	54.709735
2950.775785	124.872366	54.714740
2950.326143	125.293795	54.719745
2949.731340	114.384142	54.724749
2949.022657	119.292483	54.729754
2948.485851	113.283319	54.734759
2947.313675	115.585147	54.739764
2946.250227	117.373408	54.744769
2946.606812	115.578038	54.749773
2945.633925	116.215590	54.754778
2944.874560	109.402115	54.759783
2944.242179	118.022843	54.764788
2943.476478	117.562386	54.769793
2942.955627	107.094828	54.774797
2942.696239	117.430846	54.779802
2942.084540	117.672343	54.784807
2940.679244	114.716387	54.789812
2939.911108	116.826410	54.794817
2939.476499	112.735522	54.799821
2938.819303	114.714090	54.804826
2938.297115	116.543273	54.809831
2937.947137	119.305372	54.814836
2936.994491	124.656053	54.819841
2936.917006	114.085489	54.824845
2935.986383	117.809685	54.829850
2934.570050	111.462155	54.834855
2933.796585	115.661586	54.839860
2933.151449	121.202868	54.844865
2933.426498	114.183017	54.849869
2932.203376	118.951909	54.854874
2932.038644	114.454122	54.859879
2931.728289	113.180872	54.864884
2930.918059	115.654528	54.869889
2929.555424	110.021357	54.874893
2927.858430	118.896254	54.879898
2928.195580	119.155992	54.884903
2928.296697	115.120391	54.889908
2926.955675	120.379552	54.894913
2926.327601	110.192812	54.899917
2925.646819	115.265328	54.904922
2924.981928	110.747229	54.909927
2924.624684	114.138578	54.914932
2923.905659	106.863095	54.919937
2923.801373	116.404863	54.924941
2922.038026	119.788618	54.929946
2921.422255	106.282498	54.934951
2920.648698	112.001641	54.939956
2920.238024	117.273123	54.944961
2920.208249	110.582464	54.949965
2919.278313	122.498694	54.954970
2918.371151	113.910133	54.959975
2918.335180	113.840486	54.964980
2917.568247	128.743390	54.969985
2916.422474	118.658143	54.974989
2915.459541	120.550413	54.979994
2914.567402	111.519562	54.984999
2914.637849	108.380496	54.990004
2914.175611	109.623531	54.995009
2913.364606	109.150690	55.000013
2912.693782	116.287896	55.005018
2912.138879	112.628479	55.010023
2911.917587	108.262331	55.015028
2910.030161	112.191488	55.020033
2909.679741	108.864617	55.025037
2908.566487	113.363690	55.030042
2908.595780	105.697439	55.035047
2907.818906	112.287125	55.040052
2907.176585	113.530542	55.045057
2906.912098	107.416824	55.050061
2906.152970	111.211186	55.055066
2905.567899	108.216513	55.060071
2905.234753	115.015362	55.065076
2903.837817	106.137492	55.070081
2903.029437	112.166921	55.075085
2902.385039	110.233542	55.080090
2902.166698	115.732280	55.085095
2901.757693	105.679027	55.090100
2900.650285	113.428854	55.095105
2900.398372	106.502221	55.100109
2899.399958	107.114539	55.105114
2898.060875	102.736926	55.110119
2897.895943	105.258195	55.115124
2897.014055	114.497861	55.120129
2896.371473	107.077876	55.125133
2895.840478	115.263657	55.130138
2895.349065	113.754517	55.135143
2895.042698	100.993669	55.140148
2894.326218	106.787134	55.145153
2893.850693	104.153864	55.150157
2893.155652	112.451755	55.155162
2892.374965	111.894790	55.160167
2891.629411	111.966541	55.165172
2890.747672	109.632816	55.170177
2890.446779	104.045967	55.175181
2889.536628	114.833053	55.180186
2888.638828	100.728979	55.185191
2887.700388	107.694029	55.190196
2886.921166	111.296437	55.195201
2886.890687	106.656899	55.200205
2886.160206	116.625014	55.205210
2885.879700	105.540883	55.210215
2885.237933	115.814748	55.215220
2884.424159	113.536118	55.220225
2884.137942	109.482638	55.225229
2882.386424	110.776674	55.230234
2881.834820	99.808745	55.235239
2881.338952	109.985438	55.240244
2880.366476	117.486427	55.245249
2880.488742	102.357389	55.250253
2880.052194	111.003461	55.255258
2879.510806	103.276458	55.260263
2878.425953	104.699714	55.265268
2877.104996	107.080662	55.270273
2876.568451	102.276962	55.275277
2876.100007	105.086937	55.280282
2875.194831	104.368097	55.285287
2874.676613	103.043142	55.290292
2873.817855	112.209384	55.295297
2873.707359	101.100150	55.300301
2873.426893	105.439140	55.305306
2873.089862	103.400344	55.310311
2872.024753	103.594997	55.315316
2870.587326	106.644781	55.320321
2870.252273	100.478395	55.325325
2869.530619	104.974886	55.330330
2869.063169	109.231757	55.335335
2868.894759	108.111485	55.340340
2867.655552	108.250237	55.345345
2867.048879	100.743205	55.350349
2866.218625	105.165496	55.355354
2865.479061	105.260700	55.360359
2864.635812	106.281098	55.365364
2864.084138	115.017503	55.370369
2864.129075	108.205531	55.375373
2863.637177	111.945937	55.380378
2862.848412	101.844309	55.385383
2861.930717	104.894479	55.390388
2860.592373	113.615332	55.395393
2860.634519	110.055194	55.400397
2859.780094	119.257410	55.405402
2859.110236	109.752413	55.410407
2858.921530	114.181904	55.415412
2857.294138	106.854052	55.420417
2856.815742	105.128751	55.425421
2856.147128	117.017291	55.430426
2855.623165	115.524376	55.435431
2855.078441	109.701708	55.440436
2854.514399	109.401004	55.445441
2854.262563	113.184855	55.450445
2853.253678	108.708585	55.455450
2853.124484	119.604174	55.460455
2852.002914	112.624073	55.465460
2851.282108	115.611387	55.470465
2850.790559	111.875231	55.475469
2850.194274	113.922342	55.480474
2848.752487	105.277151	55.485479
2848.147647	103.378466	55.490484
2847.700141	110.027914	55.495489
2846.874297	103.989223	55.500493
2846.367092	112.768157	55.505498
2845.968548	106.075400	55.510503
2845.367050	112.464202	55.515508
2844.704192	115.203198	55.520513
2844.588142	110.583812	55.525517
2843.353302	110.357886	55.530522
2842.308981	115.412015	55.535527
2841.667687	110.381095	55.540532
2841.215486	110.014306	55.545537
2840.710932	103.086651	55.550541
2840.055244	108.810915	55.555546
2839.644279	106.969884	55.560551
2839.102320	108.899950	55.565556
2837.700633	112.655719	55.570561
2837.154452	104.725075	55.575565
2836.572153	114.109326	55.580570
2835.903732	104.826717	55.585575
2835.659891	103.039227	55.590580
2835.237098	112.464109	55.595585
2834.150749	108.880532	55.600589
2832.680500	117.025924	55.605594
2832.241528	111.936744	55.610599
2831.717427	118.557839	55.615604
2831.094513	117.448538	55.620609
2830.908315	108.684285	55.625613
2829.981655	110.418003	55.630618
2829.848593	110.604944	55.635623
2829.366089	107.885244	55.640628
2828.018687	112.123960	55.645633
2827.333320	111.644658	55.650637
2826.402601	118.415773	55.655642
2826.022636	103.153900	55.660647
2825.796248	100.477664	55.665652
2825.062115	108.838682	55.670657
2824.509836	107.600077	55.675661
2823.048099	103.770406	55.680666
2822.225980	101.679130	55.685671
2821.790610	105.319483	55.690676
2821.470446	107.949780	55.695681
2821.028779	104.380363	55.700685
2820.242235	112.483112	55.705690
2820.226179	96.416967	55.710695
2819.269084	97.824318	55.715700
2818.126032	108.725022	55.720705
2817.788738	99.586742	55.725709
2816.745143	103.422229	55.730714
2816.485560	105.029306	55.735719
2815.298936	113.013333	55.740724
2814.033091	112.555088	55.745729
2814.222284	96.800039	55.750733
2813.649770	98.781117	55.755738
2812.947704	104.975926	55.760743
2812.567960	96.576725	55.765748
2811.839363	102.317792	55.770753
2811.452149	96.457163	55.775757
2809.908390	103.857639	55.780762
2809.066454	102.275395	55.785767
2808.844949	103.777678	55.790772
2807.994727	105.325445	55.795777
2808.074797	101.372788	55.800781
2807.437482	108.861494	55.805786
2806.618330	101.562495	55.810791
2805.698670	102.783849	55.815796
2804.653945	111.031380	55.820801
2804.199884	99.138928	55.825805
2803.996726	104.402176	55.830810
2803.700890	108.270912	55.835815
2802.440505	102.906088	55.840820
2801.720865	106.191223	55.845825
2801.268516	101.797474	55.850829
2800.571287	100.407599	55.855834
2799.636551	99.145156	55.860839
2798.555177	93.527510	55.865844
2797.656885	102.600247	55.870849
2797.817968	106.971925	55.875853
2797.084320	108.902389	55.880858
2796.400124	106.163088	55.885863
2795.978376	110.391624	55.890868
2795.578514	106.993085	55.895873
2794.882559	105.003404	55.900877
2793.010102	106.984828	55.905882
2792.427316	104.131093	55.910887
2792.099598	97.463347	55.915892
2791.189264	102.872330	55.920897
2791.499659	99.244640	55.925901
2790.517262	99.683321	55.930906
2790.011830	98.026989	55.935911
2789.678925	104.103443	55.940916
2788.482399	100.992643	55.945921
2787.681036	96.943935	55.950925
2786.976215	103.228030	55.955930
2786.512796	92.566755	55.960935
2786.325249	93.556012	55.965940
2785.845351	94.369454	55.970945
2784.193529	98.150615	55.975949
2783.760344	96.980473	55.980954
2783.089648	100.201587	55.985959
2783.199001	103.415691	55.990964
2781.926690	103.474464	55.995969
2781.228572	94.591280	56.000973
2780.188492	101.852385	56.005978
2779.302563	98.662055	56.010983
2778.831529	94.202822	56.015988
2777.901491	105.980908	56.020993
2778.284559	101.158594	56.025997
2777.560513	101.985740	56.031002
2777.440276	97.430629	56.036007
2776.649920	99.865378	56.041012
2775.247385	101.516627	56.046017
2774.689685	94.071112	56.051021
2773.873228	105.335984	56.056026
2773.303454	102.855016	56.061031
2772.780979	98.144846	56.066036
2771.408774	108.683285	56.071041
2770.757051	93.953790	56.076045
2770.319079	101.870646	56.081050
2769.785264	101.346502	56.086055
2769.452718	97.987382	56.091060
2768.958266	92.621128	56.096065
2769.203538	87.122917	56.101069
2767.575289	92.147383	56.106074
2766.727385	96.633486	56.111079
2766.143636	97.636385	56.116084
2765.389651	99.829267	56.121089
2764.916047	92.485035	56.126093
2763.180711	94.942752	56.131098
2762.875244	99.350748	56.136103
2763.140500	102.422154	56.141108
2761.729469	101.486251	56.146113
2761.126857	99.222076	56.151117
2760.948109	100.248513	56.156122
2760.076902	103.339301	56.161127
2760.029914	100.819900	56.166132
2759.097864	99.360038	56.171137
2758.133020	86.296131	56.176141
2757.411140	97.774167	56.181146
2756.829192	95.114894	56.186151
2756.482405	99.546136	56.191156
2754.851594	101.134963	56.196161
2754.394877	91.005825	56.201165
2754.027676	92.718137	56.206170
2753.624527	95.243805	56.211175
2753.305690	95.055145	56.216180
2752.608720	96.134237	56.221185
2752.267684	92.025804	56.226189
2750.755574	91.526379	56.231194
2749.918005	99.322855	56.236199
2749.175265	99.694135	56.241204
2748.690207	109.601747	56.246209
2748.512176	87.935316	56.251213
2747.578211	95.475907	56.256218
2746.489771	101.490450	56.261223
2745.197173	94.931186	56.266228
2745.372486	95.397384	56.271233
2745.572402	96.305416	56.276237
2744.437397	99.241958	56.281242
2744.137700	98.365968	56.286247
2743.471104	99.319873	56.291252
2742.118429	104.803284	56.296257
2741.495269	95.882428	56.301261
2740.979808	102.136131	56.306266
2740.204945	105.869251	56.311271
2739.768719	103.114416	56.316276
2739.052966	103.786996	56.321281
2738.170124	100.754825	56.326285
2737.614496	101.223989	56.331290
2736.739642	90.488581	56.336295
2736.498378	93.927210	56.341300
2735.724343	100.984955	56.346305
2735.115500	99.667216	56.351309
2733.949457	99.650206	56.356314
2733.187239	94.508535	56.361319
2732.625123	96.862435	56.366324
2732.215840	97.693021	56.371329
2731.964560	92.580462	56.376333
2730.979160	97.700316	56.381338
2731.152690	94.669949	56.386343
2730.535992	100.399000	56.391348
2728.861443	104.532603	56.396353
2728.450662	99.030081	56.401357
2727.834974	98.364019	56.406362
2726.932692	98.852963	56.411367
2726.097289	101.898163	56.416372
2725.113236	107.296070	56.421377
2725.326818	98.034043	56.426381
2724.274479	100.095958	56.431386
2724.113392	97.825002	56.436391
2723.469901	102.890758	56.441396
2722.480453	96.812958	56.446401
2721.899859	95.023432	56.451405
2720.496738	97.835285	56.456410
2720.323350	94.211737	56.461415
2719.818071	101.701557	56.466420
2718.971489	88.242852	56.471425
2718.674416	90.278695	56.476429
2718.414976	102.270567	56.481434
2717.614607	95.692305	56.486439
2716.445278	89.432893	56.491444
2715.936266	94.629209	56.496449
2715.397056	91.450679	56.501453
2714.512253	101.631476	56.506458
2713.658508	87.357311	56.511463
2713.249816	96.455702	56.516468
2712.049828	104.179529	56.521473
2712.167423	97.769220	56.526477
2711.987140	103.302100	56.531482
2710.807181	100.033756	56.536487
2710.194880	97.897557	56.541492
2709.286003	95.986914	56.546497
2708.910087	94.288716	56.551501
2707.983290	98.406612	56.556506
2707.032687	104.953769	56.561511
2706.348759	89.447851	56.566516
2705.547193	94.836274	56.571521
2705.237278	90.676739	56.576525
2704.882251	100.579486	56.581530
2704.682655	97.674475	56.586535
2703.497345	93.802725	56.591540
2702.174597	99.874692	56.596545
2701.429004	94.277436	56.601549
2700.903990	90.294006	56.606554
2700.523315	91.767447	56.611559
2700.308162	93.421798	56.616564
2699.470790	98.647007	56.621569
2699.243652	92.130236	56.626573
2697.900803	100.093608	56.631578
2697.202742	97.923913	56.636583
2696.906652	96.244439	56.641588
2695.870618	99.516956	56.646593
2695.835026	97.960712	56.651597
2694.417042	99.683698	56.656602
2693.587518	98.907749	56.661607
2693.001605	97.344523	56.666612
2692.393039	100.522658	56.671617
2692.217626	98.380464	56.676621
2691.681097	96.115266	56.681626
2690.979381	98.703815	56.686631
2690.764825	95.406638	56.691636
2689.387921	102.558358	56.696641
2688.707977	94.276412	56.701645
2687.997899	110.038361	56.706650
2687.476435	100.244761	56.711655
2687.436205	94.340627	56.716660
2686.130212	103.796867	56.721665
2685.215584	95.166232	56.726669
2684.894818	103.110815	56.731674
2684.255070	103.188980	56.736679
2683.943837	104.004783	56.741684
2682.514989	100.052300	56.746689
2681.809188	91.164927	56.751693
2681.121668	96.353074	56.756698
2680.799019	94.320126	56.761703
2680.533696	98.884676	56.766708
2679.754556	101.173049	56.771713
2679.497702	95.020164	56.776717
2678.224247	100.114660	56.781722
2677.147051	94.880003	56.786727
2676.835491	94.746154	56.791732
2675.935461	98.845268	56.796737
2676.118116	91.342690	56.801741
2675.205722	86.388936	56.806746
2674.514982	94.702667	56.811751
2673.817397	83.813431	56.816756
2673.163119	103.686758	56.821761
2672.505935	89.772940	56.826765
2671.228059	91.396194	56.831770
2670.566250	89.214386	56.836775
2670.357116	98.700626	56.841780
2669.688489	95.801584	56.846785
2669.232518	93.625642	56.851789
2668.527878	93.942657	56.856794
2667.455597	100.518904	56.861799
2667.098854	93.459439	56.866804
2666.101202	101.548936	56.871809
2665.749480	84.285774	56.876813
2665.147924	94.686563	56.881818
2664.176126	88.809046	56.886823
2663.276308	95.276077	56.891828
2662.836812	100.339728	56.896833
2662.720402	101.471560	56.901837
2662.023046	97.936791	56.906842
2661.665399	102.337918	56.911847
2660.210432	97.906370	56.916852
2659.220144	99.442574	56.921857
2658.610993	101.229406	56.926861
2658.413532	104.911989	56.931866
2657.687078	94.136234	56.936871
2657.531575	89.663344	56.941876
2656.571591	91.132395	56.946881
2655.993936	83.726632	56.951885
2654.984484	90.279900	56.956890
2654.088976	92.068710	56.961895
2653.645814	87.604337	56.966900
2653.263064	92.524078	56.971905
2652.932106	86.574913	56.976909
2651.866372	92.139151	56.981914
2650.866387	98.680936	56.986919
2650.376449	97.824446	56.991924
2650.023609	99.199187	56.996929
2649.504028	97.108328	57.001933
2648.703240	99.721711	57.006938
2647.518654	92.671923	57.011943
2647.326322	84.863594	57.016948
2646.361064	97.162025	57.021953
2645.935433	85.012133	57.026957
2645.345934	88.938170	57.031962
2644.380815	86.740717	57.036967
2643.493611	79.920750	57.041972
2643.030613	91.735832	57.046977
2642.760815	84.146398	57.051981
2642.083449	90.894339	57.056986
2641.708443	93.215866	57.061991
2640.713705	91.400043	57.066996
2639.382228	98.181253	57.072001
2639.154451	84.616006	57.077005
2638.336171	91.860916	57.082010
2637.985280	82.516585	57.087015
2637.745006	93.250733	57.092020
2636.397302	99.138694	57.097025
2636.007171	95.956399	57.102029
2635.428409	100.070861	57.107034
2634.398212	99.382512	57.112039
2634.280288	94.708600	57.117044
2633.560784	99.864325	57.122049
2632.851039	84.713362	57.127053
2631.832103	98.994197	57.132058
2631.407763	97.448753	57.137063
2630.790197	93.919692	57.142068
2630.204939	94.412877	57.147073
2628.995700	89.953940	57.152077
2628.113057	96.968284	57.157082
2627.633334	99.893879	57.162087
2627.158860	93.082302	57.167092
2626.909128	93.631023	57.172097
2626.636890	89.285061	57.177101
2625.998747	101.682704	57.182106
2624.810345	89.902013	57.187111
2624.245292	91.005935	57.192116
2623.363067	101.967850	57.197121
2622.887910	92.793963	57.202125
2622.276008	96.323977	57.207130
2620.864312	97.293955	57.212135
2620.670475	98.467838	57.217140
2619.659274	100.961277	57.222145
2619.684215	95.774274	57.227149
2619.149971	89.864599	57.232154
2618.388018	95.079685	57.237159
2617.246545	97.729205	57.242164
2616.276007	104.279383	57.247169
2616.070281	88.866608	57.252173
2615.804979	92.557233	57.257178
2615.061029	89.525424	57.262183
2614.653359	80.488031	57.267188
2613.267733	88.998311	57.272193
2612.873434	87.814432	57.277197
2612.209898	90.989337	57.282202
2611.817122	89.451525	57.287207
2610.864863	81.020370	57.292212
2609.690743	99.407602	57.297217
2609.261556	97.319453	57.302221
2608.714665	90.958008	57.307226
2608.175363	94.707315	57.312231
2607.530908	90.766026	57.317236
2607.187366	97.666505	57.322241
2606.768366	94.935977	57.327245
2605.509561	102.275937	57.332250
2604.739006	94.449221	57.337255
2604.472372	81.334691	57.342260
2603.891403	98.358196	57.347265
2603.342549	86.869620	57.352269
2602.177763	93.293928	57.357274
2601.557905	95.005229	57.362279
2601.387477	93.557299	57.367284
2600.222989	95.487226	57.372289
2598.999397	80.404777	57.377293
2598.624256	85.005464	57.382298
2597.917118	91.769156	57.387303
2597.913308	88.550430	57.392308
2597.171270	95.559686	57.397313
2596.800451	94.754283	57.402317
2596.379538	93.983495	57.407322
2594.946361	91.721201	57.412327
2594.649083	94.516138	57.417332
2593.663792	92.886992	57.422337
2593.098932	90.423367	57.427341
2592.159094	88.493962	57.432346
2591.647647	94.621063	57.437351
2591.364819	85.276944	57.442356
2590.505538	86.230648	57.447361
2590.197399	89.897017	57.452365
2588.875542	94.973750	57.457370
2588.083471	94.668241	57.462375
2587.853677	90.427129	57.467380
2586.871119	88.932514	57.472385
2586.725174	85.985184	57.477389
2586.002039	89.437112	57.482394
2585.168686	83.631867	57.487399
2584.378197	85.662460	57.492404
2583.571854	93.526630	57.497409
2583.405682	88.416512	57.502413
2582.806291	84.385422	57.507418
2581.813170	90.812358	57.512423
2581.068815	87.456160	57.517428
2580.202169	88.754929	57.522433
2579.576933	83.775000	57.527437
2579.329762	83.784881	57.532442
2578.851876	89.959136	57.537447
2577.971355	82.731080	57.542452
2576.901608	89.799122	57.547457
2576.865212	87.545147	57.552461
2576.035895	88.517019	57.557466
2575.289632	87.272923	57.562471
2574.135212	83.120015	57.567476
2573.243737	95.445306	57.572481
2573.265007	87.202587	57.577485
2572.921206	84.516049	57.582490
2572.303232	91.148449	57.587495
2571.744438	83.486854	57.592500
2570.655266	91.287667	57.597505
2570.286840	86.283967	57.602509
2569.754102	80.088661	57.607514
2568.546264	87.886865	57.612519
2567.561181	81.920858	57.617524
2566.779015	89.318672	57.622529
2566.237946	87.638458	57.627533
2565.797110	94.250446	57.632538
2565.427770	96.168389	57.637543
2565.204818	89.885780	57.642548
2564.093128	90.440547	57.647553
2563.582337	85.451713	57.652557
2562.810495	85.839833	57.657562
2562.383510	86.258994	57.662567
2561.036523	84.218022	57.667572
2559.966419	92.293462	57.672577
2559.560446	79.888793	57.677581
2559.060121	87.974584	57.682586
2558.357639	83.515479	57.687591
2558.023553	79.306017	57.692596
2557.546223	90.563826	57.697601
2557.050072	88.434633	57.702605
2556.349763	91.414124	57.707610
2555.192477	89.177701	57.712615
2554.974378	76.371455	57.717620
2554.202344	92.046081	57.722625
2553.610102	76.023247	57.727629
2553.106390	83.902385	57.732634
2551.663907	85.182763	57.737639
2551.206588	83.035881	57.742644
2550.622249	86.723022	57.747649
2550.183728	84.197543	57.752653
2549.803194	80.381667	57.757658
2548.719679	92.303617	57.762663
2548.362850	86.035214	57.767668
2547.465271	89.921956	57.772673
2546.845927	81.373510	57.777677
2546.175598	93.232717	57.782682
2545.449283	86.463421	57.787687
2544.448825	77.497780	57.792692
2543.653045	83.089296	57.797697
2543.241687	87.017646	57.802701
2543.019712	89.201307	57.807706
2542.477041	86.963626	57.812711
2542.242852	90.276312	57.817716
2540.726296	86.649518	57.822721
2540.333522	89.877609	57.827725
2539.708362	86.766295	57.832730
2539.164198	88.266115	57.837735
2538.413418	83.849216	57.842740
2537.287019	86.460647	57.847745
2536.771426	82.847461	57.852749
2536.290461	77.765905	57.857754
2535.925236	93.348484	57.862759
2535.479543	85.010738	57.867764
2533.692319	86.852542	57.872769
2533.465627	83.369170	57.877773
2533.034913	84.502237	57.882778
2532.859299	91.329399	57.887783
2531.099819	90.472865	57.892788
2530.319994	93.245302	57.897793
2530.176902	86.690895	57.902797
2529.755660	86.963425	57.907802
2528.877412	92.384708	57.912807
2528.810536	91.828917	57.917812
2527.854836	101.414362	57.922817
2526.926010	93.349862	57.927821
2526.220307	92.975915	57.932826
2525.485293	90.407577	57.937831
2525.495484	85.789928	57.942836
2524.616296	89.904835	57.947841
2523.977469	83.867405	57.952845
2523.000508	83.317209	57.957850
2522.485384	89.120476	57.962855
2522.027542	77.640443	57.967860
2520.878754	85.898673	57.972865
2519.971303	84.311102	57.977869
2519.558511	90.163977	57.982874
2518.750235	92.432875	57.987879
2518.380943	83.696031	57.992884
2518.037032	89.281349	57.997889
2517.715422	91.122451	58.002893
2516.111860	88.890099	58.007898
2515.265618	87.970199	58.012903
2515.101824	83.244538	58.017908
2514.514531	95.309806	58.022913
2514.320101	95.269622	58.027917
2513.267330	94.847647	58.032922
2512.434694	97.689904	58.037927
2511.985487	87.777813	58.042932
2511.470517	95.015482	58.047937
2510.700526	82.684502	58.052941
2509.741056	91.135362	58.057946
2508.843583	91.722198	58.062951
2508.142104	82.774526	58.067956
2507.396425	97.605862	58.072961
2507.152867	82.702463	58.077965
2506.592579	88.960278	58.082970
2506.435930	87.547101	58.087975
2505.651419	82.957560	58.092980
2504.824900	89.084845	58.097985
2504.384527	90.334036	58.102989
2502.904310	91.693507	58.107994
2501.978486	94.852871	58.112999
2501.509302	93.649832	58.118004
2500.703711	97.484539	58.123009
2500.426021	78.450668	58.128013
2500.202925	87.279298	58.133018
2499.810740	86.653208	58.138023
2499.464843	84.257157	58.143028
2497.686555	94.497560	58.148033
2497.376922	83.763875	58.153037
2496.585240	91.231608	58.158042
2496.655782	96.007147	58.163047
2495.585828	82.146981	58.168052
2494.578289	86.578693	58.173057
2494.085369	85.643784	58.178061
2492.747693	92.625805	58.183066
2492.392996	93.353129	58.188071
2491.675311	88.267444	58.193076
2491.002091	96.513452	58.198081
2490.772626	88.379526	58.203085
2490.347323	94.447298	58.208090
2489.867336	90.008187	58.213095
2488.969283	92.588482	58.218100
2487.618018	85.791049	58.223105
2487.126817	85.852128	58.228109
2486.831972	86.834869	58.233114
2486.088409	88.679431	58.238119
2485.688020	84.617096	58.243124
2484.664227	90.372335	58.248129
2483.905741	87.726310	58.253133
2483.145443	90.913821	58.258138
2482.676196	92.798718	58.263143
2482.455404	81.443158	58.268148
2481.627152	88.235850	58.273153
2480.805091	83.378795	58.278157
2480.111970	78.322862	58.283162
2479.597673	83.368907	58.288167
2478.868928	82.126567	58.293172
2478.078422	92.310982	58.298177
2477.229090	77.004733	58.303181
2477.170194	76.888090	58.308186
2476.214329	87.433525	58.313191
2476.240207	78.691495	58.318196
2474.570702	79.482961	58.323201
2473.786149	85.220585	58.328205
2473.617145	84.222403	58.333210
2473.091341	84.324925	58.338215
2472.196521	77.254074	58.343220
2470.837002	89.799512	58.348225
2470.646864	86.082139	58.353229
2470.192968	83.099445	58.358234
2469.735409	85.668768	58.363239
2469.312411	75.812999	58.368244
2468.486987	87.984104	58.373249
2467.539532	78.059322	58.378253
2466.999227	87.170335	58.383258
2465.936454	84.763437	58.388263
2465.865072	81.326541	58.393268
2465.062579	91.245778	58.398273
2463.737361	82.255158	58.403277
2463.342462	85.853865	58.408282
2462.337103	89.997062	58.413287
2462.152649	80.278133	58.418292
2461.352412	92.160339	58.423297
2461.195206	79.959071	58.428301
2461.264832	85.288952	58.433306
2460.115080	90.685216	58.438311
2459.617895	81.411716	58.443316
2458.464923	83.583639	58.448321
2456.971574	83.945532	58.453325
2456.181571	81.327795	58.458330
2455.859518	86.917269	58.463335
2455.798665	73.540229	58.468340
2455.225283	84.603671	58.473345
2455.041316	80.813406	58.478349
2454.608870	74.445453	58.483354
2453.198747	80.896723	58.488359
2452.969485	70.737846	58.493364
2451.496457	83.556495	58.498369
2450.715404	79.263207	58.503373
2450.382068	74.364442	58.508378
2449.305810	79.054216	58.513383
2449.606523	80.830363	58.518388
2449.096531	77.691875	58.523393
2447.653931	78.054172	58.528397
2447.013531	80.472790	58.533402
2446.074292	78.715016	58.538407
2445.706435	77.271245	58.543412
2445.351364	84.376969	58.548417
2444.371013	78.042303	58.553421
2443.422751	76.015292	58.558426
2442.491621	79.529240	58.563431
2442.267265	77.217016	58.568436
2441.575654	79.336506	58.573441
2441.223725	71.630099	58.578445
2441.139723	75.967068	58.583450
2440.052296	78.014501	58.588455
2438.973639	74.576941	58.593460
2438.138684	80.120691	58.598465
2437.889494	80.055136	58.603469
2437.631286	82.130523	58.608474
2436.645108	79.652512	58.613479
2435.516741	80.464358	58.618484
2434.806127	85.441737	58.623489
2434.429929	86.441942	58.628493
2434.252852	83.119037	58.633498
2433.582981	77.178114	58.638503
2432.961795	75.390041	58.643508
2431.537403	84.546426	58.648513
2431.306694	84.573630	58.653517
2430.597520	79.763994	58.658522
2430.239045	82.167567	58.663527
2429.539244	75.822830	58.668532
2428.850296	84.364802	58.673537
2428.374163	86.819677	58.678541
2427.326446	90.004233	58.683546
2426.331501	89.528179	58.688551
2425.375284	72.419762	58.693556
2424.970404	85.417745	58.698561
2424.603526	71.676604	58.703565
2424.227649	79.200736	58.708570
2423.942986	79.835171	58.713575
2423.141947	72.395022	58.718580
2422.183226	81.828221	58.723585
2421.493375	76.358465	58.728589
2420.177846	84.631794	58.733594
2418.993608	80.000490	58.738599
2419.411108	73.718920	58.743604
2418.738207	86.892199	58.748609
2417.918035	79.258352	58.753613
2417.271706	79.772658	58.758618
2417.121239	83.062740	58.763623
2416.417938	79.009182	58.768628
2414.895397	80.923392	58.773633
2414.102291	77.751607	58.778637
2414.133878	77.066092	58.783642
2413.618352	77.261596	58.788647
2413.505595	74.708459	58.793652
2412.236573	83.687892	58.798657
2411.111450	75.094909	58.803661
2411.214016	77.716878	58.808666
2410.346614	86.348968	58.813671
2409.243828	85.639524	58.818676
2408.430174	81.337607	58.823681
2408.208812	79.093950	58.828685
2407.801239	83.891231	58.833690
2406.945067	91.597752	58.838695
2406.382461	89.635459	58.843700
2405.290831	92.344781	58.848705
2404.607055	84.417622	58.853709
2404.428030	85.548320	58.858714
2403.604334	90.488198	58.863719
2402.810139	87.413701	58.868724
2401.537719	92.235706	58.873729
2401.159416	91.331338	58.878733
2400.721288	81.099231	58.883738
2400.039527	93.839046	58.888743
2399.837746	83.039175	58.893748
2399.221197	84.290471	58.898753
2398.712628	91.208898	58.903757
2398.105920	79.989204	58.908762
2397.202411	85.479947	58.913767
2396.327633	79.739455	58.918772
2394.855636	92.137167	58.923777
2394.210705	81.075583	58.928781
2394.311309	83.735387	58.933786
2393.250765	75.801212	58.938791
2393.103088	73.919550	58.943796
2392.669715	84.423411	58.948801
2391.862122	80.621365	58.953805
2390.745331	77.923337	58.958810
2389.968092	88.025750	58.963815
2389.311863	80.799256	58.968820
2388.884119	84.898564	58.973825
2388.994574	86.747502	58.978829
2388.377441	82.120681	58.983834
2386.883523	91.796974	58.988839
2386.650855	82.540624	58.993844
2385.613108	82.810029	58.998849
2384.836553	81.521011	59.003853
2383.882763	81.825007	59.008858
2383.202363	83.179192	59.013863
2382.972314	79.212477	59.018868
2382.831310	81.511764	59.023873
2382.393459	75.143562	59.028877
2381.091537	83.652193	59.033882
2380.302184	85.391312	59.038887
2379.943231	77.301256	59.043892
2379.199900	77.474139	59.048897
2378.114115	76.267206	59.053901
2377.215171	76.768265	59.058906
2376.428287	81.281074	59.063911
2376.289942	81.344196	59.068916
2375.673740	85.754403	59.073921
2375.398411	79.656821	59.078925
2375.111459	79.810482	59.083930
2373.519225	78.446603	59.088935
2373.285017	76.904989	59.093940
2372.971931	77.715991	59.098945
2372.410628	79.284672	59.103949
2371.183365	70.839427	59.108954
2370.253749	78.431007	59.113959
2370.232652	78.534867	59.118964
2369.254210	78.005084	59.123969
2368.378607	83.120807	59.128973
2367.820176	75.653395	59.133978
2366.619247	81.386436	59.138983
2366.383063	82.039819	59.143988
2366.220470	82.992056	59.148993
2365.589226	78.275683	59.153997
2364.423255	81.364813	59.159002
2363.357611	83.031575	59.164007
2363.061381	68.227223	59.169012
2362.376169	88.828527	59.174017
2361.748742	76.888464	59.179021
2361.903410	86.039714	59.184026
2360.604417	91.780054	59.189031
2359.736653	80.372910	59.194036
2359.118961	79.332644	59.199041
2358.544854	81.378763	59.204045
2358.637487	75.317736	59.209050
2357.395884	87.111205	59.214055
2356.684465	77.355693	59.219060
2355.882536	84.347963	59.224065
2355.611301	76.634478	59.229069
2354.291501	79.729783	59.234074
2353.332890	84.485110	59.239079
2353.146739	79.612501	59.244084
2352.548667	85.058126	59.249089
2352.378467	82.465077	59.254093
2352.234176	74.039517	59.259098
2350.741230	79.586843	59.264103
2350.058658	74.026649	59.269108
2349.312408	82.527502	59.274113
2348.621544	76.071520	59.279117
2348.124082	83.886829	59.284122
2346.621372	81.398874	59.289127
2346.672502	69.258321	59.294132
2345.767022	83.291994	59.299137
2345.455879	71.006551	59.304141
2345.128069	72.779247	59.309146
2344.343750	88.045056	59.314151
2343.951074	68.528023	59.319156
2342.446032	74.652133	59.324161
2341.938132	75.916039	59.329165
2341.800598	70.568953	59.334170
2340.608416	75.788940	59.339175
2340.211245	70.070608	59.344180
2339.353698	73.825398	59.349185
2338.675757	72.019017	59.354189
2338.248407	77.150852	59.359194
2337.378306	72.521511	59.364199
2336.367609	71.796335	59.369204
2335.931578	75.649963	59.374209
2335.412302	81.035931	59.379213
2335.239214	74.080113	59.384218
2334.377849	82.194481	59.389223
2333.830973	72.783460	59.394228
2332.716680	81.252513	59.399233
2331.970719	79.522104	59.404237
2332.031375	87.662358	59.409242
2330.735175	88.828176	59.414247
2329.745704	77.573691	59.419252
2329.094093	81.997060	59.424257
2328.585202	82.220252	59.429261
2328.319800	72.056126	59.434266
2327.858999	82.805060	59.439271
2327.687829	72.305489	59.444276
2326.541569	79.947145	59.449281
2325.676524	81.041999	59.454285
2324.996545	69.579868	59.459290
2324.151091	84.316146	59.464295
2322.856343	73.467935	59.469300
2322.056562	72.065272	59.474305
2321.968560	72.481352	59.479309
2322.133729	83.840063	59.484314
2321.176114	83.436985	59.489319
2321.152838	79.063878	59.494324
2319.447458	74.610529	59.499329
2318.783231	82.954073	59.504333
2318.309626	77.934840	59.509338
2317.636393	88.087757	59.514343
2317.336117	76.766740	59.519348
2316.256607	79.237168	59.524353
2315.085142	80.074170	59.529357
2315.223898	76.938048	59.534362
2314.526139	77.871276	59.539367
2314.329072	73.049485	59.544372
2312.947870	84.281849	59.549377
2312.279630	80.084160	59.554381
2312.188573	70.860848	59.559386
2311.319917	73.630734	59.564391
2310.403830	70.246323	59.569396
2309.294003	78.969606	59.574401
2309.261670	75.343680	59.579405
2309.010912	71.746027	59.584410
2307.383526	74.027523	59.589415
2306.739091	67.693082	59.594420
2305.927403	76.811023	59.599425
2305.405732	76.375636	59.604429
2305.303705	81.832750	59.609434
2304.822702	77.530021	59.614439
2304.329087	74.494932	59.619444
2302.899762	70.345292	59.624449
2302.183927	72.620511	59.629453
2301.909153	71.360171	59.634458
2301.519758	73.610357	59.639463
2301.001790	74.072332	59.644468
2299.732177	78.096531	59.649473
2299.185377	76.993625	59.654477
2298.636557	76.847082	59.659482
2297.570517	82.588645	59.664487
2296.455956	68.101475	59.669492
2295.769458	75.922265	59.674497
2295.866203	70.725378	59.679501
2295.388436	67.233255	59.684506
2294.470902	71.671309	59.689511
2294.329056	70.964533	59.694516
2293.812247	83.974541	59.699521
2292.702422	71.266364	59.704525
2291.806754	70.817568	59.709530
2291.190947	78.445489	59.714535
2290.954857	70.825870	59.719540
2289.491337	76.303442	59.724545
2288.805425	65.107591	59.729549
2288.442007	77.510332	59.734554
2287.927871	83.410930	59.739559
2287.353716	70.120514	59.744564
2287.377248	74.633687	59.749569
2286.112167	72.982189	59.754573
2285.980183	71.129032	59.759578
2284.429441	82.065928	59.764583
2283.736415	74.458134	59.769588
2282.539334	74.103908	59.774593
2281.997988	64.488675	59.779597
2281.846409	72.784811	59.784602
2281.523549	72.170171	59.789607
2280.771718	73.229883	59.794612
2280.381926	69.902315	59.799617
2279.504493	71.918208	59.804621
2278.736281	71.047371	59.809626
2278.118593	81.508142	59.814631
2278.188851	66.556667	59.819636
2276.810342	72.804411	59.824641
2275.681615	66.504637	59.829645
2275.130085	57.185614	59.834650
2274.485788	68.083148	59.839655
2274.120623	62.979068	59.844660
2273.813766	69.195519	59.849665
2272.491487	67.008300	59.854669
2271.778369	71.097201	59.859674
2271.346474	68.823639	59.864679
2271.147161	71.933787	59.869684
2270.326681	73.272072	59.874689
2269.411920	72.717996	59.879693
2268.660498	65.527155	59.884698
2267.799101	70.331387	59.889703
2268.059786	60.558085	59.894708
2267.006443	67.510851	59.899713
2266.147011	61.482387	59.904718
2265.710355	71.552602	59.909722
2264.858535	63.243710	59.914727
2264.475046	57.064387	59.919732
2262.694601	69.727996	59.924737
2262.142455	66.345304	59.929742
2261.856811	66.883601	59.934746
2261.109199	68.318369	59.939751
2261.030487	64.187635	59.944756
2260.573373	71.783678	59.949761
2260.067192	71.420250	59.954766
2259.399747	64.839895	59.959770
2258.725447	75.380605	59.964775
2257.878586	61.146481	59.969780
2256.135114	70.749805	59.974785
2255.630915	72.266890	59.979790
2255.616886	67.357755	59.984794
2255.371024	73.800214	59.989799
2255.050539	66.654886	59.994804
2253.571353	69.364982	59.999809
2253.269796	66.709541	60.004814
2252.497885	63.172203	60.009818
2251.211472	76.759850	60.014823
2250.535806	69.629868	60.019828
2249.331872	82.568702	60.024833
2249.557425	68.987200	60.029838
2248.761611	65.770123	60.034842
2248.322052	69.351998	60.039847
2248.071729	64.972333	60.044852
2247.638035	71.426782	60.049857
2246.552815	76.984137	60.054862
2245.958260	61.631645	60.059866
2245.058799	63.370661	60.064871
2244.691364	67.307688	60.069876
2243.265288	75.291272	60.074881
2242.542708	60.638414	60.079886
2242.717125	71.173316	60.084890
2241.671202	74.392326	60.089895
2241.360077	66.397141	60.094900
2240.020088	69.574471	60.099905
2239.350591	63.210779	60.104910
2238.981926	66.920656	60.109914
2238.108061	71.438877	60.114919
2237.830897	68.021004	60.119924
2237.382265	75.414685	60.124929
2236.881413	76.638710	60.129934
2235.668129	71.848220	60.134938
2235.213592	76.278942	60.139943
2234.831147	71.042431	60.144948
2233.225927	74.342881	60.149953
2232.239085	76.010794	60.154958
2232.046228	70.291483	60.159962
2231.583073	74.819596	60.164967
2231.295626	71.105466	60.169972
2231.029913	77.999726	60.174977
2230.243047	75.125318	60.179982
2229.116661	73.643924	60.184986
2228.412124	83.865743	60.189991
2227.804188	75.009901	60.194996
2227.585390	75.849388	60.200001
2226.673705	76.540538	60.205006
2225.823023	73.907562	60.210010
2225.105304	80.852282	60.215015
2224.804575	73.604107	60.220020
2223.719638	85.172644	60.225025
2222.759254	80.713101	60.230030
2222.371169	72.305172	60.235034
2221.096247	75.032053	60.240039
2221.236014	66.936867	60.245044
2220.507681	80.747619	60.250049
2220.151283	75.247716	60.255054
2220.121313	72.364258	60.260058
2218.892554	79.428347	60.265063
2218.083480	80.120896	60.270068
2217.677174	83.607092	60.275073
2216.454901	82.003551	60.280078
2215.918808	78.903896	60.285082
2215.138003	80.480132	60.290087
2214.997058	72.093094	60.295092
2214.059379	76.428029	60.300097
2213.108261	78.190490	60.305102
2212.527775	75.729590	60.310106
2211.417264	81.322459	60.315111
2211.324884	64.776897	60.320116
2211.084753	66.269744	60.325121
2210.271499	72.940285	60.330126
2209.655576	72.303930	60.335130
2208.745505	77.083338	60.340135
2208.202370	74.147515	60.345140
2207.152555	75.121229	60.350145
2206.163860	77.205895	60.355150
2206.145959	78.250622	60.360154
2205.220060	76.800470	60.365159
2205.296551	73.365536	60.370164
2204.197303	73.952192	60.375169
2203.197918	77.100095	60.380174
2202.944953	72.600099	60.385178
2201.701090	72.805714	60.390183
2201.936411	68.984026	60.395188
2200.748106	75.162151	60.400193
2199.984193	73.772715	60.405198
2199.316993	71.763604	60.410202
2198.816406	76.222729	60.415207
2198.465725	68.120240	60.420212
2197.349192	76.151153	60.425217
2196.158808	68.743303	60.430222
2195.995495	69.870527	60.435226
2195.351354	76.878451	60.440231
2195.037407	69.385051	60.445236
2194.708440	78.408206	60.450241
2193.211844	75.379667	60.455246
2192.771016	73.861559	60.460250
2192.172059	72.003798	60.465255
2192.155121	72.482329	60.470260
2190.775336	70.095764	60.475265
2189.697563	71.991990	60.480270
2189.036170	69.992940	60.485274
2188.826374	76.308051	60.490279
2188.220797	77.609593	60.495284
2187.702807	76.057710	60.500289
2187.124340	79.329017	60.505294
2186.343624	71.141395	60.510298
2185.245643	83.267934	60.515303
2185.129143	77.433332	60.520308
2184.353366	73.121432	60.525313
2183.454928	71.888027	60.530318
2183.026021	76.415417	60.535322
2182.015810	82.679928	60.540327
2181.848342	76.827992	60.545332
2181.148160	77.147858	60.550337
2180.339510	67.957686	60.555342
2179.513201	71.506633	60.560346
2178.853336	69.353776	60.565351
2178.722455	68.049888	60.570356
2177.900455	73.429213	60.575361
2176.668964	72.078303	60.580366
2176.516674	72.495906	60.585370
2175.860050	74.039460	60.590375
2175.359798	70.222789	60.595380
2174.077342	69.764772	60.600385
2173.289217	80.097593	60.605390
2172.818074	62.742508	60.610394
2172.366831	78.374086	60.615399
2171.841445	74.316590	60.620404
2171.088532	67.054185	60.625409
2170.407079	77.717694	60.630414
2169.381612	65.942469	60.635418
2168.668484	76.707707	60.640423
2168.705466	67.058320	60.645428
2168.386862	74.388317	60.650433
2167.034578	71.847850	60.655438
2166.478063	73.642300	60.660442
2165.445158	74.387348	60.665447
2165.152252	67.750454	60.670452
2164.716950	73.683358	60.675457
2163.573068	74.661325	60.680462
2162.959630	71.137950	60.685466
2161.827930	82.283057	60.690471
2161.819689	68.048419	60.695476
2161.578488	85.764131	60.700481
2160.582870	74.871527	60.705486
2159.721255	70.045386	60.710490
2159.045082	79.009505	60.715495
2158.447539	75.494069	60.720500
2157.902311	79.838468	60.725505
2157.266087	82.177848	60.730510
2156.450521	70.979729	60.735514
2155.843725	68.368211	60.740519
2155.367144	59.885438	60.745524
2155.087972	69.257293	60.750529
2153.724024	70.108301	60.755534
2153.047986	69.499208	60.760538
2152.382152	80.258333	60.765543
2152.188682	66.757982	60.770548
2151.654680	67.006800	60.775553
2150.526462	72.410475	60.780558
2149.941923	71.114311	60.785562
2149.381188	78.730843	60.790567
2148.979455	68.784268	60.795572
2147.681203	75.107516	60.800577
2146.642220	81.244325	60.805582
2146.464953	76.267983	60.810586
2146.049107	79.529637	60.815591
2145.693470	70.010161	60.820596
2144.375234	68.882903	60.825601
2143.124111	65.515962	60.830606
2142.908094	71.606748	60.835610
2142.527195	73.712204	60.840615
2142.232540	71.320055	60.845620
2141.459835	68.455083	60.850625
2141.243204	66.321948	60.855630
2140.441164	71.524974	60.860634
2139.217427	78.161521	60.865639
2139.094856	72.654794	60.870644
2137.912967	74.000437	60.875649
2137.067390	72.825892	60.880654
2136.593307	73.434712	60.885658
2136.069238	80.254741	60.890663
2135.729110	79.112163	60.895668
2134.743599	72.722803	60.900673
2133.748765	74.308418	60.905678
2133.241915	74.497333	60.910682
2132.495805	80.580499	60.915687
2132.445308	71.139884	60.920692
2131.701100	73.291690	60.925697
2130.408924	78.609337	60.930702
2130.104063	64.481884	60.935706
2129.299389	76.421682	60.940711
2129.310051	64.180717	60.945716
2128.202821	66.752229	60.950721
2127.091542	69.471666	60.955726
2127.096726	60.992549	60.960730
2126.000943	63.660388	60.965735
2125.641993	64.405432	60.970740
2124.647505	68.294190	60.975745
2123.743092	64.143247	60.980750
2123.453491	63.781472	60.985754
2122.763104	69.113818	60.990759
2122.364060	61.742746	60.995764
2121.797844	61.176450	61.000769
2120.840815	66.516902	61.005774
2120.085187	61.002801	61.010778
2119.753906	70.160550	61.015783
2119.109853	62.757570	61.020788
2118.184941	76.419577	61.025793
2117.197429	73.848313	61.030798
2117.315336	70.322617	61.035802
2116.359139	70.547731	61.040807
2115.836465	68.855348	61.045812
2114.868491	75.349472	61.050817
2114.124817	65.858875	61.055822
2113.995433	74.751576	61.060826
2112.450127	74.947587	61.065831
2111.533732	67.568688	61.070836
2111.669648	70.053495	61.075841
2110.890491	68.159069	61.080846
2110.388928	68.939164	61.085850
2109.430262	75.713528	61.090855
2109.089067	65.565563	61.095860
2108.626060	72.671581	61.100865
2107.648642	78.945885	61.105870
2106.902190	61.148059	61.110874
2106.295189	76.021168	61.115879
2105.736900	67.892231	61.120884
2104.899435	74.332457	61.125889
2103.914768	64.152452	61.130894
2103.659283	57.760212	61.135898
2103.078177	71.331834	61.140903
2102.795779	68.528265	61.145908
2101.551492	73.693652	61.150913
2100.557009	78.169365	61.155918
2100.439778	70.850744	61.160922
2099.888534	76.460468	61.165927
2099.424040	68.028921	61.170932
2098.838832	71.063763	61.175937
2097.408826	66.319854	61.180942
2096.745404	60.430791	61.185946
2096.165130	70.989757	61.190951
2095.948263	66.620568	61.195956
2095.022532	65.975246	61.200961
2094.238760	79.199053	61.205966
2093.677369	67.155405	61.210970
2093.153430	71.768126	61.215975
2092.762399	77.062301	61.220980
2092.180847	64.948290	61.225985
2090.967433	75.208594	61.230990
2090.552442	74.117507	61.235994
2089.499073	77.004671	61.240999
2089.292922	70.101509	61.246004
2088.342349	77.412893	61.251009
2087.266341	80.432609	61.256014
2086.745782	73.956234	61.261018
2086.097623	71.165097	61.266023
2086.132419	74.528877	61.271028
2085.671059	70.798325	61.276033
2084.613428	78.726419	61.281038
2084.003491	66.802783	61.286042
2083.431847	83.870028	61.291047
2083.008267	71.756624	61.296052
2081.592242	68.775523	61.301057
2081.019189	69.760077	61.306062
2080.916177	75.344843	61.311066
2079.614686	73.266615	61.316071
2079.424889	71.494011	61.321076
2078.685103	76.333515	61.326081
2077.324555	76.105581	61.331086
2077.218274	64.775512	61.336090
2076.303145	66.836168	61.341095
2076.221663	69.128825	61.346100
2075.604881	67.538197	61.351105
2074.735952	75.353885	61.356110
2074.235049	64.990095	61.361114
2073.545112	70.965763	61.366119
2072.989967	65.834995	61.371124
2071.827940	74.162639	61.376129
2070.433650	71.426892	61.381134
2070.461824	68.294295	61.386138
2069.640992	73.260946	61.391143
2069.505255	59.746400	61.396148
2069.159761	59.949562	61.401153
2067.866298	72.156508	61.406158
2067.690133	66.595800	61.411162
2066.727681	64.689709	61.416167
2066.230483	66.647304	61.421172
2065.087443	68.626555	61.426177
2063.994397	77.088450	61.431182
2064.204247	66.889657	61.436186
2062.991358	74.033154	61.441191
2063.100301	68.244476	61.446196
2062.863577	73.606200	61.451201
2061.922722	79.110863	61.456206
2061.209797	70.896677	61.461210
2059.444059	66.337700	61.466215
2058.781174	61.214312	61.471220
2058.022154	71.342423	61.476225
2057.957094	67.313967	61.481230
2057.451256	71.543478	61.486234
2057.086791	73.146015	61.491239
2056.698114	63.563528	61.496244
2055.767456	67.433483	61.501249
2054.725493	71.234454	61.506254
2053.944731	70.751046	61.511258
2053.506672	76.303517	61.516263
2053.122188	72.285883	61.521268
2052.094782	78.190205	61.526273
2050.912435	75.786485	61.531278
2050.867294	74.223209	61.536282
2050.043081	83.711584	61.541287
2050.005066	71.515264	61.546292
2049.456807	73.309496	61.551297
2048.172398	77.751127	61.556302
2047.861083	67.131105	61.561306
2046.438389	73.680517	61.566311
2045.406389	72.668132	61.571316
2045.578171	66.742396	61.576321
2044.430637	78.312570	61.581326
2044.428989	69.737524	61.586330
2043.941749	75.405772	61.591335
2043.458988	73.399081	61.596340
2042.253999	72.661804	61.601345
2041.327601	70.104180	61.606350
2041.112185	73.270372	61.611354
2040.195272	77.085481	61.616359
2040.030000	78.224886	61.621364
2039.031695	65.574302	61.626369
2037.831659	73.898189	61.631374
2037.792307	69.158390	61.636378
2037.285190	75.973152	61.641383
2035.774966	68.185866	61.646388
2035.213050	70.810955	61.651393
2034.710695	74.390556	61.656398
2034.341803	70.212763	61.661402
2033.626255	71.558393	61.666407
2033.515859	77.111264	61.671412
2032.732420	80.088839	61.676417
2031.432908	68.145015	61.681422
2031.200921	71.572188	61.686426
2030.483593	77.575441	61.691431
2029.822573	76.018043	61.696436
2028.344658	79.784647	61.701441
2027.912726	81.974231	61.706446
2027.561793	71.664527	61.711450
2027.537008	80.328552	61.716455
2027.140663	71.767732	61.721460
2025.772295	75.690855	61.726465
2024.894431	71.230665	61.731470
2024.730967	67.950066	61.736474
2023.686138	69.790952	61.741479
2023.083222	67.698243	61.746484
2022.061561	71.055237	61.751489
2021.023219	65.601357	61.756494
2021.152247	62.305463	61.761498
2020.587224	72.781693	61.766503
2020.249616	69.837186	61.771508
2019.887189	65.707631	61.776513
2018.481714	72.888024	61.781518
2017.977669	68.809533	61.786522
2016.601625	71.425864	61.791527
2015.794052	69.207116	61.796532
2015.531681	66.627884	61.801537
2015.090344	72.422090	61.806542
2014.684535	66.013336	61.811546
2013.810086	72.005571	61.816551
2013.348427	72.074666	61.821556
2013.148279	70.701320	61.826561
2011.935940	72.647437	61.831566
2011.297207	72.403809	61.836570
2010.961992	72.255888	61.841575
2010.144003	71.442552	61.846580
2009.167205	74.793059	61.851585
2008.005827	74.551994	61.856590
2008.235288	63.134901	61.861594
2007.370004	71.562576	61.866599
2006.417383	76.444414	61.871604
2005.887562	67.578813	61.876609
2005.102616	78.358313	61.881614
2004.440258	66.087231	61.886618
2003.919922	71.444574	61.891623
2003.302923	69.407169	61.896628
2002.418240	63.697281	61.901633
2001.576073	70.502646	61.906638
2001.270199	58.639125	61.911642
2000.757734	73.381586	61.916647
2000.059645	66.199837	61.921652
1999.242751	59.102359	61.926657
1998.573300	65.788970	61.931662
1998.485773	56.318399	61.936666
1997.370913	62.701084	61.941671
1997.093958	67.763778	61.946676
1995.981863	64.384148	61.951681
1995.489943	64.537760	61.956686
1995.007919	59.334105	61.961690
1993.636555	68.149916	61.966695
1992.825659	70.791547	61.971700
1992.508805	59.312390	61.976705
1991.895068	67.612564	61.981710
1991.438741	52.639123	61.986714
1990.953263	61.997310	61.991719
1990.555718	69.137128	61.996724
1989.710723	65.246828	62.001729
1988.671564	67.130564	62.006734
1988.489249	56.833873	62.011738
1987.006608	69.303703	62.016743
1985.986037	66.689967	62.021748
1985.729565	67.625113	62.026753
1984.933007	71.671867	62.031758
1984.759627	59.502275	62.036762
1983.842855	72.989607	62.041767
1984.097918	68.080243	62.046772
1983.744407	73.866532	62.051777
1982.626109	77.414137	62.056782
1982.039474	70.041226	62.061786
1980.611581	74.773456	62.066791
1979.404106	68.049095	62.071796
1979.228397	72.531598	62.076801
1978.918613	75.557229	62.081806
1978.414545	74.023514	62.086810
1978.099745	83.192260	62.091815
1976.583991	74.384006	62.096820
1976.339168	75.014803	62.101825
1975.590168	72.806963	62.106830
1975.292649	68.834459	62.111834
1974.517645	71.138387	62.116839
1973.156096	65.306404	62.121844
1972.698111	66.840867	62.126849
1971.529444	72.479242	62.131854
1971.986482	63.436151	62.136858
1971.068090	66.113146	62.141863
1970.094660	72.764133	62.146868
1969.993556	73.441001	62.151873
1969.096794	70.563730	62.156878
1968.491610	69.256910	62.161882
1967.057060	74.436316	62.166887
1966.419521	54.234615	62.171892
1966.228303	70.171803	62.176897
1965.599630	73.460396	62.181902
1965.227234	57.312909	62.186906
1964.527872	66.509931	62.191911
1963.722258	69.434861	62.196916
1963.025098	73.847100	62.201921
1962.278784	70.564766	62.206926
1961.765387	66.799319	62.211930
1961.081296	68.098920	62.216935
1959.803474	61.203452	62.221940
1958.973080	69.321225	62.226945
1958.390301	75.082001	62.231950
1958.108893	71.433176	62.236954
1957.745589	70.433914	62.241959
1957.411219	73.361123	62.246964
1957.202440	65.481888	62.251969
1956.092228	75.231152	62.256974
1955.426669	74.631345	62.261978
1954.202999	77.147022	62.266983
1953.061484	81.081879	62.271988
1952.719112	70.483367	62.276993
1952.109277	77.517010	62.281998
1951.733945	66.911114	62.287002
1951.504856	71.437879	62.292007
1950.864522	72.635263	62.297012
1949.981294	62.828331	62.302017
1949.336481	72.034183	62.307022
1948.666264	63.471286	62.312026
1948.041455	65.365854	62.317031
1946.920910	65.756871	62.322036
1946.492118	65.737852	62.327041
1945.448526	71.299178	62.332046
1945.439438	61.051013	62.337050
1944.798062	73.248260	62.342055
1943.822194	73.678077	62.347060
1943.243825	64.731984	62.352065
1942.576285	75.703364	62.357070
1942.280369	62.906211	62.362074
1940.884495	79.728798	62.367079
1940.329134	81.834506	62.372084
1940.628896	71.606523	62.377089
1939.577543	76.995897	62.382094
1938.298886	65.679307	62.387098
1937.004791	71.694392	62.392103
1936.762299	62.558612	62.397108
1936.239574	64.046918	62.402113
1935.817735	72.956084	62.407118
1935.635897	62.178941	62.412122
1934.908824	67.225481	62.417127
1934.278128	63.943902	62.422132
1933.483967	68.167085	62.427137
1932.663102	67.446224	62.432142
1932.202820	68.319925	62.437146
1930.783895	73.313120	62.442151
1930.524603	71.673197	62.447156
1930.185440	74.729906	62.452161
1929.496304	72.434862	62.457166
1929.037906	66.013013	62.462170
1927.801490	65.921376	62.467175
1926.926588	66.248270	62.472180
1926.228531	67.530923	62.477185
1925.868344	83.837668	62.482190
1925.812428	63.274771	62.487194
1924.654991	79.211867	62.492199
1923.569994	72.818659	62.497204
1923.334632	71.441869	62.502209
1922.763437	71.634706	62.507214
1922.189365	66.153135	62.512218
1921.721289	81.788758	62.517223
1920.876224	70.135900	62.522228
1919.949762	67.207275	62.527233
1919.425818	70.935832	62.532238
1919.224484	61.797749	62.537242
1917.991488	71.676963	62.542247
1917.218101	76.662750	62.547252
1916.907718	71.764069	62.552257
1916.235234	70.212595	62.557262
1915.345613	62.976004	62.562266
1914.277955	66.897439	62.567271
1914.234688	74.119935	62.572276
1913.504095	78.475138	62.577281
1913.015899	71.450121	62.582286
1912.236844	68.219186	62.587290
1911.487497	67.734767	62.592295
1910.547818	67.661052	62.597300
1910.494164	64.723635	62.602305
1909.657263	75.016649	62.607310
1908.477349	75.301782	62.612314
1908.007320	72.580063	62.617319
1907.355653	78.789978	62.622324
1907.456017	67.899428	62.627329
1906.572057	75.377057	62.632334
1905.511973	68.949990	62.637338
1904.730880	71.120368	62.642343
1904.231113	71.141520	62.647348
1903.745678	69.522524	62.652353
1902.777010	73.610573	62.657358
1902.169343	74.528438	62.662362
1901.358684	65.996287	62.667367
1900.784643	65.908967	62.672372
1900.580095	70.737046	62.677377
1899.099527	73.503517	62.682382
1898.577341	62.193708	62.687386
1897.890464	72.027652	62.692391
1897.593319	67.029609	62.697396
1897.375089	65.399637	62.702401
1896.659713	78.684371	62.707406
1895.910727	69.410251	62.712410
1895.353441	69.778730	62.717415
1894.938038	70.775015	62.722420
1893.981504	73.542228	62.727425
1892.913150	74.736268	62.732430
1892.512076	69.083400	62.737434
1891.194842	65.881384	62.742439
1890.587765	70.898323	62.747444
1889.793056	62.878558	62.752449
1889.091892	65.598529	62.757454
1889.179640	71.947986	62.762458
1888.166346	76.676015	62.767463
1887.857677	70.791821	62.772468
1887.562021	67.447403	62.777473
1886.342565	79.542244	62.782478
1885.612143	66.967454	62.787482
1885.227790	70.720682	62.792487
1884.807603	72.848661	62.797492
1883.446561	72.416002	62.802497
1882.534769	70.845477	62.807502
1882.215180	70.192017	62.812506
1881.553694	74.581186	62.817511
1880.987729	72.707954	62.822516
1881.156008	74.294355	62.827521
1879.875392	77.719753	62.832526
1878.896938	70.359818	62.837530
1878.626105	82.188559	62.842535
1878.160117	76.775340	62.847540
1877.184308	68.739191	62.852545
1876.144198	76.971007	62.857550
1875.399464	74.003800	62.862554
1875.151090	77.301942	62.867559
1874.566532	69.723048	62.872564
1874.169196	73.435868	62.877569
1872.900557	76.426999	62.882574
1872.163264	70.540745	62.887578
1871.389875	75.813893	62.892583
1871.181692	75.596881	62.897588
1870.932269	73.613051	62.902593
1870.113389	80.657595	62.907598
1869.481315	72.187260	62.912602
1868.484378	76.567902	62.917607
1867.789351	70.514162	62.922612
1867.434810	65.646331	62.927617
1866.341066	77.380601	62.932622
1865.652511	70.675254	62.937626
1864.976328	72.337841	62.942631
1864.785677	69.195320	62.947636
1864.351912	72.948318	62.952641
1862.377569	64.160547	62.957646
1862.643104	70.649708	62.962650
1862.029658	75.261177	62.967655
1861.496139	75.779140	62.972660
1861.201338	69.017482	62.977665
1860.007770	77.586989	62.982670
1859.167468	71.038257	62.987674
1858.674923	65.884577	62.992679
1858.004320	70.700815	62.997684
1857.584378	70.283991	63.002689
1856.139176	85.519964	63.007694
1855.943913	71.658012	63.012698
1855.192285	69.792470	63.017703
1854.792744	68.250359	63.022708
1854.441340	71.371530	63.027713
1853.284514	84.453911	63.032718
1852.526859	63.739125	63.037722
1851.647686	70.503467	63.042727
1851.123661	72.782233	63.047732
1851.333195	69.754398	63.052737
1850.050690	72.385552	63.057742
1849.679811	56.641633	63.062746
1849.009979	71.584683	63.067751
1848.186662	73.359678	63.072756
1847.240283	69.192289	63.077761
1846.417337	77.213278	63.082766
1845.593971	63.139861	63.087770
1845.052651	72.716414	63.092775
1844.786042	66.322947	63.097780
1844.228245	64.863569	63.102785
1843.803424	74.151386	63.107790
1842.810867	61.423311	63.112794
1842.159380	66.568633	63.117799
1841.471506	71.427695	63.122804
1841.013151	67.293256	63.127809
1839.845091	77.053220	63.132814
1839.195687	67.973648	63.137818
1838.731443	71.071889	63.142823
1838.489145	72.274999	63.147828
1838.049136	69.358687	63.152833
1836.520754	68.742311	63.157838
1836.269890	67.354758	63.162842
1835.804735	75.645308	63.167847
1834.939334	68.740892	63.172852
1834.069233	65.847246	63.177857
1832.910794	70.601298	63.182862
1832.733947	62.653462	63.187866
1832.358214	75.150246	63.192871
1831.850112	65.237719	63.197876
1831.793911	64.940630	63.202881
1830.093707	69.367390	63.207886
1829.669801	60.409500	63.212890
1829.010355	71.128846	63.217895
1827.731046	75.339524	63.222900
1827.205254	69.313283	63.227905
1826.152430	75.748539	63.232910
1825.973778	69.088587	63.237914
1825.637765	76.638652	63.242919
1825.242589	79.622452	63.247924
1825.052416	72.581591	63.252929
1823.923905	81.018400	63.257934
1823.011250	69.383451	63.262938
1822.518742	75.038002	63.267943
1821.673666	73.269766	63.272948
1820.694452	67.200713	63.277953
1819.980056	86.192941	63.282958
1819.829384	72.258237	63.287962
1819.252736	81.596113	63.292967
1818.427902	76.967426	63.297972
1817.409819	68.780243	63.302977
1816.606127	76.058628	63.307982
1816.342826	63.219211	63.312986
1815.956936	79.625860	63.317991
1815.468865	69.485311	63.322996
1814.505314	69.301622	63.328001
1813.440396	82.479197	63.333006
1813.152912	70.045737	63.338010
1812.748587	69.903338	63.343015
1811.620455	69.707548	63.348020
1810.951113	64.494128	63.353025
1809.926319	68.194703	63.358030
1810.177517	66.159960	63.363034
1809.574924	63.807894	63.368039
1808.396588	66.540439	63.373044
1807.688786	69.949552	63.378049
1806.971457	73.196487	63.383054
1806.402608	72.879746	63.388058
1806.359733	74.810942	63.393063
1805.346814	67.594682	63.398068
1804.761131	63.711762	63.403073
1804.008429	76.646053	63.408078
1803.404850	64.615615	63.413082
1802.099288	73.236261	63.418087
1801.040612	69.054546	63.423092
1800.734039	68.991734	63.428097
1800.198777	73.143796	63.433102
1800.170859	73.484868	63.438106
1799.796330	73.173562	63.443111
1798.077715	74.551505	63.448116
1797.620537	66.814654	63.453121
1796.938217	73.415064	63.458126
1796.632641	69.788548	63.463130
1796.154101	74.160632	63.468135
1795.151440	73.043415	63.473140
1794.457318	71.938538	63.478145
1793.753305	70.858641	63.483150
1793.464436	67.649249	63.488154
1792.883731	70.152446	63.493159
1791.961553	67.112593	63.498164
1791.118865	73.704127	63.503169
1790.434561	72.142853	63.508174
1789.891790	59.083245	63.513178
1789.622701	66.558305	63.518183
1788.886935	68.604499	63.523188
1788.106536	67.951734	63.528193
1787.347538	69.173387	63.533198
1787.224971	64.180222	63.538202
1786.003477	65.869016	63.543207
1784.763134	69.276094	63.548212
1784.892850	65.181567	63.553217
1784.261414	72.522844	63.558222
1783.293385	61.856557	63.563226
1782.557162	77.575542	63.568231
1781.803261	70.865999	63.573236
1781.255068	72.691820	63.578241
1781.075620	75.635552	63.583246
1779.925420	70.222185	63.588250
1779.033152	77.162060	63.593255
1778.005535	66.843058	63.598260
1778.114760	70.008964	63.603265
1777.223877	72.356032	63.608270
1777.031234	66.748831	63.613274
1776.658291	58.361286	63.618279
1775.527256	71.346885	63.623284
1774.731495	67.606882	63.628289
1774.296504	66.376358	63.633294
1773.845786	69.685438	63.638298
1772.714711	67.510243	63.643303
1772.204255	64.932032	63.648308
1771.713893	63.654143	63.653313
1770.175562	60.170665	63.658318
1769.550100	52.106977	63.663322
1769.194632	61.342263	63.668327
1768.610957	66.761370	63.673332
1768.206691	62.064291	63.678337
1767.723014	76.514853	63.683342
1767.763515	67.985119	63.688346
1766.664225	70.963874	63.693351
1765.607902	66.676375	63.698356
1764.957697	56.455433	63.703361
1763.761632	72.242039	63.708366
1763.339079	62.840263	63.713370
1762.685216	72.528041	63.718375
1762.394994	65.134062	63.723380
1761.790252	61.138363	63.728385
1760.586934	63.560994	63.733390
1759.817825	62.196991	63.738394
1759.180558	65.158269	63.743399
1758.411152	69.630251	63.748404
1758.058260	60.478652	63.753409
1757.716574	63.907622	63.758414
1757.324469	53.398190	63.763418
1756.657899	62.395798	63.768423
1755.777432	71.477772	63.773428
1755.137111	57.211233	63.778433
1754.481579	65.872627	63.783438
1753.596914	59.818600	63.788442
1752.382287	57.501005	63.793447
1751.795362	65.860541	63.798452
1751.668729	66.498754	63.803457
1750.981912	70.987395	63.808462
1750.793721	75.536371	63.813466
1749.650277	71.450484	63.818471
1748.559108	67.866422	63.823476
1748.349882	62.239564	63.828481
1747.738998	61.392413	63.833486
1747.474075	67.255513	63.838490
1746.085758	70.888831	63.843495
1745.096706	74.425808	63.848500
1744.958707	64.230903	63.853505
1744.725251	69.486672	63.858510
1744.204809	64.566720	63.863514
1743.153682	67.639864	63.868519
1742.170002	66.821767	63.873524
1742.251868	59.574512	63.878529
1740.851445	60.989602	63.883534
1740.240303	66.514064	63.888538
1739.357429	69.008576	63.893543
1739.070002	66.329841	63.898548
1738.486041	59.265195	63.903553
1738.252913	73.172377	63.908558
1737.711636	60.993540	63.913562
1736.761615	61.861059	63.918567
1735.698237	57.564120	63.923572
1735.141965	61.364135	63.928577
1734.183181	64.977640	63.933582
1733.630415	67.111339	63.938586
1733.061241	58.367395	63.943591
1732.428269	69.230230	63.948596
1732.253339	60.629212	63.953601
1731.161127	69.170337	63.958606
1730.357320	54.945202	63.963610
1729.923671	60.085623	63.968615
1729.407978	70.026457	63.973620
1728.955675	57.466495	63.978625
1727.709838	66.131401	63.983630
1727.328755	59.961609	63.988634
1726.411461	57.330260	63.993639
1725.652315	61.097887	63.998644
1724.847099	57.413985	64.003649
1723.988343	65.844507	64.008654
1723.498612	64.571252	64.013658
1723.258140	67.236490	64.018663
1722.713506	61.585714	64.023668
1722.835557	61.844285	64.028673
1721.181454	59.939776	64.033678
1720.646930	65.298372	64.038682
1719.923447	67.338920	64.043687
1719.378104	66.576870	64.048692
1718.958727	71.194217	64.053697
1717.950054	71.366411	64.058702
1717.146561	66.940535	64.063706
1716.633712	71.938992	64.068711
1716.139242	69.466205	64.073716
1715.056416	62.917958	64.078721
1714.266634	67.088312	64.083726
1713.739475	69.684585	64.088730
1713.370682	70.323579	64.093735
1713.018117	73.300881	64.098740
1712.495230	71.128207	64.103745
1711.234032	70.854554	64.108750
1710.750858	70.491191	64.113754
1710.330568	65.160177	64.118759
1709.180392	66.680475	64.123764
1708.286221	52.718696	64.128769
1707.943033	64.262173	64.133774
1707.472479	68.154887	64.138778
1707.141220	62.514574	64.143783
1705.962164	66.104593	64.148788
1705.125457	60.945884	64.153793
1704.412165	69.223235	64.158798
1704.412098	65.387354	64.163802
1703.958978	64.384929	64.168807
1702.453942	67.492726	64.173812
1701.851654	57.850547	64.178817
1700.892434	62.990511	64.183822
1700.603257	61.395980	64.188826
1700.055327	59.264303	64.193831
1699.706085	65.692463	64.198836
1699.461142	61.958877	64.203841
1698.324804	63.755481	64.208846
1697.056496	65.385202	64.213850
1696.984623	61.124260	64.218855
1696.192093	65.733225	64.223860
1695.385199	58.600555	64.228865
1694.695801	64.361821	64.233870
1694.235783	62.730605	64.238874
1693.898291	57.677521	64.243879
1693.158641	62.988326	64.248884
1692.562830	62.901202	64.253889
1691.751788	69.191288	64.258894
1690.662327	58.926715	64.263898
1689.627923	63.433785	64.268903
1688.875445	67.227512	64.273908
1688.448805	61.489843	64.278913
1687.876257	60.575749	64.283918
1687.748077	62.855866	64.288922
1687.678812	59.984286	64.293927
1686.749018	69.315088	64.298932
1686.230636	62.087657	64.303937
1685.322378	68.587792	64.308942
1684.321090	66.132264	64.313946
1682.450368	62.611749	64.318951
1681.786961	60.106694	64.323956
1682.385130	56.535931	64.328961
1681.893688	66.631685	64.333966
1680.973019	61.370511	64.338970
1680.344828	66.750268	64.343975
1679.566645	67.553657	64.348980
1679.176461	63.036145	64.353985
1677.939145	71.137127	64.358990
1677.350981	62.365654	64.363994
1677.177554	58.600886	64.368999
1676.592878	63.464403	64.374004
1676.308641	59.900957	64.379009
1675.147010	65.555541	64.384014
1674.515113	60.696514	64.389018
1673.800930	65.851391	64.394023
1672.442990	63.940822	64.399028
1672.021835	60.538958	64.404033
1671.496403	58.962358	64.409038
1671.511016	58.469215	64.414042
1670.886460	68.049350	64.419047
1669.887944	58.803781	64.424052
1669.041984	57.162431	64.429057
1668.389279	62.642299	64.434062
1668.233023	68.681794	64.439066
1666.638830	64.120456	64.444071
1665.677449	69.818536	64.449076
1665.249133	62.052298	64.454081
1664.417222	63.809052	64.459086
1664.187684	66.592414	64.464090
1664.059419	66.237005	64.469095
1663.500950	64.717372	64.474100
1663.257444	66.436593	64.479105
1661.928725	62.682818	64.484110
1661.405305	60.527216	64.489114
1661.014318	67.509206	64.494119
1659.775265	69.249188	64.499124
1658.689359	60.472899	64.504129
1658.336126	69.223877	64.509134
1657.713553	55.579172	64.514138
1657.627055	60.851628	64.519143
1656.306669	61.748987	64.524148
1655.645276	52.656912	64.529153
1654.957085	65.015311	64.534158
1654.554877	52.809546	64.539162
1654.320496	61.777408	64.544167
1653.083271	65.463439	64.549172
1652.399051	61.838184	64.554177
1651.751600	66.721130	64.559182
1651.345468	55.622038	64.564186
1651.065789	52.685814	64.569191
1650.187775	63.046655	64.574196
1649.184474	57.503591	64.579201
1648.313985	62.901524	64.584206
1648.010558	58.088130	64.589210
1647.663673	64.202874	64.594215
1646.183650	66.068564	64.599220
1645.966052	65.666866	64.604225
1645.276807	64.805113	64.609230
1645.059083	65.645224	64.614234
1644.085430	62.221466	64.619239
1642.895530	68.703489	64.624244
1642.518706	63.821342	64.629249
1642.105389	69.943114	64.634254
1641.296760	56.948382	64.639258
1641.220888	54.254375	64.644263
1639.494142	58.815195	64.649268
1639.349285	58.893264	64.654273
1638.413046	55.361269	64.659278
1638.318827	52.747373	64.664282
1637.751204	52.404390	64.669287
1636.657854	56.031856	64.674292
1636.330952	53.883285	64.679297
1635.511257	55.874388	64.684302
1634.840761	62.991441	64.689306
1633.742731	61.694797	64.694311
1633.263473	62.088239	64.699316
1633.193259	55.069904	64.704321
1632.445258	58.971811	64.709326
1631.473624	60.549988	64.714330
1630.844200	55.079522	64.719335
1630.023957	65.211015	64.724340
1629.965677	64.559827	64.729345
1628.309231	62.813243	64.734350
1628.079239	62.956801	64.739354
1627.450397	61.391192	64.744359
1626.633188	49.573018	64.749364
1626.736580	57.479698	64.754369
1625.329269	61.275363	64.759374
1624.525688	66.078455	64.764378
1623.859854	69.504482	64.769383
1623.052469	62.705845	64.774388
1622.888191	58.046266	64.779393
1622.550155	64.198177	64.784398
1621.881206	54.777811	64.789402
1620.898305	63.773507	64.794407
1620.189507	66.051543	64.799412
1620.049965	63.312382	64.804417
1618.672945	64.440879	64.809422
1618.019337	58.588517	64.814426
1617.543356	56.664003	64.819431
1616.673752	69.389357	64.824436
1616.776917	61.308370	64.829441
1615.274778	62.106190	64.834446
1614.935289	56.903464	64.839450
1614.409917	57.624126	64.844455
1613.877670	67.287934	64.849460
1612.947915	57.318147	64.854465
1611.876381	59.202358	64.859470
1611.473605	64.223427	64.864474
1611.154362	65.973372	64.869479
1610.134981	62.124835	64.874484
1609.972428	56.485664	64.879489
1608.469397	70.031886	64.884494
1608.434181	57.211899	64.889498
1607.853142	54.003582	64.894503
1607.145938	63.194061	64.899508
1606.789121	59.825403	64.904513
1605.569397	51.272947	64.909518
1604.937555	51.439883	64.914522
1604.577441	62.123393	64.919527
1602.942730	59.866674	64.924532
1602.848220	56.247873	64.929537
1601.907467	62.480825	64.934542
1601.510414	58.720781	64.939546
1600.795050	57.970079	64.944551
1600.079214	66.663507	64.949556
1600.077832	62.116572	64.954561
1599.361327	65.364571	64.959566
1598.638281	66.991787	64.964570
1597.371186	66.179196	64.969575
1596.936829	61.386240	64.974580
1596.875128	54.137121	64.979585
1596.222050	67.453811	64.984590
1595.014594	62.094901	64.989594
1594.453852	61.122352	64.994599
1593.750140	66.876997	64.999604
1593.432952	58.832030	65.004609
1592.024720	67.374754	65.009614
1591.509232	61.619543	65.014618
1590.945206	66.387958	65.019623
1590.234336	62.281769	65.024628
1590.457751	59.838505	65.029633
1589.278172	66.918742	65.034638
1588.491019	71.305362	65.039642
1587.861923	65.661562	65.044647
1587.162917	72.099452	65.049652
1586.826651	55.831409	65.054657
1585.494597	61.981729	65.059662
1584.765076	62.029600	65.064666
1584.254053	66.994198	65.069671
1583.822472	66.080068	65.074676
1584.062400	63.247548	65.079681
1582.613135	61.293821	65.084686
1582.068634	60.958728	65.089690
1581.702488	57.639825	65.094695
1580.673498	66.396715	65.099700
1580.096837	62.847008	65.104705
1579.237450	57.649184	65.109710
1578.687869	56.179355	65.114714
1577.544386	61.519020	65.119719
1576.216478	66.921826	65.124724
1576.636154	48.528328	65.129729
1575.703584	68.437288	65.134734
1575.149225	58.631415	65.139738
1574.783571	60.768629	65.144743
1574.028472	67.682280	65.149748
1573.805267	63.158309	65.154753
1572.523582	65.340587	65.159758
1571.846845	62.019183	65.164762
1571.317099	68.137592	65.169767
1570.802137	63.814729	65.174772
1570.196511	64.995952	65.179777
1569.283156	61.231907	65.184782
1568.268505	61.212135	65.189786
1568.123822	54.669951	65.194791
1567.388985	64.733149	65.199796
1566.985261	54.976497	65.204801
1565.835663	59.148446	65.209806
1565.384643	58.084100	65.214810
1564.751430	54.900112	65.219815
1564.273306	62.691187	65.224820
1563.260296	58.349752	65.229825
1562.270249	62.846092	65.234830
1561.738625	56.947209	65.239834
1561.620742	63.690230	65.244839
1561.267669	64.416934	65.249844
1560.708630	63.362391	65.254849
1559.337280	58.184693	65.259854
1558.937580	61.624781	65.264858
1558.496783	57.052793	65.269863
1557.547554	60.917702	65.274868
1556.768967	62.850863	65.279873
1555.981683	65.544162	65.284878
1555.481151	68.243253	65.289882
1554.781278	63.859674	65.294887
1553.757368	76.192252	65.299892
1552.945752	65.163753	65.304897
1552.794561	71.305794	65.309902
1552.378828	61.880786	65.314906
1552.144905	58.228219	65.319911
1551.319853	65.345282	65.324916
1550.354415	57.918479	65.329921
1549.466940	65.477653	65.334926
1548.540922	56.903368	65.339930
1547.742265	61.151043	65.344935
1546.729974	60.845095	65.349940
1546.634181	52.186354	65.354945
1546.307873	60.527340	65.359950
1545.908762	60.290126	65.364954
1545.472156	62.965645	65.369959
1544.486694	65.547212	65.374964
1543.974536	62.341323	65.379969
1543.228619	61.307713	65.384974
1542.115975	67.528646	65.389978
1541.404228	59.080314	65.394983
1540.653873	58.304821	65.399988
1540.470657	55.209209	65.404993
1539.960550	57.676659	65.409998
1538.710425	62.195409	65.415002
1537.871762	60.319949	65.420007
1536.998108	62.760807	65.425012
1536.980739	55.641467	65.430017
1536.140149	59.040570	65.435022
1535.846233	57.910262	65.440026
1535.561637	52.251331	65.445031
1534.349599	61.968718	65.450036
1533.970308	57.830660	65.455041
1533.509158	70.173100	65.460046
1532.665912	57.285373	65.465050
1532.093956	59.354875	65.470055
1531.041932	63.405926	65.475060
1530.411009	62.745777	65.480065
1528.990209	67.309135	65.485070
1528.043225	57.825063	65.490074
1528.435838	63.534177	65.495079
1527.265423	70.552465	65.500084
1527.022610	54.873942	65.505089
1526.791031	65.225993	65.510094
1526.434647	66.244569	65.515098
1525.192774	59.690441	65.520103
1524.359870	65.256026	65.525108
1523.979293	60.594002	65.530113
1523.520380	63.263472	65.535118
1521.996668	61.631175	65.540122
1521.527224	60.838790	65.545127
1520.731880	69.108088	65.550132
1520.793251	61.698967	65.555137
1520.162672	57.926798	65.560142
1519.305166	62.701236	65.565146
1518.449889	61.256103	65.570151
1517.776978	64.413758	65.575156
1517.565920	58.107138	65.580161
1516.061316	63.334942	65.585166
1515.475506	64.283448	65.590170
1514.993897	59.577140	65.595175
1514.357347	60.661824	65.600180
1514.031312	58.800864	65.605185
1513.780558	67.013664	65.610190
1512.283227	60.826142	65.615194
1511.788673	59.855695	65.620199
1510.886101	63.715389	65.625204
1510.785864	65.797708	65.630209
1510.306298	72.126996	65.635214
1509.227462	66.391638	65.640218
1508.737547	62.220018	65.645223
1507.631734	59.070347	65.650228
1507.522372	61.190935	65.655233
1506.591319	56.730493	65.660238
1505.508099	61.465408	65.665242
1505.152622	63.392473	65.670247
1504.214549	64.719808	65.675252
1504.129009	57.460171	65.680257
1503.778534	69.498679	65.685262
1503.011363	61.807833	65.690266
1502.238225	62.050672	65.695271
1501.590464	65.005875	65.700276
1500.465584	49.099797	65.705281
1499.956885	55.102106	65.710286
1499.505598	55.937198	65.715290
1498.935938	57.036092	65.720295
1498.116015	65.816021	65.725300
1497.042102	50.539874	65.730305
1496.056569	64.058322	65.735310
1495.685386	55.458166	65.740314
1495.559394	59.103635	65.745319
1494.877144	62.322886	65.750324
1494.210129	54.717136	65.755329
1493.061947	64.615829	65.760334
1492.168508	64.002984	65.765338
1492.029758	57.042179	65.770343
1491.444307	55.987823	65.775348
1491.102466	50.892486	65.780353
1490.488953	63.591770	65.785358
1489.277150	57.610770	65.790362
1488.622762	64.003134	65.795367
1487.785207	66.710967	65.800372
1487.680617	56.853790	65.805377
1486.829774	59.625473	65.810382
1485.711253	60.939881	65.815386
1485.077111	63.525666	65.820391
1484.882969	68.349195	65.825396
1484.963349	62.555170	65.830401
1483.669570	62.081897	65.835406
1482.518986	66.967288	65.840410
1482.256240	60.750830	65.845415
1481.544955	62.745899	65.850420
1481.234025	63.562891	65.855425
1479.835221	57.012350	65.860430
1479.228110	58.200941	65.865434
1478.862665	59.176862	65.870439
1478.577158	56.718864	65.875444
1477.835635	55.273611	65.880449
1476.427090	57.960363	65.885454
1475.964168	62.209396	65.890458
1475.592351	54.288268	65.895463
1475.281000	57.496536	65.900468
1474.613636	53.454369	65.905473
1473.461256	53.436085	65.910478
1472.821867	56.899043	65.915482
1472.777016	58.101526	65.920487
1471.346130	60.309363	65.925492
1470.465413	52.106277	65.930497
1470.182929	59.865445	65.935502
1469.303526	56.603220	65.940506
1469.105419	59.506330	65.945511
1468.559187	63.381220	65.950516
1467.826764	56.910038	65.955521
1466.958121	59.648850	65.960526
1466.280668	57.424905	65.965530
1466.040009	52.761047	65.970535
1464.488995	64.249147	65.975540
1463.953562	51.439017	65.980545
1463.113049	57.123929	65.985550
1462.401065	52.478378	65.990554
1462.353427	45.673688	65.995559
1462.099123	61.742773	66.000564
1461.691174	54.341361	66.005569
1460.719753	47.318225	66.010574
1460.144757	49.819679	66.015578
1459.369631	47.735606	66.020583
1458.143290	52.095963	66.025588
1457.344534	58.740000	66.030593
1456.688278	57.122268	66.035598
1456.768480	50.430295	66.040602
1456.132933	58.980121	66.045607
1454.667065	64.499323	66.050612
1454.146842	55.958629	66.055617
1453.647488	54.574951	66.060622
1453.199194	62.431575	66.065626
1453.136527	56.219953	66.070631
1451.678858	60.464784	66.075636
1451.380302	55.901621	66.080641
1450.657469	53.956618	66.085646
1449.964201	58.781500	66.090650
1448.749605	55.683620	66.095655
1448.099143	61.006811	66.100660
1447.601887	54.572352	66.105665
1446.975813	60.774748	66.110670
1446.732919	58.667469	66.115674
1446.457174	47.096918	66.120679
1445.015724	57.515918	66.125684
1444.465463	49.882302	66.130689
1443.974004	56.588604	66.135694
1443.145437	58.948735	66.140698
1442.166116	49.769819	66.145703
1441.279312	63.006514	66.150708
1440.722781	55.329366	66.155713
1440.461750	54.909850	66.160718
1439.841223	57.165297	66.165722
1439.656562	51.397697	66.170727
1439.081267	58.755819	66.175732
1438.438566	52.474147	66.180737
1437.374820	60.600712	66.185742
1436.110160	61.466878	66.190746
1435.544384	51.618390	66.195751
1434.333616	49.853219	66.200756
1434.811960	58.249095	66.205761
1433.890707	50.569250	66.210766
1433.846074	61.304536	66.215770
1433.208785	61.027972	66.220775
1432.132084	58.278318	66.225780
1431.255358	50.799658	66.230785
1431.042153	61.073164	66.235790
1429.772201	65.290212	66.240794
1429.281024	56.270099	66.245799
1428.601266	65.291686	66.250804
1428.700923	64.685702	66.255809
1427.424755	59.844632	66.260814
1426.096331	62.223223	66.265818
1425.790373	64.725999	66.270823
1424.917182	64.969397	66.275828
1424.833080	61.245803	66.280833
1424.350946	64.689744	66.285838
1423.363375	65.433488	66.290842
1422.778032	57.018019	66.295847
1421.776771	61.706158	66.300852
1421.789070	58.695109	66.305857
1420.956973	61.508984	66.310862
1420.007432	61.968732	66.315866
1419.355345	50.519046	66.320871
1418.764022	59.629698	66.325876
1418.507115	55.321502	66.330881
1417.171997	62.320629	66.335886
1416.297903	67.565660	66.340890
1415.392633	62.039031	66.345895
1415.265344	68.593797	66.350900
1415.079466	60.087454	66.355905
1414.577273	59.979206	66.360910
1413.648769	61.845288	66.365914
1413.046918	60.120360	66.370919
1412.012654	60.835389	66.375924
1412.040806	58.484358	66.380929
1410.833799	56.683813	66.385934
1410.148532	56.594272	66.390938
1409.352911	48.975820	66.395943
1408.671000	67.208524	66.400948
1408.104634	60.241583	66.405953
1407.655172	61.356621	66.410958
1406.425121	58.489150	66.415962
1406.128860	57.472932	66.420967
1405.519921	63.160448	66.425972
1405.472570	55.341679	66.430977
1404.583389	55.440982	66.435982
1403.183779	61.048322	66.440986
1403.203311	56.913457	66.445991
1402.708331	60.050138	66.450996
1401.497179	66.524389	66.456001
1400.485910	56.314025	66.461006
1399.921215	59.323699	66.466010
1399.837306	50.024287	66.471015
1398.774132	57.743408	66.476020
1398.401661	53.816953	66.481025
1397.235429	55.069287	66.486030
1396.337573	51.483805	66.491034
1395.928514	53.454386	66.496039
1395.684260	56.669328	66.501044
1395.537792	47.028538	66.506049
1394.998503	52.963064	66.511054
1393.678465	56.984227	66.516058
1392.824071	53.837732	66.521063
1392.249513	56.602790	66.526068
1392.002413	57.355968	66.531073
1390.990434	58.783600	66.536078
1390.046203	57.954479	66.541082
1389.833230	56.308245	66.546087
1389.227046	64.320181	66.551092
1388.091570	56.692014	66.556097
1387.403918	56.935631	66.561102
1386.626341	52.383028	66.566106
1386.265176	55.405624	66.571111
1385.361489	56.054888	66.576116
1385.307068	52.923426	66.581121
1385.158038	59.152713	66.586126
1384.013501	60.862762	66.591130
1383.381332	48.491168	66.596135
1382.418962	62.764697	66.601140
1381.688301	50.797574	66.606145
1380.766141	59.687371	66.611150
1380.007217	56.837942	66.616154
1379.839750	56.384652	66.621159
1379.268036	50.615421	66.626164
1378.752937	42.485958	66.631169
1377.485372	53.171635	66.636174
1376.927157	55.519837	66.641178
1376.674540	52.334280	66.646183
1376.220197	52.206398	66.651188
1375.482232	53.027023	66.656193
1374.451913	56.757425	66.661198
1373.693247	56.370599	66.666202
1373.505391	51.541797	66.671207
1372.306476	62.314409	66.676212
1371.323499	59.123615	66.681217
1370.928083	61.429742	66.686222
1370.721102	59.454867	66.691226
1370.376900	53.287498	66.696231
1369.734599	58.618375	66.701236
1368.479646	53.819086	66.706241
1367.921374	57.979450	66.711246
1367.006159	52.767944	66.716250
1366.680411	59.181816	66.721255
1365.491663	64.886090	66.726260
1364.909210	52.677689	66.731265
1364.099315	57.623985	66.736270
1364.084104	55.475764	66.741274
1363.929746	50.164015	66.746279
1362.775695	61.950478	66.751284
1361.857606	60.608885	66.756289
1361.025380	54.179285	66.761294
1360.812936	58.441495	66.766298
1360.238956	50.142119	66.771303
1359.304783	53.882510	66.776308
1358.265852	50.946813	66.781313
1357.591341	48.455948	66.786318
1357.610163	58.311983	66.791322
1357.247525	46.182798	66.796327
1355.681382	56.480270	66.801332
1355.524008	49.695952	66.806337
1354.343728	55.810465	66.811342
1353.999426	52.383643	66.816346
1353.793986	55.910874	66.821351
1352.463495	56.469396	66.826356
1351.860819	46.683297	66.831361
1351.434028	52.229505	66.836366
1350.940088	64.742537	66.841370
1350.833417	52.596372	66.846375
1349.073440	60.926205	66.851380
1348.330924	47.343964	66.856385
1347.954752	46.086047	66.861390
1347.485866	57.932843	66.866394
1347.070712	43.522893	66.871399
1345.575698	52.630746	66.876404
1345.301095	51.689374	66.881409
1344.963132	46.732333	66.886414
1344.104247	48.556113	66.891418
1343.941195	56.120366	66.896423
1342.451343	61.842635	66.901428
1342.119286	47.844753	66.906433
1341.815980	53.746385	66.911438
1340.900002	56.749489	66.916442
1339.936611	52.158839	66.921447
1339.104378	54.384619	66.926452
1338.709092	55.266976	66.931457
1338.132366	56.458275	66.936462
1337.782692	53.511957	66.941466
1337.313047	48.251026	66.946471
1335.735136	53.377346	66.951476
1335.438030	53.492538	66.956481
1334.641827	52.076800	66.961486
1334.008736	51.488887	66.966490
1334.028537	44.062036	66.971495
1332.977290	52.945117	66.976500
1332.220107	49.200180	66.981505
1331.949721	54.769745	66.986510
1331.121921	48.517414	66.991514
1330.142575	56.279032	66.996519
1329.032878	55.039323	67.001524
1328.996459	49.548317	67.006529
1328.618521	44.693643	67.011534
1327.642202	47.726418	67.016538
1327.211771	44.713405	67.021543
1326.628329	49.802901	67.026548
1326.088289	38.450508	67.031553
1324.891946	47.568809	67.036558
1323.847425	47.489466	67.041562
1323.324450	43.857984	67.046567
1322.583793	45.389963	67.051572
1322.690222	52.901765	67.056577
1321.975158	42.285088	67.061582
1320.654864	56.809745	67.066586
1320.243421	50.787705	67.071591
1319.534813	52.247886	67.076596
1319.242096	55.758085	67.081601
1318.744233	56.232103	67.086606
1317.513257	53.957683	67.091610
1317.149082	48.697251	67.096615
1316.301931	58.192735	67.101620
1315.940094	52.519817	67.106625
1315.037197	54.977949	67.111630
1314.111508	58.940700	67.116634
1313.616804	47.046095	67.121639
1313.013303	51.190125	67.126644
1312.670601	51.890596	67.131649
1311.310792	48.635650	67.136654
1310.728728	51.653434	67.141658
1310.388829	47.891933	67.146663
1309.510396	61.125618	67.151668
1309.163226	56.405011	67.156673
1308.778774	57.448140	67.161678
1308.197344	53.365240	67.166682
1307.403274	52.885017	67.171687
1306.928595	56.379789	67.176692
1305.963946	50.155232	67.181697
1304.832676	54.193438	67.186702
1304.281831	52.415586	67.191706
1303.969511	50.994381	67.196711
1303.317649	60.070006	67.201716
1302.673319	51.344153	67.206721
1301.844361	54.632746	67.211726
1300.755441	63.112963	67.216730
1300.410974	52.768746	67.221735
1300.104680	58.340117	67.226740
1299.070977	56.585324	67.231745
1298.613774	54.285413	67.236750
1297.723121	70.106204	67.241754
1297.388650	53.519785	67.246759
1296.830259	60.787786	67.251764
1295.624304	52.671607	67.256769
1294.652906	55.452902	67.261774
1294.036737	58.112597	67.266778
1294.050225	59.802831	67.271783
1293.160694	60.445740	67.276788
1293.055989	51.344497	67.281793
1292.329183	59.564179	67.286798
1291.276812	65.669835	67.291802
1290.834275	52.351632	67.296807
1289.965472	66.785194	67.301812
1288.726510	55.024711	67.306817
1288.247585	52.220124	67.311822
1287.545270	61.070320	67.316826
1287.170051	50.008249	67.321831
1286.707094	53.567328	67.326836
1286.667353	46.067783	67.331841
1285.892096	48.663532	67.336846
1284.717206	60.843156	67.341850
1284.318252	48.404427	67.346855
1283.187122	55.619299	67.351860
1282.297409	58.271354	67.356865
1281.799685	55.682739	67.361870
1281.325012	57.616009	67.366874
1280.982970	43.371182	67.371879
1280.247535	53.363830	67.376884
1279.674387	44.231083	67.381889
1278.792055	54.379136	67.386894
1278.092528	46.678349	67.391898
1277.720946	50.038636	67.396903
1276.502860	63.439413	67.401908
1275.774074	50.962023	67.406913
1275.096196	54.902485	67.411918
1274.743434	59.095563	67.416922
1274.434024	58.402905	67.421927
1273.458456	63.277317	67.426932
1272.356010	55.606428	67.431937
1271.972157	65.598496	67.436942
1270.729378	57.065096	67.441946
1270.612139	49.654998	67.446951
1270.597534	64.306251	67.451956
1270.020612	58.256890	67.456961
1268.821676	49.030759	67.461966
1268.025632	58.273166	67.466970
1267.926500	49.140184	67.471975
1266.821404	60.738678	67.476980
1265.663451	51.353170	67.481985
1265.381061	50.111572	67.486990
1264.923377	57.944145	67.491994
1264.488125	53.809386	67.496999
1263.936665	60.165193	67.502004
1262.814189	57.381972	67.507009
1261.881050	61.014839	67.512014
1261.314270	52.223221	67.517018
1261.252939	57.803967	67.522023
1260.445741	65.104699	67.527028
1259.173830	61.633018	67.532033
1258.615848	60.189533	67.537038
1257.979303	67.331978	67.542042
1257.773128	53.524917	67.547047
1257.217552	64.614094	67.552052
1256.536882	58.189358	67.557057
1255.816240	64.747413	67.562062
1254.912864	59.570613	67.567066
1254.433002	64.914346	67.572071
1253.355692	63.772130	67.577076
1252.541742	57.260876	67.582081
1252.205049	67.396837	67.587086
1251.614135	71.324785	67.592090
1251.243922	54.949353	67.597095
1250.467029	67.892912	67.602100
1249.495529	56.333747	67.607105
1248.743832	58.593512	67.612110
1248.097282	58.264876	67.617114
1248.214520	53.745019	67.622119
1247.308903	61.013654	67.627124
1246.132837	59.864665	67.632129
1245.711220	53.929240	67.637134
1244.847151	53.730208	67.642138
1244.825632	51.478471	67.647143
1243.976585	53.363343	67.652148
1243.236458	52.624433	67.657153
1242.637358	54.825312	67.662158
1241.422578	57.561840	67.667162
1240.867396	52.242149	67.672167
1239.744927	58.797553	67.677172
1239.201911	50.656708	67.682177
1238.830038	53.488520	67.687182
1238.401196	58.606817	67.692186
1238.370786	49.788504	67.697191
1237.632859	56.657001	67.702196
1236.857668	57.251135	67.707201
1236.256522	59.660777	67.712206
1235.270128	60.279228	67.717210
1234.136318	53.790770	67.722215
1233.024674	57.554853	67.727220
1232.935373	48.293489	67.732225
1232.700184	51.577929	67.737230
1232.005971	59.502707	67.742234
1231.768853	52.323126	67.747239
1230.345820	48.304199	67.752244
1229.631706	48.374350	67.757249
1229.443003	47.799181	67.762254
1228.532537	58.139942	67.767258
1227.761591	47.683240	67.772263
1226.646595	57.028806	67.777268
1226.508641	52.423173	67.782273
1225.897439	51.453388	67.787278
1225.332691	52.757510	67.792282
1225.207198	48.181323	67.797287
1224.239728	59.489428	67.802292
1223.411446	60.294750	67.807297
1222.685888	53.393389	67.812302
1221.436939	59.799933	67.817306
1221.436281	56.548357	67.822311
1220.810232	56.690270	67.827316
1220.268880	61.475742	67.832321
1219.257416	55.417897	67.837326
1218.196482	61.065578	67.842330
1218.052943	52.916734	67.847335
1217.433761	54.485954	67.852340
1216.971628	50.411064	67.857345
1215.547937	46.960253	67.862350
1214.966056	54.153332	67.867354
1214.796717	58.732619	67.872359
1213.787694	60.472394	67.877364
1213.519431	52.502792	67.882369
1212.824992	54.711313	67.887374
1211.905034	54.966307	67.892378
1211.364726	59.257809	67.897383
1210.525586	66.203638	67.902388
1210.478201	59.367738	67.907393
1209.571878	50.511507	67.912398
1208.209469	69.355684	67.917402
1207.515951	60.564851	67.922407
1207.005726	61.384796	67.927412
1206.984224	53.511492	67.932417
1206.527572	57.944190	67.937422
1205.810624	63.778493	67.942426
1204.914615	42.919122	67.947431
1204.294635	61.970503	67.952436
1203.461534	57.679668	67.957441
1202.609427	53.969953	67.962446
1201.709406	59.571533	67.967450
1201.290453	56.853000	67.972455
1200.666626	60.426207	67.977460
1200.169954	63.839494	67.982465
1199.772030	56.717840	67.987470
1198.509231	65.924123	67.992474
1198.198054	53.916410	67.997479
1197.675926	64.425152	68.002484
1197.075375	61.534035	68.007489
1195.907651	58.093480	68.012494
1194.912911	67.053352	68.017498
1194.798949	63.259887	68.022503
1194.136048	63.344168	68.027508
1193.847434	57.511893	68.032513
1192.886061	54.631637	68.037518
1191.885069	63.898090	68.042522
1191.073186	55.922885	68.047527
1190.226184	63.957506	68.052532
1190.446982	63.457087	68.057537
1190.484582	53.676260	68.062542
1189.355177	63.994516	68.067546
1188.480997	57.187683	68.072551
1187.697472	57.906403	68.077556
1186.579468	58.636209	68.082561
1185.758099	60.877123	68.087566
1185.135204	59.612123	68.092570
1184.717228	58.938059	68.097575
1184.562224	66.146079	68.102580
1184.573925	55.414864	68.107585
1183.700605	53.306206	68.112590
1182.340457	57.729789	68.117594
1182.068971	59.471181	68.122599
1180.545024	68.587582	68.127604
1179.912441	66.590066	68.132609
1179.486299	59.682840	68.137614
1178.874539	65.401641	68.142618
1178.450624	59.841599	68.147623
1177.710377	62.449923	68.152628
1176.752102	56.576788	68.157633
1175.903826	53.178645	68.162638
1175.281702	60.148498	68.167642
1175.207007	54.599716	68.172647
1174.821972	58.383869	68.177652
1173.971448	59.776398	68.182657
1173.080941	59.036801	68.187662
1172.354994	62.987083	68.192666
1171.906837	58.467721	68.197671
1171.206977	61.189519	68.202676
1170.122550	56.624369	68.207681
1169.396066	59.108369	68.212686
1168.804256	56.415488	68.217690
1168.432852	59.962452	68.222695
1167.809264	60.603662	68.227700
1167.619997	60.295026	68.232705
1166.735449	54.785436	68.237710
1165.995997	60.694249	68.242714
1165.679040	54.143710	68.247719
1164.061279	56.520589	68.252724
1163.278861	61.646535	68.257729
1162.811282	49.669954	68.262734
1162.466987	60.285210	68.267738
1162.390598	57.473293	68.272743
1161.624877	63.550807	68.277748
1160.451657	52.056999	68.282753
1160.047933	52.284795	68.287758
1159.150288	65.768870	68.292762
1158.185324	49.825679	68.297767
1157.500470	52.905284	68.302772
1156.691022	54.936540	68.307777
1156.047482	53.142605	68.312782
1155.494104	61.849681	68.317786
1155.479579	53.814537	68.322791
1155.008093	58.348457	68.327796
1154.222633	63.507687	68.332801
1153.415860	63.564900	68.337806
1152.646035	63.544737	68.342810
1152.176060	54.755907	68.347815
1150.933365	56.892132	68.352820
1150.839701	58.297172	68.357825
1149.944954	52.909328	68.362830
1149.083345	58.054360	68.367834
1148.899264	52.094463	68.372839
1147.567554	59.244627	68.377844
1147.017795	48.845200	68.382849
1146.948974	50.334403	68.387854
1146.319658	58.998824	68.392858
1145.458003	50.900714	68.397863
1144.464359	50.756253	68.402868
1143.693270	48.840088	68.407873
1143.557454	50.683771	68.412878
1142.636247	51.307262	68.417882
1141.755428	46.398987	68.422887
1140.913318	57.724315	68.427892
1140.280407	61.108040	68.432897
1139.964740	55.008444	68.437902
1139.509422	58.843710	68.442906
1139.467630	47.028693	68.447911
1138.186255	61.074628	68.452916
1137.108175	55.372800	68.457921
1136.853868	53.394992	68.462926
1135.787457	63.432876	68.467930
1135.670456	54.507825	68.472935
1134.480323	57.250023	68.477940
1133.600432	55.992326	68.482945
1133.830217	55.190776	68.487950
1133.118341	57.280719	68.492954
1132.267617	51.494572	68.497959
1131.205328	57.986796	68.502964
1130.592422	63.671060	68.507969
1129.899907	57.198250	68.512974
1129.745010	58.470492	68.517978
1129.316582	53.395551	68.522983
1128.329154	55.855554	68.527988
1127.616801	51.889044	68.532993
1126.561210	56.858487	68.537998
1125.619814	62.411507	68.543002
1125.348211	49.670362	68.548007
1124.548895	55.305231	68.553012
1124.332432	64.558931	68.558017
1123.718036	57.061875	68.563022
1122.914148	57.827905	68.568026
1122.396742	52.519923	68.573031
1121.939306	58.703329	68.578036
1120.999776	53.526833	68.583041
1120.515852	51.615579	68.588046
1119.338504	51.536918	68.593050
1118.932996	50.897829	68.598055
1118.364714	56.084607	68.603060
1117.440933	55.927004	68.608065
1116.691547	49.426834	68.613070
1116.018609	56.729452	68.618074
1115.401717	44.959627	68.623079
1114.826303	57.100167	68.628084
1114.469265	49.967187	68.633089
1113.920609	50.098624	68.638094
1112.714937	61.852505	68.643098
1112.517950	56.001394	68.648103
1111.677965	60.362768	68.653108
1111.081156	55.095224	68.658113
1110.109402	50.719209	68.663118
1109.498533	56.044721	68.668122
1108.930654	49.423873	68.673127
1108.646046	51.872082	68.678132
1107.917484	48.045319	68.683137
1106.740039	48.439943	68.688142
1105.852414	59.507028	68.693146
1105.485892	59.156513	68.698151
1104.992024	63.548223	68.703156
1104.464854	53.813191	68.708161
1104.206621	53.380189	68.713166
1103.063249	55.047468	68.718170
1102.229194	56.372849	68.723175
1102.152069	50.968166	68.728180
1100.907376	51.856650	68.733185
1100.051162	52.724402	68.738190
1099.710528	57.526824	68.743194
1099.228145	54.009600	68.748199
1098.581782	55.271265	68.753204
1097.764781	51.457278	68.758209
1097.007775	56.627033	68.763214
1096.480713	60.301306	68.768218
1095.940902	58.637242	68.773223
1095.295620	56.424821	68.778228
1094.027576	59.203262	68.783233
1093.724127	53.813650	68.788238
1092.961474	60.474430	68.793242
1092.753809	46.943174	68.798247
1091.836889	57.054140	68.803252
1090.969231	53.974712	68.808257
1090.570232	55.576107	68.813262
1090.010416	52.824079	68.818266
1089.584115	54.338180	68.823271
1088.551869	51.385615	68.828276
1087.835144	53.798088	68.833281
1087.466351	53.518617	68.838286
1086.332513	65.678209	68.843290
1085.591798	59.814025	68.848295
1084.660469	61.715774	68.853300
1084.237963	54.680450	68.858305
1083.812917	49.560729	68.863310
1083.238196	62.533216	68.868314
1082.865610	45.857074	68.873319
1082.133004	46.863523	68.878324
1080.870547	56.545787	68.883329
1080.605238	51.534891	68.888334
1079.614387	50.922225	68.893338
1079.605102	43.299464	68.898343
1079.093016	49.054879	68.903348
1077.760893	58.934592	68.908353
1077.202008	58.054152	68.913358
1076.729855	55.605650	68.918362
1076.317697	53.344234	68.923367
1075.079034	49.636402	68.928372
1074.171509	60.230079	68.933377
1073.400815	53.577258	68.938382
1073.002730	50.992528	68.943386
1072.871708	48.512850	68.948391
1072.454672	51.680412	68.953396
1071.617623	51.914919	68.958401
1070.986241	48.755565	68.963406
1070.265341	50.710093	68.968410
1069.402772	49.341685	68.973415
1068.211546	55.324707	68.978420
1067.612928	55.876394	68.983425
1067.571440	49.070684	68.988430
1066.741897	60.605433	68.993434
1066.536642	54.548911	68.998439
1065.151567	52.066091	69.003444
1064.876509	51.831357	69.008449
1064.148925	44.413699	69.013454
1063.134223	54.535883	69.018458
1062.296959	51.373893	69.023463
1061.286076	47.870994	69.028468
1061.003299	50.518618	69.033473
1061.029896	50.889038	69.038478
1060.508123	61.128913	69.043482
1060.025715	60.749300	69.048487
1059.007995	56.707994	69.053492
1058.164050	57.010391	69.058497
1057.672445	53.698820	69.063502
1056.701209	58.963288	69.068506
1056.032041	52.228747	69.073511
1055.078187	53.566756	69.078516
1054.578377	60.162399	69.083521
1054.418589	51.861234	69.088526
1053.962329	60.387477	69.093530
1052.903625	59.081472	69.098535
1051.902760	52.119536	69.103540
1051.029567	55.016678	69.108545
1051.133508	47.880161	69.113550
1050.441284	57.340448	69.118554
1049.847595	50.432729	69.123559
1048.800591	55.682936	69.128564
1048.217986	56.438715	69.133569
1047.993111	54.767305	69.138574
1046.274917	61.307916	69.143578
1046.109714	56.754329	69.148583
1045.569139	58.488518	69.153588
1045.057341	65.362912	69.158593
1044.627983	54.027540	69.163598
1043.862437	62.765818	69.168602
1042.802709	61.488015	69.173607
1042.022380	61.702157	69.178612
1041.469757	60.967878	69.183617
1041.356730	57.115057	69.188622
1039.525432	53.752653	69.193626
1039.181955	59.489463	69.198631
1038.646355	62.780748	69.203636
1038.166886	60.172064	69.208641
1038.299895	58.240825	69.213646
1037.241578	61.923581	69.218650
1036.452171	55.831312	69.223655
1035.609338	59.603081	69.228660
1035.115539	62.205927	69.233665
1034.823388	54.590949	69.238670
1033.366736	57.134873	69.243674
1032.644972	58.410248	69.248679
1032.093326	57.125174	69.253684
1031.227572	59.368579	69.258689
1031.545029	53.650422	69.263694
1030.631299	56.939358	69.268698
1029.719028	54.519654	69.273703
1028.704590	53.658814	69.278708
1028.309722	59.801114	69.283713
1027.896043	57.273924	69.288718
1027.384446	57.635460	69.293722
1026.521795	54.647551	69.298727
1026.036369	56.481635	69.303732
1025.179500	53.764696	69.308737
1024.320389	52.557537	69.313742
1022.959344	58.297690	69.318746
1023.178648	51.053790	69.323751
1022.356071	55.359300	69.328756
1021.965059	66.796460	69.333761
1022.008834	55.106135	69.338766
1020.772329	58.359168	69.343770
1020.155076	55.527384	69.348775
1019.391371	62.195850	69.353780
1017.683559	59.379120	69.358785
1017.507352	57.039806	69.363790
1016.652549	61.483067	69.368794
1016.452185	53.943553	69.373799
1016.079740	52.772259	69.378804
1015.384975	62.901240	69.383809
1014.840882	54.964296	69.388814
1013.840760	58.996676	69.393818
1013.360262	53.537925	69.398823
1013.092539	54.632922	69.403828
1011.772825	48.699367	69.408833
1011.149407	48.369564	69.413838
1010.361516	57.227715	69.418842
1010.212609	56.464960	69.423847
1009.275971	53.427755	69.428852
1008.148833	60.765533	69.433857
1007.628252	57.184602	69.438862
1006.922183	70.637853	69.443866
1006.520721	55.955249	69.448871
1006.409266	59.661770	69.453876
1005.347821	63.494664	69.458881
1004.627084	52.955609	69.463886
1003.678882	62.248958	69.468890
1003.164194	56.444370	69.473895
1003.208452	52.633693	69.478900
1001.726507	63.081418	69.483905
1001.017539	49.549583	69.488910
1000.454958	57.529193	69.493914
1000.295925	53.677939	69.498919
999.678347	56.559339	69.503924
998.302997	56.548955	69.508929
997.844352	50.015995	69.513934
997.142033	61.628429	69.518938
996.812866	51.160075	69.523943
996.529027	59.635871	69.528948
995.280098	56.488737	69.533953
994.669880	55.493157	69.538958
994.000231	61.595678	69.543962
993.911404	52.611745	69.548967
992.671830	62.860078	69.553972
991.657681	58.615686	69.558977
991.368658	56.033207	69.563982
991.013446	59.030722	69.568986
990.657435	52.528340	69.573991
989.446624	57.644382	69.578996
988.343417	55.243175	69.584001
987.966828	50.694612	69.589006
987.169180	58.061224	69.594010
987.284260	47.121291	69.599015
986.179657	55.713171	69.604020
984.935650	52.866760	69.609025
984.892726	57.770560	69.614030
984.170196	56.917368	69.619034
983.711821	50.995778	69.624039
982.319765	52.968552	69.629044
981.503672	50.792505	69.634049
981.462162	44.696902	69.639054
980.773426	55.392843	69.644058
980.420096	53.397270	69.649063
980.094909	55.385484	69.654068
979.011704	55.298629	69.659073
978.321905	50.790286	69.664078
977.741410	59.365040	69.669082
976.825202	56.873788	69.674087
975.763107	54.949466	69.679092
975.238933	61.303376	69.684097
974.672249	57.019856	69.689102
974.296459	55.572443	69.694106
973.953639	58.607702	69.699111
972.957243	55.968350	69.704116
972.055604	55.195962	69.709121
971.957358	54.060210	69.714126
971.232365	55.889538	69.719130
970.654778	54.133281	69.724135
969.789089	52.537674	69.729140
968.961346	56.906836	69.734145
968.732757	51.952817	69.739150
967.450464	60.030424	69.744154
966.463225	55.974053	69.749159
966.295462	56.135007	69.754164
965.700712	60.839644	69.759169
965.212598	52.380387	69.764174
964.268139	57.040313	69.769178
963.274513	52.218893	69.774183
962.582840	55.471783	69.779188
962.150482	57.560848	69.784193
962.005422	57.550950	69.789198
961.527812	60.004194	69.794202
960.454981	62.969881	69.799207
959.645699	56.984843	69.804212
958.872236	60.023201	69.809217
958.580510	57.993790	69.814222
957.811436	62.601578	69.819226
957.175217	60.291709	69.824231
956.113941	71.472625	69.829236
955.816751	68.871020	69.834241
955.255749	58.727359	69.839246
954.006733	56.951101	69.844250
953.369246	64.150560	69.849255
952.624792	56.851857	69.854260
952.448339	62.148769	69.859265
952.249386	60.955268	69.864270
951.407357	64.628233	69.869274
951.013986	54.465340	69.874279
949.861399	59.285643	69.879284
949.114812	57.656617	69.884289
948.426867	48.902790	69.889294
947.211021	57.889103	69.894298
946.671492	48.102149	69.899303
946.141908	59.881963	69.904308
945.629750	55.246102	69.909313
945.473586	54.206317	69.914318
944.884961	60.121684	69.919322
944.163883	52.641754	69.924327
943.210591	55.474082	69.929332
942.898269	58.924492	69.934337
942.284504	60.755300	69.939342
940.926255	57.638745	69.944346
940.278880	55.736558	69.949351
939.658697	61.507338	69.954356
939.519342	55.538617	69.959361
938.613547	57.614035	69.964366
937.337240	63.387061	69.969370
936.821889	55.575860	69.974375
936.651982	58.142583	69.979380
935.798157	60.314884	69.984385
935.885956	57.572747	69.989390
934.697388	58.204567	69.994394
934.020961	57.202178	69.999399
933.532609	50.602478	70.004404
932.832925	47.167886	70.009409
931.852333	48.624173	70.014414
930.898669	56.304863	70.019418
930.229976	53.104950	70.024423
929.884045	57.680136	70.029428
929.474050	59.977731	70.034433
929.073328	56.518776	70.039438
927.758770	54.497580	70.044442
927.407742	50.620006	70.049447
926.881069	51.232016	70.054452
926.105910	60.837164	70.059457
925.130944	51.570817	70.064462
924.470001	57.995123	70.069466
924.086522	46.057087	70.074471
923.699736	52.013275	70.079476
922.961475	54.517082	70.084481
922.055021	52.806105	70.089486
920.891357	59.475581	70.094490
920.478236	52.693664	70.099495
920.218683	48.944891	70.104500
919.898103	57.802350	70.109505
918.935292	51.905983	70.114510
918.391992	56.818509	70.119514
917.654303	44.803384	70.124519
916.575986	51.243516	70.129524
915.262972	60.304500	70.134529
915.066119	54.946782	70.139534
914.492548	60.500381	70.144538
914.507308	55.708362	70.149543
913.892564	53.694806	70.154548
913.374536	53.986406	70.159553
912.066047	48.740531	70.164558
911.246301	54.112486	70.169562
911.014578	55.308290	70.174567
910.318529	50.121330	70.179572
909.349126	58.315875	70.184577
908.669948	49.149262	70.189582
908.040351	54.134986	70.194586
907.567673	50.298380	70.199591
907.238502	56.751911	70.204596
906.302848	54.003098	70.209601
905.262785	50.481157	70.214606
904.800328	56.122693	70.219610
904.379921	56.653350	70.224615
904.088833	52.665649	70.229620
902.464529	60.451731	70.234625
902.237727	49.861264	70.239630
901.583590	49.159784	70.244634
901.577951	51.609560	70.249639
900.382880	59.460672	70.254644
899.751583	52.576001	70.259649
899.371363	49.950338	70.264654
897.644620	56.857566	70.269658
897.103047	49.590444	70.274663
896.484430	50.234782	70.279668
895.771779	51.694919	70.284673
895.663212	50.403841	70.289678
894.942804	55.973904	70.294682
894.739215	56.267701	70.299687
894.025363	51.025769	70.304692
893.247005	52.973189	70.309697
892.501535	46.870273	70.314702
891.564613	54.047599	70.319706
890.817777	50.267030	70.324711
890.021880	51.443810	70.329716
889.064922	56.562179	70.334721
889.318000	56.337258	70.339726
888.493912	52.105734	70.344730
888.126599	55.876994	70.349735
886.856700	45.078367	70.354740
886.570587	50.255116	70.359745
885.929716	49.661491	70.364750
885.534401	51.921443	70.369754
884.537419	49.145247	70.374759
883.390240	53.418743	70.379764
882.836410	51.911048	70.384769
882.846762	36.651932	70.389774
881.807869	53.455283	70.394778
880.810582	48.918708	70.399783
880.132421	53.668027	70.404788
879.377638	49.766065	70.409793
879.215825	42.162737	70.414798
878.612194	52.548855	70.419802
878.297837	45.086515	70.424807
877.394542	47.703852	70.429812
876.432318	52.453669	70.434817
876.051533	48.423312	70.439822
874.753017	57.452609	70.444826
874.024362	51.743505	70.449831
873.612459	50.042170	70.454836
873.077419	51.417814	70.459841
872.941952	43.099090	70.464846
871.974363	49.091206	70.469850
871.161741	47.809013	70.474855
870.310339	45.252610	70.479860
869.656298	48.686158	70.484865
869.522452	41.858393	70.489870
868.739161	54.338857	70.494874
868.173450	45.470568	70.499879
867.083806	47.309868	70.504884
866.324570	50.640257	70.509889
866.170507	46.121488	70.514894
865.083809	51.884152	70.519898
864.151576	48.472825	70.524903
863.439293	41.038779	70.529908
863.188301	49.793923	70.534913
862.756694	53.761712	70.539918
862.471158	55.709195	70.544922
861.668856	48.190307	70.549927
860.847651	49.039865	70.554932
860.225158	50.998090	70.559937
859.444886	43.915934	70.564942
858.227466	50.724486	70.569946
857.918860	41.363767	70.574951
857.455948	44.337102	70.579956
856.761577	56.721026	70.584961
856.231734	50.780516	70.589966
854.877929	58.014647	70.594970
854.714950	51.648951	70.599975
854.087649	49.901226	70.604980
853.581714	52.008426	70.609985
853.234600	45.399943	70.614990
851.882963	57.348975	70.619994
851.314578	47.625008	70.624999
850.804934	46.592881	70.630004
849.540717	52.775143	70.635009
849.207959	49.373240	70.640014
848.227292	56.865942	70.645018
847.887344	48.991958	70.650023
847.259238	51.154819	70.655028
846.886631	52.611584	70.660033
846.964671	48.096480	70.665038
846.066128	61.615846	70.670042
845.352566	45.285918	70.675047
844.212247	46.626299	70.680052
843.054292	53.696233	70.685057
842.330702	45.336545	70.690062
842.139437	56.095694	70.695066
841.797899	46.464315	70.700071
841.144703	41.774873	70.705076
839.671408	46.844325	70.710081
839.429479	41.516049	70.715086
838.150993	46.748307	70.720090
838.030247	42.075817	70.725095
837.602271	41.117725	70.730100
837.030954	47.330901	70.735105
836.103858	42.311027	70.740110
835.139341	44.110349	70.745114
834.881628	50.474273	70.750119
834.559125	47.265605	70.755124
834.122442	60.154837	70.760129
832.745280	42.121705	70.765134
832.146041	48.340849	70.770138
831.836536	54.331168	70.775143
830.657053	53.186026	70.780148
829.768683	58.415412	70.785153
829.429328	41.649969	70.790158
828.533651	47.983832	70.795162
828.587623	43.232866	70.800167
828.426509	47.916913	70.805172
826.727495	55.362933	70.810177
825.744906	48.090054	70.815182
825.196326	53.220977	70.820186
824.729603	45.440945	70.825191
824.671504	43.379819	70.830196
824.054877	46.054240	70.835201
823.245928	42.434317	70.840206
822.371897	49.084983	70.845210
821.595095	53.491223	70.850215
821.349993	43.432038	70.855220
820.281518	49.592618	70.860225
819.417750	48.841797	70.865230
819.025806	46.377617	70.870234
818.402210	51.434551	70.875239
818.162910	46.993146	70.880244
817.204805	59.659076	70.885249
816.778848	48.716310	70.890254
816.239924	55.107090	70.895258
814.667833	48.948424	70.900263
814.052251	46.068233	70.905268
813.354320	50.743185	70.910273
813.248608	48.338918	70.915278
812.832159	41.347999	70.920282
811.497724	46.118951	70.925287
810.729439	40.989384	70.930292
810.122286	56.655820	70.935297
809.716730	45.078808	70.940302
809.612444	48.160050	70.945306
808.542319	47.916659	70.950311
807.731601	45.151600	70.955316
806.952292	51.038453	70.960321
806.299334	49.159348	70.965326
805.929783	54.803129	70.970330
805.290972	46.296697	70.975335
804.204781	48.231335	70.980340
803.693407	55.011322	70.985345
803.485155	44.828991	70.990350
802.684318	53.274129	70.995354
801.566972	58.350909	71.000359
801.048887	52.060649	71.005364
800.240551	46.944654	71.010369
800.329726	43.065900	71.015374
799.475497	46.592163	71.020378
798.565536	46.798154	71.025383
798.311859	47.368151	71.030388
797.456930	50.519950	71.035393
796.652006	45.730196	71.040398
795.362826	57.170801	71.045402
795.231589	43.018652	71.050407
794.897423	48.820966	71.055412
794.053593	53.926285	71.060417
793.041341	48.914295	71.065422
791.924840	46.447131	71.070426
791.925077	52.546225	71.075431
791.270933	49.248323	71.080436
790.634912	52.040538	71.085441
790.526274	46.448658	71.090446
789.103857	46.575468	71.095450
788.658267	43.602614	71.100455
787.972956	44.509033	71.105460
787.246289	51.527992	71.110465
786.894107	45.475752	71.115470
785.925883	58.038817	71.120474
785.062946	48.398081	71.125479
784.558286	50.880047	71.130484
783.457565	51.933016	71.135489
783.696537	45.585709	71.140494
782.573066	42.183872	71.145498
781.793071	44.207766	71.150503
781.252323	52.636379	71.155508
780.864298	55.300461	71.160513
780.650921	47.133243	71.165518
779.610452	46.862279	71.170522
778.467060	42.391415	71.175527
777.846291	49.089882	71.180532
777.232644	56.664189	71.185537
776.867681	45.151280	71.190542
776.022046	56.900757	71.195546
774.938786	52.731415	71.200551
774.423355	50.824020	71.205556
773.774949	57.591169	71.210561
773.802989	48.429754	71.215566
773.588541	55.653458	71.220570
772.405817	57.024012	71.225575
772.223187	54.730021	71.230580
770.673294	55.019586	71.235585
769.402751	41.318775	71.240590
769.068342	47.965821	71.245594
768.246770	52.186720	71.250599
767.852067	49.004240	71.255604
767.269550	48.473263	71.260609
767.215838	53.870321	71.265614
766.627711	58.463710	71.270618
765.827725	51.389686	71.275623
765.067874	38.445694	71.280628
764.516484	54.307825	71.285633
763.634935	42.620925	71.290638
762.372111	46.740972	71.295642
761.813635	49.624111	71.300647
761.672701	41.838019	71.305652
761.078244	50.742779	71.310657
760.752189	54.083841	71.315662
759.596584	49.159571	71.320666
759.063793	49.977108	71.325671
758.892931	42.821766	71.330676
756.938859	47.398891	71.335681
756.573229	43.958027	71.340686
756.044709	47.244169	71.345690
755.375363	44.821594	71.350695
755.150453	46.132677	71.355700
754.629906	52.626489	71.360705
753.683144	41.460341	71.365710
752.864352	52.111068	71.370714
752.356059	41.495829	71.375719
752.154308	45.363065	71.380724
750.620548	48.335119	71.385729
749.928570	42.995531	71.390734
749.582985	43.949938	71.395738
749.096167	36.197445	71.400743
748.511992	51.059059	71.405748
747.575288	47.302360	71.410753
746.997454	37.041651	71.415758
745.883709	53.274044	71.420762
745.640675	38.796474	71.425767
745.950441	41.643373	71.430772
744.717262	53.309245	71.435777
744.063437	50.675997	71.440782
743.429402	56.663886	71.445786
742.188283	51.997809	71.450791
741.188592	47.461286	71.455796
740.813047	53.384369	71.460801
740.355050	47.598932	71.465806
739.955607	51.372542	71.470810
739.397326	42.886672	71.475815
738.134351	46.771106	71.480820
737.246948	46.565899	71.485825
737.005168	42.270183	71.490830
736.637755	49.797176	71.495834
736.495654	40.995686	71.500839
735.362361	43.438509	71.505844
734.431735	44.248809	71.510849
733.575685	38.706029	71.515854
733.049290	48.123705	71.520858
732.452535	42.157184	71.525863
731.559105	41.878804	71.530868
731.117711	47.965130	71.535873
730.305430	38.211534	71.540878
729.705703	54.774668	71.545882
729.410766	50.137550	71.550887
729.303117	44.954825	71.555892
727.806198	47.568883	71.560897
727.690772	43.879514	71.565902
726.209879	46.115453	71.570906
725.087303	47.456373	71.575911
724.979701	47.755837	71.580916
724.206672	47.486831	71.585921
724.313433	43.843474	71.590926
723.530507	46.191544	71.595930
723.127014	43.050049	71.600935
721.986642	44.686501	71.605940
721.032129	46.173095	71.610945
720.793009	46.484037	71.615950
720.349917	44.730827	71.620954
719.102976	40.686644	71.625959
718.533875	44.595101	71.630964
717.992850	49.871173	71.635969
717.575609	36.460370	71.640974
716.415239	42.960766	71.645978
715.939885	45.076158	71.650983
715.088980	48.117153	71.655988
714.482436	46.298792	71.660993
714.569453	42.570402	71.665998
713.339788	44.012559	71.671002
712.590736	35.393205	71.676007
712.109205	45.999180	71.681012
711.559660	47.649282	71.686017
711.087749	39.502683	71.691022
709.839100	47.392208	71.696026
709.183274	54.739677	71.701031
708.938896	42.537478	71.706036
707.862513	42.318864	71.711041
706.941059	41.349803	71.716046
706.094420	50.453678	71.721050
705.287007	46.203550	71.726055
705.233472	48.704155	71.731060
704.533529	52.888043	71.736065
704.651085	43.405003	71.741070
704.127186	43.058981	71.746074
703.368533	39.315606	71.751079
702.896202	42.933948	71.756084
700.897675	44.076796	71.761089
700.325716	35.197383	71.766094
699.693828	38.086786	71.771098
699.021963	39.721135	71.776103
699.016385	40.879388	71.781108
698.248156	40.422864	71.786113
698.146129	49.826654	71.791118
696.773377	41.749914	71.796122
696.080030	46.280808	71.801127
695.744462	38.567541	71.806132
695.392574	38.296652	71.811137
694.040572	40.701166	71.816142
693.311217	44.732600	71.821146
692.595788	48.331805	71.826151
692.408772	43.079396	71.831156
691.895587	51.476841	71.836161
690.893154	46.219263	71.841166
690.268519	45.646173	71.846170
688.988497	51.766440	71.851175
689.136385	47.042807	71.856180
688.238504	43.305918	71.861185
687.175831	42.924311	71.866190
686.617197	48.573644	71.871194
685.715057	42.306179	71.876199
685.696244	37.309151	71.881204
685.240332	42.570642	71.886209
684.920883	43.025602	71.891214
683.648875	46.548852	71.896218
683.158077	45.665876	71.901223
682.636067	47.054700	71.906228
681.298307	46.518127	71.911233
680.845817	49.908876	71.916238
680.405117	54.087035	71.921242
679.475934	42.936845	71.926247
679.048954	45.064872	71.931252
678.158413	49.659945	71.936257
677.307998	40.090517	71.941262
676.697787	54.234264	71.946266
676.184111	50.098810	71.951271
676.164805	42.956986	71.956276
675.189023	49.224858	71.961281
674.095678	43.502493	71.966286
673.339550	55.101647	71.971290
672.493510	46.255769	71.976295
672.234263	43.959913	71.981300
671.828687	53.074278	71.986305
671.895081	52.828436	71.991310
670.743933	47.494899	71.996314
670.071487	48.887392	72.001319
669.205930	39.652121	72.006324
667.924958	38.034568	72.011329
667.514641	44.139648	72.016334
667.109048	46.462948	72.021338
666.643774	43.392830	72.026343
666.266395	43.004738	72.031348
665.237116	51.550992	72.036353
664.539451	42.554180	72.041358
664.204225	50.491688	72.046362
663.452090	51.359838	72.051367
662.276198	48.231472	72.056372
661.373843	55.016477	72.061377
660.941801	51.213994	72.066382
660.585053	55.436979	72.071386
660.004723	59.841156	72.076391
659.180672	44.061111	72.081396
658.118505	47.437108	72.086401
657.847556	50.203500	72.091406
657.288660	54.700709	72.096410
656.639267	47.688935	72.101415
656.193656	45.332645	72.106420
654.934565	47.198650	72.111425
654.806111	45.636266	72.116430
654.281330	54.726451	72.121434
653.784667	50.714790	72.126439
652.790304	45.773585	72.131444
651.896562	51.317315	72.136449
651.197311	44.400923	72.141454
649.505049	45.535529	72.146458
648.917475	49.153095	72.151463
649.911389	37.427145	72.156468
648.639030	48.291363	72.161473
648.313878	40.849065	72.166478
647.518012	53.099990	72.171482
646.344968	41.394388	72.176487
645.951457	43.089602	72.181492
645.186512	52.231194	72.186497
644.883292	51.034654	72.191502
644.126480	48.584847	72.196506
642.867251	52.799037	72.201511
642.459109	42.433096	72.206516
641.688610	50.449124	72.211521
641.634436	45.185012	72.216526
641.155737	47.205067	72.221530
639.935003	53.407550	72.226535
639.426520	38.834172	72.231540
638.505715	50.520349	72.236545
638.337635	47.930208	72.241550
637.521766	42.894484	72.246554
636.465536	43.900784	72.251559
635.615814	35.195282	72.256564
635.133879	49.377438	72.261569
634.836831	39.577040	72.266574
634.413076	42.286326	72.271578
633.339285	51.924491	72.276583
632.735591	44.604517	72.281588
631.911507	45.705643	72.286593
631.692496	44.663220	72.291598
630.958878	51.361689	72.296602
629.749056	47.807328	72.301607
629.554202	44.164729	72.306612
628.855454	45.380954	72.311617
628.446538	39.130050	72.316622
627.413973	45.913680	72.321626
626.088541	41.956390	72.326631
625.830996	39.194483	72.331636
625.303002	44.600556	72.336641
625.072688	40.525111	72.341646
624.563463	48.518480	72.346650
623.235567	43.344312	72.351655
622.978416	38.866515	72.356660
622.191996	45.575213	72.361665
621.813270	43.915191	72.366670
621.216881	41.660919	72.371674
619.802816	45.086949	72.376679
619.251572	40.661512	72.381684
618.692226	47.390119	72.386689
618.417093	45.737611	72.391694
618.139794	45.277511	72.396698
616.952427	44.157853	72.401703
616.207409	43.949589	72.406708
615.513109	39.309466	72.411713
615.089441	35.286097	72.416718
614.315393	44.518847	72.421722
613.760474	43.517793	72.426727
613.173986	42.697401	72.431732
612.398196	51.446928	72.436737
611.413907	39.470988	72.441742
610.576306	34.039940	72.446746
610.409736	48.329105	72.451751
609.900056	34.494060	72.456756
609.065052	41.371335	72.461761
608.229950	40.287636	72.466766
607.452276	37.621557	72.471770
606.951187	34.489298	72.476775
606.643034	45.606718	72.481780
605.869982	50.090887	72.486785
605.026152	31.797563	72.491790
604.508495	31.759150	72.496794
603.878437	39.462972	72.501799
602.915069	38.772281	72.506804
602.093165	43.129037	72.511809
601.735032	37.252310	72.516814
600.997077	37.046785	72.521818
600.281728	45.827794	72.526823
600.007502	42.602984	72.531828
598.653809	47.864756	72.536833
598.432673	37.087466	72.541838
597.909771	43.259597	72.546842
597.232358	48.177749	72.551847
596.826073	40.783700	72.556852
595.455370	41.882966	72.561857
594.961206	40.524157	72.566862
594.594010	43.661098	72.571866
593.998774	40.602205	72.576871
592.837776	38.184952	72.581876
592.011332	49.249078	72.586881
591.522736	38.503404	72.591886
591.208754	40.653915	72.596890
590.753378	44.345145	72.601895
590.447111	38.423613	72.606900
588.889899	53.650086	72.611905
588.787454	45.376261	72.616910
588.255469	42.612434	72.621914
587.142757	50.416720	72.626919
586.297488	49.305163	72.631924
585.339088	52.401304	72.636929
584.977621	40.941914	72.641934
584.592810	46.533444	72.646938
583.582718	39.659276	72.651943
583.493442	37.712442	72.656948
582.200481	45.879169	72.661953
582.048731	40.002212	72.666958
581.251879	39.570742	72.671962
580.736137	51.842353	72.676967
580.704385	43.891530	72.681972
579.099089	45.647144	72.686977
578.499347	37.442742	72.691982
578.114375	45.307458	72.696986
577.164211	46.356779	72.701991
576.467054	43.225751	72.706996
575.457189	48.933456	72.712001
575.276247	46.399993	72.717006
574.932897	49.301943	72.722010
574.129223	47.845781	72.727015
573.358552	43.393609	72.732020
572.550135	49.054563	72.737025
571.898397	41.810725	72.742030
571.147402	39.376515	72.747034
570.872278	48.026049	72.752039
570.031147	44.137366	72.757044
568.960539	40.543778	72.762049
568.563375	37.908030	72.767054
567.960750	40.152206	72.772058
567.801338	46.706902	72.777063
566.704641	32.688650	72.782068
565.878222	40.925826	72.787073
565.457085	39.595953	72.792078
565.253706	44.801154	72.797082
564.112786	44.144051	72.802087
563.181997	42.623229	72.807092
562.868960	37.874767	72.812097
562.520071	48.081456	72.817102
561.019247	40.986262	72.822106
560.211289	38.806537	72.827111
560.015517	43.902282	72.832116
559.240388	48.869153	72.837121
558.985314	39.537996	72.842126
558.583537	41.517246	72.847130
557.438590	49.758877	72.852135
556.851394	35.109016	72.857140
556.052959	40.059352	72.862145
556.061773	36.288712	72.867150
554.642738	45.140955	72.872154
553.432602	33.775282	72.877159
553.094747	33.075314	72.882164
552.492581	43.541305	72.887169
552.051216	37.880545	72.892174
551.751179	42.707987	72.897178
551.210189	43.233677	72.902183
550.566762	40.228045	72.907188
549.674124	39.334205	72.912193
549.417047	34.184997	72.917198
548.255779	45.875670	72.922202
547.010326	38.762777	72.927207
546.697522	36.757935	72.932212
545.887528	44.350101	72.937217
545.845343	51.655588	72.942222
545.394868	44.560811	72.947226
544.238329	49.125300	72.952231
543.529949	43.194124	72.957236
543.035349	49.302992	72.962241
542.743971	41.193382	72.967246
541.429879	44.954782	72.972250
540.663110	45.410614	72.977255
540.321169	45.957853	72.982260
539.736508	44.745602	72.987265
538.967262	35.149283	72.992270
538.053962	43.961054	72.997274
537.118380	45.090774	73.002279
536.640488	42.620826	73.007284
536.095267	41.434184	73.012289
536.085293	43.154077	73.017294
535.429090	47.701516	73.022298
534.188663	49.979987	73.027303
533.684666	41.448546	73.032308
532.965198	44.510070	73.037313
532.866028	41.286454	73.042318
531.755618	37.613254	73.047322
530.796522	46.468004	73.052327
530.691260	31.751759	73.057332
529.862417	41.826746	73.062337
529.037847	37.240935	73.067342
527.986986	33.663711	73.072346
527.338145	36.418675	73.077351
526.945735	40.540014	73.082356
526.564188	37.038356	73.087361
526.285085	31.094419	73.092366
524.947456	35.361930	73.097370
524.943993	31.395249	73.102375
524.395238	27.746202	73.107380
522.927334	38.896950	73.112385
522.212490	36.623518	73.117390
521.810859	29.993645	73.122394
521.089274	32.960010	73.127399
520.704386	35.504756	73.132404
519.827393	40.532501	73.137409
518.821013	38.557300	73.142414
518.696639	35.302086	73.147418
518.064809	31.612409	73.152423
517.491533	28.361488	73.157428
516.332631	32.928356	73.162433
515.717311	31.383488	73.167438
515.350184	30.647883	73.172442
514.251754	35.496084	73.177447
513.626207	30.503170	73.182452
512.761729	37.503918	73.187457
512.183216	34.183241	73.192462
512.152130	33.517547	73.197466
511.453740	40.596015	73.202471
510.874889	35.705619	73.207476
509.713124	33.753099	73.212481
509.259019	34.870186	73.217486
508.882100	38.388905	73.222490
508.248127	29.485824	73.227495
506.957124	34.794893	73.232500
506.139298	38.143651	73.237505
505.678493	36.736113	73.242510
505.232504	26.857062	73.247514
504.516318	38.451733	73.252519
504.490633	32.496345	73.257524
503.013057	29.638000	73.262529
502.378483	36.134380	73.267534
501.833177	40.055353	73.272538
501.188667	40.890875	73.277543
501.327374	24.868569	73.282548
499.977793	37.410145	73.287553
499.111599	34.183763	73.292558
498.860824	41.121982	73.297562
498.360149	40.882919	73.302567
497.131229	36.241673	73.307572
496.144913	40.042042	73.312577
495.912594	35.727363	73.317582
495.383238	35.108370	73.322586
494.819673	35.568070	73.327591
494.562331	35.921616	73.332596
493.252450	37.700052	73.337601
492.868733	35.189502	73.342606
492.256099	40.459302	73.347610
491.453685	48.989201	73.352615
490.766601	47.251775	73.357620
490.191665	47.454097	73.362625
489.587768	43.677535	73.367630
489.031404	45.139759	73.372634
487.706811	44.376393	73.377639
487.375700	36.701077	73.382644
486.426829	45.042136	73.387649
486.207075	35.042216	73.392654
485.845001	43.124835	73.397658
484.107519	47.875326	73.402663
483.568183	38.338696	73.407668
483.218746	39.330093	73.412673
482.462269	35.657044	73.417678
482.589116	38.385271	73.422682
482.139818	36.982079	73.427687
481.460654	47.711122	73.432692
480.170229	50.353021	73.437697
479.674593	51.553013	73.442702
478.636669	41.509748	73.447706
477.820658	49.855278	73.452711
477.009735	38.290967	73.457716
476.459842	45.587531	73.462721
476.003224	39.719802	73.467726
475.736955	39.348211	73.472730
475.435365	48.168057	73.477735
474.682272	39.738521	73.482740
473.489742	39.151466	73.487745
473.135246	40.288590	73.492750
472.498169	41.585446	73.497754
471.154385	41.983464	73.502759
470.365040	36.155387	73.507764
469.970906	37.779669	73.512769
469.428744	37.891909	73.517774
469.280314	40.944791	73.522778
468.799811	46.404704	73.527783
467.951979	32.530544	73.532788
466.707313	44.359457	73.537793
466.326075	43.319582	73.542798
465.612499	38.991853	73.547802
464.705906	37.249418	73.552807
464.154133	38.459425	73.557812
463.207707	47.781327	73.562817
462.955718	38.809240	73.567822
462.930977	36.734123	73.572826
462.149796	55.849372	73.577831
461.159302	38.977330	73.582836
460.439211	43.106669	73.587841
459.874630	42.865931	73.592846
458.818606	42.598887	73.597850
457.608557	46.235511	73.602855
457.572378	45.432936	73.607860
456.734420	44.142135	73.612865
456.858681	44.015841	73.617870
456.523607	42.594657	73.622874
455.252554	45.226926	73.627879
454.480454	45.816703	73.632884
454.056877	42.645525	73.637889
453.176131	42.620404	73.642894
452.332037	46.321415	73.647898
451.436500	47.042471	73.652903
451.148419	47.498386	73.657908
450.422689	44.015455	73.662913
449.505247	46.949082	73.667918
449.024844	43.184521	73.672922
448.051814	42.997594	73.677927
447.830549	37.127827	73.682932
446.944407	40.507247	73.687937
447.016830	44.727344	73.692942
445.809223	43.181751	73.697946
444.780013	48.981207	73.702951
444.768935	50.776284	73.707956
443.636668	50.874789	73.712961
443.278876	49.711693	73.717966
442.642601	48.510273	73.722970
441.534230	55.136408	73.727975
441.371613	44.716985	73.732980
440.472969	46.375229	73.737985
440.220761	43.888329	73.742990
439.586163	41.768518	73.747994
438.233969	44.693364	73.752999
438.213158	33.296809	73.758004
437.274339	33.229146	73.763009
436.432692	37.675352	73.768014
435.549249	42.190692	73.773018
434.678987	46.010262	73.778023
434.505789	39.589132	73.783028
434.274120	45.334411	73.788033
433.601511	31.476812	73.793038
432.777124	34.684213	73.798042
431.513383	46.406670	73.803047
431.257502	42.439039	73.808052
430.734847	50.747722	73.813057
430.317537	44.268561	73.818062
429.340982	45.086000	73.823066
428.409236	50.590483	73.828071
428.352950	43.654346	73.833076
427.453197	35.855449	73.838081
426.535177	35.830800	73.843086
425.753638	39.352551	73.848090
425.213505	41.895883	73.853095
424.904005	38.905675	73.858100
424.123129	45.928817	73.863105
423.102202	50.929931	73.868110
422.279853	44.220990	73.873114
421.834679	41.137592	73.878119
421.354078	33.773678	73.883124
421.216969	41.249752	73.888129
420.506999	45.063564	73.893134
419.765006	43.616201	73.898138
418.734612	46.623265	73.903143
418.281996	38.453286	73.908148
416.923898	43.667303	73.913153
416.617683	35.241724	73.918158
416.057079	34.807294	73.923162
415.879760	41.723450	73.928167
415.086233	32.977197	73.933172
413.949855	33.975176	73.938177
413.230356	35.573910	73.943182
412.735527	42.259101	73.948186
411.984856	45.500449	73.953191
411.983452	34.245431	73.958196
410.475177	37.498592	73.963201
410.358238	37.384423	73.968206
409.929459	36.477430	73.973210
409.037913	36.614422	73.978215
408.088433	37.365254	73.983220
406.898487	44.463237	73.988225
406.675523	44.457233	73.993230
406.470383	37.834752	73.998234
405.673759	44.118927	74.003239
404.857129	42.032291	74.008244
403.924337	46.749898	74.013249
403.331546	53.083614	74.018254
402.872206	41.357629	74.023258
402.342338	51.088122	74.028263
402.371641	40.346097	74.033268
400.912263	41.877431	74.038273
400.306193	39.290134	74.043278
399.828803	38.389104	74.048282
398.688699	53.209408	74.053287
398.188561	48.896819	74.058292
397.312595	48.474992	74.063297
397.259861	43.718252	74.068302
396.856397	46.723268	74.073306
395.047859	55.477310	74.078311
394.299618	44.397248	74.083316
393.548276	51.663608	74.088321
393.136719	47.520171	74.093326
392.832674	47.588849	74.098330
392.451565	48.521342	74.103335
392.279490	35.809872	74.108340
391.502447	46.233604	74.113345
390.440185	38.061932	74.118350
390.226381	42.027148	74.123354
389.398916	43.944371	74.128359
388.323601	46.901117	74.133364
387.523853	48.412956	74.138369
386.911521	40.456264	74.143374
386.934855	45.336047	74.148378
385.837220	46.819206	74.153383
385.098444	41.201545	74.158388
384.233150	43.007628	74.163393
383.839965	39.952822	74.168398
382.807739	35.621303	74.173402
381.762240	45.632387	74.178407
381.669059	43.096527	74.183412
380.975459	45.301450	74.188417
380.638387	42.152165	74.193422
380.408272	35.213855	74.198426
379.124188	52.484741	74.203431
378.214457	41.889045	74.208436
377.656711	48.707384	74.213441
377.334038	47.986670	74.218446
376.783769	50.222289	74.223450
375.551574	43.325063	74.228455
375.201630	39.308431	74.233460
374.763933	45.143094	74.238465
374.437659	37.527752	74.243470
373.049246	39.108113	74.248474
372.262851	50.990338	74.253479
372.119964	39.990081	74.258484
371.230000	50.220024	74.263489
370.338085	40.460834	74.268494
369.769262	42.751340	74.273498
368.604965	48.135433	74.278503
367.913488	48.165517	74.283508
368.074864	45.317627	74.288513
367.827903	40.978233	74.293518
366.994056	43.576249	74.298522
365.798422	49.762640	74.303527
365.163696	44.394371	74.308532
364.804778	43.093327	74.313537
363.723475	40.103564	74.318542
362.685480	47.582069	74.323546
362.045325	43.073234	74.328551
361.828523	40.237266	74.333556
361.482576	43.206770	74.338561
361.014565	39.650480	74.343566
360.736629	45.985889	74.348570
359.359160	44.148135	74.353575
359.254341	44.980781	74.358580
357.717838	51.566625	74.363585
356.608976	49.955188	74.368590
356.349031	40.114928	74.373594
355.877880	42.943268	74.378599
355.820835	42.330575	74.383604
355.114157	46.210932	74.388609
354.556305	36.928542	74.393614
353.693986	43.602906	74.398618
352.666273	45.222501	74.403623
352.007908	33.855097	74.408628
350.391122	41.008875	74.413633
350.133852	39.969868	74.418638
349.618016	42.320765	74.423642
348.860208	44.747867	74.428647
348.952224	45.536910	74.433652
348.240840	41.021735	74.438657
348.038921	46.152871	74.443662
346.660764	40.053126	74.448666
346.013045	49.502256	74.453671
345.734057	47.838192	74.458676
345.036860	48.485408	74.463681
344.276192	45.487667	74.468686
343.401186	40.166506	74.473690
342.239968	44.681311	74.478695
342.068646	45.350103	74.483700
341.709103	48.758097	74.488705
340.886762	44.222072	74.493710
340.045506	40.428194	74.498714
339.292969	51.139425	74.503719
339.044540	45.395499	74.508724
338.388701	45.043713	74.513729
337.230506	50.804112	74.518734
336.734050	49.685712	74.523738
335.993336	42.505330	74.528743
335.700716	40.497441	74.533748
335.450346	51.020375	74.538753
334.956039	41.517898	74.543758
333.848255	40.096141	74.548762
331.989752	47.869214	74.553767
332.053003	36.064340	74.558772
330.949707	42.152413	74.563777
330.081260	35.339697	74.568782
330.333905	32.638788	74.573786
329.692360	42.290922	74.578791
329.578428	34.652615	74.583796
328.933283	37.567221	74.588801
327.462482	41.286455	74.593806
327.022541	41.873004	74.598810
326.192622	40.900568	74.603815
325.839948	41.011135	74.608820
324.702743	43.335907	74.613825
324.081300	43.903830	74.618830
323.749898	37.465226	74.623834
323.195159	44.479221	74.628839
322.355861	36.724461	74.633844
321.147549	45.571028	74.638849
320.672289	32.945878	74.643854
320.564167	46.037296	74.648858
319.883996	48.800418	74.653863
319.501064	34.764525	74.658868
318.425092	44.179689	74.663873
317.434366	40.132767	74.668878
317.130070	38.213718	74.673882
316.260598	38.192217	74.678887
316.073594	35.543371	74.683892
315.059864	37.490162	74.688897
314.266350	40.490985	74.693902
313.785920	33.160218	74.698906
313.099429	43.773288	74.703911
312.171102	45.030878	74.708916
311.256908	37.716036	74.713921
311.030002	38.251864	74.718926
310.561618	38.355029	74.723930
310.204219	39.735409	74.728935
309.808854	39.595942	74.733940
308.627515	44.930074	74.738945
308.044170	42.411524	74.743950
306.816202	38.509865	74.748954
306.034503	46.932022	74.753959
305.465926	34.886912	74.758964
305.218745	40.482092	74.763969
304.649106	43.045096	74.768974
304.187460	39.222476	74.773978
303.160116	49.707272	74.778983
302.810835	33.997164	74.783988
302.072136	45.161914	74.788993
300.982256	40.834376	74.793998
300.206217	33.338370	74.799002
299.579299	47.948752	74.804007
299.158927	41.774857	74.809012
298.525921	46.521618	74.814017
297.869323	46.266278	74.819022
297.430505	42.055690	74.824026
296.122561	47.779003	74.829031
295.644504	40.939247	74.834036
295.483830	44.796285	74.839041
295.001841	44.879680	74.844046
294.119030	37.480521	74.849050
293.171339	47.855355	74.854055
292.547398	37.134525	74.859060
291.925482	42.763147	74.864065
291.234642	39.077307	74.869070
290.316434	42.506060	74.874074
289.545802	47.745725	74.879079
289.127885	40.455163	74.884084
288.524187	47.536760	74.889089
288.528608	45.274685	74.894094
287.651261	39.914467	74.899098
286.468336	52.528964	74.904103
285.962939	48.331366	74.909108
285.533955	48.357127	74.914113
285.190774	51.053809	74.919118
284.269892	47.189515	74.924122
283.589644	52.367904	74.929127
282.743255	42.974333	74.934132
281.284721	44.415958	74.939137
280.740668	42.821805	74.944142
280.438146	42.160800	74.949146
279.771736	35.058482	74.954151
279.837020	35.228065	74.959156
278.792271	42.299209	74.964161
278.486156	40.189829	74.969166
277.804090	44.468187	74.974170
276.648024	47.288015	74.979175
276.199678	35.137442	74.984180
275.145999	38.126813	74.989185
274.030747	42.018000	74.994190
273.722829	42.973480	74.999194
273.049175	44.479513	75.004199
273.159479	35.305237	75.009204
272.652913	42.400971	75.014209
271.839868	37.748904	75.019214
270.789627	35.248813	75.024218
269.913702	46.799432	75.029223
269.637187	40.769822	75.034228
269.135792	46.142145	75.039233
268.038455	46.206680	75.044238
267.535339	34.624016	75.049242
266.708792	41.321860	75.054247
266.514570	43.595140	75.059252
265.297094	44.290099	75.064257
264.404257	39.800122	75.069262
264.053492	38.971345	75.074266
263.342011	43.148963	75.079271
263.215342	40.601088	75.084276
262.802865	40.243913	75.089281
261.323984	39.081954	75.094286
260.902982	33.362096	75.099290
260.380566	41.588241	75.104295
259.767743	36.819362	75.109300
258.677559	44.421687	75.114305
258.147730	40.151315	75.119310
257.949401	42.244125	75.124314
257.036474	43.708677	75.129319
256.748603	33.103929	75.134324
255.295295	42.675351	75.139329
254.782989	31.117161	75.144334
254.567230	27.705929	75.149338
253.516539	33.263185	75.154343
252.556111	33.914088	75.159348
252.266250	43.177149	75.164353
251.494227	40.994087	75.169358
250.983388	29.956668	75.174362
250.717370	35.337588	75.179367
249.851575	34.738399	75.184372
248.628307	42.300382	75.189377
248.244449	33.278703	75.194382
247.862545	39.901913	75.199386
247.450695	38.810467	75.204391
245.906619	38.466085	75.209396
245.307981	40.191354	75.214401
244.891761	35.625212	75.219406
244.947154	39.212727	75.224410
243.947128	43.314682	75.229415
242.972117	40.639080	75.234420
242.359226	46.170244	75.239425
241.620493	37.561476	75.244430
241.034794	42.959302	75.249434
240.163545	47.007609	75.254439
239.606827	34.325391	75.259444
238.658439	43.953550	75.264449
238.052987	44.172975	75.269454
237.841872	35.360488	75.274458
237.192224	45.289130	75.279463
237.173514	45.032610	75.284468
235.701430	41.920796	75.289473
235.219058	38.504346	75.294478
234.807836	41.798445	75.299482
234.116453	43.931168	75.304487
233.007655	36.997053	75.309492
232.525029	46.486566	75.314497
231.697368	45.178255	75.319502
231.407860	33.268476	75.324506
230.309006	40.643357	75.329511
229.665425	38.214481	75.334516
228.804952	47.512199	75.339521
228.129151	47.080961	75.344526
228.286777	40.097914	75.349530
227.608300	36.989405	75.354535
226.766159	39.373745	75.359540
225.631632	44.552246	75.364545
225.477512	43.545300	75.369550
225.275263	36.398956	75.374554
223.631544	45.077819	75.379559
223.175989	41.494151	75.384564
222.132470	37.271972	75.389569
221.750703	41.208746	75.394574
221.383238	33.899288	75.399578
220.017991	42.633832	75.404583
219.656021	35.343956	75.409588
219.378062	36.917554	75.414593
218.611348	42.627840	75.419598
218.682078	28.417114	75.424602
217.451290	43.856088	75.429607
216.665298	31.640258	75.434612
215.880678	39.643733	75.439617
215.275528	40.645429	75.444622
214.744233	31.420886	75.449626
213.257872	37.239135	75.454631
213.222024	38.577823	75.459636
212.825801	38.146424	75.464641
211.968108	41.112475	75.469646
211.948045	31.524001	75.474650
210.963723	38.417438	75.479655
210.394097	31.324599	75.484660
209.921567	34.910242	75.489665
208.676666	41.679410	75.494670
207.945594	35.631418	75.499674
207.191422	41.175749	75.504679
207.304045	37.088136	75.509684
205.922350	38.036246	75.514689
205.031841	41.706566	75.519694
204.913236	41.598214	75.524698
204.142833	46.739170	75.529703
203.692258	37.290407	75.534708
202.625011	35.364002	75.539713
201.863406	44.349133	75.544718
201.527244	37.138909	75.549722
200.358421	43.216923	75.554727
200.389336	37.849843	75.559732
199.682681	35.588486	75.564737
198.299045	35.079653	75.569742
197.919216	35.517759	75.574746
197.237376	43.775577	75.579751
196.870065	32.305038	75.584756
196.387457	45.123550	75.589761
195.532902	47.144915	75.594766
194.813559	38.963861	75.599770
194.098112	44.766014	75.604775
193.578538	35.839050	75.609780
193.422520	43.202308	75.614785
191.786855	45.104165	75.619790
191.505383	42.286401	75.624794
190.775161	46.444742	75.629799
190.461351	41.799081	75.634804
189.896055	42.036495	75.639809
188.622093	39.821469	75.644814
188.241355	37.017564	75.649818
187.409588	49.786993	75.654823
187.118450	37.895261	75.659828
186.472587	43.015659	75.664833
185.013578	44.633435	75.669838
184.588558	35.662241	75.674842
184.033315	32.402756	75.679847
183.874302	27.802007	75.684852
183.680572	36.523615	75.689857
182.361096	43.853434	75.694862
181.832710	39.032203	75.699866
180.952281	42.206224	75.704871
180.198320	38.147959	75.709876
178.957759	34.652290	75.714881
178.462694	44.454572	75.719886
178.273938	35.225786	75.724890
177.334744	45.216301	75.729895
177.310382	37.500291	75.734900
177.102788	46.074290	75.739905
175.784171	48.009824	75.744910
175.188724	40.133173	75.749914
174.472979	37.852459	75.754919
173.851083	33.983518	75.759924
172.833101	39.937395	75.764929
172.308247	37.664613	75.769934
171.851428	33.634751	75.774938
171.216739	42.110262	75.779943
170.779547	34.158331	75.784948
169.516781	35.071460	75.789953
168.901186	33.386172	75.794958
168.671863	32.893406	75.799962
168.028494	40.109298	75.804967
166.989465	37.923475	75.809972
166.014983	41.354000	75.814977
165.339033	38.470844	75.819982
165.406020	36.636574	75.824986
164.308844	37.287253	75.829991
164.225009	31.671839	75.834996
162.917994	34.131537	75.840001
162.503961	40.981690	75.845006
162.125832	32.227844	75.850010
161.252349	40.417863	75.855015
160.397969	33.939075	75.860020
159.865414	33.291066	75.865025
159.637855	34.793267	75.870030
158.681737	36.431020	75.875034
157.562075	46.368796	75.880039
156.860144	40.260558	75.885044
156.346103	43.318487	75.890049
156.190752	52.446787	75.895054
155.977558	47.260492	75.900058
154.035866	51.208911	75.905063
153.866449	33.560361	75.910068
152.893101	45.962899	75.915073
152.396022	35.843214	75.920078
152.274742	37.597574	75.925082
151.182753	41.416118	75.930087
150.040815	35.163853	75.935092
149.729052	49.490089	75.940097
149.250866	47.949394	75.945102
149.328420	35.544495	75.950106
148.035701	50.175860	75.955111
147.690557	34.134707	75.960116
146.552943	44.607632	75.965121
146.052598	42.190529	75.970126
145.069854	38.598175	75.975130
144.127907	46.137609	75.980135
143.911752	41.612572	75.985140
143.398145	41.507205	75.990145
142.855330	47.187801	75.995150
142.397409	48.953296	76.000154
141.411695	50.855848	76.005159
140.832627	45.752012	76.010164
140.341229	51.764038	76.015169
139.347051	45.669193	76.020174
138.664713	49.579347	76.025178
137.488083	47.125031	76.030183
137.274430	46.517087	76.035188
136.933192	48.954511	76.040193
136.075749	38.802664	76.045198
135.051132	45.044641	76.050202
134.681788	50.802468	76.055207
133.997667	39.647942	76.060212
133.761260	44.189366	76.065217
133.277261	45.752109	76.070222
132.146411	37.623854	76.075226
131.226110	44.369364	76.080231
130.938690	34.524381	76.085236
130.522439	28.659266	76.090241
129.290273	44.239002	76.095246
128.522262	40.011456	76.100250
128.022463	50.149270	76.105255
127.402029	38.868572	76.110260
126.829004	35.581750	76.115265
125.700667	39.899131	76.120270
125.314411	42.620965	76.125274
124.604163	48.189748	76.130279
123.969154	40.259500	76.135284
123.540669	43.660769	76.140289
123.176888	41.988367	76.145294
122.376061	41.362671	76.150298
121.231364	39.899140	76.155303
120.844968	38.039970	76.160308
120.162607	40.170370	76.165313
119.828736	34.380337	76.170318
118.796748	39.274058	76.175322
118.065533	37.224939	76.180327
117.553889	39.390016	76.185332
117.162794	40.655008	76.190337
116.500768	41.808168	76.195342
115.587804	35.317330	76.200346
114.475576	44.986616	76.205351
114.227441	38.649811	76.210356
113.996262	39.155198	76.215361
113.064510	42.720898	76.220366
112.708214	37.434020	76.225370
111.666147	36.827974	76.230375
111.136696	41.159916	76.235380
109.638279	29.402551	76.240385
109.081662	34.998674	76.245390
108.514008	32.319581	76.250394
107.798480	33.972146	76.255399
107.616014	36.168021	76.260404
107.375031	40.804961	76.265409
106.747840	37.313099	76.270414
106.423859	29.880161	76.275418
105.419196	32.114367	76.280423
105.185404	38.360497	76.285428
103.770306	38.425077	76.290433
103.120887	40.746399	76.295438
102.389965	34.346322	76.300442
101.005011	39.413446	76.305447
100.319313	42.551726	76.310452
100.252362	39.609568	76.315457
99.600166	47.760080	76.320462
99.594140	44.334216	76.325466
98.696591	40.423339	76.330471
98.027231	37.891544	76.335476
97.070496	42.098989	76.340481
96.135141	37.799884	76.345486
95.957619	39.094574	76.350490
95.405117	40.284615	76.355495
94.490980	33.336118	76.360500
93.615744	34.920151	76.365505
92.950210	40.883086	76.370510
92.814636	39.038545	76.375514
91.674147	36.943946	76.380519
90.757130	36.471983	76.385524
90.251145	43.965889	76.390529
89.733720	42.034060	76.395534
89.263365	35.129079	76.400538
89.103450	37.639227	76.405543
87.934138	32.940525	76.410548
87.043293	36.751831	76.415553
86.488030	39.124113	76.420558
86.521413	33.035874	76.425562
84.740692	41.518799	76.430567
84.576036	37.116775	76.435572
83.889290	36.813743	76.440577
83.063587	41.946825	76.445582
82.745308	36.518441	76.450586
81.824066	38.994518	76.455591
80.627415	39.581356	76.460596
79.995926	41.466213	76.465601
79.396241	44.039126	76.470606
79.554779	29.066964	76.475610
78.782726	45.881424	76.480615
78.442509	36.209307	76.485620
77.244750	34.342806	76.490625
76.241432	44.570493	76.495630
76.269488	38.699468	76.500634
75.376305	37.971201	76.505639
74.856949	32.462827	76.510644
74.086933	32.602730	76.515649
72.988628	33.435192	76.520654
72.858987	32.399584	76.525658
71.921271	42.771935	76.530663
70.784367	32.089771	76.535668
70.346481	33.268847	76.540673
70.003423	44.110000	76.545678
69.771095	32.346757	76.550682
69.230631	40.900848	76.555687
68.514410	44.169884	76.560692
67.611501	44.139557	76.565697
66.558524	39.805365	76.570702
65.830849	36.091938	76.575706
64.251249	40.906671	76.580711
64.179138	39.875804	76.585716
64.027848	45.855966	76.590721
63.530848	41.455267	76.595726
63.161669	33.091853	76.600730
62.352666	32.137986	76.605735
61.705565	41.435445	76.610740
60.677133	38.739837	76.615745
60.123889	41.064805	76.620750
59.694243	32.845172	76.625754
58.872902	38.272357	76.630759
58.345959	37.446173	76.635764
57.802739	38.373327	76.640769
56.619316	47.205803	76.645774
55.702941	36.430572	76.650778
54.870020	42.609697	76.655783
54.655332	42.442038	76.660788
54.286539	43.616769	76.665793
53.610499	44.256452	76.670798
53.624908	36.146200	76.675802
52.073261	42.195145	76.680807
51.979135	40.562170	76.685812
51.060220	43.607028	76.690817
49.511004	46.166701	76.695822
48.830218	37.523969	76.700826
48.487758	49.766250	76.705831
48.586183	46.209986	76.710836
47.479770	37.304724	76.715841
47.446925	48.723443	76.720846
46.735941	35.382108	76.725850
45.538270	43.489574	76.730855
44.750009	37.666935	76.735860
44.743774	37.444591	76.740865
43.179002	55.330045	76.745870
42.379801	35.980924	76.750874
41.949613	46.432043	76.755879
41.305315	40.703924	76.760884
40.901070	48.697068	76.765889
40.186723	52.989275	76.770894
40.359300	46.491534	76.775898
39.171593	41.970856	76.780903
38.368539	42.746785	76.785908
37.903687	41.173425	76.790913
36.946111	38.669346	76.795918
36.511043	35.708601	76.800922
35.505281	44.707579	76.805927
35.265299	39.487210	76.810932
34.891279	32.945436	76.815937
33.671344	39.185786	76.820942
33.292581	33.587002	76.825946
32.430296	46.935182	76.830951
31.823527	35.819921	76.835956
30.593879	38.067455	76.840961
29.845651	35.930091	76.845966
29.671763	29.576623	76.850970
28.902532	34.599375	76.855975
28.616798	29.031220	76.860980
28.088033	34.148523	76.865985
26.609119	36.386694	76.870990
26.241867	35.157369	76.875994
25.402606	45.549553	76.880999
25.266046	35.188490	76.886004
24.934463	44.314231	76.891009
23.539756	46.835184	76.896014
23.067955	33.105108	76.901018
21.820286	37.441390	76.906023
21.743887	31.562229	76.911028
21.572142	39.915347	76.916033
20.542741	44.817721	76.921038
20.006892	41.804392	76.926042
18.793185	45.815531	76.931047
18.479940	43.191903	76.936052
18.228880	44.541043	76.941057
17.401441	48.133478	76.946062
16.673697	39.712739	76.951066
15.577279	43.045784	76.956071
15.169987	35.082439	76.961076
13.831469	37.482056	76.966081
13.103096	39.329062	76.971086
13.447213	37.494246	76.976090
12.564376	43.847319	76.981095
12.111589	44.761341	76.986100
11.850343	40.735070	76.991105
10.582239	46.684889	76.996110
9.995012	34.750810	77.001114
9.355711	41.013576	77.006119
8.819957	38.389813	77.011124
7.678972	35.805091	77.016129
6.810940	44.918212	77.021134
6.567589	35.093324	77.026139
6.229335	40.285328	77.031143
5.829647	41.015783	77.036148
5.121453	41.009711	77.041153
4.020880	43.220122	77.046158